Fri Aug 26 14:18:25 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.131955	109.487092	0.000000
0.727550	93.140103	0.005005
0.522813	107.202800	0.010010
0.659767	100.926883	0.015014
1.033107	85.904602	0.020019
0.498100	94.678452	0.025024
0.791622	86.331274	0.030029
0.510742	85.580898	0.035034
0.442188	68.716582	0.040038
-0.038889	68.392835	0.045043
-0.314044	61.336400	0.050048
-0.444289	39.103501	0.055053
-0.892231	41.068244	0.060058
-1.597816	30.247654	0.065062
-1.892187	24.994343	0.070067
-2.546805	21.505494	0.075072
-2.253832	17.672962	0.080077
-2.520857	20.498519	0.085082
-2.684406	13.889783	0.090086
-2.868653	6.047285	0.095091
-3.178827	13.337139	0.100096
-3.366177	1.632313	0.105101
-3.994882	3.523959	0.110106
-3.981971	5.397963	0.115110
-4.153312	2.378020	0.120115
-4.751311	-2.723609	0.125120
-5.263445	-1.745424	0.130125
-5.340707	-12.328469	0.135130
-5.428066	-10.859620	0.140134
-5.506712	-17.816910	0.145139
-5.961519	-2.956091	0.150144
-6.544321	-12.090566	0.155149
-6.750604	-5.417988	0.160154
-7.064660	-7.915853	0.165158
-6.856955	-7.249056	0.170163
-6.969835	-0.363236	0.175168
-7.308226	-7.533179	0.180173
-7.883179	-0.654507	0.185178
-8.373382	-6.889685	0.190182
-8.025213	-5.665810	0.195187
-8.448758	-1.474500	0.200192
-8.490780	-6.058436	0.205197
-9.470113	-13.014693	0.210202
-9.923781	-4.269374	0.215206
-9.909459	-9.289173	0.220211
-10.088317	-3.475048	0.225216
-10.094530	-0.202900	0.230221
-10.144426	-7.246925	0.235226
-10.396560	-2.690012	0.240230
-10.075276	-7.684841	0.245235
-10.692984	-8.249896	0.250240
-10.880349	-4.699616	0.255245
-10.984705	-5.648308	0.260250
-12.016443	-11.663131	0.265254
-12.379901	-18.164802	0.270259
-12.590014	-9.818063	0.275264
-12.478870	-9.689869	0.280269
-12.494017	-3.543742	0.285274
-13.340683	-14.449901	0.290278
-13.560826	-14.959800	0.295283
-13.960599	-12.018670	0.300288
-13.981539	-23.632333	0.305293
-14.009972	-10.622201	0.310298
-14.163052	-7.301878	0.315302
-13.880877	-11.208650	0.320307
-14.414830	-9.600667	0.325312
-14.985838	-21.707634	0.330317
-15.224865	-9.079149	0.335322
-15.437852	-7.616049	0.340326
-15.795079	-14.998184	0.345331
-16.698967	-5.255821	0.350336
-16.689936	-14.049022	0.355341
-16.867029	-7.896663	0.360346
-17.035459	-1.290087	0.365350
-16.837944	-17.107451	0.370355
-17.140547	-9.277803	0.375360
-17.147439	-14.284807	0.380365
-17.560936	-9.370589	0.385370
-18.247278	-8.213426	0.390374
-18.111708	-8.962201	0.395379
-18.808024	1.222394	0.400384
-18.438797	-4.792267	0.405389
-19.022031	-10.630156	0.410394
-19.885096	-0.890983	0.415398
-19.858535	-15.182164	0.420403
-20.099571	-3.878928	0.425408
-19.884537	-3.760582	0.430413
-20.287008	-7.820176	0.435418
-20.495849	-2.213347	0.440422
-20.631291	-8.026048	0.445427
-21.459979	-4.692280	0.450432
-21.746159	-6.558592	0.455437
-21.506280	-2.581305	0.460442
-22.062150	-3.579916	0.465446
-22.173442	1.002523	0.470451
-21.851648	6.086989	0.475456
