Fri Aug 26 14:07:45 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.708031	105.962668	0.000000
0.840361	104.050217	0.005005
1.072003	106.624196	0.010010
0.734527	99.697721	0.015014
0.478498	101.705405	0.020019
0.272401	98.763674	0.025024
0.572928	102.614538	0.030029
0.191704	95.128581	0.035034
-0.294114	85.368421	0.040038
0.030307	82.565548	0.045043
-0.359984	72.005935	0.050048
-0.294874	60.128943	0.055053
-0.699896	51.609030	0.060058
-1.058561	44.859877	0.065062
-1.902622	38.578593	0.070067
-2.413457	32.371976	0.075072
-2.341714	22.439622	0.080077
-2.557514	26.054496	0.085082
-2.455535	18.211773	0.090086
-2.729979	19.137184	0.095091
-2.969165	11.676601	0.100096
-3.549374	-1.033151	0.105101
-4.166986	0.005798	0.110106
-4.342564	1.165743	0.115110
-4.083904	9.895120	0.120115
-4.518142	2.189674	0.125120
-4.721284	-8.579357	0.130125
-5.501505	-0.251363	0.135130
-5.514799	-3.577425	0.140134
-5.498176	-11.036699	0.145139
-6.426877	-4.609084	0.150144
-6.957647	-12.482985	0.155149
-7.211914	-6.695034	0.160154
-6.858345	-2.045722	0.165158
-6.771387	-3.846697	0.170163
-7.406728	-2.036222	0.175168
-7.290103	-15.610569	0.180173
-7.193747	-2.357228	0.185178
-7.736324	-4.395533	0.190182
-8.497848	-6.444040	0.195187
-8.724358	-3.890489	0.200192
-8.753948	-5.474009	0.205197
-8.850996	-6.044150	0.210202
-9.165061	-9.411963	0.215206
-9.505574	-9.798670	0.220211
-9.698524	-11.805992	0.225216
-9.683137	-11.865310	0.230221
-10.620345	-6.164009	0.235226
-11.214934	-6.349811	0.240230
-11.471323	-4.661611	0.245235
-11.205811	-3.658925	0.250240
-10.949758	-3.445677	0.255245
-11.090598	-4.907475	0.260250
-11.566697	-7.911551	0.265254
-11.787413	-11.796917	0.270259
-12.732168	-5.335166	0.275264
-12.655143	-10.200165	0.280269
-13.066323	-10.635978	0.285274
-12.869726	-6.775284	0.290278
-12.944108	-13.252312	0.295283
-13.578498	-17.158687	0.300288
-13.914324	-11.693385	0.305293
-14.228368	-5.446890	0.310298
-14.507912	-5.213524	0.315302
-14.044111	-11.106818	0.320307
-14.758746	-9.834471	0.325312
-15.007534	-2.984388	0.330317
-15.467147	-5.734775	0.335322
-15.577362	-3.955442	0.340326
-15.576590	-7.350130	0.345331
-15.963341	-3.930101	0.350336
-16.691114	-16.642174	0.355341
-17.070084	-8.215312	0.360346
-17.231623	-10.259161	0.365350
-17.172206	-10.546790	0.370355
-17.030783	-13.314828	0.375360
-16.993370	-18.009148	0.380365
-17.633722	-14.249090	0.385370
-18.224120	-10.990338	0.390374
-18.538603	-10.276986	0.395379
-19.153012	-8.049006	0.400384
-18.730549	-11.196148	0.405389
-18.681253	-8.378667	0.410394
-18.798825	-9.236668	0.415398
-19.495052	-4.683325	0.420403
-20.244714	-6.581823	0.425408
-20.359429	-10.151510	0.430413
-20.366734	-10.672351	0.435418
-20.167066	-1.829396	0.440422
-20.516877	-8.431215	0.445427
-21.032789	-6.955699	0.450432
-21.051802	-5.911878	0.455437
-21.231537	-4.118557	0.460442
-21.795369	-3.198709	0.465446
-22.397633	-13.244391	0.470451
-22.954564	-2.341160	0.475456
-22.638505	-18.059869	0.480461
-23.184205	-11.407161	0.485466
-23.091179	-15.290757	0.490470
-22.749266	-8.595920	0.495475
-23.592841	-4.946583	0.500480
-24.169176	-8.355816	0.505485
-24.402980	-11.957579	0.510490
-24.278003	-2.410158	0.515494
-24.165916	-11.855244	0.520499
-24.115716	-5.064368	0.525504
-25.264388	-13.949337	0.530509
-25.696579	-9.155541	0.535514
-25.951204	-11.384205	0.540518
-25.693905	-13.274974	0.545523
-26.407098	-7.301679	0.550528
-26.200497	-16.192022	0.555533
-26.824665	-4.038176	0.560538
-27.149947	-5.047328	0.565542
-27.035879	-14.173192	0.570547
-27.301868	-9.737457	0.575552
-27.293800	-15.512337	0.580557
-27.424229	-5.425296	0.585562
-28.408414	-6.923460	0.590566
-28.445573	-0.005089	0.595571
-28.785633	-3.372019	0.600576
-28.776565	-10.077168	0.605581
-28.866197	-3.179102	0.610586
-29.120570	-2.690237	0.615590
-29.819195	-9.332654	0.620595
-30.354976	-0.413155	0.625600
-30.464787	-2.639059	0.630605
-30.164955	-6.064491	0.635610
-30.440859	-8.780207	0.640614
-30.224261	-19.250762	0.645619
-31.169090	-7.749321	0.650624
-31.701729	-12.389686	0.655629
-31.618382	-2.494110	0.660634
-31.676655	-10.754777	0.665638
-31.663985	-12.025348	0.670643
-32.901386	-5.733161	0.675648
-33.036201	-14.285619	0.680653
-33.196528	-9.730298	0.685658
-33.295189	-4.048829	0.690662
-33.286555	-13.098169	0.695667
-33.419838	-14.646560	0.700672
-33.529671	-5.470692	0.705677
-34.017337	-4.293793	0.710682
-34.703794	-3.104924	0.715686
-34.971007	-7.337378	0.720691
-35.114496	-9.036036	0.725696
-34.978771	-6.646450	0.730701
-34.977650	-5.169180	0.735706
-35.340158	-4.103513	0.740710
-35.860704	-8.486343	0.745715
-36.282827	-4.715970	0.750720
-36.260916	-8.616967	0.755725
-36.159516	-8.268913	0.760730
-37.113755	-3.378016	0.765734
-37.398324	-9.952028	0.770739
-37.947432	3.170866	0.775744
-37.416169	-9.876440	0.780749
-37.942840	-6.497899	0.785754
-38.047617	-8.930223	0.790758
-37.852778	-21.953611	0.795763
-38.816193	-4.906576	0.800768
-39.080063	-17.314401	0.805773
-39.014720	-6.546023	0.810778
-39.280130	-7.089951	0.815782
-39.324386	-9.749988	0.820787
-40.169298	-11.206562	0.825792
-40.928024	-2.739553	0.830797
-40.956700	-8.714351	0.835802
-40.565915	-7.291425	0.840806
-40.988700	-11.600892	0.845811
-41.206444	-2.085530	0.850816
-41.026295	-7.583495	0.855821
-41.109828	-0.233977	0.860826
-41.897024	-5.935657	0.865830
-42.031944	-15.551081	0.870835
-42.476416	-6.683766	0.875840
-42.567532	-10.728510	0.880845
-42.218639	-13.136559	0.885850
-43.311410	-3.155938	0.890854
-43.129423	-14.263326	0.895859
-44.112102	-5.331194	0.900864
-44.044959	-13.589241	0.905869
-44.250991	-10.567498	0.910874
-44.333544	-10.317349	0.915878
-44.948403	-14.305855	0.920883
-45.494990	-4.897475	0.925888
-45.427766	-12.032442	0.930893
-45.467102	-2.468930	0.935898
-45.482316	-12.017576	0.940902
-45.252686	-22.025102	0.945907
-45.715154	-3.281260	0.950912
-45.984669	-9.092014	0.955917
-46.117071	-8.957485	0.960922
-46.963787	-0.533721	0.965926
-47.593566	-17.076402	0.970931
-48.005592	5.962148	0.975936
-48.168432	-11.633969	0.980941
-48.400518	-7.902677	0.985946
-48.063706	-16.158418	0.990950
-47.753281	-13.833997	0.995955
-48.352676	-8.675659	1.000960
-48.492443	-3.446518	1.005965
-49.162787	-15.316509	1.010970
-49.534843	0.401473	1.015974
-49.727782	-9.685795	1.020979
-49.726143	-2.817759	1.025984
-50.229052	-10.268903	1.030989
-50.987219	-11.409964	1.035994
-51.276995	-7.312198	1.040998
-51.004084	-4.295425	1.046003
-51.490019	-6.491238	1.051008
-51.523926	0.572152	1.056013
-51.017332	-0.696231	1.061018
-51.337399	-5.629112	1.066022
-51.950024	0.094417	1.071027
-52.323372	-2.368854	1.076032
-52.775143	-9.486288	1.081037
-52.969007	-5.934946	1.086042
-53.109897	-5.093604	1.091046
-53.463596	-11.938414	1.096051
-54.143178	-4.012057	1.101056
-54.397392	-7.629625	1.106061
-54.482605	-6.119931	1.111066
-54.549234	-2.366945	1.116070
-54.320673	-7.043573	1.121075
-54.421123	0.735670	1.126080
-55.100413	-14.619263	1.131085
-54.975351	-6.568262	1.136090
-55.447628	-6.716161	1.141094
-55.559469	-5.281413	1.146099
-56.369148	-3.165393	1.151104
-56.907168	-8.684412	1.156109
-56.849361	-9.629827	1.161114
-57.100672	-2.554735	1.166118
-56.962339	-8.840263	1.171123
-57.403712	-0.960484	1.176128
-57.152643	-9.323097	1.181133
-57.943876	-5.533218	1.186138
-58.597041	3.135648	1.191142
-58.614211	-9.136591	1.196147
-58.880907	1.939743	1.201152
-58.817788	-8.345575	1.206157
-58.966066	-7.711882	1.211162
-59.803832	0.700997	1.216166
-60.170174	-16.600845	1.221171
-60.382261	-10.215209	1.226176
-60.296728	-12.857490	1.231181
-60.318714	-8.001017	1.236186
-60.328260	-7.891944	1.241190
-60.148854	-10.656405	1.246195
-61.308174	-1.665133	1.251200
-61.592490	-3.316555	1.256205
-61.759267	-2.733764	1.261210
-62.187612	-7.181566	1.266214
-61.807960	-9.281204	1.271219
-62.381517	-14.589051	1.276224
-63.185725	-6.222527	1.281229
-63.493632	-11.660319	1.286234
-63.518254	-7.531074	1.291238
-63.601372	-11.058224	1.296243
-63.758086	-5.538555	1.301248
-63.458766	-1.190837	1.306253
-63.720217	-9.584377	1.311258
-64.553350	-8.467580	1.316262
-64.644046	-10.332639	1.321267
-64.849427	-0.430074	1.326272
-64.872872	-13.217006	1.331277
-65.214073	-8.817015	1.336282
-65.786573	-4.437955	1.341286
-66.154449	-14.365108	1.346291
-66.284082	-3.892229	1.351296
-66.293917	-9.844649	1.356301
-66.237336	-19.695523	1.361306
-67.197510	-6.919910	1.366310
-67.277334	-13.604888	1.371315
-67.791079	1.565699	1.376320
-68.026420	-11.919044	1.381325
-67.667416	-7.656547	1.386330
-67.973815	-3.673247	1.391334
-68.211655	-8.947948	1.396339
-68.551499	-6.607698	1.401344
-68.693331	-8.784323	1.406349
-68.731483	-10.790437	1.411354
-70.034389	-4.725323	1.416358
-69.773932	-13.478523	1.421363
-70.183443	-9.510806	1.426368
-70.129264	-9.206018	1.431373
-70.365016	-13.509805	1.436378
-70.508444	-14.632688	1.441382
-71.151816	-17.541115	1.446387
-71.505452	-7.523725	1.451392
-71.785781	-7.695183	1.456397
-72.048898	-17.018571	1.461402
-72.117368	-12.142208	1.466406
-72.001415	-12.239330	1.471411
-71.826820	-9.257869	1.476416
-72.735544	-11.944653	1.481421
-72.867919	-11.183727	1.486426
-73.357779	-10.344996	1.491430
-73.141399	-18.974275	1.496435
-73.666131	-6.212679	1.501440
-74.300560	-19.489749	1.506445
-74.571326	-16.505383	1.511450
-74.873175	-4.468162	1.516454
-74.974248	-14.908237	1.521459
-75.202699	-6.602886	1.526464
-75.171341	-4.348905	1.531469
-75.174991	-3.823150	1.536474
-75.175618	-11.058278	1.541478
-75.554818	-10.293722	1.546483
-76.302705	-0.524981	1.551488
-76.431083	4.025368	1.556493
-76.502362	-1.968106	1.561498
-77.571551	0.216793	1.566502
-77.633672	-3.531919	1.571507
-77.669955	-4.130503	1.576512
-78.212664	-5.719547	1.581517
-78.149792	-7.599026	1.586522
-78.584254	-3.165531	1.591526
-78.138001	-5.753249	1.596531
-78.244176	-7.486189	1.601536
-78.162722	0.372294	1.606541
-78.996355	-12.161946	1.611546
-79.436331	-5.905336	1.616550
-79.281125	-10.845778	1.621555
-80.433628	-2.624333	1.626560
-81.087813	-6.752243	1.631565
-80.834689	-13.504878	1.636570
-80.989759	-1.395600	1.641574
-81.045615	-14.886139	1.646579
-81.080704	-11.448102	1.651584
-81.061202	-10.539987	1.656589
-81.214616	-18.444161	1.661594
-82.111866	-10.797118	1.666598
-82.472371	-7.776632	1.671603
-82.650072	-8.438615	1.676608
-82.596886	-11.721242	1.681613
-82.678266	-18.067465	1.686618
-83.688566	-9.811219	1.691622
-83.781791	-13.023595	1.696627
-84.083065	-16.883759	1.701632
-84.221042	-9.187262	1.706637
-84.213088	-10.453934	1.711642
-84.241928	-3.021190	1.716646
-84.113615	-14.575782	1.721651
-84.892417	-7.371107	1.726656
-85.411872	-15.379635	1.731661
-85.741994	-6.511145	1.736666
-85.651476	-4.794703	1.741670
-85.856530	-12.849021	1.746675
-86.011416	-12.663537	1.751680
-86.458730	-16.754054	1.756685
-86.658506	-12.448848	1.761690
-86.825343	-11.274447	1.766694
-87.007625	-11.758552	1.771699
-87.948867	-9.229756	1.776704
-88.301816	-10.376963	1.781709
-88.384648	-8.244404	1.786714
-88.812001	-9.845081	1.791718
-88.581558	-8.517409	1.796723
-88.657232	-9.992515	1.801728
-88.354074	-7.616345	1.806733
-88.868795	-9.655819	1.811738
-89.490910	-7.410820	1.816742
-89.871530	-17.456203	1.821747
-90.546097	-2.172000	1.826752
-90.370573	-11.361212	1.831757
-90.170794	-15.308882	1.836762
-90.740024	-10.253314	1.841766
-91.007204	-20.392285	1.846771
-91.599327	-14.516935	1.851776
-91.995127	-5.970401	1.856781
-91.826774	-12.383982	1.861786
-91.536818	-4.172002	1.866790
-91.582159	-13.845662	1.871795
-92.505163	-11.341851	1.876800
-92.871555	-8.927868	1.881805
-92.764193	-12.639694	1.886810
-93.205586	-3.273005	1.891814
-93.351464	-9.099842	1.896819
-94.102208	-11.251258	1.901824
-94.529905	-6.784018	1.906829
-94.331150	-5.267921	1.911834
-94.821501	0.949080	1.916838
-94.522047	-10.701761	1.921843
-94.354349	-8.956210	1.926848
-95.150807	0.237983	1.931853
-95.745883	-10.226413	1.936858
-95.874993	-1.617001	1.941862
-96.060924	-3.995560	1.946867
-95.976293	-0.367362	1.951872
-96.950490	-3.790572	1.956877
-96.913077	-10.655148	1.961882
-97.262352	-7.981248	1.966886
-97.520687	-6.454091	1.971891
-97.878003	-15.535028	1.976896
-97.710991	-8.142273	1.981901
-97.811373	-6.234763	1.986906
-98.204910	-2.402405	1.991910
-98.070424	-11.117008	1.996915
-98.627141	-3.037716	2.006912
-98.777551	-10.600874	2.016909
-98.095671	-9.037624	2.026906
-97.663175	-8.072251	2.036902
-97.086674	-16.375791	2.046899
-96.712260	-6.877117	2.056896
-96.241813	-6.760259	2.066893
-95.296354	-12.805664	2.076890
-95.087147	-17.025879	2.086886
-94.822008	-9.604036	2.096883
-93.782372	-8.226364	2.106880
-93.684333	-10.528657	2.116877
-93.136175	-10.366880	2.126874
-92.529593	-15.336356	2.136870
-92.452986	-6.507211	2.146867
-91.631860	-9.146995	2.156864
-91.082056	-6.261259	2.166861
-90.442969	-14.903984	2.176858
-89.984550	-11.284954	2.186854
-89.793418	-13.221618	2.196851
-88.586051	-11.676833	2.206848
-88.502035	-12.088998	2.216845
-88.272903	-14.329341	2.226842
-87.447181	-11.758988	2.236838
-86.895600	-16.048350	2.246835
-86.807717	-14.972302	2.256832
-85.939397	-16.102109	2.266829
-85.230379	-11.042786	2.276826
-85.241532	-16.026950	2.286822
-84.316751	-12.771960	2.296819
-83.895878	-14.443464	2.306816
-83.709590	-11.827402	2.316813
-82.857295	-13.258812	2.326810
-82.442518	-15.166943	2.336806
-82.419178	-16.231708	2.346803
-81.979481	-9.226669	2.356800
-81.180466	-11.942202	2.366797
-79.934631	-15.389352	2.376794
-79.773355	-9.915304	2.386790
-79.854509	-12.566652	2.396787
-79.266038	-11.894818	2.406784
-78.476252	-14.570901	2.416781
-78.339460	-12.663030	2.426778
-77.152118	-15.955359	2.436774
-76.946337	-12.426868	2.446771
-76.982324	-12.348363	2.456768
-75.721315	-19.713141	2.466765
-75.392217	-18.997754	2.476762
-75.105349	-17.236790	2.486758
-73.997645	-20.329825	2.496755
-73.923210	-24.725452	2.506752
-73.866685	-14.958715	2.516749
-72.806096	-18.161618	2.526746
-72.539930	-20.236672	2.536742
-72.136756	-19.482136	2.546739
-71.366486	-14.806137	2.556736
-70.926988	-18.286125	2.566733
-70.800422	-15.217287	2.576730
-70.081043	-9.107901	2.586726
-69.697837	-13.225334	2.596723
-68.673351	-7.223640	2.606720
-68.304750	-9.789797	2.616717
-68.395425	-21.714662	2.626714
-67.225934	-16.632004	2.636710
-67.138065	-8.431815	2.646707
-66.874357	-18.441554	2.656704
-65.759445	-16.768336	2.666701
-65.631857	-12.948914	2.676698
-64.713291	-11.656924	2.686694
-64.407188	-12.949441	2.696691
-64.225305	-17.783103	2.706688
-63.198373	-15.969478	2.716685
-62.890889	-15.089174	2.726682
-62.916460	-21.692950	2.736678
-61.775908	-13.780205	2.746675
-61.126943	-20.108884	2.756672
-61.051554	-18.897847	2.766669
-60.716526	-14.765445	2.776666
-59.887020	-18.024232	2.786662
-59.714539	-17.769117	2.796659
-58.942838	-15.640164	2.806656
-58.207070	-21.415341	2.816653
-57.883422	-17.461726	2.826650
-57.458641	-18.684025	2.836646
-57.116249	-22.617711	2.846643
-56.542932	-18.091605	2.856640
-55.648410	-17.093634	2.866637
-55.281833	-6.554734	2.876634
-55.330639	-12.800115	2.886630
-54.462353	-15.507426	2.896627
-54.087114	-17.140147	2.906624
-53.586978	-9.495139	2.916621
-52.675223	-10.980155	2.926618
-52.320364	-20.101294	2.936614
-52.033702	-19.575697	2.946611
-51.411915	-13.090000	2.956608
-50.928471	-14.726898	2.966605
-50.486538	-12.689146	2.976602
-49.608887	-18.641631	2.986598
-49.480138	-15.189842	2.996595
-49.268617	-17.291233	3.006592
-48.221828	-15.353991	3.016589
-47.779540	-15.087034	3.026586
-47.515052	-12.451469	3.036582
-46.716884	-14.473145	3.046579
-46.643257	-16.803313	3.056576
-46.268960	-15.664158	3.066573
-45.169705	-23.615114	3.076570
-44.982242	-20.913707	3.086566
-44.402441	-12.767937	3.096563
-43.769826	-10.515961	3.106560
-43.491791	-14.800745	3.116557
-43.058204	-9.337417	3.126554
-42.391586	-11.382959	3.136550
-41.937442	-10.135862	3.146547
-41.447861	-10.699868	3.156544
-40.991005	-9.941019	3.166541
-40.552250	-12.226672	3.176538
-39.448803	-17.558602	3.186534
-39.251669	-8.019650	3.196531
-39.396269	-12.286147	3.206528
-38.276351	-9.796441	3.216525
-37.957885	-16.213042	3.226522
-37.738265	-16.041291	3.236518
-36.741189	-15.787857	3.246515
-36.474487	-4.036014	3.256512
-35.756345	-8.063052	3.266509
-35.290774	-12.481570	3.276506
-35.045785	-9.418497	3.286502
-34.479392	-13.646812	3.296499
-33.565264	-5.325018	3.306496
-33.452960	-9.929279	3.316493
-32.964580	-8.263042	3.326490
-31.910150	-13.495478	3.336486
-31.617810	-10.965615	3.346483
-31.747072	-6.453654	3.356480
-31.079107	-6.396057	3.366477
-30.458801	-7.107124	3.376474
-29.990979	-11.497484	3.386470
-29.019199	-10.549553	3.396467
-29.026324	-18.020985	3.406464
-28.692968	-11.933854	3.416461
-27.588490	-10.610622	3.426458
-27.307683	-12.244479	3.436454
-27.089287	-14.103029	3.446451
-26.371123	-9.095808	3.456448
-26.025513	-13.992976	3.466445
-25.163648	-7.240555	3.476442
-24.332393	-10.043468	3.486438
-24.367232	-12.708363	3.496435
-24.264538	-11.381205	3.506432
-23.680151	-5.630920	3.516429
-23.211983	-10.037172	3.526426
-22.309802	-10.747779	3.536422
-22.121332	-8.727580	3.546419
-21.339786	-3.891778	3.556416
-20.720174	-14.305383	3.566413
-20.410581	-6.351946	3.576410
-19.414043	-12.779092	3.586406
-18.961750	-13.726919	3.596403
-19.072890	-11.156408	3.606400
-18.459001	-10.323809	3.616397
-17.720457	-5.256406	3.626394
-17.439256	-6.361320	3.636390
-17.179351	-10.348688	3.646387
-15.992401	-11.886052	3.656384
-16.066130	-11.636950	3.666381
-15.543813	-8.040536	3.676378
-14.750270	-9.985467	3.686374
-14.469137	-2.151137	3.696371
-13.857390	-12.449482	3.706368
-13.183378	-11.277797	3.716365
-12.661457	-9.876533	3.726362
-12.247887	-3.706856	3.736358
-11.675842	-4.090472	3.746355
-11.356780	-4.748301	3.756352
-11.196854	-9.971342	3.766349
-10.146031	-6.463549	3.776346
-10.065929	-5.842436	3.786342
-9.527957	-6.280933	3.796339
-8.553537	-6.543471	3.806336
-8.523613	-14.537009	3.816333
-7.367785	-6.708992	3.826330
-6.772566	-9.221739	3.836326
-6.760851	-7.611161	3.846323
-6.618038	-4.342116	3.856320
-6.132747	-2.368130	3.866317
-5.566895	-8.348098	3.876314
-4.820586	0.383122	3.886310
-4.661694	7.105622	3.896307
-4.022668	15.676162	3.906304
-3.705360	24.771952	3.916301
-3.050400	33.872194	3.926298
-2.538083	36.301294	3.936294
-2.310672	55.725138	3.946291
-2.161011	63.754192	3.956288
-1.224106	78.959081	3.966285
-0.842692	87.493741	3.976282
-0.592380	102.092814	3.986278
0.000000	126.006365	3.991283
0.246152	125.911117	3.996288
0.442953	129.819265	4.001293
0.503077	137.342622	4.006298
0.787900	139.607778	4.011302
0.860632	152.339744	4.016307
1.079155	146.870555	4.021312
0.976738	155.529676	4.026317
1.036489	162.300148	4.031322
1.321484	156.080308	4.036326
1.068402	147.052650	4.041331
1.030306	136.336925	4.046336
0.963848	136.926247	4.051341
0.801629	142.209546	4.056346
1.515782	143.673886	4.061350
0.506517	142.761727	4.066355
1.085875	143.857922	4.071360
0.849866	148.032773	4.076365
0.978427	156.659095	4.081370
1.214794	157.068395	4.086374
1.050073	155.787467	4.091379
1.053602	149.665234	4.096384
1.627469	153.391297	4.101389
1.013098	157.555458	4.106394
1.101688	159.139343	4.111398
1.416534	159.422531	4.116403
1.072760	159.305240	4.121408
1.407180	158.361038	4.126413
1.237589	161.035461	4.131418
1.554080	155.671236	4.136422
1.467273	152.179425	4.141427
1.038259	136.573418	4.146432
0.926405	137.967053	4.151437
0.798638	145.693670	4.156442
0.983290	152.476328	4.161446
1.091463	159.242423	4.166451
1.259419	158.498142	4.171456
1.208947	148.967550	4.176461
0.925392	156.534935	4.181466
1.374768	161.352866	4.186470
1.081650	158.908716	4.191475
1.313920	159.799531	4.196480
1.067354	161.948114	4.201485
1.451679	169.819631	4.206490
2.072602	177.135471	4.211494
1.403676	166.998825	4.216499
1.396098	159.309136	4.221504
1.245472	160.474696	4.226509
1.397491	165.892570	4.231514
1.762668	170.710959	4.236518
1.323562	170.788840	4.241523
1.585125	167.299733	4.246528
1.493876	170.762369	4.251533
1.697324	180.234399	4.256538
1.498510	163.365021	4.261542
1.441758	173.250874	4.266547
1.706376	171.792369	4.271552
1.641675	171.223513	4.276557
1.271716	173.982917	4.281562
1.645836	169.486053	4.286566
1.645961	183.883949	4.291571
1.886549	178.208840	4.296576
1.814773	177.005186	4.301581
1.464510	172.725507	4.306586
1.646693	175.449563	4.311590
1.641176	182.062529	4.316595
2.100475	177.966844	4.321600
1.275058	172.078069	4.326605
1.660549	179.547622	4.331610
1.825933	174.089862	4.336614
1.876787	180.228991	4.341619
2.038340	180.292443	4.346624
1.813950	168.511072	4.351629
1.666739	169.059185	4.356634
1.824269	172.454615	4.361638
2.016956	180.523649	4.366643
1.388289	177.929264	4.371648
1.622710	185.444486	4.376653
1.807883	190.759131	4.381658
1.613534	179.099623	4.386662
1.579643	188.469409	4.391667
1.855285	174.819538	4.396672
1.958165	181.675049	4.401677
1.724121	192.417400	4.406682
2.154673	183.681908	4.411686
1.835890	183.500616	4.416691
1.887121	187.814246	4.421696
1.643313	180.803555	4.426701
2.059452	183.111544	4.431706
2.095546	182.992055	4.436710
2.207702	189.292481	4.441715
1.877949	177.628746	4.446720
1.830266	179.015556	4.451725
1.820029	183.284974	4.456730
1.849267	169.024918	4.461734
1.836101	177.866301	4.466739
1.944571	184.467849	4.471744
2.355947	198.874491	4.476749
1.862968	196.141921	4.481754
2.425671	190.919681	4.486758
2.354482	182.543876	4.491763
1.817976	183.949848	4.496768
2.209474	183.262508	4.501773
2.018146	191.059150	4.506778
2.369235	193.845494	4.511782
2.124789	191.966386	4.516787
2.331482	191.307819	4.521792
2.199986	186.563815	4.526797
2.051605	194.379082	4.531802
2.740245	186.887859	4.536806
2.171022	190.950088	4.541811
1.920674	188.448655	4.546816
1.899562	184.687188	4.551821
2.196473	201.345210	4.556826
2.676945	200.327649	4.561830
2.562477	205.021415	4.566835
2.533004	189.270898	4.571840
2.245247	191.527136	4.576845
2.082917	191.460686	4.581850
2.452608	197.537524	4.586854
2.335452	212.320690	4.591859
2.553973	206.003617	4.596864
2.801904	215.854710	4.601869
2.136508	199.510349	4.606874
2.146255	197.449298	4.611878
2.446203	201.607152	4.616883
2.719424	203.513462	4.621888
2.872943	204.862621	4.626893
2.303098	191.743001	4.631898
1.941865	183.905888	4.636902
2.420770	198.017284	4.641907
2.562512	206.208154	4.646912
2.916599	195.504097	4.651917
2.461168	203.800599	4.656922
2.778730	210.654333	4.661926
2.863129	201.551957	4.666931
2.457134	189.178766	4.671936
2.452860	194.592509	4.676941
2.249890	198.461678	4.681946
2.918031	200.259045	4.686950
2.711523	201.347890	4.691955
2.800021	208.686530	4.696960
2.530703	202.774436	4.701965
2.268220	210.186705	4.706970
2.600338	208.923328	4.711974
2.772691	209.241357	4.716979
2.520444	208.821920	4.721984
2.426329	204.091074	4.726989
2.498203	205.041665	4.731994
2.535711	208.949323	4.736998
2.539238	207.328991	4.742003
2.533577	205.232374	4.747008
2.872209	207.011445	4.752013
2.584329	202.440478	4.757018
2.790279	202.411599	4.762022
2.670482	204.050079	4.767027
2.485220	217.280994	4.772032
2.751966	221.640170	4.777037
2.835199	227.511688	4.782042
3.079617	230.890436	4.787046
3.296488	220.590534	4.792051
3.042895	214.935410	4.797056
2.733762	208.520159	4.802061
2.763167	208.708588	4.807066
3.354134	201.384423	4.812070
2.783248	204.054895	4.817075
3.004209	213.641273	4.822080
3.007789	201.631401	4.827085
3.073117	212.032930	4.832090
3.237148	197.071673	4.837094
3.058197	201.535038	4.842099
3.157396	202.471884	4.847104
3.082772	196.893302	4.852109
2.964913	203.653478	4.857114
2.795932	206.818183	4.862118
2.810786	204.613971	4.867123
2.624582	206.873381	4.872128
3.410561	211.676883	4.877133
3.083673	222.345124	4.882138
2.869266	204.307571	4.887142
3.118774	219.789774	4.892147
3.100195	221.459952	4.897152
3.345269	216.457997	4.902157
3.143965	221.706277	4.907162
3.421927	223.561233	4.912166
3.150902	224.059024	4.917171
2.990502	228.057610	4.922176
3.470120	221.896027	4.927181
3.299267	229.445895	4.932186
3.381675	219.613008	4.937190
3.424162	213.990877	4.942195
3.084185	213.344660	4.947200
2.951621	214.592831	4.952205
3.286351	224.819548	4.957210
3.795723	224.496659	4.962214
3.674446	208.741438	4.967219
3.146100	209.459622	4.972224
3.163765	209.988393	4.977229
3.375761	201.938639	4.982234
3.132241	204.203809	4.987238
3.480852	220.521614	4.992243
3.345899	227.619812	4.997248
3.489089	222.845685	5.002253
3.199529	232.131917	5.007258
4.038136	227.240024	5.012262
3.563321	225.665694	5.017267
3.042537	217.904027	5.022272
3.142941	222.213173	5.027277
3.227423	228.372393	5.032282
3.397233	222.208427	5.037286
3.573877	227.657286	5.042291
3.740629	229.323918	5.047296
3.817614	232.693935	5.052301
3.529043	235.931048	5.057306
3.672749	225.411585	5.062310
3.944532	234.483872	5.067315
3.742690	218.953152	5.072320
3.620703	213.400920	5.077325
3.424542	214.361608	5.082330
3.429676	209.099626	5.087334
3.462050	228.418391	5.092339
3.610698	232.653592	5.097344
3.666567	228.120845	5.102349
3.845523	228.089841	5.107354
3.504239	227.912051	5.112358
3.988383	235.840822	5.117363
3.670271	233.669465	5.122368
3.913378	237.744430	5.127373
3.801243	221.915008	5.132378
3.966422	217.513938	5.137382
3.757112	214.563196	5.142387
3.568709	213.077148	5.147392
3.557707	209.235009	5.152397
3.707413	228.067281	5.157402
4.021534	221.880847	5.162406
4.063912	231.476057	5.167411
3.782083	229.368653	5.172416
3.408247	221.020969	5.177421
3.521849	233.430261	5.182426
3.509484	224.387231	5.187430
3.851809	233.138493	5.192435
3.707765	232.920503	5.197440
3.577086	238.325467	5.202445
3.562536	235.151414	5.207450
3.796003	229.796929	5.212454
3.413012	238.259335	5.217459
3.677537	251.347480	5.222464
4.397424	242.649167	5.227469
4.132892	247.515002	5.232474
3.933925	245.087817	5.237478
3.802194	243.811237	5.242483
4.154218	249.447927	5.247488
4.147191	262.081661	5.252493
4.019417	251.604452	5.257498
3.776071	258.877723	5.262502
4.105948	257.817168	5.267507
3.729486	258.147882	5.272512
4.074407	254.209189	5.277517
4.170241	255.662244	5.282522
4.030877	264.937762	5.287526
4.329637	261.835143	5.292531
3.743271	259.465109	5.297536
4.171984	243.491349	5.302541
4.125787	255.403529	5.307546
4.087783	257.573433	5.312550
3.902311	255.153637	5.317555
3.838104	266.448544	5.322560
3.821788	253.524264	5.327565
3.945957	253.584046	5.332570
4.088168	264.694957	5.337574
4.626362	278.509291	5.342579
4.173694	276.558191	5.347584
4.466341	266.828584	5.352589
4.336318	270.705393	5.357594
4.295501	261.790158	5.362598
4.659816	262.344050	5.367603
3.893918	262.305136	5.372608
4.470732	263.582066	5.377613
4.429378	265.809440	5.382618
4.623886	257.601035	5.387622
4.709020	248.745288	5.392627
4.369111	244.315287	5.397632
4.314714	251.416770	5.402637
4.259905	265.984633	5.407642
4.078688	255.053844	5.412646
4.354268	260.389234	5.417651
4.652462	277.059783	5.422656
4.558626	259.126786	5.427661
4.231811	268.573859	5.432666
4.773382	270.707310	5.437670
4.386911	261.058132	5.442675
4.437224	266.994899	5.447680
4.524520	267.098387	5.452685
4.895209	274.402609	5.457690
4.683063	259.338521	5.462694
4.327219	261.709770	5.467699
4.791359	264.655690	5.472704
4.635942	256.115797	5.477709
4.265191	261.735314	5.482714
4.649872	266.335562	5.487718
4.915516	278.904708	5.492723
4.460972	269.563512	5.497728
4.910629	266.766421	5.502733
4.465947	263.412565	5.507738
4.876642	270.406842	5.512742
4.904850	262.278110	5.517747
4.462636	262.128690	5.522752
4.709137	259.847276	5.527757
4.349500	268.733158	5.532762
4.365232	273.343396	5.537766
4.944864	276.271336	5.542771
4.938025	280.600358	5.547776
4.886289	274.667018	5.552781
5.001959	282.729108	5.557786
4.879040	285.681014	5.562790
5.179268	275.788874	5.567795
4.664270	275.299615	5.572800
4.792773	268.192957	5.577805
4.628169	277.383828	5.582810
4.718913	281.732458	5.587814
4.919037	280.075183	5.592819
4.556169	294.567649	5.597824
4.966893	287.363260	5.602829
4.703786	291.089954	5.607834
4.821756	284.693597	5.612838
5.231230	280.849250	5.617843
4.475421	286.338905	5.622848
4.886146	280.846078	5.627853
4.677283	282.140934	5.632858
4.707238	280.801214	5.637862
4.955080	285.479718	5.642867
4.747800	287.464014	5.647872
4.624672	281.836011	5.652877
4.821139	302.062597	5.657882
5.078577	302.332580	5.662886
4.970916	301.121850	5.667891
4.926356	307.832690	5.672896
4.988270	302.137905	5.677901
5.161068	308.425768	5.682906
5.529438	303.230588	5.687910
5.291470	305.956807	5.692915
5.354074	303.381322	5.697920
5.380173	299.897212	5.702925
5.286413	299.380332	5.707930
5.103801	300.234512	5.712934
5.262953	294.821978	5.717939
5.031497	301.878284	5.722944
5.429651	298.605161	5.727949
5.281826	300.804824	5.732954
5.612243	291.812792	5.737958
4.950326	275.562730	5.742963
4.981641	287.358461	5.747968
5.573280	291.986603	5.752973
5.163830	294.654099	5.757978
5.027852	304.868729	5.762982
5.540430	299.859903	5.767987
5.202331	302.304322	5.772992
5.401979	297.100614	5.777997
5.045849	299.399147	5.783002
5.051213	287.679999	5.788006
5.230433	293.337281	5.793011
5.275213	305.197365	5.798016
5.363674	300.830365	5.803021
5.222161	309.473502	5.808026
5.259397	309.426599	5.813030
5.225049	303.427267	5.818035
5.171940	301.309553	5.823040
5.356609	296.070213	5.828045
5.412213	314.135793	5.833050
5.349429	306.729877	5.838054
5.599742	319.108453	5.843059
5.657386	317.027277	5.848064
5.462941	310.480239	5.853069
5.511037	313.566873	5.858074
5.705908	312.135036	5.863078
5.741613	312.578745	5.868083
5.486711	313.605530	5.873088
5.375801	309.035455	5.878093
5.905756	312.553257	5.883098
5.218592	316.583258	5.888102
5.800052	316.505404	5.893107
5.934778	324.593020	5.898112
5.693431	318.863190	5.903117
5.429164	301.981724	5.908122
5.897343	309.068305	5.913126
5.730700	302.409377	5.918131
5.362654	313.969916	5.923136
5.975724	312.590024	5.928141
5.815878	314.620720	5.933146
5.790603	324.754852	5.938150
5.742505	309.402593	5.943155
5.814585	321.726664	5.948160
6.136524	320.480683	5.953165
5.810804	308.664376	5.958170
5.526990	308.594694	5.963174
5.675945	308.362721	5.968179
5.530885	320.673145	5.973184
6.074869	326.985478	5.978189
5.893127	327.599083	5.983194
6.107855	329.090578	5.988198
6.084234	321.346370	5.993203
5.773308	323.865655	5.998208
5.557593	318.935414	6.003213
5.960950	326.256718	6.008218
5.888014	323.942775	6.013222
5.949578	323.446002	6.018227
5.800066	329.448702	6.023232
6.177011	334.958156	6.028237
5.758135	331.622414	6.033242
5.781287	329.103687	6.038246
5.737779	330.069086	6.043251
5.653550	338.769756	6.048256
6.067654	328.024638	6.053261
5.884201	324.990759	6.058266
6.016522	328.890009	6.063270
5.973423	332.677368	6.068275
5.903453	338.357644	6.073280
6.028895	331.589954	6.078285
5.731526	323.062639	6.083290
5.907308	339.239786	6.088294
5.907194	326.262311	6.093299
5.706101	338.796603	6.098304
5.819970	329.249819	6.103309
6.107831	325.883134	6.108314
5.975448	322.907742	6.113318
6.106276	318.866329	6.118323
5.695608	319.252989	6.123328
6.026274	311.694065	6.128333
5.873845	320.313597	6.133338
5.566114	319.871159	6.138342
6.009119	316.243043	6.143347
5.766261	321.247890	6.148352
6.363372	328.007525	6.153357
5.907086	317.644699	6.158362
5.657621	314.010505	6.163366
5.912005	303.464273	6.168371
5.772441	312.281112	6.173376
5.398022	314.946320	6.178381
5.761279	324.048702	6.183386
5.889894	329.789804	6.188390
6.264423	322.777694	6.193395
5.591673	325.831033	6.198400
6.176143	321.662043	6.203405
6.140990	322.199041	6.208410
6.001021	323.897619	6.213414
5.842820	311.283284	6.218419
5.416246	326.984738	6.223424
5.685942	325.237534	6.228429
5.747807	326.069470	6.233434
5.479233	333.656743	6.238438
5.805409	322.434944	6.243443
5.901682	331.797194	6.248448
5.799696	326.520219	6.253453
5.960669	338.675441	6.258458
5.529857	339.501829	6.263462
5.712117	326.866112	6.268467
6.102311	334.803227	6.273472
6.038418	332.614423	6.278477
5.582060	334.609032	6.283482
5.694909	332.886247	6.288486
5.894138	324.237322	6.293491
5.539250	332.192368	6.298496
6.012498	330.426126	6.303501
5.685900	342.005540	6.308506
5.550204	334.516053	6.313510
6.126712	337.058518	6.318515
6.143601	340.425258	6.323520
5.763488	338.409072	6.328525
5.769913	336.136554	6.333530
5.608717	343.438198	6.338534
6.000718	326.976542	6.343539
5.922089	341.190677	6.348544
5.885017	335.710606	6.353549
5.940940	338.141139	6.358554
5.550938	336.620031	6.363558
5.914877	342.001799	6.368563
5.896675	345.918161	6.373568
6.053710	353.739729	6.378573
6.307381	347.834742	6.383578
6.077170	335.256912	6.388582
6.213748	331.072235	6.393587
5.622436	338.583211	6.398592
5.969636	327.092384	6.403597
6.302481	327.173460	6.408602
5.622461	332.983517	6.413606
6.002053	332.342317	6.418611
5.965064	333.980571	6.423616
5.940477	327.954402	6.428621
5.964986	329.795048	6.433626
5.939152	332.048487	6.438630
6.027621	321.021884	6.443635
5.909103	329.098311	6.448640
6.231242	328.307871	6.453645
6.200744	331.106193	6.458650
6.252876	328.048289	6.463654
6.235450	326.127493	6.468659
5.775580	319.719853	6.473664
5.869508	311.916219	6.478669
6.011360	316.677672	6.483674
5.535214	319.469448	6.488678
5.453119	318.976061	6.493683
5.670557	334.115350	6.498688
5.881955	329.409668	6.503693
5.618288	335.752842	6.508698
5.606734	334.299359	6.513702
5.934269	331.287159	6.518707
6.074632	334.315139	6.523712
5.963803	329.368565	6.528717
5.980154	327.170432	6.533722
5.872504	330.221207	6.538726
6.238674	324.286058	6.543731
5.963307	336.888859	6.548736
6.321935	328.898474	6.553741
6.114239	329.354771	6.558746
5.692328	319.875592	6.563750
5.766707	321.604070	6.568755
5.844097	323.737034	6.573760
5.775535	327.673887	6.578765
5.660943	328.754756	6.583770
5.798679	336.177530	6.588774
5.862964	330.453894	6.593779
5.746515	336.106605	6.598784
6.047348	335.506141	6.603789
5.900931	326.531386	6.608794
5.745606	336.018231	6.613798
5.966026	327.410297	6.618803
5.866255	332.914880	6.623808
5.682963	326.986186	6.628813
6.039931	333.242220	6.633818
6.104162	339.626090	6.638822
6.276419	333.714802	6.643827
5.891054	340.915307	6.648832
5.816314	337.282378	6.653837
5.932895	338.808137	6.658842
5.644677	333.620267	6.663846
5.552250	334.077599	6.668851
5.741896	328.097167	6.673856
5.715991	331.350347	6.678861
5.644398	335.562916	6.683866
5.910802	331.829417	6.688870
5.899111	334.507754	6.693875
5.350441	339.224867	6.698880
5.650755	329.592107	6.703885
5.691765	336.995141	6.708890
5.947290	341.735738	6.713894
5.777369	335.634120	6.718899
5.639050	333.817566	6.723904
5.836450	329.041298	6.728909
6.099052	339.554553	6.733914
5.935243	342.440071	6.738918
5.931293	336.920042	6.743923
5.427085	334.344220	6.748928
5.737159	335.830362	6.753933
6.084268	349.804215	6.758938
6.121208	357.419859	6.763942
6.101172	349.792137	6.768947
6.116568	344.575974	6.773952
5.947504	335.686997	6.778957
5.986080	336.174551	6.783962
6.054441	333.655113	6.788966
6.133142	338.524479	6.793971
5.973989	337.239507	6.798976
5.643600	339.046827	6.803981
5.906087	332.219834	6.808986
6.062412	345.103436	6.813990
6.294471	327.572039	6.818995
5.893506	327.836968	6.824000
5.879596	332.809335	6.829005
6.233025	335.215693	6.834010
5.843522	337.196729	6.839014
6.348928	333.679115	6.844019
6.104493	334.337281	6.849024
6.040977	337.608973	6.854029
6.186256	330.161162	6.859034
5.501444	320.915901	6.864038
5.822720	323.564540	6.869043
5.857412	334.391683	6.874048
6.121488	330.386469	6.879053
5.981078	319.683400	6.884058
5.652414	319.111345	6.889062
5.714475	326.406694	6.894067
5.746907	338.967901	6.899072
5.540309	326.089013	6.904077
6.091868	329.679384	6.909082
6.007399	345.716725	6.914086
5.928111	331.467109	6.919091
5.921374	340.519541	6.924096
6.036037	326.385261	6.929101
5.904138	323.299064	6.934106
5.896228	328.485628	6.939110
5.827472	333.023616	6.944115
5.927579	333.431989	6.949120
6.012582	333.194154	6.954125
5.968257	328.294173	6.959130
5.980585	331.569874	6.964134
5.780011	315.425113	6.969139
5.681913	325.298505	6.974144
5.555189	330.288437	6.979149
5.837829	333.506233	6.984154
5.834406	335.503086	6.989158
6.084716	329.035489	6.994163
5.913637	330.390904	6.999168
6.287964	329.997293	7.004173
5.913222	337.591606	7.009178
5.888238	321.862420	7.014182
5.748289	323.092766	7.019187
5.678921	326.498243	7.024192
5.471098	331.709606	7.029197
5.797642	339.463647	7.034202
5.601642	332.812441	7.039206
5.893491	344.823906	7.044211
5.764133	338.798227	7.049216
5.981304	338.615743	7.054221
6.152765	337.725378	7.059226
5.877282	334.490694	7.064230
6.055955	342.957448	7.069235
5.923444	338.096504	7.074240
6.024986	337.777001	7.079245
5.836279	344.393241	7.084250
5.727366	334.115523	7.089254
6.163365	332.930875	7.094259
5.681843	340.045112	7.099264
5.732141	335.086105	7.104269
6.142933	332.035632	7.109274
5.964932	336.524193	7.114278
5.955660	333.719453	7.119283
6.048426	343.882673	7.124288
6.107479	337.267684	7.129293
6.254287	324.833638	7.134298
5.889073	322.587348	7.139302
6.038799	312.886295	7.144307
5.554051	312.955464	7.149312
5.619325	306.111731	7.154317
6.166725	321.019305	7.159322
5.805668	332.955249	7.164326
5.989364	317.019572	7.169331
5.647938	315.832583	7.174336
5.948019	315.665664	7.179341
6.264760	329.742303	7.184346
5.793243	326.702655	7.189350
5.693286	318.223699	7.194355
5.861595	326.850244	7.199360
5.793597	323.444054	7.204365
6.299543	322.704089	7.209370
5.536706	318.672106	7.214374
5.898429	325.487371	7.219379
6.001184	335.595248	7.224384
6.039041	321.023685	7.229389
5.692311	315.661435	7.234394
5.512440	322.390184	7.239398
6.111275	335.340921	7.244403
6.225931	340.502077	7.249408
5.789383	332.015411	7.254413
6.059049	318.331560	7.259418
5.591215	317.996306	7.264422
5.870692	308.471203	7.269427
5.997844	320.565241	7.274432
5.906242	315.732734	7.279437
5.931117	316.624212	7.284442
5.877202	322.333620	7.289446
5.651710	325.174955	7.294451
5.813238	321.223674	7.299456
5.895259	326.307651	7.304461
6.162862	333.245140	7.309466
5.966473	329.302128	7.314470
6.241238	324.915606	7.319475
6.017493	322.976314	7.324480
6.085762	312.927282	7.329485
5.818195	311.858505	7.334490
5.586634	313.125261	7.339494
5.737050	309.757833	7.344499
5.817729	306.170313	7.349504
5.799285	308.213794	7.354509
5.977513	299.359347	7.359514
5.621286	314.489862	7.364518
6.008988	307.270067	7.369523
5.937531	309.068706	7.374528
5.856660	310.840337	7.379533
5.630618	311.780372	7.384538
6.118827	325.301973	7.389542
5.825231	310.301143	7.394547
6.042590	314.456063	7.399552
5.820336	307.391346	7.404557
5.971973	304.368572	7.409562
5.756969	317.942709	7.414566
6.192031	307.061465	7.419571
5.688749	314.416358	7.424576
5.696543	310.049260	7.429581
5.813969	313.099790	7.434586
5.950231	319.614804	7.439590
5.987128	313.389245	7.444595
5.996881	314.529846	7.449600
5.721473	310.289098	7.454605
5.943369	309.656633	7.459610
5.809838	306.191048	7.464614
5.826676	306.447873	7.469619
5.923385	314.079502	7.474624
5.850066	317.672251	7.479629
6.379597	310.471500	7.484634
5.684872	312.908173	7.489638
5.806478	306.099961	7.494643
6.078680	306.196806	7.499648
5.952910	300.708410	7.504653
5.924514	299.086713	7.509658
5.739025	308.053066	7.514662
5.752801	307.361257	7.519667
6.161736	307.598162	7.524672
5.827073	298.668549	7.529677
5.837315	298.831489	7.534682
5.439651	308.779987	7.539686
5.912789	306.804960	7.544691
5.867911	319.292770	7.549696
5.876123	322.015462	7.554701
6.046686	322.491958	7.559706
5.734541	319.307277	7.564710
5.921742	316.715554	7.569715
6.129865	318.562412	7.574720
5.843225	310.644028	7.579725
5.807843	305.641422	7.584730
5.432207	312.454430	7.589734
5.876627	319.066996	7.594739
6.353162	328.297274	7.599744
5.964589	324.773320	7.604749
5.925135	318.271750	7.609754
5.690080	311.743690	7.614758
5.895001	316.992024	7.619763
6.305323	320.240557	7.624768
6.073837	316.641528	7.629773
5.904400	309.571751	7.634778
5.690040	320.785669	7.639782
5.973669	316.027616	7.644787
5.830975	313.319581	7.649792
5.616640	322.771316	7.654797
5.833468	313.205346	7.659802
5.631089	311.170982	7.664806
6.093015	312.766354	7.669811
5.990836	317.088084	7.674816
5.958410	320.956035	7.679821
6.098688	324.581966	7.684826
5.752919	315.369340	7.689830
5.971487	319.891063	7.694835
5.767272	313.816938	7.699840
5.476278	310.537218	7.704845
6.112727	320.894181	7.709850
5.620382	329.727990	7.714854
6.403015	327.749066	7.719859
6.163315	320.867391	7.724864
5.960327	319.193782	7.729869
5.949884	304.806920	7.734874
5.477433	311.777368	7.739878
5.704448	313.760487	7.744883
5.799584	311.682964	7.749888
5.680966	313.318107	7.754893
6.088604	314.219590	7.759898
5.810620	329.056367	7.764902
5.940207	319.355283	7.769907
6.116792	322.570607	7.774912
5.922276	323.448787	7.779917
5.998759	316.255298	7.784922
6.071024	311.498518	7.789926
6.031613	306.411120	7.794931
6.152160	306.648633	7.799936
6.192903	312.014276	7.804941
6.158481	305.518254	7.809946
5.728923	309.834006	7.814950
5.449667	306.220271	7.819955
6.109587	316.554595	7.824960
5.705158	307.249868	7.829965
5.702371	305.832988	7.834970
5.800054	321.158587	7.839974
5.897006	310.950069	7.844979
5.914238	307.416720	7.849984
5.900457	312.559901	7.854989
5.995139	313.105157	7.859994
5.488123	318.502303	7.864998
