Fri Aug 26 14:10:25 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.420369	101.792831	0.000000
0.457925	96.187295	0.005005
0.399087	97.208818	0.010010
0.258493	99.359843	0.015014
0.229502	103.239832	0.020019
-0.080880	83.784187	0.025024
-0.251943	75.964942	0.030029
-0.801534	62.351876	0.035034
-0.846283	58.973724	0.040038
-1.110321	59.514683	0.045043
-1.573774	35.796173	0.050048
-1.650524	46.507579	0.055053
-2.050164	40.410166	0.060058
-2.696199	35.034465	0.065062
-2.460390	29.660666	0.070067
-2.803187	23.845463	0.075072
-3.328886	14.518620	0.080077
-3.875621	15.132065	0.085082
-3.844788	21.043273	0.090086
-3.902195	23.918467	0.095091
-4.133785	12.698263	0.100096
-4.958962	14.089026	0.105101
-4.996684	12.297940	0.110106
-4.960797	13.241437	0.115110
-5.312940	19.057255	0.120115
-6.105916	16.678267	0.125120
-6.263020	19.727164	0.130125
-6.822706	25.695517	0.135130
-6.370296	12.331427	0.140134
-6.723237	9.893418	0.145139
-6.548955	7.604268	0.150144
-6.785402	13.601380	0.155149
-7.600279	9.194742	0.160154
-7.390102	10.088957	0.165158
-7.846924	6.556683	0.170163
-7.732264	5.902929	0.175168
-8.658754	12.228934	0.180173
-9.152695	15.678277	0.185178
-9.161150	13.408087	0.190182
-9.524805	12.487132	0.195187
-9.409974	3.778713	0.200192
-9.577022	14.722450	0.205197
-9.861644	8.686231	0.210202
-10.492108	16.136695	0.215206
-11.115724	9.893837	0.220211
-10.926085	4.514579	0.225216
-11.074310	8.020821	0.230221
-11.429972	12.543254	0.235226
-11.250405	7.598983	0.240230
-11.242979	10.625425	0.245235
-11.183372	19.822344	0.250240
-11.972301	14.753627	0.255245
-12.671398	16.390507	0.260250
-12.864945	6.436170	0.265254
-13.732626	12.794146	0.270259
-13.162556	6.564744	0.275264
-13.673886	5.613000	0.280269
-13.739848	3.968676	0.285274
-13.493358	-0.087538	0.290278
-13.959475	-0.207956	0.295283
-14.333242	6.690027	0.300288
-15.078263	12.794795	0.305293
-15.199359	5.534095	0.310298
-15.044599	10.353529	0.315302
-15.593511	18.601190	0.320307
-14.955846	5.053244	0.325312
-16.405770	10.846999	0.330317
-16.599127	13.800303	0.335322
-16.604964	-1.631051	0.340326
-16.988729	14.990367	0.345331
-16.672398	10.907458	0.350336
-16.987908	3.477719	0.355341
-17.505718	10.151366	0.360346
-17.747645	0.147620	0.365350
-17.956223	10.626438	0.370355
-18.100460	5.738911	0.375360
-18.484300	10.949077	0.380365
-19.223320	11.725334	0.385370
-19.422470	12.347934	0.390374
-19.453726	9.840858	0.395379
-19.628337	9.795272	0.400384
-19.903279	16.560816	0.405389
-19.822727	12.565236	0.410394
-19.801248	10.831369	0.415398
-20.508799	18.508964	0.420403
-20.784674	14.717570	0.425408
-20.989302	15.375823	0.430413
-21.539076	4.818914	0.435418
-21.469616	6.940386	0.440422
-21.641446	19.330654	0.445427
-21.399816	14.050863	0.450432
-22.163905	15.720008	0.455437
-22.670415	17.387012	0.460442
-22.806986	2.744776	0.465446
-22.684731	13.229029	0.470451
-23.304720	0.455850	0.475456
-23.940447	5.452142	0.480461
-23.930975	10.167651	0.485466
-24.246188	3.240886	0.490470
-24.375448	11.461167	0.495475
-24.164673	8.122332	0.500480
-24.562617	6.222824	0.505485
-25.665944	16.388554	0.510490
-25.782220	12.781112	0.515494
-26.022469	5.867983	0.520499
-26.210680	1.120178	0.525504
-25.836291	4.051519	0.530509
-25.925415	14.897704	0.535514
-25.773134	3.880322	0.540518
-26.499340	9.501286	0.545523
-27.089651	4.439612	0.550528
-27.044485	9.092617	0.555533
-27.212626	12.829743	0.560538
-27.493465	2.063289	0.565542
-28.533990	17.103907	0.570547
-28.455881	7.920331	0.575552
-28.567698	11.889123	0.580557
-28.574651	15.183551	0.585562
-28.605802	4.330766	0.590566
-29.670174	13.740646	0.595571
-29.951871	8.770120	0.600576
-30.405758	1.403056	0.605581
-30.471125	5.007123	0.610586
-29.906306	0.610291	0.615590
-30.226380	1.925574	0.620595
-30.177636	7.131659	0.625600
-30.712339	5.683699	0.630605
-31.715402	7.519761	0.635610
-31.641114	-0.021285	0.640614
-32.144921	13.853798	0.645619
-31.547822	6.145930	0.650624
-31.820929	13.344606	0.655629
-32.429848	10.832562	0.660634
-32.519662	1.643498	0.665638
-32.924768	15.816415	0.670643
-33.785384	5.871033	0.675648
-33.808408	4.251660	0.680653
-34.408171	18.568778	0.685658
-34.136160	2.613288	0.690662
-34.846594	13.379044	0.695667
-34.881837	7.069889	0.700672
-34.714825	4.917908	0.705677
-35.246081	4.738033	0.710682
-34.644686	0.629725	0.715686
-34.876682	7.432869	0.720691
-35.294017	10.088863	0.725696
-35.799665	10.316274	0.730701
-36.209878	13.727271	0.735706
-36.811044	5.804189	0.740710
-37.675871	12.452776	0.745715
-37.663926	9.866210	0.750720
-37.015812	11.897586	0.755725
-37.385181	11.588104	0.760730
-37.528248	4.818028	0.765734
-37.551255	9.807503	0.770739
-38.254831	5.168412	0.775744
-38.589200	8.112034	0.780749
-38.950814	4.077737	0.785754
-39.045035	1.140720	0.790758
-39.360535	3.831476	0.795763
-39.402694	8.143749	0.800768
-40.313670	3.666659	0.805773
-40.619519	11.904944	0.810778
-40.438830	3.806347	0.815782
-40.928980	8.403500	0.820787
-41.111672	10.209904	0.825792
-40.865630	6.337250	0.830797
-40.784710	9.728722	0.835802
-40.824311	13.208560	0.840806
-41.440292	13.741042	0.845811
-41.928832	11.482329	0.850816
-42.210009	10.004386	0.855821
-42.448242	12.594531	0.860826
-42.855544	9.355094	0.865830
-43.098195	8.788610	0.870835
-43.349031	16.024946	0.875840
-43.248776	13.725176	0.880845
-43.559905	6.190356	0.885850
-43.876331	7.748672	0.890854
-44.325903	13.665075	0.895859
-44.719152	2.245433	0.900864
-44.374912	6.934127	0.905869
-45.253105	11.041224	0.910874
-45.770476	7.353871	0.915878
-46.127295	11.746773	0.920883
-45.887918	10.054908	0.925888
-45.950559	4.145476	0.930893
-46.066921	13.157822	0.935898
-46.029982	9.197507	0.940902
-47.094326	10.606528	0.945907
-46.971592	-2.171561	0.950912
-47.182095	9.864065	0.955917
-47.500453	7.803474	0.960922
-47.576085	13.528781	0.965926
-48.076905	15.514427	0.970931
-48.607518	5.128538	0.975936
-48.868811	8.022818	0.980941
-48.778531	16.885937	0.985946
-48.682210	14.526671	0.990950
-49.333406	22.144873	0.995955
-50.000267	21.476765	1.000960
-50.356509	13.594638	1.005965
-50.664224	9.105875	1.010970
-50.366685	10.157323	1.015974
-50.428536	16.592305	1.020979
-50.310663	4.536280	1.025984
-50.471281	6.544883	1.030989
-51.317377	5.411154	1.035994
-51.554183	11.379846	1.040998
-51.852808	12.059062	1.046003
-51.705751	7.809529	1.051008
-52.261619	14.758011	1.056013
-53.028672	8.467890	1.061018
-53.297141	10.091503	1.066022
-53.319153	6.026477	1.071027
-53.718071	9.837496	1.076032
-53.213772	8.126528	1.081037
-53.422502	10.202732	1.086042
-53.934188	6.324675	1.091046
-54.392140	11.274307	1.096051
-54.720963	8.323198	1.101056
-55.022562	9.392004	1.106061
-55.090363	14.236599	1.111066
-55.033147	2.702530	1.116070
-56.035900	1.602684	1.121075
-56.300089	7.736984	1.126080
-56.201777	12.308951	1.131085
-56.798856	14.328566	1.136090
-56.770406	-0.070447	1.141094
-56.879598	8.962926	1.146099
-56.664958	6.389092	1.151104
-56.678798	1.614138	1.156109
-57.816801	13.825814	1.161114
-57.795550	11.683873	1.166118
-57.933477	12.654432	1.171123
-58.104703	11.478898	1.176128
-58.926188	4.235507	1.181133
-59.438996	11.626521	1.186138
-59.311295	1.533591	1.191142
-60.153786	17.252027	1.196147
-60.099920	14.127442	1.201152
-59.820052	4.874492	1.206157
-59.996039	10.868515	1.211162
-60.035702	12.766540	1.216166
-60.120121	6.949081	1.221171
-60.398916	10.826815	1.226176
-60.916951	1.910065	1.231181
-61.307313	4.701059	1.236186
-61.214653	5.581933	1.241190
-61.961818	7.558480	1.246195
-62.338539	10.698515	1.251200
-62.465667	11.920484	1.256205
-62.694541	15.543683	1.261210
-62.773058	10.133414	1.266214
-62.875276	4.796437	1.271219
-63.585016	6.675411	1.276224
-63.930195	7.342893	1.281229
-64.132323	16.798849	1.286234
-63.954057	5.793241	1.291238
-64.226123	15.497359	1.296243
-64.414347	8.924133	1.301248
-64.332485	12.122476	1.306253
-65.228529	10.784560	1.311258
-65.375081	4.388338	1.316262
-65.443184	16.484050	1.321267
-65.633072	12.385051	1.326272
-66.197859	4.915037	1.331277
-67.000639	11.727962	1.336282
-66.607918	4.390428	1.341286
-66.921293	13.629594	1.346291
-67.344816	11.028576	1.351296
-66.929565	7.455433	1.356301
-67.482900	15.422213	1.361306
-68.024499	4.417963	1.366310
-68.246014	10.681656	1.371315
-68.718322	9.075291	1.376320
-68.587052	6.394220	1.381325
-68.820634	12.596520	1.386330
-68.772563	8.422508	1.391334
-69.697747	8.655133	1.396339
-69.863360	5.482468	1.401344
-69.977509	19.945427	1.406349
-70.464096	11.786215	1.411354
-70.178397	7.331604	1.416358
-70.411739	8.987712	1.421363
-70.331885	5.919191	1.426368
-71.188802	8.184899	1.431373
-71.182215	11.812563	1.436378
-71.441832	-2.933886	1.441382
-72.332546	11.687943	1.446387
-73.026545	6.354525	1.451392
-72.565939	5.412797	1.456397
-72.805383	7.930365	1.461402
-72.792093	3.932607	1.466406
-73.015771	5.754883	1.471411
-72.767512	1.650940	1.476416
-73.442318	5.043022	1.481421
-74.352953	11.344412	1.486426
-74.055303	11.456241	1.491430
-74.697473	7.617483	1.496435
-74.760857	11.781206	1.501440
-74.744133	12.265794	1.506445
-74.812374	11.153317	1.511450
-75.185200	8.266005	1.516454
-75.855855	6.801251	1.521459
-76.318841	12.928542	1.526464
-76.039424	4.102756	1.531469
-76.121018	8.281968	1.536474
-76.202834	6.697058	1.541478
-77.098403	4.732668	1.546483
-77.100006	6.109093	1.551488
-77.245721	11.547928	1.556493
-77.951467	17.108762	1.561498
-77.698924	2.924785	1.566502
-78.337198	8.022710	1.571507
-78.702032	4.798810	1.576512
-78.769807	6.182374	1.581517
-79.104088	3.738299	1.586522
-78.732107	4.642119	1.591526
-78.849737	2.521804	1.596531
-79.781917	1.426789	1.601536
-80.346094	1.815169	1.606541
-80.488669	8.259551	1.611546
-80.272719	-1.695261	1.616550
-80.548740	3.115314	1.621555
-80.600882	-3.852404	1.626560
-80.994223	4.121096	1.631565
-81.894628	9.519254	1.636570
-81.434748	-1.147394	1.641574
-81.768108	-1.997136	1.646579
-81.928501	0.470158	1.651584
-82.561164	8.294269	1.656589
-83.094852	4.679058	1.661594
-83.427367	12.636764	1.666598
-83.353597	10.375919	1.671603
-83.326706	10.011068	1.676608
-83.385563	2.342064	1.681613
-83.498071	3.261210	1.686618
-84.046821	-1.060310	1.691622
-84.495644	9.756454	1.696627
-84.742187	11.297562	1.701632
-84.536057	3.413299	1.706637
-85.376894	6.837560	1.711642
-85.573363	1.806315	1.716646
-86.282384	5.842781	1.721651
-86.467928	7.443991	1.726656
-86.768933	6.782194	1.731661
-86.556412	9.235717	1.736666
-86.544674	-0.010280	1.741670
-86.488341	5.621712	1.746675
-86.356130	8.742614	1.751680
-87.246642	2.756449	1.756685
-88.009766	14.156807	1.761690
-87.904788	4.934254	1.766694
-88.139195	6.622163	1.771699
-88.399689	7.168896	1.776704
-88.601233	0.518657	1.781709
-89.228814	0.363272	1.786714
-89.309194	11.119506	1.791718
-89.511204	12.682153	1.796723
-89.684840	15.955077	1.801728
-89.564946	2.165066	1.806733
-90.151805	8.577388	1.811738
-90.662080	17.919976	1.816742
-90.715727	12.040779	1.821747
-90.996768	9.148669	1.826752
-91.173192	3.867538	1.831757
-91.157429	2.416127	1.836762
-91.310078	3.116905	1.841766
-91.987780	0.441575	1.846771
-92.676157	12.054912	1.851776
-92.862917	1.754692	1.856781
-93.242139	7.021082	1.861786
-93.178178	8.953590	1.866790
-92.772310	8.618313	1.871795
-93.017654	1.146020	1.876800
-93.619733	-6.947744	1.881805
-94.576077	8.098735	1.886810
-94.505435	1.592771	1.891814
-94.514537	6.406077	1.896819
-94.567526	5.636063	1.901824
-94.151438	3.698392	1.906829
-94.992063	14.275616	1.911834
-95.240566	7.132832	1.916838
-95.510091	6.488278	1.921843
-95.819705	9.155972	1.926848
-96.223449	8.234934	1.931853
-96.942870	10.238798	1.936858
-96.849529	15.716339	1.941862
-96.977789	4.903989	1.946867
-97.237161	13.720308	1.951872
-97.053929	9.639143	1.956877
-97.661243	17.823129	1.961882
-98.435622	13.489283	1.966886
-98.620123	8.959192	1.971891
-98.806574	10.041707	1.976896
-98.487610	3.636278	1.981901
-98.663291	3.091004	1.986906
-98.601323	2.796619	1.991910
-99.327323	8.341622	1.996915
-99.876917	11.680660	2.006912
-99.669915	4.565451	2.016909
-99.069949	-0.387221	2.026906
-98.918476	5.367045	2.036902
-97.895411	1.058058	2.046899
-97.516836	1.756173	2.056896
-96.803680	7.125222	2.066893
-96.411027	3.468737	2.076890
-96.008608	8.154432	2.086886
-95.605241	10.087255	2.096883
-94.649407	14.427034	2.106880
-94.707587	10.495464	2.116877
-94.356599	6.778944	2.126874
-93.436448	6.173173	2.136870
-92.754148	5.962386	2.146867
-91.753658	1.631572	2.156864
-92.347825	1.337608	2.166861
-91.990529	1.522703	2.176858
-91.030522	3.983389	2.186854
-90.613533	8.280357	2.196851
-89.677923	4.878275	2.206848
-89.575812	4.102112	2.216845
-89.216090	5.664776	2.226842
-88.408748	9.463824	2.236838
-88.112864	4.276571	2.246835
-86.968591	2.942181	2.256832
-86.618462	7.404776	2.266829
-86.821350	13.733723	2.276826
-86.367015	7.248385	2.286822
-85.425835	11.400383	2.296819
-85.062153	10.203370	2.306816
-84.181836	3.806925	2.316813
-83.692739	13.145137	2.326810
-83.736515	5.698353	2.336806
-82.822092	7.858871	2.346803
-82.503969	10.311798	2.356800
-81.993298	7.169108	2.366797
-81.153534	7.079518	2.376794
-80.793419	5.955917	2.386790
-80.726883	10.516521	2.396787
-80.095012	12.413767	2.406784
-79.244996	15.420585	2.416781
-79.331105	15.234409	2.426778
-78.364330	12.863310	2.436774
-78.161717	12.857086	2.446771
-77.031164	5.848325	2.456768
-76.727199	10.476494	2.466765
-76.721240	16.123547	2.476762
-75.958495	15.954086	2.486758
-75.196483	13.180894	2.496755
-75.182266	14.319032	2.506752
-74.483180	8.112355	2.516749
-73.725804	7.763171	2.526746
-73.605230	10.174001	2.536742
-72.760164	7.486076	2.546739
-72.479258	12.577152	2.556736
-72.238967	17.205735	2.566733
-71.418983	15.592396	2.576730
-71.024247	7.659197	2.586726
-69.947519	10.608543	2.596723
-69.379021	17.530117	2.606720
-69.829434	14.340670	2.616717
-69.088456	12.730130	2.626714
-68.440394	11.697906	2.636710
-68.254431	11.776635	2.646707
-67.006995	13.631888	2.656704
-66.920823	11.736843	2.666701
-66.496645	9.909542	2.676698
-65.972095	9.115120	2.686694
-65.391697	12.417334	2.696691
-65.064303	7.751011	2.706688
-64.078887	2.120622	2.716685
-63.719979	6.265082	2.726682
-63.816863	6.815489	2.736678
-63.072523	2.388347	2.746675
-62.456691	3.458155	2.756672
-61.549292	4.216479	2.766669
-60.976990	10.443734	2.776666
-60.969007	12.042158	2.786662
-60.679777	6.738735	2.796659
-59.952366	5.101799	2.806656
-59.200259	9.400442	2.816653
-59.284306	14.722566	2.826650
-58.004262	9.803380	2.836646
-57.464014	7.894653	2.846643
-57.591002	15.681594	2.856640
-57.149925	10.335521	2.866637
-56.544494	7.798945	2.876634
-56.233034	12.514645	2.886630
-54.885840	8.003140	2.896627
-54.861180	4.555999	2.906624
-54.454124	6.576945	2.916621
-53.391215	15.477373	2.926618
-53.384455	16.306238	2.936614
-53.327331	8.188028	2.946611
-52.187265	10.322918	2.956608
-51.943733	5.733006	2.966605
-51.278269	10.327066	2.976602
-50.617817	13.585139	2.986598
-50.398264	15.568758	2.996595
-50.283844	12.519441	3.006592
-49.055591	6.011802	3.016589
-48.644793	11.294890	3.026586
-48.613795	9.969117	3.036582
-47.660807	9.104820	3.046579
-47.407124	5.454133	3.056576
-47.052465	5.078958	3.066573
-46.090350	17.286315	3.076570
-45.767393	12.981798	3.086566
-45.567406	10.147232	3.096563
-44.892771	7.381310	3.106560
-44.630544	13.026475	3.116557
-43.504601	10.484880	3.126554
-43.455188	11.576358	3.136550
-43.104678	8.360407	3.146547
-42.113360	4.233753	3.156544
-42.045069	8.100359	3.166541
-41.399001	7.163478	3.176538
-40.216660	11.100540	3.186534
-40.314591	9.218321	3.196531
-40.312075	10.602193	3.206528
-39.493586	8.178159	3.216525
-38.999423	17.908383	3.226522
-38.020390	18.665059	3.236518
-37.531176	6.345730	3.246515
-37.490630	8.661318	3.256512
-37.228549	11.617134	3.266509
-36.455695	5.053692	3.276506
-35.471155	-0.459355	3.286502
-35.106448	8.492763	3.296499
-35.067747	-3.088032	3.306496
-34.373619	1.558581	3.316493
-33.730817	5.275550	3.326490
-33.281437	10.023627	3.336486
-33.200446	4.366168	3.346483
-32.503881	-0.566702	3.356480
-31.486316	10.478979	3.366477
-31.195220	2.818501	3.376474
-30.530420	0.092124	3.386470
-30.358682	1.671387	3.396467
-30.245262	3.433953	3.406464
-29.177137	0.242482	3.416461
-28.862325	4.992504	3.426458
-27.986165	-0.510004	3.436454
-27.433567	2.647657	3.446451
-26.986659	-0.070136	3.456448
-27.181387	2.038171	3.466445
-26.788895	7.783426	3.476442
-25.873885	8.242804	3.486438
-24.851521	6.544105	3.496435
-24.318965	4.551049	3.506432
-24.096088	6.809740	3.516429
-24.332812	5.829750	3.526426
-23.708572	13.924197	3.536422
-22.494722	8.036501	3.546419
-22.114088	8.990881	3.556416
-21.662090	4.054909	3.566413
-21.169037	3.658186	3.576410
-20.931034	14.708043	3.586406
-20.338189	9.262315	3.596403
-19.632683	5.842209	3.606400
-19.481658	15.410458	3.616397
-18.889705	9.825489	3.626394
-18.107396	2.303933	3.636390
-17.933072	3.451987	3.646387
-17.008797	2.196200	3.656384
-16.830999	6.479731	3.666381
-16.510116	3.205039	3.676378
-15.700538	0.573325	3.686374
-14.906384	6.062813	3.696371
-14.647863	5.262297	3.706368
-14.663774	4.466497	3.716365
-13.758055	2.389999	3.726362
-13.528628	4.014131	3.736358
-12.263262	6.756718	3.746355
-11.934300	0.851582	3.756352
-11.860368	-0.107087	3.766349
-11.535010	6.557748	3.776346
-10.440585	8.028196	3.786342
-10.625653	0.435520	3.796339
-9.649760	4.544106	3.806336
-9.350323	3.645356	3.816333
-9.030120	0.468969	3.826330
-8.012754	-1.349322	3.836326
-7.532204	-0.264785	3.846323
-7.428776	1.990330	3.856320
-7.003780	7.584811	3.866317
-6.600348	3.758758	3.876314
-5.466503	0.446185	3.886310
-5.172036	-0.793901	3.896307
-4.951284	7.262001	3.906304
-4.464518	16.093755	3.916301
-4.177068	24.814000	3.926298
-3.560538	33.017361	3.936294
-2.907744	36.263963	3.946291
-2.759551	56.241742	3.956288
-2.027790	63.074566	3.966285
-1.693298	74.027078	3.976282
-0.943482	86.799720	3.986278
-0.778562	88.985085	3.996275
-0.490031	108.212499	4.006272
0.000000	124.882499	4.011277
0.488302	126.527496	4.016282
0.800021	137.295529	4.021286
0.822779	145.862354	4.026291
1.096581	142.918630	4.031296
1.202614	152.032461	4.036301
1.077295	145.269057	4.041306
1.059601	141.978424	4.046310
0.988528	148.190272	4.051315
1.420411	145.282044	4.056320
1.146279	150.367606	4.061325
1.127925	136.187729	4.066330
0.834186	133.142551	4.071334
1.062509	148.533039	4.076339
0.976823	160.834067	4.081344
1.294491	161.847592	4.086349
1.274993	154.669085	4.091354
0.966156	160.826210	4.096358
1.310470	159.317303	4.101363
1.138371	150.140972	4.106368
1.029967	151.964296	4.111373
1.148916	154.739288	4.116378
1.124697	158.716621	4.121382
1.324915	159.409919	4.126387
1.358811	158.983864	4.131392
0.857377	169.226806	4.136397
1.510287	157.001949	4.141402
1.077651	153.041948	4.146406
1.385683	150.833192	4.151411
1.496599	157.035690	4.156416
1.218254	150.410001	4.161421
1.251499	157.067506	4.166426
1.502174	156.035074	4.171430
1.015290	155.171262	4.176435
1.313443	157.725369	4.181440
1.158419	151.460119	4.186445
1.364308	156.448799	4.191450
1.716059	161.705827	4.196454
1.524508	159.084485	4.201459
1.482707	154.737773	4.206464
1.259582	160.422821	4.211469
1.459966	153.286008	4.216474
1.194538	154.887015	4.221478
1.424355	155.936363	4.226483
1.037990	153.481392	4.231488
1.162525	163.294683	4.236493
1.877337	163.300435	4.241498
1.426293	174.304307	4.246502
1.798821	174.641755	4.251507
1.531615	163.300454	4.256512
1.257369	172.040081	4.261517
1.975537	168.549452	4.266522
1.551141	168.460500	4.271526
1.275779	161.435720	4.276531
1.887303	170.717624	4.281536
1.855682	173.003547	4.286541
2.228083	157.956075	4.291546
1.479206	157.291238	4.296550
1.249732	146.753972	4.301555
1.389203	149.402385	4.306560
1.540090	172.065572	4.311565
1.759134	173.455112	4.316570
1.896961	174.680131	4.321574
1.675944	169.076867	4.326579
2.303966	181.570500	4.331584
1.724436	175.760469	4.336589
1.581659	162.137768	4.341594
1.914068	170.947451	4.346598
1.907847	178.560210	4.351603
1.899857	167.431641	4.356608
1.727460	177.914415	4.361613
2.015390	174.566700	4.366618
1.682899	162.691412	4.371622
1.565026	174.026214	4.376627
1.948431	171.245750	4.381632
1.641117	170.926603	4.386637
1.816625	162.771792	4.391642
1.913138	176.572517	4.396646
1.826731	169.534133	4.401651
1.912940	178.021493	4.406656
1.746484	175.124166	4.411661
1.784023	174.694380	4.416666
1.925176	182.765074	4.421670
1.740880	175.058574	4.426675
1.940687	176.359362	4.431680
1.918639	172.781507	4.436685
1.785273	173.327433	4.441690
1.997960	179.719731	4.446694
1.702561	183.846857	4.451699
1.750120	172.162319	4.456704
1.803030	199.045319	4.461709
2.330985	194.660506	4.466714
2.498960	209.070211	4.471718
2.570297	194.816212	4.476723
2.498337	187.376948	4.481728
2.019635	183.212146	4.486733
2.128345	178.402243	4.491738
1.999868	180.953177	4.496742
1.871486	180.099983	4.501747
1.893508	180.498331	4.506752
2.260436	190.751613	4.511757
2.310536	187.266923	4.516762
2.454922	197.868061	4.521766
2.471634	198.390621	4.526771
2.200152	183.389597	4.531776
2.094511	184.399430	4.536781
2.013777	181.653266	4.541786
2.410786	205.008984	4.546790
2.097551	214.175472	4.551795
2.403722	203.051748	4.556800
2.640249	207.823705	4.561805
2.410726	208.520642	4.566810
2.584455	205.639944	4.571814
2.397379	190.208167	4.576819
2.426023	175.650790	4.581824
2.108584	182.726728	4.586829
2.251399	191.113534	4.591834
2.529319	197.505174	4.596838
2.748020	202.153358	4.601843
2.499098	197.731319	4.606848
2.159537	190.137570	4.611853
2.260588	197.433086	4.616858
2.458995	197.038363	4.621862
2.566909	196.822240	4.626867
2.686143	197.101052	4.631872
2.285987	214.509802	4.636877
2.357321	200.262127	4.641882
2.457862	204.507939	4.646886
2.691306	206.875980	4.651891
2.847601	206.728253	4.656896
2.634087	202.829034	4.661901
2.887690	209.439594	4.666906
2.850227	202.842819	4.671910
2.443203	196.066309	4.676915
2.490777	190.778715	4.681920
2.394838	204.302550	4.686925
2.688528	199.077871	4.691930
2.964803	204.903471	4.696934
2.652732	206.812295	4.701939
3.137104	195.765232	4.706944
2.705875	192.839525	4.711949
2.786260	190.267585	4.716954
2.223925	190.554442	4.721958
2.458296	194.067588	4.726963
2.518352	203.232896	4.731968
2.643391	205.614651	4.736973
3.153107	202.577240	4.741978
2.894204	199.479172	4.746982
2.663570	210.537332	4.751987
2.873674	201.959511	4.756992
2.821887	198.946252	4.761997
2.674449	202.142369	4.767002
2.334921	202.622320	4.772006
2.285699	200.905770	4.777011
2.680730	198.227893	4.782016
2.706372	205.955923	4.787021
2.541585	199.290390	4.792026
3.030068	216.010302	4.797030
3.079860	224.924125	4.802035
3.167821	223.053338	4.807040
3.078130	211.871024	4.812045
3.401740	202.291626	4.817050
2.909483	209.594105	4.822054
3.018570	206.818382	4.827059
2.694400	204.859909	4.832064
2.755014	207.982505	4.837069
2.749350	212.981993	4.842074
2.967584	224.561882	4.847078
3.007962	228.310879	4.852083
3.105500	211.142199	4.857088
3.077026	224.699836	4.862093
3.102750	218.551950	4.867098
3.226213	227.084153	4.872102
2.913038	224.557666	4.877107
3.318016	225.981534	4.882112
3.018786	225.129628	4.887117
3.344413	233.582902	4.892122
3.019937	230.520348	4.897126
2.930910	229.363637	4.902131
3.373595	219.215209	4.907136
2.770765	220.153762	4.912141
3.238169	218.834489	4.917146
2.968872	220.885347	4.922150
3.236947	230.258720	4.927155
3.544505	225.579192	4.932160
3.383122	228.385188	4.937165
3.336608	225.750745	4.942170
3.190954	226.662409	4.947174
3.183813	231.402710	4.952179
3.301802	224.104695	4.957184
3.068747	231.648393	4.962189
3.234325	233.716963	4.967194
3.314196	223.175779	4.972198
3.457020	218.907871	4.977203
3.195626	217.575522	4.982208
2.947890	225.349289	4.987213
3.576502	223.172867	4.992218
3.455408	232.163918	4.997222
3.271058	232.274868	5.002227
3.474862	226.013833	5.007232
3.378295	239.294189	5.012237
3.633505	229.839318	5.017242
3.586304	240.362747	5.022246
3.376678	241.537466	5.027251
3.447117	236.363355	5.032256
3.616495	247.112489	5.037261
3.609148	236.626005	5.042266
3.503141	245.649515	5.047270
3.731934	234.613748	5.052275
3.627736	232.950045	5.057280
3.677847	235.656676	5.062285
3.444673	227.584449	5.067290
3.438089	222.640628	5.072294
3.565037	238.129233	5.077299
3.840112	240.145954	5.082304
3.551127	251.577048	5.087309
3.735445	245.515190	5.092314
3.683892	245.459934	5.097318
3.541859	254.982593	5.102323
4.046955	249.623746	5.107328
3.612337	241.260181	5.112333
3.778938	235.713601	5.117338
3.632060	240.358605	5.122342
3.655197	247.739038	5.127347
3.747942	242.298866	5.132352
3.687651	250.723652	5.137357
3.599968	248.592314	5.142362
3.951731	253.833550	5.147366
3.493819	259.067977	5.152371
3.910837	253.340036	5.157376
3.578345	250.240762	5.162381
3.895295	249.485903	5.167386
3.869693	254.513816	5.172390
3.808029	253.473063	5.177395
3.603612	252.584248	5.182400
3.812950	256.038030	5.187405
3.780414	253.512136	5.192410
3.817735	254.376331	5.197414
4.054509	255.658715	5.202419
4.046834	257.396766	5.207424
3.966981	256.741651	5.212429
3.768618	251.457531	5.217434
3.709576	254.813896	5.222438
3.972699	255.883374	5.227443
3.922789	250.187007	5.232448
3.631967	261.865161	5.237453
3.807502	263.299446	5.242458
4.401173	273.169466	5.247462
3.868693	266.437772	5.252467
3.842659	277.685576	5.257472
3.991038	280.304148	5.262477
4.123307	277.224254	5.267482
4.144761	270.833411	5.272486
4.005990	280.257501	5.277491
4.230645	277.071476	5.282496
4.161364	283.552006	5.287501
4.463428	281.293545	5.292506
4.408163	276.452200	5.297510
4.259229	263.355552	5.302515
4.241401	250.478942	5.307520
3.989313	260.955191	5.312525
4.250539	266.248491	5.317530
4.290616	275.954774	5.322534
4.601525	282.141996	5.327539
4.304678	252.525442	5.332544
4.293650	260.325642	5.337549
4.287628	258.542250	5.342554
3.994164	251.510762	5.347558
4.119921	269.381836	5.352563
4.315614	281.702412	5.357568
4.647602	280.008757	5.362573
4.511170	275.755841	5.367578
4.757151	266.552320	5.372582
4.318358	259.467527	5.377587
4.206918	250.006458	5.382592
3.763212	257.889843	5.387597
4.319819	276.120940	5.392602
4.159921	280.454776	5.397606
4.080948	278.040511	5.402611
4.466212	280.979698	5.407616
4.134671	286.687993	5.412621
4.266481	276.600590	5.417626
4.496131	273.277749	5.422630
4.502266	271.176093	5.427635
4.530132	275.955247	5.432640
4.549715	277.160720	5.437645
4.341717	281.505209	5.442650
4.734592	273.079227	5.447654
4.815337	280.501323	5.452659
4.558735	280.721597	5.457664
4.631784	283.826452	5.462669
4.401106	278.474590	5.467674
4.523424	277.515920	5.472678
4.706261	278.487170	5.477683
4.541849	276.636690	5.482688
4.351290	280.595657	5.487693
4.616521	280.234819	5.492698
4.445031	273.048292	5.497702
4.405638	286.376727	5.502707
4.820163	287.995263	5.507712
4.730469	301.666892	5.512717
4.928732	304.350466	5.517722
4.942445	300.586686	5.522726
4.866343	291.360535	5.527731
4.867821	284.431805	5.532736
4.664399	284.979151	5.537741
4.461304	275.231788	5.542746
4.516147	283.470987	5.547750
4.882803	301.560846	5.552755
5.109780	297.374727	5.557760
4.903669	301.586052	5.562765
4.788919	293.818054	5.567770
4.928332	302.373118	5.572774
4.838475	306.942824	5.577779
4.874628	299.432896	5.582784
5.033011	308.181160	5.587789
5.147367	301.510090	5.592794
5.024233	288.871307	5.597798
4.777919	291.652572	5.602803
5.066160	286.621702	5.607808
4.722610	297.922118	5.612813
4.969860	290.895010	5.617818
5.166993	304.192959	5.622822
4.626736	306.368271	5.627827
5.053569	303.938523	5.632832
4.957861	313.571057	5.637837
4.881404	308.695038	5.642842
5.272121	309.513703	5.647846
5.137390	309.572636	5.652851
5.171446	298.329872	5.657856
5.427624	300.011028	5.662861
5.110107	307.232557	5.667866
5.341365	308.196270	5.672870
4.710759	293.763586	5.677875
5.115380	292.909655	5.682880
4.783867	311.415105	5.687885
4.876200	311.941712	5.692890
4.733510	300.283549	5.697894
4.540107	310.785490	5.702899
4.934460	294.690466	5.707904
5.043587	307.904045	5.712909
5.169654	301.376683	5.717914
5.562937	303.276932	5.722918
5.175517	306.984987	5.727923
5.256320	296.294920	5.732928
5.375789	298.035325	5.737933
5.357629	314.530499	5.742938
5.319727	315.665832	5.747942
5.183009	321.198274	5.752947
5.449517	309.289735	5.757952
5.190319	312.129956	5.762957
4.843511	312.164961	5.767962
5.487217	324.801784	5.772966
5.508963	331.967337	5.777971
5.664835	335.454768	5.782976
5.557045	334.759709	5.787981
5.519173	324.480402	5.792986
5.457547	315.008380	5.797990
5.161976	310.043091	5.802995
5.470998	322.149901	5.808000
5.646799	326.270132	5.813005
5.371493	314.623116	5.818010
6.033408	313.770251	5.823014
5.522162	313.618892	5.828019
5.575108	315.369656	5.833024
5.260583	309.322171	5.838029
5.236616	313.865800	5.843034
5.502184	315.191161	5.848038
5.184705	333.049054	5.853043
5.949471	324.226630	5.858048
5.812301	336.232080	5.863053
5.509520	327.262663	5.868058
5.821269	328.131588	5.873062
5.403591	319.515416	5.878067
5.559574	319.139950	5.883072
5.659752	335.040925	5.888077
5.677026	331.868196	5.893082
5.707055	328.465696	5.898086
5.656187	329.182276	5.903091
6.031669	324.055556	5.908096
5.969482	327.915454	5.913101
5.642450	320.101403	5.918106
5.668384	306.464978	5.923110
5.488861	316.841378	5.928115
5.266232	313.383308	5.933120
5.684169	328.105362	5.938125
5.708158	327.354984	5.943130
5.798890	334.512960	5.948134
5.787997	341.186897	5.953139
5.808478	326.029565	5.958144
5.780597	329.403239	5.963149
5.819147	331.453634	5.968154
5.875298	331.720124	5.973158
5.576512	331.899511	5.978163
5.963453	335.347802	5.983168
5.604933	335.666201	5.988173
5.552198	333.905893	5.993178
5.717425	335.392408	5.998182
5.703543	334.119588	6.003187
5.834330	340.648082	6.008192
6.159527	358.753945	6.013197
6.365062	349.252962	6.018202
5.834489	345.121507	6.023206
5.992441	341.237186	6.028211
6.001969	330.849258	6.033216
5.928213	338.994612	6.038221
5.846163	335.663343	6.043226
5.773917	335.861241	6.048230
5.985648	332.819585	6.053235
5.957716	334.152680	6.058240
5.545420	337.051542	6.063245
5.850464	348.760363	6.068250
5.944041	346.584973	6.073254
5.860777	357.465257	6.078259
5.956996	351.720796	6.083264
5.990951	358.248553	6.088269
5.966545	352.956300	6.093274
6.281042	352.189163	6.098278
6.159190	358.193858	6.103283
6.063804	349.185811	6.108288
6.040846	340.141182	6.113293
5.850822	336.598938	6.118298
5.748846	339.699417	6.123302
5.784835	349.656310	6.128307
5.987912	347.425907	6.133312
6.031947	346.431966	6.138317
6.145742	353.738217	6.143322
6.039644	361.012270	6.148326
5.893634	362.632667	6.153331
5.751799	358.687453	6.158336
6.015912	356.713297	6.163341
5.769229	354.230222	6.168346
5.988030	358.258345	6.173350
6.189020	357.632266	6.178355
5.996630	359.250392	6.183360
6.320339	364.265078	6.188365
5.715460	360.926624	6.193370
5.943724	359.524354	6.198374
6.029171	358.185447	6.203379
6.101354	358.952472	6.208384
5.995891	354.460601	6.213389
5.712124	355.450722	6.218394
5.881587	361.963710	6.223398
5.747789	362.724841	6.228403
6.328686	369.233883	6.233408
5.786162	369.296197	6.238413
5.910575	358.580321	6.243418
6.175189	359.459751	6.248422
5.891928	365.862897	6.253427
5.799778	359.809245	6.258432
5.832685	365.217216	6.263437
5.963656	359.809021	6.268442
5.923728	354.927302	6.273446
5.900318	358.999464	6.278451
5.910035	358.086795	6.283456
5.924218	362.168923	6.288461
5.996323	360.734019	6.293466
6.122764	359.458332	6.298470
6.144459	365.440680	6.303475
5.925267	355.749563	6.308480
5.901734	366.494004	6.313485
6.235936	355.451241	6.318490
6.255318	359.630635	6.323494
5.777920	355.838906	6.328499
5.933685	346.902486	6.333504
5.825861	355.486579	6.338509
5.823397	354.727665	6.343514
5.936875	352.169531	6.348518
5.936995	353.526733	6.353523
6.187546	355.968060	6.358528
6.148893	356.891544	6.363533
6.166350	358.280848	6.368538
6.038165	347.174044	6.373542
5.732276	337.135773	6.378547
6.169134	350.007296	6.383552
5.837286	339.400435	6.388557
5.840655	349.685104	6.393562
5.803903	350.662075	6.398566
5.657432	360.489197	6.403571
5.707098	356.586931	6.408576
5.849098	361.683691	6.413581
5.610300	358.427443	6.418586
6.216722	357.804677	6.423590
6.253944	364.009230	6.428595
6.110770	358.457060	6.433600
5.854124	363.046421	6.438605
6.050329	365.777781	6.443610
6.091924	362.379801	6.448614
5.795608	362.331016	6.453619
5.930152	364.559455	6.458624
5.952750	363.806129	6.463629
5.560247	355.613120	6.468634
6.065149	356.436155	6.473638
5.824541	360.656028	6.478643
6.172983	355.410125	6.483648
5.780297	358.505251	6.488653
5.696206	359.685742	6.493658
6.238328	352.910087	6.498662
6.170639	357.061909	6.503667
6.285034	360.169831	6.508672
6.083904	365.127030	6.513677
6.064871	368.799886	6.518682
6.551988	365.348357	6.523686
6.068080	356.793098	6.528691
5.782829	342.970982	6.533696
5.854016	350.226918	6.538701
5.913447	362.359962	6.543706
6.102616	359.666658	6.548710
6.025409	356.290340	6.553715
6.015332	349.119779	6.558720
6.034050	345.203352	6.563725
5.683818	336.016695	6.568730
5.807638	345.551793	6.573734
6.151239	365.840918	6.578739
6.288210	357.429431	6.583744
5.892084	345.981536	6.588749
6.048449	338.202943	6.593754
5.818029	329.972055	6.598758
5.565521	339.141807	6.603763
5.858616	346.255626	6.608768
6.014836	350.334619	6.613773
5.929167	353.812206	6.618778
6.229302	358.416115	6.623782
6.028118	358.770128	6.628787
6.017101	362.264567	6.633792
6.194907	365.802373	6.638797
5.691434	356.959099	6.643802
6.065365	347.865326	6.648806
5.804998	350.044520	6.653811
6.012994	353.615587	6.658816
6.390368	361.415469	6.663821
5.971197	343.143886	6.668826
6.142256	343.465251	6.673830
5.912059	338.432830	6.678835
6.197776	338.451609	6.683840
5.873180	338.192096	6.688845
5.840568	343.528005	6.693850
6.170749	341.170248	6.698854
5.932403	337.866478	6.703859
5.844358	345.669216	6.708864
6.150308	339.714936	6.713869
5.872827	335.844629	6.718874
5.994901	340.517385	6.723878
5.890595	347.848101	6.728883
5.827474	338.151675	6.733888
5.946410	339.673872	6.738893
5.941664	333.625602	6.743898
6.201669	331.297754	6.748902
6.063602	335.669332	6.753907
6.147474	335.124762	6.758912
5.951834	341.099812	6.763917
5.929174	335.959150	6.768922
5.949032	334.902536	6.773926
5.874505	338.805485	6.778931
6.365411	332.702189	6.783936
6.268953	343.834452	6.788941
5.997843	341.361509	6.793946
6.214808	337.705279	6.798950
5.959464	334.122587	6.803955
5.889735	329.286643	6.808960
5.980584	336.852719	6.813965
6.237825	334.053910	6.818970
6.077051	336.707970	6.823974
5.814223	344.879601	6.828979
5.801962	339.721500	6.833984
6.294477	327.828379	6.838989
5.800037	339.481340	6.843994
6.166714	335.684743	6.848998
5.825942	332.213427	6.854003
6.109931	332.476080	6.859008
5.906811	333.273313	6.864013
5.808730	334.797661	6.869018
6.264403	338.105539	6.874022
5.954269	348.768045	6.879027
6.129649	328.879000	6.884032
5.906006	336.658555	6.889037
5.634616	351.886581	6.894042
6.077191	336.828033	6.899046
6.057666	343.626699	6.904051
6.038562	345.300101	6.909056
6.013833	340.868429	6.914061
5.620528	347.560780	6.919066
5.642279	342.932049	6.924070
5.972020	343.380565	6.929075
5.843280	334.668779	6.934080
5.847175	337.259236	6.939085
5.817155	343.626109	6.944090
5.944957	336.199972	6.949094
5.842663	345.934788	6.954099
6.136925	341.934333	6.959104
5.954476	339.950615	6.964109
5.739841	339.569579	6.969114
6.438890	338.147793	6.974118
5.802933	341.692073	6.979123
6.082405	339.421304	6.984128
6.067752	339.047096	6.989133
5.960976	335.893681	6.994138
6.017162	341.019614	6.999142
5.757139	342.293935	7.004147
5.991106	342.981986	7.009152
5.942081	336.586274	7.014157
6.279705	336.479915	7.019162
6.108692	337.332258	7.024166
5.794794	353.595108	7.029171
5.940478	337.826659	7.034176
5.999377	339.883378	7.039181
5.460838	336.904753	7.044186
6.050350	337.964546	7.049190
5.737352	342.145067	7.054195
6.255723	339.596660	7.059200
6.217153	346.138869	7.064205
5.781368	339.885630	7.069210
6.318601	338.602931	7.074214
6.208825	351.733569	7.079219
5.972035	338.463887	7.084224
5.983314	333.355905	7.089229
5.885335	334.247497	7.094234
5.992850	328.833472	7.099238
6.182517	346.783258	7.104243
6.308643	337.139624	7.109248
5.913337	332.835253	7.114253
5.731895	340.620894	7.119258
6.013392	333.442906	7.124262
5.840323	333.909598	7.129267
6.319849	333.641942	7.134272
6.010820	335.667363	7.139277
5.679057	331.960530	7.144282
6.166916	331.093637	7.149286
6.072798	338.615748	7.154291
5.887158	332.946814	7.159296
6.091752	335.180161	7.164301
5.989462	333.769248	7.169306
5.958450	341.047421	7.174310
5.947669	332.927865	7.179315
6.176910	331.073035	7.184320
6.142852	317.879369	7.189325
5.365538	320.926808	7.194330
6.013007	321.544150	7.199334
5.600208	337.230771	7.204339
5.915709	343.879200	7.209344
6.278618	339.263790	7.214349
5.894202	338.887042	7.219354
6.191097	333.260036	7.224358
6.032558	339.371675	7.229363
6.112882	328.998034	7.234368
6.327911	323.861496	7.239373
5.775415	319.445563	7.244378
5.626990	317.326839	7.249382
5.843824	326.787334	7.254387
5.924934	331.336754	7.259392
6.083964	326.367119	7.264397
5.937830	340.231060	7.269402
6.170657	332.918284	7.274406
5.927783	334.170952	7.279411
6.017517	335.612274	7.284416
6.216369	332.835211	7.289421
5.922986	326.920467	7.294426
5.746595	313.679363	7.299430
5.678133	323.234896	7.304435
6.012844	331.737421	7.309440
6.210640	331.073876	7.314445
5.974135	325.586867	7.319450
6.265729	321.779817	7.324454
6.041359	324.801275	7.329459
6.102959	317.385453	7.334464
6.250645	310.253619	7.339469
6.034215	316.247716	7.344474
5.938903	306.233622	7.349478
5.577798	310.867708	7.354483
5.963331	308.776578	7.359488
6.036085	315.042019	7.364493
5.803650	310.414908	7.369498
6.311654	310.604718	7.374502
5.758174	309.656355	7.379507
5.628221	306.370515	7.384512
5.706167	309.322755	7.389517
5.964690	326.882156	7.394522
5.996796	326.608233	7.399526
5.853820	337.156122	7.404531
6.139720	339.810238	7.409536
6.246717	328.578244	7.414541
5.823915	326.135249	7.419546
5.979366	320.612525	7.424550
6.046423	324.347897	7.429555
5.974063	327.557656	7.434560
5.921233	324.699559	7.439565
5.665571	339.105727	7.444570
6.123432	335.465773	7.449574
5.951822	338.798553	7.454579
5.813429	334.609203	7.459584
6.126349	335.924029	7.464589
5.905275	334.923910	7.469594
6.382593	331.575152	7.474598
5.794012	315.993810	7.479603
5.680872	306.716471	7.484608
5.683517	310.094879	7.489613
5.752698	333.574574	7.494618
6.331065	323.506200	7.499622
6.075587	330.901573	7.504627
6.253923	332.737218	7.509632
5.874927	336.731864	7.514637
5.584980	336.372045	7.519642
6.239633	334.403524	7.524646
6.125932	336.961671	7.529651
5.818648	331.425570	7.534656
6.033196	332.176755	7.539661
5.982274	337.072595	7.544666
6.029158	333.164440	7.549670
5.892486	333.891217	7.554675
6.265709	329.641192	7.559680
5.988501	317.725555	7.564685
5.747694	324.916166	7.569690
5.679695	320.048318	7.574694
5.905934	330.620973	7.579699
5.919610	329.717180	7.584704
6.203784	326.610462	7.589709
5.749958	343.157676	7.594714
6.238141	330.502775	7.599718
6.134640	339.225391	7.604723
6.416800	322.151243	7.609728
5.749916	311.713619	7.614733
5.665722	318.240776	7.619738
5.689387	321.995558	7.624742
6.095701	336.399894	7.629747
5.921425	331.994672	7.634752
6.402404	331.821701	7.639757
5.885255	324.622534	7.644762
5.847370	303.444295	7.649766
6.002433	308.336529	7.654771
6.092973	310.736325	7.659776
5.945885	308.301024	7.664781
5.936530	309.969740	7.669786
5.976026	296.631762	7.674790
5.909117	303.722524	7.679795
6.073268	312.504692	7.684800
5.854592	301.782158	7.689805
5.509652	316.717891	7.694810
5.912682	318.407820	7.699814
5.414625	335.797131	7.704819
5.554536	338.214553	7.709824
5.753385	329.872537	7.714829
5.699860	332.475097	7.719834
5.806373	323.710870	7.724838
5.520908	340.307797	7.729843
5.695173	339.787117	7.734848
6.064863	347.316111	7.739853
5.840483	360.641766	7.744858
6.125028	361.505438	7.749862
6.029939	352.117699	7.754867
5.827061	344.505766	7.759872
6.145528	336.224216	7.764877
5.882799	340.770226	7.769882
5.905878	336.913233	7.774886
5.677731	339.992229	7.779891
6.170508	356.496473	7.784896
6.580024	353.357581	7.789901
6.219925	351.050351	7.794906
6.014724	337.155665	7.799910
5.846845	346.951311	7.804915
5.992968	334.590107	7.809920
6.122370	333.605021	7.814925
5.842707	340.311314	7.819930
5.903298	336.625647	7.824934
5.912619	332.650577	7.829939
6.055547	335.247860	7.834944
6.079325	334.064087	7.839949
5.867611	332.983419	7.844954
5.720158	331.275822	7.849958
6.393006	333.195822	7.854963
6.248231	335.559494	7.859968
6.081240	339.508477	7.864973
5.851174	340.638930	7.869978
6.149691	334.768065	7.874982
6.098050	330.818305	7.879987
6.111260	339.630315	7.884992
6.121720	339.802681	7.889997
6.014652	339.591555	7.895002
6.148239	334.306345	7.900006
6.244597	333.639611	7.905011
6.478836	338.712512	7.910016
6.069674	325.700627	7.915021
5.766106	317.234365	7.920026
5.792806	318.774085	7.925030
5.706556	322.343503	7.930035
5.982292	336.540384	7.935040
6.268686	331.993836	7.940045
6.086914	329.086213	7.945050
5.925040	314.659624	7.950054
5.880045	319.054671	7.955059
5.885734	325.985444	7.960064
5.897370	329.590243	7.965069