-21.969959	-4.211267	0.480461
-22.585840	-2.141290	0.485466
-23.108118	-6.270812	0.490470
-23.269740	-3.417378	0.495475
-24.150751	-10.012470	0.500480
-24.335191	-21.926532	0.505485
-24.128032	-16.134550	0.510490
-24.635868	-14.223761	0.515494
-24.619296	-10.679926	0.520499
-24.991434	0.441251	0.525504
-24.833195	-7.312199	0.530509
-24.647379	-10.457348	0.535514
-25.241742	2.786435	0.540518
-25.821561	-5.769559	0.545523
-26.256012	4.244556	0.550528
-26.490517	-5.209896	0.555533
-26.610966	-8.655362	0.560538
-26.472647	-7.629760	0.565542
-26.854232	-12.951735	0.570547
-27.472162	-7.179976	0.575552
-27.749057	-2.752082	0.580557
-27.921838	-6.274818	0.585562
-27.988065	0.932756	0.590566
-28.390437	-6.075370	0.595571
-29.164232	-11.361587	0.600576
-29.035821	-9.587823	0.605581
-28.972161	-9.828710	0.610586
-29.429860	-1.497200	0.615590
-29.323712	-11.533017	0.620595
-29.596267	-7.425327	0.625600
-30.126294	-8.870872	0.630605
-30.215135	-9.768197	0.635610
-30.766892	-4.592016	0.640614
-30.544865	-14.411763	0.645619
-31.213122	-15.275820	0.650624
-31.533036	-17.114732	0.655629
-31.729346	-18.125034	0.660634
-32.014699	-12.620187	0.665638
-31.765414	-14.841943	0.670643
-32.094069	-11.408866	0.675648
-32.468699	-5.985026	0.680653
-33.064975	-13.070523	0.685658
-33.530978	-14.671562	0.690662
-33.294442	-20.529521	0.695667
-33.706208	-6.586538	0.700672
-33.653252	-9.198490	0.705677
-34.041661	-10.052337	0.710682
-34.815162	-4.313302	0.715686
-34.846067	-17.197201	0.720691
-34.843808	-4.947955	0.725696
-34.854972	-6.765341	0.730701
-34.878208	-3.072943	0.735706
-35.532426	-6.280283	0.740710
-36.245416	-17.454014	0.745715
-36.284933	-3.904334	0.750720
-36.698773	-11.287145	0.755725
-36.301302	-9.387601	0.760730
-36.543352	-6.939247	0.765734
-36.873863	-5.131993	0.770739
-37.797052	-1.998639	0.775744
-37.615102	-7.503265	0.780749
-38.047505	-6.028147	0.785754
-38.228672	-7.967755	0.790758
-37.960560	-8.879530	0.795763
-38.159953	-4.995196	0.800768
-38.908669	-10.025899	0.805773
-39.239420	-3.659797	0.810778
-39.374128	0.439086	0.815782
-39.413590	-10.535807	0.820787
-40.236791	1.905239	0.825792
-40.149464	-3.698547	0.830797
-40.629508	-5.882675	0.835802
-41.118172	-4.534835	0.840806
-40.853708	-9.081069	0.845811
-41.293357	3.259132	0.850816
-41.202197	-6.154279	0.855821
-41.373610	-7.677804	0.860826
-41.846507	-6.373546	0.865830
-42.186893	-7.927708	0.870835
-42.453743	-1.059045	0.875840
-42.580991	-6.306728	0.880845
-42.686512	-11.102229	0.885850
-42.981889	-5.434474	0.890854
-43.770026	-10.617220	0.895859
-44.194905	4.109231	0.900864
-44.427495	-2.703875	0.905869
-43.919632	-8.297208	0.910874
-44.458143	-3.189525	0.915878
-43.842392	-1.165784	0.920883
-44.552055	-8.009008	0.925888
-45.131960	0.214982	0.930893
-45.012593	-6.073974	0.935898
-45.528633	-1.567718	0.940902
-45.697064	-12.259947	0.945907
-46.448823	-7.716991	0.950912
-46.202750	-5.695801	0.955917
