Fri Aug 26 14:15:45 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.622909	106.001025	0.000000
0.425392	106.395569	0.005005
0.129405	105.103393	0.010010
0.358888	96.142943	0.015014
0.715753	97.466706	0.020019
0.187243	95.831095	0.025024
0.248621	89.892808	0.030029
-0.316891	79.341440	0.035034
-0.418935	71.562046	0.040038
-0.490988	68.507651	0.045043
-1.366117	50.253550	0.050048
-1.489225	51.392620	0.055053
-2.112367	46.408785	0.060058
-2.205814	34.505829	0.065062
-1.928241	34.348691	0.070067
-2.605582	37.060968	0.075072
-3.087416	28.869340	0.080077
-3.444880	24.340839	0.085082
-3.431747	28.328125	0.090086
-3.768875	18.054437	0.095091
-4.237080	20.534840	0.100096
-4.355297	9.322270	0.105101
-4.400686	17.437733	0.110106
-4.202433	15.644684	0.115110
-5.075378	10.411860	0.120115
-5.648171	5.243033	0.125120
-5.405539	4.249805	0.130125
-5.744058	11.335266	0.135130
-6.583402	4.692553	0.140134
-6.382024	6.502411	0.145139
-7.123547	9.696060	0.150144
-6.779061	12.825023	0.155149
-6.982806	14.549266	0.160154
-7.038329	15.937231	0.165158
-7.786016	12.181310	0.170163
-8.196548	22.533378	0.175168
-8.084961	10.873754	0.180173
-8.099671	12.268018	0.185178
-9.142151	7.615230	0.190182
-9.315872	3.931292	0.195187
-9.781615	1.298860	0.200192
-9.928810	5.842596	0.205197
-9.890630	7.513354	0.210202
-9.702992	8.085201	0.215206
-9.783805	9.489758	0.220211
-9.934286	12.034583	0.225216
-10.337108	5.690889	0.230221
-10.893827	11.253808	0.235226
-11.172333	8.459350	0.240230
-11.255369	4.027327	0.245235
-12.160469	20.103504	0.250240
-12.457443	5.612757	0.255245
-12.720371	9.589239	0.260250
-12.701577	7.609004	0.265254
-12.565964	12.383946	0.270259
-12.969413	13.946300	0.275264
-12.686015	10.463263	0.280269
-13.100642	16.598826	0.285274
-13.909175	5.604467	0.290278
-14.163349	11.787810	0.295283
-14.002484	12.120226	0.300288
-14.318778	10.565473	0.305293
-14.468971	3.328262	0.310298
-15.213539	9.676540	0.315302
-15.295130	5.785275	0.320307
-15.775715	11.013649	0.325312
-15.802240	1.972888	0.330317
-15.729506	9.307516	0.335322
-16.175999	9.984424	0.340326
-16.801438	5.621033	0.345331
-17.093123	9.061008	0.350336
-16.710721	9.165949	0.355341
-17.028891	9.016147	0.360346
-17.369028	10.593953	0.365350
-17.458884	4.808951	0.370355
-18.477946	11.696660	0.375360
-18.373680	0.313420	0.380365
-18.469521	4.355631	0.385370
-18.579300	11.209330	0.390374
-18.748900	0.802006	0.395379
-19.366097	9.534821	0.400384
-19.557523	5.714440	0.405389
-19.869085	8.426708	0.410394
-20.309856	10.535856	0.415398
-19.999820	9.244241	0.420403
-20.216735	14.839674	0.425408
-20.320771	14.495186	0.430413
-21.269844	19.834468	0.435418
-21.698971	13.444249	0.440422
-21.530532	7.185612	0.445427
-21.550303	18.489203	0.450432
-21.617246	8.445529	0.455437
-22.398883	12.929865	0.460442
-22.841831	7.620603	0.465446
-23.103715	8.252949	0.470451
-23.524466	17.682821	0.475456
-23.236495	4.809372	0.480461
-23.233097	15.837281	0.485466
-23.368934	6.253572	0.490470
-23.486020	3.731365	0.495475
-24.152952	10.415556	0.500480
-24.509326	10.214757	0.505485
-24.584454	15.256621	0.510490
-25.489642	11.066495	0.515494
-25.701630	6.822223	0.520499
-26.114666	9.616727	0.525504
-26.143121	9.152908	0.530509
-26.281556	5.197730	0.535514
-26.157408	8.889326	0.540518
-25.961502	9.175158	0.545523
-26.421547	14.723026	0.550528
-26.678883	12.482074	0.555533
-27.365389	6.704551	0.560538
-27.712940	16.290698	0.565542
-27.446897	9.770099	0.570547
-27.785663	15.498394	0.575552
-28.542945	13.955357	0.580557
-28.877760	7.930094	0.585562
-29.051184	11.614239	0.590566
-29.345946	1.966696	0.595571
-29.523428	15.053825	0.600576
-28.971875	9.513795	0.605581
-29.508476	12.441429	0.610586
-29.460236	14.550367	0.615590
-29.925481	5.236240	0.620595
-30.360329	17.610495	0.625600
-30.817239	9.626962	0.630605
-31.625033	18.727967	0.635610
-31.645497	11.065609	0.640614
-31.663395	6.199516	0.645619
-31.836648	16.403908	0.650624
-31.878586	7.773656	0.655629
-31.835659	10.867314	0.660634
-32.096330	11.455181	0.665638
-32.509373	2.936492	0.670643
-32.986212	8.686283	0.675648
-32.911670	6.820751	0.680653
-33.570042	10.374765	0.685658
-34.247303	8.221340	0.690662
-34.242298	0.181711	0.695667
-34.550379	12.260988	0.700672
-34.588431	8.283853	0.705677
-34.582330	16.261587	0.710682
-34.845277	12.838305	0.715686
-35.108515	11.711875	0.720691
-35.904440	18.960300	0.725696
-35.735532	13.024280	0.730701
-35.732828	17.513043	0.735706
-36.326494	15.498457	0.740710
-36.168577	13.762307	0.745715
-37.325644	10.652238	0.750720
-37.459561	11.388043	0.755725
-37.374894	21.830681	0.760730
-37.835516	15.521293	0.765734
-37.749573	16.770177	0.770739
-38.217938	16.308414	0.775744
-37.810646	15.821041	0.780749
-38.086289	19.590703	0.785754
-39.073778	19.889951	0.790758
-38.971869	17.912593	0.795763
-39.398746	16.742041	0.800768
-39.128903	15.013774	0.805773
-39.726796	28.327715	0.810778
-40.492364	12.176247	0.815782
-40.355571	13.050230	0.820787
-40.782878	19.387078	0.825792
-40.717963	12.989539	0.830797
-40.678647	12.591095	0.835802
-41.171115	16.432480	0.840806
-41.520076	8.109450	0.845811
-42.005940	12.886244	0.850816
-41.913976	7.661372	0.855821
-41.922010	12.202423	0.860826
-42.738988	20.055218	0.865830
-43.017036	13.866097	0.870835
-43.416234	17.123504	0.875840
-43.762000	12.485622	0.880845
-43.812350	6.976035	0.885850
-43.834650	11.987527	0.890854
-43.580070	5.854679	0.895859
-43.933824	10.981050	0.900864
-44.549586	9.080633	0.905869
-44.927225	8.854673	0.910874
-45.393758	11.404415	0.915878
-44.972584	8.184655	0.920883
-45.652022	13.039043	0.925888
-45.414657	3.843305	0.930893
-45.889540	11.098686	0.935898
-46.553252	5.285979	0.940902
-46.676449	0.876030	0.945907
-46.691367	12.330714	0.950912
-46.959331	8.477959	0.955917
-47.564217	11.621862	0.960922
-48.042680	15.979904	0.965926
-47.781466	13.275414	0.970931
-47.986108	22.450183	0.975936
-48.101975	8.307715	0.980941
-48.344499	9.490685	0.985946
-48.872440	22.838021	0.990950
-48.986308	6.199127	0.995955
-49.206981	13.165001	1.000960
-49.390185	9.454067	1.005965
-50.033430	6.431672	1.010970
-50.572786	14.342476	1.015974
-50.680167	15.150076	1.020979
-51.090097	20.408578	1.025984
-51.065304	13.707249	1.030989
-51.138855	11.118155	1.035994
-50.992219	13.926756	1.040998
-50.788438	8.693965	1.046003
-51.477365	16.928604	1.051008
-52.275742	11.222282	1.056013
-52.751197	5.946557	1.061018
-52.811682	12.571125	1.066022
-52.730262	7.430150	1.071027
-52.908939	10.526675	1.076032
-53.104975	9.566946	1.081037
-53.667360	13.216743	1.086042
-54.145328	12.544511	1.091046
-53.960755	5.878418	1.096051
-54.160426	10.050686	1.101056
-54.176952	19.151873	1.106061
-55.053441	18.677727	1.111066
-55.585772	22.636047	1.116070
-55.614811	8.353516	1.121075
-55.569015	14.268698	1.126080
-55.491073	11.368125	1.131085
-55.632204	11.564069	1.136090
-56.617849	15.852387	1.141094
-56.731159	0.035960	1.146099
-57.094960	13.952497	1.151104
-57.170529	13.046776	1.156109
-57.143542	2.384227	1.161114
-57.231667	15.881370	1.166118
-57.643305	8.947449	1.171123
-58.439856	12.921596	1.176128
-58.975180	18.386277	1.181133
-58.323623	19.376258	1.186138
-58.592316	18.728388	1.191142
-58.645999	11.109167	1.196147
-59.933578	17.393301	1.201152
-59.993612	8.126812	1.206157
-59.924608	11.959866	1.211162
-60.367086	15.739685	1.216166
-60.043091	3.537651	1.221171
-60.272063	14.914936	1.226176
-60.199234	16.453753	1.231181
-60.646634	8.658562	1.236186
-61.567194	17.558831	1.241190
-61.502125	-0.724539	1.246195
-62.278160	7.017475	1.251200
-62.450041	17.101433	1.256205
-62.868099	-2.245624	1.261210
-63.180054	3.105182	1.266214
-62.631684	6.952180	1.271219
-62.895558	19.382068	1.276224
-63.094268	12.655430	1.281229
-63.252605	9.146262	1.286234
-63.950875	7.239711	1.291238
-63.995187	2.086678	1.296243
-64.759844	6.157094	1.301248
-64.625516	5.715385	1.306253
-64.642378	3.924194	1.311258
-64.855242	4.302144	1.316262
-65.318359	0.973305	1.321267
-65.718721	3.009724	1.326272
-65.885527	4.661778	1.331277
-65.778876	7.308930	1.336282
-66.186265	18.688687	1.341286
-66.741952	7.946021	1.346291
-67.405779	7.862693	1.351296
-67.368986	8.214426	1.356301
-67.408768	5.784584	1.361306
-67.537198	7.155427	1.366310
-67.533059	6.844715	1.371315
-67.673045	12.263657	1.376320
-68.628517	6.452088	1.381325
-68.861978	6.266953	1.386330
-69.204439	16.959580	1.391334
-69.193023	18.371921	1.396339
-69.383666	22.296022	1.401344
-69.420945	6.508881	1.406349
-69.889208	14.778762	1.411354
-70.842891	21.903058	1.416358
-70.752368	14.606221	1.421363
-71.001150	14.224162	1.426368
-71.157931	12.543338	1.431373
-71.112296	12.773476	1.436378
-71.065716	15.183218	1.441382
-70.851589	8.063285	1.446387
-71.505753	17.168840	1.451392
-71.835713	7.153468	1.456397
-72.108454	10.783475	1.461402
-72.954008	21.212762	1.466406
-73.223195	16.240266	1.471411
-73.576108	13.795905	1.476416
-73.414745	20.743425	1.481421
-73.347006	7.391758	1.486426
-73.573250	6.705643	1.491430
-73.525466	10.560982	1.496435
-74.378500	11.975045	1.501440
-74.901612	8.310709	1.506445
-74.737409	9.360751	1.511450
-75.124838	7.415293	1.516454
-75.250575	0.411553	1.521459
-75.678845	11.399101	1.526464
-76.114315	5.516059	1.531469
-75.932843	4.582972	1.536474
-76.753695	6.763953	1.541478
-76.180120	8.743640	1.546483
-76.621675	2.396492	1.551488
-77.019165	2.376096	1.556493
-77.712468	11.411814	1.561498
-77.918312	5.916949	1.566502
-77.282915	4.185548	1.571507
-78.081108	9.466535	1.576512
-78.847193	3.438825	1.581517
-78.602954	-0.095058	1.586522
-79.329097	6.737549	1.591526
-79.027276	6.478561	1.596531
-78.948903	7.839350	1.601536
-79.539208	5.580643	1.606541
-80.103515	2.090395	1.611546
-80.552876	5.377755	1.616550
-80.432941	-2.496272	1.621555
-80.580027	1.933552	1.626560
-80.990291	8.631559	1.631565
-80.429242	6.721915	1.636570
-81.376174	11.586315	1.641574
-81.631114	0.417192	1.646579
-81.988523	7.638461	1.651584
-82.006555	5.407706	1.656589
-82.325608	12.379405	1.661594
-83.311069	11.862118	1.666598
-83.201123	5.973247	1.671603
-83.697245	16.269033	1.676608
-83.828886	3.309069	1.681613
-83.435436	15.320243	1.686618
-84.200064	11.775765	1.691622
-83.861132	2.175088	1.696627
-84.059755	9.023634	1.701632
-84.287070	13.288789	1.706637
-84.904184	1.929291	1.711642
-85.356002	11.867012	1.716646
-84.988034	2.872397	1.721651
-85.779278	16.592904	1.726656
-85.906877	6.473262	1.731661
-86.328838	11.527997	1.736666
-86.526441	-1.861439	1.741670
-86.628649	-4.721305	1.746675
-86.674805	4.106085	1.751680
-86.909275	6.837985	1.756685
-87.677689	9.608730	1.761690
-88.106824	9.529989	1.766694
-88.374498	5.215299	1.771699
-88.082487	11.269307	1.776704
-88.439872	-0.165429	1.781709
-88.376668	6.468349	1.786714
-88.533972	8.859216	1.791718
-89.020213	1.348479	1.796723
-89.712786	15.436422	1.801728
-89.964238	5.665084	1.806733
-89.692931	0.652729	1.811738
-90.063421	18.433115	1.816742
-90.200430	13.433714	1.821747
-90.768414	16.717399	1.826752
-90.719139	13.084161	1.831757
-91.314612	7.956834	1.836762
-91.466425	7.081967	1.841766
-91.182593	0.786386	1.846771
-92.198494	5.345159	1.851776
-92.688826	7.961878	1.856781
-92.631986	-1.164619	1.861786
-92.940771	3.296709	1.866790
-92.737633	6.115493	1.871795
-92.913692	8.332116	1.876800
-93.562395	6.022393	1.881805
-93.920061	7.163181	1.886810
-94.027657	5.237427	1.891814
-94.175149	7.503384	1.896819
-94.655246	8.935308	1.901824
-94.529235	11.380136	1.906829
-94.593105	7.666443	1.911834
-95.215472	20.585565	1.916838
-95.184180	5.157899	1.921843
-95.592343	11.355724	1.926848
-95.582177	10.553709	1.931853
-95.947061	4.507824	1.936858
-96.602493	12.465171	1.941862
-97.087833	6.406404	1.946867
-97.269133	6.263766	1.951872
-97.581900	7.138144	1.956877
-97.007569	-2.157508	1.961882
-97.535684	10.946242	1.966886
-98.039720	1.808999	1.971891
-98.426147	9.733951	1.976896
-98.913949	7.323249	1.981901
-98.818053	5.530320	1.986906
-98.486724	7.873580	1.991910
-98.854651	4.498284	1.996915
-99.515421	3.293602	2.006912
-99.329733	5.754437	2.016909
-99.013682	2.664182	2.026906
-98.258729	3.085084	2.036902
-97.994872	2.958413	2.046899
-96.922356	8.559732	2.056896
-96.629127	8.662897	2.066893
-96.331381	10.026102	2.076890
-95.875537	4.193032	2.086886
-94.899869	8.377633	2.096883
-94.725312	11.666970	2.106880
-94.617601	10.766352	2.116877
-93.447367	3.669011	2.126874
-93.651749	6.801945	2.136870
-92.638417	10.305963	2.146867
-92.094698	8.441002	2.156864
-91.811270	7.145573	2.166861
-91.122153	8.485853	2.176858
-90.749408	9.976759	2.186854
-90.323635	8.773204	2.196851
-89.473718	5.469950	2.206848
-89.619601	8.682472	2.216845
-88.769679	9.022065	2.226842
-88.217939	10.222183	2.236838
-87.500658	11.659445	2.246835
-86.844560	13.879151	2.256832
-86.654744	17.330834	2.266829
-86.604420	16.698902	2.276826
-85.575077	8.841075	2.286822
-85.369461	14.149734	2.296819
-84.669088	17.043601	2.306816
-83.919143	12.153058	2.316813
-83.948512	15.648370	2.326810
-83.219026	6.218539	2.336806
-82.552179	11.417372	2.346803
-82.391176	8.167530	2.356800
-81.454112	11.208270	2.366797
-80.818676	10.187474	2.376794
-80.633495	13.057022	2.386790
-80.469712	8.970476	2.396787
-79.535834	6.819861	2.406784
-79.133521	8.838336	2.416781
-79.039525	9.222771	2.426778
-78.362308	2.287720	2.436774
-77.838465	1.439516	2.446771
-77.003484	5.170868	2.456768
-76.936022	9.085077	2.466765
-76.246677	8.147751	2.476762
-75.684922	11.050529	2.486758
-75.050570	10.520895	2.496755
-74.702322	7.881774	2.506752
-74.272430	7.089378	2.516749
-73.771007	14.002349	2.526746
-72.837489	11.782100	2.536742
-72.558400	5.710463	2.546739
-72.489894	5.611042	2.556736
-71.538916	11.373833	2.566733
-71.176099	5.346178	2.576730
-70.654112	3.744352	2.586726
-69.815600	9.055835	2.596723
-69.580450	7.875625	2.606720
-69.648627	10.917663	2.616717
-68.570579	4.056414	2.626714
-68.061043	3.996026	2.636710
-67.574878	3.283564	2.646707
-66.819202	10.011233	2.656704
-66.632719	10.305242	2.666701
-66.579877	10.224098	2.676698
-65.775876	3.310486	2.686694
-65.274442	9.174948	2.696691
-64.249548	11.730028	2.706688
-63.714981	5.596439	2.716685
-63.501853	4.292950	2.726682
-63.466006	1.316012	2.736678
-63.095399	6.760533	2.746675
-61.907571	2.821812	2.756672
-61.342657	-0.294520	2.766669
-60.834099	-6.081944	2.776666
-60.612830	1.432157	2.786662
-60.533674	5.563116	2.796659
-59.991477	11.642971	2.806656
-59.416594	4.685839	2.816653
-58.201788	9.678984	2.826650
-58.175420	11.933385	2.836646
-57.818177	-0.698044	2.846643
-56.877232	8.763008	2.856640
-56.625040	2.483324	2.866637
-56.284024	0.649925	2.876634
-55.686687	2.641203	2.886630
-55.299509	0.927323	2.896627
-54.403302	-0.488856	2.906624
-53.984649	-4.662597	2.916621
-53.638939	-1.076805	2.926618
-52.948950	1.368866	2.936614
-52.332041	0.914805	2.946611
-52.432171	-2.069471	2.956608
-51.671952	8.132451	2.966605
-51.046707	0.451581	2.976602
-50.788407	1.060682	2.986598
-50.013493	0.547175	2.996595
-49.714803	6.173949	3.006592
-49.241511	2.343313	3.016589
-48.131286	2.354119	3.026586
-47.957288	5.561184	3.036582
-47.995619	7.024231	3.046579
-47.063125	3.454706	3.056576
-46.597669	5.013537	3.066573
-46.455076	-0.606040	3.076570
-45.236000	0.515518	3.086566
-44.936893	-3.899362	3.096563
-44.702496	1.417485	3.106560
-43.867377	-1.484334	3.116557
-43.624128	9.298577	3.126554
-43.385969	2.805674	3.136550
-42.489048	5.649933	3.146547
-42.249129	2.720413	3.156544
-41.171754	8.450855	3.166541
-40.813146	4.305466	3.176538
-40.731060	4.096229	3.186534
-40.407707	-0.322427	3.196531
-39.439710	7.544233	3.206528
-39.174429	5.804984	3.216525
-38.436038	5.930703	3.226522
-37.556397	3.699838	3.236518
-37.662189	-0.417591	3.246515
-37.691310	2.140044	3.256512
-36.636263	7.535020	3.266509
-35.961788	4.236909	3.276506
-35.069007	5.564488	3.286502
-35.115435	3.480978	3.296499
-34.487972	7.773648	3.306496
-34.425484	3.005981	3.316493
-33.592674	5.882397	3.326490
-33.296750	4.866948	3.336486
-32.436604	1.774338	3.346483
-32.106747	0.034539	3.356480
-31.561529	-1.051402	3.366477
-30.810334	-1.377489	3.376474
-30.518200	-7.033019	3.386470
-30.420646	-0.845924	3.396467
-29.249226	4.195157	3.406464
-28.967187	5.006462	3.416461
-28.775765	-6.221201	3.426458
-27.700509	-3.607441	3.436454
-27.719189	-0.269011	3.446451
-27.245061	7.208893	3.456448
-26.275282	10.143177	3.466445
-25.888777	-2.119022	3.476442
-25.798871	-1.011717	3.486438
-24.886874	0.376224	3.496435
-24.749496	-2.717889	3.506432
-24.141512	-4.019502	3.516429
-23.451376	6.497433	3.526426
-23.040836	1.951165	3.536422
-22.598795	2.620353	3.546419
-21.644464	3.032388	3.556416
-21.352752	-3.038045	3.566413
-21.367641	2.371467	3.576410
-20.263159	2.604907	3.586406
-20.296486	5.847420	3.596403
-19.562722	2.074428	3.606400
-18.653463	2.990809	3.616397
-18.757294	-2.710774	3.626394
-18.081993	-3.243615	3.636390
-17.404152	0.157425	3.646387
-17.211815	9.861746	3.656384
-16.863152	8.533986	3.666381
-15.871867	2.455996	3.676378
-15.386015	7.353572	3.686374
-14.354154	6.806395	3.696371
-14.602266	1.554914	3.706368
-14.203753	2.436780	3.716365
-13.876932	3.830304	3.726362
-13.083602	1.964492	3.736358
-12.346492	4.640406	3.746355
-11.557879	11.578356	3.756352
-11.074200	0.248166	3.766349
-11.187337	6.072106	3.776346
-10.808753	0.273238	3.786342
-9.867767	-3.398974	3.796339
-9.448122	-0.353696	3.806336
-9.474444	4.319525	3.816333
-8.803690	5.437761	3.826330
-7.458874	-0.517882	3.836326
-7.315401	2.887166	3.846323
-7.461990	1.167697	3.856320
-7.073209	1.803998	3.866317
-6.188947	-0.155163	3.876314
-5.279153	5.395473	3.886310
-4.800474	10.104106	3.896307
-4.647519	7.850173	3.906304
-4.217940	16.579924	3.916301
-3.780820	17.094662	3.926298
-3.197407	30.742078	3.936294
-3.013250	37.742474	3.946291
-2.307320	45.358529	3.956288
-1.620474	50.814017	3.966285
-1.228030	62.600072	3.976282
-0.961347	76.613608	3.986278
-0.487989	93.059455	3.996275
-0.091889	111.912140	4.006272
0.000000	127.295756	4.011277
0.178349	137.037363	4.016282
0.777597	142.341252	4.021286
0.861815	163.575326	4.026291
1.243349	155.204925	4.031296
1.688137	161.959685	4.036301
1.467416	171.475551	4.041306
1.346803	153.692311	4.046310
1.481433	155.952327	4.051315
1.230531	161.980193	4.056320
1.268590	165.397332	4.061325
1.118889	158.438383	4.066330
1.594280	161.195824	4.071334
1.658214	164.501369	4.076339
1.537321	162.277117	4.081344
1.722001	163.216417	4.086349
1.038706	149.956259	4.091354
1.456551	154.456349	4.096358
1.444342	160.061084	4.101363
1.437932	158.138539	4.106368
1.230432	157.712083	4.111373
1.453328	163.640872	4.116378
1.523317	161.266681	4.121382
1.359228	170.868640	4.126387
1.556117	167.101655	4.131392
1.500111	161.093038	4.136397
1.467862	173.566068	4.141402
1.301660	161.680683	4.146406
1.683694	162.168487	4.151411
1.741291	166.364011	4.156416
1.916533	171.395412	4.161421
1.641688	166.597752	4.166426
1.602233	168.413487	4.171430
1.341343	168.488876	4.176435
1.534556	163.504451	4.181440
1.608179	169.288808	4.186445
1.519428	173.061042	4.191450
1.567482	156.703665	4.196454
1.579565	166.218082	4.201459
1.233526	175.462403	4.206464
1.270240	174.928323	4.211469
1.110238	169.499030	4.216474
1.948706	173.120571	4.221478
1.736569	190.537973	4.226483
1.713372	197.549103	4.231488
2.207524	187.642586	4.236493
1.680570	186.955827	4.241498
1.899954	186.412288	4.246502
1.651022	186.356105	4.251507
1.973252	188.602735	4.256512
1.851557	193.980923	4.261517
1.844521	187.097825	4.266522
2.118622	184.467231	4.271526
1.572699	182.723593	4.276531
1.964824	184.671446	4.281536
2.231301	187.648074	4.286541
1.719740	181.030188	4.291546
1.928177	180.953414	4.296550
1.823128	193.108770	4.301555
1.893352	194.977031	4.306560
1.905189	196.414632	4.311565
1.964083	199.303363	4.316570
2.696096	185.715255	4.321574
2.232466	183.939822	4.326579
1.907389	178.469790	4.331584
1.892662	170.467955	4.336589
1.525436	174.302528	4.341594
1.847073	184.379348	4.346598
2.194837	191.484575	4.351603
2.314325	192.532100	4.356608
2.363381	189.813160	4.361613
1.911588	187.507550	4.366618
2.373643	185.015367	4.371622
2.119690	187.927495	4.376627
2.005107	179.510943	4.381632
1.896292	175.842172	4.386637
2.139136	186.874037	4.391642
2.131962	188.406343	4.396646
1.951841	196.217006	4.401651
2.293338	196.787051	4.406656
2.395923	195.644779	4.411661
2.279671	195.707141	4.416666
2.354605	198.226387	4.421670
2.099861	204.650326	4.426675
2.258285	198.535546	4.431680
2.162193	193.634120	4.436685
2.151466	197.558721	4.441690
2.375617	196.694908	4.446694
2.309093	196.509087	4.451699
2.435113	195.850373	4.456704
2.218883	188.240562	4.461709
2.127832	200.469672	4.466714
2.635635	192.832550	4.471718
2.213168	198.725793	4.476723
2.289075	187.514522	4.481728
2.205569	195.151958	4.486733
2.084202	201.374800	4.491738
2.261345	200.676489	4.496742
2.329497	198.761313	4.501747
2.070226	199.026272	4.506752
2.452890	196.755250	4.511757
2.241237	203.134516	4.516762
3.137878	198.410710	4.521766
2.504127	209.471505	4.526771
2.445941	205.465823	4.531776
2.592533	194.945879	4.536781
2.322984	208.480913	4.541786
2.397680	188.335596	4.546790
2.414415	206.761393	4.551795
2.474009	214.461976	4.556800
2.619291	214.705076	4.561805
2.448983	220.672959	4.566810
2.916846	217.281380	4.571814
2.905763	225.989533	4.576819
2.608407	215.000873	4.581824
2.598296	209.551393	4.586829
2.217641	219.028911	4.591834
2.697641	209.788959	4.596838
2.525156	218.610821	4.601843
3.074777	224.833603	4.606848
3.072649	221.632256	4.611853
2.430050	225.962121	4.616858
2.518064	214.321851	4.621862
2.647433	212.106084	4.626867
2.790950	223.166090	4.631872
2.851350	221.970274	4.636877
2.901201	218.090134	4.641882
3.047917	220.607699	4.646886
2.760393	230.023268	4.651891
3.298175	211.713526	4.656896
2.899355	215.736521	4.661901
2.336182	207.775768	4.666906
3.062494	207.305158	4.671910
2.890881	217.809962	4.676915
2.807309	219.793919	4.681920
2.896930	223.794650	4.686925
2.735391	211.367515	4.691930
3.031333	215.842309	4.696934
2.737994	218.887122	4.701939
3.007297	222.214486	4.706944
2.803410	216.273166	4.711949
2.795607	223.993738	4.716954
2.770284	225.184033	4.721958
2.589312	223.339278	4.726963
2.817634	225.920066	4.731968
2.758102	222.461907	4.736973
2.587437	225.715407	4.741978
3.030201	232.024429	4.746982
3.316688	235.697125	4.751987
3.060273	230.675120	4.756992
3.550747	227.703953	4.761997
2.884050	232.442524	4.767002
2.888775	217.249747	4.772006
3.061191	225.793291	4.777011
3.506069	242.232108	4.782016
3.189730	234.922595	4.787021
3.277940	234.247621	4.792026
3.132812	217.066071	4.797030
3.081835	220.497083	4.802035
3.194988	225.860862	4.807040
3.183267	225.131846	4.812045
3.070145	232.005134	4.817050
3.072817	239.559570	4.822054
3.416388	238.126680	4.827059
3.465572	233.651867	4.832064
3.575647	237.671562	4.837069
3.142038	235.632028	4.842074
3.201611	217.665649	4.847078
3.269800	231.534085	4.852083
3.354343	227.692833	4.857088
3.685039	234.012977	4.862093
3.147859	231.913641	4.867098
3.269393	230.157825	4.872102
3.584104	230.092977	4.877107
3.367532	235.808646	4.882112
3.684058	236.613529	4.887117
3.427103	228.813893	4.892122
3.198840	223.626160	4.897126
3.246728	219.815926	4.902131
3.510026	240.509694	4.907136
3.681418	238.888480	4.912141
3.333945	248.636089	4.917146
3.690696	239.057815	4.922150
3.523856	241.731767	4.927155
3.433420	241.157372	4.932160
3.636637	250.237123	4.937165
3.640345	256.149451	4.942170
3.607896	233.878947	4.947174
3.370817	234.111978	4.952179
3.330438	239.487010	4.957184
3.528698	238.554461	4.962189
3.750103	244.043757	4.967194
3.764794	234.202373	4.972198
3.673729	240.028214	4.977203
3.719477	242.425463	4.982208
4.049430	234.591391	4.987213
3.401960	228.728623	4.992218
3.821413	225.309780	4.997222
3.768565	223.698172	5.002227
3.519926	229.478941	5.007232
3.463602	234.176262	5.012237
3.505003	245.479967	5.017242
3.713318	241.366346	5.022246
3.242368	239.870452	5.027251
3.722848	247.030967	5.032256
3.539323	244.076153	5.037261
3.675007	244.232164	5.042266
3.644138	238.516994	5.047270
3.925821	240.440920	5.052275
3.522600	242.977673	5.057280
3.829980	244.505302	5.062285
3.576384	245.414770	5.067290
3.630448	244.893804	5.072294
3.829466	250.158802	5.077299
3.934360	264.328427	5.082304
4.254300	262.807467	5.087309
3.795957	261.379209	5.092314
3.648748	254.571692	5.097318
4.257391	272.392881	5.102323
3.940236	262.856245	5.107328
4.215225	248.386975	5.112333
3.762252	249.716619	5.117338
3.758639	260.628717	5.122342
4.084120	264.523133	5.127347
3.969362	269.738916	5.132352
3.954685	280.279433	5.137357
4.049858	274.462371	5.142362
4.028968	267.644672	5.147366
4.231134	275.829275	5.152371
3.916337	278.934386	5.157376
4.530724	268.983795	5.162381
3.925991	274.494161	5.167386
4.272601	269.773718	5.172390
4.277523	273.471278	5.177395
4.100112	262.356348	5.182400
4.422126	265.903298	5.187405
3.992049	262.151654	5.192410
4.098498	266.140283	5.197414
4.058698	269.072865	5.202419
4.206102	274.500927	5.207424
4.215786	272.746703	5.212429
4.056303	276.131346	5.217434
4.317183	275.094135	5.222438
4.305534	271.865788	5.227443
4.302767	278.082845	5.232448
4.579805	277.944771	5.237453
4.572797	276.360821	5.242458
4.190424	264.195818	5.247462
4.211083	265.774417	5.252467
3.716589	270.223600	5.257472
4.230787	271.019854	5.262477
4.105308	280.533604	5.267482
3.917448	276.177944	5.272486
4.130634	277.963845	5.277491
4.315233	281.427792	5.282496
4.269017	268.264503	5.287501
4.139912	280.961492	5.292506
4.396846	273.888568	5.297510
4.393859	273.904821	5.302515
4.362449	286.412600	5.307520
4.579577	284.173669	5.312525
4.186816	287.642090	5.317530
4.594708	290.849814	5.322534
4.638779	281.601769	5.327539
4.551397	288.632419	5.332544
4.762325	276.723039	5.337549
4.309945	277.293306	5.342554
4.642865	281.097985	5.347558
5.012485	289.500127	5.352563
4.442220	289.282006	5.357568
4.433943	274.594232	5.362573
4.278064	295.840537	5.367578
4.749809	275.051183	5.372582
4.683167	289.241207	5.377587
4.592469	287.047039	5.382592
4.797012	295.193317	5.387597
4.432247	289.593390	5.392602
4.618227	289.652987	5.397606
4.605396	292.644648	5.402611
4.493710	284.430071	5.407616
4.697184	285.714458	5.412621
4.292111	284.021645	5.417626
4.548535	285.898890	5.422630
4.698030	291.003935	5.427635
4.377778	292.588159	5.432640
4.709450	284.532339	5.437645
4.523787	295.922048	5.442650
4.632111	286.303335	5.447654
4.707267	299.310214	5.452659
4.503688	310.319914	5.457664
4.976426	317.329805	5.462669
4.629347	317.497706	5.467674
5.199370	319.142634	5.472678
5.166765	318.397883	5.477683
5.115457	316.918902	5.482688
5.089143	301.022217	5.487693
4.609456	296.851190	5.492698
4.815750	302.994579	5.497702
4.858757	310.232723	5.502707
4.985140	322.348971	5.507712
5.191379	305.033537	5.512717
5.003666	313.022600	5.517722
4.958996	310.909846	5.522726
5.032733	322.467988	5.527731
4.789972	321.632574	5.532736
5.228859	321.564210	5.537741
4.973456	317.513280	5.542746
4.966067	310.263200	5.547750
5.340205	316.699994	5.552755
4.882847	321.010532	5.557760
5.269147	308.694182	5.562765
5.099078	320.821784	5.567770
5.266409	306.540069	5.572774
5.268004	319.463505	5.577779
4.989396	319.396123	5.582784
5.186237	309.520011	5.587789
5.086724	314.455028	5.592794
5.017735	319.840866	5.597798
5.320851	313.187836	5.602803
5.366193	313.183910	5.607808
5.550414	319.549036	5.612813
5.464783	319.432626	5.617818
4.960332	299.649433	5.622822
5.084071	311.699648	5.627827
5.279704	313.880584	5.632832
5.700191	323.189132	5.637837
5.142586	318.859392	5.642842
5.426321	315.828652	5.647846
5.381209	315.028902	5.652851
5.126364	324.002842	5.657856
5.525403	315.136103	5.662861
5.224085	315.920129	5.667866
5.190123	316.817550	5.672870
5.266534	313.815926	5.677875
5.103411	312.908002	5.682880
5.310495	312.328410	5.687885
5.409934	321.338935	5.692890
5.145874	318.744655	5.697894
5.105205	314.201556	5.702899
4.990539	322.660133	5.707904
5.506429	326.290803	5.712909
5.196793	324.640074	5.717914
5.220530	325.205815	5.722918
5.308891	333.442964	5.727923
5.564950	339.268574	5.732928
5.931138	338.680027	5.737933
5.790514	332.200480	5.742938
5.750033	325.351009	5.747942
5.765143	323.456733	5.752947
5.660859	319.935921	5.757952
5.597512	311.679005	5.762957
5.381610	328.261910	5.767962
5.081967	324.195720	5.772966
5.744279	337.753441	5.777971
5.905995	335.776227	5.782976
5.832543	334.443059	5.787981
5.531173	327.615224	5.792986
5.492426	328.655757	5.797990
6.042019	336.023843	5.802995
5.942890	338.048199	5.808000
6.023915	317.461996	5.813005
5.500003	327.812913	5.818010
5.709678	320.339210	5.823014
5.840781	323.659636	5.828019
5.644115	327.056406	5.833024
5.722088	314.073060	5.838029
5.830416	318.374615	5.843034
5.681009	317.461392	5.848038
5.860878	313.032650	5.853043
5.642185	328.768119	5.858048
6.173747	323.987229	5.863053
5.876087	323.451422	5.868058
6.001004	312.577285	5.873062
5.868032	301.506030	5.878067
5.590841	315.529544	5.883072
5.875530	327.735041	5.888077
6.245033	333.802410	5.893082
5.950606	323.158070	5.898086
5.799902	317.553279	5.903091
5.975800	328.136918	5.908096
5.969672	322.221719	5.913101
5.845467	331.330344	5.918106
5.758424	327.395565	5.923110
6.085201	332.991867	5.928115
6.128292	335.560382	5.933120
6.233761	337.011890	5.938125
6.149699	340.185489	5.943130
6.042458	340.006006	5.948134
5.933892	342.693046	5.953139
6.198287	343.202335	5.958144
6.465992	337.950003	5.963149
6.151490	325.242888	5.968154
5.678878	322.987957	5.973158
6.075935	321.303128	5.978163
6.014193	334.261745	5.983168
6.079497	333.976306	5.988173
5.992325	340.371039	5.993178
6.124735	333.149803	5.998182
6.250643	334.648747	6.003187
6.277455	333.135456	6.008192
6.520329	329.120836	6.013197
6.330121	340.381569	6.018202
6.371344	339.830964	6.023206
6.320777	331.727070	6.028211
6.310248	340.612360	6.033216
6.328373	331.618261	6.038221
6.358995	342.626317	6.043226
6.119479	328.012466	6.048230
6.055107	318.161200	6.053235
6.038257	337.762931	6.058240
6.239834	333.201093	6.063245
6.258246	339.487639	6.068250
6.226983	330.273444	6.073254
6.440100	335.204083	6.078259
6.443035	343.944912	6.083264
6.350505	320.772506	6.088269
5.679674	326.261543	6.093274
6.062038	326.749300	6.098278
6.118913	341.391527	6.103283
5.713439	346.494410	6.108288
6.354576	338.981996	6.113293
6.388122	347.784499	6.118298
6.214879	333.046432	6.123302
6.433935	328.883663	6.128307
6.246537	336.024815	6.133312
6.257808	336.238162	6.138317
6.258984	343.141152	6.143322
6.336370	340.547490	6.148326
6.309400	342.674505	6.153331
6.386440	346.341870	6.158336
6.500462	344.400554	6.163341
6.017924	337.996386	6.168346
6.237853	331.871983	6.173350
6.196638	335.064220	6.178355
6.260096	345.538827	6.183360
6.134407	338.329300	6.188365
6.254209	340.256296	6.193370
6.317632	340.945570	6.198374
6.296484	337.642761	6.203379
5.939741	334.635809	6.208384
6.637054	336.052115	6.213389
5.968838	340.164537	6.218394
6.027892	331.594330	6.223398
6.244012	335.872779	6.228403
6.256131	334.390248	6.233408
6.266465	337.334018	6.238413
5.971326	336.041693	6.243418
6.071583	339.344779	6.248422
6.277720	337.664364	6.253427
6.078252	340.232681	6.258432
6.149859	327.769165	6.263437
6.079138	340.688057	6.268442
6.027798	339.487485	6.273446
6.030849	335.997414	6.278451
5.862581	336.808181	6.283456
6.293612	339.385898	6.288461
6.013520	340.998675	6.293466
6.273825	346.260486	6.298470
6.265575	341.804080	6.303475
6.066802	341.483827	6.308480
6.078297	347.676542	6.313485
5.961294	344.094432	6.318490
5.665529	339.341111	6.323494
6.257586	347.278384	6.328499
6.188687	356.552414	6.333504
6.291121	357.858866	6.338509
6.492765	370.735373	6.343514
6.046927	357.355831	6.348518
6.129006	359.089389	6.353523
6.200769	359.812166	6.358528
6.037631	358.932715	6.363533
6.129889	372.876606	6.368538
6.499352	358.670944	6.373542
6.556982	353.590518	6.378547
5.979249	351.155801	6.383552
6.307944	351.417801	6.388557
6.240728	358.397884	6.393562
6.451255	358.649809	6.398566
6.374888	348.363802	6.403571
5.861697	348.839137	6.408576
6.246852	349.532102	6.413581
6.537869	357.867422	6.418586
6.139211	349.336833	6.423590
6.207454	335.029394	6.428595
6.312237	337.638924	6.433600
6.031928	341.184758	6.438605
6.058213	342.224658	6.443610
6.243402	346.868588	6.448614
6.413154	343.175393	6.453619
6.184192	351.164569	6.458624
6.453993	347.721547	6.463629
6.259995	339.564052	6.468634
5.913052	331.743581	6.473638
6.132315	341.308091	6.478643
6.235210	357.547164	6.483648
6.308558	361.101213	6.488653
6.434002	362.669833	6.493658
6.584958	354.999617	6.498662
6.124472	341.989358	6.503667
6.085213	342.340284	6.508672
6.308033	342.647242	6.513677
6.426498	339.104400	6.518682
6.047604	340.973001	6.523686
5.989741	331.389630	6.528691
6.056375	341.727701	6.533696
6.190304	353.754212	6.538701
6.276058	360.564948	6.543706
6.214140	360.378408	6.548710
6.631254	357.579991	6.553715
6.360171	350.171637	6.558720
6.068324	339.295935	6.563725
6.112746	351.630604	6.568730
5.901276	351.850158	6.573734
6.477606	346.030924	6.578739
6.207315	347.110672	6.583744
6.185816	340.223439	6.588749
6.070270	345.727264	6.593754
6.245805	356.393232	6.598758
6.523791	345.150399	6.603763
6.162730	346.709345	6.608768
6.208419	340.226097	6.613773
6.461245	336.447204	6.618778
5.919267	337.929915	6.623782
6.137836	341.382257	6.628787
6.253685	344.357055	6.633792
6.105242	333.585577	6.638797
6.328434	344.506706	6.643802
6.182432	355.637181	6.648806
6.521815	356.166433	6.653811
6.129853	347.100135	6.658816
6.182747	342.706974	6.663821
6.012516	347.013942	6.668826
6.493023	359.919789	6.673830
6.097332	342.027331	6.678835
6.340895	354.204449	6.683840
6.269269	346.220884	6.688845
5.863154	347.249015	6.693850
6.320907	359.165000	6.698854
6.545790	368.633739	6.703859
6.132678	353.012362	6.708864
6.377099	345.046029	6.713869
6.349281	341.582909	6.718874
6.319669	341.922842	6.723878
6.080732	344.149297	6.728883
6.344136	356.070230	6.733888
6.218161	343.862089	6.738893
6.052240	330.549715	6.743898
6.171841	336.519954	6.748902
6.528769	335.812629	6.753907
6.079618	344.487807	6.758912
6.060015	343.880233	6.763917
6.235382	340.527845	6.768922
5.966381	340.955670	6.773926
6.341002	347.503130	6.778931
6.289608	356.695342	6.783936
6.624367	348.686469	6.788941
6.144638	346.306094	6.793946
6.324936	348.090796	6.798950
6.395685	327.914299	6.803955
5.967995	345.308466	6.808960
6.240808	340.552039	6.813965
6.153388	341.229998	6.818970
6.075856	342.485376	6.823974
6.272966	335.073734	6.828979
6.239903	339.745315	6.833984
6.106889	335.615215	6.838989
5.892585	335.930121	6.843994
6.153975	355.735319	6.848998
6.342651	359.192319	6.854003
5.915299	367.766039	6.859008
5.923424	378.129060	6.864013
6.429397	376.316538	6.869018
6.558506	367.770207	6.874022
6.488900	368.173314	6.879027
6.419496	355.532419	6.884032
6.468173	348.643748	6.889037
6.363970	349.245227	6.894042
6.516438	351.407580	6.899046
6.544865	337.878282	6.904051
6.610699	336.960019	6.909056
6.545017	342.158691	6.914061
6.248344	344.362499	6.919066
6.234387	341.890624	6.924070
6.534830	352.802894	6.929075
6.276687	351.226401	6.934080
6.319909	346.464591	6.939085
6.338836	345.936439	6.944090
6.333828	349.350828	6.949094
6.313158	348.521961	6.954099
6.042122	338.234632	6.959104
6.080445	335.770437	6.964109
5.944689	338.623059	6.969114
6.523727	331.458833	6.974118
6.449191	338.509649	6.979123
6.123409	343.647580	6.984128
6.442487	340.431002	6.989133
6.171579	324.958349	6.994138
6.256246	320.873453	6.999142
6.155161	324.451489	7.004147
6.225393	332.523785	7.009152
6.729543	328.142624	7.014157
6.347298	324.070313	7.019162
6.367572	320.419378	7.024166
6.459797	310.860105	7.029171
6.243724	318.999117	7.034176
6.099550	314.260165	7.039181
5.944789	316.340636	7.044186
6.076777	321.964098	7.049190
5.814593	310.258069	7.054195
5.799254	321.909172	7.059200
6.504133	332.834390	7.064205
6.313762	337.565264	7.069210
6.069789	341.292099	7.074214
5.951522	337.238795	7.079219
5.768407	344.600743	7.084224
6.149813	340.146943	7.089229
6.490768	340.530419	7.094234
6.078241	338.098454	7.099238
6.365240	342.040008	7.104243
5.783692	338.239165	7.109248
6.231540	344.253212	7.114253
5.964709	346.126512	7.119258
6.309598	349.568679	7.124262
6.506277	344.305257	7.129267
6.041382	351.255506	7.134272
6.310638	343.971831	7.139277
6.046723	350.729440	7.144282
6.016356	353.651075	7.149286
6.236353	345.891021	7.154291
6.172339	349.681587	7.159296
6.241855	340.328311	7.164301
6.181369	347.133337	7.169306
6.019473	355.554991	7.174310
5.762801	343.968303	7.179315
6.034736	346.539154	7.184320
6.235088	343.572011	7.189325
6.223749	335.221566	7.194330
6.086518	350.238865	7.199334
6.290946	350.691054	7.204339
6.296035	355.552849	7.209344
6.179178	352.321886	7.214349
6.031919	344.324788	7.219354
6.073018	357.950771	7.224358
6.476022	365.158197	7.229363
6.453291	368.663933	7.234368
6.372943	357.552812	7.239373
5.806092	341.926909	7.244378
6.252959	352.474701	7.249382
6.553754	364.396145	7.254387
6.180708	365.710190	7.259392
6.049578	353.097889	7.264397
6.335935	345.681838	7.269402
6.192188	351.446316	7.274406
6.348715	351.061253	7.279411
6.262091	350.789976	7.284416
6.374886	352.373220	7.289421
6.399645	340.394708	7.294426
6.178230	352.359486	7.299430
6.548913	347.499236	7.304435
6.005020	351.095602	7.309440
5.965779	340.054021	7.314445
6.156701	342.232531	7.319450
6.246120	340.855022	7.324454
6.504056	347.857241	7.329459
6.298643	356.744409	7.334464
6.221249	349.796273	7.339469
6.134481	353.454342	7.344474
5.954352	360.202073	7.349478
6.365262	347.524365	7.354483
6.304745	351.393479	7.359488
6.325331	350.760666	7.364493
6.343426	344.183638	7.369498
5.830674	355.994465	7.374502
5.931663	345.620736	7.379507
6.000120	355.313135	7.384512
6.434842	366.365856	7.389517
6.298198	349.780797	7.394522
5.856810	356.430000	7.399526
6.658526	360.316728	7.404531
6.125422	351.762778	7.409536
6.341139	342.064040	7.414541
6.400198	344.196643	7.419546
6.298752	348.926330	7.424550
6.216628	343.510167	7.429555
6.145417	343.910360	7.434560
6.171883	345.231802	7.439565
6.518984	351.321647	7.444570
6.098127	343.693009	7.449574
6.290991	347.772605	7.454579
6.487310	351.370780	7.459584
6.508496	344.609775	7.464589
6.457663	346.680396	7.469594
6.235877	350.387960	7.474598
6.479893	347.945520	7.479603
6.478299	354.817309	7.484608
6.554843	346.835985	7.489613
6.873648	349.522924	7.494618
6.238319	340.143350	7.499622
6.143651	325.959358	7.504627
6.029032	329.178841	7.509632
6.112642	329.349287	7.514637
6.397161	340.396905	7.519642
6.135033	345.505943	7.524646
6.345483	339.484252	7.529651
6.367543	345.975874	7.534656
6.444709	340.392545	7.539661
6.234117	337.568478	7.544666
6.100288	323.925251	7.549670
6.191935	318.092905	7.554675
5.780248	325.123443	7.559680
6.329855	341.678922	7.564685
6.389782	346.788437	7.569690
6.296907	351.731922	7.574694
6.061698	333.431678	7.579699
6.348458	337.854150	7.584704
6.278044	330.231066	7.589709
6.169025	323.107534	7.594714
5.944185	338.065698	7.599718
6.458951	340.953076	7.604723
6.192982	346.888439	7.609728
6.688269	343.305909	7.614733
6.128631	344.108010	7.619738
5.807813	325.178871	7.624742
6.089172	335.043752	7.629747
6.127114	345.126869	7.634752
6.201328	341.590916	7.639757
6.297184	341.053950	7.644762
6.485894	347.870798	7.649766
6.620158	336.729440	7.654771
6.208200	334.442918	7.659776
6.349797	327.277200	7.664781
6.463943	317.157699	7.669786
6.312989	315.694232	7.674790
5.832063	313.782277	7.679795
6.185886	323.996531	7.684800
6.016562	325.418057	7.689805
6.222136	317.362873	7.694810
6.289284	319.601779	7.699814
6.396019	316.165170	7.704819
6.236744	314.630234	7.709824
6.055872	316.648333	7.714829
6.447101	312.908007	7.719834
6.122097	322.060545	7.724838
5.684847	313.792242	7.729843
6.082652	330.539021	7.734848
6.055583	335.007191	7.739853
6.238442	333.169052	7.744858
6.252916	346.261342	7.749862
6.570209	337.400993	7.754867
6.035544	347.396096	7.759872
6.396173	344.859572	7.764877
6.509333	342.712750	7.769882
6.514324	334.701443	7.774886
6.340681	324.617253	7.779891
6.021615	328.324141	7.784896
5.871285	327.971036	7.789901
6.319144	332.890435	7.794906
6.317930	335.576579	7.799910
6.062111	318.639951	7.804915
6.198154	332.652923	7.809920
6.408106	340.912273	7.814925
6.400616	340.505291	7.819930
6.360021	326.600777	7.824934
6.018873	321.329351	7.829939
6.084808	325.995007	7.834944
5.911672	332.254428	7.839949
6.231729	335.649839	7.844954
6.013827	341.232873	7.849958
6.381770	341.637457	7.854963
6.554241	340.648808	7.859968
6.312218	334.903208	7.864973
6.191485	336.851835	7.869978
5.977815	334.398401	7.874982
6.381554	335.850925	7.879987
6.433150	342.622680	7.884992
6.022783	322.799503	7.889997
6.225823	322.597020	7.895002
5.961630	342.980737	7.900006
6.338062	338.619459	7.905011
6.045915	345.485864	7.910016
6.067111	349.418184	7.915021
6.324156	345.344408	7.920026
6.224814	350.152860	7.925030
6.193085	336.727840	7.930035
6.309836	344.754934	7.935040
6.321168	349.131709	7.940045
6.519186	350.189163	7.945050
6.255428	350.416858	7.950054
6.543749	345.502993	7.955059
