Fri Aug 26 14:13:05 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.270485	94.860326	0.000000
-0.139970	97.543723	0.005005
-0.014692	99.571086	0.010010
0.139985	98.303662	0.015014
-0.139046	95.930046	0.020019
0.087962	95.932644	0.025024
-0.012111	92.224573	0.030029
-0.275596	89.402460	0.035034
-0.265938	76.236944	0.040038
-0.649671	66.407072	0.045043
-0.889034	56.488290	0.050048
-0.752870	47.456979	0.055053
-1.474626	38.236554	0.060058
-1.027656	28.818351	0.065062
-2.195435	23.204340	0.070067
-2.375962	9.404117	0.075072
-2.455713	-0.874830	0.080077
-3.230939	-3.645724	0.085082
-3.777464	-6.952081	0.090086
-4.256103	3.116375	0.095091
-4.643405	-7.272866	0.100096
-4.301186	0.367815	0.105101
-4.377090	5.539518	0.110106
-4.232606	-8.991476	0.115110
-5.109220	-4.827694	0.120115
-5.300194	-4.801145	0.125120
-5.751532	-0.469466	0.130125
-5.828128	10.371600	0.135130
-5.707238	4.455719	0.140134
-6.558607	2.500245	0.145139
-6.812034	-3.063135	0.150144
-6.867562	-1.140506	0.155149
-7.130763	-0.653474	0.160154
-6.961518	-13.283806	0.165158
-7.942020	-1.887576	0.170163
-8.028372	1.684948	0.175168
-8.528166	-7.414992	0.180173
-8.612233	-8.629419	0.185178
-8.484815	-12.176741	0.190182
-8.869186	-3.125841	0.195187
-8.429540	-11.429280	0.200192
-9.412803	4.861541	0.205197
-10.204318	2.798675	0.210202
-10.080943	0.476311	0.215206
-10.192899	-3.454509	0.220211
-10.279392	-5.598670	0.225216
-10.608974	-2.193914	0.230221
-11.217913	-2.339563	0.235226
-11.184108	-4.230380	0.240230
-11.469700	-7.162926	0.245235
-11.426836	-1.886335	0.250240
-11.821199	3.160950	0.255245
-11.981888	-3.799382	0.260250
-12.451962	-9.107574	0.265254
-13.031154	-3.810059	0.270259
-12.855205	-11.645349	0.275264
-12.999842	-6.352221	0.280269
-13.252653	-0.700575	0.285274
-13.562723	-8.880960	0.290278
-14.365214	-6.313703	0.295283
-14.161788	-3.751209	0.300288
-14.429761	-12.127965	0.305293
-14.753684	8.900577	0.310298
-14.604734	-8.579631	0.315302
-15.299088	-1.789927	0.320307
-15.426472	-6.357400	0.325312
-15.982934	2.138186	0.330317
-16.225637	7.936952	0.335322
-15.849787	-3.086785	0.340326
-16.398684	-0.505229	0.345331
-16.359503	-6.079366	0.350336
-17.055555	-2.737770	0.355341
-17.661817	-1.339978	0.360346
-17.605893	-12.759971	0.365350
-17.567602	2.087356	0.370355
-17.634414	-0.844453	0.375360
-17.893669	-2.648515	0.380365
-18.967084	7.199346	0.385370
-19.212085	1.103160	0.390374
-19.179437	4.951376	0.395379
-19.510359	-0.716994	0.400384
-19.122213	2.436815	0.405389
-19.285353	-4.750917	0.410394
-19.336464	-5.869238	0.415398
-20.191025	2.321596	0.420403
-20.249959	-0.722168	0.425408
-20.534848	0.537007	0.430413
-20.771586	2.560614	0.435418
-20.936360	-4.142826	0.440422
-21.587895	-1.738273	0.445427
-21.910849	-5.550822	0.450432
-21.917077	5.554520	0.455437
-22.167548	1.835085	0.460442
-22.143288	-7.109174	0.465446
-23.011141	13.548496	0.470451
-23.000823	1.205483	0.475456
-23.157659	-3.370059	0.480461
-23.648133	-0.392654	0.485466
-23.373331	-1.327609	0.490470
-23.690969	-0.768829	0.495475
-24.387855	-3.634174	0.500480
-24.657698	-9.527178	0.505485
-24.968449	-5.381898	0.510490
-24.548869	-11.122824	0.515494
-25.084038	-0.166077	0.520499
-25.248325	-6.977155	0.525504
-25.747987	-1.467404	0.530509
-26.114735	1.759648	0.535514
-26.130764	-10.171144	0.540518
-26.184907	-0.295330	0.545523
-26.579052	-4.194867	0.550528
-26.992073	-4.836076	0.555533
-27.430398	-3.717522	0.560538
-27.162774	-3.379574	0.565542
-27.614725	1.850676	0.570547
-28.070496	1.652707	0.575552
-28.532104	-0.796869	0.580557
-29.111484	1.972924	0.585562
-29.251625	-2.772891	0.590566
-29.157889	-1.762487	0.595571
-28.886684	-0.020438	0.600576
-29.050063	-0.713170	0.605581
-29.286941	0.323401	0.610586
-29.643058	-4.198968	0.615590
-30.643124	2.847136	0.620595
-30.684148	0.841423	0.625600
-30.185446	-3.330001	0.630605
-30.844419	0.084913	0.635610
-31.115486	-0.771379	0.640614
-31.974270	4.186868	0.645619
-32.382851	4.544680	0.650624
-32.253754	7.033330	0.655629
-32.383674	-5.509298	0.660634
-31.937942	-3.379986	0.665638
-32.351716	1.793702	0.670643
-32.579199	-5.023356	0.675648
-32.995725	-0.984988	0.680653
-33.550103	4.299174	0.685658
-33.411451	-4.824242	0.690662
-34.078055	-1.335376	0.695667
-34.450237	0.149354	0.700672
-34.500279	1.827528	0.705677
-35.056910	-4.014498	0.710682
-34.987726	-5.110421	0.715686
-35.175786	-0.354678	0.720691
-35.048682	1.618607	0.725696
-35.770782	-2.799325	0.730701
-36.514002	-0.108423	0.735706
-36.566141	-2.805243	0.740710
-36.470013	-4.443181	0.745715
-36.597371	-0.035398	0.750720
-36.804555	-0.306872	0.755725
-36.927915	-2.179546	0.760730
-36.999147	-3.756627	0.765734
-37.681939	4.923138	0.770739
-37.359697	-1.163291	0.775744
-38.171938	-0.752121	0.780749
-38.964449	1.342200	0.785754
-39.237378	-8.621934	0.790758
-39.576863	-4.165307	0.795763
-39.362913	-1.493724	0.800768
-39.342690	-7.295854	0.805773
-39.903889	-8.685920	0.810778
-39.706610	-14.022086	0.815782
-40.214568	-0.630409	0.820787
-40.317042	-4.850595	0.825792
-40.622241	-1.474945	0.830797
-40.906761	-4.534202	0.835802
-41.024354	-8.296469	0.840806
-41.270116	-8.100044	0.845811
-41.971736	-2.441794	0.850816
-42.094794	-1.271090	0.855821
-42.710319	0.814657	0.860826
-42.240185	-7.559966	0.865830
-42.256455	0.063764	0.870835
-43.001331	-2.452434	0.875840
-43.569867	-0.288586	0.880845
-44.058438	0.916883	0.885850
-43.892413	-0.409247	0.890854
-44.004258	0.620512	0.895859
-44.136122	-5.018738	0.900864
-44.020100	-5.960608	0.905869
-45.098768	-5.454174	0.910874
-45.189467	-10.938486	0.915878
-45.855951	-3.324249	0.920883
-45.493529	-1.102875	0.925888
-45.476322	-7.730246	0.930893
-46.041284	-0.916398	0.935898
-45.788999	-11.085686	0.940902
-46.584039	2.986584	0.945907
-46.688610	-4.960049	0.950912
-46.516348	-5.695548	0.955917
-47.083477	-2.038679	0.960922
-47.822193	-6.555258	0.965926
-47.903831	-4.451401	0.970931
-48.213227	-9.367007	0.975936
-48.266726	-7.409895	0.980941
-48.399089	1.022821	0.985946
-48.331286	-8.032615	0.990950
-48.846052	1.025932	0.995955
-49.389304	-6.852398	1.000960
-49.650386	-17.343535	1.005965
-50.074130	-1.367621	1.010970
-49.785940	-10.944571	1.015974
-50.040946	-6.377716	1.020979
-50.350258	-7.171107	1.025984
-50.669672	-14.325011	1.030989
-51.091537	-3.173945	1.035994
-50.941242	-1.542781	1.040998
-51.673236	-8.762159	1.046003
-52.119594	-15.889969	1.051008
-52.083847	-11.823950	1.056013
-52.796579	-6.999173	1.061018
-52.719351	-11.342246	1.066022
-52.410311	-4.357606	1.071027
-52.621821	-8.794924	1.076032
-52.697913	-6.638148	1.081037
-53.731276	-4.098218	1.086042
-54.029123	-8.743548	1.091046
-54.120649	-2.708906	1.096051
-54.266377	-5.884682	1.101056
-54.059804	-1.560530	1.106061
-54.854469	-0.168202	1.111066
-55.350298	-7.955842	1.116070
-55.506609	0.183219	1.121075
-55.533782	-10.660705	1.126080
-55.473242	-5.624142	1.131085
-56.097425	-6.061636	1.136090
-56.373708	-11.624615	1.141094
-56.916834	-4.073877	1.146099
-57.016565	-1.764729	1.151104
-57.228191	-1.247763	1.156109
-57.221203	-2.435239	1.161114
-57.367567	-0.691450	1.166118
-57.297132	2.334660	1.171123
-58.269895	1.334529	1.176128
-58.663857	-3.868457	1.181133
-59.138608	-6.875949	1.186138
-59.127480	-1.347655	1.191142
-59.125192	-4.916623	1.196147
-58.807142	-4.618164	1.201152
-58.903977	-7.671842	1.206157
-59.511389	0.360291	1.211162
-59.981486	-5.311715	1.216166
-60.569033	0.056701	1.221171
-60.716623	-5.811046	1.226176
-60.671290	-7.210128	1.231181
-61.472325	-2.235565	1.236186
-61.494522	-9.318691	1.241190
-61.808530	-6.039744	1.246195
-61.773470	-8.528683	1.251200
-62.199768	-9.670843	1.256205
-62.137537	-1.809410	1.261210
-62.029689	-4.847503	1.266214
-62.572717	1.896494	1.271219
-62.977926	-11.428975	1.276224
-63.212151	-11.329256	1.281229
-63.379738	-4.191316	1.286234
-63.632493	-16.515498	1.291238
-64.244517	-3.300604	1.296243
-64.621172	-4.963003	1.301248
-64.496354	-5.526605	1.306253
-65.027136	-8.693046	1.311258
-64.715412	-9.687532	1.316262
-64.875940	-9.380995	1.321267
-65.728952	1.258255	1.326272
-65.825548	-2.266845	1.331277
-66.459354	0.758187	1.336282
-66.264670	-8.867477	1.341286
-66.805117	0.021067	1.346291
-66.634529	-2.542757	1.351296
-66.813695	-0.518624	1.356301
-67.645568	1.062988	1.361306
-67.777656	-11.162930	1.366310
-67.816930	-4.655551	1.371315
-67.912209	-4.814738	1.376320
-67.755933	-12.387543	1.381325
-68.627968	-7.164653	1.386330
-68.779209	-14.499758	1.391334
-69.226862	-9.317636	1.396339
-69.393147	-5.843397	1.401344
-69.098393	-9.328191	1.406349
-70.212063	-10.727146	1.411354
-70.262905	-12.358018	1.416358
-70.557791	-6.592261	1.421363
-70.638339	2.348060	1.426368
-70.702353	-5.927577	1.431373
-70.565637	9.334679	1.436378
-71.030195	-3.503844	1.441382
-71.888755	3.719537	1.446387
-72.091542	2.871596	1.451392
-72.297713	-3.205322	1.456397
-72.519386	3.517114	1.461402
-71.937014	2.085032	1.466406
-72.337689	1.581103	1.471411
-73.125326	2.349099	1.476416
-73.337478	-5.685182	1.481421
-73.731191	2.383278	1.486426
-73.621244	-4.865951	1.491430
-74.066279	2.815045	1.496435
-74.761291	-1.290738	1.501440
-74.717588	-9.504053	1.506445
-75.251191	-0.331848	1.511450
-75.254460	2.500101	1.516454
-75.562236	-4.924527	1.521459
-75.369816	0.240194	1.526464
-74.990478	-7.490724	1.531469
-75.817537	-5.185388	1.536474
-76.564933	-10.111887	1.541478
-76.432873	-3.327475	1.546483
-76.589054	1.799777	1.551488
-77.494446	-7.578678	1.556493
-77.703942	0.075134	1.561498
-77.864914	-6.847184	1.566502
-78.209745	-0.561139	1.571507
-78.272242	-7.581045	1.576512
-77.983447	4.895669	1.581517
-78.299231	0.857386	1.586522
-78.425889	-2.292886	1.591526
-79.238859	1.639534	1.596531
-79.308657	-1.487954	1.601536
-79.546054	6.708024	1.606541
-79.998103	2.311320	1.611546
-79.512380	-2.291502	1.616550
-80.404552	-3.383271	1.621555
-81.025320	6.220110	1.626560
-80.896946	-7.903421	1.631565
-81.167952	8.181589	1.636570
-80.985165	-4.454013	1.641574
-81.298137	-7.467712	1.646579
-82.138322	-5.416587	1.651584
-82.150114	1.181424	1.656589
-82.586220	11.391948	1.661594
-82.379330	5.810680	1.666598
-82.425556	4.593525	1.671603
-82.628450	-2.015394	1.676608
-83.595429	-3.187261	1.681613
-84.084892	-5.778024	1.686618
-83.931353	-3.834166	1.691622
-84.243575	-5.123796	1.696627
-84.222201	3.898729	1.701632
-84.311175	-4.569168	1.706637
-85.276807	-2.849674	1.711642
-85.447936	-0.798320	1.716646
-85.885969	2.357576	1.721651
-85.911333	10.397160	1.726656
-86.147482	2.404577	1.731661
-86.434626	4.515123	1.736666
-86.128691	-1.249237	1.741670
-86.217224	5.895379	1.746675
-86.499804	5.945682	1.751680
-87.100899	2.802843	1.756685
-87.484505	-0.718696	1.761690
-87.572769	-6.532405	1.766694
-87.749147	6.877247	1.771699
-87.914856	10.300780	1.776704
-88.532822	9.849665	1.781709
-89.094976	2.945516	1.786714
-89.033299	-6.093146	1.791718
-89.262973	-9.249523	1.796723
-89.409321	-5.348133	1.801728
-89.324282	-6.278851	1.806733
-89.489361	-10.109650	1.811738
-89.915942	-2.852295	1.816742
-90.620105	-5.675375	1.821747
-90.647405	1.311014	1.826752
-90.597726	-5.153738	1.831757
-91.238947	-4.699594	1.836762
-91.731408	-0.184349	1.841766
-92.019818	-9.662029	1.846771
-92.006213	-0.309279	1.851776
-91.899178	-2.398152	1.856781
-92.098307	-1.095385	1.861786
-92.336115	-5.968353	1.866790
-93.252526	-0.014079	1.871795
-93.575659	-1.083718	1.876800
-93.125860	2.050997	1.881805
-93.701930	-2.481414	1.886810
-93.409832	-5.225502	1.891814
-93.588810	-8.453044	1.896819
-94.330596	-1.330103	1.901824
-94.639294	-9.418948	1.906829
-94.768938	-4.004775	1.911834
-94.536605	-2.667949	1.916838
-95.256931	-1.619379	1.921843
-95.811970	1.491462	1.926848
-96.335467	-11.575149	1.931853
-96.148384	4.223404	1.936858
-96.115222	-3.694052	1.941862
-96.451467	3.906732	1.946867
-97.132038	3.424237	1.951872
-97.492731	1.237352	1.956877
-97.877408	0.329149	1.961882
-97.647322	-5.413908	1.966886
-97.683224	-1.997933	1.971891
-97.738599	1.383110	1.976896
-98.261163	1.454961	1.981901
-98.905454	-2.181007	1.986906
-98.958505	2.120294	1.991910
-99.276296	1.951461	1.996915
-99.230954	-0.226760	2.006912
-99.408904	-2.378469	2.016909
-98.698366	-4.107835	2.026906
-98.072187	-1.601530	2.036902
-97.805393	0.393714	2.046899
-96.737076	-1.023905	2.056896
-96.361780	0.358919	2.066893
-96.302375	-4.487441	2.076890
-96.334848	-2.505788	2.086886
-95.341153	-0.709250	2.096883
-94.421909	-6.769670	2.106880
-94.027952	-7.743348	2.116877
-93.964522	-3.695453	2.126874
-93.471513	-3.537848	2.136870
-92.836840	0.243715	2.146867
-92.012148	-0.483426	2.156864
-91.528507	-1.524919	2.166861
-91.588177	-5.842741	2.176858
-90.370671	-5.104215	2.186854
-90.325930	-4.423835	2.196851
-89.609374	1.179074	2.206848
-89.025995	-3.945266	2.216845
-88.910373	-3.694058	2.226842
-88.139746	-0.703412	2.236838
-87.178560	-6.079806	2.246835
-87.224470	-6.823444	2.256832
-86.754122	0.731086	2.266829
-85.852789	-0.524323	2.276826
-85.663514	-1.092344	2.286822
-85.419923	-5.200800	2.296819
-84.385854	-2.970239	2.306816
-83.822301	-6.374602	2.316813
-83.925441	-4.613187	2.326810
-83.130834	-3.216457	2.336806
-82.943403	-5.022759	2.346803
-82.073932	-7.290036	2.356800
-81.643640	-4.959132	2.366797
-81.238008	-0.061723	2.376794
-80.070309	-2.312080	2.386790
-80.162762	-3.913252	2.396787
-79.703182	-10.389927	2.406784
-79.233621	-2.939809	2.416781
-78.943087	-0.115158	2.426778
-77.797238	-1.747580	2.436774
-77.376294	-5.151913	2.446771
-77.086671	-6.505308	2.456768
-77.001274	0.162019	2.466765
-75.938078	-5.151065	2.476762
-75.652516	-6.313766	2.486758
-75.288816	-6.750560	2.496755
-74.388901	-6.133640	2.506752
-74.376431	-4.177991	2.516749
-73.452176	-3.115048	2.526746
-72.862834	-3.982936	2.536742
-72.380268	-7.925868	2.546739
-72.244296	-14.893831	2.556736
-71.529777	-5.508381	2.566733
-71.138864	-5.661152	2.576730
-70.620760	-10.962222	2.586726
-69.701681	-9.594375	2.596723
-69.576640	-17.431751	2.606720
-69.584921	-14.725297	2.616717
-68.071278	-12.490212	2.626714
-67.995508	-9.511751	2.636710
-68.103433	-10.207721	2.646707
-67.212155	-13.270315	2.656704
-66.850045	-14.999280	2.666701
-65.915490	-9.370128	2.676698
-65.832915	-10.133772	2.686694
-64.831559	-14.547103	2.696691
-63.815699	-7.635024	2.706688
-64.607691	-14.034035	2.716685
-63.917754	-5.832641	2.726682
-62.642101	-11.644454	2.736678
-62.566734	-17.506959	2.746675
-62.403264	-10.604712	2.756672
-61.293114	-5.848672	2.766669
-60.995963	-9.553668	2.776666
-60.959106	-4.031824	2.786662
-60.078990	-12.373226	2.796659
-59.562887	-9.751583	2.806656
-58.923697	-7.484880	2.816653
-58.215971	-6.936235	2.826650
-58.066520	-9.740782	2.836646
-58.209868	-13.177627	2.846643
-56.810824	-6.575455	2.856640
-56.470278	-2.247600	2.866637
-55.993919	-6.563354	2.876634
-55.202745	-5.790124	2.886630
-54.998445	-9.534513	2.896627
-55.012453	-7.815486	2.906624
-53.856248	-9.066228	2.916621
-53.411337	-4.957355	2.926618
-53.167775	-7.424941	2.936614
-52.276763	-4.025399	2.946611
-51.692174	-5.339192	2.956608
-51.883281	-2.502903	2.966605
-51.502011	-8.815337	2.976602
-50.640790	-4.593891	2.986598
-49.425605	-6.629902	2.996595
-49.597998	-10.334647	3.006592
-49.236024	-2.288088	3.016589
-48.715488	-5.470350	3.026586
-48.200708	-3.358499	3.036582
-47.831160	-14.100710	3.046579
-47.205889	-12.661776	3.056576
-46.418582	-6.442679	3.066573
-45.522966	-5.109189	3.076570
-45.527878	-3.778036	3.086566
-45.065782	-4.182634	3.096563
-44.786979	-5.249252	3.106560
-43.940344	-11.051286	3.116557
-43.676900	-4.136091	3.126554
-42.940017	-4.082977	3.136550
-42.394396	-5.058094	3.146547
-42.399961	1.224268	3.156544
-41.539480	-6.721286	3.166541
-41.051311	-6.480566	3.176538
-40.562934	-5.580999	3.186534
-39.640950	-3.941180	3.196531
-39.410627	-4.781679	3.206528
-39.196406	-5.809732	3.216525
-38.224244	-7.120514	3.226522
-38.036345	-5.271370	3.236518
-37.675805	-8.469901	3.246515
-36.744415	-6.093474	3.256512
-36.451203	-7.422086	3.266509
-36.757249	-7.710255	3.276506
-35.390187	-8.483827	3.286502
-35.317269	-12.644902	3.296499
-34.142617	-8.291698	3.306496
-33.919502	-11.649391	3.316493
-33.781506	-4.163484	3.326490
-32.408413	-9.233390	3.336486
-32.050790	-7.863651	3.346483
-31.922492	-11.228755	3.356480
-32.093795	-4.489783	3.366477
-31.199807	-8.775529	3.376474
-30.678063	-6.338490	3.386470
-29.717719	-8.597740	3.396467
-28.996589	-5.893981	3.406464
-29.000286	-13.429392	3.416461
-28.798100	-8.386270	3.426458
-27.855149	-9.093810	3.436454
-27.307567	-5.108622	3.446451
-27.128654	-4.145033	3.456448
-26.085723	-0.129267	3.466445
-25.820475	-3.851471	3.476442
-25.974414	-9.323496	3.486438
-25.277518	-7.468074	3.496435
-24.606268	-3.657357	3.506432
-23.486531	-0.473983	3.516429
-23.191390	0.601386	3.526426
-23.260472	-1.241004	3.536422
-22.680954	-2.962639	3.546419
-22.017893	-6.784793	3.556416
-21.545785	-3.072946	3.566413
-20.633759	-6.864173	3.576410
-19.992138	-6.840575	3.586406
-20.091973	-2.745083	3.596403
-19.991108	-5.722625	3.606400
-19.032374	-3.581696	3.616397
-18.655914	-2.290915	3.626394
-17.361799	-8.811999	3.636390
-17.167640	2.228824	3.646387
-17.143414	-4.085042	3.656384
-16.745456	-4.805926	3.666381
-16.090616	-3.301904	3.676378
-15.500730	0.888934	3.686374
-14.413912	1.574956	3.696371
-14.239469	-0.726654	3.706368
-14.147268	-6.322532	3.716365
-13.969419	-6.423122	3.726362
-12.800012	0.528413	3.736358
-12.441234	-5.701330	3.746355
-11.327007	-10.452173	3.756352
-11.519515	-0.814624	3.766349
-11.213918	0.195763	3.776346
-10.572429	0.333419	3.786342
-10.175480	-3.919289	3.796339
-9.590447	-3.503588	3.806336
-8.766394	-6.314971	3.816333
-8.338132	-2.596297	3.826330
-7.987944	-2.574839	3.836326
-7.264039	-2.253617	3.846323
-6.629504	-6.204372	3.856320
-6.769830	-8.466475	3.866317
-5.951163	-7.561313	3.876314
-5.263471	-8.178426	3.886310
-5.051888	-9.218739	3.896307
-4.253565	-0.866325	3.906304
-4.067188	0.444549	3.916301
-3.608269	5.951369	3.926298
-3.270682	8.664165	3.936294
-2.496894	17.178793	3.946291
-2.308047	27.501392	3.956288
-1.947503	33.869313	3.966285
-1.655318	61.949830	3.976282
-0.961951	73.831609	3.986278
-0.806841	98.848178	3.996275
-0.200599	110.543981	4.006272
0.000000	132.425114	4.011277
0.419768	143.132033	4.016282
0.886729	170.886981	4.021286
0.904044	167.695278	4.026291
1.129264	175.132794	4.031296
0.901734	164.256679	4.036301
1.089143	170.814251	4.041306
0.859357	171.950966	4.046310
1.414148	182.839362	4.051315
1.460907	189.118290	4.056320
1.287256	198.630018	4.061325
1.680301	191.001277	4.066330
1.673769	190.714378	4.071334
1.213174	181.810712	4.076339
1.260230	176.994574	4.081344
1.625780	191.781617	4.086349
1.704490	187.732486	4.091354
1.433542	185.259525	4.096358
1.591433	172.637156	4.101363
1.202903	176.680696	4.106368
1.544427	193.233650	4.111373
1.750470	187.810638	4.116378
1.645132	189.272818	4.121382
1.219793	175.001231	4.126387
2.015360	189.069603	4.131392
1.489752	186.114284	4.136397
1.488624	167.091247	4.141402
1.419771	188.371348	4.146406
1.369009	199.828589	4.151411
1.496754	197.568792	4.156416
1.648077	195.295833	4.161421
1.935550	198.234404	4.166426
1.713370	197.443254	4.171430
1.691277	197.206232	4.176435
1.456775	193.844928	4.181440
1.493729	192.731865	4.186445
1.993592	200.332270	4.191450
1.863683	198.862381	4.196454
1.780340	198.979737	4.201459
1.891470	198.019636	4.206464
1.538357	207.299888	4.211469
1.625639	200.035118	4.216474
1.767778	209.488194	4.221478
1.797751	199.622308	4.226483
1.663508	201.677435	4.231488
1.680869	197.106354	4.236493
1.916031	196.234507	4.241498
2.074396	198.522480	4.246502
2.056289	189.885266	4.251507
1.849110	197.665354	4.256512
1.642086	196.992065	4.261517
1.648836	196.070361	4.266522
1.724464	201.183727	4.271526
1.793828	192.039360	4.276531
1.943027	203.443324	4.281536
1.720631	204.370087	4.286541
1.866006	197.494897	4.291546
2.073208	202.397957	4.296550
1.699809	198.248376	4.301555
2.039203	206.848182	4.306560
1.978372	216.585958	4.311565
2.343956	210.736311	4.316570
1.938580	210.967080	4.321574
1.854485	204.013722	4.326579
2.233878	212.120096	4.331584
2.202521	219.910783	4.336589
2.391095	201.854734	4.341594
1.829449	206.469387	4.346598
2.098880	201.134577	4.351603
2.236300	205.668861	4.356608
1.990793	211.028378	4.361613
2.078474	218.395580	4.366618
1.821914	228.290383	4.371622
2.058873	220.394873	4.376627
1.969289	215.207702	4.381632
1.942757	219.561877	4.386637
1.999150	213.858444	4.391642
1.872874	230.838599	4.396646
2.219625	221.938924	4.401651
2.295627	222.876175	4.406656
2.198922	227.000837	4.411661
2.093951	220.654987	4.416666
1.958110	217.977492	4.421670
2.551793	226.091636	4.426675
2.272589	227.270849	4.431680
1.812898	216.342266	4.436685
2.512572	231.909370	4.441690
2.545096	243.299889	4.446694
2.487090	241.385375	4.451699
2.893471	238.376688	4.456704
2.391211	223.436845	4.461709
2.438425	222.375965	4.466714
2.012588	228.810744	4.471718
2.432015	224.781320	4.476723
2.791005	227.835309	4.481728
2.354605	224.109973	4.486733
2.481021	221.508702	4.491738
2.439109	229.835700	4.496742
2.388396	224.265995	4.501747
2.462499	235.858839	4.506752
2.748555	239.490485	4.511757
2.661477	235.074858	4.516762
2.673106	228.467247	4.521766
2.490181	221.595707	4.526771
2.591126	221.076943	4.531776
2.224462	226.812825	4.536781
2.729499	229.856729	4.541786
2.836649	245.215548	4.546790
2.879252	224.233646	4.551795
2.871610	220.596576	4.556800
2.533891	223.085173	4.561805
2.780639	216.187865	4.566810
2.478850	216.462616	4.571814
2.534394	224.458069	4.576819
2.641653	219.455380	4.581824
2.863776	230.949246	4.586829
2.816915	226.245791	4.591834
2.410340	226.299580	4.596838
2.562269	234.175629	4.601843
3.016428	243.614944	4.606848
2.924832	242.664258	4.611853
2.939441	232.452741	4.616858
2.794026	228.134781	4.621862
2.879815	233.072573	4.626867
2.613988	225.283815	4.631872
2.521725	233.808475	4.636877
3.032409	243.346554	4.641882
3.124253	250.959889	4.646886
2.844556	248.409188	4.651891
2.959794	251.662480	4.656896
2.754369	255.076428	4.661901
3.127254	245.770883	4.666906
2.841543	248.390589	4.671910
3.077813	245.092017	4.676915
2.958422	241.228737	4.681920
2.721684	249.620878	4.686925
3.203645	244.389003	4.691930
2.892631	257.541411	4.696934
3.081101	249.979297	4.701939
3.336457	250.297015	4.706944
3.042591	241.582490	4.711949
2.936989	238.213764	4.716954
2.842565	237.560905	4.721958
2.923531	254.929588	4.726963
3.302264	249.571417	4.731968
2.817016	241.535247	4.736973
2.784161	242.249007	4.741978
2.439490	255.643930	4.746982
2.614790	247.634623	4.751987
2.495726	255.119449	4.756992
2.490409	262.260707	4.761997
3.264878	272.678367	4.767002
3.168653	278.198156	4.772006
3.092129	283.104285	4.777011
3.138823	279.227794	4.782016
3.077387	271.957676	4.787021
3.762810	268.677752	4.792026
3.375891	271.202489	4.797030
3.453075	275.777807	4.802035
3.612763	276.066129	4.807040
3.387107	270.007965	4.812045
2.977662	255.012516	4.817050
3.206226	268.197978	4.822054
3.407553	262.566874	4.827059
3.539186	265.390518	4.832064
3.500273	279.079532	4.837069
3.281104	260.261183	4.842074
3.296756	264.466435	4.847078
3.230812	273.926634	4.852083
3.731069	273.677885	4.857088
3.349184	267.849686	4.862093
3.727483	262.934497	4.867098
3.234757	259.993028	4.872102
3.367332	258.362046	4.877107
3.641675	253.706648	4.882112
3.325485	260.067420	4.887117
3.458819	251.131357	4.892122
3.548522	263.455766	4.897126
3.432935	271.484212	4.902131
3.583176	266.664639	4.907136
3.677737	271.414417	4.912141
3.535041	273.872657	4.917146
3.679610	266.469229	4.922150
3.605029	264.487693	4.927155
3.613945	262.021767	4.932160
3.574994	259.927118	4.937165
3.377987	250.574261	4.942170
3.319136	268.135565	4.947174
3.520296	279.553633	4.952179
3.321057	285.165392	4.957184
3.559462	285.953977	4.962189
3.618325	283.454961	4.967194
3.564896	281.814972	4.972198
3.695822	274.910365	4.977203
3.690700	279.732612	4.982208
3.486891	277.125801	4.987213
3.643992	280.872444	4.992218
3.813111	279.871673	4.997222
3.729015	280.419409	5.002227
3.433981	281.540980	5.007232
3.600300	280.138855	5.012237
3.712329	281.241340	5.017242
3.725840	289.085182	5.022246
3.877880	290.311148	5.027251
3.793838	280.251002	5.032256
3.692404	288.046302	5.037261
3.720363	289.709196	5.042266
3.819682	301.658818	5.047270
4.321475	297.698810	5.052275
4.029518	283.877759	5.057280
4.111678	281.928763	5.062285
4.234954	286.680402	5.067290
3.776743	287.567956	5.072294
3.969080	284.918447	5.077299
3.950205	281.887380	5.082304
3.564454	292.362307	5.087309
3.564647	290.198287	5.092314
3.748124	293.482090	5.097318
3.865127	304.565271	5.102323
4.225044	311.557936	5.107328
3.933465	317.981335	5.112333
4.290500	318.523664	5.117338
4.291383	311.335575	5.122342
4.264509	313.804260	5.127347
4.406421	306.356938	5.132352
4.207331	300.525578	5.137357
3.865161	292.410161	5.142362
3.775249	290.661959	5.147366
3.683629	301.116406	5.152371
4.008035	307.554625	5.157376
4.114566	316.652640	5.162381
4.518218	313.967063	5.167386
4.456854	316.624613	5.172390
4.318663	317.142808	5.177395
4.513083	306.257858	5.182400
3.737977	298.902695	5.187405
4.399024	301.520532	5.192410
4.501221	303.001029	5.197414
4.127433	310.762814	5.202419
4.416561	302.470010	5.207424
4.026144	314.989428	5.212429
4.216051	311.413329	5.217434
4.209179	311.806676	5.222438
4.133656	311.710847	5.227443
4.136861	303.734638	5.232448
4.216515	307.227594	5.237453
4.109815	306.481733	5.242458
4.242779	315.860366	5.247462
4.176565	311.716713	5.252467
4.016136	309.353075	5.257472
4.229026	311.243438	5.262477
4.175448	299.185406	5.267482
4.463493	305.702050	5.272486
4.801832	311.922969	5.277491
4.335352	301.700895	5.282496
4.115362	312.380976	5.287501
4.480321	313.576958	5.292506
4.578084	324.568236	5.297510
4.380323	334.292595	5.302515
4.695340	329.725756	5.307520
4.499872	327.576375	5.312525
4.641588	326.738054	5.317530
4.394956	335.413345	5.322534
4.691861	331.924985	5.327539
4.573660	334.037740	5.332544
4.725097	337.114571	5.337549
4.682644	321.451332	5.342554
4.280984	322.380701	5.347558
4.456469	326.864799	5.352563
4.629379	331.997858	5.357568
4.543471	338.740413	5.362573
4.632805	327.802209	5.367578
4.564497	330.846815	5.372582
4.808624	331.982518	5.377587
5.088351	335.207051	5.382592
4.730796	330.858822	5.387597
5.075163	322.453006	5.392602
4.518204	343.179711	5.397606
4.836278	344.927152	5.402611
5.026859	340.648600	5.407616
4.621266	340.442812	5.412621
4.941084	341.490802	5.417626
4.854681	331.864422	5.422630
4.591936	340.194217	5.427635
5.123516	339.023116	5.432640
4.750785	347.240326	5.437645
5.203149	339.279589	5.442650
4.413650	332.205059	5.447654
4.517741	338.468786	5.452659
4.561497	333.181727	5.457664
5.002230	336.482431	5.462669
5.174657	336.366980	5.467674
4.791386	344.876891	5.472678
4.678008	338.842351	5.477683
5.215021	338.594207	5.482688
4.805092	331.416288	5.487693
5.293716	333.225757	5.492698
4.712466	334.173598	5.497702
5.078099	334.236869	5.502707
4.749791	339.969979	5.507712
4.503876	333.067075	5.512717
4.991757	326.505499	5.517722
4.877317	329.664853	5.522726
4.971793	326.015026	5.527731
5.184974	332.897671	5.532736
4.851776	341.124542	5.537741
4.945416	337.218582	5.542746
5.092155	347.977626	5.547750
4.789971	359.322257	5.552755
5.327833	355.018104	5.557760
5.314917	360.426873	5.562765
5.315234	358.228024	5.567770
5.188557	357.577019	5.572774
5.120942	346.163374	5.577779
5.546998	355.461593	5.582784
5.326117	352.063338	5.587789
5.198661	334.110142	5.592794
5.099419	331.091579	5.597798
5.090135	336.521921	5.602803
5.309487	345.849154	5.607808
5.321130	358.287021	5.612813
5.182376	355.644759	5.617818
5.293235	364.444737	5.622822
5.189172	359.709024	5.627827
4.982269	357.716443	5.632832
5.337157	363.197658	5.637837
5.260247	355.588235	5.642842
5.124879	360.316889	5.647846
5.139729	362.696829	5.652851
5.259223	351.870972	5.657856
4.860627	353.100418	5.662861
5.367102	360.997251	5.667866
5.208230	354.017513	5.672870
5.404467	365.857177	5.677875
5.546405	373.146393	5.682880
5.161234	378.812440	5.687885
5.912729	381.625012	5.692890
5.914705	374.822700	5.697894
5.621964	364.064182	5.702899
5.668980	359.330257	5.707904
5.413652	357.965302	5.712909
5.400109	360.128202	5.717914
5.358645	364.130402	5.722918
5.074425	366.977680	5.727923
5.361979	374.263207	5.732928
5.477327	390.588972	5.737933
5.569465	384.329432	5.742938
5.503742	386.702938	5.747942
5.531636	385.926627	5.752947
5.750093	382.899719	5.757952
5.601341	386.966084	5.762957
5.497784	380.360532	5.767962
5.558114	388.000978	5.772966
5.672204	389.913059	5.777971
5.957233	378.893735	5.782976
5.345360	384.721629	5.787981
5.873880	376.388354	5.792986
5.788347	388.167501	5.797990
5.610060	382.728339	5.802995
5.766807	385.687295	5.808000
5.630840	394.614301	5.813005
5.591276	390.529755	5.818010
5.478746	390.942718	5.823014
6.048689	387.411837	5.828019
6.030423	378.663827	5.833024
5.880651	395.698417	5.838029
6.132284	382.896792	5.843034
5.908010	388.211927	5.848038
5.899230	392.636146	5.853043
5.813485	384.692732	5.858048
5.823407	396.501314	5.863053
6.315116	384.646224	5.868058
6.147752	385.646684	5.873062
5.900683	386.621590	5.878067
5.818999	389.845456	5.883072
5.734118	395.603957	5.888077
6.023615	383.793006	5.893082
6.205442	382.666866	5.898086
5.989759	393.729135	5.903091
6.005936	388.098345	5.908096
5.891309	383.275688	5.913101
6.003762	390.389170	5.918106
6.445420	389.703460	5.923110
6.057835	381.762750	5.928115
6.188070	379.458250	5.933120
5.882772	382.669475	5.938125
5.709643	386.628906	5.943130
5.763513	384.260366	5.948134
6.114373	390.087062	5.953139
6.170914	384.731560	5.958144
6.020683	403.113971	5.963149
6.444289	400.814411	5.968154
6.303771	400.627462	5.973158
5.887960	391.064992	5.978163
6.245111	391.597815	5.983168
6.031869	397.135860	5.988173
6.444139	401.864680	5.993178
6.227833	416.530534	5.998182
6.353645	405.928285	6.003187
6.634201	411.142682	6.008192
6.208609	402.711176	6.013197
6.217787	394.148708	6.018202
6.086777	393.590124	6.023206
6.054191	398.907055	6.028211
6.197719	406.018870	6.033216
5.922463	408.507258	6.038221
6.574958	404.884428	6.043226
6.294431	414.485677	6.048230
6.411192	420.484871	6.053235
6.344583	417.129022	6.058240
6.090395	417.769683	6.063245
6.201574	418.859653	6.068250
6.327162	418.991937	6.073254
6.000503	413.063344	6.078259
6.474168	404.080544	6.083264
6.345738	403.932841	6.088269
6.382367	401.114572	6.093274
6.419302	402.399596	6.098278
6.366099	406.305558	6.103283
6.299946	408.255195	6.108288
6.157690	410.257810	6.113293
6.427440	403.866207	6.118298
6.614856	409.136234	6.123302
6.284469	409.592608	6.128307
6.323126	401.860768	6.133312
6.314126	413.153458	6.138317
6.061095	401.835084	6.143322
5.923774	395.896000	6.148326
6.145814	409.063600	6.153331
6.296026	410.735944	6.158336
5.957130	416.853537	6.163341
6.433742	399.834434	6.168346
6.318028	414.971837	6.173350
6.359472	414.095340	6.178355
6.515468	416.200214	6.183360
6.365287	421.408912	6.188365
6.770473	418.878103	6.193370
6.292706	417.076381	6.198374
6.316997	411.504431	6.203379
6.353069	395.012662	6.208384
6.278453	392.885585	6.213389
6.295174	388.096259	6.218394
6.232488	380.753526	6.223398
6.129955	391.386894	6.228403
6.279147	396.811562	6.233408
6.115038	408.232801	6.238413
6.015988	410.614663	6.243418
6.247392	413.413305	6.248422
6.215746	412.136904	6.253427
6.530127	412.704860	6.258432
6.344944	427.913201	6.263437
6.449474	413.372263	6.268442
6.715851	415.444133	6.273446
6.080657	410.262760	6.278451
6.441124	399.234843	6.283456
6.232592	403.709147	6.288461
6.259745	397.127531	6.293466
6.188968	389.893620	6.298470
6.526216	411.161379	6.303475
6.302297	392.191771	6.308480
6.180015	391.964018	6.313485
6.228114	387.634873	6.318490
6.498312	388.279309	6.323494
5.923881	391.652660	6.328499
6.194665	404.837977	6.333504
6.369747	415.488246	6.338509
6.471247	409.148147	6.343514
6.327648	399.480016	6.348518
5.792233	398.968577	6.353523
6.352115	405.705523	6.358528
6.127007	418.259385	6.363533
6.551212	410.692138	6.368538
6.617407	416.246792	6.373542
6.317295	398.155901	6.378547
6.520299	389.392417	6.383552
5.919051	394.753593	6.388557
6.210707	401.339311	6.393562
6.268067	414.706560	6.398566
6.416163	411.181243	6.403571
6.401160	401.050169	6.408576
6.230256	399.700539	6.413581
6.249270	394.610301	6.418586
6.236775	397.035631	6.423590
6.316448	404.562343	6.428595
6.303018	402.213770	6.433600
6.358203	400.215178	6.438605
6.045034	393.879536	6.443610
6.230337	407.875421	6.448614
6.348526	417.019128	6.453619
6.472999	412.523063	6.458624
6.452989	411.975670	6.463629
6.366722	406.148855	6.468634
6.304290	394.440147	6.473638
6.009033	401.142555	6.478643
6.664976	393.412686	6.483648
6.130520	400.411760	6.488653
6.372069	384.846614	6.493658
6.206133	391.563685	6.498662
5.878834	384.774671	6.503667
6.776122	400.526289	6.508672
6.054735	403.792810	6.513677
6.410966	394.809316	6.518682
6.123940	398.334071	6.523686
6.439246	397.051108	6.528691
6.724344	394.896499	6.533696
6.001562	393.240494	6.538701
6.126689	390.221789	6.543706
6.150158	389.936542	6.548710
6.053257	401.948419	6.553715
6.150096	410.718965	6.558720
6.257017	414.324754	6.563725
6.478426	415.255195	6.568730
6.463757	412.811902	6.573734
6.314698	414.062611	6.578739
6.507383	403.222164	6.583744
6.179154	400.862493	6.588749
6.180895	393.243971	6.593754
5.989868	399.996589	6.598758
6.019134	410.834071	6.603763
6.066225	415.379310	6.608768
6.122895	417.053564	6.613773
6.219970	414.206899	6.618778
6.512759	415.955120	6.623782
6.403621	415.798086	6.628787
6.827850	424.470210	6.633792
6.735351	422.320605	6.638797
6.415069	398.493864	6.643802
6.024211	396.672286	6.648806
6.007273	386.981278	6.653811
6.239038	395.056937	6.658816
6.381489	407.322613	6.663821
6.802123	400.898029	6.668826
6.442741	396.553231	6.673830
6.094630	387.027679	6.678835
5.956764	384.322000	6.683840
6.054338	388.834062	6.688845
6.041918	389.823053	6.693850
6.305985	400.370875	6.698854
6.187630	414.145127	6.703859
6.750504	412.330078	6.708864
6.339799	418.911263	6.713869
6.285723	405.919939	6.718874
6.226469	402.214939	6.723878
6.097230	403.041787	6.728883
6.389337	401.654870	6.733888
6.404429	419.837554	6.738893
6.204528	416.480311	6.743898
6.277157	413.023691	6.748902
6.459581	414.346175	6.753907
6.419553	393.190279	6.758912
6.127175	392.419541	6.763917
6.126454	390.796645	6.768922
6.172786	406.288457	6.773926
6.168414	408.538520	6.778931
6.292638	411.613274	6.783936
6.384335	422.308167	6.788941
6.569424	415.303325	6.793946
6.327574	407.551882	6.798950
6.109046	401.802609	6.803955
6.446364	393.998963	6.808960
5.965134	409.838669	6.813965
6.538562	409.629146	6.818970
6.437247	414.396804	6.823974
6.510709	406.488703	6.828979
6.177615	392.857467	6.833984
6.050463	389.726182	6.838989
6.068975	388.853257	6.843994
5.942767	408.905539	6.848998
6.113584	418.227712	6.854003
6.665295	402.734482	6.859008
6.245962	415.859578	6.864013
6.278549	411.051957	6.869018
6.449931	421.601567	6.874022
6.108573	428.143485	6.879027
6.725089	414.832614	6.884032
6.270669	429.769667	6.889037
6.462744	416.290763	6.894042
6.243044	407.529809	6.899046
5.956080	410.931171	6.904051
6.620189	402.298367	6.909056
6.233607	401.352472	6.914061
6.235638	403.440188	6.919066
6.174514	408.616034	6.924070
6.161706	415.739538	6.929075
6.541700	411.732032	6.934080
6.401216	415.547182	6.939085
6.354346	403.573455	6.944090
6.127289	397.524958	6.949094
5.903311	406.962376	6.954099
6.506627	406.336916	6.959104
6.190751	403.700079	6.964109
6.218656	411.902397	6.969114
6.199913	414.822243	6.974118
6.073648	421.273723	6.979123
6.276867	411.864796	6.984128
6.323716	423.537934	6.989133
6.353184	419.825444	6.994138
6.561015	415.123413	6.999142
6.312635	417.218481	7.004147
6.597770	412.203861	7.009152
6.297167	411.810885	7.014157
6.164642	398.850763	7.019162
6.206154	401.909920	7.024166
6.195984	411.899340	7.029171
6.615995	408.648059	7.034176
6.221030	407.323823	7.039181
6.393976	403.174550	7.044186
6.154045	395.014695	7.049190
5.843753	396.641679	7.054195
6.346176	405.361729	7.059200
6.342860	410.215367	7.064205
6.526653	414.372330	7.069210
6.243040	406.785576	7.074214
6.222002	413.866069	7.079219
6.267958	414.466326	7.084224
5.917654	412.540357	7.089229
6.250744	415.978057	7.094234
6.251586	418.088105	7.099238
6.405434	416.988466	7.104243
6.573043	416.440334	7.109248
6.360710	414.587795	7.114253
6.327190	420.059900	7.119258
6.421960	410.465380	7.124262
6.409206	414.694073	7.129267
6.177677	405.159850	7.134272
5.843570	396.986183	7.139277
6.256895	407.748049	7.144282
6.282999	398.119935	7.149286
6.190622	412.870894	7.154291
6.137964	412.689248	7.159296
6.475643	415.091697	7.164301
5.915702	414.343634	7.169306
6.292303	409.406522	7.174310
5.879270	418.933493	7.179315
6.250341	417.126160	7.184320
6.439029	422.209332	7.189325
6.551905	416.047791	7.194330
6.432304	409.814882	7.199334
6.268824	419.119502	7.204339
6.505742	405.747518	7.209344
6.707162	402.938392	7.214349
6.418983	405.125075	7.219354
6.415288	408.165962	7.224358
6.072233	405.027161	7.229363
6.620857	402.565769	7.234368
6.310424	407.688684	7.239373
6.248783	387.539058	7.244378
6.290307	390.360932	7.249382
6.312807	390.085328	7.254387
6.030588	384.640202	7.259392
6.471109	398.871586	7.264397
6.349134	395.027658	7.269402
6.257119	392.982384	7.274406
6.021604	392.920955	7.279411
6.306908	395.496070	7.284416
6.158854	404.380670	7.289421
6.170346	402.119965	7.294426
6.348926	413.487853	7.299430
6.476348	415.309277	7.304435
6.573697	405.701703	7.309440
6.327923	400.440720	7.314445
6.055225	401.454418	7.319450
6.271633	392.242761	7.324454
6.206836	406.480062	7.329459
6.870183	407.300566	7.334464
6.075990	392.883754	7.339469
6.191837	395.352376	7.344474
6.112366	388.578558	7.349478
6.390989	399.801148	7.354483
6.436543	384.276010	7.359488
6.052072	390.467127	7.364493
6.190545	402.116495	7.369498
6.607049	412.308400	7.374502
6.167682	396.067821	7.379507
6.192489	398.892300	7.384512
5.942880	401.088796	7.389517
6.325589	412.222423	7.394522
6.361944	410.808886	7.399526
6.387611	414.914539	7.404531
6.487959	421.381356	7.409536
6.293872	418.396527	7.414541
5.868348	414.973175	7.419546
6.418048	420.215272	7.424550
6.242359	427.794406	7.429555
6.570475	417.179634	7.434560
6.148719	418.434837	7.439565
6.274742	419.196633	7.444570
6.467641	421.428638	7.449574
6.226221	413.889095	7.454579
6.391509	413.053426	7.459584
6.217177	408.489991	7.464589
6.344783	413.585835	7.469594
6.183635	410.083357	7.474598
6.072942	418.607811	7.479603
6.476345	420.069895	7.484608
6.381373	419.439261	7.489613
6.098701	413.614550	7.494618
6.350942	412.882401	7.499622
6.172995	422.192439	7.504627
6.169048	416.520481	7.509632
6.307721	425.199100	7.514637
6.438475	413.498266	7.519642
6.393441	411.996161	7.524646
6.208651	429.419046	7.529651
6.281484	425.554272	7.534656
6.158372	418.629051	7.539661
6.323391	423.902568	7.544666
6.169092	414.631560	7.549670
5.988470	419.006612	7.554675
6.286583	417.821236	7.559680
5.963577	420.231640	7.564685
6.037869	416.664030	7.569690
6.068706	418.785227	7.574694
5.948555	433.581655	7.579699
6.022574	422.629959	7.584704
6.348322	418.678353	7.589709
6.401101	422.349520	7.594714
6.545243	417.945304	7.599718
6.323490	420.789191	7.604723
6.347114	419.766774	7.609728
6.122904	420.023121	7.614733
6.417851	414.456486	7.619738
6.099533	417.562178	7.624742
5.980442	427.239538	7.629747
6.282671	422.965729	7.634752
6.194582	417.354327	7.639757
6.289565	425.549372	7.644762
6.351177	419.696366	7.649766
6.063938	429.649841	7.654771
6.259079	428.682975	7.659776
6.458590	428.620253	7.664781
6.299789	424.067051	7.669786
6.471671	422.901328	7.674790
6.055828	423.260277	7.679795
6.262730	419.131024	7.684800
6.207787	418.373936	7.689805
5.805594	423.577580	7.694810
6.027397	418.791116	7.699814
6.154271	428.778191	7.704819
6.533506	439.361888	7.709824
6.368536	455.718701	7.714829
6.382597	437.819297	7.719834
6.468218	445.022399	7.724838
6.018704	428.932066	7.729843
6.716925	440.152626	7.734848
6.393369	435.090403	7.739853
6.167996	428.886610	7.744858
6.520032	428.078813	7.749862
6.141484	425.208123	7.754867
6.172686	417.170556	7.759872
6.061671	432.981116	7.764877
6.340145	434.431014	7.769882
6.474601	446.827675	7.774886
6.208689	441.126895	7.779891
6.168470	428.924328	7.784896
6.267831	431.579018	7.789901
6.372393	442.689531	7.794906
6.635357	431.012393	7.799910
6.137345	429.413136	7.804915
6.402881	426.951525	7.809920
6.259184	421.120992	7.814925
6.296723	429.125668	7.819930
6.548617	429.089591	7.824934
6.342947	427.840284	7.829939
6.342140	430.247981	7.834944
6.220251	442.947140	7.839949
6.140606	429.662389	7.844954
6.489743	429.294800	7.849958
6.174983	437.926965	7.854963
6.233302	423.231865	7.859968
6.181510	428.387281	7.864973
6.015141	426.970505	7.869978
6.279679	418.146807	7.874982
6.293294	425.781888	7.879987
6.537416	417.932631	7.884992
6.501089	415.302887	7.889997
6.269063	424.548580	7.895002
6.324728	416.231962	7.900006
6.128593	417.771572	7.905011
6.327536	422.274187	7.910016
6.387738	422.454615	7.915021
6.381159	415.191717	7.920026
6.605007	426.457653	7.925030
6.567949	420.790849	7.930035