-46.416373	-2.676089	0.960922
-46.675431	-6.239173	0.965926
-46.849821	-5.652084	0.970931
-47.848719	-1.143411	0.975936
-47.963493	-5.845727	0.980941
-48.062567	-7.250806	0.985946
-48.328512	-11.170308	0.990950
-48.333354	-13.634060	0.995955
-48.462366	-8.922320	1.000960
-49.159051	-12.344501	1.005965
-49.718620	-1.285890	1.010970
-49.787040	-4.457892	1.015974
-49.770444	-6.962946	1.020979
-50.318213	-8.794856	1.025984
-50.542040	0.291150	1.030989
-49.966312	-12.130402	1.035994
-50.350599	3.254093	1.040998
-50.092377	-13.249742	1.046003
-50.648801	-5.905739	1.051008
-51.266140	-2.449859	1.056013
-51.241295	-11.603013	1.061018
-52.000402	-5.385345	1.066022
-52.448787	-18.998314	1.071027
-52.785218	-10.650892	1.076032
-52.811515	-8.970095	1.081037
-52.554712	-14.075100	1.086042
-52.780986	-9.727853	1.091046
-53.200868	-16.736410	1.096051
-53.938516	-11.657833	1.101056
-54.382953	-11.955646	1.106061
-54.314932	-16.224528	1.111066
-54.554649	-8.547037	1.116070
-54.201775	-15.615803	1.121075
-55.018280	-5.089809	1.126080
-55.370926	-4.566712	1.131085
-55.625964	-14.432397	1.136090
-55.733803	4.914228	1.141094
-55.833576	-12.432344	1.146099
-55.872382	-10.363636	1.151104
-55.909353	-10.892563	1.156109
-56.755050	-9.859280	1.161114
-57.337847	-5.842486	1.166118
-57.104649	-7.226536	1.171123
-57.074561	-8.018996	1.176128
-57.389089	-9.836602	1.181133
-58.153557	-11.910008	1.186138
-58.892475	-9.820875	1.191142
-58.227340	-15.210911	1.196147
-58.594068	-12.426781	1.201152
-58.698537	-5.172129	1.206157
-58.836592	-11.057184	1.211162
-59.538438	-3.225483	1.216166
-59.501583	-12.627269	1.221171
-60.066430	-5.946320	1.226176
-60.463061	-7.596125	1.231181
-60.077391	-4.252122	1.236186
-60.948634	-7.770506	1.241190
-61.072387	-17.201066	1.246195
-61.344914	-11.559016	1.251200
-61.843111	-10.314092	1.256205
-61.853074	-12.172791	1.261210
-62.323178	-10.356458	1.266214
-61.630933	-9.382303	1.271219
-61.632147	-13.963097	1.276224
-62.135650	-7.886465	1.281229
-62.659325	-9.003978	1.286234
-63.087553	-4.631613	1.291238
-63.810656	-6.508987	1.296243
-64.464949	-5.726959	1.301248
-64.442255	-12.722171	1.306253
-64.162588	2.160325	1.311258
-64.674453	-6.077226	1.316262
-64.446191	-10.241349	1.321267
-64.412460	-9.971393	1.326272
-64.528387	-12.775341	1.331277
-65.654982	-16.098946	1.336282
-65.765159	-14.768909	1.341286
-66.013907	-7.203903	1.346291
-65.841441	-10.925920	1.351296
-66.404231	-9.177410	1.356301
-67.056497	-8.364061	1.361306
-67.581935	-12.569014	1.366310
-67.539618	-8.054787	1.371315
-67.450499	-10.412951	1.376320
-67.607572	-12.514491	1.381325
-67.777237	-17.271529	1.386330
-67.750353	-9.303366	1.391334
-68.089512	-10.436953	1.396339
-68.660603	-11.989994	1.401344
-68.938246	-13.443196	1.406349
-69.010866	-11.198387	1.411354
-69.498143	-13.549060	1.416358
-69.905888	-13.703894	1.421363
-70.470148	-7.064164	1.426368
-70.799557	-1.777074	1.431373