6.146318	333.447853	7.960064
6.087724	322.327040	7.965069
6.058741	322.695348	7.970074
6.167178	337.494056	7.975078
6.547149	333.341033	7.980083
6.287144	327.133171	7.985088
6.042477	324.962970	7.990093
6.159479	324.989015	7.995098
6.187569	337.205997	8.000102
6.006206	335.921267	8.005107
6.347949	336.870924	8.010112
6.348893	341.113686	8.015130
6.360572	336.817019	8.020147
6.034300	336.034701	8.025165
6.485093	337.277228	8.030182
6.139456	342.736613	8.035200
6.375614	327.625355	8.040218
6.419005	330.007382	8.045235
6.144196	328.459700	8.050253
6.170727	322.671266	8.055270
6.010989	325.656089	8.060288
5.926492	346.149275	8.065306
6.112640	345.138860	8.070323
6.078446	347.952669	8.075341
6.481377	350.237697	8.080358
6.650181	343.947448	8.085376
6.452668	343.615272	8.090394
6.908663	344.714986	8.095411
6.611963	335.653991	8.100429
6.571637	322.305604	8.105446
6.271907	321.654846	8.110464
5.816878	316.569362	8.115482
6.153858	319.953347	8.120499
6.138880	320.883404	8.125517
6.351197	324.813790	8.130534
6.454474	336.303115	8.135552
6.095260	336.857603	8.140570
6.212218	341.288807	8.145587
6.488079	342.735286	8.150605
6.382031	339.006029	8.155622
6.324965	343.107742	8.160640
5.977511	351.132943	8.165658
6.177863	350.139250	8.170675
6.041459	348.775134	8.175693
6.187076	344.189383	8.180710
6.245975	348.257263	8.185728
6.171473	353.889020	8.190746
6.539866	347.024926	8.195763
6.243736	347.938802	8.200781
6.592441	349.033131	8.205798
6.638393	342.875614	8.210816
6.222656	343.839668	8.215834
6.592222	346.600080	8.220851
6.609171	351.640117	8.225869
6.876992	341.169013	8.230886
6.382107	342.057033	8.235904
6.264964	347.051678	8.240922
6.446484	345.253074	8.245939
6.405053	347.793470	8.250957
6.517073	343.291841	8.255974
6.408208	338.783581	8.260992
6.218385	342.735559	8.266010
6.367887	345.129468	8.271027
6.291036	343.276423	8.276045
6.227490	342.598359	8.281062
6.046572	345.198339	8.286080
6.381356	361.523937	8.291098
6.933782	359.979992	8.296115
6.954977	365.505340	8.301133
6.723547	355.850379	8.306150
6.527984	354.183065	8.311168
6.353133	352.982715	8.316186
6.562024	344.101760	8.321203
6.739454	351.552960	8.326221
6.241470	343.463680	8.331238
6.445209	348.947979	8.336256
6.243082	355.281224	8.341274
6.612589	363.715484	8.346291
6.410223	367.745155	8.351309
6.844979	362.379118	8.356326
6.866151	364.957104	8.361344
6.645799	351.955444	8.366362
6.743857	342.678357	8.371379
6.221838	356.799026	8.376397
6.524068	357.443025	8.381414
6.828602	359.465678	8.386432
6.613071	352.424267	8.391450
6.739431	341.470287	8.396467
6.674836	348.233373	8.401485
6.226400	350.265968	8.406502
6.676994	348.914594	8.411520
6.438915	371.366126	8.416538
6.624546	364.337986	8.421555
6.504846	372.308803	8.426573
6.321444	374.959665	8.431590
6.749814	364.198478	8.436608
6.825819	371.883217	8.441626
6.646059	365.965951	8.446643
7.023051	367.769052	8.451661
7.008052	361.898713	8.456678
6.829740	366.552612	8.461696
6.710225	360.474496	8.466714
6.773770	350.760989	8.471731
6.511228	356.096994	8.476749
6.566764	365.179709	8.481766
6.825962	375.161633	8.486784
6.895600	373.566630	8.491802
6.777313	353.278484	8.496819
6.652577	360.423304	8.501837
6.453710	359.807331	8.506854
6.425949	365.356079	8.511872
6.527298	370.442937	8.516890
6.636190	375.616981	8.521907
6.531381	370.691537	8.526925
6.774314	370.243450	8.531942
6.733829	368.113355	8.536960
6.665151	380.904360	8.541978
6.932143	371.023474	8.546995
7.180431	380.811450	8.552013
7.005857	375.423521	8.557030
7.191118	364.861122	8.562048
6.795914	373.916196	8.567066
7.175568	372.531686	8.572083
6.742562	367.209241	8.577101
6.733087	374.657996	8.582119
6.583454	374.744376	8.587136
6.336551	378.724182	8.592154
6.869140	377.527289	8.597171
6.787997	373.358669	8.602189
6.790838	380.540434	8.607207
7.140129	371.060123	8.612224
6.545192	371.357839	8.617242
6.945561	368.938210	8.622259
6.715892	374.142876	8.627277
6.782565	371.210343	8.632295
6.930825	368.394488	8.637312
6.720232	376.909607	8.642330
6.947927	362.695838	8.647347
6.977184	369.195024	8.652365
6.666536	379.265673	8.657383
6.926930	374.460083	8.662400
6.780049	379.942180	8.667418
6.737037	370.469304	8.672435
6.695549	376.114861	8.677453
6.546860	374.099438	8.682471
7.327309	371.112574	8.687488
6.674459	374.814775	8.692506
6.934299	371.542914	8.697523
6.997142	373.492751	8.702541
6.708625	372.644596	8.707559
6.904390	381.468814	8.712576
6.605181	396.018703	8.717594
6.983912	399.257354	8.722611
7.082470	400.094003	8.727629
7.146684	396.738992	8.732647
7.179747	402.893632	8.737664
7.052095	404.967802	8.742682
7.320264	396.793922	8.747699
7.119372	391.463732	8.752717
6.992873	383.752073	8.757735
6.877173	373.678317	8.762752
6.834471	381.324741	8.767770
7.069315	386.583314	8.772787
7.398794	390.867838	8.777805
6.972762	388.267621	8.782823
7.316422	375.089772	8.787840
6.857963	382.630524	8.792858
6.712688	368.443264	8.797875
6.891308	382.274996	8.802893
6.907010	393.443496	8.807911
7.276594	394.032830	8.812928
7.481899	395.105310	8.817946
7.600547	391.883828	8.822963
7.142038	381.140800	8.827981
6.572085	369.515772	8.832999
7.101228	374.785322	8.838016
7.222064	394.972054	8.843034
6.782199	398.451760	8.848051
7.137733	396.790152	8.853069
7.096388	396.380014	8.858087
7.128725	403.986364	8.863104
7.310276	393.790580	8.868122
6.994030	396.676712	8.873139
7.125815	393.468963	8.878157
7.173584	389.232934	8.883175
7.430073	394.589119	8.888192
7.401316	385.887148	8.893210
6.940344	387.978500	8.898227
7.217230	393.363066	8.903245
7.133525	396.881989	8.908263
7.320921	402.141642	8.913280
7.401768	399.074360	8.918298
7.210875	396.828832	8.923315
7.638291	397.809928	8.928333
7.079763	393.040323	8.933351
7.394542	389.961865	8.938368
7.263771	390.152600	8.943386
7.185344	382.689064	8.948403
7.141799	385.823055	8.953421
7.398521	398.834795	8.958439
7.286969	391.363790	8.963456
6.890677	400.456914	8.968474
7.119343	396.057026	8.973491
6.996799	388.985345	8.978509
7.210620	397.175630	8.983527
7.085653	397.513777	8.988544
7.199048	394.539253	8.993562
6.940831	404.901540	8.998579
7.462909	394.166768	9.003597
7.129407	400.574130	9.008615
7.413338	389.731280	9.013632
7.243172	407.583980	9.018650
7.380396	397.559189	9.023667
7.614142	391.978300	9.028685
7.289583	399.305717	9.033703
7.247550	392.789515	9.038720
7.261438	393.907576	9.043738
7.164035	391.054231	9.048755
7.647352	396.715911	9.053773
7.743242	402.889170	9.058791
7.554523	396.935420	9.063808
7.336172	397.669939	9.068826
7.448138	402.467990	9.073843
7.509891	398.049910	9.078861
7.257185	406.151898	9.083879
7.625981	400.411131	9.088896
7.426728	391.801970	9.093914
7.387622	402.300545	9.098931
7.556938	387.723480	9.103949
7.404935	399.173701	9.108967
7.300316	397.287106	9.113984
7.474368	393.113461	9.119002
7.326419	396.241619	9.124019
7.462869	397.810789	9.129037
7.007396	402.369001	9.134055
7.229428	396.064136	9.139072
7.511149	398.402754	9.144090
7.475463	402.277100	9.149107
7.432046	393.826703	9.154125
7.599008	398.919132	9.159143
7.421673	400.761208	9.164160
7.435678	396.729240	9.169178
7.364839	400.804709	9.174195
7.911370	395.667399	9.179213
7.277297	400.496403	9.184231
7.450840	398.837884	9.189248
7.569026	407.011508	9.194266
7.493509	419.589022	9.199283
7.947388	425.353119	9.204301
7.883769	414.561210	9.209319
7.272607	400.926120	9.214336
7.080558	402.060466	9.219354
6.946936	413.296407	9.224371
7.390126	417.566389	9.229389
7.439303	423.339850	9.234407
7.530333	420.211021	9.239424
7.353823	419.976554	9.244442
7.728236	419.457505	9.249459
7.682367	414.415580	9.254477
7.459576	420.610062	9.259495
7.729276	423.054692	9.264512
7.651172	420.501280	9.269530
7.222765	419.444540	9.274547
7.533177	421.254857	9.279565
7.497906	423.870040	9.284583
7.705719	422.278763	9.289600
7.671328	412.233350	9.294618
7.568098	426.377228	9.299635
8.265792	427.328868	9.304653
7.735138	425.795766	9.309671
7.843098	421.080166	9.314688
7.885754	425.576606	9.319706
7.830396	424.764726	9.324723
8.016332	419.907604	9.329741
7.932600	420.488627	9.334759
7.448538	419.386906	9.339776
7.906268	411.035191	9.344794
7.576699	422.825482	9.349811
7.957322	414.163895	9.354829
7.898187	424.753960	9.359847
7.523010	428.801084	9.364864
7.944870	417.813671	9.369882
7.707120	419.513684	9.374899
8.424697	412.759292	9.379917
8.075323	416.281714	9.384935
8.126636	420.988233	9.389952
8.038109	411.923188	9.394970
8.007372	416.585679	9.399987
7.927129	409.974439	9.405005
8.003739	399.138617	9.410023
7.308832	391.199889	9.415040
7.730069	404.539451	9.420058
7.754956	413.579628	9.425075
8.240949	413.680648	9.430093
7.756090	411.607112	9.435111
7.762409	422.303744	9.440128
7.719314	419.195799	9.445146
7.537132	426.456880	9.450163
7.987372	415.348292	9.455181
7.871922	413.961973	9.460199
7.847342	419.134721	9.465216
7.607590	416.931509	9.470234
7.942313	421.843199	9.475251
8.166972	415.200263	9.480269
7.836358	422.667481	9.485287
7.839826	423.250706	9.490304
8.018136	416.974730	9.495322
7.729792	412.784715	9.500339
8.075434	411.462300	9.505357
8.224172	413.676466	9.510375
7.688898	418.177682	9.515392
7.860245	419.627817	9.520410
7.544397	425.776832	9.525427
7.786015	413.855012	9.530445
7.717583	422.947591	9.535463
7.624214	411.598610	9.540480
8.070230	423.044096	9.545498
8.338282	435.198918	9.550515
8.129372	417.048563	9.555533
8.096338	410.915942	9.560551
7.588618	414.810139	9.565568
7.748408	421.421558	9.570586
7.749194	436.562213	9.575603
8.273968	431.125339	9.580621
8.489696	436.361657	9.585639
8.094379	436.019253	9.590656
8.071312	438.376930	9.595674
8.106295	438.983650	9.600691
8.383546	439.792478	9.605709
8.330941	419.796973	9.610727
8.180290	418.924195	9.615744
8.114041	405.696541	9.620762
7.639794	416.382789	9.625779
8.189973	418.913130	9.630797
8.091427	429.244259	9.635815
8.071841	442.595683	9.640832
8.484832	439.088535	9.645850
8.092582	434.747443	9.650867
8.349080	425.341508	9.655885
8.186596	417.357740	9.660903
7.843756	415.934246	9.665920
8.272024	419.916232	9.670938
7.948306	427.483359	9.675955
8.044435	428.904183	9.680973
8.270211	433.280599	9.685991
8.206712	437.209774	9.691008
7.934926	432.389202	9.696026
8.232048	431.285768	9.701043
8.578602	427.713231	9.706061
8.211745	435.211343	9.711079
8.065085	438.538114	9.716096
8.331490	424.491829	9.721114
8.333512	446.776692	9.726131
8.212758	439.969786	9.731149
8.530806	442.328000	9.736167
8.236705	438.321903	9.741184
8.072353	434.715307	9.746202
8.190929	442.964623	9.751219
8.268887	439.052069	9.756237
8.545255	440.773019	9.761255
8.295041	441.111733	9.766272
8.387160	445.638344	9.771290
8.512788	439.143356	9.776307
8.409054	432.065573	9.781325
8.353567	444.763056	9.786343
8.062688	439.869719	9.791360
8.449664	429.831270	9.796378
8.343083	438.920331	9.801395
8.274086	432.259997	9.806413
8.604126	439.059499	9.811431
8.412722	437.404152	9.816448
9.110320	434.707875	9.821466
8.550546	428.786641	9.826483
8.407470	420.029871	9.831501
8.304517	423.573886	9.836519
8.309901	428.874508	9.841536
8.541960	425.386067	9.846554
8.657560	432.108506	9.851571
8.489202	422.194393	9.856589
8.250371	420.069928	9.861607
8.336136	427.472320	9.866624
8.460927	426.285270	9.871642
8.759806	444.112312	9.876659
8.426456	420.714545	9.881677
8.641793	414.123552	9.886695
8.143591	418.855670	9.891712
8.390901	427.397343	9.896730
8.711938	440.664175	9.901747
8.699199	434.761905	9.906765
8.527707	428.549854	9.911783
8.526930	432.709092	9.916800
8.525732	428.518545	9.921818
8.567593	442.725049	9.926835
8.513854	438.034621	9.931853
8.399820	441.084926	9.936871
8.333070	443.821772	9.941888
8.455394	441.369689	9.946906
8.521801	442.605802	9.951923
8.455100	439.687712	9.956941
8.798249	437.368497	9.961959
8.711653	444.958670	9.966976
8.727381	436.839854	9.971994
8.774069	445.239212	9.977011
8.751387	432.935672	9.982029
9.000390	434.458920	9.987047
8.954652	439.414072	9.992064
8.532493	427.138021	9.997082
8.621010	426.470990	10.002099
8.313719	420.633518	10.007117
8.680919	428.345524	10.012135
8.606679	436.230401	10.017152
8.773353	440.404593	10.022170
8.763865	440.611157	10.027187
8.560315	441.662094	10.032205
8.987747	439.626388	10.037223
8.697896	448.065522	10.042240
9.254015	442.566962	10.047258
8.564428	427.397791	10.052275
8.428619	424.411572	10.057293
8.709205	427.315233	10.062311
8.516124	439.702792	10.067328
8.513552	436.765251	10.072346
8.636983	431.245704	10.077363
8.459548	440.550914	10.082381
8.738076	445.862660	10.087399
8.408543	444.752657	10.092416
8.818570	440.337143	10.097434
8.872796	442.850036	10.102451
8.626245	437.785703	10.107469
8.562032	438.013411	10.112487
8.655973	439.750141	10.117504
8.750297	436.447236	10.122522
8.777753	442.915173	10.127539
8.885509	439.465016	10.132557
8.787291	436.529744	10.137575
8.920354	452.142099	10.142592
8.893657	453.424266	10.147610
8.931773	443.916629	10.152627
9.011728	449.903046	10.157645
9.216280	444.149969	10.162663
8.871187	445.519576	10.167680
8.889881	445.573437	10.172698
8.937494	443.574777	10.177715
8.734561	444.032356	10.182733
8.652000	446.118444	10.187751
8.854825	463.909971	10.192768
9.059953	464.057875	10.197786
9.235919	470.594214	10.202803
9.363130	465.850359	10.207821
9.011141	450.874747	10.212839
8.869355	452.361016	10.217856
8.991550	446.535558	10.222874
9.152122	443.250738	10.227891
8.584887	446.908068	10.232909
9.105918	453.450632	10.237927
9.011108	451.606683	10.242944
9.325070	455.940974	10.247962
9.012760	444.108534	10.252979
8.963640	440.865829	10.257997
9.067011	440.843394	10.263015
8.872998	451.031617	10.268032
9.083241	448.215566	10.273050
9.271979	454.642618	10.278067
9.097262	455.307233	10.283085
9.325718	451.118792	10.288103
9.038708	444.681737	10.293120
9.216161	439.481964	10.298138
9.318237	434.994483	10.303155
9.099195	439.885104	10.308173
9.287450	435.949067	10.313191
9.006542	438.040791	10.318208
8.932373	437.875592	10.323226
9.075113	441.400290	10.328243
8.887805	451.858856	10.333261
9.131468	461.070113	10.338279
9.481858	465.004277	10.343296
9.642709	466.932555	10.348314
9.564877	446.735829	10.353331
9.470742	450.594041	10.358349
9.223535	444.273859	10.363367
9.340941	447.385957	10.368384
9.199649	443.182506	10.373402
9.676988	448.841978	10.378419
9.094786	451.438183	10.383437
9.111197	439.601900	10.388455
9.109146	448.873496	10.393472
9.453898	444.420809	10.398490
9.461107	441.156712	10.403507
9.509678	443.440123	10.408525
9.167376	437.516583	10.413543
9.224152	441.341830	10.418560
9.147315	443.092528	10.423578
9.364331	438.915338	10.428595
8.913706	442.532421	10.433613
9.005312	445.093141	10.438631
9.016343	441.452926	10.443648
9.247067	455.383894	10.448666
9.244726	450.486653	10.453683
9.120904	463.065408	10.458701
9.266277	464.317629	10.463719
9.252912	468.005486	10.468736
9.451913	462.026060	10.473754
9.298324	473.867878	10.478771
9.322262	468.136603	10.483789
9.142639	455.314709	10.488807
9.382554	457.704024	10.493824
9.340643	469.111904	10.498842
9.586474	461.591538	10.503859
9.274498	464.906185	10.508877
9.445897	460.057627	10.513895
9.404182	472.355373	10.518912
9.157682	463.340143	10.523930
9.360862	465.460636	10.528947
9.155824	469.058421	10.533965
9.185195	472.979456	10.538983
9.381458	487.439654	10.544000
9.575671	494.244547	10.549018
9.550852	494.336740	10.554035
9.801809	487.465631	10.559053
10.060645	481.937609	10.564071
9.236016	472.030976	10.569088
9.353098	485.623073	10.574106
9.705791	482.172640	10.579123
9.970310	488.146113	10.584141
9.646480	469.855813	10.589159
9.367828	465.298220	10.594176
9.563458	467.987908	10.599194
9.962199	475.246920	10.604211
9.318917	472.831987	10.609229
9.561422	474.529812	10.614247
9.879918	481.981193	10.619264
9.593210	481.779661	10.624282
9.801654	467.174349	10.629299
9.734288	474.777319	10.634317
9.452827	476.692416	10.639335
9.884776	478.449104	10.644352
9.750855	481.729720	10.649370
9.699777	467.442512	10.654387
9.517801	463.172811	10.659405
9.608613	475.443615	10.664423
9.552170	485.351675	10.669440
9.651809	497.494893	10.674458
10.054645	492.717584	10.679475
9.915887	495.841173	10.684493
9.653944	483.726322	10.689511
10.192215	481.872160	10.694528
9.870451	476.974154	10.699546
10.011602	457.390232	10.704563
9.657924	469.727081	10.709581
9.601387	463.364583	10.714599
10.222451	461.566957	10.719616
9.688205	470.413365	10.724634
9.824490	463.339223	10.729651
9.797563	467.433116	10.734669
9.638108	467.921794	10.739687
9.637574	465.823335	10.744704
9.317821	476.141598	10.749722
9.700935	488.152315	10.754739
9.782977	487.827101	10.759757
9.952276	488.889415	10.764775
9.989861	484.506632	10.769792
9.788858	491.360435	10.774810
10.043627	487.126866	10.779827
10.080739	490.526015	10.784845
10.017510	494.341556	10.789863
9.924486	490.420900	10.794880
9.828656	487.198083	10.799898
9.995543	491.801423	10.804915
9.828533	485.386693	10.809933
9.774039	500.586500	10.814951
9.868065	491.682331	10.819968
9.289424	494.208564	10.824986
9.915627	494.312998	10.830003
9.571495	491.191953	10.835021
9.664972	495.996064	10.840039
10.099326	508.547902	10.845056
10.026872	519.698650	10.850074
10.112065	517.347007	10.855091
10.209554	519.042169	10.860109
10.212711	512.768185	10.865127
9.838862	495.984587	10.870144
9.779824	515.782914	10.875162
10.031120	517.640313	10.880179
10.244377	524.830400	10.885197
10.362434	521.725747	10.890215
10.477612	522.026506	10.895232
10.005330	508.252950	10.900250
10.059705	495.722784	10.905267
9.760693	508.158441	10.910285
9.538034	517.931459	10.915303
9.942247	512.750006	10.920320
9.928121	519.028793	10.925338
10.328134	510.067507	10.930355
10.136936	523.600338	10.935373
10.013970	520.359650	10.940391
10.122038	521.415720	10.945408
9.946458	523.377451	10.950426
9.779112	516.135977	10.955443
10.138616	524.713876	10.960461
10.497448	540.622503	10.965479
10.221355	529.021042	10.970496
10.095383	531.577782	10.975514
10.418232	530.965777	10.980531
10.623624	522.681698	10.985549
10.719851	529.681734	10.990567
10.503778	515.805167	10.995584
10.450973	523.992845	11.000602
10.461818	510.251359	11.005619
9.973560	512.612049	11.010637
10.467775	517.653561	11.015655
10.558154	512.836537	11.020672
10.768496	512.178936	11.025690
10.524853	507.063640	11.030707
10.343730	513.056015	11.035725
10.313731	520.728923	11.040743
10.329601	514.677011	11.045760
10.416019	506.670228	11.050778
10.109824	503.975600	11.055795
10.282522	509.142904	11.060813
9.790954	519.405895	11.065831
10.269288	510.255697	11.070848
9.959690	512.657996	11.075866
10.157982	527.550237	11.080883
10.576263	532.281697	11.085901
10.506959	536.063481	11.090919
10.755411	524.374043	11.095936
10.320011	532.586580	11.100954
10.492761	531.878029	11.105971
10.601701	522.854763	11.110989
10.582399	531.576847	11.116007
10.922706	532.170744	11.121024
10.518576	524.650567	11.126042
10.811586	518.530258	11.131059
10.561720	501.493832	11.136077
10.671699	503.859204	11.141095
10.611775	499.567336	11.146112
10.550133	501.277805	11.151130
10.483741	510.136592	11.156147
10.444881	508.173478	11.161165
10.318958	521.746635	11.166183
10.684815	522.749946	11.171200
10.640140	527.288410	11.176218
10.603915	529.673393	11.181235
10.810480	529.944145	11.186253
10.497048	534.669615	11.191271
10.815325	522.470711	11.196288
10.689366	529.704147	11.201306
10.775300	532.496126	11.206323
10.643210	530.831535	11.211341
10.672560	537.573754	11.216359
10.728825	527.034499	11.221376
10.555381	537.973774	11.226394
10.625284	534.570517	11.231411
10.684923	535.021928	11.236429
10.808015	530.824629	11.241447
10.830563	529.369481	11.246464
11.178761	529.785432	11.251482
11.216450	539.300186	11.256499
10.660020	520.907199	11.261517
10.387106	516.840984	11.266535
10.869959	520.454748	11.271552
10.746816	524.835022	11.276570
10.732143	535.197334	11.281587
10.899269	530.564007	11.286605
10.941474	544.297189	11.291623
11.322514	531.179673	11.296640
10.946924	530.483916	11.301658
10.708383	516.446753	11.306675
11.108724	516.665246	11.311693
10.508504	516.604040	11.316711
10.789999	520.473207	11.321728
11.195038	531.814695	11.326746
10.615777	528.733407	11.331763
10.994420	526.181447	11.336781
10.745847	536.482351	11.341799
11.259019	533.107904	11.346816
10.824668	533.020873	11.351834
10.948809	528.864434	11.356851
10.969183	536.245495	11.361869
10.604600	538.971925	11.366887
10.735065	530.286116	11.371904
10.576258	530.118316	11.376922
10.410124	532.637130	11.381939
10.970729	529.078581	11.386957
10.955211	548.185389	11.391975
11.154574	548.753896	11.396992
11.170068	547.088415	11.402010
11.122660	542.343326	11.407027
11.221163	534.959472	11.412045
10.726932	538.577052	11.417063
11.172107	536.970899	11.422080
11.330134	549.893979	11.427098
11.105862	551.345764	11.432115
11.130689	528.876657	11.437133
11.003163	536.463774	11.442151
11.257474	545.758620	11.447168
11.582050	539.560809	11.452186
11.215610	541.937250	11.457203
11.198975	524.804530	11.462221
10.761745	542.661078	11.467239
11.283255	538.853005	11.472256
11.244049	535.018630	11.477274
10.961089	536.078781	11.482291
11.455229	542.130125	11.487309
11.068329	551.442760	11.492327
11.129210	558.602938	11.497344
11.639313	564.361483	11.502362
11.397500	554.941550	11.507379
11.505039	532.478494	11.512397
10.822214	540.316166	11.517415
10.907591	549.993907	11.522432
11.466780	557.606653	11.527450
11.364370	555.356794	11.532467
11.273276	558.261543	11.537485
10.952803	568.520014	11.542503
11.278507	562.628120	11.547520
11.812351	565.789005	11.552538
11.380293	566.029807	11.557555
11.586682	561.096882	11.562573
11.255787	558.213594	11.567591
11.458224	555.840537	11.572608
11.443299	561.365258	11.577626
11.394102	563.405141	11.582643
11.401479	567.500027	11.587661
11.564147	559.172093	11.592679
11.296032	560.037438	11.597696
11.466747	563.614607	11.602714
11.380902	554.952998	11.607731
11.687453	560.011117	11.612749
11.215514	565.635396	11.617767
11.262464	557.054091	11.622784
11.513058	560.319034	11.627802
11.240551	562.488356	11.632819
11.330244	562.464894	11.637837
11.466420	565.870723	11.642855
11.711994	568.489536	11.647872
11.653335	564.017582	11.652890
11.564183	569.023709	11.657907
11.853514	562.354871	11.662925
11.416915	565.266080	11.667943
11.324296	558.823962	11.672960
11.449730	561.272139	11.677978
11.230929	553.278144	11.682995
11.679303	563.016134	11.688013
12.025639	571.220581	11.693031
11.721607	569.112561	11.698048
11.681295	562.359354	11.703066
11.710447	566.719082	11.708083
11.561260	564.836252	11.713101
11.653285	574.468792	11.718119
11.741101	573.924936	11.723136
11.712532	570.830480	11.728154
11.961892	579.128921	11.733171
11.647045	571.291878	11.738189
11.322771	570.982589	11.743207
11.798279	580.315593	11.748224
11.907731	585.230845	11.753242
11.712748	583.462437	11.758259
11.924544	583.318983	11.763277
11.888011	587.174567	11.768295
12.048870	582.037294	11.773312
11.957367	578.065891	11.778330
11.650067	580.568823	11.783347
12.117498	575.065097	11.788365
12.143321	568.771785	11.793383
11.813936	567.141065	11.798400
11.875115	560.454103	11.803418
11.700017	559.522011	11.808435
11.866899	554.737243	11.813453
11.942706	567.524821	11.818471
11.604187	563.856957	11.823488
11.917371	577.664735	11.828506
12.204995	581.252106	11.833523
12.102206	579.119064	11.838541
12.152181	569.404395	11.843559
11.897659	568.730810	11.848576
11.999584	561.343256	11.853594
11.744388	565.864016	11.858611
11.886891	576.066185	11.863629
12.122588	583.050839	11.868647
12.051879	581.307261	11.873664
11.969693	572.165411	11.878682
12.009434	581.850274	11.883699
11.919505	591.829876	11.888717
12.219156	587.179057	11.893735
12.064264	587.300969	11.898752
12.432982	581.093116	11.903770
12.158131	585.809437	11.908787
12.156782	583.203027	11.913805
12.122714	585.549814	11.918823
12.057795	589.110029	11.923840
12.588739	586.319761	11.928858
12.374147	583.371027	11.933875
12.096614	572.934207	11.938893
12.029257	570.896630	11.943911
12.075630	570.311892	11.948928
12.244261	582.119391	11.953946
12.092278	586.040286	11.958963
11.950648	575.241491	11.963981
12.483786	588.153531	11.968999
12.029716	586.248743	11.974016
11.973876	587.040015	11.979034
11.907051	588.429421	11.984051
12.161622	587.802799	11.989069
12.462550	586.796589	11.994087
12.221741	587.335805	11.999104
12.657565	575.585603	12.004122
12.346880	580.367460	12.009139
12.159279	580.718517	12.014157
12.638312	578.516978	12.019175
12.351183	584.065153	12.024192
12.557900	582.325716	12.029210
12.206622	589.853023	12.034227
12.024590	580.348033	12.039245
12.240155	576.515006	12.044263
12.332911	584.260343	12.049280
12.612323	579.906155	12.054298
12.279424	587.651497	12.059315
12.279914	580.513248	12.064333
12.061146	577.580943	12.069351
11.984169	593.929841	12.074368
12.752814	594.718972	12.079386
13.023588	606.788284	12.084403
12.691194	609.247792	12.089421
12.832531	592.500650	12.094439
12.690021	592.437605	12.099456
12.529844	577.053341	12.104474
12.211477	586.513107	12.109491
12.520251	586.272506	12.114509
12.608956	583.525848	12.119527
12.645382	592.573787	12.124544
12.840638	583.833685	12.129562
12.720208	582.785786	12.134579
12.506311	587.208606	12.139597
12.673526	581.543346	12.144615
12.632625	583.234815	12.149632
12.555262	582.615695	12.154650
12.404148	583.301885	12.159667
12.486325	593.182111	12.164685
13.016122	611.711798	12.169703
12.619075	607.541817	12.174720
12.482508	600.936119	12.179738
12.539790	606.317073	12.184755
12.826274	611.330997	12.189773
12.708349	613.608796	12.194791
12.452649	613.364565	12.199808
12.704357	608.847432	12.204826
13.084489	612.515078	12.209843
12.735815	611.628941	12.214861
12.862061	609.674822	12.219879
12.792651	616.445071	12.224896
13.348864	603.517971	12.229914
12.926586	614.543370	12.234931
12.685781	615.287705	12.239949
12.760990	611.104153	12.244967
12.612423	626.148308	12.249984
12.694920	617.220626	12.255002
12.769076	605.952731	12.260019
12.606499	615.886855	12.265037
12.616246	604.127237	12.270055
12.284724	611.042430	12.275072
12.683317	610.062038	12.280090
12.921744	626.551199	12.285107
13.373097	638.248448	12.290125
13.157307	613.112274	12.295143
12.598641	624.187316	12.300160
13.240792	621.272435	12.305178
13.320917	634.403358	12.310195
13.138410	626.700314	12.315213
13.037176	617.182724	12.320231
12.791855	625.034363	12.325248
13.203004	618.393873	12.330266
13.366195	615.648236	12.335283
12.999495	619.605724	12.340301
12.845784	617.578431	12.345319
12.997394	629.660001	12.350336
13.334937	637.073770	12.355354
13.236503	635.634294	12.360371
13.326484	633.755244	12.365389
13.113629	628.183857	12.370407
12.509892	623.601101	12.375424
13.303993	637.390850	12.380442
13.455356	636.928613	12.385459
13.305541	642.070433	12.390477
13.394560	636.130163	12.395495
13.287400	646.371244	12.400512
13.447797	632.969283	12.405530
13.299084	633.342688	12.410547
13.114201	626.331109	12.415565
13.401627	628.179739	12.420583
13.336971	629.931714	12.425600
13.659910	639.837594	12.430618
13.119157	623.632106	12.435635
12.913554	627.924262	12.440653
13.524258	630.410499	12.445671
13.417327	637.842980	12.450688
13.586062	628.927111	12.455706
13.470406	628.373908	12.460723
13.396707	625.769290	12.465741
13.683477	612.044723	12.470759
13.163781	622.763416	12.475776
13.199386	612.934200	12.480794
13.167673	613.775363	12.485811
13.366823	631.447714	12.490829
13.678140	632.323829	12.495847
13.404408	642.707604	12.500864
13.113909	641.739827	12.505882
13.533734	638.695463	12.510899
13.188644	642.179394	12.515917
13.460686	636.324233	12.520935
12.964528	635.659866	12.525952
13.239209	643.976484	12.530970
13.562513	646.311817	12.535987
13.126509	643.536396	12.541005
13.792314	648.033696	12.546023
13.286056	651.754154	12.551040
13.541782	649.035128	12.556058
13.706725	653.471561	12.561075
13.653165	660.176245	12.566093
13.705499	662.844093	12.571111
13.923948	656.880508	12.576128
13.562729	655.857472	12.581146
13.825133	656.668623	12.586163
13.400380	663.024017	12.591181
13.903430	654.046617	12.596199
13.802902	660.427265	12.601216
13.817614	655.836571	12.606234
14.007511	665.725311	12.611251
13.842664	658.395031	12.616269
13.695891	655.101222	12.621287
13.592053	657.629288	12.626304
14.164882	658.710832	12.631322
14.024751	653.459462	12.636339
13.602801	644.588217	12.641357
13.428237	650.709000	12.646375
13.612103	661.759971	12.651392
13.819327	658.581453	12.656410
13.911096	661.675490	12.661427
13.741193	665.312024	12.666445
13.897802	661.412422	12.671463
13.718171	655.864254	12.676480
13.523359	661.016241	12.681498
13.954203	654.956474	12.686515
13.694168	654.403661	12.691533
13.784461	661.092259	12.696551
13.907934	669.388252	12.701568
13.779105	656.495191	12.706586
13.823656	660.622179	12.711603
13.987906	672.004402	12.716621
14.412957	673.257273	12.721639
14.112019	669.226942	12.726656
14.098470	657.038586	12.731674
14.078115	654.185826	12.736691
14.002612	659.675829	12.741709
14.278244	668.443575	12.746727
14.003141	664.683769	12.751744
13.810869	673.944075	12.756762
14.095847	679.409516	12.761779
13.976426	681.255226	12.766797
14.665544	682.949805	12.771815
14.492834	684.292590	12.776832
14.414204	677.655754	12.781850
14.267835	665.642700	12.786867
13.857220	665.735002	12.791885
14.201421	661.118251	12.796903
14.327212	672.045731	12.801920
14.070415	671.855318	12.806938
14.491198	676.728434	12.811955
14.254721	678.431428	12.816973
14.098180	680.352343	12.821991
14.404373	686.562383	12.827008
14.326686	683.169453	12.832026
14.696870	678.526563	12.837043
14.262689	680.648490	12.842061
14.033377	671.015118	12.847079
14.302597	669.950727	12.852096
14.361381	681.519784	12.857114
14.861906	674.177416	12.862131
14.429146	685.639977	12.867149
14.668866	675.608539	12.872167
14.441743	667.366489	12.877184
14.322688	663.137434	12.882202
14.505579	652.414294	12.887219
14.500248	670.169012	12.892237
14.392632	666.572469	12.897255
14.612981	676.260821	12.902272
14.588883	680.467927	12.907290
14.404064	671.401964	12.912307
14.487151	679.035242	12.917325
14.555967	679.305355	12.922343
14.820172	684.638337	12.927360
14.635931	684.676460	12.932378
14.677764	677.355016	12.937395
14.276750	683.889751	12.942413
14.356548	675.659869	12.947431
14.571126	685.775143	12.952448
14.575090	689.428792	12.957466
14.907345	683.273916	12.962483
14.715995	685.130826	12.967501
14.813974	680.082207	12.972519
14.940484	687.434184	12.977536
14.664254	686.994340	12.982554
14.646792	678.142149	12.987571
14.864321	684.706808	12.992589
14.759937	685.120647	12.997607
14.887316	677.268351	13.002624
14.209493	687.475234	13.007642
14.926092	680.162336	13.012659
14.427999	682.934820	13.017677
14.649489	675.806304	13.022695
14.838709	686.622936	13.027712
14.575584	684.552713	13.032730
14.547163	682.442792	13.037747
14.647581	676.147296	13.042765
14.726262	686.823353	13.047783
14.798263	688.203774	13.052800
15.251936	700.613890	13.057818
15.288489	695.518029	13.062835
15.003105	694.574699	13.067853
14.770456	687.122424	13.072871
15.280013	681.596328	13.077888
14.973430	691.631808	13.082906
15.049605	686.801170	13.087923
14.550417	687.702497	13.092941
15.111301	701.137301	13.097959
15.496096	691.856413	13.102976
14.962216	696.733009	13.107994
15.046105	684.810320	13.113011
14.949406	683.746098	13.118029
14.765202	689.694832	13.123047
15.174661	700.975782	13.128064
15.145800	711.715933	13.133082
15.170489	700.209536	13.138099
15.131050	701.541040	13.143117
14.956956	701.375618	13.148135
15.268307	698.127234	13.153152
15.322850	703.218320	13.158170
15.325092	689.156154	13.163187
15.214623	706.226712	13.168205
15.221131	703.082593	13.173223
15.559984	709.167639	13.178240
15.370881	710.377283	13.183258
15.418987	705.257530	13.188275
15.625528	706.869462	13.193293
15.471540	691.070739	13.198311
14.941927	675.018099	13.203328
15.086716	691.338870	13.208346
15.112449	695.058555	13.213363
15.370587	696.924375	13.218381
15.091804	703.298080	13.223399
15.426887	707.089520	13.228416
14.907264	707.605879	13.233434
15.281705	709.627156	13.238451
15.040116	707.872303	13.243469
15.196083	699.488544	13.248487
15.393111	695.544773	13.253504
15.173670	712.547100	13.258522
15.579685	715.541729	13.263539
15.333436	723.961581	13.268557
15.347650	725.710753	13.273575
15.561483	727.700235	13.278592
15.692162	728.213173	13.283610
15.910696	716.099091	13.288627
15.642180	725.447032	13.293645
15.674244	730.825639	13.298663
15.995929	719.307701	13.303680
15.465823	713.429087	13.308698
15.635124	706.163523	13.313715
15.481825	713.139367	13.318733
15.591427	716.262194	13.323751
16.209834	720.460790	13.328768
15.711668	710.332786	13.333786
15.518543	706.976759	13.338803
15.719070	708.861018	13.343821
15.646107	716.537543	13.348839
15.666333	718.017543	13.353856
15.580908	727.321200	13.358874
15.691860	724.539499	13.363891
15.873976	720.926237	13.368909
15.622067	722.710531	13.373927
15.757386	718.858411	13.378944
15.913228	732.952729	13.383962
15.556579	726.204532	13.388979
15.655124	728.145695	13.393997
15.685645	734.897273	13.399015
15.669895	725.401029	13.404032
15.651065	727.619234	13.409050
15.986252	728.854543	13.414067
16.212063	726.553561	13.419085
15.676234	733.614216	13.424103
15.691735	735.353721	13.429120
15.874209	743.848840	13.434138
16.304956	749.108576	13.439155
16.518580	746.815800	13.444173
16.248629	730.179900	13.449191
16.232713	717.379665	13.454208
16.062016	722.600496	13.459226
15.945773	713.388139	13.464243
16.001220	714.105287	13.469261
16.165705	719.677860	13.474279
16.472688	720.254863	13.479296
16.124400	718.582891	13.484314
16.365656	719.589836	13.489331
16.452491	716.524723	13.494349
16.285237	717.850882	13.499367
16.303839	716.595142	13.504384
16.302107	718.816996	13.509402
15.938803	714.689071	13.514419
16.086613	718.771594	13.519437
16.017657	723.992364	13.524455
16.368253	715.998002	13.529472
16.020494	728.015382	13.534490
15.655311	723.799388	13.539507
16.059294	732.572428	13.544525
16.167018	739.024819	13.549543
16.590712	737.232651	13.554560
16.642575	741.484748	13.559578
16.240727	745.832732	13.564595
16.621854	745.602954	13.569613
16.687369	753.330516	13.574631
16.649370	740.451653	13.579648
16.718896	746.143158	13.584666
16.515598	744.533814	13.589683
16.249769	720.080601	13.594701
16.530100	729.289443	13.599719
16.623390	735.116096	13.604736
16.571826	730.986966	13.609754
16.412029	735.994672	13.614771
16.628944	739.943368	13.619789
16.360791	750.061257	13.624807
16.836882	741.583457	13.629824
16.700325	747.348072	13.634842
16.634763	749.627203	13.639859
16.754857	736.897292	13.644877
16.518264	742.674326	13.649895
17.026029	745.230253	13.654912
16.498275	728.656584	13.659930
16.673606	733.482727	13.664947
16.772445	738.257668	13.669965
16.625665	749.719923	13.674983
16.989699	738.791809	13.680000
16.804495	749.086124	13.685018
16.602173	743.816009	13.690035
17.105916	743.516649	13.695053
16.610924	740.715683	13.700071
16.618567	734.873254	13.705088
16.803086	737.997043	13.710106
16.577966	740.919534	13.715123
16.716777	735.214467	13.720141
16.798739	733.131534	13.725159
16.761500	737.542665	13.730176
16.910673	745.954609	13.735194
16.974387	746.383302	13.740211
17.111725	742.556108	13.745229
16.765877	754.169277	13.750247
16.754107	749.109326	13.755264
16.910545	738.929878	13.760282
16.581726	750.896989	13.765299
16.821148	752.153522	13.770317
16.688544	752.578068	13.775335
17.166350	768.670341	13.780352
17.230568	776.855693	13.785370
16.967986	778.821530	13.790387
17.151232	772.522571	13.795405
17.080585	773.000585	13.800423
17.409085	771.797574	13.805440
17.404397	768.390107	13.810458
16.760295	765.426167	13.815475
17.175755	768.775929	13.820493
16.977646	772.177042	13.825511
17.095837	767.958360	13.830528
17.419946	777.674792	13.835546
17.087476	769.370204	13.840563
17.395150	765.576443	13.845581
17.174958	764.411526	13.850599
17.221884	772.126212	13.855616
17.459796	764.007367	13.860634
17.276607	774.118352	13.865651
17.344588	768.578933	13.870669
17.497505	777.839195	13.875687
17.305041	769.951452	13.880704
16.980525	770.961284	13.885722
16.984753	774.513925	13.890739
17.391623	763.837894	13.895757
17.496141	770.934561	13.900775
17.493951	771.080034	13.905792
17.406849	771.980320	13.910810
17.343162	768.370606	13.915827
17.407117	761.263428	13.920845
17.078077	769.825577	13.925863
17.328119	767.369342	13.930880
17.616214	773.664279	13.935898
17.317607	790.824169	13.940915
17.371089	786.924817	13.945933
17.356192	787.476201	13.950951
17.473801	792.115693	13.955968
17.792927	792.776012	13.960986
17.535725	798.729836	13.966003
17.709328	786.281886	13.971021
17.553288	794.675103	13.976039
17.576840	795.062715	13.981056
17.875390	791.134673	13.986074
17.706771	798.608383	13.991091
17.757744	787.116772	13.996109
17.679040	788.104111	14.001127
17.768104	795.117990	14.006144
17.846807	796.134469	14.011162
17.732042	794.221009	14.016179
17.735795	789.748748	14.021197
17.753483	787.328687	14.026215
17.515669	789.558905	14.031232
18.146998	786.519454	14.036250
17.595286	789.641120	14.041267
17.850099	785.767224	14.046285
18.240879	800.222638	14.051303
17.765292	796.866392	14.056320
18.090116	791.261730	14.061338
17.955668	792.592254	14.066355
18.119533	795.776073	14.071373
18.141206	799.064079	14.076391
18.181042	793.601616	14.081408
17.964951	782.949984	14.086426
18.064831	790.773195	14.091443
18.118700	781.824642	14.096461
18.219822	789.941140	14.101479
18.399524	790.733617	14.106496
18.035911	783.582550	14.111514
18.202266	785.203901	14.116531
17.949350	776.599753	14.121549
18.591311	790.558473	14.126567
18.218244	784.147315	14.131584
18.240063	782.868980	14.136602
18.085979	784.357191	14.141619
18.471786	773.491935	14.146637
18.658005	785.189537	14.151655
18.789217	783.998308	14.156672
18.616015	772.850869	14.161690
18.479132	781.616628	14.166707
18.439793	785.311751	14.171725
18.083910	783.218089	14.176743
18.111451	786.527270	14.181760
17.922988	780.040036	14.186778
18.217024	786.425568	14.191795
18.356287	784.308462	14.196813
18.357582	783.894831	14.201831
18.380092	796.839191	14.206848
18.539827	800.373938	14.211866
18.502118	807.647393	14.216883
18.523510	810.645119	14.221901
18.305477	800.028493	14.226919
18.547947	811.865673	14.231936
18.866266	814.145002	14.236954
18.517039	815.837162	14.241971
18.645695	809.499354	14.246989
18.840677	805.808334	14.252007
18.580688	806.218002	14.257024
18.777378	798.897644	14.262042
18.496599	804.123015	14.267059
18.743778	811.459411	14.272077
18.629590	808.820045	14.277095
18.275949	819.554026	14.282112
18.872759	809.252326	14.287130
18.598677	813.908629	14.292147
18.942150	819.529104	14.297165
18.972998	816.652566	14.302183
18.881488	822.306054	14.307200
18.849632	808.255414	14.312218
19.086388	813.782052	14.317235
18.832658	810.864619	14.322253
18.941745	818.654851	14.327271
18.819039	820.226540	14.332288
19.018985	807.250624	14.337306
19.148939	813.491304	14.342323
18.925504	812.610903	14.347341
19.254929	812.341838	14.352359
19.029977	811.928720	14.357376
19.182144	806.448763	14.362394
19.269281	808.767241	14.367411
18.967359	788.734402	14.372429
19.148104	797.059406	14.377447
18.993339	800.977625	14.382464
19.089237	802.016673	14.387482
19.058137	807.401982	14.392499
19.092639	809.185871	14.397517
19.270220	808.877334	14.402535
18.991358	816.466043	14.407552
19.087690	805.311331	14.412570
19.001161	800.360832	14.417587
19.068209	808.870797	14.422605
19.243493	804.179326	14.427623
19.124927	808.798791	14.432640
19.272369	801.653353	14.437658
18.948583	813.165299	14.442675
19.160060	806.196076	14.447693
19.110342	800.510874	14.452711
18.925722	793.603327	14.457728
19.012230	805.941299	14.462746
19.418961	818.636509	14.467763
19.508232	822.671368	14.472781
19.588969	836.294637	14.477799
19.302731	836.190854	14.482816
19.696243	825.523177	14.487834
19.651513	829.525253	14.492851
19.623981	838.674791	14.497869
19.522638	830.864350	14.502887
19.476912	826.384004	14.507904
19.684422	829.273863	14.512922
19.757448	835.873699	14.517939
19.240570	809.502902	14.522957
19.530094	827.906127	14.527975
19.620574	840.637970	14.532992
19.762386	830.646935	14.538010
19.266516	834.930686	14.543027
19.673289	837.070017	14.548045
19.816241	832.279434	14.553063
19.736941	832.534741	14.558080
19.686315	837.856829	14.563098
19.694239	836.583809	14.568115
19.594142	831.837380	14.573133
19.880206	828.734917	14.578151
19.669314	832.475694	14.583168
19.719804	824.300798	14.588186
19.459143	828.188174	14.593203
19.630423	837.063766	14.598221
20.462038	828.038279	14.603239
20.151067	823.536117	14.608256
19.676485	833.761931	14.613274
19.761008	841.950463	14.618291
19.884620	835.228432	14.623309
20.043361	826.219349	14.628327
19.870340	833.517039	14.633344
19.907440	824.334396	14.638362
19.540030	824.770256	14.643379
19.988201	837.522143	14.648397
19.867420	845.928830	14.653415
20.115035	839.998512	14.658432
19.866319	841.798099	14.663450
20.217226	845.593417	14.668467
20.082731	851.076885	14.673485
19.964996	851.467561	14.678503