6.103792	313.211670	7.870003
5.714592	316.299952	7.875008
5.881422	316.957360	7.880013
5.836058	305.992732	7.885018
5.757522	307.593160	7.890022
5.659703	308.124096	7.895027
5.740548	318.988335	7.900032
5.676127	322.782176	7.905037
6.150124	323.591072	7.910042
5.840318	328.796167	7.915046
6.303901	310.368212	7.920051
6.134319	311.514588	7.925056
5.946123	315.394137	7.930061
6.107862	302.451589	7.935066
5.453139	306.947929	7.940070
5.629247	313.472556	7.945075
5.512550	308.694578	7.950080
5.848202	326.298960	7.955085
6.127321	330.773293	7.960090
5.678310	331.574041	7.965094
6.140552	325.038648	7.970099
5.705261	321.322656	7.975104
5.742725	326.818525	7.980109
6.238087	322.176198	7.985114
5.761626	319.811190	7.990118
5.489070	315.915817	7.995136
5.834789	318.897729	8.000154
6.080450	330.513254	8.005171
6.101637	325.404164	8.010189
5.975975	319.715214	8.015206
5.972287	318.623962	8.020224
5.970442	318.119371	8.025242
5.549666	317.525381	8.030259
6.325882	323.965108	8.035277
5.864568	318.748117	8.040294
5.871450	318.955340	8.045312
6.144699	316.426181	8.050330
5.483922	314.989137	8.055347
6.094066	321.896508	8.060365
6.231281	335.627416	8.065382
5.899781	326.805411	8.070400
6.028441	311.483746	8.075418
5.960856	319.790444	8.080435
6.198189	313.013088	8.085453
6.035837	312.318905	8.090470
6.114465	306.020671	8.095488
6.187427	305.927288	8.100506
6.050908	309.344023	8.105523
5.971779	308.895644	8.110541
6.168894	304.551232	8.115558
6.226676	304.684262	8.120576
6.197986	311.280861	8.125594
5.662385	315.728512	8.130611
6.116187	304.284990	8.135629
5.845424	310.764654	8.140646
5.656316	306.521398	8.145664
5.737342	308.036130	8.150682
5.804547	310.480769	8.155699
6.237423	318.236202	8.160717
6.322329	331.012783	8.165734
6.048963	311.708190	8.170752
6.084014	310.500461	8.175770
5.925026	318.464804	8.180787
6.141712	314.940962	8.185805
6.128737	315.113409	8.190822
5.892013	309.719449	8.195840
6.069582	318.180471	8.200858
6.174599	316.592639	8.205875
6.346914	317.395764	8.210893
5.953377	312.543742	8.215910
6.203846	320.740964	8.220928
6.208717	308.300733	8.225946
5.896121	308.901662	8.230963
6.240577	316.118626	8.235981
6.434782	322.295538	8.240998
6.415712	317.987938	8.246016
6.422474	304.758507	8.251034
6.362582	299.602091	8.256051
6.156348	298.835850	8.261069
6.257330	308.523708	8.266086
5.953621	307.592773	8.271104
6.225542	302.804393	8.276122
6.015001	301.890507	8.281139
5.680281	308.698846	8.286157
6.323904	313.190101	8.291174
5.939275	309.116134	8.296192
6.214588	305.450629	8.301210
6.212050	315.735245	8.306227
6.150258	313.737907	8.311245
6.024451	315.392134	8.316262
6.454168	321.775362	8.321280
6.480196	322.585486	8.326298
6.161507	318.914637	8.331315
6.563005	319.331804	8.336333
5.953906	311.133665	8.341350
6.063319	306.951221	8.346368
6.126997	315.594067	8.351386
6.412172	333.237008	8.356403
6.282781	314.490632	8.361421
6.172423	323.286803	8.366438
6.049634	329.591964	8.371456
6.388475	326.027011	8.376474
6.399346	332.361853	8.381491
6.507898	328.832755	8.386509
6.348395	317.737164	8.391526
6.120953	323.913458	8.396544
6.552066	319.381139	8.401562
6.133890	318.714164	8.406579
6.369605	314.319561	8.411597
6.491178	310.608568	8.416614
6.345468	311.249781	8.421632
6.125425	314.165154	8.426650
6.376464	317.161807	8.431667
6.517732	319.582294	8.436685
6.266924	318.204488	8.441702
5.992380	317.073362	8.446720
6.271790	313.549221	8.451738
6.023923	324.029820	8.456755
6.005687	325.105597	8.461773
6.286565	318.217323	8.466790
6.334394	328.853846	8.471808
6.691240	323.474757	8.476826
6.495954	326.244274	8.481843
6.462743	320.512529	8.486861
6.596133	326.932428	8.491878
6.235302	325.694822	8.496896
6.568392	313.118283	8.501914
6.547905	323.399386	8.506931
6.211931	330.362555	8.511949
6.690542	322.304309	8.516966
6.303481	331.212990	8.521984
6.615736	333.165067	8.527002
6.371049	329.589987	8.532019
6.492814	331.906220	8.537037
6.574601	321.000265	8.542054
6.275928	326.237805	8.547072
6.466752	320.799364	8.552090
6.357077	319.895019	8.557107
6.097534	327.439544	8.562125
6.842181	322.224127	8.567143
6.136785	340.993238	8.572160
6.563156	326.499318	8.577178
6.562768	325.858808	8.582195
6.527684	328.574982	8.587213
6.584457	320.039647	8.592231
6.716020	334.389938	8.597248
6.673209	329.691576	8.602266
6.613527	328.176721	8.607283
6.475844	324.730140	8.612301
6.852037	319.127146	8.617319
6.792625	326.047253	8.622336
7.050941	325.177126	8.627354
6.573246	325.791137	8.632371
6.503427	319.544412	8.637389
6.718939	318.157115	8.642407
6.282351	324.820383	8.647424
6.459660	319.485027	8.652442
6.596926	327.343291	8.657459
6.649732	331.229144	8.662477
6.653039	327.688031	8.667495
6.535868	333.225500	8.672512
6.505092	329.677071	8.677530
6.410442	323.298519	8.682547
6.309644	325.797718	8.687565
6.299578	328.484752	8.692583
6.412243	329.552771	8.697600
6.562915	326.200142	8.702618
6.924509	327.781640	8.707635
6.546705	330.784691	8.712653
6.953335	320.512932	8.717671
6.627947	339.213409	8.722688
6.430420	325.734918	8.727706
6.782286	331.170958	8.732723
6.465372	317.326075	8.737741
6.886939	323.981956	8.742759
6.924050	326.560664	8.747776
6.709577	320.046143	8.752794
6.825140	326.004940	8.757811
6.578137	338.602842	8.762829
7.093865	318.929243	8.767847
6.497608	326.074938	8.772864
6.529931	329.894555	8.777882
6.911550	325.833819	8.782899
6.514869	335.602332	8.787917
6.629027	316.587673	8.792935
6.739604	337.006357	8.797952
6.670990	331.128649	8.802970
7.150350	329.267949	8.807987
6.639796	322.297780	8.813005
6.453363	323.601706	8.818023
6.398089	332.076897	8.823040
6.540492	324.531720	8.828058
6.674468	329.995373	8.833075
6.798073	339.957421	8.838093
6.949098	339.959175	8.843111
7.067984	337.561339	8.848128
6.814153	325.347558	8.853146
6.837237	324.138535	8.858163
6.334702	326.350008	8.863181
6.952467	329.346368	8.868199
6.973167	341.239908	8.873216
7.345007	340.282681	8.878234
7.021202	334.233278	8.883251
6.760716	330.414517	8.888269
6.890939	321.157729	8.893287
6.430229	328.193963	8.898304
6.620260	328.401071	8.903322
6.680166	343.305294	8.908339
6.794831	351.059796	8.913357
7.112181	350.944141	8.918375
7.045433	358.004250	8.923392
7.080224	351.119566	8.928410
7.221399	338.765384	8.933427
6.816995	341.965072	8.938445
7.006921	327.851929	8.943463
6.930453	341.742336	8.948480
6.867819	328.605739	8.953498
7.198248	329.261177	8.958515
6.765813	334.667861	8.963533
6.857641	326.120754	8.968551
6.884631	338.470880	8.973568
6.793942	350.457505	8.978586
7.319827	352.357390	8.983603
7.012510	347.097480	8.988621
6.805995	337.489190	8.993639
7.045683	349.727317	8.998656
7.249209	355.429445	9.003674
7.230283	338.865324	9.008691
7.126419	339.159214	9.013709
6.770483	330.483015	9.018727
6.723296	327.697649	9.023744
6.881320	340.415518	9.028762
7.477009	341.193750	9.033779
7.246006	346.793125	9.038797
7.171552	328.874424	9.043815
6.768457	332.234844	9.048832
6.895548	336.080731	9.053850
7.117879	329.176323	9.058867
6.806325	336.025244	9.063885
7.089654	352.447261	9.068903
7.449843	354.704286	9.073920
7.176705	347.763411	9.078938
7.218702	337.794554	9.083955
6.906494	329.707962	9.088973
6.700455	330.046161	9.093991
7.152168	338.174191	9.099008
7.138542	352.897377	9.104026
7.523061	353.083672	9.109043
7.363540	352.067171	9.114061
7.163073	335.490295	9.119079
7.003819	339.923535	9.124096
6.988226	336.782973	9.129114
7.408207	340.201427	9.134131
7.278749	333.127740	9.139149
7.205852	328.121656	9.144167
6.923656	336.092567	9.149184
7.024138	333.959515	9.154202
7.596923	341.008402	9.159219
7.226377	333.981718	9.164237
7.581271	335.501147	9.169255
7.374097	328.704635	9.174272
7.361589	330.293889	9.179290
7.130297	333.693828	9.184307
6.984417	332.536357	9.189325
7.202760	331.685076	9.194343
7.072331	338.095565	9.199360
6.860430	332.420038	9.204378
7.226398	336.152997	9.209395
7.140948	351.979215	9.214413
7.541314	352.529096	9.219431
7.742279	348.606929	9.224448
7.427368	335.667387	9.229466
7.502271	331.906855	9.234483
7.158145	328.243121	9.239501
7.211628	332.914621	9.244519
7.304106	319.220578	9.249536
7.078664	327.804309	9.254554
7.317633	320.108405	9.259571
7.164559	328.851273	9.264589
7.601124	329.878329	9.269607
7.418328	330.531628	9.274624
7.366287	326.768772	9.279642
7.222517	325.238608	9.284659
7.117206	337.404217	9.289677
7.395782	345.597074	9.294695
7.789641	344.841535	9.299712
7.574314	341.100943	9.304730
7.568159	323.357796	9.309747
7.335750	328.136920	9.314765
6.910412	326.189873	9.319783
7.418485	329.307447	9.324800
7.142516	345.980631	9.329818
7.668729	350.218791	9.334835
7.803672	347.979391	9.339853
7.431975	325.726950	9.344871
7.237670	334.226945	9.349888
6.975463	342.396708	9.354906
7.230377	345.979711	9.359923
7.395052	355.013928	9.364941
7.781502	355.613311	9.369959
7.786419	354.621698	9.374976
7.566564	352.671055	9.379994
7.523784	339.790121	9.385011
7.251759	343.660283	9.390029
7.409559	347.637083	9.395047
7.932137	351.238370	9.400064
7.429026	344.980208	9.405082
7.367147	322.638510	9.410099
7.295298	332.848725	9.415117
7.233158	344.796189	9.420135
7.531996	347.940032	9.425152
7.440411	352.100821	9.430170
7.899646	347.538872	9.435187
7.778942	358.432014	9.440205
7.776628	347.539137	9.445223
7.832281	340.389291	9.450240
7.250064	335.692865	9.455258
7.774165	332.402008	9.460275
7.452732	340.628326	9.465293
7.621407	345.079933	9.470311
7.765179	346.767926	9.475328
7.532372	341.442771	9.480346
7.132649	341.905795	9.485363
7.309794	349.934576	9.490381
7.133683	349.185732	9.495399
7.771806	346.094858	9.500416
7.273223	346.166197	9.505434
7.202733	341.049287	9.510451
7.379358	341.141724	9.515469
7.264581	349.799749	9.520487
7.790174	364.041380	9.525504
7.763403	377.270860	9.530522
8.086310	363.266365	9.535539
7.625692	359.213685	9.540557
7.444592	356.048399	9.545575
7.705469	343.006581	9.550592
7.608974	357.414487	9.555610
7.738434	357.804586	9.560627
8.072528	369.084492	9.565645
7.728593	358.626630	9.570663
7.897298	346.350202	9.575680
7.713789	349.925732	9.580698
7.879587	348.593508	9.585715
7.820076	350.795964	9.590733
7.613153	355.678418	9.595751
7.361397	348.929863	9.600768
7.703589	358.971492	9.605786
7.998477	353.135007	9.610803
8.032430	371.006438	9.615821
7.690845	360.122197	9.620839
7.989952	351.403958	9.625856
7.553243	355.312385	9.630874
7.660806	363.165823	9.635891
7.890600	372.540186	9.640909
8.066422	373.812958	9.645927
7.913145	363.726175	9.650944
7.728299	364.846829	9.655962
7.955068	356.550083	9.660979
8.161606	361.999292	9.665997
7.968721	351.202353	9.671015
8.171143	353.556521	9.676032
7.584169	350.678479	9.681050
7.540239	341.379370	9.686067
7.750606	356.695656	9.691085
7.551810	368.405651	9.696103
7.903876	366.608946	9.701120
8.044147	373.800923	9.706138
7.936865	365.972727	9.711155
8.217863	375.518991	9.716173
7.946522	384.217187	9.721191
8.257128	368.529490	9.726208
7.891021	363.733141	9.731226
7.777814	368.181308	9.736243
8.358707	366.285862	9.741261
7.750289	367.825896	9.746279
7.863965	365.804389	9.751296
7.796315	373.385325	9.756314
8.053458	375.932938	9.761331
7.912522	373.222119	9.766349
7.803327	375.201951	9.771367
7.989708	369.675829	9.776384
7.758054	365.464428	9.781402
7.524038	377.732150	9.786419
7.673152	366.168778	9.791437
7.663133	373.037034	9.796455
8.042752	369.560393	9.801472
7.844658	383.927338	9.806490
7.932737	380.527643	9.811507
7.939512	383.941016	9.816525
8.327246	395.865805	9.821543
8.806983	385.137681	9.826560
8.197348	379.277924	9.831578
7.987771	375.792037	9.836595
8.642910	366.242069	9.841613
7.976498	368.576888	9.846631
8.162746	375.070621	9.851648
8.044836	373.110416	9.856666
8.010905	369.032323	9.861683
8.164551	374.051137	9.866701
7.714552	383.383032	9.871719
8.278179	371.780364	9.876736
8.271005	371.888795	9.881754
8.028466	375.770151	9.886771
8.331543	365.949968	9.891789
7.934449	373.547486	9.896807
8.519645	379.502605	9.901824
7.849868	380.020298	9.906842
8.195391	390.026714	9.911859
8.290216	398.140914	9.916877
8.099659	395.081229	9.921895
8.324614	394.471900	9.926912
8.746666	398.884072	9.931930
8.120218	384.976881	9.936947
8.110287	380.128227	9.941965
8.014255	380.786953	9.946983
8.448277	385.194102	9.952000
8.270800	394.868560	9.957018
8.492456	391.883545	9.962035
8.216859	381.096309	9.967053
8.149124	386.708144	9.972071
8.601544	392.573493	9.977088
8.483806	391.765068	9.982106
8.361364	387.113802	9.987123
8.300464	381.834449	9.992141
8.216282	382.942587	9.997159
8.341941	380.464800	10.002176
8.686130	387.798594	10.007194
8.346908	385.437365	10.012211
8.368374	383.616395	10.017229
8.420249	382.529112	10.022247
7.942825	379.387868	10.027264
8.167952	381.855264	10.032282
8.383674	394.797706	10.037299
8.553714	397.163233	10.042317
8.469760	402.730264	10.047335
8.577096	400.353152	10.052352
8.275122	397.654779	10.057370
7.968588	397.450076	10.062387
8.442739	401.525950	10.067405
8.350584	402.979295	10.072423
8.291921	402.417280	10.077440
8.473814	396.036668	10.082458
8.289306	399.684943	10.087475
8.824401	393.646952	10.092493
8.526389	407.811733	10.097511
8.437276	408.952197	10.102528
8.499842	406.569432	10.107546
8.308172	405.949234	10.112563
8.482781	405.376144	10.117581
8.684224	403.492438	10.122599
8.675883	398.668777	10.127616
8.612120	407.666008	10.132634
8.245620	397.669205	10.137651
8.409590	396.147923	10.142669
8.582354	402.041038	10.147687
8.453380	395.279659	10.152704
8.408678	403.554434	10.157722
8.274451	404.948061	10.162739
8.360430	390.361928	10.167757
8.496757	397.964762	10.172775
8.641137	405.487455	10.177792
8.914706	410.235157	10.182810
8.713077	404.955619	10.187827
8.923437	401.054067	10.192845
8.483549	389.730701	10.197863
8.511919	401.458994	10.202880
8.276828	405.187726	10.207898
8.689401	417.872329	10.212915
9.000551	414.775551	10.217933
8.559622	410.022395	10.222951
8.566791	409.014650	10.227968
9.082905	412.086808	10.232986
8.690511	411.349546	10.238003
8.339132	404.023219	10.243021
8.183778	408.563160	10.248039
8.966336	419.009607	10.253056
9.188824	408.804336	10.258074
8.850967	419.740792	10.263091
8.891102	412.211500	10.268109
8.896893	409.471519	10.273127
8.696724	397.211465	10.278144
8.777650	405.340455	10.283162
8.800132	412.175265	10.288179
8.551567	398.613151	10.293197
8.463939	419.864324	10.298215
9.362050	410.995991	10.303232
9.107681	415.238941	10.308250
9.288901	417.258765	10.313267
8.804564	395.456098	10.318285
8.580198	401.243795	10.323303
8.539493	402.591305	10.328320
8.760298	407.290419	10.333338
9.318969	412.018977	10.338355
8.864393	408.271442	10.343373
8.439104	412.203349	10.348391
8.753185	412.646752	10.353408
8.965535	413.528850	10.358426
8.754277	426.010801	10.363443
8.821611	416.230450	10.368461
8.660499	430.146728	10.373479
8.597982	426.606377	10.378496
8.853314	420.596156	10.383514
8.619290	432.235942	10.388531
8.789995	421.732627	10.393549
8.551653	420.422297	10.398567
8.659541	421.857121	10.403584
9.122260	422.299471	10.408602
8.889090	432.657930	10.413619
8.864511	424.835766	10.418637
9.283542	445.335931	10.423655
9.020832	435.698469	10.428672
9.349529	423.368677	10.433690
8.664619	422.519176	10.438707
9.030505	425.141379	10.443725
9.242569	427.664461	10.448743
9.125937	423.144818	10.453760
9.007439	423.428365	10.458778
8.826561	429.433352	10.463795
9.406719	432.006416	10.468813
9.254023	426.526758	10.473831
9.199917	428.176143	10.478848
9.416903	422.777777	10.483866
9.062975	429.308299	10.488883
9.146312	425.136199	10.493901
8.871479	430.130229	10.498919
9.262736	427.317607	10.503936
9.209916	425.113743	10.508954
9.200621	432.669841	10.513971
9.017106	420.227306	10.518989
9.023068	424.625376	10.524007
9.180590	425.314050	10.529024
9.079147	417.986671	10.534042
8.902192	424.480171	10.539059
9.110754	434.006188	10.544077
8.964875	436.477709	10.549095
9.197138	438.565324	10.554112
9.738700	435.199149	10.559130
9.359213	441.982952	10.564147
9.290424	438.377307	10.569165
9.185899	447.898432	10.574183
9.091848	446.732883	10.579200
9.338581	438.259430	10.584218
9.080861	443.433826	10.589235
9.447419	443.218995	10.594253
9.644784	446.501725	10.599271
9.315100	445.148812	10.604288
9.179318	436.829585	10.609306
8.955040	442.440565	10.614323
9.293859	445.556112	10.619341
9.276028	449.241559	10.624359
9.171545	453.549540	10.629376
9.383542	452.573015	10.634394
9.241985	451.102453	10.639411
9.089091	447.087043	10.644429
9.341404	456.306473	10.649447
9.274221	453.120277	10.654464
9.611660	443.824851	10.659482
9.355528	440.478736	10.664499
9.470020	440.034920	10.669517
9.132125	445.060862	10.674535
9.455190	440.147723	10.679552
9.391111	439.302541	10.684570
9.395726	451.738276	10.689587
9.397366	448.323625	10.694605
9.604264	434.677948	10.699623
8.912693	453.558628	10.704640
9.733123	440.628425	10.709658
9.554068	454.099412	10.714675
9.343818	451.528755	10.719693
9.412248	442.335171	10.724711
9.054597	456.099041	10.729728
9.658856	465.181632	10.734746
9.858968	466.176086	10.739763
9.489095	455.655937	10.744781
9.564330	440.333012	10.749799
9.200680	451.775253	10.754816
9.637501	457.213883	10.759834
9.800479	466.226331	10.764851
9.930468	470.690305	10.769869
9.725844	451.097159	10.774887
9.189767	451.773910	10.779904
9.648878	453.665269	10.784922
9.406193	457.833830	10.789939
9.433446	466.454019	10.794957
9.515024	452.976155	10.799975
9.493669	466.274283	10.804992
9.760413	469.284296	10.810010
9.942684	476.043761	10.815027
9.679175	472.705101	10.820045
10.104540	465.794274	10.825063
9.721015	472.105368	10.830080
10.144473	458.536403	10.835098
9.523318	460.321413	10.840115
9.695864	452.976606	10.845133
9.537219	440.801571	10.850151
9.674497	462.102979	10.855168
9.937020	461.803365	10.860186
10.010731	464.701427	10.865203
9.548889	461.377870	10.870221
10.108017	461.991394	10.875239
9.685552	453.644215	10.880256
9.554875	446.226706	10.885274
9.671405	455.596658	10.890291
9.412259	460.203263	10.895309
9.422783	465.948098	10.900327
9.632836	470.570012	10.905344
9.907682	468.277258	10.910362
9.815776	474.359921	10.915379
9.982532	472.396407	10.920397
9.996168	466.789858	10.925415
9.748978	474.196829	10.930432
9.876397	477.604059	10.935450
9.903342	463.759170	10.940467
10.000777	468.149320	10.945485
9.838196	472.822941	10.950503
10.093601	476.500564	10.955520
10.154008	472.025925	10.960538
9.630415	460.128594	10.965555
9.427704	479.024701	10.970573
9.939953	457.988245	10.975591
10.016234	465.578368	10.980608
9.936042	464.047760	10.985626
10.030986	466.153602	10.990643
10.157454	475.096004	10.995661
10.061537	469.112054	11.000679
9.955206	471.132475	11.005696
10.029862	470.644370	11.010714
10.022806	467.739130	11.015731
9.923318	469.111576	11.020749
10.350636	461.288462	11.025767
9.872066	477.100262	11.030784
9.804326	470.540750	11.035802
9.582058	472.557133	11.040819
9.897130	482.776616	11.045837
10.174652	487.315449	11.050855
10.044963	492.239562	11.055872
9.858382	493.833843	11.060890
9.984228	490.343044	11.065907
9.723887	498.619880	11.070925
9.840393	496.285507	11.075943
10.133640	489.676095	11.080960
10.166440	491.261465	11.085978
10.020349	493.086116	11.090995
9.934922	490.697981	11.096013
10.235821	494.431638	11.101031
10.028009	494.249432	11.106048
10.177722	491.537521	11.111066
10.351512	493.886699	11.116083
10.009851	494.473224	11.121101
9.965245	492.722488	11.126119
10.633841	502.006510	11.131136
10.242364	490.880660	11.136154
10.289039	489.507014	11.141171
10.424010	494.481435	11.146189
10.572482	488.696103	11.151207
10.479193	496.902749	11.156224
10.263086	494.074233	11.161242
10.498150	493.769426	11.166259
10.190870	493.340786	11.171277
10.344459	492.922438	11.176295
10.302867	492.196823	11.181312
10.496089	494.792273	11.186330
10.921244	492.365666	11.191347
10.544140	489.249806	11.196365
10.747247	489.174027	11.201383
10.456366	495.268743	11.206400
10.869387	489.114032	11.211418
10.831919	477.576483	11.216435
10.496935	468.653968	11.221453
10.524935	462.530812	11.226471
10.358737	462.253769	11.231488
10.336321	463.996048	11.236506
10.280731	464.124641	11.241523
10.090457	469.256987	11.246541
10.540582	485.918234	11.251559
10.511019	493.619518	11.256576
10.445001	497.078959	11.261594
10.803104	495.827230	11.266611
10.324930	493.320371	11.271629
10.551073	495.683488	11.276647
10.729987	492.487369	11.281664
10.385466	488.321913	11.286682
10.898694	482.643886	11.291699
10.275192	480.140722	11.296717
10.363929	477.138519	11.301735
10.607001	490.310291	11.306752
10.703033	496.865451	11.311770
10.562857	491.989711	11.316787
10.286309	500.407920	11.321805
10.668689	499.329129	11.326823
10.535517	498.822890	11.331840
10.298963	490.513016	11.336858
10.933689	492.739937	11.341875
10.741576	500.908326	11.346893
10.653908	494.882059	11.351911
10.515956	501.158085	11.356928
10.645434	499.594829	11.361946
10.809838	500.200388	11.366963
10.855819	500.215341	11.371981
10.796072	500.322492	11.376999
10.632785	502.986073	11.382016
10.465955	495.637285	11.387034
10.933720	501.172092	11.392051
10.655928	507.589808	11.397069
11.202617	495.686753	11.402087
10.750210	501.270157	11.407104
10.963465	498.848140	11.412122
10.877122	495.942618	11.417139
10.805789	500.841869	11.422157
10.351677	496.800766	11.427175
10.430244	489.988105	11.432192
10.657650	499.441798	11.437210
10.746145	496.281847	11.442227
10.445908	498.222013	11.447245
10.611603	501.588576	11.452263
10.723169	496.525323	11.457280
10.753952	505.564685	11.462298
10.792508	516.796029	11.467315
11.216477	521.444608	11.472333
10.601042	521.827617	11.477351
11.179919	516.073089	11.482368
10.914175	513.782450	11.487386
10.688880	501.974341	11.492403
10.803503	516.870190	11.497421
11.031359	513.672759	11.502439
11.242970	528.645032	11.507456
11.116430	522.141992	11.512474
11.002428	501.461754	11.517491
10.882481	520.455468	11.522509
10.738340	519.660615	11.527527
11.085927	516.788510	11.532544
10.849515	519.520280	11.537562
11.346321	515.059732	11.542579
10.906612	522.815420	11.547597
11.373634	518.296394	11.552615
11.235000	515.250694	11.557632
11.079400	521.987047	11.562650
11.266022	525.388224	11.567667
11.089110	509.779464	11.572685
10.701252	506.371799	11.577703
11.310580	512.594593	11.582720
10.759976	523.510591	11.587738
11.378214	520.675237	11.592755
11.033283	526.516459	11.597773
10.947354	531.970233	11.602791
11.461970	524.161900	11.607808
11.239307	526.749526	11.612826
11.118080	528.854320	11.617843
11.463989	521.217417	11.622861
11.200723	523.587312	11.627879
11.123095	532.100791	11.632896
11.195304	521.120469	11.637914
11.252244	529.351075	11.642931
11.402770	522.451461	11.647949
11.259476	527.229386	11.652967
11.398662	521.637985	11.657984
11.018964	525.632242	11.663002
10.872388	530.776736	11.668019
11.123028	523.684817	11.673037
11.118650	534.017180	11.678055
11.113449	521.202844	11.683072
10.887694	523.352313	11.688090
11.023600	518.761770	11.693107
11.254723	532.967337	11.698125
11.247449	541.823303	11.703143
11.486249	545.162713	11.708160
11.201686	547.810471	11.713178
11.041395	549.182922	11.718195
11.348276	552.066784	11.723213
11.497048	546.966168	11.728231
11.721677	545.306046	11.733248
11.439320	552.731147	11.738266
11.445348	549.517757	11.743283
11.635851	542.592977	11.748301
11.710393	537.633303	11.753319
11.811230	545.907573	11.758336
11.603798	554.365537	11.763354
11.604346	549.287997	11.768371
11.432070	540.008769	11.773389
11.427044	549.713263	11.778407
11.674748	550.416302	11.783424
11.323122	544.001945	11.788442
11.300347	545.605439	11.793459
11.431258	540.536006	11.798477
11.112476	549.216423	11.803495
11.370312	531.580283	11.808512
11.181465	552.664345	11.813530
11.449823	552.666765	11.818547
11.253986	551.611727	11.823565
11.376724	562.246194	11.828583
11.748477	568.319812	11.833600
11.608330	577.275375	11.838618
11.882066	576.566930	11.843635
12.147522	575.749326	11.848653
11.781341	565.957498	11.853671
11.675400	551.808195	11.858688
11.423469	551.168973	11.863706
11.640130	557.538123	11.868723
11.902801	569.129066	11.873741
11.488516	573.478999	11.878759
11.946330	571.135655	11.883776
11.779106	579.107708	11.888794
11.781757	570.678506	11.893811
11.870615	567.007266	11.898829
11.697680	579.347663	11.903847
12.069747	570.046780	11.908864
11.635242	567.820278	11.913882
12.083072	574.759331	11.918899
11.858111	564.633104	11.923917
11.620458	565.784082	11.928935
11.584326	571.662442	11.933952
11.835047	567.615721	11.938970
11.962573	576.583254	11.943987
12.050398	571.343803	11.949005
11.817651	577.855512	11.954023
12.229552	572.451998	11.959040
11.934341	571.601772	11.964058
11.785243	575.806280	11.969075
11.769670	571.340290	11.974093
11.812971	581.204528	11.979111
11.854055	573.488836	11.984128
11.589727	582.255461	11.989146
11.356658	572.957279	11.994163
11.837679	575.492153	11.999181
11.648242	580.444527	12.004199
11.809175	585.001537	12.009216
11.977499	601.492181	12.014234
12.022206	599.781176	12.019251
11.951813	603.654712	12.024269
11.922686	608.774631	12.029287
12.273926	603.942264	12.034304
12.059468	606.146787	12.039322
12.019390	601.965460	12.044339
12.348224	604.546123	12.049357
12.013833	605.118897	12.054375
12.493843	603.908138	12.059392
12.101011	605.528230	12.064410
11.824281	606.827301	12.069427
11.987125	606.066695	12.074445
11.927088	611.667935	12.079463
11.954763	606.835455	12.084480
12.371554	603.832645	12.089498
12.346650	606.916491	12.094515
12.424895	599.466390	12.099533
12.232974	605.539424	12.104551
12.422012	599.195496	12.109568
12.165593	599.409005	12.114586
12.466216	603.272111	12.119603
12.326608	596.616449	12.124621
12.036427	606.008780	12.129639
12.406131	598.443875	12.134656
12.766938	601.622295	12.139674
12.454409	598.433248	12.144691
12.467266	592.675308	12.149709
12.312796	596.082271	12.154727
12.393433	596.028715	12.159744
12.423345	598.050028	12.164762
12.206839	600.074994	12.169779
12.448894	595.411102	12.174797
12.655826	598.373647	12.179815
12.594998	592.093870	12.184832
12.586617	602.095549	12.189850
12.485096	611.376462	12.194867
12.597469	598.076724	12.199885
12.204987	605.834561	12.204903
12.233348	601.339633	12.209920
12.441261	600.843400	12.214938
12.334980	601.693070	12.219955
12.663030	601.780867	12.224973
12.414940	607.348271	12.229991
12.317091	606.293752	12.235008
12.661516	600.989095	12.240026
12.457678	599.692313	12.245043
12.380675	597.337564	12.250061
12.473544	609.794382	12.255079
12.440452	602.967505	12.260096
12.401785	601.092762	12.265114
12.569082	608.738200	12.270131
12.648943	615.153916	12.275149
12.770528	625.959007	12.280167
12.809507	628.865659	12.285184
12.585477	622.216820	12.290202
12.559920	629.813402	12.295219
12.591608	627.211362	12.300237
12.965214	633.644463	12.305255
12.603493	626.041953	12.310272
12.680149	624.761455	12.315290
12.933973	620.281910	12.320307
13.120737	619.770035	12.325325
12.812882	618.773458	12.330343
12.557257	619.321346	12.335360
12.858961	622.521594	12.340378
13.056580	630.004536	12.345395
13.020753	624.374082	12.350413
12.767084	612.674454	12.355431
12.775455	616.100246	12.360448
12.954839	613.891762	12.365466
12.489482	625.491955	12.370483
12.790519	624.040828	12.375501
12.795771	627.293545	12.380519
12.785955	635.250582	12.385536
12.684698	624.129953	12.390554
12.636545	637.378734	12.395571
12.772924	625.435339	12.400589
12.523468	629.459832	12.405607
12.658208	628.059842	12.410624
13.018148	628.698074	12.415642
12.986473	637.845054	12.420659
12.906672	632.322426	12.425677
13.003243	638.445225	12.430695
13.088859	627.153493	12.435712
13.081271	630.013749	12.440730
12.762338	638.564850	12.445747
13.029105	641.751607	12.450765
13.399201	649.864086	12.455783
13.082757	658.137108	12.460800
13.253252	649.770095	12.465818
12.951653	648.655782	12.470835
13.042682	644.917919	12.475853
13.099832	656.790217	12.480871
13.138609	662.666411	12.485888
13.261603	649.923538	12.490906
13.192383	659.786405	12.495923
13.470726	652.645942	12.500941
13.250137	650.013751	12.505959
13.274035	649.315802	12.510976
13.287842	644.008961	12.515994
12.760019	641.194242	12.521011
13.164310	646.098372	12.526029
13.149843	655.450957	12.531047
13.089367	652.954777	12.536064
13.415470	649.672601	12.541082
13.097883	661.514888	12.546099
13.110610	653.450138	12.551117
13.534456	647.457784	12.556135
13.498271	649.593531	12.561152
13.493184	645.315231	12.566170
13.260494	651.924784	12.571187
13.620755	643.373599	12.576205
13.736667	646.719540	12.581223
13.250081	643.497627	12.586240
13.444525	648.570125	12.591258
13.263986	649.614390	12.596275
13.343356	651.883619	12.601293
13.274445	654.930145	12.606311
13.084099	652.293246	12.611328
13.362256	646.380377	12.616346
13.353650	651.490802	12.621363
13.227034	648.342226	12.626381
13.354479	655.548937	12.631399
13.148311	658.910313	12.636416
13.419172	658.612553	12.641434
13.502514	678.370018	12.646451
13.583827	672.692909	12.651469
13.761472	670.759234	12.656487
13.477729	673.040822	12.661504
13.913618	664.976451	12.666522
13.699706	675.275250	12.671539
13.987737	669.493377	12.676557
13.726603	655.194592	12.681575
13.410842	655.048125	12.686592
13.615936	645.659594	12.691610
13.792446	653.262593	12.696627
13.832071	648.892127	12.701645
13.458556	647.564957	12.706663
13.601566	653.775202	12.711680
14.065174	657.379423	12.716698
13.758364	662.839226	12.721715
13.711353	661.196141	12.726733
13.800167	653.766462	12.731751
13.669218	665.267279	12.736768
13.759217	658.033066	12.741786
13.828837	679.588257	12.746803
13.970181	679.515782	12.751821
13.922364	673.073010	12.756839
13.787105	677.805544	12.761856
13.973542	680.941702	12.766874
13.812118	678.590619	12.771891
13.691223	675.968148	12.776909
14.203095	668.317965	12.781927
13.794217	669.751220	12.786944
14.077492	670.915768	12.791962
13.900548	679.088188	12.796979
13.986542	673.665961	12.801997
14.024090	673.237275	12.807015
14.097680	668.473366	12.812032
14.004916	673.489606	12.817050
13.821710	671.104047	12.822067
13.967608	674.533684	12.827085
13.939287	680.177343	12.832103
13.925484	677.942127	12.837120
13.942505	673.900210	12.842138
13.846889	672.012237	12.847155
13.727754	683.179878	12.852173
13.993718	680.068000	12.857191
14.087550	677.778157	12.862208
14.181817	669.915292	12.867226
14.238653	675.791835	12.872243
13.877595	676.476056	12.877261
13.978138	663.541016	12.882279
13.976505	670.521686	12.887296
14.004024	667.282838	12.892314
14.023018	671.691563	12.897331
13.841497	675.124842	12.902349
14.426484	680.893910	12.907367
14.110893	688.740795	12.912384
14.530127	688.341040	12.917402
14.559756	685.799270	12.922419
14.349074	681.729691	12.927437
14.405854	669.552515	12.932455
13.858797	681.263291	12.937472
13.977764	681.705523	12.942490
14.344625	689.878483	12.947507
14.097125	694.262436	12.952525
14.137052	688.433980	12.957543
14.271787	701.793185	12.962560
14.463407	694.776657	12.967578
14.819530	695.361839	12.972595
14.467362	701.986858	12.977613
14.760874	690.372393	12.982631
14.421607	701.116743	12.987648
14.751558	685.441535	12.992666
14.603719	691.611873	12.997683
14.508519	693.163543	13.002701
14.772297	697.205970	13.007719
14.639116	708.041310	13.012736
14.538673	698.921221	13.017754
14.722313	684.142923	13.022771
14.244603	678.338263	13.027789
14.335926	683.843378	13.032807
14.640839	697.728330	13.037824
14.408418	697.597288	13.042842
14.582126	701.401284	13.047859
14.399253	696.854016	13.052877
14.563033	693.584482	13.057895
14.841297	694.727722	13.062912
14.438277	700.685338	13.067930
14.411622	702.141133	13.072947
14.342117	697.399495	13.077965
14.838771	696.252409	13.082983
14.556423	694.033757	13.088000
14.632308	688.313309	13.093018
15.103188	695.330869	13.098035
14.676823	691.768223	13.103053
15.167369	690.230782	13.108071
14.834979	688.928763	13.113088
14.473502	696.432512	13.118106
14.771182	697.427568	13.123123
14.440847	698.854907	13.128141
14.956200	690.872824	13.133159
14.478672	701.159035	13.138176
15.090018	705.933118	13.143194
14.793963	707.831631	13.148211
15.002932	713.349996	13.153229
15.231170	702.559857	13.158247
14.963548	694.182144	13.163264
14.709596	688.598253	13.168282
14.829463	693.224800	13.173299
14.995428	704.821420	13.178317
15.101777	709.128194	13.183335
15.003109	711.418840	13.188352
15.084969	709.992363	13.193370
15.301790	698.525528	13.198387
14.829010	699.526937	13.203405
14.970882	698.826395	13.208423
15.200162	710.955942	13.213440
15.180683	707.891657	13.218458
14.940710	700.850809	13.223475
14.884573	716.817949	13.228493
15.433470	714.842245	13.233511
15.233698	723.144467	13.238528
15.060535	713.066893	13.243546
15.252138	717.628630	13.248563
14.953067	724.702966	13.253581
15.175971	720.303947	13.258599
15.221140	723.013997	13.263616
14.913742	723.661464	13.268634
15.206247	716.414632	13.273651
15.052789	714.800739	13.278669
15.482202	713.067694	13.283687
15.143860	724.310515	13.288704
15.313818	718.089432	13.293722
15.721535	712.304688	13.298739
15.497172	725.978588	13.303757
15.374780	720.790757	13.308775
15.376734	714.397023	13.313792
15.281205	720.881109	13.318810
15.915593	714.199566	13.323827
15.406749	724.279234	13.328845
15.652996	717.863242	13.333863
15.273477	721.696575	13.338880
15.356318	726.215289	13.343898
15.234541	717.874816	13.348915
15.336396	721.765740	13.353933
15.591366	715.641871	13.358951
15.328685	716.402292	13.363968
15.280779	722.105816	13.368986
15.714543	716.588406	13.374003
15.317304	719.742865	13.379021
15.215239	724.337704	13.384039
15.333906	723.457744	13.389056
15.211928	718.724270	13.394074
15.450324	729.293494	13.399091
15.397393	745.471592	13.404109
15.912997	747.679225	13.409127
15.726578	751.930610	13.414144
15.818456	746.068801	13.419162
15.982269	749.574556	13.424179
15.555816	742.553258	13.429197
15.679279	739.987403	13.434215
15.361318	732.052997	13.439232
15.315400	740.618442	13.444250
15.674314	727.930297	13.449267
15.744405	740.851485	13.454285
15.590228	739.392331	13.459303
15.935744	741.960950	13.464320
15.835491	740.581760	13.469338
16.167176	733.199437	13.474355
15.775892	741.966973	13.479373
16.045318	738.135044	13.484391
15.617979	743.784046	13.489408
15.904682	736.815812	13.494426
15.851619	731.244810	13.499443
15.773450	732.288919	13.504461
15.890849	733.091146	13.509479
16.134452	731.323915	13.514496
15.500192	734.701467	13.519514
15.515374	726.216593	13.524531
15.722782	739.561355	13.529549
15.661107	745.872926	13.534567
16.036054	756.045376	13.539584
15.898935	761.718623	13.544602
16.301227	759.519595	13.549619
16.271089	758.751162	13.554637
16.364125	765.963275	13.559655
16.649351	749.982558	13.564672
16.066514	747.539294	13.569690
16.188025	735.415109	13.574707
16.082582	740.569037	13.579725
16.228944	735.806403	13.584743
16.071053	735.360808	13.589760
15.992279	734.196018	13.594778
16.452601	746.949160	13.599795
16.200189	745.120304	13.604813
16.180424	742.841828	13.609831
16.473247	744.793822	13.614848
16.318195	745.723673	13.619866
16.136960	729.774577	13.624883
16.201027	750.043191	13.629901
15.947800	766.943594	13.634919
16.423154	761.599570	13.639936
16.706678	776.807001	13.644954
16.839856	755.242253	13.649971
16.571248	749.685871	13.654989
16.158704	742.627695	13.660007
15.941493	740.070701	13.665024
16.203481	762.015750	13.670042
16.665480	760.943482	13.675059
16.708276	769.255294	13.680077
16.134832	770.038856	13.685095
16.560386	765.557783	13.690112
16.523876	762.145856	13.695130
16.589674	760.999579	13.700147
16.873754	773.171127	13.705165
16.845999	771.057989	13.710183
16.639646	763.027300	13.715200
16.438093	768.906235	13.720218
16.712789	759.453161	13.725235
16.763748	772.595095	13.730253
16.676264	765.126549	13.735271
16.544132	757.403032	13.740288
16.431781	759.487537	13.745306
16.756212	753.791484	13.750323
16.519803	756.289768	13.755341
16.508153	765.777668	13.760359
16.634263	767.111856	13.765376
16.625613	766.324297	13.770394
17.083703	763.668471	13.775411
17.057518	760.336985	13.780429
16.559445	763.188425	13.785447
16.924707	760.035827	13.790464
16.565948	769.363184	13.795482
16.793125	761.337577	13.800499
16.675206	764.300237	13.805517
16.545638	757.860696	13.810535
17.020177	769.538699	13.815552
16.637428	766.149123	13.820570
16.871977	758.554702	13.825587
16.805170	753.755826	13.830605
16.725355	764.930020	13.835623
17.034915	762.262606	13.840640
16.447275	771.133309	13.845658
16.932916	780.909853	13.850675
17.148724	786.433487	13.855693
17.145680	785.121207	13.860711
17.005052	787.550935	13.865728
16.765460	789.361773	13.870746
16.689274	787.079453	13.875763
16.780145	785.585298	13.880781
16.896337	797.136081	13.885799
17.257056	786.401002	13.890816
16.992641	794.899509	13.895834
16.956054	785.015218	13.900851
17.348669	786.787582	13.905869
17.283002	788.258925	13.910887
17.558952	779.506214	13.915904
17.056599	781.938613	13.920922
17.071261	784.110640	13.925939
17.092144	785.382319	13.930957
16.976617	778.643947	13.935975
17.422190	774.522662	13.940992
17.185630	786.084180	13.946010
17.304728	789.899852	13.951027
17.450176	792.524875	13.956045
17.307762	796.816754	13.961063
17.492436	800.918856	13.966080
17.211853	798.794588	13.971098
17.505371	805.344359	13.976115
17.533043	803.083736	13.981133
17.658085	815.314788	13.986151
17.448511	806.457782	13.991168
17.444456	810.374682	13.996186
17.479904	804.742541	14.001203
17.719159	800.776445	14.006221
17.469986	806.359858	14.011239
17.737045	799.359945	14.016256
17.543162	805.925645	14.021274
17.671854	802.737290	14.026291
17.502707	801.293085	14.031309
17.513340	805.324458	14.036327
17.727933	808.364739	14.041344
17.870591	818.279909	14.046362
17.576768	806.513824	14.051379
17.876903	808.594071	14.056397
17.473795	804.027418	14.061415
17.758569	801.991846	14.066432
17.671009	810.488070	14.071450
17.928663	817.384248	14.076467
17.762286	823.223011	14.081485
17.809666	823.221969	14.086503
17.573315	812.349468	14.091520
17.629816	816.547267	14.096538
17.767387	812.271961	14.101555
17.847002	814.481215	14.106573
17.946735	819.413878	14.111591
17.734228	816.849830	14.116608
17.887209	819.154955	14.121626
18.036188	816.427331	14.126643
17.721611	814.753309	14.131661
17.514384	817.016690	14.136679
17.564324	812.322695	14.141696
17.751719	812.482884	14.146714
17.849942	825.349262	14.151731
18.129744	809.962612	14.156749
17.516752	815.246077	14.161767
18.048893	823.500660	14.166784
18.151269	837.253158	14.171802
18.093363	843.292784	14.176819
18.045593	842.949959	14.181837
18.509578	832.145127	14.186855
18.726412	823.650901	14.191872
18.302529	811.690473	14.196890
17.876588	812.608857	14.201907
18.163325	809.853474	14.206925
18.058870	809.396402	14.211943
17.958358	811.952428	14.216960
18.312271	828.938236	14.221978
18.244622	838.860916	14.226995
18.323674	836.854214	14.232013
18.382762	833.528373	14.237031
18.570697	830.469641	14.242048
18.303920	830.438619	14.247066
18.313603	830.386642	14.252083
18.741555	824.538753	14.257101
18.164054	816.540580	14.262119
18.633620	830.693482	14.267136
18.482403	812.622148	14.272154
18.035922	819.997177	14.277171
18.764534	825.144344	14.282189
18.396116	842.028040	14.287207
18.403339	834.715128	14.292224
18.538840	836.931461	14.297242
18.107255	838.235723	14.302259
18.619981	830.399151	14.307277
18.574704	840.886378	14.312295
18.548634	835.614091	14.317312
18.612671	833.290999	14.322330
18.391946	843.527841	14.327347
18.945295	830.317058	14.332365
18.661434	839.446602	14.337383
18.805353	835.725710	14.342400
18.646583	844.302464	14.347418
18.584525	841.118556	14.352435
18.516296	844.935005	14.357453
18.696761	843.139725	14.362471
18.233508	843.877732	14.367488
18.430357	837.952214	14.372506
18.410584	836.970730	14.377523
18.722240	846.572433	14.382541
18.620722	866.100118	14.387559
19.028169	861.511390	14.392576
18.801585	870.215476	14.397594
18.360839	872.957024	14.402611
18.563062	865.689476	14.407629
18.539461	870.653978	14.412647
18.486656	870.977796	14.417664
18.445959	872.947018	14.422682
18.583536	888.107842	14.427699
19.324127	888.109320	14.432717
18.927733	891.910602	14.437735
19.089353	889.976243	14.442752
19.445428	893.881271	14.447770
18.991900	893.759407	14.452787
19.098108	885.102499	14.457805
19.032693	890.770934	14.462823
19.284834	886.894329	14.467840
19.466544	889.450605	14.472858
19.104519	888.629700	14.477875
19.406210	880.333669	14.482893
19.093217	878.264928	14.487911
19.216753	877.911210	14.492928
19.527633	865.984665	14.497946
19.148179	861.979190	14.502963
19.135871	868.507174	14.507981
19.299759	866.099106	14.512999
19.039115	881.583850	14.518016
19.367830	881.005687	14.523034
19.491269	888.752746	14.528051
19.825238	885.791186	14.533069
19.271091	868.053924	14.538087
19.074720	863.562362	14.543104
19.413186	881.099723	14.548122
19.387900	883.662980	14.553139
19.583889	885.017855	14.558157
19.519002	887.278017	14.563175
19.455096	888.644954	14.568192
19.592013	883.113752	14.573210
19.162432	892.161872	14.578227
19.649169	876.465242	14.583245
19.523251	888.369353	14.588263
19.414276	891.393756	14.593280
19.372155	886.591000	14.598298
19.217822	888.429598	14.603315
19.608862	881.179981	14.608333
19.827331	885.876431	14.613351
19.270765	893.492686	14.618368