5.872014	333.697504	7.970074
6.235660	331.249117	7.975078
5.825537	326.801525	7.980083
5.842189	332.585333	7.985088
6.066685	335.720401	7.990093
5.981425	338.808786	7.995098
6.224445	330.817391	8.000102
5.921547	330.007179	8.005107
6.206458	319.642818	8.010112
5.647810	311.142952	8.015130
5.618068	327.345419	8.020147
6.179437	325.481386	8.025165
6.144417	332.795271	8.030182
5.939881	322.501884	8.035200
6.141196	314.003978	8.040218
5.772777	322.272277	8.045235
5.892673	325.964621	8.050253
6.085885	324.486096	8.055270
5.693586	326.238584	8.060288
5.886093	321.039680	8.065306
5.891564	335.624145	8.070323
6.413151	331.270201	8.075341
5.985781	338.417970	8.080358
6.174812	333.762373	8.085376
6.120616	336.689762	8.090394
6.089650	335.255606	8.095411
6.182707	327.879020	8.100429
5.943887	331.021335	8.105446
5.711461	331.205829	8.110464
5.919457	326.439989	8.115482
6.028296	328.527840	8.120499
5.976717	332.205861	8.125517
5.774454	333.177721	8.130534
6.092578	332.314028	8.135552
6.321780	328.302238	8.140570
5.918105	335.070797	8.145587
6.225122	326.502781	8.150605
6.150412	328.363604	8.155622
5.803895	332.788096	8.160640
5.874763	326.197562	8.165658
5.853221	332.625772	8.170675
5.932960	329.662833	8.175693
6.248111	334.956239	8.180710
5.704393	334.192021	8.185728
6.101023	326.534653	8.190746
5.568416	338.807775	8.195763
6.021160	354.398686	8.200781
6.188324	357.149610	8.205798
6.077137	365.081249	8.210816
6.284753	363.426917	8.215834
6.444093	365.585800	8.220851
6.121872	363.512216	8.225869
6.518096	359.875179	8.230886
6.177089	360.329030	8.235904
6.081024	348.059089	8.240922
6.099659	362.171337	8.245939
6.147991	364.113986	8.250957
6.210749	362.204512	8.255974
6.293102	361.705713	8.260992
6.442518	359.353581	8.266010
6.370394	362.880180	8.271027
6.226033	342.709738	8.276045
6.011141	340.518466	8.281062
5.877020	341.110509	8.286080
6.407475	345.947542	8.291098
5.893509	348.072407	8.296115
5.890494	356.978070	8.301133
6.181588	358.674649	8.306150
6.387589	355.550043	8.311168
6.117780	353.572436	8.316186
6.303101	365.310940	8.321203
6.215909	367.135843	8.326221
6.397810	355.797711	8.331238
6.592076	360.330504	8.336256
6.330020	353.103868	8.341274
6.190751	365.060159	8.346291
6.211686	354.911519	8.351309
6.152716	356.063031	8.356326
6.165415	362.173513	8.361344
6.087879	354.514224	8.366362
6.197236	366.677946	8.371379
6.307735	360.958496	8.376397
6.352527	349.038989	8.381414
6.571168	360.381004	8.386432
6.731115	351.498222	8.391450
6.256659	360.502533	8.396467
6.472884	357.016593	8.401485
6.468553	358.083863	8.406502
6.012731	355.892233	8.411520
6.223585	358.661599	8.416538
5.895205	359.504783	8.421555
6.282869	355.035992	8.426573
6.281102	356.743457	8.431590
6.027168	364.258688	8.436608
6.450060	373.953224	8.441626
6.236758	380.550156	8.446643
6.557366	383.479153	8.451661
6.663432	386.413154	8.456678
6.290476	389.222932	8.461696
6.824658	381.051845	8.466714
6.458560	378.691616	8.471731
6.180546	368.977658	8.476749
6.625787	368.166751	8.481766
6.355333	386.069770	8.486784
6.487159	384.493505	8.491802
6.705117	380.104777	8.496819
6.496225	365.700245	8.501837
6.611952	361.276948	8.506854
6.281277	360.299687	8.511872
6.416733	363.216485	8.516890
6.342682	376.579511	8.521907
6.335841	385.870772	8.526925
6.629833	382.628325	8.531942
6.292796	384.116608	8.536960
6.544067	380.413778	8.541978
6.736939	385.385429	8.546995
6.373116	380.828520	8.552013
6.770946	376.970335	8.557030
6.549193	383.798946	8.562048
6.507213	375.117996	8.567066
6.756967	374.236546	8.572083
6.534467	379.780926	8.577101
6.805111	381.780477	8.582119
6.314691	372.497199	8.587136
6.511061	373.463797	8.592154
6.660242	377.990993	8.597171
6.146601	376.259619	8.602189
6.314513	374.097099	8.607207
6.381075	385.948777	8.612224
6.439540	381.086290	8.617242
6.442180	380.606212	8.622259
6.300813	386.286277	8.627277
6.822407	382.348864	8.632295
6.703778	381.016711	8.637312
6.212211	380.866032	8.642330
6.158264	380.732419	8.647347
6.395588	385.264826	8.652365
6.984813	396.716414	8.657383
6.731351	386.402207	8.662400
6.758332	386.814542	8.667418
6.723240	387.220763	8.672435
6.542842	382.070435	8.677453
6.404171	384.708043	8.682471
6.540267	391.260045	8.687488
7.025478	394.062435	8.692506
6.352494	394.760469	8.697523
6.398228	408.309985	8.702541
6.660225	405.378613	8.707559
6.965896	409.120941	8.712576
6.830767	405.957925	8.717594
7.051375	400.331767	8.722611
6.872355	406.528915	8.727629
6.871718	388.027470	8.732647
6.753264	387.840787	8.737664
6.669960	388.298694	8.742682
7.018625	380.629838	8.747699
6.718214	372.544519	8.752717
7.086970	377.046994	8.757735
6.552100	380.162833	8.762752
6.284187	383.155061	8.767770
6.678178	388.044909	8.772787
6.713241	408.191378	8.777805
7.093006	400.934216	8.782823
6.547116	398.523086	8.787840
6.843101	399.843387	8.792858
6.957230	405.669861	8.797875
6.964137	401.355011	8.802893
7.052318	387.491157	8.807911
6.663514	380.113839	8.812928
6.598506	385.005727	8.817946
6.726180	389.170220	8.822963
6.830872	399.125740	8.827981
6.856359	399.961164	8.832999
6.589366	405.597682	8.838016
6.596105	405.252659	8.843034
6.671256	419.371930	8.848051
6.514941	407.082929	8.853069
7.048584	405.333652	8.858087
6.602151	409.148902	8.863104
6.893294	403.697944	8.868122
6.762003	406.747795	8.873139
6.694380	412.384830	8.878157
6.932946	406.954679	8.883175
6.754024	414.022772	8.888192
6.650386	408.778438	8.893210
6.730877	409.226621	8.898227
6.891919	410.334415	8.903245
7.311374	410.026113	8.908263
7.315056	413.443095	8.913280
6.857498	411.302219	8.918298
7.435893	406.592291	8.923315
7.204094	409.578900	8.928333
7.020837	399.247444	8.933351
6.797464	407.392219	8.938368
7.247046	412.860368	8.943386
7.364167	405.435825	8.948403
6.905414	410.171285	8.953421
6.853407	404.448723	8.958439
7.101512	412.848279	8.963456
7.024950	416.274600	8.968474
7.308704	405.090983	8.973491
6.737843	415.012846	8.978509
6.983821	411.213009	8.983527
6.861924	405.520261	8.988544
7.332070	416.870488	8.993562
7.529512	398.600111	8.998579
7.024380	410.616552	9.003597
7.191180	403.200053	9.008615
7.231745	414.052302	9.013632
7.042684	412.122073	9.018650
7.227128	408.735740	9.023667
7.036813	405.041702	9.028685
7.236349	402.454554	9.033703
7.163283	406.369453	9.038720
7.119398	408.761944	9.043738
7.464110	403.444649	9.048755
6.855298	391.614255	9.053773
7.078099	392.501004	9.058791
7.276891	397.812547	9.063808
7.082267	405.940222	9.068826
7.212517	395.765072	9.073843
6.940325	392.995765	9.078861
7.053153	393.943816	9.083879
7.323006	400.730603	9.088896
7.163142	404.728440	9.093914
7.248550	400.470792	9.098931
7.141757	409.869141	9.103949
7.108110	401.616049	9.108967
7.331844	407.687377	9.113984
7.288818	402.379962	9.119002
6.825913	388.920630	9.124019
6.856056	396.470535	9.129037
7.217482	401.103539	9.134055
7.181018	402.330441	9.139072
7.213105	401.719553	9.144090
7.037831	402.772417	9.149107
7.270849	405.875994	9.154125
7.191907	403.805551	9.159143
7.403567	404.965420	9.164160
7.020645	402.276465	9.169178
6.946347	398.182532	9.174195
6.890476	417.068289	9.179213
7.217317	405.398305	9.184231
7.181225	402.674283	9.189248
7.107523	408.075590	9.194266
7.003727	408.060185	9.199283
7.166465	420.307146	9.204301
7.558449	428.999873	9.209319
7.363058	417.720445	9.214336
7.309536	422.932431	9.219354
7.432758	419.760745	9.224371
7.409209	412.894560	9.229389
6.854567	409.181510	9.234407
7.423186	431.289790	9.239424
7.326479	429.064328	9.244442
7.485711	426.313046	9.249459
7.600616	431.015997	9.254477
7.231184	417.157101	9.259495
7.605585	424.262118	9.264512
7.067049	421.887708	9.269530
7.268452	420.695063	9.274547
7.348677	434.924004	9.279565
7.514416	425.355508	9.284583
7.618021	435.349086	9.289600
7.324544	429.847139	9.294618
7.510643	429.988560	9.299635
7.410811	421.404953	9.304653
7.479372	424.559384	9.309671
7.740513	419.068913	9.314688
7.157850	413.914939	9.319706
7.240993	423.804404	9.324723
7.454698	434.336234	9.329741
7.771110	424.933617	9.334759
7.579472	424.739395	9.339776
7.461772	434.795830	9.344794
7.741328	429.444493	9.349811
7.587495	422.873130	9.354829
7.245600	413.134382	9.359847
7.445429	435.177016	9.364864
7.445641	433.141580	9.369882
7.839272	429.353462	9.374899
7.764430	418.440253	9.379917
7.502989	416.177328	9.384935
7.565583	403.485035	9.389952
7.304700	408.227555	9.394970
7.826191	423.306076	9.399987
7.528292	420.023241	9.405005
7.381170	406.868161	9.410023
7.445272	405.479155	9.415040
7.568824	433.914378	9.420058
7.540228	423.678742	9.425075
7.753710	426.321483	9.430093
7.928074	426.856032	9.435111
7.318341	408.102279	9.440128
7.798243	423.663778	9.445146
7.621333	424.997752	9.450163
7.477303	423.821022	9.455181
7.750125	423.390390	9.460199
7.855335	420.344579	9.465216
7.479037	403.337427	9.470234
7.784523	413.649837	9.475251
7.661311	408.020406	9.480269
7.897339	408.097252	9.485287
7.817850	403.486599	9.490304
7.103022	404.317374	9.495322
7.268049	407.497806	9.500339
7.592600	426.690397	9.505357
8.102389	442.739541	9.510375
7.957699	428.353363	9.515392
7.473002	433.045534	9.520410
7.530913	429.934505	9.525427
7.175395	425.003925	9.530445
7.346125	430.666968	9.535463
7.572948	438.041108	9.540480
7.631102	444.914519	9.545498
7.624096	442.356368	9.550515
7.839325	446.207455	9.555533
7.477090	455.778137	9.560551
7.465269	431.222691	9.565568
7.809270	442.289633	9.570586
7.988751	449.898356	9.575603
7.671075	443.431387	9.580621
7.822812	454.174838	9.585639
8.240300	437.290204	9.590656
7.630960	441.042467	9.595674
7.635857	433.054745	9.600691
7.873005	436.233420	9.605709
7.766697	451.498069	9.610727
8.101048	452.162336	9.615744
8.014114	448.553173	9.620762
7.961880	448.198397	9.625779
7.627710	442.024317	9.630797
7.796522	446.611586	9.635815
7.698734	440.135628	9.640832
7.832239	442.683532	9.645850
7.946192	451.425871	9.650867
7.967466	456.200208	9.655885
7.896152	465.798180	9.660903
8.019921	461.319960	9.665920
7.935087	454.580061	9.670938
8.072925	461.709302	9.675955
7.999668	445.917188	9.680973
7.500380	449.235772	9.685991
8.043593	453.780528	9.691008
7.918635	459.549576	9.696026
8.064606	463.020149	9.701043
8.246754	466.150590	9.706061
7.989760	457.127555	9.711079
7.853473	446.877116	9.716096
8.044485	467.324403	9.721114
8.069724	462.031587	9.726131
8.185491	463.301060	9.731149
8.096123	456.653379	9.736167
7.969177	440.326858	9.741184
8.147158	440.251803	9.746202
7.733425	432.297704	9.751219
7.937197	447.097526	9.756237
8.110759	457.569350	9.761255
8.247448	457.595394	9.766272
8.256188	461.153602	9.771290
8.106847	448.162931	9.776307
7.908135	445.874457	9.781325
7.719201	438.134652	9.786343
8.207055	447.408879	9.791360
8.196565	450.963768	9.796378
8.343678	466.040657	9.801395
8.324428	458.053528	9.806413
7.719667	450.722427	9.811431
8.294132	449.818817	9.816448
7.944379	470.321902	9.821466
8.134735	456.609336	9.826483
8.260498	460.537469	9.831501
7.903926	463.054388	9.836519
8.191347	466.761702	9.841536
8.070206	473.442144	9.846554
8.227610	463.878081	9.851571
8.271021	461.772802	9.856589
8.083083	460.587128	9.861607
8.400454	460.809091	9.866624
8.275984	468.805957	9.871642
8.594632	462.628053	9.876659
8.525375	463.837976	9.881677
8.310209	447.872305	9.886695
8.231230	437.114356	9.891712
8.045680	437.351509	9.896730
7.898642	437.917166	9.901747
8.273675	448.461753	9.906765
7.903157	461.561747	9.911783
8.119688	458.536465	9.916800
8.258068	461.162504	9.921818
8.128271	465.711069	9.926835
8.100993	466.942857	9.931853
8.291410	476.613687	9.936871
8.423441	465.655617	9.941888
8.370297	464.341663	9.946906
8.141565	469.098127	9.951923
8.416122	471.822881	9.956941
8.113796	469.698852	9.961959
8.355239	463.220558	9.966976
8.348160	465.509501	9.971994
7.990775	466.660148	9.977011
8.220692	462.717641	9.982029
8.130494	469.055608	9.987047
8.134502	470.326705	9.992064
8.024567	478.100416	9.997082
8.219024	480.332737	10.002099
8.522258	483.400150	10.007117
8.144115	488.883594	10.012135
8.263005	485.829330	10.017152
8.458349	490.134782	10.022170
8.458088	490.327309	10.027187
8.507248	482.493612	10.032205
8.157715	490.162629	10.037223
8.663747	483.169783	10.042240
8.448972	480.527216	10.047258
8.393418	488.519673	10.052275
8.630180	488.839390	10.057293
8.557421	489.147341	10.062311
8.493119	482.369522	10.067328
8.609770	486.573622	10.072346
8.380384	494.347004	10.077363
8.790747	494.279947	10.082381
8.619714	492.618289	10.087399
8.238731	493.526471	10.092416
8.722817	484.482707	10.097434
8.420159	492.636710	10.102451
8.649127	479.482978	10.107469
8.429947	490.350470	10.112487
8.508775	480.451509	10.117504
9.026571	484.763557	10.122522
8.782433	486.994742	10.127539
8.716647	487.673976	10.132557
8.736971	487.295279	10.137575
8.813013	487.027822	10.142592
8.598443	480.768838	10.147610
8.558879	490.330323	10.152627
8.489338	484.203385	10.157645
8.551468	489.321648	10.162663
8.646973	483.888503	10.167680
8.637938	487.525219	10.172698
8.476389	489.547895	10.177715
8.586529	484.121938	10.182733
8.430417	494.714538	10.187751
8.678213	481.513694	10.192768
8.446443	485.936136	10.197786
8.595863	492.126356	10.202803
8.601095	484.536172	10.207821
8.371194	496.759115	10.212839
8.435850	488.705262	10.217856
9.017902	487.803624	10.222874
8.646656	481.628992	10.227891
8.599021	484.255596	10.232909
8.716023	485.834133	10.237927
8.668537	482.606968	10.242944
8.946421	488.934967	10.247962
8.793300	500.170860	10.252979
8.885450	487.773693	10.257997
8.793205	490.940550	10.263015
8.799744	490.567155	10.268032
8.708040	485.598638	10.273050
8.413739	493.707161	10.278067
8.741177	499.011326	10.283085
8.916612	511.508826	10.288103
8.652245	510.606434	10.293120
8.681842	505.145677	10.298138
8.668652	508.757799	10.303155
8.609854	506.999774	10.308173
8.665777	518.761682	10.313191
8.923076	513.694639	10.318208
8.810408	507.274620	10.323226
8.823045	523.341284	10.328243
9.083581	515.219053	10.333261
9.073743	512.554040	10.338279
9.020752	520.123252	10.343296
9.123419	511.479673	10.348314
9.090211	516.877864	10.353331
9.462334	510.811532	10.358349
9.364852	512.483424	10.363367
9.175506	510.906663	10.368384
9.078695	500.766806	10.373402
8.873374	498.018628	10.378419
8.809483	500.461581	10.383437
8.950191	507.621950	10.388455
9.049712	513.605362	10.393472
8.967189	512.071926	10.398490
8.861157	519.090844	10.403507
8.912949	518.603111	10.408525
8.738099	518.377872	10.413543
9.031229	518.149195	10.418560
9.112400	514.674784	10.423578
8.735453	515.415088	10.428595
8.813446	506.971004	10.433613
9.036295	506.696467	10.438631
8.619832	507.616485	10.443648
9.042578	502.659379	10.448666
8.663180	510.437191	10.453683
9.103027	518.074830	10.458701
8.979966	513.209014	10.463719
8.956408	522.386189	10.468736
9.424517	535.043254	10.473754
9.519187	530.856713	10.478771
9.313146	514.160603	10.483789
9.484993	518.236201	10.488807
9.110248	513.075071	10.493824
9.372548	510.613828	10.498842
9.060658	523.553268	10.503859
9.137336	519.236994	10.508877
9.279302	519.820768	10.513895
9.284887	516.654758	10.518912
8.918234	508.557602	10.523930
8.944927	514.034824	10.528947
9.542166	517.807515	10.533965
9.345461	514.493128	10.538983
9.093574	526.880454	10.544000
9.188403	512.971288	10.549018
9.180296	528.214403	10.554035
9.014298	515.841631	10.559053
9.029746	522.652296	10.564071
9.187989	535.771000	10.569088
9.377217	529.657402	10.574106
9.535629	544.148801	10.579123
9.773304	530.037508	10.584141
9.349719	524.685171	10.589159
8.960661	514.600275	10.594176
9.670324	528.582974	10.599194
9.199325	526.813389	10.604211
9.175207	531.553790	10.609229
9.160801	536.317926	10.614247
9.294537	538.616510	10.619264
9.473673	533.883510	10.624282
9.355369	545.789323	10.629299
9.331936	538.260381	10.634317
9.304484	543.045484	10.639335
9.334742	551.434845	10.644352
9.715876	541.236328	10.649370
9.453224	540.321046	10.654387
9.442366	536.917762	10.659405
9.771008	525.714458	10.664423
9.260835	529.211468	10.669440
9.758500	529.342247	10.674458
9.615713	536.149154	10.679475
9.778961	535.199117	10.684493
9.568255	526.124660	10.689511
9.251297	514.368659	10.694528
9.514067	517.805279	10.699546
9.314803	532.431248	10.704563
9.338988	542.068039	10.709581
9.491367	541.059736	10.714599
9.502933	528.709800	10.719616
9.729624	541.054179	10.724634
9.428477	536.140347	10.729651
9.412713	532.292879	10.734669
9.631822	527.320137	10.739687
9.490542	540.087864	10.744704
9.783008	538.410839	10.749722
9.772283	541.795376	10.754739
9.380744	541.584941	10.759757
9.559341	539.427049	10.764775
9.335025	532.784572	10.769792
9.662599	532.048781	10.774810
9.456110	536.123332	10.779827
9.778271	534.889788	10.784845
9.668476	534.903718	10.789863
9.588126	541.416895	10.794880
9.546132	526.777972	10.799898
9.377535	533.705656	10.804915
9.597359	530.935458	10.809933
9.665964	532.294327	10.814951
9.296319	537.445117	10.819968
9.816995	543.268296	10.824986
9.545577	547.703238	10.830003
9.698870	559.825538	10.835021
10.154054	560.086003	10.840039
9.834344	551.908938	10.845056
9.822502	547.483367	10.850074
9.910516	546.993149	10.855091
9.676399	542.643211	10.860109
9.715232	537.726936	10.865127
9.349860	533.264898	10.870144
9.777181	549.503696	10.875162
9.848341	564.128611	10.880179
9.804998	559.452332	10.885197
9.774862	559.561153	10.890215
9.865489	561.964278	10.895232
9.845872	568.600547	10.900250
9.997447	561.293646	10.905267
9.780424	567.843891	10.910285
10.292334	567.268738	10.915303
9.771230	574.674182	10.920320
9.919812	573.780073	10.925338
10.011361	568.783001	10.930355
9.841683	573.385137	10.935373
10.056632	570.962816	10.940391
9.870953	573.377406	10.945408
10.119851	563.104796	10.950426
9.919547	569.125441	10.955443
9.922145	571.078390	10.960461
10.100490	568.996269	10.965479
10.110464	575.429126	10.970496
10.319325	567.662041	10.975514
10.292136	563.371395	10.980531
10.176555	554.657638	10.985549
10.290836	540.095354	10.990567
10.253570	540.789083	10.995584
9.802515	536.097399	11.000602
9.723916	543.168858	11.005619
9.379950	541.622479	11.010637
9.729352	549.157454	11.015655
9.706403	565.450593	11.020672
9.986905	566.760694	11.025690
9.963118	556.095062	11.030707
10.217981	562.313068	11.035725
10.281279	562.318982	11.040743
9.932743	560.722822	11.045760
10.155323	559.706744	11.050778
10.094292	568.182907	11.055795
10.285323	559.320428	11.060813
10.331959	552.263388	11.065831
9.890512	558.485670	11.070848
10.223871	555.798772	11.075866
10.179695	563.044752	11.080883
10.023388	559.922874	11.085901
10.021861	557.518481	11.090919
10.011961	564.165859	11.095936
10.136364	555.859686	11.100954
10.152217	554.165769	11.105971
9.985743	564.753713	11.110989
10.507928	569.058787	11.116007
10.341919	565.679654	11.121024
10.358916	558.065517	11.126042
10.136311	561.034941	11.131059
10.022370	569.554055	11.136077
10.483397	578.431758	11.141095
10.501069	574.598008	11.146112
10.097613	575.995666	11.151130
10.268226	573.138453	11.156147
10.723782	585.693372	11.161165
10.599866	568.432181	11.166183
10.253961	571.401871	11.171200
10.407577	560.440382	11.176218
10.700927	564.478139	11.181235
10.203255	564.978476	11.186253
10.055201	561.375651	11.191271
10.205948	574.744849	11.196288
10.504239	579.583381	11.201306
10.537644	585.097448	11.206323
10.360406	583.023354	11.211341
10.721686	577.062826	11.216359
10.298184	577.097198	11.221376
10.168584	579.752356	11.226394
10.515994	580.376727	11.231411
9.993548	596.662462	11.236429
10.574906	587.114371	11.241447
10.688527	597.807042	11.246464
10.741574	591.604177	11.251482
10.632430	587.537716	11.256499
10.507779	586.919668	11.261517
10.733159	591.416120	11.266535
10.636335	588.139815	11.271552
10.398592	589.117213	11.276570
10.849708	580.207918	11.281587
10.351062	594.407200	11.286605
10.381146	583.913036	11.291623
10.635083	594.549145	11.296640
10.307736	594.805222	11.301658
10.582614	590.697902	11.306675
10.475549	593.586230	11.311693
10.802492	592.408740	11.316711
10.604901	582.956686	11.321728
10.573803	589.904007	11.326746
10.619720	578.088309	11.331763
10.205409	591.791640	11.336781
10.606548	585.607161	11.341799
10.817883	585.501668	11.346816
10.741738	590.442681	11.351834
10.918755	585.889871	11.356851
10.659741	597.994344	11.361869
11.017724	593.075698	11.366887
10.864341	588.590108	11.371904
10.534416	591.866569	11.376922
10.539049	592.528531	11.381939
10.645497	597.052969	11.386957
10.723424	585.964399	11.391975
10.950141	593.985534	11.396992
10.750688	594.455219	11.402010
10.865258	590.215075	11.407027
10.562656	592.054605	11.412045
10.833857	593.164193	11.417063
10.841910	585.276893	11.422080
10.712900	590.169336	11.427098
11.036510	592.024970	11.432115
10.777414	588.054436	11.437133
10.596260	594.450789	11.442151
10.765997	593.774283	11.447168
10.863243	605.589773	11.452186
10.798389	605.044462	11.457203
10.890696	621.184013	11.462221
10.950905	616.254921	11.467239
11.151583	617.164060	11.472256
11.142993	610.292315	11.477274
11.052003	609.451283	11.482291
10.737336	600.159454	11.487309
10.596633	604.293203	11.492327
11.008727	606.545301	11.497344
10.728051	617.952600	11.502362
11.057103	616.831582	11.507379
10.839322	616.562535	11.512397
10.727307	612.894131	11.517415
10.965415	618.862311	11.522432
10.880476	624.937594	11.527450
11.097542	622.344529	11.532467
10.536868	620.203903	11.537485
10.929300	622.459065	11.542503
11.204891	628.680179	11.547520
10.989848	614.172265	11.552538
11.143239	613.921164	11.557555
10.939206	619.061972	11.562573
11.026351	617.319081	11.567591
11.117181	633.847022	11.572608
11.112868	630.603641	11.577626
11.591865	625.129678	11.582643
10.910930	623.746206	11.587661
10.863077	629.799938	11.592679
11.453947	642.690421	11.597696
11.394895	643.147714	11.602714
11.079821	621.848554	11.607731
11.138052	632.628761	11.612749
11.500177	644.642868	11.617767
11.271471	638.868850	11.622784
11.431289	635.379015	11.627802
11.446002	623.145283	11.632819
10.982845	620.001746	11.637837
11.468183	615.091666	11.642855
11.411909	621.105682	11.647872
10.930210	619.571274	11.652890
11.200657	632.448525	11.657907
11.135813	642.780860	11.662925
11.077927	644.538114	11.667943
11.232655	639.903556	11.672960
11.060952	645.774612	11.677978
11.394442	638.341529	11.682995
11.546071	640.760413	11.688013
11.656949	647.751921	11.693031
11.271242	642.280046	11.698048
11.421149	645.365048	11.703066
11.887596	640.631466	11.708083
11.565407	640.397609	11.713101
11.407391	642.400818	11.718119
11.689404	644.755222	11.723136
11.732291	644.126865	11.728154
11.560959	645.835513	11.733171
11.417847	641.323064	11.738189
11.684823	635.500272	11.743207
11.496992	624.904318	11.748224
11.264391	638.674064	11.753242
11.533639	628.306733	11.758259
11.310812	643.469772	11.763277
10.841219	646.146319	11.768295
11.378559	641.726734	11.773312
11.432117	636.211715	11.778330
11.560436	642.083392	11.783347
11.341319	643.203055	11.788365
11.324506	645.086453	11.793383
11.207908	636.480108	11.798400
11.547657	657.986856	11.803418
12.052721	661.070211	11.808435
11.540166	657.350555	11.813453
11.373468	653.210991	11.818471
11.611702	651.021711	11.823488
11.508670	666.570046	11.828506
11.521256	667.565276	11.833523
12.272708	671.500175	11.838541
12.072493	670.928602	11.843559
11.948408	651.439439	11.848576
11.445808	651.530306	11.853594
11.813672	646.083107	11.858611
11.681423	643.137343	11.863629
11.491023	641.740609	11.868647
11.835894	653.217786	11.873664
11.789383	670.903193	11.878682
11.778275	667.146485	11.883699
11.791386	666.450183	11.888717
11.728508	676.697027	11.893735
11.819940	664.669065	11.898752
11.596975	673.697491	11.903770
11.647843	669.501959	11.908787
11.482686	673.604818	11.913805
11.938854	674.045007	11.918823
12.284565	668.885263	11.923840
11.961940	674.865030	11.928858
12.021525	669.904463	11.933875
11.803746	671.550920	11.938893
12.037156	675.377137	11.943911
11.954072	680.947239	11.948928
11.836897	679.264555	11.953946
11.868417	670.385832	11.958963
11.866529	678.319527	11.963981
12.268570	673.756904	11.968999
12.203441	674.612760	11.974016
12.104338	672.472844	11.979034
12.040462	672.107253	11.984051
11.803382	663.207240	11.989069
11.754025	670.343621	11.994087
11.883766	668.672985	11.999104
11.662335	670.143291	12.004122
11.923418	665.422743	12.009139
12.266298	668.275739	12.014157
12.120689	670.251774	12.019175
12.262705	665.612878	12.024192
11.922487	672.589426	12.029210
12.326886	668.865851	12.034227
12.028715	669.104764	12.039245
11.966063	660.306977	12.044263
11.956225	663.199112	12.049280
11.877605	669.027282	12.054298
12.173976	683.481535	12.059315
12.223960	687.465697	12.064333
12.372477	691.194685	12.069351
12.336662	680.436180	12.074368
12.309092	680.326858	12.079386
12.142471	678.809658	12.084403
12.099541	679.718861	12.089421
12.240983	687.765938	12.094439
12.456200	693.362181	12.099456
12.090483	690.219238	12.104474
12.495228	702.472892	12.109491
12.313686	696.820895	12.114509
12.179220	692.537453	12.119527
12.382196	692.912926	12.124544
12.155832	696.343690	12.129562
12.508948	694.111271	12.134579
12.504468	697.826214	12.139597
12.572867	697.888136	12.144615
12.232965	690.768153	12.149632
12.082696	697.790873	12.154650
11.898075	696.374300	12.159667
12.261884	697.756644	12.164685
12.086592	698.623343	12.169703
12.354550	694.043723	12.174720
12.292436	699.342331	12.179738
12.451651	702.189217	12.184755
12.654568	705.247042	12.189773
12.376362	707.436223	12.194791
12.854777	698.431103	12.199808
12.441007	710.190532	12.204826
12.738599	697.202674	12.209843
12.925755	690.966272	12.214861
12.516595	701.197620	12.219879
12.995897	691.914664	12.224896
12.983580	696.344014	12.229914
13.035343	695.275631	12.234931
12.867494	682.322384	12.239949
12.569802	673.053120	12.244967
12.808220	669.216537	12.249984
12.843162	673.367133	12.255002
12.532241	670.897292	12.260019
12.400971	671.760291	12.265037
12.631499	679.642021	12.270055
12.813369	682.696808	12.275072
12.510006	679.212811	12.280090
12.233394	690.610056	12.285107
12.860839	698.742410	12.290125
12.814189	697.045588	12.295143
12.940259	710.409263	12.300160
12.753994	694.328421	12.305178
12.633022	700.238932	12.310195
12.852889	694.612796	12.315213
12.785183	694.427676	12.320231
13.163437	710.516476	12.325248
13.238448	696.928978	12.330266
12.509384	681.740518	12.335283
12.934659	678.793147	12.340301
12.621744	688.643443	12.345319
12.876442	687.934771	12.350336
12.894755	694.571493	12.355354
12.709404	698.674346	12.360371
13.154458	697.626777	12.365389
13.101589	704.094711	12.370407
12.896171	692.983921	12.375424
12.963354	689.281289	12.380442
12.652584	693.132278	12.385459
12.758408	701.683508	12.390477
12.738608	695.438303	12.395495
12.752189	693.801529	12.400512
12.919935	697.966166	12.405530
12.790165	707.153662	12.410547
13.092868	699.330885	12.415565
12.885914	697.917789	12.420583
12.527804	696.654456	12.425600
12.241980	699.763130	12.430618
12.980789	718.733753	12.435635
12.921864	722.141608	12.440653
12.920429	722.971772	12.445671
13.031853	728.871354	12.450688
12.885328	730.326847	12.455706
12.728321	725.182244	12.460723
13.390439	716.325233	12.465741
12.895873	711.880109	12.470759
13.114553	718.031223	12.475776
13.420270	719.138601	12.480794
13.110894	722.124718	12.485811
13.719226	715.491383	12.490829
13.269682	727.846508	12.495847
13.444152	725.402068	12.500864
13.331740	716.968595	12.505882
13.278768	727.703060	12.510899
13.259034	722.606510	12.515917
12.983878	727.455475	12.520935
13.385201	720.914327	12.525952
13.503820	720.974742	12.530970
12.948661	724.885879	12.535987
13.357713	716.989733	12.541005
13.208414	718.650778	12.546023
13.312473	718.126499	12.551040
13.542767	719.854670	12.556058
13.336969	725.743684	12.561075
13.421989	721.628027	12.566093
13.439272	724.982992	12.571111
13.384132	721.674927	12.576128
13.549674	725.972453	12.581146
13.439682	712.700917	12.586163
13.650870	714.176450	12.591181
13.413508	722.077402	12.596199
13.134779	718.687388	12.601216
13.431226	713.333337	12.606234
13.274215	726.144671	12.611251
13.441281	716.496920	12.616269
13.287512	716.413558	12.621287
13.421118	714.278428	12.626304
13.469433	719.250591	12.631322
13.274456	718.668733	12.636339
13.520665	716.989426	12.641357
13.139229	731.817486	12.646375
13.647118	737.592229	12.651392
13.926151	743.774979	12.656410
13.420060	750.196734	12.661427
13.902889	745.403770	12.666445
14.279513	740.826153	12.671463
13.680914	735.661943	12.676480
13.574522	717.754115	12.681498
13.661563	715.793487	12.686515
13.769182	712.422214	12.691533
13.614885	718.950125	12.696551
13.558533	724.904229	12.701568
13.844709	726.633168	12.706586
13.664667	725.244281	12.711603
13.859478	730.196793	12.716621
13.704024	730.277790	12.721639
13.935793	731.835325	12.726656
13.712152	729.815774	12.731674
13.800230	731.550310	12.736691
13.974107	739.907932	12.741709
13.877803	733.450570	12.746727
13.528911	731.270645	12.751744
14.010763	745.099642	12.756762
13.870874	747.172622	12.761779
14.061451	748.629277	12.766797
13.937996	744.972094	12.771815
13.735309	746.988581	12.776832
14.035300	749.507452	12.781850
13.989459	751.322800	12.786867
14.365312	743.583285	12.791885
13.949573	732.562020	12.796903
13.808754	729.655444	12.801920
13.947953	725.739626	12.806938
14.052581	738.822648	12.811955
14.077737	733.482428	12.816973
13.843787	749.089087	12.821991
13.540208	749.881091	12.827008
13.405009	751.549411	12.832026
13.515401	750.967343	12.837043
13.594384	743.539129	12.842061
13.588355	747.147029	12.847079
13.628057	764.001778	12.852096
14.089602	763.099957	12.857114
13.978860	773.123942	12.862131
13.976387	779.448361	12.867149
14.250046	779.285827	12.872167
14.259324	770.656663	12.877184
13.972814	765.516433	12.882202
14.168151	771.343006	12.887219
14.229968	771.535338	12.892237
14.564606	778.914923	12.897255
14.193783	772.512912	12.902272
14.330545	775.391707	12.907290
14.015683	775.241911	12.912307
13.884898	778.979691	12.917325
13.993002	772.503112	12.922343
13.988494	779.907101	12.927360
14.149748	781.671273	12.932378
14.562831	797.773664	12.937395
14.594693	793.767249	12.942413
14.558566	781.067968	12.947431
14.118830	780.000368	12.952448
14.418675	780.676332	12.957466
14.483742	788.473423	12.962483
14.345923	790.038015	12.967501
14.220660	788.501743	12.972519
14.157514	802.699654	12.977536
14.927118	791.935597	12.982554
14.968498	801.162763	12.987571
14.666546	785.661568	12.992589
14.656956	777.799020	12.997607
14.294995	778.461264	13.002624
14.310482	776.647466	13.007642
14.268530	786.922673	13.012659
14.461305	790.180901	13.017677
14.638939	792.308587	13.022695
14.759212	807.866458	13.027712
14.872284	801.710977	13.032730
14.704830	798.650752	13.037747
14.527050	791.454995	13.042765
14.830889	785.639037	13.047783
14.545043	784.724196	13.052800
14.338227	775.980356	13.057818
14.374041	799.115608	13.062835
14.629714	793.897265	13.067853
14.613041	794.003991	13.072871
14.452376	802.366393	13.077888
14.593216	802.006794	13.082906
14.499498	803.198458	13.087923
14.634845	802.284309	13.092941
14.765140	795.233082	13.097959
14.429961	808.577130	13.102976
14.960166	799.002178	13.107994
14.640233	803.649858	13.113011
14.757232	799.472401	13.118029
15.129869	799.237653	13.123047
14.568124	804.342692	13.128064
14.743839	807.957021	13.133082
14.944951	818.263827	13.138099
15.048643	810.140637	13.143117
14.735847	805.856531	13.148135
14.932179	825.078984	13.153152
15.220838	822.058189	13.158170
14.788969	817.436024	13.163187
14.929873	816.521008	13.168205
15.198572	827.776635	13.173223
14.548044	827.524471	13.178240
14.995933	824.661915	13.183258
14.928252	835.322998	13.188275
15.263924	834.011593	13.193293
14.997327	832.850763	13.198311
14.924681	840.192804	13.203328
15.039795	837.647139	13.208346
14.658621	842.115021	13.213363
14.906606	836.459217	13.218381
15.262101	831.616631	13.223399
15.181528	837.716551	13.228416
15.222627	834.898396	13.233434
15.027350	834.913013	13.238451
14.965373	832.884058	13.243469
15.253061	825.820936	13.248487
15.032302	840.046572	13.253504
15.386061	827.990279	13.258522
14.913051	833.633762	13.263539
15.040814	840.622717	13.268557
15.424663	829.505299	13.273575
14.776475	833.333116	13.278592
14.979778	836.905286	13.283610
15.735609	850.060563	13.288627
15.443676	853.839228	13.293645
15.686752	834.283231	13.298663
15.078265	839.698507	13.303680
15.489728	832.546686	13.308698
15.248993	832.016129	13.313715
15.324450	840.401744	13.318733
15.526339	854.924495	13.323751
15.572395	850.098525	13.328768
15.751969	848.132943	13.333786
15.706544	842.276675	13.338803
15.445664	837.372268	13.343821
15.657927	830.292487	13.348839
15.389144	839.056738	13.353856
15.621331	831.450005	13.358874
15.503913	835.804237	13.363891
15.263689	835.746958	13.368909
15.690786	826.390012	13.373927
15.329429	836.740224	13.378944
15.573106	833.076352	13.383962
15.746637	835.078453	13.388979
15.210183	836.825033	13.393997
15.862330	843.438862	13.399015
15.542946	849.976745	13.404032
15.938503	854.124884	13.409050
15.972261	841.840702	13.414067
15.668580	841.332568	13.419085
15.797301	836.790369	13.424103
15.469437	831.012792	13.429120
15.739155	841.514052	13.434138
15.732469	849.641069	13.439155
15.850984	858.673223	13.444173
15.840478	852.215083	13.449191
15.717432	858.422606	13.454208
15.876654	859.338213	13.459226
15.614127	856.873433	13.464243
15.740620	854.436445	13.469261
15.825182	855.511995	13.474279
15.677919	851.388293	13.479296
15.434739	855.960921	13.484314
15.523686	852.753471	13.489331
15.867053	852.936680	13.494349
15.914820	850.029124	13.499367
15.628527	863.255150	13.504384
15.658643	861.887179	13.509402
15.600083	862.426449	13.514419
15.612617	871.434087	13.519437
16.042819	873.819097	13.524455
15.993011	886.131028	13.529472
16.113620	883.496141	13.534490
16.403679	875.968738	13.539507
15.762530	879.388380	13.544525
16.247654	880.275336	13.549543
16.180260	886.729818	13.554560
16.204550	890.175240	13.559578
16.228511	884.661596	13.564595
16.162648	889.121421	13.569613
16.193736	888.160385	13.574631
16.098090	888.077440	13.579648
16.103132	892.194874	13.584666
16.636114	888.400743	13.589683
16.075529	892.246490	13.594701
16.284580	882.402768	13.599719
16.494518	888.309155	13.604736
15.946701	885.424898	13.609754
16.301894	883.968443	13.614771
15.964654	883.904179	13.619789
16.211779	885.099583	13.624807
16.251691	882.732875	13.629824
16.431793	879.072581	13.634842
16.362401	882.895496	13.639859
15.815117	884.716348	13.644877
16.239732	890.797590	13.649895
15.971266	889.097417	13.654912
16.216902	887.714822	13.659930
16.288051	881.853013	13.664947
16.113160	891.741889	13.669965
16.373515	897.678298	13.674983
16.084751	896.397842	13.680000
16.664553	898.548129	13.685018
16.901999	900.511884	13.690035
16.475338	900.638264	13.695053
16.860011	897.280622	13.700071
16.432285	905.520556	13.705088
16.488975	900.367876	13.710106
16.796961	898.230820	13.715123
16.645234	906.238437	13.720141
16.566419	900.914355	13.725159
17.016402	894.943067	13.730176
16.821361	900.467554	13.735194
16.656973	886.996079	13.740211
16.358722	882.892722	13.745229
16.541597	890.781966	13.750247
16.514648	896.267657	13.755264
16.466047	900.396601	13.760282
16.881077	898.937139	13.765299
16.582416	897.576175	13.770317
16.395313	901.114471	13.775335
16.630543	900.459314	13.780352
16.391123	894.516470	13.785370
16.700093	892.549671	13.790387
16.310330	900.512298	13.795405
16.804363	917.776126	13.800423
16.992545	913.129978	13.805440
17.141814	923.268195	13.810458
17.182165	920.450143	13.815475
17.170008	909.599455	13.820493
16.829168	896.218561	13.825511
16.982078	896.724907	13.830528
16.761079	888.131539	13.835546
17.204794	896.406197	13.840563
16.777958	909.916065	13.845581
17.065174	911.922565	13.850599
17.268701	917.189345	13.855616
16.585236	918.902019	13.860634
16.749276	922.578147	13.865651
16.634523	925.874815	13.870669
17.023499	922.888876	13.875687
17.499254	928.842250	13.880704
16.792099	926.860089	13.885722
16.998962	919.257262	13.890739
16.801784	922.642500	13.895757
16.913375	923.085854	13.900775
17.223875	916.565087	13.905792
16.616540	928.641968	13.910810
17.287251	929.765113	13.915827
17.177708	943.585359	13.920845
17.311106	947.641797	13.925863
17.677170	948.809220	13.930880
17.529101	938.815947	13.935898
17.344944	927.698544	13.940915
17.075748	930.233481	13.945933
17.366108	928.304288	13.950951
17.226153	931.573323	13.955968
17.259042	949.234021	13.960986
17.189850	948.597858	13.966003
17.560514	948.899892	13.971021
17.382397	945.790810	13.976039
17.574835	944.599526	13.981056
17.717348	950.727866	13.986074
17.683426	951.140230	13.991091
17.629723	955.427767	13.996109
17.659604	943.418668	14.001127
17.761056	933.153024	14.006144
17.017191	926.162112	14.011162
17.557595	928.899192	14.016179
17.676846	947.575213	14.021197
17.443177	945.086993	14.026215
17.472201	940.134265	14.031232
17.294594	959.724347	14.036250
17.332284	940.215991	14.041267
17.769062	948.905155	14.046285
17.411403	949.285874	14.051303
17.798220	939.720550	14.056320
17.415299	951.304923	14.061338
17.572057	944.969026	14.066355
17.832368	952.281363	14.071373
17.626133	952.196702	14.076391
17.310380	948.474744	14.081408
17.127556	965.250723	14.086426
17.620927	966.960049	14.091443
17.866803	977.711249	14.096461
17.911547	972.090203	14.101479
17.959848	968.756519	14.106496
17.879290	976.535340	14.111514
18.063977	970.119348	14.116531
17.902046	971.605661	14.121549
17.751451	975.851486	14.126567
18.171244	967.439172	14.131584
18.103307	971.129338	14.136602
18.366583	962.040820	14.141619
18.010032	970.673637	14.146637
17.741823	975.720398	14.151655
18.228521	969.623451	14.156672
17.859615	970.056413	14.161690
18.005559	972.315284	14.166707
18.042372	972.940692	14.171725
18.141958	983.077212	14.176743
18.461454	970.107836	14.181760
18.341300	967.535669	14.186778
18.488832	966.405023	14.191795
18.359814	974.084094	14.196813
17.789423	966.116277	14.201831
18.197991	960.492236	14.206848
18.361067	968.021686	14.211866
18.461153	968.611997	14.216883
18.556176	965.864319	14.221901
18.202219	958.623342	14.226919
18.069136	951.565725	14.231936
18.112365	964.573266	14.236954
18.275950	963.178195	14.241971
18.206828	966.676044	14.246989
18.489076	970.930213	14.252007
18.489500	977.872778	14.257024
18.319445	979.581258	14.262042
18.571612	968.989176	14.267059
18.476870	980.131075	14.272077
18.319766	973.247600	14.277095
18.603140	978.669222	14.282112
18.329738	969.096225	14.287130
18.180388	974.698826	14.292147
18.367370	972.668962	14.297165
18.410480	968.392519	14.302183
18.618832	965.721868	14.307200
18.390234	972.535989	14.312218
18.675780	953.314071	14.317235
18.457927	967.274273	14.322253
18.621739	966.494536	14.327271
18.950805	965.799521	14.332288
18.830346	970.463522	14.337306
19.041928	969.881471	14.342323
18.876660	967.142762	14.347341
18.961063	977.941193	14.352359
18.826943	958.639445	14.357376
18.731203	968.998869	14.362394
18.917305	968.300867	14.367411
19.132953	967.923306	14.372429
18.978386	974.981517	14.377447
18.902249	967.504780	14.382464
18.774052	961.787590	14.387482
18.919716	957.340550	14.392499
18.750272	968.939033	14.397517
18.937958	966.997421	14.402535
19.101823	962.052095	14.407552
18.876089	970.402616	14.412570
19.120668	967.937760	14.417587
19.293248	969.709655	14.422605
18.675175	959.653851	14.427623
18.924067	946.424091	14.432640
19.214368	962.356403	14.437658
18.770864	962.819914	14.442675
19.013420	960.768776	14.447693
18.825666	974.579133	14.452711
19.168065	962.606568	14.457728
19.008627	966.585530	14.462746
19.012427	963.356603	14.467763
19.370328	959.700167	14.472781
18.841668	974.901638	14.477799
19.343602	966.119936	14.482816
19.116095	969.894906	14.487834
18.978168	967.394932	14.492851
19.130005	959.365162	14.497869
19.058736	966.729131	14.502887
18.889765	964.344442	14.507904
19.002200	965.879553	14.512922
18.993429	979.671515	14.517939
19.373483	986.630713	14.522957
19.312280	992.667712	14.527975
19.581140	990.577761	14.532992
19.436278	998.742139	14.538010
19.238214	991.928148	14.543027
19.406087	993.713402	14.548045
19.218567	998.293179	14.553063
19.375260	993.374206	14.558080
19.093372	995.857480	14.563098
19.222721	999.251853	14.568115
19.556766	996.296545	14.573133
19.139101	1003.847003	14.578151
19.511791	992.412491	14.583168
19.284809	991.504253	14.588186
19.092460	993.563339	14.593203
19.872890	995.379449	14.598221
19.673711	1005.325817	14.603239
19.498119	997.590002	14.608256
19.417350	1004.933376	14.613274
19.389801	1006.916311	14.618291
19.445610	1011.221525	14.623309
19.292791	1024.827670	14.628327
19.595869	1017.986135	14.633344
19.684179	1016.056835	14.638362
19.581630	1016.098038	14.643379
19.700864	1017.714145	14.648397
19.559425	1019.459198	14.653415
19.972268	1012.985577	14.658432
20.041715	1015.231119	14.663450
19.707704	1013.825156	14.668467
19.972734	1014.695895	14.673485
19.804673	1018.824531	14.678503
20.005660	1018.919459	14.683520
20.080708	1026.203868	14.688538
19.912617	1031.888299	14.693555
20.328471	1024.095099	14.698573
19.687084	1023.904623	14.703591
19.756399	1021.072578	14.708608