20.155266	861.479426	14.683520
20.287013	845.967429	14.688538
20.695212	851.672508	14.693555
20.391309	848.636651	14.698573
20.452175	843.862001	14.703591
20.539273	847.755196	14.708608
20.723694	846.593548	14.713626
20.258862	830.906212	14.718643
20.441186	836.289857	14.723661
20.875987	837.951466	14.728679
20.441677	829.189347	14.733696
20.214862	829.505490	14.738714
20.479907	813.512032	14.743731
20.287063	823.905408	14.748749
20.085185	824.151398	14.753767
20.209972	836.025851	14.758784
20.357779	839.480414	14.763802
20.355916	841.749639	14.768819
20.527461	844.752394	14.773837
20.575203	841.005399	14.778855
20.272502	846.253130	14.783872
20.709229	852.398725	14.788890
20.619621	836.290055	14.793907
20.283968	856.570474	14.798925
20.677161	846.332013	14.803943
20.258483	854.826110	14.808960
20.470714	849.128510	14.813978
20.667026	844.705147	14.818995
20.705659	852.550544	14.824013
20.927881	861.500266	14.829031
20.674836	868.106702	14.834048
21.098030	863.487068	14.839066
21.054833	859.078902	14.844083
20.960800	854.814348	14.849101
20.899620	850.677221	14.854119
20.247807	850.286382	14.859136
20.802817	856.268399	14.864154
21.055499	866.497761	14.869171
20.631279	870.255981	14.874189
21.072302	875.719278	14.879207
20.660021	869.708661	14.884224
21.112251	867.293515	14.889242
21.175385	868.242996	14.894259
21.074461	873.058542	14.899277
21.146115	870.219823	14.904295
20.933154	870.401269	14.909312
21.061432	875.723915	14.914330
21.310369	869.077031	14.919347
21.063783	870.459734	14.924365
21.179580	862.912109	14.929383
21.386064	863.154478	14.934400
21.346624	860.209984	14.939418
21.655681	858.577661	14.944435
21.042880	849.410987	14.949453
21.519835	846.922569	14.954471
21.344321	848.944283	14.959488
20.827795	850.286963	14.964506
21.244708	859.727066	14.969523
21.201942	857.448949	14.974541
21.587634	861.147338	14.979559
21.312923	867.694033	14.984576
21.259981	868.241875	14.989594
21.298915	864.370017	14.994611
21.097985	867.847325	14.999629
21.432944	858.015546	15.004647
21.230477	865.636561	15.009664
21.582378	875.572777	15.014682
21.629214	866.584252	15.019699
21.423854	870.156922	15.024717
21.275730	864.423907	15.029735
21.145627	876.937661	15.034752
21.550010	864.841879	15.039770
21.567912	860.711371	15.044787
21.297518	867.389933	15.049805
21.775288	874.172914	15.054823
21.302573	879.589133	15.059840
21.470186	885.754549	15.064858
21.826089	894.525688	15.069875
21.730740	899.305659	15.074893
21.834064	893.833280	15.079911
21.672078	889.317373	15.084928
21.589926	895.275532	15.089946
21.616888	898.247160	15.094963
21.571316	890.039854	15.099981
21.906132	888.618107	15.104999
22.186221	883.364357	15.110016
22.176298	897.692893	15.115034
21.934619	888.619893	15.120051
21.882983	888.050403	15.125069
22.022287	884.787748	15.130087
22.014863	878.729872	15.135104
21.985655	894.008127	15.140122
22.289118	883.474354	15.145139
21.950856	886.950958	15.150157
22.028599	888.182181	15.155175
21.602249	890.425987	15.160192
21.805177	893.291323	15.165210
22.221186	887.656656	15.170227
21.746563	896.244687	15.175245
21.978335	901.058933	15.180263
22.229974	903.118287	15.185280
22.226858	916.656845	15.190298
22.849931	914.344479	15.195315
22.854722	903.093508	15.200333
22.843863	881.674059	15.205351
22.396997	888.181295	15.210368
22.418461	887.616203	15.215386
22.576050	886.685942	15.220403
22.530632	879.024558	15.225421
22.622058	884.308764	15.230439
22.528632	879.684357	15.235456
22.530537	888.097208	15.240474
22.764380	871.243885	15.245491
22.613301	872.059465	15.250509
22.670019	870.879829	15.255527
22.295025	869.802122	15.260544
22.566504	871.511253	15.265562
22.818799	870.121290	15.270579
22.469361	865.167525	15.275597
22.379146	872.502830	15.280615
22.570714	877.143452	15.285632
22.574455	884.022331	15.290650
22.650869	870.383964	15.295667
22.761016	881.190936	15.300685
22.776451	871.307914	15.305703
22.397207	881.720878	15.310720
22.706312	885.554270	15.315738
22.913241	874.650533	15.320755
22.556429	885.940455	15.325773
22.671649	877.837505	15.330791
22.487127	873.504986	15.335808
22.156879	883.610529	15.340826
22.477414	879.331914	15.345843
22.760249	901.292765	15.350861
22.960595	901.845353	15.355879
23.274260	901.263167	15.360896
23.225621	907.951399	15.365914
23.235787	896.851070	15.370931
22.982653	887.385387	15.375949
22.886058	873.707684	15.380967
23.194413	878.402706	15.385984
22.783304	882.862615	15.391002
23.122959	889.080139	15.396019
22.959865	895.754630	15.401037
23.060317	899.876126	15.406055
23.294869	905.330554	15.411072
23.413337	904.198104	15.416090
23.539971	898.277136	15.421107
23.236009	903.686023	15.426125
23.308786	902.024213	15.431143
23.479520	894.471177	15.436160
22.910780	889.936549	15.441178
23.249018	891.935083	15.446195
23.331252	892.092658	15.451213
22.859299	894.267827	15.456231
23.453393	905.457046	15.461248
23.301355	912.249739	15.466266
23.307616	902.333415	15.471283
23.244179	907.837395	15.476301
23.499695	902.786276	15.481319
23.416685	903.619661	15.486336
23.510384	899.016606	15.491354
23.513499	906.078623	15.496371
23.436729	898.065515	15.501389
23.549379	896.814054	15.506407
23.240141	893.750619	15.511424
23.302184	905.006896	15.516442
23.797094	912.361567	15.521459
23.853869	927.314045	15.526477
23.968985	923.054781	15.531495
23.715863	900.738930	15.536512
23.635879	900.861804	15.541530
23.652777	906.435325	15.546547
23.794536	916.861863	15.551565
23.774334	917.975798	15.556583
24.227854	911.713603	15.561600
23.543158	908.023827	15.566618
23.995840	920.535235	15.571635
23.758793	917.583630	15.576653
23.967611	920.003095	15.581671
24.136940	921.885922	15.586688
24.124454	933.005502	15.591706
24.047331	923.345141	15.596723
23.743398	926.343047	15.601741
23.905302	928.968629	15.606759
24.127388	921.098324	15.611776
23.788796	931.640684	15.616794
24.400716	929.415258	15.621811
24.313749	922.770160	15.626829
24.244825	928.347583	15.631847
24.662623	925.129921	15.636864
24.256794	917.527791	15.641882
24.036979	907.043919	15.646899
24.178743	916.176605	15.651917
23.917201	917.113525	15.656935
24.533207	922.319223	15.661952
24.119510	924.040366	15.666970
24.221357	917.249111	15.671987
24.372097	915.486801	15.677005
24.243644	915.077590	15.682023
24.319560	907.993737	15.687040
23.964112	921.041214	15.692058
24.316893	924.094658	15.697075
24.165998	917.699353	15.702093
24.161293	917.103621	15.707111
24.244199	919.978182	15.712128
24.338197	942.138894	15.717146
24.619315	940.179560	15.722163
24.635772	942.786765	15.727181
24.459379	945.704857	15.732199
24.983258	945.572770	15.737216
24.591677	938.757348	15.742234
24.853772	946.201928	15.747251
24.732482	945.147830	15.752269
24.495654	944.534590	15.757287
24.779798	932.034614	15.762304
24.627774	946.492609	15.767322
24.837019	946.349550	15.772339
24.638278	949.290057	15.777357
24.839301	940.583595	15.782375
24.875766	935.023785	15.787392
24.598441	936.531196	15.792410
24.834823	943.888263	15.797427
24.781398	933.214370	15.802445
24.787913	936.684639	15.807463
25.000302	933.246498	15.812480
24.763583	941.390419	15.817498
25.222515	945.042710	15.822515
25.258040	950.127361	15.827533
24.700094	949.857601	15.832551
25.284784	951.439081	15.837568
25.610803	961.212120	15.842586
25.600292	932.897256	15.847603
25.814461	913.718021	15.852621
25.390562	921.944725	15.857639
25.402072	915.637741	15.862656
25.772997	927.937826	15.867674
25.455063	929.435781	15.872691
25.448142	909.757653	15.877709
25.389069	922.137306	15.882727
25.675537	914.825013	15.887744
25.471709	919.173765	15.892762
25.421634	916.978827	15.897779
25.654363	912.619204	15.902797
25.115870	913.627645	15.907815
25.576120	903.956210	15.912832
25.312285	917.383887	15.917850
25.440435	917.837265	15.922867
25.438730	911.882627	15.927885
25.176121	923.284135	15.932903
25.234732	915.328834	15.937920
25.620481	918.074194	15.942938
25.304715	926.135744	15.947955
25.339910	915.422819	15.952973
25.490671	918.962142	15.957991
25.837094	919.776003	15.963008
25.555769	929.066085	15.968026
25.841545	946.008910	15.973043
26.025101	941.672714	15.978061
26.067002	948.113340	15.983079
26.057449	927.501503	15.988096
25.732070	929.780084	15.993114
25.663251	927.237776	15.998131
26.039475	932.575483	16.003149
25.714035	941.175022	16.008167
25.834893	931.417561	16.013184
25.757289	940.461341	16.018202
25.783095	950.662961	16.023219
25.991425	944.445241	16.028237
25.566847	941.415533	16.033255
25.599505	945.396120	16.038272
26.035761	943.958575	16.043290
26.204036	951.158994	16.048307
26.199459	954.369067	16.053325
26.343631	948.644163	16.058343
26.311295	946.878796	16.063360
26.130212	948.699421	16.068378
25.947202	947.535014	16.073395
26.272855	949.705924	16.078413
26.229646	960.495795	16.083431
26.486271	958.792733	16.088448
26.437234	972.048155	16.093466
26.661950	976.024092	16.098483
27.002104	967.791407	16.103501
26.348155	962.010885	16.108519
26.468431	939.952423	16.113536
26.359792	939.672668	16.118554
26.053964	950.727480	16.123571
26.526901	960.360882	16.128589
26.631254	967.583883	16.133607
26.571926	968.931126	16.138624
26.703296	969.999374	16.143642
26.509158	970.783794	16.148659
26.698525	966.582384	16.153677
26.408388	969.126878	16.158695
26.645849	966.849297	16.163712
27.039342	956.250971	16.168730
26.575992	969.842292	16.173747
26.737457	965.443260	16.178765
26.566518	971.128095	16.183783
26.758255	963.470776	16.188800
26.662317	964.934170	16.193818
26.618250	967.607606	16.198835
26.684453	960.070817	16.203853
26.562536	978.651865	16.208871
26.935760	979.947541	16.213888
27.103778	981.679103	16.218906
27.001100	983.156170	16.223923
26.956265	977.104085	16.228941
27.235182	971.645368	16.233959
27.168633	977.815717	16.238976
27.238481	974.106276	16.243994
26.900670	989.915491	16.249011
27.334634	980.882413	16.254029
27.203240	975.023683	16.259047
27.122910	976.907518	16.264064
27.395474	977.742349	16.269082
26.793320	979.521240	16.274099
27.594792	975.697889	16.279117
27.189048	974.325166	16.284135
27.549313	971.829653	16.289152
27.353385	983.672089	16.294170
27.132384	981.964495	16.299187
27.456141	971.045665	16.304205
27.515703	974.226821	16.309223
26.961947	974.543377	16.314240
27.427112	981.770167	16.319258
27.010657	985.789129	16.324275
27.634235	993.827533	16.329293
27.568111	996.154118	16.334311
27.782866	995.899749	16.339328
28.161025	996.093302	16.344346
27.963871	989.225498	16.349363
27.914820	978.781267	16.354381
27.867980	975.030034	16.359399
27.859049	973.052742	16.364416
27.841110	969.640987	16.369434
27.642553	971.565319	16.374451
27.834795	966.104319	16.379469
27.904624	968.633792	16.384487
28.383973	982.125685	16.389504
28.108969	973.420741	16.394522
27.956942	979.115257	16.399539
27.877570	974.378186	16.404557
28.037440	968.467798	16.409575
27.968517	966.774397	16.414592
28.077389	972.440914	16.419610
27.868074	977.926603	16.424627
27.927920	981.824071	16.429645
28.252673	992.641877	16.434663
28.123200	997.048498	16.439680
28.250305	996.388061	16.444698
27.997493	997.809611	16.449715
28.301084	996.657801	16.454733
28.043227	992.563885	16.459751
27.936089	995.477514	16.464768
28.325841	993.434991	16.469786
28.029110	993.342307	16.474803
28.485617	999.295529	16.479821
28.171373	995.967771	16.484839
28.542250	990.848175	16.489856
28.488628	989.972883	16.494874
28.041637	984.519887	16.499891
28.472605	993.670701	16.504909
28.437430	1012.118360	16.509927
28.583920	1018.006249	16.514944
28.813683	1011.037255	16.519962
28.549363	1011.958833	16.524979
28.653471	1018.604390	16.529997
28.721599	1026.672486	16.535015
28.948855	1017.236079	16.540032
29.159560	1014.397777	16.545050
28.980285	1016.230751	16.550067
28.859622	998.741392	16.555085
28.647790	995.792159	16.560103
28.824069	1001.097902	16.565120
28.673283	1009.225320	16.570138
28.754649	1015.612489	16.575155
29.048259	1008.775564	16.580173
28.731577	1007.543604	16.585191
29.094505	1015.332271	16.590208
28.980117	1016.713336	16.595226
29.218221	1026.623174	16.600243
29.435552	1015.234900	16.605261
29.099271	1014.510912	16.610279
29.066255	1016.027628	16.615296
29.431933	1007.844599	16.620314
29.003381	1017.236543	16.625331
29.101643	1016.552195	16.630349
29.258713	1016.458283	16.635367
28.531028	1016.628353	16.640384
28.934149	1015.637767	16.645402
29.030317	1022.133086	16.650419
28.960888	1010.335034	16.655437
28.965342	1017.712462	16.660455
29.253396	1037.378436	16.665472
29.486141	1021.026908	16.670490
29.281987	1036.278876	16.675507
29.620631	1046.466557	16.680525
29.565871	1038.033398	16.685543
29.016139	1038.838471	16.690560
29.510873	1035.034464	16.695578
29.316081	1036.052514	16.700595
29.399077	1032.126423	16.705613
29.631648	1037.069967	16.710631
29.117250	1040.312096	16.715648
29.787982	1048.535684	16.720666
29.888602	1064.510229	16.725683
30.277302	1067.785322	16.730701
30.309160	1058.189970	16.735719
29.913400	1048.380339	16.740736
30.232708	1038.459380	16.745754
29.900844	1044.074622	16.750771
30.091460	1036.953925	16.755789
30.140189	1033.373990	16.760807
29.600097	1042.685486	16.765824
30.172544	1030.519244	16.770842
30.199683	1045.110368	16.775859
30.348692	1037.626925	16.780877
30.103161	1024.480372	16.785895
29.898139	1029.283766	16.790912
29.822832	1033.514707	16.795930
29.729016	1039.067638	16.800947
30.341197	1051.535372	16.805965
30.398040	1054.385610	16.810983
30.343822	1062.397033	16.816000
30.282940	1058.938299	16.821018
29.803824	1064.289299	16.826035
30.379489	1060.011945	16.831053
30.116253	1061.539263	16.836071
30.004129	1061.812306	16.841088
30.257773	1054.965808	16.846106
30.067456	1061.139676	16.851123
30.109429	1076.201881	16.856141
30.616784	1074.734322	16.861159
30.345640	1072.412840	16.866176
30.314723	1076.144581	16.871194
31.002203	1072.471500	16.876211
30.965791	1072.657018	16.881229
31.084672	1074.557183	16.886247
30.840817	1081.569360	16.891264
30.843157	1077.996639	16.896282
30.860029	1074.219688	16.901299
30.857473	1082.150493	16.906317
31.098264	1070.872139	16.911335
30.747502	1065.116961	16.916352
30.646181	1057.890232	16.921370
30.863738	1070.207984	16.926387
31.032188	1081.343666	16.931405
31.475719	1074.571735	16.936423
30.940237	1066.317550	16.941440
31.162648	1055.247192	16.946458
30.971051	1064.406611	16.951475
31.178563	1063.683160	16.956493
31.237645	1065.049844	16.961511
30.921245	1078.637303	16.966528
31.202410	1084.939741	16.971546
31.007289	1082.549618	16.976563
30.960268	1075.525864	16.981581
31.241743	1072.016980	16.986599
31.054191	1081.851112	16.991616
31.301158	1074.895194	16.996634
31.174341	1076.549594	17.001651
31.122282	1075.752949	17.006669
31.107352	1074.657038	17.011687
31.449906	1082.376323	17.016704
31.588415	1076.440824	17.021722
31.685441	1077.590164	17.026739
31.373416	1078.149949	17.031757
31.831720	1082.020114	17.036775
31.731379	1073.688708	17.041792
31.568207	1079.435484	17.046810
31.707108	1083.405871	17.051827
31.601959	1090.248135	17.056845
32.063731	1095.518924	17.061863
31.993881	1092.897859	17.066880
31.667334	1078.892887	17.071898
32.245549	1079.146810	17.076915
31.653438	1073.419739	17.081933
31.810984	1074.515476	17.086951
31.696559	1093.922288	17.091968
31.798983	1096.459327	17.096986
31.967384	1097.433456	17.102003
32.042115	1093.366629	17.107021
32.595628	1093.861081	17.112039
32.411369	1101.596125	17.117056
31.834965	1087.967715	17.122074
32.033940	1088.286995	17.127091
32.234089	1094.169711	17.132109
32.231726	1093.377951	17.137127
31.991433	1098.606572	17.142144
32.054075	1091.783486	17.147162
32.298696	1091.874756	17.152179
32.136921	1088.201354	17.157197
32.613248	1093.009134	17.162215
31.973805	1093.234893	17.167232
32.145297	1102.135831	17.172250
32.227216	1099.724662	17.177267
31.932191	1096.636887	17.182285
32.401699	1104.822405	17.187303
32.517634	1120.737813	17.192320
32.627003	1115.797750	17.197338
32.545949	1112.070750	17.202355
32.769828	1117.306002	17.207373
32.810571	1119.653834	17.212391
32.640582	1118.512634	17.217408
32.588460	1107.794253	17.222426
32.958041	1114.048223	17.227443
32.962461	1115.723219	17.232461
32.858185	1108.632628	17.237479
32.599214	1119.793856	17.242496
32.645728	1113.162619	17.247514
32.984537	1112.986763	17.252531
32.410288	1121.123359	17.257549
32.832221	1104.328893	17.262567
32.908477	1105.547741	17.267584
32.788410	1111.657041	17.272602
33.336642	1120.366790	17.277619
32.739859	1121.198127	17.282637
33.232916	1119.909513	17.287655
33.134254	1132.585808	17.292672
33.158460	1126.753294	17.297690
33.562882	1119.331035	17.302707
33.297581	1135.668726	17.307725
33.526844	1133.559657	17.312743
33.663263	1132.449645	17.317760
33.555510	1130.601328	17.322778
33.413577	1113.749479	17.327795
33.182091	1116.322730	17.332813
33.412355	1117.555470	17.337831
33.288726	1132.709777	17.342848
33.439581	1132.014079	17.347866
33.457198	1140.853789	17.352883
33.308068	1137.326730	17.357901
33.375089	1130.083229	17.362919
33.424437	1131.252619	17.367936
33.096421	1131.511940	17.372954
33.529458	1131.630679	17.377971
33.537293	1143.148010	17.382989
33.700700	1147.486977	17.388007
33.962367	1150.469442	17.393024
34.225027	1146.764659	17.398042
34.586880	1135.347496	17.403059
34.532669	1129.019111	17.408077
34.310190	1119.564310	17.413095
34.495385	1122.653349	17.418112
34.315714	1116.931475	17.423130
34.543312	1117.725977	17.428147
34.001843	1120.574708	17.433165
34.442075	1113.146876	17.438183
34.469888	1113.139359	17.443200
33.883364	1121.448278	17.448218
33.837029	1117.539149	17.453235
33.649752	1119.335509	17.458253
33.797802	1108.857357	17.463271
33.598373	1119.782100	17.468288
33.794711	1134.144985	17.473306
34.306254	1128.810946	17.478323
33.993425	1142.940691	17.483341
34.287455	1142.333153	17.488359
34.288911	1144.377840	17.493376
34.567506	1136.164130	17.498394
34.537196	1136.544356	17.503411
34.571754	1141.641835	17.508429
34.488225	1144.999933	17.513447
34.387646	1152.958654	17.518464
34.279573	1157.308334	17.523482
34.907569	1156.345845	17.528499
34.764019	1160.678959	17.533517
34.806208	1169.754697	17.538535
34.703308	1160.123467	17.543552
34.457836	1167.795488	17.548570
35.129074	1159.012554	17.553587
34.791704	1163.009775	17.558605
34.881814	1156.832478	17.563623
34.758334	1167.840099	17.568640
34.575755	1167.934767	17.573658
34.740305	1167.852313	17.578675
35.187137	1181.216877	17.583693
35.180214	1190.612694	17.588711
35.161588	1184.512277	17.593728
35.183901	1186.739912	17.598746
35.244158	1192.171073	17.603763
35.369301	1190.744079	17.608781
35.077262	1185.093327	17.613799
35.568044	1182.596398	17.618816
35.437164	1186.813938	17.623834
35.573818	1183.955582	17.628851
35.376403	1186.144844	17.633869
35.530417	1188.538166	17.638887
35.547282	1181.996725	17.643904
35.163967	1193.234164	17.648922
35.977530	1182.399889	17.653939
35.539636	1185.223036	17.658957
35.523603	1188.472804	17.663975
35.891885	1180.876267	17.668992
35.543288	1190.009702	17.674010
35.843558	1179.706624	17.679027
36.065178	1181.773840	17.684045
35.545698	1182.959214	17.689063
35.691312	1182.914422	17.694080
35.893945	1187.897384	17.699098
35.979303	1181.178023	17.704115
35.945368	1187.737840	17.709133
35.949580	1182.347075	17.714151
36.029514	1178.137408	17.719168
35.673898	1185.062886	17.724186
36.011409	1186.638691	17.729203
36.127603	1189.855249	17.734221
35.803350	1182.792566	17.739239
35.988027	1188.844979	17.744256
36.424967	1211.312391	17.749274
36.192452	1204.607799	17.754291
36.452349	1201.304221	17.759309
36.275999	1202.190021	17.764327
36.709197	1193.450444	17.769344
36.285503	1201.645686	17.774362
36.475393	1206.251943	17.779379
36.210468	1208.574794	17.784397
36.632463	1198.300090	17.789415
36.617857	1200.404088	17.794432
36.592287	1203.273493	17.799450
36.634344	1201.070488	17.804467
36.676290	1203.579089	17.809485
36.498886	1198.664717	17.814503
36.660402	1197.172100	17.819520
36.317206	1203.836876	17.824538
36.825450	1199.342769	17.829555
36.751272	1206.442186	17.834573
36.664708	1204.966102	17.839591
36.823388	1218.978314	17.844608
36.961396	1233.719588	17.849626
37.041112	1221.825592	17.854643
37.165782	1224.337095	17.859661
36.976577	1229.128612	17.864679
37.122647	1230.740540	17.869696
37.047193	1233.336852	17.874714
36.787646	1230.461279	17.879731
37.231259	1237.019345	17.884749
37.068579	1226.810409	17.889767
36.802849	1221.123992	17.894784
36.919490	1237.556944	17.899802
37.043959	1228.073313	17.904819
36.817401	1235.104948	17.909837
36.985362	1245.306694	17.914855
37.585659	1251.234458	17.919872
37.302929	1249.833093	17.924890
37.640106	1252.081141	17.929907
37.611644	1245.344764	17.934925
37.728217	1243.745531	17.939943
37.339648	1241.540139	17.944960
37.641543	1251.291848	17.949978
37.723823	1243.247509	17.954995
37.572678	1238.398466	17.960013
37.414974	1245.384671	17.965031
37.715599	1242.286182	17.970048
37.625203	1243.556232	17.975066
37.954382	1254.319861	17.980083
38.300811	1265.857137	17.985101
38.309233	1260.169048	17.990119
38.447099	1238.214775	17.995136
38.103658	1240.234276	18.000154
38.403874	1232.399007	18.005171
38.445580	1232.181045	18.010189
38.397004	1237.881628	18.015207
37.978662	1232.159008	18.020224
38.314568	1233.103909	18.025242
38.339481	1233.554434	18.030259
38.428745	1236.980321	18.035277
38.217633	1237.271934	18.040295
38.319473	1236.495502	18.045312
38.488096	1245.374869	18.050330
38.653920	1233.558976	18.055347
38.529101	1237.406356	18.060365
38.027855	1238.024008	18.065383
38.178004	1231.692170	18.070400
38.325001	1239.359921	18.075418
38.545782	1261.280385	18.080435
38.706631	1266.254096	18.085453
38.724200	1263.221764	18.090471
39.078944	1260.910107	18.095488
38.802675	1257.055681	18.100506
38.674936	1264.179239	18.105523
38.877616	1258.599761	18.110541
38.550692	1264.993784	18.115559
38.872644	1257.723163	18.120576
38.683879	1260.775776	18.125594
38.682462	1264.076931	18.130611
39.055333	1268.477990	18.135629
38.941219	1269.726488	18.140647
38.943214	1261.287543	18.145664
38.880663	1269.713765	18.150682
38.997674	1276.859182	18.155699
38.835641	1272.620894	18.160717
39.062956	1273.137737	18.165735
39.290378	1278.145267	18.170752
39.284777	1283.400517	18.175770
39.343749	1277.723487	18.180787
39.229554	1279.347539	18.185805
39.565194	1285.960304	18.190823
39.290269	1279.416921	18.195840
39.571107	1284.261501	18.200858
39.242894	1292.161052	18.205875
39.609154	1301.877522	18.210893
39.510469	1306.897963	18.215911
40.015049	1294.997729	18.220928
39.767586	1298.943112	18.225946
40.002992	1304.015678	18.230963
40.130071	1295.727655	18.235981
39.841030	1300.528424	18.240999
40.268891	1286.872890	18.246016
40.425641	1279.100962	18.251034
40.358737	1267.800963	18.256051
40.279145	1264.348258	18.261069
39.823946	1263.071574	18.266087
40.395202	1264.465828	18.271104
39.979918	1258.174679	18.276122
40.419100	1257.150064	18.281139
40.220977	1255.189573	18.286157
40.042554	1258.076474	18.291175
40.396859	1253.868252	18.296192
40.167927	1263.718394	18.301210
40.257560	1261.703633	18.306227
40.456838	1255.237906	18.311245
40.248443	1253.938576	18.316263
40.403060	1249.789848	18.321280
40.497655	1265.001809	18.326298
40.472955	1282.163707	18.331315
41.163057	1276.953302	18.336333
40.717301	1273.885809	18.341351
40.758237	1261.742203	18.346368
40.814121	1261.815523	18.351386
40.393735	1259.741314	18.356403
40.716866	1261.448753	18.361421
40.531694	1282.536203	18.366439
41.547733	1263.550481	18.371456
41.963546	1264.593396	18.376474
41.548414	1249.443903	18.381491
41.788406	1232.949042	18.386509
41.397197	1238.144396	18.391527
41.818332	1236.024376	18.396544
41.396609	1219.307506	18.401562
41.414432	1219.613968	18.406579
41.196859	1209.306292	18.411597
41.185543	1222.786400	18.416615
41.427430	1213.404416	18.421632
41.428357	1215.651163	18.426650
41.278320	1211.145936	18.431667
41.031383	1215.318436	18.436685
41.124076	1225.569760	18.441703
41.476324	1224.410360	18.446720
41.509481	1231.672955	18.451738
41.423125	1232.768807	18.456755
41.406692	1226.983613	18.461773
41.191800	1234.187000	18.466791
41.447920	1235.030715	18.471808
41.419931	1228.414191	18.476826
41.806435	1230.143318	18.481843
41.740757	1239.264288	18.486861
41.590329	1257.345139	18.491879
41.921930	1260.285175	18.496896
41.911654	1265.913533	18.501914
41.412505	1258.256357	18.506931
41.752030	1265.442865	18.511949
41.533270	1262.854426	18.516967
41.850357	1264.468133	18.521984
42.068622	1258.722126	18.527002
42.238137	1273.947677	18.532019
42.462081	1285.276819	18.537037
42.576645	1283.425431	18.542055
42.452318	1268.113881	18.547072
42.595346	1264.273066	18.552090
42.319527	1262.930584	18.557107
42.244574	1262.383648	18.562125
41.884256	1271.635714	18.567143
42.533932	1279.736457	18.572160
42.858948	1279.389178	18.577178
42.301434	1281.145369	18.582195
42.407784	1281.614774	18.587213
42.465346	1292.439650	18.592231
42.612816	1287.626151	18.597248
42.602176	1279.659379	18.602266
42.678498	1282.465596	18.607283
42.874399	1277.840219	18.612301
42.559836	1279.593297	18.617319
42.679675	1281.086237	18.622336
42.807880	1292.998334	18.627354
42.708415	1294.017336	18.632371
42.790414	1303.639209	18.637389
42.812422	1310.969844	18.642407
42.902775	1306.234661	18.647424
43.458133	1303.958036	18.652442
42.949843	1300.893962	18.657459
43.151927	1305.495190	18.662477
43.220579	1306.967700	18.667495
43.398581	1302.868967	18.672512
43.111121	1310.910504	18.677530
43.309441	1316.411726	18.682547
43.547804	1306.601051	18.687565
43.220284	1318.445264	18.692583
43.055990	1323.425432	18.697600
43.602830	1329.421506	18.702618
43.512422	1328.144825	18.707635
43.775939	1327.668265	18.712653
43.394776	1333.499556	18.717671
43.696317	1329.870734	18.722688
43.577021	1329.933458	18.727706
43.385425	1334.365614	18.732723
43.619935	1329.907782	18.737741
43.614899	1351.778310	18.742759
44.039385	1345.744547	18.747776
44.546523	1351.626889	18.752794
44.320387	1352.880211	18.757811
44.142440	1341.127238	18.762829
44.333955	1334.375512	18.767847
44.206049	1334.556343	18.772864
44.205857	1334.767782	18.777882
44.291101	1356.071992	18.782899
44.372100	1351.877898	18.787917
44.404470	1351.307937	18.792935
44.252802	1360.963066	18.797952
44.671787	1339.640244	18.802970
44.430315	1345.058469	18.807987
44.765687	1348.591226	18.813005
44.468050	1356.246203	18.818023
44.373226	1351.400983	18.823040
44.480588	1346.855646	18.828058
44.213260	1347.976525	18.833075
44.212232	1353.707612	18.838093
44.424077	1354.608720	18.843111
44.556476	1377.158472	18.848128
44.978084	1365.984324	18.853146
44.885083	1379.511982	18.858163
44.821978	1380.490614	18.863181
44.962620	1374.586241	18.868199
45.016033	1377.250873	18.873216
45.133424	1368.894896	18.878234
44.963643	1370.735895	18.883251
45.202630	1366.949546	18.888269
45.045994	1358.106061	18.893287
44.947542	1373.771051	18.898304
45.379514	1379.494691	18.903322
45.631065	1401.672472	18.908339
45.618463	1394.636921	18.913357
45.611064	1377.836459	18.918375
45.542799	1375.025756	18.923392
45.456723	1361.020991	18.928410
45.050930	1385.964605	18.933427
45.759605	1388.533529	18.938445
46.160644	1387.931414	18.943463
45.769464	1389.418719	18.948480
46.021881	1388.915484	18.953498
45.982534	1398.385886	18.958515
45.851032	1380.960956	18.963533
45.984557	1376.250591	18.968551
45.853591	1382.762470	18.973568
45.949038	1374.684463	18.978586
45.696386	1385.144283	18.983603
46.082379	1382.354372	18.988621
45.951878	1381.311149	18.993639
45.626753	1388.143595	18.998656
45.861941	1387.466316	19.003674
45.949996	1389.683741	19.008691
46.222983	1378.611620	19.013709
45.939501	1386.169731	19.018727
46.154123	1399.049904	19.023744
46.427896	1405.003311	19.028762
46.277202	1407.362052	19.033779
46.438875	1405.358150	19.038797
46.729274	1403.286868	19.043815
46.749725	1404.751111	19.048832
47.093098	1394.643171	19.053850
46.986462	1404.654231	19.058867
46.987497	1401.769618	19.063885
47.137509	1404.277202	19.068903
46.494136	1408.416795	19.073920
46.717768	1399.643473	19.078938
46.628203	1398.388747	19.083955
46.683121	1401.037369	19.088973
46.618198	1402.445476	19.093991
46.574724	1407.343740	19.099008
47.109321	1413.474294	19.104026
47.217775	1420.428595	19.109043
47.385073	1431.760338	19.114061
47.218703	1430.624866	19.119079
47.463363	1431.744933	19.124096
47.858892	1421.007159	19.129114
47.520979	1429.252266	19.134131
47.460153	1422.038019	19.139149
47.625465	1420.453272	19.144167
47.583477	1420.242027	19.149184
47.556021	1417.260861	19.154202
47.481392	1418.626299	19.159219
47.714717	1426.384832	19.164237
47.839155	1420.183164	19.169255
47.203605	1423.422132	19.174272
47.501833	1421.087696	19.179290
47.322160	1422.614657	19.184307
47.756538	1439.995567	19.189325
48.039743	1442.056382	19.194343
48.341812	1448.930057	19.199360
48.441331	1451.521249	19.204378
48.322864	1448.854051	19.209395
48.004462	1441.376940	19.214413
48.650179	1440.976571	19.219431
48.318930	1438.456114	19.224448
48.381711	1435.214741	19.229466
48.377075	1438.967712	19.234483
48.373787	1444.086949	19.239501
48.346479	1440.383071	19.244519
48.369621	1445.444545	19.249536
48.072359	1445.711705	19.254554
48.258198	1441.340319	19.259571
48.401878	1445.398406	19.264589
48.732595	1440.297558	19.269607
48.433448	1444.973705	19.274624
48.419364	1447.528934	19.279642
48.516350	1454.118958	19.284659
48.941267	1468.623252	19.289677
49.011737	1470.313245	19.294695
49.060606	1466.676396	19.299712
49.127366	1460.395331	19.304730
48.916020	1459.847533	19.309747
48.877348	1469.251596	19.314765
49.280625	1461.195052	19.319783
49.284363	1462.308448	19.324800
48.981076	1461.797056	19.329818
49.126110	1464.857694	19.334835
49.183454	1463.510662	19.339853
49.695021	1458.637274	19.344871
48.887633	1456.443413	19.349888
49.369878	1465.747435	19.354906
49.353736	1459.163694	19.359923
49.181042	1471.741302	19.364941
49.573295	1478.679843	19.369959
49.497178	1480.026583	19.374976
49.273982	1480.304302	19.379994
49.733069	1477.566114	19.385011
49.493958	1481.882625	19.390029
50.049083	1468.352307	19.395047
49.610550	1481.368946	19.400064
49.772489	1477.556700	19.405082
49.877868	1485.960034	19.410099
50.032687	1508.572735	19.415117
50.066773	1501.368925	19.420135
49.984723	1509.021960	19.425152
50.419240	1502.409064	19.430170
50.364707	1499.924411	19.435187
50.270143	1499.042845	19.440205
50.699202	1496.934185	19.445223
50.375885	1502.914317	19.450240
50.587054	1504.323627	19.455258
50.692119	1496.682730	19.460275
50.734622	1496.587719	19.465293
50.786003	1495.197432	19.470311
50.515585	1503.763427	19.475328
50.612639	1495.255922	19.480346
50.528183	1501.949953	19.485363
50.443686	1498.463252	19.490381
50.882243	1497.883695	19.495399
50.826642	1492.401162	19.500416
50.865149	1496.235792	19.505434
50.735854	1500.468938	19.510451
51.125971	1510.617314	19.515469
51.484123	1520.988426	19.520487
51.232573	1515.975056	19.525504
51.377101	1521.118638	19.530522
51.596551	1520.080883	19.535539
51.039490	1526.009051	19.540557
51.365109	1516.790598	19.545575
51.328098	1526.932900	19.550592
51.317272	1522.330179	19.555610
51.232861	1525.940953	19.560627
51.313094	1532.476809	19.565645
51.795799	1517.998352	19.570663
51.212578	1524.511267	19.575680
51.437326	1524.634037	19.580698
51.595954	1535.784157	19.585715
51.670595	1544.312228	19.590733
52.105215	1537.500485	19.595751
52.425867	1538.861194	19.600768
52.639040	1533.917478	19.605786
51.983600	1522.175610	19.610803
51.920807	1521.030318	19.615821
52.330965	1526.801584	19.620839
52.095717	1530.442155	19.625856
52.383338	1534.370554	19.630874
52.355668	1535.236378	19.635891
52.483968	1535.642411	19.640909
52.262710	1516.858529	19.645927
52.196357	1550.623756	19.650944
52.109012	1546.206514	19.655962
52.762320	1545.404169	19.660979
52.380543	1536.393675	19.665997
52.619761	1530.025774	19.671015
52.819574	1527.002893	19.676032
52.557425	1535.274122	19.681050
52.875527	1532.116058	19.686067
52.549661	1539.336845	19.691085
53.223596	1539.399147	19.696103
52.820028	1532.067803	19.701120
52.723233	1535.005156	19.706138
53.285905	1536.328184	19.711155
52.931861	1543.038958	19.716173
52.928208	1535.206685	19.721191
52.944492	1542.014436	19.726208
53.272038	1547.120064	19.731226
53.238882	1542.924763	19.736243
53.458110	1551.739598	19.741261
53.658792	1550.401802	19.746279
53.386092	1551.125893	19.751296
53.411105	1546.460780	19.756314
53.390317	1548.527911	19.761331
53.543635	1547.639308	19.766349
53.545104	1548.588959	19.771367
53.480267	1553.241278	19.776384
53.688852	1548.497090	19.781402
53.581709	1546.475063	19.786419
53.357077	1560.733419	19.791437
53.598425	1565.713616	19.796455
53.479647	1569.859933	19.801472
53.542082	1571.589056	19.806490
53.441889	1574.479607	19.811507
53.890499	1587.370824	19.816525
54.181335	1590.648628	19.821543
54.159711	1591.178993	19.826560
54.405733	1590.449526	19.831578
54.594289	1598.827341	19.836595
54.118017	1603.070351	19.841613
54.495676	1591.328539	19.846631
54.456079	1598.732002	19.851648
54.245665	1594.813599	19.856666
54.559834	1591.189070	19.861683
54.900116	1610.591922	19.866701
54.627459	1617.425753	19.871719
55.046827	1619.967171	19.876736
54.661262	1610.827838	19.881754
54.795037	1607.982487	19.886771
54.824614	1618.988646	19.891789
54.797044	1613.668972	19.896807
55.057882	1607.250339	19.901824
55.110326	1611.003928	19.906842
55.130353	1603.486680	19.911859
54.782125	1607.536184	19.916877
55.125981	1615.088239	19.921895
55.616414	1625.580830	19.926912
55.827761	1637.764240	19.931930
55.699614	1624.302315	19.936947
55.484866	1618.573117	19.941965
55.413910	1610.448327	19.946983
55.710085	1619.513153	19.952000
55.616521	1627.956996	19.957018
55.617400	1636.928948	19.962035
55.920713	1641.766972	19.967053
56.130067	1642.330805	19.972071
56.089143	1647.042542	19.977088
55.734024	1631.520455	19.982106
56.011386	1628.614874	19.987123
55.760443	1636.912808	19.992141
55.593493	1635.853154	19.997159
55.858958	1632.368745	20.002176
56.140980	1635.963517	20.007194
56.045521	1630.881629	20.012211
55.839941	1639.311360	20.017229
55.996638	1648.984907	20.022247
56.277969	1660.589381	20.027264
56.168135	1671.857124	20.032282
56.448029	1666.025652	20.037299
56.169563	1673.570479	20.042317
56.457675	1666.055648	20.047335
57.018380	1656.156725	20.052352
56.568210	1668.471553	20.057370
56.625864	1659.026499	20.062387
56.913930	1672.984210	20.067405
56.992163	1680.744910	20.072423
57.286718	1687.496769	20.077440
57.016393	1687.308448	20.082458
57.138900	1689.684651	20.087475
57.113068	1691.790455	20.092493
57.023486	1690.987001	20.097511
56.945917	1678.984641	20.102528
56.812558	1680.005786	20.107546
57.513607	1682.736891	20.112563
57.575187	1687.461082	20.117581
57.711999	1684.103994	20.122599
57.755290	1684.144561	20.127616
57.380028	1683.675926	20.132634
57.536123	1681.944267	20.137651
57.500419	1690.966124	20.142669
57.496779	1700.639415	20.147687
57.699258	1699.777865	20.152704
57.880849	1709.693727	20.157722
58.049478	1702.134366	20.162739
57.987311	1697.167200	20.167757
57.981858	1696.142360	20.172775
58.288114	1696.811031	20.177792
58.392668	1699.392007	20.182810
58.362991	1692.513636	20.187827
58.416618	1697.324276	20.192845
58.297531	1696.522259	20.197863
58.202236	1693.248645	20.202880
58.301676	1699.002071	20.207898
58.722599	1696.313974	20.212915
58.412542	1702.254237	20.217933
58.204139	1709.270607	20.222951
58.525352	1709.744442	20.227968
58.562889	1730.059270	20.232986
59.049166	1719.376618	20.238003
58.989477	1719.073450	20.243021
58.834044	1727.470167	20.248039
59.059200	1720.593135	20.253056
59.033788	1728.486760	20.258074
58.996657	1720.694333	20.263091
59.107560	1721.267185	20.268109
58.610697	1725.623885	20.273127
58.768359	1727.814736	20.278144
58.848066	1732.201593	20.283162
59.439856	1741.173117	20.288179
59.179836	1741.106270	20.293197
59.151317	1748.798411	20.298215
59.717883	1732.110230	20.303232
59.559017	1739.033691	20.308250
60.184327	1735.272325	20.313267
59.820045	1733.571185	20.318285
59.785615	1744.107694	20.323303
60.098661	1729.065331	20.328320
59.848231	1733.973815	20.333338
59.474082	1734.691617	20.338355
59.859992	1733.836221	20.343373
60.225622	1751.733081	20.348391
60.301685	1758.064537	20.353408
60.365323	1756.110573	20.358426
60.487238	1749.413710	20.363443
60.333834	1749.472279	20.368461
60.496053	1753.454965	20.373479
60.743288	1744.971297	20.378496
60.218802	1745.983911	20.383514
60.470901	1755.349166	20.388531
60.591687	1747.917158	20.393549
60.409990	1752.183769	20.398567
60.974027	1758.306703	20.403584
60.923335	1765.450024	20.408602
60.832567	1757.820570	20.413619
60.428757	1750.940464	20.418637
60.567950	1754.797344	20.423655
60.685117	1749.900074	20.428672
60.741029	1766.390308	20.433690
60.812748	1778.418824	20.438707
61.066151	1769.356656	20.443725
60.896789	1782.517803	20.448743
61.402455	1779.889085	20.453760
61.135176	1776.377137	20.458778
61.453977	1776.551540	20.463795
61.491532	1791.914847	20.468813
61.772546	1799.467297	20.473831
61.854285	1793.379448	20.478848
61.688349	1796.908293	20.483866
61.854925	1799.022023	20.488883
61.880017	1793.772994	20.493901
61.583090	1794.396721	20.498919
62.172015	1791.584621	20.503936
61.717011	1797.721056	20.508954
61.916132	1790.971130	20.513971
62.004536	1793.788171	20.518989
61.867086	1790.158174	20.524007
62.075997	1791.836111	20.529024
62.170835	1803.378193	20.534042
62.354518	1814.035423	20.539059
62.705559	1806.390811	20.544077
62.765487	1803.733656	20.549095
62.863310	1817.856804	20.554112
62.937343	1812.858932	20.559130
63.058738	1808.488023	20.564147
63.224396	1803.245508	20.569165
62.668867	1784.235670	20.574183
62.838774	1791.660244	20.579200
63.155668	1792.021141	20.584218
63.245660	1805.347058	20.589235
63.265630	1793.026469	20.594253
63.168334	1792.678660	20.599271
63.244608	1796.453825	20.604288
62.821348	1805.801175	20.609306
62.987774	1800.946716	20.614323
63.182618	1802.967681	20.619341
62.843646	1816.483472	20.624359
63.290715	1810.480753	20.629376
62.883423	1817.610185	20.634394
63.134385	1829.683415	20.639411
63.574821	1840.581560	20.644429
63.576004	1841.250397	20.649447
63.388029	1834.762701	20.654464
63.411752	1835.674188	20.659482
63.745377	1847.258018	20.664499
64.423581	1849.550881	20.669517
63.990639	1860.512432	20.674535
64.302196	1855.303993	20.679552
64.458468	1855.153396	20.684570
64.305035	1858.042814	20.689587
64.248316	1856.713512	20.694605
64.228151	1856.890196	20.699623
64.743425	1853.878108	20.704640
64.146391	1858.007432	20.709658
64.204428	1850.367394	20.714675
64.365235	1850.124569	20.719693
64.618061	1855.481769	20.724711
64.419473	1849.481728	20.729728
64.599227	1851.754364	20.734746
64.725292	1863.913336	20.739763
65.037781	1863.684767	20.744781
65.090536	1871.525258	20.749799
65.163715	1880.208356	20.754816
65.082394	1872.069281	20.759834
64.874857	1877.551813	20.764851
64.929939	1872.828283	20.769869
64.861571	1878.547932	20.774887
64.947269	1867.539383	20.779904
64.987683	1883.814381	20.784922
65.140633	1891.591943	20.789939
65.465999	1887.201881	20.794957
65.260806	1903.603501	20.799975
65.549276	1900.317438	20.804992
65.668299	1899.838113	20.810010
65.734575	1913.347690	20.815027
65.704649	1910.171159	20.820045
65.904116	1917.275592	20.825063
65.687588	1916.151054	20.830080
66.171231	1917.401207	20.835098
66.150144	1916.000078	20.840115
66.808998	1908.477919	20.845133
66.478747	1920.575426	20.850151
66.670846	1909.278878	20.855168
66.716477	1905.071225	20.860186
66.547453	1913.485925	20.865203
66.675888	1908.722562	20.870221
66.421914	1914.288077	20.875239
66.635762	1912.301242	20.880256
66.883993	1909.750457	20.885274
66.402619	1911.734701	20.890291
67.017351	1919.553991	20.895309
66.898474	1933.928727	20.900327
66.835645	1934.983088	20.905344
66.755718	1938.378645	20.910362
67.132814	1932.730775	20.915379
67.126007	1927.142677	20.920397
67.481947	1937.296618	20.925415
67.559412	1939.121271	20.930432
67.478129	1937.101486	20.935450
67.631429	1936.487431	20.940467
67.594262	1929.831048	20.945485
67.472068	1936.729941	20.950503
67.571264	1947.258388	20.955520
67.629285	1949.701473	20.960538
67.810996	1959.181939	20.965555
68.079328	1950.212033	20.970573
67.925749	1971.563630	20.975591
68.169524	1955.692386	20.980608
67.848477	1957.285586	20.985626
68.161637	1950.808190	20.990643
68.130661	1954.647425	20.995661
68.091665	1958.491066	21.000679
68.318553	1956.937713	21.005696
68.359367	1953.387230	21.010714
68.262899	1953.730435	21.015731
68.431345	1956.389866	21.020749
68.332825	1958.699529	21.025767
68.496900	1967.964987	21.030784
68.614657	1979.427872	21.035802
68.503505	1978.353198	21.040819
68.839681	1967.106768	21.045837
69.084879	1980.036251	21.050855
68.739812	1980.919954	21.055872
69.172133	1974.509207	21.060890
68.583006	1977.548533	21.065907
69.429719	1984.296591	21.070925
69.286232	2000.852801	21.075943
69.407812	2009.802992	21.080960
69.838047	1997.945427	21.085978
69.358830	2000.304899	21.090995
69.466573	1995.238610	21.096013
69.479224	1996.915564	21.101031