19.492090	886.278958	14.623386
19.552837	892.457914	14.628403
19.500142	884.867138	14.633421
19.590786	898.362740	14.638439
19.526686	913.154207	14.643456
19.717513	913.291773	14.648474
19.821812	921.704531	14.653491
19.766688	911.491704	14.658509
19.835357	917.000419	14.663527
19.920536	916.633737	14.668544
19.801818	916.702736	14.673562
19.961068	921.433660	14.678579
20.126913	916.181961	14.683597
20.293480	909.699413	14.688615
20.311919	914.149309	14.693632
20.143097	911.837216	14.698650
20.194254	919.030665	14.703667
20.332936	909.756476	14.708685
20.030528	897.628757	14.713703
19.628240	904.450998	14.718720
20.142692	903.641948	14.723738
19.440596	925.759392	14.728755
19.931359	915.262759	14.733773
20.041508	912.187723	14.738791
19.799906	916.943189	14.743808
20.225608	921.159268	14.748826
19.848223	921.347433	14.753843
19.706875	918.586103	14.758861
19.990735	927.788243	14.763879
19.868500	929.334675	14.768896
20.589105	933.624760	14.773914
19.954674	940.735617	14.778931
20.178710	937.718583	14.783949
20.410542	939.626447	14.788967
20.574257	936.069706	14.793984
20.397662	934.983248	14.799002
20.404975	943.733002	14.804019
20.377955	943.140797	14.809037
20.676620	943.252106	14.814055
20.043203	945.982638	14.819072
20.685164	942.995206	14.824090
20.788188	948.400754	14.829107
20.900574	940.213063	14.834125
20.650362	944.660614	14.839143
20.436731	945.833121	14.844160
20.668523	938.418931	14.849178
20.305662	940.974796	14.854195
20.547789	945.803275	14.859213
20.886508	942.108835	14.864231
20.730982	944.193772	14.869248
20.301478	941.114392	14.874266
20.784577	941.247477	14.879283
20.636855	945.035300	14.884301
20.712365	936.222203	14.889319
20.899928	940.327044	14.894336
20.781335	935.226920	14.899354
20.610532	938.585998	14.904371
20.540981	946.113826	14.909389
20.924345	936.053616	14.914407
20.545469	937.510622	14.919424
20.857180	930.339607	14.924442
20.663901	937.400712	14.929459
20.857272	935.871651	14.934477
21.127488	934.750339	14.939495
20.978213	944.849885	14.944512
21.261496	940.034320	14.949530
21.052835	937.251910	14.954547
21.252476	944.128767	14.959565
21.467447	944.925280	14.964583
21.126827	945.527435	14.969600
21.172037	941.105536	14.974618
20.948768	950.866319	14.979635
20.784321	939.376643	14.984653
21.235291	944.996253	14.989671
20.925702	941.670990	14.994688
21.163790	938.336194	14.999706
21.103407	937.143281	15.004723
20.908708	945.763546	15.009741
21.049407	935.021609	15.014759
20.710679	936.756380	15.019776
20.906886	950.500668	15.024794
21.082724	960.316079	15.029811
21.001430	967.176727	15.034829
21.241747	957.034637	15.039847
20.940540	965.797725	15.044864
21.267933	965.519560	15.049882
21.149167	965.254057	15.054899
21.171097	969.135389	15.059917
21.192341	967.121894	15.064935
21.330421	992.608332	15.069952
21.410006	998.516153	15.074970
21.575612	992.888933	15.079987
21.388899	996.007507	15.085005
21.726540	998.530053	15.090023
21.567078	995.875671	15.095040
21.467951	989.033682	15.100058
21.770804	999.365816	15.105075
21.577639	985.466431	15.110093
21.795531	994.741992	15.115111
21.693154	1000.596095	15.120128
21.986280	995.974639	15.125146
21.669483	990.605562	15.130163
21.496910	998.783758	15.135181
21.991445	1000.202611	15.140199
21.812300	998.229779	15.145216
21.376080	997.890628	15.150234
21.613311	993.492466	15.155251
21.932259	990.444868	15.160269
21.686738	986.361708	15.165287
21.880927	992.175945	15.170304
21.715732	984.744651	15.175322
21.779284	997.496634	15.180339
21.769415	992.950756	15.185357
22.472448	993.074845	15.190375
21.945440	996.274803	15.195392
22.166968	991.866464	15.200410
22.188287	989.916070	15.205427
21.723758	991.051905	15.210445
21.956682	987.787331	15.215463
21.758504	990.538466	15.220480
22.213778	987.984029	15.225498
22.108106	986.962263	15.230515
21.870535	997.968663	15.235533
22.268008	989.831235	15.240551
22.124042	988.244240	15.245568
22.053766	991.448824	15.250586
22.016317	1004.872933	15.255603
22.271415	1012.833073	15.260621
22.361907	1020.222408	15.265639
22.344923	1016.867351	15.270656
22.139384	1020.661036	15.275674
22.200263	1015.463519	15.280691
22.139156	1017.644215	15.285709
22.536154	1020.290065	15.290727
22.502858	1023.697177	15.295744
22.379118	1023.334619	15.300762
22.378381	1018.904076	15.305779
22.534763	1017.620604	15.310797
22.236331	1007.792737	15.315815
22.333688	1014.060708	15.320832
22.558856	1016.906877	15.325850
22.325381	1020.149498	15.330867
22.180853	1020.326655	15.335885
22.517748	1013.230580	15.340903
22.630831	1016.687482	15.345920
22.377679	1019.743822	15.350938
22.667135	1031.226756	15.355955
22.951585	1047.166409	15.360973
22.664996	1035.238102	15.365991
22.649848	1046.806341	15.371008
22.637549	1047.117543	15.376026
23.061833	1034.734579	15.381043
23.180766	1044.230698	15.386061
22.692557	1025.612022	15.391079
22.860162	1030.521553	15.396096
22.940416	1040.863123	15.401114
23.147169	1040.146156	15.406131
23.126414	1029.157905	15.411149
22.882286	1021.003594	15.416167
22.741983	1017.645647	15.421184
22.721446	1038.495798	15.426202
23.130468	1033.338744	15.431219
22.885677	1042.326611	15.436237
23.247670	1036.545726	15.441255
23.028027	1046.318620	15.446272
22.977022	1039.194567	15.451290
23.217635	1036.585185	15.456307
23.230665	1037.321626	15.461325
23.017392	1041.832877	15.466343
23.031999	1044.544578	15.471360
22.875934	1046.635923	15.476378
22.926187	1043.882610	15.481395
23.116486	1055.983749	15.486413
23.310954	1044.570664	15.491431
23.385753	1049.150672	15.496448
22.915757	1041.126192	15.501466
23.285073	1037.584756	15.506483
23.205713	1045.918872	15.511501
23.203999	1045.792931	15.516519
23.230931	1039.884335	15.521536
23.366051	1055.051995	15.526554
23.483694	1065.848499	15.531571
23.541282	1077.279203	15.536589
23.708631	1066.031271	15.541607
23.431453	1058.361765	15.546624
23.532165	1069.249269	15.551642
23.603526	1061.897875	15.556659
23.876818	1062.325557	15.561677
23.699329	1050.197219	15.566695
23.380465	1040.836412	15.571712
23.304175	1051.792488	15.576730
23.653369	1062.423553	15.581747
23.723076	1070.990089	15.586765
23.744356	1077.452961	15.591783
23.722274	1078.097042	15.596800
23.412255	1076.690526	15.601818
23.934045	1071.913530	15.606835
23.648575	1074.413184	15.611853
23.897601	1063.316638	15.616871
23.875052	1062.969881	15.621888
23.870094	1063.775396	15.626906
24.114439	1066.101042	15.631923
24.057978	1066.895641	15.636941
23.888262	1070.210394	15.641959
23.892302	1064.775562	15.646976
23.549826	1071.004737	15.651994
24.009880	1060.607473	15.657011
24.096160	1070.651481	15.662029
23.626267	1063.056158	15.667047
23.736268	1067.337204	15.672064
24.029660	1068.601189	15.677082
24.280764	1070.446108	15.682099
24.257080	1088.399815	15.687117
24.217520	1085.313345	15.692135
24.546152	1076.798436	15.697152
24.189899	1069.756611	15.702170
24.085667	1058.374245	15.707187
23.935892	1066.050313	15.712205
24.602999	1082.899240	15.717223
24.535185	1085.453369	15.722240
24.552734	1097.669794	15.727258
24.630183	1078.783113	15.732275
24.410414	1069.141777	15.737293
24.191497	1064.634740	15.742311
24.093338	1071.242437	15.747328
24.268536	1084.478865	15.752346
24.539690	1077.856898	15.757363
24.170488	1090.515381	15.762381
24.293586	1086.554684	15.767399
24.778247	1090.423957	15.772416
24.012243	1089.858442	15.777434
24.335191	1089.076045	15.782451
24.364195	1089.497581	15.787469
23.851661	1096.012014	15.792487
24.721289	1106.637815	15.797504
24.443289	1114.715715	15.802522
25.319097	1111.919063	15.807539
25.025676	1116.853061	15.812557
24.821409	1114.035225	15.817575
25.070890	1108.442247	15.822592
24.905675	1104.677912	15.827610
24.843794	1090.237303	15.832627
24.944471	1100.556793	15.837645
24.873274	1103.464898	15.842663
25.373745	1109.057920	15.847680
24.931261	1102.209386	15.852698
24.739941	1090.382973	15.857715
24.803669	1097.656587	15.862733
25.239485	1100.476285	15.867751
25.179963	1089.011200	15.872768
24.731931	1093.044624	15.877786
25.395490	1108.445630	15.882803
25.347123	1093.479056	15.887821
24.997847	1090.860524	15.892839
24.789812	1092.802177	15.897856
25.196959	1102.518537	15.902874
25.483098	1099.485496	15.907891
25.138177	1110.385604	15.912909
24.788334	1103.131331	15.917927
25.255573	1099.741893	15.922944
24.936534	1107.182402	15.927962
24.967948	1106.843023	15.932979
25.058727	1106.822600	15.937997
24.702129	1104.956279	15.943015
24.919016	1106.629806	15.948032
25.322435	1127.650735	15.953050
25.548053	1137.297549	15.958067
25.376255	1128.532329	15.963085
25.543416	1127.281885	15.968103
25.438118	1126.578786	15.973120
25.388635	1135.428995	15.978138
25.529435	1127.912130	15.983155
25.575598	1130.562128	15.988173
25.586725	1135.745357	15.993191
25.794289	1134.908340	15.998208
25.501899	1137.352277	16.003226
26.087626	1138.293043	16.008243
25.823955	1140.148690	16.013261
25.762445	1148.047733	16.018279
26.109937	1134.947671	16.023296
25.735295	1144.372369	16.028314
25.655636	1138.770668	16.033331
26.019768	1142.829130	16.038349
25.786427	1142.161744	16.043367
25.938870	1134.015064	16.048384
25.783054	1140.303563	16.053402
26.149648	1128.112551	16.058419
26.043072	1134.238748	16.063437
25.801246	1137.501625	16.068455
26.168930	1126.976695	16.073472
25.941701	1141.654895	16.078490
26.260750	1132.649151	16.083507
26.146058	1131.496238	16.088525
26.104691	1140.572401	16.093543
26.152192	1129.220015	16.098560
26.176730	1126.603236	16.103578
26.027446	1132.654032	16.108595
26.205313	1132.863045	16.113613
26.190263	1135.683518	16.118631
26.041391	1129.155330	16.123648
26.179563	1142.069366	16.128666
26.189552	1153.589579	16.133683
26.676275	1147.360053	16.138701
26.438941	1155.103439	16.143719
26.510066	1149.935846	16.148736
26.550195	1162.944055	16.153754
26.604790	1157.280420	16.158771
26.590084	1154.284742	16.163789
26.653054	1151.961775	16.168807
26.366945	1142.482206	16.173824
26.470546	1148.878639	16.178842
26.557166	1154.826441	16.183859
26.844160	1160.986043	16.188877
26.463114	1165.264672	16.193895
26.754913	1143.434920	16.198912
27.095854	1154.338721	16.203930
26.804673	1141.962937	16.208947
26.644857	1130.390366	16.213965
26.413770	1138.890158	16.218983
26.996933	1142.614720	16.224000
26.443950	1152.215510	16.229018
26.566642	1151.420109	16.234035
26.487833	1144.757931	16.239053
26.684873	1152.787133	16.244071
26.390805	1143.409788	16.249088
26.618164	1153.210972	16.254106
26.983382	1156.811681	16.259123
27.248484	1165.720222	16.264141
27.143569	1170.233568	16.269159
26.975531	1148.172449	16.274176
26.831405	1167.416767	16.279194
27.241779	1168.763530	16.284211
27.344661	1180.446022	16.289229
27.256569	1169.266198	16.294247
27.594998	1160.402589	16.299264
27.268433	1148.262681	16.304282
27.116582	1147.475312	16.309299
27.122570	1147.761578	16.314317
27.237788	1154.648505	16.319335
27.444893	1162.426838	16.324352
27.609231	1167.895489	16.329370
27.180110	1161.240511	16.334387
27.605396	1169.742265	16.339405
27.509691	1154.338045	16.344423
27.101236	1154.013501	16.349440
27.469550	1163.391961	16.354458
27.411237	1178.148033	16.359475
27.657361	1177.137754	16.364493
27.355125	1178.535509	16.369511
27.635829	1175.692648	16.374528
27.689738	1177.385245	16.379546
27.812802	1185.893035	16.384563
27.771386	1185.022198	16.389581
27.446658	1184.596256	16.394599
27.566078	1170.682772	16.399616
27.482715	1179.967464	16.404634
27.450643	1180.284903	16.409651
27.595618	1180.237108	16.414669
27.269879	1179.268529	16.419687
27.677988	1183.651511	16.424704
27.641462	1187.532524	16.429722
27.572184	1193.441496	16.434739
27.668187	1193.874694	16.439757
27.283517	1199.839085	16.444775
27.699245	1196.678554	16.449792
27.572782	1199.831963	16.454810
28.201777	1212.780083	16.459827
28.319992	1206.194504	16.464845
28.173748	1208.726148	16.469863
28.636734	1202.531857	16.474880
28.517904	1192.552848	16.479898
28.342977	1193.886602	16.484915
28.875107	1190.256671	16.489933
28.241468	1184.826413	16.494951
28.414398	1183.799128	16.499968
28.355477	1177.970124	16.504986
28.509930	1184.614271	16.510003
28.530703	1178.201662	16.515021
28.774186	1182.903763	16.520039
28.267558	1169.674728	16.525056
28.498444	1181.188969	16.530074
28.352778	1178.074822	16.535091
28.689027	1172.935371	16.540109
28.514516	1173.009901	16.545127
28.590909	1177.611784	16.550144
28.778888	1182.395110	16.555162
28.394223	1183.215567	16.560179
28.746975	1174.352877	16.565197
28.753537	1176.696624	16.570215
28.722639	1177.657660	16.575232
28.651713	1171.899955	16.580250
28.716495	1179.419590	16.585267
28.727694	1177.619072	16.590285
28.294465	1173.618743	16.595303
28.926976	1172.914376	16.600320
28.959300	1179.946763	16.605338
28.699484	1186.481842	16.610355
29.026213	1171.743978	16.615373
28.855926	1176.406358	16.620391
28.678529	1183.319921	16.625408
28.826647	1176.133254	16.630426
28.794694	1179.631704	16.635443
29.045956	1182.458058	16.640461
28.938029	1188.076403	16.645479
29.181552	1204.669506	16.650496
29.345354	1199.029879	16.655514
29.258255	1200.823327	16.660531
28.891220	1198.229634	16.665549
29.016345	1209.457404	16.670567
29.093738	1206.930214	16.675584
29.185755	1206.575085	16.680602
28.846089	1214.432259	16.685619
28.973361	1208.968729	16.690637
29.280460	1203.780159	16.695655
29.128059	1207.723399	16.700672
29.037290	1209.163970	16.705690
29.155985	1225.555623	16.710707
29.538215	1222.286694	16.715725
29.734241	1223.802535	16.720743
29.655927	1225.338998	16.725760
29.912374	1225.488441	16.730778
29.778210	1220.529514	16.735795
29.734790	1205.284366	16.740813
29.749678	1196.319634	16.745831
29.557161	1203.977169	16.750848
29.835924	1196.258915	16.755866
29.787574	1198.781628	16.760883
29.745263	1199.911698	16.765901
29.273459	1205.302681	16.770919
29.845491	1215.488891	16.775936
29.923698	1214.754061	16.780954
29.642487	1222.611605	16.785971
29.761137	1219.645646	16.790989
30.025789	1222.409962	16.796007
29.972757	1216.343344	16.801024
30.154616	1218.407342	16.806042
29.733431	1221.944311	16.811059
30.022274	1215.654053	16.816077
30.037383	1219.498632	16.821095
29.827475	1216.198822	16.826112
29.837491	1218.901797	16.831130
29.869948	1220.111746	16.836147
30.122191	1231.237688	16.841165
30.385252	1235.902041	16.846183
30.233539	1247.658929	16.851200
30.646247	1236.016085	16.856218
30.486549	1235.100545	16.861235
30.379446	1235.009947	16.866253
30.319197	1221.146487	16.871271
30.153092	1220.437072	16.876288
30.443435	1234.230039	16.881306
30.567147	1239.095969	16.886323
30.395797	1235.408301	16.891341
30.541879	1245.761832	16.896359
30.407212	1245.653434	16.901376
30.315699	1256.488931	16.906394
30.035643	1253.058024	16.911411
30.590938	1237.732255	16.916429
30.563542	1241.949529	16.921447
30.340330	1239.393397	16.926464
30.615899	1235.926479	16.931482
30.571767	1242.623657	16.936499
30.364259	1244.779837	16.941517
30.941630	1248.571595	16.946535
31.135620	1262.496349	16.951552
30.789077	1264.437495	16.956570
30.797874	1270.646761	16.961587
31.233159	1258.738455	16.966605
31.275494	1267.766938	16.971623
31.237634	1257.857337	16.976640
31.311219	1237.727705	16.981658
30.777137	1240.919339	16.986675
30.825324	1241.233750	16.991693
31.624305	1251.510878	16.996711
31.406076	1248.818270	17.001728
31.335884	1243.300268	17.006746
31.248509	1229.185406	17.011763
31.150081	1240.170291	17.016781
31.427759	1229.283775	17.021799
30.880750	1237.596117	17.026816
31.394468	1245.796962	17.031834
31.441491	1260.195875	17.036851
31.451667	1258.303991	17.041869
31.459977	1267.839543	17.046887
31.171681	1263.788225	17.051904
31.519661	1263.409022	17.056922
31.385326	1265.414958	17.061939
31.526434	1264.771318	17.066957
31.716968	1264.877375	17.071975
31.420501	1271.181507	17.076992
31.592015	1266.578916	17.082010
31.529336	1266.339390	17.087027
31.300246	1267.627933	17.092045
31.455612	1251.935230	17.097063
31.167828	1268.017824	17.102080
31.528813	1269.201873	17.107098
31.832094	1285.123029	17.112115
32.332270	1285.786790	17.117133
32.272748	1285.003974	17.122151
32.171471	1282.021753	17.127168
32.680505	1270.742585	17.132186
32.233953	1260.666240	17.137203
31.884650	1260.856347	17.142221
32.176288	1248.768442	17.147239
32.090330	1254.689499	17.152256
31.827884	1237.193628	17.157274
31.869140	1257.570512	17.162291
31.858392	1270.170156	17.167309
32.336816	1270.307129	17.172327
31.886637	1277.746037	17.177344
32.195363	1279.361100	17.182362
32.458316	1272.491029	17.187379
32.274840	1277.022946	17.192397
32.621856	1273.232472	17.197415
32.338942	1278.931738	17.202432
32.347926	1273.653863	17.207450
32.202304	1273.865907	17.212467
32.656232	1271.914399	17.217485
32.573932	1279.068812	17.222503
32.252885	1281.308947	17.227520
32.692029	1273.016579	17.232538
32.453433	1272.583536	17.237555
32.414787	1279.847918	17.242573
32.556497	1279.497674	17.247591
32.486418	1274.393054	17.252608
32.307024	1281.875010	17.257626
32.528971	1290.118147	17.262643
32.767237	1302.060506	17.267661
32.639057	1296.027653	17.272679
32.502552	1305.364865	17.277696
32.878016	1308.799908	17.282714
33.083755	1306.072840	17.287731
33.327681	1307.764266	17.292749
33.110881	1301.139293	17.297767
33.241497	1303.956049	17.302784
33.107011	1298.779399	17.307802
33.095261	1295.429787	17.312819
33.081039	1298.518401	17.317837
33.166832	1297.788699	17.322855
32.888003	1309.208813	17.327872
33.271911	1299.179873	17.332890
32.961692	1305.625013	17.337907
32.601844	1315.785956	17.342925
32.973782	1311.527691	17.347943
33.352079	1328.964617	17.352960
33.113546	1326.906321	17.357978
33.232143	1330.248816	17.362995
33.329952	1328.359060	17.368013
33.475879	1326.843664	17.373031
33.641597	1335.332262	17.378048
33.616442	1329.081385	17.383066
33.612228	1329.681668	17.388083
33.605673	1329.405000	17.393101
33.489087	1325.620424	17.398119
33.603878	1325.675158	17.403136
33.418365	1326.795974	17.408154
33.322938	1325.365494	17.413171
33.373944	1336.500742	17.418189
33.788880	1339.440494	17.423207
34.075910	1348.970564	17.428224
34.103211	1356.218397	17.433242
34.128454	1353.904434	17.438259
33.705262	1348.400334	17.443277
34.151906	1339.434580	17.448295
34.070610	1346.503657	17.453312
34.122864	1345.526710	17.458330
34.318170	1339.512904	17.463347
34.004745	1348.091887	17.468365
34.081677	1337.728867	17.473383
34.219182	1340.661321	17.478400
34.512556	1335.367552	17.483418
34.470878	1347.413488	17.488435
34.362668	1346.111229	17.493453
34.359432	1338.342145	17.498471
34.513457	1341.366701	17.503488
34.447642	1343.762766	17.508506
34.564652	1337.669632	17.513523
34.326828	1347.442365	17.518541
34.143873	1340.670096	17.523559
33.972146	1337.730393	17.528576
34.160424	1346.414300	17.533594
34.073231	1341.337572	17.538611
33.693569	1341.964753	17.543629
34.408234	1353.324888	17.548647
34.672302	1361.757160	17.553664
34.813459	1369.356503	17.558682
34.887256	1361.843660	17.563699
34.782130	1368.906988	17.568717
34.585204	1357.586201	17.573735
34.670401	1355.913000	17.578752
34.546424	1350.450676	17.583770
34.786817	1353.868888	17.588787
34.505859	1355.862948	17.593805
34.945789	1375.076515	17.598823
35.234318	1387.598088	17.603840
35.057060	1382.680539	17.608858
35.338694	1382.702985	17.613875
35.153513	1381.232825	17.618893
35.513247	1374.461257	17.623911
35.453558	1359.048096	17.628928
35.027007	1358.117293	17.633946
35.622917	1358.841892	17.638963
35.588709	1356.376238	17.643981
35.549647	1358.061236	17.648999
35.558999	1362.948161	17.654016
35.090927	1358.281026	17.659034
35.463457	1351.778874	17.664051
35.347970	1353.273798	17.669069
35.345733	1352.911251	17.674087
35.561267	1359.025244	17.679104
35.564209	1377.801920	17.684122
36.050410	1379.717566	17.689139
35.418752	1373.911398	17.694157
36.000991	1373.767120	17.699175
35.822572	1369.032793	17.704192
35.799514	1369.487688	17.709210
35.740085	1367.234243	17.714227
35.478935	1379.197606	17.719245
35.822298	1377.809257	17.724263
35.868083	1379.938641	17.729280
35.874383	1383.876146	17.734298
35.777782	1375.597716	17.739315
35.724524	1373.400114	17.744333
35.867926	1381.639743	17.749351
35.687106	1380.424526	17.754368
35.625958	1379.686140	17.759386
36.231325	1382.662523	17.764403
36.272361	1395.143739	17.769421
36.305788	1398.477417	17.774439
36.318321	1407.690493	17.779456
35.964348	1405.022152	17.784474
36.155716	1401.331624	17.789491
36.411430	1408.951018	17.794509
36.203847	1400.557311	17.799527
36.391976	1398.644017	17.804544
36.176314	1402.347840	17.809562
36.389397	1389.640905	17.814579
36.530830	1392.414965	17.819597
36.728844	1399.800340	17.824615
36.676295	1393.405382	17.829632
36.537052	1397.737937	17.834650
36.466071	1396.571889	17.839667
36.776653	1400.686086	17.844685
36.364612	1389.326186	17.849703
36.897018	1399.723800	17.854720
36.876981	1423.846912	17.859738
37.095905	1409.718932	17.864755
36.777003	1412.356382	17.869773
36.841368	1415.158224	17.874791
37.217146	1414.777846	17.879808
36.910481	1425.003155	17.884826
36.982561	1411.305138	17.889843
37.084215	1418.828600	17.894861
37.358991	1418.678544	17.899879
37.517328	1425.479968	17.904896
37.191089	1409.019504	17.909914
37.172599	1412.093023	17.914931
37.406613	1420.795092	17.919949
37.208080	1415.246525	17.924967
37.229255	1417.647990	17.929984
37.411545	1409.247228	17.935002
37.509376	1415.010334	17.940019
37.976463	1413.271358	17.945037
37.394211	1408.031847	17.950055
37.516432	1401.565493	17.955072
37.261588	1415.020602	17.960090
37.530427	1410.500653	17.965107
37.664833	1417.283708	17.970125
37.371858	1414.448077	17.975143
37.401936	1412.297456	17.980160
37.529449	1428.378651	17.985178
37.706188	1417.185842	17.990195
37.571905	1422.499093	17.995213
37.333159	1416.581243	18.000231
37.806226	1417.627930	18.005248
38.006341	1428.295049	18.010266
38.032542	1435.180165	18.015283
38.090165	1437.146766	18.020301
37.978575	1436.189011	18.025319
37.602194	1433.016066	18.030336
37.652440	1440.329789	18.035354
37.929282	1442.035039	18.040371
38.178668	1438.161901	18.045389
37.760778	1438.921270	18.050407
38.131673	1443.180721	18.055424
38.082181	1450.333251	18.060442
38.197479	1455.364654	18.065459
38.337927	1462.036332	18.070477
38.466213	1459.472779	18.075495
38.754660	1462.122974	18.080512
38.898246	1468.289232	18.085530
38.740566	1455.415913	18.090547
38.882713	1442.445428	18.095565
38.344463	1446.877988	18.100583
38.593292	1430.226983	18.105600
38.460439	1448.709294	18.110618
38.787298	1455.544452	18.115635
38.999718	1465.758393	18.120653
38.949427	1462.111791	18.125671
38.685676	1461.528023	18.130688
38.602182	1459.735909	18.135706
38.718214	1463.940371	18.140723
38.912404	1463.162227	18.145741
38.862754	1463.791680	18.150759
38.939516	1461.251928	18.155776
38.874933	1466.311341	18.160794
38.574163	1468.589367	18.165811
38.959612	1458.490670	18.170829
38.706598	1468.922247	18.175847
39.178930	1476.362774	18.180864
39.170915	1487.343203	18.185882
39.466078	1484.898833	18.190899
39.423041	1489.188029	18.195917
39.158756	1484.754221	18.200935
39.825041	1485.401596	18.205952
39.284266	1487.824291	18.210970
39.268197	1488.407490	18.215987
39.282518	1485.281003	18.221005
39.563680	1487.970207	18.226023
39.749838	1483.163307	18.231040
39.635790	1486.904975	18.236058
39.570632	1476.655516	18.241075
39.971573	1483.245619	18.246093
39.652815	1491.355281	18.251111
40.040694	1486.236104	18.256128
40.018575	1490.155966	18.261146
39.873615	1488.818392	18.266163
39.884895	1493.269547	18.271181
39.688060	1492.871022	18.276199
39.836734	1489.717305	18.281216
39.979539	1492.532193	18.286234
39.613763	1486.097606	18.291251
39.663435	1485.796402	18.296269
40.136102	1495.991932	18.301287
40.482339	1500.201588	18.306304
40.598594	1505.245479	18.311322
40.823507	1506.078340	18.316339
40.362440	1489.512561	18.321357
40.163727	1485.387283	18.326375
40.255473	1479.171801	18.331392
40.283742	1484.273568	18.336410
40.002600	1486.832565	18.341427
40.371640	1492.673393	18.346445
40.356941	1511.677022	18.351463
40.686879	1506.377510	18.356480
40.384469	1508.722069	18.361498
40.568271	1512.477330	18.366515
40.981474	1498.820810	18.371533
40.525683	1509.962488	18.376551
40.558646	1505.248863	18.381568
40.840594	1505.940299	18.386586
40.329840	1512.012787	18.391603
40.746536	1507.185767	18.396621
40.698647	1530.584360	18.401639
41.095536	1532.242525	18.406656
40.899485	1533.693203	18.411674
41.158052	1526.000042	18.416691
41.102467	1536.789089	18.421709
41.208408	1534.459382	18.426727
41.440097	1516.400302	18.431744
41.319381	1532.406629	18.436762
41.064778	1530.193018	18.441779
41.111908	1522.154078	18.446797
41.243566	1526.529694	18.451815
41.149943	1519.345812	18.456832
41.075804	1527.483677	18.461850
40.971664	1528.721227	18.466867
41.583321	1533.258799	18.471885
41.715106	1549.566660	18.476903
41.692566	1530.814990	18.481920
41.665758	1538.128128	18.486938
41.808203	1542.091808	18.491955
41.440942	1532.848730	18.496973
41.488414	1544.003594	18.501991
41.563197	1550.982178	18.507008
41.932370	1546.516002	18.512026
41.513202	1547.890964	18.517043
41.954989	1551.669183	18.522061
42.076550	1552.514982	18.527079
41.969668	1553.677219	18.532096
42.020059	1555.575530	18.537114
42.052528	1555.056094	18.542131
41.572492	1549.917393	18.547149
41.822629	1558.232005	18.552167
42.025047	1574.989646	18.557184
42.202625	1571.102412	18.562202
42.814210	1555.486736	18.567219
42.959681	1556.606528	18.572237
42.776241	1545.655911	18.577255
42.696946	1535.676866	18.582272
42.683195	1531.197729	18.587290
42.651645	1535.381004	18.592307
42.904726	1526.053969	18.597325
42.829625	1536.117054	18.602343
42.584705	1531.418284	18.607360
42.772555	1526.440694	18.612378
42.762465	1527.250184	18.617395
42.846820	1524.917527	18.622413
42.799591	1527.755696	18.627431
42.831209	1528.511355	18.632448
43.166131	1533.344482	18.637466
42.984602	1533.319119	18.642483
43.095603	1529.208727	18.647501
42.867353	1529.859677	18.652519
43.145553	1525.442384	18.657536
42.998661	1523.047900	18.662554
42.810838	1533.901716	18.667571
43.411712	1533.085497	18.672589
43.230707	1532.226909	18.677607
43.056630	1529.268604	18.682624
43.266075	1530.264823	18.687642
42.948071	1538.992936	18.692659
43.074888	1528.473713	18.697677
43.003708	1540.098333	18.702695
43.239565	1555.815632	18.707712
43.365153	1561.861647	18.712730
43.229367	1563.545945	18.717747
43.238654	1555.099465	18.722765
43.085413	1559.629901	18.727783
43.358721	1561.578713	18.732800
43.665201	1571.569784	18.737818
43.436216	1585.017840	18.742835
43.675886	1585.842095	18.747853
43.663300	1582.236935	18.752871
43.844668	1589.583955	18.757888
43.996922	1583.340081	18.762906
43.874173	1582.033756	18.767923
43.614315	1587.117294	18.772941
43.907916	1589.949746	18.777959
43.710268	1597.365246	18.782976
44.138526	1591.447633	18.787994
44.103904	1616.737787	18.793011
44.282535	1598.352363	18.798029
44.079642	1602.578111	18.803047
44.377153	1603.576402	18.808064
44.393074	1600.244516	18.813082
44.109690	1609.412248	18.818099
44.456500	1588.763146	18.823117
44.258796	1598.428781	18.828135
44.481270	1603.509812	18.833152
44.776388	1594.760031	18.838170
44.502980	1605.564098	18.843187
44.692066	1594.271424	18.848205
44.643789	1595.143668	18.853223
44.786211	1604.074686	18.858240
44.979722	1613.430106	18.863258
45.029164	1619.364918	18.868275
44.735010	1618.864775	18.873293
44.679309	1621.761083	18.878311
44.793531	1625.959554	18.883328
45.193914	1620.005245	18.888346
44.942318	1613.477093	18.893363
45.346809	1617.690330	18.898381
44.840836	1628.284463	18.903399
44.976350	1620.679850	18.908416
45.342864	1621.758919	18.913434
45.309153	1618.081300	18.918451
45.118420	1620.001380	18.923469
45.345436	1620.701373	18.928487
45.305092	1614.900893	18.933504
45.227968	1614.256504	18.938522
45.323626	1626.940821	18.943539
45.528102	1634.460990	18.948557
45.879334	1651.141883	18.953575
45.513058	1654.020279	18.958592
45.521301	1648.515186	18.963610
45.316753	1646.858667	18.968627
45.688588	1648.839487	18.973645
45.504743	1653.870183	18.978663
45.597473	1647.828062	18.983680
45.960167	1637.313077	18.988698
45.845877	1639.180231	18.993715
45.706243	1636.585782	18.998733
45.694772	1647.850875	19.003751
45.817553	1659.514803	19.008768
46.272783	1661.009260	19.013786
46.031112	1665.193722	19.018803
46.246542	1667.694367	19.023821
46.019419	1665.227147	19.028839
46.036680	1671.397364	19.033856
46.517977	1672.486968	19.038874
46.300284	1671.466824	19.043891
46.653407	1659.148158	19.048909
46.630910	1662.326487	19.053927
46.502378	1657.833630	19.058944
47.061385	1657.838138	19.063962
47.176685	1662.020671	19.068979
47.195373	1661.276155	19.073997
47.024035	1662.451591	19.079015
46.755907	1658.415977	19.084032
46.984473	1654.094745	19.089050
47.030371	1661.989916	19.094067
47.132450	1663.542512	19.099085
47.195239	1660.954414	19.104103
46.797577	1664.396287	19.109120
46.839232	1664.317239	19.114138
46.661571	1661.037572	19.119155
46.503850	1659.989156	19.124173
47.267176	1667.321340	19.129191
47.085782	1677.066532	19.134208
47.248736	1681.490963	19.139226
47.167233	1693.022614	19.144243
47.162310	1682.429136	19.149261
47.158298	1685.617215	19.154279
47.099388	1695.355969	19.159296
47.286931	1688.222920	19.164314
47.420087	1684.696036	19.169331
47.400605	1702.577121	19.174349
47.794106	1711.039902	19.179367
47.662525	1706.661118	19.184384
47.995104	1708.499730	19.189402
47.786919	1713.897159	19.194419
47.670281	1714.473932	19.199437
47.916839	1704.526112	19.204455
47.939330	1712.207194	19.209472
47.977017	1697.832643	19.214490
47.657616	1702.502597	19.219507
47.783667	1709.337559	19.224525
47.978130	1705.466603	19.229543
47.749592	1715.657822	19.234560
48.427154	1724.805390	19.239578
48.012296	1729.502836	19.244595
48.054897	1728.173913	19.249613
48.630679	1724.988370	19.254631
48.182401	1726.626660	19.259648
48.319223	1727.952942	19.264666
48.383771	1727.403259	19.269683
48.410251	1731.811081	19.274701
48.733641	1721.037072	19.279719
48.655235	1728.298359	19.284736
48.798696	1727.676428	19.289754
48.669607	1722.587180	19.294771
48.653328	1714.182475	19.299789
48.643682	1716.027033	19.304807
48.926979	1733.283483	19.309824
48.936056	1732.310081	19.314842
49.084368	1734.171074	19.319859
49.062946	1749.732936	19.324877
49.217102	1752.517695	19.329895
49.261659	1753.476481	19.334912
49.248541	1749.009813	19.339930
49.373676	1751.694947	19.344947
49.464455	1749.560081	19.349965
49.722794	1740.636069	19.354983
49.475794	1739.866643	19.360000
49.294868	1725.586068	19.365018
49.933800	1723.507876	19.370035
49.556307	1736.619396	19.375053
49.635831	1725.144877	19.380071
49.305138	1726.098969	19.385088
49.443809	1737.624772	19.390106
49.535114	1744.484092	19.395123
49.441358	1748.670791	19.400141
49.858149	1745.191255	19.405159
49.642942	1757.573762	19.410176
49.709769	1743.276690	19.415194
50.180202	1740.461006	19.420211
49.659097	1741.321666	19.425229
50.046086	1755.336680	19.430247
49.941006	1754.810251	19.435264
50.230919	1756.273650	19.440282
50.295777	1755.105364	19.445299
50.293049	1768.549889	19.450317
50.266488	1766.603709	19.455335
50.219216	1772.944959	19.460352
50.618719	1766.422679	19.465370
50.529074	1767.089927	19.470387
50.065035	1767.749194	19.475405
50.289319	1761.740202	19.480423
49.971688	1763.503325	19.485440
50.550520	1769.620858	19.490458
50.789041	1790.289538	19.495475
50.887146	1791.031700	19.500493
51.055041	1781.304374	19.505511
51.167322	1791.956983	19.510528
50.963602	1785.639070	19.515546
50.906196	1784.032215	19.520563
50.733738	1786.372356	19.525581
50.960834	1783.076986	19.530599
51.420655	1790.162978	19.535616
50.861851	1787.109892	19.540634
50.801859	1785.759066	19.545651
50.591401	1788.000980	19.550669
51.499634	1797.548185	19.555687
50.908097	1809.512780	19.560704
51.505023	1807.235986	19.565722
51.976378	1809.639999	19.570739
51.499996	1817.663893	19.575757
51.772334	1811.316034	19.580775
51.878664	1814.420683	19.585792
51.614346	1810.018358	19.590810
52.073586	1818.268977	19.595827
51.419431	1823.789523	19.600845
51.483740	1810.041917	19.605863
51.607977	1813.241610	19.610880
51.934888	1804.843392	19.615898
52.033092	1807.097213	19.620915
51.576464	1810.242173	19.625933
52.042160	1808.146760	19.630951
51.764592	1820.838830	19.635968
51.809782	1817.751662	19.640986
51.908648	1822.744700	19.646003
51.864096	1836.899553	19.651021
52.284699	1831.576362	19.656039
51.757503	1831.781546	19.661056
51.687200	1830.744757	19.666074
52.101361	1842.581195	19.671091
52.352832	1851.889846	19.676109
52.619208	1846.565416	19.681127
52.593700	1848.283065	19.686144
52.478051	1854.357270	19.691162
52.902224	1844.249171	19.696179
52.632782	1851.802191	19.701197
52.813287	1839.301988	19.706215
52.844982	1840.976015	19.711232
53.058218	1848.520157	19.716250
53.355549	1857.815360	19.721267
53.116877	1859.405247	19.726285
53.607495	1847.446909	19.731303
53.225975	1840.594909	19.736320
53.183102	1838.777497	19.741338
53.391149	1831.262490	19.746355
53.360242	1838.648974	19.751373
53.611940	1842.804001	19.756391
53.528419	1845.114523	19.761408
53.709547	1850.609174	19.766426
53.959940	1843.908103	19.771443
53.218709	1842.726456	19.776461
53.624394	1846.939563	19.781479
54.035534	1852.641407	19.786496
54.175372	1851.792811	19.791514
54.040038	1838.448662	19.796531
53.578935	1832.363316	19.801549
53.835155	1851.631248	19.806567
54.458361	1856.025091	19.811584
54.335981	1854.396786	19.816602
54.321431	1838.045193	19.821619
53.941582	1840.032611	19.826637
54.102859	1844.829740	19.831655
54.293059	1848.000234	19.836672
54.226595	1851.254873	19.841690
54.921477	1850.177844	19.846707
54.646831	1861.720740	19.851725
54.659352	1854.072059	19.856743
54.766022	1841.750612	19.861760
54.164925	1829.208000	19.866778
54.557208	1839.706586	19.871795
54.323138	1845.770824	19.876813
54.520547	1845.424521	19.881831
54.679706	1850.824759	19.886848
54.438184	1850.202802	19.891866
54.827207	1847.128369	19.896883
54.994065	1856.582745	19.901901
54.948743	1846.838085	19.906919
54.960616	1858.443670	19.911936
54.904886	1868.017916	19.916954
54.845725	1877.400192	19.921971
55.351754	1878.877291	19.926989
55.650265	1867.864063	19.932007
55.459006	1877.869683	19.937024
55.143326	1882.980932	19.942042
55.489551	1876.580519	19.947059
55.248175	1877.586986	19.952077
55.420986	1878.342768	19.957095
55.469265	1878.912805	19.962112
55.196419	1875.524838	19.967130
55.241805	1871.194203	19.972147
55.177445	1889.691553	19.977165
55.481462	1888.400814	19.982183
56.044474	1898.188021	19.987200
55.553838	1905.841776	19.992218
56.103062	1898.529251	19.997235
55.896955	1904.882654	20.002253
55.718200	1898.431422	20.007271
56.257088	1902.387109	20.012288
55.557086	1909.363383	20.017306
56.048160	1910.827034	20.022323
56.197973	1928.508412	20.027341
56.367538	1917.161768	20.032359
56.998523	1912.427512	20.037376
56.811049	1918.708589	20.042394
57.009589	1918.030738	20.047411
56.864930	1913.713902	20.052429
56.700781	1909.687289	20.057447
56.772121	1893.849309	20.062464
56.928691	1910.630184	20.067482
56.903499	1905.300637	20.072499
56.817891	1910.287706	20.077517
56.887536	1916.011181	20.082535
57.226238	1910.766992	20.087552
57.006663	1907.714719	20.092570
57.319579	1906.160652	20.097587
57.151679	1905.356811	20.102605
56.958380	1905.118677	20.107623
56.987043	1911.574390	20.112640
57.058893	1911.392807	20.117658
57.084950	1903.180245	20.122675
57.165218	1909.460659	20.127693
57.252598	1920.757873	20.132711
57.275938	1922.041875	20.137728
57.315424	1927.372403	20.142746
57.284523	1916.359938	20.147763
57.249065	1925.577597	20.152781
57.182331	1929.583399	20.157799
57.563621	1948.399603	20.162816
57.533425	1958.209772	20.167834
57.701759	1958.303511	20.172851
58.049527	1951.391573	20.177869
57.769088	1962.326342	20.182887
57.958779	1952.627088	20.187904
58.156985	1973.355908	20.192922
58.239765	1971.408461	20.197939
58.175083	1973.233211	20.202957
58.227588	1986.088610	20.207975
58.248685	1979.031854	20.212992
58.391009	1980.912741	20.218010
58.300185	1977.089299	20.223027
58.032913	1982.426578	20.228045
58.284851	1985.259268	20.233063
58.584447	1996.024851	20.238080
58.785678	2002.153916	20.243098
58.851124	1998.107316	20.248115
58.807555	1997.252554	20.253133
58.855003	2007.183210	20.258151
59.153652	1997.826744	20.263168
59.117696	2004.620769	20.268186
59.327292	1999.150493	20.273203
59.087716	1996.975510	20.278221
58.628325	1992.357349	20.283239
59.296220	1995.693346	20.288256
59.205195	2002.745261	20.293274
59.099600	1985.284197	20.298291
59.801691	1999.752137	20.303309
59.607335	1999.697210	20.308327
59.431268	1991.282539	20.313344
59.035561	2001.238005	20.318362
59.315714	2013.057551	20.323379
59.401462	2012.870647	20.328397
59.452983	2012.089445	20.333415
59.490760	2025.329033	20.338432
59.707010	2025.364817	20.343450
59.708875	2029.410457	20.348467
60.289806	2037.588581	20.353485
60.159788	2041.181366	20.358503
60.497803	2037.322703	20.363520
60.568487	2042.039313	20.368538
60.739767	2028.552606	20.373555
60.691377	2023.015188	20.378573
60.154846	2004.434569	20.383591
60.721694	2007.432836	20.388608
60.201676	2018.032540	20.393626
60.471097	2024.810586	20.398643
60.602341	2026.409169	20.403661
60.423056	2031.268840	20.408679
60.788307	2040.919652	20.413696
60.856009	2039.201772	20.418714
60.642615	2032.544437	20.423731
60.299527	2036.018910	20.428749
60.694534	2042.805813	20.433767
61.265462	2045.342685	20.438784
61.025023	2058.998015	20.443802
60.894331	2062.868632	20.448819
61.223063	2064.326012	20.453837
61.123313	2061.892556	20.458855
60.904693	2049.438568	20.463872
60.902045	2056.309480	20.468890
61.021267	2069.126148	20.473907
61.498198	2077.954827	20.478925
61.505753	2083.018962	20.483943
61.930626	2084.164717	20.488960
62.060257	2080.865532	20.493978
62.336074	2066.308436	20.498995
61.558083	2070.387137	20.504013
61.309249	2078.385187	20.509031
61.858700	2073.430045	20.514048
61.607164	2074.220345	20.519066
61.819340	2094.379060	20.524083
62.282939	2090.967913	20.529101
62.369493	2096.654097	20.534119
62.742715	2082.886589	20.539136
62.659554	2090.028837	20.544154
62.857894	2092.756275	20.549171
62.801266	2082.530387	20.554189
62.449487	2076.017664	20.559207
62.965320	2061.132856	20.564224
63.218874	2066.733067	20.569242
62.760162	2057.103150	20.574259
62.825972	2054.681789	20.579277
62.699958	2069.073581	20.584295
63.036916	2063.706538	20.589312
63.143455	2073.031558	20.594330
62.753067	2067.203376	20.599347
63.287440	2072.532639	20.604365
63.361924	2085.684502	20.609383
63.326691	2090.174607	20.614400
63.581498	2087.711193	20.619418
63.189008	2093.781243	20.624435
63.310733	2092.187497	20.629453
63.095102	2095.982979	20.634471
63.455437	2096.236183	20.639488
63.243193	2097.960838	20.644506
63.472798	2095.876903	20.649523
63.673230	2086.513591	20.654541
63.216117	2091.640607	20.659559
63.420714	2094.253457	20.664576
63.477166	2106.701212	20.669594
63.589713	2118.546922	20.674611
63.999537	2113.884920	20.679629
64.003924	2114.382900	20.684647
64.049555	2111.917334	20.689664
64.155451	2116.757875	20.694682
63.955533	2118.199733	20.699699
64.374997	2116.704803	20.704717
64.146512	2132.952518	20.709735
64.359217	2131.107908	20.714752
64.315906	2124.177893	20.719770
64.358236	2127.030617	20.724787
64.590523	2124.504429	20.729805
64.932838	2132.369437	20.734823
64.823246	2119.901581	20.739840
64.636069	2122.367140	20.744858
64.665054	2129.892749	20.749875
64.945763	2132.919808	20.754893
65.284460	2149.521065	20.759911
65.232457	2145.650516	20.764928
65.372077	2154.657989	20.769946
65.364372	2154.116387	20.774963
65.421084	2143.169040	20.779981
65.094954	2150.977176	20.784999
65.282707	2145.595468	20.790016
65.376734	2146.385619	20.795034
65.244209	2153.702844	20.800051
65.561244	2142.440399	20.805069
65.394585	2160.092381	20.810087
65.539063	2168.363766	20.815104
65.375381	2167.019587	20.820122
65.406397	2177.110694	20.825139
65.878668	2163.428693	20.830157
65.732002	2171.448749	20.835175
65.995556	2170.738675	20.840192
66.263297	2181.749183	20.845210
66.221823	2196.367768	20.850227
66.300029	2191.817340	20.855245
66.339852	2189.210649	20.860263
66.359382	2189.993466	20.865280
66.328585	2190.954540	20.870298
66.649466	2183.333452	20.875315
67.050423	2176.536228	20.880333
66.553920	2176.414728	20.885351
66.822076	2174.409994	20.890368
67.004381	2171.377160	20.895386
66.664658	2174.513448	20.900403
66.933567	2168.652015	20.905421
67.221711	2169.642330	20.910439
67.310075	2164.872566	20.915456
67.351160	2167.223693	20.920474
67.314237	2163.335012	20.925491
67.398804	2169.365528	20.930509
67.247693	2165.750258	20.935527
67.161659	2179.488942	20.940544
67.481578	2182.775006	20.945562
67.479639	2197.422152	20.950579
67.337310	2206.814393	20.955597
67.413327	2200.869367	20.960615
67.254914	2202.667705	20.965632
67.502448	2193.382215	20.970650
67.188574	2205.316466	20.975667
67.779768	2215.033186	20.980685
67.716010	2219.493049	20.985703
67.670675	2223.022190	20.990720
67.947006	2223.484145	20.995738
68.004957	2228.875007	21.000755
68.131078	2217.213028	21.005773
68.452696	2239.977477	21.010791
68.242918	2242.102569	21.015808