20.199413	1037.173681	14.713626
19.997530	1042.270094	14.718643
20.343532	1039.123572	14.723661
20.259692	1042.563768	14.728679
20.076981	1034.106378	14.733696
20.608837	1033.868928	14.738714
20.282710	1022.464306	14.743731
20.223752	1018.667638	14.748749
20.035645	1012.025656	14.753767
20.468667	1005.586765	14.758784
20.706800	1011.100646	14.763802
20.377891	1018.293314	14.768819
20.513507	1013.431266	14.773837
20.496324	1024.602143	14.778855
20.633555	1010.525044	14.783872
20.717802	1013.730785	14.788890
20.387235	1018.042510	14.793907
20.587047	1009.803279	14.798925
20.505404	1011.201357	14.803943
20.456759	1009.003051	14.808960
20.438214	1007.724694	14.813978
20.539184	1006.762239	14.818995
20.390363	1008.309629	14.824013
20.369889	1014.094145	14.829031
20.280476	1021.842807	14.834048
20.305090	1008.187181	14.839066
20.092142	1017.889552	14.844083
20.208869	1012.979952	14.849101
20.186970	1012.210194	14.854119
20.320069	1016.014233	14.859136
20.230725	1030.677144	14.864154
20.305593	1037.895315	14.869171
20.577715	1032.276716	14.874189
20.694712	1047.128417	14.879207
20.805553	1038.177201	14.884224
20.511233	1040.517252	14.889242
20.126618	1040.091140	14.894259
20.553394	1032.040620	14.899277
20.478823	1039.594479	14.904295
20.499646	1047.196603	14.909312
20.799793	1047.503307	14.914330
20.939909	1065.696527	14.919347
21.185669	1062.369951	14.924365
21.439976	1050.070221	14.929383
20.973490	1044.986333	14.934400
20.904800	1025.178872	14.939418
20.752794	1032.454454	14.944435
20.970487	1027.349253	14.949453
20.799168	1036.281459	14.954471
20.938649	1045.272575	14.959488
21.131331	1050.654691	14.964506
20.849044	1053.074920	14.969523
21.287163	1058.456694	14.974541
21.061701	1057.068541	14.979559
21.246248	1052.435545	14.984576
21.448422	1052.937382	14.989594
21.004837	1049.064895	14.994611
21.094789	1045.989795	14.999629
21.237885	1050.956760	15.004647
21.134801	1053.137652	15.009664
20.945813	1048.042115	15.014682
21.198364	1055.923740	15.019699
21.318889	1056.239476	15.024717
21.224228	1056.746504	15.029735
20.998589	1054.004558	15.034752
21.495177	1046.094639	15.039770
20.991563	1053.933051	15.044787
21.472195	1062.334580	15.049805
21.374594	1053.974380	15.054823
21.363386	1056.185148	15.059840
21.464784	1058.214284	15.064858
21.190058	1052.349467	15.069875
21.196543	1049.735480	15.074893
21.065195	1046.682213	15.079911
21.787584	1063.301567	15.084928
21.317120	1055.485407	15.089946
21.589283	1073.509755	15.094963
21.786659	1072.923601	15.099981
21.821119	1072.911915	15.104999
21.349354	1066.844246	15.110016
21.931495	1065.630148	15.115034
21.275783	1066.937732	15.120051
21.800054	1070.125465	15.125069
21.583624	1072.472327	15.130087
21.584407	1085.107874	15.135104
22.183405	1076.894822	15.140122
21.762256	1089.479302	15.145139
21.846225	1074.649906	15.150157
21.805124	1079.803346	15.155175
22.068610	1074.577394	15.160192
21.905845	1080.077976	15.165210
22.025860	1076.073552	15.170227
21.716115	1065.663573	15.175245
21.683239	1060.348070	15.180263
21.589732	1075.002198	15.185280
21.698153	1070.463100	15.190298
21.867704	1075.735218	15.195315
22.022086	1068.604395	15.200333
21.838351	1078.217044	15.205351
21.920562	1076.307622	15.210368
22.202530	1086.049736	15.215386
21.595400	1077.809881	15.220403
21.631088	1080.044908	15.225421
21.932666	1080.483932	15.230439
22.075665	1091.629910	15.235456
22.347603	1095.147266	15.240474
22.093962	1095.193059	15.245491
22.273358	1096.802962	15.250509
22.569909	1084.644952	15.255527
22.003394	1084.928805	15.260544
22.582158	1078.079037	15.265562
22.055559	1086.362849	15.270579
21.848281	1085.363177	15.275597
22.127033	1087.645566	15.280615
21.951983	1102.328192	15.285632
22.216798	1096.369888	15.290650
22.111503	1102.969204	15.295667
22.579311	1101.763438	15.300685
22.324174	1104.375104	15.305703
22.427348	1110.973522	15.310720
22.340391	1096.924949	15.315738
22.636987	1105.620238	15.320755
22.291187	1097.008330	15.325773
22.576330	1103.821408	15.330791
22.320798	1106.152272	15.335808
22.757400	1102.180601	15.340826
22.729687	1105.132394	15.345843
22.811016	1101.140299	15.350861
22.663871	1093.990141	15.355879
22.415951	1100.119363	15.360896
23.046014	1096.029209	15.365914
22.804724	1105.351036	15.370931
22.747016	1095.419345	15.375949
23.006230	1098.743025	15.380967
22.498763	1098.036240	15.385984
22.872214	1097.059758	15.391002
23.133417	1110.936018	15.396019
22.767742	1103.179260	15.401037
22.517174	1101.353205	15.406055
22.860250	1127.360128	15.411072
23.258193	1122.706513	15.416090
22.923360	1123.787418	15.421107
23.082679	1123.453337	15.426125
23.111646	1117.332934	15.431143
22.627701	1121.725368	15.436160
23.219342	1112.206956	15.441178
23.220907	1119.004232	15.446195
23.142090	1120.089457	15.451213
23.142286	1113.597998	15.456231
23.145830	1124.131400	15.461248
23.454650	1118.425011	15.466266
22.698201	1120.527758	15.471283
22.907443	1113.094889	15.476301
23.246666	1121.379610	15.481319
23.009907	1121.637367	15.486336
23.491745	1115.029892	15.491354
23.242265	1119.145982	15.496371
22.990422	1118.585587	15.501389
23.202878	1116.693751	15.506407
23.187046	1110.201633	15.511424
23.200461	1111.250406	15.516442
23.374785	1121.722503	15.521459
23.277167	1117.029283	15.526477
23.701926	1110.033069	15.531495
23.101820	1111.458230	15.536512
23.305007	1113.998537	15.541530
23.465543	1115.504082	15.546547
23.270331	1118.365193	15.551565
23.800239	1125.462058	15.556583
23.461411	1133.035010	15.561600
23.707618	1132.027845	15.566618
23.678971	1133.427148	15.571635
23.263822	1126.097801	15.576653
23.580457	1134.682687	15.581671
23.692567	1142.643020	15.586688
23.861936	1147.855228	15.591706
23.824734	1143.711166	15.596723
23.777254	1145.167051	15.601741
24.208105	1148.214710	15.606759
23.690191	1143.820449	15.611776
23.725657	1135.815029	15.616794
23.970457	1142.751167	15.621811
23.682796	1141.379003	15.626829
23.885266	1144.500089	15.631847
23.759226	1143.222681	15.636864
24.006114	1142.347951	15.641882
23.863819	1140.669135	15.646899
23.502729	1145.537903	15.651917
24.041265	1145.425644	15.656935
23.702143	1149.953325	15.661952
23.814326	1150.715326	15.666970
23.674957	1144.681082	15.671987
23.675541	1146.817443	15.677005
24.087897	1152.020221	15.682023
23.969985	1159.918547	15.687040
24.232793	1163.535166	15.692058
24.098128	1169.034557	15.697075
24.085132	1169.907566	15.702093
24.361781	1172.127178	15.707111
24.245659	1167.468383	15.712128
24.636061	1156.318185	15.717146
24.626987	1162.381838	15.722163
24.149134	1167.833676	15.727181
24.906734	1167.267591	15.732199
24.695576	1176.799356	15.737216
24.510668	1153.920337	15.742234
24.433402	1149.552140	15.747251
24.573367	1143.692154	15.752269
24.772649	1137.804000	15.757287
24.243961	1144.055845	15.762304
24.284372	1136.844911	15.767322
24.709738	1141.676436	15.772339
24.549306	1146.353018	15.777357
24.519179	1151.353293	15.782375
24.544688	1157.279018	15.787392
24.512930	1165.328032	15.792410
24.747890	1167.156506	15.797427
24.846510	1168.974650	15.802445
24.929560	1156.625772	15.807463
24.829158	1166.686237	15.812480
24.802498	1160.053777	15.817498
25.054756	1159.553748	15.822515
25.033142	1163.344038	15.827533
24.856732	1146.122018	15.832551
24.632769	1141.300141	15.837568
24.798907	1158.104020	15.842586
24.829211	1160.851131	15.847603
24.906698	1168.390836	15.852621
25.099250	1159.294295	15.857639
24.977755	1162.175493	15.862656
25.166061	1163.493683	15.867674
25.016085	1165.208522	15.872691
24.874490	1164.264890	15.877709
24.588898	1167.515619	15.882727
24.609014	1163.069141	15.887744
24.909984	1158.108725	15.892762
24.673790	1160.865771	15.897779
24.748086	1164.530677	15.902797
24.765328	1158.781311	15.907815
24.597403	1178.228114	15.912832
24.584906	1187.078864	15.917850
24.869870	1196.605979	15.922867
25.148600	1188.682580	15.927885
24.860793	1188.026798	15.932903
25.344995	1207.047053	15.937920
25.265630	1210.723269	15.942938
25.504411	1203.626588	15.947955
25.539819	1213.476588	15.952973
25.888089	1206.668971	15.957991
25.376921	1199.458684	15.963008
25.432910	1194.858291	15.968026
25.692169	1190.617568	15.973043
25.234327	1199.638647	15.978061
25.550845	1193.075818	15.983079
25.859418	1209.671377	15.988096
25.532064	1207.538532	15.993114
25.976339	1204.048478	15.998131
25.757498	1205.436374	16.003149
25.653984	1191.374526	16.008167
25.887643	1184.266027	16.013184
25.627234	1189.078107	16.018202
25.853792	1187.622721	16.023219
25.579927	1188.359624	16.028237
25.702249	1192.995350	16.033255
25.719708	1199.846987	16.038272
25.694485	1208.289476	16.043290
25.966666	1201.073988	16.048307
25.700802	1210.809948	16.053325
25.886457	1200.549975	16.058343
26.110300	1206.021960	16.063360
25.996941	1205.023437	16.068378
26.109780	1204.904875	16.073395
25.731995	1208.747473	16.078413
26.430994	1203.368469	16.083431
26.487192	1198.566073	16.088448
25.705702	1207.129465	16.093466
26.160464	1205.108376	16.098483
26.115362	1200.094534	16.103501
25.937765	1194.432296	16.108519
26.127859	1202.222725	16.113536
25.936900	1207.257524	16.118554
26.451359	1202.311194	16.123571
26.076819	1199.450398	16.128589
26.107674	1198.530407	16.133607
26.408778	1195.229903	16.138624
25.916436	1214.477950	16.143642
26.154676	1221.288908	16.148659
26.334003	1224.754437	16.153677
26.455985	1225.155156	16.158695
26.605232	1224.027383	16.163712
26.645668	1231.301486	16.168730
26.705358	1223.787715	16.173747
26.440115	1233.990648	16.178765
26.622718	1231.544872	16.183783
26.771013	1229.969125	16.188800
26.731037	1230.092104	16.193818
26.712103	1222.751521	16.198835
26.748551	1239.496773	16.203853
26.986802	1228.335506	16.208871
26.787578	1229.382679	16.213888
26.640113	1227.994992	16.218906
26.678096	1227.566193	16.223923
26.563624	1235.205242	16.228941
26.906033	1222.598187	16.233959
26.783550	1220.613322	16.238976
26.420607	1227.467392	16.243994
26.587072	1221.394973	16.249011
26.714997	1226.367505	16.254029
26.525420	1220.088590	16.259047
26.843017	1227.827620	16.264064
26.506086	1233.304874	16.269082
26.952951	1236.394236	16.274099
26.904979	1244.600445	16.279117
27.186969	1249.612112	16.284135
27.108188	1240.791304	16.289152
27.288477	1243.190029	16.294170
27.353435	1241.810292	16.299187
26.851332	1249.159406	16.304205
27.093346	1235.602301	16.309223
27.589822	1244.190797	16.314240
27.240919	1242.623034	16.319258
27.591036	1235.972907	16.324275
27.522280	1235.526013	16.329293
27.597443	1232.115515	16.334311
27.728188	1229.526336	16.339328
27.343436	1232.549518	16.344346
27.552158	1222.961280	16.349363
27.399007	1222.259284	16.354381
27.509484	1222.592367	16.359399
27.689248	1232.451459	16.364416
27.382698	1241.704623	16.369434
27.649903	1228.844187	16.374451
27.602050	1231.470935	16.379469
27.507485	1236.907298	16.384487
27.616581	1236.155004	16.389504
27.642025	1239.218463	16.394522
27.694810	1227.565366	16.399539
27.805346	1231.199397	16.404557
27.535350	1229.748736	16.409575
27.604203	1231.906035	16.414592
27.780141	1238.944450	16.419610
28.043342	1220.842873	16.424627
27.822436	1230.202616	16.429645
27.817899	1227.192690	16.434663
28.172727	1238.264754	16.439680
27.896203	1230.206883	16.444698
28.200359	1234.271513	16.449715
27.894279	1227.196540	16.454733
28.152133	1223.208492	16.459751
28.158430	1234.006616	16.464768
27.909315	1241.227976	16.469786
28.311299	1226.374186	16.474803
28.335127	1229.251703	16.479821
28.338723	1237.544553	16.484839
28.078090	1226.341041	16.489856
28.052484	1234.266053	16.494874
28.118768	1232.800904	16.499891
28.484047	1228.527886	16.504909
28.215437	1231.782293	16.509927
28.051600	1230.012148	16.514944
28.274613	1228.386899	16.519962
28.430666	1233.310872	16.524979
28.402519	1233.283688	16.529997
28.495132	1233.868859	16.535015
28.178765	1224.927261	16.540032
27.983474	1242.254549	16.545050
28.249239	1246.593402	16.550067
28.269763	1251.377537	16.555085
28.510824	1255.758108	16.560103
28.636073	1263.306196	16.565120
28.278089	1267.928361	16.570138
28.546848	1254.098835	16.575155
28.553233	1262.369172	16.580173
28.519648	1253.983132	16.585191
28.370687	1259.431127	16.590208
28.705956	1251.281148	16.595226
28.793974	1256.783764	16.600243
28.429997	1253.302779	16.605261
28.448048	1263.243871	16.610279
28.941623	1270.804043	16.615296
28.637455	1283.622909	16.620314
28.729984	1273.263784	16.625331
29.006156	1280.513827	16.630349
28.976943	1280.480497	16.635367
29.413644	1273.561256	16.640384
29.296568	1282.986912	16.645402
29.002112	1276.594918	16.650419
29.352586	1271.588894	16.655437
29.191005	1277.486983	16.660455
29.311749	1269.042194	16.665472
29.389086	1271.971347	16.670490
29.320079	1266.680342	16.675507
29.472109	1273.028218	16.680525
29.370669	1274.047547	16.685543
29.420284	1249.500342	16.690560
28.995961	1254.082340	16.695578
29.033559	1258.270529	16.700595
29.554044	1267.363382	16.705613
29.277912	1275.614596	16.710631
29.510380	1277.307770	16.715648
29.468919	1282.963097	16.720666
29.807640	1276.248458	16.725683
29.521605	1270.751402	16.730701
29.360754	1279.035162	16.735719
29.723074	1273.418223	16.740736
29.506412	1275.354894	16.745754
29.503089	1281.884751	16.750771
29.456592	1272.607621	16.755789
29.442737	1280.325697	16.760807
29.713932	1276.373429	16.765824
29.450642	1277.105533	16.770842
29.430981	1269.935456	16.775859
29.615565	1284.265592	16.780877
29.347855	1299.606590	16.785895
29.770726	1296.627935	16.790912
29.925876	1305.070789	16.795930
29.541242	1298.446675	16.800947
29.825943	1296.335289	16.805965
29.533759	1301.852934	16.810983
29.970836	1307.862951	16.816000
29.710620	1302.232477	16.821018
30.129996	1310.520586	16.826035
30.387304	1321.948713	16.831053
30.047772	1317.870617	16.836071
30.035134	1308.622911	16.841088
30.588795	1323.176481	16.846106
30.597079	1310.125925	16.851123
30.260926	1296.936503	16.856141
30.015037	1297.700612	16.861159
30.374177	1287.760716	16.866176
30.486794	1305.188447	16.871194
30.197094	1301.676953	16.876211
30.219243	1303.639561	16.881229
30.269022	1321.506281	16.886247
30.212835	1316.008139	16.891264
30.386383	1325.483242	16.896282
30.462647	1316.881254	16.901299
30.631899	1321.695899	16.906317
30.185934	1324.037507	16.911335
30.360035	1326.206832	16.916352
30.617175	1328.568357	16.921370
30.598681	1325.049346	16.926387
30.810350	1320.686614	16.931405
30.628839	1321.775217	16.936423
30.571189	1312.149508	16.941440
30.429630	1314.973894	16.946458
30.587049	1320.588801	16.951475
31.261063	1333.157574	16.956493
31.195026	1334.537467	16.961511
30.891959	1322.494745	16.966528
31.012014	1315.429128	16.971546
30.839534	1320.681989	16.976563
31.175023	1319.578861	16.981581
30.796629	1317.782153	16.986599
31.142654	1323.389786	16.991616
31.152266	1320.077839	16.996634
31.519072	1330.501156	17.001651
31.197763	1334.852540	17.006669
31.107310	1328.002731	17.011687
31.382423	1309.593096	17.016704
31.045522	1315.423821	17.021722
30.837938	1319.290436	17.026739
31.274774	1337.756473	17.031757
31.096917	1344.572303	17.036775
31.221808	1340.658579	17.041792
31.415564	1343.699006	17.046810
31.561469	1344.989097	17.051827
31.569884	1340.437099	17.056845
30.857153	1348.645870	17.061863
31.631680	1345.268473	17.066880
31.692302	1340.809332	17.071898
31.495429	1348.470726	17.076915
31.459348	1340.160774	17.081933
31.209863	1350.036271	17.086951
31.506312	1343.025231	17.091968
31.549177	1341.595277	17.096986
31.506732	1358.195134	17.102003
32.128531	1364.924338	17.107021
31.957891	1365.638865	17.112039
31.854035	1356.313817	17.117056
31.846756	1358.789099	17.122074
31.727155	1364.283048	17.127091
32.096785	1364.146594	17.132109
31.915063	1369.927928	17.137127
32.547474	1365.480742	17.142144
31.707166	1349.939799	17.147162
32.273482	1364.412537	17.152179
32.332241	1356.412860	17.157197
32.027355	1355.270579	17.162215
32.134682	1342.034165	17.167232
32.339516	1344.504822	17.172250
32.063371	1364.101222	17.177267
32.384477	1360.781794	17.182285
32.578519	1358.337376	17.187303
32.087800	1345.241411	17.192320
32.072265	1344.565322	17.197338
31.981375	1353.974315	17.202355
32.169657	1359.417170	17.207373
31.837249	1368.011705	17.212391
32.326916	1363.100749	17.217408
32.227934	1356.422670	17.222426
32.322774	1367.945550	17.227443
32.413138	1358.501900	17.232461
32.470890	1380.940212	17.237479
32.446132	1381.398495	17.242496
32.419171	1391.820040	17.247514
32.780986	1395.134113	17.252531
32.775204	1393.759066	17.257549
32.637162	1390.826703	17.262567
32.720471	1395.064612	17.267584
32.849702	1386.533238	17.272602
32.862246	1385.051198	17.277619
33.421234	1387.258436	17.282637
32.998997	1396.842118	17.287655
32.868613	1388.852940	17.292672
32.803957	1387.468126	17.297690
32.722331	1393.095027	17.302707
32.908468	1375.898389	17.307725
32.518416	1388.434055	17.312743
32.441040	1385.347080	17.317760
32.523373	1394.315712	17.322778
32.327757	1393.263714	17.327795
32.542775	1409.135563	17.332813
32.270036	1415.720039	17.337831
32.374273	1416.571652	17.342848
33.125898	1428.235311	17.347866
33.186073	1432.792412	17.352883
33.156674	1428.000125	17.357901
33.205829	1443.910454	17.362919
33.197735	1436.688015	17.367936
33.603101	1433.901414	17.372954
33.586752	1419.677490	17.377971
33.741362	1416.169379	17.382989
33.460479	1421.729483	17.388007
33.749801	1418.506513	17.393024
33.628704	1424.855942	17.398042
33.778922	1427.139452	17.403059
33.677491	1418.732340	17.408077
33.829146	1417.929230	17.413095
34.150965	1423.019953	17.418112
33.956077	1416.233707	17.423130
34.054616	1417.581672	17.428147
34.043799	1413.240934	17.433165
34.441764	1413.718609	17.438183
34.397885	1417.155812	17.443200
34.438112	1419.292343	17.448218
34.320254	1411.253868	17.453235
34.301604	1405.481608	17.458253
34.178214	1401.025856	17.463271
33.806508	1400.159065	17.468288
34.044675	1388.757868	17.473306
33.663354	1393.014468	17.478323
34.234244	1413.738214	17.483341
34.615614	1420.265031	17.488359
34.256374	1416.691757	17.493376
34.633229	1407.670536	17.498394
34.135462	1401.821395	17.503411
34.068355	1399.780551	17.508429
34.259137	1412.623434	17.513447
34.128956	1419.826348	17.518464
34.822122	1419.336561	17.523482
34.130928	1412.444552	17.528499
34.400838	1414.280233	17.533517
34.329329	1419.548960	17.538535
34.528696	1406.459115	17.543552
34.377993	1413.030901	17.548570
34.333045	1421.170448	17.553587
34.438438	1416.720097	17.558605
34.364896	1421.992297	17.563623
34.665500	1435.960506	17.568640
35.125770	1432.796125	17.573658
34.683693	1444.863401	17.578675
34.731470	1435.107602	17.583693
34.506824	1436.758353	17.588711
34.967561	1438.214029	17.593728
34.642547	1439.706837	17.598746
34.832855	1443.666164	17.603763
34.873722	1441.532764	17.608781
34.942003	1446.549358	17.613799
34.961994	1437.012480	17.618816
34.903015	1438.590100	17.623834
34.863606	1447.833336	17.628851
34.652652	1441.762800	17.633869
35.086184	1459.588844	17.638887
35.026861	1459.503397	17.643904
35.190359	1450.830956	17.648922
34.778776	1470.300236	17.653939
34.944588	1460.633343	17.658957
35.389601	1457.209399	17.663975
35.201821	1462.704526	17.668992
35.610099	1450.468911	17.674010
35.348863	1454.984542	17.679027
35.650872	1457.597877	17.684045
35.790471	1453.126412	17.689063
35.396600	1457.044152	17.694080
35.756857	1449.593942	17.699098
35.335736	1459.284782	17.704115
35.809986	1475.608640	17.709133
36.085437	1477.266738	17.714151
36.206222	1467.894033	17.719168
36.049262	1455.989419	17.724186
36.030823	1454.281821	17.729203
35.523209	1442.258241	17.734221
35.969110	1448.601451	17.739239
35.844931	1444.868495	17.744256
35.952359	1437.631226	17.749274
36.052138	1464.711635	17.754291
36.213797	1472.329883	17.759309
36.385906	1472.937399	17.764327
36.342670	1462.905418	17.769344
36.376932	1454.533967	17.774362
36.080174	1451.869304	17.779379
36.013179	1451.955466	17.784397
36.431684	1445.771145	17.789415
36.112188	1461.653679	17.794432
36.684898	1464.433152	17.799450
36.192346	1466.523253	17.804467
36.357479	1468.687681	17.809485
36.752600	1473.154773	17.814503
36.691112	1466.284622	17.819520
36.734750	1458.183111	17.824538
36.623129	1449.635558	17.829555
36.248993	1438.017235	17.834573
36.928468	1450.818773	17.839591
36.536704	1461.846271	17.844608
36.574905	1458.633990	17.849626
36.521080	1467.002159	17.854643
36.650780	1470.147256	17.859661
36.892356	1470.526205	17.864679
36.650936	1476.013908	17.869696
36.749751	1471.469893	17.874714
36.593613	1467.965973	17.879731
36.630981	1474.325461	17.884749
36.479523	1465.307572	17.889767
36.652710	1475.088927	17.894784
36.835011	1492.928875	17.899802
36.540105	1499.169690	17.904819
36.552262	1501.881809	17.909837
37.128371	1495.941179	17.914855
37.267056	1501.849397	17.919872
37.602315	1491.824742	17.924890
37.253475	1489.881401	17.929907
37.063530	1499.062894	17.934925
37.099981	1494.007869	17.939943
37.216633	1494.611398	17.944960
37.319953	1488.324655	17.949978
37.440489	1497.189560	17.954995
37.293020	1506.692650	17.960013
37.801128	1508.314528	17.965031
37.713905	1514.873312	17.970048
37.744475	1511.747417	17.975066
37.558359	1510.065920	17.980083
37.614188	1504.083215	17.985101
37.825987	1517.642433	17.990119
38.063379	1517.630709	17.995136
37.740024	1507.244681	18.000154
37.516454	1505.881444	18.005171
37.658040	1506.414818	18.010189
37.513390	1514.768749	18.015207
37.541265	1520.025187	18.020224
37.750350	1511.869489	18.025242
38.005929	1513.527530	18.030259
37.599659	1514.237723	18.035277
37.968860	1517.758954	18.040295
37.693347	1522.182150	18.045312
38.405621	1524.965150	18.050330
38.371039	1539.512654	18.055347
38.557375	1539.884425	18.060365
38.731942	1526.176653	18.065383
38.342854	1514.746803	18.070400
38.144475	1515.361511	18.075418
38.313500	1510.816022	18.080435
38.710466	1512.240608	18.085453
38.947745	1502.411085	18.090471
38.898154	1511.072109	18.095488
39.064778	1509.619717	18.100506
38.837405	1506.669685	18.105523
38.394094	1507.723320	18.110541
38.755469	1502.750249	18.115559
38.792172	1505.954013	18.120576
38.896910	1512.006377	18.125594
39.023498	1510.692764	18.130611
38.885941	1516.186400	18.135629
38.881129	1501.329446	18.140647
38.626173	1507.595603	18.145664
39.155352	1505.764868	18.150682
38.822674	1508.679002	18.155699
38.624867	1508.362648	18.160717
39.091762	1496.881589	18.165735
39.031365	1512.834282	18.170752
39.211131	1509.035055	18.175770
39.102129	1501.872483	18.180787
39.070500	1505.812730	18.185805
39.084629	1503.298473	18.190823
39.415951	1506.926587	18.195840
38.984179	1510.973317	18.200858
39.124497	1518.746388	18.205875
39.212618	1532.602588	18.210893
39.516556	1533.293724	18.215911
39.099881	1541.128280	18.220928
38.777377	1541.645548	18.225946
39.214052	1546.364969	18.230963
39.302174	1545.685356	18.235981
39.392260	1543.001475	18.240999
39.551718	1559.087240	18.246016
39.501276	1556.198015	18.251034
39.647249	1558.005671	18.256051
39.572292	1554.135639	18.261069
39.627496	1556.885246	18.266087
39.684728	1556.860547	18.271104
39.841573	1557.868080	18.276122
40.023961	1556.091334	18.281139
39.698342	1554.500982	18.286157
39.857810	1543.638966	18.291175
39.662707	1552.231146	18.296192
39.566483	1549.219661	18.301210
39.879748	1568.232203	18.306227
39.868854	1567.034667	18.311245
39.931801	1575.883331	18.316263
40.373177	1571.421656	18.321280
40.215063	1570.793004	18.326298
40.270289	1574.139066	18.331315
40.065993	1572.264731	18.336333
40.332854	1568.890594	18.341351
40.095818	1576.712975	18.346368
39.932187	1576.220883	18.351386
40.388005	1586.472699	18.356403
40.356641	1597.576713	18.361421
40.751242	1586.428750	18.366439
40.582814	1599.375033	18.371456
41.122888	1593.291656	18.376474
40.922721	1593.202889	18.381491
40.817649	1584.802577	18.386509
40.778769	1571.399406	18.391527
40.651960	1585.743554	18.396544
41.121315	1595.213771	18.401562
41.230922	1593.669263	18.406579
40.798426	1586.547556	18.411597
41.171518	1580.376571	18.416615
41.497839	1580.761262	18.421632
40.771801	1577.680572	18.426650
41.120806	1576.297611	18.431667
40.995557	1595.428950	18.436685
41.110618	1586.823947	18.441703
40.804391	1597.951822	18.446720
41.290783	1590.021161	18.451738
41.247824	1592.896512	18.456755
41.452415	1593.309624	18.461773
41.335629	1586.110360	18.466791
40.959326	1582.227279	18.471808
41.289218	1590.857660	18.476826
41.292199	1590.121873	18.481843
40.959026	1595.513444	18.486861
41.437259	1608.816651	18.491879
41.438293	1612.830732	18.496896
41.243430	1614.527355	18.501914
41.716546	1614.343229	18.506931
41.745475	1611.722509	18.511949
41.908578	1619.239608	18.516967
42.275191	1611.283404	18.521984
41.741120	1617.091275	18.527002
41.765381	1608.418346	18.532019
41.741376	1612.925484	18.537037
42.224742	1612.332656	18.542055
42.298042	1605.179529	18.547072
42.315875	1610.860442	18.552090
42.082122	1606.342925	18.557107
41.875556	1614.987414	18.562125
42.049616	1615.979647	18.567143
41.828578	1623.007437	18.572160
42.019024	1622.002615	18.577178
42.059007	1628.052477	18.582195
42.002297	1641.331697	18.587213
42.081199	1636.225841	18.592231
42.179982	1637.523290	18.597248
41.944810	1645.032981	18.602266
42.692133	1644.004572	18.607283
42.374966	1653.284848	18.612301
42.595708	1654.099398	18.617319
43.033676	1658.174851	18.622336
42.597136	1650.154326	18.627354
42.715472	1646.755962	18.632371
42.909711	1664.884562	18.637389
43.094273	1657.483713	18.642407
42.856075	1647.961674	18.647424
42.638968	1642.636811	18.652442
43.238707	1644.187630	18.657459
43.017864	1659.158715	18.662477
43.223141	1649.652836	18.667495
43.690189	1649.431784	18.672512
43.175682	1647.520531	18.677530
43.246739	1631.815353	18.682547
43.183229	1631.765270	18.687565
43.102795	1634.999920	18.692583
43.007013	1627.895200	18.697600
42.849362	1648.565390	18.702618
43.249766	1651.254954	18.707635
43.427493	1663.080706	18.712653
43.308728	1657.699500	18.717671
43.345571	1658.489033	18.722688
43.397003	1655.318839	18.727706
43.621483	1653.361957	18.732723
43.549205	1658.877031	18.737741
43.272857	1655.338141	18.742759
43.530769	1661.319368	18.747776
43.744229	1680.975588	18.752794
44.023302	1684.390962	18.757811
43.802356	1693.151338	18.762829
43.904883	1679.483068	18.767847
43.879165	1685.704128	18.772864
43.946561	1680.956664	18.777882
44.202653	1683.315244	18.782899
44.342095	1672.330033	18.787917
44.163319	1664.717502	18.792935
44.079442	1673.554359	18.797952
44.489063	1681.752641	18.802970
44.276420	1674.975372	18.807987
44.415062	1673.072879	18.813005
44.408315	1670.634434	18.818023
44.145349	1674.951570	18.823040
44.270257	1671.233435	18.828058
44.579152	1672.072131	18.833075
44.176821	1682.830006	18.838093
44.509595	1678.442020	18.843111
44.282066	1675.362593	18.848128
44.480235	1686.061688	18.853146
44.454133	1668.045728	18.858163
44.319187	1675.789140	18.863181
44.453020	1698.250721	18.868199
44.651920	1697.443399	18.873216
44.517194	1698.976029	18.878234
44.644767	1703.393316	18.883251
44.692522	1699.456809	18.888269
44.822894	1698.704339	18.893287
44.796439	1698.493849	18.898304
44.950739	1700.966112	18.903322
44.869823	1717.133627	18.908339
45.268496	1718.163479	18.913357
45.469781	1716.434269	18.918375
45.500704	1716.880736	18.923392
45.394632	1726.506888	18.928410
45.780362	1706.833050	18.933427
45.683860	1706.507231	18.938445
45.480788	1688.922756	18.943463
45.397783	1688.105676	18.948480
45.461967	1692.135190	18.953498
45.554827	1687.967595	18.958515
45.592811	1692.247346	18.963533
45.727025	1696.635195	18.968551
45.574545	1694.134228	18.973568
45.495402	1702.907246	18.978586
45.875645	1712.161021	18.983603
46.035182	1722.115055	18.988621
45.604215	1728.156222	18.993639
45.780884	1720.516729	18.998656
45.651776	1715.301222	19.003674
46.069978	1720.238166	19.008691
46.081280	1719.318037	19.013709
45.666703	1719.294211	19.018727
45.299873	1715.254988	19.023744
45.041407	1733.652962	19.028762
45.967246	1738.318365	19.033779
45.919423	1748.995836	19.038797
46.155327	1747.280169	19.043815
46.444714	1742.684322	19.048832
46.393511	1743.878896	19.053850
46.517494	1742.227993	19.058867
46.779923	1746.665321	19.063885
46.722470	1741.766861	19.068903
46.789277	1738.625817	19.073920
46.504704	1746.824912	19.078938
46.532207	1740.218517	19.083955
46.799262	1745.450406	19.088973
46.816019	1766.106201	19.093991
46.977976	1765.238354	19.099008
46.786651	1757.498346	19.104026
47.149926	1761.367697	19.109043
46.967036	1773.303318	19.114061
47.195455	1767.965857	19.119079
47.261397	1766.768968	19.124096
46.917589	1767.974387	19.129114
47.039487	1766.648862	19.134131
47.284820	1766.594876	19.139149
47.401876	1774.737763	19.144167
47.406851	1764.243659	19.149184
47.074209	1771.544510	19.154202
47.125602	1763.324886	19.159219
47.233066	1760.089143	19.164237
46.954547	1763.872221	19.169255
47.095492	1756.083636	19.174272
47.085953	1773.120580	19.179290
47.546485	1778.256081	19.184307
47.604129	1780.831769	19.189325
47.376347	1783.808512	19.194343
47.566213	1777.135798	19.199360
47.769039	1786.436171	19.204378
47.839711	1780.053420	19.209395
48.064501	1782.830308	19.214413
47.958041	1788.312874	19.219431
47.748204	1777.198938	19.224448
47.888386	1784.615531	19.229466
47.981015	1805.707695	19.234483
48.437489	1805.497756	19.239501
48.220219	1815.232790	19.244519
48.096436	1806.415552	19.249536
48.204344	1802.933573	19.254554
48.074157	1812.270028	19.259571
47.983346	1801.415265	19.264589
47.869200	1804.528957	19.269607
48.299387	1800.681212	19.274624
47.959812	1795.769857	19.279642
48.192710	1805.838751	19.284659
48.690066	1810.428871	19.289677
48.490483	1824.115490	19.294695
48.892589	1820.433063	19.299712
48.967794	1825.505492	19.304730
48.960654	1821.716365	19.309747
49.233137	1819.518455	19.314765
48.831360	1822.307694	19.319783
49.134662	1819.600043	19.324800
49.434562	1819.420793	19.329818
49.084396	1817.092603	19.334835
49.124844	1798.062576	19.339853
49.140534	1797.129136	19.344871
48.985840	1790.715196	19.349888
49.092137	1816.318167	19.354906
49.206511	1806.532861	19.359923
49.240383	1811.769516	19.364941
49.114907	1812.107788	19.369959
49.479226	1812.827406	19.374976
49.203166	1807.199239	19.379994
49.278662	1806.559453	19.385011
49.558541	1816.286513	19.390029
49.605263	1815.487100	19.395047
49.734088	1803.730268	19.400064
49.603623	1816.825437	19.405082
49.430453	1810.171363	19.410099
49.759755	1825.571342	19.415117
49.988702	1839.913953	19.420135
50.110972	1851.098350	19.425152
50.032854	1839.862878	19.430170
49.865254	1837.458922	19.435187
50.350692	1842.167674	19.440205
50.054290	1839.603886	19.445223
49.984823	1838.850965	19.450240
50.014802	1839.692069	19.455258
49.953065	1842.715555	19.460275
50.266066	1839.422550	19.465293
50.074397	1837.707171	19.470311
50.065576	1840.911772	19.475328
50.112651	1846.458816	19.480346
50.364638	1863.455126	19.485363
50.359591	1867.448120	19.490381
50.443659	1871.679712	19.495399
50.528337	1863.792541	19.500416
50.844363	1870.266579	19.505434
50.689737	1867.560789	19.510451
50.697200	1865.770221	19.515469
50.460795	1869.742430	19.520487
50.506018	1862.962812	19.525504
50.475531	1875.944625	19.530522
50.668624	1883.128951	19.535539
51.092849	1886.941501	19.540557
51.046322	1896.949807	19.545575
51.042165	1888.902881	19.550592
51.165831	1880.198564	19.555610
51.137783	1886.164428	19.560627
51.218788	1882.415214	19.565645
51.133293	1889.567176	19.570663
51.455112	1902.412102	19.575680
51.403301	1911.872110	19.580698
51.548258	1907.822590	19.585715
51.750313	1910.123340	19.590733
51.534116	1912.148371	19.595751
51.520265	1903.825228	19.600768
51.353169	1912.167058	19.605786
51.373886	1914.432924	19.610803
51.725535	1900.318585	19.615821
51.390261	1909.021125	19.620839
51.688672	1922.302069	19.625856
52.039916	1927.808092	19.630874
51.810555	1935.001407	19.635891
52.079802	1929.878455	19.640909
51.869569	1921.257664	19.645927
52.300958	1931.052719	19.650944
52.373598	1926.509508	19.655962
52.156356	1923.141248	19.660979
52.217577	1922.841363	19.665997
51.892504	1925.460880	19.671015
52.065144	1920.974687	19.676032
52.233456	1921.298778	19.681050
51.974850	1937.393168	19.686067
52.761949	1936.188132	19.691085
52.935063	1942.940077	19.696103
52.447784	1938.887997	19.701120
52.838879	1940.146269	19.706138
52.956429	1950.728683	19.711155
53.357291	1947.201064	19.716173
53.315202	1943.843400	19.721191
53.063659	1926.786963	19.726208
53.315946	1925.665196	19.731226
52.919791	1919.544433	19.736243
53.085678	1922.368385	19.741261
53.211354	1936.149621	19.746279
53.298064	1933.605068	19.751296
53.404317	1936.858043	19.756314
53.203469	1941.096141	19.761331
53.295794	1933.520184	19.766349
53.231990	1941.104306	19.771367
53.269757	1942.827859	19.776384
53.562988	1936.763864	19.781402
53.231058	1941.764011	19.786419
53.627549	1938.429585	19.791437
53.763605	1937.010322	19.796455
53.378204	1936.524345	19.801472
53.847809	1945.559194	19.806490
53.479175	1945.095853	19.811507
53.803830	1957.833076	19.816525
54.168015	1964.612088	19.821543
54.018562	1960.318049	19.826560
53.782123	1959.859373	19.831578
54.456713	1960.117264	19.836595
54.198774	1958.626794	19.841613
54.364902	1960.115761	19.846631
54.545995	1966.942215	19.851648
54.403914	1951.752796	19.856666
54.193904	1955.503156	19.861683
54.675608	1955.734272	19.866701
54.508671	1965.887601	19.871719
54.397369	1959.245930	19.876736
54.795387	1951.155294	19.881754
54.308340	1956.675075	19.886771
54.847003	1955.414041	19.891789
54.809177	1956.354073	19.896807
54.641647	1955.297668	19.901824
54.637745	1955.077352	19.906842
54.425851	1961.100268	19.911859
54.675127	1969.210035	19.916877
55.255353	1973.528509	19.921895
54.983536	1984.190501	19.926912
55.215260	1980.168482	19.931930
54.900455	1985.323771	19.936947
55.171684	1980.522400	19.941965
55.323943	1976.834659	19.946983
55.368282	1976.957139	19.952000
55.459537	1975.582720	19.957018
55.273455	1975.933587	19.962035
55.175944	1971.205409	19.967053
55.371576	1990.208313	19.972071
55.582029	1995.385970	19.977088
55.895676	1997.656733	19.982106
55.736440	2001.171971	19.987123
55.501765	2005.945547	19.992141
56.011283	2008.690763	19.997159
55.630130	2004.189783	20.002176
55.971486	2006.617185	20.007194
55.561035	2008.558858	20.012211
55.576039	2006.432574	20.017229
55.757533	2006.262290	20.022247
55.837833	2018.463223	20.027264
56.098439	2022.938775	20.032282
56.274514	2025.912642	20.037299
56.220361	2028.512084	20.042317
55.781748	2026.074555	20.047335
55.965194	2020.074964	20.052352
56.444985	2020.934409	20.057370
56.964541	2025.625274	20.062387
56.831355	2020.426092	20.067405
56.848151	2018.138575	20.072423
56.677898	2024.448531	20.077440
56.808489	2019.640643	20.082458
56.506998	2027.018801	20.087475
56.960294	2034.702341	20.092493
56.965128	2041.802429	20.097511
57.266171	2049.837898	20.102528
57.291178	2045.447246	20.107546
57.202687	2043.624260	20.112563
57.095075	2041.141506	20.117581
57.303546	2048.149929	20.122599
57.056843	2054.317157	20.127616
57.377645	2042.284115	20.132634
57.140866	2047.629253	20.137651
57.255081	2042.871248	20.142669
57.406265	2045.397695	20.147687
57.142045	2051.119507	20.152704
57.472247	2054.271362	20.157722
57.352331	2069.343845	20.162739
57.721712	2071.514418	20.167757
57.516982	2071.110764	20.172775
57.692002	2068.287344	20.177792
58.016281	2063.196813	20.182810
57.925044	2072.634641	20.187827
57.739493	2070.422805	20.192845
58.024057	2065.250090	20.197863
58.123358	2070.871127	20.202880
58.377949	2079.260994	20.207898
58.353418	2081.395064	20.212915
58.404096	2090.002886	20.217933
58.594988	2088.139553	20.222951
58.562940	2089.277517	20.227968
58.646184	2093.455639	20.232986
58.243735	2090.283448	20.238003
58.650194	2091.400478	20.243021
58.880034	2083.247601	20.248039
58.567984	2091.646799	20.253056
58.943976	2085.087009	20.258074
58.800295	2093.396875	20.263091
58.972579	2090.703270	20.268109
58.800086	2088.236923	20.273127
58.671718	2094.347870	20.278144
59.083361	2087.665758	20.283162
58.832518	2082.017798	20.288179
58.991463	2086.979429	20.293197
59.155903	2088.219350	20.298215
59.096811	2113.094226	20.303232
59.390959	2109.703117	20.308250
59.331746	2115.796992	20.313267
59.193430	2110.810031	20.318285
59.596368	2109.140910	20.323303
59.312655	2117.078095	20.328320
59.395132	2113.385411	20.333338
59.673259	2104.846293	20.338355
59.920328	2114.177820	20.343373
60.079796	2104.842942	20.348391
59.735181	2107.831617	20.353408
59.679678	2109.282516	20.358426
59.672496	2111.773667	20.363443
60.084471	2128.158315	20.368461
60.046084	2130.859463	20.373479
60.058569	2133.988212	20.378496
60.293164	2132.357923	20.383514
60.174036	2133.667245	20.388531
60.034373	2135.860275	20.393549
60.031378	2129.763437	20.398567
59.872231	2138.224061	20.403584
60.192734	2149.027469	20.408602
60.059609	2150.114899	20.413619
60.659180	2151.899332	20.418637
60.893266	2152.787571	20.423655
60.691242	2158.506045	20.428672
60.731480	2147.381347	20.433690
60.485373	2152.349254	20.438707
60.886082	2158.993259	20.443725
61.099921	2167.884998	20.448743
61.158659	2171.915468	20.453760
61.122215	2175.004503	20.458778
61.176843	2184.476487	20.463795
61.115527	2176.820202	20.468813
61.516999	2178.092656	20.473831
61.168643	2171.885465	20.478848
61.357490	2176.255457	20.483866
61.308283	2183.496566	20.488883
61.031987	2172.746198	20.493901
61.011264	2176.243061	20.498919
61.073158	2195.762491	20.503936
61.787910	2195.689070	20.508954
61.954676	2197.411499	20.513971
61.770666	2208.568062	20.518989
61.908011	2205.008835	20.524007
61.654730	2206.152847	20.529024
61.907479	2203.702331	20.534042
62.296049	2201.713530	20.539059
62.638019	2208.492937	20.544077
63.041164	2194.670166	20.549095
62.796029	2185.505544	20.554112
62.805467	2177.200738	20.559130
62.564037	2184.137244	20.564147
62.643536	2183.837665	20.569165
62.670416	2178.910175	20.574183
62.345591	2181.425544	20.579200
62.785565	2173.457670	20.584218
62.977742	2179.935325	20.589235
62.940680	2173.786969	20.594253
62.834115	2170.912695	20.599271
62.485885	2174.921317	20.604288
62.762097	2176.633016	20.609306
63.043102	2184.150932	20.614323
63.219821	2186.701827	20.619341
63.414503	2196.079425	20.624359
63.197112	2194.267025	20.629376
63.464600	2196.756450	20.634394
63.092931	2195.059594	20.639411
63.037078	2206.827395	20.644429
63.004442	2204.651697	20.649447
63.561631	2204.864753	20.654464
63.490234	2201.549476	20.659482
63.649669	2201.906515	20.664499
63.663049	2200.894515	20.669517
63.583706	2199.363593	20.674535
63.592576	2218.913397	20.679552
63.752864	2221.839259	20.684570
64.350188	2212.751750	20.689587
64.378059	2217.598119	20.694605
64.327183	2213.212928	20.699623
64.245785	2221.778257	20.704640
63.895283	2223.271940	20.709658
64.214786	2216.638842	20.714675
64.062201	2213.891653	20.719693
64.376548	2213.722775	20.724711
64.441506	2226.049321	20.729728
64.065074	2221.904174	20.734746
64.332355	2225.876939	20.739763
63.657786	2242.162604	20.744781
64.144252	2244.886199	20.749799
64.384868	2248.112000	20.754816
64.890735	2255.001614	20.759834
64.955182	2258.731398	20.764851
65.253704	2275.039165	20.769869
65.334241	2269.674084	20.774887
65.159367	2270.247285	20.779904
65.343244	2270.673108	20.784922
65.531666	2276.116223	20.789939
65.337200	2273.549123	20.794957
65.164484	2270.448435	20.799975
65.461411	2269.641606	20.804992
65.610459	2261.491759	20.810010
65.706533	2261.176975	20.815027
65.303295	2268.530046	20.820045
65.757270	2269.980535	20.825063
65.357460	2277.102690	20.830080
65.549975	2273.077243	20.835098
65.594017	2280.423799	20.840115
65.693386	2293.398320	20.845133
65.877354	2292.359755	20.850151
65.883178	2295.985058	20.855168
66.121598	2293.988066	20.860186
66.125901	2288.044681	20.865203
65.833249	2299.732640	20.870221
66.153453	2310.514101	20.875239
66.444384	2314.432708	20.880256
66.377533	2308.437275	20.885274
66.775338	2316.852296	20.890291
66.715429	2320.913897	20.895309
66.934898	2316.849528	20.900327
66.694863	2319.061363	20.905344
66.664406	2325.993479	20.910362
66.750524	2306.261485	20.915379
66.463976	2308.944490	20.920397
67.288374	2313.635310	20.925415
67.119164	2328.314875	20.930432
67.011363	2334.747768	20.935450
67.361396	2338.458351	20.940467
67.090705	2341.918421	20.945485
67.510733	2338.807488	20.950503
67.833482	2333.603504	20.955520
67.435971	2334.410198	20.960538
67.447554	2330.150962	20.965555
67.750166	2342.989728	20.970573
67.684350	2327.870171	20.975591
67.975833	2328.339205	20.980608
67.708307	2333.802830	20.985626
67.629501	2327.774536	20.990643
67.507906	2336.788016	20.995661
67.358820	2337.723299	21.000679
67.517493	2357.780135	21.005696
67.662346	2361.869828	21.010714
67.927399	2357.271302	21.015731
67.692938	2365.649080	21.020749
67.556040	2376.836284	21.025767
68.088111	2383.491481	21.030784
68.241896	2380.620822	21.035802
68.743897	2377.307761	21.040819
68.628556	2382.574127	21.045837
68.690917	2390.479643	21.050855
68.919312	2388.446329	21.055872
68.683956	2397.755279	21.060890
68.567580	2396.327943	21.065907
69.011909	2398.916103	21.070925
69.367301	2404.743540	21.075943
68.975633	2407.322998	21.080960