69.777193	1993.672187	21.106048
69.887821	1993.525540	21.111066
69.628820	2002.080528	21.116083
69.720702	1994.100630	21.121101
69.751995	1992.489362	21.126119
69.889825	1996.946133	21.131136
70.164348	2003.180502	21.136154
70.072305	2016.907318	21.141171
70.518236	2016.850483	21.146189
70.418567	2019.744180	21.151207
70.475222	2027.486298	21.156224
70.950854	2021.264459	21.161242
70.505829	2023.009516	21.166259
70.932205	2016.309334	21.171277
70.685848	2012.617350	21.176295
70.614336	2024.406390	21.181312
70.398541	2007.053934	21.186330
70.932352	2012.326406	21.191347
70.501592	2006.280406	21.196365
70.635913	2017.330466	21.201383
71.098380	2034.019591	21.206400
71.067488	2038.972876	21.211418
70.804772	2035.071987	21.216435
71.318331	2032.104319	21.221453
71.388372	2035.094678	21.226471
71.288167	2033.289275	21.231488
71.570197	2028.574553	21.236506
71.152869	2047.830737	21.241523
71.546133	2050.486740	21.246541
71.929012	2051.250798	21.251559
71.844179	2059.961740	21.256576
72.073245	2050.215226	21.261594
72.350842	2042.610352	21.266611
72.717451	2045.772298	21.271629
72.621934	2039.718275	21.276647
72.371865	2036.175193	21.281664
72.692523	2014.715391	21.286682
72.333990	2012.801882	21.291699
72.236538	2009.550637	21.296717
72.425861	2026.907156	21.301735
72.167998	2041.092170	21.306752
72.412069	2035.329274	21.311770
72.442827	2040.774754	21.316787
72.565527	2037.012682	21.321805
72.767562	2038.139424	21.326823
72.700691	2037.225116	21.331840
73.299415	2034.768074	21.336858
72.739051	2045.680147	21.341875
72.662357	2044.312913	21.346893
73.027461	2054.762153	21.351911
73.004627	2054.715182	21.356928
73.447154	2056.347304	21.361946
73.305345	2069.116191	21.366963
73.352496	2067.003808	21.371981
73.436220	2068.928490	21.376999
73.259441	2068.466812	21.382016
73.436613	2071.857081	21.387034
73.305440	2075.967573	21.392051
73.666819	2084.034674	21.397069
73.948942	2089.617766	21.402087
73.814413	2091.245057	21.407104
73.627564	2084.624545	21.412122
73.674575	2094.552107	21.417139
73.658757	2094.156890	21.422157
74.227760	2096.627742	21.427175
74.117487	2110.464769	21.432192
74.423994	2105.339099	21.437210
74.301959	2108.062716	21.442227
74.212355	2102.796737	21.447245
74.215780	2112.235612	21.452263
74.341576	2111.262899	21.457280
74.758915	2118.806884	21.462298
74.535230	2132.191350	21.467315
74.881360	2139.970502	21.472333
75.372207	2126.219313	21.477351
75.117148	2137.137558	21.482368
75.002105	2133.573433	21.487386
75.068677	2127.472053	21.492403
75.730808	2126.712496	21.497421
75.389754	2128.100532	21.502439
75.287091	2131.417611	21.507456
75.551157	2120.737759	21.512474
75.339056	2132.334154	21.517491
75.701585	2141.742381	21.522509
75.876713	2152.218100	21.527527
76.021616	2154.300531	21.532544
76.082121	2146.647359	21.537562
75.714669	2149.301889	21.542579
75.741877	2155.647404	21.547597
76.374225	2152.241480	21.552615
76.180804	2157.049681	21.557632
76.021329	2144.636862	21.562650
76.126550	2148.685319	21.567667
75.953136	2152.177526	21.572685
76.475226	2171.088757	21.577703
76.554768	2176.463564	21.582720
76.536276	2173.506124	21.587738
76.817717	2178.966268	21.592755
76.510632	2181.043331	21.597773
76.816368	2173.405617	21.602791
76.611831	2174.573577	21.607808
76.619416	2173.982202	21.612826
77.022347	2182.128089	21.617843
77.100590	2194.376786	21.622861
77.227925	2193.110326	21.627879
77.209355	2195.653737	21.632896
77.437357	2183.556123	21.637914
77.458309	2187.661892	21.642931
77.479019	2185.623043	21.647949
77.495616	2189.458077	21.652967
77.594536	2204.398754	21.657984
77.838992	2204.079783	21.663002
77.682418	2216.437642	21.668019
77.715576	2215.375201	21.673037
78.198314	2204.812739	21.678055
77.901377	2204.335050	21.683072
78.320639	2206.336900	21.688090
78.118057	2209.578027	21.693107
78.054953	2218.017406	21.698125
78.321728	2211.121083	21.703143
78.421912	2214.980981	21.708160
78.171109	2204.340213	21.713178
78.248821	2212.947024	21.718195
78.682077	2228.656218	21.723213
78.727671	2232.654014	21.728231
78.663630	2228.854700	21.733248
78.955571	2215.244869	21.738266
79.060657	2225.980858	21.743283
79.248627	2225.317212	21.748301
79.252010	2224.792765	21.753319
79.027569	2233.478188	21.758336
78.951015	2219.212477	21.763354
78.834080	2234.395080	21.768371
78.774881	2246.141321	21.773389
79.224816	2243.461251	21.778407
79.287530	2257.905810	21.783424
79.536423	2254.490137	21.788442
80.094742	2262.327830	21.793459
79.999340	2268.225391	21.798477
80.109043	2260.532950	21.803495
80.060894	2271.131868	21.808512
80.141144	2273.596785	21.813530
80.450473	2278.456139	21.818547
80.269001	2277.745864	21.823565
80.276506	2266.196949	21.828583
80.133886	2268.816491	21.833600
80.317265	2265.152227	21.838618
80.405151	2269.234969	21.843635
80.572350	2280.611450	21.848653
81.181918	2278.111660	21.853671
80.751728	2284.563151	21.858688
81.139875	2276.751608	21.863706
81.665828	2277.275638	21.868723
81.405810	2273.295376	21.873741
81.216357	2280.419479	21.878759
81.686681	2280.803839	21.883776
81.552352	2284.801256	21.888794
81.531329	2278.994343	21.893811
81.496783	2275.856339	21.898829
81.716484	2272.460988	21.903847
81.412730	2276.626799	21.908864
81.362249	2280.557508	21.913882
82.036614	2275.686959	21.918899
81.848823	2283.334696	21.923917
81.907695	2270.613224	21.928935
81.669573	2276.507760	21.933952
81.909469	2286.175012	21.938970
81.907240	2293.667623	21.943987
81.760468	2297.105215	21.949005
82.132564	2297.454374	21.954023
82.199918	2305.400086	21.959040
82.505695	2315.445281	21.964058
82.554463	2324.214451	21.969075
82.788215	2334.412891	21.974093
83.038755	2330.706596	21.979111
82.619181	2316.345883	21.984128
82.547219	2334.800636	21.989146
83.065664	2327.470587	21.994163
82.787715	2329.413735	21.999181
82.971492	2326.882395	22.004199
82.877832	2335.705305	22.009216
83.245834	2337.191258	22.014234
83.282947	2335.916742	22.019251
83.442195	2345.880621	22.024269
83.658489	2337.543510	22.029287
83.431406	2337.818690	22.034304
83.220941	2348.903700	22.039322
83.711706	2337.923321	22.044339
83.770972	2354.991121	22.049357
84.161326	2364.161590	22.054375
84.289269	2355.487912	22.059392
84.295054	2354.862095	22.064410
84.276354	2349.537664	22.069427
84.604128	2350.875238	22.074445
84.867796	2343.796300	22.079463
84.490206	2356.002463	22.084480
84.958123	2345.394887	22.089498
84.867118	2344.418045	22.094515
84.466576	2350.356829	22.099533
84.781519	2348.919129	22.104551
84.797205	2352.438741	22.109568
84.819404	2338.870813	22.114586
84.953298	2342.457232	22.119603
84.628702	2350.236756	22.124621
85.201316	2359.877494	22.129639
85.265014	2365.942831	22.134656
85.422387	2362.557167	22.139674
85.358534	2369.068423	22.144691
85.293470	2369.447774	22.149709
85.354351	2368.747103	22.154727
85.290336	2382.851710	22.159744
85.382170	2398.074535	22.164762
85.730966	2397.998108	22.169779
85.645467	2403.755307	22.174797
85.894968	2399.780901	22.179815
85.977626	2407.484420	22.184832
86.039689	2409.551375	22.189850
86.316770	2412.427506	22.194867
86.514737	2420.223537	22.199885
86.585245	2416.520007	22.204903
86.398199	2422.242527	22.209920
86.263976	2420.461317	22.214938
87.319820	2431.399719	22.219955
86.786083	2436.870087	22.224973
87.007668	2438.271540	22.229991
86.755046	2438.942043	22.235008
86.740689	2434.339636	22.240026
86.806724	2434.023192	22.245043
86.907418	2451.838920	22.250061
87.215946	2462.170967	22.255079
87.293769	2450.251200	22.260096
87.310070	2454.894275	22.265114
87.492410	2447.121013	22.270131
87.697430	2452.574204	22.275149
87.664535	2461.100519	22.280167
88.042159	2466.665705	22.285184
88.189904	2472.916821	22.290202
88.375321	2479.518705	22.295219
88.487678	2477.645446	22.300237
88.582698	2473.669827	22.305255
88.449922	2482.890245	22.310272
88.836437	2476.237127	22.315290
88.554963	2469.176739	22.320307
88.453730	2481.810205	22.325325
88.470989	2478.335874	22.330343
88.732383	2473.463292	22.335360
88.493475	2483.050552	22.340378
88.773865	2466.914363	22.345395
88.611247	2481.722410	22.350413
88.702228	2481.761867	22.355431
89.145175	2489.254682	22.360448
89.042339	2495.472232	22.365466
89.502651	2483.846366	22.370483
89.071917	2496.480647	22.375501
89.225248	2498.189397	22.380519
89.662592	2505.345398	22.385536
89.611481	2516.304708	22.390554
89.606213	2518.543116	22.395571
89.822564	2517.587844	22.400589
89.790378	2513.363759	22.405607
89.758726	2507.429031	22.410624
89.655833	2523.594370	22.415642
90.230211	2528.453554	22.420659
90.002018	2547.611394	22.425677
90.322653	2538.229081	22.430695
90.576541	2542.387034	22.435712
90.638148	2536.601889	22.440730
90.531364	2537.028768	22.445747
90.541448	2553.678351	22.450765
90.767532	2566.402938	22.455783
90.965857	2558.096927	22.460800
90.776007	2568.563437	22.465818
91.208771	2566.069043	22.470835
91.114908	2567.595364	22.475853
90.793651	2574.664359	22.480871
91.492874	2578.730892	22.485888
91.551275	2591.333270	22.490906
91.514131	2588.684800	22.495923
91.493213	2593.355798	22.500941
91.496660	2587.144161	22.505959
92.091328	2598.047162	22.510976
91.589128	2617.822136	22.515994
92.125832	2610.801578	22.521011
92.126368	2621.958054	22.526029
92.279189	2617.635708	22.531047
92.249932	2606.269035	22.536064
92.158551	2609.028983	22.541082
92.823815	2615.808691	22.546099
93.056224	2624.442111	22.551117
93.025989	2617.598187	22.556135
92.808812	2600.390548	22.561152
93.015939	2619.174553	22.566170
93.209463	2624.111996	22.571187
93.345826	2632.820339	22.576205
93.335814	2631.717254	22.581223
93.432498	2626.983892	22.586240
93.313977	2632.064601	22.591258
93.949955	2622.582651	22.596275
93.768598	2629.743504	22.601293
93.499308	2626.310602	22.606311
93.741843	2619.184350	22.611328
93.846331	2614.882154	22.616346
93.705261	2617.375264	22.621363
93.888330	2630.608403	22.626381
93.926324	2636.983970	22.631399
94.066943	2642.955368	22.636416
94.191928	2653.467591	22.641434
93.996826	2653.905067	22.646451
94.064483	2655.908059	22.651469
94.137084	2670.048430	22.656487
94.842856	2667.457865	22.661504
94.388077	2674.273111	22.666522
94.573257	2671.094515	22.671539
94.358415	2680.220506	22.676557
94.381698	2676.887221	22.681575
94.832422	2696.438173	22.686592
94.811921	2704.549231	22.691610
94.964540	2700.207960	22.696627
95.408860	2708.407609	22.701645
95.591520	2713.053255	22.706663
95.823868	2719.890937	22.711680
95.799963	2723.905974	22.716698
95.773904	2718.970775	22.721715
95.666278	2719.792295	22.726733
95.696771	2719.146839	22.731751
95.854470	2714.268244	22.736768
95.807708	2711.823241	22.741786
96.237028	2725.649322	22.746803
96.523535	2735.363212	22.751821
96.487352	2744.903268	22.756839
96.571065	2726.771277	22.761856
96.607513	2738.591318	22.766874
96.931827	2738.553419	22.771891
97.143331	2743.888915	22.776909
96.695620	2742.330064	22.781927
96.864046	2738.453420	22.786944
97.144089	2737.788045	22.791962
97.273038	2742.514651	22.796979
97.612205	2750.405617	22.801997
97.689024	2756.541633	22.807015
97.964873	2758.493286	22.812032
97.613620	2765.443939	22.817050
97.871822	2753.723124	22.822067
97.668412	2754.518530	22.827085
97.478149	2749.545767	22.832103
97.945230	2749.226843	22.837120
97.759053	2754.898835	22.842138
98.048449	2753.493486	22.847155
97.806375	2767.679771	22.852173
97.747622	2776.813070	22.857191
98.181541	2776.530869	22.862208
98.335433	2795.522180	22.867226
98.676319	2796.987145	22.872243
99.092469	2798.247873	22.877261
98.979129	2791.034937	22.882279
99.295494	2793.002378	22.887296
98.951794	2802.804955	22.892314
99.113349	2792.573047	22.897331
99.288157	2790.904645	22.902349
99.191328	2801.347340	22.907367
99.343297	2807.080321	22.912384
99.525643	2821.768662	22.917402
99.525827	2822.724893	22.922419
99.629050	2821.812467	22.927437
99.365610	2828.474895	22.932455
99.866891	2834.393360	22.937472
100.010536	2842.021293	22.942490
99.958632	2840.022080	22.947507
99.958092	2837.292128	22.952525
100.025006	2839.503557	22.957543
100.769207	2833.230158	22.962560
101.142668	2843.539691	22.967578
101.436280	2836.919842	22.972595
101.388665	2827.197047	22.977613
101.019973	2823.037905	22.982631
100.847807	2818.646178	22.987648
100.678944	2821.973690	22.992666
100.961097	2843.829734	22.997683
101.100593	2846.070892	23.002701
101.212385	2849.834438	23.007719
101.345187	2852.420652	23.012736
101.616805	2856.645351	23.017754
101.196062	2857.155835	23.022771
101.869387	2867.122024	23.027789
101.493611	2873.707275	23.032807
102.068554	2868.100901	23.037824
101.852951	2865.899933	23.042842
102.242018	2866.170717	23.047859
102.392118	2865.383546	23.052877
101.922383	2871.923460	23.057895
102.104773	2876.906891	23.062912
102.504555	2885.258736	23.067930
102.504284	2894.395613	23.072947
102.843153	2888.788114	23.077965
102.840095	2895.798225	23.082983
102.977713	2880.201492	23.088000
102.956104	2888.177094	23.093018
102.817025	2893.305263	23.098035
103.384366	2901.839329	23.103053
103.365114	2914.936906	23.108071
103.634992	2912.382611	23.113088
103.635970	2915.172411	23.118106
103.633868	2912.786705	23.123123
103.417319	2918.889550	23.128141
103.606719	2917.982638	23.133159
103.604713	2925.027314	23.138176
103.917666	2936.829685	23.143194
104.273178	2943.061243	23.148211
104.399359	2939.434152	23.153229
104.297454	2945.695898	23.158247
104.373464	2938.699598	23.163264
104.088831	2946.037616	23.168282
104.543087	2957.073162	23.173299
104.997989	2960.404579	23.178317
105.123007	2971.081101	23.183335
105.203308	2965.551709	23.188352
105.341093	2962.026958	23.193370
105.362050	2963.349226	23.198387
105.414219	2951.429965	23.203405
105.359038	2964.536328	23.208423
105.679564	2972.742748	23.213440
105.827257	2984.258426	23.218458
105.905589	2984.807986	23.223475
105.880953	2981.087592	23.228493
105.870751	2979.719403	23.233511
106.055125	2977.749665	23.238528
106.021168	2979.841104	23.243546
105.963055	2990.041173	23.248563
106.249927	3002.904943	23.253581
106.330074	3008.592360	23.258599
106.461570	3011.873144	23.263616
106.388692	3011.401576	23.268634
106.149349	3013.689114	23.273651
106.626824	3030.474673	23.278669
106.523951	3034.820842	23.283687
106.587398	3036.701444	23.288704
106.831451	3049.451981	23.293722
106.812590	3061.126196	23.298739
107.469861	3047.427297	23.303757
107.926587	3054.182830	23.308775
108.161893	3062.405716	23.313792
108.583252	3054.146811	23.318810
108.549283	3040.220989	23.323827
109.071260	3031.315207	23.328845
108.656307	3032.613821	23.333863
108.537899	3029.965313	23.338880
108.357106	3030.836112	23.343898
108.486540	3031.829041	23.348915
108.726959	3024.908106	23.353933
108.297025	3032.436055	23.358951
108.562119	3027.060927	23.363968
108.862662	3036.324628	23.368986
108.677241	3053.510092	23.374003
108.808165	3047.672961	23.379021
109.054707	3056.307546	23.384039
108.846451	3051.801448	23.389056
109.365973	3059.137400	23.394074
109.178068	3062.685693	23.399091
109.414036	3077.072377	23.404109
109.303202	3088.142330	23.409127
109.438906	3079.804798	23.414144
109.282667	3073.908217	23.419162
109.896434	3088.425456	23.424179
110.062655	3094.541357	23.429197
110.249739	3104.267771	23.434215
110.118916	3099.929504	23.439232
110.486335	3101.402989	23.444250
110.610087	3119.963791	23.449267
110.722149	3123.626356	23.454285
110.750370	3130.095147	23.459303
110.733267	3121.143850	23.464320
110.771958	3121.642776	23.469338
110.723512	3137.099529	23.474355
111.203703	3146.338474	23.479373
111.176435	3161.353248	23.484391
111.367806	3157.801180	23.489408
111.575767	3157.424753	23.494426
111.382350	3156.593213	23.499443
111.345757	3154.332777	23.504461
111.797026	3164.321081	23.509479
112.142259	3177.453629	23.514496
112.295422	3171.411004	23.519514
112.206775	3179.163618	23.524531
112.262025	3175.200349	23.529549
112.247320	3183.266534	23.534567
112.668813	3195.500348	23.539584
112.852156	3185.125954	23.544602
112.970530	3191.350334	23.549619
113.013018	3188.105492	23.554637
113.084564	3195.602774	23.559655
113.054994	3186.565013	23.564672
113.609839	3183.799039	23.569690
113.466448	3182.565191	23.574707
113.577441	3176.822650	23.579725
113.281204	3197.503565	23.584743
113.617160	3206.313669	23.589760
114.071317	3212.249066	23.594778
113.677404	3219.989259	23.599795
113.682038	3211.189183	23.604813
113.971302	3219.078658	23.609831
113.962663	3230.621989	23.614848
114.535967	3234.784028	23.619866
114.231062	3241.146917	23.624883
114.403005	3249.726930	23.629901
114.733813	3257.931880	23.634919
114.871425	3265.245318	23.639936
115.217431	3255.031771	23.644954
115.255243	3263.705266	23.649971
115.412835	3268.910442	23.654989
115.206580	3266.588035	23.660007
115.207629	3264.959268	23.665024
115.477978	3263.421131	23.670042
115.093813	3268.982083	23.675059
115.394577	3276.115472	23.680077
115.966703	3279.005775	23.685095
115.993969	3278.619605	23.690112
116.372523	3268.965935	23.695130
116.187166	3271.680648	23.700147
116.321935	3291.524466	23.705165
116.824848	3285.073860	23.710183
116.955514	3288.960806	23.715200
117.218816	3293.395210	23.720218
117.239955	3294.569134	23.725235
117.383787	3279.823250	23.730253
117.377770	3258.535916	23.735271
117.006673	3268.535536	23.740288
117.346378	3265.156033	23.745306
117.241685	3289.812388	23.750323
117.430810	3283.921934	23.755341
117.901571	3288.317725	23.760359
117.535306	3285.657270	23.765376
117.656113	3288.946081	23.770394
117.620897	3295.689925	23.775411
117.527274	3296.708129	23.780429
117.719659	3314.024389	23.785447
117.987668	3311.400894	23.790464
117.755080	3306.563967	23.795482
118.249583	3316.299445	23.800499
118.739639	3324.451227	23.805517
119.021330	3322.267463	23.810535
119.043870	3320.853120	23.815552
119.267968	3320.512052	23.820570
119.222265	3322.138248	23.825587
119.391668	3322.976631	23.830605
119.378426	3324.907077	23.835623
119.470612	3349.299305	23.840640
119.615181	3345.486212	23.845658
119.750454	3353.847897	23.850675
119.928201	3343.344880	23.855693
119.787052	3343.606694	23.860711
119.739415	3340.760908	23.865728
119.982677	3358.337564	23.870746
119.705896	3374.088876	23.875763
119.996761	3373.020962	23.880781
120.240864	3370.738890	23.885799
120.341351	3393.498146	23.890816
120.556016	3395.986477	23.895834
120.717868	3400.594511	23.900851
120.792039	3402.849067	23.905869
121.052701	3419.630873	23.910887
121.022358	3429.031510	23.915904
121.270303	3421.847289	23.920922
121.193927	3431.782176	23.925939
121.404848	3440.690767	23.930957
121.494895	3450.757564	23.935975
121.722462	3453.108178	23.940992
121.746187	3454.243836	23.946010
122.019044	3474.868027	23.951027
122.053378	3476.172470	23.956045
122.469442	3471.935182	23.961063
122.507609	3478.831792	23.966080
122.632633	3483.530798	23.971098
122.716045	3494.678069	23.976115
122.646803	3496.973901	23.981133
122.639271	3499.247502	23.986151
122.907547	3504.656447	23.991168
123.261573	3493.614595	23.996186
123.344000	3511.437374	24.001203
123.273489	3509.213737	24.006221
123.504817	3518.160219	24.011239
123.144856	3522.117289	24.016256
123.413304	3532.958030	24.021274
123.586802	3542.080806	24.026291
123.856206	3548.231296	24.031309
124.046831	3547.693439	24.036327
124.106547	3564.531916	24.041344
124.388389	3570.402731	24.046362
124.295017	3571.982715	24.051379
124.095213	3574.062169	24.056397
124.820333	3577.266416	24.061415
124.769441	3597.395128	24.066432
125.078928	3598.022343	24.071450
124.769166	3603.587594	24.076467
125.026943	3597.279198	24.081485
125.544044	3590.943056	24.086503
125.621999	3605.522042	24.091520
126.021957	3613.407081	24.096538
125.980719	3615.083107	24.101555
125.891953	3616.646597	24.106573
126.082279	3616.711622	24.111591
126.068974	3617.483779	24.116608
126.539108	3601.790465	24.121626
126.633534	3613.583117	24.126643
126.446125	3609.045227	24.131661
126.661863	3608.973734	24.136679
126.278297	3630.615604	24.141696
126.826201	3631.543415	24.146714
126.744182	3629.021715	24.151731
127.107154	3636.031938	24.156749
127.230386	3641.113167	24.161767
127.084384	3662.191000	24.166784
127.220121	3664.931530	24.171802
127.174251	3663.893932	24.176819
127.792432	3679.111644	24.181837
127.894335	3671.460847	24.186855
127.745221	3675.022157	24.191872
127.413231	3679.909148	24.196890
127.850860	3701.429563	24.201907
128.395126	3703.440530	24.206925
128.748830	3700.336516	24.211943
128.777526	3709.283080	24.216960
129.379389	3710.095182	24.221978
129.405933	3706.666512	24.226995
129.501577	3713.030329	24.232013
129.935383	3703.711854	24.237031
129.610458	3699.593036	24.242048
129.858629	3701.176668	24.247066
129.898982	3700.283456	24.252083
130.040494	3701.100950	24.257101
130.256983	3706.379145	24.262119
130.158746	3705.280261	24.267136
130.085069	3707.886121	24.272154
130.411436	3710.697978	24.277171
130.055460	3714.572407	24.282189
130.201259	3714.944206	24.287207
130.232473	3728.479545	24.292224
130.368304	3731.892347	24.297242
130.759040	3728.302816	24.302259
130.231315	3746.315509	24.307277
130.711273	3758.685792	24.312295
130.522182	3771.406435	24.317312
131.099981	3777.799363	24.322330
131.268695	3783.457455	24.327347
131.385963	3790.635399	24.332365
131.451741	3801.984449	24.337383
131.699525	3819.958537	24.342400
131.873756	3812.659388	24.347418
132.349134	3824.787398	24.352435
132.515125	3845.305558	24.357453
132.764574	3837.281375	24.362471
132.724409	3840.017755	24.367488
133.000854	3833.608528	24.372506
132.867192	3826.575090	24.377523
132.674055	3838.829285	24.382541
132.985184	3845.393162	24.387559
132.882688	3845.535340	24.392576
133.319083	3852.654155	24.397594
133.695126	3867.553069	24.402611
133.632044	3855.168247	24.407629
133.567399	3857.886348	24.412647
133.661063	3862.441992	24.417664
133.868902	3869.201865	24.422682
134.123350	3868.294249	24.427699
134.392307	3863.606337	24.432717
134.402759	3861.347957	24.437735
134.585625	3869.506783	24.442752
134.558417	3883.540554	24.447770
134.705701	3888.008950	24.452787
134.864155	3892.807015	24.457805
134.961792	3887.277798	24.462823
135.170017	3902.894090	24.467840
135.320995	3913.021096	24.472858
135.360635	3916.764537	24.477875
135.257878	3923.200348	24.482893
135.664499	3908.605569	24.487911
135.496970	3933.799682	24.492928
135.408566	3941.688305	24.497946
135.706284	3934.445631	24.502963
135.876362	3969.466352	24.507981
136.163081	3966.473723	24.512999
136.029627	3971.424569	24.518016
136.631131	3984.978625	24.523034
136.556681	3978.646072	24.528051
136.418982	4003.636792	24.533069
137.222782	4016.398712	24.538087
137.212765	4023.000028	24.543104
137.298176	4019.682072	24.548122
137.736011	4021.375081	24.553139
137.413908	4021.425199	24.558157
138.303773	4040.653588	24.563175
137.952219	4036.510431	24.568192
138.246018	4038.184835	24.573210
138.391519	4037.881242	24.578227
138.181901	4039.883370	24.583245
138.389955	4036.385346	24.588263
138.330525	4049.843506	24.593280
138.662952	4057.676129	24.598298
139.038406	4065.861873	24.603315
138.831020	4067.888907	24.608333
139.469338	4073.922171	24.613351
139.567761	4076.665417	24.618368
140.094797	4072.565372	24.623386
140.098267	4061.388376	24.628403
140.107868	4070.458030	24.633421
140.081630	4068.221118	24.638439
140.064236	4062.627693	24.643456
139.954223	4070.952148	24.648474
140.145465	4071.566227	24.653491
140.235054	4087.059116	24.658509
140.716554	4092.974769	24.663527
140.884776	4094.930701	24.668544
140.704115	4088.204327	24.673562
141.139729	4097.135074	24.678579
141.130693	4110.970502	24.683597
141.919332	4107.041192	24.688615
142.075730	4107.622822	24.693632
141.968608	4109.094523	24.698650
141.990044	4110.107483	24.703667
141.886132	4127.830474	24.708685
142.094512	4103.797500	24.713703
142.195777	4111.126410	24.718720
141.929231	4121.103909	24.723738
142.096986	4125.919526	24.728755
141.970623	4142.989516	24.733773
142.395311	4135.704900	24.738791
142.759526	4149.914660	24.743808
142.521444	4154.080144	24.748826
142.888701	4165.628677	24.753843
142.787836	4175.119590	24.758861
143.219136	4183.703857	24.763879
143.336164	4191.162910	24.768896
143.299407	4193.920907	24.773914
143.537979	4204.043908	24.778931
143.707261	4210.727849	24.783949
143.799218	4216.783098	24.788967
143.982352	4213.301545	24.793984
143.919075	4231.457039	24.799002
144.299291	4227.357724	24.804019
144.099689	4223.430746	24.809037
144.673643	4250.002796	24.814055
144.837467	4259.477794	24.819072
144.870315	4266.113558	24.824090
145.040243	4264.022835	24.829107
145.296357	4273.928513	24.834125
145.240947	4279.129268	24.839143
145.513248	4285.964483	24.844160
146.170931	4297.587825	24.849178
146.276923	4286.483105	24.854195
146.204116	4307.228348	24.859213
146.516144	4300.488314	24.864231
146.397934	4304.240629	24.869248
146.391077	4301.953325	24.874266
146.905310	4305.531423	24.879283
147.179087	4318.401329	24.884301
147.057131	4325.367380	24.889319
146.907277	4319.898657	24.894336
147.238452	4328.766871	24.899354
147.351782	4324.803776	24.904371
147.558710	4342.399674	24.909389
147.409306	4346.510363	24.914407
147.816622	4339.774418	24.919424
148.060189	4356.600790	24.924442
148.483994	4363.516607	24.929459
148.333641	4368.454411	24.934477
148.361802	4372.490116	24.939495
148.709116	4363.415183	24.944512
148.528491	4377.350126	24.949530
148.930979	4386.690186	24.954547
149.182486	4397.265795	24.959565
149.074681	4392.396523	24.964583
149.326123	4395.829328	24.969600
149.827014	4411.135362	24.974618
150.335123	4411.365547	24.979635
150.219758	4412.844868	24.984653
150.332996	4405.861142	24.989671
150.655241	4407.363866	24.994688
150.348793	4414.131418	24.999706
150.833037	4403.062427	25.004723
150.465508	4421.196040	25.009741
150.599108	4415.411711	25.014759
150.928798	4429.188333	25.019776
150.789917	4440.695901	25.024794
150.674593	4432.040161	25.029811
150.949260	4458.327696	25.034829
151.512319	4465.449129	25.039847
151.380958	4463.840869	25.044864
151.256277	4473.471369	25.049882
151.808469	4487.784696	25.054899
152.128479	4490.979586	25.059917
151.954234	4487.013883	25.064935
152.489349	4496.342821	25.069952
152.359130	4513.839870	25.074970
152.451905	4506.502622	25.079987
152.727713	4507.842140	25.085005
152.608171	4523.661505	25.090023
153.079105	4530.453262	25.095040
153.082751	4537.103141	25.100058
153.114361	4531.675542	25.105075
152.943456	4536.856476	25.110093
153.357083	4558.375338	25.115111
153.963615	4552.359515	25.120128
153.891016	4560.062876	25.125146
154.189032	4580.517127	25.130163
154.467674	4586.246736	25.135181
154.337256	4592.586087	25.140199
154.451627	4589.544436	25.145216
154.520045	4596.701899	25.150234
154.789928	4607.543063	25.155251
155.133377	4621.409225	25.160269
154.783359	4617.982194	25.165287
154.910629	4628.713006	25.170304
155.084281	4638.656975	25.175322
155.335821	4644.261409	25.180339
155.595134	4654.428779	25.185357
156.032669	4663.009149	25.190375
156.227535	4657.691820	25.195392
156.521522	4665.035138	25.200410
156.791529	4671.785634	25.205427
156.753705	4678.385206	25.210445
156.794432	4684.669536	25.215463
156.835881	4679.669631	25.220480
157.210080	4694.503232	25.225498
157.342342	4694.612022	25.230515
157.644273	4699.760420	25.235533
157.872546	4701.855421	25.240551
157.794927	4694.784512	25.245568
157.848801	4700.871104	25.250586
157.944932	4709.072221	25.255603
158.247341	4718.188149	25.260621
158.237261	4734.751349	25.265639
158.410276	4738.701455	25.270656
158.318739	4756.899752	25.275674
158.597113	4752.696232	25.280691
158.558046	4760.069348	25.285709
158.981591	4777.177419	25.290727
159.088325	4784.067008	25.295744
159.620222	4797.307403	25.300762
159.592613	4801.014150	25.305779
160.165451	4794.192295	25.310797
160.549015	4798.864018	25.315815
160.391930	4788.797378	25.320832
160.145240	4799.441318	25.325850
160.631519	4807.878441	25.330867
160.997834	4814.538243	25.335885
160.846126	4814.893256	25.340903
161.347802	4811.365152	25.345920
161.096274	4826.974912	25.350938
161.232014	4829.119055	25.355955
161.462660	4841.876105	25.360973
161.659475	4844.436858	25.365991
161.506066	4845.199316	25.371008
161.914839	4834.324887	25.376026
161.947415	4855.202702	25.381043
161.930276	4866.846251	25.386061
162.110096	4863.396654	25.391079
162.395697	4870.419406	25.396096
162.711781	4880.432869	25.401114
162.781724	4895.241407	25.406131
162.891358	4894.839222	25.411149
162.881181	4909.884352	25.416167
163.163412	4912.526510	25.421184
163.478974	4916.315580	25.426202
163.581360	4919.926357	25.431219
163.612391	4924.858168	25.436237
163.779644	4940.128214	25.441255
163.876155	4947.578147	25.446272
163.978245	4946.006096	25.451290
163.950613	4958.743467	25.456307
164.741902	4964.677463	25.461325
165.002265	4968.064799	25.466343
164.908463	4964.263227	25.471360
165.048282	4973.868595	25.476378
165.321786	4967.872922	25.481395
165.966575	4967.346384	25.486413
165.869637	4968.317850	25.491431
166.206564	4964.465001	25.496448
166.322625	4971.107006	25.501466
166.405350	4978.963124	25.506483
166.430043	4988.870504	25.511501
166.540243	4990.333693	25.516519
166.572244	4990.117198	25.521536
166.504821	4992.592854	25.526554
166.590732	4999.425794	25.531571
166.882757	5008.587675	25.536589
166.681860	5021.535140	25.541607
167.421934	5035.159951	25.546624
167.183702	5045.767997	25.551642
167.323298	5053.040817	25.556659
167.780714	5058.919505	25.561677
167.682087	5060.699293	25.566695
168.104405	5077.949881	25.571712
168.212895	5092.462183	25.576730
168.265478	5085.307721	25.581747
168.983300	5108.367581	25.586765
169.071158	5120.080170	25.591783
169.322082	5128.023799	25.596800
169.229553	5125.093183	25.601818
169.589281	5130.627265	25.606835
169.717812	5142.494516	25.611853
169.732324	5142.602704	25.616871
169.795323	5147.131881	25.621888
169.986579	5156.549418	25.626906
170.224959	5163.273457	25.631923
170.377434	5165.970576	25.636941
170.649925	5181.697913	25.641959
170.891216	5192.013590	25.646976
170.726229	5194.097276	25.651994
171.036859	5194.298247	25.657011
171.245156	5215.199621	25.662029
171.471723	5215.391584	25.667047
171.487535	5217.178823	25.672064
171.938463	5234.343037	25.677082
171.791577	5237.658099	25.682100
172.372012	5238.603031	25.687117
172.080145	5251.650048	25.692135
172.435118	5259.217695	25.697152
172.856604	5273.662472	25.702170
172.802416	5269.987242	25.707188
173.025625	5283.102446	25.712205
173.019467	5294.602516	25.717223
173.286180	5301.356917	25.722240
173.552649	5303.464981	25.727258
173.280518	5321.530977	25.732276
173.661697	5318.191988	25.737293
173.263731	5331.227172	25.742311
173.914173	5350.680470	25.747328
174.118795	5361.185030	25.752346
174.498387	5367.224291	25.757364
175.225201	5358.657953	25.762381
175.047289	5364.765072	25.767399
174.813231	5373.210444	25.772416
175.537287	5383.851947	25.777434
175.498163	5392.188066	25.782452
175.248566	5387.643627	25.787469
175.776715	5390.714734	25.792487
175.851423	5406.485685	25.797504
176.071533	5405.482333	25.802522
176.077867	5411.680730	25.807540
176.420971	5419.897379	25.812557
176.507917	5434.081873	25.817575
176.822804	5440.762539	25.822592
176.894570	5446.587760	25.827610
177.175482	5452.550874	25.832628
177.395156	5466.114987	25.837645
177.376882	5475.533746	25.842663
177.546565	5477.199201	25.847680
177.998258	5485.162233	25.852698
177.875160	5487.312031	25.857716
178.356330	5488.733287	25.862733
178.418722	5506.889429	25.867751
178.491784	5521.890540	25.872768
178.879425	5517.199510	25.877786
178.495689	5521.006040	25.882804
179.312371	5529.328931	25.887821
179.026559	5548.214826	25.892839
179.242945	5549.320621	25.897856
179.604783	5570.782461	25.902874
179.663949	5575.710068	25.907892
180.170404	5580.265009	25.912909
180.406520	5590.474395	25.917927
180.642568	5587.555680	25.922944
181.390508	5578.925976	25.927962
182.370397	5555.010867	25.932980
182.522845	5543.020627	25.937997
182.562098	5546.275199	25.943015
182.406457	5523.442850	25.948032
182.443318	5515.864533	25.953050
182.402791	5525.722385	25.958068
182.972518	5513.919722	25.963085
183.172311	5511.637971	25.968103
182.554143	5515.790340	25.973120
182.477750	5513.520023	25.978138
182.371071	5515.345301	25.983156
182.925005	5525.502013	25.988173
182.875744	5530.149774	25.993191
183.249833	5534.397031	25.998208
183.351551	5543.645629	26.003226
182.962774	5559.656170	26.008244
183.499388	5556.535994	26.013261
183.814980	5579.586477	26.018279
183.862705	5575.737490	26.023296
184.255911	5583.899066	26.028314
184.093091	5605.799322	26.033332
184.529707	5604.156193	26.038349
184.890714	5616.603089	26.043367
185.079619	5631.393706	26.048384
185.223530	5637.125685	26.053402
185.352911	5651.805636	26.058420
185.455720	5638.980257	26.063437
185.518022	5653.257143	26.068455
185.687151	5668.666399	26.073472
185.696901	5671.455258	26.078490
186.042324	5682.130634	26.083508
186.160677	5689.132394	26.088525
186.779184	5699.380162	26.093543
186.804914	5717.273913	26.098560
187.296179	5707.535116	26.103578
187.022197	5713.862486	26.108596
187.373147	5718.621598	26.113613
187.590359	5723.442568	26.118631
187.265970	5729.392688	26.123648
187.751667	5736.782354	26.128666
187.832114	5749.856989	26.133684
188.015515	5752.984989	26.138701
188.337004	5759.977247	26.143719
188.603220	5773.332322	26.148736
188.792074	5786.948822	26.153754
188.748971	5788.050840	26.158772
189.074078	5807.918288	26.163789
189.102955	5812.033117	26.168807
188.987290	5817.916047	26.173824
189.460428	5830.749677	26.178842
189.509097	5845.126690	26.183860
189.930443	5849.230930	26.188877
190.452608	5859.430656	26.193895
190.258083	5870.281747	26.198912
190.460892	5876.531785	26.203930
190.577479	5893.275186	26.208948
191.107805	5902.776055	26.213965
190.861604	5917.710403	26.218983
191.151673	5931.715300	26.224000
191.581841	5934.441902	26.229018
191.535040	5942.081856	26.234036
191.864284	5954.328749	26.239053
192.445299	5965.147539	26.244071
192.241591	5974.892148	26.249088
192.797456	5988.947250	26.254106
192.646011	5997.926144	26.259124
192.994958	6001.577667	26.264141
193.235826	6020.713498	26.269159
192.937543	6025.993601	26.274176
193.353570	6025.133329	26.279194
193.474321	6049.811997	26.284212
193.818584	6058.555914	26.289229
194.177324	6069.582987	26.294247
194.422148	6077.174438	26.299264
194.564436	6083.598115	26.304282
194.745219	6101.174535	26.309300
194.827594	6105.050666	26.314317
195.296110	6116.246919	26.319335
195.536569	6128.719247	26.324352
195.652283	6120.045672	26.329370
195.450298	6133.612798	26.334388
195.908255	6142.825179	26.339405
196.091203	6144.308702	26.344423
196.213528	6164.558498	26.349440
196.917066	6166.980573	26.354458
196.930213	6173.673763	26.359476
196.965187	6178.860989	26.364493
197.322377	6190.645975	26.369511
197.317639	6193.958018	26.374528
197.433243	6191.711388	26.379546
197.673286	6217.214538	26.384564
197.920186	6222.375095	26.389581
198.125476	6231.165985	26.394599
198.395146	6241.705120	26.399616
198.612093	6252.429243	26.404634
198.627585	6250.583305	26.409652
198.879438	6273.010098	26.414669
199.235737	6283.374780	26.419687
199.117623	6286.657141	26.424704
199.676729	6282.074959	26.429722
199.444086	6300.467225	26.434740
199.526240	6303.077604	26.439757
200.325150	6317.388692	26.444775
200.256973	6327.339669	26.449792
200.684376	6318.308119	26.454810
200.590326	6326.091327	26.459828
200.970700	6334.097403	26.464845
200.913183	6346.692033	26.469863
200.847271	6357.889565	26.474880
201.219132	6367.304865	26.479898
201.690932	6380.309553	26.484916
201.746147	6371.758919	26.489933
201.599254	6382.104140	26.494951
201.705223	6410.684113	26.499968
202.278979	6408.697581	26.504986
202.596062	6428.188151	26.510004
202.637964	6431.287790	26.515021
202.984373	6444.545642	26.520039
202.968741	6457.664153	26.525056
203.365525	6467.520720	26.530074
203.587682	6483.241236	26.535092
203.533788	6489.657719	26.540109
204.202432	6500.516850	26.545127
203.936931	6510.801692	26.550144
204.342457	6510.025109	26.555162
204.769694	6517.818784	26.560180
204.706636	6525.016415	26.565197
205.179220	6527.913281	26.570215
205.199277	6552.668282	26.575232
205.456574	6555.238803	26.580250
205.581788	6567.584165	26.585268
206.070954	6579.683468	26.590285
206.298001	6584.348456	26.595303
206.254847	6597.951175	26.600320
206.407859	6608.193011	26.605338
206.606832	6611.665976	26.610356
206.761062	6630.168805	26.615373
207.044959	6633.031929	26.620391
207.011355	6645.935558	26.625408
207.667188	6644.785385	26.630426
207.859747	6663.228615	26.635444
208.081748	6682.481721	26.640461
208.312124	6678.995503	26.645479
208.881851	6694.305376	26.650496
208.692929	6699.262440	26.655514
208.889359	6704.831899	26.660532
209.064992	6714.337907	26.665549
209.603220	6723.115081	26.670567
210.051058	6730.166960	26.675584
210.080436	6729.006985	26.680602
210.315594	6729.440699	26.685620
210.009959	6736.530969	26.690637
210.594635	6738.428667	26.695655
210.756997	6761.643397	26.700672
210.875072	6756.823556	26.705690
210.976003	6768.961331	26.710708
210.934311	6778.996819	26.715725
211.239768	6786.894803	26.720743
211.307758	6797.730826	26.725760
211.809735	6806.491586	26.730778
211.811883	6832.616634	26.735796
211.663745	6837.734695	26.740813
212.279788	6847.942458	26.745831
212.682136	6858.050913	26.750848
212.456339	6868.711743	26.755866
213.055044	6891.135802	26.760884
212.761564	6895.304219	26.765901
213.205126	6908.357875	26.770919
213.620567	6914.963450	26.775936
214.091497	6921.213143	26.780954
214.144898	6937.907358	26.785972
214.363006	6943.565062	26.790989
214.599773	6930.948369	26.796007
214.572084	6940.792358	26.801024
214.658435	6956.846946	26.806042
215.005642	6957.642037	26.811060
214.859300	6980.557859	26.816077
215.208973	6982.198589	26.821095
215.511407	7002.361292	26.826112
216.091491	7010.907956	26.831130
216.067529	7016.079340	26.836148
216.068495	7030.022759	26.841165
216.656977	7031.405337	26.846183
216.230946	7059.740840	26.851200
216.488664	7067.491694	26.856218
216.781354	7086.604789	26.861236
216.683769	7109.358497	26.866253
217.457245	7119.478766	26.871271
217.568532	7134.235331	26.876288
217.795395	7147.638578	26.881306
217.986030	7162.891062	26.886324
217.942004	7177.378257	26.891341
218.344409	7183.117832	26.896359
218.568514	7201.184186	26.901376
218.803393	7226.588528	26.906394
219.297872	7237.759331	26.911412
219.583815	7248.552218	26.916429
220.117923	7255.571929	26.921447
220.369090	7266.379711	26.926464
220.307954	7269.296653	26.931482
220.915847	7271.683263	26.936500
221.114468	7270.755765	26.941517
222.256213	7274.874448	26.946535
222.377808	7286.138059	26.951552
222.489188	7283.595210	26.956570
222.757338	7281.839264	26.961588
222.583814	7291.279971	26.966605
222.755553	7288.058472	26.971623
222.691067	7286.546881	26.976640
222.638270	7297.177868	26.981658
222.886630	7296.485703	26.986676
222.833004	7316.050719	26.991693
223.147659	7311.152774	26.996711
223.541040	7326.831574	27.001728
223.100168	7341.169173	27.006746
223.783988	7348.134043	27.011764
223.803259	7364.837118	27.016781
223.960311	7377.512696	27.021799
224.619339	7392.986037	27.026816
224.529211	7407.237513	27.031834
224.838018	7414.042969	27.036852
225.107010	7440.136807	27.041869
225.628872	7439.585156	27.046887
225.711295	7455.375615	27.051904
225.864930	7463.973099	27.056922
226.472479	7468.796900	27.061940
226.340243	7474.610332	27.066957
227.055505	7483.338213	27.071975
227.123696	7494.427167	27.076992
227.076227	7495.896164	27.082010
227.377066	7515.223107	27.087028
227.266893	7523.129293	27.092045
227.714846	7540.734952	27.097063
227.778667	7547.726973	27.102080
228.465033	7557.122336	27.107098
228.529595	7552.575797	27.112116
228.728673	7572.575276	27.117133
228.743050	7577.456729	27.122151
229.317017	7590.831516	27.127168
229.329007	7603.267811	27.132186
229.517139	7604.933748	27.137204
229.622962	7628.278340	27.142221
229.820632	7627.344659	27.147239
230.043088	7637.396316	27.152256
230.223165	7656.243416	27.157274
230.331485	7658.117512	27.162292
230.842106	7676.224964	27.167309
231.117085	7675.598094	27.172327
231.726768	7698.226633	27.177344
232.053313	7702.746984	27.182362
232.172899	7695.786270	27.187380
232.308677	7705.873558	27.192397
232.627684	7718.410508	27.197415
232.313236	7722.942263	27.202432
232.562116	7728.083998	27.207450
233.072351	7739.486267	27.212468
233.171754	7765.831113	27.217485
233.271444	7772.344096	27.222503
233.477855	7783.894716	27.227520
233.650219	7795.491685	27.232538
234.358722	7815.866717	27.237556
234.091103	7819.175784	27.242573
234.052593	7841.242457	27.247591
234.455623	7853.075047	27.252608
234.467607	7874.941326	27.257626
234.791437	7887.468170	27.262644
235.133067	7912.758976	27.267661
235.523223	7926.591971	27.272679
235.964367	7942.235447	27.277696
235.719389	7949.689259	27.282714
236.233582	7957.258497	27.287732
236.765128	7961.579677	27.292749
237.551020	7983.410835	27.297767
237.652853	7992.704851	27.302784
237.580991	7993.953541	27.307802
238.096558	8006.059151	27.312820
238.300037	8011.286957	27.317837
238.143088	8024.141303	27.322855
238.971589	8028.173180	27.327872