68.217448	2247.588481	21.020826
68.297356	2245.193304	21.025843
68.654374	2240.129214	21.030861
68.743393	2243.669001	21.035879
68.473910	2235.653787	21.040896
68.714497	2242.190239	21.045914
68.535390	2246.466086	21.050931
68.747759	2247.228349	21.055949
68.984153	2254.027404	21.060967
68.952160	2269.136904	21.065984
69.564432	2264.288700	21.071002
69.228460	2271.669208	21.076019
69.499521	2264.077934	21.081037
69.390489	2274.212992	21.086055
69.559235	2269.443309	21.091072
69.936802	2258.344946	21.096090
69.436955	2266.177022	21.101107
69.425549	2264.058006	21.106125
69.389288	2265.471239	21.111143
69.540251	2264.197992	21.116160
69.377381	2269.563283	21.121178
69.206440	2282.302197	21.126195
70.116169	2287.326919	21.131213
70.287191	2286.984717	21.136231
69.642412	2297.357843	21.141248
70.032413	2290.467603	21.146266
70.010137	2307.734313	21.151283
69.727564	2308.365343	21.156301
69.995190	2321.755567	21.161319
70.201427	2322.386237	21.166336
70.777302	2312.948573	21.171354
70.356133	2322.901870	21.176371
70.348286	2311.311183	21.181389
70.613607	2326.961454	21.186407
70.792272	2330.787120	21.191424
71.157787	2329.048093	21.196442
71.464084	2329.874636	21.201459
71.532832	2328.850883	21.206477
71.837109	2319.824752	21.211495
71.980661	2314.566647	21.216512
71.715624	2299.572832	21.221530
71.674560	2295.198746	21.226547
71.923796	2295.775381	21.231565
71.699202	2286.052081	21.236583
71.378184	2288.317582	21.241600
71.647296	2285.056607	21.246618
71.988821	2281.702303	21.251635
72.013423	2282.175048	21.256653
72.035775	2282.446161	21.261671
71.994142	2285.835875	21.266688
72.220994	2288.852411	21.271706
71.884977	2289.902039	21.276723
71.683066	2283.555264	21.281741
71.956070	2282.130463	21.286759
71.895655	2288.881063	21.291776
72.507239	2299.749743	21.296794
72.478752	2311.267226	21.301811
72.236646	2312.835595	21.306829
72.346583	2316.018670	21.311847
72.014448	2307.593432	21.316864
72.357947	2308.414181	21.321882
72.793120	2316.372117	21.326899
72.652593	2313.600973	21.331917
72.767948	2332.455830	21.336935
72.595659	2337.412330	21.341952
72.628055	2336.621468	21.346970
72.863601	2337.856681	21.351987
73.119627	2337.684291	21.357005
73.150613	2343.562253	21.362023
72.862985	2343.818509	21.367040
73.047978	2359.579151	21.372058
73.014299	2360.742667	21.377075
73.282980	2372.030873	21.382093
73.450536	2362.379029	21.387111
73.257649	2366.628646	21.392128
73.424105	2366.230345	21.397146
73.533694	2382.081647	21.402163
73.692071	2382.236903	21.407181
74.048906	2376.702561	21.412199
74.040085	2384.376183	21.417216
74.100419	2382.867714	21.422234
73.950157	2384.813133	21.427251
74.128809	2390.595532	21.432269
74.693597	2395.446758	21.437287
74.474223	2404.993117	21.442304
74.592043	2411.223678	21.447322
74.821844	2407.921461	21.452339
74.882347	2412.273657	21.457357
75.273732	2401.352947	21.462375
74.841285	2393.650230	21.467392
74.847967	2396.827302	21.472410
75.196616	2396.766731	21.477427
74.961193	2407.625330	21.482445
75.042506	2402.853445	21.487463
75.100426	2400.398550	21.492480
75.170753	2396.647765	21.497498
75.131453	2411.834267	21.502515
75.238357	2412.534058	21.507533
75.100726	2405.890035	21.512551
75.127949	2406.255071	21.517568
75.409067	2423.888093	21.522586
75.462958	2427.995154	21.527603
75.493233	2426.743841	21.532621
75.604794	2417.062814	21.537639
75.691535	2424.737354	21.542656
75.760542	2436.668955	21.547674
75.829104	2440.508630	21.552691
75.890410	2440.477016	21.557709
76.306485	2439.613789	21.562727
76.001276	2445.092819	21.567744
75.906792	2441.730625	21.572762
76.009190	2448.664233	21.577779
76.418637	2465.119060	21.582797
76.724700	2464.721113	21.587815
76.223952	2471.969557	21.592832
76.569157	2463.621836	21.597850
76.722585	2464.273358	21.602867
76.604878	2471.228619	21.607885
76.977508	2472.382535	21.612903
77.091062	2486.721582	21.617920
77.301955	2487.461994	21.622938
77.218103	2488.491309	21.627955
77.500364	2491.871661	21.632973
77.353992	2484.963865	21.637991
77.271675	2499.383915	21.643008
77.276042	2492.440022	21.648026
77.324909	2487.142956	21.653043
77.468954	2482.831528	21.658061
77.317757	2490.704100	21.663079
77.610551	2508.079748	21.668096
77.753573	2501.325718	21.673114
77.539568	2514.664833	21.678131
77.948335	2501.058740	21.683149
78.413245	2503.656370	21.688167
78.093286	2507.414529	21.693184
78.256158	2512.483007	21.698202
78.251926	2515.254674	21.703219
78.281968	2511.263967	21.708237
78.682643	2527.313091	21.713255
78.313207	2535.743560	21.718272
78.828189	2526.495159	21.723290
78.919210	2530.530186	21.728307
78.689808	2535.751271	21.733325
79.120816	2533.039441	21.738343
78.931157	2532.317859	21.743360
78.721779	2525.710211	21.748378
78.759222	2540.695512	21.753395
78.783345	2539.135859	21.758413
79.484964	2536.309308	21.763431
79.946828	2543.508901	21.768448
79.921768	2549.455621	21.773466
79.807043	2534.621255	21.778483
80.150267	2524.904101	21.783501
80.359953	2513.954803	21.788519
79.897435	2521.689653	21.793536
80.076448	2521.630245	21.798554
80.225794	2514.843664	21.803571
79.911522	2525.395853	21.808589
80.342771	2515.579786	21.813607
80.275697	2514.905396	21.818624
80.062939	2514.840707	21.823642
80.174008	2514.911806	21.828659
80.263655	2528.752802	21.833677
80.539644	2530.363611	21.838695
80.370300	2539.889629	21.843712
80.385268	2546.379264	21.848730
80.731930	2545.823506	21.853747
80.666399	2541.847672	21.858765
80.632385	2535.127504	21.863783
80.871866	2553.742347	21.868800
80.930890	2567.897432	21.873818
80.929875	2568.083819	21.878835
81.088639	2572.606961	21.883853
81.206971	2563.499198	21.888871
80.898109	2570.496883	21.893888
81.013422	2576.832041	21.898906
81.059096	2583.695632	21.903923
81.198636	2598.232708	21.908941
81.635867	2593.563160	21.913959
81.601127	2594.496466	21.918976
81.608342	2597.462037	21.923994
81.682446	2607.754976	21.929011
81.773333	2615.697216	21.934029
81.911496	2623.370149	21.939047
82.226669	2617.810659	21.944064
82.438672	2622.328681	21.949082
82.218749	2614.782142	21.954099
82.131229	2630.197258	21.959117
82.471789	2630.949048	21.964135
82.419475	2642.868114	21.969152
82.408837	2643.273767	21.974170
82.481643	2640.128505	21.979187
82.756707	2634.616283	21.984205
83.120202	2635.250885	21.989223
83.136137	2636.384602	21.994240
83.023404	2638.728178	21.999258
83.309901	2629.379589	22.004275
83.169596	2625.721514	22.009293
83.491564	2632.873491	22.014311
83.283607	2639.448364	22.019328
83.511329	2647.593393	22.024346
83.423023	2648.759120	22.029363
83.524748	2660.679464	22.034381
83.743624	2651.669619	22.039399
83.961679	2649.858840	22.044416
84.118711	2652.722194	22.049434
84.168085	2653.254213	22.054451
84.064250	2660.677638	22.059469
84.151356	2654.803325	22.064487
84.421065	2656.370938	22.069504
84.134105	2655.471982	22.074522
84.451725	2650.584338	22.079539
84.414488	2652.019846	22.084557
84.341262	2650.604738	22.089575
84.578090	2660.209604	22.094592
84.493984	2678.628785	22.099610
84.571457	2674.488635	22.104627
84.732513	2677.215657	22.109645
84.876650	2680.854254	22.114663
85.178984	2677.679562	22.119680
85.147807	2678.539728	22.124698
85.519214	2686.021726	22.129715
85.318838	2697.954413	22.134733
85.417236	2698.788094	22.139751
85.595980	2694.575363	22.144768
85.203324	2708.797727	22.149786
85.410554	2705.123400	22.154803
85.665360	2693.526289	22.159821
85.866502	2697.326442	22.164839
85.987740	2702.508762	22.169856
85.669530	2720.702483	22.174874
86.217925	2714.364979	22.179891
86.140175	2722.210436	22.184909
86.018692	2714.897857	22.189927
86.182482	2716.860693	22.194944
86.065498	2720.006581	22.199962
86.384350	2722.497585	22.204979
86.298988	2734.876330	22.209997
86.672710	2742.436893	22.215015
86.546961	2743.441184	22.220032
86.506137	2748.415202	22.225050
86.627450	2741.689710	22.230067
86.733753	2753.438975	22.235085
86.892493	2762.083986	22.240103
87.029010	2759.585245	22.245120
86.852847	2764.567714	22.250138
87.358196	2765.650489	22.255155
86.911821	2773.348216	22.260173
87.482728	2788.058147	22.265191
87.665205	2786.218177	22.270208
87.457489	2799.357691	22.275226
88.119972	2782.290705	22.280243
88.217272	2788.742360	22.285261
87.807773	2789.390011	22.290279
87.997053	2789.123860	22.295296
87.990459	2805.170364	22.300314
88.468407	2806.970680	22.305331
88.319090	2813.205099	22.310349
88.647935	2807.261538	22.315367
88.141424	2815.069640	22.320384
88.322550	2815.931475	22.325402
88.379168	2800.053958	22.330419
88.218137	2811.971126	22.335437
88.377237	2830.800760	22.340455
88.526126	2824.086725	22.345472
88.386931	2842.574616	22.350490
88.552875	2853.061698	22.355507
89.215618	2870.118146	22.360525
89.061721	2863.703723	22.365543
89.213338	2861.155276	22.370560
89.169739	2865.050378	22.375578
89.446513	2860.412056	22.380595
89.517709	2872.252079	22.385613
89.590812	2901.443973	22.390631
89.834909	2895.027540	22.395648
89.548312	2888.255039	22.400666
90.314899	2881.287007	22.405683
90.021104	2872.445241	22.410701
90.224757	2875.295060	22.415719
90.163564	2882.519417	22.420736
90.561221	2882.208197	22.425754
90.860476	2890.768271	22.430771
90.739234	2881.470408	22.435789
90.442844	2886.156021	22.440807
90.967522	2887.084302	22.445824
91.257652	2888.238466	22.450842
91.179241	2887.565827	22.455859
91.126759	2892.121940	22.460877
90.908734	2903.423137	22.465895
91.442239	2883.065401	22.470912
91.108070	2895.744949	22.475930
91.443888	2882.064711	22.480947
91.716391	2891.749361	22.485965
91.574311	2894.836064	22.490983
91.561641	2885.619134	22.496000
91.743211	2896.075404	22.501018
91.861781	2888.643321	22.506035
91.680594	2891.262699	22.511053
91.669798	2918.921202	22.516071
92.126753	2909.915190	22.521088
91.800512	2913.791187	22.526106
92.014178	2905.810912	22.531123
92.153293	2920.360940	22.536141
91.982664	2937.783909	22.541159
93.037134	2926.573434	22.546176
92.494733	2925.960408	22.551194
92.860105	2935.065682	22.556211
93.165205	2931.944168	22.561229
92.921306	2934.907863	22.566247
92.989964	2931.728479	22.571264
92.863104	2928.532194	22.576282
92.962503	2944.047878	22.581299
93.360281	2948.208825	22.586317
93.069550	2961.452909	22.591335
93.333915	2955.345753	22.596352
93.239338	2956.215803	22.601370
93.098758	2966.135236	22.606387
93.618372	2985.546435	22.611405
93.111993	2986.647874	22.616423
93.809423	2978.835268	22.621440
93.891452	2997.235222	22.626458
94.167393	3001.118477	22.631475
94.054093	2998.384017	22.636493
94.252370	3008.998713	22.641511
94.449641	3003.668920	22.646528
94.471719	3008.339698	22.651546
94.039316	3012.648850	22.656563
94.307010	3020.626864	22.661581
94.464252	3030.569398	22.666599
94.772806	3027.598824	22.671616
94.815429	3022.397255	22.676634
94.917554	3025.834161	22.681651
95.292236	3035.787030	22.686669
95.308545	3049.431542	22.691687
95.313252	3048.007425	22.696704
95.525960	3054.993528	22.701722
95.448689	3056.100753	22.706739
95.769869	3060.166344	22.711757
95.402768	3060.441294	22.716775
96.126617	3060.527454	22.721792
95.538881	3050.503637	22.726810
95.815778	3059.537533	22.731827
96.205651	3057.497972	22.736845
96.241335	3073.443450	22.741863
96.525834	3071.338234	22.746880
96.248758	3071.801159	22.751898
96.536116	3071.245151	22.756915
96.740339	3071.472180	22.761933
96.355923	3073.659276	22.766951
96.554820	3083.680570	22.771968
96.503714	3075.646759	22.776986
96.494263	3090.993305	22.782003
97.194588	3100.078074	22.787021
97.119153	3104.568380	22.792039
97.343782	3103.965327	22.797056
97.477986	3107.605559	22.802074
97.092322	3104.803023	22.807091
97.524339	3116.192514	22.812109
97.766197	3120.901694	22.817127
97.904540	3124.604407	22.822144
97.824569	3122.341313	22.827162
97.418265	3125.538628	22.832179
98.022268	3128.215692	22.837197
97.607000	3130.524376	22.842215
98.082728	3135.313924	22.847232
98.303698	3149.302227	22.852250
98.305552	3145.246334	22.857267
98.665931	3137.419858	22.862285
98.425519	3155.633466	22.867303
98.573332	3146.811182	22.872320
98.591469	3154.234757	22.877338
98.345574	3166.307398	22.882355
98.941490	3159.293241	22.887373
98.358541	3170.894444	22.892391
98.972081	3175.672016	22.897408
99.145333	3180.114153	22.902426
99.178234	3190.723142	22.907443
99.172051	3199.536068	22.912461
99.457800	3211.828956	22.917479
99.881099	3214.152273	22.922496
100.327402	3200.618713	22.927514
100.831552	3194.335273	22.932531
100.766559	3187.559718	22.937549
100.492980	3178.023460	22.942567
100.649639	3164.553958	22.947584
100.795900	3164.395496	22.952602
101.066703	3156.980630	22.957619
100.633687	3155.643592	22.962637
100.634989	3161.030930	22.967655
100.639957	3153.313436	22.972672
100.865787	3165.498844	22.977690
100.839173	3177.966587	22.982707
101.156537	3180.274832	22.987725
101.277004	3191.296268	22.992743
101.180697	3179.583079	22.997760
101.088360	3189.220540	23.002778
101.402445	3194.881116	23.007795
101.328828	3185.039138	23.012813
101.200135	3190.844398	23.017831
101.517721	3195.276691	23.022848
101.863226	3203.738187	23.027866
101.559632	3213.604232	23.032883
102.094031	3206.912093	23.037901
101.889969	3219.555830	23.042919
101.940383	3208.823433	23.047936
101.963227	3224.581676	23.052954
102.030182	3236.574094	23.057971
102.132370	3231.341098	23.062989
102.386782	3238.964633	23.068007
102.499145	3244.814439	23.073024
102.528507	3258.226679	23.078042
102.343393	3257.346552	23.083059
102.858856	3265.011514	23.088077
102.858409	3260.425720	23.093095
103.175369	3275.096685	23.098112
103.792263	3273.836042	23.103130
103.723706	3278.249572	23.108147
103.991871	3269.275932	23.113165
103.800274	3274.090512	23.118183
103.577327	3282.804668	23.123200
103.951788	3272.921285	23.128218
103.736214	3275.227301	23.133235
103.836118	3266.011586	23.138253
104.299770	3265.693242	23.143271
104.226963	3274.756444	23.148288
104.541277	3275.906869	23.153306
104.602519	3280.297035	23.158323
104.627802	3294.385354	23.163341
104.858176	3301.555016	23.168359
104.850252	3298.024532	23.173376
105.094366	3297.172260	23.178394
104.689520	3305.119395	23.183411
104.758674	3300.955148	23.188429
104.928882	3309.573388	23.193447
105.218353	3312.087987	23.198464
105.478635	3309.904454	23.203482
105.384443	3319.614865	23.208499
105.517347	3314.105633	23.213517
105.550699	3310.559253	23.218535
105.721181	3337.874560	23.223552
105.889830	3340.417443	23.228570
106.421724	3346.672234	23.233587
106.466700	3348.101309	23.238605
106.075345	3349.159612	23.243623
106.169385	3342.693791	23.248640
106.361966	3339.283579	23.253658
105.822899	3355.233574	23.258675
106.402896	3365.135723	23.263693
106.755137	3371.049221	23.268711
106.436177	3376.136151	23.273728
106.745938	3378.275173	23.278746
106.593112	3392.994128	23.283763
106.937211	3384.188510	23.288781
107.131099	3396.341174	23.293799
106.922596	3412.937269	23.298816
107.218127	3420.444013	23.303834
107.019125	3428.943047	23.308851
107.694321	3430.204573	23.313869
107.761074	3439.826867	23.318887
107.679870	3442.588568	23.323904
108.114839	3441.065869	23.328922
107.987056	3450.601678	23.333939
108.482638	3454.652831	23.338957
108.793017	3458.341453	23.343975
108.875765	3460.777793	23.348992
109.183985	3436.496652	23.354010
108.820775	3436.635285	23.359027
109.004468	3430.692026	23.364045
108.806531	3439.837916	23.369063
108.733997	3455.194595	23.374080
108.933892	3446.354587	23.379098
108.717121	3469.220201	23.384115
108.769910	3465.074244	23.389133
109.183852	3473.323216	23.394151
109.057576	3481.126059	23.399168
109.372231	3481.825110	23.404186
109.583755	3495.486909	23.409203
109.606353	3498.481796	23.414221
109.924224	3502.156636	23.419239
110.121486	3513.554524	23.424256
110.235499	3506.703636	23.429274
109.957684	3514.163968	23.434291
110.322550	3512.803676	23.439309
110.613094	3531.578861	23.444327
110.490037	3533.368670	23.449344
110.346955	3533.940148	23.454362
110.568470	3535.534281	23.459379
111.028306	3536.466382	23.464397
111.133654	3553.360924	23.469415
111.068919	3555.684521	23.474432
111.528834	3556.673423	23.479450
111.413099	3566.699785	23.484467
111.574989	3556.470598	23.489485
111.724794	3562.286273	23.494503
111.650537	3556.067513	23.499520
112.308645	3566.734038	23.504538
112.112266	3582.378383	23.509555
112.255958	3578.183530	23.514573
112.220061	3575.430618	23.519591
111.871996	3586.963955	23.524608
112.182803	3574.410697	23.529626
112.099134	3584.880258	23.534643
112.449633	3594.512113	23.539661
112.728811	3591.334555	23.544679
112.899123	3605.533098	23.549696
112.910578	3604.300415	23.554714
112.744274	3621.161565	23.559731
113.030902	3637.084253	23.564749
113.276754	3632.564173	23.569767
112.850645	3641.947688	23.574784
113.422899	3648.988511	23.579802
113.654010	3648.718991	23.584819
113.578879	3654.298282	23.589837
113.669880	3656.484021	23.594855
113.508585	3675.086675	23.599872
114.076903	3680.382732	23.604890
114.078857	3690.453964	23.609907
114.273105	3692.279605	23.614925
114.217399	3691.937959	23.619943
114.630769	3704.561656	23.624960
114.626085	3704.814906	23.629978
114.901434	3706.094519	23.634995
114.943816	3704.591891	23.640013
115.624413	3689.762153	23.645031
115.847596	3682.045177	23.650048
115.662970	3684.226489	23.655066
115.928419	3676.228344	23.660083
115.846141	3675.786681	23.665101
116.283905	3675.554423	23.670119
116.431082	3681.714574	23.675136
116.416541	3670.891015	23.680154
116.677295	3671.428030	23.685171
116.752053	3663.336486	23.690189
116.650022	3659.205120	23.695207
116.675345	3658.248022	23.700224
116.575059	3642.072257	23.705242
116.628561	3644.844578	23.710259
116.883033	3647.042740	23.715277
117.103352	3659.810086	23.720295
116.971533	3671.846367	23.725312
117.209121	3656.492258	23.730330
117.130191	3666.673913	23.735347
117.306121	3665.153652	23.740365
117.169859	3671.960767	23.745383
117.474588	3664.524630	23.750400
117.593631	3671.572900	23.755418
117.543761	3664.261409	23.760435
117.371495	3686.198752	23.765453
117.814663	3693.127129	23.770471
117.732660	3694.699095	23.775488
117.964571	3691.128038	23.780506
117.854421	3698.316157	23.785523
117.730687	3709.363305	23.790541
118.419278	3709.783210	23.795559
118.119714	3724.152845	23.800576
118.228664	3730.858680	23.805594
118.517366	3746.285614	23.810611
118.392644	3750.540723	23.815629
119.307784	3767.880667	23.820647
119.080674	3770.131729	23.825664
119.053315	3769.331170	23.830682
119.277406	3770.498831	23.835699
119.352478	3791.930671	23.840717
119.408966	3796.002922	23.845735
119.445436	3807.394468	23.850752
119.716469	3808.766291	23.855770
119.991149	3823.160225	23.860787
119.614783	3824.550782	23.865805
120.263114	3826.384646	23.870823
120.391533	3833.074862	23.875840
120.682174	3831.372603	23.880858
120.592219	3837.512914	23.885875
120.784936	3847.971159	23.890893
120.989721	3832.158040	23.895911
121.024228	3836.142191	23.900928
121.257349	3835.076981	23.905946
121.279642	3840.394973	23.910963
121.251177	3857.632571	23.915981
121.446474	3862.718477	23.920999
121.368020	3861.894307	23.926016
121.451268	3860.347429	23.931034
121.603616	3869.218062	23.936051
121.783906	3895.124996	23.941069
122.215213	3890.727478	23.946087
122.204744	3897.631874	23.951104
121.996094	3896.742754	23.956122
122.092502	3903.731513	23.961139
122.030786	3919.468809	23.966157
122.336101	3923.278254	23.971175
122.691826	3940.033175	23.976192
122.960207	3932.391119	23.981210
122.839145	3937.018142	23.986227
122.552589	3946.313805	23.991245
123.445780	3962.259126	23.996263
123.402851	3971.213869	24.001280
123.506407	3976.525561	24.006298
123.747523	3969.528458	24.011315
123.379622	3985.193544	24.016333
123.754275	3989.970653	24.021351
123.419265	3990.319524	24.026368
123.817296	3999.022563	24.031386
124.511876	4011.460661	24.036403
124.333564	4017.463288	24.041421
124.777466	4021.459492	24.046439
124.461317	4019.368776	24.051456
124.693749	4017.337841	24.056474
124.721123	4023.188507	24.061491
124.741124	4035.870524	24.066509
125.147259	4042.482861	24.071527
125.345901	4047.517799	24.076544
125.692134	4041.567971	24.081562
125.363681	4040.558619	24.086579
125.269175	4054.085424	24.091597
125.696389	4054.896382	24.096615
126.054018	4057.804481	24.101632
125.940453	4063.686572	24.106650
126.260677	4067.629447	24.111667
126.009066	4076.951299	24.116685
126.377698	4084.371189	24.121703
126.538761	4076.890970	24.126720
126.456294	4086.868253	24.131738
126.800195	4082.591611	24.136755
126.742155	4084.986829	24.141773
126.913508	4091.995555	24.146791
127.286485	4099.711467	24.151808
127.301791	4106.387832	24.156826
127.450313	4103.675566	24.161843
127.451789	4106.149897	24.166861
127.611125	4122.225396	24.171879
127.909144	4124.820844	24.176896
127.793237	4137.094836	24.181914
128.177718	4129.504059	24.186931
128.293230	4135.716640	24.191949
128.147846	4135.092256	24.196967
128.305534	4148.049608	24.201984
128.534672	4152.615850	24.207002
128.833729	4148.434551	24.212019
128.797474	4161.788240	24.217037
128.902891	4162.314735	24.222055
129.083600	4178.203891	24.227072
129.034758	4183.157458	24.232090
128.954462	4180.878500	24.237107
128.944025	4195.629596	24.242125
129.345770	4200.989619	24.247143
129.559093	4207.464751	24.252160
129.439324	4216.128573	24.257178
130.145854	4218.606775	24.262195
130.350038	4236.518684	24.267213
130.332027	4233.273657	24.272231
130.250051	4237.560101	24.277248
130.623386	4231.956344	24.282266
131.107416	4237.202564	24.287283
131.426274	4244.964840	24.292301
131.364559	4244.655682	24.297319
131.619693	4243.643836	24.302336
131.414522	4245.399154	24.307354
131.375964	4240.689635	24.312371
131.408417	4244.510067	24.317389
131.748744	4230.720795	24.322407
131.684646	4237.529512	24.327424
131.637106	4236.668948	24.332442
131.862791	4251.787337	24.337459
131.854153	4256.311717	24.342477
132.195802	4263.615941	24.347495
131.953120	4270.035840	24.352512
132.123188	4273.850634	24.357530
132.494078	4283.195615	24.362547
132.399533	4294.225949	24.367565
132.527120	4288.054420	24.372583
132.981875	4300.751000	24.377600
132.690984	4314.409578	24.382618
132.836717	4320.705895	24.387635
133.133472	4321.568740	24.392653
133.441782	4341.879139	24.397671
133.383273	4341.572637	24.402688
133.567364	4350.062960	24.407706
133.856209	4354.345356	24.412723
133.811692	4363.265820	24.417741
134.190193	4363.380513	24.422759
134.664577	4365.484555	24.427776
134.493960	4372.332001	24.432794
134.385901	4366.336012	24.437811
134.946758	4377.056038	24.442829
134.891528	4385.160688	24.447847
135.309273	4391.477806	24.452864
135.493583	4394.403475	24.457882
135.462435	4381.716675	24.462899
135.442914	4388.117652	24.467917
135.328873	4388.097554	24.472935
135.768236	4392.028264	24.477952
135.401774	4400.493855	24.482970
135.613050	4400.811339	24.487987
136.074697	4409.577269	24.493005
136.268117	4414.385865	24.498023
136.710078	4422.962328	24.503040
136.563032	4435.699041	24.508058
136.538538	4431.517550	24.513075
136.512114	4437.824929	24.518093
136.804530	4437.754174	24.523111
136.865188	4444.830774	24.528128
136.871600	4457.108032	24.533146
137.296099	4454.633662	24.538163
137.326197	4466.799923	24.543181
137.373084	4483.455084	24.548199
137.555915	4487.204810	24.553216
137.364136	4485.258807	24.558234
137.919718	4493.072712	24.563251
137.772716	4511.923353	24.568269
137.796626	4508.236171	24.573287
138.231293	4519.433602	24.578304
138.277073	4530.177097	24.583322
138.656846	4533.113390	24.588339
138.711477	4535.992989	24.593357
139.017551	4555.233965	24.598375
139.036127	4552.806999	24.603392
139.411090	4563.227815	24.608410
139.395554	4557.596123	24.613427
139.406608	4563.370595	24.618445
139.371938	4572.482168	24.623463
139.497550	4571.765075	24.628480
139.670135	4585.531611	24.633498
139.924044	4591.482916	24.638515
140.242645	4598.292156	24.643533
140.221548	4602.285134	24.648551
140.490079	4601.021828	24.653568
140.551740	4622.990169	24.658586
140.621267	4618.535173	24.663603
140.624075	4627.754568	24.668621
140.847175	4635.232064	24.673639
141.237623	4645.701019	24.678656
141.113803	4647.693065	24.683674
141.524377	4657.688591	24.688691
141.418442	4658.986603	24.693709
141.611135	4668.896114	24.698727
142.064415	4661.060833	24.703744
141.761653	4679.613945	24.708762
142.145625	4679.087040	24.713779
142.299346	4685.246515	24.718797
142.297799	4707.025945	24.723815
142.643922	4697.294552	24.728832
142.724185	4701.735761	24.733850
142.522415	4700.514106	24.738867
142.870553	4709.209475	24.743885
143.209855	4732.583511	24.748903
143.460383	4729.694293	24.753920
142.974969	4721.108713	24.758938
143.379046	4735.978784	24.763955
143.774085	4747.327721	24.768973
143.854488	4757.478868	24.773991
143.757422	4753.652651	24.779008
143.876142	4772.073953	24.784026
144.098398	4774.403527	24.789043
143.883873	4782.435305	24.794061
143.808002	4791.395582	24.799079
144.503563	4800.522992	24.804096
144.588592	4816.178248	24.809114
144.642320	4823.862108	24.814131
144.997793	4830.725667	24.819149
145.191725	4845.650642	24.824167
145.463595	4836.653556	24.829184
145.374018	4849.072281	24.834202
145.656964	4854.924459	24.839219
145.981810	4855.678796	24.844237
145.623596	4857.230737	24.849255
146.110334	4868.047819	24.854272
145.956674	4892.287918	24.859290
146.450520	4891.027391	24.864307
146.470490	4896.507033	24.869325
146.504425	4912.126136	24.874343
146.625757	4913.136268	24.879360
146.801040	4921.947031	24.884378
147.056007	4928.794711	24.889395
147.587908	4927.569291	24.894413
147.513203	4923.073547	24.899431
148.123068	4924.825137	24.904448
147.972928	4940.311945	24.909466
148.363184	4953.760792	24.914483
148.619273	4953.023369	24.919501
148.866248	4950.197799	24.924519
148.837536	4944.609072	24.929536
148.737538	4950.918615	24.934554
148.845440	4951.630977	24.939571
149.401246	4950.297670	24.944589
148.952968	4950.604219	24.949607
149.532692	4949.128305	24.954624
149.399605	4963.870714	24.959642
149.338309	4971.907127	24.964659
149.750108	4964.731559	24.969677
149.423712	4964.015382	24.974695
149.770680	4973.364445	24.979712
149.855837	4995.187538	24.984730
149.852298	4991.438246	24.989747
150.319003	4992.082122	24.994765
150.267135	5009.706390	24.999783
150.363592	5010.852971	25.004800
150.438260	5017.081683	25.009818
150.700458	5038.994054	25.014835
151.158020	5039.105913	25.019853
151.319031	5040.324514	25.024871
151.504609	5045.664784	25.029888
151.779260	5054.864169	25.034906
151.715016	5055.748534	25.039923
151.950295	5061.993290	25.044941
151.814408	5058.592862	25.049959
152.130205	5061.425570	25.054976
152.441503	5081.385966	25.059994
152.471709	5089.493410	25.065011
152.452995	5084.225044	25.070029
152.449219	5096.349654	25.075047
152.737660	5092.728488	25.080064
152.712115	5106.684090	25.085082
152.772241	5112.482662	25.090099
153.124719	5118.311475	25.095117
153.429342	5129.807301	25.100135
153.746093	5132.235843	25.105152
153.826994	5143.539243	25.110170
153.897726	5145.235908	25.115187
154.204925	5147.735382	25.120205
153.853576	5166.754245	25.125223
154.268273	5161.500447	25.130240
154.239948	5172.461031	25.135258
154.474186	5181.436349	25.140275
154.564965	5190.093105	25.145293
154.874644	5191.910398	25.150311
155.133161	5202.804247	25.155328
155.324503	5218.651626	25.160346
155.569183	5217.865466	25.165363
155.594451	5206.548692	25.170381
155.595917	5217.384719	25.175399
155.874321	5229.143523	25.180416
156.178754	5232.688239	25.185434
156.013009	5249.216225	25.190451
156.573538	5252.165530	25.195469
156.426619	5263.122537	25.200487
156.714399	5261.692052	25.205504
156.906298	5276.857592	25.210522
156.777284	5294.992874	25.215539
157.373622	5291.134343	25.220557
157.329013	5292.741659	25.225575
157.197226	5296.319580	25.230592
157.604061	5311.937788	25.235610
157.527330	5311.059622	25.240627
158.044425	5331.802631	25.245645
157.813610	5347.359163	25.250663
158.142079	5349.678588	25.255680
157.952949	5355.225645	25.260698
158.364014	5370.729610	25.265715
158.901972	5371.782224	25.270733
158.567025	5382.361387	25.275751
158.799291	5388.019611	25.280768
159.271563	5396.822245	25.285786
159.199201	5403.244433	25.290803
159.464187	5400.570659	25.295821
159.691580	5415.976998	25.300839
159.797339	5425.477483	25.305856
160.411228	5426.960193	25.310874
160.091533	5440.182185	25.315891
160.664546	5427.599453	25.320909
160.873490	5440.338263	25.325927
160.748599	5453.858214	25.330944
160.956277	5465.492451	25.335962
160.896898	5468.835020	25.340979
161.284668	5465.706519	25.345997
161.309747	5478.937991	25.351015
161.574605	5494.490077	25.356032
161.886202	5482.443585	25.361050
161.947200	5495.701042	25.366067
161.836010	5490.374355	25.371085
161.888977	5501.729675	25.376103
161.777279	5511.961657	25.381120
162.361957	5519.692566	25.386138
162.643309	5536.482641	25.391155
162.518003	5536.713662	25.396173
162.872987	5546.336392	25.401191
163.184891	5557.206360	25.406208
163.306765	5567.206302	25.411226
163.296512	5571.750200	25.416243
163.838166	5570.999860	25.421261
164.067866	5566.829037	25.426279
164.221995	5564.080959	25.431296
164.429820	5570.724734	25.436314
164.288600	5575.405816	25.441331
164.702591	5570.540267	25.446349
164.718155	5576.708928	25.451367
164.682983	5576.976421	25.456384
165.173964	5574.699885	25.461402
165.335346	5592.525101	25.466419
165.289307	5604.262060	25.471437
165.310839	5603.412773	25.476455
165.220745	5606.154089	25.481472
165.977065	5615.837479	25.486490
165.793297	5628.397662	25.491507
165.871739	5623.454922	25.496525
166.036483	5636.696330	25.501543
166.208596	5656.161351	25.506560
166.359131	5653.331749	25.511578
166.792009	5656.259959	25.516595
166.575447	5670.027930	25.521613
166.913569	5676.171658	25.526631
166.947628	5687.271199	25.531648
166.860506	5703.317027	25.536666
166.712931	5721.345142	25.541683
167.287764	5731.470361	25.546701
167.796566	5743.616609	25.551719
167.641031	5755.531698	25.556736
168.089714	5765.143114	25.561754
168.705088	5770.555573	25.566771
168.497385	5773.870785	25.571789
168.593303	5781.248604	25.576807
168.916611	5789.007695	25.581824
168.598768	5794.432877	25.586842
169.017585	5812.874799	25.591859
169.369085	5807.886341	25.596877
169.335393	5826.581810	25.601895
169.633967	5836.541764	25.606912
169.886329	5838.181807	25.611930
170.205703	5845.471201	25.616947
170.317511	5862.565755	25.621965
170.611414	5853.422692	25.626983
170.902633	5857.133731	25.632000
171.047261	5852.650958	25.637018
171.063992	5873.813402	25.642035
171.752191	5871.982773	25.647053
171.857051	5870.890068	25.652071
171.840115	5878.961011	25.657088
171.895002	5872.579302	25.662106
171.930937	5878.217741	25.667123
171.843314	5875.368364	25.672141
172.108518	5893.897417	25.677159
172.609483	5903.346092	25.682176
172.736498	5902.650826	25.687194
172.576875	5916.959367	25.692212
172.658906	5920.671422	25.697229
172.806506	5923.723007	25.702247
172.969116	5931.620816	25.707264
172.892826	5946.317296	25.712282
173.157318	5959.426614	25.717300
173.250486	5978.083549	25.722317
173.486679	5984.265348	25.727335
173.730573	5998.359611	25.732352
174.039740	6012.386904	25.737370
173.923743	6008.531803	25.742388
174.141032	6022.150419	25.747405
174.497654	6033.673446	25.752423
174.745010	6044.055006	25.757440
174.864136	6059.352479	25.762458
174.957643	6069.420247	25.767476
174.936334	6068.053606	25.772493
175.103767	6076.575741	25.777511
175.242585	6090.992629	25.782528
175.330406	6101.522169	25.787546
175.383190	6119.882498	25.792564
176.290730	6135.009938	25.797581
176.343674	6141.071957	25.802599
176.212520	6146.351381	25.807616
176.715085	6150.054830	25.812634
176.993115	6168.613732	25.817652
177.116809	6174.993040	25.822669
177.415881	6180.559038	25.827687
177.139258	6196.136049	25.832704
177.532305	6194.925854	25.837722
177.492153	6199.802857	25.842740
177.704486	6219.063347	25.847757
177.726994	6223.324520	25.852775
178.196522	6247.336817	25.857792
178.509019	6238.462141	25.862810
178.325557	6261.509165	25.867828
178.733926	6262.174801	25.872845
179.003992	6280.839227	25.877863
179.209629	6287.613028	25.882880
179.577210	6296.059911	25.887898
179.560720	6308.585048	25.892916
179.726406	6317.401139	25.897933
180.215207	6325.336720	25.902951
180.031511	6333.875763	25.907968
180.207308	6332.096456	25.912986
180.603788	6352.483764	25.918004
180.645548	6353.108623	25.923021
181.094404	6356.659485	25.928039
181.285023	6376.362301	25.933056
181.514831	6379.076024	25.938074
181.522957	6383.011178	25.943092
181.410363	6395.229354	25.948109
181.957870	6402.126747	25.953127
181.481285	6416.327191	25.958144
182.043163	6420.794852	25.963162
182.185327	6434.305518	25.968180
182.587231	6446.418372	25.973197
182.800495	6452.919571	25.978215
182.813567	6456.803463	25.983232
182.906393	6463.320259	25.988250
183.223156	6479.512230	25.993268
183.213332	6491.967007	25.998285
183.601318	6489.782157	26.003303
183.661101	6507.838742	26.008320
184.007273	6515.057941	26.013338
184.044698	6533.979816	26.018356
184.128488	6542.098504	26.023373
184.645705	6547.987361	26.028391
184.672644	6570.127605	26.033408
184.976363	6563.855280	26.038426
185.418102	6576.956388	26.043444
185.679087	6583.639607	26.048461
185.689927	6583.218098	26.053479
185.665146	6582.375975	26.058496
186.085663	6595.142630	26.063514
186.469716	6592.705843	26.068532
186.269312	6609.622419	26.073549
186.628866	6607.625073	26.078567
186.924255	6610.533809	26.083584
187.049227	6602.177446	26.088602
187.074717	6604.541049	26.093620
187.186653	6620.758721	26.098637
187.787954	6627.060673	26.103655
187.698794	6636.039707	26.108672
187.517349	6629.154727	26.113690
188.079164	6639.771774	26.118708
188.291508	6653.688366	26.123725
188.600513	6646.269294	26.128743
188.607575	6649.765884	26.133760
188.596548	6649.865482	26.138778
189.154031	6664.021924	26.143796
188.828987	6673.085052	26.148813
189.234747	6671.314105	26.153831
189.160424	6683.561238	26.158848
189.480779	6707.565798	26.163866
189.433103	6710.584782	26.168884
189.263428	6724.863951	26.173901
189.935161	6733.424679	26.178919
190.111027	6752.274718	26.183936
190.305561	6762.453408	26.188954
190.534410	6772.241637	26.193972
190.362676	6789.567451	26.198989
190.794935	6797.695135	26.204007
191.077213	6813.147774	26.209024
191.103200	6812.594474	26.214042
191.510371	6831.111845	26.219060
191.717680	6848.473405	26.224077
192.142807	6841.778018	26.229095
192.880647	6858.261483	26.234112
193.109746	6848.089436	26.239130
193.290626	6855.208234	26.244148
193.352792	6853.531801	26.249165
193.876619	6842.398407	26.254183
193.838798	6850.308878	26.259200
193.606395	6847.778626	26.264218
194.055981	6863.836615	26.269236
194.203168	6865.180607	26.274253
194.211513	6876.594237	26.279271
194.313580	6884.321948	26.284288
194.396730	6891.162395	26.289306
194.856980	6891.030783	26.294324
194.642016	6896.190886	26.299341
195.266311	6895.484454	26.304359
195.664669	6905.120093	26.309376
195.928957	6909.504779	26.314394
196.312247	6899.649631	26.319412
196.299562	6902.852606	26.324429
196.247149	6898.655955	26.329447
196.267408	6925.176125	26.334464
196.411167	6927.603433	26.339482
196.769832	6934.697740	26.344500
197.078025	6946.471956	26.349517
197.278825	6953.331991	26.354535
197.193359	6961.761328	26.359552
196.867561	6980.007837	26.364570
197.559225	6979.350894	26.369588
197.441523	6988.931179	26.374605
197.358459	6999.187945	26.379623
197.671836	7011.933690	26.384640
198.104221	7028.613236	26.389658
198.451373	7032.855622	26.394676
198.261569	7047.371780	26.399693
198.407714	7066.851817	26.404711
198.772109	7085.597083	26.409728
198.866939	7101.385361	26.414746
199.470704	7104.757570	26.419764
199.421221	7126.361097	26.424781
199.770233	7132.023787	26.429799
199.595885	7142.793623	26.434816
199.691496	7155.952192	26.439834
200.409282	7152.061743	26.444852
200.768018	7170.580686	26.449869
201.161917	7169.903801	26.454887
201.342000	7164.297672	26.459904
201.436929	7168.980276	26.464922
201.514535	7174.723116	26.469940
201.620318	7187.005681	26.474957
202.178182	7190.422935	26.479975
202.436156	7203.174282	26.484992
202.212607	7215.647041	26.490010
202.347791	7215.124080	26.495028
202.653925	7228.038417	26.500045
202.774289	7241.325780	26.505063
202.971971	7249.086111	26.510080
203.059886	7255.603955	26.515098
203.625344	7270.154231	26.520116
203.386746	7282.986102	26.525133
203.620695	7295.656019	26.530151
203.402075	7301.476586	26.535168
203.873233	7324.498793	26.540186
204.544421	7325.054103	26.545204
204.370821	7349.938249	26.550221
204.852702	7350.876601	26.555239
204.653099	7362.944809	26.560256
205.101419	7381.374254	26.565274
205.695884	7391.620461	26.570292
205.491394	7408.112231	26.575309
205.710587	7421.204396	26.580327
206.121725	7428.644296	26.585344
205.961412	7441.284147	26.590362
206.267290	7449.804310	26.595380
206.563075	7464.390412	26.600397
206.740404	7473.072658	26.605415
207.402024	7485.938145	26.610432
207.419514	7494.680013	26.615450
207.967794	7502.537398	26.620468
207.736288	7513.796196	26.625485
207.965985	7520.434119	26.630503
208.498441	7536.195677	26.635520
208.444239	7540.276529	26.640538
208.592071	7549.553743	26.645556
208.794657	7573.618812	26.650573
208.573483	7572.340000	26.655591
208.757810	7587.568618	26.660608
209.365644	7602.548214	26.665626
209.889491	7611.574347	26.670644
209.525543	7619.220232	26.675661
210.104036	7644.966326	26.680679
210.363904	7652.025782	26.685696
210.238069	7662.453736	26.690714
210.731041	7683.171608	26.695732
210.809975	7691.187383	26.700749
210.974066	7705.601608	26.705767
211.637969	7708.582580	26.710784
211.635107	7730.002771	26.715802
212.041566	7730.567741	26.720820
211.818227	7736.392336	26.725837
211.994798	7757.513128	26.730855
212.408748	7750.797054	26.735872
212.549088	7777.845908	26.740890
213.106690	7785.272621	26.745908
213.069130	7795.649023	26.750925
212.923827	7804.785745	26.755943
213.856928	7823.067549	26.760960
213.592185	7834.678980	26.765978
213.620486	7841.054779	26.770996
213.783455	7861.357002	26.776013
214.082364	7855.384899	26.781031
214.675872	7866.316580	26.786048
214.715329	7868.567677	26.791066
214.960358	7877.078571	26.796084
215.046791	7890.210681	26.801101
215.249593	7890.965212	26.806119
215.626912	7906.394505	26.811136
215.740403	7919.752882	26.816154
216.262686	7910.333315	26.821172
216.129032	7927.404871	26.826189
216.484770	7939.573258	26.831207
217.101091	7940.837977	26.836224
217.196200	7962.079022	26.841242
217.364574	7970.933375	26.846260
217.455360	7980.923692	26.851277
217.670195	7990.140185	26.856295
218.166644	7996.455781	26.861312
217.959414	8007.704786	26.866330
218.193241	8010.601233	26.871348
218.137980	8023.856522	26.876365
218.155121	8031.373792	26.881383
218.456118	8045.842737	26.886400
218.547191	8065.101946	26.891418
218.752575	8084.876910	26.896436
219.042149	8100.799889	26.901453
219.267151	8113.219205	26.906471
219.499170	8131.073778	26.911488
219.725748	8156.389201	26.916506
219.853305	8168.577479	26.921524
220.146077	8183.884417	26.926541
220.619438	8208.148091	26.931559
221.326731	8217.272244	26.936576
221.389425	8225.896925	26.941594
222.001815	8224.999726	26.946612
222.461708	8236.628030	26.951629
222.562421	8237.038570	26.956647
222.608727	8234.366866	26.961664
222.596475	8247.183109	26.966682
223.074676	8247.872679	26.971700
222.976413	8264.115056	26.976717
223.025968	8264.145248	26.981735
223.502027	8281.958817	26.986752
223.352455	8290.632361	26.991770
223.696482	8302.288217	26.996788
223.713384	8316.274381	27.001805
224.158907	8329.906536	27.006823
224.374612	8345.314004	27.011840
224.257523	8354.920159	27.016858
224.739974	8366.800753	27.021876
224.803078	8381.670057	27.026893
225.157640	8396.863370	27.031911
225.885568	8399.626127	27.036928
225.871382	8424.654226	27.041946
226.070201	8430.618522	27.046964
226.282168	8444.091386	27.051981
226.624408	8461.471348	27.056999
227.056503	8453.189457	27.062016
227.108324	8459.388170	27.067034
227.202258	8479.780748	27.072052
227.599937	8479.999835	27.077069
227.481742	8492.668576	27.082087
227.960404	8513.001293	27.087104
227.888395	8519.522383	27.092122
228.067835	8528.517349	27.097140
228.483934	8537.257636	27.102157
228.077051	8553.036871	27.107175
228.780366	8567.604600	27.112192
228.751233	8585.724424	27.117210
228.857641	8592.726051	27.122228
228.976661	8602.317674	27.127245
229.273455	8631.004042	27.132263
229.614993	8649.583980	27.137280
230.051407	8664.988925	27.142298
230.273619	8673.813133	27.147316
230.598780	8683.429533	27.152333
230.849361	8703.558031	27.157351
231.057419	8706.032393	27.162368
231.233335	8711.596238	27.167386
231.380834	8730.989427	27.172404
231.572333	8746.470454	27.177421
231.585300	8768.328221	27.182439
232.379016	8775.431281	27.187456
232.383448	8788.472613	27.192474
232.665067	8805.155145	27.197492
232.653554	8813.283359	27.202509
232.787495	8827.699998	27.207527
233.325482	8845.378186	27.212544
233.805386	8869.891125	27.217562
233.517183	8888.569346	27.222580
234.563716	8894.799612	27.227597
234.401930	8906.061030	27.232615
234.947461	8924.281145	27.237632
235.016996	8944.908504	27.242650
235.003411	8949.479013	27.247668
235.152831	8952.625535	27.252685
235.309289	8969.084602	27.257703
235.588095	8984.555393	27.262720