69.172432	2412.477655	21.085978
69.451463	2411.563146	21.090995
69.506537	2409.888195	21.096013
69.868025	2405.874282	21.101031
69.660421	2402.002627	21.106048
69.534403	2395.489325	21.111066
69.919508	2400.674623	21.116083
69.505805	2401.363913	21.121101
69.659481	2405.553234	21.126119
69.799949	2396.186447	21.131136
69.618863	2403.833209	21.136154
70.075767	2395.812106	21.141171
69.590065	2402.625772	21.146189
69.633689	2411.238002	21.151207
69.804377	2418.811064	21.156224
69.780389	2424.987928	21.161242
70.121418	2430.685058	21.166259
70.173289	2430.500237	21.171277
69.912768	2436.483543	21.176295
70.333931	2435.392260	21.181312
70.488457	2442.156756	21.186330
70.652759	2441.342165	21.191347
70.719317	2441.281297	21.196365
70.804282	2443.524602	21.201383
70.665456	2450.442079	21.206400
70.903939	2444.910334	21.211418
71.240651	2435.945345	21.216435
71.049822	2441.485430	21.221453
71.166159	2444.042607	21.226471
70.850410	2443.766690	21.231488
70.727412	2453.872425	21.236506
71.012017	2462.762761	21.241523
71.495526	2461.604962	21.246541
71.530243	2465.159524	21.251559
71.646122	2468.420567	21.256576
71.281766	2470.235183	21.261594
71.373780	2465.647791	21.266611
71.340901	2483.834675	21.271629
71.613298	2485.720579	21.276647
71.878690	2486.654457	21.281664
71.816012	2492.401838	21.286682
71.960885	2491.328321	21.291699
72.006937	2497.011434	21.296717
72.008467	2493.833081	21.301735
72.065009	2494.139870	21.306752
71.955778	2511.764276	21.311770
72.315497	2518.995504	21.316787
72.210346	2516.916271	21.321805
71.944373	2518.835503	21.326823
72.183440	2529.667601	21.331840
71.955462	2530.839254	21.336858
72.337383	2541.548125	21.341875
72.944149	2546.976685	21.346893
72.495657	2546.475264	21.351911
72.620549	2538.979193	21.356928
73.210383	2548.134495	21.361946
73.185410	2543.880900	21.366963
73.299225	2555.120705	21.371981
73.489046	2547.519841	21.376999
73.790121	2550.199761	21.382016
73.188661	2540.762208	21.387034
73.586791	2535.944088	21.392051
73.820616	2545.293682	21.397069
73.575833	2538.388536	21.402087
74.083917	2538.328357	21.407104
73.919230	2549.507372	21.412122
73.857803	2531.161504	21.417139
73.813615	2546.528731	21.422157
73.811167	2550.666650	21.427175
74.380558	2543.852505	21.432192
74.057275	2542.817158	21.437210
74.353147	2547.994300	21.442227
74.325370	2541.440401	21.447245
74.437539	2543.575335	21.452263
74.600421	2543.467909	21.457280
74.296319	2549.600059	21.462298
74.698173	2536.269567	21.467315
74.366679	2539.041660	21.472333
74.772499	2548.563306	21.477351
74.566303	2541.648995	21.482368
74.653066	2553.338011	21.487386
74.825526	2561.437914	21.492403
74.967137	2567.535391	21.497421
74.594652	2572.554651	21.502439
74.907352	2564.814719	21.507456
74.898252	2566.223714	21.512474
75.223803	2581.306171	21.517491
75.666708	2590.408626	21.522509
75.341048	2588.777156	21.527527
75.553663	2592.881600	21.532544
75.442112	2591.415625	21.537562
75.521276	2594.789711	21.542579
75.830933	2596.344754	21.547597
75.443582	2589.408133	21.552615
75.849206	2587.568126	21.557632
75.381198	2608.129941	21.562650
75.812577	2599.670878	21.567667
76.014838	2619.995796	21.572685
76.205156	2614.828130	21.577703
76.125190	2602.348990	21.582720
76.018858	2612.247077	21.587738
76.474726	2621.079267	21.592755
76.613117	2632.978063	21.597773
76.663285	2632.995491	21.602791
76.551119	2628.695486	21.607808
76.548882	2627.707986	21.612826
76.739880	2634.435316	21.617843
76.567252	2640.114649	21.622861
76.674911	2645.286407	21.627879
77.084254	2640.715841	21.632896
76.997041	2658.122352	21.637914
77.189495	2656.593259	21.642931
77.152163	2655.680654	21.647949
77.188409	2653.828717	21.652967
77.427364	2651.645396	21.657984
77.675479	2659.572606	21.663002
77.515871	2661.658343	21.668019
77.789148	2656.670268	21.673037
77.703701	2655.793559	21.678055
78.082934	2650.738491	21.683072
77.869692	2654.489500	21.688090
77.838069	2655.627433	21.693107
78.198834	2654.801181	21.698125
78.099809	2666.329833	21.703143
78.305471	2674.086922	21.708160
78.405965	2688.459682	21.713178
78.326265	2688.699317	21.718195
78.793057	2684.460649	21.723213
78.583621	2689.574484	21.728231
78.912001	2684.902895	21.733248
78.684438	2680.740774	21.738266
78.727471	2680.279594	21.743283
78.712687	2677.450913	21.748301
78.688335	2678.796015	21.753319
79.040981	2672.406918	21.758336
78.997067	2669.696392	21.763354
78.716802	2684.147367	21.768371
78.869881	2691.041581	21.773389
79.248226	2695.035032	21.778407
79.341345	2701.285282	21.783424
79.128726	2710.628727	21.788442
79.209381	2710.597224	21.793459
79.582661	2703.557912	21.798477
79.477173	2711.123601	21.803495
79.253112	2709.574139	21.808512
79.440772	2722.554161	21.813530
79.663572	2729.387038	21.818547
79.938873	2722.495528	21.823565
79.561438	2733.120754	21.828583
79.624107	2739.132743	21.833600
79.781891	2756.501204	21.838618
79.645075	2757.674459	21.843635
79.972450	2754.161282	21.848653
80.010608	2768.581684	21.853671
80.863259	2763.699050	21.858688
80.411861	2774.102267	21.863706
80.540508	2768.300323	21.868723
81.263013	2761.844141	21.873741
80.765886	2770.928931	21.878759
81.041991	2776.756210	21.883776
81.034283	2771.319505	21.888794
81.380609	2772.663711	21.893811
81.244340	2767.183902	21.898829
81.144211	2774.931835	21.903847
81.289384	2782.464839	21.908864
81.627914	2800.256519	21.913882
81.777972	2791.181548	21.918899
82.004904	2791.891038	21.923917
81.649276	2794.165113	21.928935
81.752895	2789.894594	21.933952
81.827742	2790.577266	21.938970
81.776677	2793.188962	21.943987
82.024190	2788.649867	21.949005
82.149941	2787.143772	21.954023
82.167478	2789.577515	21.959040
82.197258	2784.198091	21.964058
82.296134	2800.101884	21.969075
82.592046	2805.225442	21.974093
82.346554	2812.326937	21.979111
82.275270	2809.841576	21.984128
82.557171	2818.404279	21.989146
82.510839	2818.815460	21.994163
82.768138	2810.740037	21.999181
82.923095	2818.375684	22.004199
82.839886	2801.260643	22.009216
82.847280	2822.269437	22.014234
82.685543	2829.458892	22.019251
83.178884	2836.060323	22.024269
82.932945	2838.923292	22.029287
83.197779	2839.295495	22.034304
82.980997	2834.509913	22.039322
83.328569	2851.325009	22.044339
83.385488	2859.433568	22.049357
83.115634	2869.297291	22.054375
83.421109	2863.635056	22.059392
83.538771	2875.956999	22.064410
83.656856	2880.593824	22.069427
83.839380	2871.573723	22.074445
83.854711	2881.626601	22.079463
84.341967	2869.620744	22.084480
84.620348	2881.166520	22.089498
84.621829	2881.081067	22.094515
84.628018	2873.076273	22.099533
84.270793	2883.237653	22.104551
84.784529	2867.869604	22.109568
84.798061	2874.892922	22.114586
84.771566	2891.210825	22.119603
85.020916	2884.932418	22.124621
84.970335	2888.923261	22.129639
85.252972	2881.699159	22.134656
85.526103	2882.584513	22.139674
85.201691	2890.181207	22.144691
85.166466	2894.671477	22.149709
85.568234	2896.950729	22.154727
85.132127	2898.129561	22.159744
85.461837	2889.108628	22.164762
85.404187	2889.496325	22.169779
85.470113	2898.190530	22.174797
85.432329	2909.296357	22.179815
85.333272	2917.460787	22.184832
85.832026	2908.334624	22.189850
86.038541	2933.854154	22.194867
86.321473	2935.236648	22.199885
86.220024	2941.129076	22.204903
86.251910	2943.724723	22.209920
86.400200	2931.351840	22.214938
86.319557	2939.671218	22.219955
86.198223	2941.081937	22.224973
86.403627	2947.661961	22.229991
86.407445	2955.087647	22.235008
86.925867	2957.295091	22.240026
86.448990	2965.827665	22.245043
86.690620	2959.386318	22.250061
86.650375	2976.268224	22.255079
86.953608	2983.865075	22.260096
87.345321	2984.457391	22.265114
87.207360	2988.338772	22.270131
87.405368	2981.493915	22.275149
87.617527	2983.117826	22.280167
87.344178	2990.551962	22.285184
87.883140	3004.487445	22.290202
87.664316	3017.669836	22.295219
87.971408	3013.919903	22.300237
88.028837	3012.888375	22.305255
87.689986	3008.522577	22.310272
88.010243	3007.087176	22.315290
87.867588	3014.583032	22.320307
88.592479	3025.860549	22.325325
88.519510	3029.946435	22.330343
88.600452	3036.189230	22.335360
88.407509	3030.102723	22.340378
88.153839	3031.098510	22.345395
88.420055	3031.713523	22.350413
88.684055	3025.858861	22.355431
88.626382	3038.047252	22.360448
88.854703	3044.118766	22.365466
88.637762	3065.077556	22.370483
88.851112	3053.846441	22.375501
89.632970	3057.445758	22.380519
89.479547	3039.230471	22.385536
89.623012	3036.509652	22.390554
90.077298	3036.814490	22.395571
89.998489	3033.339251	22.400589
89.853033	3032.752760	22.405607
90.369725	3032.665993	22.410624
90.435500	3028.413934	22.415642
90.675364	3025.299375	22.420659
90.565697	3024.322267	22.425677
90.532934	3030.942560	22.430695
90.437466	3017.815386	22.435712
90.691450	3015.964229	22.440730
90.275629	3021.867756	22.445747
90.467262	3017.091128	22.450765
91.049377	3025.547223	22.455783
90.895150	3023.260956	22.460800
90.809762	3014.131003	22.465818
90.729312	3027.405477	22.470835
90.554387	3018.841781	22.475853
90.557999	3027.321668	22.480871
90.530288	3049.917403	22.485888
90.822571	3040.305716	22.490906
91.000008	3053.659991	22.495923
91.047036	3063.600727	22.500941
91.305833	3066.019038	22.505959
91.192593	3064.919395	22.510976
91.258068	3071.527564	22.515994
91.356252	3091.818723	22.521011
91.416370	3100.163602	22.526029
91.460726	3101.977768	22.531047
91.705103	3114.854560	22.536064
92.229161	3119.071598	22.541082
92.117677	3119.161537	22.546099
92.294630	3124.508856	22.551117
92.358234	3113.054841	22.556135
92.688230	3117.169536	22.561152
92.850911	3123.696311	22.566170
92.582634	3121.828616	22.571187
93.221452	3132.548342	22.576205
93.025581	3130.385322	22.581223
93.119902	3134.457810	22.586240
93.380950	3130.244760	22.591258
93.404546	3129.114340	22.596275
93.359945	3120.927976	22.601293
93.546550	3123.433282	22.606311
93.507953	3127.397062	22.611328
93.953211	3123.969612	22.616346
93.993932	3130.490129	22.621363
94.113978	3131.645509	22.626381
94.168303	3124.639912	22.631399
93.800581	3132.458067	22.636416
94.002832	3126.761324	22.641434
94.086199	3124.952500	22.646451
94.251573	3128.234362	22.651469
94.176233	3125.512879	22.656487
93.728446	3132.696493	22.661504
94.397285	3142.600428	22.666522
94.407269	3152.445985	22.671539
94.332284	3151.794863	22.676557
94.694635	3143.371542	22.681575
94.664076	3169.739444	22.686592
95.270617	3163.361142	22.691610
95.210046	3170.866376	22.696627
95.226157	3179.574787	22.701645
95.529297	3181.187707	22.706663
95.646187	3174.544774	22.711680
95.593924	3179.971984	22.716698
95.499038	3180.640068	22.721715
95.488850	3185.079170	22.726733
95.212256	3181.237023	22.731751
95.453926	3184.144061	22.736768
95.712813	3182.762388	22.741786
95.443201	3192.749338	22.746803
95.557682	3200.116865	22.751821
95.902568	3206.104008	22.756839
95.935700	3201.295198	22.761856
95.932243	3212.796697	22.766874
96.143950	3237.362697	22.771891
96.094317	3227.052983	22.776909
96.195664	3233.968085	22.781927
96.520322	3246.422173	22.786944
96.581681	3256.348160	22.791962
96.629617	3265.329398	22.796979
96.398632	3260.271328	22.801997
97.271385	3264.288928	22.807015
97.232283	3281.019447	22.812032
97.364064	3275.598746	22.817050
97.521939	3275.924489	22.822067
97.589606	3278.580892	22.827085
97.570102	3270.011815	22.832103
97.497282	3268.022145	22.837120
97.904724	3281.239781	22.842138
97.623320	3298.127975	22.847155
97.884903	3306.110186	22.852173
98.313974	3292.105793	22.857191
98.309877	3296.121050	22.862208
98.132242	3291.468121	22.867226
98.115178	3302.602526	22.872243
98.946074	3302.697239	22.877261
99.041716	3300.286817	22.882279
99.105754	3293.099742	22.887296
99.490314	3281.538839	22.892314
99.260307	3278.364834	22.897331
99.282586	3285.427980	22.902349
99.484176	3275.719824	22.907367
99.532882	3281.453271	22.912384
99.368778	3283.299912	22.917402
99.037656	3287.378707	22.922419
99.099143	3291.279598	22.927437
99.256156	3307.443062	22.932455
99.157997	3312.088418	22.937472
99.269222	3307.374730	22.942490
99.836828	3328.227458	22.947507
99.595792	3333.643074	22.952525
99.578503	3340.311570	22.957543
99.613323	3344.955167	22.962560
100.191009	3354.201148	22.967578
100.104907	3364.235370	22.972595
100.464596	3367.143000	22.977613
100.270577	3365.964387	22.982631
100.393175	3375.278077	22.987648
100.389854	3392.277715	22.992666
100.617471	3390.809366	22.997683
100.389591	3398.129280	23.002701
100.703911	3412.674480	23.007719
100.753344	3420.159534	23.012736
100.908163	3418.266965	23.017754
101.207066	3421.316627	23.022771
101.792188	3428.954996	23.027789
102.039574	3435.841125	23.032807
102.083896	3436.231894	23.037824
102.472539	3429.770646	23.042842
102.386569	3417.304500	23.047859
101.997355	3416.550795	23.052877
102.091420	3401.478034	23.057895
101.992192	3403.980538	23.062912
102.051761	3418.562250	23.067930
102.459224	3428.551224	23.072947
101.979382	3430.535411	23.077965
102.204184	3427.429441	23.082983
102.158691	3434.919813	23.088000
102.932600	3443.194748	23.093018
102.990357	3448.358727	23.098035
102.851545	3457.766815	23.103053
102.933422	3451.249167	23.108071
103.025167	3455.353691	23.113088
103.062387	3452.633570	23.118106
103.463042	3465.767183	23.123123
103.222268	3486.897451	23.128141
103.547471	3487.380206	23.133159
103.470895	3492.896511	23.138176
103.555950	3486.223703	23.143194
103.810625	3493.929328	23.148211
103.571132	3500.525169	23.153229
104.271955	3509.600562	23.158247
104.048700	3515.575266	23.163264
104.090269	3507.577307	23.168282
104.391584	3517.355611	23.173299
104.216222	3534.868223	23.178317
104.607960	3531.206003	23.183335
104.915608	3536.018637	23.188352
104.928187	3534.261825	23.193370
105.059298	3531.473419	23.198387
104.611865	3539.607154	23.203405
104.904309	3546.391624	23.208423
104.933035	3548.044147	23.213440
104.881863	3558.126693	23.218458
104.911319	3560.883773	23.223475
105.321148	3586.038018	23.228493
105.832214	3582.322491	23.233511
105.475082	3589.012428	23.238528
105.622674	3593.670094	23.243546
105.605419	3598.558579	23.248563
105.640658	3605.572490	23.253581
106.101102	3604.970550	23.258599
105.645385	3614.058782	23.263616
105.938294	3623.980483	23.268634
106.336665	3626.942102	23.273651
106.483957	3627.496747	23.278669
107.049583	3629.690615	23.283687
107.078573	3644.501361	23.288704
107.440370	3648.137795	23.293722
107.595219	3653.463464	23.298739
107.415924	3653.822773	23.303757
107.471457	3649.325978	23.308775
107.359346	3655.996728	23.313792
107.495823	3653.169594	23.318810
107.509975	3642.707682	23.323827
107.721787	3646.140219	23.328845
107.646231	3650.040432	23.333863
107.787099	3653.824888	23.338880
108.107203	3665.806544	23.343898
107.967491	3670.808801	23.348915
108.071083	3678.162438	23.353933
108.256346	3680.175661	23.358951
108.420208	3670.899256	23.363968
108.132490	3677.935071	23.368986
108.671297	3688.023677	23.374003
108.918459	3696.017776	23.379021
109.019893	3692.722657	23.384039
109.065582	3694.874392	23.389056
108.711433	3702.214088	23.394074
108.996626	3684.816758	23.399091
108.818038	3693.378981	23.404109
109.161750	3700.480619	23.409127
109.422473	3714.706161	23.414144
109.628990	3722.103759	23.419162
109.540531	3712.683557	23.424179
109.362138	3722.565067	23.429197
109.495799	3734.566328	23.434215
109.766341	3743.266959	23.439232
109.734816	3745.907313	23.444250
109.914048	3755.707911	23.449267
109.934029	3774.212961	23.454285
110.124595	3775.243778	23.459303
110.375381	3769.791775	23.464320
110.456804	3778.727024	23.469338
110.858655	3787.148421	23.474355
110.903180	3786.068358	23.479373
111.109796	3784.934653	23.484391
111.095922	3787.550171	23.489408
111.037516	3795.847544	23.494426
111.517989	3794.980512	23.499443
111.553146	3812.851990	23.504461
111.716614	3815.272620	23.509479
111.759606	3804.215907	23.514496
111.867942	3807.860273	23.519514
111.883116	3795.996741	23.524531
112.008046	3809.214564	23.529549
112.962480	3824.481059	23.534567
112.862667	3823.013154	23.539584
112.656044	3814.517139	23.544602
112.921003	3807.664702	23.549619
112.861052	3815.630919	23.554637
113.402088	3822.143228	23.559655
113.315237	3811.214038	23.564672
113.070644	3810.453581	23.569690
113.262948	3806.945451	23.574707
113.328413	3819.149916	23.579725
113.205327	3827.880312	23.584743
113.403218	3827.950492	23.589760
113.366543	3833.621658	23.594778
113.600292	3825.476856	23.599795
112.961785	3831.936097	23.604813
113.230906	3842.420278	23.609831
113.611135	3853.044979	23.614848
113.788141	3867.305768	23.619866
114.312528	3872.059498	23.624883
114.318843	3884.756125	23.629901
114.398281	3878.207140	23.634919
114.507943	3881.769252	23.639936
114.247954	3891.272182	23.644954
114.508954	3903.247417	23.649971
114.601069	3910.899624	23.654989
114.746901	3903.055695	23.660007
115.063116	3907.658782	23.665024
114.995509	3927.086629	23.670042
115.303599	3924.848205	23.675059
115.196358	3928.611379	23.680077
115.511905	3924.074033	23.685095
115.610445	3937.693748	23.690112
115.707948	3949.539812	23.695130
116.304651	3943.942369	23.700147
116.138343	3951.237139	23.705165
115.988412	3951.007971	23.710183
116.090764	3954.438673	23.715200
116.269932	3945.993000	23.720218
116.805177	3961.113406	23.725235
116.813207	3965.676115	23.730253
117.056367	3966.301065	23.735271
117.080902	3973.989071	23.740288
116.935812	3978.613498	23.745306
117.233188	3976.215766	23.750323
117.265327	3966.984968	23.755341
117.164730	3972.637724	23.760359
117.291965	3965.431073	23.765376
116.972188	3967.712335	23.770394
117.112291	3978.813219	23.775411
117.491155	3985.344524	23.780429
117.401459	3993.997206	23.785447
117.870560	4003.291992	23.790464
117.760801	4019.999478	23.795482
117.972335	4017.810794	23.800499
118.032321	4017.242784	23.805517
117.913364	4024.978403	23.810535
118.416531	4032.639259	23.815552
118.970788	4034.765511	23.820570
119.176655	4030.870159	23.825587
119.242552	4039.006258	23.830605
119.318645	4037.015412	23.835623
119.425423	4035.445887	23.840640
119.198525	4039.903158	23.845658
119.575525	4054.874685	23.850675
119.887788	4064.831492	23.855693
119.810220	4069.325490	23.860711
120.025771	4064.664801	23.865728
119.899385	4064.378310	23.870746
119.567271	4063.530466	23.875763
119.510890	4069.482528	23.880781
119.758263	4080.929746	23.885799
120.061453	4084.016730	23.890816
120.014978	4089.187651	23.895834
120.547050	4110.889550	23.900851
120.966969	4107.806743	23.905869
120.487184	4115.570172	23.910887
121.153582	4114.939308	23.915904
120.639807	4127.821237	23.920922
121.029204	4137.459913	23.925939
121.030582	4143.141033	23.930957
121.188898	4142.197892	23.935975
121.651070	4154.890016	23.940992
121.656407	4163.985648	23.946010
121.668723	4156.983036	23.951027
121.956787	4167.237203	23.956045
121.734462	4164.895110	23.961063
122.110384	4176.044619	23.966080
121.907204	4188.650980	23.971098
122.061708	4186.354372	23.976115
122.345440	4193.938991	23.981133
122.197516	4214.061414	23.986151
122.793247	4211.304724	23.991168
122.625535	4213.271960	23.996186
122.623949	4227.658685	24.001203
122.809175	4241.107317	24.006221
123.194544	4242.133083	24.011239
123.415518	4243.954586	24.016256
124.161698	4242.433840	24.021274
124.971323	4222.650230	24.026291
124.941835	4209.451945	24.031309
124.869469	4205.249524	24.036327
124.951167	4198.892607	24.041344
124.941598	4197.388527	24.046362
124.607256	4171.255827	24.051379
124.784468	4169.517509	24.056397
124.823638	4167.822777	24.061415
125.160251	4169.935587	24.066432
124.857481	4171.961721	24.071450
125.022655	4167.570823	24.076467
125.093116	4161.452391	24.081485
124.953591	4187.652524	24.086503
125.440062	4191.749417	24.091520
125.323078	4194.889213	24.096538
125.370007	4196.920875	24.101555
125.283328	4193.333010	24.106573
125.290178	4201.112243	24.111591
125.550373	4209.382297	24.116608
125.311822	4227.296800	24.121626
125.676118	4227.072787	24.126643
125.838142	4239.890611	24.131661
125.957615	4252.923386	24.136679
126.275402	4260.619515	24.141696
125.939074	4271.595907	24.146714
126.204223	4271.671400	24.151731
126.380542	4275.144304	24.156749
126.527424	4291.944649	24.161767
126.897512	4300.671084	24.166784
126.954094	4314.613249	24.171802
126.790599	4326.099341	24.176819
127.418865	4325.442845	24.181837
127.482163	4327.879140	24.186855
127.661750	4343.206745	24.191872
127.707614	4357.630375	24.196890
127.693115	4352.942303	24.201907
128.178836	4354.066080	24.206925
128.043812	4370.616849	24.211943
128.306018	4373.161061	24.216960
128.312552	4376.868737	24.221978
128.491083	4378.914650	24.226995
128.946277	4387.425870	24.232013
128.687492	4410.516954	24.237031
129.170304	4404.634094	24.242048
129.091864	4402.954495	24.247066
129.103324	4406.430997	24.252083
129.297500	4415.462635	24.257101
128.965421	4427.126543	24.262119
129.375953	4430.667171	24.267136
129.099350	4450.904582	24.272154
129.467197	4463.267567	24.277171
129.602402	4459.379969	24.282189
129.522427	4477.020677	24.287207
130.411704	4476.093124	24.292224
130.695149	4483.210768	24.297242
130.655415	4493.067953	24.302259
131.080831	4495.501550	24.307277
131.170380	4499.963323	24.312295
131.184090	4504.714665	24.317312
131.646583	4495.006268	24.322330
131.266538	4494.181647	24.327347
131.840503	4499.091957	24.332365
131.443208	4501.334852	24.337383
131.634947	4498.779899	24.342400
131.551319	4501.059180	24.347418
131.700833	4511.322488	24.352435
132.256073	4523.962507	24.357453
132.066109	4534.493316	24.362471
131.726135	4528.580699	24.367488
132.144965	4542.693899	24.372506
132.236856	4549.743545	24.377523
132.543371	4550.497533	24.382541
132.829498	4573.210442	24.387559
133.093330	4574.015266	24.392576
132.888645	4591.107353	24.397594
132.991792	4584.412385	24.402611
133.207706	4579.483216	24.407629
132.983225	4600.242949	24.412647
133.828598	4600.556372	24.417664
133.548033	4603.475509	24.422682
133.583363	4614.596252	24.427699
133.766350	4615.009647	24.432717
134.021423	4635.685289	24.437735
134.130872	4634.137391	24.442752
134.113369	4634.386306	24.447770
134.124710	4643.020410	24.452787
134.506347	4650.274339	24.457805
134.657196	4662.576554	24.462823
134.410081	4664.666675	24.467840
134.946234	4674.225974	24.472858
134.824174	4677.884293	24.477875
135.199567	4685.227587	24.482893
135.234543	4692.778548	24.487911
135.379463	4709.671122	24.492928
135.408883	4717.216645	24.497946
135.583815	4713.000855	24.502963
136.102263	4707.513212	24.507981
136.076171	4726.436741	24.512999
136.340050	4718.176374	24.518016
136.408224	4719.848114	24.523034
136.598081	4721.709231	24.528051
136.559451	4728.072233	24.533069
136.721592	4745.808076	24.538087
136.959285	4741.165862	24.543104
137.233706	4740.261429	24.548122
137.314599	4746.432226	24.553139
137.709175	4756.903720	24.558157
137.628978	4765.144958	24.563175
137.663278	4773.194770	24.568192
137.859168	4774.966574	24.573210
137.829804	4785.466211	24.578227
138.236886	4774.775179	24.583245
138.071208	4789.752896	24.588263
138.005445	4801.201978	24.593280
138.558420	4800.661351	24.598298
138.233483	4805.064631	24.603315
138.913719	4819.863325	24.608333
138.937200	4818.331953	24.613351
139.186950	4813.530023	24.618368
139.481560	4814.595205	24.623386
139.671103	4812.813873	24.628403
140.077602	4804.152492	24.633421
139.652551	4812.905123	24.638439
139.850752	4827.166527	24.643456
140.316310	4825.054986	24.648474
140.862115	4826.892260	24.653491
141.114759	4807.327303	24.658509
141.373142	4811.781806	24.663527
140.771826	4802.478760	24.668544
141.214610	4786.899185	24.673562
140.954801	4782.283915	24.678579
141.278458	4793.902781	24.683597
141.045821	4799.522692	24.688615
141.373615	4803.079433	24.693632
141.523969	4799.063147	24.698650
141.493092	4800.826070	24.703667
141.752736	4799.980750	24.708685
141.500655	4809.631280	24.713703
141.635749	4824.372813	24.718720
141.966423	4820.675655	24.723738
141.638113	4829.889852	24.728755
142.053887	4835.617145	24.733773
141.904747	4855.576335	24.738791
141.558719	4854.465479	24.743808
141.988418	4873.185628	24.748826
142.425319	4900.386012	24.753843
142.511877	4884.754497	24.758861
142.893682	4906.673290	24.763879
142.740918	4918.697836	24.768896
143.129298	4902.021880	24.773914
143.234056	4926.972976	24.778931
143.541194	4929.295634	24.783949
143.617340	4939.621111	24.788967
143.699872	4938.241514	24.793984
144.076260	4947.263987	24.799002
144.182499	4960.700200	24.804019
144.079612	4950.378856	24.809037
144.354602	4965.679509	24.814055
144.273352	4982.007824	24.819072
144.573699	4988.507529	24.824090
144.579396	4989.829185	24.829107
144.968855	5008.637807	24.834125
144.788801	5013.438389	24.839143
145.014552	5014.309134	24.844160
145.119211	5024.491337	24.849178
145.385775	5044.243971	24.854195
145.526105	5035.260928	24.859213
145.899410	5061.578178	24.864231
145.673318	5073.128148	24.869248
146.371801	5061.965456	24.874266
146.441238	5074.163837	24.879283
146.679231	5074.505550	24.884301
146.867865	5084.179147	24.889319
146.796548	5096.465742	24.894336
146.848498	5080.766848	24.899354
147.262510	5099.237156	24.904371
147.410244	5103.462753	24.909389
147.526398	5114.609096	24.914407
147.639946	5104.020389	24.919424
147.743421	5102.246116	24.924442
147.562379	5129.116929	24.929459
147.659623	5133.602912	24.934477
147.831634	5132.259873	24.939495
148.003700	5145.774355	24.944512
148.366583	5159.798897	24.949530
148.676225	5164.614814	24.954547
148.785415	5173.865233	24.959565
149.263711	5175.618361	24.964583
149.216096	5177.709043	24.969600
149.520823	5184.233388	24.974618
149.477994	5181.241388	24.979635
149.711540	5180.220195	24.984653
149.782860	5189.296599	24.989671
149.595407	5210.808821	24.994688
149.834689	5216.064989	24.999706
150.044462	5206.992137	25.004723
150.541207	5214.408292	25.009741
150.572476	5233.872648	25.014759
150.508247	5228.772279	25.019776
150.775135	5219.450636	25.024794
150.932923	5238.645936	25.029811
151.174737	5251.458366	25.034829
151.427137	5252.722693	25.039847
151.265912	5258.558894	25.044864
151.661237	5252.193814	25.049882
151.111905	5264.813779	25.054899
151.731685	5262.469849	25.059917
151.868195	5278.672989	25.064935
151.524883	5281.074867	25.069952
151.888233	5285.197495	25.074970
152.079618	5303.494343	25.079987
152.265228	5301.262196	25.085005
152.720136	5311.958200	25.090023
152.338096	5318.889385	25.095040
152.877654	5334.360644	25.100058
153.054223	5329.468964	25.105075
152.961086	5335.992178	25.110093
153.437845	5344.049113	25.115111
153.213867	5353.919667	25.120128
153.511515	5357.291821	25.125146
153.915892	5364.053237	25.130163
153.842917	5380.292240	25.135181
153.940419	5374.431181	25.140199
153.869527	5393.346596	25.145216
154.599939	5391.310548	25.150234
154.686936	5397.906747	25.155251
154.768150	5405.589693	25.160269
154.728933	5413.761713	25.165287
155.139474	5428.303026	25.170304
155.352785	5439.538607	25.175322
155.026831	5439.930251	25.180339
155.000072	5444.359861	25.185357
155.506339	5452.219702	25.190375
155.681288	5465.544582	25.195392
155.710825	5469.012160	25.200410
155.727995	5478.182365	25.205427
156.033917	5479.343679	25.210445
156.325473	5504.746278	25.215463
156.146752	5507.072055	25.220480
156.515374	5520.770859	25.225498
157.013518	5533.123759	25.230515
156.906900	5536.877698	25.235533
157.146856	5537.812546	25.240551
157.431419	5562.019983	25.245568
157.712048	5557.528705	25.250586
157.786822	5558.205182	25.255603
157.737206	5561.300003	25.260621
157.888680	5577.308529	25.265639
157.864216	5587.413297	25.270656
158.275011	5585.420677	25.275674
158.509077	5603.269264	25.280691
158.965102	5604.703934	25.285709
159.239320	5601.918184	25.290727
159.100820	5600.999084	25.295744
159.731696	5607.741111	25.300762
159.800133	5616.174239	25.305779
159.900924	5627.266470	25.310797
160.337822	5616.062098	25.315815
159.903284	5622.739578	25.320832
160.376630	5620.762467	25.325850
160.731532	5616.366935	25.330867
160.539327	5618.492805	25.335885
160.962398	5616.766578	25.340903
160.468252	5633.162918	25.345920
160.691187	5634.570749	25.350938
160.802529	5644.878521	25.355955
160.735918	5652.660343	25.360973
161.040483	5665.321250	25.365991
161.347030	5675.728067	25.371008
161.418888	5673.043257	25.376026
161.307665	5697.123100	25.381043
161.583485	5706.751889	25.386061
161.818336	5708.924918	25.391079
161.628840	5729.156500	25.396096
162.164075	5728.732249	25.401114
162.306770	5746.266918	25.406131
162.240483	5756.182583	25.411149
162.807257	5763.045129	25.416167
163.029537	5776.675369	25.421184
163.331529	5782.512220	25.426202
163.449538	5785.262165	25.431219
163.568720	5777.967668	25.436237
164.364688	5768.721201	25.441255
164.571757	5766.583511	25.446272
164.449415	5753.016615	25.451290
164.555816	5754.603584	25.456307
164.696533	5755.995816	25.461325
164.569096	5758.821850	25.466343
164.772451	5765.608401	25.471360
165.086376	5767.901702	25.476378
165.078653	5776.602445	25.481395
165.224460	5777.012188	25.486413
165.355792	5777.285294	25.491431
165.649891	5791.002218	25.496448
165.867142	5804.005101	25.501466
165.968717	5802.199491	25.506483
166.024014	5811.468095	25.511501
166.149786	5811.742067	25.516519
166.317984	5815.491156	25.521536
166.732318	5827.630032	25.526554
166.422631	5829.881542	25.531571
166.489853	5843.103520	25.536589
166.742128	5844.017526	25.541607
166.757568	5847.881946	25.546624
167.088569	5864.790815	25.551642
167.244001	5876.108280	25.556659
167.410866	5881.454831	25.561677
167.427725	5891.035651	25.566695
167.615124	5907.285090	25.571712
167.430566	5914.848642	25.576730
168.063508	5930.773049	25.581747
168.009698	5938.827626	25.586765
168.509761	5951.253115	25.591783
168.688894	5967.140884	25.596800
169.003108	5965.447356	25.601818
169.272609	5979.610179	25.606835
168.661125	5982.764138	25.611853
169.433420	5993.531082	25.616871
169.695329	6015.820266	25.621888
170.030515	6015.174626	25.626906
170.153077	6016.954813	25.631923
169.939394	6028.440321	25.636941
170.182831	6043.617373	25.641959
170.269265	6047.717000	25.646976
170.153142	6061.270718	25.651994
170.620667	6062.217512	25.657011
170.330582	6076.369677	25.662029
170.902169	6079.642497	25.667047
171.012116	6094.676229	25.672064
171.532515	6113.711828	25.677082
171.945416	6116.763142	25.682100
171.688911	6117.645893	25.687117
172.280465	6124.410019	25.692135
172.317405	6131.471991	25.697152
172.187964	6142.571971	25.702170
172.736403	6146.596534	25.707188
172.832565	6162.898285	25.712205
173.089869	6159.973036	25.717223
173.154222	6161.828589	25.722240
173.093449	6166.910784	25.727258
173.231125	6177.391530	25.732276
173.646844	6196.629756	25.737293
173.900066	6187.969489	25.742311
173.834933	6215.032194	25.747328
174.166916	6230.858515	25.752346
174.198486	6224.063606	25.757364
174.128205	6229.554508	25.762381
174.737892	6244.554752	25.767399
174.808373	6244.420660	25.772416
174.663664	6247.341001	25.777434
175.147763	6255.157293	25.782452
175.307388	6265.801976	25.787469
175.655249	6265.062811	25.792487
175.651907	6265.214842	25.797504
175.303655	6277.624266	25.802522
175.614461	6285.334971	25.807540
175.657911	6302.689913	25.812557
175.847569	6314.652596	25.817575
176.280937	6328.120961	25.822592
176.305249	6334.559955	25.827610
176.867303	6348.166134	25.832628
176.628587	6359.014940	25.837645
176.819929	6365.472133	25.842663
176.874418	6386.843900	25.847680
177.612596	6400.678390	25.852698
177.782472	6402.375488	25.857716
177.517653	6403.401597	25.862733
178.358153	6417.920955	25.867751
178.249389	6429.153627	25.872768
178.527426	6423.917562	25.877786
179.022953	6428.575451	25.882804
179.064939	6443.727380	25.887821
179.700910	6451.747394	25.892839
179.835718	6448.083562	25.897856
179.668785	6451.600856	25.902874
179.697265	6448.850081	25.907892
179.855063	6452.676682	25.912909
180.186879	6456.024782	25.917927
180.465920	6469.962374	25.922944
180.325589	6478.876656	25.927962
180.583917	6471.143533	25.932980
180.495982	6491.404340	25.937997
180.743943	6500.343410	25.943015
181.079318	6502.137863	25.948032
180.914559	6514.351572	25.953050
181.213648	6519.207375	25.958068
181.269247	6529.379117	25.963085
181.607370	6546.641062	25.968103
181.529573	6559.030665	25.973120
181.883207	6569.010819	25.978138
182.165832	6572.578099	25.983156
182.274567	6590.904891	25.988173
182.404048	6603.887286	25.993191
182.662202	6606.561872	25.998208
182.816254	6620.452748	26.003226
183.146676	6636.437500	26.008244
183.116358	6653.753752	26.013261
183.230824	6658.480499	26.018279
183.646753	6663.870579	26.023296
183.874878	6667.572633	26.028314
184.135127	6673.119537	26.033332
184.168439	6677.173910	26.038349
184.292074	6686.880576	26.043367
184.634845	6698.065211	26.048384
184.980133	6707.854179	26.053402
185.070724	6706.220654	26.058420
185.060790	6720.197115	26.063437
185.598068	6728.652465	26.068455
185.663077	6722.360402	26.073472
186.231397	6734.400147	26.078490
186.894588	6725.887301	26.083508
186.733847	6743.315490	26.088525
186.617831	6754.925144	26.093543
186.700873	6748.071519	26.098560
186.714108	6743.088093	26.103578
186.946762	6743.515905	26.108596
186.851936	6751.031106	26.113613
187.394283	6765.827605	26.118631
187.518722	6768.583012	26.123648
187.324117	6774.598514	26.128666
187.714649	6792.512295	26.133684
187.745982	6795.822007	26.138701
187.834541	6800.394987	26.143719
187.758617	6816.948243	26.148736
188.073914	6828.765432	26.153754
188.228928	6847.798706	26.158772
188.566333	6853.261046	26.163789
188.634592	6874.265053	26.168807
189.119480	6873.943324	26.173824
189.131806	6893.664940	26.178842
189.937754	6889.697653	26.183860
190.128497	6895.668984	26.188877
190.072989	6892.350372	26.193895
190.692559	6919.130736	26.198912
190.956313	6928.380079	26.203930
191.145562	6921.942334	26.208948
191.033398	6925.842632	26.213965
191.077629	6921.324692	26.218983
191.422231	6935.931141	26.224000
191.182428	6949.129114	26.229018
191.282987	6951.522079	26.234036
191.882993	6961.397797	26.239053
191.948625	6969.049102	26.244071
191.795079	6976.999705	26.249088
192.089594	6985.477187	26.254106
192.599662	7001.121767	26.259124
192.470705	7012.938791	26.264141
192.650737	7016.809401	26.269159
192.885992	7022.101445	26.274176
192.831792	7045.040891	26.279194
193.607802	7050.715960	26.284212
193.928503	7059.230438	26.289229
193.969625	7071.627128	26.294247
194.231439	7074.926262	26.299264
194.197837	7080.197044	26.304282
194.891055	7091.043246	26.309300
194.918087	7098.893181	26.314317
194.708883	7103.291617	26.319335
195.254604	7119.514759	26.324352
195.351971	7120.168836	26.329370
195.517732	7121.569901	26.334388
196.064421	7123.028463	26.339405
195.958082	7150.780838	26.344423
195.720111	7150.464314	26.349440
195.856592	7156.526255	26.354458
196.325322	7170.163363	26.359476
196.462709	7180.186989	26.364493
196.740995	7203.598902	26.369511
196.955448	7199.597367	26.374528
197.035354	7220.413705	26.379546
197.261561	7227.771787	26.384564
197.170639	7243.083969	26.389581
197.622845	7256.408030	26.394599
197.562749	7270.386405	26.399616
197.849128	7288.951413	26.404634
198.061710	7284.416644	26.409652
198.357482	7315.853840	26.414669
198.359802	7319.439653	26.419687
198.982811	7335.546778	26.424704
198.774662	7357.718212	26.429722
199.056591	7359.091740	26.434740
199.315592	7374.662081	26.439757
199.596426	7388.278094	26.444775
200.285905	7395.305255	26.449792
200.118540	7405.638470	26.454810
200.211769	7397.889624	26.459828
200.747436	7401.739672	26.464845
201.066125	7424.785695	26.469863
200.920216	7424.720010	26.474880
200.978697	7429.566163	26.479898
201.289702	7445.949255	26.484916
201.764784	7443.059350	26.489933
202.003226	7448.846650	26.494951
202.473201	7437.992748	26.499968
202.723682	7446.654084	26.504986
202.487611	7460.063353	26.510004
202.609519	7464.691286	26.515021
202.705328	7480.659637	26.520039
203.199383	7471.490897	26.525056
203.249216	7487.646353	26.530074
203.497100	7488.027616	26.535092
203.619758	7490.515074	26.540109
203.503646	7500.799325	26.545127
203.838989	7517.071357	26.550144
203.776055	7527.527285	26.555162
204.036252	7542.002143	26.560180
204.398100	7560.669324	26.565197
204.495752	7579.586012	26.570215
204.984579	7582.805699	26.575232
204.844473	7595.941259	26.580250
205.005581	7607.950273	26.585268
204.956534	7631.915642	26.590285
205.252144	7642.309500	26.595303
205.688694	7652.116335	26.600320
205.483741	7673.015417	26.605338
205.857925	7683.914799	26.610356
206.048426	7709.655043	26.615373
206.480917	7719.026891	26.620391
206.677106	7735.532295	26.625408
207.149023	7751.192928	26.630426
207.322554	7767.667162	26.635444
208.320163	7763.650912	26.640461
207.889373	7773.097209	26.645479
208.537885	7781.257922	26.650496
208.280546	7796.972149	26.655514
208.438623	7808.631345	26.660532
208.951811	7813.634106	26.665549
208.968415	7827.585179	26.670567
209.381338	7834.178868	26.675584
209.174047	7843.489382	26.680602
209.329887	7859.410832	26.685620
209.720983	7870.086706	26.690637
209.619152	7882.392548	26.695655
210.128313	7890.533964	26.700672
210.296681	7894.450773	26.705690
210.711794	7911.645194	26.710708
211.100775	7916.929348	26.715725
210.877982	7924.082959	26.720743
211.163148	7941.906932	26.725760
211.326680	7950.149540	26.730778
211.609597	7959.636349	26.735796
212.170204	7975.921072	26.740813
211.995649	7987.351199	26.745831
212.231679	8000.128575	26.750848
212.368917	8011.759575	26.755866
212.544015	8021.471563	26.760884
213.002056	8027.477415	26.765901
212.915521	8041.274230	26.770919
213.419997	8055.383135	26.775936
213.478473	8061.533288	26.780954
213.879928	8069.691553	26.785972
214.036616	8082.427670	26.790989
214.178371	8095.080882	26.796007
214.537814	8101.269429	26.801024
214.361630	8104.614843	26.806042
215.162083	8104.152414	26.811060
215.052762	8098.486850	26.816077
215.305179	8121.922903	26.821095
215.753726	8119.763133	26.826112
215.933914	8127.858006	26.831130
215.846031	8129.374407	26.836148
216.365671	8135.847411	26.841165
216.883479	8157.752091	26.846183
216.806222	8154.487148	26.851200
216.901908	8158.525825	26.856218
217.108501	8181.413457	26.861236
217.659463	8177.659235	26.866253
217.701277	8191.249917	26.871271
217.552923	8191.983330	26.876288
217.552687	8211.806183	26.881306
217.622939	8221.360964	26.886324
218.068160	8232.495859	26.891341
218.133404	8254.205925	26.896359
218.391963	8260.659637	26.901376
218.530610	8272.476846	26.906394
218.632146	8304.820466	26.911412
219.436600	8312.221552	26.916429
219.541633	8333.079433	26.921447
219.532186	8342.870835	26.926464
219.900099	8353.534814	26.931482
219.822958	8360.732215	26.936500
220.503791	8375.356919	26.941517
220.193707	8391.919633	26.946535
220.851353	8409.708167	26.951552
220.991032	8415.615332	26.956570
221.114616	8432.745131	26.961588
221.684030	8439.175765	26.966605
221.639934	8452.590592	26.971623
221.540314	8461.531064	26.976640
221.786768	8480.438138	26.981658
221.914943	8502.293393	26.986676
222.715750	8508.246039	26.991693
223.160073	8516.707220	26.996711
223.783350	8533.942426	27.001728
223.967574	8542.538826	27.006746
224.265061	8554.157848	27.011764
224.293193	8545.484164	27.016781
223.931976	8565.249942	27.021799
224.424431	8572.440829	27.026816
224.493052	8571.997619	27.031834
224.624701	8595.895066	27.036852
224.905957	8589.704453	27.041869
225.025353	8617.142910	27.046887
225.128423	8627.813554	27.051904
225.453026	8644.252424	27.056922
225.620149	8663.733997	27.061940
226.137412	8660.894166	27.066957
226.290258	8683.689762	27.071975
226.223932	8698.989852	27.076992
226.628982	8707.712960	27.082010
226.727400	8731.113778	27.087028
227.174809	8737.702424	27.092045
227.282765	8754.863369	27.097063
227.572109	8770.799548	27.102080
227.783825	8779.186566	27.107098
227.687424	8797.942133	27.112116
228.227599	8797.854868	27.117133
228.655511	8823.332393	27.122151
228.340850	8822.708909	27.127168
228.662384	8833.528771	27.132186
229.112267	8838.601656	27.137204
229.725667	8837.761069	27.142221
230.022370	8855.675685	27.147239
230.420153	8861.192369	27.152256
230.679484	8858.222182	27.157274
230.823796	8865.360044	27.162292
231.317445	8878.539918	27.167309
231.215545	8885.185724	27.172327
230.851245	8881.567545	27.177344
231.321944	8893.582868	27.182362
231.129851	8910.317103	27.187380
231.569049	8919.012895	27.192397
232.085633	8933.609944	27.197415
232.128509	8943.159889	27.202432
232.290873	8956.340881	27.207450
232.147847	8978.914548	27.212468
232.660911	8982.796867	27.217485
232.819219	9004.307054	27.222503
232.826715	9023.643372	27.227520
233.520217	9040.625019	27.232538
233.576373	9062.552135	27.237556
234.023346	9059.988389	27.242573
234.029267	9078.409436	27.247591
234.251519	9087.776829	27.252608
234.809300	9105.572112	27.257626
234.809626	9124.486593	27.262644
235.296140	9137.838249	27.267661
235.594811	9152.261025	27.272679
235.831911	9163.173155	27.277696
236.018939	9160.836139	27.282714
236.219763	9172.843146	27.287732
236.422955	9186.744094	27.292749
236.864452	9202.634858	27.297767
236.788107	9218.069537	27.302784
237.295066	9210.653323	27.307802
237.267494	9228.454613	27.312820
237.419409	9248.636906	27.317837
237.822031	9263.122514	27.322855