238.556785	8043.801625	27.332890
239.053475	8047.016995	27.337908
239.112828	8067.016667	27.342925
239.182035	8070.734258	27.347943
239.681895	8081.093395	27.352960
239.921765	8092.506407	27.357978
240.002674	8100.209457	27.362996
240.349546	8121.240957	27.368013
240.588167	8129.803423	27.373031
240.967558	8142.934248	27.378048
241.349420	8146.416916	27.383066
241.436695	8153.373946	27.388084
241.429367	8166.785985	27.393101
241.767674	8176.062220	27.398119
242.517788	8190.742276	27.403136
242.188121	8199.573199	27.408154
242.765324	8209.339478	27.413172
242.721317	8220.998814	27.418189
242.699694	8236.250507	27.423207
243.153005	8242.787528	27.428224
243.327983	8245.323750	27.433242
244.038955	8266.611276	27.438260
244.027124	8278.758133	27.443277
243.891022	8276.657776	27.448295
244.616577	8291.468017	27.453312
244.990532	8294.942473	27.458330
245.482892	8300.860974	27.463348
245.927875	8311.225627	27.468365
245.724293	8313.546134	27.473383
246.450173	8303.750504	27.478400
246.493446	8310.335601	27.483418
246.274606	8311.282021	27.488436
247.032849	8320.653959	27.493453
246.967755	8322.697188	27.498471
247.277190	8333.240808	27.503488
247.302864	8328.157124	27.508506
247.427598	8341.094117	27.513524
247.663231	8355.863875	27.518541
247.538431	8361.973189	27.523559
248.010198	8376.131620	27.528576
248.068677	8386.973218	27.533594
248.182799	8403.586699	27.538612
248.454559	8419.721038	27.543629
248.791240	8440.407215	27.548647
249.034754	8446.695995	27.553664
249.130811	8482.106269	27.558682
249.604055	8481.978892	27.563700
249.489803	8504.651676	27.568717
249.749908	8524.412223	27.573735
250.274418	8540.740941	27.578752
250.364901	8562.905206	27.583770
250.949330	8566.829978	27.588788
250.884144	8588.314482	27.593805
250.931547	8601.194242	27.598823
251.602055	8618.292724	27.603840
251.590480	8639.557418	27.608858
251.880702	8658.154771	27.613876
251.803728	8668.117853	27.618893
252.425708	8696.033824	27.623911
252.919235	8709.071514	27.628928
253.173931	8724.037495	27.633946
253.445745	8746.713612	27.638964
253.986561	8761.909747	27.643981
253.575352	8776.060725	27.648999
254.170525	8784.413288	27.654016
254.388053	8803.309402	27.659034
254.701283	8821.483442	27.664052
254.945507	8840.062882	27.669069
255.279989	8860.462575	27.674087
255.821722	8867.203894	27.679104
255.729924	8890.546121	27.684122
255.918094	8898.608503	27.689140
256.326457	8913.995869	27.694157
256.330851	8931.356203	27.699175
256.890485	8936.970823	27.704192
257.162318	8966.466610	27.709210
257.636772	8977.228007	27.714228
257.816245	8978.718619	27.719245
258.020165	9004.294404	27.724263
258.384315	9004.319766	27.729280
258.419272	9026.044916	27.734298
258.911853	9030.306117	27.739316
259.198916	9039.192965	27.744333
259.214037	9059.926741	27.749351
259.362288	9061.801079	27.754368
259.505080	9076.519566	27.759386
259.725048	9097.609823	27.764404
260.115708	9105.830200	27.769421
260.149959	9125.329779	27.774439
260.755627	9143.123948	27.779456
260.595063	9163.171671	27.784474
261.113880	9174.898685	27.789492
261.707491	9186.636163	27.794509
262.425414	9196.087442	27.799527
262.859268	9203.966478	27.804544
263.180955	9221.520789	27.809562
263.166812	9221.810264	27.814580
263.270978	9226.466642	27.819597
263.237120	9221.243594	27.824615
263.320147	9231.794562	27.829632
263.731180	9249.578092	27.834650
263.641128	9257.652374	27.839668
264.206238	9261.131984	27.844685
264.424925	9284.795760	27.849703
264.663380	9280.909992	27.854720
264.613748	9302.525505	27.859738
265.141870	9321.345377	27.864756
265.747799	9330.732075	27.869773
265.339265	9357.246670	27.874791
265.857112	9356.812412	27.879808
266.030371	9376.738936	27.884826
266.142395	9396.930749	27.889844
266.676032	9409.438593	27.894861
267.103846	9422.139725	27.899879
267.482868	9440.610380	27.904896
267.654738	9456.256021	27.909914
268.118175	9468.130762	27.914932
268.177421	9467.392190	27.919949
268.614466	9493.955296	27.924967
268.743111	9494.178344	27.929984
269.040089	9508.734253	27.935002
268.939813	9522.483781	27.940020
269.605584	9544.477568	27.945037
269.725725	9554.217847	27.950055
270.102577	9566.125074	27.955072
270.045103	9584.588056	27.960090
270.354237	9599.022167	27.965108
270.809416	9615.653097	27.970125
271.152846	9629.772484	27.975143
271.699304	9631.007108	27.980160
271.659255	9650.575637	27.985178
272.361275	9646.320841	27.990196
273.226584	9660.507393	27.995213
273.254524	9666.950126	28.000231
273.455409	9666.312628	28.005248
273.572543	9679.289627	28.010266
273.451191	9690.882998	28.015284
273.896102	9694.889723	28.020301
274.219853	9716.273938	28.025319
274.354661	9716.805441	28.030336
274.572325	9746.607687	28.035354
274.386433	9751.369344	28.040372
275.183555	9766.681109	28.045389
275.126881	9779.473700	28.050407
275.528549	9806.409006	28.055424
275.774731	9806.787410	28.060442
275.998152	9832.999072	28.065460
276.267476	9842.529997	28.070477
276.479697	9865.886107	28.075495
276.848150	9870.432042	28.080512
277.218274	9879.129554	28.085530
277.159304	9894.372640	28.090548
277.577203	9907.261929	28.095565
278.162501	9921.388084	28.100583
278.708942	9929.117296	28.105600
278.924615	9944.503946	28.110618
278.928119	9958.512324	28.115636
279.312827	9953.246007	28.120653
279.451845	9981.965289	28.125671
279.838204	9984.528832	28.130688
280.274256	10002.432326	28.135706
280.339238	10014.416811	28.140724
280.932133	10020.216024	28.145741
281.242300	10036.686785	28.150759
281.292590	10033.107999	28.155776
281.496371	10040.606446	28.160794
281.383836	10056.814671	28.165812
282.049723	10054.908143	28.170829
282.251769	10084.713362	28.175847
282.320269	10090.518462	28.180864
282.829900	10100.188918	28.185882
282.999918	10120.208308	28.190900
283.121032	10127.378668	28.195917
283.330050	10140.676362	28.200935
283.615188	10163.547893	28.205952
284.051734	10180.482179	28.210970
284.241544	10200.732217	28.215988
284.527702	10205.515218	28.221005
284.577553	10223.147529	28.226023
284.975671	10244.381851	28.231040
285.306504	10257.206004	28.236058
285.545312	10279.207146	28.241076
285.901207	10290.925503	28.246093
286.297746	10321.742751	28.251111
286.564062	10333.039365	28.256128
286.431870	10352.383016	28.261146
286.736848	10379.893061	28.266164
286.936655	10386.362962	28.271181
287.173182	10413.144886	28.276199
287.606608	10432.053250	28.281216
287.956350	10458.012480	28.286234
288.397350	10480.399157	28.291252
288.403158	10504.141831	28.296269
288.723635	10524.204536	28.301287
288.966963	10542.741617	28.306304
289.639988	10560.428784	28.311322
290.009408	10583.856043	28.316340
290.378561	10597.116503	28.321357
291.001216	10611.313147	28.326375
291.212559	10629.609016	28.331392
291.399779	10645.209064	28.336410
291.511313	10666.412706	28.341428
292.111548	10675.583113	28.346445
292.296764	10682.993145	28.351463
292.766127	10697.905197	28.356480
293.057401	10703.612657	28.361498
293.744630	10729.311333	28.366516
293.810614	10727.100299	28.371533
293.483189	10738.120174	28.376551
293.774299	10747.796572	28.381568
294.316726	10759.363044	28.386586
294.606949	10776.810056	28.391604
295.402840	10790.474676	28.396621
295.461827	10812.318153	28.401639
295.648257	10822.228751	28.406656
296.458111	10826.598849	28.411674
296.353820	10832.083762	28.416692
296.932231	10847.471520	28.421709
296.997988	10854.707612	28.426727
297.502361	10871.761424	28.431744
297.482414	10880.870613	28.436762
297.334726	10891.805762	28.441780
297.672264	10904.108336	28.446797
298.263256	10928.164601	28.451815
298.076815	10941.256048	28.456832
299.040978	10964.111259	28.461850
298.776521	10980.823873	28.466868
299.200779	10989.437700	28.471885
299.476906	11013.899890	28.476903
299.715914	11028.260778	28.481920
299.839467	11054.549698	28.486938
299.944157	11075.110742	28.491956
300.119645	11080.798454	28.496973
300.589532	11106.477811	28.501991
301.129500	11131.776863	28.507008
301.733656	11135.092879	28.512026
301.772406	11168.733202	28.517044
302.225702	11174.728177	28.522061
302.868463	11182.184002	28.527079
302.723127	11194.400911	28.532096
303.298966	11203.414345	28.537114
303.230591	11216.904396	28.542132
303.890288	11235.664678	28.547149
303.938419	11258.675492	28.552167
304.304149	11269.631971	28.557184
304.748644	11275.473630	28.562202
305.060788	11301.986140	28.567220
305.249039	11317.264521	28.572237
305.705109	11329.286847	28.577255
306.020927	11349.524830	28.582272
306.468775	11362.154705	28.587290
306.753673	11384.295221	28.592308
307.023666	11393.861570	28.597325
307.567959	11407.338472	28.602343
307.312435	11416.863503	28.607360
307.441297	11436.612847	28.612378
307.689725	11464.906895	28.617396
307.967454	11476.344515	28.622413
308.342365	11503.204343	28.627431
308.682523	11531.070569	28.632448
309.129375	11539.283279	28.637466
309.516241	11558.080046	28.642484
310.028703	11576.364697	28.647501
310.370278	11579.566952	28.652519
310.655936	11601.057145	28.657536
310.980151	11612.651806	28.662554
311.255788	11636.202344	28.667572
311.615964	11646.307360	28.672589
311.988708	11655.895738	28.677607
311.915839	11683.078143	28.682624
312.297664	11694.414435	28.687642
312.720126	11719.527334	28.692660
313.148482	11740.989157	28.697677
313.710043	11755.928751	28.702695
314.098992	11773.790759	28.707712
314.019240	11783.695942	28.712730
314.148187	11801.573194	28.717748
314.370452	11815.419443	28.722765
315.052109	11834.650552	28.727783
314.922331	11865.400720	28.732800
315.471253	11883.152671	28.737818
315.587046	11905.288554	28.742836
315.535083	11926.620121	28.747853
315.925629	11953.070824	28.752871
316.524171	11969.207892	28.757888
316.880615	11986.367851	28.762906
317.333201	12013.551028	28.767924
317.527527	12035.115933	28.772941
318.102551	12053.343945	28.777959
318.222287	12075.946748	28.782976
319.267130	12083.223505	28.787994
319.269027	12094.884432	28.793012
319.788096	12116.705167	28.798029
320.326130	12112.374311	28.803047
320.208726	12131.215425	28.808064
320.856399	12130.040955	28.813082
321.351126	12145.749107	28.818100
321.822033	12149.158679	28.823117
322.280628	12151.929160	28.828135
322.363109	12160.631472	28.833152
322.535083	12151.125328	28.838170
322.913384	12174.477414	28.843188
322.822182	12186.080265	28.848205
323.049541	12186.335346	28.853223
323.378018	12197.585518	28.858240
323.974435	12209.883384	28.863258
324.017614	12227.613352	28.868276
324.341908	12237.383244	28.873293
324.410436	12255.579788	28.878311
324.570488	12279.556471	28.883328
325.089575	12280.817648	28.888346
325.188978	12308.558312	28.893364
325.340823	12326.470390	28.898381
326.014717	12349.959823	28.903399
326.141493	12367.913736	28.908416
326.460212	12388.414479	28.913434
326.605212	12416.163990	28.918452
326.993684	12437.601243	28.923469
327.417660	12450.333460	28.928487
327.861076	12473.644204	28.933504
328.419319	12495.737161	28.938522
328.408682	12515.124114	28.943540
328.869802	12529.792610	28.948557
329.486119	12541.291846	28.953575
329.579122	12571.774811	28.958592
329.808538	12589.340343	28.963610
330.518849	12614.106482	28.968628
330.728486	12635.906524	28.973645
331.257751	12650.460299	28.978663
331.117889	12673.524217	28.983680
331.566517	12693.708238	28.988698
331.692737	12704.646006	28.993716
331.684495	12734.443972	28.998733
332.201443	12764.431791	29.003751
332.463935	12793.568777	29.008768
332.710958	12798.409063	29.013786
333.088596	12836.616291	29.018804
333.210900	12869.305627	29.023821
333.708975	12895.510397	29.028839
333.887930	12922.162769	29.033856
334.838966	12948.088679	29.038874
335.142639	12983.295170	29.043892
334.911783	13001.220103	29.048909
335.609911	13020.844592	29.053927
336.186281	13047.839471	29.058944
336.545695	13081.616447	29.063962
337.294972	13097.869965	29.068980
337.300927	13124.325349	29.073997
337.928057	13132.880161	29.079015
337.956915	13155.065783	29.084032
338.397116	13164.088651	29.089050
339.104634	13200.928438	29.094068
339.104381	13216.891386	29.099085
339.616376	13237.770326	29.104103
339.769215	13261.853590	29.109120
340.302246	13265.929479	29.114138
340.987866	13282.777272	29.119156
341.240423	13301.621956	29.124173
341.512850	13312.843628	29.129191
341.571151	13329.028079	29.134208
342.167039	13338.004688	29.139226
342.680933	13351.677194	29.144244
342.954282	13376.259735	29.149261
343.379081	13385.919841	29.154279
344.041522	13400.545043	29.159296
343.835650	13416.657012	29.164314
344.472837	13423.340923	29.169332
344.515433	13432.397399	29.174349
344.901762	13446.636149	29.179367
344.984132	13443.803299	29.184384
344.915745	13470.779162	29.189402
345.167293	13485.443135	29.194420
345.560129	13498.446173	29.199437
345.803510	13514.886180	29.204455
346.190520	13548.536536	29.209472
346.926380	13571.361003	29.214490
347.025657	13582.679266	29.219508
347.478283	13609.286843	29.224525
348.004372	13622.152378	29.229543
348.150790	13647.528723	29.234560
348.474037	13668.898582	29.239578
348.764015	13690.216802	29.244596
348.760227	13716.462949	29.249613
349.249876	13734.980625	29.254631
349.755088	13758.134914	29.259648
350.267709	13781.673347	29.264666
350.596930	13803.307695	29.269684
350.780538	13830.750111	29.274701
351.325789	13854.340398	29.279719
351.299182	13883.615653	29.284736
351.899248	13907.636429	29.289754
352.406807	13924.825156	29.294772
352.641928	13953.949245	29.299789
353.223859	13965.429444	29.304807
353.548274	13983.410967	29.309824
353.490708	14010.152221	29.314842
353.911781	14033.522057	29.319860
354.407648	14066.610055	29.324877
354.837237	14082.374177	29.329895
355.300342	14112.044086	29.334912
355.630818	14128.401590	29.339930
356.106819	14152.198826	29.344948
355.947031	14179.752051	29.349965
356.664155	14205.223457	29.354983
357.082112	14224.990717	29.360000
357.612813	14232.537845	29.365018
358.364279	14254.861741	29.370036
358.495434	14283.803566	29.375053
358.991236	14296.276364	29.380071
359.207904	14313.504415	29.385088
359.500359	14327.332109	29.390106
360.117374	14349.841266	29.395124
359.922919	14373.705261	29.400141
360.471461	14383.488727	29.405159
360.832273	14413.923491	29.410176
361.059891	14439.660903	29.415194
361.243581	14447.047393	29.420212
361.782507	14469.859391	29.425229
362.226790	14490.529193	29.430247
362.463587	14522.537206	29.435264
362.604584	14533.300036	29.440282
363.225253	14562.655578	29.445300
363.376320	14593.322242	29.450317
363.710215	14608.653252	29.455335
364.489081	14644.960502	29.460352
364.627799	14672.919575	29.465370
365.186310	14683.349054	29.470388
365.056064	14713.045956	29.475405
365.375345	14740.692789	29.480423
366.045086	14764.429050	29.485440
366.143111	14790.477658	29.490458
367.122743	14815.428984	29.495476
367.396978	14841.526024	29.500493
367.760444	14859.612833	29.505511
367.934802	14877.969117	29.510528
368.231861	14900.819287	29.515546
368.995382	14907.253517	29.520564
369.265151	14930.297460	29.525581
369.789557	14932.729667	29.530599
369.818708	14951.345488	29.535616
370.454912	14972.162791	29.540634
370.792774	14983.867937	29.545652
371.281447	15008.093781	29.550669
371.690448	15029.136007	29.555687
372.151355	15029.882184	29.560704
372.280649	15054.644076	29.565722
372.866191	15059.880701	29.570740
373.075300	15079.195007	29.575757
373.424112	15100.060351	29.580775
374.117795	15106.590792	29.585792
374.086204	15124.202467	29.590810
374.705183	15146.734372	29.595828
375.320124	15159.144977	29.600845
375.517321	15160.317512	29.605863
375.739066	15175.780134	29.610880
376.296107	15196.281557	29.615898
376.400452	15214.626958	29.620916
376.534237	15239.407339	29.625933
376.862235	15259.726573	29.630951
377.670282	15280.612208	29.635968
377.768426	15304.722369	29.640986
378.111528	15307.688163	29.646004
378.386614	15338.968359	29.651021
378.740451	15350.658611	29.656039
378.908693	15384.264165	29.661056
379.294965	15410.537194	29.666074
379.865291	15439.826130	29.671092
379.963710	15471.310907	29.676109
380.466719	15500.323018	29.681127
380.665477	15523.438739	29.686144
380.938653	15547.411418	29.691162
381.097595	15571.569299	29.696180
381.591987	15609.896580	29.701197
382.143634	15634.369234	29.706215
382.903423	15671.079352	29.711232
382.729829	15705.859870	29.716250
383.256195	15736.141484	29.721268
383.715375	15766.310433	29.726285
384.054210	15788.324536	29.731303
384.422919	15823.617756	29.736320
384.402573	15864.564944	29.741338
385.182371	15891.260587	29.746356
385.661875	15914.626796	29.751373
386.546877	15947.436401	29.756391
387.078609	15971.934697	29.761408
387.223029	15996.878636	29.766426
387.623966	16019.126527	29.771444
387.975863	16044.799382	29.776461
388.588781	16072.907763	29.781479
389.422606	16087.097778	29.786496
389.176015	16108.953882	29.791514
389.888507	16131.737693	29.796532
389.964047	16151.598161	29.801549
390.344535	16175.138020	29.806567
390.701547	16199.370082	29.811584
390.850479	16228.359462	29.816602
391.691803	16246.632178	29.821620
391.893474	16272.515068	29.826637
392.142584	16304.391500	29.831655
392.751066	16321.696176	29.836672
393.158396	16348.314635	29.841690
393.427071	16363.338215	29.846708
393.909465	16393.602448	29.851725
394.103258	16409.117795	29.856743
394.809243	16433.816958	29.861760
394.967167	16458.535149	29.866778
395.242024	16473.621021	29.871796
395.754304	16502.592149	29.876813
396.009655	16521.354311	29.881831
396.751368	16542.074785	29.886848
396.751397	16566.043887	29.891866
397.051079	16595.736787	29.896884
397.629401	16616.637541	29.901901
397.729421	16643.872767	29.906919
398.616051	16662.618908	29.911936
398.903868	16698.485373	29.916954
399.063961	16724.012125	29.921972
399.440959	16753.497409	29.926989
399.517625	16779.040382	29.932007
400.199258	16801.725566	29.937024
400.490865	16832.800330	29.942042
401.253897	16869.389062	29.947060
401.505694	16892.918251	29.952077
401.818710	16925.085817	29.957095
402.519402	16940.724821	29.962112
402.768107	16980.722862	29.967130
403.344346	16999.186014	29.972148
403.738248	17023.795550	29.977165
404.026138	17040.683331	29.982183
404.589464	17075.771682	29.987200
405.225961	17102.023868	29.992218
405.544308	17121.399031	29.997236
406.088205	17155.302956	30.002253
405.978224	17171.835871	30.007271
406.574596	17194.815901	30.012288
407.130086	17226.744078	30.017306
407.371913	17240.458581	30.022324
407.892211	17266.526936	30.027341
408.337394	17293.112385	30.032359
409.083514	17317.326342	30.037376
409.423150	17339.544247	30.042394
410.068309	17359.857394	30.047412
410.587465	17384.368929	30.052429
410.548329	17403.351516	30.057447
411.085215	17414.468105	30.062464
411.215111	17444.722541	30.067482
411.659560	17459.729090	30.072500
412.368445	17491.396934	30.077517
412.794169	17516.870750	30.082535
413.163383	17543.774753	30.087552
413.172447	17562.099327	30.092570
413.449241	17596.497287	30.097588
413.608443	17624.691210	30.102605
414.309084	17656.155301	30.107623
414.848610	17688.358367	30.112640
414.786689	17711.785784	30.117658
415.380747	17744.163652	30.122676
416.042845	17777.548053	30.127693
416.477028	17812.894746	30.132711
416.851050	17830.411009	30.137728
417.257677	17857.259086	30.142746
418.057604	17896.231942	30.147764
418.554433	17913.179561	30.152781
418.278677	17933.962021	30.157799
418.695575	17959.336719	30.162816
419.470429	17989.993824	30.167834
420.166933	18008.786675	30.172852
420.938528	18033.979906	30.177869
420.900222	18068.863654	30.182887
421.359722	18083.587226	30.187904
422.014614	18110.220120	30.192922
422.101284	18128.198331	30.197940
422.663947	18150.158184	30.202957
422.718221	18165.886186	30.207975
423.243127	18189.892462	30.212992
423.265063	18213.105276	30.218010
423.699021	18238.869361	30.223028
424.447756	18266.542861	30.228045
424.485834	18300.953967	30.233063
425.111428	18306.308446	30.238080
425.805485	18343.744611	30.243098
426.232517	18372.662333	30.248116
426.507977	18402.058549	30.253133
426.859122	18425.100334	30.258151
427.239242	18458.523493	30.263168
427.590788	18490.618177	30.268186
427.922757	18510.889692	30.273204
429.020107	18540.745690	30.278221
429.330376	18560.938509	30.283239
429.853447	18578.798660	30.288256
430.168068	18619.421577	30.293274
430.746001	18641.948185	30.298292
431.322640	18661.284684	30.303309
431.292756	18685.321087	30.308327
432.244051	18699.507388	30.313344
432.669507	18730.965530	30.318362
432.884751	18759.354541	30.323380
433.603132	18769.837176	30.328397
433.646250	18800.173574	30.333415
433.931208	18827.945348	30.338432
434.455335	18847.789295	30.343450
435.138649	18867.153615	30.348468
435.312919	18897.810896	30.353485
435.750753	18928.730438	30.358503
436.431490	18948.973386	30.363520
436.632432	18973.201643	30.368538
437.237336	18999.022256	30.373556
437.936496	19017.348172	30.378573
438.107145	19052.466497	30.383591
438.407986	19084.904892	30.388608
438.588128	19106.179899	30.393626
439.006337	19134.809520	30.398644
439.867090	19154.500293	30.403661
440.549433	19190.625845	30.408679
441.037885	19221.019923	30.413696
441.135943	19244.304247	30.418714
441.584010	19271.924910	30.423732
442.061172	19293.198106	30.428749
441.998778	19316.273740	30.433767
443.028079	19341.649676	30.438784
443.709102	19370.371402	30.443802
443.981025	19400.894236	30.448820
444.480922	19415.271375	30.453837
444.827974	19446.780788	30.458855
444.994706	19471.539365	30.463872
445.800150	19492.862758	30.468890
446.044114	19519.972219	30.473908
446.720472	19550.975656	30.478925
446.926740	19572.714622	30.483943
447.097246	19592.285856	30.488960
447.773303	19632.039625	30.493978
448.108836	19661.750603	30.498996
448.612450	19677.068712	30.504013
449.035449	19712.016266	30.509031
449.519537	19744.326147	30.514048
450.040007	19765.144550	30.519066
450.478416	19795.414641	30.524084
450.730364	19809.994936	30.529101
451.351896	19851.709864	30.534119
451.509503	19874.593962	30.539136
452.010064	19899.035760	30.544154
451.990871	19929.750054	30.549172
452.509442	19955.452701	30.554189
453.178811	19989.768514	30.559207
453.933234	20024.728212	30.564224
454.373277	20050.462163	30.569242
454.525424	20081.484873	30.574260
454.798720	20104.155372	30.579277
455.104426	20141.699686	30.584295
455.597609	20161.208621	30.589312
455.931404	20207.063156	30.594330
456.543241	20236.498228	30.599348
457.096645	20270.327147	30.604365
457.444456	20310.007037	30.609383
457.923264	20351.423032	30.614400
458.281347	20384.916109	30.619418
458.695812	20423.480193	30.624436
459.385552	20450.306733	30.629453
459.940422	20494.718595	30.634471
460.390237	20528.361907	30.639488
461.309451	20561.799522	30.644506
461.406499	20604.267426	30.649524
462.189754	20621.905725	30.654541
462.662155	20656.878868	30.659559
463.014193	20687.056378	30.664576
463.887705	20717.013752	30.669594
463.741728	20745.916795	30.674612
464.240259	20779.199137	30.679629
465.024523	20803.199855	30.684647
465.156906	20841.631766	30.689664
465.920312	20875.005718	30.694682
466.269791	20909.455081	30.699700
467.058156	20945.624242	30.704717
467.289217	20976.528673	30.709735
467.795155	20999.088172	30.714752
468.588114	21034.435409	30.719770
468.871707	21072.547274	30.724788
469.491147	21093.288503	30.729805
470.008795	21109.793391	30.734823
470.482733	21145.803366	30.739840
470.817967	21172.338579	30.744858
470.891568	21204.291447	30.749876
471.210919	21226.172604	30.754893
471.484319	21268.822995	30.759911
472.266546	21311.526952	30.764928
472.832773	21339.087913	30.769946
473.228582	21379.034183	30.774964
473.444257	21411.161139	30.779981
474.252712	21458.631715	30.784999
474.442884	21489.916104	30.790016
475.464670	21520.180182	30.795034
475.631382	21561.103932	30.800052
476.651211	21589.295974	30.805069
476.627400	21622.604197	30.810087
477.307185	21651.904448	30.815104
478.486876	21671.927225	30.820122
478.384252	21709.449646	30.825140
478.919388	21735.594345	30.830157
479.803093	21757.956900	30.835175
480.027031	21787.069260	30.840192
480.671144	21809.962017	30.845210
481.110601	21835.281381	30.850228
481.697641	21866.479311	30.855245
481.802699	21892.097229	30.860263
482.428567	21918.708255	30.865280
483.026033	21934.847573	30.870298
483.129300	21966.405308	30.875316
483.913292	21994.963214	30.880333
483.925343	22022.112238	30.885351
484.525957	22044.822482	30.890368
484.908340	22066.246140	30.895386
485.351059	22108.631884	30.900404
485.626746	22122.970098	30.905421
486.282661	22159.793975	30.910439
486.089910	22189.647890	30.915456
486.993330	22220.430647	30.920474
487.340888	22268.019156	30.925492
488.062093	22295.980681	30.930509
488.394321	22327.307470	30.935527
488.670287	22364.664779	30.940544
489.108771	22404.397967	30.945562
489.218973	22446.090592	30.950580
489.891026	22482.805141	30.955597
490.926546	22528.195677	30.960615
491.194250	22575.443507	30.965632
491.705685	22614.995155	30.970650
492.044054	22646.694301	30.975668
492.959541	22672.256571	30.980685
493.932669	22702.757520	30.985703
494.843068	22726.513477	30.990720
495.528530	22740.093277	30.995738
496.031487	22764.696242	31.000756
496.459542	22781.178568	31.005773
496.947777	22811.660390	31.010791
497.427339	22844.917583	31.015808
497.929956	22860.781759	31.020826
498.477134	22895.311236	31.025844
498.517057	22917.932845	31.030861
499.033432	22944.644446	31.035879
499.295048	22981.164743	31.040896
500.000156	23012.270276	31.045914
500.042318	23053.987411	31.050932
500.840758	23092.149403	31.055949
501.266265	23116.322537	31.060967
501.411818	23151.186698	31.065984
501.933719	23185.076083	31.071002
502.399736	23231.094002	31.076020
502.938944	23270.661592	31.081037
503.395352	23297.970670	31.086055
503.772036	23342.871656	31.091072
504.495043	23374.000247	31.096090
504.925369	23421.768212	31.101108
505.543774	23468.603388	31.106125
506.006463	23496.651090	31.111143
506.122353	23544.777934	31.116160
507.199529	23573.254566	31.121178
507.687671	23608.906633	31.126196
507.926757	23658.366857	31.131213
508.587103	23682.630504	31.136231
508.940534	23723.270569	31.141248
509.759725	23763.939316	31.146266
510.380779	23806.793821	31.151284
511.022199	23827.995804	31.156301
511.468147	23865.980351	31.161319
511.609452	23909.573275	31.166336
512.446168	23940.072091	31.171354
512.942939	23974.996764	31.176372
513.690237	24005.187321	31.181389
514.515904	24035.087678	31.186407
514.708106	24069.257389	31.191424
515.184368	24103.850561	31.196442
515.646556	24132.948233	31.201460
515.888108	24163.141931	31.206477
516.574752	24198.726237	31.211495
516.895797	24235.378607	31.216512
517.487968	24262.971201	31.221530
517.778667	24298.813223	31.226548
518.392758	24331.862381	31.231565
518.985087	24352.503828	31.236583
519.218815	24389.138477	31.241600
520.108826	24423.914247	31.246618
520.135810	24465.782044	31.251636
520.829222	24489.150498	31.256653
521.556360	24522.435148	31.261671
522.184515	24564.241160	31.266688
522.698513	24587.479675	31.271706
523.191125	24624.561047	31.276724
523.631391	24655.539759	31.281741
524.137760	24687.828988	31.286759
524.888762	24737.705109	31.291776
524.831899	24763.389851	31.296794
525.663825	24802.731651	31.301812
525.897988	24840.871092	31.306829
526.446710	24877.407043	31.311847
526.869497	24922.569826	31.316864
527.933370	24958.602322	31.321882
528.336509	24992.273128	31.326900
528.885884	25031.589849	31.331917
529.595483	25068.941604	31.336935
530.509902	25105.579030	31.341952
530.876749	25138.762806	31.346970
531.623963	25164.765257	31.351988
532.000232	25187.040056	31.357005
532.798469	25213.236854	31.362023
533.579359	25245.629598	31.367040
534.079678	25275.285443	31.372058
534.500637	25299.063797	31.377076
535.076561	25323.898712	31.382093
535.480565	25353.942525	31.387111
535.735812	25389.374923	31.392128
536.094869	25419.514306	31.397146
536.599121	25452.462343	31.402164
537.207247	25487.492397	31.407181
537.756617	25523.656565	31.412199
538.013031	25562.122538	31.417216
538.472242	25596.859980	31.422234
539.222816	25639.350668	31.427252
539.630895	25677.338230	31.432269
540.526066	25712.918048	31.437287
541.104450	25745.943502	31.442304
541.190452	25776.309202	31.447322
541.941933	25810.792962	31.452340
542.448707	25856.305000	31.457357
543.330702	25894.686861	31.462375
543.552931	25922.876520	31.467392
543.951673	25968.626823	31.472410
544.688210	26003.441872	31.477428
545.067410	26041.769570	31.482445
545.748841	26078.565123	31.487463
546.250132	26123.490871	31.492480
546.313471	26166.822765	31.497498
546.971123	26198.888639	31.502516
547.573824	26245.265089	31.507533
548.187186	26290.041043	31.512551
548.543512	26340.052107	31.517568
549.149204	26375.741362	31.522586
550.206015	26426.578947	31.527604
550.309649	26462.201154	31.532621
550.930502	26501.016664	31.537639
551.295293	26546.539723	31.542656
552.078081	26592.225335	31.547674
552.730904	26629.487709	31.552692
553.466707	26671.414071	31.557709
553.915995	26698.210655	31.562727
554.167403	26736.660688	31.567744
554.765137	26772.870131	31.572762
555.165087	26813.464973	31.577780
555.555018	26853.524248	31.582797
556.186884	26888.142237	31.587815
556.359275	26934.802143	31.592832
556.941441	26977.296589	31.597850
557.525709	27021.806929	31.602868
558.076766	27083.229010	31.607885
558.736487	27109.095914	31.612903
559.116513	27170.481683	31.617920
559.975535	27206.524822	31.622938
560.727945	27245.517209	31.627956
561.364860	27292.364753	31.632973
561.947713	27327.730593	31.637991
562.297182	27375.646959	31.643008
562.999771	27421.056195	31.648026
563.957651	27469.061356	31.653044
564.267386	27506.852779	31.658061
565.144906	27544.745493	31.663079
565.856812	27587.834094	31.668096
565.764365	27637.722295	31.673114
566.444060	27681.144767	31.678132
567.112621	27728.405536	31.683149
567.508363	27759.680369	31.688167
567.960395	27809.566395	31.693184
569.040733	27854.936758	31.698202
569.633784	27892.463579	31.703220
569.849920	27940.193458	31.708237
570.823535	27975.234137	31.713255
571.151788	28017.599638	31.718272
571.561840	28063.359234	31.723290
572.464958	28102.860729	31.728308
573.088610	28140.515974	31.733325
574.023452	28176.391023	31.738343
574.187801	28218.163046	31.743360
575.310482	28260.809896	31.748378
575.781118	28285.532116	31.753396
576.331871	28327.092516	31.758413
576.986382	28370.583587	31.763431
577.458916	28408.882271	31.768448
578.160629	28438.795834	31.773466
578.492785	28471.238331	31.778484
579.120315	28522.400828	31.783501
580.126059	28556.091214	31.788519
580.554848	28589.928358	31.793536
580.893482	28622.502820	31.798554
581.974028	28658.387641	31.803572
582.264644	28697.176595	31.808589
582.689357	28740.034235	31.813607
583.405466	28774.850910	31.818624
584.087706	28805.596057	31.823642
584.569875	28848.242717	31.828660
585.191581	28893.516135	31.833677
585.727378	28925.384068	31.838695
585.973632	28977.662627	31.843712
586.370354	29015.847836	31.848730
587.105057	29058.954965	31.853748
587.358288	29100.070234	31.858765
588.325176	29142.958092	31.863783
588.857805	29189.756709	31.868800
589.496422	29229.965253	31.873818
590.200114	29271.231970	31.878836
590.673755	29310.385488	31.883853
591.086863	29339.833311	31.888871
591.394759	29381.180827	31.893888
591.875565	29437.956127	31.898906
593.033007	29471.106095	31.903924
593.642846	29512.514328	31.908941
593.849435	29546.381324	31.913959
594.321338	29581.098328	31.918976
595.145043	29623.996843	31.923994
596.177933	29646.016303	31.929012
596.320468	29695.013289	31.934029
597.031385	29735.603472	31.939047
597.405728	29779.147476	31.944064
598.336791	29817.036082	31.949082
598.728262	29846.696595	31.954100
599.057975	29901.252730	31.959117
599.757670	29945.011921	31.964135
600.339436	29986.653040	31.969152
600.488081	30038.443809	31.974170
600.736046	30089.485999	31.979188
601.619172	30137.951558	31.984205
602.542779	30186.290827	31.989223
603.148056	30246.961771	31.994240
603.631967	30301.020874	31.999258
604.279806	30341.324978	32.004276
604.691392	30397.032779	32.009293
605.544643	30442.678128	32.014311
605.988497	30497.534135	32.019328
606.692461	30557.893534	32.024346
607.175837	30604.892678	32.029364
608.070087	30652.181960	32.034381
608.675261	30701.305279	32.039399
609.506791	30755.267210	32.044416
609.951035	30813.436364	32.049434
610.736591	30854.725125	32.054452
611.523932	30898.453734	32.059469
612.218851	30948.859550	32.064487
612.652030	30995.936935	32.069504
613.364414	31037.578808	32.074522
613.964542	31085.034975	32.079540
614.682823	31143.623862	32.084557
615.157940	31187.028723	32.089575
615.837748	31239.593213	32.094592
616.202027	31281.902950	32.099610
617.403791	31339.064330	32.104628
617.818589	31377.472360	32.109645
618.433270	31423.511022	32.114663
618.907527	31451.074855	32.119680
619.278965	31515.313338	32.124698
620.353679	31559.232507	32.129716
620.774644	31620.271219	32.134733
621.102979	31659.439177	32.139751
622.285756	31710.896146	32.144768
622.236640	31757.494040	32.149786
623.167536	31810.760521	32.154804
624.051947	31860.728153	32.159821
624.639395	31914.958684	32.164839
625.588831	31956.900553	32.169856
625.898923	32016.276122	32.174874
626.469258	32051.140001	32.179892
627.211762	32099.119994	32.184909
628.287288	32139.361025	32.189927
629.237774	32182.668682	32.194944
629.667578	32218.566199	32.199962
630.229503	32254.405280	32.204980
630.719751	32288.428586	32.209997
631.479873	32341.520717	32.215015
632.177242	32376.023989	32.220032
632.743031	32425.378791	32.225050
633.236804	32463.087456	32.230068
633.866237	32494.092883	32.235085
633.923396	32537.641495	32.240103
634.920415	32573.716843	32.245120
635.240678	32611.926929	32.250138
636.327129	32652.710936	32.255156
636.199004	32692.204773	32.260173
637.008259	32736.926389	32.265191
637.701339	32770.185565	32.270208
638.453913	32818.058176	32.275226
639.211834	32862.320229	32.280244
639.575949	32900.334358	32.285261
640.134355	32949.059352	32.290279
640.819347	32993.370967	32.295296
641.768066	33037.553115	32.300314
642.744700	33072.450286	32.305332
643.324179	33106.284021	32.310349
644.254718	33145.892081	32.315367
644.900349	33176.744274	32.320384
645.624985	33225.652664	32.325402
646.265296	33261.791056	32.330420
647.038201	33298.022668	32.335437
647.385750	33341.749023	32.340455
648.239074	33377.133736	32.345472
648.241760	33417.695982	32.350490
648.922617	33459.828099	32.355508
649.610622	33503.969632	32.360525
650.398384	33546.970384	32.365543
651.151311	33582.446940	32.370560
651.816336	33629.886167	32.375578
652.649765	33667.784377	32.380596
653.159060	33703.937608	32.385613
653.310552	33764.714756	32.390631
654.114563	33806.347911	32.395648
654.476694	33857.824139	32.400666
655.198444	33900.140444	32.405684
655.651557	33949.162338	32.410701
655.966533	34013.246599	32.415719
656.816179	34070.217403	32.420736
657.559756	34120.370431	32.425754
658.010655	34176.404668	32.430772
658.769246	34232.783142	32.435789
659.366106	34296.938189	32.440807
659.923858	34353.740240	32.445824
660.941497	34416.837532	32.450842
661.536974	34477.338984	32.455860
662.094773	34529.342770	32.460877
663.083271	34588.120553	32.465895
663.674786	34627.177233	32.470912
664.179901	34680.757571	32.475930
665.245521	34734.370918	32.480948
666.237120	34785.479558	32.485965
666.718522	34839.531858	32.490983
667.499679	34879.590060	32.496000
668.201597	34930.788405	32.501018
668.762594	34983.513588	32.506036
669.638011	35030.455352	32.511053
670.016576	35084.088027	32.516071
670.899126	35138.224066	32.521088
671.542498	35184.930423	32.526106
671.951246	35231.180239	32.531124
672.776552	35284.434068	32.536141
673.415016	35344.400210	32.541159
674.252728	35384.007977	32.546176
674.716038	35432.032744	32.551194
675.192677	35486.005244	32.556212
676.049699	35535.480091	32.561229
676.741532	35597.904518	32.566247
677.482695	35645.323788	32.571264
678.062505	35698.016210	32.576282
678.805181	35750.784574	32.581300
679.432108	35786.467823	32.586317
679.978200	35832.609054	32.591335
680.955156	35879.056360	32.596352
681.904106	35914.177544	32.601370
682.011483	35954.064465	32.606388
682.698968	36009.143593	32.611405
683.280795	36058.049180	32.616423
683.958888	36109.399513	32.621440
684.569263	36140.470198	32.626458
685.397406	36198.455441	32.631476
686.484947	36246.435463	32.636493
686.780017	36290.384757	32.641511
687.711463	36325.180552	32.646528
688.431975	36377.953927	32.651546
689.043605	36421.772016	32.656564
689.988839	36469.553389	32.661581
689.925801	36533.893821	32.666599
690.769503	36571.536407	32.671616
691.965228	36628.649928	32.676634
692.664660	36674.067254	32.681652
693.473401	36716.445214	32.686669
693.553342	36773.682233	32.691687
694.564094	36829.256952	32.696704
695.073791	36874.704242	32.701722
695.334408	36933.747279	32.706740
696.449745	36987.598874	32.711757
696.914581	37044.055858	32.716775
697.493031	37099.376094	32.721792
698.367525	37151.653174	32.726810
699.336514	37209.935410	32.731828
700.193086	37263.752105	32.736845
700.800371	37325.562438	32.741863
701.589987	37374.514581	32.746880
702.236931	37429.736484	32.751898
702.945302	37484.594861	32.756916
704.027819	37530.384362	32.761933
704.749828	37586.511871	32.766951
705.263609	37635.216675	32.771968
706.287259	37687.003917	32.776986
706.542098	37744.981439	32.782004
707.239173	37796.079943	32.787021
707.873681	37856.262449	32.792039
708.722275	37903.802818	32.797056
709.317819	37955.043976	32.802074
709.691991	38019.561105	32.807092
710.558996	38069.982490	32.812109
711.017292	38139.804955	32.817127
711.788183	38196.046597	32.822144
712.712432	38244.625653	32.827162
713.610222	38306.444180	32.832180
714.773410	38367.785243	32.837197
715.420370	38418.134199	32.842215
716.020616	38470.741755	32.847232
717.100865	38508.559612	32.852250
717.699761	38557.227965	32.857268
718.545539	38603.410738	32.862285
718.947410	38661.051658	32.867303
719.877965	38710.819640	32.872320
720.592277	38746.209669	32.877338
721.239295	38807.638662	32.882356
721.884943	38863.231231	32.887373
722.427760	38918.106396	32.892391
722.832809	38966.192444	32.897408
723.691437	39025.122846	32.902426
724.054943	39076.921348	32.907444
725.165871	39133.713269	32.912461
725.387701	39194.260979	32.917479
726.218724	39258.008755	32.922496
726.849297	39310.746441	32.927514
727.313377	39362.650125	32.932532
728.283468	39412.166940	32.937549
728.787474	39476.478502	32.942567
729.362747	39534.708181	32.947584
730.034082	39583.607882	32.952602
730.661009	39658.683189	32.957620
731.756205	39715.909120	32.962637
732.196250	39776.000780	32.967655
732.869405	39829.005033	32.972672
734.071811	39895.397232	32.977690
734.545333	39953.340322	32.982708
735.421940	40021.693490	32.987725
736.213839	40082.679839	32.992743
736.749871	40138.337018	32.997760
737.882117	40194.053307	33.002778
738.614995	40263.251747	33.007796
739.336497	40327.316954	33.012813
739.762341	40387.526352	33.017831
740.776556	40448.909167	33.022848
741.352351	40516.039553	33.027866
741.920090	40591.133621	33.032884
743.116220	40648.738406	33.037901
744.109289	40703.098978	33.042919
744.783978	40763.422462	33.047936
745.911010	40814.214530	33.052954
746.421890	40874.747226	33.057972
747.925518	40928.061261	33.062989
748.684217	40981.744363	33.068007
748.994121	41038.286509	33.073024
749.988091	41087.474564	33.078042
750.419282	41149.057626	33.083060
751.419439	41191.465192	33.088077
752.268826	41249.618849	33.093095
752.690500	41301.065756	33.098112
753.277373	41348.262325	33.103130
753.928134	41408.445855	33.108148
755.262441	41467.504900	33.113165
755.611815	41535.679266	33.118183
756.648864	41593.621214	33.123200
757.244540	41644.693993	33.128218
757.948699	41712.693515	33.133236
758.571234	41761.125040	33.138253
759.175785	41814.631798	33.143271
759.964505	41886.900450	33.148288
760.971675	41947.143822	33.153306
761.301888	42012.893995	33.158324
762.164714	42071.724483	33.163341
762.731467	42148.063689	33.168359
763.274020	42209.720943	33.173376
764.671612	42282.680381	33.178394
764.895416	42350.541615	33.183412
765.655733	42422.158676	33.188429
766.401230	42484.797074	33.193447
767.017288	42551.819917	33.198464
768.080473	42616.414201	33.203482
768.692969	42684.993912	33.208500
769.909709	42753.650547	33.213517
770.942297	42812.949933	33.218535
771.729486	42881.515712	33.223552
772.478978	42931.062211	33.228570
773.026669	42989.368644	33.233588
774.021333	43056.308786	33.238605
774.952946	43119.318489	33.243623
775.522537	43180.620054	33.248640
776.077000	43231.835761	33.253658
777.035502	43296.024559	33.258676
777.850199	43359.843776	33.263693
778.497866	43411.367967	33.268711
779.103479	43466.314363	33.273728
779.995247	43518.502889	33.278746
780.904011	43572.333419	33.283764
781.369429	43639.863724	33.288781
782.086502	43686.083626	33.293799
782.996109	43751.122600	33.298816
783.503895	43803.030012	33.303834
783.941019	43875.657200	33.308852
784.986706	43934.236488	33.313869
785.513899	44016.445454	33.318887
785.951720	44082.109134	33.323904
786.703348	44140.374203	33.328922
787.425570	44223.122847	33.333940
788.345729	44291.147297	33.338957