6.569328	416.253838	7.935040
6.231895	413.443187	7.940045
6.160073	415.801827	7.945050
6.283250	417.968758	7.950054
6.423315	414.220067	7.955059
6.065183	427.734272	7.960064
6.390472	424.488246	7.965069
6.148062	426.857629	7.970074
6.095746	419.775853	7.975078
6.271325	416.145018	7.980083
6.239178	423.157642	7.985088
6.295113	427.587612	7.990093
6.203999	424.169139	7.995098
6.656075	423.219217	8.000102
6.266473	421.884653	8.005107
6.392543	418.694955	8.010112
6.494192	431.120473	8.015130
6.260145	430.604653	8.020147
6.479980	423.501745	8.025165
6.214223	417.793507	8.030182
6.244141	429.284861	8.035200
5.862174	437.113525	8.040218
6.108415	438.331115	8.045235
6.137804	427.796107	8.050253
6.084219	433.367841	8.055270
6.417241	423.262065	8.060288
6.350791	418.441089	8.065306
6.182931	426.413130	8.070323
6.372795	417.692887	8.075341
6.161460	421.985896	8.080358
6.471184	418.504305	8.085376
6.287841	426.876368	8.090394
6.221903	428.511772	8.095411
6.571269	425.263837	8.100429
6.050125	432.713401	8.105446
6.369734	435.112404	8.110464
6.643656	442.103684	8.115482
6.499796	447.818861	8.120499
6.786961	434.308956	8.125517
6.349335	432.256472	8.130534
6.444431	418.558743	8.135552
6.315381	423.296510	8.140570
6.162833	419.883737	8.145587
6.211130	431.596282	8.150605
6.226252	444.891827	8.155622
6.640101	443.277945	8.160640
6.672614	443.809322	8.165658
6.637283	444.509045	8.170675
6.681612	429.743134	8.175693
6.352918	436.190795	8.180710
6.674907	428.914198	8.185728
6.451591	421.044041	8.190746
6.265328	430.767178	8.195763
6.336395	416.606156	8.200781
6.240653	430.395454	8.205798
6.543152	427.044368	8.210816
6.456909	437.439868	8.215834
6.490518	440.694403	8.220851
6.641320	432.933242	8.225869
6.454288	433.508268	8.230886
6.488122	425.197304	8.235904
6.749856	436.043530	8.240922
6.315845	434.242935	8.245939
6.531614	430.570853	8.250957
6.457018	440.544840	8.255974
6.734233	443.515306	8.260992
6.862760	440.759322	8.266010
6.350461	427.099353	8.271027
6.600594	423.100046	8.276045
6.255234	427.609573	8.281062
6.578144	429.392709	8.286080
6.653280	441.934175	8.291098
6.504807	445.119235	8.296115
6.697653	431.289518	8.301133
6.676812	439.775134	8.306150
6.307273	430.656011	8.311168
6.534649	434.334790	8.316186
6.538163	442.845017	8.321203
7.112115	449.994705	8.326221
6.648079	442.834172	8.331238
6.583140	435.630438	8.336256
6.546431	428.185638	8.341274
6.134055	429.714043	8.346291
6.686790	439.748140	8.351309
6.627263	447.586564	8.356326
6.791933	444.793395	8.361344
6.771832	444.531428	8.366362
6.418017	452.485097	8.371379
6.438476	449.335702	8.376397
6.668485	447.750442	8.381414
6.675411	449.863631	8.386432
6.814843	449.879768	8.391450
6.788484	450.164704	8.396467
6.705966	452.468535	8.401485
6.674527	456.500025	8.406502
7.102563	446.180636	8.411520
6.715171	447.541059	8.416538
6.839085	451.021366	8.421555
6.463310	440.050839	8.426573
6.788777	448.690815	8.431590
6.789281	455.525864	8.436608
6.838808	452.595994	8.441626
6.575597	449.487609	8.446643
6.874629	447.512925	8.451661
7.066214	451.383463	8.456678
6.428914	437.847085	8.461696
6.791680	428.746484	8.466714
6.609909	450.646595	8.471731
6.944550	443.289131	8.476749
6.793513	454.594091	8.481766
6.609858	445.420773	8.486784
6.705193	445.992860	8.491802
6.763258	448.644015	8.496819
6.705280	446.756471	8.501837
6.681901	446.211006	8.506854
6.427262	447.762189	8.511872
7.098622	455.676160	8.516890
6.837287	453.946504	8.521907
6.622426	451.395453	8.526925
6.748689	445.474698	8.531942
6.574240	437.341317	8.536960
6.513969	449.657729	8.541978
6.847183	450.498878	8.546995
6.722356	445.081099	8.552013
6.898033	451.481793	8.557030
6.811405	445.976019	8.562048
6.575776	459.525200	8.567066
6.891747	450.390850	8.572083
6.725386	454.938784	8.577101
6.635475	460.273198	8.582119
6.910261	451.000099	8.587136
6.838844	447.776651	8.592154
6.765710	454.825127	8.597171
7.272273	454.821971	8.602189
6.794326	452.182500	8.607207
6.810168	460.832821	8.612224
6.868320	454.973158	8.617242
7.152460	468.034341	8.622259
6.780792	453.124905	8.627277
6.962410	457.905826	8.632295
7.161269	459.411648	8.637312
6.961324	450.755236	8.642330
6.272545	458.309801	8.647347
6.966734	461.606651	8.652365
7.346050	469.853263	8.657383
7.244382	474.974927	8.662400
7.524734	465.688332	8.667418
6.964528	452.717424	8.672435
6.977813	447.884026	8.677453
7.052483	440.623841	8.682471
6.509079	441.503650	8.687488
6.589336	446.795787	8.692506
6.633041	457.218401	8.697523
6.874082	461.144355	8.702541
6.898749	466.893257	8.707559
7.123785	474.826236	8.712576
7.245050	467.359979	8.717594
6.914605	471.535852	8.722611
6.869108	472.473833	8.727629
7.067216	474.626683	8.732647
7.043973	469.959905	8.737664
7.169627	472.739389	8.742682
7.547496	477.896840	8.747699
7.351057	467.355945	8.752717
7.424351	471.825547	8.757735
7.122809	463.298550	8.762752
7.077394	451.673850	8.767770
6.957941	458.593846	8.772787
7.204331	469.562396	8.777805
6.897873	462.102778	8.782823
7.034689	456.237179	8.787840
7.366324	467.504865	8.792858
7.102390	471.398996	8.797875
7.175528	470.409333	8.802893
7.021390	478.297212	8.807911
6.747688	476.720951	8.812928
7.372518	473.385940	8.817946
7.125924	472.524949	8.822963
7.119054	472.519685	8.827981
7.366716	474.961452	8.832999
7.067475	480.640874	8.838016
6.968069	472.047689	8.843034
7.161936	478.407694	8.848051
7.068191	481.363343	8.853069
7.204501	480.142948	8.858087
6.820731	477.466720	8.863104
7.150836	469.778607	8.868122
7.357844	476.575201	8.873139
7.068963	470.513957	8.878157
6.968133	477.806584	8.883175
7.118483	482.494554	8.888192
7.377202	467.950840	8.893210
6.969757	481.842355	8.898227
6.923777	474.556762	8.903245
6.838269	468.520656	8.908263
6.617594	483.796828	8.913280
6.990678	501.299981	8.918298
7.296238	499.523081	8.923315
7.568137	505.217723	8.928333
7.451074	502.654594	8.933351
7.587025	501.298560	8.938368
8.133737	502.866985	8.943386
7.652526	486.873250	8.948403
7.414726	470.134764	8.953421
7.608808	480.341484	8.958439
7.237028	480.617087	8.963456
7.290591	474.956939	8.968474
7.312631	481.899093	8.973491
7.222404	474.825507	8.978509
7.117919	472.755862	8.983527
7.152188	477.042202	8.988544
7.150435	471.504271	8.993562
7.484904	481.594464	8.998579
7.388821	484.096063	9.003597
7.658778	473.583530	9.008615
7.395872	476.275195	9.013632
7.221803	471.442560	9.018650
6.955725	476.204832	9.023667
7.446799	484.733838	9.028685
7.146866	491.798706	9.033703
7.644222	496.956493	9.038720
7.587465	500.108349	9.043738
7.589592	506.905298	9.048755
7.295660	501.324490	9.053773
7.622994	506.874808	9.058791
7.480839	501.910969	9.063808
7.183342	505.598903	9.068826
7.615247	495.452445	9.073843
7.496872	499.573216	9.078861
7.682006	495.612413	9.083879
7.128586	496.001500	9.088896
7.369119	495.386542	9.093914
7.516856	491.832332	9.098931
7.609656	500.256105	9.103949
7.437383	500.806745	9.108967
7.461626	495.220581	9.113984
7.660161	492.886014	9.119002
7.984431	498.793397	9.124019
7.590198	492.458226	9.129037
7.529578	481.747860	9.134055
7.205762	478.437477	9.139072
7.421638	484.598406	9.144090
7.729875	493.073836	9.149107
7.563319	492.023665	9.154125
7.734873	500.047030	9.159143
7.685889	497.911939	9.164160
7.587958	483.161822	9.169178
7.721339	489.297729	9.174195
7.330684	476.448722	9.179213
7.183368	479.456891	9.184231
7.402561	493.733666	9.189248
7.781310	489.222036	9.194266
7.597528	501.033873	9.199283
7.523092	498.290546	9.204301
7.883205	499.843845	9.209319
8.052754	505.892080	9.214336
8.004853	502.447219	9.219354
7.321301	490.562102	9.224371
6.988257	489.036103	9.229389
7.687304	486.254397	9.234407
7.929072	499.416870	9.239424
7.952551	495.998765	9.244442
7.899520	497.897242	9.249459
7.799469	501.920491	9.254477
7.781643	488.129842	9.259495
7.514344	488.493315	9.264512
7.978858	490.295434	9.269530
7.622199	475.503558	9.274547
7.829191	481.694270	9.279565
7.863606	477.564442	9.284583
7.327488	475.625113	9.289600
7.534896	483.548219	9.294618
7.484783	487.304925	9.299635
7.679072	484.273620	9.304653
7.638721	495.012287	9.309671
7.736542	491.895018	9.314688
7.792532	498.696200	9.319706
7.902006	497.498916	9.324723
7.659041	505.195519	9.329741
7.857149	499.014263	9.334759
7.503160	507.526537	9.339776
7.767117	502.600449	9.344794
7.689572	498.592185	9.349811
7.570375	506.067556	9.354829
8.039956	497.736049	9.359847
7.675464	510.794116	9.364864
7.722482	503.263668	9.369882
7.917838	509.639230	9.374899
7.782792	506.274205	9.379917
7.547033	507.898190	9.384935
7.449305	505.994740	9.389952
7.829114	508.340200	9.394970
7.950787	514.165528	9.399987
7.791280	519.110025	9.405005
8.176776	522.054179	9.410023
7.626908	504.221896	9.415040
8.106709	516.277551	9.420058
7.681102	506.854707	9.425075
7.810720	520.088302	9.430093
8.109713	523.538208	9.435111
7.817349	528.714823	9.440128
7.874768	532.871345	9.445146
8.195824	523.833992	9.450163
7.797062	532.113417	9.455181
8.245692	524.002901	9.460199
8.344438	515.189505	9.465216
7.949129	501.173608	9.470234
7.600213	495.689721	9.475251
7.499899	515.844771	9.480269
8.272346	512.903317	9.485287
7.760132	527.921974	9.490304
8.078843	525.496112	9.495322
8.140469	512.046509	9.500339
8.081072	528.174884	9.505357
7.986773	526.892565	9.510375
7.788470	522.218316	9.515392
7.960865	518.085930	9.520410
7.969966	518.201251	9.525427
8.035317	527.654903	9.530445
8.286890	515.649420	9.535463
8.101598	521.718195	9.540480
8.314857	511.741463	9.545498
8.585833	520.995846	9.550515
7.937291	509.840537	9.555533
7.993448	516.521784	9.560551
7.848498	520.138635	9.565568
7.895991	512.298854	9.570586
8.192334	524.897451	9.575603
7.806058	514.190434	9.580621
7.941943	522.800005	9.585639
7.775117	520.579122	9.590656
8.132439	518.311344	9.595674
8.097002	521.573489	9.600691
7.990373	517.377253	9.605709
8.131551	520.103836	9.610727
8.065901	520.521117	9.615744
8.245754	510.022591	9.620762
8.412465	515.121415	9.625779
8.010245	513.429467	9.630797
8.090231	516.058284	9.635815
7.961153	520.638298	9.640832
8.018493	519.180898	9.645850
8.248973	521.574855	9.650867
8.302036	517.770304	9.655885
8.093267	525.477371	9.660903
7.861653	529.069849	9.665920
8.512996	536.841812	9.670938
8.531527	538.404117	9.675955
8.435760	530.012301	9.680973
8.111854	523.457896	9.685991
8.000949	532.945304	9.691008
8.203134	535.709726	9.696026
8.547920	541.629708	9.701043
8.508097	537.845926	9.706061
8.374477	528.421788	9.711079
8.451030	539.199083	9.716096
8.151619	527.045859	9.721114
8.256743	520.655020	9.726131
7.845413	527.137669	9.731149
8.211431	541.035033	9.736167
8.391465	543.856552	9.741184
8.336089	550.230142	9.746202
8.838023	549.874273	9.751219
8.562791	542.586477	9.756237
8.534469	529.908226	9.761255
8.049445	530.517028	9.766272
8.478211	529.645554	9.771290
8.408833	523.411266	9.776307
8.152353	532.915028	9.781325
8.237219	541.172805	9.786343
8.714793	552.771259	9.791360
8.831197	544.766106	9.796378
8.594381	533.751797	9.801395
8.388053	531.230962	9.806413
8.287637	530.640686	9.811431
8.148323	529.185502	9.816448
8.121883	540.745661	9.821466
8.607188	538.590492	9.826483
8.654794	549.549017	9.831501
8.664132	540.213065	9.836519
8.572267	538.551685	9.841536
8.418361	535.498847	9.846554
8.306335	536.967875	9.851571
8.573273	545.320378	9.856589
8.783198	543.507873	9.861607
8.489267	536.854125	9.866624
8.521167	522.793786	9.871642
8.639609	525.034782	9.876659
8.545489	527.242604	9.881677
8.636154	533.524026	9.886695
8.279368	527.318707	9.891712
8.720995	538.348416	9.896730
8.590054	533.184015	9.901747
8.934056	535.541365	9.906765
8.553213	532.990900	9.911783
8.407159	527.058871	9.916800
8.230495	530.191533	9.921818
8.803222	534.242579	9.926835
8.781783	546.060727	9.931853
8.736296	542.489256	9.936871
8.345353	528.930229	9.941888
8.573250	550.170258	9.946906
8.899941	540.551375	9.951923
8.667000	556.201888	9.956941
8.544844	547.788927	9.961959
8.742030	538.751918	9.966976
8.476963	554.527347	9.971994
8.682225	549.856527	9.977011
8.565642	558.729477	9.982029
8.987797	547.353795	9.987047
8.754032	544.344946	9.992064
8.285018	553.758738	9.997082
8.785711	549.256507	10.002099
8.485848	552.329463	10.007117
8.493786	551.564532	10.012135
8.651491	548.810300	10.017152
8.499236	559.771548	10.022170
8.796736	549.109521	10.027187
8.706386	564.725218	10.032205
8.716302	550.598855	10.037223
8.981622	556.632196	10.042240
8.728633	554.235383	10.047258
8.816899	553.984943	10.052275
8.653580	553.940925	10.057293
8.748743	551.224830	10.062311
9.167250	546.293602	10.067328
8.843119	557.713936	10.072346
9.069294	549.054245	10.077363
8.988491	554.125347	10.082381
8.559278	554.261577	10.087399
9.019912	553.782755	10.092416
8.827830	544.143659	10.097434
9.118140	549.147512	10.102451
9.013922	552.313078	10.107469
8.962897	554.473170	10.112487
8.663999	552.408540	10.117504
8.486272	552.751757	10.122522
8.783094	553.065268	10.127539
8.535723	548.196689	10.132557
8.659403	549.796271	10.137575
9.112931	555.405849	10.142592
8.926866	555.324348	10.147610
8.832047	553.158519	10.152627
9.048385	561.392680	10.157645
8.593774	561.236231	10.162663
8.438219	562.551099	10.167680
8.613345	571.126183	10.172698
9.276978	572.707968	10.177715
9.194470	580.120856	10.182733
9.013620	575.806779	10.187751
9.307800	574.138937	10.192768
9.279431	577.586176	10.197786
8.940084	570.062209	10.202803
9.090156	581.506553	10.207821
8.885511	574.551723	10.212839
8.965803	575.927698	10.217856
8.857548	577.547615	10.222874
9.184028	574.763946	10.227891
9.435221	578.912398	10.232909
9.188240	586.303561	10.237927
9.167859	570.780778	10.242944
9.167813	579.357894	10.247962
8.999371	577.588517	10.252979
9.022748	576.511925	10.257997
8.909714	578.927818	10.263015
9.310558	585.167276	10.268032
9.332517	576.880180	10.273050
9.087950	577.091798	10.278067
9.335286	574.418277	10.283085
9.013253	578.649667	10.288103
8.875639	578.923525	10.293120
9.099062	577.263544	10.298138
9.219012	571.359509	10.303155
9.011011	571.328758	10.308173
9.274899	575.522569	10.313191
9.003612	574.024815	10.318208
8.734022	583.028892	10.323226
8.813631	581.495438	10.328243
8.892081	575.654665	10.333261
9.044035	572.434284	10.338279
9.250636	571.499572	10.343296
9.339840	572.580682	10.348314
9.339233	576.935589	10.353331
9.351745	572.793370	10.358349
9.024653	576.883542	10.363367
9.040021	578.998587	10.368384
9.666192	586.465235	10.373402
9.488692	574.166771	10.378419
9.369462	575.507541	10.383437
8.804231	585.400215	10.388455
9.307827	582.790931	10.393472
9.336425	596.068713	10.398490
9.354175	599.833811	10.403507
9.577481	604.179108	10.408525
9.362753	595.584885	10.413543
9.633552	584.463110	10.418560
9.277413	575.464897	10.423578
8.937514	576.524456	10.428595
9.202794	599.951920	10.433613
9.219204	606.610988	10.438631
9.596862	598.732387	10.443648
9.170040	607.334940	10.448666
9.438175	604.320518	10.453683
9.618617	603.762247	10.458701
9.779037	601.566140	10.463719
9.804248	598.532738	10.468736
9.659251	589.201855	10.473754
9.050197	590.764051	10.478771
9.462608	603.155292	10.483789
9.634843	603.620740	10.488807
9.731945	595.318781	10.493824
9.430243	589.881160	10.498842
9.353177	594.531987	10.503859
9.675505	601.979679	10.508877
9.522775	606.191027	10.513895
9.800961	598.892780	10.518912
9.647808	584.072285	10.523930
9.392186	577.961645	10.528947
9.459044	576.281861	10.533965
9.373121	592.660567	10.538983
9.930909	589.190812	10.544000
9.656623	581.290651	10.549018
9.262386	588.209300	10.554035
9.554474	593.717798	10.559053
9.473723	599.754544	10.564071
9.881692	600.511481	10.569088
9.661519	611.997711	10.574106
10.079453	612.491175	10.579123
9.924235	584.271973	10.584141
9.470307	585.952022	10.589159
9.672138	580.022612	10.594176
9.209239	574.423909	10.599194
9.570497	586.946175	10.604211
9.950871	593.943031	10.609229
9.636863	583.833766	10.614247
9.884246	587.051888	10.619264
9.601104	586.603665	10.624282
9.623737	590.222839	10.629299
9.965175	602.413699	10.634317
9.642271	600.690459	10.639335
9.727476	586.684884	10.644352
9.884995	593.284109	10.649370
9.503966	597.512066	10.654387
9.871877	598.439335	10.659405
9.991593	607.540595	10.664423
9.727627	593.535732	10.669440
9.651775	591.269119	10.674458
9.870631	613.495204	10.679475
9.894586	601.215846	10.684493
9.748415	611.122180	10.689511
9.772706	600.736181	10.694528
9.940677	605.026980	10.699546
9.784022	608.752964	10.704563
9.776815	601.726360	10.709581
9.711353	605.400277	10.714599
10.062441	609.836130	10.719616
9.943208	597.285589	10.724634
9.513217	593.843398	10.729651
9.727479	595.971658	10.734669
9.803972	609.008472	10.739687
9.963194	601.084987	10.744704
9.618225	605.017009	10.749722
9.737390	607.308393	10.754739
9.638092	613.673067	10.759757
9.683219	612.703535	10.764775
9.721295	610.873600	10.769792
9.680748	612.385152	10.774810
9.777009	609.397489	10.779827
9.999585	613.708190	10.784845
10.092851	636.805892	10.789863
10.228426	630.220932	10.794880
10.266504	615.989150	10.799898
9.674499	607.816565	10.804915
9.904669	604.419905	10.809933
10.094275	621.232247	10.814951
10.347037	619.892729	10.819968
10.057314	613.367681	10.824986
9.867870	610.850518	10.830003
10.069795	610.932662	10.835021
9.964329	624.717313	10.840039
10.206325	625.244482	10.845056
10.134983	626.142316	10.850074
9.913728	618.842929	10.855091
10.231370	623.694231	10.860109
10.340017	636.549340	10.865127
10.313984	618.010559	10.870144
9.666805	607.536603	10.875162
9.741489	618.418374	10.880179
10.133589	624.195322	10.885197
10.246153	632.638170	10.890215
10.472760	631.880215	10.895232
10.242699	625.519435	10.900250
10.411836	631.327944	10.905267
10.435541	624.466925	10.910285
10.039844	613.139645	10.915303
10.238184	623.172221	10.920320
10.185258	629.135220	10.925338
10.094961	632.244986	10.930355
10.285819	629.454022	10.935373
10.332630	633.665866	10.940391
10.310135	628.143738	10.945408
10.279096	632.869457	10.950426
10.198651	629.530620	10.955443
10.245257	626.029997	10.960461
10.314769	636.142597	10.965479
10.315725	634.163810	10.970496
10.311099	632.876988	10.975514
10.375092	632.652416	10.980531
10.255009	626.504879	10.985549
10.175009	637.451769	10.990567
10.363048	631.319371	10.995584
10.694085	630.115982	11.000602
10.157969	631.575311	11.005619
10.494697	626.896625	11.010637
10.766311	633.386587	11.015655
10.336720	629.139626	11.020672
10.550908	625.433037	11.025690
10.464272	638.962313	11.030707
10.294448	628.625454	11.035725
10.312758	635.331572	11.040743
10.319504	624.339243	11.045760
10.703554	630.186871	11.050778
10.023250	624.397947	11.055795
10.535685	622.285880	11.060813
10.608540	639.394118	11.065831
10.342553	631.779810	11.070848
10.791186	626.455720	11.075866
10.281675	630.280826	11.080883
10.382626	622.618859	11.085901
10.482896	631.921968	11.090919
10.495428	621.755529	11.095936
10.287428	625.353817	11.100954
10.152179	634.576836	11.105971
10.374016	635.662544	11.110989
10.478561	631.499672	11.116007
10.504765	629.687362	11.121024
10.321336	629.245702	11.126042
10.426185	643.925395	11.131059
10.677585	647.663592	11.136077
10.722116	644.680822	11.141095
10.451775	653.255877	11.146112
10.713260	647.938829	11.151130
10.744984	662.446892	11.156147
10.871301	644.452387	11.161165
10.587486	638.507057	11.166183
10.454821	641.279451	11.171200
10.689745	650.179765	11.176218
10.692912	659.169815	11.181235
10.824017	648.915475	11.186253
10.531792	653.590349	11.191271
11.008370	652.869210	11.196288
10.952843	652.489683	11.201306
10.478277	654.614748	11.206323
10.659511	651.405573	11.211341
10.795478	654.937690	11.216359
10.960731	657.613211	11.221376
10.714379	651.343318	11.226394
10.974694	658.841713	11.231411
10.732836	653.416846	11.236429
11.000785	662.318336	11.241447
10.736870	658.257005	11.246464
11.088914	650.309788	11.251482
10.631309	649.718318	11.256499
11.072370	650.347033	11.261517
10.790681	648.058813	11.266535
10.656172	650.670556	11.271552
10.825200	646.008508	11.276570
10.717530	650.733540	11.281587
11.042246	648.063739	11.286605
11.155772	650.094084	11.291623
11.059447	646.022441	11.296640
11.285780	646.242792	11.301658
10.837710	641.544286	11.306675
10.836200	636.375481	11.311693
11.211174	645.200342	11.316711
10.738977	646.431977	11.321728
10.945008	641.082540	11.326746
11.017330	651.134753	11.331763
10.991846	646.673398	11.336781
11.392829	652.644625	11.341799
10.953697	635.413484	11.346816
11.054447	631.573083	11.351834
10.531111	643.169649	11.356851
10.772181	643.412950	11.361869
11.240550	642.652065	11.366887
10.781510	653.266674	11.371904
11.274960	655.354629	11.376922
11.336645	653.334828	11.381939
11.275008	650.425388	11.386957
11.192623	652.246404	11.391975
11.054074	655.884376	11.396992
11.233742	654.953853	11.402010
11.171805	659.056407	11.407027
11.129167	653.635234	11.412045
10.975373	652.276965	11.417063
10.852278	655.360284	11.422080
11.311441	651.208465	11.427098
11.013158	651.538896	11.432115
10.977262	656.360048	11.437133
10.974157	656.732881	11.442151
11.072138	654.155183	11.447168
11.194741	647.865715	11.452186
10.885245	659.933908	11.457203
10.889362	665.742876	11.462221
11.189356	663.140035	11.467239
10.869203	665.102209	11.472256
11.438862	667.610630	11.477274
11.144675	673.857351	11.482291
11.188771	678.369419	11.487309
11.241208	683.088465	11.492327
11.115925	691.186534	11.497344
11.192403	686.728227	11.502362
11.262780	689.765651	11.507379
11.436968	682.694994	11.512397
11.678398	677.090736	11.517415
11.199842	678.427501	11.522432
11.209201	680.164810	11.527450
11.517464	686.888918	11.532467
11.150404	681.556116	11.537485
11.407798	682.926615	11.542503
11.248797	685.570577	11.547520
11.402136	683.646952	11.552538
11.327095	682.964361	11.557555
11.220518	688.919954	11.562573
11.579362	681.482887	11.567591
11.247840	680.530971	11.572608
11.538925	678.219839	11.577626
11.693118	682.923043	11.582643
11.480208	680.093954	11.587661
11.888484	677.038766	11.592679
11.796191	690.979202	11.597696
11.949720	671.787579	11.602714
11.503023	672.036981	11.607731
11.665172	671.942288	11.612749
11.916745	679.612460	11.617767
11.669040	683.100181	11.622784
11.784397	675.057265	11.627802
11.805069	668.916199	11.632819
11.416154	664.328393	11.637837
11.705134	663.021101	11.642855
11.516713	661.018150	11.647872
11.322868	662.383167	11.652890
11.659164	678.453226	11.657907
11.834655	676.472506	11.662925
11.877335	674.411482	11.667943
11.396165	674.562112	11.672960
11.744651	682.498054	11.677978
11.589956	681.872044	11.682995
11.390934	681.407565	11.688013
11.590637	683.800025	11.693031
11.181713	684.813535	11.698048
11.400706	689.026986	11.703066
11.199829	677.735601	11.708083
11.777408	678.728057	11.713101
11.871506	683.917127	11.718119
11.474569	685.966995	11.723136
11.841417	680.264316	11.728154
11.662039	680.696152	11.733171
11.868740	694.104062	11.738189
12.634207	689.554261	11.743207
11.944745	698.860445	11.748224
12.122061	684.038905	11.753242
11.852735	692.291940	11.758259
11.808306	688.953796	11.763277
12.114621	683.759141	11.768295
11.813315	685.431215	11.773312
11.912833	677.643220	11.778330
11.810798	683.493966	11.783347
11.865303	681.083973	11.788365
12.083813	686.263141	11.793383
11.972289	684.585874	11.798400
12.145264	678.231750	11.803418
12.168496	682.150641	11.808435
11.886082	683.444246	11.813453
12.093625	680.846329	11.818471
12.020319	694.222098	11.823488
12.030128	676.034269	11.828506
12.226947	681.418778	11.833523
12.008730	678.085604	11.838541
11.958470	677.859886	11.843559
11.978313	687.058785	11.848576
11.765259	679.600311	11.853594
11.793280	687.832294	11.858611
11.688386	694.699624	11.863629
12.062943	679.137346	11.868647
11.869581	681.458465	11.873664
12.046262	687.571921	11.878682
11.781685	691.456732	11.883699
11.963716	702.902489	11.888717
12.007697	695.675380	11.893735
12.017606	704.648625	11.898752
12.261035	706.377894	11.903770
12.344561	701.931109	11.908787
12.106395	709.851108	11.913805
12.279335	704.210170	11.918823
12.092245	716.644338	11.923840
11.891793	719.465166	11.928858
12.098063	710.221536	11.933875
12.060628	711.492779	11.938893
12.330311	704.748060	11.943911
12.388377	709.324231	11.948928
12.089602	707.000795	11.953946
12.356683	709.307032	11.958963
12.077849	714.771918	11.963981
12.425208	710.429216	11.968999
12.157398	713.724419	11.974016
12.062812	708.737337	11.979034
12.341334	709.325091	11.984051
12.025692	714.230838	11.989069
12.257009	712.607483	11.994087
12.155567	711.714414	11.999104
12.611467	727.134755	12.004122
12.511692	723.120434	12.009139
12.498714	723.144523	12.014157
12.489554	714.253158	12.019175
12.149348	710.143734	12.024192
12.394438	721.589153	12.029210
12.226647	732.193175	12.034227
12.326230	737.741158	12.039245
12.591128	738.858037	12.044263
12.578905	739.509993	12.049280
12.407815	737.687366	12.054298
12.294661	730.718230	12.059315
12.043702	747.551950	12.064333
12.658170	728.638783	12.069351
12.687653	740.789949	12.074368
12.190740	736.723852	12.079386
12.428956	738.832621	12.084403
12.350187	734.916009	12.089421
12.379037	736.148532	12.094439
12.131968	738.575847	12.099456
12.257991	743.188782	12.104474
12.586695	753.068595	12.109491
12.499164	763.470797	12.114509
12.769381	761.431139	12.119527
12.998338	762.178086	12.124544
12.552329	761.259768	12.129562
12.857920	756.447046	12.134579
12.613364	767.526931	12.139597
12.770448	760.250629	12.144615
12.780455	766.036622	12.149632
12.756274	764.314191	12.154650
13.061081	748.030589	12.159667
12.718064	743.340945	12.164685
12.457232	738.452320	12.169703
12.469966	752.250223	12.174720
12.954051	755.977461	12.179738
12.907630	766.029292	12.184755
12.641111	767.594974	12.189773
12.844924	757.496504	12.194791
12.793983	766.113191	12.199808
12.758971	764.035851	12.204826
12.899885	760.883425	12.209843
12.795962	761.104705	12.214861
12.912191	773.333902	12.219879
12.857043	774.547949	12.224896
13.038764	765.667863	12.229914
13.112178	757.716644	12.234931
13.114399	767.104514	12.239949
12.950059	761.825330	12.244967
12.908900	763.277032	12.249984
12.965556	757.635247	12.255002
13.123576	761.526858	12.260019
12.832671	776.381883	12.265037
12.826655	760.130884	12.270055
12.910978	761.357928	12.275072
13.050185	768.461827	12.280090
13.089745	763.450688	12.285107
12.587881	760.947433	12.290125
13.095775	755.961207	12.295143
13.244399	747.651154	12.300160
12.749209	756.595772	12.305178
13.063249	755.833666	12.310195
12.855467	765.617139	12.315213
13.015874	759.605760	12.320231
13.023357	766.591316	12.325248
13.034469	772.730579	12.330266
13.620244	753.708248	12.335283
13.242368	770.000033	12.340301
13.044148	768.566623	12.345319
13.064185	759.850564	12.350336
13.044209	765.107910	12.355354
13.295359	764.863665	12.360371
13.402984	769.078695	12.365389
13.061157	764.789635	12.370407
13.495001	770.885170	12.375424
12.897039	768.620932	12.380442
13.256740	755.415062	12.385459
13.249719	769.818795	12.390477
13.324515	761.883138	12.395495
12.999095	768.813232	12.400512
13.417840	761.928523	12.405530
13.598849	766.870563	12.410547
13.120888	770.214275	12.415565
13.064888	766.931565	12.420583
13.085307	775.833783	12.425600
13.269046	780.232619	12.430618
13.764400	791.351948	12.435635
13.567638	787.857628	12.440653
13.373896	773.835378	12.445671
13.164563	766.411001	12.450688
12.939467	784.957436	12.455706
13.210167	783.662450	12.460723
13.267693	791.242965	12.465741
13.339752	790.064110	12.470759
12.988975	780.588445	12.475776
12.956048	787.592924	12.480794
13.233398	792.235957	12.485811
13.604164	799.439512	12.490829
13.485332	789.075686	12.495847
13.391597	793.501948	12.500864
13.727664	811.105841	12.505882
13.712943	805.639252	12.510899
13.467933	798.816847	12.515917
13.455658	797.007355	12.520935
13.662242	807.019818	12.525952
13.635567	818.621217	12.530970
13.938979	811.113835	12.535987
13.785103	805.214487	12.541005
13.537942	795.637477	12.546023
13.413621	794.757433	12.551040
13.449111	807.078116	12.556058
13.685227	803.342831	12.561075
13.832483	806.532403	12.566093
13.811120	814.778445	12.571111
13.661425	814.195832	12.576128
13.552610	817.999616	12.581146
14.093945	817.748058	12.586163
13.933310	818.098086	12.591181
14.037708	807.819410	12.596199
13.848817	798.842380	12.601216
13.476237	800.692814	12.606234
14.010677	806.747454	12.611251
13.751093	817.315327	12.616269
14.126265	813.997034	12.621287
14.084570	798.565731	12.626304
13.601652	793.863143	12.631322
13.933646	793.107707	12.636339
13.717838	808.039426	12.641357
14.000934	805.253008	12.646375
13.786743	811.607239	12.651392
13.569112	813.297854	12.656410
14.057427	802.157855	12.661427
13.904269	802.516186	12.666445
13.837422	808.957925	12.671463
13.915835	815.380206	12.676480
13.773923	811.842628	12.681498
14.089153	810.629066	12.686515
13.980277	806.003934	12.691533
13.965401	805.977827	12.696551
14.516256	802.505955	12.701568
14.326780	811.586033	12.706586
14.539258	804.039164	12.711603
14.439242	806.490929	12.716621
13.915495	796.016578	12.721639
14.177658	793.201864	12.726656
13.979341	806.710786	12.731674
14.282712	796.082412	12.736691
14.546628	813.274674	12.741709
14.391099	799.350594	12.746727
14.407239	796.930780	12.751744
13.840845	796.507717	12.756762
14.012509	787.222099	12.761779
14.129080	798.129015	12.766797
14.176892	801.409806	12.771815
14.533662	807.324855	12.776832
13.818163	813.113371	12.781850
14.202534	809.569591	12.786867
14.027075	813.487889	12.791885
13.874074	822.937825	12.796903
14.393814	819.063706	12.801920
13.989946	821.070488	12.806938
14.105631	822.418882	12.811955
14.690922	828.954749	12.816973
14.237201	828.059718	12.821991
14.638654	813.865875	12.827008
14.257947	825.768546	12.832026
14.024236	814.728333	12.837043
14.467665	819.828341	12.842061
14.173303	819.148334	12.847079
14.606690	814.407215	12.852096
13.819690	820.191087	12.857114
14.330558	817.814161	12.862131
14.539241	815.506374	12.867149
13.997349	827.427831	12.872167
14.440577	839.984849	12.877184
14.338727	851.020476	12.882202
14.653548	836.944242	12.887219
14.385672	844.641714	12.892237
14.410744	846.802616	12.897255
14.637957	842.065188	12.902272
14.379524	845.838626	12.907290
14.212830	855.312801	12.912307
14.515859	853.277491	12.917325
14.489134	853.436261	12.922343
14.569376	845.297752	12.927360
14.143128	846.105691	12.932378
14.248771	851.933624	12.937395
14.221491	848.286675	12.942413
14.352884	866.316955	12.947431
14.756203	857.156175	12.952448
14.518675	860.588698	12.957466
14.635458	868.507151	12.962483
14.410053	866.292189	12.967501
14.349926	870.407132	12.972519
14.712883	867.368436	12.977536
15.047784	864.864270	12.982554
14.737486	872.754547	12.987571
15.231061	873.760094	12.992589
14.769012	874.769263	12.997607
15.170188	860.275631	13.002624
14.851801	860.615508	13.007642
14.493997	866.256833	13.012659
14.619547	872.245772	13.017677
14.775798	868.778522	13.022695
14.799697	872.643704	13.027712
14.870633	873.926487	13.032730
15.202162	869.617769	13.037747
15.132078	862.865932	13.042765
14.687574	863.200198	13.047783
15.052515	857.690260	13.052800
14.622436	866.583770	13.057818
14.882208	878.172168	13.062835
15.199954	883.686229	13.067853
14.959133	888.788652	13.072871
15.048172	884.647069	13.077888
15.162361	880.653047	13.082906
14.915047	876.081008	13.087923
15.159088	884.929529	13.092941
14.951513	881.468431	13.097959
14.896906	881.811419	13.102976
15.172620	875.198238	13.107994
14.776917	883.957020	13.113011
15.244668	874.618946	13.118029
15.188133	883.735166	13.123047
15.276812	876.251722	13.128064
15.221878	886.440642	13.133082
14.940545	881.075498	13.138099
15.024312	881.280180	13.143117
14.999695	881.924605	13.148135
15.271697	878.458265	13.153152
14.930353	887.088667	13.158170
15.221908	891.331893	13.163187
15.555087	875.813755	13.168205
15.086182	886.685652	13.173223
15.126307	874.132196	13.178240
15.323350	878.005134	13.183258
15.305908	878.623196	13.188275
15.471898	884.107237	13.193293
15.533780	892.595969	13.198311
15.201822	878.607779	13.203328
15.258418	891.682610	13.208346
15.501271	899.915956	13.213363
15.861842	900.371025	13.218381
15.644709	897.425796	13.223399
15.658935	883.443662	13.228416
15.023029	884.375761	13.233434
15.598451	877.520261	13.238451
15.498087	882.376757	13.243469
15.544110	880.258385	13.248487
15.705730	874.817966	13.253504
15.564120	885.853495	13.258522
15.165713	880.992561	13.263539
15.638801	893.046361	13.268557
15.539737	908.341831	13.273575
15.543131	914.955705	13.278592
15.872751	916.176126	13.283610
15.965449	906.855404	13.288627
15.592652	891.175777	13.293645
15.398035	890.442368	13.298663
15.819936	903.119513	13.303680
15.656653	903.204873	13.308698
15.586561	902.881256	13.313715
15.989569	902.256767	13.318733
15.644047	912.187995	13.323751
15.651402	918.148016	13.328768
15.587258	914.692981	13.333786
15.391425	911.047016	13.338803
15.806857	904.812850	13.343821
15.495267	903.526465	13.348839
15.363321	911.265917	13.353856
15.669005	899.649375	13.358874
15.495943	906.893464	13.363891
15.524194	909.325272	13.368909
15.628186	924.870002	13.373927
16.050499	922.831891	13.378944
16.072169	937.783547	13.383962
15.844753	933.173683	13.388979
16.042088	932.189903	13.393997
15.898457	930.378759	13.399015
16.041762	931.426221	13.404032
16.579525	929.568947	13.409050
16.008785	925.425940	13.414067
16.200034	912.886796	13.419085
15.835367	915.786870	13.424103
15.832392	901.791621	13.429120
15.949607	918.896376	13.434138
16.009624	929.190497	13.439155
16.364029	924.878204	13.444173
15.813503	941.872354	13.449191
15.990086	950.542067	13.454208
16.311111	936.035608	13.459226
15.835279	937.457172	13.464243
15.969752	935.220883	13.469261
15.912863	935.639965	13.474279
16.155029	930.284817	13.479296
16.031826	933.576480	13.484314
15.772566	940.496339	13.489331
16.017857	939.792265	13.494349
15.586613	942.248283	13.499367
15.973292	953.760167	13.504384
16.139082	957.082577	13.509402
16.295594	959.721636	13.514419
16.725182	956.388534	13.519437
15.833255	965.085762	13.524455
15.610115	954.277342	13.529472
16.331607	962.250006	13.534490
16.542644	960.582451	13.539507
16.319881	954.788451	13.544525
16.185939	965.450457	13.549543
16.403092	967.796058	13.554560
16.680140	965.786871	13.559578
16.289851	969.053854	13.564595
16.505381	955.409544	13.569613
16.379915	955.530041	13.574631
16.555832	957.837881	13.579648
16.736675	957.345808	13.584666
16.446481	960.934870	13.589683
16.822382	949.544044	13.594701
16.550103	957.702989	13.599719
16.471339	955.698709	13.604736
16.740684	955.199169	13.609754
16.408455	960.558836	13.614771
16.656074	953.703853	13.619789
16.603800	962.207235	13.624807
16.943545	953.870487	13.629824
16.853688	946.260179	13.634842
16.620003	960.386938	13.639859
16.677330	952.548588	13.644877
16.605663	951.313206	13.649895
16.601543	954.355963	13.654912
16.930848	951.294090	13.659930
16.596285	956.404816	13.664947
16.804443	961.778176	13.669965
16.964622	960.932722	13.674983
16.635695	959.046285	13.680000
16.818803	963.644077	13.685018
16.673539	962.319169	13.690035
16.841479	948.088994	13.695053
16.667220	957.725344	13.700071
16.553859	954.798662	13.705088
16.953581	964.812700	13.710106
16.913653	991.803700	13.715123
16.845288	989.949274	13.720141
16.828460	986.344850	13.725159
16.838908	988.896203	13.730176
17.259645	979.114122	13.735194
16.838948	990.609726	13.740211
17.037908	977.826343	13.745229
17.234135	984.618500	13.750247
17.039573	983.771472	13.755264
17.283447	985.049428	13.760282
16.945143	985.884704	13.765299
17.054300	981.910377	13.770317
17.132517	986.802212	13.775335
17.179074	986.397317	13.780352
17.406516	979.283538	13.785370
17.191627	992.369155	13.790387
17.453202	982.615009	13.795405
17.238814	987.858509	13.800423
17.113896	986.883875	13.805440
16.916055	979.126267	13.810458
16.839310	983.770833	13.815475
17.242620	993.664410	13.820493
17.350079	985.818241	13.825511
17.293656	988.083365	13.830528
17.297194	978.590298	13.835546
16.985365	981.624165	13.840563
17.213812	978.486474	13.845581
16.967803	982.415793	13.850599
17.057486	987.034449	13.855616
16.767666	987.309920	13.860634
16.969236	1003.508545	13.865651
17.635290	1004.370483	13.870669
17.961052	1006.045939	13.875687
17.514987	1007.352422	13.880704
17.329864	989.762659	13.885722
16.956705	995.109775	13.890739
17.452829	1011.335129	13.895757
17.530911	1015.643178	13.900775
17.501145	1012.690849	13.905792
17.540062	1011.532917	13.910810
17.580838	1022.688454	13.915827
17.685196	1013.776109	13.920845
17.793531	1010.805434	13.925863
17.712786	1011.692128	13.930880
17.943351	1004.533672	13.935898
17.801841	1011.091249	13.940915
17.641782	1000.020518	13.945933
17.647847	992.101772	13.950951
17.187621	994.155216	13.955968
17.800178	1005.603565	13.960986
17.855228	1014.292230	13.966003
17.716835	1016.964590	13.971021
17.817458	1017.662102	13.976039
17.869533	1020.756081	13.981056
17.932025	1010.285001	13.986074
17.797495	1024.683546	13.991091
17.843080	1013.823783	13.996109
17.816649	1010.186136	14.001127
17.793761	1015.283066	14.006144
18.025451	1014.637911	14.011162
17.482383	1012.216772	14.016179
18.061130	1011.766887	14.021197
18.254801	1010.206171	14.026215
17.871982	1016.271153	14.031232
18.096216	1011.726646	14.036250
17.518629	1019.772210	14.041267
17.772289	1009.391286	14.046285
17.720150	1015.057650	14.051303
17.612186	1025.706179	14.056320
17.892570	1002.918978	14.061338
17.917672	1011.861609	14.066355
17.620710	1003.115893	14.071373
17.961754	1014.417175	14.076391
18.050602	1029.472056	14.081408
18.400697	1019.678861	14.086426
17.889961	1027.837095	14.091443
18.399363	1032.690211	14.096461
18.609526	1026.361732	14.101479
17.987529	1015.485988	14.106496
18.051413	1015.056305	14.111514
18.314348	1023.961913	14.116531
18.402117	1032.411967	14.121549
18.472832	1018.319949	14.126567
18.270376	1017.654026	14.131584
18.007985	1014.583283	14.136602
18.201509	1025.285856	14.141619
18.125221	1037.567299	14.146637
18.608153	1033.582102	14.151655
18.364662	1033.541096	14.156672
18.772504	1032.881138	14.161690
18.363634	1023.067254	14.166707
18.179386	1012.918607	14.171725
18.634703	1018.632194	14.176743
18.184302	1028.393626	14.181760
18.517204	1027.120495	14.186778
18.372995	1042.281099	14.191795
18.260637	1037.987804	14.196813
18.268739	1033.902969	14.201831
18.455348	1051.170613	14.206848
18.315664	1041.033946	14.211866
18.656539	1040.703145	14.216883
18.414396	1045.020034	14.221901
18.776153	1040.548781	14.226919
18.565529	1046.170403	14.231936
18.720292	1043.331347	14.236954
18.552631	1047.251638	14.241971
18.849564	1048.016415	14.246989
18.914910	1037.181963	14.252007
18.654825	1042.536734	14.257024
18.990850	1035.661644	14.262042
18.801984	1039.878720	14.267059
18.738376	1039.197490	14.272077
18.861278	1025.905215	14.277095
18.582129	1028.773057	14.282112
18.894908	1035.256757	14.287130
18.711090	1040.706949	14.292147
18.626067	1036.254765	14.297165
19.132288	1038.280819	14.302183
18.551464	1042.319083	14.307200
18.637683	1033.561029	14.312218
19.161138	1040.239144	14.317235
18.794623	1040.412950	14.322253
18.824036	1036.245902	14.327271
18.870392	1036.456411	14.332288
18.401667	1027.712179	14.337306
18.818934	1033.854567	14.342323
18.726500	1049.780277	14.347341
18.776274	1057.478876	14.352359
19.043970	1061.138885	14.357376
19.079917	1053.736159	14.362394
18.891849	1059.777146	14.367411
18.855741	1062.026494	14.372429
18.705193	1059.294930	14.377447
18.560828	1067.285688	14.382464
18.740291	1066.137429	14.387482
19.295588	1083.095240	14.392499
19.068168	1091.739561	14.397517
19.405397	1079.464747	14.402535
18.954587	1088.115445	14.407552
19.332279	1092.607236	14.412570
19.238374	1096.938927	14.417587
19.405927	1090.326728	14.422605
19.532546	1081.786420	14.427623
19.079936	1088.692260	14.432640
19.283944	1082.064921	14.437658
19.495707	1077.456068	14.442675
19.465890	1088.499561	14.447693
19.347389	1080.246724	14.452711
19.540903	1084.773500	14.457728
19.661089	1091.877334	14.462746
19.766627	1087.449117	14.467763
19.428553	1096.577722	14.472781
19.483552	1096.603851	14.477799
19.544708	1095.218392	14.482816
19.267461	1095.349898	14.487834
19.865647	1093.442174	14.492851
19.615240	1087.349482	14.497869
19.843229	1077.865597	14.502887
19.442042	1097.358100	14.507904
19.629416	1095.353394	14.512922
19.563386	1083.911370	14.517939
19.558392	1090.627600	14.522957
19.803115	1084.442040	14.527975
19.810822	1087.347280	14.532992
19.550004	1088.394557	14.538010
19.465177	1080.770785	14.543027
19.489796	1088.328149	14.548045
19.534345	1090.871052	14.553063
19.609233	1082.329330	14.558080
19.467205	1086.498100	14.563098
19.401976	1083.715380	14.568115
19.535261	1091.555624	14.573133
19.876057	1077.920119	14.578151
19.815591	1090.407415	14.583168
19.794117	1107.208900	14.588186
20.158179	1109.250783	14.593203
20.166048	1111.830958	14.598221
20.142706	1091.539811	14.603239
19.779913	1090.677946	14.608256
19.653026	1090.003411	14.613274
19.795143	1101.985809	14.618291
19.840108	1115.024746	14.623309
19.989381	1109.062320	14.628327
19.991496	1111.605521	14.633344
19.964089	1122.531896	14.638362
20.027020	1112.038599	14.643379
20.285910	1112.793524	14.648397