237.853173	9280.737911	27.327872
238.371101	9292.679840	27.332890
238.484451	9298.853433	27.337908
238.932012	9317.389077	27.342925
239.043976	9326.120222	27.347943
239.433255	9346.972879	27.352960
239.470510	9348.725630	27.357978
239.400700	9361.785197	27.362996
239.916761	9376.616311	27.368013
240.196166	9395.140326	27.373031
240.278405	9417.752072	27.378048
240.493320	9429.826510	27.383066
240.721210	9444.620455	27.388084
241.539481	9455.600138	27.393101
241.698804	9460.974166	27.398119
242.081977	9472.441509	27.403136
242.476432	9483.809227	27.408154
242.965263	9482.940651	27.413172
243.117326	9489.998617	27.418189
243.530307	9479.512322	27.423207
243.372523	9491.149141	27.428224
243.698176	9500.844783	27.433242
243.569501	9504.113591	27.438260
243.997485	9512.404128	27.443277
244.143569	9531.422620	27.448295
244.399726	9536.547959	27.453312
244.561809	9538.546501	27.458330
244.522895	9562.983222	27.463348
244.887614	9563.658910	27.468365
245.228022	9566.955730	27.473383
245.283516	9591.927150	27.478400
245.566177	9590.048778	27.483418
245.287833	9604.883779	27.488436
245.786890	9618.236987	27.493453
246.281263	9637.109803	27.498471
246.031834	9647.602278	27.503488
246.603504	9658.443669	27.508506
246.542010	9676.904222	27.513524
246.999456	9685.550176	27.518541
246.950912	9704.854885	27.523559
247.207721	9731.149614	27.528576
247.493541	9739.219277	27.533594
247.698117	9763.002685	27.538612
247.769098	9779.895653	27.543629
248.546713	9794.152802	27.548647
248.545989	9814.097420	27.553664
248.969561	9831.876410	27.558682
248.905217	9856.462711	27.563700
249.192411	9876.340469	27.568717
249.885259	9893.253543	27.573735
250.185878	9913.883844	27.578752
250.632159	9926.904504	27.583770
250.223243	9942.050573	27.588788
250.343840	9954.926205	27.593805
251.291159	9979.411996	27.598823
251.424508	9988.822102	27.603840
251.637086	10005.383813	27.608858
251.714395	10023.317929	27.613876
251.976885	10044.254256	27.618893
252.687968	10040.979909	27.623911
253.373337	10076.942415	27.628928
253.446321	10078.493918	27.633946
253.766768	10079.593285	27.638964
254.023418	10095.955620	27.643981
254.106943	10091.617071	27.648999
254.172614	10096.027093	27.654016
254.595487	10112.019414	27.659034
254.889833	10119.320684	27.664052
255.156968	10143.388472	27.669069
255.301666	10136.312452	27.674087
255.235029	10155.209991	27.679104
255.732618	10162.353343	27.684122
255.599111	10179.979439	27.689140
255.685508	10199.639375	27.694157
256.228941	10216.730716	27.699175
256.161777	10240.105541	27.704192
256.932290	10251.734077	27.709210
257.085290	10262.719938	27.714228
257.219178	10272.130103	27.719245
257.574673	10289.377065	27.724263
257.475553	10316.965720	27.729280
258.146660	10322.004574	27.734298
258.300360	10343.147617	27.739316
258.510960	10366.889814	27.744333
258.886647	10381.200519	27.749351
259.007862	10404.407297	27.754368
259.100884	10407.824875	27.759386
259.555232	10422.941127	27.764404
260.057136	10444.800476	27.769421
260.282611	10456.128795	27.774439
260.480274	10469.160126	27.779456
260.699717	10480.786193	27.784474
260.733015	10493.243227	27.789492
261.242945	10515.530814	27.794509
261.761329	10530.971868	27.799527
262.048391	10543.664121	27.804544
262.290713	10544.412579	27.809562
262.522033	10563.099958	27.814580
262.774975	10578.557118	27.819597
263.086713	10567.362931	27.824615
262.977756	10585.092939	27.829632
263.132887	10591.399383	27.834650
263.408055	10609.053823	27.839668
263.637688	10627.053213	27.844685
264.079974	10639.569809	27.849703
264.163771	10657.162524	27.854720
264.642999	10662.130307	27.859738
264.990830	10668.413092	27.864756
265.223885	10678.287951	27.869773
265.652827	10692.464308	27.874791
265.715300	10710.126699	27.879808
266.242141	10718.092958	27.884826
266.487524	10731.559084	27.889844
266.590261	10747.867018	27.894861
266.571800	10758.993533	27.899879
266.826465	10775.511489	27.904896
267.339598	10781.796993	27.909914
267.474892	10811.307497	27.914932
267.464411	10821.668706	27.919949
267.986038	10841.570989	27.924967
268.030723	10856.508249	27.929984
268.756479	10873.650746	27.935002
269.137489	10886.344394	27.940020
269.175348	10896.530772	27.945037
269.405751	10921.135736	27.950055
269.383620	10943.241443	27.955072
269.977889	10964.234505	27.960090
270.124928	10976.680468	27.965108
270.276476	10986.953392	27.970125
270.431240	10997.001641	27.975143
270.571593	11026.884281	27.980160
271.305171	11032.254612	27.985178
271.468686	11059.683491	27.990196
271.269695	11082.003188	27.995213
271.949606	11092.216014	28.000231
272.084460	11120.258840	28.005248
272.026357	11136.844753	28.010266
273.041788	11159.496462	28.015284
273.135069	11185.736607	28.020301
273.626745	11198.807927	28.025319
273.696191	11214.726762	28.030336
273.977643	11227.761365	28.035354
274.346987	11247.975125	28.040372
274.381605	11264.218334	28.045389
274.605304	11274.211794	28.050407
274.887509	11293.447706	28.055424
275.440066	11311.662713	28.060442
276.023202	11333.775690	28.065460
276.184328	11343.734724	28.070477
276.355118	11355.978317	28.075495
276.732004	11378.022415	28.080512
276.811429	11383.829392	28.085530
276.983657	11403.685631	28.090548
277.179094	11435.328572	28.095565
277.956608	11445.965298	28.100583
277.869038	11460.494202	28.105600
278.188397	11474.552440	28.110618
278.741734	11479.458385	28.115636
278.771958	11507.271790	28.120653
279.019491	11507.271134	28.125671
279.492942	11529.432995	28.130688
279.460477	11543.530271	28.135706
280.135492	11550.324463	28.140724
279.841241	11577.187538	28.145741
280.365028	11582.139159	28.150759
280.830119	11604.763417	28.155776
281.022281	11614.076774	28.160794
281.446741	11620.597400	28.165812
281.603182	11641.220483	28.170829
282.052444	11643.079816	28.175847
282.406837	11659.415674	28.180864
282.637536	11671.050203	28.185882
283.069171	11682.489262	28.190900
282.979322	11692.156008	28.195917
283.233956	11709.849419	28.200935
283.582545	11731.377336	28.205952
283.717723	11733.541342	28.210970
284.055350	11739.115617	28.215988
284.288318	11760.127932	28.221005
284.609236	11777.722675	28.226023
285.032049	11802.106227	28.231040
285.083864	11814.349697	28.236058
285.923444	11820.546840	28.241076
286.034569	11832.727408	28.246093
286.422026	11839.017050	28.251111
286.764266	11850.356455	28.256128
286.868984	11868.076513	28.261146
287.641970	11872.654707	28.266164
287.560000	11880.469954	28.271181
287.901156	11885.206953	28.276199
287.926432	11907.514819	28.281216
288.418918	11914.763844	28.286234
288.547386	11936.559931	28.291252
288.601727	11946.962192	28.296269
288.720608	11957.114430	28.301287
288.989990	11984.064006	28.306304
289.835928	12006.042135	28.311322
289.827682	12019.422369	28.316340
290.265630	12039.026349	28.321357
290.225982	12054.217674	28.326375
290.497066	12065.997730	28.331392
291.185006	12085.114450	28.336410
291.580034	12100.253928	28.341428
291.308779	12121.752488	28.346445
291.356028	12139.920665	28.351463
291.649920	12162.155437	28.356480
291.979797	12188.398043	28.361498
292.273541	12212.214894	28.366516
292.195797	12240.251442	28.371533
292.546130	12267.100406	28.376551
293.231024	12285.690471	28.381568
293.374414	12311.463366	28.386586
294.144621	12326.576194	28.391604
294.448363	12353.091502	28.396621
294.655048	12368.269992	28.401639
294.715797	12388.330933	28.406656
294.637636	12401.577068	28.411674
295.302153	12426.694284	28.416692
295.548789	12461.703428	28.421709
296.244194	12476.414361	28.426727
296.126387	12492.335012	28.431744
296.404964	12519.962836	28.436762
297.242175	12539.988313	28.441780
297.381271	12554.880649	28.446797
297.770005	12579.210519	28.451815
298.380244	12595.197902	28.456832
298.408852	12607.634965	28.461850
299.297427	12621.258093	28.466868
299.599941	12640.615377	28.471885
299.323833	12647.826458	28.476903
299.958717	12664.185836	28.481920
299.623582	12676.663785	28.486938
300.332124	12693.595907	28.491956
300.257488	12710.488927	28.496973
300.588766	12724.328361	28.501991
301.281877	12736.602059	28.507008
301.241572	12759.739007	28.512026
301.512043	12768.068151	28.517044
301.744781	12793.436230	28.522061
301.788628	12804.503732	28.527079
302.145460	12829.947275	28.532096
302.052942	12838.942415	28.537114
302.641960	12853.739678	28.542132
303.258787	12886.118379	28.547149
303.507610	12908.642093	28.552167
303.607913	12921.513451	28.557184
303.826400	12946.069242	28.562202
304.518685	12970.507092	28.567220
304.565055	12994.505547	28.572237
304.632252	13020.941783	28.577255
304.652233	13036.936175	28.582272
305.227028	13067.783873	28.587290
306.014684	13082.768282	28.592308
306.482575	13114.475839	28.597325
306.569218	13133.267249	28.602343
307.254029	13152.556068	28.607360
307.580742	13171.483822	28.612378
308.004290	13178.450391	28.617396
308.134631	13191.178311	28.622413
308.798811	13201.656845	28.627431
309.378384	13199.858209	28.632448
309.795900	13219.112922	28.637466
309.968825	13223.083831	28.642484
310.169876	13233.085019	28.647501
310.502910	13250.938199	28.652519
310.889843	13246.393795	28.657536
310.762771	13271.622747	28.662554
310.833721	13283.279988	28.667572
311.353768	13302.518823	28.672589
311.918556	13310.401338	28.677607
311.956028	13326.731145	28.682624
311.658845	13351.658269	28.687642
312.582890	13362.529065	28.692660
312.811629	13393.784854	28.697677
312.771950	13405.819392	28.702695
313.128096	13433.963845	28.707712
313.139181	13457.478909	28.712730
313.992880	13479.994398	28.717748
314.462550	13488.921270	28.722765
315.113788	13502.641989	28.727783
315.582472	13515.045874	28.732800
315.812398	13538.369073	28.737818
315.855862	13547.425484	28.742836
315.881662	13568.481544	28.747853
316.156561	13579.554582	28.752871
316.992678	13598.093982	28.757888
316.725764	13609.339811	28.762906
316.884487	13626.532058	28.767924
317.592940	13655.544104	28.772941
317.607734	13680.419933	28.777959
318.087162	13694.034906	28.782976
318.049764	13718.202059	28.787994
318.452728	13733.208983	28.793012
318.695084	13753.941005	28.798029
319.119439	13785.028036	28.803047
319.624465	13805.460268	28.808064
319.794818	13827.864661	28.813082
320.042538	13848.359104	28.818100
320.470386	13879.745753	28.823117
321.043679	13894.003114	28.828135
321.370462	13910.057850	28.833152
321.052603	13935.424759	28.838170
321.076360	13946.442371	28.843188
321.772817	13982.998027	28.848205
322.193605	13991.054830	28.853223
322.517686	14024.718987	28.858240
322.627913	14048.370932	28.863258
322.897373	14065.420017	28.868276
323.625769	14078.352277	28.873293
323.730878	14104.323056	28.878311
324.397365	14131.273877	28.883328
324.451207	14149.117685	28.888346
324.756472	14162.842220	28.893364
325.502404	14181.601505	28.898381
325.314125	14209.146581	28.903399
326.092906	14221.928985	28.908416
326.385959	14244.886369	28.913434
326.554912	14266.678842	28.918452
326.966509	14283.292293	28.923469
327.055123	14305.441543	28.928487
327.370167	14332.365256	28.933504
327.559711	14365.634103	28.938522
327.704873	14380.640621	28.943540
328.480697	14423.545073	28.948557
328.698292	14432.821126	28.953575
329.187450	14457.857817	28.958592
329.435436	14481.700444	28.963610
329.919833	14505.130485	28.968628
330.604197	14524.414460	28.973645
330.591472	14545.038629	28.978663
331.182569	14563.563436	28.983680
331.194008	14590.016857	28.988698
331.439206	14609.164014	28.993716
331.554134	14632.844377	28.998733
332.410352	14650.705852	29.003751
333.686128	14661.491061	29.008768
333.641691	14667.409918	29.013786
333.802298	14674.654834	29.018804
334.469619	14686.096925	29.023821
334.384146	14706.015707	29.028839
335.294738	14706.556082	29.033856
334.807329	14731.486206	29.038874
335.444633	14744.531006	29.043892
335.659522	14759.877519	29.048909
335.686649	14787.490954	29.053927
336.292305	14788.274609	29.058944
336.731245	14824.524587	29.063962
336.911465	14837.716407	29.068980
337.493121	14851.189974	29.073997
337.714085	14876.010004	29.079015
338.118348	14887.862673	29.084032
338.583670	14903.893525	29.089050
338.847593	14926.069892	29.094068
339.329430	14939.259040	29.099085
339.319771	14958.888366	29.104103
339.557981	14965.489684	29.109120
339.825259	14987.381368	29.114138
340.204218	15013.459186	29.119156
340.921735	15027.732847	29.124173
340.761645	15046.823532	29.129191
341.336048	15056.843354	29.134208
341.486302	15086.522438	29.139226
342.019417	15102.059704	29.144244
342.537422	15115.925507	29.149261
342.377574	15138.594449	29.154279
343.030352	15159.276741	29.159296
343.389068	15178.331002	29.164314
343.281433	15188.194947	29.169332
343.747438	15209.736972	29.174349
343.977816	15227.304810	29.179367
344.544307	15245.035094	29.184384
344.763810	15267.228249	29.189402
344.985602	15288.912604	29.194420
345.559012	15313.362514	29.199437
345.807754	15334.237384	29.204455
345.806633	15356.913455	29.209472
346.127918	15374.205145	29.214490
346.142397	15402.500454	29.219508
346.917684	15428.867701	29.224525
347.418890	15458.161112	29.229543
348.232240	15467.496515	29.234560
348.318281	15489.461207	29.239578
348.678245	15511.607513	29.244596
349.474664	15523.560596	29.249613
349.312286	15548.709631	29.254631
349.975009	15554.044933	29.259648
350.189475	15574.767491	29.264666
350.255658	15598.987226	29.269684
350.985842	15616.048089	29.274701
351.398163	15626.614557	29.279719
351.639916	15646.925531	29.284736
351.682723	15677.010725	29.289754
351.964472	15701.891847	29.294772
352.720957	15727.163359	29.299789
352.660865	15737.193890	29.304807
353.256526	15769.852422	29.309824
353.524876	15785.785193	29.314842
353.731715	15826.479006	29.319860
353.866789	15841.153467	29.324877
354.308477	15867.497458	29.329895
354.388545	15905.482412	29.334912
355.088448	15927.263605	29.339930
355.060706	15963.149396	29.344948
355.852726	15985.238462	29.349965
356.410620	16007.604035	29.354983
356.702386	16039.012271	29.360000
357.172172	16062.266480	29.365018
357.630565	16077.693000	29.370036
357.652000	16100.859140	29.375053
357.882440	16122.833661	29.380071
358.499820	16148.695887	29.385088
358.768659	16171.801487	29.390106
359.498717	16184.472786	29.395124
360.570081	16204.535178	29.400141
360.674970	16216.220514	29.405159
361.254573	16232.875838	29.410176
361.327510	16243.596552	29.415194
361.883895	16260.877710	29.420212
362.125466	16271.948030	29.425229
361.806925	16294.696737	29.430247
362.381095	16316.444257	29.435264
362.925275	16338.231213	29.440282
362.693441	16365.255568	29.445300
363.309324	16385.581723	29.450317
363.240573	16413.566170	29.455335
363.555379	16436.810218	29.460352
363.806130	16471.058619	29.465370
364.354929	16494.749543	29.470388
365.137037	16520.043382	29.475405
365.260121	16553.575898	29.480423
366.075353	16568.293472	29.485440
366.596204	16587.090175	29.490458
366.591382	16604.111588	29.495476
367.066398	16627.874174	29.500493
367.436743	16649.669597	29.505511
367.619576	16671.825871	29.510528
368.011822	16700.133768	29.515546
368.446944	16720.409459	29.520564
368.873814	16734.495926	29.525581
368.975802	16765.050535	29.530599
369.078264	16779.244392	29.535616
369.747853	16805.885830	29.540634
369.645545	16837.609399	29.545652
370.522493	16849.683435	29.550669
370.423934	16885.468269	29.555687
370.836895	16910.254730	29.560704
370.954152	16940.892519	29.565722
371.658429	16972.032761	29.570740
372.115428	16980.685306	29.575757
372.187245	17019.134884	29.580775
372.776554	17044.282556	29.585792
372.852905	17076.875714	29.590810
373.085187	17107.195804	29.595828
373.686317	17135.898220	29.600845
374.023093	17164.695529	29.605863
374.641550	17200.716756	29.610880
375.270038	17221.815670	29.615898
375.702436	17248.001919	29.620916
376.330931	17270.380085	29.625933
376.613808	17307.426580	29.630951
377.050127	17321.922616	29.635968
377.439927	17340.604643	29.640986
377.639897	17366.403995	29.646004
378.636481	17385.503283	29.651021
378.824969	17409.646247	29.656039
379.149558	17424.513512	29.661056
379.844363	17449.610547	29.666074
379.265526	17474.965910	29.671092
380.422686	17497.091474	29.676109
380.590658	17508.101318	29.681127
381.156429	17534.131375	29.686144
381.248102	17566.062835	29.691162
381.475407	17589.230301	29.696180
381.881397	17604.454584	29.701197
382.089570	17633.342103	29.706215
382.576950	17664.359305	29.711232
383.205552	17679.504771	29.716250
383.306414	17719.824264	29.721268
383.740333	17737.223735	29.726285
384.232510	17762.295868	29.731303
384.399408	17787.879831	29.736320
384.793610	17816.416484	29.741338
385.478284	17841.048132	29.746356
386.618276	17857.118564	29.751373
386.966056	17874.019873	29.756391
387.531555	17892.068626	29.761408
387.636366	17908.224453	29.766426
387.609322	17925.367360	29.771444
388.373344	17933.069170	29.776461
388.911489	17961.084566	29.781479
389.174191	17973.002249	29.786496
389.410865	17981.518981	29.791514
389.539678	18018.189679	29.796532
389.930368	18037.712442	29.801549
390.277987	18057.305103	29.806567
390.298936	18085.736014	29.811584
390.799594	18111.009434	29.816602
390.724465	18131.394475	29.821620
391.442276	18160.026555	29.826637
391.753042	18180.958036	29.831655
392.108203	18212.021970	29.836672
392.738611	18236.251944	29.841690
392.594896	18279.251334	29.846708
393.211107	18305.113486	29.851725
393.217120	18333.869272	29.856743
394.273626	18361.122270	29.861760
394.957288	18374.787758	29.866778
394.999274	18403.114781	29.871796
395.281850	18424.335197	29.876813
395.637948	18446.902437	29.881831
395.593426	18472.021141	29.886848
396.532008	18493.828106	29.891866
396.776295	18525.250945	29.896884
396.930280	18545.209071	29.901901
397.427280	18576.763222	29.906919
397.620796	18611.232807	29.911936
398.492354	18649.766438	29.916954
398.518558	18679.682012	29.921972
398.941094	18704.715669	29.926989
399.439025	18742.770664	29.932007
399.889635	18774.187056	29.937024
399.988769	18791.645914	29.942042
400.537600	18828.334882	29.947060
400.780872	18864.155442	29.952077
401.227011	18895.528504	29.957095
401.404171	18925.244061	29.962112
402.442259	18956.878851	29.967130
402.874062	18990.806605	29.972148
403.430059	19019.604135	29.977165
403.462038	19050.606009	29.982183
403.855231	19079.315256	29.987200
404.679613	19115.469093	29.992218
404.918087	19142.054522	29.997236
405.360277	19168.709354	30.002253
405.922211	19195.926807	30.007271
406.053728	19227.431515	30.012288
406.822587	19253.448063	30.017306
406.915546	19280.909223	30.022324
407.813291	19310.626906	30.027341
408.259982	19331.506880	30.032359
408.477089	19361.646489	30.037376
409.147904	19374.341756	30.042394
409.420843	19409.312127	30.047412
410.194660	19425.870484	30.052429
410.866577	19448.149646	30.057447
410.639640	19467.839498	30.062464
411.127831	19490.962303	30.067482
411.682755	19510.821095	30.072500
411.822373	19540.050650	30.077517
412.328665	19563.808819	30.082535
412.365021	19592.056317	30.087552
412.898314	19623.277993	30.092570
412.942333	19655.473020	30.097588
413.828447	19684.953010	30.102605
414.159694	19711.253106	30.107623
413.964639	19744.907012	30.112640
414.839496	19774.211991	30.117658
415.142248	19808.679325	30.122676
415.121186	19843.620430	30.127693
415.848027	19881.793645	30.132711
416.062400	19916.135935	30.137728
416.583089	19953.741184	30.142746
417.153831	19984.824932	30.147764
417.438927	20019.920863	30.152781
418.009622	20049.178838	30.157799
418.385583	20082.005228	30.162816
418.833856	20118.402702	30.167834
419.340344	20144.808778	30.172852
419.443549	20177.917875	30.177869
419.942929	20210.617861	30.182887
420.417763	20242.942643	30.187904
420.972446	20269.979503	30.192922
421.240664	20304.149823	30.197940
421.894922	20327.563669	30.202957
422.661043	20353.190396	30.207975
422.740010	20381.457673	30.212992
423.260796	20410.553372	30.218010
423.403171	20434.716750	30.223028
424.275747	20466.531399	30.228045
424.408570	20486.027268	30.233063
424.567636	20520.284457	30.238080
425.022176	20540.539011	30.243098
425.148839	20578.352120	30.248116
425.784166	20612.244692	30.253133
426.295975	20639.181330	30.258151
426.234704	20689.862365	30.263168
427.234705	20702.216618	30.268186
428.426337	20733.091170	30.273204
428.876703	20753.359231	30.278221
429.873516	20775.115469	30.283239
429.870320	20800.881506	30.288256
430.095922	20820.293764	30.293274
430.919400	20839.429736	30.298292
431.161100	20864.772321	30.303309
431.503343	20881.993018	30.308327
431.728431	20911.647272	30.313344
432.268093	20928.957323	30.318362
432.505051	20958.647709	30.323380
432.571817	20980.270963	30.328397
433.071080	21011.133696	30.333415
433.247088	21052.857356	30.338432
433.869699	21071.114995	30.343450
434.473590	21106.043194	30.348468
434.369581	21142.395867	30.353485
435.051734	21180.787078	30.358503
435.448413	21206.516668	30.363520
436.532607	21232.202442	30.368538
437.537166	21247.330078	30.373556
437.533655	21266.013927	30.378573
438.358732	21286.514849	30.383591
438.869275	21318.835847	30.388608
439.360860	21329.108774	30.393626
439.766430	21357.421385	30.398644
439.883173	21382.114345	30.403661
440.193166	21406.467650	30.408679
440.063159	21439.766823	30.413696
440.653158	21461.612432	30.418714
440.754576	21493.826814	30.423732
441.542590	21534.293630	30.428749
441.897256	21551.980545	30.433767
442.544451	21591.805967	30.438784
442.496498	21621.415340	30.443802
442.718299	21646.534568	30.448820
443.459546	21692.739833	30.453837
443.769211	21729.540984	30.458855
444.251611	21760.350653	30.463872
444.797507	21790.967249	30.468890
445.457104	21827.000114	30.473908
446.101089	21856.994964	30.478925
447.061393	21889.196333	30.483943
447.142188	21915.115034	30.488960
447.340477	21934.153531	30.493978
448.010942	21967.316340	30.498996
448.510551	22005.497475	30.504013
449.302491	22029.397407	30.509031
449.192057	22063.806655	30.514048
449.712646	22084.020928	30.519066
450.628608	22106.846440	30.524084
450.615063	22147.957430	30.529101
451.072105	22165.262478	30.534119
451.534238	22189.308728	30.539136
451.542130	22225.456416	30.544154
451.875823	22242.502714	30.549172
452.339860	22275.597080	30.554189
453.191091	22306.034249	30.559207
453.087887	22340.973622	30.564224
453.400255	22371.545332	30.569242
453.967998	22402.431180	30.574260
454.010836	22446.010941	30.579277
454.951803	22474.987416	30.584295
455.002906	22508.677230	30.589312
455.190821	22547.836792	30.594330
456.038294	22589.674006	30.599348
456.693564	22632.084644	30.604365
457.710656	22657.277229	30.609383
457.769872	22707.085334	30.614400
458.229919	22742.620158	30.619418
458.882919	22770.738309	30.624436
458.811469	22807.708219	30.629453
459.687507	22840.214927	30.634471
460.271421	22872.640789	30.639488
460.506539	22905.228424	30.644506
461.268357	22943.421102	30.649524
461.642187	22974.477046	30.654541
462.204107	22985.144298	30.659559
462.794708	23023.275320	30.664576
463.649911	23044.152520	30.669594
464.612768	23074.643005	30.674612
464.426966	23111.542819	30.679629
464.920099	23133.632843	30.684647
465.068768	23168.837771	30.689664
465.538190	23202.368855	30.694682
466.180579	23228.410372	30.699700
466.478693	23256.477039	30.704717
466.777845	23298.318966	30.709735
467.045398	23333.101262	30.714752
467.613500	23370.636150	30.719770
468.363914	23413.273771	30.724788
468.448180	23454.764021	30.729805
469.201558	23476.270475	30.734823
469.655208	23515.017753	30.739840
470.308082	23544.110155	30.744858
470.322893	23585.276579	30.749876
470.973516	23625.946003	30.754893
471.687516	23663.679899	30.759911
471.788043	23692.359298	30.764928
472.369336	23730.960743	30.769946
472.974264	23770.278964	30.774964
472.835926	23802.420679	30.779981
473.492533	23843.993255	30.784999
473.980604	23894.034570	30.790016
474.642724	23925.660080	30.795034
475.364326	23955.930393	30.800052
475.543495	24003.416564	30.805069
476.238351	24036.629595	30.810087
476.451797	24072.331573	30.815104
477.157171	24117.505409	30.820122
478.014080	24147.312601	30.825140
478.208857	24187.795049	30.830157
478.702854	24223.655838	30.835175
479.587412	24264.372298	30.840192
480.161050	24292.839883	30.845210
480.741128	24312.073997	30.850228
481.156789	24343.523684	30.855245
482.021427	24378.688801	30.860263
482.037274	24401.290571	30.865280
481.955520	24434.220730	30.870298
482.928895	24462.929656	30.875316
482.970320	24493.932291	30.880333
483.498232	24515.544485	30.885351
483.947238	24547.368464	30.890368
484.114147	24588.544874	30.895386
484.724767	24619.983603	30.900404
484.793950	24646.027741	30.905421
485.753968	24690.341708	30.910439
485.847995	24732.894757	30.915456
486.025008	24772.717613	30.920474
486.712160	24805.351735	30.925492
487.000369	24854.794625	30.930509
487.810018	24902.304849	30.935527
488.247071	24945.203075	30.940544
488.696246	24983.783274	30.945562
489.179643	25025.903477	30.950580
489.471789	25077.122091	30.955597
489.861247	25116.887280	30.960615
490.906376	25139.923685	30.965632
491.454859	25177.212244	30.970650
492.378245	25215.162942	30.975668
492.701955	25250.609712	30.980685
493.365320	25290.376841	30.985703
494.455391	25320.832007	30.990720
494.883893	25350.657134	30.995738
495.405031	25373.459402	31.000756
495.689137	25402.858392	31.005773
496.483702	25422.338250	31.010791
496.701868	25464.930403	31.015808
496.917752	25499.876187	31.020826
497.661742	25520.678508	31.025844
498.034577	25551.732300	31.030861
498.638632	25588.254609	31.035879
499.095720	25619.415464	31.040896
499.237117	25643.300950	31.045914
500.051375	25677.199610	31.050932
500.306423	25722.308141	31.055949
500.857511	25759.154994	31.060967
501.175682	25798.212177	31.065984
501.691751	25841.258013	31.071002
501.930883	25877.711263	31.076020
502.288267	25920.187909	31.081037
503.028150	25952.461781	31.086055
503.436853	25994.285972	31.091072
504.221547	26042.358927	31.096090
504.973716	26083.497849	31.101108
505.200565	26123.530499	31.106125
505.717264	26171.765561	31.111143
506.407865	26198.290080	31.116160
506.762765	26243.611750	31.121178
507.801056	26274.512501	31.126196
508.048634	26315.945329	31.131213
508.399096	26363.934974	31.136231
508.893714	26397.214694	31.141248
509.457486	26434.029208	31.146266
510.216234	26470.408957	31.151284
510.274755	26511.157459	31.156301
510.966302	26539.894280	31.161319
512.218167	26577.354016	31.166336
512.392507	26596.223729	31.171354
513.306064	26616.760628	31.176372
514.023797	26644.570798	31.181389
514.684030	26659.901547	31.186407
515.213831	26676.630383	31.191424
515.693142	26704.136469	31.196442
516.455436	26737.975487	31.201460
516.722613	26751.161792	31.206477
517.104655	26780.162021	31.211495
517.698044	26814.785872	31.216512
517.533613	26841.419066	31.221530
517.861365	26855.373381	31.226548
518.236900	26893.324057	31.231565
518.311703	26926.796408	31.236583
519.013373	26962.130469	31.241600
518.953605	27009.130046	31.246618
519.538414	27044.210676	31.251636
520.236086	27082.408604	31.256653
520.293817	27129.459690	31.261671
521.017445	27173.815936	31.266688
521.472901	27209.852380	31.271706
522.709772	27241.229319	31.276724
523.424605	27274.697411	31.281741
523.931951	27326.956357	31.286759
524.479360	27353.947106	31.291776
524.741514	27403.128531	31.296794
525.510524	27429.395973	31.301812
525.446552	27467.871205	31.306829
526.133498	27520.709440	31.311847
526.706648	27551.299022	31.316864
527.168277	27601.587532	31.321882
527.704669	27637.561575	31.326900
528.299913	27671.756819	31.331917
528.792053	27719.101904	31.336935
529.873880	27751.458148	31.341952
530.040772	27791.686722	31.346970
530.475779	27836.310563	31.351988
531.518807	27881.143228	31.357005
531.514361	27923.560320	31.362023
532.765488	27959.341500	31.367040
532.842668	28010.145943	31.372058
533.057937	28050.911058	31.377076
533.407643	28087.869352	31.382093
533.880444	28147.347465	31.387111
534.231862	28182.384230	31.392128
534.886401	28237.744940	31.397146
535.626587	28280.388162	31.402164
536.248465	28327.581734	31.407181
536.514032	28381.543338	31.412199
536.726659	28426.101961	31.417216
537.520826	28483.154481	31.422234
537.795576	28532.254505	31.427252
538.369571	28579.013669	31.432269
539.031662	28633.230240	31.437287
539.941659	28676.144926	31.442304
540.892805	28715.204000	31.447322
541.843764	28746.286463	31.452340
542.338019	28782.616728	31.457357
542.744496	28826.501335	31.462375
543.353835	28860.462516	31.467392
543.822309	28918.148462	31.472410
544.757761	28942.988745	31.477428
545.480456	28983.404935	31.482445
545.629885	29024.517243	31.487463
545.974333	29058.753859	31.492480
546.812071	29095.176586	31.497498
547.443035	29135.417733	31.502516
547.728044	29172.602970	31.507533
548.236843	29216.308144	31.512551
548.670862	29254.209870	31.517568
548.791154	29301.098205	31.522586
549.533243	29335.545178	31.527604
549.888360	29376.531359	31.532621
550.229793	29426.457504	31.537639
550.604528	29469.785872	31.542656
550.989725	29532.694947	31.547674
551.629420	29588.933916	31.552692
552.385846	29618.303410	31.557709
552.916747	29685.121907	31.562727
553.696769	29717.028904	31.567744
554.255435	29755.114423	31.572762
554.486184	29805.905737	31.577780
555.102713	29852.566373	31.582797
555.453313	29892.536601	31.587815
556.332688	29938.138826	31.592832
556.768245	29987.147770	31.597850
557.436866	30022.865229	31.602868
558.366904	30067.884636	31.607885
558.627356	30117.572224	31.612903
559.231441	30156.789218	31.617920
559.872455	30202.732551	31.622938
560.546262	30240.959075	31.627956
560.605316	30284.540581	31.632973
561.247758	30345.212330	31.637991
562.208980	30375.695161	31.643008
562.674952	30437.412365	31.648026
563.605505	30482.312497	31.653044
563.926037	30525.872770	31.658061
564.285668	30579.319811	31.663079
564.983379	30626.993610	31.668096
565.723077	30672.353714	31.673114
566.183509	30712.592893	31.678132
566.552034	30754.047506	31.683149
566.895931	30806.182752	31.688167
567.397402	30853.723270	31.693184
568.161043	30905.224501	31.698202
568.760006	30962.036163	31.703220
569.187175	30998.090007	31.708237
569.496121	31070.415546	31.713255
570.343494	31111.998618	31.718272
570.806897	31177.182569	31.723290
571.335230	31225.029510	31.728308
572.488992	31276.256004	31.733325
572.686172	31332.935267	31.738343
573.401998	31380.664878	31.743360
573.850420	31430.389576	31.748378
574.335320	31488.604852	31.753396
575.042830	31543.763936	31.758413
575.193474	31594.287648	31.763431
575.719370	31655.392287	31.768448
577.017166	31700.022962	31.773466
577.261072	31764.427444	31.778484
578.144711	31804.495396	31.783501
578.530441	31869.459715	31.788519
579.436322	31914.139220	31.793536
580.130985	31958.807451	31.798554
580.513621	32010.465570	31.803572
581.408439	32047.282901	31.808589
581.460522	32110.182143	31.813607
582.291686	32156.858823	31.818624
583.062682	32202.350164	31.823642
583.494924	32257.048255	31.828660
584.071129	32293.245516	31.833677
584.700740	32355.954445	31.838695
585.901245	32389.096084	31.843712
586.523717	32443.588042	31.848730
587.481969	32479.201440	31.853748
587.871392	32520.959780	31.858765
588.256262	32559.393614	31.863783
588.837014	32593.814248	31.868800
589.651669	32636.707777	31.873818
590.043044	32677.144853	31.878836
590.590120	32712.266334	31.883853
590.975912	32760.442452	31.888871
591.695654	32798.767700	31.893888
592.118900	32835.489148	31.898906
592.326265	32874.204073	31.903924
593.064808	32925.094673	31.908941
593.915867	32956.736414	31.913959
594.658592	32993.275644	31.918976
595.212322	33027.979370	31.923994
595.229936	33071.301328	31.929012
596.072305	33104.695845	31.934029
596.431433	33154.565003	31.939047
597.161058	33196.101038	31.944064
598.053540	33237.535938	31.949082
598.357943	33283.254006	31.954100
599.001214	33326.460127	31.959117
599.337993	33380.524850	31.964135
599.932032	33422.095085	31.969152
600.098774	33473.480651	31.974170
600.755069	33529.449557	31.979188
601.317220	33583.144643	31.984205
601.836091	33641.303744	31.989223
602.421044	33675.554809	31.994240
603.214989	33736.623818	31.999258
603.836206	33798.889507	32.004276
604.450204	33855.877426	32.009293
605.150493	33911.992238	32.014311
605.818039	33969.503200	32.019328
606.934987	34018.257520	32.024346
607.018303	34065.446872	32.029364
607.899370	34103.009685	32.034381
608.618685	34166.759585	32.039399
609.089066	34206.182062	32.044416
609.518460	34266.272497	32.049434
610.058331	34316.350208	32.054452
610.678895	34375.254197	32.059469
611.396381	34414.815625	32.064487
611.879804	34483.047865	32.069504
612.337240	34528.441343	32.074522
613.201381	34602.266974	32.079540
614.258889	34634.934968	32.084557
614.854316	34703.624673	32.089575
615.039829	34754.586838	32.094592
615.974497	34808.505254	32.099610
616.329381	34865.226440	32.104628
616.972984	34917.970195	32.109645
617.454776	34974.273596	32.114663
618.202850	35033.532608	32.119680
619.338778	35081.780632	32.124698
619.704796	35133.398453	32.129716
620.344054	35192.067877	32.134733
620.898364	35237.985226	32.139751
621.572613	35286.065327	32.144768
622.142601	35345.441454	32.149786
622.764403	35392.948275	32.154804
623.499335	35442.517768	32.159821
623.877528	35508.392357	32.164839
624.759970	35550.870314	32.169856
625.546259	35596.145343	32.174874
626.570495	35648.117193	32.179892
627.069236	35694.587943	32.184909
627.892098	35741.343448	32.189927
628.481300	35777.980971	32.194944
629.746089	35818.180633	32.199962
629.738395	35857.250664	32.204980
630.509980	35895.099277	32.209997
631.219559	35941.196312	32.215015
631.492681	35986.558385	32.220032
632.113329	36024.215747	32.225050
632.829054	36080.757559	32.230068
633.283387	36120.672972	32.235085
633.803188	36174.583581	32.240103
634.176459	36218.830367	32.245120
634.699592	36254.935226	32.250138
635.063689	36310.672465	32.255156
635.583310	36350.375810	32.260173
636.628324	36395.207598	32.265191
637.324040	36440.346778	32.270208
637.790615	36488.816026	32.275226
638.212578	36534.535480	32.280244
639.075814	36586.831878	32.285261
639.569230	36639.944745	32.290279
640.058701	36697.522465	32.295296
640.710580	36747.601137	32.300314
641.472472	36805.573035	32.305332
641.870920	36859.959537	32.310349
642.572444	36905.743761	32.315367
643.167014	36970.545875	32.320384
643.805225	37028.259412	32.325402
644.555893	37093.910202	32.330420
645.162523	37150.471837	32.335437
646.039587	37200.263589	32.340455
646.601842	37254.031209	32.345472
647.503829	37309.737910	32.350490
648.261290	37366.548538	32.355508
649.130317	37419.579580	32.360525
649.852420	37457.495586	32.365543
650.628366	37511.875568	32.370560
651.417255	37556.673793	32.375578
652.141901	37611.820817	32.380596
652.724841	37654.703711	32.385613
653.409704	37701.086632	32.390631
653.688786	37750.681879	32.395648
654.467888	37789.778402	32.400666
654.521246	37855.552729	32.405684
655.201868	37908.500489	32.410701
656.234070	37970.815624	32.415719
656.492635	38027.572878	32.420736
657.544717	38077.801041	32.425754
658.518873	38132.297183	32.430772
659.215533	38178.287242	32.435789
659.995952	38230.233790	32.440807
660.224234	38276.594179	32.445824
661.038115	38334.960513	32.450842
661.802028	38381.123920	32.455860
662.699249	38433.002188	32.460877
663.048961	38490.821489	32.465895
663.643593	38536.764962	32.470912
664.631110	38579.827022	32.475930
665.402321	38636.297398	32.480948
665.787598	38683.468948	32.485965
666.678324	38733.793326	32.490983
666.768061	38799.299278	32.496000
667.574078	38841.713480	32.501018
667.863996	38909.566326	32.506036
668.559560	38971.114679	32.511053
669.581897	39030.791088	32.516071
670.110109	39087.173998	32.521088
670.626864	39132.378331	32.526106
671.279151	39193.010777	32.531124
672.132374	39242.912162	32.536141
673.367615	39290.262592	32.541159
673.946437	39350.951185	32.546176
674.698623	39402.234625	32.551194
675.307320	39455.292246	32.556212
675.854033	39511.591172	32.561229
676.684961	39555.514318	32.566247
676.878560	39618.103894	32.571264
677.491852	39666.917945	32.576282
678.309703	39712.778581	32.581300
678.562195	39761.592096	32.586317
679.426125	39813.308119	32.591335
679.978353	39874.470296	32.596352
680.283716	39920.480716	32.601370
680.632051	39990.990281	32.606388
681.387180	40045.019430	32.611405
682.443884	40111.163007	32.616423
682.957146	40168.354220	32.621440
683.914119	40221.884403	32.626458
684.347323	40281.580085	32.631476
684.800630	40346.964552	32.636493
685.913149	40401.451210	32.641511
686.220181	40476.528517	32.646528
686.940235	40535.130422	32.651546
687.682272	40607.889041	32.656564
688.276349	40667.541766	32.661581
689.005518	40731.948455	32.666599
689.488175	40805.140215	32.671616
690.701603	40863.103337	32.676634
691.766070	40917.687310	32.681652
692.661229	40979.343103	32.686669
693.902207	41027.069575	32.691687
694.434575	41081.717818	32.696704
695.098244	41119.541843	32.701722
695.954913	41183.360823	32.706740
696.712229	41235.286559	32.711757
697.630928	41284.651195	32.716775
697.903449	41334.641464	32.721792
698.947959	41377.320752	32.726810
699.446971	41437.584881	32.731828
699.816511	41480.344145	32.736845
700.451854	41531.536958	32.741863
701.352377	41589.196549	32.746880
701.957539	41654.434804	32.751898
702.562710	41709.579248	32.756916
703.166670	41775.943825	32.761933
704.048304	41830.014628	32.766951
704.609519	41900.377057	32.771968
705.046250	41952.904644	32.776986
705.375559	42015.024598	32.782004
705.992075	42084.392363	32.787021
707.245550	42148.911348	32.792039
707.249484	42212.562490	32.797056
708.519416	42271.855068	32.802074
709.797731	42325.549106	32.807092
710.473519	42391.366759	32.812109
710.982785	42459.285059	32.817127
711.728448	42526.274972	32.822144
712.133330	42578.619269	32.827162
712.956704	42643.124439	32.832180
713.441764	42710.566595	32.837197
714.569113	42768.554492	32.842215
714.841724	42833.430575	32.847232
715.659068	42898.867191	32.852250
716.067362	42972.931625	32.857268
716.688775	43043.946132	32.862285
717.998080	43102.482154	32.867303
718.503924	43168.708082	32.872320
719.582502	43233.997501	32.877338
720.409410	43294.076526	32.882356
720.676782	43352.718484	32.887373
721.771943	43416.399303	32.892391
722.419990	43483.091066	32.897408
723.164342	43545.504927	32.902426
723.981115	43609.583844	32.907444
724.893143	43670.846088	32.912461
725.825928	43721.061575	32.917479
726.180245	43781.506449	32.922496
727.106968	43830.989411	32.927514
727.668932	43876.835357	32.932532
728.043497	43933.684790	32.937549
728.639366	43987.014724	32.942567
729.399919	44050.110609	32.947584
730.476349	44095.155844	32.952602
731.295972	44151.240776	32.957620
731.684952	44205.874820	32.962637
732.475491	44273.805511	32.967655
733.192705	44328.369785	32.972672
733.826414	44383.491170	32.977690
734.574147	44456.609527	32.982708
734.906483	44514.504377	32.987725
735.897636	44565.851257	32.992743
737.146235	44622.079337	32.997760
737.935969	44688.233983	33.002778
738.890263	44745.330493	33.007796
739.165359	44807.675468	33.012813
740.034735	44860.218519	33.017831
740.563457	44924.788855	33.022848
741.168724	44984.717198	33.027866
742.003673	45045.641006	33.032884
742.554935	45108.905311	33.037901
743.331610	45173.766697	33.042919
744.046197	45254.907309	33.047936
744.603080	45320.885010	33.052954
745.591578	45389.016007	33.057972
745.752965	45458.699235	33.062989
747.019830	45533.018086	33.068007
747.498751	45604.771432	33.073024
748.497829	45674.084551	33.078042
749.022074	45752.163333	33.083060
749.455379	45825.917088	33.088077
750.728752	45902.930919	33.093095
751.371531	45974.786456	33.098112
752.223058	46043.193797	33.103130
753.109958	46111.013866	33.108148
753.812869	46193.057959	33.113165
754.726457	46257.717723	33.118183
755.503245	46325.675772	33.123200
756.211639	46399.989548	33.128218
757.160182	46467.491128	33.133236
757.414743	46549.081263	33.138253
758.507123	46617.471838	33.143271
759.429559	46679.284756	33.148288
760.085283	46743.979733	33.153306
760.951664	46811.077619	33.158324
761.797138	46884.814966	33.163341
763.244904	46935.666037	33.168359
764.014521	46988.216956	33.173376
765.255435	47045.603669	33.178394
766.449995	47093.590843	33.183412
766.673426	47160.233159	33.188429
767.635491	47202.512650	33.193447
768.349543	47261.101651	33.198464
768.561964	47315.441802	33.203482
769.543669	47372.528085	33.208500
770.149753	47434.234165	33.213517
770.552564	47494.415810	33.218535
771.124500	47554.482721	33.223552
772.057485	47624.931882	33.228570
772.755602	47691.824508	33.233588
773.236672	47762.850546	33.238605
774.291823	47812.126206	33.243623
775.146341	47879.912353	33.248640
775.575537	47965.016820	33.253658
776.834511	48016.475414	33.258676
777.599961	48071.034952	33.263693
778.473374	48126.381265	33.268711
779.648415	48183.964589	33.273728
780.498132	48229.217916	33.278746
780.993517	48278.094594	33.283764
781.471857	48332.313543	33.288781
782.230228	48367.168051	33.293799
783.190316	48423.861784	33.298816
783.309764	48481.376105	33.303834
784.247916	48538.181087	33.308852
784.932925	48608.210069	33.313869
785.714449	48674.890159	33.318887
786.095974	48735.660448	33.323904
786.731521	48818.369857	33.328922