789.426212	44360.019894	33.343975
790.072996	44436.569608	33.348992
791.316092	44503.443828	33.354010
791.989371	44584.961666	33.359028
792.626093	44648.173432	33.364045
793.914121	44711.492730	33.369063
794.457030	44789.792995	33.374080
795.540060	44853.214188	33.379098
796.169626	44937.630859	33.384116
796.789956	45000.175673	33.389133
797.921199	45071.073057	33.394151
798.679509	45139.681942	33.399168
799.894136	45206.948565	33.404186
800.521797	45278.892812	33.409204
801.328235	45341.839753	33.414221
802.412874	45400.404189	33.419239
803.007270	45473.650992	33.424256
803.921331	45539.004456	33.429274
804.586408	45604.396869	33.434292
805.511636	45668.895007	33.439309
806.646907	45734.847178	33.444327
807.290244	45804.247736	33.449344
808.263441	45864.696828	33.454362
808.826982	45927.575690	33.459380
809.583380	45994.517491	33.464397
810.481034	46058.837596	33.469415
810.823476	46126.932270	33.474432
811.990912	46188.288220	33.479450
813.074471	46249.138674	33.484468
813.920353	46306.711533	33.489485
815.160270	46377.684704	33.494503
815.359087	46448.864443	33.499520
816.164937	46508.822596	33.504538
816.828841	46584.377496	33.509556
817.674351	46652.174041	33.514573
818.474275	46715.847014	33.519591
818.857161	46789.801591	33.524608
820.054820	46862.933715	33.529626
820.857566	46937.297870	33.534644
821.630331	47002.513111	33.539661
822.616206	47066.518715	33.544679
823.039028	47152.918011	33.549696
823.763604	47215.364205	33.554714
824.357155	47297.309185	33.559732
825.355882	47375.136311	33.564749
826.225370	47447.859605	33.569767
826.893196	47531.957432	33.574784
827.454256	47606.355085	33.579802
828.722162	47693.225886	33.584820
829.223513	47771.138124	33.589837
830.088566	47842.465267	33.594855
830.979469	47928.212636	33.599872
831.844671	48009.561188	33.604890
832.473685	48073.871921	33.609908
833.426541	48137.487133	33.614925
834.328933	48207.158423	33.619943
835.182855	48275.464637	33.624960
836.100848	48342.717220	33.629978
837.273043	48410.328999	33.634996
838.103800	48489.786695	33.640013
839.375503	48548.172034	33.645031
840.115798	48622.671646	33.650048
841.023023	48674.585076	33.655066
841.501833	48743.982315	33.660084
842.289744	48810.421424	33.665101
843.551840	48870.903183	33.670119
843.885792	48947.523252	33.675136
844.373626	49013.054345	33.680154
845.429908	49086.329531	33.685172
846.356390	49159.460663	33.690189
847.103004	49238.124251	33.695207
848.030792	49320.252254	33.700224
848.874414	49388.247072	33.705242
849.650706	49451.368320	33.710260
850.946799	49533.692828	33.715277
851.446380	49600.242385	33.720295
852.604090	49692.294306	33.725312
853.418019	49747.154016	33.730330
854.403983	49830.211164	33.735348
855.413452	49891.601732	33.740365
856.476073	49951.035508	33.745383
856.949271	50029.592530	33.750400
857.696031	50105.045002	33.755418
858.325059	50174.657291	33.760436
859.427672	50247.745501	33.765453
860.402433	50327.940076	33.770471
861.406056	50407.099135	33.775488
862.045606	50484.461318	33.780506
862.913476	50559.478844	33.785524
863.648456	50635.352474	33.790541
864.579653	50699.237599	33.795559
864.960032	50792.148872	33.800576
866.398372	50871.444325	33.805594
867.114189	50941.444032	33.810612
867.623720	51031.982461	33.815629
868.744856	51102.489010	33.820647
869.514409	51193.854425	33.825664
870.337684	51269.248179	33.830682
871.594402	51355.463945	33.835700
872.333284	51437.774443	33.840717
873.149382	51521.104567	33.845735
874.360296	51605.784529	33.850752
874.801657	51673.823407	33.855770
875.696357	51751.555066	33.860788
876.812149	51832.416270	33.865805
877.572515	51910.447777	33.870823
878.592287	51992.710194	33.875840
879.856883	52077.883393	33.880858
880.865778	52137.261564	33.885876
881.801099	52213.254714	33.890893
882.645281	52289.028181	33.895911
883.571015	52359.733489	33.900928
884.644066	52429.549204	33.905946
885.785480	52494.058298	33.910964
886.410349	52562.735610	33.915981
887.557287	52621.372183	33.920999
888.322017	52695.919129	33.926016
888.987074	52766.691562	33.931034
889.686551	52840.774554	33.936052
890.274987	52909.338331	33.941069
891.459236	52975.854299	33.946087
892.500079	53038.887217	33.951104
893.307983	53104.000428	33.956122
894.256366	53166.877235	33.961140
895.280346	53231.457273	33.966157
895.719751	53285.902762	33.971175
896.757606	53354.100480	33.976192
897.426858	53425.563987	33.981210
897.967766	53498.616998	33.986228
898.658602	53581.461435	33.991245
899.355922	53650.915323	33.996263
900.410307	53735.912150	34.001280
900.812320	53808.475185	34.006298
902.014622	53892.702859	34.011316
902.612421	53979.556128	34.016333
903.701248	54061.416420	34.021351
904.696297	54148.316051	34.026368
905.780480	54224.026788	34.031386
906.859221	54310.205248	34.036404
907.358665	54401.391130	34.041421
908.581779	54481.017146	34.046439
909.688197	54579.304306	34.051456
910.396994	54654.233217	34.056474
911.448460	54728.014249	34.061492
912.150224	54813.588771	34.066509
912.807661	54901.492964	34.071527
913.812310	54986.470408	34.076544
915.034258	55077.103455	34.081562
916.134885	55169.869388	34.086580
916.707330	55256.414888	34.091597
918.081701	55326.572021	34.096615
919.388648	55419.496666	34.101632
920.118573	55505.075634	34.106650
920.938738	55571.250604	34.111668
921.601245	55663.681651	34.116685
922.544677	55738.469888	34.121703
923.638347	55826.341249	34.126720
925.037309	55913.994544	34.131738
926.018711	55991.910277	34.136756
926.694299	56071.531948	34.141773
927.532317	56153.603069	34.146791
928.782760	56238.110067	34.151808
929.329533	56323.676191	34.156826
930.287623	56413.039063	34.161844
931.071446	56493.569276	34.166861
931.897757	56579.763643	34.171879
932.969753	56678.020557	34.176896
934.072747	56755.957834	34.181914
935.387042	56839.995030	34.186932
936.173671	56922.260329	34.191949
937.068243	57007.717806	34.196967
938.149075	57084.925466	34.201984
939.105377	57167.215826	34.207002
939.915780	57238.479001	34.212020
940.834245	57325.155360	34.217037
942.377979	57405.747566	34.222055
943.060922	57479.372989	34.227072
943.924127	57562.337406	34.232090
945.055568	57635.058073	34.237108
945.818459	57718.488000	34.242125
946.584751	57793.835554	34.247143
947.998715	57869.443280	34.252160
948.956549	57954.356316	34.257178
949.776632	58028.253210	34.262196
950.766180	58111.617574	34.267213
951.679590	58177.152339	34.272231
952.551087	58251.776091	34.277248
953.378295	58336.799416	34.282266
954.334633	58402.423050	34.287284
955.146384	58475.417542	34.292301
955.994918	58549.602748	34.297319
956.665222	58628.417266	34.302336
957.515753	58706.355869	34.307354
958.570298	58769.787956	34.312372
959.210740	58857.652376	34.317389
960.141416	58938.142608	34.322407
961.073447	59024.955888	34.327424
961.620968	59110.512828	34.332442
962.661120	59201.487278	34.337460
963.476446	59290.604577	34.342477
964.345026	59383.201421	34.347495
965.292282	59473.976152	34.352512
965.942815	59576.506918	34.357530
967.268551	59675.059365	34.362548
968.012351	59773.658489	34.367565
969.221404	59862.868507	34.372583
970.271375	59965.224802	34.377600
971.220812	60066.305939	34.382618
972.421824	60161.759283	34.387636
973.238289	60257.279188	34.392653
974.601492	60351.461088	34.397671
975.506648	60444.910781	34.402688
976.324058	60551.888433	34.407706
977.587947	60641.523185	34.412724
978.921280	60730.634745	34.417741
979.855381	60819.941700	34.422759
981.603489	60905.324387	34.427776
982.291793	60993.011824	34.432794
984.067655	61075.776566	34.437812
984.673186	61149.431507	34.442829
985.832519	61236.040043	34.447847
986.890353	61311.688612	34.452864
987.410932	61390.275842	34.457882
988.100832	61462.355095	34.462900
989.011435	61557.074171	34.467917
990.021203	61641.238726	34.472935
991.024560	61738.235521	34.477952
991.976654	61824.764450	34.482970
993.126489	61918.428540	34.487988
993.882249	61996.329099	34.493005
994.944069	62088.589596	34.498023
996.038495	62181.389754	34.503040
996.715374	62277.857118	34.508058
998.258218	62371.892205	34.513076
998.793826	62463.026945	34.518093
999.731580	62559.410487	34.523111
1000.811645	62644.896872	34.528128
1001.923077	62740.279225	34.533146
1003.101559	62819.743459	34.538164
1004.317704	62917.572682	34.543181
1005.423316	63007.880051	34.548199
1006.331476	63093.477036	34.553216
1007.429277	63174.936373	34.558234
1008.684967	63257.327293	34.563252
1009.742589	63352.137976	34.568269
1011.121002	63436.200613	34.573287
1011.896522	63515.122074	34.578304
1012.175974	63604.705596	34.583322
1013.666747	63698.285362	34.588340
1014.362544	63777.675863	34.593357
1015.398972	63868.098412	34.598375
1016.349817	63954.799564	34.603392
1016.838190	64045.972779	34.608410
1018.143700	64143.590331	34.613428
1019.471015	64232.424246	34.618445
1020.024180	64327.247521	34.623463
1021.437917	64409.573333	34.628480
1021.956619	64492.975684	34.633498
1022.699316	64577.470317	34.638516
1023.882526	64673.526288	34.643533
1024.790929	64758.818739	34.648551
1025.790982	64843.894628	34.653568
1026.641282	64944.422362	34.658586
1027.553171	65040.819521	34.663604
1028.743543	65137.654848	34.668621
1029.386054	65227.896716	34.673639
1030.468939	65317.114390	34.678656
1031.151978	65424.298563	34.683674
1032.555459	65512.264142	34.688692
1033.636922	65621.982840	34.693709
1034.459290	65730.742040	34.698727
1035.862447	65830.148962	34.703744
1036.577092	65927.453899	34.708762
1037.875658	66028.922824	34.713780
1039.557594	66123.520181	34.718797
1040.436853	66229.005804	34.723815
1041.649813	66311.774288	34.728832
1042.983766	66405.717774	34.733850
1044.090441	66491.782954	34.738868
1045.132354	66588.330390	34.743885
1046.075051	66683.469101	34.748903
1047.567538	66770.291905	34.753920
1048.602014	66868.000189	34.758938
1049.638830	66955.882242	34.763956
1050.534801	67039.645811	34.768973
1051.439425	67139.635647	34.773991
1052.618207	67230.301353	34.779008
1053.358299	67334.008773	34.784026
1054.433729	67422.513237	34.789044
1056.100848	67509.216408	34.794061
1057.116789	67602.827597	34.799079
1057.949376	67693.510848	34.804096
1059.062440	67791.045817	34.809114
1059.817813	67884.875881	34.814132
1061.033311	67979.153858	34.819149
1062.225673	68081.464275	34.824167
1063.633106	68164.999963	34.829184
1064.176484	68266.348422	34.834202
1065.359356	68363.608774	34.839220
1066.796315	68446.596258	34.844237
1067.748308	68552.162476	34.849255
1068.909273	68640.410897	34.854272
1069.709938	68737.016668	34.859290
1070.748531	68834.047987	34.864308
1072.199776	68921.644336	34.869325
1072.815750	69024.434467	34.874343
1074.052676	69119.010889	34.879360
1075.067020	69229.768646	34.884378
1076.146951	69313.390703	34.889396
1077.220795	69413.926601	34.894413
1078.564263	69506.974525	34.899431
1079.352829	69601.210924	34.904448
1080.538946	69698.190868	34.909466
1081.502050	69796.725578	34.914484
1082.998911	69889.978955	34.919501
1084.171529	69971.017893	34.924519
1085.449358	70061.747822	34.929536
1086.341382	70149.023791	34.934554
1087.275658	70245.519416	34.939572
1088.505913	70328.697097	34.944589
1089.422373	70437.202003	34.949607
1090.509129	70522.815208	34.954624
1091.358623	70626.848118	34.959642
1092.471259	70728.218925	34.964660
1093.816555	70810.949648	34.969677
1094.814759	70897.027459	34.974695
1095.628767	70981.791772	34.979712
1096.593858	71074.359627	34.984730
1097.622531	71163.156483	34.989748
1098.761680	71244.679523	34.994765
1100.056363	71334.144783	34.999783
1101.391928	71412.370248	35.004800
1101.906080	71503.186071	35.009818
1103.028870	71602.430983	35.014836
1103.922615	71685.146105	35.019853
1104.514927	71795.923479	35.024871
1105.863241	71895.147060	35.029888
1107.030344	71998.680041	35.034906
1107.849470	72097.822111	35.039924
1109.387411	72204.781109	35.044941
1110.328045	72305.133575	35.049959
1111.246203	72415.191574	35.054976
1112.336324	72524.425346	35.059994
1113.459037	72631.260727	35.065012
1114.646202	72724.002474	35.070029
1116.051200	72846.727983	35.075047
1117.047758	72955.686794	35.080064
1118.352851	73055.972717	35.085082
1119.281682	73167.982701	35.090100
1120.356080	73268.343334	35.095117
1121.462966	73378.122648	35.100135
1122.899058	73490.359014	35.105152
1123.621775	73596.285278	35.110170
1124.908769	73722.972310	35.115188
1126.368570	73834.281823	35.120205
1127.333482	73942.578311	35.125223
1128.512786	74049.499258	35.130240
1130.040516	74157.012375	35.135258
1131.157392	74259.827376	35.140276
1133.037837	74349.502994	35.145293
1134.034937	74452.831367	35.150311
1135.350219	74553.615339	35.155328
1136.542586	74653.430843	35.160346
1137.583269	74750.471043	35.165364
1138.897670	74844.897689	35.170381
1139.783506	74953.235914	35.175399
1141.501159	75041.431875	35.180416
1142.855052	75139.919390	35.185434
1143.428511	75232.334736	35.190452
1144.822943	75315.135234	35.195469
1145.573487	75422.343739	35.200487
1146.641439	75519.129138	35.205504
1147.880193	75623.070413	35.210522
1148.971922	75723.931579	35.215540
1150.228364	75815.317931	35.220557
1151.295227	75922.935202	35.225575
1152.486930	76029.013423	35.230592
1153.284581	76124.639698	35.235610
1154.915895	76224.063365	35.240628
1155.972906	76322.626750	35.245645
1156.916593	76419.928743	35.250663
1158.052506	76521.115356	35.255680
1160.028105	76617.548069	35.260698
1160.468874	76723.872572	35.265716
1161.949931	76810.857081	35.270733
1162.794492	76918.538246	35.275751
1164.198092	77016.404164	35.280768
1165.157121	77118.798617	35.285786
1166.062364	77219.973069	35.290804
1167.565705	77328.706068	35.295821
1168.071505	77428.436016	35.300839
1169.539271	77530.081440	35.305856
1170.705859	77624.692820	35.310874
1171.823627	77723.201155	35.315892
1172.877704	77811.053396	35.320909
1174.106151	77917.462635	35.325927
1175.004222	78005.542471	35.330944
1175.807903	78113.817442	35.335962
1177.150128	78213.774766	35.340980
1178.183573	78304.672140	35.345997
1179.304762	78421.804593	35.351015
1180.393357	78530.163541	35.356032
1181.549029	78635.560769	35.361050
1182.573162	78760.614773	35.366068
1184.003557	78864.969320	35.371085
1184.890890	78970.320919	35.376103
1185.844059	79090.244086	35.381120
1187.264042	79194.398807	35.386138
1188.229610	79304.604218	35.391156
1189.516723	79414.316618	35.396173
1190.951028	79546.227407	35.401191
1192.080760	79667.506483	35.406208
1193.215015	79771.581165	35.411226
1194.595309	79891.137270	35.416244
1196.050035	80013.684834	35.421261
1197.406608	80132.548882	35.426279
1198.510731	80247.487334	35.431296
1199.936339	80365.961565	35.436314
1201.114341	80478.989115	35.441332
1202.328662	80591.656735	35.446349
1203.906463	80707.764936	35.451367
1205.087825	80818.854953	35.456384
1206.644496	80922.209389	35.461402
1208.052037	81027.044398	35.466420
1209.264685	81125.942845	35.471437
1210.506390	81235.568145	35.476455
1211.880143	81342.221326	35.481472
1213.650904	81440.362530	35.486490
1214.714712	81547.508171	35.491508
1215.901712	81651.759037	35.496525
1216.877254	81746.186189	35.501543
1217.855888	81851.648510	35.506560
1219.492485	81946.784304	35.511578
1220.535257	82054.771358	35.516596
1221.535027	82152.845013	35.521613
1222.810421	82259.783056	35.526631
1223.821683	82369.740058	35.531648
1225.044343	82481.083626	35.536666
1226.029175	82594.023068	35.541684
1227.346252	82695.951600	35.546701
1228.680335	82822.825399	35.551719
1229.963012	82933.363185	35.556736
1230.842259	83037.261628	35.561754
1231.857621	83155.456717	35.566772
1233.106913	83273.869293	35.571789
1234.263394	83384.327116	35.576807
1235.307713	83512.617506	35.581824
1237.231934	83622.209195	35.586842
1238.372837	83750.105507	35.591860
1239.094160	83856.730358	35.596877
1240.470544	83988.658357	35.601895
1241.633549	84107.239877	35.606912
1243.345344	84227.497709	35.611930
1243.908960	84345.400595	35.616948
1245.555254	84456.014403	35.621965
1246.942079	84571.458641	35.626983
1248.165736	84697.889153	35.632000
1249.963712	84812.408737	35.637018
1251.074713	84918.951547	35.642036
1252.409499	85025.827383	35.647053
1253.327954	85131.982805	35.652071
1254.495112	85232.093743	35.657088
1255.852350	85334.988465	35.662106
1257.004454	85439.423372	35.667124
1258.462468	85535.714038	35.672141
1259.566845	85646.568836	35.677159
1260.330366	85756.311339	35.682176
1261.839971	85854.457743	35.687194
1262.770079	85967.951229	35.692212
1263.655914	86070.174323	35.697229
1265.119175	86184.472683	35.702247
1266.579035	86310.328616	35.707264
1267.818560	86421.634197	35.712282
1268.875002	86545.425086	35.717300
1270.202133	86664.853265	35.722317
1271.512336	86788.466299	35.727335
1272.718742	86913.578634	35.732352
1274.136898	87030.877927	35.737370
1275.451746	87156.443289	35.742388
1276.428630	87281.516894	35.747405
1277.899793	87403.016577	35.752423
1278.783295	87542.754876	35.757440
1280.233956	87657.960705	35.762458
1281.558359	87792.904806	35.767476
1282.933882	87917.716321	35.772493
1284.309074	88051.386464	35.777511
1285.327009	88183.528758	35.782528
1287.110491	88308.379812	35.787546
1288.383502	88430.015969	35.792564
1289.732225	88556.887330	35.797581
1290.857472	88678.877003	35.802599
1292.289634	88818.358540	35.807616
1293.968085	88944.255130	35.812634
1295.346663	89073.037659	35.817652
1296.815951	89186.104847	35.822669
1298.279157	89306.194252	35.827687
1300.107407	89428.685895	35.832704
1301.540377	89540.011205	35.837722
1302.577300	89658.039304	35.842740
1303.676352	89763.714510	35.847757
1305.300158	89892.804602	35.852775
1306.275671	90004.152158	35.857792
1308.048667	90122.827926	35.862810
1309.142523	90238.099345	35.867828
1310.138116	90357.099822	35.872845
1311.289611	90481.069862	35.877863
1312.446668	90608.131895	35.882880
1313.953837	90730.488760	35.887898
1315.339848	90852.877657	35.892916
1316.435210	90976.414905	35.897933
1318.053277	91101.278088	35.902951
1318.973015	91231.776266	35.907968
1320.584615	91356.273973	35.912986
1321.598070	91481.853862	35.918004
1322.882397	91609.736797	35.923021
1324.642305	91736.392914	35.928039
1325.705925	91868.430354	35.933056
1327.445257	91979.045312	35.938074
1328.673998	92109.714647	35.943092
1329.572425	92234.732553	35.948109
1330.985023	92355.830637	35.953127
1332.351232	92483.210219	35.958144
1333.695591	92602.659571	35.963162
1335.183120	92735.369917	35.968180
1336.171278	92866.079952	35.973197
1338.023356	92985.984110	35.978215
1339.376296	93112.886760	35.983232
1340.741291	93233.780278	35.988250
1341.796592	93356.813802	35.993268
1342.774831	93468.693365	35.998285
1344.080854	93577.581766	36.003303
1345.275381	93699.847185	36.008320
1346.774468	93815.652194	36.013338
1348.039511	93939.403229	36.018356
1349.000637	94064.482241	36.023373
1350.695029	94181.031403	36.028391
1351.703392	94303.353550	36.033408
1353.097548	94431.966378	36.038426
1354.929540	94554.921835	36.043444
1356.383854	94668.303386	36.048461
1358.146068	94783.652798	36.053479
1359.342809	94908.559131	36.058496
1360.761183	95019.843460	36.063514
1362.162234	95140.396622	36.068532
1363.745165	95245.052249	36.073549
1365.406236	95364.361641	36.078567
1366.656511	95486.473354	36.083584
1367.949572	95606.550789	36.088602
1369.608096	95726.292938	36.093620
1370.920414	95851.375209	36.098637
1372.590865	95964.106744	36.103655
1373.210540	96077.483919	36.108672
1374.489727	96199.568574	36.113690
1375.885160	96320.368022	36.118708
1377.015778	96451.172459	36.123725
1378.859666	96573.614339	36.128743
1379.911036	96699.349066	36.133760
1381.375356	96831.852447	36.138778
1382.714036	96950.013846	36.143796
1384.135385	97089.281397	36.148813
1385.523080	97211.492539	36.153831
1387.098411	97345.945628	36.158848
1388.327313	97477.943289	36.163866
1390.015624	97603.912075	36.168884
1391.121464	97738.376528	36.173901
1392.747681	97863.291187	36.178919
1393.831081	97987.124582	36.183936
1395.732206	98116.839907	36.188954
1397.097324	98244.763041	36.193972
1398.626174	98381.091234	36.198989
1400.302269	98498.521358	36.204007
1401.689119	98619.216851	36.209024
1403.429002	98754.233436	36.214042
1404.598836	98873.252289	36.219060
1405.944341	99000.915297	36.224077
1407.339204	99122.460804	36.229095
1408.286406	99257.057780	36.234112
1409.689443	99376.929605	36.239130
1411.320797	99508.682892	36.244148
1411.885875	99640.666068	36.249165
1413.861753	99773.672573	36.254183
1415.322072	99913.415478	36.259200
1417.044262	100048.757205	36.264218
1418.282398	100182.919775	36.269236
1419.333795	100321.105381	36.274253
1420.943456	100443.015451	36.279271
1422.301489	100585.477504	36.284288
1423.856745	100708.588738	36.289306
1425.332344	100839.027872	36.294324
1426.694907	100975.507059	36.299341
1428.282970	101107.577877	36.304359
1429.791274	101245.455428	36.309376
1430.706292	101383.501974	36.314394
1432.425475	101513.512886	36.319412
1433.721196	101656.737334	36.324429
1435.149471	101784.652020	36.329447
1436.495546	101909.892239	36.334464
1437.976602	102035.644411	36.339482
1439.392606	102154.573633	36.344500
1440.270014	102282.233691	36.349517
1441.857370	102405.612580	36.354535
1443.396118	102518.996275	36.359552
1444.940956	102651.663263	36.364570
1446.814963	102777.204974	36.369588
1447.897942	102897.773526	36.374605
1449.557337	103017.175126	36.379623
1450.817275	103151.663466	36.384640
1452.292740	103279.348410	36.389658
1454.097818	103406.361288	36.394676
1454.993423	103534.378363	36.399693
1456.655161	103662.568299	36.404711
1458.013536	103802.280302	36.409728
1458.888120	103935.766779	36.414746
1460.866973	104070.261058	36.419764
1462.108123	104217.498988	36.424781
1463.549021	104351.177922	36.429799
1464.864205	104490.367012	36.434816
1466.263270	104640.561818	36.439834
1468.242958	104777.417143	36.444852
1469.233642	104923.023506	36.449869
1470.746312	105067.471513	36.454887
1472.102086	105226.804798	36.459904
1473.790268	105370.034925	36.464922
1475.497361	105514.239040	36.469940
1476.871307	105668.740700	36.474957
1478.295001	105806.041778	36.479975
1479.942795	105960.375353	36.484992
1481.728637	106106.142016	36.490010
1483.177454	106244.962530	36.495028
1484.927902	106397.392834	36.500045
1486.294648	106541.451423	36.505063
1487.569373	106678.741181	36.510080
1488.848218	106830.207073	36.515098
1490.682977	106973.078805	36.520116
1492.187277	107129.443469	36.525133
1493.457916	107284.894205	36.530151
1495.219977	107433.675451	36.535168
1496.722422	107580.468908	36.540186
1498.454407	107726.136759	36.545204
1499.502649	107892.656742	36.550221
1501.092091	108041.289962	36.555239
1502.980086	108184.767120	36.560256
1504.245672	108335.823268	36.565274
1505.663000	108484.117450	36.570292
1506.967905	108653.073869	36.575309
1508.304414	108798.909250	36.580327
1510.018947	108959.446819	36.585344
1511.486161	109114.900571	36.590362
1512.948393	109271.294178	36.595380
1514.648517	109442.209182	36.600397
1516.504456	109586.736970	36.605415
1518.024625	109731.596600	36.610432
1519.458313	109884.434024	36.615450
1521.469228	110032.756549	36.620468
1523.031912	110189.176675	36.625485
1524.571924	110327.200507	36.630503
1525.877910	110477.891897	36.635520
1527.461484	110632.243689	36.640538
1529.480679	110771.069696	36.645556
1530.664268	110914.566275	36.650573
1532.157250	111062.758173	36.655591
1533.883262	111204.649722	36.660608
1535.396850	111335.808200	36.665626
1536.989935	111482.502524	36.670644
1538.273414	111631.845399	36.675661
1540.232896	111762.352693	36.680679
1541.430451	111881.933188	36.685696
1542.653160	112018.009278	36.690714
1543.930114	112158.072247	36.695732
1545.256531	112303.505223	36.700749
1546.400350	112431.947941	36.705767
1548.030892	112572.426735	36.710784
1549.713489	112716.981620	36.715802
1551.568257	112856.779841	36.720820
1552.761798	113003.923068	36.725837
1554.224850	113145.102330	36.730855
1556.040628	113283.678100	36.735872
1557.575228	113434.790298	36.740890
1559.179455	113577.242881	36.745908
1560.499446	113730.571094	36.750925
1562.347331	113876.157549	36.755943
1564.145939	114041.904874	36.760960
1565.577831	114183.524248	36.765978
1567.529968	114324.112000	36.770996
1569.211469	114479.390973	36.776013
1570.505003	114621.566260	36.781031
1572.296201	114764.362199	36.786048
1573.710061	114919.329581	36.791066
1575.383000	115063.831919	36.796084
1577.150211	115221.941685	36.801101
1578.669291	115372.544340	36.806119
1580.270018	115510.718158	36.811136
1581.921407	115672.576718	36.816154
1583.646479	115824.151130	36.821172
1584.697606	115987.169885	36.826189
1586.096325	116143.730188	36.831207
1588.115400	116286.623406	36.836224
1589.210380	116463.272042	36.841242
1590.941266	116614.125829	36.846260
1592.480935	116788.423774	36.851277
1593.851894	116952.779495	36.856295
1595.295347	117117.847625	36.861312
1596.519838	117299.337901	36.866330
1598.250886	117468.104507	36.871348
1600.170117	117653.623274	36.876365
1601.610835	117819.088118	36.881383
1603.000680	117983.737153	36.886400
1604.420574	118180.548835	36.891418
1606.143168	118345.249130	36.896436
1607.749120	118527.320163	36.901453
1609.095709	118706.591183	36.906471
1610.840211	118888.769230	36.911488
1612.440119	119083.439319	36.916506
1614.097122	119271.277331	36.921524
1615.984201	119449.009027	36.926541
1617.725080	119639.854692	36.931559
1619.231137	119812.852648	36.936576
1620.879266	119998.729513	36.941594
1622.849706	120188.337143	36.946612
1624.068907	120377.758198	36.951629
1625.669847	120562.402028	36.956647
1627.433128	120738.370409	36.961664
1629.070751	120934.198343	36.966682
1630.860076	121105.991007	36.971700
1632.700599	121287.937169	36.976717
1633.853960	121471.652879	36.981735
1635.718168	121646.810512	36.986752
1637.303525	121837.386798	36.991770
1639.025533	122025.418378	36.996788
1640.786451	122199.034277	37.001805
1642.071137	122383.177818	37.006823
1643.927833	122568.780818	37.011840
1646.138676	122738.498074	37.016858
1648.098988	122896.292582	37.021876
1649.623256	123051.897552	37.026893
1650.989967	123205.764352	37.031911
1653.048027	123353.549187	37.036928
1654.316281	123522.439717	37.041946
1656.031824	123669.391037	37.046964
1657.213422	123828.401437	37.051981
1658.606675	123998.276715	37.056999
1660.627992	124155.470502	37.062016
1662.148772	124335.501497	37.067034
1663.274046	124506.346720	37.072052
1664.581432	124688.087071	37.077069
1665.876329	124873.699471	37.082087
1667.689837	125055.172415	37.087104
1669.210279	125239.444714	37.092122
1671.456265	125421.384818	37.097140
1673.808300	125594.365323	37.102157
1675.274426	125777.417945	37.107175
1677.128601	125954.486394	37.112192
1678.667209	126145.268165	37.117210
1680.346015	126330.345397	37.122228
1682.203403	126514.025511	37.127245
1683.519492	126702.776588	37.132263
1685.191950	126883.391576	37.137280
1686.599213	127086.897668	37.142298
1688.332056	127277.020135	37.147316
1690.227863	127466.813627	37.152333
1691.764145	127671.089113	37.157351
1693.416606	127866.403116	37.162368
1695.012593	128062.145504	37.167386
1696.841700	128269.905394	37.172404
1698.501491	128466.603983	37.177421
1700.149524	128677.794279	37.182439
1701.849923	128868.804509	37.187456
1703.304765	129093.412184	37.192474
1705.077041	129301.147977	37.197492
1706.183949	129506.235142	37.202509
1707.835510	129726.463729	37.207527
1709.857340	129945.354373	37.212544
1711.308839	130164.702859	37.217562
1712.891981	130390.756555	37.222580
1715.235918	130617.619260	37.227597
1716.547022	130846.141103	37.232615
1718.248021	131060.405540	37.237632
1719.750083	131293.911833	37.242650
1721.573062	131520.022981	37.247668
1723.657058	131741.679174	37.252685
1725.139710	131964.927320	37.257703
1726.924879	132196.034401	37.262720
1728.584274	132428.570707	37.267738
1730.181255	132655.712655	37.272756
1731.856772	132887.551031	37.277773
1733.786776	133110.760803	37.282791
1736.555549	133328.245439	37.287808
1738.851491	133537.823499	37.292826
1740.772597	133750.074796	37.297844
1742.830313	133953.119086	37.302861
1744.816798	134163.661881	37.307879
1746.258315	134357.376030	37.312896
1748.206165	134563.307931	37.317914
1750.064023	134761.628621	37.322932
1752.394264	134948.227997	37.327949
1753.885193	135148.916946	37.332967
1755.801503	135335.265128	37.337984
1757.620114	135532.859363	37.343002
1759.220621	135726.275528	37.348020
1760.865519	135916.348285	37.353037
1762.408029	136109.343675	37.358055
1764.102758	136279.183121	37.363072
1765.631008	136464.949194	37.368090
1766.751076	136650.068932	37.373108
1768.855328	136822.727224	37.378125
1770.146827	137022.211925	37.383143
1771.980949	137197.692735	37.388160
1773.532525	137405.526595	37.393178
1774.671850	137603.565481	37.398196
1776.103757	137808.767591	37.403213
1777.988265	138026.387171	37.408231
1779.629669	138233.703177	37.413248
1781.154322	138453.233521	37.418266
1782.373542	138665.870887	37.423284
1784.379343	138890.391803	37.428301
1785.402918	139128.086956	37.433319
1787.630533	139362.474079	37.438336
1789.190452	139597.029741	37.443354
1790.847699	139834.985174	37.448372
1792.817116	140086.294491	37.453389
1794.195541	140340.501756	37.458407
1796.100417	140579.881811	37.463424
1798.114261	140840.820463	37.468442
1799.453599	141093.032672	37.473460
1801.242571	141343.856367	37.478477
1803.058287	141603.789345	37.483495
1804.901699	141872.222428	37.488512
1806.694206	142130.321641	37.493530
1808.793752	142402.601282	37.498548
1811.210032	142655.453566	37.503565
1812.494877	142918.471336	37.508583
1814.246004	143179.653838	37.513600
1816.304481	143437.160129	37.518618
1818.109673	143700.748357	37.523636
1819.800356	143974.191810	37.528653
1821.656325	144245.034630	37.533671
1823.822963	144504.293767	37.538688
1825.698658	144780.213118	37.543706
1827.308201	145055.121981	37.548724
1829.709954	145319.387415	37.553741
1831.503571	145583.088895	37.558759
1833.267535	145844.422940	37.563776
1835.313442	146111.095919	37.568794
1837.253599	146386.925148	37.573812
1839.274009	146643.400327	37.578829
1840.801345	146920.705518	37.583847
1842.824047	147180.013408	37.588864
1844.420262	147449.086030	37.593882
1846.552531	147728.421043	37.598900
1848.848829	147977.523603	37.603917
1850.804902	148227.848028	37.608935
1852.712440	148492.422448	37.613952
1854.608623	148753.420596	37.618970
1856.569326	149009.282077	37.623988
1858.684833	149263.292921	37.629005
1860.331491	149523.254798	37.634023
1862.121603	149784.211059	37.639040
1864.479766	150035.128790	37.644058
1865.805728	150298.685720	37.649076
1868.217949	150552.072617	37.654093
1870.187139	150809.807289	37.659111
1871.760835	151070.879622	37.664128
1873.279858	151324.789941	37.669146
1875.309329	151591.556637	37.674164
1877.291751	151845.422637	37.679181
1878.961450	152102.372245	37.684199
1880.660834	152368.178593	37.689216
1882.258721	152628.962611	37.694234
1883.758087	152893.875964	37.699252
1885.393080	153137.481925	37.704269
1887.170675	153401.948180	37.709287
1888.631374	153648.020708	37.714304
1890.364993	153906.834684	37.719322
1892.440959	154180.270888	37.724340
1894.304711	154440.044486	37.729357
1895.792943	154702.822758	37.734375
1897.780260	154974.969070	37.739392
1899.565788	155247.985898	37.744410
1901.311539	155529.363093	37.749428
1903.373244	155789.264313	37.754445
1905.424815	156069.047811	37.759463
1907.304067	156338.234148	37.764480
1909.457010	156619.553235	37.769498
1910.718648	156910.546069	37.774516
1912.513036	157198.905783	37.779533
1914.943712	157494.302334	37.784551
1916.230708	157783.873687	37.789568
1918.390204	158075.608426	37.794586
1920.060716	158377.449705	37.799604
1922.228567	158663.790634	37.804621
1924.478561	158962.472448	37.809639
1926.052171	159263.952368	37.814656
1928.096307	159566.452331	37.819674
1929.842055	159877.747266	37.824692
1931.824552	160181.427807	37.829709
1933.861952	160491.055432	37.834727
1935.503110	160812.603828	37.839744
1937.803459	161118.842037	37.844762
1939.405719	161433.201301	37.849780
1941.638545	161740.303640	37.854797
1943.376357	162064.712591	37.859815
1945.401398	162381.613367	37.864832
1947.650960	162695.548025	37.869850
1949.504128	163016.046205	37.874868
1951.557235	163334.381930	37.879885
1953.883208	163650.226410	37.884903
1955.586669	163971.895232	37.889920
1957.530169	164291.522276	37.894938
1959.243882	164615.211324	37.899956
1961.910598	164926.844523	37.904973
1964.120326	165231.465745	37.909991
1965.889128	165550.465801	37.915008
1968.078887	165868.348042	37.920026
1969.906543	166186.745200	37.925044
1972.345558	166488.136868	37.930061
1974.685423	166802.635509	37.935079
1976.297485	167123.102022	37.940096
1977.805668	167441.478523	37.945114
1979.569290	167758.585133	37.950132
1981.643383	168090.906476	37.955149
1983.719800	168402.215629	37.960167
1985.527643	168736.371706	37.965184
1987.892229	169059.637528	37.970202
1989.523726	169374.727701	37.975220
1991.571594	169701.423121	37.980237
1993.659691	170027.174159	37.985255
1995.357713	170354.434845	37.990272
1997.608972	170677.001764	37.995290
1999.126744	170999.887403	38.000308
2001.596996	171334.599879	38.005325
2003.545301	171656.837277	38.010343
2005.283359	172000.529518	38.015360
2007.067570	172324.509474	38.020378
2008.508207	172663.184663	38.025396
2010.680919	173008.413708	38.030413
2012.905268	173347.173103	38.035431
2014.510112	173674.995991	38.040448
2016.911942	173984.995396	38.045466
2019.168040	174307.919785	38.050484
2021.266588	174624.203581	38.055501
2023.945507	174915.814956	38.060519
2025.843089	175231.561027	38.065536
2028.111643	175528.063757	38.070554
2030.116412	175834.703659	38.075572
2031.893538	176137.062754	38.080589
2034.032513	176434.554014	38.085607
2036.220359	176744.076724	38.090624
2038.592696	177041.051311	38.095642
2040.651298	177366.393187	38.100660
2042.328468	177674.475016	38.105677
2044.702676	177980.824079	38.110695
2046.459975	178296.768755	38.115712
2048.085657	178598.207909	38.120730
2049.648285	178934.629931	38.125748
2051.545709	179271.534494	38.130765
2053.806994	179590.554724	38.135783
2055.598929	179941.954815	38.140800
2057.420730	180284.208501	38.145818
2059.053476	180642.569683	38.150836
2061.202801	180981.778120	38.155853
2063.504914	181326.526190	38.160871
2065.366063	181675.788841	38.165888
2067.287923	182019.024011	38.170906
2069.128149	182393.360567	38.175924
2071.271332	182753.301417	38.180941
2073.364533	183117.340560	38.185959
2075.274046	183495.378861	38.190976
2076.957460	183860.322752	38.195994
2079.193363	184240.675240	38.201012
2081.264381	184620.318302	38.206029
2083.524103	184999.806458	38.211047
2085.546543	185379.485379	38.216064
2088.294196	185756.716149	38.221082
2090.464692	186134.215937	38.226100
2092.340393	186501.171492	38.231117
2094.627264	186964.912188	38.236135
2096.261281	187347.782956	38.241152
2098.791228	187729.499691	38.246170
2100.478658	188121.864372	38.251188
2102.315565	188512.175232	38.256205
2104.450373	188895.710166	38.261223
2106.322776	189301.537614	38.266240
2108.497079	189702.544349	38.271258
2110.432239	190106.536141	38.276276
2112.755478	190511.408774	38.281293
2114.827799	190911.267219	38.286311
2116.875309	191322.332465	38.291328
2118.734686	191729.846954	38.296346
2120.998208	192132.499230	38.301364
2123.017059	192541.820492	38.306381
2125.500457	192962.069341	38.311399
2127.478120	193372.619008	38.316416
2129.504759	193780.774712	38.321434
2131.658245	194201.510869	38.326452
2133.903833	194623.504120	38.331469
2135.941726	195017.945419	38.336487
2138.009544	195447.233706	38.341504
2140.536605	195854.911595	38.346522
2143.223688	196246.029511	38.351540
2145.516999	196656.286303	38.356557
2148.418643	197050.649884	38.361575
2150.986066	197446.616074	38.366592
2153.104217	197833.940510	38.371610
2155.422700	198224.791040	38.376628
2156.963516	198602.859525	38.381645
2159.121031	198981.620447	38.386663
2161.125940	199367.823422	38.391680
2163.178193	199725.087149	38.396698
2164.974192	200101.697118	38.401716
2166.754952	200481.155389	38.406733
2168.961658	200852.114752	38.411751
2170.718060	201234.982469	38.416768
2172.471318	201626.767756	38.421786
2174.987286	202019.121119	38.426804
2177.039396	202411.572974	38.431821
2179.174026	202804.165286	38.436839
2180.691117	203205.466024	38.441856
2182.993418	203614.698065	38.446874
2185.139621	204020.602168	38.451892
2186.633251	204445.584506	38.456909
2189.136041	204869.013589	38.461927
2191.336517	205302.270713	38.466944
2192.998837	205737.568555	38.471962
2195.503300	206151.347037	38.476980
2198.080274	206597.859452	38.481997
2200.152126	207030.479774	38.487015
2202.264110	207461.570531	38.492032
2204.658087	207899.426269	38.497050
2207.177977	208347.526126	38.502068
2208.912876	208787.569185	38.507085
2211.278402	209223.272571	38.512103
2213.723935	209671.107048	38.517120
2215.680366	210108.806303	38.522138
2218.329993	210555.873873	38.527156
2220.164554	211029.005924	38.532173
2222.325953	211474.601386	38.537191
2224.320855	211941.054325	38.542208
2226.644828	212395.847379	38.547226
2229.274908	212851.203164	38.552244
2231.154030	213312.849556	38.557261
2233.824797	213764.796230	38.562279
2236.738816	214229.331281	38.567296
2238.856307	214678.824895	38.572314
2241.350270	215129.581468	38.577332
2243.437013	215586.194011	38.582349
2245.741816	216048.692228	38.587367
2247.758215	216518.526741	38.592384
2250.009169	216986.343757	38.597402
2252.660662	217435.020604	38.602420
2254.823555	217890.531343	38.607437
2257.072480	218348.747320	38.612455
2259.385887	218821.637128	38.617472
2261.349804	219289.932787	38.622490
2264.174446	219742.522208	38.627508
2266.331224	220202.760862	38.632525
2268.688214	220665.712286	38.637543
2270.589303	221137.042051	38.642560
2272.847771	221600.796860	38.647578
2275.221655	222066.896510	38.652596
2277.495471	222529.048902	38.657613
2279.653305	222991.829218	38.662631
2281.452558	223477.630778	38.667648
2283.645881	223949.983196	38.672666
2286.212092	224427.917396	38.677684
2288.041746	224915.772286	38.682701
2290.465642	225378.714950	38.687719
2292.851058	225857.693615	38.692736
2295.234617	226346.072086	38.697754
2297.243337	226823.762933	38.702772
2300.058310	227303.741642	38.707789
2302.955217	227770.040121	38.712807
2305.415616	228233.053093	38.717824
2307.772876	228702.560031	38.722842
2310.385502	229127.722386	38.727860
2312.488756	229571.991507	38.732877
2314.878567	230008.162771	38.737895
2316.796861	230453.451059	38.742912
2318.657763	230898.062149	38.747930
2320.946877	231348.474680	38.752948
2322.965275	231800.046846	38.757965
2325.090756	232256.835270	38.762983
2327.525214	232710.476001	38.768000
2329.897660	233168.368495	38.773018
2332.325371	233630.875527	38.778036
2334.027381	234102.005393	38.783053
2336.593292	234570.307558	38.788071
2339.517956	235035.047696	38.793088
2341.850286	235509.024903	38.798106
2344.192819	235972.177982	38.803124
2346.532561	236439.243144	38.808141
2348.947144	236909.420752	38.813159
2351.068974	237385.384555	38.818176
2353.082886	237865.225871	38.823194
2355.603099	238343.260273	38.828212
2357.774681	238841.467865	38.833229
2360.254693	239334.266525	38.838247
2363.072712	239820.940348	38.843264
2365.285493	240313.956800	38.848282
2367.862718	240800.336196	38.853300
2369.913581	241289.311574	38.858317
2372.345134	241785.898607	38.863335
2374.622723	242282.813478	38.868352
2376.795026	242802.987680	38.873370
2379.406366	243288.544146	38.878388
2381.987929	243793.918660	38.883405
2384.338351	244302.503406	38.888423
2387.109464	244812.774321	38.893440
2389.003261	245312.104886	38.898458
2391.756013	245820.293204	38.903476
2394.242763	246330.426867	38.908493
2396.884057	246837.080404	38.913511
2398.945493	247341.079376	38.918528
2401.142110	247869.493274	38.923546
2403.956032	248367.809221	38.928564
2406.496220	248889.130218	38.933581
2408.878610	249397.188796	38.938599
2411.250502	249913.325455	38.943616
2413.473422	250437.917269	38.948634
2415.802434	250951.644201	38.953652
2418.019794	251471.457983	38.958669
2420.610816	251987.604839	38.963687
2424.418923	252480.546466	38.968704
2427.066319	252981.516304	38.973722
2430.217948	253493.455758	38.978740
2432.001661	254000.500589	38.983757
2434.333341	254504.181574	38.988775
2436.633326	254998.594178	38.993792
2438.691259	255522.660707	38.998810
2441.228048	256024.068990	39.003828
2443.152418	256546.120276	39.008845
2445.440140	257055.768047	39.013863
2447.853366	257577.662975	39.018880
2450.061870	258103.880395	39.023898
2452.305994	258621.250621	39.028916
2454.648714	259155.342391	39.033933
2456.516846	259688.007061	39.038951
2459.026456	260226.970463	39.043968
2460.854861	260772.514513	39.048986
2463.705228	261305.450884	39.054004
2465.798934	261865.985426	39.059021
2468.419752	262405.327811	39.064039
2470.796306	262931.065898	39.069056
2473.138706	263470.624232	39.074074
2475.676294	263986.146906	39.079092
2477.741658	264513.602136	39.084109
2480.454379	265053.933048	39.089127
2482.737118	265590.111807	39.094144
2485.060590	266135.806080	39.099162
2487.298759	266676.380108	39.104180
2489.625645	267212.772010	39.109197