20.256415	1114.215036	14.653415
20.163967	1115.204542	14.658432
20.375719	1117.248050	14.663450
20.177941	1116.625576	14.668467
20.079718	1113.775405	14.673485
20.390086	1104.777293	14.678503
20.784077	1108.739537	14.683520
20.375348	1108.468640	14.688538
20.436182	1104.094716	14.693555
20.229328	1116.494370	14.698573
20.285586	1113.575966	14.703591
20.149684	1110.835803	14.708608
20.263152	1111.711199	14.713626
20.462101	1109.859321	14.718643
20.243760	1112.099179	14.723661
20.487370	1105.150088	14.728679
20.595458	1107.165554	14.733696
20.176099	1105.924335	14.738714
20.642129	1105.826509	14.743731
20.290476	1110.687478	14.748749
20.223519	1103.449074	14.753767
20.418922	1102.490833	14.758784
20.375588	1108.929019	14.763802
20.875939	1107.954856	14.768819
20.286746	1110.978281	14.773837
20.110079	1103.621260	14.778855
20.484263	1122.399785	14.783872
20.618239	1134.847371	14.788890
20.566427	1138.576077	14.793907
20.584455	1138.794153	14.798925
21.005832	1138.864223	14.803943
21.150354	1141.975387	14.808960
20.901516	1136.589327	14.813978
21.086851	1133.534060	14.818995
21.099965	1127.977832	14.824013
20.849144	1106.888961	14.829031
21.044582	1124.032226	14.834048
20.507734	1113.641777	14.839066
20.794481	1117.257806	14.844083
20.763060	1112.696274	14.849101
20.854701	1117.892165	14.854119
20.843884	1122.359247	14.859136
20.645271	1126.401137	14.864154
21.267061	1138.217359	14.869171
21.321447	1137.975343	14.874189
21.214194	1116.842016	14.879207
21.224000	1117.686215	14.884224
20.957782	1113.924936	14.889242
21.285018	1108.389233	14.894259
20.978389	1109.774999	14.899277
21.182721	1115.328881	14.904295
21.020915	1112.236148	14.909312
20.846554	1110.953628	14.914330
21.080351	1118.715120	14.919347
21.197809	1130.209075	14.924365
21.280090	1141.086827	14.929383
21.480585	1135.075392	14.934400
21.000201	1130.397565	14.939418
21.292779	1131.970904	14.944435
21.126112	1140.312302	14.949453
21.259970	1133.755826	14.954471
21.427374	1137.706018	14.959488
21.165075	1147.267816	14.964506
21.562595	1136.267978	14.969523
21.080634	1139.659716	14.974541
21.334581	1140.898246	14.979559
21.228619	1145.187645	14.984576
21.053856	1134.447322	14.989594
21.295115	1142.248687	14.994611
20.937699	1144.311387	14.999629
21.207073	1137.781148	15.004647
21.176661	1151.724932	15.009664
21.311137	1156.544939	15.014682
21.494959	1164.213246	15.019699
21.129168	1165.709212	15.024717
21.148453	1169.613046	15.029735
21.738684	1172.083624	15.034752
21.707663	1167.578819	15.039770
21.906081	1171.281195	15.044787
21.768438	1170.737719	15.049805
22.012326	1163.236301	15.054823
21.671628	1166.918473	15.059840
21.646618	1172.836281	15.064858
21.851226	1165.012776	15.069875
21.634133	1169.243745	15.074893
21.718234	1171.777345	15.079911
21.649406	1156.949556	15.084928
21.582020	1161.258199	15.089946
21.747035	1172.552274	15.094963
21.782634	1194.492037	15.099981
21.836271	1189.974046	15.104999
21.808564	1191.026059	15.110016
21.929266	1192.398946	15.115034
21.971938	1189.930768	15.120051
22.011778	1185.433860	15.125069
22.175343	1185.518825	15.130087
22.161999	1173.450007	15.135104
22.408223	1188.212278	15.140122
22.413552	1183.474593	15.145139
22.373117	1184.115179	15.150157
22.064885	1168.822884	15.155175
22.174579	1167.414083	15.160192
22.237649	1172.036930	15.165210
22.323502	1179.190326	15.170227
22.187764	1169.706219	15.175245
22.078116	1161.486679	15.180263
22.525072	1164.273050	15.185280
22.293382	1170.548082	15.190298
22.162120	1162.158339	15.195315
22.390933	1158.301042	15.200333
22.373998	1171.583185	15.205351
22.454512	1173.811234	15.210368
22.341185	1162.045166	15.215386
22.284169	1165.064637	15.220403
22.456795	1178.882157	15.225421
22.081350	1180.013557	15.230439
22.459122	1178.799701	15.235456
22.324197	1180.515342	15.240474
22.582570	1187.654504	15.245491
22.480966	1187.288451	15.250509
22.351791	1172.375371	15.255527
22.610844	1177.084470	15.260544
22.580930	1173.785000	15.265562
22.419753	1174.135119	15.270579
22.575941	1173.798357	15.275597
22.449225	1179.618394	15.280615
22.765246	1178.562475	15.285632
22.536673	1184.158533	15.290650
22.657297	1175.855797	15.295667
22.417052	1176.151954	15.300685
22.094535	1170.831004	15.305703
23.178498	1182.657348	15.310720
23.094484	1188.795786	15.315738
22.946928	1175.797971	15.320755
23.010495	1173.440150	15.325773
22.553699	1162.194614	15.330791
23.184480	1171.219748	15.335808
22.688308	1169.892655	15.340826
22.916300	1174.303634	15.345843
23.009032	1184.589654	15.350861
23.263221	1198.388178	15.355879
23.297201	1185.942756	15.360896
23.293317	1188.300711	15.365914
23.132382	1168.927142	15.370931
23.147006	1168.899597	15.375949
23.001046	1171.522666	15.380967
23.033400	1168.529080	15.385984
23.093763	1166.380040	15.391002
22.934929	1160.333025	15.396019
23.364130	1169.133925	15.401037
23.036793	1174.092110	15.406055
23.262518	1172.138228	15.411072
23.279639	1193.623279	15.416090
23.372830	1193.157470	15.421107
23.251018	1185.747694	15.426125
23.104634	1197.342731	15.431143
23.384432	1195.408830	15.436160
23.250157	1202.451342	15.441178
23.307079	1197.352172	15.446195
23.463124	1198.798452	15.451213
23.319184	1202.083925	15.456231
23.579475	1195.555078	15.461248
23.299189	1204.318137	15.466266
23.188763	1194.445070	15.471283
23.355978	1192.364596	15.476301
22.802400	1205.588307	15.481319
23.412134	1190.440248	15.486336
23.499475	1198.682165	15.491354
23.487801	1203.152557	15.496371
23.698620	1206.853010	15.501389
23.618324	1217.099716	15.506407
23.712243	1218.596695	15.511424
24.003069	1221.331646	15.516442
24.145147	1216.509545	15.521459
24.140698	1202.896140	15.526477
23.966956	1204.646230	15.531495
24.125170	1192.777904	15.536512
24.131148	1200.849455	15.541530
24.094535	1195.556567	15.546547
23.836917	1188.694950	15.551565
23.801040	1192.831438	15.556583
23.915065	1195.590756	15.561600
23.390156	1191.661455	15.566618
23.766576	1200.637845	15.571635
23.690791	1197.799946	15.576653
23.481406	1200.505477	15.581671
23.800412	1194.977341	15.586688
23.757746	1195.589873	15.591706
23.919692	1208.323488	15.596723
24.134140	1222.939258	15.601741
23.658827	1224.351295	15.606759
23.943831	1214.574440	15.611776
23.965993	1219.566584	15.616794
24.195299	1226.057038	15.621811
24.125284	1218.304670	15.626829
24.034956	1216.333720	15.631847
24.310633	1213.024533	15.636864
24.017887	1227.466811	15.641882
24.056658	1223.181498	15.646899
24.401383	1224.579469	15.651917
23.865963	1231.195300	15.656935
24.354897	1225.924719	15.661952
24.421102	1236.249612	15.666970
24.600971	1240.715437	15.671987
24.518052	1239.317685	15.677005
24.367804	1237.258232	15.682023
24.575052	1246.822716	15.687040
24.820042	1236.269441	15.692058
24.488500	1234.881997	15.697075
24.570954	1224.893676	15.702093
24.238613	1231.089726	15.707111
24.467559	1237.018509	15.712128
24.607871	1241.288522	15.717146
24.501803	1246.426870	15.722163
24.601372	1242.397174	15.727181
24.595083	1246.573249	15.732199
24.608418	1239.290732	15.737216
24.632734	1247.457278	15.742234
24.595038	1238.342877	15.747251
24.589420	1237.756752	15.752269
24.703750	1243.324687	15.757287
24.691140	1246.034301	15.762304
24.855350	1242.909721	15.767322
24.674882	1248.062810	15.772339
24.643582	1238.341500	15.777357
24.304716	1257.802385	15.782375
24.625668	1259.929893	15.787392
24.877774	1263.361998	15.792410
25.027237	1267.286611	15.797427
25.132855	1264.843335	15.802445
24.907423	1267.358870	15.807463
25.193147	1259.992909	15.812480
25.328128	1262.954102	15.817498
25.320173	1267.253517	15.822515
25.303500	1253.932310	15.827533
25.098929	1264.962096	15.832551
24.914880	1260.174980	15.837568
25.296134	1266.114773	15.842586
25.095659	1262.112853	15.847603
25.465878	1254.853659	15.852621
25.352342	1263.597096	15.857639
25.227159	1262.499412	15.862656
25.238716	1259.628970	15.867674
25.211582	1264.448922	15.872691
25.437232	1251.105768	15.877709
25.127417	1262.057264	15.882727
25.194890	1262.791505	15.887744
25.392101	1261.432187	15.892762
25.386805	1261.057450	15.897779
25.406198	1262.821656	15.902797
25.343615	1263.292125	15.907815
24.988412	1264.546610	15.912832
25.503953	1269.345188	15.917850
25.441583	1285.209623	15.922867
25.589160	1278.584686	15.927885
25.648325	1293.369856	15.932903
25.561409	1279.014996	15.937920
25.723572	1291.745482	15.942938
25.568158	1288.901031	15.947955
26.127709	1289.053732	15.952973
26.001839	1284.841375	15.957991
25.992825	1282.709434	15.963008
26.221464	1280.490000	15.968026
25.712058	1274.832043	15.973043
25.647688	1270.966720	15.978061
25.785618	1280.428405	15.983079
25.659909	1276.534762	15.988096
25.780875	1271.611792	15.993114
25.959278	1290.342081	15.998131
26.133057	1272.573083	16.003149
25.768310	1279.657820	16.008167
26.146117	1284.373705	16.013184
26.312111	1278.111974	16.018202
26.075416	1281.560226	16.023219
26.448203	1270.021358	16.028237
25.981194	1287.308945	16.033255
26.176423	1274.951965	16.038272
26.150214	1278.992293	16.043290
26.107004	1284.111399	16.048307
26.151686	1276.344303	16.053325
26.008949	1279.998833	16.058343
26.187936	1276.824609	16.063360
26.432190	1269.884822	16.068378
26.192364	1274.463337	16.073395
26.267831	1274.603044	16.078413
25.968392	1279.550603	16.083431
26.123465	1265.416853	16.088448
26.272759	1286.569013	16.093466
26.615463	1297.573571	16.098483
26.413854	1301.395061	16.103501
26.759993	1308.949796	16.108519
26.235147	1308.087904	16.113536
26.764785	1304.152181	16.118554
26.174871	1300.242443	16.123571
26.740822	1295.723556	16.128589
26.620866	1306.831712	16.133607
26.550799	1309.228389	16.138624
26.806172	1305.919191	16.143642
26.608195	1304.400493	16.148659
27.112693	1297.729445	16.153677
27.090663	1304.741898	16.158695
26.940321	1298.592528	16.163712
26.799153	1297.181749	16.168730
26.492211	1302.382947	16.173747
26.729225	1300.518812	16.178765
26.836834	1294.521786	16.183783
26.898828	1301.511688	16.188800
27.026307	1305.370304	16.193818
27.195479	1301.733701	16.198835
26.723808	1299.481287	16.203853
26.939973	1298.485089	16.208871
27.126238	1307.478516	16.213888
27.289119	1299.320622	16.218906
26.981686	1302.937682	16.223923
27.127603	1296.426606	16.228941
27.095963	1296.365239	16.233959
26.989570	1304.501669	16.238976
27.231221	1297.211983	16.243994
26.840078	1303.641275	16.249011
27.039844	1299.315100	16.254029
27.008405	1305.476950	16.259047
26.831303	1316.720241	16.264064
27.514332	1316.194153	16.269082
27.324857	1317.763666	16.274099
27.383617	1319.894134	16.279117
27.189320	1322.341713	16.284135
27.201598	1328.717672	16.289152
27.433153	1321.527377	16.294170
27.454386	1326.668019	16.299187
27.833918	1321.954087	16.304205
27.523713	1324.271390	16.309223
27.306606	1326.163942	16.314240
27.897987	1320.173638	16.319258
27.695464	1325.393299	16.324275
27.548928	1310.561701	16.329293
27.815378	1315.670472	16.334311
27.742753	1327.459238	16.339328
27.938444	1318.456782	16.344346
27.716788	1319.614739	16.349363
27.386462	1312.363606	16.354381
27.618315	1329.589762	16.359399
27.811100	1321.910042	16.364416
27.767007	1316.182781	16.369434
27.363360	1318.116999	16.374451
27.937294	1320.940430	16.379469
27.755764	1326.500806	16.384487
28.037138	1334.469579	16.389504
28.279505	1342.640090	16.394522
28.044206	1336.450285	16.399539
28.178347	1330.619530	16.404557
27.975759	1335.968592	16.409575
28.010204	1337.986083	16.414592
28.153576	1338.705355	16.419610
28.269727	1342.133396	16.424627
27.930581	1339.481646	16.429645
28.261858	1342.563768	16.434663
28.370126	1341.448667	16.439680
28.279536	1339.143228	16.444698
28.342564	1342.996107	16.449715
28.204182	1339.221188	16.454733
28.280287	1334.450353	16.459751
27.823412	1339.157352	16.464768
28.211908	1335.328804	16.469786
28.177492	1338.893896	16.474803
28.633342	1340.811063	16.479821
27.982621	1340.713539	16.484839
27.858798	1341.808928	16.489856
28.507023	1352.538734	16.494874
28.446819	1367.276279	16.499891
28.467500	1365.183886	16.504909
28.741042	1372.358630	16.509927
28.617452	1368.925386	16.514944
29.205161	1372.210586	16.519962
28.697920	1369.259954	16.524979
28.751890	1366.218789	16.529997
28.658672	1372.803693	16.535015
28.753943	1376.304420	16.540032
28.929833	1360.516861	16.545050
28.913694	1363.656233	16.550067
29.085118	1362.786919	16.555085
28.857051	1364.791635	16.560103
28.851063	1369.005562	16.565120
28.596826	1361.568993	16.570138
28.710163	1364.855465	16.575155
28.535283	1367.375767	16.580173
28.826282	1367.854304	16.585191
28.896889	1362.964396	16.590208
28.864844	1357.083767	16.595226
28.847196	1371.578003	16.600243
29.074148	1373.597084	16.605261
29.299263	1377.579371	16.610279
29.206936	1386.868678	16.615296
29.435909	1381.853122	16.620314
29.187242	1384.438563	16.625331
29.439420	1384.105788	16.630349
29.514731	1379.215143	16.635367
29.269405	1378.540102	16.640384
29.333164	1364.900175	16.645402
29.271827	1371.641062	16.650419
29.473019	1380.073622	16.655437
29.505708	1381.327682	16.660455
29.493439	1388.698412	16.665472
29.913085	1378.588078	16.670490
29.522339	1383.998007	16.675507
29.586214	1384.448790	16.680525
29.650913	1371.067490	16.685543
29.703688	1384.099096	16.690560
29.933901	1377.032065	16.695578
29.407770	1363.329347	16.700595
29.607294	1370.821728	16.705613
29.840034	1370.031230	16.710631
29.638611	1370.479137	16.715648
29.713093	1379.004008	16.720666
29.679749	1381.707403	16.725683
29.619076	1383.913279	16.730701
29.768646	1378.439869	16.735719
29.823392	1382.398189	16.740736
30.121637	1370.956070	16.745754
29.740497	1376.392904	16.750771
29.766911	1374.593109	16.755789
30.010182	1374.116552	16.760807
29.824653	1375.272044	16.765824
30.041756	1384.377474	16.770842
30.020754	1380.568491	16.775859
29.845580	1388.804032	16.780877
29.910005	1393.713905	16.785895
29.798909	1411.040873	16.790912
30.216454	1404.919814	16.795930
30.172426	1401.840252	16.800947
29.910881	1406.450584	16.805965
30.010779	1406.472879	16.810983
29.691853	1408.267683	16.816000
29.953738	1418.877798	16.821018
30.369070	1433.430905	16.826035
30.159600	1429.878476	16.831053
30.560165	1425.864991	16.836071
30.740724	1427.250668	16.841088
30.631550	1424.913397	16.846106
30.583675	1422.045871	16.851123
30.793794	1432.294822	16.856141
30.649128	1425.260892	16.861159
30.507235	1428.290466	16.866176
30.907420	1424.396963	16.871194
31.047389	1424.873770	16.876211
30.808704	1430.578777	16.881229
30.999756	1424.874830	16.886247
30.579566	1419.477493	16.891264
31.112716	1412.817722	16.896282
31.125826	1413.468915	16.901299
30.470073	1417.219125	16.906317
30.908002	1415.440462	16.911335
30.973426	1423.269328	16.916352
31.210665	1420.111256	16.921370
31.017134	1426.364657	16.926387
30.909896	1430.203040	16.931405
31.139287	1414.735309	16.936423
31.014474	1427.639961	16.941440
30.969545	1424.866650	16.946458
31.298301	1416.537709	16.951475
31.394662	1424.276551	16.956493
31.235298	1415.641753	16.961511
30.973157	1425.288881	16.966528
31.067531	1416.478877	16.971546
31.301347	1416.745411	16.976563
31.365101	1421.929953	16.981581
31.447212	1415.839026	16.986599
31.295216	1426.459935	16.991616
31.390050	1418.438815	16.996634
31.443569	1427.418257	17.001651
31.207965	1428.458470	17.006669
31.707134	1420.286034	17.011687
31.524671	1418.297847	17.016704
31.475232	1413.000579	17.021722
31.564337	1416.865194	17.026739
31.170988	1421.915776	17.031757
31.362498	1414.655940	17.036775
31.330587	1421.976092	17.041792
31.515712	1433.898368	17.046810
31.824725	1438.763861	17.051827
31.620716	1449.938841	17.056845
31.703428	1444.144459	17.061863
31.582902	1442.490612	17.066880
31.654680	1445.307039	17.071898
31.656290	1453.780175	17.076915
31.528913	1448.510811	17.081933
31.697403	1448.598166	17.086951
31.885349	1450.604394	17.091968
31.774342	1450.435461	17.096986
32.089429	1451.705520	17.102003
31.984175	1461.407137	17.107021
32.154841	1470.182167	17.112039
32.364210	1480.437574	17.117056
32.163897	1470.966517	17.122074
32.616945	1460.762573	17.127091
32.540492	1466.521228	17.132109
32.753635	1451.059152	17.137127
32.641413	1446.904593	17.142144
32.116299	1437.136981	17.147162
32.536749	1429.705793	17.152179
32.187831	1440.168020	17.157197
32.193049	1432.018834	17.162215
32.531240	1437.747637	17.167232
31.946475	1445.311667	17.172250
32.452730	1457.174493	17.177267
32.161006	1462.493289	17.182285
32.695369	1455.341003	17.187303
32.766406	1460.710617	17.192320
32.459628	1462.784404	17.197338
32.836202	1453.958847	17.202355
32.635713	1462.368778	17.207373
32.970300	1463.121401	17.212391
32.623772	1467.520916	17.217408
32.707342	1463.215947	17.222426
32.948478	1465.308570	17.227443
32.658708	1462.655426	17.232461
32.662302	1463.096661	17.237479
32.904570	1458.650220	17.242496
32.853705	1462.615533	17.247514
32.666388	1469.265617	17.252531
33.131057	1472.166046	17.257549
32.911224	1464.320130	17.262567
32.821072	1462.629994	17.267584
32.584845	1475.387924	17.272602
33.282799	1490.162165	17.277619
32.778856	1487.005870	17.282637
33.096756	1476.453726	17.287655
33.321476	1480.167851	17.292672
33.198961	1481.846874	17.297690
33.522152	1487.436016	17.302707
33.417138	1484.684674	17.307725
33.272541	1480.288993	17.312743
33.380249	1485.217399	17.317760
33.360705	1485.119434	17.322778
33.467460	1477.415171	17.327795
33.198545	1488.846436	17.332813
33.471012	1476.594056	17.337831
33.555199	1479.821972	17.342848
33.341490	1480.464300	17.347866
33.715893	1486.673480	17.352883
33.410029	1505.943302	17.357901
33.900343	1499.886622	17.362919
34.194348	1497.363490	17.367936
33.783312	1487.325622	17.372954
33.917847	1478.149569	17.377971
33.653295	1486.626290	17.382989
33.968166	1493.037248	17.388007
34.247948	1495.445753	17.393024
33.759290	1494.849618	17.398042
34.058656	1485.881430	17.403059
33.853584	1491.694833	17.408077
34.011578	1504.867938	17.413095
34.081265	1512.083945	17.418112
34.036058	1509.436898	17.423130
34.201347	1508.660051	17.428147
34.121770	1504.418344	17.433165
34.372174	1502.728831	17.438183
34.502034	1507.395016	17.443200
34.009464	1504.789219	17.448218
34.414698	1497.439268	17.453235
34.432549	1499.298413	17.458253
34.399984	1504.075093	17.463271
34.425113	1498.005632	17.468288
34.954889	1496.619765	17.473306
34.964820	1495.504186	17.478323
34.381955	1485.998006	17.483341
34.412216	1480.994425	17.488359
34.429928	1477.999912	17.493376
34.243799	1488.042343	17.498394
34.568973	1490.951871	17.503411
34.729905	1498.036900	17.508429
34.618514	1499.486973	17.513447
34.607181	1494.294202	17.518464
34.401669	1501.843390	17.523482
34.769400	1496.815665	17.528499
34.510816	1501.050016	17.533517
34.445380	1489.475093	17.538535
34.561586	1501.139899	17.543552
34.525720	1519.146387	17.548570
34.755129	1522.250713	17.553587
34.734603	1525.182511	17.558605
34.879563	1521.240361	17.563623
34.923624	1523.698194	17.568640
35.111535	1520.863369	17.573658
34.982461	1518.983625	17.578675
34.988746	1520.885599	17.583693
34.688395	1516.084964	17.588711
35.252693	1526.038981	17.593728
35.195883	1548.309152	17.598746
35.535231	1538.264879	17.603763
35.764778	1539.598756	17.608781
35.003864	1528.523416	17.613799
35.066107	1533.739785	17.618816
35.318544	1550.435923	17.623834
35.612700	1551.463092	17.628851
35.936695	1555.666712	17.633869
36.014257	1548.844290	17.638887
35.825736	1535.019446	17.643904
35.365439	1532.209802	17.648922
35.432416	1527.102661	17.653939
35.427804	1525.358175	17.658957
35.538583	1535.692081	17.663975
35.870356	1549.352565	17.668992
35.796717	1547.770305	17.674010
35.746034	1543.246375	17.679027
36.133879	1547.380091	17.684045
35.853663	1539.931713	17.689063
36.268378	1543.559465	17.694080
36.165416	1549.742003	17.699098
36.369377	1545.809596	17.704115
35.778727	1531.555051	17.709133
35.748866	1542.040248	17.714151
36.189072	1541.719221	17.719168
36.061491	1543.051895	17.724186
36.430695	1539.358854	17.729203
36.153877	1539.651243	17.734221
36.161197	1541.193291	17.739239
36.514583	1538.140194	17.744256
36.165477	1541.053724	17.749274
36.181014	1541.127024	17.754291
36.343368	1548.577930	17.759309
36.517365	1546.209178	17.764327
36.480721	1540.758399	17.769344
36.004382	1546.727666	17.774362
36.190642	1541.425221	17.779379
36.344672	1539.656034	17.784397
36.238341	1541.673375	17.789415
36.361351	1543.579269	17.794432
36.249498	1560.701369	17.799450
36.328721	1552.695243	17.804467
36.627393	1561.582933	17.809485
36.446412	1562.608338	17.814503
36.522213	1568.501115	17.819520
36.184420	1564.397428	17.824538
36.524063	1569.374955	17.829555
36.721033	1578.568827	17.834573
36.632900	1583.953792	17.839591
36.915727	1584.982727	17.844608
36.881499	1587.099302	17.849626
37.250924	1583.182151	17.854643
37.520309	1590.786827	17.859661
37.071275	1590.455924	17.864679
37.269324	1583.598950	17.869696
37.195414	1583.626215	17.874714
37.579419	1573.426645	17.879731
37.429081	1577.940810	17.884749
36.992018	1591.509587	17.889767
37.454976	1584.598745	17.894784
37.407961	1576.587016	17.899802
37.209953	1573.395696	17.904819
36.982617	1576.271337	17.909837
37.055662	1590.669579	17.914855
37.639676	1593.059134	17.919872
37.467002	1590.296219	17.924890
37.631960	1599.596073	17.929907
37.927253	1597.501924	17.934925
37.588442	1595.427605	17.939943
37.651567	1586.480368	17.944960
37.758101	1599.535321	17.949978
37.993358	1602.922777	17.954995
37.816057	1587.606581	17.960013
37.734468	1598.929854	17.965031
37.981003	1597.932068	17.970048
37.794871	1601.987901	17.975066
38.054986	1603.335959	17.980083
38.112976	1598.031377	17.985101
37.865017	1600.247504	17.990119
37.978291	1588.278614	17.995136
37.686681	1599.549379	18.000154
37.603444	1598.135869	18.005171
37.592587	1603.108014	18.010189
38.048983	1597.138635	18.015207
38.191430	1593.951110	18.020224
38.221209	1606.588821	18.025242
38.316378	1609.448970	18.030259
38.192776	1607.309584	18.035277
38.177199	1613.813060	18.040295
38.608840	1612.246801	18.045312
38.509876	1613.208945	18.050330
38.593704	1610.746924	18.055347
38.993270	1620.739266	18.060365
38.582460	1611.938391	18.065383
38.753664	1612.381937	18.070400
38.629112	1612.142526	18.075418
39.198592	1608.336237	18.080435
39.083683	1606.126069	18.085453
38.811297	1608.450142	18.090471
38.836263	1596.293021	18.095488
38.737338	1601.026409	18.100506
38.730747	1614.143167	18.105523
39.254215	1612.998119	18.110541
39.217710	1612.827053	18.115559
39.072612	1605.149324	18.120576
38.757640	1593.445924	18.125594
38.618934	1611.253919	18.130611
39.240866	1601.099342	18.135629
38.848769	1612.808646	18.140647
38.696533	1609.572322	18.145664
38.916551	1607.310008	18.150682
38.715209	1610.784377	18.155699
39.228993	1620.241375	18.160717
39.222506	1634.860322	18.165735
39.255879	1635.606200	18.170752
39.270649	1634.862251	18.175770
39.413739	1631.460020	18.180787
39.520351	1633.242242	18.185805
39.785781	1639.998628	18.190823
39.845644	1630.521691	18.195840
40.095871	1627.705551	18.200858
39.793750	1633.912814	18.205875
39.935364	1624.697713	18.210893
39.434475	1637.203469	18.215911
39.798709	1627.003791	18.220928
40.138085	1628.039703	18.225946
40.026006	1624.017626	18.230963
39.935814	1627.316900	18.235981
40.155435	1621.362286	18.240999
40.494583	1612.378373	18.246016
40.290481	1610.680717	18.251034
39.768759	1602.212701	18.256051
39.984038	1594.892285	18.261069
39.951459	1595.206609	18.266087
40.263796	1611.410633	18.271104
40.447039	1624.977534	18.276122
40.684862	1612.550571	18.281139
40.428506	1591.790196	18.286157
40.207277	1589.284154	18.291175
40.632015	1588.062959	18.296192
40.391878	1596.864141	18.301210
40.339735	1585.637387	18.306227
40.635805	1582.211347	18.311245
40.153555	1595.705111	18.316263
40.561834	1592.981135	18.321280
40.247737	1590.641032	18.326298
40.292386	1609.455599	18.331315
40.532955	1610.778298	18.336333
40.445816	1620.158440	18.341351
40.818024	1613.896044	18.346368
40.543059	1620.944845	18.351386
40.102086	1620.085656	18.356403
40.452293	1615.707579	18.361421
40.867316	1627.076630	18.366439
41.244148	1641.711643	18.371456
41.307975	1643.336423	18.376474
41.128059	1628.967357	18.381491
41.509510	1615.340893	18.386509
41.142861	1620.611440	18.391527
41.181254	1612.602176	18.396544
41.042256	1611.105826	18.401562
40.807292	1621.531483	18.406579
41.188407	1630.595724	18.411597
40.929759	1636.651050	18.416615
41.183725	1636.620955	18.421632
41.339959	1642.851534	18.426650
41.427607	1646.646997	18.431667
41.603301	1644.956479	18.436685
41.521127	1646.114831	18.441703
41.141724	1641.405366	18.446720
41.226248	1635.629574	18.451738
41.195507	1638.039108	18.456755
41.680968	1648.996411	18.461773
41.476928	1666.199238	18.466791
41.799905	1666.473986	18.471808
42.066488	1668.149252	18.476826
41.616751	1666.852760	18.481843
41.960134	1668.645460	18.486861
41.747579	1671.663985	18.491879
41.915222	1664.483504	18.496896
41.691637	1660.914290	18.501914
42.171149	1662.606898	18.506931
41.957322	1657.265723	18.511949
42.041650	1671.763262	18.516967
42.094060	1669.498632	18.521984
42.000821	1661.146916	18.527002
41.858284	1672.927859	18.532019
42.262535	1673.350902	18.537037
42.232786	1684.252740	18.542055
42.798307	1688.598672	18.547072
43.032534	1671.397391	18.552090
42.399094	1666.784277	18.557107
42.366886	1658.445151	18.562125
42.246925	1662.702139	18.567143
42.420459	1667.472021	18.572160
42.881571	1668.766699	18.577178
42.532537	1677.714266	18.582195
42.776303	1675.214711	18.587213
42.857682	1680.431299	18.592231
42.671296	1678.999128	18.597248
42.601029	1683.068499	18.602266
42.446465	1688.116692	18.607283
42.661507	1683.630252	18.612301
42.993950	1679.513707	18.617319
42.695994	1678.234608	18.622336
42.914721	1683.909506	18.627354
42.713326	1685.556648	18.632371
42.579614	1678.833343	18.637389
42.456975	1695.928850	18.642407
42.760150	1708.015971	18.647424
43.222162	1709.651346	18.652442
43.187378	1712.664292	18.657459
43.253495	1703.296799	18.662477
43.308499	1705.251169	18.667495
43.366870	1701.325616	18.672512
44.060586	1704.559661	18.677530
43.595540	1712.064136	18.682547
43.789826	1708.256279	18.687565
43.352416	1698.544297	18.692583
43.455407	1705.007255	18.697600
43.638754	1704.691502	18.702618
43.525315	1706.378601	18.707635
43.813816	1700.782474	18.712653
44.059819	1712.626030	18.717671
43.653472	1710.697915	18.722688
43.715730	1698.358188	18.727706
43.584280	1710.197392	18.732723
44.097372	1722.561116	18.737741
43.982417	1728.562542	18.742759
43.870299	1731.669584	18.747776
44.125468	1725.179213	18.752794
44.073209	1719.528835	18.757811
43.837321	1715.759549	18.762829
43.837184	1727.726645	18.767847
43.460395	1728.470113	18.772864
44.123201	1736.654243	18.777882
44.196460	1749.563003	18.782899
44.283262	1744.149749	18.787917
44.226818	1752.426933	18.792935
43.880946	1752.051561	18.797952
44.275271	1741.976524	18.802970
44.158021	1755.132705	18.807987
44.388362	1752.761465	18.813005
44.488029	1766.089015	18.818023
44.856223	1772.359224	18.823040
45.372796	1766.651826	18.828058
44.889346	1771.618701	18.833075
45.297103	1744.944760	18.838093
45.154018	1742.852573	18.843111
44.737378	1745.470530	18.848128
44.709470	1738.579247	18.853146
44.805370	1750.247377	18.858163
44.885964	1762.167213	18.863181
45.162947	1760.583994	18.868199
45.006786	1770.533552	18.873216
45.133346	1769.412421	18.878234
45.015570	1772.289971	18.883251
45.174942	1767.117882	18.888269
45.248519	1769.555374	18.893287
45.040858	1764.916970	18.898304
45.487926	1764.168826	18.903322
45.198995	1765.144776	18.908339
45.205989	1762.849335	18.913357
45.379767	1767.991602	18.918375
45.244407	1781.661876	18.923392
45.401539	1786.317576	18.928410
45.260660	1792.853249	18.933427
45.633176	1794.332149	18.938445
45.606374	1788.649382	18.943463
45.413932	1788.635140	18.948480
45.561107	1777.285712	18.953498
45.290490	1796.364161	18.958515
45.821344	1799.295367	18.963533
46.545824	1785.489131	18.968551
46.705165	1780.597917	18.973568
46.940280	1772.747306	18.978586
46.953902	1768.740341	18.983603
46.623539	1774.324028	18.988621
46.586444	1769.772678	18.993639
46.392144	1753.373359	18.998656
46.587929	1737.380392	19.003674
46.333363	1739.319847	19.008691
46.272253	1739.395613	19.013709
46.278043	1730.744416	19.018727
46.104132	1742.410366	19.023744
46.516962	1748.998674	19.028762
46.301214	1763.524072	19.033779
46.528325	1757.782847	19.038797
46.904781	1767.207654	19.043815
46.831157	1766.868792	19.048832
46.865674	1765.544235	19.053850
46.674603	1769.626122	19.058867
46.640760	1766.478637	19.063885
47.168127	1764.206321	19.068903
46.812881	1759.051240	19.073920
47.080570	1761.950827	19.078938
46.815453	1768.527926	19.083955
46.785474	1756.798983	19.088973
47.008841	1759.187905	19.093991
46.694175	1768.227998	19.099008
46.640311	1758.942274	19.104026
46.754995	1785.424396	19.109043
47.239088	1788.672158	19.114061
47.621149	1787.744782	19.119079
47.179494	1793.560403	19.124096
47.313194	1786.287325	19.129114
47.467407	1797.851730	19.134131
47.219203	1793.478414	19.139149
47.474816	1791.668139	19.144167
47.124173	1801.464952	19.149184
47.700089	1801.514124	19.154202
47.546240	1816.455973	19.159219
47.626295	1807.862606	19.164237
47.814653	1811.216378	19.169255
47.431990	1811.717760	19.174272
47.725219	1813.568778	19.179290
47.661965	1813.868947	19.184307
47.650798	1821.599455	19.189325
48.197454	1824.155809	19.194343
48.089609	1832.608296	19.199360
48.550102	1830.040262	19.204378
48.277999	1830.915762	19.209395
48.129370	1819.381982	19.214413
48.367606	1821.541373	19.219431
48.384205	1835.954913	19.224448
48.841787	1834.078474	19.229466
48.581728	1831.389088	19.234483
48.476856	1827.268011	19.239501
48.769556	1806.876350	19.244519
48.160329	1818.793168	19.249536
48.451718	1816.200970	19.254554
48.407493	1834.458394	19.259571
48.538169	1836.656625	19.264589
48.923341	1847.686471	19.269607
48.898644	1846.771927	19.274624
48.789640	1838.940150	19.279642
49.139165	1846.649227	19.284659
48.821852	1838.954027	19.289677
49.083835	1835.738380	19.294695
49.063384	1833.387241	19.299712
49.232384	1833.127370	19.304730
49.016346	1840.530012	19.309747
49.178420	1842.789629	19.314765
49.177584	1842.470991	19.319783
48.946476	1840.247326	19.324800
49.049748	1837.816961	19.329818
49.149926	1834.733807	19.334835
48.771452	1830.914111	19.339853
49.231228	1835.342818	19.344871
49.221023	1859.748977	19.349888
49.574238	1849.815984	19.354906
49.257465	1854.722217	19.359923
49.513612	1852.277516	19.364941
49.740077	1856.174491	19.369959
49.678948	1856.714179	19.374976
50.115027	1854.875800	19.379994
49.987383	1842.631815	19.385011
49.975347	1844.189526	19.390029
49.806140	1844.304214	19.395047
50.015375	1849.523037	19.400064
49.972803	1843.950009	19.405082
49.925221	1852.459396	19.410099
49.716509	1848.414443	19.415117
50.057474	1852.508192	19.420135
50.101694	1872.399266	19.425152
50.601025	1868.704833	19.430170
50.561960	1870.869533	19.435187
50.724880	1875.502264	19.440205
51.087812	1863.885652	19.445223
50.548285	1861.463842	19.450240
50.526351	1846.470382	19.455258
50.557949	1842.002996	19.460275
50.474891	1847.917442	19.465293
50.937347	1849.129872	19.470311
50.747991	1865.380678	19.475328
50.496351	1869.367873	19.480346
50.876144	1865.079806	19.485363
50.490378	1877.548870	19.490381
50.846187	1866.065913	19.495399
51.052348	1866.103224	19.500416
50.698180	1871.179390	19.505434
51.251512	1864.677262	19.510451
50.740966	1870.995954	19.515469
50.898122	1868.983243	19.520487
50.799978	1883.260047	19.525504
50.985243	1884.894345	19.530522
50.996474	1890.588991	19.535539
51.040350	1893.851661	19.540557
51.202218	1889.685883	19.545575
51.182669	1892.371429	19.550592
51.366482	1909.523572	19.555610
51.483192	1914.643206	19.560627
51.482242	1920.753183	19.565645
51.767574	1921.519807	19.570663
51.670732	1916.728405	19.575680
51.848174	1913.914084	19.580698
51.972642	1916.558275	19.585715
51.770916	1926.546574	19.590733
51.602322	1909.183711	19.595751
51.710124	1915.655464	19.600768
51.647309	1921.917089	19.605786
51.929745	1922.703100	19.610803
52.142604	1942.059893	19.615821
52.284858	1939.920102	19.620839
52.469547	1934.586227	19.625856
52.159150	1937.206605	19.630874
52.784039	1937.904583	19.635891
52.370569	1933.935673	19.640909
52.549296	1917.859991	19.645927
52.298381	1921.462064	19.650944
52.417120	1934.496425	19.655962
52.432208	1932.477423	19.660979
52.308662	1939.827834	19.665997
52.700118	1934.884660	19.671015
52.579760	1933.508462	19.676032
52.471656	1939.695091	19.681050
52.927085	1933.163997	19.686067
52.478652	1935.834270	19.691085
52.694588	1931.720027	19.696103
52.478776	1939.091115	19.701120
53.021177	1955.742488	19.706138
53.013460	1954.007911	19.711155
52.739088	1958.124901	19.716173
53.128283	1952.787584	19.721191
53.265695	1953.921236	19.726208
52.912120	1958.656495	19.731226
53.377684	1961.575802	19.736243
53.368614	1980.077218	19.741261
53.640472	1982.569079	19.746279
53.771545	1983.766837	19.751296
53.740888	1980.230640	19.756314
53.896701	1976.848454	19.761331
53.788501	1972.961400	19.766349
53.824677	1961.266206	19.771367
53.842020	1967.136656	19.776384
53.721962	1967.511946	19.781402
53.842197	1973.707219	19.786419
53.693682	1973.695604	19.791437
54.409109	1963.516799	19.796455
54.136077	1979.490392	19.801472
54.054170	1975.400420	19.806490
54.089905	1964.371192	19.811507
54.108077	1974.145393	19.816525
54.470642	1973.110586	19.821543
54.414830	1968.145517	19.826560
54.456660	1969.941015	19.831578
54.687601	1961.264120	19.836595
54.394063	1970.354676	19.841613
54.389017	1955.579410	19.846631
54.804391	1966.737177	19.851648
54.474293	1971.121633	19.856666
54.833092	1957.738286	19.861683
54.526484	1974.367221	19.866701
54.577324	1970.332325	19.871719
54.728632	1971.255523	19.876736
54.350748	1983.767616	19.881754
54.868844	1999.008959	19.886771
54.966799	1996.528906	19.891789
54.960723	1990.656648	19.896807
55.222146	1995.207799	19.901824
55.009334	1994.432993	19.906842
55.376342	1989.862854	19.911859
55.078365	1996.284200	19.916877
55.079942	1991.139770	19.921895
54.909165	1996.095897	19.926912
55.098014	2006.607277	19.931930
55.219355	2004.606439	19.936947
55.509850	2014.085788	19.941965
55.299982	2014.052167	19.946983
55.940724	2014.280603	19.952000
55.307800	2013.037852	19.957018
55.300496	2008.980440	19.962035
55.475150	2032.487017	19.967053
55.855570	2034.232961	19.972071
56.205808	2037.119741	19.977088
55.981628	2041.976893	19.982106
56.331668	2038.419284	19.987123
56.312240	2040.006567	19.992141
56.649514	2032.048415	19.997159
56.366016	2036.447723	20.002176
56.448463	2038.258995	20.007194
56.382038	2037.199453	20.012211
56.687508	2044.315848	20.017229
56.531110	2023.930743	20.022247
56.331707	2011.517926	20.027264
56.192793	2022.661037	20.032282
56.295657	2025.971354	20.037299
56.618297	2031.459764	20.042317
56.672312	2017.868195	20.047335
56.411234	2034.515345	20.052352
56.373611	2034.006763	20.057370
56.665673	2029.025387	20.062387
56.681452	2043.369792	20.067405
56.619798	2042.176957	20.072423
56.926176	2048.759859	20.077440
56.760339	2056.019067	20.082458
57.110125	2048.696460	20.087475
57.370477	2054.538572	20.092493
57.022162	2060.071491	20.097511
57.548835	2062.665707	20.102528
57.234834	2055.373858	20.107546
57.200711	2057.272712	20.112563
57.133117	2070.951593	20.117581
57.506391	2084.003241	20.122599
57.786395	2089.457280	20.127616
57.760301	2080.858217	20.132634
58.066361	2072.472543	20.137651
57.943113	2075.587690	20.142669
57.960553	2072.713045	20.147687
58.002115	2065.640400	20.152704
57.859193	2073.893326	20.157722
58.084974	2071.907779	20.162739
57.916785	2072.325280	20.167757
58.148936	2074.277357	20.172775
57.605394	2070.650574	20.177792
57.675679	2072.624696	20.182810
57.972947	2086.313057	20.187827
58.268362	2089.170510	20.192845
58.272568	2103.785020	20.197863
58.588021	2087.946686	20.202880
58.513662	2098.691613	20.207898
58.821141	2097.090993	20.212915
58.721372	2095.582183	20.217933
58.367386	2088.930890	20.222951
58.721219	2084.211293	20.227968
58.766650	2087.145538	20.232986
58.785681	2080.234192	20.238003
59.167130	2088.702142	20.243021
59.052138	2090.698802	20.248039
58.844184	2093.883946	20.253056
59.273360	2103.114523	20.258074
59.384161	2107.660751	20.263091
59.042305	2103.686965	20.268109
59.434884	2116.410569	20.273127
59.728899	2112.662842	20.278144
59.587167	2123.664437	20.283162
59.532376	2118.150033	20.288179
59.252711	2116.157965	20.293197
59.341452	2120.136404	20.298215
59.620333	2105.177947	20.303232
59.697905	2113.535423	20.308250
59.504261	2104.350181	20.313267
59.399760	2108.453382	20.318285
59.399167	2110.643681	20.323303
59.374692	2112.061335	20.328320
59.523671	2131.122152	20.333338
59.893011	2127.034475	20.338355
60.203312	2128.134908	20.343373
60.098468	2136.987877	20.348391
60.449803	2132.991370	20.353408
60.230949	2138.305332	20.358426
60.322066	2137.959749	20.363443
60.729937	2140.629280	20.368461
60.708555	2137.785917	20.373479
60.562645	2126.352505	20.378496
60.228471	2134.808813	20.383514
60.216306	2138.118124	20.388531
60.277587	2139.074283	20.393549
60.524479	2145.975765	20.398567
60.867196	2154.086842	20.403584
60.617823	2156.719842	20.408602
60.895367	2163.468229	20.413619
60.700688	2156.564879	20.418637
60.870993	2159.915216	20.423655
61.349101	2150.401290	20.428672
60.980225	2159.408993	20.433690
61.160759	2152.993207	20.438707
61.433114	2143.609153	20.443725
61.211387	2150.602534	20.448743
61.368507	2147.822901	20.453760
61.149953	2160.016806	20.458778
61.416020	2165.132194	20.463795
61.445554	2164.370145	20.468813
61.372999	2169.367834	20.473831
61.512621	2168.443470	20.478848
61.549505	2169.444456	20.483866
61.498583	2168.164731	20.488883
61.595520	2175.424104	20.493901
61.866220	2192.443064	20.498919
62.192168	2190.050570	20.503936
62.027392	2182.350408	20.508954
62.362152	2191.201236	20.513971
62.586648	2180.038340	20.518989
62.316739	2188.244814	20.524007
62.733041	2178.765743	20.529024
62.742345	2177.195761	20.534042
62.367380	2185.762590	20.539059
62.529524	2181.704004	20.544077
62.354143	2185.379580	20.549095
62.632736	2174.211421	20.554112
62.676710	2187.974011	20.559130
62.772161	2180.245958	20.564147
62.829523	2180.489482	20.569165
62.837992	2182.088214	20.574183
62.689238	2175.272386	20.579200
62.927260	2181.316842	20.584218
62.949402	2171.391033	20.589235
62.883006	2188.443538	20.594253
62.960001	2191.328702	20.599271
63.318232	2200.920688	20.604288
62.976022	2202.987451	20.609306
63.186810	2196.791013	20.614323
63.604435	2202.201568	20.619341
63.228574	2204.431369	20.624359
63.426916	2207.733167	20.629376
63.363029	2203.088043	20.634394
63.325714	2207.521650	20.639411
63.627907	2210.094031	20.644429
63.639018	2226.935679	20.649447
64.074845	2229.727110	20.654464
63.851743	2225.567541	20.659482
63.639895	2232.467892	20.664499
63.728231	2230.847728	20.669517
63.843533	2224.044421	20.674535
64.078657	2218.781508	20.679552
64.128894	2226.647806	20.684570
63.913047	2240.905349	20.689587
64.005836	2240.426953	20.694605
64.363718	2252.218733	20.699623
64.332894	2250.939029	20.704640
64.388711	2251.706686	20.709658
64.641958	2251.039197	20.714675
64.723239	2242.574825	20.719693
64.741865	2243.316713	20.724711
64.637436	2244.279742	20.729728
64.600440	2253.418866	20.734746
64.609243	2258.624831	20.739763
64.928862	2274.033018	20.744781
64.487458	2278.624236	20.749799
65.051736	2277.466484	20.754816
65.079396	2268.691695	20.759834
64.843464	2275.864070	20.764851
65.135063	2274.187008	20.769869
65.136622	2290.888184	20.774887
65.726025	2289.729675	20.779904
65.755560	2291.318825	20.784922
65.576339	2290.693419	20.789939
66.217139	2279.541389	20.794957
66.071976	2284.995408	20.799975
66.268673	2281.114468	20.804992
66.008419	2284.541331	20.810010
65.916511	2287.828370	20.815027
65.928146	2276.894225	20.820045
65.856758	2286.180740	20.825063
66.153372	2276.401499	20.830080
66.312179	2286.292837	20.835098
66.123215	2280.777181	20.840115
66.846359	2275.996879	20.845133
66.194932	2284.319604	20.850151
66.508710	2280.410967	20.855168
66.191558	2287.943150	20.860186
66.399319	2288.021241	20.865203
66.758058	2283.780537	20.870221
66.550823	2285.299247	20.875239
66.763710	2283.464016	20.880256
66.383549	2288.295023	20.885274
66.731052	2298.829214	20.890291
66.752357	2308.325383	20.895309
66.906711	2313.653878	20.900327
67.016973	2306.671433	20.905344
66.846075	2313.559128	20.910362
66.609289	2317.089647	20.915379
67.109412	2317.671361	20.920397
67.375248	2331.390051	20.925415
67.979538	2330.620564	20.930432
68.005227	2321.514677	20.935450
67.562195	2329.776574	20.940467
68.038037	2329.532044	20.945485
67.874083	2337.924072	20.950503
68.052871	2324.962977	20.955520
67.828567	2314.002425	20.960538
67.561135	2317.670267	20.965555
68.081011	2321.300743	20.970573
68.324111	2320.196149	20.975591
68.321201	2319.322373	20.980608
68.149135	2317.212538	20.985626
67.991717	2321.298779	20.990643
68.310589	2312.125158	20.995661
68.275016	2315.210916	21.000679
68.425639	2314.960212	21.005696
68.093356	2313.620135	21.010714
68.407999	2303.497226	21.015731
68.496549	2311.073558	21.020749
68.347610	2316.376687	21.025767
68.477963	2311.549806	21.030784