235.835508	9013.388956	27.267738
236.034903	9021.430755	27.272756
236.747826	9036.313074	27.277773
236.775467	9051.507310	27.282791
237.177701	9058.062099	27.287808
237.627151	9076.527794	27.292826
238.061925	9073.852319	27.297844
238.310991	9084.835194	27.302861
238.497637	9086.927768	27.307879
238.992425	9094.535279	27.312896
239.197191	9098.689815	27.317914
239.391099	9087.117081	27.322932
239.815316	9095.291239	27.327949
239.959226	9105.829553	27.332967
240.319732	9105.770293	27.337984
240.306089	9107.458363	27.343002
240.371638	9113.168956	27.348020
240.931155	9118.856318	27.353037
240.607011	9132.795167	27.358055
240.753680	9135.032885	27.363072
240.900896	9144.737215	27.368090
241.139336	9160.075523	27.373108
241.301691	9170.099541	27.378125
241.195854	9189.491608	27.383143
241.433172	9206.004597	27.388160
241.625852	9222.568751	27.393178
241.916195	9244.728029	27.398196
242.160836	9254.941342	27.403213
242.221165	9284.360118	27.408231
242.739107	9307.090217	27.413248
243.020667	9318.147102	27.418266
243.256888	9337.287166	27.423284
243.561371	9348.289986	27.428301
243.601258	9361.676650	27.433319
243.770064	9379.987438	27.438336
244.508473	9396.807763	27.443354
244.736334	9406.354444	27.448372
245.042138	9417.072949	27.453389
245.024576	9432.590256	27.458407
245.240212	9444.333124	27.463424
245.356846	9450.799914	27.468442
245.915239	9464.544782	27.473460
246.303657	9469.027574	27.478477
246.166715	9488.996254	27.483495
246.389869	9496.832498	27.488512
247.269635	9515.768366	27.493530
247.466379	9526.784908	27.498548
247.923389	9522.906160	27.503565
247.847410	9538.423178	27.508583
248.085915	9549.584779	27.513600
248.321089	9562.271851	27.518618
247.960834	9567.736309	27.523636
248.552024	9574.318695	27.528653
248.491041	9592.368687	27.533671
248.930441	9615.796514	27.538688
249.479887	9625.416374	27.543706
249.429837	9649.630826	27.548724
249.697838	9666.641452	27.553741
249.969125	9680.718489	27.558759
250.179893	9693.649402	27.563776
250.708637	9696.746468	27.568794
251.017563	9700.386075	27.573812
251.502096	9720.438212	27.578829
251.305375	9739.485074	27.583847
251.681058	9751.698910	27.588864
252.176969	9758.416172	27.593882
252.380823	9778.117410	27.598900
252.653748	9784.218999	27.603917
252.471663	9807.374424	27.608935
252.699924	9815.923553	27.613952
253.275160	9826.410912	27.618970
253.494658	9843.716564	27.623988
253.382948	9857.935453	27.629005
254.099974	9874.374353	27.634023
254.271123	9892.511631	27.639040
254.646161	9912.448416	27.644058
254.349977	9924.558586	27.649076
254.841313	9933.376227	27.654093
254.626554	9955.324520	27.659111
255.186635	9980.085345	27.664128
255.658046	9995.375444	27.669146
255.642287	10015.202686	27.674164
256.230902	10023.345347	27.679181
256.296834	10047.131808	27.684199
256.177015	10054.241826	27.689216
257.048450	10080.302488	27.694234
256.950702	10101.689676	27.699252
257.428614	10123.031468	27.704269
257.232728	10143.180522	27.709287
257.672333	10154.257503	27.714304
258.023530	10175.451745	27.719322
258.229177	10196.930730	27.724340
258.648552	10207.385738	27.729357
258.950236	10237.305196	27.734375
259.327499	10250.883091	27.739392
259.824600	10269.168903	27.744410
259.712699	10284.619516	27.749428
260.143001	10283.071745	27.754445
260.416692	10305.639024	27.759463
260.564915	10319.779908	27.764480
261.305700	10332.196190	27.769498
261.542818	10347.235734	27.774516
262.219490	10332.739120	27.779533
262.703829	10326.273226	27.784551
262.670028	10329.969474	27.789568
263.095858	10337.806094	27.794586
263.153580	10348.058582	27.799604
263.320049	10346.684491	27.804621
263.172004	10352.030889	27.809639
263.501816	10365.297362	27.814656
263.922467	10384.352959	27.819674
263.731784	10387.448482	27.824692
264.388441	10397.159404	27.829709
264.242349	10414.004694	27.834727
264.108152	10414.764436	27.839744
264.547938	10431.502742	27.844762
264.648119	10460.200447	27.849780
264.875687	10468.456348	27.854797
265.291380	10482.025272	27.859815
265.403508	10505.874590	27.864832
265.725488	10517.266896	27.869850
265.820387	10550.752180	27.874868
266.121956	10572.365063	27.879885
266.704058	10580.758420	27.884903
266.990237	10599.557321	27.889920
267.686747	10610.477754	27.894938
268.562093	10616.198504	27.899956
268.921255	10614.870172	27.904973
268.947106	10617.177399	27.909991
269.142007	10635.775843	27.915008
269.313787	10644.548852	27.920026
269.188133	10651.328476	27.925044
269.449282	10666.048795	27.930061
269.907595	10669.943191	27.935079
269.592463	10691.866929	27.940096
270.164671	10703.378264	27.945114
270.552883	10726.562867	27.950132
270.964552	10736.220543	27.955149
270.832680	10758.643120	27.960167
270.824809	10777.248015	27.965184
271.325677	10789.130458	27.970202
271.455547	10816.883170	27.975220
271.531454	10831.004127	27.980237
271.995908	10846.166554	27.985255
272.379013	10876.791104	27.990272
272.743722	10886.854009	27.995290
272.543448	10908.043374	28.000308
273.092886	10934.294293	28.005325
273.473495	10958.572853	28.010343
273.663965	10980.051946	28.015360
274.100185	10985.137060	28.020378
274.353859	11007.758824	28.025396
274.534683	11027.344984	28.030413
275.205216	11038.913842	28.035431
275.499095	11060.743197	28.040448
275.927988	11081.771657	28.045466
275.867731	11095.573002	28.050484
276.224856	11105.195156	28.055501
276.525040	11121.908455	28.060519
276.377187	11146.111657	28.065536
276.667840	11151.282629	28.070554
277.235050	11177.540596	28.075572
277.588516	11188.707386	28.080589
277.808432	11202.452561	28.085607
277.989612	11219.408657	28.090624
278.372681	11246.276372	28.095642
279.122157	11261.997851	28.100660
279.153742	11282.160080	28.105677
279.495311	11287.379998	28.110695
279.471727	11297.601460	28.115712
279.677468	11313.164504	28.120730
279.969934	11340.614816	28.125748
280.166234	11349.163311	28.130765
280.800426	11359.831813	28.135783
280.885055	11377.065159	28.140800
281.127475	11381.122776	28.145818
281.353034	11393.863114	28.150836
281.800075	11414.579684	28.155853
281.851979	11418.717491	28.160871
282.307586	11437.715044	28.165888
282.738455	11441.553883	28.170906
282.720041	11462.623992	28.175924
282.875535	11484.304878	28.180941
283.386887	11502.892809	28.185959
283.327314	11527.521661	28.190976
283.684866	11534.819999	28.195994
283.623317	11555.694844	28.201012
283.983316	11580.144771	28.206029
284.786351	11596.445504	28.211047
284.684984	11620.765227	28.216064
285.361574	11627.568713	28.221082
285.623921	11647.430170	28.226100
285.894172	11671.603691	28.231117
286.273317	11686.663252	28.236135
286.331338	11705.751394	28.241152
287.214443	11722.664977	28.246170
287.184759	11743.374031	28.251188
287.204925	11748.280993	28.256205
287.692130	11766.604549	28.261223
287.967653	11792.867743	28.266240
288.401780	11800.918406	28.271258
288.461105	11823.606148	28.276276
288.778090	11843.784542	28.281293
289.092539	11858.333306	28.286311
289.354978	11882.303069	28.291328
289.779275	11894.397069	28.296346
290.098611	11904.739144	28.301364
290.545450	11912.418433	28.306381
291.226301	11928.507972	28.311399
291.449346	11930.247862	28.316416
291.652291	11940.513348	28.321434
291.908041	11949.829641	28.326452
292.151293	11967.878768	28.331469
292.669043	11971.366322	28.336487
292.924797	11991.166018	28.341504
293.420547	12007.410747	28.346522
293.537625	12007.272552	28.351540
293.586915	12022.851070	28.356557
294.063195	12036.089612	28.361575
293.854949	12055.415339	28.366592
294.202099	12066.005785	28.371610
294.558552	12084.747874	28.376628
294.257199	12096.585531	28.381645
295.026218	12113.157256	28.386663
294.990744	12141.806030	28.391680
295.161396	12163.797951	28.396698
295.783873	12184.728044	28.401716
296.030632	12209.256417	28.406733
296.372425	12225.004286	28.411751
296.528180	12252.606682	28.416768
296.745496	12272.883155	28.421786
297.060623	12294.236985	28.426804
297.394105	12310.772487	28.431821
298.172365	12334.359382	28.436839
298.127146	12347.395141	28.441856
298.016271	12367.599659	28.446874
299.138792	12390.804627	28.451892
299.035349	12405.134680	28.456909
299.479501	12418.659532	28.461927
299.985833	12444.167743	28.466944
299.719282	12459.157933	28.471962
300.232895	12470.748954	28.476980
300.173111	12485.732236	28.481997
300.801320	12500.794727	28.487015
300.724422	12521.537250	28.492032
301.306401	12541.949862	28.497050
301.497403	12563.493840	28.502068
301.659721	12583.545537	28.507085
302.501466	12602.203116	28.512103
302.527713	12628.556811	28.517120
303.310167	12635.877846	28.522138
303.381995	12657.756261	28.527156
304.092208	12663.803347	28.532173
304.127676	12686.056914	28.537191
304.172720	12702.214525	28.542208
304.564386	12712.855246	28.547226
305.012421	12735.976183	28.552244
304.716625	12743.304081	28.557261
304.858470	12759.143525	28.562279
305.354724	12787.928386	28.567296
305.671043	12813.990872	28.572314
306.645601	12825.627189	28.577332
306.441066	12849.490891	28.582349
306.834180	12869.232232	28.587367
307.331301	12887.732176	28.592384
307.437896	12910.931747	28.597402
308.019753	12925.209187	28.602420
308.246836	12944.385946	28.607437
308.832665	12975.339193	28.612455
309.375164	12968.380201	28.617472
309.423543	12995.207792	28.622490
309.857086	13009.451545	28.627508
309.817219	13025.047929	28.632525
310.159948	13042.829974	28.637543
310.647162	13056.973831	28.642560
310.636898	13068.163633	28.647578
311.033405	13078.781703	28.652596
311.402045	13110.245817	28.657613
311.903288	13124.378067	28.662631
312.183069	13139.631102	28.667648
312.436564	13163.146002	28.672666
312.741863	13173.813062	28.677684
312.752514	13199.468939	28.682701
313.756178	13210.548341	28.687719
313.926956	13230.612040	28.692736
313.964094	13245.890305	28.697754
314.701438	13257.690136	28.702772
314.843955	13271.774136	28.707789
314.857666	13283.389801	28.712807
315.358158	13305.893804	28.717824
315.373287	13329.228127	28.722842
315.554229	13347.376697	28.727860
315.914441	13364.891063	28.732877
316.405718	13384.425031	28.737895
316.765000	13402.517469	28.742912
316.985203	13430.124186	28.747930
317.468526	13449.302618	28.752948
317.775852	13462.783208	28.757965
318.353506	13465.194351	28.762983
318.572227	13495.340342	28.768000
318.747888	13514.209895	28.773018
319.165725	13514.741711	28.778036
319.655114	13536.568768	28.783053
319.994054	13553.616093	28.788071
320.199910	13572.250476	28.793088
320.170731	13588.518296	28.798106
320.689656	13607.362923	28.803124
320.789092	13629.699221	28.808141
321.292494	13631.430362	28.813159
321.732173	13654.433725	28.818176
321.911556	13664.795400	28.823194
322.128623	13679.635473	28.828212
322.566454	13702.913923	28.833229
322.633524	13709.494113	28.838247
323.280836	13724.393557	28.843264
323.355798	13745.587471	28.848282
323.675925	13753.820936	28.853300
323.650818	13777.784191	28.858317
324.147451	13801.416772	28.863335
324.178014	13832.419975	28.868352
324.559741	13855.530502	28.873370
325.135119	13877.091928	28.878388
325.597207	13887.836037	28.883405
326.011218	13899.686609	28.888423
326.271513	13928.907849	28.893440
326.556379	13955.226287	28.898458
327.098692	13964.151588	28.903476
327.355298	13991.548188	28.908493
327.481587	14004.498385	28.913511
327.767549	14024.990270	28.918528
328.038290	14051.948954	28.923546
328.282818	14072.463130	28.928564
328.658909	14100.011816	28.933581
329.270739	14116.129766	28.938599
329.545471	14129.972760	28.943616
329.301983	14164.262441	28.948634
329.621520	14183.757654	28.953652
330.157505	14220.341966	28.958669
330.984388	14229.589420	28.963687
331.664031	14239.396666	28.968704
331.970464	14260.918292	28.973722
332.453356	14275.256375	28.978740
332.755612	14292.717463	28.983757
332.683127	14315.100281	28.988775
333.426784	14339.254048	28.993792
333.442329	14352.985970	28.998810
333.583115	14371.846017	29.003828
333.812353	14390.629151	29.008845
334.289014	14411.230718	29.013863
334.624141	14428.251001	29.018880
334.642675	14460.195043	29.023898
334.918679	14477.290895	29.028916
335.172581	14508.405701	29.033933
335.874443	14544.023709	29.038951
335.841446	14562.784677	29.043968
336.362260	14585.861808	29.048986
336.608216	14605.255219	29.054004
337.176775	14631.110402	29.059021
337.747791	14657.192620	29.064039
337.716661	14667.938165	29.069056
337.943207	14705.389532	29.074074
338.244931	14714.943209	29.079092
338.819673	14754.345859	29.084109
339.149786	14776.271778	29.089127
339.468586	14792.994909	29.094144
339.655240	14824.385983	29.099162
340.284070	14847.465565	29.104180
340.739549	14872.571257	29.109197
341.381335	14890.084253	29.114215
341.672838	14896.967834	29.119232
341.780482	14923.248882	29.124250
342.548186	14949.477737	29.129268
343.018307	14950.235161	29.134285
343.448437	14953.904301	29.139303
344.384448	14958.887425	29.144320
344.831981	14962.440165	29.149338
344.907781	14963.565318	29.154356
345.246613	14983.061507	29.159373
345.008096	14994.098489	29.164391
346.013059	14994.144178	29.169408
345.912491	14994.756748	29.174426
346.094095	15014.637475	29.179444
346.374664	15027.561193	29.184461
346.458242	15046.746631	29.189479
346.580732	15050.621592	29.194496
346.633706	15070.854010	29.199514
346.907809	15087.931757	29.204532
347.800809	15102.111875	29.209549
347.957499	15117.660427	29.214567
348.388744	15135.607515	29.219584
348.447741	15160.279480	29.224602
348.765535	15181.828803	29.229620
349.061962	15202.866694	29.234637
349.245066	15231.530322	29.239655
349.680620	15251.355970	29.244672
349.944892	15275.475024	29.249690
350.178237	15302.356032	29.254708
350.478325	15331.705876	29.259725
350.715918	15367.650362	29.264743
351.323814	15391.349714	29.269760
351.246276	15425.325269	29.274778
351.952201	15461.932886	29.279796
351.938264	15487.102994	29.284813
352.426175	15518.697811	29.289831
353.420183	15545.227028	29.294848
353.534889	15579.024491	29.299866
353.819661	15598.981354	29.304884
354.369332	15624.607118	29.309901
354.752353	15646.538434	29.314919
355.319981	15667.300904	29.319936
355.252020	15695.394770	29.324954
355.712660	15723.100032	29.329972
356.228316	15741.615670	29.334989
356.417358	15772.764745	29.340007
356.554511	15797.213759	29.345024
356.732499	15824.991596	29.350042
357.187380	15855.657260	29.355060
357.685198	15885.236151	29.360077
358.384347	15919.170623	29.365095
358.771777	15936.155687	29.370112
359.123311	15979.973028	29.375130
359.801450	15986.569414	29.380148
360.317779	15998.623292	29.385165
360.548025	16021.883207	29.390183
361.267719	16032.092572	29.395200
361.624250	16055.004402	29.400218
361.865603	16061.833047	29.405236
362.139848	16084.028149	29.410253
362.081843	16110.191335	29.415271
362.810776	16118.848566	29.420288
363.106070	16155.900441	29.425306
362.830930	16181.686944	29.430324
363.591652	16207.065864	29.435341
363.505181	16233.634760	29.440359
364.016910	16252.341006	29.445376
364.618410	16281.853835	29.450394
365.097762	16307.295643	29.455412
365.378508	16326.347442	29.460429
365.380244	16364.064460	29.465447
365.862937	16385.611577	29.470464
366.103141	16409.309427	29.475482
366.220858	16434.318154	29.480500
367.129959	16469.367411	29.485517
367.064494	16510.875774	29.490535
367.500301	16522.999370	29.495552
367.830360	16552.630677	29.500570
367.856166	16578.822511	29.505588
368.569793	16610.001821	29.510605
368.768340	16635.869950	29.515623
369.757826	16662.840446	29.520640
369.638938	16695.141247	29.525658
369.998425	16717.314336	29.530676
370.203045	16746.456962	29.535693
370.620450	16769.489665	29.540711
371.168678	16797.246013	29.545728
371.482829	16828.086746	29.550746
371.752523	16856.843553	29.555764
372.368135	16879.596013	29.560781
372.728486	16915.252660	29.565799
373.065237	16945.651037	29.570816
373.140496	16974.861525	29.575834
373.422184	17010.041031	29.580852
373.935082	17039.524601	29.585869
374.274425	17073.308672	29.590887
374.385612	17097.472802	29.595904
374.948215	17134.829224	29.600922
375.460497	17166.625107	29.605940
376.590707	17183.517749	29.610957
376.361275	17223.628686	29.615975
376.731528	17242.282120	29.620992
377.306224	17277.950288	29.626010
377.842205	17297.907713	29.631028
379.302136	17312.336023	29.636045
379.443857	17324.259545	29.641063
379.923700	17338.088726	29.646080
379.953945	17360.762326	29.651098
380.860393	17380.478967	29.656116
382.165608	17372.480515	29.661133
382.485187	17383.296164	29.666151
382.881720	17383.888272	29.671168
383.281261	17391.529778	29.676186
383.081501	17391.769363	29.681204
383.808302	17396.931004	29.686221
383.709626	17408.494027	29.691239
384.210002	17407.831820	29.696256
384.358841	17419.444755	29.701274
384.853756	17441.272266	29.706292
384.929061	17442.991451	29.711309
384.977492	17454.563185	29.716327
385.307661	17486.179484	29.721344
385.372469	17503.111930	29.726362
385.407740	17526.012358	29.731380
386.292978	17555.012346	29.736397
386.429911	17574.807925	29.741415
386.668286	17610.570131	29.746432
387.148925	17630.981878	29.751450
387.231360	17680.331444	29.756468
387.744450	17710.150822	29.761485
388.276549	17734.932480	29.766503
388.101312	17757.423750	29.771520
388.528436	17795.576404	29.776538
388.809093	17835.861889	29.781556
389.233932	17865.954253	29.786573
389.811116	17905.075568	29.791591
390.453284	17929.227566	29.796608
390.763118	17954.637930	29.801626
390.942678	17996.045010	29.806644
391.539950	18021.341224	29.811661
392.080033	18050.733667	29.816679
392.371857	18083.045497	29.821696
392.825441	18105.774094	29.826714
392.792142	18136.904753	29.831732
393.594864	18160.116032	29.836749
393.773759	18201.788983	29.841767
393.789586	18229.532361	29.846784
394.137144	18256.383924	29.851802
394.502958	18293.409978	29.856820
395.342393	18328.227090	29.861837
395.554692	18360.059007	29.866855
395.983471	18381.660974	29.871872
396.512541	18415.117779	29.876890
396.699541	18440.800602	29.881908
397.395485	18473.732452	29.886925
397.499204	18502.795516	29.891943
398.200601	18534.463132	29.896960
398.723731	18563.966390	29.901978
398.741175	18597.686367	29.906996
399.776688	18620.937769	29.912013
400.273450	18650.931712	29.917031
400.440770	18663.515412	29.922048
401.192845	18688.933702	29.927066
400.919419	18729.819023	29.932084
401.857058	18752.460386	29.937101
402.501228	18781.686114	29.942119
402.868987	18798.793643	29.947136
403.020075	18818.146060	29.952154
403.235451	18857.976334	29.957172
404.111412	18879.572416	29.962189
403.976666	18913.569336	29.967207
404.579345	18933.274842	29.972224
405.060248	18953.896425	29.977242
405.320362	18984.136205	29.982260
405.897484	19003.352988	29.987277
406.363462	19033.055386	29.992295
407.209689	19058.680621	29.997312
407.051199	19077.626623	30.002330
407.641135	19118.555246	30.007348
408.059972	19128.187655	30.012365
408.540837	19158.323846	30.017383
408.777338	19181.188582	30.022400
409.506560	19202.908951	30.027418
409.876896	19235.235748	30.032436
410.074769	19253.121930	30.037453
411.077980	19289.273577	30.042471
410.824154	19312.347474	30.047488
411.340088	19339.395443	30.052506
411.665152	19363.756541	30.057524
412.063393	19385.256980	30.062541
412.721941	19412.781950	30.067559
413.028156	19437.367196	30.072576
413.257664	19460.094358	30.077594
413.565827	19488.710096	30.082612
413.938647	19505.375216	30.087629
414.478181	19543.494853	30.092647
414.823700	19571.289902	30.097664
415.409915	19610.716505	30.102682
415.430014	19630.993570	30.107700
415.884909	19665.563376	30.112717
416.347824	19706.582507	30.117735
416.674434	19728.941067	30.122752
417.119595	19767.991923	30.127770
417.323079	19800.800519	30.132788
417.840325	19840.680575	30.137805
418.510755	19875.754219	30.142823
418.749571	19900.868610	30.147840
419.302554	19923.040521	30.152858
419.978987	19951.473247	30.157876
420.473594	19968.536786	30.162893
421.387428	19994.007418	30.167911
421.663467	20015.148500	30.172928
422.097613	20023.995547	30.177946
422.269503	20049.752343	30.182964
422.495870	20076.429430	30.187981
422.852132	20094.121141	30.192999
422.877606	20129.352509	30.198016
423.509203	20148.959978	30.203034
423.459302	20179.875355	30.208052
423.703028	20210.176450	30.213069
424.441671	20249.795426	30.218087
424.610980	20286.502055	30.223104
425.216313	20316.026764	30.228122
425.686736	20358.998368	30.233140
426.067171	20398.180603	30.238157
426.445420	20426.742578	30.243175
426.763187	20461.467821	30.248192
427.381637	20497.757428	30.253210
427.135993	20530.769849	30.258228
427.861220	20567.049280	30.263245
429.136461	20594.157688	30.268263
429.591540	20624.357021	30.273280
429.934962	20666.470851	30.278298
429.974052	20699.534000	30.283316
430.813624	20729.901091	30.288333
431.504449	20756.835344	30.293351
431.874166	20791.559402	30.298368
432.368440	20802.501400	30.303386
432.880045	20850.964499	30.308404
433.356316	20873.496934	30.313421
433.734725	20897.700003	30.318439
433.822372	20926.396402	30.323456
434.527307	20955.976071	30.328474
434.635860	20992.124837	30.333492
434.903513	21013.584216	30.338509
435.714478	21051.304397	30.343527
435.640020	21098.128138	30.348544
436.452274	21120.210498	30.353562
436.658112	21162.706955	30.358580
437.211977	21193.289838	30.363597
438.150357	21207.530587	30.368615
439.101736	21228.555207	30.373632
439.635165	21244.975666	30.378650
440.439953	21269.384504	30.383668
440.963277	21283.531966	30.388685
441.224068	21292.172798	30.393703
441.499121	21313.846177	30.398720
442.133604	21323.736747	30.403738
442.281666	21349.423139	30.408756
442.269929	21378.331539	30.413773
443.047261	21394.486692	30.418791
443.429923	21425.001813	30.423808
443.526289	21440.340531	30.428826
443.892525	21474.150171	30.433844
443.922142	21494.465590	30.438861
444.366631	21531.567677	30.443879
444.688482	21565.043188	30.448896
445.199311	21596.277880	30.453914
445.713769	21641.678040	30.458932
445.751386	21678.338267	30.463949
446.547911	21705.617522	30.468967
446.694634	21744.055335	30.473984
447.172309	21774.992184	30.479002
447.915184	21812.332679	30.484020
448.403458	21851.210373	30.489037
448.858176	21877.727988	30.494055
449.346253	21910.577948	30.499072
450.348172	21941.168065	30.504090
450.801217	21962.902909	30.509108
451.193205	21982.726437	30.514125
451.494903	22001.906909	30.519143
452.070667	22030.124538	30.524160
452.887938	22042.741919	30.529178
453.328924	22063.758433	30.534196
453.636493	22086.842966	30.539213
454.149436	22101.902514	30.544231
454.328811	22126.889996	30.549248
454.719591	22143.788355	30.554266
454.957175	22168.678368	30.559284
455.635552	22193.266001	30.564301
456.931760	22200.880388	30.569319
456.859721	22225.932410	30.574336
457.660965	22242.368879	30.579354
457.917510	22262.118994	30.584372
458.285478	22274.958120	30.589389
458.880217	22301.467145	30.594407
459.062268	22331.610507	30.599424
459.412054	22336.686846	30.604442
459.622852	22367.817821	30.609460
459.994901	22397.565221	30.614477
460.493244	22422.579246	30.619495
460.674680	22456.311921	30.624512
461.168439	22484.928410	30.629530
461.359149	22517.680343	30.634548
461.805529	22552.370298	30.639565
462.063560	22587.582498	30.644583
462.720335	22635.932609	30.649600
462.961914	22676.632229	30.654618
463.526759	22704.264875	30.659636
463.477865	22755.644421	30.664653
464.408478	22784.180696	30.669671
464.684173	22835.061280	30.674688
465.211930	22873.467245	30.679706
465.699948	22913.162201	30.684724
465.851671	22958.128985	30.689741
466.372755	23005.603841	30.694759
467.054151	23052.516746	30.699776
467.669457	23093.007386	30.704794
468.127542	23131.096112	30.709812
468.360347	23178.862700	30.714829
469.572998	23216.012656	30.719847
469.505181	23256.180287	30.724864
470.006703	23292.455333	30.729882
471.556185	23330.374536	30.734900
471.365762	23363.597934	30.739917
471.956415	23403.720224	30.744935
472.369502	23433.494385	30.749952
473.329489	23477.710932	30.754970
473.811661	23500.435022	30.759988
474.582487	23540.573773	30.765005
474.994353	23550.733929	30.770023
475.470810	23575.898157	30.775040
476.688531	23598.931230	30.780058
477.364403	23620.544740	30.785076
477.678412	23631.686992	30.790093
477.780391	23651.690042	30.795111
478.351600	23675.683250	30.800128
478.781254	23694.630593	30.805146
479.357166	23712.436701	30.810164
479.286718	23729.793684	30.815181
479.718323	23764.127868	30.820199
480.209546	23791.918832	30.825216
480.253712	23818.073259	30.830234
480.757734	23853.476898	30.835252
480.587297	23892.132549	30.840269
481.070702	23922.067113	30.845287
481.409069	23971.702288	30.850304
481.718148	24009.000716	30.855322
482.658127	24035.698446	30.860340
483.283087	24077.339688	30.865357
484.757281	24090.797682	30.870375
485.102858	24102.030073	30.875392
485.000637	24133.225183	30.880410
485.387774	24162.037629	30.885428
485.893362	24202.478097	30.890445
486.294526	24220.381377	30.895463
486.779578	24259.264296	30.900480
487.283279	24293.847259	30.905498
487.841658	24328.345939	30.910516
488.284309	24356.909890	30.915533
488.598396	24399.642889	30.920551
488.682217	24429.621463	30.925568
489.158957	24472.285061	30.930586
490.161305	24507.157289	30.935604
489.998032	24547.538279	30.940621
490.667709	24583.568322	30.945639
490.766485	24634.847571	30.950656
491.429134	24673.798440	30.955674
491.845693	24722.639699	30.960692
492.337827	24768.600280	30.965709
493.291179	24808.296087	30.970727
493.620839	24845.611832	30.975744
493.851981	24897.414621	30.980762
495.162297	24935.399402	30.985780
495.497864	24971.406323	30.990797
495.619590	25013.001467	30.995815
496.078860	25057.647046	31.000832
496.650802	25108.139735	31.005850
497.253367	25143.884216	31.010868
497.419846	25193.037295	31.015885
497.677766	25242.504879	31.020903
498.793671	25288.830877	31.025920
499.323041	25340.063854	31.030938
499.988607	25372.171465	31.035956
500.859732	25414.200584	31.040973
501.723023	25438.693933	31.045991
502.193289	25470.377089	31.051008
502.511259	25508.605920	31.056026
503.376414	25545.883842	31.061044
503.545311	25591.498488	31.066061
504.327151	25611.144869	31.071079
504.701414	25651.216886	31.076096
504.762584	25683.659236	31.081114
505.251405	25718.961108	31.086132
505.431259	25758.949849	31.091149
506.057559	25804.708644	31.096167
506.707793	25842.671512	31.101184
507.130684	25881.921165	31.106202
508.118944	25918.377998	31.111220
508.236745	25969.341700	31.116237
509.003289	25984.478469	31.121255
509.489279	26028.035033	31.126272
509.658160	26066.408211	31.131290
510.505004	26096.662320	31.136308
511.175685	26134.262322	31.141325
511.897280	26173.320685	31.146343
512.455890	26192.079683	31.151360
512.972537	26230.481193	31.156378
513.396279	26254.557333	31.161396
514.045024	26291.908248	31.166413
514.599800	26318.346681	31.171431
515.067578	26342.858467	31.176448
515.407557	26381.471047	31.181466
516.035397	26411.146687	31.186484
516.599763	26450.343823	31.191501
516.991616	26477.787425	31.196519
517.449124	26496.278047	31.201536
517.792253	26535.459230	31.206554
518.158540	26564.537493	31.211572
518.487096	26598.153131	31.216589
518.827869	26630.262754	31.221607
519.468214	26661.093382	31.226624
519.524628	26700.060397	31.231642
520.330848	26740.079973	31.236660
520.713644	26772.796328	31.241677
521.011408	26823.430805	31.246695
521.696313	26859.873369	31.251712
521.872205	26916.392113	31.256730
522.548241	26955.364281	31.261748
522.883172	26997.246335	31.266765
523.295614	27043.110754	31.271783
524.240380	27087.653651	31.276800
524.848492	27137.343133	31.281818
525.314025	27174.326030	31.286836
526.029135	27222.393731	31.291853
526.371772	27267.732306	31.296871
526.799542	27302.458671	31.301888
527.306658	27358.933406	31.306906
528.034428	27397.127298	31.311924
528.483448	27442.506586	31.316941
528.853697	27493.491708	31.321959
529.629403	27530.547054	31.326976
530.019381	27583.867851	31.331994
530.509240	27629.443449	31.337012
531.272939	27674.237036	31.342029
532.020348	27720.758722	31.347047
532.586226	27757.461605	31.352064
532.736958	27812.033759	31.357082
533.282792	27858.397528	31.362100
534.175485	27899.821709	31.367117
535.094188	27947.739346	31.372135
535.883947	27983.099451	31.377152
535.683001	28022.677909	31.382170
536.640184	28064.585384	31.387188
537.594011	28101.430750	31.392205
538.179605	28137.309585	31.397223
538.608220	28179.615608	31.402240
538.866992	28210.786100	31.407258
539.522932	28247.855080	31.412276
539.887628	28289.419136	31.417293
540.399961	28325.031603	31.422311
541.319150	28362.609700	31.427328
541.407219	28407.080282	31.432346
541.731659	28444.081134	31.437364
542.370101	28483.163218	31.442381
543.284382	28506.786434	31.447399
545.933180	28507.391725	31.452416
547.128053	28533.524823	31.457434
547.574669	28549.086243	31.462452
548.095619	28551.862094	31.467469
548.329247	28548.475810	31.472487
548.807992	28558.508002	31.477504
549.258556	28588.258674	31.482522
549.700843	28583.127007	31.487540
549.996552	28598.534979	31.492557
549.615268	28623.270192	31.497575
550.177434	28639.426797	31.502592
550.319419	28667.803474	31.507610
550.282362	28700.632540	31.512628
550.341489	28739.128988	31.517645
550.999132	28797.733319	31.522663
551.538337	28837.103322	31.527680
551.939709	28887.663601	31.532698
552.233739	28923.797796	31.537716
552.656200	28960.474608	31.542733
552.572835	29030.837810	31.547751
553.706493	29068.036179	31.552768
554.066474	29118.230544	31.557786
554.631514	29165.959592	31.562804
555.304020	29216.946217	31.567821
555.627709	29266.002522	31.572839
556.365567	29315.746653	31.577856
556.861211	29374.757107	31.582874
557.189984	29420.936987	31.587892
557.913893	29473.945260	31.592909
558.219416	29535.337156	31.597927
558.822850	29580.678199	31.602944
559.501211	29632.417139	31.607962
560.314146	29696.006073	31.612980
561.036159	29742.112815	31.617997
561.182558	29802.620057	31.623015
561.847287	29845.417414	31.628032
562.267361	29905.774897	31.633050
562.696597	29958.956716	31.638068
563.508388	30016.718796	31.643085
563.939814	30082.030761	31.648103
564.896176	30132.943867	31.653120
565.582257	30199.082555	31.658138
565.971291	30244.591184	31.663156
566.567273	30300.813689	31.668173
567.020473	30350.029412	31.673191
568.156507	30400.656042	31.678208
568.954632	30454.502332	31.683226
569.804137	30500.338079	31.688244
570.399381	30538.128634	31.693261
571.170254	30570.190144	31.698279
571.996272	30610.075169	31.703296
572.562233	30655.215813	31.708314
572.997666	30691.552348	31.713332
573.649224	30728.196653	31.718349
573.958128	30767.878026	31.723367
574.456674	30810.033200	31.728384
575.140677	30853.177325	31.733402
575.750602	30889.291082	31.738420
576.439709	30938.528378	31.743437
576.880789	30978.379220	31.748455
577.541981	31022.791527	31.753472
578.009862	31081.710053	31.758490
578.329415	31119.829055	31.763508
578.973737	31152.549636	31.768525
579.563952	31207.960046	31.773543
580.155126	31251.808493	31.778560
580.524913	31289.572307	31.783578
580.828229	31336.809807	31.788596
581.689639	31388.309730	31.793613
581.999526	31436.128012	31.798631
582.827648	31484.763387	31.803648
583.626518	31542.392676	31.808666
583.456082	31600.173021	31.813684
584.233443	31639.732567	31.818701
585.203016	31698.732787	31.823719
585.792950	31738.669387	31.828736
586.451738	31791.169061	31.833754
587.060483	31834.219480	31.838772
588.390033	31868.484469	31.843789
589.042179	31908.348495	31.848807
589.865244	31939.936204	31.853824
591.114717	31972.115035	31.858842
591.371008	32005.396783	31.863860
591.912443	32023.822447	31.868877
592.085398	32062.143011	31.873895
592.715385	32094.045489	31.878912
593.277207	32121.868468	31.883930
593.565030	32156.403573	31.888948
594.322640	32180.668621	31.893965
594.548895	32218.721985	31.898983
595.162960	32252.258198	31.904000
595.280947	32296.979061	31.909018
595.472085	32342.030009	31.914036
596.121031	32381.269583	31.919053
596.126782	32434.586908	31.924071
596.945838	32478.971437	31.929088
597.663541	32543.848325	31.934106
598.071947	32602.843645	31.939124
598.888808	32651.420287	31.944141
599.143650	32706.058735	31.949159
599.839955	32757.796381	31.954176
600.587005	32819.097671	31.959194
600.813153	32879.462396	31.964212
601.855056	32927.536824	31.969229
602.492800	32992.870094	31.974247
603.093269	33039.717492	31.979264
604.043159	33092.832621	31.984282
604.542834	33145.543819	31.989300
605.189983	33191.872206	31.994317
605.824506	33247.805883	31.999335
606.450815	33298.733896	32.004352
606.986179	33344.182286	32.009370
607.642530	33407.927110	32.014388
608.104275	33448.190405	32.019405
608.893088	33509.430320	32.024423
609.410797	33559.117765	32.029440
610.515109	33611.318748	32.034458
610.409339	33666.433104	32.039476
611.325573	33714.257052	32.044493
611.792644	33773.044228	32.049511
612.671305	33833.853836	32.054528
613.420499	33880.894920	32.059546
613.757733	33940.594217	32.064564
614.583815	33994.236690	32.069581
614.956370	34045.686515	32.074599
615.562552	34098.984150	32.079616
616.630370	34154.353330	32.084634
617.009110	34214.881493	32.089652
617.728557	34265.708843	32.094669
618.305130	34326.143305	32.099687
619.067609	34387.826127	32.104704
619.516598	34433.505284	32.109722
619.872636	34488.423453	32.114740
620.719873	34538.188365	32.119757
621.232057	34591.704200	32.124775
621.720908	34656.939380	32.129792
622.702401	34706.000959	32.134810
622.938907	34768.651927	32.139828
623.792093	34823.272287	32.144845
624.319381	34877.684298	32.149863
624.851974	34932.854331	32.154880
625.889390	34986.099726	32.159898
626.466930	35037.576965	32.164916
627.180384	35097.891169	32.169933
627.475027	35151.271577	32.174951
628.078180	35205.350167	32.179968
628.800114	35253.435478	32.184986
629.169572	35314.998837	32.190004
630.061290	35363.797723	32.195021
630.866685	35422.511542	32.200039
631.500786	35472.609005	32.205056
632.904613	35508.398512	32.210074
633.675450	35553.701207	32.215092
634.728780	35591.726770	32.220109
635.624741	35620.514023	32.225127
636.333149	35637.171790	32.230144
636.994411	35665.148387	32.235162
637.195393	35695.106159	32.240180
637.750572	35721.689359	32.245197
638.407347	35755.433179	32.250215
638.762980	35780.144347	32.255232
639.480938	35819.967630	32.260250
640.195189	35858.204530	32.265268
640.619952	35885.111734	32.270285
641.052781	35925.479109	32.275303
641.442207	35964.525511	32.280320
642.247320	36012.966328	32.285338
642.437135	36050.475883	32.290356
643.070158	36100.448541	32.295373
643.737782	36140.191741	32.300391
644.395710	36183.249749	32.305408
644.858099	36239.350945	32.310426
645.667959	36296.125339	32.315444
646.267784	36337.251550	32.320461
646.793911	36395.189548	32.325479
647.077639	36455.884342	32.330496
647.870854	36509.728012	32.335514
648.498043	36574.195119	32.340532
649.282104	36627.275421	32.345549
649.557102	36688.712037	32.350567
649.972108	36748.470378	32.355584
650.591555	36805.490759	32.360602
651.105554	36869.698162	32.365620
651.823726	36936.422212	32.370637
652.132964	37008.300300	32.375655
653.012814	37083.200824	32.380672
653.746996	37145.370320	32.385690
654.026790	37224.677197	32.390708
654.878063	37291.988670	32.395725
655.671824	37361.535109	32.400743
656.002334	37436.775320	32.405760
656.891411	37506.768996	32.410778
657.509784	37578.208827	32.415796
658.769537	37641.341303	32.420813
659.152587	37715.518309	32.425831
660.143820	37790.960432	32.430848
661.138081	37837.839359	32.435866
661.306829	37914.092882	32.440884
662.514088	37967.749305	32.445901
663.347884	38025.915738	32.450919
663.721349	38081.112380	32.455936
664.701606	38142.740585	32.460954
665.042307	38210.286189	32.465972
665.943685	38268.632466	32.470989
666.521604	38327.971468	32.476007
667.231252	38393.424020	32.481024
668.197241	38441.807363	32.486042
669.149406	38494.474065	32.491060
670.038808	38548.288922	32.496077
671.415181	38566.432240	32.501095
672.077265	38606.952376	32.506112
673.487535	38631.319282	32.511130
674.138069	38670.292038	32.516148
674.947550	38691.837320	32.521165
675.406826	38727.728698	32.526183
675.929747	38768.441543	32.531200
676.208877	38799.181964	32.536218
676.960308	38838.619920	32.541236
677.529327	38870.143724	32.546253
677.709218	38917.284582	32.551271
678.245605	38962.390707	32.556288
679.060630	39001.838034	32.561306
679.342973	39041.602336	32.566324
679.767933	39084.594945	32.571341
680.416198	39131.366140	32.576359
680.843780	39175.338713	32.581376
681.233568	39223.269662	32.586394
681.501995	39277.790100	32.591412
681.913553	39344.809673	32.596429
682.757953	39399.316641	32.601447
683.576319	39458.071146	32.606464
684.712127	39513.576485	32.611482
685.445385	39565.837209	32.616500
686.077984	39612.023756	32.621517
687.016325	39666.997397	32.626535
687.314764	39719.206024	32.631552
688.123126	39780.422993	32.636570
688.743067	39843.364306	32.641588
689.088782	39897.115388	32.646605
689.985280	39956.447218	32.651623
690.832818	40034.993059	32.656640
691.389743	40095.510142	32.661658
692.128300	40149.023619	32.666676
692.400972	40209.243766	32.671693
693.288802	40258.705805	32.676711
693.840384	40337.001575	32.681728
695.253722	40401.028913	32.686746
695.933375	40469.426844	32.691764
696.636197	40532.673463	32.696781
697.145128	40583.042670	32.701799
697.242185	40652.613313	32.706816
698.357025	40713.759908	32.711834
698.833265	40785.548689	32.716852
699.385611	40856.775643	32.721869
700.216362	40922.868397	32.726887
700.940512	41006.553344	32.731904
701.745997	41063.562350	32.736922
702.535462	41135.031573	32.741940
702.975703	41197.334389	32.746957
704.117249	41268.414046	32.751975
704.975811	41346.279862	32.756992
705.382939	41399.316750	32.762010
706.228185	41463.928958	32.767028
706.683891	41540.365596	32.772045
707.617644	41607.943300	32.777063
707.719317	41674.518646	32.782080
708.632076	41747.627712	32.787098
709.093942	41819.264009	32.792116
709.802914	41900.557717	32.797133
710.946476	41969.191709	32.802151
710.832208	42055.591636	32.807168
711.853678	42126.888838	32.812186
712.857203	42201.054158	32.817204
713.595819	42272.212447	32.822221
714.405685	42348.887707	32.827239
715.521233	42416.547123	32.832256
716.453564	42478.479712	32.837274
717.462182	42542.936847	32.842292
718.482050	42587.051794	32.847309
719.627031	42650.596218	32.852327
720.027906	42709.127203	32.857344
721.038317	42770.251528	32.862362
721.469004	42820.650711	32.867380
721.984116	42880.891063	32.872397
722.841075	42933.817357	32.877415
723.380050	42990.316267	32.882432
724.208761	43054.271611	32.887450
724.760397	43109.054792	32.892468
724.957455	43177.523650	32.897485
726.177543	43221.792127	32.902503
726.505781	43288.975909	32.907520
727.958284	43326.655698	32.912538
728.823649	43369.474334	32.917556
729.623062	43409.052241	32.922573
730.733379	43452.389511	32.927591
731.207540	43491.398342	32.932608
731.714341	43546.436265	32.937626
732.309973	43594.363726	32.942644
732.716114	43638.772396	32.947661
733.476927	43687.578838	32.952679
733.746346	43749.074229	32.957696
734.564851	43802.856164	32.962714
735.444931	43860.714712	32.967732
736.097455	43919.310931	32.972749
736.699081	43966.865078	32.977767
738.299170	44021.677066	32.982784
739.466490	44071.679795	32.987802
740.381871	44107.464731	32.992820
741.068330	44154.651862	32.997837
741.879722	44196.335628	33.002855
742.174985	44247.144984	33.007872
742.760214	44299.427392	33.012890
743.398798	44351.416977	33.017908
743.697095	44410.752771	33.022925
744.561484	44471.113864	33.027943
745.133174	44532.039364	33.032960
745.912373	44595.880362	33.037978
747.012827	44646.261668	33.042996
748.138712	44703.293474	33.048013
748.630725	44766.116995	33.053031
749.258074	44814.870787	33.058048
749.852291	44878.829948	33.063066
750.754459	44931.918444	33.068084
751.194068	45007.737032	33.073101
751.890233	45060.908506	33.078119
752.573861	45126.714164	33.083136
753.228024	45202.537967	33.088154
753.863803	45259.780328	33.093172
754.341832	45336.871819	33.098189
755.276591	45398.628753	33.103207
755.766984	45475.889590	33.108224
756.022992	45546.039181	33.113242
757.210491	45626.709089	33.118260
758.074969	45701.609923	33.123277
758.758095	45781.340464	33.128295
759.701829	45853.085581	33.133312
760.183656	45930.336666	33.138330
761.219702	45997.703096	33.143348
761.955384	46084.777101	33.148365
762.812841	46151.450650	33.153383
763.412250	46226.141465	33.158400
764.462289	46294.309990	33.163418
765.388375	46359.354051	33.168436
766.481822	46434.708783	33.173453
767.003189	46508.874983	33.178471
767.598796	46573.604204	33.183488
768.218033	46652.873337	33.188506
769.118612	46732.921333	33.193524
769.588597	46800.865389	33.198541
770.203531	46871.589519	33.203559
771.224962	46945.982964	33.208576
772.082819	47027.822604	33.213594
773.231003	47095.060996	33.218612
773.575437	47171.230659	33.223629
774.451300	47238.967351	33.228647
775.320427	47313.316128	33.233664
776.120751	47378.939411	33.238682
777.616682	47434.813484	33.243700
778.752514	47477.041192	33.248717
779.676739	47533.934458	33.253735
780.213648	47576.236606	33.258752
781.082832	47627.350176	33.263770
781.796757	47668.403975	33.268788
782.433984	47719.085717	33.273805
782.921845	47774.092698	33.278823