788.035802	48869.911905	33.333940
788.765360	48943.566443	33.338957
789.604904	48998.091366	33.343975
790.186663	49074.679581	33.348992
790.523647	49143.442113	33.354010
791.677120	49212.128366	33.359028
792.221115	49293.019008	33.364045
793.252118	49368.918259	33.369063
794.042095	49448.803172	33.374080
794.320638	49525.459077	33.379098
795.248131	49594.681472	33.384116
795.848228	49678.405469	33.389133
796.975336	49763.838228	33.394151
797.621022	49843.943111	33.399168
798.255399	49925.214180	33.404186
799.244557	50000.755081	33.409204
799.997514	50084.779437	33.414221
800.961865	50168.321981	33.419239
801.362467	50254.521334	33.424256
802.400270	50340.957150	33.429274
803.460646	50417.450037	33.434292
804.446583	50501.635787	33.439309
805.307587	50575.186527	33.444327
806.015343	50651.811009	33.449344
806.734594	50729.484255	33.454362
808.029206	50810.086234	33.459380
808.582256	50896.144041	33.464397
809.691155	50971.372113	33.469415
810.549102	51047.221596	33.474432
811.068714	51119.055603	33.479450
812.262448	51195.890965	33.484468
812.877245	51264.920302	33.489485
813.733209	51346.054325	33.494503
814.521905	51427.395250	33.499520
815.641247	51504.983513	33.504538
816.505816	51580.093418	33.509556
817.118723	51650.358027	33.514573
818.359953	51720.265619	33.519591
819.110894	51796.893501	33.524608
820.092187	51858.344289	33.529626
820.855228	51918.513111	33.534644
821.901332	51988.996046	33.539661
822.824523	52055.512029	33.544679
823.875234	52125.387225	33.549696
824.449481	52182.884287	33.554714
825.446138	52247.143122	33.559732
826.317695	52301.930315	33.564749
827.159796	52364.131776	33.569767
828.117851	52416.343119	33.574784
828.887994	52486.408609	33.579802
829.902659	52540.452744	33.584820
831.082767	52602.716124	33.589837
831.444581	52650.737016	33.594855
832.352958	52709.632393	33.599872
832.990317	52771.018909	33.604890
833.897433	52832.021901	33.609908
834.423601	52878.859715	33.614925
834.837883	52941.717790	33.619943
835.526698	52992.067697	33.624960
836.208238	53059.548012	33.629978
837.069258	53129.500045	33.634996
838.153701	53187.875657	33.640013
838.406162	53256.745838	33.645031
839.124616	53325.967644	33.650048
839.839146	53403.473389	33.655066
840.118790	53485.805627	33.660084
840.929196	53559.582517	33.665101
841.924164	53641.133196	33.670119
842.593126	53724.373835	33.675136
842.939850	53813.353745	33.680154
843.759683	53900.494844	33.685172
844.647001	53984.031467	33.690189
845.708031	54091.897847	33.695207
846.784114	54176.538484	33.700224
847.758417	54271.579612	33.705242
848.617859	54346.085393	33.710260
850.166070	54418.895841	33.715277
850.994622	54508.841184	33.720295
852.155891	54580.718850	33.725312
853.121568	54670.744716	33.730330
853.813529	54738.981286	33.735348
854.804524	54812.303678	33.740365
855.699678	54897.873676	33.745383
856.777126	54966.164805	33.750400
857.156046	55048.335173	33.755418
858.081345	55119.574089	33.760436
859.349200	55203.321585	33.765453
859.935079	55278.132354	33.770471
860.765455	55352.500285	33.775488
861.864779	55432.477817	33.780506
862.325684	55504.821707	33.785524
863.388169	55593.241261	33.790541
864.204300	55675.092606	33.795559
865.763025	55741.728947	33.800576
866.646284	55823.722239	33.805594
867.499807	55890.494087	33.810612
868.278049	55957.144942	33.815629
868.940117	56033.762515	33.820647
869.994547	56114.755572	33.825664
870.479628	56194.173118	33.830682
871.687810	56273.788468	33.835700
872.310965	56346.685565	33.840717
872.977957	56427.651396	33.845735
873.794600	56502.126321	33.850752
874.878576	56596.640755	33.855770
875.522073	56666.656114	33.860788
876.719120	56741.559881	33.865805
877.646500	56829.011449	33.870823
878.397140	56906.731897	33.875840
878.870044	56988.223484	33.880858
880.078368	57070.670438	33.885876
881.084548	57149.111352	33.890893
881.907616	57231.846670	33.895911
882.621968	57302.745228	33.900928
883.803854	57384.020208	33.905946
884.751416	57465.958501	33.910964
885.533276	57537.113058	33.915981
886.477341	57620.052393	33.920999
888.070886	57683.112887	33.926016
889.011284	57758.812937	33.931034
890.239025	57821.880107	33.936052
890.821420	57890.978192	33.941069
891.437618	57962.463590	33.946087
892.204349	58026.147356	33.951104
892.899941	58094.715751	33.956122
893.739011	58156.287349	33.961140
894.230914	58216.609350	33.966157
895.198804	58291.490342	33.971175
896.025196	58356.969497	33.976192
896.572740	58440.416424	33.981210
897.457296	58516.247801	33.986228
897.957879	58593.151861	33.991245
898.620424	58685.778069	33.996263
899.474935	58771.051805	34.001280
900.433999	58872.658084	34.006298
901.384604	58959.417565	34.011316
902.002379	59053.583840	34.016333
902.623653	59141.616797	34.021351
903.949932	59229.356778	34.026368
904.475796	59324.867581	34.031386
905.418369	59428.162375	34.036404
906.457000	59528.290591	34.041421
907.520142	59620.630151	34.046439
908.677152	59712.898485	34.051456
909.556241	59805.792747	34.056474
910.814808	59898.514361	34.061492
911.634233	59996.532911	34.066509
912.489729	60081.678176	34.071527
913.265280	60172.988569	34.076544
914.268693	60271.068197	34.081562
915.467150	60356.964901	34.086580
916.809070	60450.966893	34.091597
917.365791	60549.686845	34.096615
918.537867	60633.417537	34.101632
919.350096	60727.433419	34.106650
920.547417	60821.680888	34.111668
921.643496	60910.576802	34.116685
922.210969	60992.117776	34.121703
923.396224	61076.607512	34.126720
924.324506	61164.448063	34.131738
925.067090	61252.222886	34.136756
926.120505	61340.183846	34.141773
926.747290	61433.250162	34.146791
927.766938	61525.635341	34.151808
928.568082	61610.123405	34.156826
929.889477	61714.875429	34.161844
930.675884	61800.942616	34.166861
931.623678	61891.491982	34.171879
933.084385	61979.208254	34.176896
933.733273	62059.898193	34.181914
935.114913	62150.741793	34.186932
936.000267	62225.780646	34.191949
937.090255	62315.018083	34.196967
938.102156	62395.526007	34.201984
938.682894	62485.856162	34.207002
939.742608	62558.798905	34.212020
941.083240	62634.255556	34.217037
942.158514	62719.052908	34.222055
942.883393	62799.435908	34.227072
944.026872	62881.843011	34.232090
944.817518	62966.856435	34.237108
946.125122	63027.265896	34.242125
946.963406	63110.221364	34.247143
948.544405	63171.911668	34.252160
949.206513	63250.754957	34.257178
949.988893	63315.405955	34.262196
950.839595	63385.585620	34.267213
951.112965	63459.792897	34.272231
952.628815	63530.299904	34.277248
953.365451	63609.158049	34.282266
954.038844	63685.652344	34.287284
955.295335	63755.643277	34.292301
956.151477	63834.318938	34.297319
956.948261	63898.139905	34.302336
957.829190	63970.639832	34.307354
958.472727	64041.163791	34.312372
958.901450	64113.943435	34.317389
959.815075	64209.982571	34.322407
960.732310	64280.768472	34.327424
961.320518	64381.220750	34.332442
962.605572	64465.054452	34.337460
963.449845	64558.946949	34.342477
964.458792	64652.953441	34.347495
965.340196	64738.750121	34.352512
966.294167	64829.328217	34.357530
967.229127	64913.268562	34.362548
968.613691	65005.635200	34.367565
969.206051	65109.432433	34.372583
969.921491	65203.752571	34.377600
971.189556	65290.757127	34.382618
971.773627	65388.814658	34.387636
973.156745	65481.132619	34.392653
973.816835	65577.938182	34.397671
975.028102	65682.800008	34.402688
976.242672	65781.932161	34.407706
976.827772	65879.681216	34.412724
978.305870	65974.132430	34.417741
979.533150	66070.224811	34.422759
980.691248	66161.649615	34.427776
981.310263	66256.463529	34.432794
982.208545	66355.919405	34.437812
983.544865	66448.773676	34.442829
984.855588	66532.268379	34.447847
985.594269	66617.175633	34.452864
986.990765	66710.008831	34.457882
987.924155	66803.313327	34.462900
988.508903	66892.392463	34.467917
989.748791	66990.898604	34.472935
991.261209	67066.747061	34.477952
992.223694	67152.596296	34.482970
992.865614	67246.359327	34.487988
994.380688	67325.538464	34.493005
995.086682	67424.344656	34.498023
996.397148	67503.359919	34.503040
997.042827	67596.078957	34.508058
997.833485	67684.103104	34.513076
999.078988	67770.214274	34.518093
1000.057761	67867.821048	34.523111
1000.902723	67952.519926	34.528128
1001.823388	68039.195424	34.533146
1003.296782	68125.835831	34.538164
1004.734887	68217.344730	34.543181
1005.566320	68293.486454	34.548199
1006.142677	68380.989166	34.553216
1007.466432	68461.936488	34.558234
1008.041793	68547.147842	34.563252
1009.095769	68641.807932	34.568269
1010.241909	68733.459095	34.573287
1010.926188	68815.241556	34.578304
1012.416492	68904.294373	34.583322
1013.147137	68999.911559	34.588340
1014.064402	69090.073644	34.593357
1014.814902	69181.655017	34.598375
1015.926531	69270.647738	34.603392
1016.629802	69362.180115	34.608410
1017.491914	69465.579500	34.613428
1018.477085	69569.061455	34.618445
1019.541635	69662.887824	34.623463
1020.399157	69757.880192	34.628480
1021.905185	69834.111418	34.633498
1022.534082	69936.947443	34.638516
1023.484892	70027.569814	34.643533
1024.534450	70108.039417	34.648551
1025.458999	70210.387255	34.653568
1026.389852	70297.556328	34.658586
1026.886609	70400.452748	34.663604
1028.284670	70497.649599	34.668621
1029.440496	70589.932717	34.673639
1030.028436	70699.110359	34.678656
1031.201238	70799.572851	34.683674
1032.169228	70906.627879	34.688692
1032.818746	71004.386400	34.693709
1034.252989	71110.951755	34.698727
1034.868588	71218.126235	34.703744
1036.397202	71319.890473	34.708762
1037.415686	71433.436847	34.713780
1038.285884	71531.606256	34.718797
1039.669196	71647.731071	34.723815
1040.872366	71748.597761	34.728832
1042.132149	71855.712569	34.733850
1043.026524	71958.426571	34.738868
1044.596935	72046.344152	34.743885
1045.748988	72142.939489	34.748903
1046.681343	72240.202641	34.753920
1048.613074	72329.622754	34.758938
1049.234505	72428.670146	34.763956
1050.700033	72512.882002	34.768973
1051.692534	72605.070985	34.773991
1052.695858	72693.243651	34.779008
1053.726602	72776.865424	34.784026
1054.836308	72873.609350	34.789044
1056.471945	72949.880150	34.794061
1057.916594	73042.012944	34.799079
1058.805694	73122.339460	34.804096
1059.948123	73202.259482	34.809114
1061.177403	73291.564217	34.814132
1061.428548	73371.040859	34.819149
1061.927397	73454.912223	34.824167
1063.225041	73554.491861	34.829184
1064.792894	73629.381924	34.834202
1065.505559	73727.862673	34.839220
1066.643206	73819.577315	34.844237
1067.381717	73917.522770	34.849255
1068.436985	74016.723887	34.854272
1069.398313	74112.570801	34.859290
1070.441701	74201.603541	34.864308
1071.902990	74294.194072	34.869325
1073.065563	74382.980873	34.874343
1074.282220	74494.267608	34.879360
1075.256819	74572.229257	34.884378
1076.013429	74675.735211	34.889396
1076.714762	74764.303746	34.894413
1077.877626	74870.191841	34.899431
1078.626183	74971.774883	34.904448
1079.704804	75072.534270	34.909466
1080.722400	75182.752855	34.914484
1082.306047	75283.510423	34.919501
1083.539361	75383.955565	34.924519
1084.216556	75473.150867	34.929536
1085.987365	75565.836950	34.934554
1086.590245	75667.001955	34.939572
1087.886597	75766.070688	34.944589
1089.113665	75865.327907	34.949607
1090.132995	75967.024562	34.954624
1091.540250	76058.388225	34.959642
1092.214599	76151.614341	34.964660
1093.581474	76238.234733	34.969677
1094.379120	76322.575243	34.974695
1095.381312	76422.072187	34.979712
1096.559607	76495.612173	34.984730
1097.326847	76592.650863	34.989748
1098.436990	76683.454854	34.994765
1099.492426	76768.922024	34.999783
1100.485309	76866.889294	35.004800
1101.840606	76944.975894	35.009818
1102.945694	77048.094684	35.014836
1103.930871	77131.851148	35.019853
1105.394929	77221.575777	35.024871
1106.129086	77316.937412	35.029888
1107.202580	77404.202574	35.034906
1107.993501	77513.287840	35.039924
1108.953135	77613.365817	35.044941
1110.190285	77717.239318	35.049959
1110.923043	77833.492245	35.054976
1112.285819	77936.320925	35.059994
1113.630035	78040.609699	35.065012
1114.688204	78144.854719	35.070029
1116.121049	78248.167717	35.075047
1117.247985	78359.775676	35.080064
1118.378129	78449.936360	35.085082
1119.568229	78557.329456	35.090100
1120.663429	78661.950723	35.095117
1121.681631	78764.532106	35.100135
1122.606992	78876.553588	35.105152
1123.849831	78982.128557	35.110170
1124.659382	79100.959251	35.115188
1125.825680	79207.459126	35.120205
1126.758026	79315.440045	35.125223
1127.920956	79440.741511	35.130240
1129.073393	79557.379798	35.135258
1130.138099	79692.579268	35.140276
1131.038613	79794.625371	35.145293
1132.299890	79916.315744	35.150311
1133.853917	80038.062434	35.155328
1134.931573	80154.727543	35.160346
1135.619516	80271.390457	35.165364
1137.205485	80390.359206	35.170381
1138.382658	80499.345488	35.175399
1139.463882	80627.414226	35.180416
1140.622069	80748.174097	35.185434
1142.216626	80862.519260	35.190452
1143.190100	80986.868983	35.195469
1144.262947	81109.392068	35.200487
1145.670515	81223.729806	35.205504
1147.060140	81327.973222	35.210522
1147.809791	81445.138213	35.215540
1148.990376	81559.905410	35.220557
1150.452193	81663.416670	35.225575
1151.673002	81785.907011	35.230592
1152.828947	81896.688467	35.235610
1153.922550	82007.049291	35.240628
1154.672186	82129.031655	35.245645
1155.889063	82232.355079	35.250663
1157.053432	82356.009645	35.255680
1158.286599	82468.060993	35.260698
1159.303572	82585.987330	35.265716
1160.438967	82716.895258	35.270733
1161.268325	82819.660313	35.275751
1162.605869	82950.043717	35.280768
1164.385898	83067.903969	35.285786
1165.629197	83176.560914	35.290804
1166.722189	83289.156813	35.295821
1168.076068	83384.797549	35.300839
1169.752572	83499.546119	35.305856
1171.051084	83598.465172	35.310874
1172.334731	83697.893704	35.315892
1173.005652	83789.980321	35.320909
1174.633194	83856.969873	35.325927
1175.775555	83946.614208	35.330944
1176.966682	84036.352600	35.335962
1177.982918	84130.160463	35.340980
1178.877891	84225.267258	35.345997
1179.973546	84316.782630	35.351015
1180.886472	84417.715849	35.356032
1181.825431	84513.032158	35.361050
1182.862503	84617.684676	35.366068
1184.182144	84731.290005	35.371085
1185.301021	84837.058310	35.376103
1186.231860	84949.090454	35.381120
1187.085354	85062.731638	35.386138
1188.585361	85171.736349	35.391156
1189.608643	85284.262257	35.396173
1190.792284	85396.890356	35.401191
1191.743070	85524.988846	35.406208
1193.081620	85647.350755	35.411226
1194.565948	85765.014722	35.416244
1195.556125	85887.051728	35.421261
1196.953942	85998.445042	35.426279
1198.115018	86118.023480	35.431296
1199.482947	86239.344247	35.436314
1201.209315	86346.100615	35.441332
1202.172909	86462.454582	35.446349
1203.940736	86568.483023	35.451367
1204.968312	86682.914471	35.456384
1206.112407	86790.966933	35.461402
1207.467958	86905.766378	35.466420
1208.876761	87031.063082	35.471437
1210.132199	87122.917290	35.476455
1211.066225	87238.290538	35.481472
1212.203656	87355.444698	35.486490
1213.416752	87464.933540	35.491508
1214.051052	87575.944847	35.496525
1215.766471	87700.993940	35.501543
1216.806667	87829.456153	35.506560
1217.780530	87946.511411	35.511578
1219.173196	88059.510125	35.516596
1220.378475	88195.475680	35.521613
1221.619236	88317.268409	35.526631
1222.451103	88440.088405	35.531648
1223.465646	88576.490931	35.536666
1225.060130	88689.815484	35.541684
1225.806044	88828.440694	35.546701
1227.209080	88954.798343	35.551719
1228.482893	89084.991186	35.556736
1230.326814	89201.485117	35.561754
1231.528575	89317.965403	35.566772
1232.788373	89440.976405	35.571789
1234.654432	89565.325609	35.576807
1235.877610	89673.008826	35.581824
1237.249723	89791.251366	35.586842
1238.715415	89903.016455	35.591860
1239.958571	90012.953629	35.596877
1241.707538	90113.104703	35.601895
1242.781764	90229.722470	35.606912
1243.764287	90341.779858	35.611930
1245.315123	90440.796917	35.616948
1246.095971	90555.319802	35.621965
1247.320393	90662.816293	35.626983
1248.475781	90787.522009	35.632000
1249.430742	90900.561646	35.637018
1250.392794	91014.487764	35.642036
1251.776446	91121.910420	35.647053
1253.445794	91220.632785	35.652071
1254.947819	91322.790783	35.657088
1255.878972	91416.407070	35.662106
1257.133555	91514.041634	35.667124
1258.285773	91626.280183	35.672141
1259.403296	91715.432500	35.677159
1260.960962	91825.137249	35.682176
1261.987412	91921.807391	35.687194
1263.292612	92021.108696	35.692212
1264.093504	92125.811979	35.697229
1265.678717	92243.739501	35.702247
1266.835010	92349.224735	35.707264
1267.992409	92457.675954	35.712282
1269.521213	92556.842816	35.717300
1270.472162	92691.892472	35.722317
1271.340721	92790.820656	35.727335
1272.438942	92915.290559	35.732352
1273.598453	93035.074518	35.737370
1274.817529	93172.125170	35.742388
1275.990348	93291.996787	35.747405
1277.180393	93424.756380	35.752423
1278.668519	93558.534832	35.757440
1279.678468	93692.705168	35.762458
1281.139335	93826.831254	35.767476
1282.265543	93958.690503	35.772493
1283.483973	94094.135661	35.777511
1285.116694	94231.823789	35.782528
1286.155038	94366.068694	35.787546
1287.609433	94497.321462	35.792564
1288.632017	94645.043731	35.797581
1290.346878	94776.016312	35.802599
1291.634008	94915.725951	35.807616
1292.408398	95053.031653	35.812634
1294.203871	95194.526707	35.817652
1295.363593	95342.129551	35.822669
1296.721775	95475.771762	35.827687
1298.699351	95614.578519	35.832704
1299.781351	95757.188562	35.837722
1300.858300	95884.956765	35.842740
1301.745940	96038.093847	35.847757
1302.961547	96180.304753	35.852775
1304.617848	96319.367467	35.857792
1306.092832	96472.985673	35.862810
1307.713579	96606.617209	35.867828
1308.944532	96750.919860	35.872845
1310.678955	96862.934768	35.877863
1312.331993	96995.751663	35.882880
1313.476387	97132.932856	35.887898
1314.957001	97262.950917	35.892916
1316.777386	97389.050348	35.897933
1317.702158	97515.416450	35.902951
1319.127340	97652.657608	35.907968
1320.224504	97774.649895	35.912986
1321.840044	97897.854973	35.918004
1323.370687	98016.167906	35.923021
1324.446254	98148.268231	35.928039
1326.214108	98259.978656	35.933056
1327.404149	98371.449815	35.938074
1329.231186	98494.383433	35.943092
1330.501731	98617.023839	35.948109
1331.238918	98739.988595	35.953127
1333.107644	98855.792718	35.958144
1334.106014	98984.029389	35.963162
1335.250504	99107.515304	35.968180
1336.269970	99226.292609	35.973197
1337.309584	99349.111217	35.978215
1338.831123	99482.440716	35.983232
1339.637077	99625.884475	35.988250
1341.143196	99744.042829	35.993268
1342.590200	99874.152852	35.998285
1343.341974	100004.625160	36.003303
1344.847324	100115.343382	36.008320
1345.817290	100245.858769	36.013338
1347.436190	100371.392833	36.018356
1348.509749	100501.766354	36.023373
1350.072080	100631.164212	36.028391
1351.416339	100749.123245	36.033408
1353.071366	100883.413939	36.038426
1354.384747	101005.498967	36.043444
1355.230614	101141.995829	36.048461
1356.974885	101264.864177	36.053479
1358.123210	101397.321506	36.058496
1359.383699	101528.418050	36.063514
1361.054672	101669.264015	36.068532
1362.149151	101810.466558	36.073549
1363.439022	101947.848537	36.078567
1365.213731	102092.204698	36.083584
1366.514239	102219.976102	36.088602
1367.987716	102361.236132	36.093620
1369.148566	102493.315599	36.098637
1370.600106	102639.753003	36.103655
1371.874499	102775.492664	36.108672
1373.141089	102921.262792	36.113690
1374.243149	103066.387209	36.118708
1375.962793	103219.492416	36.123725
1377.403216	103368.901582	36.128743
1378.843165	103514.114837	36.133760
1380.053422	103673.209715	36.138778
1381.365346	103815.375947	36.143796
1382.695842	103974.656414	36.148813
1384.445060	104124.730936	36.153831
1386.264261	104261.431559	36.158848
1387.432550	104406.412054	36.163866
1389.219147	104553.705973	36.168884
1390.552083	104698.319771	36.173901
1392.090485	104835.383427	36.178919
1393.357618	104983.787110	36.183936
1394.321339	105128.168605	36.188954
1395.772751	105270.091085	36.193972
1397.219786	105430.691678	36.198989
1398.829707	105572.489326	36.204007
1400.746733	105706.682752	36.209024
1402.270657	105849.192324	36.214042
1403.925181	105991.415896	36.219060
1405.120784	106130.211894	36.224077
1406.739542	106269.107435	36.229095
1408.158586	106401.048048	36.234112
1409.551721	106539.193662	36.239130
1410.848258	106682.845280	36.244148
1412.382228	106826.092828	36.249165
1413.322920	106954.737169	36.254183
1415.176926	107094.715306	36.259200
1416.083069	107237.377576	36.264218
1417.556222	107384.377570	36.269236
1418.576702	107525.717186	36.274253
1420.380039	107674.569068	36.279271
1422.052223	107805.042833	36.284288
1423.533247	107955.340937	36.289306
1424.580303	108106.024254	36.294324
1425.955200	108254.628321	36.299341
1427.470590	108382.326287	36.304359
1429.031396	108525.995213	36.309376
1430.364794	108678.868247	36.314394
1431.974195	108820.983794	36.319412
1433.093758	108957.647353	36.324429
1434.638866	109113.000140	36.329447
1435.891364	109251.216584	36.334464
1436.932020	109386.854280	36.339482
1438.251349	109515.880389	36.344500
1439.650700	109654.532091	36.349517
1440.695441	109802.712292	36.354535
1442.459492	109935.398966	36.359552
1443.456134	110080.772624	36.364570
1444.706911	110226.855521	36.369588
1446.431428	110375.820026	36.374605
1447.893790	110541.007346	36.379623
1449.478523	110677.643270	36.384640
1450.803299	110840.304450	36.389658
1452.266480	110985.837497	36.394676
1453.807423	111143.812321	36.399693
1455.030608	111304.741397	36.404711
1456.333518	111454.803290	36.409728
1457.671219	111614.536552	36.414746
1459.054534	111767.897181	36.419764
1461.016682	111935.372029	36.424781
1462.160402	112089.532245	36.429799
1463.938660	112244.165052	36.434816
1465.713003	112404.937224	36.439834
1467.413057	112555.411172	36.444852
1469.274819	112703.768035	36.449869
1470.917160	112855.178018	36.454887
1472.789424	113016.191335	36.459904
1473.972572	113151.073020	36.464922
1475.617038	113301.330464	36.469940
1477.444258	113438.395794	36.474957
1479.024477	113597.478716	36.479975
1480.444139	113740.049384	36.484992
1481.613835	113889.013462	36.490010
1482.774496	114042.278950	36.495028
1484.524987	114183.062355	36.500045
1485.932180	114337.305326	36.505063
1487.665464	114488.441658	36.510080
1488.872608	114648.741382	36.515098
1490.182768	114808.036513	36.520116
1491.988689	114959.987876	36.525133
1493.179133	115116.271770	36.530151
1494.097983	115270.480542	36.535168
1495.928019	115444.054681	36.540186
1497.208716	115601.645631	36.545204
1498.746648	115763.801208	36.550221
1500.289953	115935.481766	36.555239
1501.887218	116093.165059	36.560256
1503.449467	116259.314261	36.565274
1504.833440	116428.409138	36.570292
1506.460243	116590.414988	36.575309
1507.771426	116756.960632	36.580327
1509.076173	116927.351143	36.585344
1510.714534	117102.066358	36.590362
1512.232300	117269.457308	36.595380
1513.818239	117434.060656	36.600397
1515.199322	117616.415878	36.605415
1516.854236	117783.978037	36.610432
1518.237703	117955.578625	36.615450
1519.552817	118127.355526	36.620468
1521.182690	118301.139031	36.625485
1523.005475	118466.915019	36.630503
1524.523034	118646.552274	36.635520
1525.977843	118820.327360	36.640538
1527.274796	118990.626955	36.645556
1529.184748	119154.933694	36.650573
1530.801865	119322.952505	36.655591
1532.488255	119493.751849	36.660608
1533.902171	119654.662415	36.665626
1535.391897	119842.757513	36.670644
1537.089903	119990.407979	36.675661
1537.877587	120155.806988	36.680679
1539.747290	120309.926501	36.685696
1541.077736	120465.132658	36.690714
1542.186610	120629.240603	36.695732
1544.095030	120784.421511	36.700749
1545.238882	120964.343452	36.705767
1546.601429	121117.035619	36.710784
1548.067750	121287.090706	36.715802
1549.624227	121472.456079	36.720820
1551.102101	121647.026831	36.725837
1552.127691	121824.446816	36.730855
1554.020099	121998.929252	36.735872
1555.876193	122173.265895	36.740890
1557.578018	122344.240333	36.745908
1559.251542	122524.454906	36.750925
1561.499955	122687.214412	36.755943
1563.225823	122855.447270	36.760960
1565.082411	123016.911772	36.765978
1566.652574	123191.563830	36.770996
1568.419459	123352.396697	36.776013
1570.058244	123518.692337	36.781031
1571.600655	123666.634651	36.786048
1573.219760	123830.549732	36.791066
1575.098037	124000.539748	36.796084
1576.738461	124160.659788	36.801101
1577.975118	124334.201665	36.806119
1579.269808	124505.451774	36.811136
1580.756027	124674.148268	36.816154
1582.168299	124846.409104	36.821172
1583.587919	125020.800818	36.826189
1585.197987	125199.553095	36.831207
1586.682505	125375.623516	36.836224
1588.230583	125560.768260	36.841242
1589.546418	125753.650668	36.846260
1591.418835	125935.689210	36.851277
1592.677904	126121.059102	36.856295
1594.388733	126317.790167	36.861312
1595.741886	126504.212832	36.866330
1597.077127	126699.329549	36.871348
1598.791348	126897.978572	36.876365
1600.111230	127090.676361	36.881383
1601.489485	127287.742953	36.886400
1602.901370	127507.210463	36.891418
1604.645865	127714.371678	36.896436
1606.606958	127915.017103	36.901453
1608.182472	128128.372624	36.906471
1610.185059	128330.574121	36.911488
1611.608994	128522.628013	36.916506
1613.175162	128734.935047	36.921524
1615.267828	128932.063180	36.926541
1617.018904	129134.485335	36.931559
1618.434187	129326.709196	36.936576
1620.245121	129530.583008	36.941594
1621.441921	129731.850918	36.946612
1623.244307	129936.501965	36.951629
1624.747029	130142.723176	36.956647
1626.206312	130344.473339	36.961664
1627.727673	130553.117016	36.966682
1629.239253	130762.384945	36.971700
1630.827730	130968.304979	36.976717
1632.390965	131177.325825	36.981735
1633.760787	131395.627454	36.986752
1635.581996	131602.960757	36.991770
1637.220422	131822.453499	36.996788
1639.087290	132035.516874	37.001805
1640.747032	132243.906137	37.006823
1642.206038	132449.054020	37.011840
1643.977208	132658.785593	37.016858
1645.367451	132861.852514	37.021876
1647.105863	133055.692301	37.026893
1648.820089	133259.142053	37.031911
1650.349165	133450.148520	37.036928
1652.326077	133649.003930	37.041946
1653.670439	133849.988906	37.046964
1655.256004	134037.588509	37.051981
1656.902930	134242.588632	37.056999
1658.163136	134450.301900	37.062016
1660.286468	134659.099953	37.067034
1661.712048	134867.182789	37.072052
1663.281395	135061.920541	37.077069
1664.632459	135281.995520	37.082087
1666.242739	135503.985390	37.087104
1668.303410	135718.876329	37.092122
1669.719344	135941.634588	37.097140
1671.462597	136161.170619	37.102157
1672.954895	136388.601624	37.107175
1674.607322	136606.199746	37.112192
1676.592907	136833.061299	37.117210
1677.873846	137055.198848	37.122228
1679.621849	137284.789851	37.127245
1681.447779	137518.938235	37.132263
1683.166929	137743.358539	37.137280
1684.323673	137987.638524	37.142298
1686.135957	138225.891496	37.147316
1687.904823	138466.944282	37.152333
1689.607992	138702.754789	37.157351
1691.390611	138948.706352	37.162368
1693.022386	139185.520248	37.167386
1694.587080	139430.632622	37.172404
1696.357153	139673.747282	37.177421
1698.006676	139911.374258	37.182439
1699.732932	140156.389110	37.187456
1701.643142	140403.470558	37.192474
1703.339600	140652.528241	37.197492
1704.833811	140904.258389	37.202509
1706.756019	141152.890126	37.207527
1708.448298	141408.247064	37.212544
1710.135380	141645.140744	37.217562
1712.309906	141901.072475	37.222580
1714.308746	142150.535037	37.227597
1716.588960	142387.505017	37.232615
1718.231177	142624.156635	37.237632
1719.876903	142857.267973	37.242650
1721.498579	143103.583203	37.247668
1723.009187	143341.362916	37.252685
1724.894462	143585.761197	37.257703
1726.744378	143834.506706	37.262720
1728.411011	144074.258236	37.267738
1729.555492	144316.922435	37.272756
1731.517563	144570.870457	37.277773
1732.844072	144813.483352	37.282791
1734.335641	145076.162984	37.287808
1736.410625	145326.480064	37.292826
1738.189245	145576.603362	37.297844
1740.112219	145820.524386	37.302861
1741.962784	146074.751173	37.307879
1743.536584	146328.806534	37.312896
1745.136846	146580.853660	37.317914
1746.628432	146840.686642	37.322932
1748.751597	147091.956811	37.327949
1750.686066	147348.905711	37.332967
1752.291346	147613.040314	37.337984
1753.414698	147863.771744	37.343002
1755.188862	148130.903519	37.348020
1756.831495	148380.795049	37.353037
1759.059387	148641.080902	37.358055
1760.533006	148882.306575	37.363072
1762.656626	149108.403813	37.368090
1764.345254	149360.463304	37.373108
1766.211145	149581.944362	37.378125
1768.222722	149829.107085	37.383143
1769.369131	150068.002765	37.388160
1771.263473	150303.850980	37.393178
1773.401670	150553.231325	37.398196
1775.045739	150791.519642	37.403213
1776.832776	151037.643927	37.408231
1778.217918	151280.988556	37.413248
1780.031246	151530.233548	37.418266
1781.554126	151787.153675	37.423284
1783.301110	152039.749699	37.428301
1785.257573	152296.147751	37.433319
1786.769271	152563.443926	37.438336
1788.432733	152818.404834	37.443354
1790.053885	153083.820492	37.448372
1791.745144	153343.209606	37.453389
1794.390724	153611.007094	37.458407
1796.146114	153883.704646	37.463424
1798.055259	154145.716586	37.468442
1800.164270	154418.717108	37.473460
1801.847602	154668.694511	37.478477
1803.831657	154933.719625	37.483495
1805.136719	155215.557308	37.488512
1807.103837	155481.311155	37.493530
1808.743152	155744.387946	37.498548
1811.028625	156005.524666	37.503565
1812.396973	156276.516595	37.508583
1814.410220	156560.180147	37.513600
1816.406216	156823.599816	37.518618
1818.379111	157091.416619	37.523636
1819.900782	157368.660887	37.528653
1822.100233	157644.214109	37.533671
1823.470635	157920.329259	37.538688
1825.137279	158200.233440	37.543706
1826.950947	158471.737353	37.548724
1828.786514	158763.335323	37.553741
1830.985021	159041.853035	37.558759
1832.277436	159332.992381	37.563776
1834.333146	159611.991942	37.568794
1836.536550	159905.010758	37.573812
1838.040151	160188.935760	37.578829
1839.741388	160473.275642	37.583847
1841.308927	160773.925894	37.588864
1843.155956	161061.445017	37.593882
1844.191462	161357.432747	37.598900
1845.895799	161660.719322	37.603917
1848.420697	161968.196173	37.608935
1849.794265	162278.951461	37.613952
1851.543018	162581.105578	37.618970
1853.541101	162898.558927	37.623988
1854.915646	163208.302875	37.629005
1857.374161	163527.109585	37.634023
1858.991862	163843.395235	37.639040
1860.663784	164148.361724	37.644058
1862.810167	164469.760813	37.649076
1864.703671	164789.055150	37.654093
1866.893069	165092.701210	37.659111
1868.477858	165408.098000	37.664128
1870.472434	165727.761968	37.669146
1872.668032	166027.348420	37.674164
1874.357027	166347.189826	37.679181
1876.440804	166660.343663	37.684199
1877.979531	166985.175797	37.689216
1879.705701	167289.894086	37.694234
1881.606113	167608.248311	37.699252
1883.272902	167906.211159	37.704269
1886.275696	168177.329305	37.709287
1887.817619	168477.815287	37.714304
1889.775238	168757.452896	37.719322
1891.759218	169047.422876	37.724340
1893.515245	169328.084459	37.729357
1895.901729	169627.123330	37.734375
1897.207424	169924.604827	37.739392
1898.579965	170213.150984	37.744410
1900.250607	170512.787395	37.749428
1901.580796	170829.111517	37.754445
1903.819967	171142.870319	37.759463
1905.213183	171472.176799	37.764480
1906.607027	171792.482101	37.769498
1908.883583	172123.101468	37.774516
1910.708301	172448.002489	37.779533
1912.578178	172784.490831	37.784551
1914.348375	173127.433904	37.789568
1916.174803	173462.839967	37.794586
1918.061793	173801.475997	37.799604
1919.874372	174163.362203	37.804621
1921.822605	174502.182190	37.809639
1923.724514	174848.223295	37.814656
1925.645882	175205.462553	37.819674
1927.469875	175561.943966	37.824692
1929.373823	175923.455676	37.829709
1931.593164	176266.774144	37.834727
1933.261227	176636.516064	37.839744
1935.614092	176994.775351	37.844762
1937.381502	177357.139984	37.849780
1939.440791	177723.752825	37.854797
1941.549309	178080.023018	37.859815
1943.752795	178440.241865	37.864832
1945.927179	178794.396820	37.869850
1948.073345	179164.456328	37.874868
1950.065909	179519.709223	37.879885
1952.193851	179870.624906	37.884903
1954.387179	180225.087468	37.889920
1956.406707	180594.766319	37.894938
1958.487697	180954.252597	37.899956
1960.541445	181297.464475	37.904973
1962.535795	181642.947309	37.909991
1964.969713	181994.433172	37.915008
1967.063080	182347.497259	37.920026
1969.154935	182688.955891	37.925044
1970.810313	183035.995139	37.930061
1972.819240	183389.685825	37.935079
1974.549901	183736.487313	37.940096
1976.274037	184096.371370	37.945114
1978.125322	184463.653403	37.950132
1979.719414	184820.309315	37.955149
1981.476711	185189.538984	37.960167
1983.639690	185554.465235	37.965184
1985.614111	185932.985285	37.970202
1987.839413	186288.659191	37.975220
1989.576137	186659.903943	37.980237
1991.157591	187022.182797	37.985255
1993.515324	187447.790022	37.990272
1995.052143	187857.956759	37.995290
1997.279910	188229.232203	38.000308
1998.967011	188608.797192	38.005325
2001.314759	188982.901308	38.010343
2003.221225	189352.198579	38.015360
2005.559881	189725.163613	38.020378
2007.666608	190106.014611	38.025396
2009.668105	190481.015813	38.030413
2011.489208	190851.931465	38.035431
2013.463653	191221.960822	38.040448
2015.516494	191574.300437	38.045466
2017.878274	191930.707898	38.050484
2020.039079	192281.432564	38.055501
2021.587454	192630.526313	38.060519
2023.371619	192982.708648	38.065536
2025.336068	193347.945338	38.070554
2027.588720	193698.710542	38.075572
2029.239428	194057.927310	38.080589
2031.225231	194422.477948	38.085607
2032.962781	194791.640443	38.090624
2034.483423	195167.492839	38.095642
2036.825477	195532.753153	38.100660
2038.402206	195920.461313	38.105677
2040.448549	196307.106836	38.110695
2042.687875	196697.863845	38.115712
2044.431891	197093.195101	38.120730
2046.721097	197490.550944	38.125748
2048.290280	197893.963931	38.130765
2050.050337	198303.546352	38.135783
2052.145084	198717.192909	38.140800
2053.724622	199126.780284	38.145818
2055.996948	199542.154189	38.150836
2057.835175	199973.091992	38.155853
2060.298217	200384.247125	38.160871
2062.330673	200804.361077	38.165888
2064.459162	201230.735513	38.170906
2066.355264	201656.258134	38.175924
2068.385543	202093.395219	38.180941
2071.054312	202517.605837	38.185959
2073.221433	202955.485875	38.190976
2075.117223	203387.007783	38.195994
2077.810044	203812.995925	38.201012
2079.717814	204234.915792	38.206029
2081.918725	204665.046858	38.211047
2084.282257	205097.897075	38.216064
2086.119988	205519.195592	38.221082
2088.457345	205943.160747	38.226100
2090.479654	206377.743424	38.231117
2093.088080	206804.487882	38.236135
2095.280374	207230.154819	38.241152
2097.308515	207656.686434	38.246170
2099.343084	208079.915457	38.251188
2101.546017	208511.248069	38.256205
2103.985528	208949.073280	38.261223
2105.621890	209378.183950	38.266240
2107.773874	209810.466740	38.271258
2110.391473	210241.839493	38.276276
2112.317301	210675.454504	38.281293
2114.324550	211091.884834	38.286311
2116.543872	211516.310281	38.291328
2118.492748	211953.226164	38.296346
2121.099989	212377.109840	38.301364
2123.149998	212814.519321	38.306381
2125.305901	213229.024291	38.311399
2127.447774	213649.603445	38.316416
2129.250030	214093.937604	38.321434
2131.309742	214524.666692	38.326452
2132.873062	214961.240196	38.331469
2134.770453	215405.993036	38.336487
2137.140368	215845.642897	38.341504
2138.993271	216306.865321	38.346522
2140.951019	216754.201432	38.351540
2142.765979	217206.691794	38.356557
2144.894449	217661.420151	38.361575
2146.919286	218127.266562	38.366592
2149.712968	218590.961417	38.371610
2151.854144	219039.465027	38.376628
2153.582495	219487.779183	38.381645
2155.816782	219929.079628	38.386663
2158.067466	220358.818985	38.391680
2159.954045	220797.227221	38.396698
2162.199593	221220.921705	38.401716
2164.322281	221660.894102	38.406733
2166.406550	222099.094397	38.411751
2168.663446	222530.078655	38.416768
2171.030677	222973.849547	38.421786
2173.019474	223417.298415	38.426804
2175.399918	223854.208409	38.431821
2177.489178	224299.547166	38.436839
2179.587052	224732.462058	38.441856
2181.513123	225195.660021	38.446874
2184.273784	225637.439500	38.451892
2186.578212	226084.040562	38.456909
2188.815619	226540.686665	38.461927
2190.694361	226990.250002	38.466944
2193.007282	227445.105979	38.471962
2195.001207	227903.441074	38.476980
2197.031633	228359.280786	38.481997
2199.130202	228824.560083	38.487015
2201.701040	229289.029009	38.492032
2203.701302	229759.531103	38.497050
2206.182458	230218.043652	38.502068
2208.222464	230701.241137	38.507085
2210.387295	231174.333528	38.512103
2212.709885	231652.304051	38.517120
2214.928864	232120.967117	38.522138
2217.235856	232589.184284	38.527156
2219.545966	233077.596739	38.532173
2221.947342	233555.604370	38.537191
2224.275107	234030.015675	38.542208
2226.359848	234509.773763	38.547226
2228.747248	234977.442843	38.552244
2230.946722	235469.960210	38.557261
2232.883924	235953.982155	38.562279
2235.316748	236438.637696	38.567296
2237.255059	236927.459590	38.572314
2239.840640	237421.921340	38.577332
2242.096824	237912.419886	38.582349
2244.084728	238407.278092	38.587367
2246.429596	238889.581436	38.592384
2249.143795	239385.214225	38.597402
2251.172436	239870.537463	38.602420
2253.549825	240360.200418	38.607437
2255.408518	240862.517932	38.612455
2257.915396	241356.223523	38.617472
2260.575230	241846.347924	38.622490
2263.256689	242337.407943	38.627508
2265.654980	242832.727993	38.632525
2267.630360	243320.745927	38.637543
2270.119776	243803.017956	38.642560
2272.371954	244307.934598	38.647578
2274.294389	244805.559945	38.652596
2276.450153	245291.513292	38.657613
2278.862947	245780.677085	38.662631
2281.305867	246281.012260	38.667648
2282.976871	246783.498537	38.672666
2285.578148	247284.670225	38.677684
2287.702450	247780.199241	38.682701
2289.875405	248283.136912	38.687719
2292.417461	248776.235804	38.692736
2294.800646	249280.509712	38.697754
2296.865857	249774.213477	38.702772
2299.189952	250282.608835	38.707789
2301.094112	250797.062916	38.712807
2303.527046	251298.528830	38.717824
2305.592015	251800.279063	38.722842
2307.749506	252293.935486	38.727860
2310.088858	252776.867852	38.732877
2312.408152	253258.455511	38.737895
2314.666763	253738.196737	38.742912
2317.049772	254236.079182	38.747930
2319.437693	254711.224785	38.752948
2321.613966	255208.754993	38.757965
2323.605065	255704.686556	38.762983
2326.348077	256196.968535	38.768000
2328.465672	256698.261851	38.773018
2330.753647	257194.090931	38.778036
2333.486033	257687.080261	38.783053
2335.859821	258180.123505	38.788071
2338.564832	258677.837823	38.793088
2340.562525	259192.983476	38.798106
2342.459177	259698.287278	38.803124
2345.323426	260194.395827	38.808141
2347.278608	260719.447762	38.813159
2349.360445	261222.252444	38.818176
2351.913588	261757.620729	38.823194
2354.001100	262266.058776	38.828212
2356.703494	262787.301966	38.833229
2359.381238	263318.122242	38.838247
2361.913091	263829.735123	38.843264
2364.462231	264346.651379	38.848282
2367.074602	264859.618375	38.853300
2369.627520	265363.067390	38.858317
2371.688811	265898.847360	38.863335
2374.382503	266401.253416	38.868352
2376.789182	266937.786917	38.873370
2378.927459	267462.117107	38.878388
2381.272729	267983.567643	38.883405
2383.680620	268524.791027	38.888423
2386.058090	269043.411591	38.893440
2388.754890	269574.221536	38.898458
2390.729400	270107.045725	38.903476
2393.661001	270625.774457	38.908493
2395.934199	271162.381118	38.913511
2398.293683	271694.805956	38.918528
2400.657475	272236.852568	38.923546
2402.934194	272785.207918	38.928564
2404.866291	273320.965688	38.933581
2407.475962	273877.313190	38.938599
2409.494367	274425.342735	38.943616
2412.000200	274990.003826	38.948634
2414.090801	275539.589425	38.953652
2416.773611	276097.942489	38.958669
2418.687984	276659.077894	38.963687
2421.452884	277216.115261	38.968704
2423.766994	277777.663134	38.973722
2426.000229	278342.622589	38.978740
2428.860474	278911.746788	38.983757
2431.286661	279479.588385	38.988775
2433.944345	280033.320899	38.993792
2436.450150	280603.503418	38.998810
2439.099841	281173.811556	39.003828
2441.559345	281733.733179	39.008845
2444.091025	282296.534221	39.013863
2446.549704	282868.636455	39.018880
2448.965529	283441.680361	39.023898
2451.041741	284000.602858	39.028916
2453.815940	284560.402628	39.033933
2455.976841	285134.894424	39.038951
2458.276811	285703.138507	39.043968
2460.903823	286265.791339	39.048986
2463.442982	286836.274068	39.054004
2465.890635	287399.377006	39.059021
2468.454196	287964.488498	39.064039
2471.045234	288500.694859	39.069056
2473.425115	289050.641191	39.074074
2475.743408	289587.896683	39.079092
2478.462612	290109.545815	39.084109
2480.519137	290647.518686	39.089127
2483.370266	291187.724655	39.094144
2485.841539	291729.254600	39.099162
2488.174354	292279.357925	39.104180