68.793724	2326.560985	21.035802
68.716417	2342.766375	21.040819
68.590219	2335.517758	21.045837
68.701442	2337.305646	21.050855
69.015233	2335.088605	21.055872
68.961386	2334.737184	21.060890
68.941712	2339.594136	21.065907
68.961397	2344.419713	21.070925
69.037360	2367.976813	21.075943
69.178202	2368.687053	21.080960
69.116842	2378.656905	21.085978
69.301285	2368.285971	21.090995
69.479406	2364.145958	21.096013
69.328758	2373.934037	21.101031
69.579983	2390.795263	21.106048
69.949906	2374.250721	21.111066
70.014318	2382.421012	21.116083
70.127820	2382.646330	21.121101
69.987027	2392.824229	21.126119
70.235968	2377.904923	21.131136
70.672067	2375.479475	21.136154
70.432107	2381.285974	21.141171
70.401449	2376.035992	21.146189
70.336904	2383.181726	21.151207
70.481375	2382.408084	21.156224
70.780546	2372.874561	21.161242
70.700104	2373.537198	21.166259
70.898765	2380.064405	21.171277
71.003691	2372.426318	21.176295
70.650474	2371.461903	21.181312
70.932679	2378.326418	21.186330
70.277091	2375.698530	21.191347
71.120249	2390.293116	21.196365
70.906663	2393.810570	21.201383
71.417987	2394.892346	21.206400
71.640328	2395.116499	21.211418
71.213371	2396.656803	21.216435
71.294567	2394.782101	21.221453
71.433372	2399.996271	21.226471
71.282644	2401.604028	21.231488
71.473161	2395.341245	21.236506
71.245967	2397.636291	21.241523
71.295998	2409.340397	21.246541
71.722920	2417.574192	21.251559
71.553589	2425.383239	21.256576
72.020997	2425.133709	21.261594
72.019298	2417.988760	21.266611
71.543621	2420.745400	21.271629
71.858672	2422.006069	21.276647
71.856166	2425.455949	21.281664
72.541515	2438.790651	21.286682
72.292635	2445.539049	21.291699
72.750242	2431.966385	21.296717
72.731312	2434.692943	21.301735
72.915249	2433.253549	21.306752
72.727207	2429.729143	21.311770
72.658344	2438.024357	21.316787
72.670935	2436.510648	21.321805
73.025376	2435.117296	21.326823
72.815567	2438.561583	21.331840
72.796717	2433.858891	21.336858
72.981713	2434.578040	21.341875
72.932844	2429.826370	21.346893
72.842457	2433.914824	21.351911
72.835902	2447.385660	21.356928
73.255860	2452.022707	21.361946
73.289393	2453.958410	21.366963
73.349235	2458.014011	21.371981
73.190910	2462.409714	21.376999
73.278621	2461.834266	21.382016
73.670024	2468.413553	21.387034
73.652511	2465.099290	21.392051
74.067361	2453.868716	21.397069
74.563487	2460.557936	21.402087
74.135444	2456.559616	21.407104
74.935167	2453.708291	21.412122
74.405984	2453.983176	21.417139
74.046692	2442.491259	21.422157
74.414702	2445.182823	21.427175
74.454179	2445.066195	21.432192
74.292571	2451.535903	21.437210
74.611282	2455.535421	21.442227
74.698965	2458.223292	21.447245
74.868567	2460.226179	21.452263
74.546823	2457.028716	21.457280
75.105693	2454.129678	21.462298
74.526671	2460.209912	21.467315
74.689459	2461.513226	21.472333
74.862654	2462.101661	21.477351
74.693555	2466.019328	21.482368
75.126823	2472.910856	21.487386
75.131469	2482.797901	21.492403
75.226806	2483.436331	21.497421
75.018337	2489.755548	21.502439
75.268365	2486.573208	21.507456
75.513660	2488.154031	21.512474
75.395014	2481.828892	21.517491
75.511308	2498.073713	21.522509
75.827098	2503.001564	21.527527
75.641458	2505.571040	21.532544
75.974448	2507.532714	21.537562
75.767406	2512.706082	21.542579
75.955305	2508.267847	21.547597
76.028806	2502.540833	21.552615
76.125586	2514.408154	21.557632
76.382958	2532.250079	21.562650
76.791865	2530.564197	21.567667
76.679669	2531.866145	21.572685
76.714049	2536.597962	21.577703
76.599102	2538.481046	21.582720
76.865700	2522.905573	21.587738
76.903429	2535.908802	21.592755
76.918848	2521.685343	21.597773
77.047598	2528.201397	21.602791
76.955542	2530.917263	21.607808
77.058258	2526.422853	21.612826
76.883229	2528.510965	21.617843
77.036852	2528.689011	21.622861
77.281639	2522.310430	21.627879
76.911980	2530.258016	21.632896
77.162941	2541.037770	21.637914
77.445450	2553.302264	21.642931
77.345258	2549.410681	21.647949
77.664169	2553.874125	21.652967
77.136699	2551.349348	21.657984
77.314889	2556.279701	21.663002
77.805662	2571.768803	21.668019
77.895243	2577.719732	21.673037
77.890614	2569.379043	21.678055
77.951118	2571.686127	21.683072
77.859306	2567.285114	21.688090
77.960946	2572.640830	21.693107
78.237882	2582.154154	21.698125
78.252341	2596.578108	21.703143
77.806744	2596.451788	21.708160
78.268279	2596.218951	21.713178
78.396229	2597.281528	21.718195
78.429032	2609.657526	21.723213
78.616505	2608.214412	21.728231
78.688246	2621.619536	21.733248
78.962677	2615.829642	21.738266
79.028113	2621.105797	21.743283
79.052524	2626.104296	21.748301
79.557690	2618.160775	21.753319
79.035028	2619.693905	21.758336
79.385014	2620.819752	21.763354
79.041467	2631.490135	21.768371
79.309779	2644.568004	21.773389
79.646986	2641.315254	21.778407
79.496022	2652.362795	21.783424
79.514707	2639.517926	21.788442
79.439445	2640.293384	21.793459
79.475895	2652.646752	21.798477
79.949712	2659.292179	21.803495
79.874054	2668.983531	21.808512
80.213522	2669.123175	21.813530
80.236869	2666.414786	21.818547
79.972201	2669.649891	21.823565
80.094766	2671.647501	21.828583
80.087122	2691.787419	21.833600
80.304405	2690.601610	21.838618
80.421295	2701.598010	21.843635
80.357204	2695.425260	21.848653
80.821836	2692.218940	21.853671
80.705284	2715.269940	21.858688
80.815368	2714.646817	21.863706
80.821420	2713.168819	21.868723
81.037710	2722.521232	21.873741
80.912519	2723.932522	21.878759
80.791021	2713.040932	21.883776
81.647979	2727.712548	21.888794
81.663355	2734.744985	21.893811
82.034786	2741.103403	21.898829
82.077096	2719.285278	21.903847
81.918302	2715.623707	21.908864
81.863434	2710.891833	21.913882
81.943034	2716.067972	21.918899
82.205495	2706.214914	21.923917
82.307764	2707.537137	21.928935
81.955736	2709.712791	21.933952
82.659685	2717.139829	21.938970
82.474153	2718.412179	21.943987
81.977619	2723.485501	21.949005
82.158607	2727.320314	21.954023
82.624177	2729.302400	21.959040
82.610018	2708.799688	21.964058
82.620154	2724.600458	21.969075
82.819772	2723.679349	21.974093
82.972346	2711.211246	21.979111
82.733616	2723.935736	21.984128
82.813511	2725.955776	21.989146
83.038432	2727.246280	21.994163
83.281755	2741.558973	21.999181
83.237319	2745.258460	22.004199
83.526274	2746.359100	22.009216
83.506355	2745.715187	22.014234
83.633991	2751.903265	22.019251
83.717469	2750.820342	22.024269
83.585984	2738.513220	22.029287
83.294551	2743.093829	22.034304
83.502943	2743.657858	22.039322
83.628691	2741.861397	22.044339
83.360072	2744.008289	22.049357
83.886167	2749.828192	22.054375
84.012066	2760.132048	22.059392
84.071786	2764.654835	22.064410
84.088901	2762.433436	22.069427
84.053654	2764.433534	22.074445
84.208127	2766.558742	22.079463
84.048152	2774.237084	22.084480
84.483467	2787.983391	22.089498
84.793941	2795.661087	22.094515
84.440641	2792.459008	22.099533
84.666180	2790.167283	22.104551
84.259358	2803.770138	22.109568
84.563167	2814.084199	22.114586
84.903531	2823.994909	22.119603
84.783561	2822.871067	22.124621
85.002961	2818.743458	22.129639
85.230408	2835.302666	22.134656
85.346287	2836.995196	22.139674
86.037770	2834.523615	22.144691
85.915648	2838.557136	22.149709
86.004773	2840.724087	22.154727
86.131182	2832.261880	22.159744
86.041327	2830.568411	22.164762
85.930308	2832.712869	22.169779
85.712832	2832.216486	22.174797
85.585873	2831.598704	22.179815
85.791429	2848.745206	22.184832
86.091069	2848.584914	22.189850
86.300805	2860.580057	22.194867
86.104624	2859.193499	22.199885
86.323819	2861.466446	22.204903
86.607423	2867.718651	22.209920
86.584753	2883.909710	22.214938
86.839018	2880.625647	22.219955
87.085790	2884.200922	22.224973
87.001592	2880.174221	22.229991
87.192349	2885.222640	22.235008
87.071227	2886.399759	22.240026
87.221208	2875.702509	22.245043
87.197203	2883.230329	22.250061
87.579588	2891.439717	22.255079
87.576416	2900.283544	22.260096
87.577956	2906.118890	22.265114
87.965990	2899.181338	22.270131
87.550275	2902.329538	22.275149
87.861139	2905.386708	22.280167
87.974800	2907.455165	22.285184
87.597325	2895.495530	22.290202
88.115107	2894.657433	22.295219
88.285401	2914.116588	22.300237
88.651562	2920.990333	22.305255
88.517418	2923.403513	22.310272
88.430951	2922.631087	22.315290
88.616570	2923.631052	22.320307
88.546246	2929.919447	22.325325
88.398699	2921.288392	22.330343
88.288625	2923.675733	22.335360
88.689325	2925.838370	22.340378
89.013973	2941.962783	22.345395
89.060527	2947.585987	22.350413
89.044459	2953.140041	22.355431
89.084738	2937.312241	22.360448
88.962507	2951.183352	22.365466
89.234520	2941.704254	22.370483
89.560557	2956.550245	22.375501
89.818002	2963.807040	22.380519
90.011047	2967.920921	22.385536
89.915926	2964.779610	22.390554
90.169614	2961.801763	22.395571
89.928670	2968.457594	22.400589
90.093959	2971.414352	22.405607
89.937798	2968.247826	22.410624
90.363757	2967.588140	22.415642
90.478137	2955.816999	22.420659
90.524118	2961.089971	22.425677
90.429016	2959.406774	22.430695
90.390156	2957.724291	22.435712
90.448374	2970.386942	22.440730
90.500554	2964.757783	22.445747
90.607604	2974.919516	22.450765
90.800507	2979.532086	22.455783
91.009368	2983.880216	22.460800
91.039943	2989.812063	22.465818
91.240708	2984.475375	22.470835
91.143328	2989.060551	22.475853
91.185803	2998.137184	22.480871
91.413922	3006.739907	22.485888
91.283418	2999.302326	22.490906
91.455765	3003.542526	22.495923
91.426928	3003.625896	22.500941
91.352785	3011.777017	22.505959
91.825119	3021.875593	22.510976
91.881265	3032.266212	22.515994
91.916618	3027.788477	22.521011
92.102379	3031.505837	22.526029
92.285314	3035.315165	22.531047
92.511702	3046.310509	22.536064
92.230559	3055.090382	22.541082
92.472425	3055.661834	22.546099
92.400188	3053.583711	22.551117
92.667611	3050.300725	22.556135
92.881102	3053.732878	22.561152
92.809288	3064.493766	22.566170
92.995708	3069.460853	22.571187
92.759795	3083.797935	22.576205
92.996036	3082.359815	22.581223
93.333186	3076.916650	22.586240
92.811171	3083.281735	22.591258
93.308147	3080.887747	22.596275
93.825677	3096.407855	22.601293
93.929167	3095.088242	22.606311
94.110271	3090.158567	22.611328
94.177220	3095.197916	22.616346
94.440070	3092.726757	22.621363
94.213949	3095.602450	22.626381
94.412932	3098.541360	22.631399
94.709582	3087.066836	22.636416
94.446394	3093.076015	22.641434
94.982380	3098.209615	22.646451
94.652019	3088.013101	22.651469
94.642736	3091.543067	22.656487
94.734998	3089.369895	22.661504
94.546615	3086.482947	22.666522
94.703325	3082.226170	22.671539
94.916013	3104.162796	22.676557
94.939878	3113.681086	22.681575
95.432442	3103.653116	22.686592
95.479199	3113.578138	22.691610
95.393490	3113.206413	22.696627
95.129712	3117.615537	22.701645
95.575460	3110.119754	22.706663
95.648631	3113.835723	22.711680
95.284943	3123.884619	22.716698
95.277609	3121.594392	22.721715
95.914043	3131.348712	22.726733
95.691264	3135.233852	22.731751
96.094278	3132.160138	22.736768
96.471678	3140.323074	22.741786
96.212824	3133.381996	22.746803
95.898670	3135.463432	22.751821
96.314043	3155.572728	22.756839
96.686267	3156.767738	22.761856
96.594246	3157.044003	22.766874
96.795427	3153.881775	22.771891
96.526118	3152.667542	22.776909
96.908822	3156.426857	22.781927
97.187026	3167.095438	22.786944
97.137873	3168.245590	22.791962
96.698872	3177.933818	22.796979
96.883653	3182.336243	22.801997
97.264124	3186.499897	22.807015
97.453265	3193.518085	22.812032
97.650571	3198.107933	22.817050
97.625942	3196.404274	22.822067
97.914948	3200.225528	22.827085
97.695677	3201.582068	22.832103
97.687361	3201.255102	22.837120
97.905936	3212.706249	22.842138
98.232656	3212.958349	22.847155
99.077384	3206.697583	22.852173
99.287408	3211.730470	22.857191
99.367561	3197.638424	22.862208
99.151804	3184.264716	22.867226
99.392012	3173.625833	22.872243
99.229158	3171.640708	22.877261
99.272341	3176.311356	22.882279
99.489326	3174.267093	22.887296
99.107883	3170.838929	22.892314
99.609442	3171.713972	22.897331
99.329260	3177.694264	22.902349
99.285943	3172.089376	22.907367
99.897059	3168.778107	22.912384
99.097059	3170.559610	22.917402
99.314810	3194.143061	22.922419
99.651592	3201.220325	22.927437
99.772831	3196.056919	22.932455
100.135583	3194.182483	22.937472
99.750674	3200.677758	22.942490
100.258877	3207.087639	22.947507
100.129402	3214.474211	22.952525
100.014389	3219.242092	22.957543
100.297538	3211.689522	22.962560
100.293882	3224.923779	22.967578
100.580877	3230.209804	22.972595
100.807990	3234.002827	22.977613
101.075646	3243.110804	22.982631
101.128883	3238.794353	22.987648
101.139245	3239.177768	22.992666
101.663045	3233.219450	22.997683
101.594839	3241.893670	23.002701
101.297602	3238.992084	23.007719
101.709021	3228.541131	23.012736
101.427502	3234.622646	23.017754
101.516922	3246.052893	23.022771
101.479571	3253.964840	23.027789
101.498477	3262.922186	23.032807
101.524017	3265.241115	23.037824
102.015799	3270.072344	23.042842
101.874414	3287.803515	23.047859
102.088793	3283.278907	23.052877
102.084425	3292.375606	23.057895
102.379098	3288.513914	23.062912
102.233484	3299.305370	23.067930
102.423235	3299.553547	23.072947
102.482089	3313.945916	23.077965
102.399814	3318.677164	23.082983
102.859313	3324.132041	23.088000
102.767469	3329.395017	23.093018
102.749286	3340.245561	23.098035
103.131435	3344.071281	23.103053
103.174305	3353.435243	23.108071
103.217596	3349.123470	23.113088
103.392068	3365.817662	23.118106
103.320257	3374.640847	23.123123
103.333342	3369.790910	23.128141
103.482818	3384.721556	23.133159
104.008418	3383.519262	23.138176
103.870612	3390.881954	23.143194
104.137865	3395.457806	23.148211
104.049478	3397.226378	23.153229
104.339762	3406.425600	23.158247
104.429140	3410.883965	23.163264
104.797406	3422.807460	23.168282
104.873496	3416.843039	23.173299
104.612871	3414.491211	23.178317
104.657194	3419.237493	23.183335
105.022252	3421.538301	23.188352
105.227358	3439.199894	23.193370
105.283366	3440.895491	23.198387
105.549005	3443.568429	23.203405
105.190888	3442.011353	23.208423
105.453421	3440.632236	23.213440
105.753862	3447.484854	23.218458
105.737228	3460.370968	23.223475
106.567923	3461.927018	23.228493
105.997433	3466.150421	23.233511
106.137238	3465.781452	23.238528
106.245672	3457.151316	23.243546
106.123728	3464.653597	23.248563
106.404740	3463.959650	23.253581
106.143094	3471.985518	23.258599
106.576589	3484.555385	23.263616
106.978543	3489.634217	23.268634
106.668941	3496.477678	23.273651
107.160895	3493.077594	23.278669
107.230448	3504.252289	23.283687
106.907706	3496.311035	23.288704
106.819680	3498.426743	23.293722
106.867010	3512.344479	23.298739
107.115287	3504.835091	23.303757
107.350843	3516.993931	23.308775
107.688157	3524.746666	23.313792
107.823869	3534.064705	23.318810
107.814287	3537.765241	23.323827
108.189909	3524.296052	23.328845
107.952847	3536.402240	23.333863
108.424366	3533.456666	23.338880
108.188796	3542.365397	23.343898
108.437215	3549.759551	23.348915
108.745112	3550.052463	23.353933
108.840229	3556.296381	23.358951
108.773636	3550.830716	23.363968
108.868980	3555.124066	23.368986
109.227948	3546.095075	23.374003
109.247266	3543.324058	23.379021
109.023905	3551.763775	23.384039
108.985092	3536.721032	23.389056
109.508700	3550.438397	23.394074
109.531480	3564.268466	23.399091
109.807225	3568.129738	23.404109
109.593545	3572.392299	23.409127
109.898906	3572.414172	23.414144
109.986083	3565.879858	23.419162
109.845942	3576.194040	23.424179
110.345072	3568.724475	23.429197
110.333867	3582.086418	23.434215
110.378478	3583.051562	23.439232
110.504362	3589.145516	23.444250
110.549752	3596.893234	23.449267
110.648819	3597.165003	23.454285
110.279588	3591.295106	23.459303
110.540481	3599.839356	23.464320
110.352463	3616.296688	23.469338
110.748473	3619.804689	23.474355
111.188660	3625.856033	23.479373
111.558666	3619.782661	23.484391
111.793502	3619.705046	23.489408
112.432647	3621.369839	23.494426
112.101225	3629.059456	23.499443
112.339397	3615.040325	23.504461
112.357235	3611.379475	23.509479
112.481397	3614.503710	23.514496
112.541590	3618.739424	23.519514
112.520383	3615.318212	23.524531
112.687854	3613.095393	23.529549
112.845783	3611.565270	23.534567
112.569599	3621.701817	23.539584
112.929038	3616.021461	23.544602
112.517096	3617.928804	23.549619
112.878506	3620.924572	23.554637
112.906016	3623.798735	23.559655
112.982108	3624.683232	23.564672
113.062476	3645.672162	23.569690
113.014878	3646.058297	23.574707
113.482718	3639.802406	23.579725
113.321458	3645.082593	23.584743
113.463816	3668.492187	23.589760
113.967329	3676.013958	23.594778
113.954915	3672.973269	23.599795
114.048102	3671.320660	23.604813
114.172202	3672.431244	23.609831
114.077106	3677.129864	23.614848
114.249917	3690.535830	23.619866
113.929213	3693.038127	23.624883
114.297926	3706.883884	23.629901
114.585027	3723.551403	23.634919
114.614079	3725.907720	23.639936
114.866107	3726.102021	23.644954
115.140299	3725.813124	23.649971
115.224846	3733.100306	23.654989
115.372849	3743.082505	23.660007
115.114206	3740.373670	23.665024
115.560451	3750.157940	23.670042
115.359743	3752.202846	23.675059
115.841210	3752.711768	23.680077
115.968631	3761.298969	23.685095
115.634165	3768.433621	23.690112
115.566087	3772.136999	23.695130
115.740788	3783.049310	23.700147
115.924491	3789.431017	23.705165
116.431779	3794.335724	23.710183
116.434218	3798.160691	23.715200
116.477693	3789.423729	23.720218
116.311223	3809.611720	23.725235
117.020677	3820.188298	23.730253
117.107282	3819.511980	23.735271
116.818413	3821.428588	23.740288
117.122565	3816.833059	23.745306
117.037278	3824.367656	23.750323
117.556288	3836.845551	23.755341
117.422712	3837.655388	23.760359
117.455096	3838.268950	23.765376
118.133144	3843.652086	23.770394
117.320047	3841.102153	23.775411
117.679474	3859.633352	23.780429
117.717747	3855.738865	23.785447
118.087001	3856.754481	23.790464
118.742840	3872.982823	23.795482
118.203962	3885.129921	23.800499
118.701766	3887.842530	23.805517
118.840662	3892.517400	23.810535
118.504860	3891.193529	23.815552
118.960589	3898.921678	23.820570
119.016029	3909.246631	23.825587
119.148788	3908.017091	23.830605
119.157474	3908.331343	23.835623
119.259698	3917.269730	23.840640
119.280538	3926.855202	23.845658
119.435337	3939.080557	23.850675
119.864179	3938.773892	23.855693
120.515085	3952.689529	23.860711
120.180505	3947.205498	23.865728
120.279238	3938.529299	23.870746
120.125393	3950.572307	23.875763
120.272360	3966.911523	23.880781
120.420780	3968.583313	23.885799
120.446483	3968.443570	23.890816
120.944635	3967.905175	23.895834
120.674106	3988.737664	23.900851
121.102871	3982.175268	23.905869
121.157632	3993.216850	23.910887
121.249128	3991.959010	23.915904
121.956802	3976.831242	23.920922
121.913985	3977.488079	23.925939
121.791600	3974.088864	23.930957
121.924109	3994.539828	23.935975
122.148090	3994.381840	23.940992
122.519780	3991.183452	23.946010
122.648006	3989.187636	23.951027
122.701765	3988.118735	23.956045
122.662192	3995.119188	23.961063
122.481456	3991.214582	23.966080
123.030347	3978.611306	23.971098
122.713147	3993.324736	23.976115
123.011701	3989.250820	23.981133
122.770587	3984.828517	23.986151
123.153171	3992.568094	23.991168
123.487172	4002.941264	23.996186
123.325213	4014.310134	24.001203
123.231122	4013.567254	24.006221
123.712511	4015.553337	24.011239
123.456632	4017.988772	24.016256
123.758180	4029.317051	24.021274
123.834438	4043.136004	24.026291
124.196250	4042.164328	24.031309
123.924185	4035.903559	24.036327
124.277046	4045.131241	24.041344
124.225916	4050.650060	24.046362
124.110979	4066.361009	24.051379
124.410201	4060.525762	24.056397
124.634454	4061.327244	24.061415
124.914475	4090.261556	24.066432
125.025863	4081.305564	24.071450
124.692103	4081.221785	24.076467
124.826480	4087.245146	24.081485
125.201844	4092.325134	24.086503
124.803545	4102.398898	24.091520
125.720510	4106.327739	24.096538
125.524296	4107.491377	24.101555
125.733715	4127.911579	24.106573
125.964529	4132.704766	24.111591
125.906040	4142.245889	24.116608
126.034963	4142.708709	24.121626
126.326981	4147.653342	24.126643
126.560950	4157.688669	24.131661
126.686071	4161.693460	24.136679
126.744561	4163.568648	24.141696
126.795456	4158.819927	24.146714
126.514490	4173.774054	24.151731
126.646756	4185.520169	24.156749
127.065340	4186.512342	24.161767
127.115913	4201.228652	24.166784
127.436569	4209.643947	24.171802
127.424004	4214.604456	24.176819
127.749280	4214.635856	24.181837
127.958441	4228.090220	24.186855
128.016298	4229.735102	24.191872
128.251698	4226.005537	24.196890
128.306610	4229.904490	24.201907
128.282951	4232.026042	24.206925
128.786636	4237.572166	24.211943
128.478759	4254.796788	24.216960
128.724223	4252.542810	24.221978
128.549484	4252.244892	24.226995
128.701900	4263.691227	24.232013
129.266456	4269.628737	24.237031
129.187058	4283.342698	24.242048
129.367766	4272.854469	24.247066
129.498855	4278.616431	24.252083
130.032248	4280.578666	24.257101
130.284001	4267.033522	24.262119
130.571926	4284.881898	24.267136
130.232086	4274.481025	24.272154
130.464609	4274.798310	24.277171
130.693767	4282.700778	24.282189
131.092974	4276.051345	24.287207
130.979797	4278.609788	24.292224
130.609861	4273.427857	24.297242
131.083215	4285.534412	24.302259
131.366398	4303.030036	24.307277
131.406356	4293.848335	24.312295
131.496793	4298.139470	24.317312
131.232658	4296.744440	24.322330
131.755935	4290.716421	24.327347
131.628201	4302.278992	24.332365
131.893083	4312.745166	24.337383
131.579170	4322.139927	24.342400
132.080992	4323.087586	24.347418
132.110345	4314.153721	24.352435
132.220991	4331.073374	24.357453
132.440274	4340.123155	24.362471
132.149866	4348.280141	24.367488
132.555902	4339.742130	24.372506
132.850564	4361.449737	24.377523
132.915916	4378.266014	24.382541
132.888327	4368.782314	24.387559
133.065995	4381.493642	24.392576
133.344638	4384.761246	24.397594
133.753587	4398.209883	24.402611
133.695008	4404.717907	24.407629
134.084174	4390.570508	24.412647
133.712810	4404.276359	24.417664
134.168997	4391.696700	24.422682
134.179616	4391.783403	24.427699
134.140559	4395.608644	24.432717
134.528768	4408.403997	24.437735
134.353323	4413.358355	24.442752
134.484355	4411.753444	24.447770
134.778877	4412.998516	24.452787
134.996243	4431.877525	24.457805
134.762552	4441.667028	24.462823
134.720790	4446.625833	24.467840
134.884622	4455.785309	24.472858
135.161620	4461.919158	24.477875
134.991374	4474.441679	24.482893
136.021953	4483.106399	24.487911
136.053997	4494.457991	24.492928
136.513079	4491.927686	24.497946
136.405396	4497.821583	24.502963
136.253699	4498.697399	24.507981
136.891605	4488.674446	24.512999
136.525601	4503.200192	24.518016
136.607552	4498.159318	24.523034
136.879589	4512.509982	24.528051
136.656683	4525.324810	24.533069
136.915686	4524.675284	24.538087
136.881419	4543.091722	24.543104
137.396764	4545.684916	24.548122
137.610205	4535.627019	24.553139
137.591410	4552.617534	24.558157
138.093241	4567.696308	24.563175
137.808842	4578.150306	24.568192
138.044939	4570.481399	24.573210
138.558247	4572.449951	24.578227
138.290523	4564.951021	24.583245
138.560691	4575.558561	24.588263
138.478159	4591.040817	24.593280
138.570922	4596.461645	24.598298
138.775109	4592.938873	24.603315
138.595743	4605.939518	24.608333
138.978013	4610.952293	24.613351
139.002260	4619.931575	24.618368
139.288252	4628.412434	24.623386
139.914569	4642.013638	24.628403
139.571853	4648.666990	24.633421
139.827087	4647.863384	24.638439
139.770703	4660.245206	24.643456
139.849871	4661.842620	24.648474
140.102572	4669.315479	24.653491
140.028263	4682.252475	24.658509
140.435994	4689.609670	24.663527
140.719929	4705.416892	24.668544
140.950015	4696.943985	24.673562
141.110989	4716.106676	24.678579
141.201925	4717.913743	24.683597
141.442202	4712.803970	24.688615
141.491638	4720.390562	24.693632
141.887691	4714.745198	24.698650
142.246120	4713.120639	24.703667
142.271146	4720.543743	24.708685
142.782264	4727.127319	24.713703
142.586043	4719.929676	24.718720
142.695005	4719.909534	24.723738
142.925824	4735.002235	24.728755
142.584602	4743.577642	24.733773
142.678925	4738.825165	24.738791
142.893336	4736.465488	24.743808
142.951718	4731.936400	24.748826
143.328734	4726.511789	24.753843
142.860259	4737.610036	24.758861
143.347549	4748.430075	24.763879
143.416907	4759.596108	24.768896
143.595926	4770.483093	24.773914
143.802812	4764.138033	24.778931
143.441209	4777.536473	24.783949
143.531154	4789.882976	24.788967
143.793855	4793.620287	24.793984
143.900620	4817.248389	24.799002
143.943683	4813.624403	24.804019
144.227989	4824.422430	24.809037
144.667202	4836.001235	24.814055
144.961934	4839.209602	24.819072
145.225718	4843.353934	24.824090
145.460036	4853.165486	24.829107
145.349764	4870.217887	24.834125
145.308480	4866.086211	24.839143
145.863022	4867.338180	24.844160
145.555815	4869.907976	24.849178
146.273268	4885.240681	24.854195
146.424302	4887.928522	24.859213
146.611694	4887.208066	24.864231
146.669752	4894.667132	24.869248
147.067349	4889.592788	24.874266
147.008343	4885.397582	24.879283
147.007848	4887.603985	24.884301
147.084827	4894.656081	24.889319
147.192111	4902.704052	24.894336
147.471994	4899.254660	24.899354
147.657069	4906.163674	24.904371
147.470218	4901.606439	24.909389
147.753555	4918.843806	24.914407
148.269188	4929.905744	24.919424
147.871707	4934.610732	24.924442
148.314069	4935.416174	24.929459
148.211638	4943.414747	24.934477
148.739189	4949.680202	24.939495
148.691988	4958.664462	24.944512
148.447759	4969.604836	24.949530
148.690545	4963.345655	24.954547
148.642425	4972.030203	24.959565
148.565253	4973.361592	24.964583
149.094587	4988.468000	24.969600
149.461996	4996.077801	24.974618
149.719934	4990.962045	24.979635
150.026175	5009.247031	24.984653
149.933626	5019.510434	24.989671
150.111998	5025.928129	24.994688
150.295451	5020.044316	24.999706
150.757425	5026.986020	25.004723
150.582050	5028.348485	25.009741
150.518768	5049.601298	25.014759
150.836657	5046.303785	25.019776
150.727075	5056.620363	25.024794
150.884155	5058.347724	25.029811
150.972386	5076.269005	25.034829
151.338539	5082.547009	25.039847
151.318917	5091.135639	25.044864
151.641620	5098.534647	25.049882
151.632398	5100.868693	25.054899
151.717676	5116.568318	25.059917
151.903460	5123.994966	25.064935
152.473150	5124.723777	25.069952
152.559599	5133.589465	25.074970
152.788440	5138.758848	25.079987
153.241789	5140.929344	25.085005
153.001492	5134.795819	25.090023
153.448944	5133.788660	25.095040
153.614096	5138.200934	25.100058
153.823586	5134.156413	25.105075
153.542698	5133.262649	25.110093
153.732005	5136.212869	25.115111
153.681671	5147.612416	25.120128
153.888157	5155.351502	25.125146
154.167857	5154.212635	25.130163
153.836674	5170.479026	25.135181
154.359390	5175.536380	25.140199
154.629756	5187.078568	25.145216
154.598035	5187.989396	25.150234
154.484487	5205.165724	25.155251
154.598642	5222.155105	25.160269
154.844140	5230.169077	25.165287
155.245714	5241.346814	25.170304
155.173585	5248.630591	25.175322
155.596133	5260.433218	25.180339
155.656838	5276.079989	25.185357
155.833776	5277.674862	25.190375
156.000647	5275.445622	25.195392
155.884445	5301.350184	25.200410
156.391591	5299.052181	25.205427
156.216820	5315.026046	25.210445
156.518713	5323.631016	25.215463
157.115580	5325.652930	25.220480
156.812813	5345.617640	25.225498
157.018313	5347.848845	25.230515
156.994591	5350.090486	25.235533
157.573686	5355.786198	25.240551
158.108593	5367.713445	25.245568
157.808483	5373.590237	25.250586
157.898625	5376.360231	25.255603
158.057425	5386.423726	25.260621
157.966678	5396.071538	25.265639
158.495690	5391.983527	25.270656
158.857685	5408.745106	25.275674
159.005258	5406.395750	25.280691
159.752135	5409.192920	25.285709
159.637289	5412.057964	25.290727
160.061271	5417.376967	25.295744
159.865265	5412.063462	25.300762
159.968843	5409.354798	25.305779
160.040879	5408.118830	25.310797
159.900731	5424.579818	25.315815
160.455467	5431.734507	25.320832
160.476765	5442.554911	25.325850
160.552011	5436.182765	25.330867
160.476551	5437.930583	25.335885
160.419608	5449.495488	25.340903
161.548227	5457.671939	25.345920
160.915278	5471.820198	25.350938
161.149287	5476.941524	25.355955
161.466162	5479.130153	25.360973
161.231173	5488.885698	25.365991
161.557072	5499.125258	25.371008
161.622553	5516.349763	25.376026
161.624165	5521.832408	25.381043
161.839054	5525.618350	25.386061
161.743532	5551.018157	25.391079
162.100715	5548.323650	25.396096
162.329625	5572.416669	25.401114
162.313260	5577.485464	25.406131
162.780450	5586.247904	25.411149
162.950565	5597.865936	25.416167
163.385949	5591.945873	25.421184
163.535253	5610.101226	25.426202
164.078391	5607.955411	25.431219
164.470149	5600.725851	25.436237
165.007875	5605.130738	25.441255
165.180071	5589.270612	25.446272
165.020013	5581.366242	25.451290
164.961795	5576.864567	25.456307
165.203795	5567.726524	25.461325
164.656479	5580.444242	25.466343
165.137763	5581.783427	25.471360
165.250907	5597.172943	25.476378
165.520598	5606.458564	25.481395
165.655304	5603.754495	25.486413
165.687351	5615.968528	25.491431
165.910131	5617.246951	25.496448
165.877726	5628.078983	25.501466
166.048042	5630.101055	25.506483
166.368981	5626.531499	25.511501
166.171840	5649.576685	25.516519
166.119703	5650.455993	25.521536
166.498869	5662.641267	25.526554
166.519134	5678.310464	25.531571
166.845397	5683.562688	25.536589
166.784030	5691.350018	25.541607
167.148137	5704.775042	25.546624
166.931771	5709.789785	25.551642
167.700778	5731.071644	25.556659
167.814639	5730.697202	25.561677
167.706111	5752.150431	25.566695
168.256634	5749.163798	25.571712
168.280271	5760.015593	25.576730
168.410339	5774.291505	25.581747
168.713239	5770.011340	25.586765
169.128348	5777.926547	25.591783
169.255544	5793.241439	25.596800
169.034810	5811.265208	25.601818
169.341095	5814.765515	25.606835
169.274044	5821.723600	25.611853
169.868978	5833.897493	25.616871
170.018199	5829.338207	25.621888
170.284557	5842.952165	25.626906
170.186315	5863.299113	25.631923
170.702723	5854.320228	25.636941
170.389965	5870.691698	25.641959
170.576058	5874.756821	25.646976
171.000294	5888.387269	25.651994
171.069485	5880.440763	25.657011
171.375814	5896.267633	25.662029
171.371408	5906.511498	25.667047
171.961487	5902.950492	25.672064
172.145287	5912.457979	25.677082
172.166461	5923.957360	25.682100
172.868467	5913.267075	25.687117
172.945076	5927.071625	25.692135
172.968087	5915.000286	25.697152
172.741480	5925.079889	25.702170
173.055268	5930.485645	25.707188
173.068069	5939.262181	25.712205
173.344647	5956.192237	25.717223
173.503537	5952.196450	25.722240
173.505013	5969.289300	25.727258
173.587442	5974.020849	25.732276
174.023183	5979.202453	25.737293
174.032138	5987.329346	25.742311
174.053539	5990.031220	25.747328
173.921802	6007.621496	25.752346
174.041418	6018.205971	25.757364
174.297644	6035.192932	25.762381
174.573332	6046.204523	25.767399
174.925238	6052.614505	25.772416
175.136315	6066.196200	25.777434
175.125346	6068.600088	25.782452
175.408567	6083.587896	25.787469
175.665596	6096.619517	25.792487
175.760202	6085.127211	25.797504
175.827862	6097.790578	25.802522
176.122766	6117.442116	25.807540
176.263063	6116.192315	25.812557
176.855773	6127.296648	25.817575
177.095804	6130.469570	25.822592
177.407847	6133.602870	25.827610
177.779621	6129.169850	25.832628
177.772285	6130.297894	25.837645
177.605658	6126.737860	25.842663
178.630063	6124.037248	25.847680
178.650055	6117.149464	25.852698
178.448866	6112.751988	25.857716
178.785778	6114.290463	25.862733
179.118713	6122.073408	25.867751
178.828511	6116.625999	25.872768
178.958398	6134.488174	25.877786
179.295217	6130.010090	25.882804
179.405487	6121.640406	25.887821
179.780211	6135.490243	25.892839
179.969201	6145.546301	25.897856
179.978378	6147.880774	25.902874
180.073640	6154.337061	25.907892
180.309632	6141.632649	25.912909
180.327685	6152.959045	25.917927
180.588584	6170.030634	25.922944
180.992526	6169.737287	25.927962
180.766087	6175.397683	25.932980
180.881382	6171.954738	25.937997
180.931183	6189.958858	25.943015
181.504285	6196.662746	25.948032
181.455797	6200.931767	25.953050
181.483780	6222.137015	25.958068
181.560461	6222.538579	25.963085
181.612220	6240.479311	25.968103
181.968989	6247.030654	25.973120
182.260192	6253.778451	25.978138
182.240327	6274.400912	25.983156
182.837420	6269.500315	25.988173
182.523669	6293.382046	25.993191
182.941273	6304.497966	25.998208
183.308190	6313.866670	26.003226
183.270340	6326.170977	26.008244
183.724752	6331.068830	26.013261
183.497913	6350.145257	26.018279
183.910842	6354.569759	26.023296
183.789627	6366.293615	26.028314
184.102874	6386.725446	26.033332
184.655075	6381.547706	26.038349
184.881732	6399.934869	26.043367
185.146506	6409.057518	26.048384
185.238287	6414.778929	26.053402
185.373035	6426.993299	26.058420
185.467197	6427.098572	26.063437
185.518927	6444.029364	26.068455
185.502321	6450.215912	26.073472
185.995504	6466.803363	26.078490
186.051098	6476.861431	26.083508
186.454197	6483.626616	26.088525
186.283601	6496.974480	26.093543
186.522646	6506.423168	26.098560
187.127990	6513.504116	26.103578
186.980833	6525.329971	26.108596
187.303549	6525.125027	26.113613
187.614521	6524.871404	26.118631
187.917526	6533.492559	26.123648
187.874424	6543.035700	26.128666
188.033552	6541.369409	26.133684
188.134263	6551.912943	26.138701
188.225150	6572.477459	26.143719
188.249289	6570.563860	26.148736
189.007522	6589.818629	26.153754
189.006855	6602.212035	26.158772
189.265721	6596.631648	26.163789
189.579693	6601.510402	26.168807
189.580719	6619.932914	26.173824
189.561116	6615.854287	26.178842
189.953127	6626.409333	26.183860
190.227002	6640.237374	26.188877
190.314865	6652.516016	26.193895
190.169750	6655.761619	26.198912
190.323478	6667.253457	26.203930
190.504395	6669.940068	26.208948
190.992193	6683.416006	26.213965
190.789427	6706.536004	26.218983
190.850998	6714.699222	26.224000
191.377518	6726.688647	26.229018
191.246614	6752.433404	26.234036
191.636936	6753.963620	26.239053
191.921074	6768.667739	26.244071
192.131230	6784.557704	26.249088
192.598733	6795.195797	26.254106
192.606075	6810.830095	26.259124
193.201446	6812.221062	26.264141
193.354351	6824.079313	26.269159
193.404531	6835.129646	26.274176
193.569871	6838.380613	26.279194
194.024644	6859.081361	26.284212
194.343929	6854.419582	26.289229
194.430368	6864.416239	26.294247
194.052034	6877.708332	26.299264
194.829437	6874.932427	26.304282
194.634610	6888.798903	26.309300
194.928361	6895.625461	26.314317
195.747290	6909.299399	26.319335
195.730367	6915.906006	26.324352
196.241349	6915.349756	26.329370
195.837804	6928.775239	26.334388
195.973514	6933.091516	26.339405
196.258802	6935.878718	26.344423
196.196227	6946.062772	26.349440
196.579022	6948.332866	26.354458
196.114903	6963.725015	26.359476
196.840575	6982.265519	26.364493
196.771542	6995.951495	26.369511
196.923747	6999.160339	26.374528
197.447437	7014.490289	26.379546
197.255712	7024.287266	26.384564
198.261294	7039.119200	26.389581
197.965669	7050.236128	26.394599
198.702150	7056.586591	26.399616
198.527612	7072.018980	26.404634
198.605717	7063.382389	26.409652
199.239419	7083.578857	26.414669
199.328455	7086.459772	26.419687
199.387341	7090.371347	26.424704
199.466880	7092.347736	26.429722
199.768089	7115.083574	26.434740
199.978290	7116.566101	26.439757
200.629616	7109.870080	26.444775
200.409010	7118.367837	26.449792
200.696717	7141.364670	26.454810
200.470079	7144.165311	26.459828
200.789353	7148.535137	26.464845
200.962726	7170.397565	26.469863
200.896886	7170.205757	26.474880
201.089599	7173.285209	26.479898
201.275339	7193.308464	26.484916
201.549844	7203.983157	26.489933
202.044020	7221.878070	26.494951
202.207271	7234.672556	26.499968
202.463300	7236.725659	26.504986
202.846797	7253.236196	26.510004
202.493880	7251.823187	26.515021
203.246084	7260.999806	26.520039
203.140889	7276.393159	26.525056
203.339461	7278.246861	26.530074
203.508657	7299.478723	26.535092
203.795250	7302.032171	26.540109
204.203366	7303.976369	26.545127
203.795296	7322.778963	26.550144
204.508023	7330.465414	26.555162
204.496624	7338.861251	26.560180
204.419895	7363.013686	26.565197
204.996230	7370.453054	26.570215
205.112163	7383.097168	26.575232
205.424662	7378.351078	26.580250
205.745610	7393.084694	26.585268
205.778552	7409.088026	26.590285
206.394236	7424.713371	26.595303
206.401876	7434.618430	26.600320
206.525662	7431.770577	26.605338
206.406191	7444.258812	26.610356
206.839221	7463.359936	26.615373
207.154149	7473.662296	26.620391
207.288786	7484.633577	26.625408
207.641904	7495.589791	26.630426
207.542512	7513.069141	26.635444
207.933559	7518.138182	26.640461
208.341736	7529.177394	26.645479
208.486418	7545.952672	26.650496
208.512482	7542.119280	26.655514
208.627616	7558.504558	26.660532
208.959832	7569.542993	26.665549
209.274170	7587.879815	26.670567
208.966405	7602.487341	26.675584
209.935636	7603.911718	26.680602
210.227401	7622.460444	26.685620
210.143219	7625.778811	26.690637
210.523366	7632.544840	26.695655
210.461356	7645.229465	26.700672
211.171225	7640.920235	26.705690
210.997260	7650.907352	26.710708
211.120087	7669.027831	26.715725
211.634334	7677.004197	26.720743
211.681973	7686.511706	26.725760
212.213815	7690.113007	26.730778
212.449798	7700.831871	26.735796
212.252524	7706.503979	26.740813
212.820799	7715.775759	26.745831
212.779691	7719.822999	26.750848
212.969942	7718.435880	26.755866
213.110455	7731.360530	26.760884
213.556127	7746.179190	26.765901
213.488643	7742.631817	26.770919
213.477135	7752.530557	26.775936
213.761142	7767.775334	26.780954
213.879797	7771.349428	26.785972
213.849637	7791.160707	26.790989
214.286500	7795.995393	26.796007
214.187449	7810.861028	26.801024
214.517469	7821.388533	26.806042
214.528244	7837.862916	26.811060
214.871642	7861.439172	26.816077
215.151942	7870.834787	26.821095
215.126894	7883.419113	26.826112
215.219908	7896.547005	26.831130
215.753949	7915.244568	26.836148
216.061842	7941.358333	26.841165
216.701606	7945.697397	26.846183
216.544830	7964.306829	26.851200
216.812781	7964.596573	26.856218
217.339846	7983.345803	26.861236
217.483559	7992.658566	26.866253
217.633407	7996.764532	26.871271
217.828924	8018.665562	26.876288
218.379953	8014.744028	26.881306
218.644181	8038.961075	26.886324
218.964458	8046.737341	26.891341
219.395477	8038.247396	26.896359
219.355398	8051.146717	26.901376
219.667539	8064.711003	26.906394
219.845144	8069.156776	26.911412
220.121698	8069.369414	26.916429
220.042839	8071.449494	26.921447
219.864319	8085.178580	26.926464
220.059901	8090.691777	26.931482
220.824017	8109.353719	26.936500
220.756113	8122.263736	26.941517
220.886747	8125.640300	26.946535
220.997027	8149.609959	26.951552
221.611355	8162.697919	26.956570
222.041724	8169.431073	26.961588
222.008710	8171.194640	26.966605
222.410877	8172.060165	26.971623
222.829101	8196.667011	26.976640
223.024814	8190.155189	26.981658
223.185118	8194.969898	26.986676
223.485050	8213.704213	26.991693
223.448894	8211.051619	26.996711
223.656571	8221.914102	27.001728
223.843705	8224.644173	27.006746
224.418581	8227.632736	27.011764
224.240504	8234.691102	27.016781
224.856422	8232.849363	27.021799
224.921904	8256.327327	27.026816
224.987814	8262.899422	27.031834
225.440740	8264.123263	27.036852
225.298484	8280.429288	27.041869
225.642055	8291.071763	27.046887
225.668307	8290.076349	27.051904
225.752677	8307.237396	27.056922
226.103066	8316.230857	27.061940
226.253976	8338.982138	27.066957
226.431973	8338.806024	27.071975
226.654874	8365.022019	27.076992
226.882403	8367.433276	27.082010
227.165033	8396.815994	27.087028
227.190140	8404.531027	27.092045
227.590400	8406.236633	27.097063
227.694984	8428.979452	27.102080
227.693085	8443.199062	27.107098
228.473850	8452.592829	27.112116
228.383267	8474.046442	27.117133
228.675568	8475.961443	27.122151
228.881868	8489.375196	27.127168
229.021967	8509.785836	27.132186
229.389802	8518.568314	27.137204
229.698125	8542.798100	27.142221
229.674846	8539.856162	27.147239
230.212645	8551.548264	27.152256
230.469836	8572.540586	27.157274
230.497331	8567.990104	27.162292
231.051011	8595.218861	27.167309
231.186449	8599.917579	27.172327
231.398885	8614.975304	27.177344
231.531505	8620.173284	27.182362
232.432296	8625.810474	27.187380
232.339001	8632.997861	27.192397
232.164090	8640.557865	27.197415
232.323786	8642.752409	27.202432
232.433487	8650.132351	27.207450
232.809341	8668.571171	27.212468
233.004444	8686.198364	27.217485
233.840914	8689.089450	27.222503
233.624464	8713.382217	27.227520
234.029418	8718.566240	27.232538
234.214054	8724.387570	27.237556
234.423622	8736.200347	27.242573
234.691973	8747.937681	27.247591
234.656340	8769.061057	27.252608
235.252950	8778.297393	27.257626
235.380533	8793.788370	27.262644
234.894388	8804.680286	27.267661
235.653051	8816.391843	27.272679
235.773945	8832.635286	27.277696