783.756692	47842.406949	33.283840
784.143201	47897.556532	33.288858
784.717442	47962.641006	33.293876
785.219984	48026.496861	33.298893
786.077106	48100.065623	33.303911
786.945146	48170.260954	33.308928
787.629792	48233.007229	33.313946
788.329440	48302.666132	33.318964
788.946924	48376.140236	33.323981
789.866610	48451.655271	33.328999
790.922532	48518.659195	33.334016
791.061895	48604.178190	33.339034
792.109745	48673.176678	33.344052
793.323022	48748.678629	33.349069
793.838282	48824.055405	33.354087
794.725812	48908.136820	33.359104
795.381875	48990.337609	33.364122
796.527693	49059.163850	33.369140
797.134937	49136.437985	33.374157
798.078829	49201.822751	33.379175
798.755697	49283.641756	33.384192
799.800339	49360.000780	33.389210
800.530976	49426.146958	33.394228
801.037928	49513.889763	33.399245
802.038451	49586.232585	33.404263
802.536035	49662.247555	33.409280
803.675809	49737.669316	33.414298
804.186291	49821.376230	33.419316
805.435473	49896.477794	33.424333
807.196430	49955.005732	33.429351
808.213016	50008.164267	33.434368
808.759097	50074.353699	33.439386
810.071407	50135.716804	33.444404
810.490488	50206.532399	33.449421
811.384213	50265.936384	33.454439
811.778544	50324.019997	33.459456
812.314954	50397.981412	33.464474
813.071259	50475.559533	33.469492
813.958935	50547.087784	33.474509
814.606202	50613.111166	33.479527
815.373496	50689.334303	33.484544
815.755636	50770.957730	33.489562
816.765420	50842.107243	33.494580
817.384905	50934.526357	33.499597
818.662411	51005.096889	33.504615
819.720449	51073.348084	33.509632
820.416072	51149.583898	33.514650
821.389789	51207.497291	33.519668
822.127530	51289.225375	33.524685
823.042566	51355.057343	33.529703
823.952533	51429.318241	33.534720
824.616880	51505.895444	33.539738
826.023428	51564.451014	33.544756
826.634462	51645.504074	33.549773
826.946096	51725.243637	33.554791
827.979697	51793.095809	33.559808
829.055733	51861.087104	33.564826
829.767755	51935.076720	33.569844
830.286223	52008.970152	33.574861
830.959885	52083.706524	33.579879
831.896630	52147.847930	33.584896
832.404121	52215.378274	33.589914
833.696124	52284.204058	33.594932
834.421516	52347.372838	33.599949
834.586745	52411.293381	33.604967
835.748030	52475.856323	33.609984
836.575089	52552.069958	33.615002
837.185817	52622.217692	33.620020
838.163424	52696.567028	33.625037
839.185100	52766.929644	33.630055
840.090574	52840.892025	33.635072
841.288762	52910.708729	33.640090
841.980550	52976.320608	33.645108
842.628732	53050.159184	33.650125
843.422468	53126.538076	33.655143
844.096893	53199.417547	33.660160
844.698957	53274.921888	33.665178
845.966599	53355.720492	33.670196
846.961100	53429.430421	33.675213
847.634275	53502.260407	33.680231
848.471764	53575.324484	33.685248
849.429701	53654.786526	33.690266
850.143967	53727.452617	33.695284
851.136984	53804.606345	33.700301
851.871168	53890.685072	33.705319
853.213983	53960.767155	33.710336
853.681540	54051.184672	33.715354
854.600831	54106.671139	33.720372
855.698474	54193.580320	33.725389
856.302826	54272.745123	33.730407
857.278707	54349.460343	33.735424
857.851049	54420.954663	33.740442
858.842374	54491.700542	33.745460
859.940175	54578.345338	33.750477
860.548762	54667.528263	33.755495
861.663944	54731.883118	33.760512
862.479218	54821.167342	33.765530
863.448891	54884.602360	33.770548
864.194984	54980.453999	33.775565
864.937077	55059.410152	33.780583
866.269834	55134.768749	33.785600
867.116375	55216.088605	33.790618
867.987296	55287.298593	33.795636
868.988009	55365.139692	33.800653
869.367951	55441.090568	33.805671
870.016781	55516.835293	33.810688
870.952036	55594.655693	33.815706
871.984448	55675.682399	33.820724
873.362155	55751.839675	33.825741
874.605946	55819.759378	33.830759
876.379737	55866.364686	33.835776
877.068089	55938.256883	33.840794
877.948045	56001.367121	33.845812
879.198884	56069.849682	33.850829
879.660420	56124.355277	33.855847
880.334159	56180.840450	33.860864
881.127948	56258.299003	33.865882
881.693786	56323.629700	33.870900
882.412577	56398.663869	33.875917
883.023157	56478.860312	33.880935
883.641149	56543.810103	33.885952
884.626631	56611.487487	33.890970
885.661566	56694.061470	33.895988
886.178377	56779.323827	33.901005
886.880141	56861.393322	33.906023
887.942134	56934.964441	33.911040
888.451897	57018.020005	33.916058
889.769694	57095.722475	33.921076
890.758440	57170.679073	33.926093
891.455394	57252.098787	33.931111
892.997416	57309.951410	33.936128
893.563094	57377.822890	33.941146
894.425080	57440.958719	33.946164
895.645927	57504.374285	33.951181
896.402399	57578.874661	33.956199
897.290542	57635.671661	33.961216
898.578354	57683.716905	33.966234
899.583949	57747.400794	33.971252
900.613796	57800.809106	33.976269
901.224959	57879.105118	33.981287
902.150481	57936.770417	33.986304
902.835973	58003.409840	33.991322
903.266848	58071.259959	33.996340
904.377603	58141.112025	34.001357
904.879573	58226.533732	34.006375
905.424933	58297.752743	34.011392
906.476414	58379.247670	34.016410
907.170336	58465.134016	34.021428
908.184186	58561.357080	34.026445
908.726303	58650.248767	34.031463
909.374004	58735.402749	34.036480
910.287726	58827.484145	34.041498
911.132666	58919.285451	34.046516
912.177894	59012.062289	34.051533
912.853234	59119.695064	34.056551
913.770351	59208.030407	34.061568
915.279600	59306.027492	34.066586
916.585708	59392.024372	34.071604
918.144106	59465.209481	34.076621
919.287081	59542.092584	34.081639
920.546787	59617.445015	34.086656
921.595130	59690.355750	34.091674
922.601066	59767.349511	34.096692
923.639072	59823.590320	34.101709
924.650394	59894.557935	34.106727
925.672344	59958.453979	34.111744
926.626504	60027.804183	34.116762
927.094320	60094.900997	34.121780
928.095622	60164.902532	34.126797
928.673799	60240.635156	34.131815
929.573669	60311.222567	34.136832
930.349964	60393.602613	34.141850
930.869311	60479.206772	34.146868
932.123875	60561.133153	34.151885
932.455870	60664.104230	34.156903
933.031537	60743.168248	34.161920
934.200173	60834.198466	34.166938
935.105697	60928.320949	34.171956
935.866514	61009.490152	34.176973
936.722230	61111.330832	34.181991
937.788728	61211.252816	34.187008
938.673334	61303.436719	34.192026
939.440245	61397.791466	34.197044
940.220527	61495.904490	34.202061
941.526660	61598.955730	34.207079
942.333143	61691.931838	34.212096
943.617343	61791.201951	34.217114
944.611312	61876.047125	34.222132
945.470320	61978.258023	34.227149
946.414503	62075.499611	34.232167
947.640343	62167.836196	34.237184
948.527036	62254.224932	34.242202
949.469725	62344.605925	34.247220
950.959250	62421.634029	34.252237
951.777154	62518.916009	34.257255
952.563805	62592.369867	34.262272
953.808489	62678.887937	34.267290
954.417405	62766.334542	34.272308
955.725774	62829.459162	34.277325
956.390067	62913.555266	34.282343
958.010281	62972.447365	34.287360
959.030934	63027.704355	34.292378
960.207982	63105.245345	34.297396
961.020896	63170.062201	34.302413
962.211630	63230.135914	34.307431
962.887822	63297.354617	34.312448
964.158970	63373.609383	34.317466
964.704811	63442.507343	34.322484
965.920692	63504.742824	34.327501
967.567206	63568.759931	34.332519
968.576559	63625.241795	34.337536
969.514639	63682.944010	34.342554
970.056224	63749.646793	34.347572
971.001036	63814.951242	34.352589
971.566409	63888.215476	34.357607
972.729698	63956.486978	34.362624
973.554376	64033.541281	34.367642
973.736524	64119.754967	34.372660
975.093892	64196.847137	34.377677
975.538833	64291.902412	34.382695
976.548374	64379.026429	34.387712
977.753578	64455.465698	34.392730
978.598159	64546.889210	34.397748
979.893172	64619.446920	34.402765
980.456053	64714.934924	34.407783
981.496163	64811.431573	34.412800
982.526905	64903.903644	34.417818
983.270697	64995.458433	34.422836
984.527297	65090.346073	34.427853
985.162518	65181.671536	34.432871
986.389246	65264.149595	34.437888
987.856261	65351.123474	34.442906
988.498185	65441.094013	34.447924
989.846505	65527.042368	34.452941
990.475381	65627.227481	34.457959
991.859702	65714.671320	34.462976
992.788291	65805.769778	34.467994
993.490873	65908.078096	34.473012
994.224956	65992.502892	34.478029
995.550648	66091.137886	34.483047
996.489474	66181.134487	34.488064
997.860283	66263.897282	34.493082
998.609049	66351.644853	34.498100
999.886751	66450.079787	34.503117
1001.035635	66533.333854	34.508135
1001.823730	66621.937286	34.513152
1002.928412	66713.701706	34.518170
1003.453685	66802.916494	34.523188
1004.648799	66896.016063	34.528205
1005.579491	66984.326314	34.533223
1006.483005	67076.300634	34.538240
1008.027532	67168.403436	34.543258
1008.478703	67264.918811	34.548276
1009.329255	67373.902308	34.553293
1010.015814	67475.731910	34.558311
1010.757987	67573.330155	34.563328
1011.873064	67673.631268	34.568346
1012.846198	67786.700268	34.573364
1013.955429	67893.562635	34.578381
1014.867508	68001.576830	34.583399
1015.973039	68102.115377	34.588416
1017.062929	68205.157754	34.593434
1018.198012	68309.352207	34.598452
1018.945918	68422.193138	34.603469
1019.969738	68525.063464	34.608487
1020.901628	68624.883942	34.613504
1022.172893	68712.868548	34.618522
1022.818330	68810.239615	34.623540
1023.968586	68914.668435	34.628557
1024.613727	69010.925906	34.633575
1025.541169	69114.535419	34.638592
1026.694706	69218.882645	34.643610
1027.967083	69327.067937	34.648628
1028.568075	69421.839477	34.653645
1029.629147	69524.226762	34.658663
1030.752832	69634.614684	34.663680
1032.117157	69746.320672	34.668698
1033.163221	69853.840539	34.673716
1034.316048	69956.696487	34.678733
1035.769889	70044.986479	34.683751
1036.468665	70138.915914	34.688768
1038.132409	70250.925736	34.693786
1039.053012	70344.283151	34.698804
1040.711759	70442.699407	34.703821
1041.941679	70526.403388	34.708839
1042.810572	70616.211123	34.713856
1043.874992	70697.883439	34.718874
1044.917253	70798.100378	34.723892
1045.820880	70886.371224	34.728909
1046.897831	70988.141240	34.733927
1047.412595	71084.452019	34.738944
1048.491431	71187.628300	34.743962
1049.511343	71294.347641	34.748980
1050.670234	71392.155055	34.753997
1051.799433	71494.780119	34.759015
1052.731147	71599.146093	34.764032
1053.527496	71708.219604	34.769050
1054.816842	71830.540473	34.774068
1055.594125	71926.192892	34.779085
1057.014906	72036.665052	34.784103
1058.023417	72143.072989	34.789120
1058.936600	72245.025356	34.794138
1060.185914	72347.774373	34.799156
1061.295207	72458.094142	34.804173
1062.483850	72560.156835	34.809191
1063.647141	72660.931991	34.814208
1064.787145	72768.322555	34.819226
1065.930215	72877.764899	34.824244
1066.725523	72977.002679	34.829261
1068.039625	73078.363902	34.834279
1069.185347	73177.383235	34.839296
1070.726531	73267.754000	34.844314
1071.728626	73364.364563	34.849332
1072.789578	73467.058589	34.854349
1074.022508	73558.491595	34.859367
1074.631488	73658.229565	34.864384
1076.277470	73754.006696	34.869402
1077.450046	73838.103789	34.874420
1078.643847	73933.495976	34.879437
1080.081244	74022.264208	34.884455
1080.729386	74109.914306	34.889472
1081.938256	74214.754106	34.894490
1082.195192	74305.100309	34.899508
1083.590610	74399.652141	34.904525
1084.891738	74498.398876	34.909543
1085.707515	74589.963686	34.914560
1086.734759	74682.002551	34.919578
1088.027379	74781.904301	34.924596
1088.942454	74874.353948	34.929613
1090.074163	74969.848166	34.934631
1091.161709	75069.858911	34.939648
1092.332708	75160.306382	34.944666
1093.329100	75250.502671	34.949684
1093.997489	75335.582290	34.954701
1095.583184	75419.012049	34.959719
1096.189118	75517.250076	34.964736
1097.198123	75602.036850	34.969754
1098.283398	75693.348138	34.974772
1099.229759	75792.965540	34.979789
1099.936810	75885.881721	34.984807
1100.847312	75986.303439	34.989824
1102.056085	76088.591832	34.994842
1103.138827	76200.501918	34.999860
1104.999640	76278.951333	35.004877
1107.037792	76361.718227	35.009895
1107.579228	76454.902819	35.014912
1109.089155	76555.968050	35.019930
1109.885421	76650.228370	35.024948
1110.406604	76733.207191	35.029965
1111.905951	76826.674647	35.034983
1112.649313	76929.608695	35.040000
1113.799514	77035.266662	35.045018
1115.090199	77136.406183	35.050036
1116.149138	77230.298272	35.055053
1117.373707	77332.145530	35.060071
1117.753200	77447.907184	35.065088
1119.238300	77557.948751	35.070106
1120.684436	77662.106292	35.075124
1121.342379	77776.445203	35.080141
1122.667524	77871.108804	35.085159
1123.710512	77988.390963	35.090176
1124.702266	78089.491871	35.095194
1126.290474	78192.058482	35.100212
1127.509149	78304.969504	35.105229
1128.577519	78400.777031	35.110247
1129.438857	78509.095300	35.115264
1130.905493	78621.424294	35.120282
1131.562579	78730.243953	35.125300
1132.812718	78846.078681	35.130317
1134.644086	78952.613488	35.135335
1135.503191	79049.976059	35.140352
1136.751852	79157.641173	35.145370
1138.028634	79258.524654	35.150388
1139.209418	79364.389538	35.155405
1140.708906	79460.615054	35.160423
1141.708335	79577.505368	35.165440
1142.761218	79671.343406	35.170458
1144.038499	79776.472728	35.175476
1145.070502	79877.269880	35.180493
1146.164040	79978.412548	35.185511
1147.295908	80091.914494	35.190528
1148.639281	80193.487809	35.195546
1149.521195	80292.232116	35.200564
1150.509646	80403.654601	35.205581
1151.814743	80513.888023	35.210599
1152.647242	80621.192849	35.215616
1153.378990	80743.818194	35.220634
1154.382401	80846.004252	35.225652
1155.231455	80974.832967	35.230669
1156.942900	81093.316512	35.235687
1158.604223	81196.833086	35.240704
1159.936862	81304.987557	35.245722
1161.246671	81423.560357	35.250740
1161.973275	81529.022727	35.255757
1163.410824	81639.404675	35.260775
1164.258360	81750.284326	35.265792
1165.129482	81862.161651	35.270810
1166.736123	81968.540277	35.275828
1167.564528	82088.039689	35.280845
1168.960507	82202.522676	35.285863
1170.359946	82299.356371	35.290880
1171.478640	82388.758814	35.295898
1172.804153	82482.107732	35.300916
1173.969389	82589.406300	35.305933
1175.176512	82670.573003	35.310951
1176.060944	82779.588454	35.315968
1177.216898	82877.108207	35.320986
1178.502363	82970.642355	35.326004
1179.413135	83063.994399	35.331021
1180.861819	83161.837006	35.336039
1181.669306	83258.791468	35.341056
1182.474885	83372.902287	35.346074
1183.853750	83488.292739	35.351092
1184.603426	83593.809903	35.356109
1186.484907	83694.450514	35.361127
1187.506686	83800.255524	35.366144
1188.618147	83907.770175	35.371162
1190.150083	84013.002411	35.376180
1191.420829	84135.292501	35.381197
1192.296650	84238.460997	35.386215
1193.532783	84356.462021	35.391232
1194.869682	84457.025368	35.396250
1196.138872	84563.998429	35.401268
1197.403800	84686.823961	35.406285
1198.658694	84799.628784	35.411303
1199.688686	84913.229322	35.416320
1200.890450	85030.389506	35.421338
1202.092366	85141.670709	35.426356
1202.866853	85263.092512	35.431373
1204.081832	85388.272994	35.436391
1205.052123	85514.239716	35.441408
1206.163852	85635.192436	35.446426
1207.460918	85765.709113	35.451444
1208.681336	85890.827569	35.456461
1209.861530	86014.685669	35.461479
1211.204861	86148.212704	35.466496
1212.138221	86278.864334	35.471514
1213.617815	86398.837951	35.476532
1214.696189	86541.012147	35.481549
1216.014715	86663.140789	35.486567
1217.304748	86789.367405	35.491584
1218.532494	86925.336335	35.496602
1219.927469	87044.312027	35.501620
1221.150448	87175.226727	35.506637
1222.658261	87297.835447	35.511655
1224.087568	87423.485554	35.516672
1225.478703	87546.354249	35.521690
1226.938286	87661.824860	35.526708
1228.074061	87777.967272	35.531725
1229.033012	87901.918514	35.536743
1230.687172	88021.035247	35.541760
1231.859085	88148.832152	35.546778
1233.104005	88263.552847	35.551796
1234.018462	88378.464824	35.556813
1235.434931	88493.831362	35.561831
1236.895593	88612.891900	35.566848
1237.686170	88738.140139	35.571866
1239.248197	88858.846021	35.576884
1240.576211	88982.136065	35.581901
1241.848070	89097.730236	35.586919
1243.035373	89212.526949	35.591936
1244.160172	89337.054032	35.596954
1245.242197	89457.659646	35.601972
1246.128284	89582.541739	35.606989
1247.664918	89705.561528	35.612007
1249.364571	89810.598509	35.617024
1250.575625	89937.788728	35.622042
1251.991418	90054.758276	35.627060
1253.016195	90166.479007	35.632077
1254.360780	90267.149862	35.637095
1255.350997	90379.180929	35.642112
1256.543046	90488.101340	35.647130
1257.446196	90594.025465	35.652148
1258.753485	90712.991551	35.657165
1259.834626	90824.351103	35.662183
1261.009736	90936.659643	35.667200
1262.137195	91054.793263	35.672218
1263.671654	91161.774438	35.677236
1264.989187	91286.583814	35.682253
1266.119208	91397.063385	35.687271
1267.976440	91516.415985	35.692288
1268.843729	91629.636850	35.697306
1270.106998	91747.308458	35.702324
1270.974321	91877.690883	35.707341
1272.491074	91994.411463	35.712359
1273.803343	92123.420255	35.717376
1275.184385	92254.738276	35.722394
1276.393619	92370.849112	35.727412
1278.016718	92497.415673	35.732429
1278.770933	92634.219497	35.737447
1279.896337	92757.112984	35.742464
1280.683241	92888.792386	35.747482
1282.248963	93022.619878	35.752500
1283.365575	93165.719631	35.757517
1284.585061	93299.298036	35.762535
1286.242706	93436.091580	35.767552
1287.529735	93576.188167	35.772570
1289.416556	93705.633893	35.777588
1290.412044	93842.785814	35.782605
1291.724988	93971.561492	35.787623
1293.125844	94107.409354	35.792640
1294.737712	94244.251651	35.797658
1296.019082	94369.535593	35.802676
1296.906194	94508.355112	35.807693
1298.190345	94641.447631	35.812711
1299.593244	94775.029250	35.817728
1300.820446	94919.640986	35.822746
1302.682043	95042.137496	35.827764
1303.932879	95176.961355	35.832781
1305.308940	95312.666270	35.837799
1306.950661	95434.767588	35.842816
1308.044025	95580.341225	35.847834
1309.383215	95700.766794	35.852852
1310.900968	95843.651745	35.857869
1312.200274	95962.981748	35.862887
1313.327058	96087.396709	35.867904
1314.687082	96217.872953	35.872922
1316.265785	96351.700175	35.877940
1317.598440	96477.567727	35.882957
1318.709606	96607.032222	35.887975
1320.084309	96736.202710	35.892992
1321.316422	96862.657880	35.898010
1322.756042	96990.285497	35.903028
1323.765222	97132.266744	35.908045
1324.899905	97262.541556	35.913063
1326.648807	97396.143915	35.918080
1327.812173	97528.912601	35.923098
1329.412578	97667.330899	35.928116
1331.060167	97802.649391	35.933133
1331.671265	97935.619833	35.938151
1333.146304	98052.826104	35.943168
1334.126427	98204.400198	35.948186
1335.529469	98331.354383	35.953204
1337.475299	98472.866257	35.958221
1338.379751	98605.388182	35.963239
1339.825120	98733.833249	35.968256
1341.373197	98857.458293	35.973274
1342.996900	98979.639547	35.978292
1344.164960	99088.162979	35.983309
1345.595380	99201.830860	35.988327
1347.277265	99311.023018	35.993344
1348.377191	99429.750605	35.998362
1349.334435	99542.022793	36.003380
1350.638202	99657.702324	36.008397
1352.397954	99772.233729	36.013415
1353.557366	99881.813408	36.018432
1355.255472	100015.954430	36.023450
1356.483071	100122.202840	36.028468
1357.357745	100247.319894	36.033485
1358.538176	100370.019145	36.038503
1359.871348	100495.458798	36.043520
1360.910110	100623.023891	36.048538
1362.478405	100756.490925	36.053556
1363.695922	100889.886330	36.058573
1365.080112	101023.991651	36.063591
1366.948129	101157.299583	36.068608
1368.049626	101283.450268	36.073626
1369.298886	101423.600230	36.078644
1370.960782	101561.138293	36.083661
1371.713377	101705.842101	36.088679
1373.445670	101835.649438	36.093696
1374.399216	101985.711394	36.098714
1376.095424	102129.623618	36.103732
1377.422915	102270.120021	36.108749
1378.162549	102425.732327	36.113767
1379.719130	102563.975624	36.118784
1381.011729	102723.078568	36.123802
1382.599393	102865.933244	36.128820
1384.091513	103019.947850	36.133837
1385.000480	103183.081108	36.138855
1386.822493	103330.009185	36.143872
1388.230058	103481.427296	36.148890
1390.417111	103628.933818	36.153908
1391.551040	103778.329234	36.158925
1392.974129	103926.754755	36.163943
1395.019905	104059.856604	36.168960
1396.533335	104202.880745	36.173978
1398.224307	104344.749430	36.178996
1399.893788	104469.784217	36.184013
1401.055026	104610.316423	36.189031
1403.185510	104733.048910	36.194048
1404.212433	104859.377010	36.199066
1405.745120	104976.092038	36.204084
1407.429450	105113.324397	36.209101
1408.556004	105249.262078	36.214119
1409.873146	105367.432107	36.219136
1411.131352	105512.644389	36.224154
1412.437504	105644.219324	36.229172
1413.882459	105777.218641	36.234189
1414.760142	105920.120819	36.239207
1416.234370	106054.460713	36.244224
1417.394783	106204.598230	36.249242
1419.062835	106339.289478	36.254260
1420.236079	106463.800277	36.259277
1421.710876	106605.699454	36.264295
1423.247327	106750.049539	36.269312
1424.739879	106893.519467	36.274330
1425.802988	107044.601476	36.279348
1427.985795	107179.076446	36.284365
1428.866928	107336.312563	36.289383
1430.059321	107458.389419	36.294400
1431.630521	107610.028852	36.299418
1433.319545	107744.798465	36.304436
1434.955039	107875.988394	36.309453
1436.326504	108015.931367	36.314471
1437.490720	108133.310571	36.319488
1439.147468	108259.527911	36.324506
1440.503072	108392.500602	36.329524
1441.775551	108518.195393	36.334541
1443.354438	108651.641551	36.339559
1444.408670	108770.739247	36.344576
1445.947661	108899.614839	36.349594
1447.410848	109035.426421	36.354612
1448.822568	109156.625535	36.359629
1449.360893	109299.442434	36.364647
1450.900696	109440.988119	36.369664
1452.263370	109592.719425	36.374682
1453.523327	109755.677430	36.379700
1455.257547	109897.346877	36.384717
1456.470236	110048.076334	36.389735
1458.280846	110198.091995	36.394752
1459.642133	110353.567774	36.399770
1461.377484	110508.161732	36.404788
1463.147633	110647.888375	36.409805
1464.347674	110806.789863	36.414823
1465.632829	110952.249120	36.419840
1467.382212	111099.564315	36.424858
1468.474858	111257.102254	36.429876
1470.884757	111389.744700	36.434893
1472.395404	111543.870901	36.439911
1474.453425	111674.869835	36.444928
1476.714447	111810.377739	36.449946
1478.527270	111930.940622	36.454964
1480.154335	112064.265435	36.459981
1481.475211	112195.355656	36.464999
1482.666114	112317.208746	36.470016
1484.175507	112452.493666	36.475034
1484.975387	112588.003668	36.480052
1486.339844	112736.666441	36.485069
1487.542935	112880.294759	36.490087
1488.744947	113027.817260	36.495104
1490.349246	113177.560562	36.500122
1491.730570	113335.646119	36.505140
1493.479409	113472.039019	36.510157
1494.560986	113628.764768	36.515175
1496.045572	113784.566060	36.520192
1497.555799	113945.107303	36.525210
1498.715054	114094.708069	36.530228
1500.870687	114242.125146	36.535245
1501.779436	114409.458497	36.540263
1503.518616	114571.818547	36.545280
1505.410213	114728.334183	36.550298
1506.244317	114891.217008	36.555316
1507.897991	115049.343726	36.560333
1509.335767	115215.406229	36.565351
1510.984140	115384.188926	36.570368
1512.276334	115536.463707	36.575386
1513.716880	115714.716493	36.580404
1515.400949	115883.698854	36.585421
1517.010576	116061.153320	36.590439
1518.453955	116220.459294	36.595456
1519.751531	116378.875443	36.600474
1521.182295	116542.344914	36.605492
1522.778199	116713.741955	36.610509
1524.908771	116885.982467	36.615527
1526.318418	117047.821266	36.620544
1528.141505	117203.520941	36.625562
1529.157098	117374.580096	36.630580
1530.989171	117530.888554	36.635597
1532.345326	117696.404096	36.640615
1533.725127	117869.362130	36.645632
1535.278196	118026.261483	36.650650
1536.469448	118195.495914	36.655668
1538.083363	118350.522598	36.660685
1539.480005	118508.843550	36.665703
1540.774076	118662.931936	36.670720
1542.081526	118817.424761	36.675738
1543.459025	118984.363257	36.680756
1545.201654	119150.941233	36.685773
1546.570750	119312.326745	36.690791
1548.062590	119480.733693	36.695808
1549.617670	119650.653679	36.700826
1550.986206	119828.734246	36.705844
1552.579595	119991.888922	36.710861
1554.125081	120170.729982	36.715879
1555.532725	120348.654658	36.720896
1557.475285	120528.386932	36.725914
1558.808878	120706.667275	36.730932
1560.572074	120883.245224	36.735949
1562.175331	121064.313976	36.740967
1563.686454	121238.789023	36.745984
1565.568327	121421.566608	36.751002
1566.853159	121600.962252	36.756020
1568.747853	121783.587319	36.761037
1570.507747	121963.506894	36.766055
1571.470487	122143.361089	36.771072
1573.571850	122330.738904	36.776090
1575.054478	122509.384862	36.781108
1576.877910	122689.044169	36.786125
1578.274754	122873.400911	36.791143
1579.546343	123068.256312	36.796160
1581.456120	123249.414318	36.801178
1583.032396	123442.143690	36.806196
1584.969931	123620.863415	36.811213
1586.360464	123808.485735	36.816231
1588.207073	124003.636806	36.821248
1589.810779	124167.479645	36.826266
1591.171433	124364.940844	36.831284
1593.492748	124546.839919	36.836301
1594.647832	124715.474042	36.841319
1596.209210	124903.747272	36.846336
1598.401743	125088.624726	36.851354
1599.827856	125276.400614	36.856372
1601.402637	125450.021635	36.861389
1603.021789	125638.796756	36.866407
1605.138560	125818.043884	36.871424
1606.980674	125979.027902	36.876442
1608.780053	126147.504284	36.881460
1610.710814	126304.530269	36.886477
1612.691914	126470.391633	36.891495
1613.987437	126644.581370	36.896512
1615.987634	126805.937335	36.901530
1616.998532	126981.771338	36.906548
1618.600480	127147.034736	36.911565
1620.417990	127316.972099	36.916583
1621.478177	127480.912907	36.921600
1623.201656	127658.795678	36.926618
1624.540616	127839.365287	36.931636
1625.751894	128014.538144	36.936653
1627.407984	128197.533946	36.941671
1628.421036	128386.428713	36.946688
1630.229965	128577.166997	36.951706
1631.591765	128774.661990	36.956724
1632.656383	128970.821238	36.961741
1634.331578	129170.908307	36.966759
1636.105754	129374.368499	36.971776
1637.751537	129574.715816	36.976794
1638.971516	129783.098218	36.981812
1640.370656	129981.481196	36.986829
1642.067101	130194.815810	36.991847
1643.427907	130394.906851	36.996864
1644.851830	130597.678847	37.001882
1646.483004	130802.398875	37.006900
1648.165841	130998.230212	37.011917
1649.911730	131200.333240	37.016935
1651.110046	131396.165675	37.021952
1652.780132	131602.926258	37.026970
1654.111811	131806.251226	37.031988
1655.445569	132020.095459	37.037005
1657.031512	132227.087824	37.042023
1658.866096	132447.263856	37.047040
1660.884110	132661.892943	37.052058
1662.837140	132882.369952	37.057076
1664.117895	133098.879647	37.062093
1666.135383	133325.020681	37.067111
1667.633713	133548.337950	37.072128
1669.741712	133762.971110	37.077146
1671.079197	133989.855835	37.082164
1673.168778	134196.563398	37.087181
1674.855543	134425.121688	37.092199
1676.886333	134636.103964	37.097216
1679.575877	134828.699640	37.102234
1681.797898	135030.708170	37.107252
1683.663603	135225.349848	37.112269
1685.624573	135416.196128	37.117287
1687.049719	135619.765228	37.122304
1688.972811	135822.623276	37.127322
1690.190684	136019.526419	37.132340
1691.693901	136226.563021	37.137357
1693.116643	136434.171435	37.142375
1694.886498	136632.742493	37.147392
1697.028568	136839.352522	37.152410
1698.462749	137057.367560	37.157428
1700.001444	137263.870379	37.162445
1701.789616	137475.525462	37.167463
1703.212262	137689.091142	37.172480
1704.421853	137894.556676	37.177498
1706.136052	138120.997401	37.182516
1707.486924	138344.932374	37.187533
1709.138389	138577.019504	37.192551
1710.706557	138815.745067	37.197568
1712.273091	139049.573640	37.202586
1714.314625	139272.225366	37.207604
1716.114154	139498.101113	37.212621
1718.016089	139727.921442	37.217639
1719.943124	139967.523408	37.222656
1721.980993	140185.167241	37.227674
1724.001802	140407.218394	37.232692
1725.585617	140632.587426	37.237709
1727.570165	140857.806316	37.242727
1728.671077	141095.080516	37.247744
1730.836811	141299.993285	37.252762
1732.667101	141521.597006	37.257780
1734.305288	141751.798093	37.262797
1736.094922	141973.270611	37.267815
1738.036143	142195.228193	37.272832
1739.926399	142416.509396	37.277850
1741.367894	142646.021934	37.282868
1742.793576	142867.072892	37.287885
1744.601754	143090.438605	37.292903
1746.440668	143322.240360	37.297920
1748.260527	143545.606320	37.302938
1750.023207	143760.872281	37.307956
1751.251820	143987.581294	37.312973
1753.100592	144217.913481	37.317991
1754.619800	144451.800943	37.323008
1756.336822	144693.806845	37.328026
1757.805402	144924.620288	37.333044
1759.510342	145170.146008	37.338061
1760.981011	145392.089620	37.343079
1762.523781	145617.805207	37.348096
1763.864948	145858.542530	37.353114
1765.520819	146092.327483	37.358132
1767.064707	146335.726243	37.363149
1768.878736	146568.574920	37.368167
1770.152851	146824.887946	37.373184
1771.827488	147077.332193	37.378202
1773.497782	147328.572566	37.383220
1774.856489	147590.473593	37.388237
1776.785772	147852.223672	37.393255
1778.070311	148129.649284	37.398272
1779.963185	148392.676999	37.403290
1781.727798	148671.122328	37.408308
1783.459469	148946.464507	37.413325
1785.050009	149226.716853	37.418343
1786.780626	149503.801017	37.423360
1788.450600	149797.803193	37.428378
1790.325748	150074.931289	37.433396
1792.281840	150359.321407	37.438413
1795.016281	150642.728744	37.443431
1796.793826	150925.804149	37.448448
1798.668053	151208.827900	37.453466
1800.746291	151486.820152	37.458484
1802.605773	151772.667061	37.463501
1804.235227	152044.461394	37.468519
1806.868901	152323.958131	37.473536
1808.649548	152601.494581	37.478554
1810.985426	152881.307042	37.483572
1812.379562	153169.137648	37.488589
1814.672145	153429.499959	37.493607
1816.468660	153700.476657	37.498624
1818.549232	153980.245476	37.503642
1820.560149	154237.570710	37.508660
1822.387789	154507.683228	37.513677
1824.372075	154767.439579	37.518695
1825.952568	155049.525655	37.523712
1827.600261	155311.583735	37.528730
1829.478421	155574.863877	37.533748
1831.154789	155856.012283	37.538765
1833.397279	156123.820898	37.543783
1834.906480	156405.391499	37.548800
1836.689869	156678.428090	37.553818
1838.843240	156946.825591	37.558836
1840.656817	157219.542621	37.563853
1842.383846	157498.824878	37.568871
1844.319124	157771.588973	37.573888
1845.643422	158049.451189	37.578906
1847.335484	158327.130502	37.583924
1849.287027	158611.918001	37.588941
1851.118772	158902.019328	37.593959
1852.956018	159196.259795	37.598976
1854.799954	159478.452899	37.603994
1856.676695	159764.120694	37.609012
1858.870793	160046.477726	37.614029
1860.323193	160335.489596	37.619047
1862.219036	160629.677003	37.624064
1864.125765	160917.237059	37.629082
1866.080230	161208.625057	37.634100
1867.334420	161494.105674	37.639117
1869.080629	161787.331530	37.644135
1870.626838	162087.851815	37.649152
1872.326912	162399.610724	37.654170
1874.517460	162694.625172	37.659188
1876.334680	163006.521139	37.664205
1878.027158	163315.454470	37.669223
1880.035601	163630.396092	37.674240
1882.460842	163919.755238	37.679258
1884.104094	164204.679450	37.684276
1885.830668	164487.865240	37.689293
1887.739880	164754.988462	37.694311
1889.412302	165041.232133	37.699328
1890.968209	165343.429078	37.704346
1892.509314	165633.822024	37.709364
1894.288229	165935.504447	37.714381
1895.838045	166232.272223	37.719399
1897.917140	166536.234048	37.724416
1900.414473	166830.368420	37.729434
1902.943022	167124.727728	37.734452
1904.647836	167431.075238	37.739469
1906.390985	167729.850839	37.744487
1907.836362	168041.891473	37.749504
1909.424014	168356.895117	37.754522
1911.343585	168664.230328	37.759540
1913.296126	168980.779764	37.764557
1914.681733	169300.237583	37.769575
1916.155719	169635.490987	37.774592
1918.147774	169971.541418	37.779610
1919.966583	170308.344103	37.784628
1921.680036	170660.769719	37.789645
1923.685109	170992.493017	37.794663
1925.306676	171344.428292	37.799680
1927.212862	171698.733448	37.804698
1929.541170	172065.786398	37.809716
1931.037346	172432.894448	37.814733
1932.804644	172783.188451	37.819751
1934.683638	173151.459342	37.824768
1936.397547	173531.325363	37.829786
1938.453469	173893.363019	37.834804
1940.370143	174270.585318	37.839821
1942.664887	174644.233240	37.844839
1945.060595	175008.572248	37.849856
1947.340062	175369.718389	37.854874
1950.188569	175715.844574	37.859892
1952.236066	176077.347425	37.864909
1954.415100	176434.882246	37.869927
1956.820914	176780.180254	37.874944
1958.057989	177137.902806	37.879962
1960.649506	177490.133552	37.884980
1962.267280	177847.317336	37.889997
1964.485455	178204.536164	37.895015
1966.672591	178555.234252	37.900032
1968.133637	178900.840337	37.905050
1970.756959	179250.203496	37.910068
1972.306376	179615.176829	37.915085
1974.704739	179965.060395	37.920103
1976.674951	180311.989655	37.925120
1978.766677	180666.393680	37.930138
1980.635725	181013.646166	37.935156
1982.360284	181373.977004	37.940173
1984.592406	181731.868248	37.945191
1986.743476	182077.455398	37.950208
1988.045743	182439.100620	37.955226
1990.063734	182791.390854	37.960244
1991.907328	183149.195600	37.965261
1993.954489	183511.897316	37.970279
1995.746004	183872.024129	37.975296
1997.693198	184231.340688	37.980314
1999.651502	184591.799782	37.985332
2002.424595	184944.843903	37.990349
2006.286416	185244.508994	37.995367
2009.415277	185568.595936	38.000384
2011.221927	185887.962265	38.005402
2013.372567	186213.879852	38.010420
2014.876875	186528.596379	38.015437
2016.389991	186874.528309	38.020455
2018.367028	187230.752157	38.025472
2019.670968	187543.750360	38.030490
2021.087452	187854.115808	38.035508
2023.032938	188169.454360	38.040525
2024.714697	188490.524419	38.045543
2026.022928	188816.200125	38.050560
2027.758840	189150.827198	38.055578
2029.261037	189495.067445	38.060596
2031.128390	189842.020525	38.065613
2032.951260	190209.301702	38.070631
2034.561665	190577.379131	38.075648
2035.862569	190951.119367	38.080666
2037.896565	191324.314900	38.085684
2039.838634	191708.625922	38.090701
2041.790421	192102.487275	38.095719
2044.012913	192484.140880	38.100736
2045.895994	192887.210498	38.105754
2048.053647	193279.849772	38.110772
2050.123945	193674.027925	38.115789
2052.105503	194085.036547	38.120807
2054.225734	194478.803002	38.125824
2056.210718	194892.125152	38.130842
2058.243842	195296.906308	38.135860
2060.618632	195709.611515	38.140877
2063.341050	196088.962722	38.145895
2066.576355	196486.371767	38.150912
2068.699395	196871.838545	38.155930
2071.203397	197254.935549	38.160948
2073.720384	197644.966204	38.165965
2075.494935	198009.965790	38.170983
2077.816100	198410.265852	38.176000
2079.192410	198807.538813	38.181018
2081.480057	199197.634667	38.186036
2083.252242	199599.496634	38.191053
2084.850540	200006.543312	38.196071
2087.005519	200403.750005	38.201088
2088.493504	200822.805723	38.206106
2091.018132	201232.175357	38.211124
2093.256483	201639.507571	38.216141
2094.670325	202059.619450	38.221159
2096.827624	202471.005243	38.226176
2099.027365	202899.100216	38.231194
2101.510592	203309.903795	38.236212
2104.280025	203710.959984	38.241229
2106.510392	204118.172169	38.246247
2108.754687	204511.843443	38.251264
2110.959095	204929.603526	38.256282
2113.358617	205331.838440	38.261300
2115.194915	205738.353291	38.266317
2117.140708	206142.845089	38.271335
2119.726325	206549.016308	38.276352
2121.577348	206968.994842	38.281370
2123.541024	207384.536534	38.286388
2125.493787	207794.720656	38.291405
2127.436815	208220.098110	38.296423
2129.550235	208639.657904	38.301440
2130.947712	209065.020185	38.306458
2132.673331	209499.223284	38.311476
2134.807880	209927.215899	38.316493
2136.669764	210373.770705	38.321511
2138.913688	210806.117124	38.326528
2140.776682	211247.948190	38.331546
2142.678765	211699.808244	38.336564
2144.940799	212151.409760	38.341581
2147.530049	212605.577605	38.346599
2149.902144	213043.775656	38.351616
2151.745329	213475.756528	38.356634
2154.768418	213910.882219	38.361652
2156.791935	214327.212880	38.366669
2158.738432	214742.463658	38.371687
2160.826956	215146.007083	38.376704
2163.228816	215566.522697	38.381722
2164.957479	215979.293754	38.386740
2167.076485	216406.306826	38.391757
2168.821594	216832.082914	38.396775
2170.939222	217258.919200	38.401792
2172.829179	217696.359321	38.406810
2174.658408	218135.562147	38.411828
2177.474140	218559.090009	38.416845
2179.639526	219010.358904	38.421863
2181.937993	219445.374295	38.426880
2184.138203	219882.869462	38.431898
2186.238189	220337.579019	38.436916
2188.807529	220774.407595	38.441933
2190.595648	221235.212376	38.446951
2193.242448	221664.662194	38.451968
2195.515956	222108.447376	38.456986
2197.812252	222546.919745	38.462004
2200.227743	222990.454536	38.467021
2202.499514	223444.808568	38.472039
2204.747569	223892.612159	38.477056
2206.729634	224338.958403	38.482074
2209.608993	224791.439890	38.487092
2212.322888	225224.741686	38.492109
2214.409338	225661.367480	38.497127
2217.005133	226088.463693	38.502144
2219.145109	226537.910228	38.507162
2221.116066	226980.854183	38.512180
2223.425844	227422.856212	38.517197
2225.559486	227867.400584	38.522215
2227.931132	228310.307363	38.527232
2230.091360	228756.701883	38.532250
2232.101484	229217.549131	38.537268
2234.406945	229665.444984	38.542285
2236.315219	230127.298477	38.547303
2238.612462	230586.118942	38.552320
2240.523336	231042.433489	38.557338
2242.525244	231511.308587	38.562356
2244.652052	231982.958382	38.567373
2246.282992	232456.590313	38.572391
2248.519014	232941.686512	38.577408
2250.975431	233429.720263	38.582426
2253.086934	233910.567141	38.587444
2255.457045	234392.745128	38.592461
2257.815998	234879.573272	38.597479
2260.355259	235358.726284	38.602496
2262.476411	235850.340882	38.607514
2264.948764	236343.653093	38.612532
2267.452629	236828.500337	38.617549
2269.374346	237322.151016	38.622567
2271.915429	237802.748757	38.627584
2274.103969	238294.806916	38.632602
2276.233484	238786.467067	38.637620
2278.648362	239274.017479	38.642637
2280.756278	239760.547936	38.647655
2283.481703	240247.768995	38.652672
2286.048696	240738.367127	38.657690
2287.791879	241228.355892	38.662708
2290.342461	241719.462866	38.667725
2293.059310	242211.152708	38.672743
2295.396523	242683.213169	38.677760
2297.738200	243163.274018	38.682778
2300.144416	243647.108912	38.687796
2302.767733	244117.242153	38.692813
2304.602345	244615.034013	38.697831
2306.954099	245081.676447	38.702848
2309.252281	245533.973557	38.707866
2311.264314	245997.161229	38.712884
2313.683681	246447.710075	38.717901
2315.779483	246919.951375	38.722919
2317.989915	247377.541754	38.727936
2320.115666	247842.333146	38.732954
2322.049478	248312.970428	38.737972
2324.362858	248789.339187	38.742989
2326.455628	249266.172846	38.748007
2328.376797	249746.664442	38.753024
2330.769948	250225.455493	38.758042
2333.287594	250719.644928	38.763060
2336.029977	251200.512602	38.768077
2338.095015	251697.614542	38.773095
2341.049691	252188.835631	38.778112
2342.844325	252689.964612	38.783130
2344.918371	253191.708908	38.788148
2347.537023	253684.603181	38.793165
2349.590175	254194.069451	38.798183
2352.776912	254681.461398	38.803200
2354.955753	255182.395077	38.808218
2357.126040	255691.405913	38.813236
2359.926150	256192.975884	38.818253
2361.596196	256711.332202	38.823271
2363.880125	257227.304864	38.828288
2366.083993	257742.068697	38.833306
2368.321628	258266.807738	38.838324
2371.119824	258785.107176	38.843341
2373.482752	259310.355757	38.848359
2376.204902	259835.520775	38.853376
2378.868104	260364.426534	38.858394
2380.963884	260896.694872	38.863412
2383.476093	261417.465896	38.868429
2385.301018	261957.569362	38.873447
2387.233279	262498.974344	38.878464
2389.956454	263038.958223	38.883482
2392.529134	263584.449201	38.888500
2395.089652	264112.362831	38.893517
2397.288059	264668.269576	38.898535
2399.224963	265215.375128	38.903552
2401.999159	265767.071739	38.908570
2404.379188	266327.767172	38.913588
2406.819525	266876.538033	38.918605
2408.883609	267441.289431	38.923623
2411.458243	268004.637403	38.928640
2414.270964	268561.468448	38.933658
2417.460134	269099.950896	38.938676
2420.242783	269649.160760	38.943693
2423.019832	270182.392921	38.948711
2425.179101	270733.750611	38.953728
2428.165259	271264.429543	38.958746
2430.322766	271808.618807	38.963764
2432.632355	272343.028475	38.968781
2435.064643	272887.041351	38.973799
2438.047064	273417.733329	38.978816
2440.651369	273956.785663	38.983834
2442.268883	274491.340536	38.988852
2444.922463	275028.930742	38.993869
2447.234779	275585.109968	38.998887
2449.302627	276123.825454	39.003904
2451.630510	276667.169782	39.008922
2454.447652	277205.177343	39.013940
2456.911751	277750.677158	39.018957
2459.156044	278293.439281	39.023975
2461.757474	278835.405578	39.028992
2464.654363	279379.607651	39.034010
2466.828165	279930.216337	39.039028
2469.390822	280461.638181	39.044045
2471.543226	280999.748099	39.049063
2473.352567	281512.309864	39.054080
2475.861526	282037.024619	39.059098