2490.718877	292825.183222	39.109197
2492.901453	293371.973996	39.114215
2495.562439	293914.470681	39.119232
2497.890855	294469.302726	39.124250
2500.406074	295040.248084	39.129268
2502.829899	295589.697659	39.134285
2505.198475	296162.254445	39.139303
2507.914198	296716.878052	39.144320
2510.246017	297280.822778	39.149338
2512.447156	297863.721727	39.154356
2515.181688	298437.239762	39.159373
2517.479047	299016.608326	39.164391
2519.385123	299612.203419	39.169408
2521.933036	300210.180140	39.174426
2524.260623	300815.876788	39.179444
2527.070804	301409.940798	39.184461
2529.596940	302012.724520	39.189479
2532.097491	302624.314316	39.194496
2534.614319	303219.013178	39.199514
2537.362351	303832.911352	39.204532
2540.697594	304433.891556	39.209549
2543.059237	305038.671701	39.214567
2546.074229	305643.774607	39.219584
2548.323844	306247.567955	39.224602
2550.779773	306864.927688	39.229620
2553.051981	307484.288351	39.234637
2555.358843	308108.027220	39.239655
2557.985260	308723.281437	39.244672
2560.387921	309349.578770	39.249690
2562.532524	309981.010040	39.254708
2565.237914	310621.305589	39.259725
2568.190232	311244.244043	39.264743
2571.137503	311878.241325	39.269760
2574.002414	312512.471372	39.274778
2576.290261	313147.950175	39.279796
2578.927645	313772.224082	39.284813
2581.431264	314416.357363	39.289831
2584.011460	315063.337587	39.294848
2586.766250	315692.998370	39.299866
2589.355530	316333.233703	39.304884
2591.929847	316968.818038	39.309901
2594.857138	317605.455047	39.314919
2597.474307	318241.268357	39.319936
2600.103010	318875.751098	39.324954
2602.841315	319518.962610	39.329972
2605.082132	320158.308684	39.334989
2607.706078	320801.671232	39.340007
2610.218740	321438.951288	39.345024
2613.002216	322081.381620	39.350042
2615.437461	322734.158628	39.355060
2618.226184	323379.258137	39.360077
2620.963071	324025.878205	39.365095
2623.595748	324668.723729	39.370112
2626.119456	325307.770187	39.375130
2628.462925	325963.377903	39.380148
2631.098422	326618.143067	39.385165
2633.579698	327271.221699	39.390183
2635.972231	327930.291254	39.395200
2638.759963	328592.764298	39.400218
2640.856414	329249.701518	39.405236
2643.434576	329866.137669	39.410253
2645.991758	330517.679563	39.415271
2648.415192	331153.426081	39.420288
2650.702346	331788.828192	39.425306
2653.190517	332437.354933	39.430324
2655.863216	333086.070270	39.435341
2658.161492	333745.360487	39.440359
2661.116179	334408.291430	39.445376
2664.049710	335059.900256	39.450394
2666.243861	335732.667024	39.455412
2668.935855	336390.860055	39.460429
2672.098095	337055.918342	39.465447
2674.255436	337726.244703	39.470464
2677.404941	338393.563474	39.475482
2680.005761	339075.844143	39.480500
2682.712532	339744.779398	39.485517
2685.396540	340430.724456	39.490535
2687.817287	341115.429102	39.495552
2690.679661	341796.703927	39.500570
2692.837851	342497.882696	39.505588
2696.010946	343188.897091	39.510605
2698.308898	343894.996779	39.515623
2701.552152	344598.449599	39.520640
2704.578856	345288.709250	39.525658
2707.008613	345994.948056	39.530676
2709.786285	346701.498381	39.535693
2712.751013	347409.374115	39.540711
2715.435879	348111.877258	39.545728
2718.679350	348809.460798	39.550746
2721.343255	349523.728368	39.555764
2724.343631	350228.318148	39.560781
2726.869273	350935.806441	39.565799
2729.836727	351650.081772	39.570816
2733.006672	352354.801939	39.575834
2735.481540	353057.459756	39.580852
2738.531843	353751.113602	39.585869
2741.421911	354460.166331	39.590887
2743.927384	355171.215125	39.595904
2747.255038	355876.618619	39.600922
2749.933631	356578.000353	39.605940
2752.889716	357277.649967	39.610957
2756.540394	357973.753443	39.615975
2758.805542	358669.068164	39.620992
2761.889845	359364.898687	39.626010
2764.391895	360070.385495	39.631028
2767.304319	360761.597417	39.636045
2770.010480	361470.897930	39.641063
2772.826833	362158.468071	39.646080
2775.633278	362857.277406	39.651098
2777.645321	363568.511635	39.656116
2780.886095	364262.506007	39.661133
2784.079377	364976.158240	39.666151
2786.215866	365693.657611	39.671168
2789.056322	366402.058425	39.676186
2791.842331	367104.976474	39.681204
2794.381909	367816.937243	39.686221
2797.418884	368530.627437	39.691239
2799.593604	369257.864199	39.696256
2802.308755	369977.953822	39.701274
2805.146637	370702.440249	39.706292
2808.229549	371426.971182	39.711309
2810.684339	372139.875112	39.716327
2813.812948	372866.008414	39.721344
2816.649631	373591.534654	39.726362
2819.637974	374320.869146	39.731380
2822.422341	375041.931435	39.736397
2825.734294	375754.810916	39.741415
2828.167789	376458.764267	39.746432
2831.645549	377142.093099	39.751450
2834.711718	377824.708610	39.756468
2837.619249	378502.898333	39.761485
2840.442779	379177.436174	39.766503
2842.748276	379848.947146	39.771520
2846.134935	380519.867491	39.776538
2848.215785	381208.830835	39.781556
2851.111530	381891.089165	39.786573
2853.651256	382577.614721	39.791591
2856.142079	383271.803764	39.796608
2858.942401	383965.596710	39.801626
2861.591009	384674.893783	39.806644
2864.444822	385392.876320	39.811661
2867.051011	386099.557210	39.816679
2869.846263	386822.927768	39.821696
2872.651015	387553.417095	39.826714
2875.367061	388275.745273	39.831732
2877.953592	389009.062139	39.836749
2881.028743	389748.206333	39.841767
2883.266401	390502.701254	39.846784
2886.111350	391261.686612	39.851802
2889.338286	392016.841940	39.856820
2892.803140	392763.075789	39.861837
2896.101732	393518.325290	39.866855
2899.032422	394273.709713	39.871872
2901.794640	395020.793321	39.876890
2904.797972	395797.686885	39.881908
2907.293208	396557.421113	39.886925
2910.322030	397321.705513	39.891943
2912.647686	398104.906557	39.896960
2915.796719	398887.548428	39.901978
2918.677465	399696.629558	39.906996
2921.012561	400477.674361	39.912013
2924.020572	401270.179363	39.917031
2927.206274	402072.752484	39.922048
2929.992621	402870.551488	39.927066
2933.310762	403672.288825	39.932084
2936.234054	404486.256271	39.937101
2939.052128	405298.135953	39.942119
2942.175169	406105.080809	39.947136
2944.957994	406918.223311	39.952154
2948.002751	407725.729244	39.957172
2950.847294	408548.417140	39.962189
2954.045747	409368.135307	39.967207
2957.052480	410195.594114	39.972224
2960.208987	411005.695061	39.977242
2963.067212	411825.728583	39.982260
2966.042171	412650.215624	39.987277
2968.818539	413474.449242	39.992295
2971.825705	414305.899968	39.997312
2974.881470	415130.532539	40.002330
2978.136496	415957.783184	40.007348
2981.137835	416786.457412	40.012365
2984.779951	417610.599125	40.017383
2987.680355	418424.354578	40.022400
2990.567160	419248.043924	40.027418
2994.132627	420065.273563	40.032436
2997.278359	420886.986696	40.037453
2999.799572	421698.195475	40.042471
3002.618884	422534.002775	40.047488
3005.660448	423338.643942	40.052506
3009.230357	424159.755969	40.057524
3012.101027	424970.427004	40.062541
3015.189154	425795.137802	40.067559
3017.880434	426607.085770	40.072576
3020.679300	427426.213604	40.077594
3023.791594	428252.387142	40.082612
3026.537925	429065.642421	40.087629
3029.507333	429860.884895	40.092647
3032.157072	430664.333742	40.097664
3035.228818	431459.142127	40.102682
3038.433782	432245.507529	40.107700
3041.232202	433029.731332	40.112717
3044.279144	433823.234540	40.117735
3047.287779	434637.886055	40.122752
3050.105164	435440.910102	40.127770
3052.717316	436250.703919	40.132788
3055.739714	437060.702890	40.137805
3058.662857	437877.403179	40.142823
3061.298278	438699.974177	40.147840
3064.497453	439540.559696	40.152858
3067.625778	440377.935969	40.157876
3070.693796	441216.193672	40.162893
3074.057830	442060.025660	40.167911
3077.010299	442906.409233	40.172928
3080.257648	443750.233263	40.177946
3083.761514	444599.635987	40.182964
3086.549268	445452.697023	40.187981
3089.751059	446294.189323	40.192999
3092.669362	447167.756264	40.198016
3095.758405	448029.993160	40.203034
3098.669226	448901.356919	40.208052
3101.502981	449775.821359	40.213069
3104.969362	450653.275419	40.218087
3107.677682	451543.427095	40.223104
3110.450124	452425.294861	40.228122
3113.852095	453325.952956	40.233140
3116.414949	454234.571124	40.238157
3119.797655	455137.512547	40.243175
3122.852828	456056.308471	40.248192
3125.549049	456966.026488	40.253210
3128.942764	457881.190878	40.258228
3131.948150	458805.199589	40.263245
3135.591552	459722.498894	40.268263
3139.111330	460644.814939	40.273280
3142.514522	461574.567772	40.278298
3146.050707	462491.281355	40.283316
3148.757892	463411.959604	40.288333
3152.349537	464333.560125	40.293351
3155.564744	465254.916591	40.298368
3159.165085	466175.910335	40.303386
3162.485530	467085.143241	40.308404
3165.579323	468017.716532	40.313421
3168.966478	468928.452408	40.318439
3171.938746	469854.938879	40.323456
3175.050357	470769.600482	40.328474
3178.888687	471674.213528	40.333492
3181.992919	472609.097160	40.338509
3184.887154	473527.874136	40.343527
3188.091856	474456.685631	40.348544
3191.058272	475374.691030	40.353562
3194.461430	476294.391088	40.358580
3197.134212	477234.166242	40.363597
3200.715575	478153.126736	40.368615
3203.712535	479093.044289	40.373632
3206.786187	480022.208349	40.378650
3210.177091	480953.133211	40.383668
3212.816039	481893.292551	40.388685
3216.275289	482830.294477	40.393703
3219.413490	483765.526351	40.398720
3222.362917	484709.045638	40.403738
3226.001712	485654.113321	40.408756
3229.174876	486597.129844	40.413773
3231.848719	487538.503662	40.418791
3235.238190	488492.403337	40.423808
3238.584286	489428.014676	40.428826
3241.747258	490345.815919	40.433844
3245.030527	491252.612945	40.438861
3248.193607	492161.741340	40.443879
3251.671192	493065.226005	40.448896
3254.393200	493965.752225	40.453914
3257.874709	494880.759532	40.458932
3260.774615	495809.043853	40.463949
3263.975221	496714.112771	40.468967
3267.414711	497644.866508	40.473984
3270.382176	498560.934586	40.479002
3273.839344	499488.749548	40.484020
3276.855758	500432.329672	40.489037
3280.282792	501360.684665	40.494055
3283.768535	502308.247707	40.499072
3286.925004	503249.408351	40.504090
3290.586657	504184.490699	40.509108
3293.862228	505138.090199	40.514125
3297.249218	506085.470112	40.519143
3300.762589	507026.276919	40.524160
3303.888825	507981.571098	40.529178
3307.114766	508936.684694	40.534196
3310.355741	509904.458118	40.539213
3313.899648	510868.194366	40.544231
3316.874961	511843.219247	40.549248
3319.784184	512820.097451	40.554266
3323.411778	513790.760508	40.559284
3326.345274	514788.014630	40.564301
3330.025125	515776.180616	40.569319
3333.766156	516765.623636	40.574336
3336.396122	517766.781697	40.579354
3339.812620	518757.689722	40.584372
3343.146627	519771.963230	40.589389
3346.223684	520783.687679	40.594407
3349.810743	521790.432055	40.599424
3352.896795	522801.802718	40.604442
3357.042032	523805.695952	40.609460
3360.406421	524819.886075	40.614477
3363.928308	525846.234267	40.619495
3367.136411	526856.675740	40.624512
3370.394930	527866.429341	40.629530
3374.095572	528885.329980	40.634548
3377.489155	529913.994108	40.639565
3380.625479	530941.512460	40.644583
3384.333071	531969.564068	40.649600
3387.726752	533001.048204	40.654618
3391.121760	534039.580296	40.659636
3394.495072	535069.446353	40.664653
3397.510631	536101.645252	40.669671
3400.933354	537144.290149	40.674688
3404.392034	538191.713443	40.679706
3408.029804	539232.547717	40.684724
3411.343553	540293.472745	40.689741
3414.278254	541333.139498	40.694759
3417.735688	542385.334760	40.699776
3420.995665	543438.476018	40.704794
3424.619433	544490.619017	40.709812
3427.760750	545557.748421	40.714829
3431.235550	546629.700387	40.719847
3435.367162	547689.770145	40.724864
3438.581815	548752.449302	40.729882
3442.178498	549817.735352	40.734900
3445.539091	550879.405038	40.739917
3448.990332	551944.377853	40.744935
3452.680668	553009.871936	40.749952
3456.341189	554073.371872	40.754970
3459.826951	555125.426105	40.759988
3463.309235	556181.098064	40.765005
3467.127142	557227.643777	40.770010
3470.892193	558227.152648	40.775015
3473.339590	559184.581338	40.780020
3476.460554	560082.700443	40.785024
3479.709235	560940.997841	40.790029
3482.540240	561738.721907	40.795034
3485.522618	562485.941849	40.800039
3488.221999	563179.771618	40.805044
3491.080704	563807.194989	40.810048
3492.899727	564389.450321	40.815053
3495.552400	564908.175306	40.820058
3497.758403	565377.084982	40.825063
3499.257512	565807.021307	40.830068
3501.533452	566164.066891	40.835072
3503.632539	566503.154393	40.840077
3505.511457	566777.398619	40.845082
3506.983734	567019.417071	40.850087
3507.957876	567223.703418	40.855092
3509.424136	567398.389322	40.860096
3510.539527	567526.136310	40.865101
3511.901389	567629.545026	40.870106
3512.778528	567691.058352	40.875111
3513.804727	567737.186012	40.880116
3514.327817	567759.846590	40.885120
3515.156533	567750.681077	40.890125
3515.468419	567719.305790	40.895130
3516.273276	567669.730293	40.900135
3516.751052	567597.162000	40.905140
3517.417989	567514.523008	40.910144
3518.036060	567416.177033	40.915149
3518.330164	567309.546618	40.920154
3518.898653	567168.130321	40.925159
3519.087610	567021.349090	40.930164
3519.389230	566868.272613	40.935168
3519.309616	566704.509025	40.940173
3519.479975	566528.604022	40.945178
3519.747776	566346.304635	40.950183
3520.146090	566151.680644	40.955188
3520.460946	565951.191718	40.960192
3520.345930	565740.422616	40.965197
3520.233886	565521.966696	40.970202
3520.167125	565303.700487	40.975207
3519.969551	565084.396040	40.980212
3520.427038	564866.542214	40.985216
3520.367051	564645.199482	40.990221
3520.275240	564419.438375	40.995226
3520.350406	564175.618503	41.000231
3520.043148	563940.942789	41.005236
3520.066032	563703.951073	41.010240
3519.729448	563458.121288	41.015245
3519.769794	563223.728663	41.020250
3519.824213	562994.351521	41.025255
3519.475730	562748.759839	41.030260
3519.473419	562511.547057	41.035264
3518.986228	562267.624349	41.040269
3519.021002	562029.542222	41.045274
3519.437523	561790.642449	41.050279
3519.025210	561548.802800	41.055284
3518.936101	561308.917125	41.060288
3518.842380	561062.547395	41.065293
3518.357530	560824.421338	41.070298
3518.677167	560592.544985	41.075303
3518.461735	560357.482093	41.080308
3518.284234	560114.622084	41.085312
3517.823357	559880.040030	41.090317
3517.875794	559649.392477	41.095322
3517.936734	559419.191268	41.100327
3517.739320	559173.401235	41.105332
3517.810519	558951.478929	41.110336
3517.475843	558717.557635	41.115341
3517.153906	558481.720537	41.120346
3516.896789	558248.883303	41.125351
3516.784238	558026.218686	41.130356
3516.697374	557802.792233	41.135360
3516.516496	557577.165379	41.140365
3516.065906	557360.419785	41.145370
3516.722240	557144.502975	41.150375
3515.786925	556936.467833	41.155380
3515.774411	556706.577415	41.160384
3515.788387	556490.899528	41.165389
3515.767367	556285.876622	41.170394
3515.122657	556079.540187	41.175399
3515.284958	555872.622339	41.180404
3515.273562	555659.697410	41.185408
3515.419201	555461.670132	41.190413
3514.882090	555264.399170	41.195418
3514.535266	555059.154745	41.200423
3514.179040	554855.265248	41.205428
3514.497756	554664.485321	41.210432
3514.125079	554460.340409	41.215437
3514.332565	554277.361899	41.220442
3514.246907	554086.434717	41.225447
3513.646396	553892.066300	41.230452
3513.819625	553697.323038	41.235456
3513.442569	553524.627424	41.240461
3513.204256	553336.225322	41.245466
3513.370660	553143.786370	41.250471
3513.360908	552974.695102	41.255476
3512.888827	552783.505898	41.260480
3512.921315	552611.085395	41.265485
3512.714933	552439.101758	41.270490
3512.481002	552263.751970	41.275495
3512.204486	552095.041838	41.280500
3512.116019	551925.445510	41.285504
3512.110442	551761.966953	41.290509
3511.991156	551602.525609	41.295514
3512.143457	551429.566991	41.300519
3511.792295	551274.028383	41.305524
3511.664502	551110.660648	41.310528
3511.728096	550946.707928	41.315533
3511.339684	550792.375551	41.320538
3511.686415	550619.727119	41.325543
3511.224527	550477.971062	41.330548
3511.375882	550309.521563	41.335552
3511.151355	550167.724971	41.340557
3511.008848	550010.227254	41.345562
3510.709311	549854.411140	41.350567
3510.878095	549710.436344	41.355572
3510.721920	549561.080206	41.360576
3510.715652	549420.799674	41.365581
3510.050150	549282.279396	41.370586
3510.421744	549140.177022	41.375591
3510.112914	548995.966473	41.380596
3510.311195	548861.932989	41.385600
3509.829711	548717.494623	41.390605
3509.511475	548593.846658	41.395610
3509.788914	548457.684530	41.400615
3509.469666	548322.971440	41.405620
3509.450708	548193.238689	41.410624
3509.569931	548068.109374	41.415629
3509.359797	547946.399232	41.420634
3509.468213	547818.453025	41.425639
3509.148635	547686.146793	41.430644
3509.054226	547561.598744	41.435648
3509.340182	547434.576399	41.440653
3509.240062	547313.597220	41.445658
3508.939494	547182.539855	41.450663
3508.736311	547074.850805	41.455668
3508.454561	546954.147819	41.460672
3508.605890	546840.718738	41.465677
3508.211019	546718.522326	41.470682
3508.718148	546609.863740	41.475687
3507.825995	546496.241837	41.480692
3508.256659	546384.324169	41.485696
3508.076984	546278.485361	41.490701
3507.891166	546169.226636	41.495706
3508.216964	546055.008806	41.500711
3507.661759	545962.050726	41.505716
3507.641671	545845.923310	41.510720
3507.372518	545748.895520	41.515725
3507.737809	545649.052273	41.520730
3507.554832	545543.710666	41.525735
3507.472292	545439.056688	41.530740
3507.533421	545346.350162	41.535744
3507.672026	545247.896987	41.540749
3507.232998	545145.961776	41.545754
3507.578435	545057.031484	41.550759
3507.427851	544956.709676	41.555764
3507.026899	544848.428481	41.560768
3507.426638	544753.854084	41.565773
3507.210867	544668.730504	41.570778
3507.107739	544560.752559	41.575783
3506.813148	544472.722495	41.580788
3507.168701	544374.027450	41.585792
3507.066614	544284.909784	41.590797
3506.584753	544190.116190	41.595802
3506.985456	544089.248896	41.600807
3507.046875	544019.520473	41.605812
3506.526258	543919.348501	41.610816
3507.158799	543839.067221	41.615821
3506.528344	543744.796398	41.620826
3506.930351	543650.917541	41.625831
3506.455462	543567.486794	41.630836
3506.696079	543475.291771	41.635840
3506.307631	543394.361644	41.640845
3506.212020	543315.850377	41.645850
3506.279025	543232.333068	41.650855
3506.313049	543156.315903	41.655860
3506.121274	543072.938411	41.660864
3506.203297	542984.688334	41.665869
3506.065786	542907.086541	41.670874
3506.275809	542827.216674	41.675879
3505.811339	542750.872163	41.680884
3506.148258	542666.755700	41.685888
3505.750281	542582.199644	41.690893
3505.944132	542517.221514	41.695898
3505.856934	542442.828755	41.700903
3506.011910	542373.579692	41.705908
3505.745949	542283.265855	41.710912
3505.765891	542217.961074	41.715917
3506.048027	542150.049351	41.720922
3506.042357	542067.038690	41.725927
3506.069004	542002.285157	41.730932
3505.767000	541918.615283	41.735936
3505.757776	541844.458400	41.740941
3505.769166	541763.103343	41.745946
3505.967151	541685.492103	41.750951
3505.801622	541610.704112	41.755956
3505.854605	541533.416371	41.760960
3506.110210	541460.976948	41.765965
3505.684184	541388.894744	41.770970
3505.844128	541310.582733	41.775975
3505.471946	541240.755396	41.780980
3505.325700	541169.282472	41.785984
3505.918820	541098.901627	41.790989
3505.619381	541024.936020	41.795994
3505.560612	540939.058267	41.800999
3505.480392	540869.032493	41.806004
3505.668960	540804.146973	41.811008
3505.633723	540741.006674	41.816013
3505.297580	540671.522783	41.821018
3505.251836	540597.112664	41.826023
3504.787003	540529.358761	41.831028
3505.409961	540473.460883	41.836032
3504.995518	540396.540811	41.841037
3505.047327	540347.775612	41.846042
3505.211975	540277.507186	41.851047
3504.907423	540207.663605	41.856052
3505.055013	540138.353093	41.861056
3505.339848	540080.744971	41.866061
3505.050267	540021.968015	41.871066
3505.272908	539943.033948	41.876071
3504.904813	539891.212574	41.881076
3504.863729	539823.187669	41.886080
3505.153917	539764.470254	41.891085
3505.053958	539696.403510	41.896090
3504.907241	539631.111271	41.901095
3504.635779	539579.726464	41.906100
3504.682989	539512.239670	41.911104
3505.313391	539461.519168	41.916109
3504.720644	539403.541325	41.921114
3504.720851	539334.953844	41.926119
3504.706175	539279.552494	41.931124
3504.842744	539216.579138	41.936128
3504.797906	539160.427139	41.941133
3504.556673	539098.317134	41.946138
3504.779412	539039.254605	41.951143
3504.800975	538983.796003	41.956148
3504.562923	538916.199462	41.961152
3504.684350	538868.675807	41.966157
3504.810825	538804.947137	41.971162
3504.825551	538745.714321	41.976167
3504.552555	538692.162248	41.981172
3504.199778	538649.844575	41.986176
3504.776261	538583.931171	41.991181
3504.391163	538532.962398	41.996186
3504.532205	538465.405115	42.001191
3504.522584	538422.580365	42.006196
3504.537495	538366.465884	42.011200
3504.401665	538303.832344	42.016205
3504.362115	538247.574837	42.021210
3504.288165	538192.932855	42.026215
3504.353193	538141.288559	42.031220
3504.211365	538084.542990	42.036224
3504.206779	538034.267896	42.041229
3503.704312	537990.310555	42.046234
3504.020765	537945.370076	42.051239
3503.928408	537895.259072	42.056244
3504.170790	537842.277470	42.061248
3504.407385	537798.254785	42.066253
3504.019008	537739.885251	42.071258
3503.908479	537697.325401	42.076263
3503.669587	537658.459308	42.081268
3503.735800	537614.915454	42.086272
3503.781119	537558.188746	42.091277
3503.511393	537515.552407	42.096282
3503.818138	537467.340418	42.101287
3503.880787	537442.267061	42.106292
3503.831213	537386.862901	42.111296
3503.923184	537339.791086	42.116301
3503.698816	537298.052882	42.121306
3504.019649	537254.820482	42.126311
3503.878370	537211.810835	42.131316
3503.972993	537162.926094	42.136320
3503.916532	537119.550629	42.141325
3503.793653	537081.620992	42.146330
3503.868030	537030.474046	42.151335
3503.655316	536978.515953	42.156340
3504.187686	536931.021788	42.161344
3504.054277	536879.252274	42.166349
3503.749876	536844.017709	42.171354
3503.970412	536798.081504	42.176359
3503.883645	536752.494941	42.181364
3503.993237	536704.210093	42.186368
3503.738204	536660.108998	42.191373
3503.730877	536612.697637	42.196378
3503.696542	536569.568523	42.201383
3503.554057	536531.589973	42.206388
3503.634443	536488.493066	42.211392
3503.883992	536438.625135	42.216397
3503.601214	536396.792413	42.221402
3503.957572	536351.437462	42.226407
3503.530724	536313.301184	42.231412
3503.595152	536265.474707	42.236416
3504.005443	536223.936235	42.241421
3503.253146	536183.182544	42.246426
3503.847561	536145.088178	42.251431
3504.078528	536102.721547	42.256436
3503.634472	536055.376083	42.261440
3503.994572	536006.898624	42.266445
3503.693705	535975.939525	42.271450
3503.818845	535911.391273	42.276455
3503.883139	535881.281144	42.281460
3503.795686	535825.725117	42.286464
3503.942977	535790.165687	42.291469
3503.956292	535743.351919	42.296474
3503.750277	535683.233217	42.301479
3503.380048	535642.670027	42.306484
3503.441842	535600.982430	42.311488
3503.707838	535553.121932	42.316493
3503.471385	535529.450447	42.321498
3503.795844	535481.580585	42.326503
3503.727816	535443.889244	42.331508
3503.672667	535408.360261	42.336512
3503.722682	535369.291245	42.341517
3503.449571	535321.211755	42.346522
3503.719276	535277.275931	42.351527
3503.443246	535237.653207	42.356532
3503.320573	535199.315269	42.361536
3503.765701	535156.157131	42.366541
3503.199176	535116.428225	42.371546
3503.484218	535074.100127	42.376551
3503.355773	535041.199103	42.381556
3503.377168	535001.781059	42.386560
3503.609763	534960.517850	42.391565
3503.555454	534929.417182	42.396570
3503.417713	534882.825141	42.401575
3503.427799	534857.301863	42.406580
3503.511476	534809.366293	42.411584
3503.951369	534774.060557	42.416589
3503.450112	534737.290325	42.421594
3503.012556	534684.804197	42.426599
3503.288352	534647.006679	42.431604
3503.266195	534612.678512	42.436608
3503.244289	534569.993807	42.441613
3503.247513	534540.745821	42.446618
3503.471986	534495.656552	42.451623
3503.628289	534460.394088	42.456628
3503.429401	534414.816674	42.461632
3503.197044	534374.228026	42.466637
3502.957380	534339.530255	42.471642
3503.320401	534303.530424	42.476647
3503.066439	534281.721978	42.481652
3503.353068	534236.219403	42.486656
3503.460724	534202.272673	42.491661
3503.049271	534170.873362	42.496666
3503.158111	534129.324704	42.501671
3503.080218	534103.511575	42.506676
3503.327722	534072.563241	42.511680
3503.420445	534038.819773	42.516685
3503.332610	533991.008535	42.521690
3503.497867	533947.436830	42.526695
3503.282761	533915.100181	42.531700
3503.552357	533880.976380	42.536704
3503.662079	533837.664659	42.541709
3503.188203	533794.997380	42.546714
3503.191931	533756.887195	42.551719
3503.301619	533720.623105	42.556724
3503.204312	533683.031856	42.561728
3503.104010	533654.049688	42.566733
3503.468936	533613.365703	42.571738
3503.098537	533575.766295	42.576743
3503.341596	533538.876818	42.581748
3502.931579	533499.370286	42.586752
3503.247765	533474.149048	42.591757
3503.206966	533443.948891	42.596762
3503.452652	533405.296577	42.601767
3503.189001	533371.455790	42.606772
3503.263081	533333.987890	42.611776
3503.215948	533301.623567	42.616781
3503.281655	533263.451939	42.621786
3503.235379	533221.521744	42.626791
3503.293074	533182.797329	42.631796
3503.109407	533150.403529	42.636800
3503.363626	533107.771715	42.641805
3503.166418	533076.286057	42.646810
3503.372686	533032.704890	42.651815
3503.381475	532989.708114	42.656820
3503.234146	532967.528433	42.661824
3503.176947	532918.651197	42.666829
3503.118387	532888.200777	42.671834
3503.550721	532846.194890	42.676839
3503.255600	532811.602338	42.681844
3503.215154	532780.695726	42.686848
3503.100850	532744.816189	42.691853
3503.167011	532713.590746	42.696858
3503.268569	532680.496875	42.701863
3503.161120	532650.103851	42.706868
3502.868835	532619.437433	42.711872
3502.950166	532583.174573	42.716877
3502.892085	532549.148605	42.721882
3503.002512	532517.513021	42.726887
3502.927080	532485.906282	42.731892
3502.877053	532454.094120	42.736896
3503.205928	532413.965814	42.741901
3503.370061	532381.364925	42.746906
3503.334724	532358.562594	42.751911
3503.048255	532318.882188	42.756916
3502.777475	532290.578030	42.761920
3502.966410	532251.125530	42.766925
3502.745283	532222.108612	42.771930
3503.099580	532178.249798	42.776935
3502.978002	532154.302499	42.781940
3503.358081	532125.191809	42.786945
3503.342724	532085.116055	42.791949
3503.037829	532061.348159	42.796954
3503.108983	532023.625184	42.801959
3503.014238	531987.891560	42.806964
3503.256140	531950.695651	42.811969
3503.442758	531921.111110	42.816973
3502.927758	531890.024474	42.821978
3503.073594	531846.901887	42.826983
3503.433327	531810.492848	42.831988
3503.073435	531784.165125	42.836993
3503.441275	531739.396414	42.841997
3503.494784	531713.407023	42.847002
3503.276202	531666.211769	42.852007
3503.542487	531626.493584	42.857012
3503.236403	531588.525942	42.862017
3503.234797	531558.466354	42.867021
3503.142586	531524.644421	42.872026
3503.191180	531484.053348	42.877031
3503.188820	531450.267592	42.882036
3503.554619	531422.668115	42.887041
3503.083678	531377.625870	42.892045
3503.045425	531342.334852	42.897050
3503.398221	531299.732125	42.902055
3503.326239	531271.696928	42.907060
3503.285428	531229.306278	42.912065
3503.191582	531193.519981	42.917069
3502.940723	531155.038952	42.922074
3503.089922	531125.257016	42.927079
3503.268606	531087.111770	42.932084
3502.922014	531055.996933	42.937089
3502.765765	531008.034291	42.942093
3502.769066	530991.719173	42.947098
3502.721675	530964.233379	42.952103
3503.145375	530931.638825	42.957108
3503.036441	530909.449655	42.962113
3503.457517	530868.144100	42.967117
3503.256110	530834.589141	42.972122
3503.203594	530797.284695	42.977127
3502.714278	530773.291371	42.982132
3502.682544	530743.284946	42.987137
3502.999210	530717.101556	42.992141
3502.978283	530684.676285	42.997146
3502.944360	530651.195501	43.002151
3502.956531	530623.246525	43.007156
3502.976583	530582.153536	43.012161
3502.822631	530551.410360	43.017165
3502.326830	530528.172924	43.022170
3502.877950	530495.507101	43.027175
3503.022955	530461.897277	43.032180
3503.246893	530435.324907	43.037185
3503.460378	530405.229191	43.042189
3503.150890	530373.200543	43.047194
3503.226294	530323.487232	43.052199
3503.034316	530296.375026	43.057204
3502.695438	530263.796763	43.062209
3503.172074	530216.941288	43.067213
3502.955537	530200.558678	43.072218
3502.840710	530160.492489	43.077223
3502.843804	530130.630309	43.082228
3502.569824	530097.386891	43.087233
3503.032142	530069.568112	43.092237
3502.749133	530044.785984	43.097242
3502.661683	530004.060409	43.102247
3502.553187	529984.488192	43.107252
3502.629106	529961.664356	43.112257
3503.021520	529926.201781	43.117261
3502.790310	529902.519194	43.122266
3502.866912	529865.242355	43.127271
3502.882147	529838.147312	43.132276
3502.513245	529824.607998	43.137281
3503.181384	529788.246054	43.142285
3502.886581	529746.041193	43.147290
3503.105368	529722.791842	43.152295
3502.882442	529690.395541	43.157300
3502.592169	529657.455692	43.162305
3503.149119	529630.578076	43.167309
3502.947344	529601.250160	43.172314
3502.833759	529564.807807	43.177319
3502.816609	529532.681250	43.182324
3502.598717	529500.686571	43.187329
3502.728461	529470.551382	43.192333
3502.654213	529452.282388	43.197338
3502.469813	529430.958568	43.202343
3502.812345	529404.516733	43.207348
3502.505224	529380.845016	43.212353
3502.743940	529343.037867	43.217357
3502.633095	529322.054943	43.222362
3502.459655	529287.534819	43.227367
3502.552715	529267.074041	43.232372
3502.658200	529249.683283	43.237377
3502.881630	529210.165876	43.242381
3502.918019	529175.663167	43.247386
3502.831598	529153.820041	43.252391
3502.925693	529123.437799	43.257396
3502.973535	529084.350225	43.262401
3503.088765	529047.467940	43.267405
3503.036729	529019.676619	43.272410
3503.366526	528992.530880	43.277415
3503.021710	528961.360419	43.282420
3502.917842	528923.806821	43.287425
3503.344747	528893.523343	43.292429
3502.841433	528862.629121	43.297434
3502.993077	528825.337652	43.302439
3502.911416	528796.593589	43.307444
3502.744261	528761.718570	43.312449
3502.903169	528732.584396	43.317453
3502.575221	528718.282127	43.322458
3502.873474	528680.060908	43.327463
3502.993160	528647.356903	43.332468
3502.779874	528621.856156	43.337473
3503.247538	528592.069271	43.342477
3503.166894	528554.309552	43.347482
3502.888092	528523.732136	43.352487
3502.524267	528485.210473	43.357492
3502.895107	528461.481961	43.362497
3502.989422	528424.550822	43.367501
3502.821007	528400.049933	43.372506
3502.934172	528369.914802	43.377511
3502.971133	528333.395242	43.382516
3502.992821	528307.353681	43.387521
3502.775026	528266.441543	43.392525
3502.632558	528252.865367	43.397530
3502.962474	528221.991069	43.402535
3502.929486	528186.640368	43.407540
3502.826874	528162.279890	43.412545
3502.847426	528116.696655	43.417549
3503.084025	528096.211720	43.422554
3502.852585	528064.266016	43.427559
3503.313219	528034.579698	43.432564
3502.968967	528000.536060	43.437569
3503.562989	527961.460890	43.442573
3503.009309	527937.069457	43.447578
3502.781817	527891.121117	43.452583
3503.169924	527869.504211	43.457588
3503.088309	527831.944035	43.462593
3502.902371	527794.500717	43.467597
3502.522199	527769.477581	43.472602
3502.674171	527736.766294	43.477607
3503.084269	527709.555054	43.482612
3502.808464	527678.219713	43.487617
3503.058681	527651.436165	43.492621
3503.134648	527614.555979	43.497626
3502.930547	527575.049831	43.502631
3502.794830	527545.354481	43.507636
3502.827921	527520.065094	43.512641
3502.821178	527483.701085	43.517645
3502.766767	527465.023308	43.522650
3502.703777	527429.473777	43.527655
3502.722990	527404.891473	43.532660
3502.198318	527380.947802	43.537665
3502.512158	527349.066615	43.542669
3502.408102	527331.957774	43.547674
3502.550063	527304.434852	43.552679
3502.923856	527283.524367	43.557684
3502.388967	527248.601830	43.562689
3502.352648	527219.041382	43.567693
3502.235528	527207.122333	43.572698
3502.430572	527180.749363	43.577703
3502.664197	527144.397384	43.582708
3502.699063	527127.770345	43.587713
3502.507656	527092.542102	43.592717
3502.537680	527079.491930	43.597722
3502.654579	527055.850782	43.602727
3502.627063	527020.899058	43.607732
3502.483498	527005.155903	43.612737
3502.798699	526970.553667	43.617741
3502.688908	526943.975816	43.622746
3502.517834	526920.429607	43.627751
3502.954194	526893.917776	43.632756
3502.564090	526868.692998	43.637761
3502.493902	526837.071817	43.642765
3502.782026	526810.381407	43.647770
3502.535672	526775.110500	43.652775
3502.682717	526750.507088	43.657780
3502.294861	526729.512771	43.662785
3502.916835	526696.473924	43.667789
3502.570645	526674.163411	43.672794
3502.693040	526648.254019	43.677799
3502.732206	526622.156045	43.682804
3502.547141	526589.947704	43.687809
3502.824252	526554.745864	43.692813
3502.741967	526543.828211	43.697818
3502.407255	526519.500821	43.702823
3502.691829	526494.674050	43.707828
3502.339610	526461.735844	43.712833
3502.532206	526431.533563	43.717837
3502.333410	526418.065006	43.722842
3502.181634	526394.313373	43.727847
3502.635674	526359.486453	43.732852
3502.624390	526336.569169	43.737857
3502.353861	526314.749992	43.742861
3502.506218	526287.374455	43.747866
3502.622747	526265.343850	43.752871
3502.608066	526238.749783	43.757876
3502.244854	526212.965478	43.762881
3502.866482	526186.725638	43.767885
3502.504536	526164.517462	43.772890
3502.324488	526136.236268	43.777895
3502.287106	526105.313447	43.782900
3502.519088	526087.949216	43.787905
3502.540325	526062.810009	43.792909
3502.431371	526043.282380	43.797914
3502.622891	526021.340446	43.802919
3502.654707	525996.854313	43.807924
3502.414484	525974.626877	43.812929
3502.766492	525940.570331	43.817933
3502.097324	525909.846115	43.822938
3502.354640	525903.761284	43.827943
3502.309899	525873.594667	43.832948
3502.401508	525859.526245	43.837953
3502.051348	525821.599165	43.842957
3502.189013	525820.116902	43.847962
3502.137810	525793.275759	43.852967
3502.465852	525773.125620	43.857972
3502.116366	525749.554720	43.862977
3502.166701	525721.186417	43.867981
3502.355522	525712.492716	43.872986
3502.285023	525685.855854	43.877991
3502.432536	525664.675789	43.882996
3502.339885	525645.699153	43.888001
3502.661746	525617.842493	43.893005
3502.589512	525586.823141	43.898010
3502.357153	525557.591740	43.903015
3502.826910	525540.189794	43.908020
3502.448302	525517.277882	43.913025
3502.530046	525496.762656	43.918029
3502.176969	525476.012812	43.923034
3502.512065	525439.136626	43.928039
3502.625504	525424.157598	43.933044
3502.474050	525396.273379	43.938049
3502.435970	525370.235341	43.943053
3502.617347	525347.638997	43.948058
3502.438655	525329.733179	43.953063
3502.762130	525296.032053	43.958068
3502.655643	525276.805166	43.963073
3502.756018	525245.204026	43.968077
3502.605359	525222.709515	43.973082
3502.634091	525192.177288	43.978087
3502.054076	525163.754759	43.983092
3502.271017	525143.318702	43.988097
3502.782417	525114.172094	43.993101
3502.743189	525105.261603	43.998106
3502.511037	525065.147823	44.003111
3502.781944	525041.479125	44.008116
3502.424340	525014.079572	44.013121
3502.273543	524982.265011	44.018125
3502.620623	524958.936950	44.023130
3502.413046	524936.853826	44.028135
3502.380640	524908.194406	44.033140
3502.130554	524879.518420	44.038145
3502.308916	524863.823381	44.043149
3502.303353	524846.041103	44.048154
3502.385802	524826.733788	44.053159
3502.744016	524800.330704	44.058164
3502.276277	524771.587601	44.063169
3502.513431	524747.369482	44.068173
3502.481459	524723.948863	44.073178
3502.267507	524700.657276	44.078183
3502.532792	524679.507698	44.083188
3502.512183	524666.513413	44.088193
3503.041860	524632.224367	44.093197
3502.689838	524617.216108	44.098202
3502.169984	524581.024750	44.103207
3502.640743	524552.890805	44.108212
3502.132014	524537.201546	44.113217
3502.175794	524496.640089	44.118221
3502.119686	524488.336355	44.123226
3502.202623	524466.308002	44.128231
3502.186423	524444.496553	44.133236
3502.180614	524433.313372	44.138241
3502.109485	524413.172918	44.143245
3502.286110	524395.714341	44.148250
3502.318773	524376.514880	44.153255
3502.210522	524346.858477	44.158260
3502.203074	524322.375376	44.163265
3502.196890	524306.708401	44.168269
3502.206727	524278.192191	44.173274
3502.250163	524258.386331	44.178279
3502.513502	524235.019659	44.183284
3502.517580	524216.277832	44.188289
3502.300175	524185.932743	44.193293
3502.472145	524167.315859	44.198298
3502.188998	524154.160411	44.203303
3502.422673	524122.938909	44.208308
3502.350758	524095.644149	44.213313
3502.288056	524068.247140	44.218317
3502.619335	524048.597698	44.223322
3502.693208	524034.227831	44.228327
3502.137498	523994.715363	44.233332
3502.550055	523986.136865	44.238337
3502.373726	523960.016826	44.243341
3502.137591	523940.959329	44.248346
3501.872494	523920.495652	44.253351
3502.190613	523893.139785	44.258356
3502.332518	523881.429348	44.263361
3502.486260	523856.517264	44.268365
3502.523779	523840.691799	44.273370
3502.350943	523809.331300	44.278375
3502.477443	523783.063029	44.283380
3502.435343	523763.320128	44.288385
3502.560793	523740.024431	44.293389
3502.238880	523717.150979	44.298394
3502.407287	523693.445465	44.303399
3502.872662	523660.373094	44.308404
3502.498907	523637.356427	44.313409
3502.511336	523614.128481	44.318413
3502.260643	523597.138413	44.323418
3502.413597	523570.311408	44.328423
3502.670430	523537.271185	44.333428
3502.454227	523522.845144	44.338433
3502.563263	523506.202040	44.343437
3502.675164	523463.762707	44.348442
3502.285705	523438.128256	44.353447
3502.737318	523409.894128	44.358452
3502.280856	523384.773827	44.363457
3502.522037	523362.970947	44.368461
3502.732235	523337.696434	44.373466
3502.350119	523309.591833	44.378471
3502.455802	523285.693827	44.383476
3502.248865	523265.824694	44.388481
3502.209899	523238.069610	44.393485
3502.343559	523222.782670	44.398490
3502.727248	523192.543323	44.403495
3502.815014	523179.178045	44.408500
3502.543751	523157.958408	44.413505
3502.670902	523121.662411	44.418509
3502.621746	523104.690740	44.423514
3502.376110	523076.715564	44.428519
3502.391104	523039.630656	44.433524
3501.946485	523026.599992	44.438529
3502.609382	522998.080200	44.443533
3502.640409	522979.533984	44.448538
3502.541269	522955.213805	44.453543
3502.122472	522928.927948	44.458548
3502.524390	522902.363172	44.463553
3502.430694	522878.495467	44.468557
3502.104859	522850.381144	44.473562
3502.349447	522844.448063	44.478567
3502.370740	522811.341937	44.483572
3502.247426	522792.617941	44.488577
3502.172934	522772.223617	44.493581
3502.553531	522749.037651	44.498586
3502.608029	522723.685442	44.503591
3502.563842	522700.263182	44.508596
3502.645310	522682.917954	44.513601
3502.443446	522651.156178	44.518605
3502.628608	522629.713523	44.523610
3502.140122	522607.569493	44.528615
3502.303072	522590.413008	44.533620
3502.246909	522559.535284	44.538625
3502.178823	522546.395172	44.543629
3502.365969	522514.874854	44.548634
3502.532226	522497.213877	44.553639
3502.556964	522472.923933	44.558644
3501.854639	522443.960394	44.563649
3502.088428	522422.106752	44.568653
3502.086150	522415.204171	44.573658
3502.188788	522392.161617	44.578663
3502.254024	522368.016341	44.583668
3502.172940	522342.482965	44.588673
3502.080378	522318.966795	44.593677
3502.008588	522299.276747	44.598682
3502.523528	522286.599909	44.603687
3502.506454	522256.068114	44.608692
3502.025935	522243.294207	44.613697
3502.152243	522215.662452	44.618701
3502.361539	522200.916838	44.623706
3502.189017	522183.761652	44.628711
3502.333322	522156.782009	44.633716
3502.260331	522137.746946	44.638721
3502.336139	522113.398018	44.643725
3502.185011	522081.375063	44.648730
3502.235564	522076.126877	44.653735
3502.469939	522042.632988	44.658740
3502.269140	522031.427758	44.663745
3502.287878	522010.413117	44.668749
3502.267974	521984.667991	44.673754
3501.987131	521965.161148	44.678759
3502.549454	521928.391109	44.683764
3502.173122	521914.895242	44.688769
3501.591695	521907.629030	44.693773
3501.996918	521897.135595	44.698778
3502.069008	521875.860501	44.703783
3502.123647	521854.588088	44.708788
3501.941376	521837.736308	44.713793
3502.155044	521821.226003	44.718797
3502.025368	521808.245919	44.723802
3501.708945	521787.484640	44.728807
3501.725060	521760.372986	44.733812
3501.773191	521765.202809	44.738817
3502.149599	521746.903481	44.743821
3502.419836	521722.825926	44.748826
3501.958860	521705.866183	44.753831
3502.224360	521674.684430	44.758836