235.782762	8856.454331	27.282714
235.994467	8865.494909	27.287732
236.109091	8892.994515	27.292749
236.436479	8909.505804	27.297767
236.962510	8930.434578	27.302784
237.170371	8939.033792	27.307802
237.862189	8961.395386	27.312820
237.545133	8971.594919	27.317837
238.267042	8984.284703	27.322855
238.487786	8993.229222	27.327872
238.562038	9006.455538	27.332890
239.109507	9026.894884	27.337908
239.197838	9035.288595	27.342925
239.588425	9039.483601	27.347943
240.097171	9042.779367	27.352960
239.658296	9050.064918	27.357978
240.561196	9056.270202	27.362996
240.708776	9075.647913	27.368013
241.020870	9081.673670	27.373031
241.132448	9092.156982	27.378048
241.052673	9091.130675	27.383066
241.512333	9107.640491	27.388084
241.632040	9132.471861	27.393101
241.883873	9130.825636	27.398119
242.107270	9146.459849	27.403136
242.496787	9159.226760	27.408154
242.811164	9169.252325	27.413172
242.831793	9181.221089	27.418189
243.153967	9182.929455	27.423207
243.404795	9202.344896	27.428224
243.569273	9204.627164	27.433242
244.174557	9216.902733	27.438260
243.880272	9233.331137	27.443277
244.230727	9245.043376	27.448295
244.485075	9259.561538	27.453312
244.342224	9277.885975	27.458330
245.077539	9285.219287	27.463348
245.182348	9297.904332	27.468365
245.382406	9312.067909	27.473383
245.424965	9324.478516	27.478400
245.481861	9329.404337	27.483418
245.870889	9336.314844	27.488436
246.429910	9359.161703	27.493453
246.775044	9366.969387	27.498471
246.770167	9374.519003	27.503488
246.837763	9384.583105	27.508506
247.141802	9396.037461	27.513524
247.404320	9424.402007	27.518541
247.853877	9421.127423	27.523559
248.151620	9442.395411	27.528576
248.131484	9454.777979	27.533594
248.292731	9464.385533	27.538612
248.692610	9477.428886	27.543629
248.822271	9489.639767	27.548647
249.579016	9502.731768	27.553664
249.614161	9517.558937	27.558682
250.068772	9531.367329	27.563700
249.869912	9543.559931	27.568717
250.350513	9558.684022	27.573735
250.563568	9569.338082	27.578752
250.671286	9584.987518	27.583770
251.004387	9597.615125	27.588788
250.953530	9616.648583	27.593805
251.406639	9635.824608	27.598823
251.780856	9651.407352	27.603840
252.004216	9656.222097	27.608858
252.372269	9673.005576	27.613876
252.359261	9683.546505	27.618893
252.764098	9707.453379	27.623911
252.875439	9714.359901	27.628928
252.851357	9738.273603	27.633946
253.362871	9751.729159	27.638964
253.465889	9772.071188	27.643981
253.819661	9793.450832	27.648999
253.946175	9811.964340	27.654016
254.629513	9836.642600	27.659034
255.000064	9850.366441	27.664052
255.035480	9866.153662	27.669069
255.628882	9873.799774	27.674087
255.937550	9871.317426	27.679104
256.241906	9902.287268	27.684122
256.459950	9905.972595	27.689140
256.398408	9912.344108	27.694157
256.843244	9924.973486	27.699175
257.204847	9924.711944	27.704192
257.274420	9940.677033	27.709210
257.672217	9949.360809	27.714228
257.832623	9973.722844	27.719245
257.752497	9972.955442	27.724263
258.385344	9990.342074	27.729280
258.283828	10005.383504	27.734298
258.823018	10016.170171	27.739316
258.930509	10036.991705	27.744333
259.582993	10049.358357	27.749351
259.663097	10051.966440	27.754368
259.506351	10064.885325	27.759386
260.009766	10087.511255	27.764404
260.475719	10113.789762	27.769421
260.336375	10120.798610	27.774439
260.959527	10136.829236	27.779456
261.148926	10156.507826	27.784474
261.722252	10169.884601	27.789492
261.774525	10173.365303	27.794509
261.851380	10188.467517	27.799527
262.144590	10190.805642	27.804544
262.376153	10211.990094	27.809562
262.770378	10220.990289	27.814580
263.332860	10227.170038	27.819597
263.579554	10224.943566	27.824615
263.529096	10224.979816	27.829632
263.848153	10246.479051	27.834650
264.206738	10254.635482	27.839668
264.124661	10263.757211	27.844685
264.570459	10278.139014	27.849703
264.845974	10289.977246	27.854720
265.059167	10302.958682	27.859738
265.165333	10312.095331	27.864756
265.393138	10329.030689	27.869773
265.651419	10338.951956	27.874791
265.447953	10357.542639	27.879808
266.250319	10375.632594	27.884826
266.467919	10390.289971	27.889844
266.525389	10405.423795	27.894861
266.694721	10423.722859	27.899879
267.286284	10439.401880	27.904896
267.395714	10460.422501	27.909914
267.926948	10480.752314	27.914932
268.270747	10490.240414	27.919949
268.077641	10509.937882	27.924967
268.531147	10516.630405	27.929984
268.861700	10531.421863	27.935002
269.234828	10549.253601	27.940020
269.952659	10560.495857	27.945037
269.662291	10576.719603	27.950055
270.218779	10579.304113	27.955072
270.355948	10596.863206	27.960090
270.824712	10589.746017	27.965108
271.466993	10613.610775	27.970125
271.591295	10624.156119	27.975143
271.976818	10625.984214	27.980160
272.096820	10651.982654	27.985178
272.296369	10661.657486	27.990196
272.400474	10667.005721	27.995213
272.520242	10681.912208	28.000231
273.192343	10686.603684	28.005248
273.217773	10705.032780	28.010266
273.476778	10694.263486	28.015284
274.007543	10706.573748	28.020301
274.024358	10730.245548	28.025319
274.719028	10747.604321	28.030336
275.209286	10761.951160	28.035354
275.178178	10756.032622	28.040372
275.442965	10770.521923	28.045389
275.745133	10780.673401	28.050407
275.769808	10785.200471	28.055424
275.639000	10793.736446	28.060442
276.217889	10815.129580	28.065460
276.004303	10826.539107	28.070477
275.981271	10860.763168	28.075495
276.318937	10873.128863	28.080512
277.068486	10891.202285	28.085530
276.916453	10912.646174	28.090548
277.554138	10931.617983	28.095565
277.531382	10954.374246	28.100583
278.314081	10957.315120	28.105600
278.009005	10990.942363	28.110618
278.504622	11009.358550	28.115636
279.135211	11024.978313	28.120653
279.161702	11041.500454	28.125671
279.675767	11054.707116	28.130688
280.218604	11072.449784	28.135706
280.391067	11086.439032	28.140724
280.665134	11090.731585	28.145741
281.068490	11117.295956	28.150759
281.294702	11119.474125	28.155776
281.234087	11126.973136	28.160794
281.580628	11137.660991	28.165812
282.241552	11150.216514	28.170829
281.912181	11171.413605	28.175847
282.386905	11177.263167	28.180864
282.812641	11195.466234	28.185882
282.848893	11213.660491	28.190900
283.173807	11214.307696	28.195917
283.567301	11252.686072	28.200935
283.947299	11258.976673	28.205952
283.939499	11267.875773	28.210970
283.821966	11280.890434	28.215988
284.781742	11303.276287	28.221005
284.484736	11319.031235	28.226023
284.867026	11340.862901	28.231040
285.602752	11362.033321	28.236058
285.571065	11375.249394	28.241076
285.725558	11402.711767	28.246093
286.041999	11414.534870	28.251111
286.374989	11426.655371	28.256128
286.682291	11444.558207	28.261146
286.854031	11474.133562	28.266164
287.321805	11482.990301	28.271181
287.352912	11516.828225	28.276199
287.992340	11536.024566	28.281216
287.918535	11557.482274	28.286234
288.549621	11577.737743	28.291252
288.765931	11594.170826	28.296269
289.063125	11619.239956	28.301287
289.503851	11634.466672	28.306304
289.963455	11649.614679	28.311322
290.141562	11663.038271	28.316340
291.131798	11668.454081	28.321357
291.071563	11693.594744	28.326375
291.389380	11703.112768	28.331392
291.910979	11713.306375	28.336410
291.931222	11716.640787	28.341428
292.080767	11729.819423	28.346445
292.346948	11743.924034	28.351463
292.822579	11757.860270	28.356480
292.791298	11776.043482	28.361498
292.986585	11800.497198	28.366516
293.530791	11816.863640	28.371533
293.507254	11827.265325	28.376551
293.934911	11853.665919	28.381568
294.462896	11871.225359	28.386586
294.233489	11893.042383	28.391604
294.817529	11897.612101	28.396621
294.690226	11927.585224	28.401639
294.931245	11945.994608	28.406656
295.199826	11962.157791	28.411674
295.812942	11987.361373	28.416692
296.416928	11994.649902	28.421709
296.830406	12014.740792	28.426727
297.355835	12026.724362	28.431744
297.900246	12039.068116	28.436762
297.841887	12047.823889	28.441780
298.196402	12054.829200	28.446797
298.522198	12068.751103	28.451815
298.698828	12083.646696	28.456832
299.165373	12094.379570	28.461850
299.195780	12100.292280	28.466868
299.763259	12120.460353	28.471885
299.606995	12130.851293	28.476903
300.091259	12151.749146	28.481920
300.662318	12161.979506	28.486938
300.707559	12178.259745	28.491956
301.262257	12181.179477	28.496973
301.490578	12199.527933	28.501991
301.450939	12206.379941	28.507008
301.746804	12215.519564	28.512026
301.987428	12231.100002	28.517044
302.715119	12245.351022	28.522061
302.184838	12263.463980	28.527079
302.852036	12271.320635	28.532096
303.188072	12283.832771	28.537114
303.576045	12305.724674	28.542132
303.809075	12321.937910	28.547149
303.766426	12338.235129	28.552167
303.785111	12357.532110	28.557184
304.266863	12376.839120	28.562202
304.257086	12409.601921	28.567220
304.864051	12420.834144	28.572237
305.000218	12449.658721	28.577255
305.419511	12473.143751	28.582272
305.948145	12486.472310	28.587290
306.073880	12514.111302	28.592308
306.634755	12537.037555	28.597325
306.888076	12557.207641	28.602343
307.193522	12578.032761	28.607360
307.527628	12603.198506	28.612378
307.790090	12622.858841	28.617396
307.777323	12639.764272	28.622413
308.394406	12660.970422	28.627431
308.924363	12690.081413	28.632448
309.390345	12707.771285	28.637466
309.686255	12735.260955	28.642484
310.011219	12745.747833	28.647501
310.394850	12763.292689	28.652519
310.693999	12782.164350	28.657536
311.377870	12789.494437	28.662554
311.235953	12817.203962	28.667572
311.702609	12837.625337	28.672589
312.200834	12858.070239	28.677607
312.382685	12859.980791	28.682624
312.951080	12868.547795	28.687642
313.053129	12876.982148	28.692660
313.114210	12899.058260	28.697677
313.127882	12921.748077	28.702695
313.703907	12931.116003	28.707712
313.977878	12955.394764	28.712730
314.256899	12978.352804	28.717748
314.536212	12996.874094	28.722765
315.144576	13015.865214	28.727783
315.219436	13026.441711	28.732800
315.669464	13049.951096	28.737818
315.623177	13067.951579	28.742836
316.027301	13080.930479	28.747853
316.513359	13111.173144	28.752871
316.758624	13129.497762	28.757888
317.145843	13138.181515	28.762906
317.282462	13168.475515	28.767924
318.000034	13181.888837	28.772941
318.570404	13202.168146	28.777959
318.678313	13221.584750	28.782976
319.069004	13222.048108	28.787994
319.114818	13245.971189	28.793012
319.642442	13256.044700	28.798029
319.816698	13269.520564	28.803047
319.787898	13286.160652	28.808064
320.477831	13316.545588	28.813082
320.979592	13337.887296	28.818100
321.216393	13354.738724	28.823117
321.603916	13371.181442	28.828135
321.667122	13385.802040	28.833152
321.992001	13385.580914	28.838170
322.003855	13423.685243	28.843188
322.352689	13428.655114	28.848205
322.977735	13445.594601	28.853223
322.939922	13461.418352	28.858240
323.543932	13486.603257	28.863258
323.093486	13501.231279	28.868276
323.251015	13530.609970	28.873293
323.788277	13546.909529	28.878311
324.125184	13578.524589	28.883328
324.826263	13597.568178	28.888346
325.014512	13630.172791	28.893364
325.179635	13652.075688	28.898381
325.842802	13674.153708	28.903399
325.811894	13689.869204	28.908416
326.805158	13714.226435	28.913434
327.139657	13735.465157	28.918452
327.582922	13748.792112	28.923469
328.200646	13763.494044	28.928487
328.436425	13780.052322	28.933504
329.001829	13782.279052	28.938522
329.072529	13806.540025	28.943540
329.299507	13817.579607	28.948557
329.576833	13833.269342	28.953575
330.019237	13845.544900	28.958592
330.312309	13853.296253	28.963610
330.673940	13886.660647	28.968628
330.985128	13896.082918	28.973645
331.319309	13911.334383	28.978663
331.575539	13924.257939	28.983680
332.551527	13938.045263	28.988698
332.140628	13947.835773	28.993716
332.683315	13962.972711	28.998733
333.246088	13980.336069	29.003751
333.352620	13995.673570	29.008768
334.007483	14008.080374	29.013786
333.796519	14028.466422	29.018804
333.995246	14037.350466	29.023821
334.368282	14054.342365	29.028839
334.836462	14075.472233	29.033856
335.107534	14094.905385	29.038874
335.335925	14124.545553	29.043892
335.871639	14138.231036	29.048909
336.121516	14161.302421	29.053927
336.791986	14187.693748	29.058944
336.732239	14194.707507	29.063962
337.450205	14220.756736	29.068980
337.393236	14242.555938	29.073997
337.563601	14262.560752	29.079015
337.774180	14289.289091	29.084032
338.159257	14299.559045	29.089050
338.030172	14334.544901	29.094068
338.712585	14357.407075	29.099085
339.331487	14377.749569	29.104103
339.838611	14411.805954	29.109120
340.095465	14421.148521	29.114138
340.696677	14451.185917	29.119156
340.594905	14468.586861	29.124173
341.314729	14489.235885	29.129191
341.279671	14505.110606	29.134208
341.946724	14533.236725	29.139226
342.032556	14543.303911	29.144244
342.508794	14572.552488	29.149261
342.639203	14587.684634	29.154279
342.757504	14608.190577	29.159296
343.572057	14632.330484	29.164314
343.959877	14645.489851	29.169332
344.315650	14670.067568	29.174349
344.746017	14676.509381	29.179367
344.860003	14697.082413	29.184384
345.033673	14713.704862	29.189402
345.563358	14732.435204	29.194420
345.882006	14744.544284	29.199437
346.156593	14758.908806	29.204455
346.210641	14784.582137	29.209472
346.619671	14806.511557	29.214490
347.011201	14830.894428	29.219508
347.173175	14862.346216	29.224525
348.103565	14874.344352	29.229543
348.397162	14891.380950	29.234560
349.029610	14911.248188	29.239578
349.100049	14924.056075	29.244596
349.268337	14946.740032	29.249613
349.747383	14969.340898	29.254631
349.914194	14988.339580	29.259648
350.360339	15015.073322	29.264666
350.561208	15025.918708	29.269684
351.203461	15049.103784	29.274701
351.428776	15069.732523	29.279719
351.906137	15095.713034	29.284736
352.462242	15110.896174	29.289754
352.562982	15136.556394	29.294772
352.757793	15155.452980	29.299789
353.279147	15168.405588	29.304807
353.548106	15192.763791	29.309824
354.170685	15211.416979	29.314842
354.472179	15228.954801	29.319860
355.011031	15251.676177	29.324877
355.236321	15270.438647	29.329895
355.544806	15288.559702	29.334912
355.927515	15302.140360	29.339930
356.344161	15333.505904	29.344948
356.378058	15344.238505	29.349965
356.918634	15361.167593	29.354983
357.531343	15387.806446	29.360000
357.509325	15402.653464	29.365018
358.305646	15419.485941	29.370036
358.540924	15431.343148	29.375053
359.016817	15455.798958	29.380071
359.347983	15474.399867	29.385088
359.654339	15486.084973	29.390106
360.082903	15499.200690	29.395124
360.323361	15519.331715	29.400141
360.911407	15534.285987	29.405159
361.462728	15546.883623	29.410176
361.695605	15576.828545	29.415194
361.678006	15593.115182	29.420212
361.911869	15617.233047	29.425229
362.246691	15629.172786	29.430247
362.588398	15655.184654	29.435264
362.973032	15679.506520	29.440282
363.197280	15705.296713	29.445300
363.172837	15726.062951	29.450317
364.016947	15756.585708	29.455335
364.069085	15781.594281	29.460352
364.819592	15800.379728	29.465370
365.044231	15835.243783	29.470388
365.356244	15854.694465	29.475405
365.368176	15877.236480	29.480423
366.027874	15907.181795	29.485440
366.345625	15930.364771	29.490458
366.924330	15955.256853	29.495476
367.055276	15978.986932	29.500493
367.517153	15997.896467	29.505511
367.900803	16031.703355	29.510528
367.881427	16042.334100	29.515546
368.679571	16062.464151	29.520564
369.105398	16090.731192	29.525581
369.499371	16115.033208	29.530599
369.619580	16130.689290	29.535616
370.175955	16158.285490	29.540634
370.249770	16173.355060	29.545652
370.750116	16205.075372	29.550669
370.946601	16227.945961	29.555687
371.289888	16249.972551	29.560704
371.752179	16285.637391	29.565722
372.523438	16307.954315	29.570740
372.538534	16324.814465	29.575757
372.857052	16345.199510	29.580775
373.403920	16376.840221	29.585792
373.612851	16391.314103	29.590810
373.766786	16402.271805	29.595828
374.321775	16458.151976	29.600845
374.954487	16470.172200	29.605863
375.049999	16501.817059	29.610880
375.316565	16534.452345	29.615898
375.719548	16562.606778	29.620916
376.264958	16590.969643	29.625933
376.733180	16615.011219	29.630951
376.995760	16641.273625	29.635968
377.187719	16671.280320	29.640986
377.732619	16694.675215	29.646004
378.058207	16730.280045	29.651021
378.664972	16750.529052	29.656039
379.466610	16781.751755	29.661056
379.964546	16801.423971	29.666074
380.217568	16824.965536	29.671092
380.537828	16839.965678	29.676109
380.970006	16847.020687	29.681127
381.584790	16877.593569	29.686144
382.036428	16882.355679	29.691162
382.652424	16896.374922	29.696180
382.784606	16913.160507	29.701197
383.324896	16937.453420	29.706215
383.656105	16949.628273	29.711232
384.580600	16955.570700	29.716250
385.060603	16960.802185	29.721268
385.445234	16977.728558	29.726285
385.775628	16982.759088	29.731303
386.168752	16992.767090	29.736320
386.228034	17009.071385	29.741338
386.613541	17019.538567	29.746356
386.592069	17039.285572	29.751373
386.869443	17043.913769	29.756391
387.613899	17066.201008	29.761408
387.405802	17094.659814	29.766426
388.069359	17118.971670	29.771444
388.126247	17134.281516	29.776461
388.730952	17162.569667	29.781479
389.356123	17185.911605	29.786496
389.228749	17203.492734	29.791514
389.473462	17217.547904	29.796532
389.441865	17248.335711	29.801549
389.955504	17275.636955	29.806567
390.732453	17303.001476	29.811584
391.251601	17331.499023	29.816602
391.673891	17353.880970	29.821620
391.856442	17385.602170	29.826637
392.145537	17407.069986	29.831655
392.388498	17430.206405	29.836672
393.106182	17465.599943	29.841690
393.622961	17488.997026	29.846708
393.741223	17516.502298	29.851725
393.930868	17532.325590	29.856743
394.258260	17558.812893	29.861760
394.904160	17584.858983	29.866778
395.459100	17610.338090	29.871796
395.841281	17634.346958	29.876813
396.230121	17646.112140	29.881831
396.421037	17678.034668	29.886848
396.268844	17698.551284	29.891866
397.028205	17727.087826	29.896884
397.349658	17760.537881	29.901901
397.205445	17777.300917	29.906919
398.008393	17801.566666	29.911936
398.482891	17842.080959	29.916954
399.368039	17867.957524	29.921972
399.658677	17885.720570	29.926989
400.233291	17920.717120	29.932007
400.725230	17948.638627	29.937024
401.244683	17979.581868	29.942042
401.404839	17987.996800	29.947060
401.434083	18018.978515	29.952077
401.975764	18044.239155	29.957095
402.451854	18075.808396	29.962112
402.988303	18104.898220	29.967130
403.542544	18122.399340	29.972148
403.955036	18161.647856	29.977165
404.432164	18181.511084	29.982183
404.993639	18201.474915	29.987200
405.121011	18230.698104	29.992218
405.042313	18253.724491	29.997236
406.223143	18272.214788	30.002253
406.694360	18288.061196	30.007271
406.978890	18309.066398	30.012288
407.713123	18333.539354	30.017306
408.160600	18346.748836	30.022324
408.380461	18371.358773	30.027341
408.274804	18394.749618	30.032359
409.532117	18415.186543	30.037376
409.243164	18442.086879	30.042394
409.723329	18458.260541	30.047412
410.320123	18486.659262	30.052429
410.813553	18503.727974	30.057447
411.432283	18529.602681	30.062464
412.014488	18539.209322	30.067482
412.316511	18555.233910	30.072500
412.726892	18585.677068	30.077517
412.735086	18603.712174	30.082535
413.335542	18615.167034	30.087552
413.645912	18648.563493	30.092570
413.841491	18662.842159	30.097588
414.358149	18693.237354	30.102605
414.372955	18723.540152	30.107623
414.953634	18741.997981	30.112640
415.328959	18775.302417	30.117658
415.710013	18801.435602	30.122676
416.308467	18823.340122	30.127693
416.485606	18847.085492	30.132711
417.216441	18864.932529	30.137728
417.559727	18902.986666	30.142746
417.892063	18933.164546	30.147764
418.083686	18957.293168	30.152781
418.752785	18990.874438	30.157799
419.150478	19011.161529	30.162816
419.163573	19037.175421	30.167834
420.099284	19062.376048	30.172852
420.245412	19086.884654	30.177869
420.732755	19113.393406	30.182887
421.463330	19135.220852	30.187904
421.737847	19157.233038	30.192922
422.159030	19180.896599	30.197940
422.707213	19208.697450	30.202957
422.938891	19228.132455	30.207975
423.417386	19237.218587	30.212992
423.634550	19268.116181	30.218010
424.191053	19288.069271	30.223028
424.568783	19313.388679	30.228045
424.700994	19339.175947	30.233063
425.409874	19360.507924	30.238080
425.625448	19399.732741	30.243098
426.062155	19423.855376	30.248116
426.194541	19460.433494	30.253133
426.670597	19488.125935	30.258151
427.280609	19513.548433	30.263168
427.280104	19546.413595	30.268186
428.241211	19573.601036	30.273204
428.404937	19606.415460	30.278221
428.984293	19645.817898	30.283239
429.466048	19671.551189	30.288256
429.702880	19697.404775	30.293274
430.091772	19726.557910	30.298292
430.899812	19751.204384	30.303309
430.941462	19791.448967	30.308327
431.888690	19809.585399	30.313344
432.271300	19842.315601	30.318362
432.672542	19864.776382	30.323380
432.902011	19895.723598	30.328397
433.488201	19926.413156	30.333415
434.311434	19947.266767	30.338432
434.459388	19985.283930	30.343450
434.931139	20001.062159	30.348468
435.872878	20034.501699	30.353485
435.848018	20059.518310	30.358503
436.542904	20080.429953	30.363520
436.761481	20110.463100	30.368538
437.167128	20137.415587	30.373556
437.317932	20167.168745	30.378573
437.812800	20192.641645	30.383591
438.706306	20208.385974	30.388608
438.422625	20245.655817	30.393626
438.994193	20274.130575	30.398644
439.728195	20307.457609	30.403661
439.714051	20336.965029	30.408679
440.368466	20362.792395	30.413696
440.667520	20409.486818	30.418714
441.477655	20432.390042	30.423732
442.224776	20468.634259	30.428749
442.463701	20496.977903	30.433767
443.108703	20514.226965	30.438784
443.463203	20547.948348	30.443802
443.794791	20585.716955	30.448820
444.603985	20612.885272	30.453837
444.516602	20646.397618	30.458855
444.898785	20671.465369	30.463872
445.623669	20702.507326	30.468890
445.807969	20728.913816	30.473908
446.146298	20755.138408	30.478925
446.421276	20791.728407	30.483943
446.906953	20821.278790	30.488960
447.356723	20861.796901	30.493978
447.636751	20889.363892	30.498996
448.459934	20915.797538	30.504013
448.514468	20962.638753	30.509031
449.056497	20996.047392	30.514048
449.786769	21027.487076	30.519066
450.313101	21063.589855	30.524084
450.560703	21095.167970	30.529101
451.005673	21136.521410	30.534119
451.811975	21160.108460	30.539136
451.744050	21187.053978	30.544154
451.957289	21211.302066	30.549172
452.671245	21234.473936	30.554189
452.768392	21271.294699	30.559207
453.342288	21305.059049	30.564224
453.795003	21339.720574	30.569242
454.598977	21370.346901	30.574260
454.981224	21404.539315	30.579277
455.437742	21435.674758	30.584295
455.940572	21469.532593	30.589312
456.392696	21501.104794	30.594330
456.950817	21533.658857	30.599348
457.643998	21563.279147	30.604365
458.163862	21595.649715	30.609383
458.670158	21616.592360	30.614400
458.619244	21651.718265	30.619418
459.342411	21682.446117	30.624436
460.051861	21707.401058	30.629453
460.311184	21735.490574	30.634471
461.039398	21752.279160	30.639488
461.272895	21799.669489	30.644506
461.654579	21815.305240	30.649524
462.431555	21845.570037	30.654541
462.747916	21878.509826	30.659559
463.134480	21911.173361	30.664576
463.790802	21938.493685	30.669594
464.329538	21972.150919	30.674612
465.204616	21989.220137	30.679629
465.491345	22009.224322	30.684647
465.966619	22031.183212	30.689664
466.534227	22055.535136	30.694682
466.744798	22092.011208	30.699700
467.470473	22112.427379	30.704717
467.535418	22138.247753	30.709735
467.995762	22162.862935	30.714752
468.311462	22202.715949	30.719770
468.872235	22221.894176	30.724788
469.447751	22249.733004	30.729805
469.774369	22284.466372	30.734823
470.344555	22317.398971	30.739840
470.796549	22344.157712	30.744858
470.905837	22380.504753	30.749876
471.630073	22412.617374	30.754893
471.973229	22445.996247	30.759911
472.187196	22483.622520	30.764928
472.656971	22520.254910	30.769946
473.104860	22560.808404	30.774964
473.735590	22597.169448	30.779981
474.098906	22638.020610	30.784999
474.647544	22667.361762	30.790016
475.339085	22704.680312	30.795034
475.669838	22740.165773	30.800052
476.451851	22770.330105	30.805069
476.685484	22808.705874	30.810087
477.420048	22839.920306	30.815104
478.002011	22873.344869	30.820122
478.280525	22902.962219	30.825140
478.973955	22927.529430	30.830157
479.287200	22962.044908	30.835175
479.610657	22987.920929	30.840192
480.371915	23022.986020	30.845210
480.620247	23047.831195	30.850228
481.165424	23084.990000	30.855245
481.774694	23124.040895	30.860263
482.229228	23143.204962	30.865280
482.589536	23175.963139	30.870298
482.853385	23213.709410	30.875316
483.418216	23228.717468	30.880333
483.686204	23268.902322	30.885351
484.195371	23298.598098	30.890368
484.825155	23337.570392	30.895386
484.976156	23374.298220	30.900404
485.474023	23400.672106	30.905421
485.722012	23442.288523	30.910439
486.634532	23466.961315	30.915456
487.367828	23500.148528	30.920474
487.522793	23527.239465	30.925492
488.627332	23554.909305	30.930509
488.712006	23592.292406	30.935527
489.208527	23629.093297	30.940544
490.067848	23655.834632	30.945562
490.183099	23693.567033	30.950580
490.671693	23716.871692	30.955597
491.331008	23750.614285	30.960615
492.069840	23774.265523	30.965632
492.644829	23798.801700	30.970650
492.860471	23831.412862	30.975668
494.062400	23845.665014	30.980685
494.453634	23883.481194	30.985703
494.456482	23910.293013	30.990720
494.861331	23939.310876	30.995738
495.584588	23975.495744	31.000756
496.155559	24005.303020	31.005773
496.479829	24029.827959	31.010791
496.788855	24061.268542	31.015808
497.381183	24090.800893	31.020826
497.544735	24135.237647	31.025844
498.131045	24160.739354	31.030861
498.363423	24193.967791	31.035879
499.129732	24232.155953	31.040896
499.710716	24267.674699	31.045914
500.079150	24306.752771	31.050932
500.466690	24339.767717	31.055949
500.887615	24372.663771	31.060967
501.229942	24423.670718	31.065984
501.847584	24458.324665	31.071002
502.306519	24496.858194	31.076020
503.001858	24534.716738	31.081037
503.777258	24577.264520	31.086055
504.439618	24617.656114	31.091072
505.065004	24647.986709	31.096090
505.449297	24679.157451	31.101108
506.358948	24712.331870	31.106125
506.802818	24742.014687	31.111143
507.324400	24769.296695	31.116160
507.901031	24802.643177	31.121178
508.285010	24835.311925	31.126196
508.775437	24861.044317	31.131213
509.347471	24896.736201	31.136231
509.690743	24920.595729	31.141248
510.254983	24948.092523	31.146266
510.668697	24987.525089	31.151284
511.258250	25013.052660	31.156301
511.380758	25051.519560	31.161319
511.666335	25085.543778	31.166336
512.368609	25123.105338	31.171354
512.343047	25165.804341	31.176372
513.260865	25197.929245	31.181389
513.920418	25238.215096	31.186407
513.983103	25280.167530	31.191424
514.707094	25309.674868	31.196442
515.312156	25359.290896	31.201460
515.683399	25392.385950	31.206477
516.270685	25430.623231	31.211495
516.614890	25469.359763	31.216512
517.299325	25497.628560	31.221530
518.058913	25542.127318	31.226548
518.818976	25558.035738	31.231565
519.324208	25593.865657	31.236583
519.207155	25626.651610	31.241600
520.284454	25649.588812	31.246618
520.594223	25690.555677	31.251636
521.403575	25705.641294	31.256653
522.018689	25740.771837	31.261671
522.183754	25765.298408	31.266688
522.793919	25793.825656	31.271706
523.010223	25834.617772	31.276724
523.902053	25871.241174	31.281741
524.438432	25893.030501	31.286759
525.042676	25931.272415	31.291776
525.201412	25967.175900	31.296794
526.141048	26000.158192	31.301812
526.480251	26032.861139	31.306829
526.888499	26068.296211	31.311847
526.992986	26107.248246	31.316864
527.798076	26138.842378	31.321882
528.129465	26189.109768	31.326900
528.773871	26218.213718	31.331917
529.528204	26256.597203	31.336935
529.702704	26294.205196	31.341952
530.462260	26342.086896	31.346970
531.018817	26379.502852	31.351988
531.402230	26428.403947	31.357005
531.820795	26465.304345	31.362023
532.365663	26508.100670	31.367040
532.986212	26548.723860	31.372058
533.262650	26594.665283	31.377076
533.810999	26637.366540	31.382093
534.663176	26673.232850	31.387111
535.209906	26723.253164	31.392128
535.617110	26753.955872	31.397146
536.350755	26801.836376	31.402164
536.588477	26849.339148	31.407181
537.361754	26888.270736	31.412199
537.600616	26942.713044	31.417216
538.422133	26968.554596	31.422234
538.810463	27015.800467	31.427252
539.905881	27051.597983	31.432269
540.498376	27099.077713	31.437287
540.477134	27141.280927	31.442304
541.120754	27177.186919	31.447322
541.624725	27231.095755	31.452340
542.223484	27270.345976	31.457357
542.962662	27295.208487	31.462375
543.621330	27342.406715	31.467392
544.434125	27375.455246	31.472410
544.954756	27414.711590	31.477428
545.345624	27456.478407	31.482445
546.083986	27495.859021	31.487463
546.125084	27527.852356	31.492480
546.438337	27565.371585	31.497498
547.363491	27611.454498	31.502516
547.688908	27651.443248	31.507533
548.362992	27699.569000	31.512551
548.939908	27744.391790	31.517568
549.249557	27783.555284	31.522586
549.969201	27825.891078	31.527604
550.401084	27862.178868	31.532621
550.880052	27907.624027	31.537639
551.676693	27955.036057	31.542656
552.497427	27985.568807	31.547674
552.961740	28031.180854	31.552692
553.212258	28068.571728	31.557709
553.869952	28104.287556	31.562727
554.308283	28152.779748	31.567744
555.004983	28185.519005	31.572762
555.525002	28210.410435	31.577780
556.234095	28244.740633	31.582797
556.981286	28287.129985	31.587815
557.198144	28327.756378	31.592832
557.749965	28354.652975	31.597850
558.061827	28387.705290	31.602868
558.633938	28429.123540	31.607885
558.983681	28468.307392	31.612903
559.745832	28504.165676	31.617920
559.956121	28545.931238	31.622938
560.927706	28588.039779	31.627956
561.423071	28630.544896	31.632973
562.147270	28669.651879	31.637991
562.793558	28729.313306	31.643008
563.193227	28756.986283	31.648026
564.080756	28799.380136	31.653044
565.175795	28841.590076	31.658061
565.843643	28860.081676	31.663079
565.920643	28899.176078	31.668096
566.812208	28935.451106	31.673114
567.028232	28968.765790	31.678132
567.299716	29002.855672	31.683149
568.054595	29041.535100	31.688167
568.381324	29095.482784	31.693184
569.116936	29126.182196	31.698202
569.701596	29182.017804	31.703220
570.048495	29212.784179	31.708237
570.620702	29254.298901	31.713255
570.762400	29316.644784	31.718272
571.720758	29357.663461	31.723290
572.009884	29404.506817	31.728308
572.561046	29446.960698	31.733325
573.361088	29485.614973	31.738343
574.024475	29535.383842	31.743360
574.561029	29589.913294	31.748378
575.342660	29636.250684	31.753396
575.804965	29681.063963	31.758413
576.458777	29723.843771	31.763431
577.078983	29774.669229	31.768448
577.755385	29820.302820	31.773466
578.356008	29860.992613	31.778484
578.644478	29913.026806	31.783501
579.195092	29945.254336	31.788519
579.536066	30005.915169	31.793536
580.539975	30046.826998	31.798554
581.095700	30094.572269	31.803572
581.595265	30151.725910	31.808589
582.429432	30185.028515	31.813607
582.816528	30230.215005	31.818624
583.556448	30275.138070	31.823642
584.445150	30313.236482	31.828660
585.293596	30350.380410	31.833677
585.948074	30386.107046	31.838695
586.477808	30426.903812	31.843712
586.784220	30466.667137	31.848730
587.303401	30503.704569	31.853748
588.219207	30543.803022	31.858765
588.729806	30570.140035	31.863783
589.253172	30624.118011	31.868800
589.653830	30649.713689	31.873818
589.942373	30689.846860	31.878836
590.402954	30740.756445	31.883853
590.927296	30778.640623	31.888871
591.678764	30829.479858	31.893888
592.354108	30873.048871	31.898906
592.979947	30919.362834	31.903924
593.029680	30959.413599	31.908941
593.891455	30994.849843	31.913959
594.334427	31046.262311	31.918976
594.893144	31077.813963	31.923994
595.863195	31115.420768	31.929012
596.410862	31161.576764	31.934029
596.961063	31201.809269	31.939047
597.868369	31241.208720	31.944064
598.111937	31276.330790	31.949082
598.531353	31324.915598	31.954100
598.750953	31373.240836	31.959117
599.547476	31414.870390	31.964135
600.688910	31459.695602	31.969152
601.115161	31498.696316	31.974170
601.811946	31546.840209	31.979188
602.252582	31591.597797	31.984205
602.778326	31634.894590	31.989223
603.338467	31688.521932	31.994240
603.781601	31730.864581	31.999258
604.591523	31774.901308	32.004276
604.799046	31838.603710	32.009293
606.084817	31872.932384	32.014311
606.801757	31923.476243	32.019328
607.261262	31977.265395	32.024346
608.146709	32016.309389	32.029364
608.374382	32063.522358	32.034381
609.322000	32098.529898	32.039399
609.964821	32147.233574	32.044416
610.496229	32184.607164	32.049434
611.535985	32224.063728	32.054452
611.608980	32277.003491	32.059469
612.366117	32317.743298	32.064487
612.861249	32363.138888	32.069504
613.402434	32420.001511	32.074522
613.973012	32459.038457	32.079540
614.724812	32522.696154	32.084557
615.172680	32555.626510	32.089575
615.883111	32608.537424	32.094592
616.245289	32658.670477	32.099610
616.937348	32707.374121	32.104628
617.510859	32759.225686	32.109645
617.989631	32808.203002	32.114663
618.973005	32859.074330	32.119680
619.480586	32902.123711	32.124698
620.423596	32952.464183	32.129716
620.405859	33004.813005	32.134733
621.535068	33050.326331	32.139751
622.517858	33095.540127	32.144768
622.905175	33143.887620	32.149786
623.517210	33179.202101	32.154804
624.146144	33234.548636	32.159821
624.811401	33286.734942	32.164839
625.309689	33328.029107	32.169856
625.633148	33382.298253	32.174874
626.271132	33430.923493	32.179892
626.422926	33486.477735	32.184909
627.391752	33538.870299	32.189927
628.200231	33592.002361	32.194944
628.934643	33650.020498	32.199962
629.726747	33681.659891	32.204980
630.016209	33739.817087	32.209997
630.854266	33783.999092	32.215015
631.223208	33830.960140	32.220032
631.872244	33888.189302	32.225050
632.954059	33928.477085	32.230068
633.600232	33976.647113	32.235085
634.160138	34028.788444	32.240103
634.793091	34071.454019	32.245120
635.520113	34110.849035	32.250138
636.429025	34147.408690	32.255156
636.878011	34188.718549	32.260173
637.422291	34222.806156	32.265191
637.913507	34266.303454	32.270208
638.344573	34302.925122	32.275226
639.032102	34345.841976	32.280244
639.711958	34398.749531	32.285261
639.971887	34434.936533	32.290279
640.650615	34481.528366	32.295296
641.207987	34534.708228	32.300314
642.415195	34581.034661	32.305332
642.697414	34629.914058	32.310349
643.379535	34677.675457	32.315367
644.153256	34728.615576	32.320384
644.725178	34777.380668	32.325402
645.439715	34812.011754	32.330420
646.219476	34865.903892	32.335437
646.631738	34920.011441	32.340455
647.413164	34967.366038	32.345472
648.103701	35018.705486	32.350490
648.942849	35066.658290	32.355508
649.398439	35120.772254	32.360525
650.349500	35160.678107	32.365543
651.304179	35212.229811	32.370560
651.748963	35253.649897	32.375578
652.546810	35295.445045	32.380596
652.904053	35351.307324	32.385613
653.395239	35395.161027	32.390631
654.377960	35441.277713	32.395648
654.837602	35480.881307	32.400666
655.927193	35532.690993	32.405684
655.939993	35590.030142	32.410701
656.751200	35629.591932	32.415719
657.558300	35672.012340	32.420736
658.053460	35730.250490	32.425754
658.470035	35779.219116	32.430772
659.000880	35835.586766	32.435789
659.562696	35889.641898	32.440807
660.420213	35935.279646	32.445824
660.762663	36016.684097	32.450842
661.857639	36059.724372	32.455860
662.524175	36114.130504	32.460877
662.971441	36168.874410	32.465895
663.840674	36227.789155	32.470912
664.631641	36275.081965	32.475930
665.442319	36324.142249	32.480948
665.927243	36378.444546	32.485965
666.581611	36425.898061	32.490983
667.398158	36470.531654	32.496000
667.835843	36540.813715	32.501018
668.569615	36581.982746	32.506036
669.014326	36649.159443	32.511053
669.682633	36696.857993	32.516071
670.456637	36752.387187	32.521088
671.255150	36809.955083	32.526106
672.067825	36867.520930	32.531124
672.604537	36921.886105	32.536141
673.301126	36969.460723	32.541159
674.389973	37019.541603	32.546176
675.085121	37069.797705	32.551194
675.921501	37105.943792	32.556212
676.679041	37160.129764	32.561229
676.897509	37201.696372	32.566247
677.692962	37252.569616	32.571264
678.182387	37309.946693	32.576282
679.186425	37355.305424	32.581300
679.697637	37408.158216	32.586317
680.408717	37449.971111	32.591335
681.206818	37476.272045	32.596352
681.847423	37514.466444	32.601370
682.410151	37553.324340	32.606388
682.994644	37610.864479	32.611405
683.909957	37656.749856	32.616423
684.245766	37695.542160	32.621440
684.610063	37744.074477	32.626458
684.906172	37794.482929	32.631476
685.913155	37847.967854	32.636493
686.661806	37892.773078	32.641511
687.617531	37939.601289	32.646528
688.246496	38000.904341	32.651546
688.980236	38045.731177	32.656564
689.846064	38091.106662	32.661581
690.105687	38147.143227	32.666599
691.049322	38193.733582	32.671616
691.497372	38250.910942	32.676634
692.409386	38304.550908	32.681652
693.103051	38358.123821	32.686669
693.474629	38416.584568	32.691687
694.331794	38466.028276	32.696704
694.644203	38532.137487	32.701722
695.236946	38591.063848	32.706740
696.469252	38648.815783	32.711757
697.042102	38712.785546	32.716775
697.847792	38769.744195	32.721792
698.302803	38832.986459	32.726810
698.853322	38895.075766	32.731828
699.550924	38955.624652	32.736845
700.222677	39020.895276	32.741863
701.236075	39076.304692	32.746880
701.365611	39138.112423	32.751898
702.594991	39204.801868	32.756916
703.457388	39267.893455	32.761933
703.869678	39329.075921	32.766951
704.404666	39386.862499	32.771968
705.052025	39451.183313	32.776986
706.095113	39518.705864	32.782004
706.465488	39582.203805	32.787021
707.206722	39650.589547	32.792039
707.875545	39705.472411	32.797056
708.704726	39776.045606	32.802074
709.395946	39845.786763	32.807092
710.231029	39907.145359	32.812109
711.088916	39977.398538	32.817127
711.782893	40027.484661	32.822144
712.248761	40107.272761	32.827162
713.347437	40163.683546	32.832180
714.042344	40224.799248	32.837197
714.757892	40286.689780	32.842215
715.821929	40348.899367	32.847232
716.404312	40408.085256	32.852250
717.191281	40471.761268	32.857268
717.962911	40524.498941	32.862285
718.420585	40588.523794	32.867303
719.348242	40650.192615	32.872320
719.956061	40705.302529	32.877338
720.801782	40765.650009	32.882356
721.412723	40823.966155	32.887373
722.234655	40880.839286	32.892391
723.118533	40935.268051	32.897408
723.327685	40998.156466	32.902426
724.509071	41054.917177	32.907444
725.063729	41110.820614	32.912461
725.766688	41171.368524	32.917479
726.907924	41217.915662	32.922496
727.695661	41276.711450	32.927514
727.954308	41330.738899	32.932532
728.842011	41363.412008	32.937549
729.421161	41420.134605	32.942567
730.192192	41465.588844	32.947584
730.690549	41522.982032	32.952602
731.391681	41571.350324	32.957620
732.169314	41623.786145	32.962637
732.378914	41699.964378	32.967655
733.908159	41750.752956	32.972672
734.823863	41794.427125	32.977690
735.265911	41849.021814	32.982708
735.873582	41898.524834	32.987725
736.591723	41959.692377	32.992743
737.346690	42012.872641	32.997760
738.281122	42070.193055	33.002778
738.959968	42135.294827	33.007796
739.991277	42182.126768	33.012813
740.479918	42256.429330	33.017831
741.292607	42310.499441	33.022848
741.733841	42365.038618	33.027866
742.138924	42430.082683	33.032884
743.462884	42488.184748	33.037901
744.127638	42551.468406	33.042919
744.728177	42601.132240	33.047936
745.808799	42657.982370	33.052954
746.587103	42713.918330	33.057972
747.729337	42766.875689	33.062989
748.639361	42827.193543	33.068007
748.801497	42875.167922	33.073024
750.045209	42929.912474	33.078042
750.722669	42988.862842	33.083060
751.404322	43038.141864	33.088077
751.926934	43097.356975	33.093095
752.793479	43139.523481	33.098112
754.101026	43197.554076	33.103130
754.439400	43263.882310	33.108148
755.162504	43309.259277	33.113165
755.664056	43367.694087	33.118183
756.414958	43424.439396	33.123200
757.183469	43482.023344	33.128218
757.620730	43541.151729	33.133236
758.795091	43605.099117	33.138253
759.359140	43662.171403	33.143271
759.929547	43721.551524	33.148288
761.162538	43783.725587	33.153306
761.342558	43855.184649	33.158324
762.174586	43906.814144	33.163341
762.573192	43981.041647	33.168359
763.230351	44054.931865	33.173376
764.117657	44119.633850	33.178394
765.034281	44200.391345	33.183412
765.690201	44263.472546	33.188429
766.200207	44338.537818	33.193447
766.894952	44408.963411	33.198464
767.855590	44487.564482	33.203482
768.451331	44558.999045	33.208500
769.774100	44618.137938	33.213517
770.380277	44700.046193	33.218535
771.401570	44765.968987	33.223552
772.126340	44839.908216	33.228570
772.544240	44902.205968	33.233588
773.567428	44972.518962	33.238605
774.226102	45040.883730	33.243623
774.879722	45091.031948	33.248640
775.809763	45183.695580	33.253658
776.814102	45251.823744	33.258676
777.725006	45310.237893	33.263693
778.404321	45376.411819	33.268711
779.296808	45433.045332	33.273728
780.265048	45489.705150	33.278746
781.087516	45552.466767	33.283764
781.803102	45595.059955	33.288781
782.319259	45658.774124	33.293799