-70.623854	-11.124552	1.436378
-70.906308	-2.092693	1.441382
-70.813683	-10.180760	1.446387
-70.967358	-4.082668	1.451392
-70.817260	-4.409777	1.456397
-71.185980	-8.085494	1.461402
-72.039447	-4.010739	1.466406
-71.848483	-8.763820	1.471411
-72.804904	-2.645139	1.476416
-73.285135	-6.648332	1.481421
-73.320924	-11.461016	1.486426
-73.509919	-1.747707	1.491430
-74.050294	-8.591978	1.496435
-73.613852	-11.336402	1.501440
-73.773906	-2.753857	1.506445
-73.825110	-12.287459	1.511450
-73.914578	1.387053	1.516454
-74.445290	-6.151561	1.521459
-74.928225	0.829837	1.526464
-75.255195	3.610942	1.531469
-75.125654	-12.572309	1.536474
-76.550373	-3.495473	1.541478
-75.953042	-11.522922	1.546483
-76.162243	-7.646553	1.551488
-76.665345	-4.221114	1.556493
-76.629470	-11.455652	1.561498
-77.112191	-9.602554	1.566502
-76.933731	-6.700836	1.571507
-77.321783	-11.306817	1.576512
-77.973140	-7.526114	1.581517
-78.003425	-5.999715	1.586522
-78.552304	-5.876319	1.591526
-78.049398	-12.013026	1.596531
-78.244572	-11.773865	1.601536
-78.725723	-8.984574	1.606541
-79.174093	-11.151486	1.611546
-79.779544	-10.516263	1.616550
-79.577071	-17.314846	1.621555
-79.897215	-5.470972	1.626560
-80.673044	-3.271690	1.631565
-80.918260	-14.081668	1.636570
-81.066300	-10.885514	1.641574
-81.170517	-11.179353	1.646579
-81.163497	-7.814360	1.651584
-81.574902	-4.668944	1.656589
-81.120082	-9.940817	1.661594
-81.777982	-10.180084	1.666598
-82.201469	-13.489781	1.671603
-82.486873	-0.879384	1.676608
-82.391948	-5.013256	1.681613
-82.558333	-13.092630	1.686618
-83.829069	-0.730599	1.691622
-84.181824	-11.874998	1.696627
-84.177408	-7.158725	1.701632
-84.419718	-11.993034	1.706637
-84.297090	-8.579605	1.711642
-84.512152	-7.951383	1.716646
-84.200934	-10.834492	1.721651
-84.721809	-7.583451	1.726656
-85.161132	-9.400608	1.731661
-85.391624	-11.958935	1.736666
-85.839644	-5.587232	1.741670
-85.600220	-9.212109	1.746675
-85.648972	-4.155374	1.751680
-86.508986	-8.058306	1.756685
-86.919875	-17.700410	1.761690
-87.346291	-5.064898	1.766694
-87.460675	-11.355419	1.771699
-87.559649	-13.776041	1.776704
-87.675472	-14.618547	1.781709
-87.909840	-17.982998	1.786714
-88.315161	-8.561867	1.791718
-88.711375	-17.140110	1.796723
-88.491080	-13.349597	1.801728
-88.758257	-11.479441	1.806733
-88.793017	-16.845920	1.811738
-90.013160	-12.442002	1.816742
-90.365542	-5.680243	1.821747
-90.281552	-7.866772	1.826752
-90.430230	-4.449063	1.831757
-90.272795	-2.993020	1.836762
-90.566964	4.259534	1.841766
-90.179607	-9.382326	1.846771
-90.779165	-10.826533	1.851776
-91.889499	-5.038217	1.856781
-91.595358	-10.835545	1.861786
-91.774944	1.081357	1.866790
-92.443140	-8.254943	1.871795
-92.614072	0.914570	1.876800
-93.283819	-4.242317	1.881805
-93.240384	-13.540725	1.886810
-93.558139	-3.430897	1.891814
-93.496137	-3.611417	1.896819
-92.989931	-8.932418	1.901824
-93.701067	-5.183533	1.906829
-94.204565	-9.654484	1.911834