2477.725380	282566.203766	39.064116
2479.923917	283103.173663	39.069133
2482.496452	283648.994515	39.074151
2484.520885	284189.665378	39.079168
2487.104142	284738.421754	39.084186
2489.093615	285306.691934	39.089204
2491.355735	285855.337046	39.094221
2494.009163	286425.018179	39.099239
2496.321363	286998.327942	39.104256
2499.139602	287580.593679	39.109274
2501.560502	288154.866845	39.114292
2503.761780	288730.261006	39.119309
2506.164582	289316.613267	39.124327
2508.190783	289921.859176	39.129344
2510.831077	290510.524939	39.134362
2513.004941	291136.658553	39.139380
2515.370547	291736.172087	39.144397
2517.606044	292352.610054	39.149415
2520.226930	292981.245277	39.154432
2522.999357	293593.550139	39.159450
2525.802040	294226.841256	39.164468
2528.341172	294849.477768	39.169485
2531.222497	295472.029084	39.174503
2533.689427	296110.176206	39.179520
2536.181119	296746.509882	39.184538
2538.830647	297379.054507	39.189556
2541.142195	298007.709588	39.194573
2544.675241	298642.082912	39.199591
2546.896163	299286.706641	39.204608
2549.583054	299919.343849	39.209626
2552.135745	300551.943903	39.214644
2554.891147	301183.718104	39.219661
2557.292218	301822.597434	39.224679
2560.375910	302467.557086	39.229696
2563.036360	303098.054251	39.234714
2565.213896	303746.769498	39.239732
2568.133831	304382.541786	39.244749
2570.716491	305026.786475	39.249767
2573.135394	305667.697865	39.254784
2576.302525	306300.539590	39.259802
2578.890713	306953.897365	39.264820
2581.555997	307583.958133	39.269837
2584.379894	308221.753467	39.274855
2586.790355	308867.803535	39.279872
2589.808388	309498.698820	39.284890
2592.466210	310135.352954	39.289908
2595.114687	310753.522289	39.294925
2597.401961	311401.055359	39.299943
2599.875814	312039.388053	39.304960
2602.835456	312666.215232	39.309978
2605.372999	313307.287341	39.314996
2608.315969	313939.049228	39.320013
2611.243750	314576.159961	39.325031
2614.163272	315199.558328	39.330048
2616.870830	315809.403425	39.335066
2619.608235	316447.152136	39.340084
2622.179311	317064.107535	39.345101
2624.881094	317686.617214	39.350119
2627.629943	318300.863139	39.355136
2629.738739	318914.540306	39.360154
2632.701633	319530.664398	39.365172
2635.267714	320148.465612	39.370189
2638.048284	320767.188909	39.375207
2640.406183	321395.941730	39.380224
2643.240088	322000.885245	39.385242
2645.741821	322594.300814	39.390260
2648.644882	323179.830175	39.395277
2651.254320	323759.916189	39.400295
2653.632584	324343.100343	39.405312
2656.224944	324932.357994	39.410330
2658.829975	325520.615675	39.415348
2661.109180	326111.452882	39.420365
2663.929495	326706.104657	39.425383
2666.228975	327311.129805	39.430400
2669.091428	327893.604250	39.435418
2671.571152	328487.572239	39.440436
2674.782521	329093.519437	39.445453
2677.460404	329709.105055	39.450471
2679.746270	330304.445873	39.455488
2682.610543	330923.585936	39.460506
2685.211727	331543.721088	39.465524
2687.819293	332165.037610	39.470541
2690.349830	332777.527786	39.475559
2692.549488	333416.467841	39.480576
2694.983142	334050.363264	39.485594
2697.652652	334695.449012	39.490612
2700.109452	335339.542068	39.495629
2702.457254	335984.985353	39.500647
2705.098140	336652.008911	39.505664
2707.662687	337307.947531	39.510682
2709.927877	337987.053854	39.515700
2712.498574	338670.716283	39.520717
2715.278080	339352.963608	39.525735
2717.501908	340043.908042	39.530752
2720.516184	340743.136619	39.535770
2723.031075	341453.766172	39.540788
2725.680701	342147.291764	39.545805
2728.767089	342849.967249	39.550823
2731.617444	343563.570512	39.555840
2733.914968	344269.687652	39.560858
2736.962246	344984.980723	39.565876
2739.754290	345701.896180	39.570893
2742.869649	346425.161989	39.575911
2745.874567	347141.379862	39.580928
2749.023810	347853.452020	39.585946
2751.924302	348559.360508	39.590964
2754.847032	349272.046113	39.595981
2758.479000	349971.953202	39.600999
2761.352211	350664.229944	39.606016
2764.343867	351370.317440	39.611034
2767.443259	352063.949054	39.616052
2769.587191	352760.832969	39.621069
2772.882667	353446.645899	39.626087
2775.452264	354163.867874	39.631104
2778.364794	354849.177724	39.636122
2781.535546	355545.409818	39.641140
2783.695394	356241.175337	39.646157
2786.612521	356942.714194	39.651175
2789.381969	357649.178080	39.656192
2792.286706	358346.200074	39.661210
2794.912884	359049.713559	39.666228
2797.428311	359751.048108	39.671245
2800.389494	360442.994468	39.676263
2803.505712	361153.683098	39.681280
2806.073135	361844.948810	39.686298
2808.682898	362550.487079	39.691316
2811.304780	363264.826909	39.696333
2814.248443	363972.332366	39.701351
2817.413399	364678.848640	39.706368
2820.450148	365377.333911	39.711386
2823.366078	366073.819138	39.716404
2826.494998	366763.386709	39.721421
2829.385145	367455.255700	39.726439
2831.939397	368130.257755	39.731456
2834.661739	368793.586397	39.736474
2837.816675	369449.737053	39.741492
2840.199836	370106.296660	39.746509
2842.993992	370762.447599	39.751527
2845.734193	371432.907636	39.756544
2848.724421	372095.280648	39.761562
2851.486397	372767.478777	39.766580
2853.545205	373451.095319	39.771597
2856.264160	374126.206038	39.776615
2858.871131	374824.093754	39.781632
2861.326890	375526.040637	39.786650
2864.012479	376230.821639	39.791668
2866.998467	376941.338769	39.796685
2869.857169	377647.981060	39.801703
2872.572064	378370.763362	39.806720
2875.464391	379096.234175	39.811738
2878.652449	379814.267972	39.816756
2881.150238	380555.059643	39.821773
2884.559201	381280.947181	39.826791
2886.970995	382017.759524	39.831808
2889.225542	382758.501208	39.836826
2892.217909	383512.656671	39.841844
2895.187789	384260.689967	39.846861
2898.499883	385000.366801	39.851879
2901.580982	385760.469677	39.856896
2904.217616	386521.885131	39.861914
2907.373068	387279.271824	39.866932
2910.278430	388040.574226	39.871949
2913.512762	388801.827579	39.876967
2916.434662	389559.763935	39.881984
2919.370968	390333.246590	39.887002
2922.561453	391106.159042	39.892020
2925.478485	391879.342880	39.897037
2928.202505	392662.861804	39.902055
2931.231038	393424.130685	39.907072
2934.014536	394197.362831	39.912090
2937.457483	394966.670269	39.917108
2940.505449	395749.279133	39.922125
2943.798921	396519.218042	39.927143
2946.359804	397306.711663	39.932160
2949.422288	398095.315955	39.937178
2952.163065	398875.591284	39.942196
2955.174979	399653.571139	39.947213
2958.123387	400438.014062	39.952231
2961.380745	401228.760086	39.957248
2963.938564	402024.649386	39.962266
2967.362964	402814.859451	39.967284
2970.528469	403601.286660	39.972301
2973.169699	404384.276240	39.977319
2975.618061	405180.679901	39.982336
2978.274779	405982.336695	39.987354
2981.095020	406788.645651	39.992372
2984.162492	407604.096723	39.997389
2987.041538	408415.398014	40.002407
2990.031035	409231.611106	40.007424
2993.127133	410052.634722	40.012442
2996.511599	410871.761364	40.017460
2999.447095	411683.439420	40.022477
3002.293921	412491.104316	40.027495
3005.342971	413305.081903	40.032512
3008.106352	414126.155474	40.037530
3011.377009	414935.585256	40.042548
3014.807853	415762.511954	40.047565
3017.851986	416573.735862	40.052583
3021.127313	417393.288971	40.057600
3024.426344	418208.102855	40.062618
3027.304895	418995.690280	40.067636
3030.133184	419781.435236	40.072653
3032.969690	420553.444302	40.077671
3035.628012	421317.209467	40.082688
3038.462615	422098.415591	40.087706
3041.755023	422879.369143	40.092724
3044.314848	423677.143745	40.097741
3046.910259	424460.269143	40.102759
3049.742400	425251.113861	40.107776
3052.839812	426054.273239	40.112794
3055.912288	426867.465242	40.117812
3058.818199	427683.885731	40.122829
3061.723781	428493.246208	40.127847
3064.836321	429316.948406	40.132864
3067.645600	430140.208679	40.137882
3070.919814	430974.280234	40.142900
3073.723516	431818.447866	40.147917
3076.827842	432652.929468	40.152935
3079.588668	433504.005769	40.157952
3082.584760	434351.925434	40.162970
3086.371819	435204.889971	40.167988
3088.815947	436064.291788	40.173005
3092.214625	436925.578343	40.178023
3095.297474	437792.382800	40.183040
3098.278697	438656.687835	40.188058
3101.998421	439521.646919	40.193076
3104.625239	440395.729201	40.198093
3108.281197	441276.430737	40.203111
3111.258208	442150.477802	40.208128
3114.303831	443043.769569	40.213146
3117.531387	443919.917123	40.218164
3120.256910	444816.860551	40.223181
3123.371348	445706.628824	40.228199
3127.161699	446604.278906	40.233216
3129.957323	447508.150345	40.238234
3133.201526	448391.555848	40.243252
3136.911189	449292.014719	40.248269
3140.274953	450174.607469	40.253287
3143.770373	451071.173062	40.258304
3146.648274	451963.952616	40.263322
3149.801113	452857.805831	40.268340
3152.678203	453752.414177	40.273357
3156.059542	454656.944591	40.278375
3159.210783	455563.029155	40.283392
3162.009660	456469.273131	40.288410
3165.220864	457371.216571	40.293428
3168.494270	458294.856563	40.298445
3171.483446	459203.149120	40.303463
3174.967794	460123.983669	40.308480
3177.606948	461050.400821	40.313498
3181.116515	461962.755783	40.318516
3184.429329	462886.394980	40.323533
3187.832448	463799.878879	40.328551
3190.509933	464724.778024	40.333568
3193.514029	465655.276292	40.338586
3196.732375	466594.517698	40.343604
3200.189049	467532.609864	40.348621
3203.015524	468455.413184	40.353639
3206.478799	469383.160235	40.358656
3209.789519	470325.000674	40.363674
3213.018787	471256.915096	40.368692
3215.982920	472187.304837	40.373709
3219.733623	473120.443820	40.378727
3222.935065	474049.278225	40.383744
3225.958854	474984.994572	40.388762
3229.269283	475914.259351	40.393780
3232.883943	476846.246219	40.398797
3236.453683	477782.168283	40.403815
3239.569978	478690.683469	40.408832
3242.714799	479590.069110	40.413850
3246.412058	480477.372057	40.418868
3249.121255	481349.406641	40.423885
3252.270615	482237.451534	40.428903
3255.719272	483117.285878	40.433920
3258.829559	484006.344920	40.438938
3262.325110	484899.576178	40.443956
3265.039964	485783.404772	40.448973
3267.956543	486680.301335	40.453991
3271.035893	487581.251394	40.459008
3273.875022	488495.888422	40.464026
3277.200364	489399.765999	40.469044
3280.184944	490335.830019	40.474061
3283.107340	491265.952807	40.479079
3286.890269	492194.020852	40.484096
3289.774222	493134.308675	40.489114
3293.133880	494075.369909	40.494132
3296.328592	495029.087025	40.499149
3299.448900	495983.912648	40.504167
3303.092829	496936.782692	40.509184
3305.908102	497912.375677	40.514202
3309.644139	498876.081270	40.519220
3312.862442	499858.882471	40.524237
3315.597178	500847.179313	40.529255
3319.291975	501832.038353	40.534272
3322.446087	502819.229687	40.539290
3325.825615	503808.784359	40.544308
3329.727015	504806.996015	40.549325
3332.588410	505798.205085	40.554343
3336.578852	506784.741945	40.559360
3339.859986	507790.740831	40.564378
3343.129275	508790.985376	40.569396
3346.749550	509794.726312	40.574413
3350.100603	510807.390959	40.579431
3354.089362	511811.131549	40.584448
3357.370451	512823.107848	40.589466
3360.742621	513820.915295	40.594484
3364.230836	514818.129977	40.599501
3367.210308	515827.469804	40.604519
3370.676216	516836.509053	40.609536
3373.888866	517858.132388	40.614554
3377.191622	518876.246852	40.619572
3380.882400	519900.457888	40.624589
3383.912835	520923.286921	40.629607
3387.541704	521949.815372	40.634624
3391.214462	522978.319173	40.639642
3394.497925	524000.020658	40.644660
3398.303602	525016.135965	40.649677
3401.698318	526033.091810	40.654695
3405.471006	527051.116644	40.659712
3408.813182	528074.254177	40.664730
3411.793286	529078.682058	40.669748
3415.584388	530102.948144	40.674765
3419.002711	531134.273701	40.679783
3422.234786	532165.847950	40.684800
3425.583034	533198.376730	40.689818
3429.288018	534227.553996	40.694836
3432.119501	535251.513118	40.699853
3435.268578	536295.573731	40.704871
3438.493262	537339.939053	40.709888
3441.998911	538395.921135	40.714906
3445.520605	539439.967633	40.719924
3448.843223	540488.124677	40.724941
3452.360504	541554.330977	40.729959
3455.819345	542595.717418	40.734976
3459.553807	543650.772715	40.739994
3463.067620	544703.465344	40.745012
3466.757935	545740.540117	40.750016
3470.116028	546750.460720	40.755021
3473.484699	547693.113347	40.760026
3476.519348	548605.927644	40.765031
3479.611752	549449.580274	40.770036
3482.538454	550242.571770	40.775040
3485.250236	550979.489916	40.780045
3487.867796	551658.868112	40.785050
3490.822218	552285.876750	40.790055
3492.951382	552872.416711	40.795060
3495.259776	553394.612946	40.800064
3497.253413	553857.023931	40.805069
3499.125847	554292.245313	40.810074
3500.656671	554681.216055	40.815079
3502.155894	555010.373192	40.820084
3503.853668	555315.066053	40.825088
3505.079674	555594.697228	40.830093
3506.475696	555812.684337	40.835098
3507.989393	556009.140882	40.840103
3508.965791	556160.601477	40.845108
3510.198764	556279.758541	40.850112
3511.099237	556384.996256	40.855117
3512.157348	556449.856862	40.860122
3513.320033	556487.967316	40.865127
3513.701733	556512.882686	40.870132
3514.657147	556496.050710	40.875136
3514.643756	556476.002647	40.880141
3515.731383	556419.903821	40.885146
3516.038949	556351.363224	40.890151
3516.471848	556274.762425	40.895156
3516.614945	556181.723483	40.900160
3516.900057	556087.405402	40.905165
3517.410548	555964.708717	40.910170
3517.682679	555851.847349	40.915175
3517.993411	555709.781201	40.920180
3517.917337	555558.526661	40.925184
3518.261283	555394.540449	40.930189
3519.009306	555227.021439	40.935194
3518.786558	555063.671724	40.940199
3519.210902	554880.266781	40.945204
3519.053625	554681.972504	40.950208
3519.118578	554486.907246	40.955213
3519.104578	554287.428220	40.960218
3519.143231	554088.239271	40.965223
3519.254306	553877.726836	40.970228
3519.006230	553661.184823	40.975232
3518.812490	553470.365484	40.980237
3518.924972	553239.585465	40.985242
3519.072597	553023.171519	40.990247
3518.782297	552810.792901	40.995252
3518.725046	552583.495183	41.000256
3518.687522	552371.723019	41.005261
3518.478944	552143.384978	41.010266
3518.432658	551913.358480	41.015271
3517.803208	551691.612556	41.020276
3518.429610	551468.862813	41.025280
3517.738771	551247.721619	41.030285
3518.155568	551015.695737	41.035290
3517.978886	550799.493782	41.040295
3517.755171	550572.636891	41.045300
3517.630926	550358.027780	41.050304
3517.618675	550135.855865	41.055309
3517.659487	549914.023607	41.060314
3517.441770	549695.244314	41.065319
3517.085808	549459.739338	41.070324
3517.111130	549243.579012	41.075328
3517.195047	549028.914220	41.080333
3516.612465	548805.952156	41.085338
3516.811492	548587.088253	41.090343
3516.816241	548376.296229	41.095348
3516.782114	548151.627845	41.100352
3516.351999	547937.023983	41.105357
3516.134382	547711.068670	41.110362
3515.880536	547503.470053	41.115367
3515.740165	547300.175141	41.120372
3515.899341	547088.582733	41.125376
3515.507540	546894.221568	41.130381
3515.534115	546667.706258	41.135386
3515.074998	546466.609775	41.140391
3514.929497	546270.088196	41.145396
3515.185199	546071.388721	41.150400
3515.036637	545871.391013	41.155405
3514.892493	545659.066959	41.160410
3514.775768	545466.954197	41.165415
3514.422392	545270.801214	41.170420
3514.234713	545082.717331	41.175424
3514.353143	544895.890738	41.180429
3513.933462	544696.218098	41.185434
3513.750398	544514.613554	41.190439
3513.697945	544321.366497	41.195444
3513.503270	544138.551056	41.200448
3513.208251	543954.843106	41.205453
3513.018615	543772.423939	41.210458
3513.370535	543593.338509	41.215463
3513.304916	543424.678259	41.220468
3513.429763	543241.598754	41.225472
3513.203054	543070.493832	41.230477
3512.908354	542884.405717	41.235482
3512.838426	542710.403989	41.240487
3512.405510	542537.210954	41.245492
3512.871091	542357.687709	41.250496
3511.930543	542197.095900	41.255501
3512.085536	542024.408018	41.260506
3511.970790	541857.143014	41.265511
3511.515240	541701.299246	41.270516
3511.480654	541543.878671	41.275520
3511.764725	541390.532195	41.280525
3512.025809	541225.565017	41.285530
3511.459305	541067.365931	41.290535
3511.453504	540905.605887	41.295540
3511.245989	540759.825136	41.300544
3511.103894	540613.227466	41.305549
3511.167577	540453.865985	41.310554
3510.908231	540301.798438	41.315559
3510.716294	540152.787955	41.320564
3510.972622	540001.693226	41.325568
3510.841400	539858.657717	41.330573
3510.824741	539701.161055	41.335578
3510.637395	539571.767635	41.340583
3510.066051	539425.877159	41.345588
3510.287635	539275.332702	41.350592
3509.914842	539140.730326	41.355597
3510.099548	538990.641126	41.360602
3510.034870	538863.737512	41.365607
3509.476181	538730.065520	41.370612
3509.663191	538591.948220	41.375616
3509.042629	538464.221286	41.380621
3509.538564	538335.665102	41.385626
3509.100405	538211.379667	41.390631
3508.851588	538091.492238	41.395636
3509.158756	537964.370808	41.400640
3508.862992	537849.370069	41.405645
3508.866507	537718.720231	41.410650
3508.934640	537612.417696	41.415655
3508.395315	537499.364159	41.420660
3508.541207	537373.671130	41.425664
3508.579626	537263.092362	41.430669
3508.447504	537151.532583	41.435674
3508.484925	537033.352202	41.440679
3507.903222	536924.779549	41.445684
3507.961330	536814.093171	41.450688
3507.854166	536708.464695	41.455693
3507.723128	536586.883866	41.460698
3508.431688	536488.575756	41.465703
3507.808410	536385.491208	41.470708
3507.819756	536277.575765	41.475712
3507.512617	536173.987322	41.480717
3508.272649	536071.339322	41.485722
3507.852824	535956.642860	41.490727
3507.647514	535853.589660	41.495732
3507.585339	535746.989896	41.500736
3507.534226	535655.790209	41.505741
3507.326566	535543.473142	41.510746
3507.112868	535448.471748	41.515751
3507.216546	535361.826492	41.520756
3507.612319	535249.463291	41.525760
3507.511432	535162.697516	41.530765
3507.094208	535061.130721	41.535770
3507.056901	534974.605472	41.540775
3506.848877	534876.981385	41.545780
3507.272711	534773.066539	41.550784
3507.144814	534685.345307	41.555789
3506.983580	534579.657390	41.560794
3507.012413	534495.232898	41.565799
3507.213902	534410.176901	41.570804
3506.766978	534313.038780	41.575808
3506.490075	534226.646474	41.580813
3506.779049	534127.177429	41.585818
3506.593509	534039.561457	41.590823
3506.425456	533952.747644	41.595828
3506.837889	533871.632306	41.600832
3506.820968	533793.201099	41.605837
3506.515932	533695.885225	41.610842
3506.529035	533606.272018	41.615847
3506.061584	533522.270797	41.620852
3506.653862	533435.737945	41.625856
3506.289344	533344.822396	41.630861
3506.291498	533269.254683	41.635866
3505.818611	533190.890777	41.640871
3505.951497	533119.128075	41.645876
3506.281673	533035.855447	41.650880
3505.904906	532959.841435	41.655885
3505.934584	532882.454724	41.660890
3506.218476	532795.764205	41.665895
3506.001215	532713.128506	41.670900
3506.357556	532630.755453	41.675904
3505.714124	532555.787514	41.680909
3505.813188	532479.243510	41.685914
3506.213355	532411.312090	41.690919
3505.622443	532336.888542	41.695924
3505.529161	532254.985860	41.700928
3505.652786	532183.420820	41.705933
3505.852626	532110.383395	41.710938
3505.427221	532028.682017	41.715943
3505.381776	531967.161675	41.720948
3505.672828	531882.729695	41.725952
3505.573941	531820.763826	41.730957
3505.647355	531751.016837	41.735962
3505.737963	531670.441327	41.740967
3505.561644	531608.889306	41.745972
3505.612555	531534.411637	41.750976
3505.291678	531467.040656	41.755981
3505.688003	531394.572862	41.760986
3505.492025	531325.217979	41.765991
3505.251023	531252.546457	41.770996
3505.574557	531179.937740	41.776000
3505.352434	531111.391434	41.781005
3505.448338	531044.658357	41.786010
3505.377614	530969.994978	41.791015
3505.050865	530905.643232	41.796020
3505.126412	530841.228567	41.801024
3505.435086	530771.288666	41.806029
3504.866863	530706.469969	41.811034
3505.413790	530630.348954	41.816039
3505.097439	530566.144982	41.821044
3505.239997	530498.596170	41.826048
3504.843185	530439.993566	41.831053
3504.869418	530379.965255	41.836058
3505.089954	530310.036601	41.841063
3504.494169	530253.226592	41.846068
3504.926206	530189.609303	41.851072
3504.992306	530124.890438	41.856077
3505.185956	530069.467495	41.861082
3504.597187	530002.986715	41.866087
3504.704780	529945.159478	41.871092
3504.836633	529877.206263	41.876096
3504.810290	529821.111492	41.881101
3504.491172	529765.062039	41.886106
3504.590744	529703.206310	41.891111
3504.353915	529652.733379	41.896116
3504.817175	529585.129950	41.901120
3504.773051	529537.547415	41.906125
3504.307186	529477.440466	41.911130
3504.679672	529421.231561	41.916135
3504.582948	529361.922754	41.921140
3504.573607	529301.492158	41.926144
3504.572245	529243.426980	41.931149
3504.397325	529195.662117	41.936154
3504.772808	529130.839841	41.941159
3504.253987	529083.279166	41.946164
3504.767879	529019.995997	41.951168
3504.859689	528970.174357	41.956173
3504.518330	528907.124455	41.961178
3504.812362	528849.011568	41.966183
3503.993410	528791.776688	41.971188
3504.399773	528724.530221	41.976192
3504.332147	528682.941370	41.981197
3504.263305	528635.057235	41.986202
3504.614220	528574.869414	41.991207
3504.747279	528530.680340	41.996212
3504.662633	528464.667306	42.001216
3504.193657	528411.657196	42.006221
3504.349945	528354.167922	42.011226
3504.572616	528289.566738	42.016231
3504.627442	528229.070864	42.021236
3504.663730	528183.838036	42.026240
3504.273837	528139.326112	42.031245
3504.258374	528077.178445	42.036250
3504.704754	528015.411903	42.041255
3504.389154	527969.779813	42.046260
3504.616147	527900.895003	42.051264
3504.589622	527852.145224	42.056269
3504.243557	527801.128156	42.061274
3504.383334	527740.012428	42.066279
3504.416587	527688.633702	42.071284
3504.356516	527639.787625	42.076288
3504.370604	527589.217359	42.081293
3503.998102	527532.612659	42.086298
3504.383311	527475.386135	42.091303
3504.178380	527429.180913	42.096308
3504.195356	527371.960876	42.101312
3504.443155	527323.418294	42.106317
3504.061339	527269.735244	42.111322
3504.121737	527217.292734	42.116327
3504.102339	527164.761697	42.121332
3503.960684	527116.782643	42.126336
3503.997368	527072.502948	42.131341
3503.936436	527019.272634	42.136346
3504.121799	526966.457101	42.141351
3504.391314	526915.491927	42.146356
3504.322040	526867.601445	42.151360
3503.743266	526819.538226	42.156365
3504.190533	526767.335949	42.161370
3504.143740	526711.130374	42.166375
3504.200722	526666.392831	42.171380
3504.094916	526614.779721	42.176384
3503.978020	526579.236358	42.181389
3503.902004	526518.652273	42.186394
3504.251120	526479.510169	42.191399
3504.089263	526428.308022	42.196404
3504.362579	526380.211354	42.201408
3504.157501	526331.685240	42.206413
3503.828039	526274.514369	42.211418
3504.189140	526227.108690	42.216423
3503.705258	526184.720422	42.221428
3504.115028	526127.232395	42.226432
3504.212599	526078.104162	42.231437
3504.129398	526028.399406	42.236442
3504.242317	525976.497912	42.241447
3504.147780	525927.650881	42.246452
3504.277533	525870.003823	42.251456
3503.935760	525821.748981	42.256461
3504.023960	525769.548285	42.261466
3504.501442	525723.230918	42.266471
3503.921204	525671.990211	42.271476
3504.070451	525632.070729	42.276480
3503.874734	525571.803194	42.281485
3503.825214	525525.416024	42.286490
3504.282369	525465.650908	42.291495
3503.823076	525417.715134	42.296500
3503.613190	525376.188396	42.301504
3503.805685	525333.541031	42.306509
3503.715958	525282.927746	42.311514
3504.010753	525242.480692	42.316519
3503.136112	525211.132007	42.321524
3503.683163	525155.683826	42.326528
3503.856516	525121.653049	42.331533
3503.459695	525070.935618	42.336538
3503.621071	525021.592049	42.341543
3503.529406	524996.669956	42.346548
3503.861639	524938.936981	42.351552
3503.876156	524900.597952	42.356557
3503.895895	524852.686353	42.361562
3503.993324	524807.331734	42.366567
3503.835428	524764.787452	42.371572
3504.009316	524713.979852	42.376576
3503.606278	524665.226570	42.381581
3503.475721	524620.360193	42.386586
3503.622069	524572.276750	42.391591
3503.505749	524534.712703	42.396596
3503.522314	524495.767652	42.401600
3503.590114	524454.698614	42.406605
3503.472047	524419.754202	42.411610
3503.663925	524371.360679	42.416615
3503.316003	524331.917701	42.421620
3503.210677	524289.817135	42.426624
3503.560415	524248.552452	42.431629
3503.307933	524204.963136	42.436634
3503.531716	524167.798548	42.441639
3503.340618	524128.834363	42.446644
3503.192890	524097.369932	42.451648
3503.634264	524056.946858	42.456653
3503.366936	524017.742311	42.461658
3503.490334	523977.166956	42.466663
3503.129037	523942.662189	42.471668
3503.141324	523901.801612	42.476672
3503.253568	523867.827531	42.481677
3503.216699	523834.531521	42.486682
3503.340998	523786.045634	42.491687
3503.352274	523755.059466	42.496692
3503.516738	523711.756328	42.501696
3503.596728	523675.973048	42.506701
3503.137646	523641.583483	42.511706
3503.185293	523599.809612	42.516711
3503.363170	523563.708509	42.521716
3503.381420	523512.668654	42.526720
3503.292554	523479.530998	42.531725
3502.909594	523444.726023	42.536730
3503.465509	523406.449608	42.541735
3503.065136	523375.929680	42.546740
3503.252465	523329.649171	42.551744
3503.154418	523302.659213	42.556749
3502.935139	523260.724290	42.561754
3503.175452	523223.655277	42.566759
3502.968677	523198.596592	42.571764
3503.092703	523161.998954	42.576768
3502.953955	523130.027017	42.581773
3502.893114	523099.302472	42.586778
3503.173921	523061.521338	42.591783
3502.807657	523033.464131	42.596788
3503.221705	522985.736404	42.601792
3503.441193	522947.561418	42.606797
3503.113922	522914.812155	42.611802
3503.299662	522879.564523	42.616807
3503.051644	522841.008523	42.621812
3503.393799	522798.329787	42.626816
3503.229468	522764.295179	42.631821
3503.067574	522724.516203	42.636826
3503.407626	522693.022953	42.641831
3502.918224	522654.705520	42.646836
3502.934678	522625.580196	42.651840
3502.965441	522592.270576	42.656845
3503.089167	522551.035842	42.661850
3502.980709	522522.181660	42.666855
3502.763484	522507.553185	42.671860
3503.010292	522470.581856	42.676864
3503.252951	522442.781359	42.681869
3503.449713	522397.705440	42.686874
3503.393262	522364.308054	42.691879
3502.917434	522333.747108	42.696884
3502.932513	522286.431691	42.701888
3503.272951	522255.038130	42.706893
3503.088149	522219.191399	42.711898
3503.242361	522174.574837	42.716903
3503.266778	522146.102269	42.721908
3502.975592	522107.500493	42.726912
3503.218362	522075.113962	42.731917
3502.923013	522038.729690	42.736922
3503.038786	521997.696049	42.741927
3503.172804	521967.291309	42.746932
3503.002091	521931.189678	42.751936
3502.870411	521894.678770	42.756941
3503.054274	521872.781670	42.761946
3502.992012	521835.302421	42.766951
3502.947907	521815.607405	42.771956
3503.534242	521769.712935	42.776960
3503.257448	521744.208933	42.781965
3503.111089	521699.536793	42.786970
3503.134467	521653.074472	42.791975
3503.069021	521623.707779	42.796980
3503.356179	521589.801499	42.801985
3503.129402	521549.777198	42.806989
3503.054038	521519.303252	42.811994
3502.926525	521491.911126	42.816999
3503.009229	521438.485047	42.822004
3503.012261	521406.537338	42.827009
3502.823104	521374.165949	42.832013
3502.978479	521338.566279	42.837018
3503.077304	521313.103791	42.842023
3502.906432	521279.066444	42.847028
3503.027402	521250.325007	42.852033
3503.337691	521222.511472	42.857037
3503.203395	521185.999052	42.862042
3503.323716	521145.466021	42.867047
3503.145785	521116.821203	42.872052
3503.004025	521072.549400	42.877057
3503.065225	521033.335406	42.882061
3503.163069	521007.217406	42.887066
3503.030602	520971.409603	42.892071
3502.973733	520939.722069	42.897076
3503.104702	520901.454280	42.902081
3502.843775	520862.541878	42.907085
3502.987283	520834.098401	42.912090
3503.048300	520791.759419	42.917095
3502.907347	520762.452994	42.922100
3502.969202	520724.548207	42.927105
3502.940333	520692.704560	42.932109
3503.083697	520651.460964	42.937114
3503.044035	520623.751049	42.942119
3502.640602	520600.229916	42.947124
3503.252815	520568.890934	42.952129
3502.895393	520536.241361	42.957133
3502.665456	520509.518294	42.962138
3503.035307	520472.522348	42.967143
3503.089211	520443.537665	42.972148
3503.017065	520408.374102	42.977153
3503.261218	520367.113957	42.982157
3502.776031	520334.332596	42.987162
3502.885609	520303.071216	42.992167
3503.214763	520269.810219	42.997172
3503.072207	520228.005095	43.002177
3503.218249	520198.854368	43.007181
3502.832718	520168.324852	43.012186
3503.387231	520117.138291	43.017191
3502.943539	520094.731230	43.022196
3502.738194	520057.218920	43.027201
3502.867254	520026.256241	43.032205
3502.895763	519993.091745	43.037210
3502.880410	519965.628677	43.042215
3502.829839	519926.580058	43.047220
3503.074382	519894.137636	43.052225
3502.976974	519871.978694	43.057229
3502.733385	519848.129004	43.062234
3502.769187	519809.973734	43.067239
3502.867710	519787.733769	43.072244
3502.949209	519748.059331	43.077249
3503.103555	519725.860975	43.082253
3502.706255	519690.947734	43.087258
3502.247892	519649.895521	43.092263
3502.398027	519624.774651	43.097268
3503.072053	519594.582929	43.102273
3502.647220	519565.872456	43.107277
3502.512166	519538.729532	43.112282
3503.031461	519506.495416	43.117287
3502.790911	519480.931104	43.122292
3503.092812	519448.075514	43.127297
3502.716892	519413.158231	43.132301
3502.800597	519376.052635	43.137306
3502.767111	519352.572560	43.142311
3502.840950	519328.218981	43.147316
3502.914468	519291.417126	43.152321
3502.965680	519262.581534	43.157325
3502.751408	519225.471497	43.162330
3502.947235	519192.732594	43.167335
3502.699767	519174.022948	43.172340
3502.620168	519131.952659	43.177345
3502.756376	519105.018650	43.182349
3502.629193	519079.587138	43.187354
3502.845742	519036.815287	43.192359
3503.117361	519020.897389	43.197364
3502.709488	518974.845783	43.202369
3502.609706	518953.945690	43.207373
3502.402789	518937.900564	43.212378
3502.545059	518905.824495	43.217383
3502.410083	518875.908271	43.222388
3502.909884	518847.757987	43.227393
3502.983039	518816.045259	43.232397
3502.294061	518804.308563	43.237402
3502.451985	518760.990572	43.242407
3502.547604	518741.067744	43.247412
3502.584879	518712.182755	43.252417
3502.670850	518689.741349	43.257421
3502.641490	518657.137001	43.262426
3502.424957	518614.078414	43.267431
3502.207784	518604.586546	43.272436
3502.456644	518578.339573	43.277441
3502.711920	518557.585223	43.282445
3502.610330	518543.791271	43.287450
3502.765286	518512.518714	43.292455
3502.684425	518478.208324	43.297460
3503.004050	518441.315474	43.302465
3502.930305	518418.948877	43.307469
3502.269673	518391.532643	43.312474
3502.575040	518372.685465	43.317479
3502.695220	518335.924169	43.322484
3502.580115	518303.785932	43.327489
3502.389343	518287.737527	43.332493
3502.565220	518265.231030	43.337498
3502.744195	518239.145486	43.342503
3502.580728	518206.006508	43.347508
3502.643351	518164.818336	43.352513
3502.417949	518150.841644	43.357517
3502.675007	518111.689544	43.362522
3502.667551	518085.884729	43.367527
3502.780782	518066.512602	43.372532
3502.624181	518029.239124	43.377537
3502.675893	517993.294001	43.382541
3502.310012	517972.333006	43.387546
3502.974446	517929.034362	43.392551
3503.005377	517916.328018	43.397556
3502.550647	517881.973502	43.402561
3502.935280	517864.272561	43.407565
3502.704982	517831.294283	43.412570
3502.976434	517800.001966	43.417575
3502.703931	517779.883003	43.422580
3502.899126	517739.680990	43.427585
3502.795677	517707.791555	43.432589
3502.580452	517683.933656	43.437594
3502.585661	517639.779008	43.442599
3502.877776	517611.658499	43.447604
3502.728645	517585.622766	43.452609
3503.030789	517556.643712	43.457613
3502.768639	517526.290679	43.462618
3503.077447	517493.580525	43.467623
3502.763210	517459.203083	43.472628
3502.680298	517433.358374	43.477633
3502.716860	517393.684078	43.482637
3502.406017	517368.227549	43.487642
3502.853415	517343.661084	43.492647
3502.661491	517319.446088	43.497652
3502.599996	517286.541037	43.502657
3502.764922	517253.651079	43.507661
3502.550698	517226.919116	43.512666
3502.727957	517195.539266	43.517671
3502.608395	517181.041054	43.522676
3502.771778	517147.747836	43.527681
3502.514562	517117.997999	43.532685
3502.489635	517095.722452	43.537690
3502.428953	517064.681765	43.542695
3502.670442	517046.195546	43.547700
3502.622222	517013.791837	43.552705
3502.695492	516988.829299	43.557709
3502.692074	516961.055884	43.562714
3502.803103	516922.527987	43.567719
3502.691712	516897.795646	43.572724
3502.664957	516874.814329	43.577729
3502.558852	516838.638700	43.582733
3502.341292	516820.324424	43.587738
3502.636425	516785.295986	43.592743
3502.797287	516757.042929	43.597748
3502.410067	516729.026325	43.602753
3502.322564	516706.255808	43.607757
3502.237110	516680.258852	43.612762
3502.531270	516656.773564	43.617767
3502.344627	516628.977581	43.622772
3502.425637	516611.221458	43.627777
3502.477639	516584.295589	43.632781
3502.290046	516559.272047	43.637786
3502.519029	516534.385268	43.642791
3502.354761	516511.575966	43.647796
3502.171212	516499.405766	43.652801
3502.444212	516463.270970	43.657805
3502.294249	516441.517901	43.662810
3502.309213	516417.117890	43.667815
3502.497109	516389.767225	43.672820
3502.438944	516372.889398	43.677825
3502.714885	516341.341014	43.682829
3502.424490	516317.744476	43.687834
3502.621318	516284.746415	43.692839
3502.586793	516262.471009	43.697844
3502.376639	516237.198345	43.702849
3502.671859	516208.973663	43.707853
3502.313705	516182.161241	43.712858
3502.440199	516153.710655	43.717863
3502.718715	516137.082604	43.722868
3502.524238	516105.758112	43.727873
3502.338172	516082.044114	43.732877
3502.419778	516053.499487	43.737882
3502.576422	516021.464835	43.742887
3502.668691	515994.279495	43.747892
3502.396889	515971.889310	43.752897
3502.559251	515947.616760	43.757901
3502.706003	515928.387628	43.762906
3502.635493	515891.699862	43.767911
3502.479202	515859.915173	43.772916
3502.224340	515840.294719	43.777921
3502.247759	515819.925183	43.782925
3502.285399	515802.527641	43.787930
3502.307158	515780.242695	43.792935
3502.446242	515747.554798	43.797940
3502.555706	515728.734478	43.802945
3502.754528	515700.473345	43.807949
3502.267957	515683.560515	43.812954
3502.564221	515651.503276	43.817959
3502.777831	515618.097716	43.822964
3502.776759	515596.975490	43.827969
3502.988031	515560.394228	43.832973
3502.596058	515540.139330	43.837978
3502.433933	515513.043039	43.842983
3502.574561	515480.757564	43.847988
3502.443975	515456.025614	43.852993
3502.665560	515427.609143	43.857997
3502.562722	515403.225666	43.863002
3502.747159	515367.958787	43.868007
3502.658257	515343.623449	43.873012
3502.414206	515318.959322	43.878017
3502.656556	515293.513684	43.883021
3502.282940	515276.683601	43.888026
3502.611148	515232.218888	43.893031
3502.444471	515212.482990	43.898036
3502.377481	515181.842337	43.903041
3502.183873	515147.037027	43.908045
3502.304999	515140.666139	43.913050
3502.367476	515111.114273	43.918055
3502.061774	515105.918882	43.923060
3502.239496	515074.483710	43.928065
3502.222843	515041.767962	43.933069
3502.478058	515025.495094	43.938074
3502.722845	514994.301372	43.943079
3502.292965	514973.950712	43.948084
3502.561903	514962.515360	43.953089
3502.438883	514931.378731	43.958093
3501.995726	514904.425803	43.963098
3502.410740	514874.818573	43.968103
3502.678326	514852.998017	43.973108
3502.115183	514828.685153	43.978113
3502.626136	514796.542109	43.983117
3502.331854	514779.850316	43.988122
3502.110090	514753.366787	43.993127
3502.264926	514728.437873	43.998132
3502.277466	514705.396406	44.003137
3502.374650	514693.685070	44.008141
3502.370154	514662.831881	44.013146
3502.219181	514636.992507	44.018151
3502.427069	514615.029621	44.023156
3502.069553	514590.432263	44.028161
3502.418477	514569.102755	44.033165
3501.931748	514542.912130	44.038170
3502.580678	514519.267168	44.043175
3502.499520	514496.895335	44.048180
3502.549288	514475.309742	44.053185
3502.428691	514456.775567	44.058189
3502.499722	514433.674130	44.063194
3502.166919	514405.896403	44.068199
3502.752879	514380.798944	44.073204
3502.564389	514358.443589	44.078209
3502.683152	514326.259651	44.083213
3502.430674	514306.233313	44.088218
3502.727856	514281.936856	44.093223
3502.490054	514250.009893	44.098228
3501.930422	514222.166261	44.103233
3502.201296	514180.681667	44.108237
3502.323703	514188.325978	44.113242
3502.270263	514151.530097	44.118247
3502.378757	514139.009863	44.123252
3502.210672	514119.474290	44.128257
3502.489069	514081.265327	44.133261
3502.203336	514067.545949	44.138266
3502.620797	514041.768259	44.143271
3502.433879	514017.143333	44.148276
3502.185776	513992.729554	44.153281
3502.783243	513962.940732	44.158285
3502.374362	513937.241020	44.163290
3502.555400	513894.811616	44.168295
3502.372032	513879.664425	44.173300
3502.091333	513855.003387	44.178305
3502.834010	513830.586398	44.183309
3502.529482	513816.063007	44.188314
3502.596785	513786.457144	44.193319
3502.526399	513766.099178	44.198324
3502.697902	513739.250001	44.203329
3502.753277	513704.704824	44.208333
3502.540508	513679.427881	44.213338
3502.372743	513647.034862	44.218343
3502.339021	513631.006995	44.223348
3502.369751	513609.977623	44.228353
3502.621387	513578.174623	44.233357
3502.228163	513552.572597	44.238362
3502.468521	513522.384632	44.243367
3502.333749	513499.918693	44.248372
3502.572865	513468.722422	44.253377
3502.747073	513448.678864	44.258381
3502.520124	513433.437128	44.263386
3502.175594	513405.558379	44.268391
3502.376328	513378.703956	44.273396
3502.067099	513337.811311	44.278401
3502.055279	513328.586353	44.283405
3501.801189	513303.063055	44.288410
3502.118713	513283.450736	44.293415
3502.283985	513262.954521	44.298420
3502.521921	513248.951161	44.303425
3502.608934	513219.189761	44.308429
3502.145306	513204.387965	44.313434
3502.314129	513170.680951	44.318439
3502.489562	513149.930887	44.323444
3502.147081	513118.824334	44.328449
3502.358607	513101.799702	44.333453
3502.209368	513091.688400	44.338458
3502.438314	513062.509626	44.343463
3502.071865	513048.801798	44.348468
3502.218639	513023.417289	44.353473
3502.635378	512988.612417	44.358477
3502.310692	512969.906329	44.363482
3502.148738	512944.216770	44.368487
3502.387996	512914.481448	44.373492
3502.368490	512906.669203	44.378497
3502.515355	512874.124578	44.383501
3502.350829	512853.578238	44.388506
3502.216248	512823.749632	44.393511
3502.563978	512795.207295	44.398516
3502.690042	512784.195759	44.403521
3502.759257	512755.999213	44.408525
3502.338323	512728.231837	44.413530
3502.334068	512692.533719	44.418535
3502.382067	512670.996018	44.423540
3502.036945	512648.662280	44.428545
3502.177554	512622.521667	44.433549
3501.922003	512608.644879	44.438554
3502.238979	512582.275056	44.443559
3502.043635	512562.287729	44.448564
3501.765316	512545.086530	44.453569
3502.147354	512515.983634	44.458573
3501.908594	512511.281073	44.463578
3502.141789	512477.965747	44.468583
3502.372977	512466.988025	44.473588
3502.298158	512441.536093	44.478593
3502.383924	512418.630704	44.483597
3502.099907	512401.480638	44.488602
3502.307833	512383.800189	44.493607
3502.377673	512362.208190	44.498612
3502.343611	512342.497989	44.503617
3502.612382	512309.580113	44.508621
3502.292839	512291.931205	44.513626
3502.131104	512256.206051	44.518631
3502.249573	512236.824932	44.523636
3502.581585	512221.394037	44.528641
3502.678792	512192.183519	44.533645
3502.360853	512164.348566	44.538650
3502.795948	512132.967535	44.543655
3502.505397	512102.707838	44.548660
3502.385873	512089.011062	44.553665
3502.493738	512057.680783	44.558669
3502.425030	512029.605080	44.563674
3502.539433	512006.139888	44.568679
3502.186313	511978.864709	44.573684
3501.992404	511958.624169	44.578689
3502.344552	511924.734341	44.583693
3502.125379	511906.161677	44.588698
3502.585151	511893.483912	44.593703
3502.529243	511870.347544	44.598708
3502.316031	511846.832216	44.603713
3502.711646	511817.624903	44.608717
3502.300727	511796.005989	44.613722
3502.010939	511767.712035	44.618727
3502.460072	511744.900273	44.623732
3502.721087	511725.748390	44.628737
3502.609996	511702.166501	44.633741
3502.475914	511679.193259	44.638746
3502.463914	511646.771345	44.643751
3502.366300	511620.665927	44.648756
3502.174855	511594.625487	44.653761
3502.517595	511573.443636	44.658765
3502.308312	511547.305031	44.663770
3502.571141	511527.144070	44.668775
3502.287171	511495.066684	44.673780
3502.581005	511480.952002	44.678785
3502.561089	511453.018827	44.683789
3502.206131	511426.801812	44.688794
3502.535076	511407.033804	44.693799
3502.455191	511380.370483	44.698804
3502.194057	511353.231048	44.703809
3502.443764	511312.195051	44.708813
3502.509334	511289.543089	44.713818
3502.468030	511272.101728	44.718823