783.482825	45711.570729	33.298816
783.753928	45764.031955	33.303834
784.317838	45822.824070	33.308852
784.830214	45880.808338	33.313869
785.595852	45949.956280	33.318887
786.688271	46020.173232	33.323904
787.778555	46078.789192	33.328922
788.425799	46137.493250	33.333940
789.001228	46212.339553	33.338957
789.767132	46278.844261	33.343975
790.558407	46344.408985	33.348992
791.574855	46410.799172	33.354010
792.134794	46486.597685	33.359028
793.072045	46553.854623	33.364045
793.757881	46610.535932	33.369063
794.983828	46687.673768	33.374080
795.981640	46745.021688	33.379098
796.340419	46820.928551	33.384116
797.404693	46876.729238	33.389133
798.273519	46949.526967	33.394151
798.981323	47015.112964	33.399168
799.541916	47081.063677	33.404186
800.412144	47151.508532	33.409204
801.265956	47226.460370	33.414221
801.912776	47293.834314	33.419239
802.823694	47358.048545	33.424256
804.154780	47424.652115	33.429274
804.828156	47495.172968	33.434292
805.396424	47561.693247	33.439309
806.248211	47635.590277	33.444327
806.858059	47697.094093	33.449344
807.668260	47761.015159	33.454362
808.207089	47836.631699	33.459380
809.038119	47913.000124	33.464397
810.038493	47998.433407	33.469415
810.717724	48065.874192	33.474432
811.795749	48133.404933	33.479450
812.554686	48210.171489	33.484468
812.916869	48279.338759	33.489485
814.168651	48364.734285	33.494503
814.919130	48432.247311	33.499520
815.860220	48504.507365	33.504538
816.285523	48579.252013	33.509556
817.308627	48654.080992	33.514573
818.252488	48726.834791	33.519591
818.994694	48808.350884	33.524608
820.176626	48878.537477	33.529626
820.593797	48950.678052	33.534644
821.931619	49019.518551	33.539661
822.871909	49087.870721	33.544679
823.435278	49163.013349	33.549696
824.325108	49233.980401	33.554714
824.880916	49307.081156	33.559732
826.057036	49373.512111	33.564749
826.864066	49441.797510	33.569767
827.476857	49508.715133	33.574784
828.516983	49578.818399	33.579802
829.405063	49662.352057	33.584820
830.090700	49727.000306	33.589837
830.855604	49797.994881	33.594855
831.849446	49872.256663	33.599872
832.642019	49930.435436	33.604890
833.024064	49995.169661	33.609908
833.870149	50056.681028	33.614925
834.880585	50122.690737	33.619943
835.586048	50184.224335	33.624960
836.463057	50250.894205	33.629978
837.140367	50323.662939	33.634996
837.538808	50391.692091	33.640013
838.489479	50468.208610	33.645031
839.067415	50539.221925	33.650048
839.873984	50611.977777	33.655066
840.711326	50701.774259	33.660084
841.517739	50770.563546	33.665101
842.708902	50854.351732	33.670119
843.159016	50927.695546	33.675136
844.402359	51013.203500	33.680154
845.166323	51090.491428	33.685172
846.378165	51168.178111	33.690189
847.180915	51229.743648	33.695207
848.107332	51311.069115	33.700224
849.122366	51385.642516	33.705242
849.658690	51461.366317	33.710260
850.559782	51545.271762	33.715277
851.740202	51609.867257	33.720295
852.104102	51696.375154	33.725312
853.275896	51769.653589	33.730330
854.142294	51843.973197	33.735348
855.008076	51919.103051	33.740365
855.952714	51993.265428	33.745383
856.734137	52070.515944	33.750400
858.095507	52146.885503	33.755418
858.717337	52235.013058	33.760436
859.533668	52302.590471	33.765453
860.510915	52369.554569	33.770471
861.018904	52446.190830	33.775488
861.979405	52514.024828	33.780506
863.150591	52602.814916	33.785524
864.113170	52672.528354	33.790541
864.975367	52745.902354	33.795559
865.674542	52830.122285	33.800576
866.937343	52898.916447	33.805594
867.829044	52970.426219	33.810612
868.628455	53033.275255	33.815629
869.759248	53101.584345	33.820647
870.937148	53177.903586	33.825664
871.519668	53245.108821	33.830682
872.367316	53321.024336	33.835700
872.893474	53384.150980	33.840717
873.915857	53455.034420	33.845735
874.563379	53531.399408	33.850752
875.938056	53606.322597	33.855770
876.396239	53677.440077	33.860788
877.721241	53751.245095	33.865805
878.680063	53808.009246	33.870823
879.560069	53884.124043	33.875840
880.390640	53953.039212	33.880858
880.975300	54019.461664	33.885876
881.933949	54091.204900	33.890893
882.938595	54157.290261	33.895911
883.600321	54228.504285	33.900928
884.279876	54299.279113	33.905946
885.232643	54371.226618	33.910964
886.433665	54444.445617	33.915981
887.378155	54510.636257	33.920999
888.094537	54580.798697	33.926016
889.234270	54646.067056	33.931034
890.020337	54720.326044	33.936052
890.773519	54789.496180	33.941069
891.943679	54858.367467	33.946087
892.294334	54917.418529	33.951104
893.193013	54975.644026	33.956122
893.888872	55046.526138	33.961140
894.310683	55117.894101	33.966157
895.368643	55192.162875	33.971175
895.845958	55271.072337	33.976192
896.613422	55350.379881	33.981210
897.618974	55425.980172	33.986228
898.215352	55503.865663	33.991245
899.571313	55585.215056	33.996263
900.274873	55666.514399	34.001280
901.192834	55742.521697	34.006298
902.122269	55830.380695	34.011316
902.863728	55912.358456	34.016333
904.039465	55990.845167	34.021351
904.771510	56077.489085	34.026368
905.503183	56171.328962	34.031386
906.332363	56250.560290	34.036404
906.996944	56345.012510	34.041421
908.119971	56443.064354	34.046439
908.962999	56530.705227	34.051456
910.271224	56612.755391	34.056474
911.414731	56705.970011	34.061492
911.897170	56794.047703	34.066509
912.935502	56869.115864	34.071527
913.899081	56965.264403	34.076544
915.402404	57052.374050	34.081562
916.760949	57142.120358	34.086580
917.049616	57221.293480	34.091597
918.387711	57300.847791	34.096615
919.063713	57378.132095	34.101632
920.307586	57460.587578	34.106650
921.443216	57542.617169	34.111668
922.375885	57623.355882	34.116685
923.407033	57691.427915	34.121703
924.321685	57774.714189	34.126720
925.421905	57861.028781	34.131738
925.990374	57926.186205	34.136756
926.911833	58008.769706	34.141773
927.857434	58091.191507	34.146791
928.932056	58170.321361	34.151808
929.762601	58244.457819	34.156826
931.162615	58314.626100	34.161844
932.113405	58397.453205	34.166861
932.764760	58475.156265	34.171879
933.548320	58551.794678	34.176896
934.666711	58624.216588	34.181914
935.409925	58712.399958	34.186932
936.551777	58796.774673	34.191949
937.516807	58865.784390	34.196967
938.216449	58954.355182	34.201984
939.063141	59030.219438	34.207002
940.162225	59107.810531	34.212020
940.750108	59188.361308	34.217037
942.065493	59262.121608	34.222055
942.819600	59353.495626	34.227072
943.900304	59435.242721	34.232090
944.873396	59513.120560	34.237108
945.895936	59590.066849	34.242125
946.896267	59672.346270	34.247143
948.158664	59752.066030	34.252160
948.805800	59827.153663	34.257178
949.732275	59908.097187	34.262196
950.389567	59986.082665	34.267213
951.455723	60062.213473	34.272231
952.322549	60144.762126	34.277248
953.587666	60239.307019	34.282266
953.943814	60305.231797	34.287284
954.831545	60379.074715	34.292301
955.754872	60438.448969	34.297319
956.634144	60523.212357	34.302336
957.596453	60600.019298	34.307354
958.482449	60680.376691	34.312372
958.870031	60765.084528	34.317389
960.703742	60842.630098	34.322407
961.549387	60936.261864	34.327424
962.278654	61023.341728	34.332442
963.501635	61090.583224	34.337460
964.324796	61182.807873	34.342477
965.400060	61257.637031	34.347495
965.989547	61339.872082	34.352512
967.218779	61425.166468	34.357530
968.255161	61509.478374	34.362548
968.918628	61588.138969	34.367565
969.824865	61676.674818	34.372583
970.721555	61758.103847	34.377600
972.051629	61850.600246	34.382618
972.965917	61934.666752	34.387636
973.678420	62030.013538	34.392653
975.312983	62103.099722	34.397671
976.337067	62197.056668	34.402688
977.441328	62263.446293	34.407706
978.691596	62348.930509	34.412724
979.609141	62434.283237	34.417741
981.267311	62502.366070	34.422759
982.124019	62571.054945	34.427776
982.842717	62650.216747	34.432794
983.991671	62725.697240	34.437812
984.555606	62806.732073	34.442829
985.377594	62884.732762	34.447847
986.468403	62970.826337	34.452864
987.304547	63062.644518	34.457882
988.739811	63134.929170	34.462900
989.496865	63223.803969	34.467917
990.622092	63307.715696	34.472935
991.394331	63393.309577	34.477952
992.388513	63477.204292	34.482970
993.603949	63572.390098	34.487988
994.213922	63653.800355	34.493005
995.513116	63731.039392	34.498023
996.319634	63821.598877	34.503040
996.975778	63917.689703	34.508058
998.007141	63996.041119	34.513076
998.954005	64092.992641	34.518093
1000.054678	64177.139020	34.523111
1000.970237	64269.253155	34.528128
1001.831587	64364.079273	34.533146
1002.995900	64461.935319	34.538164
1003.874535	64560.456629	34.543181
1005.297300	64642.522269	34.548199
1006.373690	64731.473010	34.553216
1007.050076	64826.690524	34.558234
1008.079684	64917.687728	34.563252
1009.011661	65017.443372	34.568269
1010.206888	65110.719927	34.573287
1011.502110	65200.423296	34.578304
1012.232146	65285.935255	34.583322
1013.790311	65380.973294	34.588340
1014.369419	65470.099019	34.593357
1015.531965	65550.587402	34.598375
1016.641842	65638.010369	34.603392
1017.524608	65731.838012	34.608410
1019.030644	65806.157963	34.613428
1019.990312	65892.332650	34.618445
1020.648998	65978.782400	34.623463
1021.675166	66062.199617	34.628480
1022.948544	66144.603634	34.633498
1023.672940	66216.988843	34.638516
1024.555850	66300.283527	34.643533
1025.595291	66374.817067	34.648551
1026.431691	66449.287462	34.653568
1026.850637	66538.188631	34.658586
1028.094450	66615.755386	34.663604
1028.804881	66712.671486	34.668621
1029.874656	66805.669924	34.673639
1030.633049	66892.639098	34.678656
1031.630856	66992.056723	34.683674
1032.483009	67086.223372	34.688692
1033.462124	67188.658409	34.693709
1034.584686	67293.908007	34.698727
1035.608977	67394.127169	34.703744
1036.928006	67500.182787	34.708762
1038.002791	67594.000083	34.713780
1039.077248	67702.671533	34.718797
1040.044854	67806.275839	34.723815
1041.252906	67906.107507	34.728832
1041.935163	68005.318600	34.733850
1043.494287	68109.249943	34.738868
1044.339546	68207.429717	34.743885
1045.673654	68311.821128	34.748903
1046.763644	68407.139644	34.753920
1047.595694	68518.441950	34.758938
1048.809898	68614.235773	34.763956
1049.821191	68726.853412	34.768973
1050.880178	68836.513497	34.773991
1051.812536	68929.927285	34.779008
1052.671627	69034.047317	34.784026
1054.202875	69136.739780	34.789044
1055.364395	69238.261813	34.794061
1056.371930	69331.386749	34.799079
1057.865644	69434.839740	34.804096
1058.312900	69536.911031	34.809114
1059.944922	69641.476744	34.814132
1061.256534	69742.508826	34.819149
1061.925047	69843.565421	34.824167
1063.283197	69937.093868	34.829184
1064.362159	70046.509025	34.834202
1065.407280	70136.350977	34.839220
1066.311446	70231.698818	34.844237
1067.190046	70338.638863	34.849255
1068.554979	70433.295169	34.854272
1069.562495	70534.770265	34.859290
1070.829768	70630.037717	34.864308
1072.233905	70728.019754	34.869325
1073.451782	70827.538237	34.874343
1074.944904	70917.401802	34.879360
1075.895416	71003.981336	34.884378
1077.078058	71099.643618	34.889396
1078.033540	71184.475246	34.894413
1079.090090	71268.379551	34.899431
1080.501366	71354.356604	34.904448
1081.165795	71437.499273	34.909466
1082.559799	71523.656878	34.914484
1083.789763	71612.461949	34.919501
1084.582797	71690.785383	34.924519
1085.712726	71780.201847	34.929536
1086.782781	71878.024889	34.934554
1087.449071	71954.481740	34.939572
1088.734765	72037.656258	34.944589
1089.502792	72133.361520	34.949607
1090.672413	72224.280477	34.954624
1091.700966	72314.879744	34.959642
1092.635776	72413.257770	34.964660
1093.525270	72507.691614	34.969677
1094.348662	72596.322650	34.974695
1095.360541	72686.773804	34.979712
1096.315598	72777.373433	34.984730
1097.121585	72862.145086	34.989748
1098.146357	72962.955610	34.994765
1099.171095	73067.718209	34.999783
1100.907021	73159.958129	35.004800
1101.757925	73252.108146	35.009818
1103.020770	73347.208821	35.014836
1103.729727	73452.820040	35.019853
1104.933559	73550.311807	35.024871
1106.050635	73652.351842	35.029888
1106.777241	73749.779299	35.034906
1108.125508	73852.974720	35.039924
1109.128783	73952.183761	35.044941
1110.571316	74072.413912	35.049959
1111.609562	74172.656953	35.054976
1112.675073	74276.860659	35.059994
1113.790215	74377.269828	35.065012
1114.816816	74487.078908	35.070029
1116.032988	74599.594871	35.075047
1117.399095	74696.913577	35.080064
1118.060709	74817.344633	35.085082
1119.327084	74919.796935	35.090100
1120.719495	75022.179345	35.095117
1121.624594	75142.434627	35.100135
1122.843510	75253.850912	35.105152
1124.009228	75365.896609	35.110170
1124.974678	75466.966497	35.115188
1125.916097	75580.846688	35.120205
1127.142722	75696.253663	35.125223
1128.785567	75804.452181	35.130240
1129.912036	75921.535081	35.135258
1131.021283	76022.762008	35.140276
1132.442992	76132.946992	35.145293
1133.877243	76239.140318	35.150311
1135.202733	76338.396693	35.155328
1136.506971	76444.053704	35.160346
1137.169104	76552.838559	35.165364
1138.344290	76655.590334	35.170381
1139.821699	76755.546630	35.175399
1140.873758	76848.273054	35.180416
1141.985921	76959.282296	35.185434
1143.282969	77065.652226	35.190452
1144.425135	77164.420790	35.195469
1145.393394	77267.397102	35.200487
1146.166126	77365.349831	35.205504
1147.161488	77480.800402	35.210522
1148.447138	77591.975234	35.215540
1149.753695	77694.469796	35.220557
1150.930916	77816.962133	35.225575
1152.378488	77914.431754	35.230592
1153.457784	78013.897247	35.235610
1154.345860	78118.206717	35.240628
1155.779680	78225.167942	35.245645
1156.823590	78336.522777	35.250663
1158.206625	78441.440513	35.255680
1159.043304	78554.399342	35.260698
1160.442222	78646.938531	35.265716
1161.610199	78751.498209	35.270733
1162.332072	78873.458061	35.275751
1163.605758	78972.643401	35.280768
1164.980633	79083.227643	35.285786
1166.158973	79180.021560	35.290804
1167.595981	79278.207102	35.295821
1168.153454	79384.067721	35.300839
1169.995973	79491.920401	35.305856
1171.320991	79592.632888	35.310874
1172.773493	79680.555797	35.315892
1174.116742	79763.770532	35.320909
1174.779051	79855.706311	35.325927
1176.279136	79925.936913	35.330944
1177.289879	80019.123892	35.335962
1178.229223	80106.722623	35.340980
1179.408838	80197.261443	35.345997
1180.125093	80291.027268	35.351015
1181.309986	80378.347924	35.356032
1182.391153	80470.106517	35.361050
1183.467066	80575.396887	35.366068
1184.786841	80671.730578	35.371085
1185.331148	80779.080857	35.376103
1186.769247	80878.386787	35.381120
1187.987170	80987.482735	35.386138
1189.133035	81098.326031	35.391156
1190.005135	81206.969887	35.396173
1191.309774	81317.751330	35.401191
1192.375162	81428.709816	35.406208
1193.526253	81542.493390	35.411226
1194.489028	81656.952889	35.416244
1196.242564	81773.367602	35.421261
1197.108488	81902.603378	35.426279
1198.161207	82010.145299	35.431296
1199.370282	82137.086184	35.436314
1200.567331	82255.401300	35.441332
1201.843881	82366.584016	35.446349
1203.091550	82498.981278	35.451367
1204.309346	82611.985919	35.456384
1205.235676	82745.676020	35.461402
1206.520507	82876.498167	35.466420
1208.451033	82997.515005	35.471437
1209.924349	83117.944670	35.476455
1211.242960	83229.884450	35.481472
1212.316126	83352.620047	35.486490
1213.497274	83461.604592	35.491508
1215.539086	83586.483779	35.496525
1216.386033	83700.944238	35.501543
1217.472969	83807.385318	35.506560
1218.956785	83913.841044	35.511578
1219.629673	84021.943875	35.516596
1220.992379	84131.447561	35.521613
1222.399873	84251.208046	35.526631
1223.515591	84363.830072	35.531648
1224.729057	84495.228282	35.536666
1225.589426	84610.894031	35.541684
1227.248442	84714.284437	35.546701
1228.469109	84842.515365	35.551719
1229.695622	84955.198495	35.556736
1231.416190	85060.760000	35.561754
1232.492482	85171.883466	35.566772
1234.468792	85271.995335	35.571789
1235.367397	85392.169242	35.576807
1236.801090	85497.181450	35.581824
1238.002899	85603.877415	35.586842
1238.942760	85715.581753	35.591860
1240.204245	85818.265044	35.596877
1241.504641	85924.034498	35.601895
1242.557343	86034.265277	35.606912
1243.758267	86137.212557	35.611930
1245.027453	86250.806460	35.616948
1246.473706	86361.395391	35.621965
1247.286743	86477.696902	35.626983
1248.688068	86591.258897	35.632000
1250.105140	86707.340590	35.637018
1250.950429	86825.007031	35.642036
1252.856703	86921.853481	35.647053
1253.973455	87030.620791	35.652071
1254.626318	87129.551156	35.657088
1256.251197	87218.243567	35.662106
1257.443568	87310.931931	35.667124
1258.165389	87415.263534	35.672141
1259.449332	87521.915739	35.677159
1260.732873	87626.376091	35.682176
1261.862680	87730.645314	35.687194
1262.866282	87830.866722	35.692212
1264.462932	87944.745732	35.697229
1265.419916	88055.607321	35.702247
1266.595476	88171.707072	35.707264
1268.024126	88282.115925	35.712282
1268.904884	88402.596488	35.717300
1270.308511	88517.901748	35.722317
1271.239355	88638.071332	35.727335
1272.996127	88767.085168	35.732352
1274.091837	88878.587243	35.737370
1275.317577	89003.743521	35.742388
1276.714426	89121.941607	35.747405
1278.233787	89252.059037	35.752423
1279.122546	89387.623210	35.757440
1280.321438	89512.747796	35.762458
1282.126178	89624.319737	35.767476
1283.251132	89746.301205	35.772493
1284.641887	89874.223569	35.777511
1286.121623	90007.113237	35.782528
1287.319763	90118.337882	35.787546
1288.796115	90251.153124	35.792564
1290.190883	90371.130773	35.797581
1291.324540	90489.147132	35.802599
1292.548390	90625.627960	35.807616
1294.075587	90753.241358	35.812634
1295.183452	90873.392411	35.817652
1296.847767	91001.834659	35.822669
1297.961795	91132.074068	35.827687
1299.240468	91255.406526	35.832704
1300.614619	91377.609328	35.837722
1301.918114	91495.666575	35.842740
1303.141817	91631.721078	35.847757
1304.704973	91756.025223	35.852775
1306.028625	91886.336653	35.857792
1307.588257	92003.101282	35.862810
1308.190917	92133.095075	35.867828
1309.966262	92254.922124	35.872845
1311.366815	92392.486102	35.877863
1312.407430	92515.632617	35.882880
1314.091740	92633.660376	35.887898
1315.099965	92766.952470	35.892916
1316.538469	92891.965094	35.897933
1317.804717	93018.880876	35.902951
1319.024051	93147.097298	35.907968
1320.685524	93270.885355	35.912986
1321.562869	93398.268835	35.918004
1323.045865	93520.488668	35.923021
1324.429093	93655.450038	35.928039
1325.686894	93776.983481	35.933056
1327.016061	93904.742359	35.938074
1328.155917	94034.914131	35.943092
1329.927393	94158.397127	35.948109
1331.440522	94297.967486	35.953127
1332.373317	94430.353274	35.958144
1334.000520	94545.862266	35.963162
1335.225530	94682.310412	35.968180
1336.777692	94790.391632	35.973197
1338.165307	94911.617813	35.978215
1339.074065	95041.348137	35.983232
1340.984179	95170.593583	35.988250
1341.966211	95275.634401	35.993268
1343.352981	95387.432014	35.998285
1344.846482	95501.469670	36.003303
1346.177291	95612.871186	36.008320
1347.719352	95713.782794	36.013338
1348.473311	95833.767582	36.018356
1349.911003	95944.557890	36.023373
1351.078703	96062.374984	36.028391
1352.021218	96184.131735	36.033408
1353.435852	96293.304359	36.038426
1354.747334	96424.967877	36.043444
1355.918498	96538.501753	36.048461
1357.317875	96672.218817	36.053479
1358.459632	96808.004727	36.058496
1359.791776	96931.136134	36.063514
1360.962323	97073.522987	36.068532
1362.711594	97201.559604	36.073549
1364.010298	97333.938791	36.078567
1365.565047	97455.402354	36.083584
1367.291286	97593.420451	36.088602
1368.511073	97736.018128	36.093620
1369.920568	97864.756821	36.098637
1371.544826	97994.552796	36.103655
1372.499891	98128.446601	36.108672
1374.307880	98254.652908	36.113690
1375.974634	98393.824652	36.118708
1377.455327	98514.619259	36.123725
1378.865012	98635.361992	36.128743
1380.319499	98767.279226	36.133760
1381.679253	98876.405936	36.138778
1382.815526	99024.752367	36.143796
1384.641972	99145.242007	36.148813
1386.505444	99265.777046	36.153831
1387.821302	99394.320985	36.158848
1389.489052	99510.209545	36.163866
1390.499245	99633.502955	36.168884
1391.887717	99763.279439	36.173901
1393.400457	99884.391162	36.178919
1394.328470	100016.205321	36.183936
1395.734625	100136.941585	36.188954
1396.850070	100271.567359	36.193972
1398.363242	100402.227107	36.198989
1399.935202	100526.869059	36.204007
1400.959820	100676.546274	36.209024
1402.336925	100803.805859	36.214042
1403.234685	100945.403014	36.219060
1404.841120	101080.843172	36.224077
1406.722022	101223.759143	36.229095
1407.952925	101360.146365	36.234112
1409.943627	101493.677458	36.239130
1411.298946	101633.203269	36.244148
1412.813854	101751.152128	36.249165
1414.640341	101888.070081	36.254183
1415.676629	102024.477690	36.259200
1417.279533	102142.211412	36.264218
1418.780965	102272.994601	36.269236
1419.816992	102407.388000	36.274253
1421.570042	102541.011071	36.279271
1422.621058	102672.588624	36.284288
1424.516431	102797.252302	36.289306
1425.652736	102934.003115	36.294324
1426.885200	103066.657029	36.299341
1428.157619	103202.538304	36.304359
1429.314003	103345.690399	36.309376
1430.522699	103479.845752	36.314394
1432.140535	103613.620998	36.319412
1433.621076	103749.383371	36.324429
1434.924870	103884.628617	36.329447
1435.951637	104029.109757	36.334464
1437.275667	104162.248277	36.339482
1438.709820	104289.651945	36.344500
1440.091178	104420.589101	36.349517
1441.842844	104549.174211	36.354535
1442.970608	104694.175032	36.359552
1444.666387	104817.863029	36.364570
1445.917398	104956.747093	36.369588
1447.192578	105093.396406	36.374605
1448.362001	105234.399086	36.379623
1449.716319	105388.116423	36.384640
1450.964528	105518.457295	36.389658
1452.584155	105673.554743	36.394676
1453.869690	105833.092049	36.399693
1455.433796	105974.366062	36.404711
1456.512180	106142.052055	36.409728
1458.269183	106286.974470	36.414746
1459.313494	106453.919200	36.419764
1461.061623	106610.611277	36.424781
1462.769768	106765.890143	36.429799
1464.200783	106930.976468	36.434816
1465.331984	107080.577155	36.439834
1467.165621	107245.995419	36.444852
1468.694927	107404.969588	36.449869
1470.956814	107561.725550	36.454887
1472.222833	107720.488555	36.459904
1473.504572	107862.904849	36.464922
1475.366902	108022.793753	36.469940
1476.680320	108170.823820	36.474957
1478.957435	108314.545312	36.479975
1480.435208	108462.614452	36.484992
1482.242696	108611.698082	36.490010
1483.774873	108747.941618	36.495028
1485.324372	108900.401668	36.500045
1486.966745	109035.589362	36.505063
1488.178660	109174.826367	36.510080
1489.954664	109312.923618	36.515098
1491.656651	109458.210354	36.520116
1492.547862	109603.877509	36.525133
1494.410439	109747.707503	36.530151
1495.579648	109891.455791	36.535168
1496.962701	110039.229357	36.540186
1498.335422	110189.160961	36.545204
1499.957045	110342.808121	36.550221
1501.592896	110493.448265	36.555239
1502.796819	110645.842903	36.560256
1504.610906	110804.560040	36.565274
1506.071521	110951.589844	36.570292
1507.241299	111105.120433	36.575309
1508.786937	111261.814314	36.580327
1509.888058	111422.141620	36.585344
1511.677933	111570.390912	36.590362
1513.403442	111737.102814	36.595380
1514.660379	111889.190189	36.600397
1516.349140	112042.846964	36.605415
1517.635756	112202.400683	36.610432
1519.120219	112354.505356	36.615450
1520.701400	112517.007582	36.620468
1522.062413	112693.723408	36.625485
1524.013226	112841.775383	36.630503
1525.141133	113002.574854	36.635520
1526.780515	113162.534499	36.640538
1528.620057	113320.789633	36.645556
1529.813848	113487.338791	36.650573
1531.293259	113640.261362	36.655591
1532.782245	113811.116143	36.660608
1534.417094	113964.764159	36.665626
1536.241782	114126.588928	36.670644
1537.656520	114269.340082	36.675661
1539.594251	114418.453214	36.680679
1540.881447	114561.656577	36.685696
1542.225153	114706.487790	36.690714
1543.912384	114850.340260	36.695732
1545.131582	114983.511034	36.700749
1547.114116	115125.479602	36.705767
1548.544400	115264.883927	36.710784
1550.056150	115402.982429	36.715802
1551.617988	115545.221029	36.720820
1552.545684	115694.788276	36.725837
1554.093416	115850.626595	36.730855
1555.558581	116006.567206	36.735872
1557.009536	116156.042195	36.740890
1558.872945	116309.816671	36.745908
1560.081993	116473.396447	36.750925
1561.695305	116630.508867	36.755943
1563.300124	116793.001090	36.760960
1564.783972	116956.971462	36.765978
1566.313539	117123.916095	36.770996
1567.622779	117299.254324	36.776013
1569.308452	117463.487232	36.781031
1571.316247	117643.360604	36.786048
1572.765151	117800.630372	36.791066
1574.673392	117964.615207	36.796084
1575.961328	118140.873926	36.801101
1577.923552	118300.399741	36.806119
1579.645490	118469.438648	36.811136
1580.954367	118638.796283	36.816154
1582.673923	118807.050651	36.821172
1583.944486	118983.683841	36.826189
1585.658101	119160.426474	36.831207
1587.562753	119331.850807	36.836224
1589.047752	119499.510525	36.841242
1590.794926	119660.521553	36.846260
1592.445867	119840.752643	36.851277
1594.072356	120004.396918	36.856295
1595.258142	120181.771864	36.861312
1596.707283	120363.076957	36.866330
1598.483292	120540.272899	36.871348
1600.257186	120723.457229	36.876365
1602.135043	120899.192894	36.881383
1603.711528	121070.333569	36.886400
1604.951179	121247.438640	36.891418
1606.860441	121416.930738	36.896436
1608.362603	121595.835874	36.901453
1610.096088	121778.118143	36.906471
1611.947788	121951.617360	36.911488
1613.502740	122124.605380	36.916506
1615.081754	122291.742471	36.921524
1616.375077	122475.035208	36.926541
1618.095930	122652.985103	36.931559
1619.635004	122833.260175	36.936576
1621.209272	123013.010484	36.941594
1622.807393	123193.366809	36.946612
1624.116028	123383.651173	36.951629
1625.948749	123572.535561	36.956647
1627.585421	123757.353839	36.961664
1629.040743	123932.839021	36.966682
1630.866417	124117.375836	36.971700
1632.263774	124314.425129	36.976717
1634.012890	124496.501839	36.981735
1635.755705	124682.157841	36.986752
1637.225772	124870.102604	36.991770
1639.073856	125057.405843	36.996788
1640.488944	125259.645681	37.001805
1642.101045	125431.345183	37.006823
1643.550603	125619.880201	37.011840
1644.961778	125804.146729	37.016858
1646.874523	125977.831588	37.021876
1648.212147	126157.480584	37.026893
1649.779313	126338.553609	37.031911
1651.239656	126509.951433	37.036928
1652.732455	126700.539964	37.041946
1654.280674	126873.879393	37.046964
1656.116358	127064.758792	37.051981
1657.383522	127249.206488	37.056999
1659.320701	127442.837590	37.062016
1660.622368	127644.129984	37.067034
1662.356487	127814.907028	37.072052
1664.217734	128016.482064	37.077069
1666.207225	128208.256279	37.082087
1667.938276	128397.775207	37.087104
1669.132282	128584.676181	37.092122
1671.038878	128777.620462	37.097140
1672.526742	128985.297486	37.102157
1674.397055	129189.642636	37.107175
1676.758133	129382.328650	37.112192
1677.948254	129583.584311	37.117210
1679.874966	129773.129747	37.122228
1681.287998	129976.661742	37.127245
1682.826960	130181.494645	37.132263
1684.948723	130374.336616	37.137280
1686.119182	130584.836848	37.142298
1688.119126	130797.568982	37.147316
1689.487962	130998.625893	37.152333
1691.200382	131213.764821	37.157351
1693.060543	131427.143553	37.162368
1695.103902	131623.923999	37.167386
1697.207958	131818.818030	37.172404
1699.618406	132019.857165	37.177421
1701.239841	132224.369774	37.182439
1703.004286	132415.462071	37.187456
1704.601253	132615.057203	37.192474
1706.065469	132801.135200	37.197492
1707.748892	133004.702869	37.202509
1709.448157	133200.770003	37.207527
1711.327234	133406.872202	37.212544
1713.096591	133610.327795	37.217562
1714.556835	133813.540592	37.222580
1716.241848	134025.297053	37.227597
1717.636836	134234.853715	37.232615
1719.257446	134437.016605	37.237632
1720.812171	134661.421976	37.242650
1722.642375	134866.295040	37.247668
1724.405150	135074.504114	37.252685
1726.239993	135281.814690	37.257703
1728.362225	135504.460976	37.262720
1729.512817	135719.887043	37.267738
1731.291103	135925.242526	37.272756
1733.062533	136151.677306	37.277773
1734.804943	136370.618186	37.282791
1736.370562	136589.460740	37.287808
1737.753770	136803.041126	37.292826
1739.512788	137026.385900	37.297844
1741.557786	137257.136185	37.302861
1743.385331	137476.792435	37.307879
1745.513533	137681.847566	37.312896
1747.384635	137881.334641	37.317914
1749.874438	138085.421606	37.322932
1752.028578	138296.985431	37.327949
1753.676680	138489.631788	37.332967
1755.856388	138678.186095	37.337984
1757.484257	138879.009714	37.343002
1759.231473	139079.308008	37.348020
1760.881488	139282.058840	37.353037
1762.521901	139465.218005	37.358055
1764.257952	139644.796972	37.363072
1765.484181	139823.732610	37.368090
1766.882089	140011.804803	37.373108
1768.079839	140198.550997	37.378125
1769.774557	140393.596429	37.383143
1771.357209	140597.518235	37.388160
1772.561985	140813.847865	37.393178
1774.095484	141017.753732	37.398196
1775.728781	141235.224201	37.403213
1777.256492	141457.661562	37.408231
1778.812231	141678.864557	37.413248
1780.330169	141916.585546	37.418266
1782.036980	142154.976318	37.423284
1783.697484	142388.933542	37.428301
1785.273866	142640.583921	37.433319
1787.293912	142870.895866	37.438336
1788.853552	143123.300119	37.443354
1790.427438	143375.284631	37.448372
1792.549497	143635.980343	37.453389
1794.024095	143877.766188	37.458407
1795.628472	144137.466321	37.463424
1797.806515	144400.226072	37.468442
1799.448163	144662.258412	37.473460
1801.156085	144931.579625	37.478477
1802.550312	145203.070653	37.483495
1804.523128	145465.220628	37.488512
1806.670107	145748.464443	37.493530
1808.836174	146002.641887	37.498548
1811.463849	146247.623073	37.503565
1813.222112	146512.286811	37.508583
1815.312825	146774.488632	37.513600
1816.915942	147032.338035	37.518618
1819.189931	147283.230394	37.523636
1821.100264	147542.963779	37.528653
1822.539384	147799.636735	37.533671
1824.348163	148051.087521	37.538688
1826.168981	148316.905769	37.543706
1827.908130	148584.261204	37.548724
1829.945847	148840.147988	37.553741
1831.886596	149103.577981	37.558759
1833.849263	149360.329382	37.563776
1835.649137	149632.833994	37.568794
1837.408862	149904.102323	37.573812
1839.494191	150162.945542	37.578829
1841.233901	150426.413347	37.583847
1843.074164	150686.477688	37.588864
1844.819480	150959.517934	37.593882
1846.864756	151240.801647	37.598900
1848.360936	151507.638268	37.603917
1850.046392	151782.240546	37.608935
1851.929957	152046.518874	37.613952
1853.778729	152326.036245	37.618970
1855.717203	152608.333679	37.623988
1857.284488	152879.862536	37.629005
1859.049075	153150.460745	37.634023
1860.697027	153432.934503	37.639040
1862.067735	153716.138302	37.644058
1864.281481	154003.160153	37.649076
1866.474170	154287.889107	37.654093
1867.959386	154576.118929	37.659111
1870.182011	154856.745856	37.664128
1871.810775	155143.699466	37.669146
1873.594501	155431.125468	37.674164
1875.417585	155726.201492	37.679181
1877.109417	156008.414566	37.684199
1879.808249	156294.306027	37.689216
1882.000025	156565.691726	37.694234
1884.152913	156832.451189	37.699252
1886.013339	157086.727713	37.704269
1888.148533	157343.641157	37.709287
1890.022190	157591.824310	37.714304
1891.321437	157841.837087	37.719322
1893.083942	158109.056576	37.724340
1895.127977	158357.203688	37.729357
1896.597267	158627.682936	37.734375
1898.568788	158890.557049	37.739392
1899.597571	159158.377778	37.744410
1901.449681	159439.960075	37.749428
1903.294869	159715.565281	37.754445
1904.909013	160006.454736	37.759463
1906.709720	160300.287237	37.764480
1908.419531	160591.164544	37.769498
1910.266201	160900.646180	37.774516
1911.930022	161188.588069	37.779533
1914.122446	161495.276583	37.784551
1915.669599	161801.178313	37.789568
1917.551634	162110.888895	37.794586
1919.507569	162422.227232	37.799604
1921.323305	162741.561893	37.804621
1923.106095	163066.375199	37.809639
1925.334186	163378.856512	37.814656
1927.090300	163700.541229	37.819674
1929.066156	164025.354654	37.824692
1931.389084	164340.885553	37.829709
1932.951766	164673.028670	37.834727
1935.206101	164998.032054	37.839744
1937.234467	165325.522579	37.844762
1939.184241	165654.360052	37.849780
1941.237944	165982.649695	37.854797
1942.945411	166314.714892	37.859815
1945.154166	166643.034366	37.864832
1947.674723	166965.314059	37.869850
1949.344949	167295.117080	37.874868
1951.651235	167616.811007	37.879885
1953.576836	167950.259443	37.884903
1955.314151	168276.412654	37.889920
1957.576782	168603.514065	37.894938
1959.201483	168933.433421	37.899956
1961.140399	169268.917498	37.904973
1962.815899	169608.723064	37.909991
1964.871499	169953.194422	37.915008
1966.993670	170292.400385	37.920026
1968.928217	170639.814182	37.925044
1970.831118	170971.096189	37.930061
1972.811195	171313.477905	37.935079
1974.674179	171655.574673	37.940096
1976.730684	171998.074595	37.945114
1978.516425	172346.598773	37.950132
1980.417081	172680.415478	37.955149
1982.565235	173031.514789	37.960167
1984.751552	173386.241319	37.965184
1986.143412	173734.883876	37.970202
1988.275688	174089.799787	37.975220
1990.702537	174440.874769	37.980237
1992.811012	174792.965903	37.985255
1994.612656	175136.357388	37.990272
1996.513707	175499.962945	37.995290
1998.664985	175840.877676	38.000308
2000.834179	176188.343321	38.005325
2003.093162	176538.132944	38.010343
2005.022869	176877.867432	38.015360
2006.758025	177229.214497	38.020378
2008.640558	177580.438510	38.025396
2010.988932	177927.451781	38.030413
2012.807497	178284.453774	38.035431
2014.547529	178630.523300	38.040448
2016.367075	178960.149813	38.045466
2018.160302	179299.686638	38.050484
2020.763402	179620.888768	38.055501
2022.356388	179953.195612	38.060519
2024.400134	180289.040012	38.065536
2026.891755	180613.488581	38.070554
2028.604330	180951.241032	38.075572
2030.914942	181274.932813	38.080589
2032.915832	181612.439660	38.085607
2035.349925	181939.416307	38.090624
2037.356008	182270.956197	38.095642
2039.352254	182613.140671	38.100660
2041.365902	182940.008462	38.105677
2043.139801	183280.248879	38.110695
2044.914409	183636.821661	38.115712
2046.799605	183980.933214	38.120730
2048.122825	184341.261638	38.125748
2050.316758	184698.763597	38.130765
2052.232469	185073.987795	38.135783
2054.223954	185442.445470	38.140800
2056.114151	185823.848400	38.145818
2058.223464	186188.328187	38.150836
2060.152208	186561.854116	38.155853
2061.979328	186987.008766	38.160871
2063.843772	187418.356807	38.165888
2066.551290	187804.668905	38.170906
2068.248177	188194.873434	38.175924
2069.920614	188584.752977	38.180941
2072.327075	188976.627861	38.185959
2074.485430	189369.152346	38.190976
2076.775298	189766.610750	38.195994
2079.009962	190146.629253	38.201012
2081.595633	190539.853306	38.206029
2083.603299	190937.537505	38.211047
2085.816973	191322.109797	38.216064
2088.240706	191698.878108	38.221082
2090.378085	192095.707805	38.226100
2092.857680	192473.663678	38.231117
2094.647037	192868.721217	38.236135
2096.702741	193259.649039	38.241152
2098.784488	193647.805335	38.246170
2100.671251	194043.943662	38.251188
2102.368607	194451.593955	38.256205
2104.631990	194854.331225	38.261223
2106.665386	195252.939728	38.266240
2108.923446	195656.493105	38.271258
2110.893562	196066.366630	38.276276
2112.829970	196468.931021	38.281293
2115.193536	196878.593321	38.286311
2117.134259	197275.647243	38.291328
2119.469149	197685.722763	38.296346
2121.431399	198103.350940	38.301364
2123.977086	198500.822105	38.306381
2126.481084	198901.780870	38.311399
2128.078658	199315.862136	38.316416
2130.606699	199708.182632	38.321434
2132.528077	200117.033646	38.326452
2134.958094	200515.772727	38.331469
2136.876569	200925.769358	38.336487
2139.283202	201331.626688	38.341504
2141.310262	201732.031785	38.346522
2143.162217	202136.021411	38.351540
2145.605271	202541.393333	38.356557
2148.081429	202948.488410	38.361575
2150.053738	203355.281794	38.366592
2151.913191	203747.919017	38.371610
2154.320298	204146.746294	38.376628
2156.353808	204546.699473	38.381645
2158.413043	204931.560260	38.386663
2160.346013	205319.997846	38.391680
2162.508259	205690.440708	38.396698
2164.887524	206078.226044	38.401716
2167.049373	206462.108491	38.406733
2168.769107	206847.483012	38.411751
2170.614295	207241.374114	38.416768
2172.837469	207627.687793	38.421786
2174.613997	208030.583670	38.426804
2176.646283	208448.148878	38.431821
2178.450442	208845.580195	38.436839
2180.300033	209270.643825	38.441856
2182.711407	209691.530832	38.446874
2184.568909	210126.374955	38.451892
2186.547449	210541.411748	38.456909
2188.398701	210984.082500	38.461927
2190.376730	211430.062090	38.466944
2192.576792	211869.580746	38.471962
2195.219578	212308.345269	38.476980
2197.415343	212758.738623	38.481997
2199.734781	213207.004883	38.487015
2201.500777	213664.808049	38.492032
2204.080025	214103.788178	38.497050
2206.309859	214575.339977	38.502068
2208.482946	215029.423455	38.507085
2211.181429	215485.254786	38.512103
2213.461661	215943.971558	38.517120
2215.800004	216392.467463	38.522138
2218.059743	216856.828067	38.527156
2220.294119	217314.029204	38.532173
2222.910009	217766.751127	38.537191
2225.199131	218228.314067	38.542208
2227.558348	218677.316953	38.547226
2229.726658	219150.991743	38.552244
2231.525892	219609.964630	38.557261
2234.071606	220068.872476	38.562279
2235.815659	220536.237897	38.567296
2237.967677	221014.158996	38.572314
2239.950657	221485.095159	38.577332
2242.200765	221960.689737	38.582349
2244.716703	222442.263926	38.587367
2246.825839	222927.890058	38.592384
2249.454968	223401.622538	38.597402
2252.105956	223877.993778	38.602420
2254.089679	224345.602946	38.607437
2256.995948	224818.886161	38.612455
2259.589867	225286.781567	38.617472
2262.163466	225736.135176	38.622490
2264.092727	226207.792249	38.627508
2266.541119	226682.772664	38.632525
2268.861428	227143.648290	38.637543
2270.730330	227615.924326	38.642560
2273.035240	228082.187857	38.647578
2275.337230	228566.463215	38.652596
2277.186272	229045.728096	38.657613
2279.681298	229519.938476	38.662631
2281.227670	230002.933666	38.667648
2283.575195	230489.792373	38.672666
2285.795938	230982.843720	38.677684
2287.825174	231459.691410	38.682701
2290.015842	231969.310209	38.687719
2291.858365	232465.823548	38.692736
2294.484330	232967.981260	38.697754
2296.525810	233462.506705	38.702772
2298.968090	233953.641410	38.707789
2301.566352	234449.120830	38.712807
2303.585786	234956.324774	38.717824
2306.199535	235447.786908	38.722842
2308.469466	235934.322840	38.727860
2310.560108	236402.239737	38.732877
2313.152597	236868.502938	38.737895
2315.532753	237346.763737	38.742912
2317.979410	237812.794386	38.747930
2320.261053	238275.776243	38.752948
2323.001886	238733.351235	38.757965
2325.995919	239195.585819	38.762983
2328.024711	239659.544940	38.768000
2330.151753	240123.488044	38.773018
2332.371703	240601.565647	38.778036
2334.724479	241084.041943	38.783053
2336.941389	241556.199359	38.788071
2338.787245	242036.669733	38.793088
2340.478846	242524.098284	38.798106
2343.440799	243017.755174	38.803124
2345.309152	243511.352604	38.808141
2347.724866	244005.905326	38.813159
2349.755774	244520.229591	38.818176
2352.250881	245022.718838	38.823194
2354.326419	245537.897436	38.828212
2356.504583	246060.349399	38.833229
2358.983121	246570.636148	38.838247
2361.510204	247105.935682	38.843264
2363.422980	247623.598294	38.848282
2366.075020	248152.321556	38.853300
2367.671478	248695.559970	38.858317
2370.165595	249232.560462	38.863335
2372.319463	249781.500543	38.868352
2374.637862	250327.746020	38.873370
2377.183951	250883.048249	38.878388
2379.290138	251446.596515	38.883405
2381.458041	252008.812285	38.888423
2383.570496	252583.735604	38.893440
2386.029594	253139.729288	38.898458
2388.364836	253720.608439	38.903476
2391.066316	254304.857510	38.908493
2393.553488	254867.241475	38.913511
2395.876570	255454.034059	38.918528
2398.436613	256029.229693	38.923546
2401.103386	256606.158955	38.928564
2403.078017	257188.857861	38.933581
2406.413880	257755.720747	38.938599
2409.027525	258336.130555	38.943616
2411.878650	258904.816402	38.948634
2414.611124	259489.266463	38.953652
2416.952650	260049.694910	38.958669
2420.060525	260602.076558	38.963687
2422.521721	261169.186781	38.968704
2425.055138	261717.461507	38.973722
2427.738775	262281.382006	38.978740
2429.624426	262850.884822	38.983757
2432.069809	263398.809432	38.988775
2434.635423	263958.294786	38.993792
2437.478006	264514.584585	38.998810
2439.950986	265075.069064	39.003828
2442.167023	265641.254531	39.008845
2444.828687	266187.302281	39.013863
2447.016361	266749.726949	39.018880
2449.407282	267301.423942	39.023898
2451.605285	267865.821781	39.028916
2454.166335	268427.213623	39.033933
2456.688687	268990.741662	39.038951
2458.981132	269556.079998	39.043968
2461.389593	270123.250915	39.048986
2463.415015	270679.810854	39.054004
2465.764197	271259.149544	39.059021
2468.419129	271814.182274	39.064039
2470.761408	272360.701276	39.069056
2472.960973	272898.273865	39.074074
2475.609263	273432.166911	39.079092