-94.628767	5.865932	1.916838
-94.741976	-5.549877	1.921843
-94.722192	-2.019197	1.926848
-95.203992	-2.988212	1.931853
-95.577736	-4.872525	1.936858
-96.226994	-2.594877	1.941862
-96.293520	1.613607	1.946867
-96.205809	-4.164236	1.951872
-96.454284	-3.704812	1.956877
-96.104740	-13.474810	1.961882
-97.390412	-10.889272	1.966886
-97.196819	-15.810432	1.971891
-97.526973	-10.225848	1.976896
-97.928674	-15.285266	1.981901
-97.728764	-12.712745	1.986906
-98.492000	-8.791240	1.991910
-98.898064	-13.470342	1.996915
-99.112143	-14.032958	2.006912
-98.298002	-10.231840	2.016909
-98.036775	-17.589938	2.026906
-97.756726	-19.071731	2.036902
-96.977470	-9.376444	2.046899
-96.789835	-10.191304	2.056896
-95.932223	-10.125328	2.066893
-95.344932	-13.337004	2.076890
-94.878810	-11.116228	2.086886
-94.875661	-2.716054	2.096883
-93.960518	-8.135977	2.106880
-93.515430	-9.079619	2.116877
-93.033594	-8.046006	2.126874
-92.310164	-11.228196	2.136870
-92.610726	2.556830	2.146867
-91.885196	-5.250521	2.156864
-91.168294	-9.090576	2.166861
-90.019675	-8.883016	2.176858
-89.728511	-6.840898	2.186854
-89.734086	-6.292077	2.196851
-88.957883	-2.218963	2.206848
-88.415375	-6.513354	2.216845
-88.103952	-4.034081	2.226842
-87.646036	-3.804506	2.236838
-87.190670	-6.191048	2.246835
-86.712267	-2.334485	2.256832
-85.947856	-6.600073	2.266829
-85.512617	-4.529705	2.276826
-84.968688	-3.930230	2.286822
-84.252969	-4.063900	2.296819
-84.130302	-8.711056	2.306816
-83.693122	-7.942912	2.316813
-82.861263	-9.855901	2.326810
-82.685767	1.628115	2.336806
-82.066554	-5.953615	2.346803
-81.562231	-5.024869	2.356800
-81.041751	-12.822466	2.366797
-80.200720	-9.899817	2.376794
-79.597154	-15.331411	2.386790
-79.602385	-15.685436	2.396787
-79.512606	-14.372209	2.406784
-78.617832	-9.354580	2.416781
-78.031389	-7.760734	2.426778
-77.063520	-7.620061	2.436774
-77.056420	-8.191409	2.446771
-76.784249	-6.076644	2.456768
-76.108205	-3.562279	2.466765
-75.564982	-14.575457	2.476762
-74.960825	-11.511393	2.486758
-74.647711	-9.795798	2.496755
-73.953056	-6.105949	2.506752
-72.840359	-6.323601	2.516749
-72.814115	-10.445746	2.526746
-72.682569	-9.034488	2.536742
-72.376575	-8.724239	2.546739
-71.335199	-4.584711	2.556736
-71.374461	-4.420271	2.566733
-70.381778	-3.234955	2.576730
-70.048328	-1.649232	2.586726
-69.258370	-6.055008	2.596723
-68.374035	-1.292334	2.606720
-68.430658	-4.574810	2.616717
-68.488505	-10.771372	2.626714
-67.582663	-5.270807	2.636710
-67.128288	-7.939119	2.646707
-66.425934	-5.441521	2.656704
-65.777972	-4.801226	2.666701
-65.531501	-5.504875	2.676698
-64.981932	-4.060504	2.686694
-64.268708	-9.563025	2.696691
-64.122856	-10.162311	2.706688
-63.364306	-8.528741	2.716685
-62.418950	-5.669848	2.726682
-62.672178	-5.373895	2.736678
-62.295004	-6.721930	2.746675
-61.292789	-14.642048	2.756672
-60.879918	-15.758063	2.766669
-60.658170	-8.389748	2.776666
-59.801204	-15.070856	2.786662