3501.952249	521675.230656	44.763841
3502.412000	521647.293902	44.768845
3502.106002	521616.150556	44.773850
3501.860578	521605.203862	44.778855
3501.772446	521583.298177	44.783860
3502.030197	521577.211324	44.788865
3502.218055	521547.754601	44.793869
3502.421646	521532.202912	44.798874
3502.292307	521516.803793	44.803879
3502.391579	521498.748814	44.808884
3501.996091	521475.580649	44.813889
3502.197904	521456.602639	44.818893
3501.870523	521438.563582	44.823898
3502.349693	521415.410376	44.828903
3502.566419	521391.038215	44.833908
3502.300571	521386.040558	44.838913
3502.108678	521352.661679	44.843917
3502.115366	521335.679086	44.848922
3502.179198	521303.872784	44.853927
3502.417870	521282.722004	44.858932
3502.247121	521262.894667	44.863937
3502.055057	521235.965526	44.868941
3502.474139	521214.333049	44.873946
3501.706971	521202.509790	44.878951
3501.929616	521185.493403	44.883956
3502.302203	521173.089631	44.888961
3502.207560	521151.990515	44.893965
3502.174528	521124.582885	44.898970
3501.867475	521123.471660	44.903975
3501.938476	521098.264999	44.908980
3502.274403	521078.912851	44.913985
3502.352962	521057.786635	44.918989
3502.189525	521046.020465	44.923994
3502.078433	521033.389483	44.928999
3502.326935	521003.922138	44.934004
3502.006092	520996.362921	44.939009
3502.033521	520963.200908	44.944013
3501.998612	520946.526649	44.949018
3501.998713	520933.122393	44.954023
3501.987417	520908.482495	44.959028
3502.004995	520892.404705	44.964033
3502.152678	520872.628028	44.969037
3502.707920	520850.016331	44.974042
3502.480587	520836.042664	44.979047
3502.127805	520796.388415	44.984052
3502.255479	520788.708895	44.989057
3502.505960	520776.222977	44.994061
3502.376151	520732.099306	44.999066
3502.241698	520726.929779	45.004071
3502.280867	520689.481892	45.009076
3501.947428	520687.921201	45.014081
3502.395755	520654.037827	45.019085
3502.904934	520637.177734	45.024090
3502.022657	520607.784704	45.029095
3502.196381	520590.019285	45.034100
3502.188807	520559.683745	45.039105
3502.032977	520537.938079	45.044109
3501.664049	520522.726288	45.049114
3501.906997	520520.068016	45.054119
3502.253599	520495.069311	45.059124
3502.159753	520476.740659	45.064129
3502.121543	520466.667878	45.069133
3502.005167	520437.558442	45.074138
3502.018055	520436.095010	45.079143
3502.215576	520413.487858	45.084148
3502.092693	520393.903767	45.089153
3501.935033	520374.073089	45.094157
3502.067311	520342.354663	45.099162
3501.895592	520334.066351	45.104167
3502.112541	520314.479657	45.109172
3502.380522	520304.510291	45.114177
3501.895488	520269.360160	45.119181
3502.171624	520244.825509	45.124186
3502.250026	520234.482437	45.129191
3502.357055	520208.764568	45.134196
3502.067338	520203.518212	45.139201
3501.787805	520172.669785	45.144205
3502.052363	520175.652290	45.149210
3501.425617	520168.291394	45.154215
3502.131573	520133.913078	45.159220
3502.065293	520118.905711	45.164225
3502.164145	520102.562361	45.169229
3502.131609	520075.908455	45.174234
3502.010510	520060.607183	45.179239
3501.795074	520034.183236	45.184244
3502.092886	520028.240642	45.189249
3502.085675	520006.773367	45.194253
3501.651648	519981.290448	45.199258
3502.190586	519974.705563	45.204263
3502.191665	519953.236914	45.209268
3501.469773	519941.607079	45.214273
3501.808173	519937.371579	45.219277
3501.762861	519908.350739	45.224282
3502.127361	519892.923317	45.229287
3502.231534	519888.623459	45.234292
3502.216455	519865.443728	45.239297
3501.755980	519843.996333	45.244301
3502.335643	519823.142985	45.249306
3502.238080	519819.227270	45.254311
3502.004249	519799.054831	45.259316
3502.222913	519776.040159	45.264321
3502.220870	519755.579606	45.269325
3502.414826	519733.123065	45.274330
3502.107732	519716.388854	45.279335
3502.440546	519684.940064	45.284340
3502.223725	519672.626644	45.289345
3501.971598	519649.785812	45.294349
3502.314446	519632.295202	45.299354
3501.929067	519614.212336	45.304359
3502.150807	519596.387748	45.309364
3502.172361	519568.867682	45.314369
3502.218501	519549.760038	45.319373
3502.562855	519525.767841	45.324378
3501.975001	519511.294538	45.329383
3502.129792	519488.642100	45.334388
3502.088466	519471.715038	45.339393
3502.398274	519455.741262	45.344397
3502.507137	519422.865192	45.349402
3502.172379	519397.768908	45.354407
3501.852620	519376.702055	45.359412
3502.275963	519369.227712	45.364417
3501.899194	519349.631222	45.369421
3502.023871	519331.367811	45.374426
3501.791523	519316.083011	45.379431
3501.838881	519295.412486	45.384436
3501.870568	519284.269593	45.389441
3501.495608	519271.526835	45.394445
3501.843777	519249.499080	45.399450
3501.849156	519249.095049	45.404455
3501.977486	519226.143903	45.409460
3501.887053	519210.584909	45.414465
3501.644757	519193.386384	45.419469
3501.939869	519184.117554	45.424474
3502.246337	519167.841570	45.429479
3502.285322	519146.466543	45.434484
3502.100493	519132.988489	45.439489
3502.272966	519118.598044	45.444493
3501.946961	519090.828703	45.449498
3501.778947	519075.130431	45.454503
3501.659798	519070.764269	45.459508
3501.804952	519043.828692	45.464513
3501.981497	519023.036852	45.469517
3501.887823	519012.215638	45.474522
3501.857448	519005.668483	45.479527
3502.025364	518978.578038	45.484532
3502.047146	518975.903485	45.489537
3501.633557	518954.044192	45.494541
3502.021282	518935.789717	45.499546
3501.760345	518928.824809	45.504551
3501.990699	518901.623697	45.509556
3501.781687	518881.546831	45.514561
3501.734912	518883.368482	45.519565
3501.568583	518858.194591	45.524570
3501.779078	518856.750638	45.529575
3502.125345	518831.547331	45.534580
3502.011978	518811.253879	45.539585
3502.380258	518802.225403	45.544589
3501.854608	518775.897679	45.549594
3502.135029	518779.432424	45.554599
3502.054403	518752.985005	45.559604
3502.034535	518716.700065	45.564609
3502.099105	518714.825204	45.569613
3502.132489	518675.860662	45.574618
3502.214425	518675.898303	45.579623
3502.338232	518655.013308	45.584628
3502.433453	518637.207154	45.589633
3501.955732	518612.736471	45.594637
3502.436766	518588.469353	45.599642
3502.408044	518569.019178	45.604647
3501.999296	518546.200863	45.609652
3502.424750	518528.393579	45.614657
3501.981212	518500.994129	45.619661
3502.267653	518486.383679	45.624666
3501.679210	518466.113239	45.629671
3501.850624	518439.877997	45.634676
3501.836618	518432.874410	45.639681
3501.827515	518420.426728	45.644685
3501.847428	518415.383500	45.649690
3501.882158	518397.284039	45.654695
3501.764580	518376.688187	45.659700
3502.188084	518364.525944	45.664705
3502.015380	518338.142450	45.669709
3502.037113	518307.646118	45.674714
3501.882581	518306.863730	45.679719
3501.999514	518277.914968	45.684724
3501.872283	518276.624313	45.689729
3501.908340	518268.957628	45.694733
3502.435387	518239.037733	45.699738
3502.532362	518233.428025	45.704743
3502.524423	518199.458339	45.709748
3502.613508	518172.983386	45.714753
3502.595685	518152.674085	45.719757
3503.070690	518125.634965	45.724762
3502.775927	518101.689317	45.729767
3502.575393	518062.910632	45.734772
3502.545374	518039.074884	45.739777
3502.867806	518014.428208	45.744781
3502.625222	517988.206120	45.749786
3502.455967	517960.158066	45.754791
3502.798553	517933.592798	45.759796
3502.330026	517912.546828	45.764801
3502.499405	517882.530602	45.769805
3502.388910	517859.110288	45.774810
3502.127750	517810.713294	45.779815
3501.951398	517744.510440	45.784820
3502.199256	517627.333185	45.789825
3501.661233	517467.836521	45.794829
3501.527823	517255.550993	45.799834
3501.680573	517011.007999	45.804839
3501.237302	516698.654606	45.809844
3501.048837	516348.699931	45.814849
3500.332147	515932.327451	45.819853
3499.672464	515476.108061	45.824858
3499.084141	514994.958080	45.829863
3498.205690	514451.068997	45.834868
3497.604930	513873.537057	45.839873
3497.148658	513252.193978	45.844877
3496.677414	512570.066353	45.849882
3495.431073	511868.612280	45.854887
3494.517000	511096.774926	45.859892
3493.563673	510302.257742	45.864897
3492.284757	509452.269188	45.869901
3491.576366	508564.867682	45.874906
3490.024249	507640.165565	45.879911
3488.866845	506673.725727	45.884916
3487.723384	505658.486092	45.889921
3486.251634	504606.295315	45.894925
3484.898375	503507.338238	45.899930
3483.317369	502384.970351	45.904935
3481.943686	501220.498085	45.909940
3480.621324	500011.866849	45.914945
3478.853670	498764.796190	45.919949
3477.355666	497473.966521	45.924954
3475.550752	496161.062178	45.929959
3474.226281	494798.037233	45.934964
3472.379911	493402.402985	45.939969
3470.211416	491977.654509	45.944973
3468.140423	490521.093007	45.949978
3466.248823	489034.667013	45.954983
3464.263300	487510.228671	45.959988
3462.679200	485954.964517	45.964993
3460.609242	484370.115706	45.969997
3458.704316	482744.861631	45.975002
3456.486134	481098.112941	45.980007
3454.077166	479419.586263	45.985012
3452.044504	477705.494950	45.990017
3449.442406	475984.281992	45.995021
3447.075248	474218.918379	46.000026
3445.053508	472428.282372	46.005031
3442.521447	470606.533845	46.010036
3439.857971	468757.296517	46.015041
3437.444075	466900.025235	46.020045
3435.500667	465016.728681	46.025050
3432.909751	463095.939071	46.030055
3430.217721	461174.289919	46.035060
3427.657995	459205.298125	46.040065
3424.871743	457226.401006	46.045069
3422.629298	455219.561731	46.050074
3419.761228	453197.861547	46.055079
3417.014694	451145.995011	46.060084
3413.868226	449080.539301	46.065089
3411.193538	446995.989320	46.070093
3408.655099	444884.088425	46.075098
3405.429880	442771.646991	46.080103
3402.693231	440624.802335	46.085108
3399.759982	438470.195262	46.090113
3396.844321	436299.737219	46.095117
3394.267810	434102.431323	46.100122
3391.005323	431899.611857	46.105127
3387.917612	429670.874356	46.110132
3385.241018	427425.654027	46.115137
3382.288932	425179.667521	46.120141
3379.234793	422892.080672	46.125146
3376.220615	420605.804288	46.130151
3372.963193	418297.915816	46.135156
3369.605288	415981.067058	46.140161
3366.256569	413653.871786	46.145165
3363.187904	411305.483638	46.150170
3360.165306	408954.907970	46.155175
3356.646954	406590.918006	46.160180
3353.492085	404225.404319	46.165185
3350.018522	401835.843851	46.170189
3347.093191	399422.148348	46.175194
3343.480739	397016.989396	46.180199
3339.922016	394590.867623	46.185204
3336.903139	392171.270201	46.190209
3333.152548	389737.051616	46.195213
3329.961924	387285.649063	46.200218
3326.318040	384838.013418	46.205223
3322.599507	382383.882716	46.210228
3319.447568	379912.315375	46.215233
3315.784247	377448.392795	46.220237
3312.519105	374972.650170	46.225242
3309.007033	372487.246016	46.230247
3305.667587	369983.580441	46.235252
3301.902611	367471.069727	46.240257
3298.007796	364974.468321	46.245261
3294.737143	362461.039417	46.250266
3290.991033	359942.821665	46.255271
3287.813301	357433.887812	46.260276
3284.054665	354912.386340	46.265281
3280.275505	352377.265048	46.270285
3276.986807	349840.774452	46.275290
3273.300090	347298.938036	46.280295
3269.422884	344768.888183	46.285300
3265.966380	342225.338484	46.290305
3262.141582	339675.431148	46.295309
3258.670834	337124.193441	46.300314
3254.696572	334560.038421	46.305319
3250.891799	332003.871250	46.310324
3247.244351	329444.279002	46.315329
3243.480721	326889.905497	46.320333
3239.677359	324329.856152	46.325338
3235.820817	321786.676296	46.330343
3231.888242	319224.198302	46.335348
3228.122833	316672.560834	46.340353
3224.066058	314122.044994	46.345357
3220.505552	311564.338833	46.350362
3216.627911	309016.621705	46.355367
3212.840999	306463.617418	46.360372
3209.165335	303915.658786	46.365377
3205.312024	301364.396672	46.370381
3201.575723	298807.523562	46.375386
3197.498139	296268.964124	46.380391
3193.339463	293727.378766	46.385396
3189.437651	291186.995104	46.390401
3185.410215	288645.560277	46.395405
3181.294144	286122.293019	46.400410
3177.488390	283592.544206	46.405415
3173.514504	281069.274090	46.410420
3169.779546	278553.391441	46.415425
3165.786829	276052.591095	46.420429
3161.801240	273538.650700	46.425434
3158.006313	271043.270917	46.430439
3154.029138	268536.493854	46.435444
3150.041830	266045.873198	46.440449
3145.484656	263547.768035	46.445453
3141.916031	261052.583579	46.450458
3137.490987	258582.409602	46.455463
3133.855746	256106.868635	46.460468
3129.982953	253642.651821	46.465473
3126.003546	251186.457789	46.470477
3121.982309	248738.433273	46.475482
3117.840615	246299.154744	46.480487
3113.492130	243851.550463	46.485492
3109.423213	241428.274821	46.490497
3105.684167	239001.792726	46.495501
3101.975341	236592.554655	46.500506
3097.335463	234184.795954	46.505511
3093.676781	231784.538783	46.510516
3089.708027	229383.226218	46.515521
3085.135213	227005.790660	46.520525
3081.181909	224635.006286	46.525530
3077.238348	222269.341224	46.530535
3072.872445	219919.257268	46.535540
3068.527563	217574.399053	46.540545
3064.146357	215247.640299	46.545549
3060.153481	212923.305489	46.550554
3055.922813	210614.483939	46.555559
3051.435456	208322.454642	46.560564
3047.545016	206044.591397	46.565569
3042.989331	203784.480253	46.570573
3039.205526	201524.403789	46.575578
3034.672762	199282.504711	46.580583
3030.786006	197045.223496	46.585588
3026.607361	194825.568998	46.590593
3021.748814	192617.491665	46.595597
3017.782366	190423.753800	46.600602
3013.219435	188254.876571	46.605607
3008.632383	186102.343333	46.610612
3004.296720	183960.561588	46.615617
2999.879691	181842.596458	46.620621
2995.428950	179741.006228	46.625626
2990.646757	177654.565277	46.630631
2986.405760	175593.310708	46.635636
2982.014245	173551.532689	46.640641
2977.090539	171522.849854	46.645645
2972.302567	169516.120922	46.650650
2967.693128	167554.443032	46.655655
2963.145279	165596.845456	46.660660
2958.257068	163672.336912	46.665665
2953.456488	161761.591993	46.670669
2948.496226	159889.621574	46.675674
2943.453809	158056.182653	46.680679
2938.314897	156236.050578	46.685684
2933.133063	154426.442875	46.690689
2927.068812	152630.761293	46.695693
2921.371950	150928.513160	46.700698
2915.770982	149292.233640	46.705703
2909.232658	147704.314438	46.710708
2902.928656	146152.506879	46.715713
2895.952302	144675.669738	46.720717
2889.280529	143237.891009	46.725722
2882.756612	141876.103504	46.730727
2876.805735	140564.877952	46.735732
2870.370709	139313.077757	46.740737
2864.458690	138101.419968	46.745741
2859.237705	136953.615463	46.750746
2853.644935	135843.020118	46.755751
2848.899372	134785.420238	46.760756
2843.738425	133763.555169	46.765761
2838.431504	132777.533450	46.770765
2834.141513	131818.649017	46.775770
2829.714025	130895.093864	46.780775
2824.973312	129998.536064	46.785780
2820.638511	129135.133143	46.790785
2816.270577	128299.965420	46.795789
2812.379432	127475.182880	46.800794
2808.121912	126680.287648	46.805799
2803.945900	125901.586381	46.810804
2800.284180	125138.133328	46.815809
2796.282466	124395.275273	46.820813
2792.409092	123661.809797	46.825818
2788.492307	122942.341710	46.830823
2784.583572	122230.401677	46.835828
2780.910409	121546.225838	46.840833
2777.325384	120861.437830	46.845837
2773.820137	120183.186109	46.850842
2770.250293	119515.231656	46.855847
2765.969393	118864.630661	46.860852
2762.209078	118204.333377	46.865857
2758.489364	117582.012131	46.870861
2754.634761	116951.609311	46.875866
2750.731080	116337.857111	46.880871
2746.905605	115726.836739	46.885876
2742.887504	115135.489102	46.890881
2739.077273	114537.735569	46.895885
2735.252452	113958.024011	46.900890
2731.853224	113375.114892	46.905895
2728.107420	112818.346830	46.910900
2724.617428	112256.525357	46.915905
2720.380595	111704.021321	46.920909
2716.879529	111153.343884	46.925914
2713.214775	110625.293002	46.930919
2709.234800	110084.203984	46.935924
2706.005500	109539.344993	46.940929
2702.037949	109022.349757	46.945933
2698.707264	108487.693588	46.950938
2695.063633	107979.766030	46.955943
2691.708965	107462.927502	46.960948
2688.480470	106942.250639	46.965953
2684.657672	106435.238243	46.970957
2681.498061	105918.596080	46.975962
2677.944811	105401.654396	46.980967
2674.851583	104886.212580	46.985972
2671.446108	104377.920305	46.990977
2667.779586	103853.431245	46.995981
2664.413395	103337.165954	47.000986
2661.019384	102819.349570	47.005991
2657.503379	102302.500878	47.010996
2654.599138	101787.497104	47.016001
2651.060274	101266.244994	47.021005
2647.475056	100741.449576	47.026010
2644.260398	100219.807873	47.031015
2641.228766	99695.172009	47.036020
2637.652568	99170.947167	47.041025
2633.733076	98650.126867	47.046029
2630.851470	98106.226273	47.051034
2627.600947	97578.748745	47.056039
2623.484980	97056.256690	47.061044
2620.303376	96518.822491	47.066049
2616.823488	95995.511953	47.071053
2613.572052	95455.590596	47.076058
2610.104541	94925.141427	47.081063
2606.563757	94380.759761	47.086068
2603.356417	93845.027643	47.091073
2599.981993	93305.010409	47.096077
2596.662796	92755.362225	47.101082
2593.383591	92203.976890	47.106087
2589.677138	91664.307180	47.111092
2586.097862	91118.693472	47.116097
2582.379915	90563.238632	47.121101
2579.593961	90011.930876	47.126106
2575.607487	89460.832811	47.131111
2572.092518	88914.740988	47.136116
2569.110981	88360.851508	47.141121
2565.575462	87810.971712	47.146125
2561.943081	87250.115073	47.151130
2558.773005	86698.687380	47.156135
2554.946173	86136.434056	47.161140
2551.703363	85574.926471	47.166145
2548.228598	85021.367528	47.171149
2545.020557	84452.177942	47.176154
2541.229967	83881.794571	47.181159
2537.702022	83324.338637	47.186164
2534.737071	82758.358742	47.191169
2531.188896	82195.618382	47.196173
2527.614102	81622.033051	47.201178
2524.365583	81049.043723	47.206183
2520.553340	80472.914921	47.211188
2517.285340	79903.127483	47.216193
2513.585069	79329.824580	47.221197
2510.194834	78751.379563	47.226202
2506.639258	78166.203008	47.231207
2503.254279	77602.666335	47.236212
2499.755396	77023.245863	47.241217
2496.313897	76439.815651	47.246221
2492.976320	75847.796954	47.251226
2489.701170	75266.398016	47.256231
2485.759406	74689.153614	47.261236
2482.744352	74101.008957	47.266241
2478.746592	73515.023808	47.271245
2475.855473	72922.162045	47.276250
2472.285557	72341.405884	47.281255
2468.126129	71752.145307	47.286260
2465.159844	71163.778806	47.291265
2461.525800	70580.265383	47.296269
2458.076806	69994.177814	47.301274
2454.445277	69395.505302	47.306279
2451.502876	68803.195325	47.311284
2447.697155	68204.450513	47.316289
2444.098035	67625.079858	47.321293
2440.839351	67025.084033	47.326298
2437.370571	66439.016885	47.331303
2433.456059	65844.628767	47.336308
2430.458150	65244.323337	47.341313
2426.938315	64659.282751	47.346317
2423.393034	64046.771483	47.351322
2419.800917	63447.845378	47.356327
2416.018599	62852.612510	47.361332
2413.050789	62245.596102	47.366337
2409.315890	61652.942218	47.371341
2405.978664	61050.404232	47.376346
2402.421705	60451.227779	47.381351
2399.184886	59853.666058	47.386356
2395.830716	59232.055584	47.391361
2392.249419	58636.423893	47.396365
2388.887078	58019.706353	47.401370
2385.233302	57406.711064	47.406375
2381.658006	56799.061657	47.411380
2378.307092	56188.068050	47.416385
2374.749000	55577.065214	47.421389
2371.564629	54971.850498	47.426394
2368.042792	54353.203013	47.431399
2364.614803	53737.323180	47.436404
2361.359728	53121.705345	47.441409
2357.772411	52498.289026	47.446413
2353.995008	51874.988705	47.451418
2350.611584	51252.011684	47.456423
2347.193899	50639.161635	47.461428
2343.582053	50012.479238	47.466433
2339.898523	49398.828158	47.471437
2336.485795	48772.567214	47.476442
2333.073421	48147.896341	47.481447
2329.322495	47531.622934	47.486452
2325.866418	46902.737273	47.491457
2322.411835	46283.565951	47.496461
2318.944752	45659.619077	47.501466
2315.732952	45035.827375	47.506471
2311.836003	44411.087957	47.511476
2308.630428	43786.803804	47.516481
2304.609846	43168.656482	47.521485
2301.564757	42545.244692	47.526490
2298.113265	41923.860401	47.531495
2294.636541	41298.464910	47.536500
2291.469947	40660.110700	47.541505
2287.783970	40029.641889	47.546509
2284.251605	39398.920167	47.551514
2280.592761	38768.648564	47.556519
2277.012342	38147.214434	47.561524
2273.932076	37512.337523	47.566529
2270.178636	36890.110798	47.571533
2266.563172	36250.783835	47.576538
2263.540307	35621.063502	47.581543
2259.524674	34988.518057	47.586548
2256.492381	34350.596411	47.591553
2252.479270	33724.585500	47.596557
2249.250129	33080.242362	47.601562
2246.043905	32458.643777	47.606567
2242.191522	31810.164866	47.611572
2238.755854	31190.179887	47.616577
2235.572181	30546.820536	47.621581
2231.853102	29912.493763	47.626586
2228.144404	29274.021413	47.631591
2224.893736	28640.693878	47.636596
2221.292456	27990.857325	47.641601
2217.786150	27366.524779	47.646605
2214.059521	26736.771099	47.651610
2210.542489	26089.554695	47.656615
2207.128619	25463.580932	47.661620
2203.973510	24816.646802	47.666625
2200.343540	24181.281016	47.671629
2196.833016	23541.950901	47.676634
2193.405675	22892.764563	47.681639
2189.563040	22267.331230	47.686644
2186.132070	21629.146149	47.691649
2182.406033	20993.460041	47.696653
2179.076183	20358.182522	47.701658
2175.222945	19718.617484	47.706663
2171.329810	19074.120126	47.711668
2168.162113	18444.111263	47.716673
2164.343665	17811.659023	47.721677
2160.990635	17186.172231	47.726682
2157.414781	16549.559344	47.731687
2153.931699	15922.860783	47.736692
2150.532516	15295.232375	47.741697
2146.749428	14675.090059	47.746701
2143.554519	14041.059427	47.751706
2139.901069	13427.393219	47.756711
2135.903546	12801.367886	47.761716
2132.573230	12179.159696	47.766721
2129.008198	11563.175329	47.771725
2125.282247	10950.908266	47.776730
2121.689443	10332.736830	47.781735
2117.785380	9725.836572	47.786740
2114.428034	9113.334902	47.791745
2110.379079	8512.931755	47.796749
2106.392825	7929.753169	47.801754
2101.803115	7351.760366	47.806759
2096.947766	6796.557241	47.811764
2092.363409	6250.316727	47.816769
2087.958734	5731.543627	47.821773
2083.325060	5219.438094	47.826778
2079.213536	4712.632715	47.831783
2074.764424	4236.161871	47.836788
2070.688281	3776.717223	47.841793
2066.208305	3316.056049	47.846797
2061.994990	2872.030980	47.851802
2057.555842	2459.981233	47.856807
2052.955604	2057.363256	47.861812
2048.551161	1692.755056	47.866817
2042.761711	1350.299068	47.871821
2037.625235	1047.008619	47.876826
2032.288626	762.076228	47.881831
2026.936318	513.154732	47.886836
2022.157863	287.505362	47.891841
2016.666622	101.468754	47.896845
2004.956215	113.883413	47.901850
1996.409035	120.775458	47.906855
1991.228766	126.390533	47.911860
1988.690055	129.158426	47.916865
1986.993896	131.013750	47.921869
1985.244084	124.667569	47.926874
1983.939712	127.075678	47.931879
1981.195927	126.936392	47.936884
1978.338550	120.825863	47.941889
1975.559353	117.667573	47.946893
1972.059211	117.788371	47.951898
1969.279524	117.505978	47.956903
1965.380635	123.975145	47.961908
1962.617544	117.501936	47.966913
1959.056651	118.413628	47.971917
1955.583585	113.822600	47.976922
1952.491023	121.909482	47.981927
1949.233218	115.326611	47.986932
1946.159264	118.832696	47.991937
1942.637339	125.429854	47.996941
1939.485513	119.611928	48.001946
1936.070704	122.019470	48.006951
1933.064213	128.118798	48.011956
1929.918570	116.279355	48.016961
1926.195383	119.744118	48.021965
1922.578472	109.778182	48.026970
1918.990278	113.013130	48.031975
1915.615880	128.268568	48.036980
1912.289009	113.894723	48.041985
1908.909113	119.166324	48.046989
1905.221555	125.219793	48.051994
1901.903055	115.631351	48.056999
1897.968999	122.273670	48.062004
1894.764827	123.012790	48.067009
1891.627487	120.805580	48.072013
1888.110507	118.050023	48.077018
1885.484597	119.088282	48.082023
1882.041461	123.686365	48.087028
1878.809743	113.834488	48.092033
1875.137167	120.394983	48.097037
1871.562716	118.097620	48.102042
1868.161371	112.226791	48.107047
1863.942233	115.126512	48.112052
1860.803798	113.874918	48.117057
1857.413787	112.931395	48.122061
1853.753950	122.441654	48.127066
1850.644046	121.514646	48.132071
1846.983080	124.007961	48.137076
1843.798202	106.315445	48.142081
1840.191761	112.425889	48.147085
1836.803732	115.971369	48.152090
1833.620284	113.461298	48.157095
1829.737602	117.646907	48.162100
1826.425089	114.483053	48.167105
1822.820071	127.860332	48.172109
1819.130280	130.608070	48.177114
1815.644984	114.487220	48.182119
1812.152971	122.728020	48.187124
1809.222179	115.452038	48.192129
1805.573529	122.005648	48.197133
1802.005481	117.068758	48.202138
1798.868853	115.364478	48.207143
1795.114339	118.710739	48.212148
1791.502666	111.895069	48.217153
1788.297077	107.929978	48.222157
1784.606044	111.791535	48.227162
1781.132115	106.517304	48.232167
1777.687027	111.979386	48.237172
1774.529334	112.505640	48.242177
1771.060424	113.956680	48.247181
1767.423260	114.434174	48.252186
1763.942298	105.646156	48.257191
1759.995431	117.608671	48.262196
1756.562356	115.305136	48.267201
1753.216125	103.674120	48.272205
1749.780696	115.379865	48.277210
1746.724131	118.503608	48.282215
1743.082278	121.863976	48.287220
1739.333688	115.809931	48.292225
1735.569517	109.935481	48.297229
1732.017949	118.093802	48.302234
1729.049911	112.804113	48.307239
1725.700251	120.589329	48.312244
1722.132679	120.037281	48.317249
1719.109084	115.512366	48.322253
1714.960982	119.805731	48.327258
1711.389467	112.816145	48.332263
1707.784401	116.009440	48.337268
1704.719314	109.327009	48.342273
1701.416542	108.816006	48.347277
1697.250768	113.295617	48.352282
1694.118908	112.565026	48.357287
1690.222142	119.448318	48.362292
1686.911297	104.002699	48.367297
1683.615055	106.556315	48.372301
1680.373593	114.587278	48.377306
1677.096466	111.955763	48.382311
1672.873314	118.535519	48.387316
1669.542115	111.951457	48.392321
1666.107106	110.461306	48.397325
1662.496259	116.423749	48.402330
1659.548038	107.625596	48.407335
1655.570573	111.740547	48.412340
1652.346085	112.622051	48.417345
1648.823099	113.556341	48.422349
1644.937772	108.336668	48.427354
1641.863761	109.267517	48.432359
1637.943954	111.927681	48.437364
1634.383544	102.668004	48.442369
1630.978697	100.771373	48.447373
1627.659990	115.910554	48.452378
1624.416114	98.989734	48.457383
1620.968585	105.034322	48.462388
1617.137747	108.079267	48.467393
1613.873068	105.882414	48.472397
1610.043146	99.584793	48.477402
1606.952025	98.196148	48.482407
1603.526886	110.147055	48.487412
1599.878994	100.388482	48.492417
1596.236021	103.378878	48.497421
1592.617579	101.056758	48.502426
1589.377591	105.104384	48.507431
1585.521054	111.918142	48.512436
1582.307435	101.456074	48.517441
1578.876289	102.917069	48.522445
1575.347033	109.828582	48.527450
1572.121562	108.704455	48.532455
1568.113038	107.480747	48.537460
1564.588555	104.783344	48.542465
1561.080741	111.621918	48.547469
1557.685794	109.185923	48.552474
1554.638569	104.487542	48.557479
1551.059641	101.893526	48.562484
1547.396252	101.239353	48.567489
1543.863327	102.750993	48.572493
1540.059007	107.870370	48.577498
1537.156308	109.116243	48.582503
1533.071126	107.132527	48.587508
1529.721455	101.854810	48.592513
1526.334112	101.654375	48.597517
1522.748280	103.924050	48.602522
1519.547137	111.490001	48.607527
1515.597466	106.859321	48.612532
1512.052954	101.551823	48.617537
1509.096858	104.609319	48.622541
1505.410918	105.654405	48.627546
1501.874646	98.466387	48.632551
1498.128822	114.203542	48.637556
1494.707473	113.555993	48.642561
1491.339441	103.946864	48.647565
1487.620910	113.830085	48.652570
1484.553066	105.395423	48.657575
1480.898163	105.679555	48.662580
1477.399333	99.561372	48.667585
1474.288164	104.702577	48.672589
1470.249115	99.712500	48.677594
1466.658025	104.529778	48.682599
1463.016596	103.970270	48.687604
1459.842884	102.989956	48.692609
1456.665295	100.798549	48.697613
1452.875721	102.530475	48.702618
1449.552922	98.352720	48.707623
1445.758681	111.838525	48.712628
1442.162927	109.145902	48.717633
1438.440775	109.064025	48.722637
1435.081933	106.663553	48.727642
1431.959491	98.952398	48.732647
1428.577523	101.155548	48.737652
1424.866994	110.256088	48.742657
1421.425730	105.707639	48.747661
1417.630107	102.717104	48.752666
1414.447777	99.235650	48.757671
1410.804759	101.985625	48.762676
1407.775411	99.122592	48.767681
1404.080748	98.387882	48.772685
1400.174643	105.142924	48.777690
1396.459100	104.158368	48.782695
1393.125556	114.241092	48.787700
1389.764059	106.127394	48.792705
1386.277466	101.519568	48.797709
1382.712137	113.416367	48.802714
1379.481234	101.599798	48.807719
1375.587353	105.556229	48.812724
1371.981179	98.129181	48.817729
1369.132954	95.275925	48.822733
1365.490519	111.417752	48.827738
1361.955427	104.118842	48.832743
1358.654590	104.702211	48.837748
1354.663760	106.633148	48.842753
1351.210486	96.119844	48.847757
1347.657695	106.594187	48.852762
1344.623351	98.774422	48.857767
1340.841923	105.623955	48.862772
1337.337734	104.233192	48.867777
1333.868507	95.585793	48.872781
1330.026891	105.883634	48.877786
1326.699195	100.400050	48.882791
1323.464647	99.808863	48.887796
1320.044672	92.767288	48.892801
1316.399745	95.802300	48.897805
1312.577541	110.200437	48.902810
1309.272336	100.417052	48.907815
1306.088819	104.414776	48.912820
1302.382694	105.273201	48.917825
1299.324614	96.678869	48.922829
1295.225519	100.967799	48.927834
1292.134723	108.424832	48.932839
1287.984719	103.126193	48.937844
1284.252091	101.587500	48.942849
1280.977778	95.627388	48.947853
1277.878000	105.094765	48.952858
1274.635529	97.753488	48.957863
1271.074496	107.545758	48.962868
1267.507843	98.518072	48.967873
1263.787123	95.908200	48.972877
1260.066404	106.797817	48.977882
1256.735587	100.792719	48.982887
1253.139779	103.579651	48.987892
1250.112857	103.142813	48.992897
1246.161950	105.368097	48.997901
1242.913168	98.726985	49.002906
1239.487455	95.527041	49.007911
1235.712376	95.738158	49.012916
1232.121881	97.698541	49.017921
1228.976453	97.346587	49.022925
1225.171281	98.207783	49.027930
1221.893141	94.912107	49.032935
1218.013518	95.348302	49.037940
1214.649818	99.155783	49.042945
1211.405700	102.302420	49.047949
1207.747380	99.379127	49.052954
1204.573487	87.740387	49.057959
1200.463828	94.134823	49.062964
1197.171272	84.260916	49.067969
1193.736544	90.721134	49.072973
1189.870008	98.390661	49.077978
1186.879555	95.009081	49.082983
1183.560420	99.942229	49.087988
1180.084683	102.678841	49.092993
1176.349886	94.363869	49.097997
1172.740458	93.191985	49.103002
1169.366191	93.343884	49.108007
1165.243327	102.147951	49.113012
1161.991887	102.128875	49.118017
1159.080834	95.922416	49.123021
1155.085161	100.296498	49.128026
1151.885046	92.765156	49.133031
1147.901328	105.404106	49.138036
1144.684811	84.363193	49.143041
1141.251493	95.388401	49.148045
1137.542787	100.967474	49.153050
1134.382163	90.424482	49.158055
1130.312788	94.079225	49.163060
1127.181022	96.284582	49.168065
1123.815152	99.263519	49.173069
1119.897983	104.868716	49.178074
1116.786938	95.257624	49.183079
1113.315452	94.371153	49.188084
1109.875981	91.192352	49.193089
1106.362411	87.246818	49.198093
1102.381722	99.499323	49.203098
1098.949346	88.963838	49.208103
1095.653782	92.729083	49.213108
1092.249920	96.052451	49.218113
1089.096618	99.428566	49.223117
1084.978321	97.203300	49.228122
1081.638810	91.522283	49.233127
1077.931064	94.788552	49.238132
1074.791545	97.324144	49.243137
1071.509333	91.975887	49.248141
1067.964248	99.842153	49.253146
1064.110012	92.893527	49.258151
1060.423998	96.415838	49.263156
1057.058299	92.665587	49.268161
1053.636883	93.634742	49.273165
1050.243149	92.337552	49.278170
1046.976713	93.712845	49.283175
1043.043550	99.833054	49.288180
1039.397333	95.604462	49.293185
1036.181749	90.815303	49.298189
1032.748927	95.924340	49.303194
1028.875710	101.582812	49.308199
1025.477331	101.368328	49.313204
1021.964940	102.750273	49.318209
1018.572530	99.443937	49.323213
1015.127646	101.283600	49.328218
1011.597742	87.666064	49.333223
1008.172401	91.571737	49.338228
1004.311661	92.172694	49.343233
1001.711824	98.129650	49.348237
997.714253	92.297985	49.353242
994.194602	94.528930	49.358247
990.600886	92.573192	49.363252
987.351514	94.917088	49.368257
983.904901	90.521396	49.373261
979.886735	90.419213	49.378266
976.478243	84.960919	49.383271
972.852445	87.955019	49.388276
969.402771	95.347701	49.393281
965.791023	91.594636	49.398285
962.388599	94.288218	49.403290
959.013805	87.473786	49.408295
955.754548	94.248382	49.413300
952.320906	89.970897	49.418305
948.490969	84.502282	49.423309
944.926432	88.685885	49.428314
941.530738	88.958201	49.433319
938.144492	96.711163	49.438324
934.556945	91.748971	49.443329
931.254781	90.855148	49.448333
927.426758	91.836991	49.453338
923.977355	82.601308	49.458343
920.416915	87.211372	49.463348
917.279093	82.669551	49.468353
913.545774	80.735557	49.473357
909.620330	84.396388	49.478362
906.569521	82.216950	49.483367
903.343804	88.185914	49.488372
899.693308	90.712477	49.493377
896.349136	85.029053	49.498381
892.372557	93.933744	49.503386
889.013307	92.397093	49.508391
885.432628	93.970012	49.513396
881.605308	92.287930	49.518401
878.502362	81.188698	49.523405
874.862426	89.756253	49.528410
872.042076	86.490601	49.533415
867.883441	81.759688	49.538420
864.422351	88.920037	49.543425
860.789305	85.081723	49.548429
857.611771	87.392300	49.553434
854.360506	87.942693	49.558439
850.728722	93.993855	49.563444
846.915803	95.824388	49.568449
843.204351	86.351106	49.573453
839.674279	94.205553	49.578458
836.448226	82.353554	49.583463
833.114839	86.482202	49.588468
829.770649	85.221619	49.593473
826.453554	78.072373	49.598477
822.455030	89.334260	49.603482
818.779371	93.085930	49.608487
815.331731	93.549840	49.613492
811.907348	85.050584	49.618497
808.500282	79.465550	49.623501
804.941497	94.351002	49.628506
801.681514	88.243208	49.633511
797.649935	86.589772	49.638516
794.324686	105.425117	49.643521
791.115090	86.651587	49.648525
787.386568	90.601310	49.653530
784.017208	89.382615	49.658535
780.433353	91.832379	49.663540
776.633101	82.420392	49.668545
773.504600	83.337653	49.673549
769.733577	94.665368	49.678554
766.676858	89.449733	49.683559
762.534285	88.613991	49.688564
759.285098	82.093248	49.693569
756.115790	72.696945	49.698573
752.377850	77.011957	49.703578
748.660813	74.714794	49.708583
745.707916	88.733986	49.713588
742.083841	89.785341	49.718593
738.686769	85.745800	49.723597
734.760398	85.679982	49.728602
731.151436	80.341520	49.733607
727.775156	82.401480	49.738612
724.341306	90.696522	49.743617
721.023772	86.875551	49.748621
717.052692	77.373117	49.753626
713.959645	74.197394	49.758631
710.522487	83.353469	49.763636
706.528747	88.201842	49.768641
703.417308	72.257219	49.773645
699.930543	85.103536	49.778650
696.620946	79.987391	49.783655
692.768426	83.731803	49.788660
689.343550	84.537025	49.793665
685.957642	84.703446	49.798669
682.120476	92.982185	49.803674
678.514009	91.452409	49.808679
675.162762	91.458415	49.813684
671.828636	93.448546	49.818689
668.397205	79.284272	49.823693
664.767588	84.360696	49.828698
661.128962	86.521613	49.833703
658.118611	87.793807	49.838708
654.742527	85.930785	49.843713
651.153234	80.715822	49.848717
647.259602	91.508984	49.853722
643.522641	84.216328	49.858727
640.151218	76.110653	49.863732
636.438558	86.255559	49.868737
633.355336	75.406405	49.873741
629.935997	79.662341	49.878746
626.135460	88.637715	49.883751
622.753899	85.285460	49.888756
619.236406	83.773480	49.893761
615.763930	72.510376	49.898765
612.334393	84.234172	49.903770
608.878363	81.798324	49.908775
605.802901	76.063629	49.913780
601.712199	80.724631	49.918785
598.197325	78.161907	49.923789
594.465960	89.043701	49.928794
591.048261	84.491716	49.933799
587.403458	73.790107	49.938804
584.108705	71.980873	49.943809
580.991864	73.715729	49.948813
577.056683	81.202992	49.953818
574.048168	77.071354	49.958823
570.719546	80.493782	49.963828
566.779714	80.290881	49.968833
563.275420	69.633843	49.973837
559.827071	82.132503	49.978842
556.274899	78.965003	49.983847
552.549160	87.700953	49.988852
549.217538	74.865736	49.993857
545.880050	69.791924	49.998861
541.946766	72.096799	50.003866
538.573781	72.315009	50.008871
534.969061	65.884461	50.013876
531.401009	71.745390	50.018881
528.463629	64.862949	50.023885
524.693060	75.598986	50.028890
521.590241	72.437466	50.033895
517.746719	74.041854	50.038900
514.012161	76.315796	50.043905
510.603468	74.375618	50.048909
506.919132	73.345197	50.053914
503.554778	63.947677	50.058919
500.241440	76.561355	50.063924
496.663987	74.995454	50.068929
493.018027	70.327169	50.073933
489.307406	70.768786	50.078938
486.147723	72.709633	50.083943
483.120175	77.644887	50.088948
479.288368	83.312773	50.093953
475.845156	75.597947	50.098957
472.052759	77.890390	50.103962
468.521874	83.644304	50.108967
464.951726	74.209224	50.113972
461.315157	78.138335	50.118977
458.347090	72.244582	50.123981
454.459687	79.702271	50.128986
451.234309	68.144483	50.133991
447.949810	66.501347	50.138996
443.754829	75.652026	50.144001
440.637267	77.915342	50.149005
437.400197	73.664287	50.154010
433.609103	75.270015	50.159015
429.999570	73.525626	50.164020
426.220097	80.947533	50.169025
423.047628	72.709692	50.174029
419.285545	83.618419	50.179034
416.258210	78.600744	50.184039
412.461259	78.141511	50.189044
408.839881	89.490232	50.194049
405.790339	77.686781	50.199053
402.041900	81.937027	50.204058
398.885466	73.756803	50.209063
395.407759	84.412458	50.214068
391.488976	82.213195	50.219073
388.052368	77.692664	50.224077
384.350377	84.172394	50.229082
381.069439	93.753410	50.234087
377.997163	85.360772	50.239092
373.626145	87.917311	50.244097
370.210131	80.612711	50.249101
366.699236	86.977274	50.254106
363.562522	84.716371	50.259111
360.178854	83.256359	50.264116
356.704809	70.794532	50.269121
353.215799	73.795872	50.274125
349.578544	81.537321	50.279130
346.132888	70.621273	50.284135
342.777859	79.445048	50.289140
338.812741	81.900435	50.294145
335.663010	70.517551	50.299149
332.261576	70.793999	50.304154
328.068345	70.681205	50.309159
324.837936	74.657825	50.314164
321.103494	76.982392	50.319169
318.150397	75.885612	50.324173
314.726295	78.766124	50.329178
311.330982	79.547809	50.334183
307.734952	80.642308	50.339188
304.159246	72.976619	50.344193
300.461451	81.758851	50.349197
296.625010	80.685705	50.354202
293.484034	78.264130	50.359207
289.736396	78.363535	50.364212
286.305985	78.340788	50.369217
282.958140	76.359534	50.374221
279.305688	74.855962	50.379226
275.778219	66.584840	50.384231
272.741899	74.346625	50.389236
269.050304	83.722664	50.394241
265.607484	78.143293	50.399245
261.810311	80.784509	50.404250
258.227542	76.280429	50.409255
255.005677	74.282730	50.414260
251.323762	81.917247	50.419265
248.232836	73.312414	50.424269
244.176836	78.420459	50.429274
240.779081	75.614938	50.434279
237.387700	73.691088	50.439284
233.742236	72.151635	50.444289
230.250591	69.604337	50.449293
226.769891	74.676597	50.454298
223.545091	67.155606	50.459303
220.176537	76.158657	50.464308
216.347533	73.679702	50.469313
213.097738	72.100797	50.474317
209.448327	70.147523	50.479322
205.631880	73.645936	50.484327
202.683754	69.552410	50.489332
198.818196	77.610979	50.494337
195.336510	62.195527	50.499341
191.682113	71.742938	50.504346
188.260798	67.719922	50.509351
184.866741	76.635200	50.514356
181.226281	84.218979	50.519361
178.039699	68.466524	50.524365
174.197921	76.050007	50.529370
171.069445	76.182742	50.534375
167.191335	71.370332	50.539380
163.723936	74.406294	50.544385
160.626072	67.469812	50.549389
156.537470	80.346565	50.554394
153.024236	73.810100	50.559399
149.871224	75.462051	50.564404
146.415670	75.797569	50.569409
142.954767	70.015402	50.574413
139.092715	88.241439	50.579418
135.726927	78.787268	50.584423
132.813007	74.011403	50.589428
128.924490	79.118695	50.594433
125.390636	77.957340	50.599437
121.869019	76.031639	50.604442
118.144942	70.375869	50.609447
114.875718	78.376401	50.614452
110.980581	77.726865	50.619457
107.787765	75.265934	50.624461
104.305391	81.018656	50.629466
100.851095	81.540640	50.634471
97.011916	79.278418	50.639476
93.446289	83.680566	50.644481
89.960597	80.942543	50.649485
86.724479	81.123685	50.654490
83.305246	81.374465	50.659495
79.833315	73.986886	50.664500
76.280106	70.259663	50.669505
72.770294	75.023269	50.674509
69.107435	77.412652	50.679514
65.665869	82.238400	50.684519
62.002829	74.545231	50.689524
58.377054	81.392764	50.694529
55.740860	83.011716	50.699533
52.191928	80.406928	50.704538
48.639769	75.173644	50.709543
44.864960	80.820047	50.714548
40.917761	90.277029	50.719553
37.709770	69.279433	50.724557
34.034373	76.011310	50.729562
30.626952	77.867397	50.734567
27.406446	71.532146	50.739572
23.512204	82.701910	50.744577
20.100322	78.212395	50.749581
16.409252	80.112647	50.754586
13.163068	80.836352	50.759591
9.880777	83.400601	50.764596
6.522644	81.797467	50.769601
2.986227	71.835237	50.774605