2477.801562	273991.321330	39.084109
2480.243139	274536.084114	39.089127
2482.041513	275093.387778	39.094144
2484.563333	275655.324240	39.099162
2486.964622	276217.631156	39.104180
2489.279465	276791.807577	39.109197
2491.632009	277359.066346	39.114215
2494.382299	277940.683902	39.119232
2496.874206	278509.969751	39.124250
2499.469758	279085.965046	39.129268
2501.882917	279663.050994	39.134285
2504.736728	280231.963002	39.139303
2507.238589	280811.083357	39.144320
2509.789538	281394.305471	39.149338
2512.542129	281977.085269	39.154356
2514.758923	282572.209135	39.159373
2517.815254	283160.925138	39.164391
2519.739852	283752.427947	39.169408
2522.180787	284342.956671	39.174426
2524.947678	284935.638887	39.179444
2527.602257	285547.733775	39.184461
2530.021658	286149.499519	39.189479
2532.319828	286761.638952	39.194496
2534.656800	287373.335088	39.199514
2537.497470	287984.312396	39.204532
2539.704035	288606.605908	39.209549
2542.790524	289218.168225	39.214567
2545.320673	289822.371638	39.219584
2547.751275	290453.347083	39.224602
2550.402702	291060.312867	39.229620
2552.241577	291694.922666	39.234637
2555.003565	292325.218294	39.239655
2557.415383	292963.712171	39.244672
2559.860548	293617.021819	39.249690
2562.355095	294246.145834	39.254708
2565.362480	294889.350635	39.259725
2568.239527	295533.406557	39.264743
2570.824870	296183.924140	39.269760
2573.197087	296816.289467	39.274778
2576.086048	297460.169819	39.279796
2579.115427	298104.909619	39.284813
2581.467321	298740.024040	39.289831
2583.813102	299384.830157	39.294848
2586.369971	300032.109246	39.299866
2589.119649	300682.041704	39.304884
2592.035685	301332.955981	39.309901
2594.716640	301975.800839	39.314919
2597.147909	302621.570822	39.319936
2599.261231	303268.118616	39.324954
2602.071019	303923.891835	39.329972
2604.173568	304590.377746	39.334989
2607.179636	305237.650712	39.340007
2610.019293	305890.272100	39.345024
2612.634569	306549.773692	39.350042
2615.985970	307198.237204	39.355060
2617.993434	307861.979094	39.360077
2620.376831	308508.824786	39.365095
2623.497807	309159.100772	39.370112
2626.003525	309806.722588	39.375130
2628.597987	310454.601161	39.380148
2631.457754	311117.100252	39.385165
2634.005194	311775.983884	39.390183
2637.027263	312426.941838	39.395200
2639.264728	313077.556046	39.400218
2641.944218	313724.793000	39.405236
2644.631032	314360.928834	39.410253
2647.206501	314972.810497	39.415271
2649.427572	315601.007110	39.420288
2651.743248	316221.211399	39.425306
2654.433417	316856.144470	39.430324
2656.852033	317492.506591	39.435341
2659.335393	318126.007238	39.440359
2661.769010	318770.647163	39.445376
2663.918388	319433.390192	39.450394
2666.768586	320072.845333	39.455412
2669.118500	320734.268471	39.460429
2671.841968	321401.967225	39.465447
2674.215245	322064.482706	39.470464
2676.924470	322752.158219	39.475482
2679.774152	323422.545968	39.480500
2682.166693	324110.908207	39.485517
2684.819169	324798.761846	39.490535
2687.867407	325485.831958	39.495552
2690.933090	326171.060969	39.500570
2694.082977	326852.713179	39.505588
2696.293492	327537.925268	39.510605
2699.389091	328224.307225	39.515623
2702.600868	328913.399339	39.520640
2705.135189	329611.895886	39.525658
2707.961489	330296.152638	39.530676
2711.513010	330976.301478	39.535693
2715.460406	331623.523515	39.540711
2718.486866	332292.771330	39.545728
2721.200973	332965.988152	39.550746
2724.126291	333621.808486	39.555764
2726.644073	334297.645113	39.560781
2729.262348	334971.145536	39.565799
2731.569613	335632.861357	39.570816
2733.976831	336310.657339	39.575834
2736.758333	336986.581650	39.580852
2739.539556	337667.490485	39.585869
2742.304451	338338.649063	39.590887
2745.286155	339015.950341	39.595904
2747.776726	339701.736078	39.600922
2750.290380	340389.990676	39.605940
2753.242029	341086.913958	39.610957
2755.974367	341779.393852	39.615975
2758.359502	342476.022733	39.620992
2760.779971	343172.302518	39.626010
2763.580226	343880.961373	39.631028
2765.858103	344590.244882	39.636045
2768.520320	345301.076930	39.641063
2771.844313	346007.632255	39.646080
2774.721877	346721.621681	39.651098
2777.823909	347421.309764	39.656116
2780.617187	348134.065072	39.661133
2783.328156	348840.656158	39.666151
2786.109637	349558.099122	39.671168
2788.832180	350270.337637	39.676186
2791.811700	350986.552156	39.681204
2794.686175	351699.572533	39.686221
2797.210882	352420.009705	39.691239
2800.145532	353139.504910	39.696256
2802.828242	353860.721779	39.701274
2805.624535	354574.324188	39.706292
2808.502033	355294.768230	39.711309
2811.641468	356012.797309	39.716327
2814.536079	356738.250421	39.721344
2816.854586	357462.204530	39.726362
2819.844195	358173.945471	39.731380
2822.691179	358893.423577	39.736397
2825.161885	359616.846959	39.741415
2828.009389	360334.592615	39.746432
2830.499784	361041.350753	39.751450
2832.853634	361737.569322	39.756468
2835.609147	362431.326653	39.761485
2838.157021	363149.152970	39.766503
2840.258429	363853.319798	39.771520
2842.823397	364584.820115	39.776538
2845.319816	365317.275891	39.781556
2848.081384	366053.118635	39.786573
2851.118345	366788.367654	39.791591
2853.913169	367529.033372	39.796608
2856.563760	368274.517194	39.801626
2859.261752	369032.010810	39.806644
2862.138905	369806.991346	39.811661
2864.671540	370579.520997	39.816679
2867.589720	371343.785143	39.821696
2870.562266	372112.225936	39.826714
2873.635144	372897.048112	39.831732
2876.464524	373681.277812	39.836749
2879.206810	374456.681968	39.841767
2882.256880	375245.772941	39.846784
2885.011134	376050.366052	39.851802
2887.827401	376845.577637	39.856820
2890.976798	377646.337655	39.861837
2894.185283	378443.594068	39.866855
2897.950950	379231.418116	39.871872
2900.918230	380035.731532	39.876890
2903.480819	380831.091434	39.881908
2906.967697	381631.830305	39.886925
2909.836778	382426.283423	39.891943
2913.368102	383220.837076	39.896960
2916.422692	384015.972278	39.901978
2919.619516	384798.423297	39.906996
2922.893979	385591.499935	39.912013
2926.152516	386377.488918	39.917031
2929.363206	387155.129596	39.922048
2932.363479	387936.197480	39.927066
2935.316455	388714.741513	39.932084
2938.409354	389500.000064	39.937101
2941.015125	390290.854597	39.942119
2944.011440	391063.747701	39.947136
2947.195039	391849.347751	39.952154
2949.830543	392632.222897	39.957172
2952.898034	393416.727142	39.962189
2955.461024	394204.170461	39.967207
2958.727227	394993.402540	39.972224
2961.514096	395790.783753	39.977242
2964.429437	396603.053174	39.982260
2967.495987	397402.108791	39.987277
2970.106359	398202.018335	39.992295
2973.592048	398998.220950	39.997312
2976.470249	399807.905233	40.002330
2979.114331	400596.237008	40.007348
2982.192347	401401.532134	40.012365
2984.967420	402209.377019	40.017383
2987.985819	403011.689454	40.022400
2990.748387	403828.235206	40.027418
2993.650784	404647.412179	40.032436
2996.777541	405454.733120	40.037453
2999.615251	406274.974514	40.042471
3002.899432	407088.082552	40.047488
3006.104727	407888.016809	40.052506
3009.018636	408710.737591	40.057524
3012.453258	409524.643907	40.062541
3015.173418	410339.086699	40.067559
3018.968048	411136.635937	40.072576
3022.109768	411946.197458	40.077594
3025.012543	412745.698497	40.082612
3028.233534	413528.072093	40.087629
3030.902765	414304.179787	40.092647
3034.057127	415057.622970	40.097664
3036.909868	415822.973614	40.102682
3040.333336	416580.367796	40.107700
3043.498691	417329.530590	40.112717
3045.948485	418098.554116	40.117735
3049.205895	418859.230532	40.122752
3052.438561	419627.823320	40.127770
3055.182909	420404.707065	40.132788
3058.232684	421158.858678	40.137805
3060.762650	421952.102635	40.142823
3063.363957	422731.298018	40.147840
3066.392918	423524.757643	40.152858
3068.705662	424330.534090	40.157876
3071.757746	425148.298152	40.162893
3074.024865	425969.033217	40.167911
3076.940985	426790.493390	40.172928
3079.572104	427633.045539	40.177946
3082.234566	428491.177993	40.182964
3085.377565	429356.932882	40.187981
3088.133178	430226.147533	40.192999
3091.229134	431093.249163	40.198016
3094.485413	431969.941401	40.203034
3097.522379	432857.949719	40.208052
3100.675082	433742.210262	40.213069
3104.017356	434645.352184	40.218087
3107.073349	435535.610277	40.223104
3110.152480	436437.041625	40.228122
3113.117406	437348.048901	40.233140
3116.788271	438240.915252	40.238157
3120.446035	439149.707405	40.243175
3123.279271	440050.753266	40.248192
3126.411104	440958.580220	40.253210
3129.868670	441873.688032	40.258228
3133.317363	442781.478243	40.263245
3136.397478	443709.688395	40.268263
3139.762910	444615.684359	40.273280
3142.787830	445531.992228	40.278298
3145.504172	446458.150759	40.283316
3149.125583	447376.546192	40.288333
3151.928291	448306.587039	40.293351
3154.900461	449240.189540	40.298368
3158.312776	450189.580909	40.303386
3160.946777	451128.843898	40.308404
3163.937785	452073.757734	40.313421
3166.750952	453022.486044	40.318439
3169.705075	453979.673358	40.323456
3173.252265	454938.887145	40.328474
3176.468307	455892.194177	40.333492
3179.909523	456848.089418	40.338509
3183.446534	457805.481951	40.343527
3187.085214	458758.717782	40.348544
3190.399700	459709.478581	40.353562
3193.996160	460654.440510	40.358580
3197.591540	461591.276665	40.363597
3200.812466	462533.115040	40.368615
3204.148909	463481.341569	40.373632
3207.098935	464422.814400	40.378650
3210.676388	465363.884754	40.383668
3213.731757	466307.001470	40.388685
3217.004990	467247.407966	40.393703
3220.065429	468189.307703	40.398720
3223.298578	469131.883643	40.403738
3226.362028	470081.896694	40.408756
3229.821344	471020.092847	40.413773
3232.748089	471960.335347	40.418791
3235.854467	472898.730778	40.423808
3239.224411	473835.215750	40.428826
3242.213156	474760.461927	40.433844
3245.291977	475650.852271	40.438861
3248.565056	476565.816319	40.443879
3251.823871	477472.916310	40.448896
3254.955456	478378.976306	40.453914
3258.204197	479290.813620	40.458932
3261.228194	480195.778420	40.463949
3264.367552	481119.674600	40.468967
3267.206220	482046.839130	40.473984
3270.847998	482972.160732	40.479002
3273.678437	483905.566039	40.484020
3276.681272	484846.446820	40.489037
3279.731996	485801.219894	40.494055
3282.840541	486753.506472	40.499072
3286.290656	487707.141875	40.504090
3289.382078	488671.302374	40.509108
3292.466023	489646.182964	40.514125
3296.035190	490622.990640	40.519143
3299.279852	491600.188666	40.524160
3302.922621	492577.916102	40.529178
3306.212897	493563.289467	40.534196
3310.035710	494543.882194	40.539213
3312.920913	495531.706485	40.544231
3316.713966	496529.494513	40.549248
3319.977821	497510.834111	40.554266
3323.017359	498505.182199	40.559284
3326.269781	499513.978050	40.564301
3330.226688	500514.289115	40.569319
3333.177092	501523.748024	40.574336
3336.612247	502537.137949	40.579354
3339.649515	503558.369570	40.584372
3342.762653	504563.665362	40.589389
3345.851234	505600.796677	40.594407
3349.353609	506630.744176	40.599424
3352.644646	507658.134429	40.604442
3355.776809	508703.283930	40.609460
3359.552942	509748.960123	40.614477
3362.873619	510791.410220	40.619495
3366.355087	511838.636513	40.624512
3369.989709	512885.056302	40.629530
3372.960518	513954.281553	40.634548
3376.209515	515006.636044	40.639565
3379.471952	516065.293908	40.644583
3382.868489	517132.547356	40.649600
3386.900016	518186.296336	40.654618
3389.983236	519254.036138	40.659636
3393.628358	520304.815889	40.664653
3397.571930	521366.173378	40.669671
3401.112239	522425.901830	40.674688
3405.027293	523475.889902	40.679706
3408.907314	524526.504549	40.684724
3412.717758	525565.038467	40.689741
3416.733153	526591.501704	40.694759
3420.335776	527616.141002	40.699776
3424.242555	528641.758534	40.704794
3427.501279	529670.511159	40.709812
3431.057031	530688.388316	40.714829
3434.437576	531706.112908	40.719847
3437.513069	532717.929761	40.724864
3440.946753	533745.379287	40.729882
3444.491391	534770.369912	40.734900
3447.341173	535795.336823	40.739917
3450.687091	536822.905772	40.744935
3453.758412	537856.709651	40.749952
3457.288567	538887.697915	40.754970
3460.610575	539919.086527	40.759988
3464.446932	540948.955964	40.765005
3468.039833	541955.079387	40.770010
3471.500513	542947.330936	40.775015
3474.253686	543867.731273	40.780020
3477.237631	544763.884192	40.785024
3479.981087	545582.604711	40.790029
3483.338016	546364.814100	40.795034
3485.618151	547089.308390	40.800039
3488.532612	547759.150327	40.805044
3491.052482	548372.598008	40.810048
3493.420868	548932.136095	40.815053
3495.288508	549447.681183	40.820058
3497.068220	549908.716661	40.825063
3499.380985	550334.407975	40.830068
3501.242991	550716.465680	40.835072
3503.594966	551015.835627	40.840077
3505.188779	551279.773449	40.845082
3507.055471	551526.017738	40.850087
3508.753633	551708.740985	40.855092
3510.245509	551867.665502	40.860096
3511.429322	551978.527768	40.865101
3512.640054	552063.496092	40.870106
3513.799812	552127.358711	40.875111
3514.516150	552143.283079	40.880116
3514.883798	552142.622617	40.885120
3515.400317	552112.179631	40.890125
3516.437104	552088.592780	40.895130
3516.979951	552022.956882	40.900135
3517.801565	551938.325488	40.905140
3517.829214	551847.834889	40.910144
3518.307462	551733.344616	40.915149
3518.622083	551608.321755	40.920154
3518.892107	551468.625164	40.925159
3519.191952	551315.549845	40.930164
3519.904144	551162.609531	40.935168
3520.021503	550987.840470	40.940173
3519.946241	550799.424181	40.945178
3520.411520	550611.373347	40.950183
3520.470531	550415.388922	40.955188
3520.168324	550213.022102	40.960192
3520.256516	550008.429231	40.965197
3520.478994	549792.750715	40.970202
3520.136948	549578.413240	40.975207
3520.484370	549358.986951	40.980212
3520.133140	549135.089842	40.985216
3520.017691	548903.106769	40.990221
3520.213555	548687.412964	40.995226
3519.785250	548443.100186	41.000231
3520.040241	548205.163031	41.005236
3519.517182	547985.395112	41.010240
3519.775213	547743.123947	41.015245
3519.545824	547512.087842	41.020250
3519.628718	547284.921362	41.025255
3519.443575	547042.202512	41.030260
3519.030939	546816.311488	41.035264
3519.116315	546572.837254	41.040269
3519.525789	546343.641279	41.045274
3519.034163	546117.749797	41.050279
3518.620817	545867.096993	41.055284
3518.654445	545643.328103	41.060288
3518.232848	545410.924702	41.065293
3518.607423	545179.952283	41.070298
3518.265704	544952.758834	41.075303
3517.801767	544723.870074	41.080308
3517.711940	544497.383606	41.085312
3517.852823	544264.217354	41.090317
3517.645844	544041.614038	41.095322
3517.418104	543807.289359	41.100327
3517.157048	543590.722794	41.105332
3517.241980	543370.828819	41.110336
3516.966426	543139.617967	41.115341
3516.872082	542926.535369	41.120346
3516.465854	542714.906291	41.125351
3516.429347	542496.122623	41.130356
3516.252591	542287.267890	41.135360
3515.856415	542071.249484	41.140365
3516.019900	541864.447798	41.145370
3515.499224	541661.774116	41.150375
3515.392752	541456.366147	41.155380
3515.549539	541256.850839	41.160384
3515.476567	541050.776970	41.165389
3515.514035	540854.242394	41.170394
3515.141658	540654.347063	41.175399
3515.214755	540452.014366	41.180404
3515.189081	540258.700606	41.185408
3514.759388	540064.339763	41.190413
3514.697072	539867.503457	41.195418
3514.302645	539682.037692	41.200423
3514.384648	539483.713693	41.205428
3514.174171	539293.433174	41.210432
3514.191210	539101.101519	41.215437
3513.889450	538921.447549	41.220442
3513.757754	538735.071565	41.225447
3513.706585	538557.839303	41.230452
3513.776264	538376.308157	41.235456
3513.482398	538189.597139	41.240461
3513.405468	538018.501088	41.245466
3513.421344	537834.605259	41.250471
3513.380294	537657.207903	41.255476
3512.942526	537486.865453	41.260480
3512.889116	537305.388534	41.265485
3513.345137	537135.808237	41.270490
3512.766468	536968.852890	41.275495
3512.627483	536804.041504	41.280500
3512.309163	536637.443962	41.285504
3511.970633	536465.008844	41.290509
3511.882908	536301.541983	41.295514
3511.664393	536146.549435	41.300519
3511.913959	535991.884848	41.305524
3511.371495	535839.808051	41.310528
3511.669231	535693.538280	41.315533
3511.352927	535535.130756	41.320538
3511.418749	535394.480962	41.325543
3511.165746	535237.771364	41.330548
3510.919151	535097.921999	41.335552
3510.707855	534950.313527	41.340557
3510.360038	534807.808830	41.345562
3510.326965	534673.811272	41.350567
3510.457792	534527.956937	41.355572
3510.423622	534399.645110	41.360576
3510.517867	534253.642345	41.365581
3510.496596	534113.495524	41.370586
3509.860835	533992.673470	41.375591
3509.922402	533859.659567	41.380596
3509.738126	533738.311793	41.385600
3509.786015	533608.217325	41.390605
3509.783557	533477.575600	41.395610
3509.635681	533348.012419	41.400615
3509.581803	533225.078857	41.405620
3509.378017	533103.476437	41.410624
3509.429385	532987.371225	41.415629
3509.623276	532860.267278	41.420634
3509.195023	532733.762367	41.425639
3509.337644	532606.210786	41.430644
3509.177722	532496.377135	41.435648
3508.989064	532372.449504	41.440653
3508.950836	532263.601912	41.445658
3509.022349	532143.860907	41.450663
3508.983820	532030.379281	41.455668
3509.031777	531914.113951	41.460672
3508.983798	531797.711459	41.465677
3508.699804	531674.194810	41.470682
3508.713445	531566.340331	41.475687
3508.363715	531446.003885	41.480692
3508.118556	531342.568440	41.485696
3508.370899	531240.817101	41.490701
3507.976152	531139.820253	41.495706
3508.084875	531036.428016	41.500711
3508.090756	530919.656823	41.505716
3508.446974	530834.452586	41.510720
3508.159822	530720.746469	41.515725
3508.492216	530611.625980	41.520730
3508.101123	530505.940630	41.525735
3507.821996	530396.258881	41.530740
3508.292161	530302.221149	41.535744
3508.133098	530197.655394	41.540749
3508.092203	530095.890414	41.545754
3507.605464	529990.366850	41.550759
3507.683508	529881.128777	41.555764
3507.357033	529791.088902	41.560768
3506.984812	529698.285802	41.565773
3507.361762	529606.523721	41.570778
3507.178413	529522.603524	41.575783
3506.972348	529428.261876	41.580788
3506.954475	529333.688824	41.585792
3506.922267	529259.060025	41.590797
3507.144285	529166.462852	41.595802
3506.666313	529082.686409	41.600807
3506.632362	528984.487351	41.605812
3506.775398	528911.088339	41.610816
3506.615953	528837.836711	41.615821
3506.826928	528742.015101	41.620826
3506.501154	528668.032975	41.625831
3506.700193	528588.227397	41.630836
3506.545895	528505.555252	41.635840
3506.292483	528422.998738	41.640845
3506.598761	528341.664071	41.645850
3506.609551	528261.331803	41.650855
3506.402348	528178.867296	41.655860
3506.352462	528096.831075	41.660864
3506.237650	528027.697903	41.665869
3506.336838	527948.609099	41.670874
3506.363874	527886.403527	41.675879
3506.215176	527806.496230	41.680884
3506.086780	527728.751036	41.685888
3506.170594	527647.245241	41.690893
3506.214594	527571.184752	41.695898
3505.914187	527497.091367	41.700903
3506.224007	527426.126118	41.705908
3505.836160	527356.729713	41.710912
3506.100754	527281.086535	41.715917
3505.860363	527201.290579	41.720922
3505.914088	527145.927440	41.725927
3506.095406	527070.144909	41.730932
3506.055089	526992.532782	41.735936
3505.848805	526919.579999	41.740941
3505.987717	526841.334663	41.745946
3505.837385	526769.933804	41.750951
3506.021069	526699.890946	41.755956
3505.904104	526633.319687	41.760960
3505.776355	526569.117190	41.765965
3506.285607	526489.401770	41.770970
3505.773908	526418.105618	41.775975
3505.715953	526342.608016	41.780980
3506.069136	526282.661237	41.785984
3505.789120	526203.570636	41.790989
3505.845964	526133.242292	41.795994
3505.560272	526069.867910	41.800999
3505.754329	526002.640616	41.806004
3505.892983	525929.276095	41.811008
3505.476757	525863.402388	41.816013
3505.760789	525798.628351	41.821018
3505.558711	525735.591977	41.826023
3505.710644	525652.249852	41.831028
3505.709722	525591.851319	41.836032
3505.195435	525520.500371	41.841037
3505.129701	525455.325718	41.846042
3505.419276	525406.517718	41.851047
3505.512266	525344.189196	41.856052
3505.343716	525283.916101	41.861056
3504.900117	525222.174262	41.866061
3504.900046	525153.965373	41.871066
3504.899627	525097.796099	41.876071
3504.885179	525034.777581	41.881076
3505.036694	524982.815799	41.886080
3504.892012	524924.552426	41.891085
3504.990616	524864.084727	41.896090
3504.874911	524815.942155	41.901095
3505.366286	524748.410374	41.906100
3504.907143	524698.557609	41.911104
3504.945053	524642.531586	41.916109
3504.918335	524582.233245	41.921114
3504.659878	524534.212626	41.926119
3504.574925	524477.802003	41.931124
3504.355512	524421.512824	41.936128
3504.633573	524376.531629	41.941133
3504.738161	524318.932126	41.946138
3504.299119	524271.643971	41.951143
3504.410456	524211.020194	41.956148
3504.496712	524163.901812	41.961152
3504.129640	524126.274841	41.966157
3504.217326	524070.188291	41.971162
3504.352554	524043.818432	41.976167
3504.358577	523979.129198	41.981172
3504.479538	523950.746160	41.986176
3504.541090	523899.801772	41.991181
3504.707254	523838.613588	41.996186
3504.542042	523799.594000	42.001191
3504.483452	523742.823505	42.006196
3504.465914	523692.092160	42.011200
3504.396077	523640.361127	42.016205
3504.610497	523578.660429	42.021210
3504.499810	523539.681980	42.026215
3504.194362	523484.409882	42.031220
3504.530094	523443.648689	42.036224
3504.160341	523399.168078	42.041229
3504.388236	523348.044559	42.046234
3503.909275	523302.925646	42.051239
3504.221226	523252.997875	42.056244
3504.313774	523216.858699	42.061248
3504.419278	523163.536658	42.066253
3504.208089	523118.728141	42.071258
3504.384268	523076.781454	42.076263
3504.228731	523023.650630	42.081268
3504.173914	522980.278452	42.086272
3504.031954	522932.284336	42.091277
3504.071946	522884.312119	42.096282
3504.178609	522853.107448	42.101287
3504.249139	522809.513674	42.106292
3504.013774	522759.820393	42.111296
3504.150532	522726.897657	42.116301
3504.155369	522680.290579	42.121306
3504.003338	522636.730878	42.126311
3504.185539	522582.739585	42.131316
3503.660804	522531.427762	42.136320
3503.878690	522496.829105	42.141325
3504.022006	522454.280957	42.146330
3504.084340	522426.206133	42.151335
3504.144570	522368.302833	42.156340
3504.293836	522327.819204	42.161344
3503.867849	522286.719556	42.166349
3504.145064	522241.680948	42.171354
3503.947403	522202.107505	42.176359
3503.750827	522157.746989	42.181364
3504.188241	522114.345806	42.186368
3503.528410	522082.754750	42.191373
3503.584908	522042.788575	42.196378
3503.751695	522006.533817	42.201383
3503.607402	521964.079263	42.206388
3504.180777	521924.536185	42.211392
3503.840933	521890.929747	42.216397
3503.943147	521842.440249	42.221402
3503.643816	521803.738058	42.226407
3503.984091	521757.377917	42.231412
3504.218954	521726.352239	42.236416
3503.733055	521688.132248	42.241421
3504.374317	521641.976818	42.246426
3504.030975	521607.513601	42.251431
3503.993157	521558.944096	42.256436
3504.064639	521512.574552	42.261440
3503.402811	521464.908046	42.266445
3504.148273	521430.274944	42.271450
3503.574965	521405.421084	42.276455
3503.561384	521357.250201	42.281460
3503.843933	521322.487298	42.286464
3503.432069	521292.417898	42.291469
3504.113997	521249.580572	42.296474
3503.708413	521210.439695	42.301479
3503.903704	521166.921972	42.306484
3503.970699	521134.762067	42.311488
3503.849616	521084.288950	42.316493
3504.250316	521037.513806	42.321498
3503.788725	520993.442655	42.326503
3503.609158	520958.700335	42.331508
3503.954985	520923.926561	42.336512
3503.667517	520896.406904	42.341517
3503.771119	520845.142051	42.346522
3503.713943	520812.597565	42.351527
3503.773743	520768.646114	42.356532
3504.249881	520740.301819	42.361536
3503.575374	520692.684948	42.366541
3503.719189	520645.646068	42.371546
3503.404980	520610.520662	42.376551
3503.875279	520575.525052	42.381556
3504.049659	520530.194382	42.386560
3503.945866	520494.884753	42.391565
3503.849454	520450.049494	42.396570
3503.790140	520416.546909	42.401575
3503.987538	520373.177487	42.406580
3504.191473	520331.570701	42.411584
3503.776030	520294.696437	42.416589
3504.016986	520245.373312	42.421594
3503.605614	520207.339105	42.426599
3503.783161	520154.800269	42.431604
3503.821864	520127.732238	42.436608
3503.544293	520098.747968	42.441613
3503.840056	520055.009457	42.446618
3503.448017	520022.817552	42.451623
3503.622279	519978.593750	42.456628
3503.756311	519947.630082	42.461632
3503.770449	519906.857856	42.466637
3503.931188	519868.733670	42.471642
3503.667164	519836.219026	42.476647
3503.862541	519790.781825	42.481652
3503.684320	519754.221946	42.486656
3503.952371	519714.417554	42.491661
3504.073753	519672.972784	42.496666
3503.821346	519636.424132	42.501671
3503.530641	519591.817855	42.506676
3503.835716	519555.635806	42.511680
3503.719336	519521.938303	42.516685
3503.761290	519474.407242	42.521690
3503.423875	519444.674927	42.526695
3503.303180	519416.118361	42.531700
3503.212234	519370.825106	42.536704
3503.075107	519341.968556	42.541709
3503.098125	519300.890742	42.546714
3502.930705	519285.495013	42.551719
3503.420229	519253.063302	42.556724
3503.593413	519217.102468	42.561728
3503.237856	519187.876396	42.566733
3503.311080	519154.602062	42.571738
3503.468638	519135.930093	42.576743
3503.384231	519106.359260	42.581748
3503.432373	519070.014307	42.586752
3502.760816	519029.598144	42.591757
3503.150524	518996.072578	42.596762
3503.158254	518967.243090	42.601767
3503.296646	518946.759477	42.606772
3503.098342	518914.585192	42.611776
3503.138001	518876.880262	42.616781
3503.397026	518846.398631	42.621786
3503.329500	518824.082092	42.626791
3503.244404	518797.635473	42.631796
3503.392111	518760.266205	42.636800
3503.086148	518739.196228	42.641805
3503.381833	518703.466976	42.646810
3503.037685	518683.713258	42.651815
3503.115555	518642.020118	42.656820
3503.311580	518610.993361	42.661824
3503.045028	518587.901000	42.666829
3502.950169	518552.181724	42.671834
3502.984209	518523.095199	42.676839
3503.245307	518491.957243	42.681844
3503.378539	518468.701666	42.686848
3502.961211	518435.602714	42.691853
3503.202278	518403.510054	42.696858
3503.226644	518385.916210	42.701863
3503.248947	518350.631786	42.706868
3503.288025	518316.705502	42.711872
3503.130876	518287.749029	42.716877
3503.642294	518257.781226	42.721882
3503.062762	518227.932721	42.726887
3503.198633	518195.906344	42.731892
3503.124275	518161.946925	42.736896
3503.340971	518131.470285	42.741901
3503.169986	518097.021718	42.746906
3503.246473	518069.439691	42.751911
3503.034005	518037.668759	42.756916
3503.165363	518003.324115	42.761920
3503.079735	517985.797275	42.766925
3503.461074	517957.663556	42.771930
3503.336848	517927.441124	42.776935
3503.150463	517895.867415	42.781940
3503.285356	517857.943237	42.786945
3503.224682	517832.398204	42.791949
3503.324424	517804.560006	42.796954
3503.435351	517778.786555	42.801959
3503.564167	517744.290447	42.806964
3503.395968	517697.289928	42.811969
3503.172504	517670.056194	42.816973
3503.545514	517635.017771	42.821978
3503.435521	517606.002110	42.826983
3503.070973	517572.943254	42.831988
3503.258084	517546.653468	42.836993
3503.304377	517518.369367	42.841997
3503.345885	517477.837636	42.847002
3502.814524	517452.012303	42.852007
3503.143413	517437.142110	42.857012
3503.426116	517402.066739	42.862017
3503.332480	517370.880624	42.867021
3503.460380	517339.962394	42.872026
3503.333094	517306.261111	42.877031
3503.108643	517274.893512	42.882036
3503.400516	517243.294278	42.887041
3503.250843	517203.749189	42.892045
3503.384611	517168.948427	42.897050
3503.372560	517146.519703	42.902055
3503.312453	517112.857895	42.907060
3503.844369	517075.928296	42.912065
3503.379902	517047.218641	42.917069
3503.056244	517008.304937	42.922074
3503.000050	516986.890947	42.927079
3503.532084	516948.852046	42.932084
3503.370725	516916.969744	42.937089
3502.910614	516890.023314	42.942093
3503.124887	516855.662890	42.947098
3503.012452	516828.914273	42.952103
3502.708339	516807.639396	42.957108
3503.047139	516779.056216	42.962113
3502.907651	516761.032116	42.967117
3503.273795	516727.504662	42.972122
3503.112051	516695.521089	42.977127
3503.174162	516670.509263	42.982132
3503.081645	516637.960300	42.987137
3502.617857	516615.752227	42.992141
3503.091803	516586.542722	42.997146
3502.852787	516565.106115	43.002151
3503.035398	516529.489603	43.007156
3503.322476	516503.988794	43.012161
3502.939298	516488.119400	43.017165
3503.009787	516444.606018	43.022170
3502.902536	516423.199093	43.027175
3503.045566	516393.435772	43.032180
3502.804003	516365.748582	43.037185
3502.767226	516348.262452	43.042189
3502.726511	516307.235968	43.047194
3503.023058	516289.849122	43.052199
3503.026920	516264.391940	43.057204
3503.067315	516236.559795	43.062209
3502.791342	516213.112022	43.067213
3502.650879	516186.568151	43.072218
3502.874981	516163.092884	43.077223
3502.465747	516133.011662	43.082228
3503.010362	516117.804016	43.087233
3502.635678	516101.529576	43.092237
3503.142725	516068.079409	43.097242
3502.527190	516050.027634	43.102247
3502.809728	516024.879512	43.107252
3502.770014	515992.320803	43.112257
3502.788508	515975.128058	43.117261
3503.027422	515951.700536	43.122266
3503.138086	515933.434782	43.127271
3503.044081	515892.516174	43.132276
3502.851210	515864.316292	43.137281
3502.782979	515848.649201	43.142285
3502.830922	515815.320273	43.147290
3502.427076	515784.934986	43.152295
3502.753175	515762.552203	43.157300
3502.986248	515754.298931	43.162305
3502.994308	515727.428596	43.167309
3502.884714	515694.123890	43.172314
3502.987410	515669.103927	43.177319
3502.632015	515648.288934	43.182324
3502.887077	515622.236950	43.187329
3502.984250	515599.536646	43.192333
3503.317377	515570.951842	43.197338
3503.020997	515544.683053	43.202343
3502.462738	515515.934375	43.207348
3502.798355	515490.222489	43.212353
3502.711352	515473.700890	43.217357
3503.090709	515447.780471	43.222362
3502.576617	515431.930226	43.227367
3503.199850	515401.737152	43.232372
3503.172166	515379.156739	43.237377
3502.701164	515353.923006	43.242381
3502.836284	515320.780966	43.247386
3502.853005	515306.259526	43.252391
3502.726721	515272.301034	43.257396
3503.010618	515247.050458	43.262401
3502.595869	515222.765573	43.267405
3502.749686	515201.971491	43.272410
3502.854423	515175.488340	43.277415
3502.687129	515151.114408	43.282420
3502.784393	515129.976126	43.287425
3502.725277	515100.443121	43.292429
3502.774674	515077.295673	43.297434
3502.976222	515063.148524	43.302439
3503.260255	515035.881002	43.307444
3503.295338	515008.198444	43.312449
3503.073235	514986.101365	43.317453
3502.943541	514944.126807	43.322458
3503.082950	514922.477509	43.327463
3502.972366	514892.901656	43.332468
3502.778476	514859.759294	43.337473
3502.615647	514849.147207	43.342477
3502.640521	514816.575670	43.347482
3502.653916	514806.087371	43.352487
3502.597516	514781.594702	43.357492
3503.148500	514766.737484	43.362497
3502.584849	514732.190333	43.367501
3502.905348	514700.933717	43.372506
3502.827938	514683.552627	43.377511
3502.854347	514664.491668	43.382516
3502.660370	514624.542738	43.387521
3502.710299	514609.057511	43.392525
3502.897558	514590.324325	43.397530
3502.427889	514558.938272	43.402535
3502.523522	514541.933399	43.407540
3502.937026	514516.661322	43.412545
3502.714394	514495.622265	43.417549
3502.668537	514467.497479	43.422554
3502.684921	514444.051614	43.427559
3502.782934	514420.542591	43.432564
3502.932600	514408.923638	43.437569
3502.582777	514390.929164	43.442573
3502.942314	514361.884009	43.447578
3502.919365	514337.687844	43.452583
3503.051410	514310.694627	43.457588
3503.074660	514271.769615	43.462593
3503.215576	514257.580662	43.467597
3503.122511	514220.891929	43.472602
3502.849737	514198.902309	43.477607
3502.781146	514171.738375	43.482612
3503.173002	514142.637315	43.487617
3502.886976	514122.716725	43.492621
3502.726043	514089.113635	43.497626
3502.992298	514068.602855	43.502631
3502.617354	514043.250940	43.507636
3502.789401	514008.688329	43.512641
3502.277323	513996.667832	43.517645
3502.578501	513969.143457	43.522650
3502.828338	513952.668457	43.527655
3502.605998	513935.409815	43.532660
3502.820317	513911.428072	43.537665
3502.661427	513885.084310	43.542669
3502.776376	513860.865854	43.547674
3502.978034	513844.751148	43.552679
3502.698508	513819.686483	43.557684
3502.783581	513795.875906	43.562689
3503.133187	513772.729978	43.567693
3502.748082	513733.665328	43.572698
3502.694352	513720.413644	43.577703
3502.769163	513694.436501	43.582708
3502.869554	513667.043609	43.587713
3502.641797	513644.037730	43.592717
3502.870813	513615.969279	43.597722
3502.788448	513592.789434	43.602727
3502.914249	513567.812496	43.607732
3503.074886	513540.359560	43.612737
3502.852285	513514.025008	43.617741
3502.962951	513493.134237	43.622746
3502.725895	513460.801949	43.627751
3502.748162	513449.151598	43.632756
3502.778245	513421.870002	43.637761
3502.571619	513410.709012	43.642765
3502.356343	513374.087475	43.647770
3502.533256	513366.446559	43.652775
3502.425940	513346.043265	43.657780
3502.234159	513324.392590	43.662785
3502.538932	513305.387284	43.667789
3502.577031	513287.381429	43.672794
3502.769913	513268.746425	43.677799
3502.444462	513237.788711	43.682804
3502.593624	513215.832712	43.687809
3502.635569	513205.842961	43.692813
3502.021628	513175.887987	43.697818
3502.406685	513158.634699	43.702823
3502.041108	513158.187362	43.707828
3502.387340	513133.931648	43.712833
3502.382160	513118.705436	43.717837
3502.476033	513099.984771	43.722842
3502.499560	513074.468235	43.727847
3502.579657	513062.354774	43.732852
3502.553854	513029.030612	43.737857
3502.524607	513023.539266	43.742861
3502.562956	512996.305969	43.747866
3502.522031	512985.370957	43.752871
3502.566087	512958.943435	43.757876
3502.508841	512945.741981	43.762881
3502.456692	512917.110818	43.767885
3502.417485	512897.503007	43.772890
3502.426015	512885.400530	43.777895
3502.458913	512865.579768	43.782900
3502.505626	512843.437437	43.787905
3502.684912	512825.812387	43.792909
3502.854535	512801.331469	43.797914
3503.028247	512774.782578	43.802919
3502.632697	512758.356173	43.807924
3502.581732	512741.321486	43.812929
3502.881904	512713.189720	43.817933
3502.594589	512692.359678	43.822938
3502.511172	512663.430327	43.827943
3502.533802	512649.308562	43.832948
3502.821102	512619.867633	43.837953
3502.523203	512601.005573	43.842957
3502.636066	512573.104361	43.847962
3502.671219	512567.098588	43.852967
3502.617977	512542.399783	43.857972
3502.913421	512519.361047	43.862977
3502.566568	512494.556578	43.867981
3502.699200	512469.879144	43.872986
3502.638174	512450.274098	43.877991
3502.543761	512425.884031	43.882996
3502.889614	512405.005453	43.888001
3502.783390	512383.289575	43.893005
3502.723263	512352.288602	43.898010
3502.786851	512331.302568	43.903015
3502.483802	512321.870103	43.908020
3502.688030	512291.886751	43.913025
3502.551301	512271.839423	43.918029
3502.497397	512244.971978	43.923034
3502.530140	512230.696944	43.928039
3502.113453	512212.911741	43.933044
3502.625260	512177.787474	43.938049
3502.537151	512172.204103	43.943053
3502.439569	512143.679269	43.948058
3502.591863	512141.638586	43.953063
3502.294101	512120.758889	43.958068
3502.659135	512103.406567	43.963073
3502.598071	512090.860411	43.968077
3502.486862	512082.608113	43.973082
3502.776253	512051.602507	43.978087
3502.490702	512029.863559	43.983092
3502.664944	512002.254202	43.988097
3502.542406	511993.095971	43.993101
3502.512927	511961.887663	43.998106
3502.802926	511947.118484	44.003111
3502.371887	511920.510801	44.008116
3502.591323	511900.256240	44.013121
3502.302791	511880.988347	44.018125
3502.545223	511857.502944	44.023130
3502.753924	511839.519096	44.028135
3502.716409	511825.254580	44.033140
3502.994945	511800.250706	44.038145
3503.056225	511779.516329	44.043149
3502.932296	511746.960752	44.048154
3503.178603	511726.197503	44.053159
3502.852172	511697.203113	44.058164
3502.559660	511649.243273	44.063169
3502.511157	511649.099522	44.068173
3502.686908	511623.707920	44.073178
3502.831288	511600.842456	44.078183
3502.637795	511582.618308	44.083188
3502.863173	511560.950401	44.088193
3503.093952	511534.591977	44.093197
3502.658918	511497.646719	44.098202
3502.994882	511470.364131	44.103207
3502.698135	511450.945642	44.108212
3502.839321	511423.995833	44.113217
3502.829393	511417.391461	44.118221
3502.743679	511386.947020	44.123226
3503.004560	511359.726327	44.128231
3502.727055	511341.968780	44.133236
3502.948532	511308.904591	44.138241
3502.570899	511283.699341	44.143245
3502.423588	511254.272740	44.148250
3502.432039	511236.218423	44.153255
3502.577625	511227.522240	44.158260
3503.051009	511187.207447	44.163265
3502.820373	511180.435598	44.168269
3503.176295	511140.290231	44.173274
3502.829004	511109.381614	44.178279
3502.748123	511091.088873	44.183284
3503.133441	511062.839682	44.188289
3502.855917	511037.265413	44.193293
3502.774501	511016.552111	44.198298
3503.025498	510997.753751	44.203303
3502.674352	510960.592305	44.208308
3502.875139	510933.127994	44.213313
3502.565915	510922.081830	44.218317
3502.612378	510889.094314	44.223322
3502.739384	510869.558648	44.228327
3502.840439	510844.328544	44.233332
3502.611309	510822.326792	44.238337
3503.051439	510809.247635	44.243341
3502.727905	510779.696172	44.248346
3502.966496	510754.293217	44.253351
3502.560232	510727.881121	44.258356
3502.864786	510710.183484	44.263361
3503.029490	510689.431399	44.268365
3502.537222	510656.123733	44.273370
3502.656284	510643.749967	44.278375
3502.653022	510613.341443	44.283380
3502.860408	510591.876558	44.288385
3502.924144	510567.105630	44.293389
3502.894960	510545.778346	44.298394
3502.657526	510519.440445	44.303399
3502.642049	510495.135586	44.308404
3502.889221	510464.788630	44.313409
3502.578315	510449.254073	44.318413
3502.559761	510431.102062	44.323418
3502.907866	510406.589181	44.328423
3502.683075	510384.636497	44.333428
3503.262566	510357.263421	44.338433
3503.007645	510338.845490	44.343437
3502.492827	510298.278477	44.348442
3503.149386	510274.725982	44.353447
3502.617206	510253.173942	44.358452
3502.919871	510225.288947	44.363457
3502.714075	510208.981301	44.368461
3502.673397	510185.335431	44.373466
3502.910248	510163.411427	44.378471
3502.655957	510135.007747	44.383476
3502.820194	510110.825551	44.388481
3502.658523	510094.410044	44.393485
3502.848962	510078.040587	44.398490
3502.583751	510051.403540	44.403495
3502.413373	510031.459101	44.408500
3502.398422	510011.339152	44.413505
3502.659094	509992.386647	44.418509
3502.341720	509965.354100	44.423514
3502.661138	509944.980296	44.428519
3502.211516	509926.743417	44.433524
3502.364903	509912.043791	44.438529
3502.907568	509885.885901	44.443533
3502.463330	509872.590469	44.448538
3502.706850	509853.035259	44.453543
3502.522229	509824.922705	44.458548
3502.501794	509800.062658	44.463553
3502.427378	509789.785981	44.468557
3502.527954	509765.512234	44.473562
3502.868041	509745.689685	44.478567
3502.590965	509718.347795	44.483572
3502.787190	509697.387611	44.488577
3502.917761	509680.320948	44.493581
3502.697460	509649.389351	44.498586
3502.679859	509617.114880	44.503591
3502.511964	509607.911713	44.508596
3502.344819	509576.265618	44.513601
3502.527406	509565.999219	44.518605
3502.474601	509543.917591	44.523610
3502.786638	509527.831174	44.528615
3502.498940	509509.518122	44.533620
3502.551503	509478.291519	44.538625
3502.650990	509461.431164	44.543629
3502.706968	509441.702833	44.548634
3502.806338	509414.604376	44.553639
3502.307906	509400.610854	44.558644
3502.542105	509369.154010	44.563649
3502.688784	509367.870312	44.568653
3502.347788	509340.083727	44.573658
3502.684913	509319.201923	44.578663
3502.843462	509293.304446	44.583668
3502.787913	509271.474990	44.588673
3502.412840	509250.754346	44.593677
3502.591158	509236.806654	44.598682
3502.622372	509206.389724	44.603687
3502.772294	509191.639452	44.608692
3502.390360	509147.114532	44.613697
3502.419375	509146.403907	44.618701
3502.489203	509122.537316	44.623706
3502.430058	509114.880386	44.628711
3502.484300	509093.386614	44.633716
3502.524681	509060.345321	44.638721
3502.285949	509052.312822	44.643725
3502.125034	509037.005536	44.648730
3502.660495	509014.781103	44.653735
3502.313717	508997.687026	44.658740
3502.696200	508976.848094	44.663745
3502.533998	508955.387793	44.668749
3502.554482	508930.721588	44.673754
3502.965790	508912.450292	44.678759
3502.570666	508885.579076	44.683764
3502.653681	508858.028174	44.688769
3502.682502	508858.578462	44.693773
3502.347218	508826.351617	44.698778
3502.226348	508802.514160	44.703783
3502.214309	508792.277485	44.708788
3502.531595	508771.801449	44.713793
3502.725038	508746.805392	44.718797
3502.549480	508730.239145	44.723802
3502.320197	508713.782111	44.728807
3502.362186	508694.105349	44.733812
3502.412290	508683.505869	44.738817
3502.308840	508661.481177	44.743821