-59.641087	-10.740266	2.796659
-59.088418	-10.316375	2.806656
-58.387411	-6.567329	2.816653
-58.053173	-3.299683	2.826650
-56.945204	-12.531855	2.836646
-56.930847	-10.459309	2.846643
-56.898850	-6.998891	2.856640
-55.846468	-9.906027	2.866637
-55.459109	-12.513221	2.876634
-55.239139	-9.509710	2.886630
-54.454621	-7.417699	2.896627
-54.031687	-8.687330	2.906624
-53.295814	-8.795627	2.916621
-52.977944	-6.444065	2.926618
-52.535667	-6.075843	2.936614
-51.877736	-2.548162	2.946611
-51.514085	-0.612359	2.956608
-50.838781	-4.373081	2.966605
-50.169246	-6.884832	2.976602
-49.927498	0.825652	2.986598
-49.686899	-2.889561	2.996595
-48.582432	-1.588604	3.006592
-48.168070	-0.272063	3.016589
-48.238934	-4.892256	3.026586
-47.578263	-6.385798	3.036582
-47.271277	-0.902858	3.046579
-46.387265	3.638132	3.056576
-45.535198	3.666961	3.066573
-45.347582	-3.229872	3.076570
-44.936248	-2.489379	3.086566
-44.285106	-1.843243	3.096563
-44.072411	0.296622	3.106560
-43.098750	-1.581427	3.116557
-42.482306	1.778492	3.126554
-42.356404	2.509575	3.136550
-42.477244	-0.385948	3.146547
-41.557120	-3.472056	3.156544
-40.973500	-1.152367	3.166541
-40.189363	-4.828667	3.176538
-39.373222	-0.448167	3.186534
-39.480544	-1.860145	3.196531
-39.047029	-5.567381	3.206528
-38.451791	-3.734158	3.216525
-37.834332	-9.453011	3.226522
-37.475792	-7.966226	3.236518
-36.594307	-2.569566	3.246515
-36.505406	1.613731	3.256512
-36.220314	-6.340450	3.266509
-35.113745	-13.807998	3.276506
-34.892622	-4.912754	3.286502
-34.593214	-8.681470	3.296499
-33.700750	-8.060236	3.306496
-33.376948	-6.995681	3.316493
-33.287869	-10.243823	3.326490
-32.253884	-3.119173	3.336486
-32.027495	-5.394039	3.346483
-31.091855	-4.025616	3.356480
-30.808750	-9.920485	3.366477
-30.557873	-15.699464	3.376474
-29.964837	-4.907660	3.386470
-29.380107	-3.877394	3.396467
-28.722362	0.825533	3.406464
-27.998503	-2.942749	3.416461
-27.678468	-3.119343	3.426458
-27.716556	-3.604463	3.436454
-27.111914	-6.783998	3.446451
-26.250690	-9.240066	3.456448
-26.069699	-6.708806	3.466445
-25.050933	-2.527741	3.476442
-25.183495	-2.804923	3.486438
-24.503515	1.641127	3.496435
-23.587025	-5.587761	3.506432
-23.422545	-7.133921	3.516429
-22.741324	-5.801910	3.526426
-22.129153	-8.779884	3.536422
-21.907872	-0.169754	3.546419
-21.506410	-3.393678	3.556416
-20.639220	-4.862355	3.566413
-20.101167	-4.151095	3.576410
-20.108368	-8.933251	3.586406
-19.032048	-11.052189	3.596403
-18.866830	-5.059350	3.606400
-18.576978	-11.329057	3.616397
-17.646929	-8.512127	3.626394
-17.063792	-13.230979	3.636390
-17.180923	-4.916607	3.646387
-16.284357	-2.468250	3.656384
-15.543879	-5.922350	3.666381
-15.789438	-8.861808	3.676378
-14.709101	-4.810701	3.686374
-14.239095	-8.675669	3.696371
-14.181065	-8.792463	3.706368
-13.267403	-5.976148	3.716365
-12.844068	-7.651307	3.726362
-12.251716	-11.465634	3.736358
-11.950302	-9.738712	3.746355
-11.559945	-7.439614	3.756352