3502.356963	511239.744714	44.723828
3502.490403	511218.342759	44.728833
3502.629674	511197.494568	44.733837
3502.599728	511173.041891	44.738842
3502.380324	511131.372378	44.743847
3502.593333	511116.614346	44.748852
3502.502725	511081.732393	44.753857
3502.766658	511064.596271	44.758861
3502.021853	511030.168986	44.763866
3502.016740	511018.873904	44.768871
3502.260291	510984.040565	44.773876
3502.038527	510974.140725	44.778881
3502.215937	510947.688683	44.783885
3502.060781	510932.836464	44.788890
3501.926453	510913.845850	44.793895
3502.585292	510887.823066	44.798900
3502.293673	510872.790304	44.803905
3502.391546	510831.776528	44.808909
3502.232945	510822.068466	44.813914
3501.949356	510806.681381	44.818919
3502.236785	510767.856793	44.823924
3502.073256	510761.023911	44.828929
3502.183962	510734.480990	44.833933
3502.044114	510715.188390	44.838938
3502.042887	510693.504016	44.843943
3501.996464	510668.851306	44.848948
3502.166469	510666.807698	44.853953
3502.191302	510617.433377	44.858957
3502.044543	510623.306068	44.863962
3502.393849	510587.244978	44.868967
3502.278087	510572.134098	44.873972
3502.146213	510549.108227	44.878977
3502.034538	510523.204669	44.883981
3502.013484	510511.508221	44.888986
3502.108758	510478.310459	44.893991
3502.583292	510451.811248	44.898996
3502.003756	510444.589075	44.904001
3502.164773	510407.296068	44.909005
3502.152344	510395.799902	44.914010
3502.294963	510364.763011	44.919015
3502.328904	510349.527735	44.924020
3501.986199	510321.491242	44.929025
3502.131241	510311.786006	44.934029
3502.298332	510285.031739	44.939034
3502.447106	510276.586668	44.944039
3502.111955	510246.531617	44.949044
3502.148955	510234.775473	44.954049
3502.263129	510196.934457	44.959053
3502.157939	510190.344373	44.964058
3502.365820	510158.792561	44.969063
3502.172383	510148.080828	44.974068
3502.164721	510127.052186	44.979073
3502.576997	510092.442538	44.984077
3502.176892	510074.500774	44.989082
3502.055965	510055.759071	44.994087
3502.009297	510032.466935	44.999092
3501.705128	510017.233481	45.004097
3502.249626	509985.175012	45.009101
3501.933684	509979.525398	45.014106
3501.910948	509954.615589	45.019111
3501.927431	509927.178030	45.024116
3501.832261	509918.871569	45.029121
3502.257659	509902.515819	45.034125
3502.259593	509884.107793	45.039130
3502.150060	509865.263197	45.044135
3502.180144	509846.396851	45.049140
3502.106431	509826.588415	45.054145
3502.260717	509791.412984	45.059149
3502.240120	509776.185573	45.064154
3502.264348	509748.090836	45.069159
3502.053873	509726.084501	45.074164
3501.926563	509714.000461	45.079169
3502.066701	509689.670032	45.084173
3501.870251	509671.897794	45.089178
3502.024634	509659.215110	45.094183
3502.066479	509643.876973	45.099188
3502.334086	509618.517924	45.104193
3502.672932	509589.415681	45.109197
3502.465173	509569.829476	45.114202
3502.099003	509540.735976	45.119207
3502.390655	509517.894677	45.124212
3502.372852	509493.588487	45.129217
3502.400639	509473.208989	45.134221
3502.261649	509452.199775	45.139226
3502.182567	509423.061357	45.144231
3502.240714	509399.550128	45.149236
3501.947097	509378.917905	45.154241
3502.371584	509358.274774	45.159245
3501.938113	509331.158242	45.164250
3502.092282	509314.541413	45.169255
3502.080917	509295.680779	45.174260
3502.134696	509277.415195	45.179265
3502.500386	509253.956735	45.184269
3502.094354	509233.039184	45.189274
3502.108959	509213.720488	45.194279
3502.091260	509186.589414	45.199284
3502.239439	509177.588996	45.204289
3502.071669	509149.573377	45.209293
3502.108298	509139.430292	45.214298
3502.000985	509107.420825	45.219303
3502.333766	509094.810743	45.224308
3502.050663	509073.218169	45.229313
3502.211533	509051.052123	45.234317
3502.282595	509033.993980	45.239322
3501.857684	509014.188616	45.244327
3502.297334	508992.886933	45.249332
3502.272810	508968.933933	45.254337
3502.410130	508953.731495	45.259341
3502.077447	508932.701212	45.264346
3502.044006	508924.838480	45.269351
3502.333121	508896.599955	45.274356
3502.181349	508872.363978	45.279361
3502.189921	508844.169004	45.284365
3501.949259	508821.459850	45.289370
3502.137056	508805.644166	45.294375
3502.133157	508780.578042	45.299380
3502.188691	508769.271717	45.304385
3502.379933	508739.585460	45.309389
3502.266901	508713.779656	45.314394
3502.148797	508692.009513	45.319399
3502.142051	508670.020262	45.324404
3502.273850	508663.241274	45.329409
3501.743524	508633.515769	45.334413
3501.599593	508622.391675	45.339418
3501.942599	508602.415799	45.344423
3501.931970	508570.743128	45.349428
3502.168198	508569.748090	45.354433
3502.504081	508542.207697	45.359437
3502.222132	508517.436560	45.364442
3502.291404	508495.233460	45.369447
3502.460737	508475.334867	45.374452
3502.406682	508449.368091	45.379457
3502.497877	508419.091481	45.384461
3502.545057	508397.446477	45.389466
3502.401425	508379.613953	45.394471
3502.677243	508350.922471	45.399476
3502.417661	508327.660651	45.404481
3502.458323	508294.617561	45.409485
3502.292393	508274.266478	45.414490
3502.383447	508251.252597	45.419495
3502.331145	508226.142585	45.424500
3502.283800	508210.312389	45.429505
3502.184029	508180.670245	45.434509
3502.004097	508158.656710	45.439514
3501.728368	508131.916832	45.444519
3501.925176	508116.401607	45.449524
3501.776433	508109.666011	45.454529
3501.872866	508085.490937	45.459533
3501.943033	508074.585290	45.464538
3501.907159	508058.500945	45.469543
3501.990239	508021.768589	45.474548
3501.960102	508007.297337	45.479553
3501.853713	508001.362121	45.484557
3502.405264	507989.221403	45.489562
3501.993682	507958.467218	45.494567
3502.124797	507938.220745	45.499572
3502.106150	507928.690663	45.504577
3501.926824	507896.740100	45.509581
3502.082083	507881.432842	45.514586
3502.113457	507857.368382	45.519591
3502.510937	507835.768887	45.524596
3501.982400	507822.535113	45.529601
3502.023746	507802.958131	45.534605
3502.240962	507776.292192	45.539610
3502.101248	507751.497579	45.544615
3502.222559	507728.175502	45.549620
3502.036466	507708.885982	45.554625
3501.795795	507696.666535	45.559629
3502.203135	507672.795457	45.564634
3502.197901	507650.400866	45.569639
3502.061370	507622.730441	45.574644
3502.124571	507613.540493	45.579649
3501.935763	507583.103908	45.584653
3501.966630	507571.396942	45.589658
3501.372451	507555.953752	45.594663
3501.861898	507532.775830	45.599668
3501.976092	507535.027910	45.604673
3501.566135	507525.457568	45.609677
3502.160531	507500.043873	45.614682
3501.796801	507493.997168	45.619687
3501.583030	507464.623468	45.624692
3501.327980	507451.498111	45.629697
3501.716187	507437.969997	45.634701
3501.956811	507429.054966	45.639706
3501.575938	507399.707136	45.644711
3502.018882	507388.389865	45.649716
3501.833343	507385.442733	45.654721
3501.598165	507352.642135	45.659725
3501.672722	507347.788195	45.664730
3501.383728	507338.854640	45.669735
3502.139769	507326.076242	45.674740
3501.825536	507301.307999	45.679745
3501.901698	507294.990990	45.684749
3501.765677	507269.791429	45.689754
3501.520845	507257.168717	45.694759
3501.803115	507244.363087	45.699764
3501.791649	507228.324444	45.704769
3501.937168	507202.828745	45.709773
3502.008502	507199.185858	45.714778
3501.613186	507173.421174	45.719783
3501.718381	507156.153691	45.724788
3502.008904	507162.615515	45.729793
3501.956716	507132.913333	45.734797
3501.833221	507116.690230	45.739802
3501.944941	507094.226120	45.744807
3502.215300	507078.193895	45.749812
3501.858309	507062.158391	45.754817
3501.898442	507015.341654	45.759821
3502.122866	506955.935867	45.764826
3501.649768	506851.895480	45.769831
3501.461767	506684.604250	45.774836
3501.365743	506484.306186	45.779841
3501.037318	506227.038462	45.784845
3500.561297	505928.170928	45.789850
3500.409928	505581.170207	45.794855
3499.932003	505183.157656	45.799860
3499.090087	504743.569096	45.804865
3498.517246	504262.302206	45.809869
3497.825380	503726.799715	45.814874
3497.099589	503163.178600	45.819879
3496.754427	502532.821070	45.824884
3495.673919	501879.439597	45.829889
3494.688440	501180.849622	45.834893
3493.691696	500428.027924	45.839898
3492.796648	499637.603160	45.844903
3492.052314	498800.527392	45.849908
3490.795475	497921.438662	45.854913
3489.493020	496999.247393	45.859917
3488.447429	496038.845731	45.864922
3487.163942	495032.528931	45.869927
3485.759312	493990.215805	45.874932
3484.219165	492907.508600	45.879937
3482.836888	491789.150251	45.884941
3481.363860	490636.838329	45.889946
3479.896601	489428.531217	45.894951
3478.170635	488196.783653	45.899956
3476.249999	486932.185413	45.904961
3474.500129	485624.467917	45.909965
3473.074183	484282.235824	45.914970
3471.474788	482915.309377	45.919975
3469.324926	481496.102185	45.924980
3467.742412	480059.749689	45.929985
3465.722081	478578.760090	45.934989
3464.118895	477068.707507	45.939994
3462.048243	475533.210050	45.944999
3459.815082	473946.836441	45.950004
3457.264851	472349.183481	45.955009
3455.383916	470719.718639	45.960013
3453.268017	469061.304948	45.965018
3450.823032	467366.818701	45.970023
3448.646209	465632.414370	45.975028
3446.282729	463896.342214	45.980033
3444.306140	462130.588877	45.985037
3441.554338	460330.520949	45.990042
3439.098843	458510.990347	45.995047
3436.837758	456666.441819	46.000052
3434.142397	454804.406557	46.005057
3431.525775	452916.702321	46.010061
3429.568815	451003.181610	46.015066
3426.622147	449058.880092	46.020071
3424.205408	447091.806162	46.025076
3421.651539	445117.401338	46.030081
3419.029386	443113.979377	46.035085
3415.987674	441083.816102	46.040090
3413.273770	439039.148165	46.045095
3410.392904	436966.625316	46.050100
3407.661432	434886.710788	46.055105
3404.740833	432776.199482	46.060109
3401.661349	430658.339349	46.065114
3398.634953	428525.140484	46.070119
3395.819959	426370.392005	46.075124
3392.947087	424207.716940	46.080129
3389.979502	422009.642985	46.085133
3387.017888	419804.133858	46.090138
3383.572341	417585.738948	46.095143
3380.951842	415360.947434	46.100148
3377.771716	413119.476800	46.105153
3374.897583	410855.559569	46.110157
3371.699169	408583.849134	46.115162
3368.137349	406298.061034	46.120167
3365.460642	403996.325250	46.125172
3362.252437	401675.815785	46.130177
3358.722774	399355.021158	46.135181
3355.557566	397009.018455	46.140186
3351.870391	394667.128425	46.145191
3348.507919	392299.323140	46.150196
3345.579397	389945.968868	46.155201
3342.150768	387573.097799	46.160205
3338.849930	385168.854512	46.165210
3335.537759	382772.638493	46.170215
3331.967190	380366.057483	46.175220
3328.828621	377961.195141	46.180225
3325.103002	375535.634226	46.185229
3321.893307	373100.809484	46.190234
3318.239071	370672.342327	46.195239
3314.698568	368231.020571	46.200244
3311.055420	365774.693119	46.205249
3307.354863	363311.382380	46.210253
3304.063736	360859.085732	46.215258
3300.384647	358392.468625	46.220263
3297.078914	355915.733594	46.225268
3293.193676	353444.408335	46.230273
3289.754051	350962.221926	46.235277
3286.062895	348474.394010	46.240282
3282.293972	345986.340827	46.245287
3278.923755	343495.779956	46.250292
3274.876019	341004.636683	46.255297
3271.331296	338508.865717	46.260301
3267.867386	336002.406741	46.265306
3264.058753	333511.218374	46.270311
3260.474704	330994.523617	46.275316
3256.846192	328489.423803	46.280321
3253.236588	325974.598327	46.285325
3249.326460	323452.057835	46.290330
3245.739230	320945.189761	46.295335
3242.020374	318411.684627	46.300340
3237.904880	315898.094237	46.305345
3234.136993	313367.287357	46.310349
3230.441873	310854.067865	46.315354
3226.212927	308345.991100	46.320359
3222.730066	305834.667953	46.325364
3218.611353	303320.902260	46.330369
3214.976587	300812.438730	46.335373
3211.329786	298294.291199	46.340378
3207.160617	295792.453656	46.345383
3203.757360	293297.186029	46.350388
3200.055500	290780.071662	46.355393
3195.917101	288276.645638	46.360397
3191.970027	285767.060409	46.365402
3187.702979	283269.754505	46.370407
3183.851610	280780.010392	46.375412
3179.480423	278294.693819	46.380417
3175.850923	275814.529273	46.385421
3172.009139	273326.352803	46.390426
3168.043467	270853.681284	46.395431
3164.150245	268386.125563	46.400436
3160.151424	265924.506821	46.405441
3156.262749	263455.299320	46.410445
3152.440760	261005.327838	46.415450
3148.163475	258535.410323	46.420455
3144.331351	256089.643914	46.425460
3140.167165	253645.667461	46.430465
3136.444199	251205.809131	46.435469
3132.692659	248763.244113	46.440474
3127.683918	246348.040722	46.445479
3124.219396	243925.665804	46.450484
3120.355675	241525.357010	46.455489
3116.111995	239117.393630	46.460493
3111.833765	236724.825238	46.465498
3107.647656	234339.791397	46.470503
3103.896022	231963.490256	46.475508
3099.868534	229600.314546	46.480513
3095.782351	227238.136008	46.485517
3091.552220	224891.666790	46.490522
3087.533733	222558.231411	46.495527
3083.385131	220208.494920	46.500532
3079.154750	217891.149582	46.505537
3074.794602	215583.818510	46.510541
3070.886201	213281.855186	46.515546
3066.467403	210991.397285	46.520551
3062.366560	208712.777008	46.525556
3058.160900	206446.495677	46.530561
3053.883475	204198.688322	46.535565
3049.661131	201954.107909	46.540570
3045.299356	199730.206755	46.545575
3041.029703	197507.672471	46.550580
3036.868812	195301.071751	46.555585
3032.444243	193102.620971	46.560589
3028.164003	190943.810329	46.565594
3023.977166	188783.777059	46.570599
3019.538843	186644.960494	46.575604
3014.930357	184517.876584	46.580609
3010.102844	182413.280039	46.585613
3005.922805	180320.749925	46.590618
3001.334945	178256.798512	46.595623
2996.793716	176206.001988	46.600628
2992.037632	174180.687028	46.605633
2987.479119	172170.249083	46.610637
2982.945292	170192.486592	46.615642
2978.285062	168238.168114	46.620647
2973.723927	166290.354337	46.625652
2968.711236	164376.129723	46.630657
2963.823866	162480.345794	46.635661
2958.642938	160626.652661	46.640666
2953.640214	158803.049078	46.645671
2949.052281	157003.362559	46.650676
2943.762595	155238.571186	46.655681
2937.783785	153513.099996	46.660685
2932.139598	151795.379573	46.665690
2926.348840	150114.652455	46.670695
2919.998099	148523.841376	46.675700
2913.291249	146993.551287	46.680705
2907.031820	145509.744838	46.685709
2900.517508	144095.317037	46.690714
2893.669672	142734.573816	46.695719
2887.539602	141412.499504	46.700724
2881.858325	140169.605622	46.705729
2875.659975	138970.120311	46.710733
2870.668999	137801.813213	46.715738
2864.714552	136689.917486	46.720743
2860.379292	135621.687265	46.725748
2854.625341	134589.323478	46.730753
2850.225470	133593.435596	46.735757
2845.754852	132630.604917	46.740762
2840.949420	131699.611232	46.745767
2835.981441	130792.348388	46.750772
2831.546567	129921.274398	46.755777
2827.578030	129079.045455	46.760781
2823.469760	128246.153202	46.765786
2818.924820	127453.284651	46.770791
2815.417721	126663.017120	46.775796
2811.473453	125898.983063	46.780801
2807.252512	125149.632947	46.785805
2803.935457	124396.887381	46.790810
2800.030375	123678.383320	46.795815
2796.414423	122954.480180	46.800820
2792.705943	122247.188727	46.805825
2788.514984	121546.496490	46.810829
2785.278545	120851.327514	46.815834
2780.788906	120181.762182	46.820839
2777.099436	119507.467706	46.825844
2773.657791	118859.902516	46.830849
2769.435284	118204.051524	46.835853
2765.837290	117561.009031	46.840858
2761.703563	116945.171579	46.845863
2758.068666	116324.103997	46.850868
2754.174732	115719.922633	46.855873
2750.450145	115113.448721	46.860877
2747.047710	114519.649925	46.865882
2742.671541	113933.399740	46.870887
2739.132708	113369.419539	46.875892
2734.953315	112794.829360	46.880897
2731.282512	112230.976483	46.885901
2728.048834	111670.446442	46.890906
2724.033507	111129.601063	46.895911
2720.034142	110576.111156	46.900916
2716.731894	110042.787015	46.905921
2712.676093	109498.235106	46.910925
2709.401805	108976.136116	46.915930
2705.604617	108451.494717	46.920935
2702.454931	107934.947599	46.925940
2699.093856	107417.398665	46.930945
2695.270588	106899.293827	46.935949
2692.194114	106382.593386	46.940954
2688.627303	105861.705815	46.945959
2685.376764	105345.060947	46.950964
2682.046027	104823.033976	46.955969
2678.763459	104309.880269	46.960973
2675.481426	103784.480610	46.965978
2671.900595	103264.474411	46.970983
2668.550515	102740.792410	46.975988
2665.133343	102218.540042	46.980993
2661.565172	101697.056672	46.985997
2658.311987	101170.143403	46.991002
2655.012264	100646.105664	46.996007
2651.990994	100116.720297	47.001012
2648.692633	99584.971866	47.006017
2645.055614	99060.262434	47.011021
2641.650249	98507.438000	47.016026
2637.914470	97971.247181	47.021031
2634.372184	97432.023293	47.026036
2631.627058	96901.542455	47.031041
2628.098616	96361.788203	47.036045
2624.693021	95809.176115	47.041050
2621.087271	95272.350131	47.046055
2617.752281	94715.972146	47.051060
2614.150442	94176.800840	47.056065
2610.936648	93627.463542	47.061069
2607.595239	93077.342664	47.066074
2603.903661	92518.353247	47.071079
2600.793115	91970.376537	47.076084
2597.087536	91417.953427	47.081089
2593.870402	90861.131600	47.086093
2590.231807	90291.349387	47.091098
2586.830069	89733.281186	47.096103
2583.594725	89165.490566	47.101108
2580.009841	88600.674674	47.106113
2576.436621	88039.577586	47.111117
2573.344897	87473.982302	47.116122
2569.668891	86902.568556	47.121127
2565.863028	86335.810520	47.126132
2562.520768	85763.846261	47.131137
2559.303503	85199.813652	47.136141
2555.848987	84627.787682	47.141146
2552.372222	84057.859877	47.146151
2549.055707	83477.425826	47.151156
2545.384069	82908.656413	47.156161
2541.549353	82327.691309	47.161165
2538.279650	81739.079705	47.166170
2534.849995	81180.608834	47.171175
2531.811761	80596.227563	47.176180
2528.351360	80017.042867	47.181185
2524.644463	79430.656231	47.186189
2521.132968	78847.617313	47.191194
2517.642756	78263.368134	47.196199
2514.196972	77678.044920	47.201204
2510.569823	77095.010343	47.206209
2506.894902	76511.335268	47.211213
2503.414047	75916.289167	47.216218
2500.004169	75328.674144	47.221223
2496.660488	74749.366737	47.226228
2492.985137	74157.564447	47.231233
2489.700601	73568.254106	47.236237
2486.418921	72974.651689	47.241242
2482.828715	72387.370587	47.246247
2479.380714	71791.306394	47.251252
2475.881426	71191.657650	47.256257
2472.533639	70597.585698	47.261261
2469.244945	69995.639765	47.266266
2465.599791	69410.478012	47.271271
2462.299384	68810.084932	47.276276
2458.610544	68199.787359	47.281281
2455.272297	67595.080152	47.286285
2451.845750	66994.019081	47.291290
2448.323804	66389.559384	47.296295
2444.911774	65776.210731	47.301300
2441.576171	65177.996619	47.306305
2438.029063	64569.172998	47.311309
2434.375945	63958.241733	47.316314
2431.144482	63346.878948	47.321319
2427.364410	62739.443473	47.326324
2424.124797	62125.547939	47.331329
2420.088978	61516.392536	47.336333
2416.569200	60910.992196	47.341338
2413.434530	60298.369622	47.346343
2409.763778	59677.723253	47.351348
2406.659255	59061.421079	47.356353
2403.004550	58451.019866	47.361357
2399.366548	57830.777259	47.366362
2396.021152	57219.134394	47.371367
2392.868476	56592.071608	47.376372
2389.237920	55976.856463	47.381377
2385.724603	55352.794566	47.386381
2382.432678	54735.750581	47.391386
2378.849713	54115.094637	47.396391
2375.716113	53476.069675	47.401396
2371.986242	52860.284840	47.406401
2368.535172	52235.540794	47.411405
2364.929170	51600.808373	47.416410
2361.390155	50965.353369	47.421415
2358.067820	50347.586070	47.426420
2354.897690	49716.884439	47.431425
2351.034647	49074.351583	47.436429
2347.803685	48447.639580	47.441434
2343.967181	47829.499980	47.446439
2340.383243	47178.934702	47.451444
2337.029704	46553.689289	47.456449
2333.531700	45915.774276	47.461453
2330.269779	45287.454830	47.466458
2326.923177	44652.615241	47.471463
2323.375465	44014.375230	47.476468
2319.987163	43367.827964	47.481473
2316.130894	42728.411001	47.486477
2312.647544	42082.810154	47.491482
2309.276906	41443.386571	47.496487
2305.935350	40807.477082	47.501492
2302.236411	40160.875762	47.506497
2298.559231	39531.155126	47.511501
2295.189114	38884.286982	47.516506
2291.744595	38239.421436	47.521511
2288.012549	37599.805730	47.526516
2284.826699	36958.830823	47.531521
2281.392867	36325.495425	47.536525
2277.863954	35672.694714	47.541530
2274.418133	35032.401329	47.546535
2271.379730	34384.780767	47.551540
2267.793725	33728.251991	47.556545
2263.910026	33083.522159	47.561549
2260.353594	32429.247776	47.566554
2256.633978	31783.410618	47.571559
2253.220348	31132.855989	47.576564
2249.769626	30488.582613	47.581569
2246.067403	29836.129981	47.586573
2242.730384	29202.183462	47.591578
2239.318533	28558.135466	47.596583
2235.971938	27909.364067	47.601588
2232.447151	27254.006725	47.606593
2228.923708	26611.266809	47.611597
2225.506742	25962.815558	47.616602
2221.770895	25312.324897	47.621607
2218.214276	24654.040822	47.626612
2214.382049	24007.719222	47.631617
2210.930661	23368.448389	47.636621
2207.349100	22716.288465	47.641626
2203.727073	22081.089282	47.646631
2199.832093	21443.488768	47.651636
2196.248504	20805.359961	47.656641
2192.948778	20172.338395	47.661645
2189.540830	19536.687462	47.666650
2185.316649	18903.996434	47.671655
2181.902275	18284.088831	47.676660
2177.598432	17660.767376	47.681665
2172.604418	17070.439644	47.686669
2168.748858	16477.482902	47.691674
2164.000158	15895.107268	47.696679
2160.013184	15325.818500	47.701684
2156.098509	14775.390328	47.706689
2151.512124	14233.703973	47.711693
2147.652777	13699.442428	47.716698
2143.820927	13185.273374	47.721703
2139.803457	12670.048598	47.726708
2135.927206	12170.948807	47.731713
2132.324109	11677.429368	47.736717
2128.332316	11182.368895	47.741722
2124.541801	10701.516153	47.746727
2120.734208	10234.619169	47.751732
2117.043223	9771.963669	47.756737
2113.330409	9303.748925	47.761741
2109.564096	8849.145832	47.766746
2106.149137	8404.719507	47.771751
2102.651637	7951.865909	47.776756
2099.520068	7501.644055	47.781761
2095.964110	7069.833704	47.786765
2092.110750	6621.594013	47.791770
2088.693128	6183.133595	47.796775
2084.928593	5763.630972	47.801780
2081.416209	5317.962001	47.806785
2077.755018	4895.548602	47.811789
2074.589227	4474.346353	47.816794
2070.575535	4053.684538	47.821799
2067.116769	3637.255948	47.826804
2063.354493	3205.872885	47.831809
2059.615026	2810.407007	47.836813
2056.186976	2395.286919	47.841818
2052.265941	1993.118164	47.846823
2048.553063	1608.546245	47.851828
2045.021525	1221.160612	47.856833
2040.993957	838.157067	47.861837
2037.117716	460.434355	47.866842
2032.313673	104.048295	47.871847
2015.666755	97.287181	47.876852
2000.822962	114.071416	47.881857
1992.963888	113.168558	47.886861
1988.868549	124.012120	47.891866
1987.248108	122.954558	47.896871
1986.488282	120.459601	47.901876
1985.953697	106.736349	47.906881
1984.204253	115.329228	47.911885
1981.767397	115.284570	47.916890
1979.064600	126.158177	47.921895
1975.164328	130.808453	47.926900
1972.112965	118.925876	47.931905
1969.029525	123.252873	47.936909
1966.346189	110.243687	47.941914
1962.787883	112.515405	47.946919
1958.996205	114.336232	47.951924
1956.106050	118.009894	47.956929
1952.088023	129.268529	47.961933
1949.259235	116.835630	47.966938
1946.235491	118.397737	47.971943
1942.841760	127.085179	47.976948
1939.328234	116.742504	47.981953
1936.054334	128.277627	47.986957
1932.809360	124.027610	47.991962
1929.586486	110.289325	47.996967
1926.100149	119.560646	48.001972
1923.441609	103.918562	48.006977
1919.416705	114.605626	48.011981
1915.558171	119.761930	48.016986
1911.835666	124.242174	48.021991
1908.840922	122.958749	48.026996
1905.419394	116.208404	48.032001
1902.051450	116.169458	48.037005
1898.786147	110.805819	48.042010
1895.362695	109.962438	48.047015
1891.742989	115.461218	48.052020
1888.399796	108.752469	48.057025
1884.902276	107.154997	48.062029
1881.929725	115.027082	48.067034
1878.045388	114.777446	48.072039
1874.817656	124.555844	48.077044
1871.591313	113.058022	48.082049
1867.881378	112.559784	48.087053
1864.643006	111.494613	48.092058
1860.895026	106.889466	48.097063
1856.963532	113.939537	48.102068
1854.162479	111.755950	48.107073
1850.783220	120.861912	48.112077
1847.408492	110.203429	48.117082
1843.594836	116.912463	48.122087
1840.220342	115.533126	48.127092
1836.713822	109.764118	48.132097
1832.932447	105.923464	48.137101
1829.432602	100.023709	48.142106
1826.486478	98.131620	48.147111
1822.699446	107.705996	48.152116
1819.752051	101.628512	48.157121
1815.805389	108.133621	48.162125
1812.600186	108.502783	48.167130
1809.489777	104.877239	48.172135
1805.362137	110.524676	48.177140
1801.760405	109.569848	48.182145
1798.320308	113.632823	48.187149
1795.323653	102.997768	48.192154
1791.710350	100.453394	48.197159
1787.993611	114.243554	48.202164
1784.573485	107.353807	48.207169
1781.235710	104.918409	48.212173
1777.561071	109.239349	48.217178
1774.015324	110.974457	48.222183
1770.397550	113.356682	48.227188
1767.243986	112.139117	48.232193
1763.723857	111.839135	48.237197
1760.001841	105.189365	48.242202
1756.892252	100.633569	48.247207
1753.462568	97.889781	48.252212
1750.091116	99.398449	48.257217
1746.314257	101.343533	48.262221
1742.919719	107.326120	48.267226
1739.491774	102.430738	48.272231
1735.858660	109.032581	48.277236
1732.394387	101.817525	48.282241
1728.931326	103.100011	48.287245
1725.539915	100.372415	48.292250
1722.175486	96.520667	48.297255
1718.044088	93.266011	48.302260
1715.094245	91.162544	48.307265
1711.139521	101.335649	48.312269
1707.981705	101.346272	48.317274
1704.653733	99.481989	48.322279
1701.149101	100.128714	48.327284
1697.613606	93.905502	48.332289
1694.257526	101.489267	48.337293
1690.536181	98.582076	48.342298
1687.320094	89.145445	48.347303
1683.445475	100.055880	48.352308
1679.891627	99.166377	48.357313
1676.545302	99.478421	48.362317
1673.034605	93.327283	48.367322
1669.914344	101.488105	48.372327
1665.746883	101.579945	48.377332
1662.883836	92.430050	48.382337
1659.063013	102.519041	48.387341
1655.410705	98.041400	48.392346
1651.794607	102.501928	48.397351
1648.272736	105.713946	48.402356
1645.532979	90.685676	48.407361
1641.955237	91.793031	48.412365
1638.516526	94.489074	48.417370
1634.624662	103.693794	48.422375
1630.928843	101.130644	48.427380
1627.489577	96.664141	48.432385
1623.828613	92.902851	48.437389
1620.421363	93.759050	48.442394
1617.247994	87.466835	48.447399
1613.583691	89.451357	48.452404
1610.379397	80.854454	48.457409
1606.633937	87.296612	48.462413
1603.038987	89.178593	48.467418
1599.696204	82.302156	48.472423
1596.344285	83.871069	48.477428
1593.158142	82.269458	48.482433
1589.384868	90.971668	48.487437
1585.889638	99.178197	48.492442
1582.413138	87.320753	48.497447
1578.634783	94.052768	48.502452
1575.073210	85.438712	48.507457
1571.845294	91.164416	48.512461
1568.217188	96.218430	48.517466
1564.880318	92.033387	48.522471
1560.895120	89.426704	48.527476
1557.630496	81.775656	48.532481
1554.202955	89.123773	48.537485
1550.475693	96.619782	48.542490
1547.119494	91.074193	48.547495
1543.883799	102.005407	48.552500
1540.545065	83.767483	48.557505
1536.696042	86.119278	48.562509
1533.197280	85.901413	48.567514
1529.823553	85.749507	48.572519
1525.991355	91.986875	48.577524
1522.759611	83.156980	48.582529
1518.808642	85.398096	48.587533
1515.843883	91.180918	48.592538
1512.490001	88.178592	48.597543
1508.687503	84.448839	48.602548
1505.472707	88.033841	48.607553
1501.791038	83.820219	48.612557
1498.100911	87.589933	48.617562
1495.041983	90.619174	48.622567
1491.615713	88.441189	48.627572
1488.178786	87.400632	48.632577
1484.438462	86.283914	48.637581
1480.521026	85.530116	48.642586
1477.594625	90.816596	48.647591
1473.483446	90.586491	48.652596
1470.327455	87.740028	48.657601
1466.668703	92.482446	48.662605
1463.139859	93.085505	48.667610
1459.719727	97.395321	48.672615
1456.205036	98.420114	48.677620
1453.055301	96.543934	48.682625
1449.408333	86.535343	48.687629
1446.015636	99.882749	48.692634
1442.124120	90.193790	48.697639
1438.196372	95.708894	48.702644
1434.787399	89.323664	48.707649
1431.508882	98.363319	48.712653
1428.412024	92.052893	48.717658
1425.329341	92.877572	48.722663
1421.521312	92.220645	48.727668
1418.034988	89.178834	48.732673
1414.086498	91.789727	48.737677
1410.585934	91.587973	48.742682
1407.225494	87.017486	48.747687
1403.588634	84.318642	48.752692
1400.507255	87.167888	48.757697
1397.136625	91.656660	48.762701
1393.208700	88.895555	48.767706
1390.078351	87.728198	48.772711
1386.435872	86.953760	48.777716
1382.731076	84.081999	48.782721
1379.492043	88.309847	48.787725
1375.569071	90.129011	48.792730
1372.039463	72.101182	48.797735
1368.446433	81.370115	48.802740
1365.377074	72.454866	48.807745
1361.602220	84.479207	48.812749
1358.411051	85.545400	48.817754
1355.190893	86.015002	48.822759
1351.095924	94.520525	48.827764
1347.953535	91.111983	48.832769
1344.562628	94.746553	48.837773
1340.512607	87.553136	48.842778
1337.259137	84.892701	48.847783
1333.806365	86.214746	48.852788
1330.640666	85.957714	48.857793
1326.877515	93.114474	48.862797
1323.027639	87.076294	48.867802
1319.713096	87.633356	48.872807
1316.020016	86.183444	48.877812
1312.562809	77.252642	48.882817
1309.534911	86.740494	48.887821
1305.882388	90.811248	48.892826
1302.563437	79.606375	48.897831
1298.490682	81.164126	48.902836
1295.388648	83.636949	48.907841
1291.904314	92.569437	48.912845
1288.183971	91.016206	48.917850
1284.389665	88.300756	48.922855
1281.292988	83.508901	48.927860
1277.515365	92.104233	48.932865
1274.232465	93.820614	48.937869
1270.503919	85.602754	48.942874
1267.467068	93.544956	48.947879
1263.693055	91.984262	48.952884
1260.412914	87.334859	48.957889
1256.782934	92.499911	48.962893
1253.241322	90.529729	48.967898
1249.780091	91.353234	48.972903
1246.047851	88.400343	48.977908
1242.966027	86.118155	48.982913
1239.324487	85.273986	48.987917
1235.774512	88.996596	48.992922
1232.310340	87.242149	48.997927
1228.616799	89.889304	49.002932
1225.375324	84.927009	49.007937
1221.636108	83.028718	49.012941
1217.716606	83.123144	49.017946
1214.758828	81.947926	49.022951
1211.073668	84.422938	49.027956
1207.761322	85.096725	49.032961
1204.374038	84.431280	49.037965
1200.818004	87.699263	49.042970
1197.092988	81.154463	49.047975
1193.850635	77.233167	49.052980
1189.932124	78.146838	49.057985
1186.533157	85.493683	49.062989
1183.104206	89.985218	49.067994
1179.971729	81.430991	49.072999
1176.089106	89.558625	49.078004
1172.879467	78.640477	49.083009
1169.433142	82.998678	49.088013
1165.350367	81.916321	49.093018
1161.990111	85.941592	49.098023
1158.517038	85.545765	49.103028
1155.100148	88.845876	49.108033
1151.594927	84.022720	49.113037
1148.087840	79.604809	49.118042
1144.718210	76.658766	49.123047
1141.265081	78.774970	49.128052
1137.929879	82.622340	49.133057
1134.174893	80.153887	49.138061
1130.957025	76.254098	49.143066
1127.577612	74.916734	49.148071
1123.458776	76.541788	49.153076
1120.007568	71.662778	49.158081
1116.671046	77.990686	49.163085
1112.986523	86.641132	49.168090
1109.966703	78.594555	49.173095
1106.432831	89.116603	49.178100
1102.857030	84.513244	49.183105
1099.114132	81.581016	49.188109
1095.481489	83.630257	49.193114
1091.876297	88.215669	49.198119
1088.211491	90.652724	49.203124
1084.537294	84.429056	49.208129
1081.454701	87.740411	49.213133
1077.678415	89.043236	49.218138
1074.656458	87.621763	49.223143
1071.116778	88.593537	49.228148
1067.918841	85.187351	49.233153
1064.022975	85.328735	49.238157
1060.293978	84.469728	49.243162
1056.927481	86.376307	49.248167
1053.229455	88.457876	49.253172
1050.143407	81.544726	49.258177
1046.416228	86.611029	49.263181
1043.065951	76.357029	49.268186
1039.837733	74.097653	49.273191
1036.161860	84.192560	49.278196
1032.692263	85.052190	49.283201
1029.042168	79.603049	49.288205
1025.588944	84.145828	49.293210
1022.221143	74.315332	49.298215
1018.099053	84.599917	49.303220
1014.856477	74.386105	49.308225
1011.546007	76.451642	49.313229
1008.083521	87.196692	49.318234
1004.741308	83.199217	49.323239
1000.819471	85.185918	49.328244
997.952600	79.099184	49.333249
994.166206	77.480345	49.338253
990.704944	87.668396	49.343258
987.326563	85.097049	49.348263
983.463976	80.800938	49.353268
979.694363	85.355005	49.358273
976.328206	84.974193	49.363277
972.471479	83.594090	49.368282
969.649800	79.224535	49.373287
966.250723	89.472509	49.378292
962.764725	82.058494	49.383297
959.571471	84.362048	49.388301
955.383332	82.483055	49.393306
952.655932	82.075580	49.398311
948.561638	80.526821	49.403316
944.800603	87.749708	49.408321
941.558049	79.003855	49.413325
937.850019	82.089881	49.418330
934.786077	80.152952	49.423335
930.839430	79.815050	49.428340
927.528627	80.153274	49.433345
923.935429	86.144672	49.438349
920.786658	82.515722	49.443354
917.252865	86.605989	49.448359
913.243980	83.148893	49.453364
909.752428	80.512918	49.458369
906.264109	77.987170	49.463373
903.068506	77.320395	49.468378
899.113821	68.052672	49.473383
895.652331	78.101554	49.478388
892.660335	79.487954	49.483393
889.201124	75.733332	49.488397
885.337505	76.426527	49.493402
881.969659	74.850117	49.498407
878.467031	84.266342	49.503412
874.840835	79.680356	49.508417
871.218946	83.398371	49.513421
868.092775	90.462328	49.518426
864.616020	75.302195	49.523431
860.940021	82.597268	49.528436
857.953061	86.140519	49.533441
853.865394	79.519359	49.538445
850.256411	83.146783	49.543450
847.100480	74.213464	49.548455
843.247847	82.969181	49.553460
839.413908	72.126140	49.558465
836.190312	66.325914	49.563469
832.737537	80.489391	49.568474
829.568208	76.961729	49.573479
826.294912	81.805537	49.578484
822.793658	70.202049	49.583489
819.142710	79.710964	49.588493
815.328482	84.161261	49.593498
811.834705	82.085618	49.598503
808.066873	81.798990	49.603508
805.215197	74.517213	49.608513
801.868907	79.862756	49.613517
797.394390	87.275809	49.618522
794.530090	75.430806	49.623527
790.626719	86.155908	49.628532
787.407904	82.699228	49.633537
783.639556	77.486832	49.638541
780.160908	82.833998	49.643546
777.291733	75.213272	49.648551
773.427976	79.231531	49.653556
769.629699	79.341944	49.658561
766.559836	79.357948	49.663565
762.729628	82.080205	49.668570
759.366395	83.163747	49.673575
755.883820	78.931902	49.678580
752.200619	77.540637	49.683585
748.495996	73.751476	49.688589
745.376882	78.077753	49.693594
742.133810	73.201202	49.698599
738.379925	79.062605	49.703604
734.661298	75.838759	49.708609
731.034971	81.487322	49.713613
727.563357	76.541948	49.718618
724.223001	76.717120	49.723623
720.622527	85.661378	49.728628
717.607395	75.570403	49.733633
713.611496	76.543634	49.738637
709.945047	79.771902	49.743642
706.922082	77.502763	49.748647
703.196446	89.693460	49.753652
699.548896	73.572890	49.758657
696.592061	78.905268	49.763661
693.029845	77.482523	49.768666
689.649733	75.126619	49.773671
685.765312	84.750979	49.778676
681.986802	82.656405	49.783681
678.881203	79.242228	49.788685
675.522267	78.661016	49.793690
672.028371	69.059025	49.798695
668.171257	71.627296	49.803700
664.642918	77.643413	49.808705
661.279786	71.102490	49.813709
657.648668	79.773114	49.818714
654.034823	69.294479	49.823719
650.632065	73.579499	49.828724
647.112698	73.453525	49.833729
643.816346	68.942781	49.838733
640.066100	84.145962	49.843738
636.919518	71.373688	49.848743
633.188802	66.693288	49.853748
629.978072	72.169594	49.858753
626.631250	76.319362	49.863757
622.116962	85.633665	49.868762
619.086763	67.202444	49.873767
615.211942	74.797393	49.878772
612.396358	80.405173	49.883777
608.866418	78.717994	49.888781
604.911645	81.133802	49.893786
601.584743	73.799492	49.898791
597.807348	78.066910	49.903796
594.641519	78.705299	49.908801
591.522242	75.093952	49.913805
587.864094	78.279813	49.918810
583.976100	72.187596	49.923815
580.386705	70.734299	49.928820
577.326374	69.802902	49.933825
574.088222	69.196573	49.938829
570.227932	75.495322	49.943834
566.950439	69.573819	49.948839
563.060956	67.499705	49.953844
559.186141	63.531434	49.958849
556.376491	69.827970	49.963853
552.741047	73.174811	49.968858
549.547010	65.500300	49.973863
545.483310	77.598092	49.978868
542.019404	67.627639	49.983873
538.561453	70.791829	49.988877
534.985908	75.736492	49.993882
531.731479	66.967264	49.998887
527.905125	58.400968	50.003892
524.586835	63.087287	50.008897
521.734291	67.223388	50.013901
517.517189	70.198886	50.018906
514.560844	61.955883	50.023911
510.328574	73.665476	50.028916
506.700906	67.671952	50.033921
503.684003	71.105997	50.038925
499.990982	68.257847	50.043930
496.630287	62.896626	50.048935
493.096103	69.125630	50.053940
489.607464	66.438648	50.058945
485.926316	64.860447	50.063949
482.524495	69.208608	50.068954
479.280139	54.493292	50.073959
475.804651	58.640954	50.078964
472.099702	59.651179	50.083969
468.833581	56.167117	50.088973
464.722176	61.562190	50.093978
461.394345	56.755831	50.098983
458.061964	65.455882	50.103988
454.631024	63.939972	50.108993
451.033822	68.008513	50.113997
447.416278	68.657131	50.119002
444.018960	62.972599	50.124007
440.662066	56.870500	50.129012
437.138779	62.645406	50.134017
433.946326	62.655223	50.139021
429.732789	76.446764	50.144026
426.512867	68.295427	50.149031
423.033838	71.950116	50.154036
419.499645	72.686998	50.159041
416.147866	65.998825	50.164045
412.559292	62.169511	50.169050
408.767034	68.002113	50.174055
405.410065	70.343860	50.179060
401.928916	62.242690	50.184065
398.842158	58.544058	50.189069
394.731329	64.220617	50.194074
391.654392	59.998451	50.199079
387.737163	65.841019	50.204084
384.254808	67.436681	50.209089
380.732896	60.256162	50.214093
377.113757	69.269774	50.219098
373.904228	65.466874	50.224103
370.421669	61.953248	50.229108
366.932915	66.447827	50.234113
363.570867	68.578404	50.239117
360.017670	71.697331	50.244122
356.540426	61.270267	50.249127
353.436813	69.966347	50.254132
349.561576	74.916557	50.259137
346.121874	64.255864	50.264141
342.392271	73.340460	50.269146
338.988361	67.324787	50.274151
335.435151	74.584959	50.279156
331.783448	74.432175	50.284161
328.367382	70.351397	50.289165
324.840080	75.326533	50.294170
321.607453	67.506217	50.299175
318.001267	69.760226	50.304180
314.251967	67.382764	50.309185
310.893922	69.547524	50.314189
307.122867	81.770609	50.319194
303.813056	70.757515	50.324199
300.680124	72.175405	50.329204
296.941827	65.411392	50.334209
293.429559	69.137706	50.339213
289.960780	71.411454	50.344218
286.304376	65.843214	50.349223
282.666665	61.006036	50.354228
279.251906	71.484249	50.359233
275.621029	60.967230	50.364237
272.060646	72.012266	50.369242
268.822350	68.489100	50.374247
265.155304	67.408597	50.379252
261.922199	71.755822	50.384257
259.220872	69.667618	50.389261
255.409867	73.044988	50.394266
251.098295	71.147368	50.399271
247.978564	74.891667	50.404276
244.319868	69.697103	50.409281
240.735804	64.465613	50.414285
237.122850	75.531491	50.419290
233.837818	69.905442	50.424295
230.455464	76.490472	50.429300
226.865995	73.572463	50.434305
223.671932	64.170658	50.439309
219.878100	69.345482	50.444314
216.342752	64.533507	50.449319
212.683481	66.618629	50.454324
209.195462	70.363322	50.459329
205.730323	64.717866	50.464333
202.144550	67.335696	50.469338
198.739128	63.041319	50.474343
195.305067	65.531130	50.479348
191.902556	62.087326	50.484353
188.235437	58.488574	50.489357
184.339325	71.240477	50.494362
181.454658	66.140548	50.499367
178.127411	61.267709	50.504372
174.146362	68.673593	50.509377
171.247755	65.167158	50.514381
166.970991	78.025785	50.519386
163.673930	65.599748	50.524391
160.433906	64.009867	50.529396
156.776419	67.211491	50.534401
153.420728	64.114734	50.539405
149.470087	68.754011	50.544410
146.181697	65.099464	50.549415
142.627042	72.223839	50.554420
139.061530	67.530465	50.559425
136.021709	64.925519	50.564429
131.977404	68.510064	50.569434
128.967036	62.749527	50.574439
125.201356	59.280023	50.579444
121.350126	70.560167	50.584449
118.241467	68.772674	50.589453
114.493307	73.984691	50.594458
111.302100	63.873806	50.599463
107.534541	67.639887	50.604468
104.154579	66.992426	50.609473
100.762621	62.803535	50.614477
96.854011	69.777383	50.619482
93.706188	64.797531	50.624487
90.449532	58.951966	50.629492
86.874745	70.236526	50.634497
83.747859	67.006084	50.639501
79.841668	65.972335	50.644506
76.058138	67.115069	50.649511
72.416699	62.420876	50.654516
68.763023	65.837047	50.659521
65.818203	72.195785	50.664525
61.925699	71.947659	50.669530
58.673094	67.218238	50.674535
55.150831	68.500626	50.679540
51.610098	74.920510	50.684545
48.123347	60.727079	50.689549
44.845837	59.557491	50.694554
40.893270	63.709878	50.699559
37.477318	60.666815	50.704564
33.898895	70.044259	50.709569
30.817389	61.346287	50.714573
27.162411	71.944168	50.719578
23.892980	57.903567	50.724583
20.170360	66.917495	50.729588
16.175238	69.773085	50.734593
13.204608	60.580141	50.739597
9.690867	62.338921	50.744602
6.221152	64.448339	50.749607
3.067375	74.129820	50.754612