3502.221077	508636.881740	44.748826
3502.414238	508626.411266	44.753831
3502.424520	508609.059408	44.758836
3502.533592	508581.756096	44.763841
3502.447956	508562.502505	44.768845
3502.194010	508546.503047	44.773850
3502.451969	508531.230905	44.778855
3502.052130	508513.791438	44.783860
3502.718151	508492.251989	44.788865
3502.280095	508475.322793	44.793869
3502.157841	508451.636271	44.798874
3502.493647	508432.518671	44.803879
3502.237639	508412.787014	44.808884
3502.459008	508399.134422	44.813889
3502.688249	508384.572716	44.818893
3502.159178	508382.990584	44.823898
3502.398679	508353.144656	44.828903
3502.517632	508340.113197	44.833908
3502.306400	508315.481976	44.838913
3502.597940	508295.009258	44.843917
3502.469317	508279.696126	44.848922
3502.528079	508243.926415	44.853927
3502.554135	508239.534226	44.858932
3502.846172	508217.195109	44.863937
3502.506667	508195.155986	44.868941
3502.624916	508172.188145	44.873946
3502.609280	508149.947238	44.878951
3502.164167	508133.170044	44.883956
3502.314643	508117.308921	44.888961
3502.412950	508106.298000	44.893965
3502.287024	508079.484235	44.898970
3502.315437	508066.012665	44.903975
3501.983127	508041.803318	44.908980
3502.463008	508027.757070	44.913985
3502.435442	508020.649460	44.918989
3502.138784	508001.932332	44.923994
3502.178758	507992.393129	44.928999
3502.342708	507970.527506	44.934004
3502.756566	507953.263360	44.939009
3502.434161	507934.550149	44.944013
3502.396620	507914.228969	44.949018
3502.438221	507897.073121	44.954023
3502.559742	507875.415711	44.959028
3502.477846	507860.901885	44.964033
3502.187435	507837.543139	44.969037
3502.200190	507823.972896	44.974042
3502.064856	507815.974041	44.979047
3502.056757	507792.621729	44.984052
3502.382264	507767.048556	44.989057
3502.523407	507761.125117	44.994061
3502.036223	507738.603865	44.999066
3502.324653	507723.477431	45.004071
3502.164216	507727.285369	45.009076
3502.448993	507696.775296	45.014081
3502.108622	507678.215862	45.019085
3502.338294	507668.899122	45.024090
3502.607788	507648.882865	45.029095
3502.453173	507637.557857	45.034100
3502.308187	507603.482762	45.039105
3502.526784	507601.481551	45.044109
3502.460935	507575.817612	45.049114
3502.647247	507548.500291	45.054119
3502.361311	507523.173148	45.059124
3502.513983	507520.375134	45.064129
3502.486719	507495.209452	45.069133
3502.288195	507467.850979	45.074138
3502.817504	507455.309700	45.079143
3502.526602	507437.297101	45.084148
3502.438364	507428.483644	45.089153
3502.125755	507399.780886	45.094157
3502.078930	507391.919342	45.099162
3502.511259	507373.491472	45.104167
3502.359884	507351.320876	45.109172
3502.455917	507332.642639	45.114177
3502.639091	507313.345519	45.119181
3502.494510	507304.641635	45.124186
3502.711563	507258.605198	45.129191
3502.535679	507260.145793	45.134196
3502.695919	507230.864697	45.139201
3502.615258	507205.151951	45.144205
3502.324836	507186.180565	45.149210
3502.552269	507167.380779	45.154215
3502.644480	507151.981622	45.159220
3502.722364	507130.329867	45.164225
3502.772914	507109.237196	45.169229
3502.844280	507084.912954	45.174234
3502.811974	507049.759711	45.179239
3502.867986	507039.561622	45.184244
3502.605181	507002.880418	45.189249
3502.767135	506990.244568	45.194253
3502.490463	506967.336233	45.199258
3502.858316	506940.847019	45.204263
3502.677253	506925.691912	45.209268
3502.630413	506889.935221	45.214273
3502.572652	506876.021946	45.219277
3502.741963	506847.797952	45.224282
3502.593697	506831.628780	45.229287
3502.646271	506827.433801	45.234292
3502.692224	506797.211178	45.239297
3503.019744	506764.119850	45.244301
3502.702907	506742.125381	45.249306
3502.553755	506721.618089	45.254311
3502.569025	506693.417759	45.259316
3502.473536	506668.563891	45.264321
3502.464152	506647.782525	45.269325
3502.288470	506640.192835	45.274330
3502.589663	506625.719019	45.279335
3502.694948	506611.225231	45.284340
3502.381144	506586.657412	45.289345
3502.532039	506562.975675	45.294349
3502.494578	506539.878094	45.299354
3502.695571	506518.105362	45.304359
3502.957385	506500.358675	45.309364
3502.376568	506467.004451	45.314369
3502.301031	506463.333744	45.319373
3502.835747	506446.956966	45.324378
3502.513054	506424.458472	45.329383
3502.524805	506407.658584	45.334388
3502.835221	506376.485912	45.339393
3502.529138	506360.038094	45.344397
3502.278851	506336.721078	45.349402
3502.396783	506321.367465	45.354407
3502.135108	506290.283630	45.359412
3502.308808	506279.461343	45.364417
3502.606344	506254.848264	45.369421
3502.353292	506244.041913	45.374426
3502.825039	506224.446189	45.379431
3502.494148	506209.616305	45.384436
3502.501291	506185.451858	45.389441
3502.426226	506162.510853	45.394445
3502.452300	506148.482930	45.399450
3502.555353	506116.635722	45.404455
3502.555867	506109.220113	45.409460
3502.456058	506083.407429	45.414465
3502.448720	506064.642723	45.419469
3502.518356	506042.032128	45.424474
3502.459041	506020.753158	45.429479
3502.327280	506007.355009	45.434484
3502.320610	505982.889692	45.439489
3502.678437	505963.361783	45.444493
3502.591867	505948.594500	45.449498
3502.572008	505921.709712	45.454503
3502.181995	505917.785123	45.459508
3502.671199	505886.835793	45.464513
3502.852899	505866.124445	45.469517
3502.560198	505853.457447	45.474522
3503.071516	505821.041583	45.479527
3502.711764	505816.809577	45.484532
3502.629155	505785.394095	45.489537
3502.881952	505755.137077	45.494541
3502.279380	505734.749368	45.499546
3502.663233	505720.766244	45.504551
3502.122110	505697.039416	45.509556
3502.234673	505681.080585	45.514561
3502.318873	505653.775523	45.519565
3502.500973	505652.334641	45.524570
3502.520777	505631.648147	45.529575
3502.635766	505614.326786	45.534580
3502.395035	505585.861420	45.539585
3502.161503	505567.433944	45.544589
3502.267373	505555.259581	45.549594
3502.651049	505532.901997	45.554599
3502.647064	505518.777238	45.559604
3502.372593	505494.958132	45.564609
3502.795912	505464.875756	45.569613
3502.343278	505444.817435	45.574618
3502.653588	505427.818590	45.579623
3502.401803	505409.242406	45.584628
3502.522402	505387.682256	45.589633
3502.347411	505362.132209	45.594637
3501.866878	505348.131886	45.599642
3502.462158	505330.180511	45.604647
3502.183417	505322.757501	45.609652
3502.359572	505299.170635	45.614657
3502.440599	505281.702811	45.619661
3501.808255	505270.248464	45.624666
3502.155088	505258.742632	45.629671
3502.032728	505251.850185	45.634676
3502.518980	505235.530015	45.639681
3502.525080	505215.198192	45.644685
3502.153143	505203.047433	45.649690
3502.365140	505171.483861	45.654695
3502.497637	505151.434972	45.659700
3502.632442	505139.861142	45.664705
3502.623616	505124.071927	45.669709
3502.556223	505100.623532	45.674714
3502.793219	505086.259050	45.679719
3502.982503	505066.957945	45.684724
3502.439354	505040.304278	45.689729
3502.790171	505014.722238	45.694733
3502.727623	504996.418767	45.699738
3503.020408	504965.598913	45.704743
3502.885620	504958.254211	45.709748
3502.408284	504919.532593	45.714753
3502.846237	504898.578171	45.719757
3502.806684	504879.665573	45.724762
3502.710977	504847.392420	45.729767
3502.346372	504831.052845	45.734772
3502.697375	504812.079383	45.739777
3502.648954	504774.249182	45.744781
3502.593002	504764.571396	45.749786
3502.440446	504736.040166	45.754791
3502.499415	504714.690396	45.759796
3502.569947	504694.650512	45.764801
3502.212859	504672.003254	45.769805
3502.410863	504660.570555	45.774810
3502.210339	504624.125797	45.779815
3501.870154	504567.673614	45.784820
3502.027143	504445.405677	45.789825
3501.851989	504295.389338	45.794829
3501.110844	504087.893018	45.799834
3501.666360	503831.806942	45.804839
3500.798265	503542.234158	45.809844
3500.554331	503189.438211	45.814849
3500.079804	502799.533010	45.819853
3499.604502	502366.677038	45.824858
3499.359117	501879.779718	45.829863
3498.589687	501353.637502	45.834868
3497.835740	500766.866252	45.839873
3497.328179	500150.712004	45.844877
3496.165209	499491.028776	45.849882
3495.361468	498777.861428	45.854887
3494.164029	498028.329098	45.859892
3493.395251	497233.919250	45.864897
3492.826228	496397.790111	45.869901
3491.373377	495519.497589	45.874906
3490.498199	494584.519519	45.879911
3488.906545	493626.117018	45.884916
3487.760871	492614.365028	45.889921
3486.469076	491565.907772	45.894925
3485.227451	490491.312188	45.899930
3483.744788	489365.669866	45.904935
3482.043011	488213.209713	45.909940
3480.708968	487004.184889	45.914945
3479.251746	485766.694668	45.919949
3477.378124	484487.744391	45.924954
3475.663070	483177.036369	45.929959
3474.130962	481831.174020	45.934964
3472.696391	480443.845689	45.939969
3470.833778	479027.908671	45.944973
3468.462155	477574.321721	45.949978
3466.769973	476082.890360	45.954983
3464.913849	474578.253265	45.959988
3462.963345	473024.249599	45.964993
3461.032082	471441.426583	45.969997
3458.822757	469838.975470	45.975002
3456.659107	468185.386394	45.980007
3454.346438	466521.945169	45.985012
3452.471633	464802.934972	45.990017
3450.511207	463068.536187	45.995021
3447.650003	461318.568731	46.000026
3445.536913	459520.643882	46.005031
3443.276301	457721.238667	46.010036
3440.959843	455893.163944	46.015041
3438.394625	454030.571265	46.020045
3435.988428	452144.017589	46.025050
3433.823672	450230.902406	46.030055
3431.274625	448283.063927	46.035060
3428.572603	446329.875192	46.040065
3426.140454	444345.596388	46.045069
3423.130285	442337.289776	46.050074
3421.034145	440308.364259	46.055079
3417.959606	438262.453109	46.060084
3415.099681	436196.530275	46.065089
3412.478327	434102.785106	46.070093
3409.542730	431989.607213	46.075098
3407.116192	429867.557596	46.080103
3403.720761	427726.273036	46.085108
3401.077896	425560.058212	46.090113
3398.123162	423375.815680	46.095117
3395.280889	421176.974527	46.100122
3392.019543	418960.015449	46.105127
3389.160527	416732.160603	46.110132
3386.035091	414474.799326	46.115137
3383.049113	412226.460748	46.120141
3379.771067	409945.875813	46.125146
3377.155128	407653.638171	46.130151
3373.599591	405348.474428	46.135156
3370.902267	403033.554351	46.140161
3367.780988	400691.214676	46.145165
3364.186519	398351.097241	46.150170
3361.462665	395978.938692	46.155175
3358.145224	393606.534838	46.160180
3354.892746	391229.065112	46.165185
3351.740179	388830.685061	46.170189
3348.126294	386423.081974	46.175194
3345.129527	383982.856139	46.180199
3341.504445	381566.645129	46.185204
3337.858291	379128.271543	46.190209
3334.738215	376676.257640	46.195213
3331.244011	374228.168092	46.200218
3327.822150	371755.893695	46.205223
3324.520528	369298.750970	46.210228
3320.700662	366808.675272	46.215233
3317.429337	364324.448156	46.220237
3313.896404	361826.659726	46.225242
3310.672520	359321.142966	46.230247
3306.948867	356814.684616	46.235252
3303.111629	354304.635666	46.240257
3300.091354	351778.602157	46.245261
3296.175436	349262.475751	46.250266
3292.741505	346723.913057	46.255271
3289.203372	344190.005982	46.260276
3285.621733	341654.418785	46.265281
3281.727372	339114.374417	46.270285
3278.195286	336562.904621	46.275290
3274.611378	333997.634034	46.280295
3271.119094	331451.504475	46.285300
3266.953277	328894.933792	46.290305
3263.785730	326329.800647	46.295309
3259.864019	323765.640150	46.300314
3255.469755	321200.504754	46.305319
3252.052243	318636.615356	46.310324
3248.689123	316072.186179	46.315329
3244.871405	313507.478616	46.320333
3240.630898	310939.056544	46.325338
3236.909659	308364.842894	46.330343
3233.135376	305799.359671	46.335348
3229.277779	303226.481546	46.340353
3225.835054	300666.571716	46.345357
3221.871899	298098.783190	46.350362
3218.104040	295520.487716	46.355367
3214.546753	292964.700864	46.360372
3210.431513	290379.466146	46.365377
3206.765643	287816.534353	46.370381
3202.534958	285260.591620	46.375386
3198.758920	282697.201711	46.380391
3194.671301	280141.355744	46.385396
3190.697849	277579.549095	46.390401
3186.902076	275031.075236	46.395405
3182.671212	272498.555609	46.400410
3178.689461	269948.863653	46.405415
3174.980492	267413.013039	46.410420
3171.010024	264883.911080	46.415425
3166.936601	262359.780491	46.420429
3162.604833	259852.694898	46.425434
3159.136660	257317.791910	46.430439
3154.856955	254805.503397	46.435444
3150.575507	252299.587952	46.440449
3146.512678	249797.341396	46.445453
3142.408894	247311.949421	46.450458
3138.693981	244824.936280	46.455463
3134.435372	242356.239600	46.460468
3130.669061	239879.317123	46.465473
3126.495833	237417.132176	46.470477
3122.333604	234978.486863	46.475482
3118.391415	232526.651917	46.480487
3114.041016	230087.859725	46.485492
3109.937155	227662.979898	46.490497
3105.902666	225242.390794	46.495501
3101.486448	222835.054780	46.500506
3097.681065	220425.131876	46.505511
3093.787108	218041.106699	46.510516
3089.503542	215667.849737	46.515521
3085.321465	213295.584136	46.520525
3081.266047	210933.146757	46.525530
3077.071397	208572.610436	46.530535
3073.166557	206242.028117	46.535540
3068.373725	203907.636947	46.540545
3064.169318	201581.332835	46.545549
3059.414815	199286.648850	46.550554
3055.576360	196991.423460	46.555559
3051.329767	194712.851577	46.560564
3046.897391	192448.405035	46.565569
3042.394610	190209.298094	46.570573
3038.155788	187978.647918	46.575578
3033.944311	185764.056372	46.580583
3029.230251	183570.649346	46.585588
3024.550765	181394.550461	46.590593
3020.151394	179227.625815	46.595597
3015.355150	177082.878934	46.600602
3010.840892	174962.687391	46.605607
3006.336332	172867.755962	46.610612
3001.522046	170790.445777	46.615617
2996.705160	168737.787386	46.620621
2992.277455	166716.224438	46.625626
2987.744282	164701.406814	46.630631
2982.803442	162722.670877	46.635636
2977.485107	160771.062835	46.640641
2972.903145	158833.833860	46.645645
2967.903054	156948.454620	46.650650
2962.505909	155081.536322	46.655655
2957.436617	153181.246149	46.660660
2951.878454	151375.242529	46.665665
2946.279194	149609.186462	46.670669
2939.988602	147913.627751	46.675674
2934.060505	146254.600055	46.680679
2927.606351	144657.446087	46.685684
2920.608351	143116.094495	46.690689
2914.049032	141633.721680	46.695693
2906.987269	140213.128675	46.700698
2900.605793	138856.976569	46.705703
2893.988503	137555.492227	46.710708
2887.903609	136317.546579	46.715713
2882.068808	135125.902752	46.720717
2876.528247	133979.176727	46.725722
2871.488736	132883.668343	46.730727
2866.082529	131845.373434	46.735732
2861.193895	130822.567271	46.740737
2856.254423	129846.056752	46.745741
2851.366361	128911.320171	46.750746
2846.762098	127991.747450	46.755751
2842.310060	127127.882182	46.760756
2838.002814	126286.754231	46.765761
2834.002471	125453.608678	46.770765
2829.430844	124659.157367	46.775770
2825.518102	123867.646160	46.780775
2821.617991	123096.243275	46.785780
2817.566136	122357.284142	46.790785
2814.203287	121618.269805	46.795789
2810.285984	120913.031397	46.800794
2806.432764	120197.138831	46.805799
2802.542062	119509.433408	46.810804
2798.903407	118821.065269	46.815809
2795.367249	118135.580268	46.820813
2791.386154	117478.763083	46.825818
2787.845869	116819.205691	46.830823
2784.042055	116167.101558	46.835828
2779.769383	115530.734740	46.840833
2776.668529	114896.625173	46.845837
2772.647361	114278.169562	46.850842
2768.766146	113674.591864	46.855847
2764.838974	113070.967780	46.860852
2760.903943	112482.358163	46.865857
2757.041492	111886.054730	46.870861
2753.089927	111316.932477	46.875866
2749.511522	110751.588157	46.880871
2745.351433	110192.280701	46.885876
2741.491155	109641.796802	46.890881
2738.086913	109107.421935	46.895885
2734.346809	108571.480244	46.900890
2731.105633	108034.464865	46.905895
2727.059042	107505.287090	46.910900
2723.409067	106987.624157	46.915905
2720.142975	106462.586995	46.920909
2716.357558	105945.863503	46.925914
2713.139621	105429.021433	46.930919
2709.779103	104919.429742	46.935924
2706.171272	104408.498694	46.940929
2702.813825	103894.752681	46.945933
2699.480864	103384.277543	46.950938
2695.987980	102863.640920	46.955943
2692.875567	102357.977441	46.960948
2688.954946	101849.524058	46.965953
2685.750491	101330.112426	46.970957
2682.552837	100827.612558	46.975962
2679.132092	100315.343045	46.980967
2675.771496	99795.827684	46.985972
2671.883819	99283.863245	46.990977
2669.330221	98761.938542	46.995981
2665.734853	98243.260089	47.000986
2662.240217	97718.690147	47.005991
2658.984774	97198.806604	47.010996
2655.329652	96680.162997	47.016001
2652.082674	96142.719612	47.021005
2648.503382	95629.025104	47.026010
2645.136328	95094.858978	47.031015
2641.970745	94564.343200	47.036020
2638.311602	94025.742408	47.041025
2635.306249	93500.684166	47.046029
2631.536895	92962.169967	47.051034
2628.022463	92434.172234	47.056039
2624.878818	91894.232577	47.061044
2621.628950	91354.077636	47.066049
2617.991657	90805.568471	47.071053
2614.365799	90268.197896	47.076058
2610.851656	89723.767919	47.081063
2607.424202	89174.557132	47.086068
2603.931789	88645.974452	47.091073
2600.904664	88089.161849	47.096077
2597.330107	87540.156723	47.101082
2594.189675	86984.411729	47.106087
2590.433107	86439.343118	47.111092
2586.805844	85888.484249	47.116097
2583.640801	85327.616843	47.121101
2580.369739	84772.252037	47.126106
2576.574906	84213.968771	47.131111
2573.151447	83662.371192	47.136116
2569.598628	83096.132668	47.141121
2566.617919	82530.095835	47.146125
2562.808609	81971.807921	47.151130
2559.281192	81402.042651	47.156135
2556.182178	80842.891747	47.161140
2552.405957	80270.939948	47.166145
2549.098951	79702.622922	47.171149
2545.587184	79133.333306	47.176154
2542.111393	78559.934762	47.181159
2538.525168	77987.911580	47.186164
2535.399862	77423.016903	47.191169
2532.042304	76845.304990	47.196173
2528.318337	76275.726640	47.201178
2524.489808	75688.867229	47.206183
2521.228141	75110.732837	47.211188
2517.548157	74533.475984	47.216193
2514.412415	73955.448435	47.221197
2510.557318	73381.507208	47.226202
2507.341856	72802.590073	47.231207
2503.496416	72226.551725	47.236212
2499.919040	71632.250651	47.241217
2496.666092	71058.380377	47.246221
2493.083855	70490.992202	47.251226
2489.359732	69900.289321	47.256231
2486.280641	69326.220559	47.261236
2482.528665	68747.673248	47.266241
2479.415021	68157.461012	47.271245
2475.652531	67572.016186	47.276250
2472.178035	66991.287920	47.281255
2468.842942	66406.101602	47.286260
2465.614956	65829.404776	47.291265
2461.955074	65237.586827	47.296269
2458.356503	64642.606050	47.301274
2454.923173	64064.369350	47.306279
2451.640216	63461.008633	47.311284
2448.159051	62884.983559	47.316289
2444.582209	62287.865837	47.321293
2441.157512	61695.047933	47.326298
2437.231227	61100.811944	47.331303
2434.245400	60506.393182	47.336308
2430.306452	59909.579800	47.341313
2427.231910	59315.831993	47.346317
2423.709164	58726.292989	47.351322
2420.361186	58127.438855	47.356327
2417.008662	57530.427680	47.361332
2413.463596	56932.135163	47.366337
2410.102341	56322.909455	47.371341
2406.429328	55714.458397	47.376346
2403.406223	55119.714769	47.381351
2399.860060	54514.605562	47.386356
2396.109131	53895.846551	47.391361
2392.731017	53288.452368	47.396365
2388.861647	52681.772053	47.401370
2385.501006	52083.072141	47.406375
2382.272031	51473.145364	47.411380
2378.512880	50860.709978	47.416385
2375.605839	50242.944064	47.421389
2371.882079	49637.195985	47.426394
2368.198776	49022.241372	47.431399
2364.790067	48409.429747	47.436404
2361.168624	47792.462583	47.441409
2357.609851	47173.891445	47.446413
2354.351319	46569.871179	47.451418
2350.638157	45959.405533	47.456423
2347.570409	45336.578182	47.461428
2343.823788	44725.231718	47.466433
2340.358054	44104.675774	47.471437
2336.939148	43479.919195	47.476442
2333.239897	42866.625216	47.481447
2329.876801	42250.620043	47.486452
2326.340071	41622.142385	47.491457
2322.729488	41010.572913	47.496461
2319.338986	40391.675757	47.501466
2315.323085	39769.006914	47.506471
2312.477956	39153.471130	47.511476
2308.792658	38531.908527	47.516481
2305.483854	37910.546134	47.521485
2301.885179	37280.758169	47.526490
2298.427541	36663.398194	47.531495
2294.725236	36039.571134	47.536500
2291.067419	35422.290899	47.541505
2288.027972	34804.729535	47.546509
2283.986232	34187.868278	47.551514
2280.718278	33561.143485	47.556519
2277.146054	32941.862421	47.561524
2273.344991	32323.966262	47.566529
2270.050053	31703.918130	47.571533
2266.375867	31086.995901	47.576538
2262.592798	30478.208257	47.581543
2259.119930	29861.170794	47.586548
2255.563948	29248.397916	47.591553
2252.475623	28631.850764	47.596557
2248.269980	28021.053353	47.601562
2244.877502	27413.677116	47.606567
2241.380601	26794.682722	47.611572
2237.900425	26194.814430	47.616577
2234.459720	25582.875106	47.621581
2230.514562	24971.102553	47.626586
2226.742296	24372.100571	47.631591
2223.048594	23781.232574	47.636596
2219.208246	23197.367265	47.641601
2215.558803	22610.150806	47.646605
2211.309370	22038.356379	47.651610
2206.498016	21472.221412	47.656615
2202.231014	20920.378227	47.661620
2197.949066	20386.922319	47.666625
2194.227065	19855.103981	47.671629
2190.287138	19334.678132	47.676634
2186.398682	18818.058420	47.681639
2182.231448	18319.318642	47.686644
2178.277060	17826.151000	47.691649
2174.826223	17347.633003	47.696653
2170.842945	16869.235041	47.701658
2167.257827	16399.618358	47.706663
2163.183767	15927.651078	47.711668
2159.464967	15468.796296	47.716673
2155.660689	15012.530491	47.721677
2151.848140	14559.097949	47.726682
2147.936272	14122.519608	47.731687
2144.328811	13673.771589	47.736692
2140.527098	13251.968909	47.741697
2137.032664	12827.382952	47.746701
2133.567094	12423.167902	47.751706
2129.755392	12011.379525	47.756711
2126.195891	11598.212311	47.761716
2121.632319	11211.760654	47.766721
2117.819692	10828.283365	47.771725
2113.593808	10458.958447	47.776730
2109.629461	10099.023678	47.781735
2105.871808	9738.601541	47.786740
2101.946434	9408.007762	47.791745
2098.048771	9057.230576	47.796749
2093.988402	8739.701151	47.801754
2090.054722	8418.837193	47.806759
2086.258876	8102.648047	47.811764
2082.517361	7799.198390	47.816769
2079.017573	7503.932472	47.821773
2074.886616	7219.245537	47.826778
2071.216931	6929.322922	47.831783
2068.023083	6640.492334	47.836788
2063.611652	6371.195965	47.841793
2060.206119	6101.133046	47.846797
2056.890850	5836.411612	47.851802
2052.775319	5578.521349	47.856807
2049.842028	5310.830255	47.861812
2046.015257	5061.950047	47.866817
2042.814471	4808.602419	47.871821
2039.320460	4553.860945	47.876826
2035.944817	4301.060257	47.881831
2032.815777	4051.316346	47.886836
2029.119949	3797.072588	47.891841
2025.537109	3534.752122	47.896845
2022.061265	3296.673014	47.901850
2018.722625	3047.950180	47.906855
2015.437767	2792.644049	47.911860
2011.306278	2553.680075	47.916865
2008.162738	2311.211567	47.921869
2004.476297	2069.422505	47.926874
2000.926998	1833.551067	47.931879
1997.340347	1595.030802	47.936884
1993.415269	1368.197035	47.941889
1990.148126	1141.934498	47.946893
1986.267663	912.290032	47.951898
1982.293009	691.120078	47.956903
1978.492872	486.810833	47.961908
1974.127498	288.669470	47.966913
1969.271146	111.847935	47.971917
1959.166811	102.733449	47.976922
1950.033421	111.387157	47.981927
1944.624800	105.923611	47.986932
1940.459262	108.906715	47.991937
1938.197740	107.354106	47.996941
1936.178179	111.350967	48.001946
1933.429409	120.263846	48.006951
1931.388474	106.952162	48.011956
1928.341357	113.798107	48.016961
1925.177016	110.699746	48.021965
1921.752244	113.637165	48.026970
1918.127929	112.065703	48.031975
1914.982712	106.939588	48.036980
1911.422499	106.335740	48.041985
1908.374979	99.425905	48.046989
1904.925383	105.398027	48.051994
1901.392338	104.451434	48.056999
1898.659267	105.373479	48.062004
1895.262210	107.395435	48.067009
1891.091507	99.303174	48.072013
1887.861739	111.369204	48.077018
1884.733345	113.741649	48.082023
1880.809304	110.258498	48.087028
1877.737998	114.172279	48.092033
1874.654501	114.870457	48.097037
1871.208404	113.223807	48.102042
1867.840715	113.203760	48.107047
1864.328242	107.834256	48.112052
1861.068171	108.224562	48.117057
1857.677175	109.293298	48.122061
1853.872147	106.709106	48.127066
1850.434218	107.146077	48.132071
1846.934255	102.429519	48.137076
1843.167939	114.946047	48.142081
1840.097528	109.090134	48.147085
1836.611448	111.556214	48.152090
1833.269361	105.995683	48.157095
1829.972217	94.132369	48.162100
1826.352470	105.629510	48.167105
1822.999264	108.796238	48.172109
1819.632868	109.472011	48.177114
1816.009434	107.941551	48.182119
1812.533660	104.439262	48.187124
1809.092496	114.867753	48.192129
1805.574706	112.593196	48.197133
1802.097182	104.288662	48.202138
1798.644616	108.024505	48.207143
1795.134816	105.258331	48.212148
1791.658030	98.855078	48.217153
1788.105100	103.881518	48.222157
1784.717176	103.333123	48.227162
1781.116004	106.490990	48.232167
1778.106561	94.247555	48.237172
1774.372930	102.677800	48.242177
1771.016725	89.729047	48.247181
1767.856032	97.497487	48.252186
1764.062938	96.803350	48.257191
1760.897319	93.879212	48.262196
1757.007872	99.362982	48.267201
1752.898986	102.432193	48.272205
1750.246252	106.964194	48.277210
1746.339479	102.532424	48.282215
1742.932199	99.687027	48.287220
1739.939254	106.999098	48.292225
1736.189759	103.994995	48.297229
1732.693635	99.325310	48.302234
1728.794924	99.748586	48.307239
1725.592797	98.718869	48.312244
1722.495397	103.617466	48.317249
1718.767055	103.027149	48.322253
1715.536910	103.444446	48.327258
1711.744029	106.825141	48.332263
1708.338132	93.267208	48.337268
1704.620760	107.123852	48.342273
1701.213715	99.555002	48.347277
1698.353178	96.978852	48.352282
1694.235944	101.770425	48.357287
1690.756096	105.725652	48.362292
1686.965485	106.334584	48.367297
1683.452246	107.729239	48.372301
1680.251752	99.644197	48.377306
1676.872829	101.894295	48.382311
1673.828493	97.198594	48.387316
1670.038396	98.259859	48.392321
1666.770962	91.358977	48.397325
1663.119394	98.694462	48.402330
1659.374874	106.661340	48.407335
1656.022938	101.858493	48.412340
1652.388648	109.153329	48.417345
1648.921456	96.544568	48.422349
1645.797543	99.280153	48.427354
1641.913877	107.012428	48.432359
1638.531114	103.498848	48.437364
1634.991603	101.173909	48.442369
1631.455216	105.254997	48.447373
1628.126018	97.791100	48.452378
1624.215946	103.689370	48.457383
1620.509247	95.319299	48.462388
1617.507594	100.240961	48.467393
1614.233585	100.804297	48.472397
1611.048723	102.480037	48.477402
1607.064689	104.001757	48.482407
1603.616072	92.054496	48.487412
1599.871948	97.060081	48.492417
1596.718967	97.629890	48.497421
1593.312985	104.012844	48.502426
1589.411734	108.704372	48.507431
1586.183812	99.199944	48.512436
1582.195287	102.452913	48.517441
1578.672065	107.060293	48.522445
1575.701612	106.522871	48.527450
1572.149645	95.838200	48.532455
1568.915562	98.331513	48.537460
1564.657960	101.313156	48.542465
1561.120060	96.567741	48.547469
1557.925299	93.762054	48.552474
1554.312335	105.473269	48.557479
1551.532154	95.693520	48.562484
1548.093748	103.191983	48.567489
1544.361516	97.654252	48.572493
1541.008793	95.993105	48.577498
1536.921178	104.810640	48.582503
1533.834725	94.746375	48.587508
1529.874322	99.057975	48.592513
1526.491793	94.857849	48.597517
1523.312990	91.008824	48.602522
1519.463762	94.923476	48.607527
1516.117293	91.929439	48.612532
1512.471546	99.846144	48.617537
1509.087548	98.291106	48.622541
1505.731779	93.504697	48.627546
1501.924286	97.086993	48.632551
1499.240651	85.634450	48.637556
1495.527958	96.766406	48.642561
1491.752740	93.604990	48.647565
1488.020014	88.507102	48.652570
1484.448167	102.040535	48.657575
1481.099695	95.123820	48.662580
1477.442448	109.141942	48.667585
1474.100729	105.786505	48.672589
1470.516192	102.006962	48.677594
1467.241084	102.953288	48.682599
1463.835587	98.823182	48.687604
1459.997853	105.719424	48.692609
1456.469051	107.097538	48.697613
1453.333965	106.914775	48.702618
1449.999183	104.716178	48.707623
1446.980726	98.988272	48.712628
1442.785757	98.302937	48.717633
1439.181142	93.463521	48.722637
1435.934063	99.790109	48.727642
1432.074821	107.575538	48.732647
1428.591075	93.618499	48.737652
1425.000128	98.635054	48.742657
1421.163006	104.461871	48.747661
1418.074505	104.993185	48.752666
1414.393118	103.490772	48.757671
1411.623214	100.682246	48.762676
1407.708423	96.169518	48.767681
1404.088698	96.454492	48.772685
1400.698564	88.297778	48.777690
1396.737143	97.181093	48.782695
1393.464327	87.696347	48.787700
1389.894101	96.525101	48.792705
1386.769539	86.390869	48.797709
1383.450035	87.739575	48.802714
1379.701554	93.489320	48.807719
1376.027136	93.238654	48.812724
1372.671234	94.795503	48.817729
1369.165368	91.715564	48.822733
1366.026236	89.777586	48.827738
1362.137440	89.392612	48.832743
1358.872621	81.852307	48.837748
1355.227801	93.059116	48.842753
1351.445189	93.885132	48.847757
1348.277853	98.845248	48.852762
1344.910966	97.391967	48.857767
1341.342406	89.044739	48.862772
1337.787903	89.816268	48.867777
1334.206313	87.067655	48.872781
1330.445456	84.856300	48.877786
1326.929629	93.221014	48.882791
1323.281718	90.175845	48.887796
1320.283913	92.613416	48.892801
1316.671335	88.600984	48.897805
1313.199208	87.268490	48.902810
1309.917027	90.993657	48.907815
1306.094742	84.400655	48.912820
1302.394097	92.658098	48.917825
1298.804778	88.920453	48.922829
1295.583879	87.023684	48.927834
1292.247919	90.595875	48.932839
1289.014848	79.168783	48.937844
1285.330732	89.495873	48.942849
1281.688994	88.101199	48.947853
1278.105829	89.608010	48.952858
1274.468050	81.847364	48.957863
1271.114042	82.954682	48.962868
1267.508307	92.447013	48.967873
1264.010703	89.394275	48.972877
1260.979076	88.755674	48.977882
1257.183166	98.533868	48.982887
1253.479759	89.935567	48.987892
1250.143336	85.889652	48.992897
1246.587351	79.002116	48.997901
1243.043699	85.093300	49.002906
1239.383324	93.157820	49.007911
1235.723976	88.950203	49.012916
1232.775524	86.254910	49.017921
1229.020623	88.810330	49.022925
1225.969660	81.742950	49.027930
1222.225217	86.922609	49.032935
1218.943710	83.175030	49.037940
1215.058746	88.063357	49.042945
1211.611815	97.584756	49.047949
1208.083969	85.789115	49.052954
1204.484133	87.871156	49.057959
1201.276333	87.339075	49.062964
1197.546228	88.036713	49.067969
1193.776941	91.777598	49.072973
1190.605735	86.089326	49.077978
1186.667969	92.460157	49.082983
1183.429334	80.002587	49.087988
1179.881774	90.074311	49.092993
1176.850521	89.903886	49.097997
1173.325561	78.718400	49.103002
1169.519023	81.550776	49.108007
1166.481149	82.861991	49.113012
1162.763484	87.550278	49.118017
1158.797759	93.150357	49.123021
1155.684807	84.997997	49.128026
1151.558901	89.642264	49.133031
1148.420809	82.847881	49.138036
1145.039687	89.318726	49.143041
1141.608886	85.768398	49.148045
1138.418392	86.236520	49.153050
1134.203447	86.462314	49.158055
1131.072917	85.342420	49.163060
1127.558068	79.669686	49.168065
1123.642648	90.345989	49.173069
1120.407196	84.746822	49.178074
1117.199301	86.204726	49.183079
1113.684687	81.835398	49.188084
1110.445646	88.473950	49.193089
1106.427916	80.313741	49.198093
1103.136274	84.208070	49.203098
1099.576852	88.058661	49.208103
1096.071719	89.043989	49.213108
1092.810587	85.695044	49.218113
1088.704503	81.269092	49.223117
1085.658041	83.217552	49.228122
1082.082827	91.686429	49.233127
1078.695427	93.105841	49.238132
1074.992508	87.468714	49.243137
1071.026837	91.657785	49.248141
1068.082574	86.237921	49.253146
1064.608982	101.505575	49.258151
1060.836610	87.492313	49.263156
1057.246137	92.024771	49.268161
1053.701470	89.093280	49.273165
1050.646359	83.975406	49.278170
1047.010111	84.335755	49.283175
1043.706834	86.289394	49.288180
1040.269335	84.065709	49.293185
1036.319226	89.948098	49.298189
1032.749094	94.306553	49.303194
1028.984911	88.805518	49.308199
1026.144080	85.840402	49.313204
1022.804379	85.502874	49.318209
1019.064237	84.851199	49.323213
1015.293758	91.161200	49.328218
1011.500202	93.795423	49.333223
1008.467069	88.648823	49.338228
1004.827097	90.224613	49.343233
1001.448286	87.397024	49.348237
998.155791	92.114053	49.353242
994.088722	95.787416	49.358247
991.165488	85.881341	49.363252
987.752001	82.223938	49.368257
984.019771	84.712579	49.373261
980.322650	80.434954	49.378266
976.794401	90.880156	49.383271
973.272937	83.572848	49.388276
969.494413	87.875162	49.393281
966.177946	88.603350	49.398285
963.382392	85.150313	49.403290
959.517256	95.511919	49.408295
956.159133	85.565981	49.413300
952.776813	89.240323	49.418305
948.863763	94.632907	49.423309
945.076128	90.945166	49.428314
941.579645	87.325998	49.433319
938.407623	82.153574	49.438324
935.167681	91.484573	49.443329
931.552215	90.626844	49.448333
927.995092	83.881904	49.453338
923.904973	93.864089	49.458343
921.110995	87.576147	49.463348
917.330671	80.647660	49.468353
913.645334	93.151567	49.473357
910.532645	86.454504	49.478362
907.152370	81.978876	49.483367
903.405417	79.018787	49.488372
899.982464	82.209086	49.493377
896.072211	89.233699	49.498381
892.813418	82.524583	49.503386
889.126943	87.442148	49.508391
885.700405	80.208664	49.513396
882.745116	79.887242	49.518401
878.664819	78.098990	49.523405
875.495401	75.308427	49.528410
871.546001	87.106806	49.533415
868.486263	80.857080	49.538420
864.685969	81.420153	49.543425
861.237932	87.458513	49.548429
857.802702	79.195026	49.553434
854.172084	92.493992	49.558439
850.882227	86.001684	49.563444
847.428924	90.136327	49.568449
844.089125	82.598289	49.573453
840.504361	82.593151	49.578458
836.818388	80.686577	49.583463
833.653332	76.525465	49.588468
829.588008	76.063637	49.593473
826.137789	89.828054	49.598477
823.124198	74.880514	49.603482
819.422362	82.100472	49.608487
815.935847	75.417329	49.613492
812.040026	79.671477	49.618497
808.447548	77.740862	49.623501
805.288403	79.871398	49.628506
801.761922	89.063511	49.633511
798.470708	79.698800	49.638516
794.983693	82.063869	49.643521
791.131154	86.206881	49.648525
787.852858	78.466296	49.653530
783.829524	87.115670	49.658535
780.665879	89.129853	49.663540
777.284592	85.049862	49.668545
773.629161	83.344181	49.673549
770.627444	83.241964	49.678554
766.796593	81.522464	49.683559
763.151362	81.314783	49.688564
759.650598	85.738388	49.693569
755.949783	80.793838	49.698573
752.879251	76.016924	49.703578
749.119384	87.893369	49.708583
745.800820	75.169935	49.713588
742.282886	83.139537	49.718593
738.652601	79.319772	49.723597
735.840582	77.302476	49.728602
731.512210	95.427110	49.733607
728.148984	88.731112	49.738612
724.785250	90.045637	49.743617
721.320744	88.044493	49.748621
717.841020	78.959075	49.753626
713.883762	81.739032	49.758631
710.878568	82.649740	49.763636
707.089371	79.284978	49.768641
703.212016	82.909855	49.773645
699.749341	77.137324	49.778650
696.639900	84.173327	49.783655
693.231721	78.240457	49.788660
689.691201	79.478104	49.793665
685.883971	86.537313	49.798669
682.777468	78.238506	49.803674
679.180606	84.581613	49.808679
675.847368	82.259492	49.813684
672.517518	80.797365	49.818689
668.718287	84.773907	49.823693
665.243270	80.164373	49.828698
661.299413	90.490789	49.833703
657.981761	84.043969	49.838708
654.375394	79.119534	49.843713
651.073100	83.471125	49.848717
648.404867	79.742051	49.853722
644.355074	75.781969	49.858727
640.329371	82.074779	49.863732
637.396631	79.408751	49.868737
633.172712	83.394462	49.873741
630.054019	70.601979	49.878746
626.349094	81.292984	49.883751
622.919047	79.811661	49.888756
619.518175	81.366091	49.893761
616.170757	80.175619	49.898765
613.164772	77.679180	49.903770
609.352330	84.128616	49.908775
606.029068	83.766432	49.913780
601.989746	82.310358	49.918785
598.201390	79.280834	49.923789
594.614890	76.998151	49.928794
591.635206	87.038435	49.933799
588.464664	80.385235	49.938804
584.563860	81.384759	49.943809
581.028586	78.163983	49.948813
577.390114	73.200270	49.953818
574.012272	86.143517	49.958823
570.358665	81.618746	49.963828
567.011734	77.467004	49.968833
563.859927	82.921444	49.973837
560.654979	76.340043	49.978842
556.663026	76.347712	49.983847
552.870725	88.320959	49.988852
549.521593	79.278519	49.993857
545.875485	84.518852	49.998861
542.476870	81.419173	50.003866
539.114892	76.073909	50.008871
535.391480	86.318557	50.013876
532.111989	75.898573	50.018881
528.317845	82.829208	50.023885
525.180183	77.559755	50.028890
521.749014	85.275423	50.033895
518.023126	76.418190	50.038900
514.555115	73.411575	50.043905
511.141418	80.931538	50.048909
507.534692	69.629222	50.053914
503.607746	79.279145	50.058919
500.480169	77.829844	50.063924
497.043191	76.969698	50.068929
493.542479	78.663068	50.073933
489.957895	80.223966	50.078938
486.296256	74.476121	50.083943
482.996198	85.344545	50.088948
479.550415	85.090033	50.093953
475.744478	80.899034	50.098957
472.709089	74.471582	50.103962
469.168070	80.742737	50.108967
465.118269	76.213227	50.113972
461.996115	78.031161	50.118977
458.562602	74.164993	50.123981
455.094781	73.521620	50.128986
451.448796	78.360155	50.133991
448.019722	75.005812	50.138996
444.743143	68.982901	50.144001
440.639189	81.412779	50.149005
437.236630	80.604229	50.154010
434.034466	84.611228	50.159015
430.388594	85.925418	50.164020
426.764004	82.611006	50.169025
423.116570	90.970939	50.174029
420.038423	78.912486	50.179034
416.220806	72.689077	50.184039
413.182430	74.291498	50.189044
409.417941	65.800962	50.194049
405.960945	76.598905	50.199053
402.368763	71.428706	50.204058
398.696136	71.601816	50.209063
395.562462	70.659666	50.214068
392.536739	68.425752	50.219073
388.295883	71.262552	50.224077
385.206312	75.634829	50.229082
381.638606	77.028602	50.234087
377.845733	77.780404	50.239092
374.083427	75.085375	50.244097
370.334968	84.992254	50.249101
366.974501	71.573100	50.254106
363.839365	75.215337	50.259111
360.244748	82.260453	50.264116
357.063298	74.406800	50.269121
353.022682	80.831670	50.274125
350.044691	70.538792	50.279130
346.289997	71.724405	50.284135
342.796500	74.672646	50.289140
339.097354	71.515386	50.294145
335.542007	85.508135	50.299149
332.574362	71.154661	50.304154
328.822294	72.267103	50.309159
325.397893	74.597164	50.314164
321.777060	86.977148	50.319169
318.547644	81.652411	50.324173
314.884118	69.131480	50.329178
311.307577	79.603200	50.334183
307.840704	73.695357	50.339188
304.554787	72.160005	50.344193
300.576473	75.484277	50.349197
297.291954	78.263951	50.354202
293.631463	83.867205	50.359207
289.970833	83.231726	50.364212
286.612529	74.484993	50.369217
283.191777	78.079958	50.374221
279.810976	69.706879	50.379226
276.219070	77.428603	50.384231
272.798028	76.819101	50.389236
269.382450	81.280107	50.394241
265.837248	82.670392	50.399245
262.500801	69.238035	50.404250
258.575290	75.319135	50.409255
255.279911	78.059376	50.414260
251.816528	78.756736	50.419265
248.247414	80.976463	50.424269
244.845433	73.910118	50.429274
241.118041	86.120037	50.434279
237.317758	81.836454	50.439284
234.562026	80.054059	50.444289
230.812416	82.599273	50.449293
227.294259	81.293072	50.454298
223.707157	86.062354	50.459303
220.263259	75.085920	50.464308
217.263022	68.725807	50.469313
213.400903	75.562649	50.474317
209.874806	62.020636	50.479322
205.768444	76.681281	50.484327
202.332203	75.055455	50.489332
199.426846	69.120323	50.494337
195.642891	76.286674	50.499341
192.121198	71.314342	50.504346
188.650465	76.521076	50.509351
185.091263	81.615039	50.514356
181.705748	68.497218	50.519361
177.896405	73.936998	50.524365
174.889340	67.100244	50.529370
171.146717	74.706238	50.534375
167.752976	81.318309	50.539380
164.126677	78.102283	50.544385
160.430377	75.833600	50.549389
157.375874	73.911074	50.554394
153.647910	82.470217	50.559399
150.014423	70.998151	50.564404
146.963407	76.155361	50.569409
142.935146	77.953054	50.574413
139.569141	72.111795	50.579418
136.492373	66.484927	50.584423
132.966773	80.055441	50.589428
129.214000	69.908546	50.594433
125.327938	73.886010	50.599437
122.093396	78.056261	50.604442
118.799285	78.176807	50.609447
115.067803	80.247828	50.614452
111.426372	73.035298	50.619457
108.088054	80.243005	50.624461
104.671346	75.820639	50.629466
101.289093	78.296020	50.634471
97.644805	74.744295	50.639476
93.977713	76.201034	50.644481
90.306281	79.189662	50.649485
87.136495	75.934211	50.654490
83.515935	83.132081	50.659495
79.972357	82.063972	50.664500
77.026094	69.219464	50.669505
72.716576	71.143211	50.674509
69.453932	77.326767	50.679514
66.210723	76.477642	50.684519
62.570522	84.725745	50.689524
59.131095	71.834639	50.694529
55.159214	85.000093	50.699533
52.121604	69.338336	50.704538
48.912972	78.370269	50.709543
45.394001	79.516060	50.714548
41.840297	70.094307	50.719553
37.622771	84.864019	50.724557
34.253070	84.088374	50.729562
31.063557	77.121865	50.734567
27.824283	72.478905	50.739572
24.253122	76.546555	50.744577
20.191045	80.798205	50.749581
16.944109	74.274061	50.754586
13.440300	69.409708	50.759591
10.074009	72.518510	50.764596
6.600288	75.447892	50.769601
3.233156	82.618967	50.774605