2492.051932	267769.515245	39.114215
2494.729770	268319.434753	39.119232
2497.046674	268884.646297	39.124250
2499.532409	269442.208744	39.129268
2501.918037	270011.263369	39.134285
2504.831174	270576.727493	39.139303
2507.104318	271151.786463	39.144320
2509.192720	271728.318178	39.149338
2511.634405	272306.772178	39.154356
2514.609727	272889.355268	39.159373
2517.016295	273474.105518	39.164391
2519.750644	274052.934092	39.169408
2521.898796	274661.843447	39.174426
2524.226951	275244.257185	39.179444
2526.455071	275844.916962	39.184461
2529.808811	276455.022294	39.189479
2532.849354	277053.286445	39.194496
2535.112059	277659.489051	39.199514
2537.307613	278250.206149	39.204532
2540.317477	278857.248250	39.209549
2542.747186	279456.198606	39.214567
2545.935769	280049.007546	39.219584
2548.203688	280661.585256	39.224602
2551.622339	281254.425037	39.229620
2555.176554	281828.345544	39.234637
2557.943978	282418.433086	39.239655
2560.959441	282994.180406	39.244672
2563.912960	283569.170913	39.249690
2566.487901	284130.401570	39.254708
2569.444936	284702.004932	39.259725
2571.741340	285270.354499	39.264743
2574.365153	285840.629061	39.269760
2576.658473	286420.472540	39.274778
2579.293508	286987.510825	39.279796
2581.511366	287567.660843	39.284813
2584.562935	288142.165956	39.289831
2587.200569	288717.238285	39.294848
2589.148363	289291.016336	39.299866
2591.451899	289878.546815	39.304884
2594.095446	290455.862515	39.309901
2596.674769	291044.735792	39.314919
2599.142398	291617.066202	39.319936
2601.841225	292203.624774	39.324954
2604.679486	292792.999754	39.329972
2607.383321	293372.310150	39.334989
2610.349272	293958.632538	39.340007
2612.929334	294554.301773	39.345024
2615.341340	295134.351451	39.350042
2618.207648	295708.789929	39.355060
2621.187879	296272.110171	39.360077
2623.797505	296857.494387	39.365095
2626.228692	297427.210514	39.370112
2628.920661	298016.175186	39.375130
2631.184892	298587.175050	39.380148
2633.395285	299179.249022	39.385165
2636.069671	299762.003575	39.390183
2638.772484	300351.246587	39.395200
2641.113578	300950.770340	39.400218
2643.318631	301536.447729	39.405236
2645.720930	302114.218392	39.410253
2647.949251	302695.944681	39.415271
2650.691132	303256.819355	39.420288
2653.118806	303835.176594	39.425306
2655.604819	304413.061431	39.430324
2658.227707	304997.213925	39.435341
2660.566191	305593.817002	39.440359
2663.361058	306179.985407	39.445376
2666.185933	306768.629982	39.450394
2668.468901	307375.069664	39.455412
2671.170994	307977.147020	39.460429
2673.993857	308580.467424	39.465447
2676.441440	309188.128490	39.470464
2679.162801	309807.389835	39.475482
2682.241115	310412.348504	39.480500
2684.923066	311026.524006	39.485517
2687.817139	311647.359262	39.490535
2690.879081	312254.150030	39.495552
2693.906065	312864.212527	39.500570
2696.329888	313485.274445	39.505588
2699.590627	314088.330385	39.510605
2702.317150	314716.181281	39.515623
2705.406389	315317.420479	39.520640
2708.379773	315929.405039	39.525658
2711.104892	316536.927956	39.530676
2714.228083	317144.253824	39.535693
2716.698443	317747.358786	39.540711
2720.002282	318356.847863	39.545728
2722.542396	318967.995363	39.550746
2724.956457	319573.824819	39.555764
2727.659881	320190.563428	39.560781
2730.150588	320809.711686	39.565799
2732.633934	321421.975342	39.570816
2735.049953	322059.717523	39.575834
2737.777878	322684.993215	39.580852
2741.045690	323308.348630	39.585869
2743.418353	323945.459993	39.590887
2746.098321	324576.728538	39.595904
2748.856608	325222.260468	39.600922
2751.836574	325852.879155	39.605940
2754.776376	326504.959561	39.610957
2757.449429	327149.535429	39.615975
2759.971679	327778.419291	39.620992
2762.951665	328420.643498	39.626010
2766.049699	329066.213288	39.631028
2769.424514	329693.386522	39.636045
2772.109396	330328.623324	39.641063
2774.979944	330966.383227	39.646080
2777.987853	331593.151705	39.651098
2780.543528	332230.356246	39.656116
2783.580223	332864.786267	39.661133
2786.036031	333511.954772	39.666151
2788.278565	334146.030330	39.671168
2791.359422	334787.803207	39.676186
2794.009638	335435.796203	39.681204
2796.922970	336086.704812	39.686221
2799.929319	336728.607957	39.691239
2802.794436	337365.119021	39.696256
2805.317267	338011.488503	39.701274
2808.041529	338658.398515	39.706292
2810.865308	339298.915060	39.711309
2813.458674	339957.109108	39.716327
2815.995850	340614.133053	39.721344
2818.838032	341268.408921	39.726362
2821.255686	341933.898082	39.731380
2824.543171	342582.525881	39.736397
2826.746909	343252.689790	39.741415
2829.830857	343893.944672	39.746432
2832.424793	344522.938774	39.751450
2835.077774	345163.171916	39.756468
2838.019916	345806.391165	39.761485
2840.722729	346443.422536	39.766503
2843.802715	347073.130684	39.771520
2846.665609	347705.092296	39.776538
2849.206970	348343.431341	39.781556
2852.116168	348984.464784	39.786573
2854.543909	349635.044023	39.791591
2856.868074	350295.033555	39.796608
2859.911926	350950.714125	39.801626
2862.483196	351630.263267	39.806644
2865.647824	352291.856319	39.811661
2868.728319	352952.637532	39.816679
2871.650747	353621.644172	39.821696
2874.511283	354304.336883	39.826714
2877.380115	354990.486837	39.831732
2880.428677	355665.210967	39.836749
2882.906690	356347.056964	39.841767
2885.929162	357036.839445	39.846784
2889.483690	357722.974777	39.851802
2892.619396	358405.180147	39.856820
2895.600178	359085.822820	39.861837
2898.056101	359783.642089	39.866855
2900.962123	360467.332639	39.871872
2904.110893	361165.468499	39.876890
2906.507512	361866.721417	39.881908
2909.908891	362565.773848	39.886925
2912.422324	363277.417927	39.891943
2915.616871	363993.754390	39.896960
2918.465679	364698.722358	39.901978
2921.278098	365409.736106	39.906996
2924.310892	366114.894676	39.912013
2927.134109	366837.478826	39.917031
2930.003931	367559.809531	39.922048
2933.065235	368291.569763	39.927066
2936.267698	369011.911448	39.932084
2939.542801	369726.826186	39.937101
2942.084011	370460.157146	39.942119
2945.341974	371176.583422	39.947136
2948.619015	371903.579529	39.952154
2951.555771	372631.623062	39.957172
2954.765341	373353.169540	39.962189
2957.785199	374074.929311	39.967207
2960.691279	374796.054394	39.972224
2963.669584	375516.921151	39.977242
2966.614435	376244.031384	39.982260
2969.821179	376954.412141	39.987277
2973.257541	377674.440675	39.992295
2976.380035	378399.033025	39.997312
2979.554296	379115.694317	40.002330
2982.077635	379840.796505	40.007348
2984.848443	380561.534204	40.012365
2988.023244	381287.837577	40.017383
2990.966394	382007.875398	40.022400
2993.779830	382726.115199	40.027418
2996.285909	383463.580584	40.032436
2999.709700	384195.006392	40.037453
3002.318852	384928.792039	40.042471
3005.163681	385665.356253	40.047488
3008.163408	386410.864955	40.052506
3011.026637	387146.420918	40.057524
3014.143358	387889.968427	40.062541
3016.448560	388649.471450	40.067559
3019.850764	389393.588117	40.072576
3022.540806	390134.653582	40.077594
3025.559874	390888.963550	40.082612
3028.785301	391637.040525	40.087629
3031.929268	392367.536764	40.092647
3034.792741	393085.143053	40.097664
3037.386452	393810.921914	40.102682
3040.435803	394532.962611	40.107700
3043.052309	395271.503542	40.112717
3046.112474	396008.585679	40.117735
3048.650614	396752.054526	40.122752
3051.873773	397489.875370	40.127770
3054.424289	398251.317571	40.132788
3057.498157	398998.732761	40.137805
3060.236014	399762.577189	40.142823
3063.124965	400534.370725	40.147840
3066.330438	401294.194450	40.152858
3069.253877	402077.117393	40.157876
3072.644409	402856.145001	40.162893
3075.630722	403638.599940	40.167911
3078.881160	404426.199680	40.172928
3081.673724	405208.984964	40.177946
3084.698576	406017.161783	40.182964
3088.657671	406799.254808	40.187981
3091.947194	407582.993351	40.192999
3095.093456	408387.574069	40.198016
3098.720565	409175.656755	40.203034
3101.280749	409976.475980	40.208052
3104.610990	410781.750355	40.213069
3107.742865	411579.942902	40.218087
3111.039426	412395.484013	40.223104
3114.587634	413176.959146	40.228122
3117.616212	413974.472567	40.233140
3120.321636	414786.828327	40.238157
3123.848483	415594.017639	40.243175
3126.266636	416417.282208	40.248192
3129.645810	417235.964843	40.253210
3132.365422	418064.631670	40.258228
3135.777622	418880.918695	40.263245
3139.113413	419711.144215	40.268263
3141.964822	420546.722109	40.273280
3145.717494	421359.268517	40.278298
3148.786500	422193.431312	40.283316
3152.186888	423025.283837	40.288333
3155.508878	423848.974017	40.293351
3158.682716	424683.221415	40.298368
3162.119443	425502.731337	40.303386
3165.348447	426329.419577	40.308404
3168.778157	427158.873777	40.313421
3172.052370	427984.020834	40.318439
3175.490795	428806.732342	40.323456
3178.799969	429629.985984	40.328474
3181.332139	430457.066825	40.333492
3184.497501	431290.079882	40.338509
3187.711447	432117.288174	40.343527
3191.112114	432956.157902	40.348544
3194.686960	433779.651219	40.353562
3197.656119	434619.678728	40.358580
3200.897142	435442.748988	40.363597
3204.199149	436268.250642	40.368615
3207.330850	437093.793785	40.373632
3210.810745	437924.451414	40.378650
3213.962445	438759.772181	40.383668
3216.907207	439584.933139	40.388685
3220.108358	440422.395778	40.393703
3223.006681	441260.676524	40.398720
3226.045186	442100.312381	40.403738
3229.527019	442935.648756	40.408756
3232.489275	443782.848204	40.413773
3235.756150	444623.294175	40.418791
3238.695040	445476.581704	40.423808
3241.792314	446307.885746	40.428826
3244.692503	447131.859754	40.433844
3247.778700	447951.626495	40.438861
3250.735838	448774.911143	40.443879
3253.705374	449586.542304	40.448896
3256.814444	450414.778048	40.453914
3259.980501	451253.468849	40.458932
3262.629089	452087.454854	40.463949
3266.131069	452929.144876	40.468967
3269.335826	453793.357063	40.473984
3272.450404	454639.821974	40.479002
3275.485229	455511.144769	40.484020
3278.470425	456380.110047	40.489037
3281.537512	457254.066735	40.494055
3285.121852	458149.147494	40.499072
3288.069453	459029.291833	40.504090
3291.320701	459931.751040	40.509108
3294.551530	460820.389473	40.514125
3298.063248	461721.250538	40.519143
3301.095850	462631.826542	40.524160
3304.643675	463550.295980	40.529178
3307.701624	464473.887501	40.534196
3310.911125	465401.440807	40.539213
3314.206883	466328.778079	40.544231
3317.448679	467273.727815	40.549248
3320.643719	468217.521474	40.554266
3323.913556	469167.504150	40.559284
3327.259983	470123.573402	40.564301
3330.692859	471075.589435	40.569319
3334.104488	472040.665174	40.574336
3337.572741	472990.899961	40.579354
3341.152453	473959.264824	40.584372
3344.348980	474928.791040	40.589389
3348.039844	475883.863372	40.594407
3351.487839	476857.771779	40.599424
3355.222428	477823.107109	40.604442
3358.616504	478795.544513	40.609460
3361.789537	479772.694810	40.614477
3365.596456	480738.194294	40.619495
3368.814994	481715.922712	40.624512
3372.590347	482681.358032	40.629530
3376.299268	483647.600664	40.634548
3379.616569	484627.399066	40.639565
3382.805385	485596.372747	40.644583
3385.772828	486581.090061	40.649600
3389.284536	487556.943822	40.654618
3392.775139	488546.441212	40.659636
3396.180184	489534.074260	40.664653
3399.492893	490514.253011	40.669671
3403.076714	491509.990277	40.674688
3406.613219	492492.624893	40.679706
3410.089472	493476.715396	40.684724
3413.193378	494466.993035	40.689741
3417.290615	495450.051106	40.694759
3420.622208	496441.118587	40.699776
3424.309762	497407.746569	40.704794
3427.990019	498397.822847	40.709812
3431.359955	499386.571769	40.714829
3434.842169	500363.205803	40.719847
3438.284013	501338.924968	40.724864
3441.411603	502314.174463	40.729882
3445.596381	503295.736174	40.734900
3448.883013	504270.778379	40.739917
3453.042808	505233.038458	40.744935
3456.572345	506198.552122	40.749952
3460.319093	507160.545262	40.754970
3463.872108	508114.202234	40.759988
3467.109238	509072.321360	40.765005
3470.723223	510008.096908	40.770010
3473.855513	510924.681995	40.775015
3476.684489	511784.021554	40.780020
3479.866723	512601.806042	40.785024
3482.741903	513356.716998	40.790029
3485.897683	514055.731515	40.795034
3488.807186	514702.922708	40.800039
3491.068215	515296.394275	40.805044
3493.511616	515835.822170	40.810048
3495.273888	516330.067805	40.815053
3497.433431	516756.688209	40.820058
3499.516013	517175.847255	40.825063
3500.920989	517534.865733	40.830068
3503.157635	517854.531684	40.835072
3504.136255	518127.360688	40.840077
3506.295227	518364.215629	40.845082
3507.245367	518552.668388	40.850087
3508.708864	518714.477838	40.855092
3509.997326	518838.916133	40.860096
3510.845214	518954.400394	40.865101
3512.064122	519017.259928	40.870106
3512.647879	519071.095835	40.875111
3513.265623	519097.106208	40.880116
3514.190876	519091.922331	40.885120
3514.383283	519073.244836	40.890125
3515.369250	519029.546790	40.895130
3515.326379	518975.273697	40.900135
3516.389830	518902.281272	40.905140
3516.723048	518815.794179	40.910144
3516.939758	518721.462262	40.915149
3517.486178	518595.174896	40.920154
3517.994826	518470.253067	40.925159
3518.238900	518336.903821	40.930164
3518.628740	518177.321545	40.935168
3518.557325	518020.430119	40.940173
3518.709373	517847.725902	40.945178
3518.854097	517671.341157	40.950183
3518.507271	517485.806589	40.955188
3518.936625	517310.028155	40.960192
3518.649092	517121.102264	40.965197
3518.879449	516921.810218	40.970202
3518.871755	516734.347651	40.975207
3518.749482	516528.198950	40.980212
3519.218118	516321.854384	40.985216
3518.823828	516109.944713	40.990221
3518.991807	515895.776630	40.995226
3518.808108	515683.323512	41.000231
3518.720714	515472.868611	41.005236
3518.402071	515257.153140	41.010240
3518.416647	515053.078385	41.015245
3518.670318	514833.334975	41.020250
3518.480508	514625.252558	41.025255
3518.445460	514394.758272	41.030260
3518.527022	514171.905348	41.035264
3518.425374	513950.690710	41.040269
3518.091686	513727.542334	41.045274
3517.948085	513516.058029	41.050279
3517.563291	513289.532479	41.055284
3517.384663	513070.433424	41.060288
3517.258635	512865.692862	41.065293
3517.326455	512631.926312	41.070298
3517.417845	512415.598580	41.075303
3517.197459	512207.585524	41.080308
3517.006025	511990.538851	41.085312
3516.476509	511782.063308	41.090317
3516.677232	511566.108798	41.095322
3516.588460	511361.037795	41.100327
3516.501832	511151.677101	41.105332
3516.176024	510933.727232	41.110336
3515.917259	510726.555394	41.115341
3515.900454	510528.521090	41.120346
3515.895582	510332.801945	41.125351
3515.364326	510128.689520	41.130356
3515.625693	509930.200044	41.135360
3515.490279	509732.021677	41.140365
3515.166616	509534.222847	41.145370
3514.996165	509341.541684	41.150375
3514.911851	509145.011433	41.155380
3514.892690	508957.798884	41.160384
3514.466462	508762.678273	41.165389
3514.047995	508571.235655	41.170394
3514.307105	508392.092649	41.175399
3513.777818	508204.999945	41.180404
3513.956150	508028.588573	41.185408
3513.681608	507851.236688	41.190413
3513.269991	507667.044056	41.195418
3513.796683	507492.034563	41.200423
3513.575137	507316.029639	41.205428
3513.382601	507140.471997	41.210432
3513.169608	506964.814484	41.215437
3513.282867	506792.887277	41.220442
3513.164463	506620.035609	41.225447
3512.570337	506465.768981	41.230452
3512.928751	506290.468228	41.235456
3512.463122	506115.697117	41.240461
3512.560335	505957.533982	41.245466
3512.205175	505790.459964	41.250471
3512.156020	505622.226530	41.255476
3512.041584	505467.622223	41.260480
3511.770593	505318.085453	41.265485
3511.793139	505156.545027	41.270490
3511.646920	505000.931643	41.275495
3511.816749	504845.015136	41.280500
3511.464161	504698.107996	41.285504
3511.093144	504554.027483	41.290509
3511.460266	504404.936847	41.295514
3510.822065	504256.808339	41.300519
3510.538157	504117.401941	41.305524
3510.637233	503986.057552	41.310528
3510.146476	503835.379097	41.315533
3510.621878	503705.335833	41.320538
3510.045402	503573.386443	41.325543
3510.286167	503442.267317	41.330548
3510.150869	503301.467601	41.335552
3509.964691	503186.507895	41.340557
3509.895931	503052.254664	41.345562
3509.858885	502922.637280	41.350567
3509.872787	502804.565528	41.355572
3509.486319	502667.835296	41.360576
3509.573699	502554.644469	41.365581
3509.549925	502430.772837	41.370586
3509.071714	502304.750662	41.375591
3508.953680	502188.763231	41.380596
3508.965996	502073.864704	41.385600
3508.974039	501960.530196	41.390605
3509.037399	501832.552608	41.395610
3508.809617	501717.032624	41.400615
3508.580710	501610.746343	41.405620
3508.821363	501495.555393	41.410624
3508.319452	501385.525305	41.415629
3508.947542	501280.818964	41.420634
3508.531222	501178.494763	41.425639
3508.260639	501063.935038	41.430644
3508.647288	500960.424619	41.435648
3508.087084	500858.776584	41.440653
3508.000006	500741.965348	41.445658
3508.412307	500651.720890	41.450663
3507.824543	500541.495913	41.455668
3507.919533	500428.791975	41.460672
3507.692604	500336.878745	41.465677
3508.115996	500234.921897	41.470682
3508.013204	500138.193806	41.475687
3507.805091	500037.444112	41.480692
3507.658081	499938.400101	41.485696
3507.663864	499841.804552	41.490701
3507.802587	499746.348439	41.495706
3507.605065	499659.321752	41.500711
3507.535026	499556.427589	41.505716
3507.563652	499471.736615	41.510720
3506.987275	499368.415233	41.515725
3506.970150	499273.131691	41.520730
3507.035653	499184.496692	41.525735
3506.848661	499100.846522	41.530740
3507.174890	499015.198134	41.535744
3506.377373	498927.452932	41.540749
3506.804282	498846.380727	41.545754
3507.100704	498762.754344	41.550759
3506.783349	498685.027226	41.555764
3506.948819	498589.307053	41.560768
3506.821467	498516.394776	41.565773
3506.685806	498426.070444	41.570778
3506.718854	498344.753925	41.575783
3506.583893	498264.371614	41.580788
3506.564859	498188.614366	41.585792
3506.639966	498106.078623	41.590797
3506.543638	498019.985452	41.595802
3506.282758	497942.750355	41.600807
3506.066731	497870.050566	41.605812
3506.317740	497788.242784	41.610816
3506.369333	497726.554584	41.615821
3506.343701	497635.198775	41.620826
3506.291481	497553.386399	41.625831
3506.317681	497487.511687	41.630836
3506.021629	497409.067847	41.635840
3505.921810	497337.811150	41.640845
3506.059481	497256.674245	41.645850
3505.936977	497182.795552	41.650855
3506.263997	497123.484851	41.655860
3506.427181	497039.314166	41.660864
3505.976293	496971.239916	41.665869
3505.778484	496894.393329	41.670874
3505.868732	496817.350083	41.675879
3505.817287	496754.058556	41.680884
3505.540333	496678.434637	41.685888
3505.684215	496627.630821	41.690893
3505.831415	496550.123013	41.695898
3505.731044	496486.080770	41.700903
3505.258844	496425.730620	41.705908
3505.483617	496355.377780	41.710912
3505.115832	496292.133502	41.715917
3505.393222	496224.750159	41.720922
3505.431119	496179.110254	41.725927
3505.221820	496112.155495	41.730932
3505.613238	496037.484382	41.735936
3505.190724	495982.475637	41.740941
3504.926200	495913.408379	41.745946
3505.341572	495851.908151	41.750951
3505.113177	495809.185977	41.755956
3505.250772	495736.925475	41.760960
3504.985588	495696.227966	41.765965
3504.918070	495625.816186	41.770970
3505.114545	495565.812815	41.775975
3504.897614	495515.869052	41.780980
3504.781058	495452.784028	41.785984
3504.860686	495400.471528	41.790989
3504.434713	495336.676917	41.795994
3504.713662	495277.517760	41.800999
3504.752599	495233.288315	41.806004
3505.046401	495173.217731	41.811008
3505.263229	495122.245959	41.816013
3505.077903	495064.066908	41.821018
3504.720853	495007.277423	41.826023
3504.535484	494962.274330	41.831028
3504.896120	494908.149421	41.836032
3504.694218	494859.564194	41.841037
3504.610056	494805.861521	41.846042
3504.752798	494756.465055	41.851047
3504.700868	494695.891012	41.856052
3504.915533	494625.683011	41.861056
3504.902746	494577.572289	41.866061
3504.762316	494522.968613	41.871066
3504.866455	494476.606372	41.876071
3504.552514	494424.351686	41.881076
3504.938621	494362.042082	41.886080
3504.646396	494316.094426	41.891085
3504.544681	494262.594473	41.896090
3504.620235	494220.173842	41.901095
3504.551477	494163.588711	41.906100
3504.732747	494105.197408	41.911104
3504.647043	494057.197329	41.916109
3504.609866	494002.020318	41.921114
3504.974546	493949.405930	41.926119
3504.272514	493904.581018	41.931124
3504.566663	493849.048956	41.936128
3504.243943	493799.519803	41.941133
3504.738497	493753.296517	41.946138
3504.701054	493696.906699	41.951143
3504.346969	493653.390080	41.956148
3504.428836	493592.235363	41.961152
3504.490752	493551.784024	41.966157
3504.332343	493492.130471	41.971162
3504.580114	493455.184197	41.976167
3504.262270	493405.501511	41.981172
3504.564267	493349.108052	41.986176
3504.073294	493304.500944	41.991181
3504.240002	493266.506533	41.996186
3504.261297	493227.019949	42.001191
3504.267596	493177.387045	42.006196
3504.242957	493111.096925	42.011200
3504.024339	493082.856189	42.016205
3504.041163	493042.713437	42.021210
3503.635933	492990.669907	42.026215
3503.873085	492951.401461	42.031220
3503.923975	492905.951479	42.036224
3503.686621	492877.662780	42.041229
3503.884742	492836.178489	42.046234
3503.663397	492791.578387	42.051239
3503.476953	492761.817291	42.056244
3503.978614	492709.227726	42.061248
3503.624396	492683.430949	42.066253
3503.543757	492645.372471	42.071258
3503.661032	492598.043019	42.076263
3503.690257	492564.511543	42.081268
3503.938389	492527.714408	42.086272
3503.351070	492492.561968	42.091277
3503.389543	492463.219713	42.096282
3504.146285	492424.020514	42.101287
3503.778995	492381.613097	42.106292
3503.906228	492346.652080	42.111296
3503.663597	492300.993477	42.116301
3503.792999	492258.205461	42.121306
3503.844037	492227.295495	42.126311
3503.550677	492186.239346	42.131316
3503.783534	492152.069339	42.136320
3503.961598	492112.302961	42.141325
3503.574211	492076.058061	42.146330
3503.604210	492030.507695	42.151335
3503.393648	491992.265805	42.156340
3503.806890	491964.682054	42.161344
3503.636224	491933.906974	42.166349
3503.760577	491895.107776	42.171354
3503.898453	491852.822235	42.176359
3503.593253	491823.229244	42.181364
3503.893478	491785.210312	42.186368
3503.600377	491734.912306	42.191373
3503.543862	491702.705126	42.196378
3503.649150	491664.514244	42.201383
3503.770319	491628.593092	42.206388
3504.205031	491586.866561	42.211392
3503.898406	491546.164199	42.216397
3503.884652	491507.839958	42.221402
3504.006382	491462.071616	42.226407
3503.729693	491428.686207	42.231412
3503.516413	491384.535142	42.236416
3503.727612	491357.032219	42.241421
3503.615957	491311.198744	42.246426
3503.679603	491277.760041	42.251431
3503.569198	491243.388909	42.256436
3503.547819	491204.610613	42.261440
3503.715350	491166.711767	42.266445
3503.149652	491135.441061	42.271450
3503.692906	491084.303778	42.276455
3503.396851	491061.726995	42.281460
3504.077679	491023.394434	42.286464
3503.653582	490982.910822	42.291469
3503.710918	490949.876357	42.296474
3503.455726	490911.891160	42.301479
3503.533865	490877.388860	42.306484
3503.528429	490832.900851	42.311488
3503.627216	490799.859608	42.316493
3503.569260	490767.044677	42.321498
3503.774559	490724.291000	42.326503
3503.595944	490684.980355	42.331508
3503.674451	490651.487456	42.336512
3503.912548	490620.797586	42.341517
3503.667309	490582.103028	42.346522
3503.757204	490547.648646	42.351527
3503.525245	490516.425721	42.356532
3503.732697	490470.237044	42.361536
3503.771379	490437.860857	42.366541
3503.318613	490397.127640	42.371546
3503.842099	490361.090372	42.376551
3503.685374	490324.249872	42.381556
3503.743620	490283.285329	42.386560
3503.519051	490248.626701	42.391565
3503.323796	490211.185920	42.396570
3503.509156	490175.150328	42.401575
3503.255973	490141.000910	42.406580
3503.405626	490107.445237	42.411584
3503.549469	490082.021005	42.416589
3503.476327	490043.803298	42.421594
3503.706188	490010.386431	42.426599
3503.526261	489979.810816	42.431604
3503.761013	489941.847945	42.436608
3503.707145	489903.475382	42.441613
3503.498447	489851.036918	42.446618
3503.552367	489823.959700	42.451623
3503.053509	489796.008921	42.456628
3503.834092	489753.617502	42.461632
3503.638139	489712.337463	42.466637
3503.433696	489674.947289	42.471642
3503.673561	489640.720021	42.476647
3503.244339	489607.000812	42.481652
3503.719934	489574.251780	42.486656
3503.563063	489544.681747	42.491661
3503.313810	489504.419486	42.496666
3503.713907	489469.964889	42.501671
3503.128964	489438.794674	42.506676
3503.716410	489399.614002	42.511680
3503.693726	489370.426773	42.516685
3503.474208	489331.775524	42.521690
3503.327039	489295.890600	42.526695
3503.183502	489261.469625	42.531700
3503.625793	489223.775688	42.536704
3503.605905	489203.829846	42.541709
3503.714514	489163.359484	42.546714
3503.286449	489120.346325	42.551719
3503.027762	489087.609503	42.556724
3503.356886	489049.377201	42.561728
3503.389699	489030.483518	42.566733
3503.396774	488993.260770	42.571738
3503.424256	488965.832608	42.576743
3503.396646	488936.897836	42.581748
3503.945138	488895.348221	42.586752
3503.730798	488862.048462	42.591757
3503.571076	488816.366441	42.596762
3503.755331	488779.923679	42.601767
3503.544471	488742.279686	42.606772
3503.707013	488709.122966	42.611776
3503.471836	488682.593757	42.616781
3503.118264	488640.678768	42.621786
3503.570446	488604.143387	42.626791
3503.324611	488573.625706	42.631796
3503.404029	488538.309805	42.636800
3503.235787	488505.305128	42.641805
3503.318617	488466.655141	42.646810
3503.417508	488443.002879	42.651815
3503.370360	488406.898272	42.656820
3503.453015	488362.490337	42.661824
3503.353539	488333.313072	42.666829
3503.191976	488300.912991	42.671834
3503.152735	488268.190766	42.676839
3503.073360	488236.333332	42.681844
3503.113939	488209.760390	42.686848
3503.419650	488189.560527	42.691853
3502.989859	488151.747118	42.696858
3503.050754	488123.807173	42.701863
3502.897575	488096.456069	42.706868
3503.362279	488062.796362	42.711872
3503.341356	488035.323554	42.716877
3503.399249	488001.171433	42.721882
3503.311614	487966.637821	42.726887
3503.377480	487947.081054	42.731892
3503.053813	487911.674908	42.736896
3502.758794	487880.052320	42.741901
3503.132461	487849.588313	42.746906
3503.316024	487825.871413	42.751911
3502.922447	487794.162968	42.756916
3503.023792	487762.983541	42.761920
3503.083524	487743.477977	42.766925
3502.967016	487709.099802	42.771930
3503.333886	487679.141599	42.776935
3503.083841	487648.319671	42.781940
3503.242620	487613.090303	42.786945
3503.313516	487580.854558	42.791949
3503.161162	487557.088498	42.796954
3503.454018	487521.585510	42.801959
3503.185414	487499.958835	42.806964
3502.865213	487464.601623	42.811969
3503.363135	487431.693002	42.816973
3502.944156	487407.160048	42.821978
3503.401481	487381.278460	42.826983
3503.062870	487351.328380	42.831988
3503.485699	487325.502575	42.836993
3503.585763	487288.160186	42.841997
3503.531831	487260.388065	42.847002
3503.478812	487208.977003	42.852007
3503.003130	487183.543331	42.857012
3503.285429	487143.848760	42.862017
3503.260949	487120.870290	42.867021
3503.078281	487080.944848	42.872026
3503.149466	487052.496243	42.877031
3503.269859	487031.212459	42.882036
3503.270425	486988.682214	42.887041
3502.911053	486965.351537	42.892045
3502.969109	486935.237896	42.897050
3503.054940	486899.311086	42.902055
3502.780443	486885.109605	42.907060
3503.006888	486848.049546	42.912065
3503.104355	486813.282486	42.917069
3503.076478	486795.355206	42.922074
3503.339522	486764.502169	42.927079
3502.963184	486731.475538	42.932084
3503.557130	486708.955847	42.937089
3503.268609	486680.916112	42.942093
3503.257111	486647.680991	42.947098
3503.367792	486609.173523	42.952103
3502.872459	486584.651133	42.957108
3503.145028	486547.835735	42.962113
3503.432367	486525.110926	42.967117
3503.233820	486492.510726	42.972122
3503.212953	486462.307415	42.977127
3502.824110	486441.203083	42.982132
3503.066943	486399.290173	42.987137
3503.204543	486369.769201	42.992141
3502.908957	486337.537364	42.997146
3502.848874	486310.724231	43.002151
3502.783058	486285.780934	43.007156
3502.916740	486260.604498	43.012161
3502.925950	486233.073261	43.017165
3502.983258	486208.817867	43.022170
3503.316361	486180.074324	43.027175
3502.973686	486158.255229	43.032180
3502.967027	486126.685180	43.037185
3502.645203	486099.811383	43.042189
3502.853868	486073.006530	43.047194
3502.978588	486053.539223	43.052199
3502.924088	486025.158791	43.057204
3502.638989	485994.642082	43.062209
3502.773076	485978.254586	43.067213
3502.734895	485955.630107	43.072218
3502.853969	485920.403040	43.077223
3502.889150	485902.010277	43.082228
3502.947085	485869.520390	43.087233
3503.124082	485843.225212	43.092237
3502.987482	485828.092031	43.097242
3503.123022	485781.748843	43.102247
3502.817783	485761.842926	43.107252
3503.147709	485736.837158	43.112257
3503.176022	485710.362830	43.117261
3502.864678	485674.747546	43.122266
3503.483904	485652.272898	43.127271
3502.718112	485618.950874	43.132276
3503.026751	485583.289417	43.137281
3503.354348	485555.960004	43.142285
3503.176246	485531.336053	43.147290
3503.003043	485503.023648	43.152295
3502.817065	485481.936948	43.157300
3502.935706	485450.194469	43.162305
3503.170576	485432.931941	43.167309
3502.887496	485404.484905	43.172314
3502.973622	485373.201973	43.177319
3502.847569	485348.317049	43.182324
3502.982350	485319.198637	43.187329
3503.061139	485294.736398	43.192333
3502.686097	485266.101352	43.197338
3502.769822	485236.131947	43.202343
3502.852720	485218.286629	43.207348
3503.080064	485190.770105	43.212353
3502.982951	485161.232830	43.217357
3502.972088	485130.217084	43.222362
3502.651051	485105.261077	43.227367
3502.638239	485090.360494	43.232372
3502.732778	485061.449928	43.237377
3502.708711	485038.518807	43.242381
3502.665191	485012.610153	43.247386
3502.538728	484987.674195	43.252391
3502.578954	484967.915564	43.257396
3502.832130	484941.960622	43.262401
3502.743592	484912.724644	43.267405
3502.637851	484898.697139	43.272410
3502.752329	484872.662629	43.277415
3502.710484	484853.876463	43.282420
3502.739262	484821.237357	43.287425
3502.375869	484801.591839	43.292429
3502.525099	484781.967563	43.297434
3503.061850	484755.159892	43.302439
3502.936296	484738.003194	43.307444
3502.803247	484707.914945	43.312449
3502.423951	484689.534719	43.317453
3502.628859	484661.515564	43.322458
3502.747083	484638.460671	43.327463
3502.915647	484622.925191	43.332468
3502.763868	484593.647933	43.337473
3502.607051	484556.995651	43.342477
3502.527820	484545.792757	43.347482
3502.778014	484522.313004	43.352487
3502.344982	484495.352680	43.357492
3502.728042	484477.510319	43.362497
3502.640925	484455.901644	43.367501
3502.785160	484437.540689	43.372506
3502.981347	484406.895430	43.377511
3502.593764	484392.001976	43.382516
3502.695080	484360.007363	43.387521
3502.689833	484337.830069	43.392525
3502.559052	484325.018411	43.397530
3502.676532	484295.597650	43.402535
3502.798125	484279.766019	43.407540
3502.919481	484240.846832	43.412545
3502.651121	484226.591424	43.417549
3502.615091	484203.155729	43.422554
3502.577802	484179.619154	43.427559
3502.600192	484153.648289	43.432564
3502.606124	484139.653239	43.437569
3502.780194	484113.102980	43.442573
3502.454927	484094.865201	43.447578
3502.758928	484072.841487	43.452583
3502.616560	484055.282487	43.457588
3502.635660	484025.421840	43.462593
3502.677733	484005.459614	43.467597
3502.470080	483995.438282	43.472602
3502.578131	483964.805866	43.477607
3502.615350	483947.572444	43.482612
3502.681813	483918.967243	43.487617
3502.854446	483889.183485	43.492621
3502.543917	483868.518136	43.497626
3502.530826	483850.686182	43.502631
3502.478978	483832.708674	43.507636
3502.831027	483814.062040	43.512641
3502.830621	483787.437333	43.517645
3502.770320	483771.532446	43.522650
3502.638668	483739.522288	43.527655
3502.728426	483719.299667	43.532660
3502.559607	483690.073877	43.537665
3502.664640	483667.221683	43.542669
3502.523690	483650.318787	43.547674
3502.563051	483631.417461	43.552679
3502.154694	483611.827954	43.557684
3502.780127	483579.548089	43.562689
3502.438321	483566.465510	43.567693
3502.370853	483556.169469	43.572698
3502.485126	483523.564854	43.577703
3502.652556	483517.274012	43.582708
3502.102535	483495.685513	43.587713
3502.690469	483472.959978	43.592717
3502.518564	483452.525116	43.597722
3502.445785	483423.182836	43.602727
3502.537318	483409.881125	43.607732
3502.451644	483388.877012	43.612737
3502.868036	483363.702402	43.617741
3502.508638	483349.157218	43.622746
3502.750618	483315.926022	43.627751
3502.555305	483298.677544	43.632756
3502.798252	483283.583860	43.637761
3502.669592	483253.441587	43.642765
3503.016224	483228.176568	43.647770
3502.874532	483208.393486	43.652775
3502.743673	483188.760262	43.657780
3502.856600	483157.973932	43.662785
3502.827940	483128.523184	43.667789
3502.926128	483109.763642	43.672794
3502.999778	483074.638231	43.677799
3502.676015	483064.735414	43.682804
3502.552740	483027.316449	43.687809
3502.447538	483003.485521	43.692813
3502.573034	482978.102937	43.697818
3502.803272	482956.139650	43.702823
3502.641293	482944.645334	43.707828
3502.370653	482920.991597	43.712833
3502.600642	482906.505855	43.717837
3502.272073	482882.658977	43.722842
3502.584882	482861.339523	43.727847
3502.642872	482841.828049	43.732852
3502.493254	482816.083818	43.737857
3502.380458	482802.207091	43.742861
3502.212373	482771.514251	43.747866
3502.758868	482756.625446	43.752871
3502.774918	482743.334914	43.757876
3502.279021	482724.313682	43.762881
3502.521963	482702.247012	43.767885
3502.443874	482695.741422	43.772890
3503.037071	482663.363633	43.777895
3502.316626	482637.960560	43.782900
3502.392599	482617.384980	43.787905
3502.700487	482603.291038	43.792909
3502.575094	482577.087916	43.797914
3503.118791	482555.580541	43.802919
3502.669354	482540.492833	43.807924
3502.555669	482508.325774	43.812929
3502.499913	482489.437867	43.817933
3502.280250	482472.899621	43.822938
3502.598880	482444.303002	43.827943
3502.573458	482424.955565	43.832948
3502.043273	482399.471970	43.837953
3502.633895	482388.820123	43.842957
3502.458274	482372.325443	43.847962
3502.592094	482341.635305	43.852967
3502.336199	482326.012011	43.857972
3502.651543	482313.584009	43.862977
3502.856793	482283.135272	43.867981
3502.400283	482259.509455	43.872986
3502.529004	482236.398850	43.877991
3502.742589	482218.075019	43.882996
3502.586348	482198.596079	43.888001
3502.574841	482173.233509	43.893005
3502.288518	482159.130581	43.898010
3502.441924	482132.024375	43.903015
3502.660524	482115.013338	43.908020
3502.819039	482097.758998	43.913025
3502.515103	482079.616591	43.918029
3502.215901	482056.370203	43.923034
3502.423194	482027.941731	43.928039
3502.589175	482007.098707	43.933044
3502.431562	481999.089388	43.938049
3502.875820	481982.750472	43.943053
3502.360777	481954.030053	43.948058
3502.696961	481925.227646	43.953063
3502.320906	481916.949112	43.958068
3502.496797	481899.843433	43.963073
3502.556392	481865.778572	43.968077
3502.274369	481850.057813	43.973082
3502.449700	481827.090934	43.978087
3502.433984	481817.998359	43.983092
3502.199360	481788.627666	43.988097
3502.688787	481775.313176	43.993101
3502.079751	481761.815914	43.998106
3502.751264	481734.224174	44.003111
3502.513866	481720.871157	44.008116
3502.637218	481693.667815	44.013121
3502.689916	481663.797424	44.018125
3502.489935	481653.268108	44.023130
3502.355217	481616.049661	44.028135
3502.174664	481608.548995	44.033140
3502.059876	481592.549311	44.038145
3502.583014	481571.144846	44.043149
3502.211783	481559.328373	44.048154
3502.326905	481539.856915	44.053159
3502.352699	481525.401674	44.058164
3501.906756	481510.312426	44.063169
3502.464933	481479.908268	44.068173
3502.136583	481483.546879	44.073178
3502.332524	481463.860636	44.078183
3502.042417	481441.622497	44.083188
3502.593847	481434.311016	44.088193
3502.361044	481414.388254	44.093197
3502.098898	481403.413682	44.098202
3502.401125	481387.551013	44.103207
3501.962647	481355.785832	44.108212
3501.922731	481356.701540	44.113217
3502.156778	481339.333555	44.118221
3502.489316	481316.947819	44.123226
3502.606469	481310.866035	44.128231
3502.326354	481279.985586	44.133236
3502.602991	481263.823598	44.138241
3502.663609	481239.054648	44.143245
3502.230795	481229.117104	44.148250
3502.551497	481196.374460	44.153255
3502.385969	481190.235558	44.158260
3502.212960	481159.792974	44.163265
3502.497840	481150.703766	44.168269
3502.363946	481130.158893	44.173274
3502.501611	481108.359015	44.178279
3502.430775	481100.436792	44.183284
3502.311256	481070.339421	44.188289
3502.453415	481058.745861	44.193293
3502.568965	481034.928115	44.198298
3502.293573	481013.798746	44.203303
3502.437299	480999.072018	44.208308
3502.336513	480975.136255	44.213313
3502.187668	480959.191756	44.218317
3502.319219	480940.020182	44.223322
3502.227190	480926.492275	44.228327
3501.817389	480905.434206	44.233332
3502.372989	480893.270881	44.238337
3502.191547	480877.078718	44.243341
3502.457225	480861.019083	44.248346
3502.446967	480841.010432	44.253351
3502.295281	480822.893409	44.258356
3502.243051	480808.298057	44.263361
3502.292373	480789.543344	44.268365
3501.746307	480774.014187	44.273370
3502.498151	480746.307156	44.278375
3502.377448	480748.246094	44.283380
3501.906507	480729.925987	44.288385
3502.003012	480718.895126	44.293389
3501.797672	480712.105325	44.298394
3502.275389	480678.579202	44.303399
3502.258228	480674.994112	44.308404
3502.226269	480656.504546	44.313409
3502.074956	480636.770243	44.318413
3502.287879	480635.473791	44.323418
3502.196798	480618.307200	44.328423
3502.286125	480582.365262	44.333428
3502.104544	480590.882814	44.338433
3502.262610	480562.307758	44.343437
3501.887203	480554.483187	44.348442
3502.055854	480537.023431	44.353447
3502.102992	480527.869797	44.358452
3501.955207	480506.315633	44.363457
3502.479511	480502.646245	44.368461
3502.192680	480492.180196	44.373466
3502.409111	480463.798008	44.378471
3502.438748	480445.147013	44.383476
3502.196495	480431.035671	44.388481
3502.339770	480411.103647	44.393485
3502.436461	480394.463447	44.398490
3502.178962	480380.303900	44.403495
3502.326145	480361.280787	44.408500
3502.110556	480356.665322	44.413505
3502.354580	480335.049954	44.418509
3502.042246	480322.364330	44.423514
3502.643974	480294.730402	44.428519
3502.284784	480283.264821	44.433524
3502.266299	480261.387005	44.438529
3502.573354	480239.357436	44.443533
3502.157458	480233.105521	44.448538
3502.375553	480204.015148	44.453543
3502.326095	480192.602368	44.458548
3502.130430	480172.571188	44.463553
3502.268291	480166.081476	44.468557
3502.244754	480144.709615	44.473562
3502.083587	480131.596049	44.478567
3502.163168	480116.019415	44.483572
3502.034543	480096.280904	44.488577
3502.473056	480077.464782	44.493581
3502.452725	480068.877247	44.498586
3502.389368	480042.508641	44.503591
3502.369848	480026.189338	44.508596
3502.676641	480009.920307	44.513601
3502.329365	479985.970865	44.518605
3502.276734	479966.068765	44.523610
3502.488008	479954.109903	44.528615
3502.387117	479933.002462	44.533620
3502.518588	479916.609016	44.538625
3502.560767	479890.324801	44.543629
3502.320300	479881.367149	44.548634
3502.388293	479857.555026	44.553639
3502.586981	479841.100508	44.558644
3502.348637	479814.809286	44.563649
3502.752178	479787.407451	44.568653
3502.210695	479783.651078	44.573658
3501.982425	479759.025826	44.578663
3502.494249	479748.030727	44.583668
3502.227700	479728.414288	44.588673
3502.333547	479710.912858	44.593677
3502.275203	479695.458342	44.598682
3502.356882	479675.686579	44.603687
3502.363359	479662.344397	44.608692
3502.100329	479636.562067	44.613697
3502.547638	479629.821843	44.618701
3502.373932	479618.225844	44.623706
3502.524294	479595.461740	44.628711
3502.027707	479576.083048	44.633716
3502.280399	479553.707239	44.638721
3502.525163	479531.484238	44.643725
3502.197432	479519.053039	44.648730
3501.865032	479500.255125	44.653735
3501.909771	479495.902107	44.658740
3502.166131	479473.171868	44.663745
3502.414491	479448.118216	44.668749
3502.533723	479451.839247	44.673754
3502.709807	479426.493595	44.678759
3502.917730	479402.911691	44.683764
3502.518868	479379.171497	44.688769
3502.426588	479353.058920	44.693773
3502.826322	479337.633843	44.698778
3502.907607	479313.414548	44.703783
3502.602408	479290.821969	44.708788
3502.571422	479268.641510	44.713793
3502.804164	479245.156581	44.718797
3502.500716	479219.935756	44.723802
3502.469571	479210.288180	44.728807
3502.353977	479182.814476	44.733812
3502.358332	479173.717252	44.738817
3502.536082	479141.548495	44.743821
3502.395520	479134.343643	44.748826
3502.304392	479111.161595	44.753831
3502.750985	479088.401203	44.758836
3502.629288	479061.787358	44.763841
3502.927581	479041.576804	44.768845
3502.630004	479025.552422	44.773850
3502.668967	479001.339236	44.778855
3502.424721	478968.528282	44.783860
3502.302868	478957.934467	44.788865
3502.486038	478926.269800	44.793869
3502.454379	478926.375770	44.798874
3502.359054	478891.520002	44.803879
3502.422797	478878.825231	44.808884
3502.436433	478865.127504	44.813889
3502.767686	478839.200859	44.818893
3502.503213	478809.323885	44.823898
3502.428231	478789.625933	44.828903
3502.563012	478779.699588	44.833908
3502.554101	478757.868742	44.838913
3503.075683	478734.338111	44.843917
3503.016201	478717.669915	44.848922
3502.743130	478677.939183	44.853927
3502.640097	478658.498122	44.858932
3502.788894	478642.353353	44.863937
3502.770421	478602.127971	44.868941
3502.748559	478591.366737	44.873946
3502.621576	478561.366825	44.878951
3502.708588	478547.505791	44.883956
3502.773361	478518.789952	44.888961
3502.649443	478487.020581	44.893965
3502.270716	478474.495418	44.898970
3502.701564	478453.555952	44.903975
3502.709338	478438.494230	44.908980
3502.936791	478408.135642	44.913985
3502.750575	478388.403963	44.918989
3503.174302	478362.512691	44.923994
3502.831754	478332.596430	44.928999
3503.134382	478305.460437	44.934004
3502.557575	478280.735507	44.939009
3502.705714	478249.327638	44.944013
3502.434977	478222.381804	44.949018
3502.549730	478208.010766	44.954023
3502.488594	478183.306517	44.959028
3502.394546	478173.819718	44.964033
3502.620496	478148.211571	44.969037
3502.659230	478134.054453	44.974042
3502.518350	478109.160341	44.979047
3502.666532	478089.881651	44.984052
3502.407982	478065.612258	44.989057
3502.501494	478049.222791	44.994061
3502.204369	478034.915689	44.999066
3502.173536	478012.430213	45.004071
3502.618160	478000.585190	45.009076
3502.481726	477976.397738	45.014081
3502.677817	477949.429337	45.019085
3502.497447	477935.457758	45.024090
3502.233110	477909.672822	45.029095
3502.152507	477889.873550	45.034100
3502.365740	477875.739589	45.039105
3502.220670	477856.607331	45.044109
3502.411633	477843.386534	45.049114
3502.226479	477821.531287	45.054119
3502.395756	477801.945724	45.059124
3502.410268	477795.221537	45.064129
3502.507527	477759.120344	45.069133
3502.397263	477756.762058	45.074138
3502.572742	477736.114094	45.079143
3502.802318	477714.598490	45.084148
3502.268973	477687.591534	45.089153
3502.428469	477670.989247	45.094157
3502.424116	477657.495444	45.099162
3502.249235	477629.927198	45.104167
3502.199716	477620.382598	45.109172
3501.934034	477596.416845	45.114177
3502.128276	477579.253103	45.119181
3502.347257	477581.543895	45.124186
3502.234991	477556.139053	45.129191
3502.514545	477532.391607	45.134196
3502.174312	477512.682809	45.139201
3502.178711	477499.136968	45.144205
3502.261052	477488.510398	45.149210
3502.405926	477466.249517	45.154215
3502.366865	477454.984775	45.159220
3502.207954	477434.742248	45.164225
3502.544063	477409.570650	45.169229
3502.302742	477392.727195	45.174234
3502.250494	477375.551049	45.179239
3502.193438	477367.119393	45.184244
3502.400485	477349.650160	45.189249
3502.642039	477333.843426	45.194253
3502.237531	477316.166069	45.199258
3502.442015	477292.480491	45.204263
3502.368632	477270.455469	45.209268
3502.060512	477254.582566	45.214273
3502.273297	477245.704517	45.219277
3502.311382	477220.629540	45.224282
3502.232480	477214.879951	45.229287
3502.244412	477193.245887	45.234292
3502.416124	477173.153749	45.239297
3502.519683	477154.992811	45.244301
3502.238310	477139.722143	45.249306
3502.004532	477122.624515	45.254311
3502.317721	477100.539104	45.259316
3502.103514	477081.821018	45.264321
3502.103465	477064.080442	45.269325
3502.227182	477060.573699	45.274330
3502.190469	477037.632877	45.279335
3502.355264	477035.737112	45.284340
3502.100743	477011.263313	45.289345
3502.347872	476989.541830	45.294349
3502.385963	476981.903855	45.299354
3502.271358	476955.942447	45.304359
3502.332434	476946.835124	45.309364
3501.995512	476917.016414	45.314369
3502.168206	476904.555835	45.319373
3502.273658	476892.206796	45.324378
3502.120824	476871.153913	45.329383
3502.245752	476858.245839	45.334388
3502.283967	476843.380048	45.339393
3502.556373	476811.242402	45.344397
3502.619365	476800.921649	45.349402
3502.284368	476777.723609	45.354407
3502.169601	476757.321722	45.359412
3502.177011	476748.222638	45.364417
3502.576509	476732.390733	45.369421
3502.485728	476717.241633	45.374426
3502.274158	476697.612894	45.379431
3502.417025	476684.600801	45.384436
3502.414688	476669.690614	45.389441
3502.644289	476648.123029	45.394445
3502.335203	476636.798641	45.399450
3502.603612	476618.763076	45.404455
3502.575708	476579.949303	45.409460
3502.109456	476569.710757	45.414465
3502.397280	476543.382790	45.419469
3502.237873	476528.496914	45.424474
3502.221587	476511.819690	45.429479
3502.426705	476493.844377	45.434484
3502.522982	476479.777928	45.439489
3502.277541	476454.594237	45.444493
3502.104377	476446.281253	45.449498
3501.935968	476422.349146	45.454503
3502.220514	476406.939168	45.459508
3501.892996	476394.960392	45.464513
3502.346285	476375.379432	45.469517
3502.244641	476359.271328	45.474522
3501.954941	476358.912018	45.479527
3502.488724	476333.657425	45.484532
3502.276451	476312.815238	45.489537
3502.497330	476301.711415	45.494541
3502.424752	476280.695812	45.499546
3502.431224	476266.491515	45.504551
3502.453525	476238.081457	45.509556
3502.080809	476229.243412	45.514561
3501.835774	476203.250534	45.519565
3501.942245	476193.225898	45.524570
3502.208846	476177.060307	45.529575
3502.087388	476170.912599	45.534580
3502.046806	476148.729292	45.539585
3502.299856	476132.616312	45.544589
3502.061776	476123.251798	45.549594
3502.290895	476099.156256	45.554599
3502.248062	476077.984121	45.559604
3502.446389	476074.465553	45.564609
3502.231283	476052.309271	45.569613
3502.187241	476044.026531	45.574618
3502.091420	476027.613910	45.579623
3502.091242	476016.241013	45.584628
3502.082682	476012.906264	45.589633
3502.088700	475983.032448	45.594637
3502.217456	475977.300646	45.599642
3502.355683	475968.332401	45.604647
3502.328573	475935.784695	45.609652
3502.436764	475925.810171	45.614657
3502.337376	475906.061911	45.619661
3502.218025	475886.973840	45.624666
3501.907942	475859.322488	45.629671
3502.371137	475849.595954	45.634676
3501.623166	475843.495067	45.639681
3502.014335	475825.995523	45.644685
3502.037870	475801.223871	45.649690
3502.010170	475798.650260	45.654695
3502.326932	475797.337265	45.659700
3501.867774	475778.150302	45.664705
3502.014387	475755.027476	45.669709
3501.802190	475750.612326	45.674714
3501.847369	475740.142022	45.679719
3501.897914	475719.814184	45.684724
3502.103152	475720.793159	45.689729
3502.096851	475704.214636	45.694733
3502.195530	475688.832894	45.699738
3502.028017	475674.452959	45.704743
3502.356478	475655.850949	45.709748
3502.047178	475643.211659	45.714753
3502.145356	475626.212418	45.719757
3502.082521	475617.123623	45.724762
3502.007984	475594.793193	45.729767
3502.327548	475577.405617	45.734772
3501.959544	475570.487283	45.739777
3502.155811	475556.252824	45.744781
3502.394681	475548.431280	45.749786
3502.094693	475531.999376	45.754791
3501.971174	475504.672216	45.759796
3501.585454	475500.031260	45.764801
3502.120726	475488.372475	45.769805
3501.899568	475480.066457	45.774810
3501.867507	475447.821820	45.779815
3501.974671	475391.039603	45.784820
3501.504478	475291.835800	45.789825
3501.696946	475130.757505	45.794829
3501.451354	474941.842417	45.799834
3501.063981	474688.343912	45.804839
3501.028421	474380.393516	45.809844
3500.562307	474045.307087	45.814849
3500.600029	473653.616466	45.819853
3499.735471	473216.709037	45.824858
3498.846694	472732.270590	45.829863
3498.365878	472204.982119	45.834868
3497.588288	471640.409641	45.839873
3497.071366	471018.692940	45.844877
3496.294278	470366.756020	45.849882
3495.241028	469659.011477	45.854887
3494.534235	468905.772382	45.859892
3493.325012	468113.890631	45.864897
3492.396383	467285.211309	45.869901
3491.424489	466411.333300	45.874906
3490.465822	465492.696091	45.879911
3489.084435	464541.803415	45.884916
3487.741067	463544.566421	45.889921
3486.530810	462494.891849	45.894925
3485.248030	461424.522726	45.899930
3483.681257	460306.218181	45.904935
3482.685975	459139.886654	45.909940
3481.029207	457952.124418	45.914945
3479.347999	456713.831932	45.919949
3477.737986	455449.225384	45.924954
3476.088051	454153.711196	45.929959
3473.926884	452797.189417	45.934964
3472.152945	451418.281630	45.939969
3470.808617	450006.345742	45.944973
3468.805343	448572.378436	45.949978
3466.587470	447097.470991	45.954983
3464.695733	445581.884561	45.959988
3462.881045	444047.474693	45.964993
3460.806452	442485.984342	45.969997
3458.616019	440886.698307	45.975002
3456.590897	439262.176853	45.980007
3454.470092	437600.550619	45.985012
3452.137850	435922.245907	45.990017
3449.636750	434211.900924	45.995021
3447.776618	432471.409256	46.000026
3445.631188	430704.962392	46.005031
3443.546516	428915.643056	46.010036
3441.022973	427089.180433	46.015041
3438.241163	425236.841562	46.020045
3436.023978	423370.912967	46.025050
3433.800752	421477.032218	46.030055
3430.957966	419558.584532	46.035060
3428.440904	417618.510983	46.040065
3426.022928	415646.953688	46.045069
3423.560984	413655.288847	46.050074
3420.412983	411650.054525	46.055079
3417.849056	409620.145003	46.060084
3415.061837	407582.574889	46.065089
3412.709593	405494.927590	46.070093
3409.806546	403397.988550	46.075098
3407.040421	401294.187776	46.080103
3404.466772	399150.884554	46.085108
3401.062011	397007.869515	46.090113
3397.822856	394832.909949	46.095117
3395.212039	392652.731291	46.100122
3392.130935	390455.828886	46.105127
3388.994550	388244.954228	46.110132
3386.199834	386016.185410	46.115137
3383.140828	383766.821743	46.120141
3379.862462	381518.641177	46.125146
3376.573544	379238.549330	46.130151
3373.601365	376948.535216	46.135156
3370.379999	374660.091937	46.140161
3367.405465	372340.224645	46.145165
3364.046982	370008.130637	46.150170
3360.858865	367675.486858	46.155175
3357.480367	365332.341611	46.160180
3354.473271	362973.627698	46.165185
3351.424353	360590.616278	46.170189
3347.634835	358219.222526	46.175194
3344.187287	355822.252417	46.180199
3341.255574	353410.199576	46.185204
3337.729831	351004.360941	46.190209
3334.371144	348585.378431	46.195213
3331.150942	346156.333405	46.200218
3327.506899	343705.262959	46.205223
3324.071385	341255.715172	46.210228
3320.191372	338801.107749	46.215233
3316.899734	336333.526126	46.220237
3313.452603	333867.710944	46.225242
3309.930175	331394.065052	46.230247
3306.473467	328918.164631	46.235252
3302.693436	326433.739615	46.240257
3299.051010	323934.030006	46.245261
3295.434191	321433.860706	46.250266
3292.269992	318947.162155	46.255271
3288.618509	316430.451244	46.260276
3284.369826	313935.447853	46.265281
3280.974283	311406.613620	46.270285
3277.479233	308897.484299	46.275290
3273.810665	306394.895878	46.280295
3270.212099	303860.563865	46.285300
3266.469587	301332.901415	46.290305
3262.566604	298796.186407	46.295309
3259.090081	296277.183799	46.300314
3254.919232	293749.550531	46.305319
3251.521448	291206.798995	46.310324
3247.848057	288677.046054	46.315329
3244.107334	286129.715566	46.320333
3240.331526	283590.925124	46.325338
3236.378831	281048.964902	46.330343
3232.871410	278507.866361	46.335348
3228.736446	275974.624170	46.340353
3224.826242	273436.379435	46.345357
3220.686128	270903.493404	46.350362
3217.072398	268382.524245	46.355367
3213.500210	265844.879771	46.360372
3209.260589	263323.598859	46.365377
3205.806600	260786.043227	46.370381
3201.855115	258260.351422	46.375386
3197.495981	255737.600949	46.380391
3193.751312	253211.601236	46.385396
3189.438065	250689.925627	46.390401
3185.223409	248182.101147	46.395405
3181.371195	245676.834417	46.400410
3177.268386	243178.350620	46.405415
3173.537788	240686.353137	46.410420
3169.343419	238199.931824	46.415425
3165.562409	235725.626901	46.420429
3161.429434	233247.541478	46.425434
3157.124493	230778.411172	46.430439
3153.222147	228321.104765	46.435444
3148.845280	225870.974272	46.440449
3144.725342	223423.579744	46.445453
3140.598808	220994.858424	46.450458
3136.364877	218560.914078	46.455463
3132.396867	216151.719887	46.460468
3128.013723	213755.541978	46.465473
3123.926107	211351.872669	46.470477
3119.771700	208963.642350	46.475482
3115.359222	206593.863444	46.480487
3111.330961	204222.854075	46.485492
3107.163532	201881.463485	46.490497
3102.591075	199533.011713	46.495501
3098.696646	197206.722075	46.500506
3094.312795	194893.330358	46.505511
3089.783241	192579.161337	46.510516
3085.384586	190289.843922	46.515521
3081.445439	188023.520491	46.520525
3076.716468	185760.881410	46.525530
3071.918969	183522.467954	46.530535
3067.459970	181289.680892	46.535540
3062.923102	179097.165131	46.540545
3058.513557	176913.977930	46.545549
3054.171708	174745.349904	46.550554
3049.298830	172593.921593	46.555559
3044.656642	170460.033771	46.560564
3039.798385	168363.525619	46.565569
3035.058715	166271.184960	46.570573
3030.275207	164210.265496	46.575578
3025.088997	162187.631957	46.580583
3020.517518	160178.343386	46.585588
3015.284364	158211.974034	46.590593
3009.916731	156255.642088	46.595597
3004.798681	154346.870264	46.600602
2999.438766	152450.633264	46.605607
2994.091920	150549.495763	46.610612
2988.142818	148762.346301	46.615617
2981.882499	147017.832063	46.620621
2975.919099	145326.251354	46.625626
2969.058127	143698.385145	46.630631
2962.323351	142115.263461	46.635636
2955.133360	140597.661430	46.640641
2948.450810	139145.105877	46.645645
2941.484509	137758.719787	46.650650
2934.985102	136429.653754	46.655655
2929.060000	135153.446781	46.660660
2922.531715	133938.686998	46.665665
2917.018727	132773.898002	46.670669
2911.437651	131667.360644	46.675674
2906.167273	130599.765867	46.680679
2901.267928	129567.781734	46.685684
2895.999046	128589.087248	46.690689
2891.314475	127630.675930	46.695693
2886.671038	126718.921814	46.700698
2882.495452	125831.586411	46.705703
2877.933938	124962.492686	46.710708
2873.929734	124132.732649	46.715713
2869.481345	123314.289067	46.720717
2864.915276	122520.159168	46.725722
2861.472290	121755.222886	46.730727
2857.305459	120999.329109	46.735732
2853.307373	120258.213865	46.740737
2849.449324	119531.028838	46.745741
2845.657453	118815.953619	46.750746
2841.601780	118125.323091	46.755751
2838.365558	117434.539504	46.760756
2834.211005	116772.484421	46.765761
2830.188301	116098.124381	46.770765
2826.288189	115445.602863	46.775770
2822.462450	114802.694116	46.780775
2818.526219	114170.583547	46.785780
2814.483449	113557.890758	46.790785
2810.733343	112943.242858	46.795789
2807.250974	112349.517242	46.800794
2802.706541	111756.793157	46.805799
2799.434699	111164.694582	46.810804
2794.959355	110608.849685	46.815809
2791.548965	110052.517256	46.820813
2787.699104	109497.507940	46.825818
2783.804158	108956.346483	46.830823
2780.108671	108409.225394	46.835828
2776.713867	107893.517806	46.840833
2772.636843	107362.414612	46.845837
2769.299573	106839.658320	46.850842
2765.460109	106325.581684	46.855847
2762.233173	105809.205585	46.860852
2758.756235	105305.473765	46.865857
2755.310616	104794.842120	46.870861
2752.151491	104291.775147	46.875866
2748.406920	103779.756365	46.880871
2744.901523	103270.021659	46.885876
2741.551105	102767.592173	46.890881
2738.292768	102264.444192	46.895885
2734.950609	101756.156457	46.900890
2731.323274	101254.479532	46.905895
2728.152827	100747.057769	46.910900
2724.628685	100234.729367	46.915905
2721.300372	99726.166109	46.920909
2718.092452	99208.021830	46.925914
2714.917760	98698.243500	46.930919
2711.356027	98184.275956	46.935924
2707.612287	97664.384531	46.940929
2704.521985	97149.496146	46.945933
2701.228269	96627.175185	46.950938
2697.736895	96115.466981	46.955943
2694.551424	95587.110018	46.960948
2691.333446	95076.100635	46.965953
2687.770022	94536.001965	46.970957
2684.166478	94003.314705	46.975962
2680.738026	93484.523839	46.980967
2677.725944	92955.663796	46.985972
2674.104030	92417.542878	46.990977
2670.865257	91880.210475	46.995981
2667.455107	91330.512852	47.000986
2663.687644	90804.221992	47.005991
2660.340169	90253.632110	47.010996
2657.107389	89718.687878	47.016001
2653.295501	89169.625961	47.021005
2649.905622	88626.924641	47.026010
2646.304126	88089.856387	47.031015
2643.380359	87547.013424	47.036020
2639.644884	87001.130679	47.041025
2636.398146	86447.927924	47.046029
2632.957428	85898.970888	47.051034
2629.243923	85342.558746	47.056039
2625.946695	84789.103271	47.061044
2622.414548	84234.958198	47.066049
2619.009795	83677.107417	47.071053
2615.628713	83125.005510	47.076058
2611.789349	82557.907703	47.081063
2608.549442	81995.491316	47.086068
2604.819588	81442.358657	47.091073
2601.204305	80884.239945	47.096077
2597.939358	80318.444208	47.101082
2594.562434	79759.663072	47.106087
2591.184229	79197.489493	47.111092
2587.353242	78649.368640	47.116097
2583.567736	78088.576485	47.121101
2580.649748	77514.465208	47.126106
2576.983699	76947.695976	47.131111
2573.934347	76387.370215	47.136116
2570.201685	75828.216404	47.141121
2566.678763	75253.396097	47.146125
2563.221927	74678.488872	47.151130
2559.679701	74122.579037	47.156135
2556.468014	73543.746816	47.161140
2552.814985	72970.989357	47.166145
2549.493084	72402.763948	47.171149
2545.986503	71822.961217	47.176154
2542.368348	71248.572256	47.181159
2538.802084	70671.229390	47.186164
2535.286288	70102.449011	47.191169
2531.795316	69522.345608	47.196173
2528.429280	68938.998209	47.201178
2524.945957	68371.196584	47.206183
2521.756492	67792.100748	47.211188
2518.244393	67215.708811	47.216193
2514.571876	66631.363317	47.221197
2511.344306	66044.657891	47.226202
2507.605692	65461.301679	47.231207
2504.331733	64877.797756	47.236212
2501.347363	64295.372992	47.241217
2497.578495	63706.108718	47.246221
2494.058649	63110.123890	47.251226
2490.475748	62521.931212	47.256231
2487.194075	61931.909584	47.261236
2483.507081	61332.198354	47.266241
2480.005560	60733.075726	47.271245
2476.791430	60142.407409	47.276250
2473.158107	59559.852256	47.281255
2470.075346	58955.713915	47.286260
2466.521132	58346.657453	47.291265
2463.054415	57753.630770	47.296269
2458.987467	57149.544745	47.301274
2455.614835	56553.436600	47.306279
2452.492721	55943.574253	47.311284
2448.911815	55343.474408	47.316289
2445.566598	54738.455134	47.321293
2441.963055	54134.449507	47.326298
2438.379947	53527.886798	47.331303
2434.864480	52913.710134	47.336308
2431.098200	52312.016074	47.341313
2427.570293	51710.420959	47.346317
2424.670306	51101.861038	47.351322
2420.913106	50501.512814	47.356327
2417.449940	49895.742785	47.361332
2414.174251	49278.174316	47.366337
2410.362793	48671.406130	47.371341
2406.998093	48050.827402	47.376346
2403.241428	47452.303145	47.381351
2400.213887	46839.861388	47.386356
2396.737858	46223.745144	47.391361
2393.118155	45611.054693	47.396365
2389.643708	44999.417426	47.401370
2386.242760	44379.687239	47.406375
2382.690920	43763.517233	47.411380
2379.052215	43150.795751	47.416385
2375.722992	42536.749483	47.421389
2372.277250	41922.573565	47.426394
2368.845959	41305.210493	47.431399
2365.418401	40685.283634	47.436404
2361.978506	40063.708774	47.441409
2358.553417	39439.537210	47.446413
2355.188033	38810.987045	47.451418
2351.397892	38187.459947	47.456423
2348.086307	37560.839744	47.461428
2344.076790	36941.497304	47.466433
2340.994155	36313.781193	47.471437
2337.581294	35685.894055	47.476442
2333.878395	35070.272909	47.481447
2330.571973	34428.771496	47.486452
2326.855386	33807.864733	47.491457
2323.534107	33180.728586	47.496461
2320.105872	32543.068543	47.501466
2316.479263	31918.204363	47.506471
2312.798893	31290.033643	47.511476
2309.511031	30664.641038	47.516481
2305.768435	30032.462077	47.521485
2302.369705	29403.658355	47.526490
2298.665481	28787.791755	47.531495
2295.003729	28158.217953	47.536500
2291.665312	27533.162884	47.541505
2288.112109	26916.499091	47.546509
2284.510512	26284.502655	47.551514
2280.481426	25667.653117	47.556519
2277.327399	25040.593347	47.561524
2273.841251	24420.840060	47.566529
2270.173962	23802.914369	47.571533
2267.004456	23174.673630	47.576538
2263.104305	22568.561536	47.581543
2259.330395	21938.521728	47.586548
2255.935714	21325.913796	47.591553
2251.982062	20715.901295	47.596557
2248.431611	20093.993647	47.601562
2244.890413	19495.755489	47.606567
2241.443555	18894.442712	47.611572
2237.950032	18279.994468	47.616577
2234.180251	17685.210595	47.621581
2230.249340	17092.623355	47.626586
2226.368818	16498.219367	47.631591
2222.894457	15898.023452	47.636596
2219.301482	15318.977801	47.641601
2215.278491	14737.876205	47.646605
2211.403909	14166.888162	47.651610
2206.985564	13607.798534	47.656615
2202.565009	13062.000544	47.661620
2198.307174	12523.702385	47.666625
2193.910728	11998.977983	47.671629
2189.821960	11481.647013	47.676634
2185.666927	10990.884168	47.681639
2181.131453	10510.006497	47.686644
2176.908046	10046.774792	47.691649
2172.764412	9595.292015	47.696653
2168.783120	9147.222932	47.701658
2164.605748	8722.852006	47.706663
2160.011735	8307.205986	47.711668
2155.688629	7919.557094	47.716673
2150.863372	7535.843152	47.721677
2146.554702	7178.202484	47.726682
2142.235408	6843.297540	47.731687
2138.540551	6511.409397	47.736692
2134.570638	6185.792034	47.741697
2129.960455	5880.129294	47.746701
2126.389715	5590.209253	47.751706
2122.529007	5308.253689	47.756711
2118.801165	5025.326106	47.761716
2114.699554	4764.261582	47.766721
2110.829398	4506.424216	47.771725
2107.574136	4253.573759	47.776730
2103.735973	4016.471862	47.781735
2100.224119	3776.885727	47.786740
2096.850884	3539.486727	47.791745
2092.922268	3319.159996	47.796749
2089.655449	3088.281455	47.801754
2086.038278	2865.842379	47.806759
2082.608905	2639.016601	47.811764
2078.997352	2425.514540	47.816769
2075.903615	2207.007938	47.821773
2072.461977	2004.198057	47.826778
2068.806146	1793.459972	47.831783
2065.087913	1593.792196	47.836788
2061.789242	1387.704983	47.841793
2057.822369	1195.917445	47.846797
2054.446637	1001.755649	47.851802
2050.760112	803.278232	47.856807
2046.846028	619.341344	47.861812
2042.717303	442.748092	47.866817
2038.013317	288.699257	47.871821
2034.045213	140.137029	47.876826
2026.829974	102.706813	47.881831
2017.511500	117.625002	47.886836
2012.316863	121.881887	47.891841
2008.103863	126.052435	47.896845
2005.739167	106.381426	47.901850
2002.647603	119.950856	47.906855
2000.407822	117.629231	47.911860
1997.930313	113.408408	47.916865
1994.858348	114.841923	47.921869
1991.513808	112.284117	47.926874
1988.733596	122.040266	47.931879
1985.000471	118.248975	47.936884
1981.763333	113.266864	47.941889
1978.283962	121.549965	47.946893
1975.338384	111.406743	47.951898
1971.788416	113.091821	47.956903
1968.195275	113.825011	47.961908
1965.026532	115.811422	47.966913
1961.502525	115.689140	47.971917
1957.829658	118.709454	47.976922
1954.181432	124.503679	47.981927
1951.350642	124.324129	47.986932
1948.316146	119.253535	47.991937
1944.929796	125.639748	47.996941
1941.681794	117.223531	48.001946
1937.925962	120.278904	48.006951
1934.577167	115.494508	48.011956
1931.103202	110.634682	48.016961
1927.453884	116.944762	48.021965
1923.811516	110.348956	48.026970
1920.356361	120.577139	48.031975
1917.107486	113.803033	48.036980
1913.583498	106.166925	48.041985
1910.299369	109.541186	48.046989
1906.873288	107.492784	48.051994
1903.389607	113.033611	48.056999
1899.419075	115.106848	48.062004
1896.314204	110.392060	48.067009
1892.397257	119.771472	48.072013
1889.638562	115.069244	48.077018
1886.291384	108.595179	48.082023
1882.862992	113.684482	48.087028
1879.488829	109.919595	48.092033
1876.009893	115.962716	48.097037
1872.498620	118.885120	48.102042
1868.888885	125.495924	48.107047
1865.302060	107.173075	48.112052
1861.814527	105.362029	48.117057
1858.213113	116.894277	48.122061
1855.239725	109.087062	48.127066
1851.188856	115.791831	48.132071
1847.867222	121.310605	48.137076
1844.733732	112.651959	48.142081
1841.097198	115.862775	48.147085
1837.583585	113.391409	48.152090
1834.052230	106.734048	48.157095
1830.536463	113.997769	48.162100
1827.207023	119.350081	48.167105
1823.231641	119.310717	48.172109
1819.842655	116.845266	48.177114
1816.411677	113.715643	48.182119
1813.159364	118.347280	48.187124
1809.921798	109.154353	48.192129
1806.263108	115.513351	48.197133
1803.147904	105.260520	48.202138
1799.107771	104.620640	48.207143
1795.942007	104.898191	48.212148
1792.567714	111.121177	48.217153
1788.622291	111.289122	48.222157
1785.003614	104.521975	48.227162
1781.692987	113.911421	48.232167
1778.312510	110.479718	48.237172
1775.280928	104.601948	48.242177
1771.212859	106.437278	48.247181
1767.917696	103.495329	48.252186
1764.411798	113.133463	48.257191
1760.846111	116.228854	48.262196
1757.408801	101.334379	48.267201
1753.989010	118.956977	48.272205
1750.770658	105.167359	48.277210
1747.155887	107.036542	48.282215
1743.185469	108.768092	48.287220
1739.633308	98.073926	48.292225
1736.322734	110.095569	48.297229
1733.404181	104.165412	48.302234
1729.990563	102.017014	48.307239
1726.377519	102.449605	48.312244
1722.562909	100.689480	48.317249
1718.698778	115.552873	48.322253
1715.088096	110.790282	48.327258
1711.940207	102.510385	48.332263
1708.620051	103.887633	48.337268
1705.248059	96.667661	48.342273
1701.382175	104.441447	48.347277
1698.248766	93.549242	48.352282
1694.404869	103.423472	48.357287
1690.897998	108.407938	48.362292
1687.593103	101.977942	48.367297
1683.924140	111.138424	48.372301
1680.681423	98.988256	48.377306
1677.112924	96.750076	48.382311
1673.725002	100.374616	48.387316
1670.553833	101.450273	48.392321
1666.644158	102.596580	48.397325
1662.994728	97.197799	48.402330
1659.662816	106.369094	48.407335
1656.238351	102.412751	48.412340
1652.825098	105.962143	48.417345
1648.877230	102.928810	48.422349
1645.582092	100.360189	48.427354
1642.499870	84.274716	48.432359
1638.753069	104.232384	48.437364
1635.151349	101.613406	48.442369
1631.719597	97.920788	48.447373
1628.274197	102.626774	48.452378
1624.393270	101.879877	48.457383
1620.696423	99.917940	48.462388
1617.601876	101.446740	48.467393
1614.303925	105.503364	48.472397
1610.974971	102.114282	48.477402
1607.191695	96.366188	48.482407
1603.465830	98.622826	48.487412
1600.458088	94.240969	48.492417
1596.864621	98.482790	48.497421
1593.031950	104.350023	48.502426
1589.477469	97.832340	48.507431
1586.536028	109.853474	48.512436
1582.999972	103.858097	48.517441
1578.880577	105.736233	48.522445
1575.646428	104.366663	48.527450
1572.172460	98.102203	48.532455
1568.474550	97.975386	48.537460
1565.565192	98.690767	48.542465
1561.531738	102.580300	48.547469
1558.413931	102.299921	48.552474
1554.795681	101.423564	48.557479
1551.197185	97.443702	48.562484
1547.621441	98.183711	48.567489
1544.135856	108.324875	48.572493
1541.109949	94.929291	48.577498
1537.390969	100.484606	48.582503
1533.850883	101.646167	48.587508
1530.480690	101.278524	48.592513
1526.336292	105.166346	48.597517
1523.065009	101.119739	48.602522
1519.436259	100.029889	48.607527
1516.112995	92.641014	48.612532
1512.843622	98.917276	48.617537
1508.983822	102.140716	48.622541
1505.881998	96.530177	48.627546
1502.428290	95.280209	48.632551
1498.825823	104.094989	48.637556
1495.587183	102.995041	48.642561
1491.748473	103.545034	48.647565
1487.953375	100.345578	48.652570
1484.599414	107.875182	48.657575
1481.217664	102.877681	48.662580
1477.794280	94.479354	48.667585
1474.150864	100.573396	48.672589
1470.643515	104.918879	48.677594
1467.340350	104.673686	48.682599
1463.725480	104.122674	48.687604
1460.480974	94.276006	48.692609
1456.845482	102.403076	48.697613
1453.214120	105.850389	48.702618
1450.117047	97.170326	48.707623
1446.295918	100.087200	48.712628
1442.630503	90.862862	48.717633
1439.035756	96.259642	48.722637
1435.509904	99.532348	48.727642
1431.989403	92.655068	48.732647
1428.767119	100.660877	48.737652
1425.141174	96.859308	48.742657
1421.717534	96.455703	48.747661
1418.162283	104.737962	48.752666
1414.870360	98.372426	48.757671
1411.042040	104.036515	48.762676
1407.628144	91.954176	48.767681
1404.122402	97.517436	48.772685
1401.082795	95.801235	48.777690
1397.375835	92.739932	48.782695
1393.451585	100.165314	48.787700
1390.185762	95.909072	48.792705
1386.550110	95.623890	48.797709
1383.344080	92.832627	48.802714
1380.122736	97.035523	48.807719
1375.813180	99.420996	48.812724
1372.517865	89.120354	48.817729
1369.312297	102.242428	48.822733
1365.991305	100.785158	48.827738
1362.369166	98.068154	48.832743
1358.823344	94.728679	48.837748
1355.100596	96.298330	48.842753
1351.696074	99.697687	48.847757
1348.199123	96.929563	48.852762
1344.428918	89.385660	48.857767
1340.989324	93.821841	48.862772
1337.712232	91.775622	48.867777
1334.233220	92.007058	48.872781
1330.496191	102.756823	48.877786
1327.532048	94.239586	48.882791
1323.491319	101.319277	48.887796
1320.187905	89.925266	48.892801
1316.605885	97.895322	48.897805
1312.978405	89.493993	48.902810
1309.401758	96.460321	48.907815
1306.108557	95.292957	48.912820
1303.050020	89.922479	48.917825
1299.045904	93.332910	48.922829
1295.388458	90.706832	48.927834
1292.275828	84.712037	48.932839
1288.634884	98.930074	48.937844
1285.311290	89.775945	48.942849
1281.827374	98.151504	48.947853
1278.594745	92.757507	48.952858
1274.799037	96.094374	48.957863
1271.113837	105.855329	48.962868
1267.587894	97.846316	48.967873
1264.021853	98.996123	48.972877
1260.538045	100.550737	48.977882
1257.295619	91.276413	48.982887
1253.234710	95.353737	48.987892
1250.143205	87.213838	48.992897
1246.702405	98.534414	48.997901
1243.077849	86.779126	49.002906
1239.608243	93.421916	49.007911
1236.393442	92.523925	49.012916
1232.750801	88.845205	49.017921
1228.993530	95.931398	49.022925
1225.671167	94.028277	49.027930
1222.177892	88.235106	49.032935
1218.474780	93.898698	49.037940
1215.381043	77.052671	49.042945
1211.463013	94.126354	49.047949
1207.940333	94.598713	49.052954
1204.706144	89.932621	49.057959
1201.087234	94.254356	49.062964
1197.810777	92.856611	49.067969
1194.307274	92.095310	49.072973
1190.456886	87.224583	49.077978
1186.863573	83.971618	49.082983
1183.414805	84.916519	49.087988
1180.157214	83.863847	49.092993
1176.512877	84.734789	49.097997
1173.192474	78.905230	49.103002
1170.054101	84.604302	49.108007
1165.907265	77.796091	49.113012
1162.699051	77.700661	49.118017
1158.930100	88.322515	49.123021
1155.555508	83.684613	49.128026
1152.311464	80.573437	49.133031
1148.411184	96.476956	49.138036
1145.052712	83.224975	49.143041
1141.213469	87.675920	49.148045
1137.963167	89.782646	49.153050
1134.325796	79.962397	49.158055
1131.022915	97.367428	49.163060
1127.961121	92.579600	49.168065
1124.002416	89.646104	49.173069
1120.568982	84.906636	49.178074
1116.892346	85.719338	49.183079
1113.448824	86.312260	49.188084
1109.855643	90.702762	49.193089
1106.493015	90.925596	49.198093
1103.275588	97.779073	49.203098
1099.937260	98.314494	49.208103
1095.900712	97.462173	49.213108
1092.590583	93.554547	49.218113
1089.151050	92.169544	49.223117
1085.470789	86.294773	49.228122
1081.986759	84.087811	49.233127
1078.187343	88.409178	49.238132
1075.045560	87.499840	49.243137
1071.141638	88.240360	49.248141
1067.727208	90.378966	49.253146
1064.926013	85.936555	49.258151
1061.252356	85.401068	49.263156
1057.772960	82.949784	49.268161
1053.862349	90.844448	49.273165
1050.411254	89.347358	49.278170
1046.758871	76.951058	49.283175
1043.244611	86.998606	49.288180
1040.035705	79.256663	49.293185
1036.653567	80.760672	49.298189
1033.078934	90.852421	49.303194
1029.380470	82.076228	49.308199
1025.656590	86.787629	49.313204
1022.468109	71.927380	49.318209
1019.014714	87.736019	49.323213
1015.342882	85.656373	49.328218
1012.293196	80.844534	49.333223
1008.560173	82.937827	49.338228
1005.386956	79.872592	49.343233
1001.624177	77.987436	49.348237
997.970419	86.481184	49.353242
994.449470	86.627437	49.358247
990.520211	85.606573	49.363252
987.707579	83.361552	49.368257
984.028134	76.977320	49.373261
980.307903	84.253906	49.378266
976.977340	82.810828	49.383271
973.536039	86.326665	49.388276
970.091839	75.948047	49.393281
966.189494	87.511303	49.398285
962.733789	86.616041	49.403290
959.600963	77.856217	49.408295
955.506695	86.535594	49.413300
952.562357	82.558397	49.418305
949.115765	84.145212	49.423309
945.194710	82.699143	49.428314
941.785162	93.556121	49.433319
938.473182	85.937802	49.438324
934.968080	78.865230	49.443329
931.713216	93.301565	49.448333
928.049844	86.968620	49.453338
924.179534	82.594575	49.458343
920.406953	86.997197	49.463348
917.314125	76.633495	49.468353
913.693457	87.887156	49.473357
910.114419	78.007255	49.478362
907.213718	77.639362	49.483367
903.589119	77.747977	49.488372
900.109101	86.736693	49.493377
896.297984	85.169117	49.498381
892.737051	79.737703	49.503386
889.603729	79.326931	49.508391
885.480208	90.396284	49.513396
882.206876	82.246790	49.518401
878.940458	86.203637	49.523405
875.235323	83.110490	49.528410
871.938456	77.600011	49.533415
868.444413	87.761474	49.538420
864.692967	76.529054	49.543425
861.274181	85.786644	49.548429
857.772591	80.421927	49.553434
854.362140	80.563650	49.558439
850.818430	77.907277	49.563444
847.732061	81.314091	49.568449
843.734786	80.911263	49.573453
840.115034	81.803725	49.578458
837.092945	72.321187	49.583463
832.920708	77.975572	49.588468
829.684903	76.543072	49.593473
826.507808	84.750661	49.598477
822.582875	94.147156	49.603482
819.449291	80.107287	49.608487
815.525589	86.460125	49.613492
812.269635	73.821841	49.618497
808.777181	80.737120	49.623501
805.008773	80.286016	49.628506
801.712421	85.104887	49.633511
798.226146	86.916189	49.638516
795.144422	83.090109	49.643521
791.187469	86.335064	49.648525
787.795976	84.398468	49.653530
784.617522	76.003276	49.658535
780.829932	76.969327	49.663540
777.519971	83.128554	49.668545
773.782829	84.143698	49.673549
769.678353	72.225957	49.678554
766.674171	69.941180	49.683559
762.957755	86.698731	49.688564
759.623781	76.518128	49.693569
756.509754	76.544118	49.698573
753.288202	83.075553	49.703578
749.332220	81.309091	49.708583
745.558255	79.381422	49.713588
742.006759	81.541396	49.718593
738.603585	77.543908	49.723597
734.875437	81.174020	49.728602
732.214093	79.060498	49.733607
728.486517	80.498092	49.738612
724.902632	77.288019	49.743617
721.191222	73.335354	49.748621
717.302868	77.379538	49.753626
714.038289	76.179316	49.758631
710.253392	79.179201	49.763636
706.678881	70.352147	49.768641
703.938192	75.650821	49.773645
700.360067	75.571897	49.778650
697.325190	69.682152	49.783655
692.794568	78.682564	49.788660
689.432317	75.162756	49.793665
685.890466	77.242142	49.798669
682.397058	73.084708	49.803674
679.668379	73.095011	49.808679
675.801143	76.952419	49.813684
672.645202	75.713145	49.818689
668.712543	82.548267	49.823693
664.959144	76.957035	49.828698
661.988878	68.703462	49.833703
658.118396	78.670434	49.838708
654.503317	76.756010	49.843713
650.988873	77.296750	49.848717
646.989712	78.472919	49.853722
644.366359	74.970967	49.858727
640.596282	77.860987	49.863732
637.058427	77.994096	49.868737
633.505789	74.070512	49.873741
630.218785	86.948986	49.878746
626.843207	77.600606	49.883751
622.995566	90.547377	49.888756
619.565518	83.985183	49.893761
615.973335	81.108605	49.898765
612.298526	73.809419	49.903770
608.957937	78.062564	49.908775
605.404291	79.745173	49.913780
602.139026	76.944252	49.918785
598.981935	73.262810	49.923789
595.295210	79.468045	49.928794
591.974081	71.167867	49.933799
587.898380	74.788824	49.938804
584.408167	76.518506	49.943809
580.969977	79.844072	49.948813
577.357643	78.274072	49.953818
574.140864	68.828222	49.958823
570.705643	72.162818	49.963828
567.241656	73.192411	49.968833
563.501252	78.131044	49.973837
559.713108	78.553057	49.978842
556.499158	65.531821	49.983847
553.045313	76.000235	49.988852
549.519226	79.801384	49.993857
546.224929	74.173504	49.998861
542.195533	78.394684	50.003866
539.254322	73.097807	50.008871
535.575509	77.957254	50.013876
532.281221	69.769965	50.018881
528.834813	81.252764	50.023885
524.719384	74.126590	50.028890
521.408646	78.362441	50.033895
517.951345	81.074073	50.038900
514.138831	74.413260	50.043905
510.944098	74.075365	50.048909
507.844714	75.415191	50.053914
504.647909	77.491500	50.058919
500.378664	78.045364	50.063924
496.922427	70.130060	50.068929
493.252121	71.372110	50.073933
489.792902	79.338901	50.078938
486.521375	75.498125	50.083943
482.900784	78.440820	50.088948
479.341878	70.487721	50.093953
475.932529	74.359286	50.098957
472.420258	74.339741	50.103962
469.329400	73.590221	50.108967
465.109547	73.332828	50.113972
461.495235	70.950091	50.118977
458.386281	73.446151	50.123981
454.746081	78.416651	50.128986
451.774751	75.411810	50.133991
447.972286	80.863141	50.138996
444.260827	76.685909	50.144001
441.027133	72.573502	50.149005
437.065113	80.144022	50.154010
433.901665	63.337532	50.159015
430.601573	71.032785	50.164020
426.981331	71.261003	50.169025
423.360022	73.972868	50.174029
420.016334	83.320021	50.179034
416.552080	71.511503	50.184039
412.889034	78.848824	50.189044
409.264002	73.636279	50.194049
405.872455	83.848238	50.199053
402.147383	73.064228	50.204058
399.030107	76.267088	50.209063
395.497665	84.991912	50.214068
391.900625	77.044765	50.219073
388.353067	77.185744	50.224077
384.545324	88.566621	50.229082
381.378530	69.204415	50.234087
378.024716	81.988889	50.239092
374.340869	75.906006	50.244097
370.867086	80.483621	50.249101
367.449483	88.105432	50.254106
364.071238	83.034801	50.259111
360.212469	78.915318	50.264116
356.753665	77.650470	50.269121
353.171604	72.298373	50.274125
349.475205	79.378307	50.279130
346.382185	70.520660	50.284135
343.204038	79.829388	50.289140
339.599742	80.377830	50.294145
336.104222	80.510715	50.299149
332.314728	83.615761	50.304154
328.792601	78.842777	50.309159
325.405768	81.340985	50.314164
321.654480	82.494428	50.319169
318.235130	77.088531	50.324173
314.711351	87.074316	50.329178
311.245277	74.921264	50.334183
307.529009	81.694256	50.339188
303.849345	75.702483	50.344193
300.858885	71.125137	50.349197
297.449197	75.452340	50.354202
294.037317	77.416627	50.359207
290.256666	79.492109	50.364212
286.937652	76.658476	50.369217
283.169576	72.955148	50.374221
279.710564	71.620744	50.379226
276.004727	66.673900	50.384231
272.501150	76.833702	50.389236
269.211155	77.934318	50.394241
265.810794	82.310692	50.399245
261.996393	89.042023	50.404250
258.918145	81.529811	50.409255
255.557987	84.384532	50.414260
252.002726	75.927887	50.419265
248.190651	80.263960	50.424269
244.704032	82.825167	50.429274
241.342247	85.135992	50.434279
237.419755	77.527439	50.439284
234.148235	80.409490	50.444289
230.985538	77.706549	50.449293
226.910602	84.728373	50.454298
223.734422	81.125887	50.459303
220.328386	75.490151	50.464308
216.662253	70.622555	50.469313
213.635453	74.482043	50.474317
209.910616	75.305526	50.479322
206.343331	71.763935	50.484327
202.601658	82.729582	50.489332
199.031383	86.509176	50.494337
195.329128	76.189884	50.499341
191.511038	89.419962	50.504346
188.617207	71.559181	50.509351
185.186644	81.036926	50.514356
181.813686	73.225776	50.519361
178.416005	78.088945	50.524365
174.662218	90.771190	50.529370
171.186410	80.998760	50.534375
167.435900	82.044539	50.539380
164.354787	81.119539	50.544385
161.087360	78.493023	50.549389
156.986529	85.771980	50.554394
153.394902	84.613260	50.559399
150.120126	76.470463	50.564404
146.591361	74.213659	50.569409
143.581891	80.123672	50.574413
139.688735	82.131272	50.579418
136.340833	78.327752	50.584423
132.581861	84.354459	50.589428
129.255557	82.841232	50.594433
125.646196	82.374957	50.599437
121.990737	81.830440	50.604442
118.668814	68.705898	50.609447
114.804217	83.205516	50.614452
111.340531	83.504314	50.619457
108.042513	76.320570	50.624461
104.814013	73.207127	50.629466
101.399214	73.419224	50.634471
97.594704	82.698939	50.639476
94.097670	77.852491	50.644481
90.482388	74.036827	50.649485
86.777715	88.789953	50.654490
83.341984	74.057013	50.659495
80.318686	78.937831	50.664500
76.710105	71.239315	50.669505
73.247012	71.933484	50.674509
69.255622	90.834518	50.679514
66.210203	74.810149	50.684519
62.801123	67.738618	50.689524
58.979932	75.891504	50.694529
55.650932	69.449729	50.699533
51.737801	76.588742	50.704538
48.289709	80.112054	50.709543
45.018104	82.054532	50.714548
41.588879	79.162170	50.719553
38.194199	73.521538	50.724557
34.443168	79.059813	50.729562
30.844259	77.095515	50.734567
27.508826	73.565312	50.739572
23.858981	81.156867	50.744577
20.786412	76.728387	50.749581
17.238875	89.318416	50.754586
13.536257	77.275030	50.759591
9.852815	68.164540	50.764596
6.319039	71.634760	50.769601
2.891650	73.949499	50.774605