-10.578839	-9.074908	3.766349
-10.092105	-6.052743	3.776346
-10.166462	-6.076068	3.786342
-9.191548	-5.179410	3.796339
-8.998671	-7.727816	3.806336
-8.482725	-6.493611	3.816333
-7.548208	0.139699	3.826330
-7.239230	-9.170808	3.836326
-7.061104	-6.664443	3.846323
-6.329273	3.386692	3.856320
-5.905813	-6.014498	3.866317
-5.382217	5.032040	3.876314
-4.695184	4.950355	3.886310
-4.519830	8.499326	3.896307
-3.915522	18.361258	3.906304
-3.621645	19.316438	3.916301
-3.039144	31.614566	3.926298
-2.650283	31.579305	3.936294
-2.288047	43.610805	3.946291
-1.882123	61.578129	3.956288
-1.246773	79.728322	3.966285
-0.777483	90.016783	3.976282
-0.381973	105.008123	3.986278
0.000000	118.400594	3.991283
0.268500	124.319110	3.996288
0.432716	139.786002	4.001293
0.442798	138.746720	4.006298
0.704975	134.390625	4.011302
0.838549	146.445531	4.016307
1.198628	153.232462	4.021312
0.834907	154.703226	4.026317
1.035790	168.604743	4.031322
1.354217	163.578675	4.036326
1.049475	158.706580	4.041331
0.584834	138.360553	4.046336
0.881651	149.561163	4.051341
1.121589	156.262400	4.056346
1.182826	152.317227	4.061350
1.078624	169.471048	4.066355
0.988781	158.336216	4.071360
1.439748	162.018091	4.076365
0.918827	159.754885	4.081370
1.055047	158.376431	4.086374
0.970594	166.668889	4.091379
1.219438	165.842360	4.096384
1.535271	174.145262	4.101389
1.129645	159.165111	4.106394
1.351707	155.988980	4.111398
1.154156	157.819839	4.116403
1.374085	155.482414	4.121408
1.394544	166.039545	4.126413
1.042023	160.320696	4.131418
1.217735	156.867051	4.136422
1.234334	163.574591	4.141427
1.234788	164.441339	4.146432
1.065952	164.970621	4.151437
1.071732	174.679015	4.156442
1.471157	166.830989	4.161446
1.114023	170.338136	4.166451
1.110947	161.337929	4.171456
1.106657	163.122881	4.176461
1.001574	166.185833	4.181466
1.168306	165.052558	4.186470
1.258276	169.410721	4.191475
1.136836	166.841713	4.196480
1.252178	172.300049	4.201485
1.313285	186.609312	4.206490
1.459367	176.434295	4.211494
1.658819	186.558620	4.216499
1.903195	184.600189	4.221504
1.397497	173.526932	4.226509
1.245449	170.045223	4.231514
1.547166	163.091914	4.236518
1.287252	172.250067	4.241523
1.580526	178.968318	4.246528
1.937029	179.200677	4.251533
1.631123	177.296288	4.256538
1.911298	168.438634	4.261542
1.069913	167.620503	4.266547
1.475861	171.790268	4.271552
1.501333	184.532731	4.276557
1.823700	183.625153	4.281562
1.650627	177.846722	4.286566
1.064055	178.346136	4.291571
1.514512	178.978309	4.296576
1.703901	187.161702	4.301581
1.865497	178.521817	4.306586
2.080967	175.890861	4.311590
1.775611	192.595143	4.316595
1.882950	192.638512	4.321600
2.053827	176.575190	4.326605
1.590188	171.145715	4.331610
1.559712	170.457586	4.336614
1.284069	175.084642	4.341619
1.897875	181.079125	4.346624
2.069278	193.314830	4.351629
2.128212	191.834514	4.356634
1.722190	176.999938	4.361638
1.558857	178.306629	4.366643
1.794383	187.836894	4.371648
1.923151	183.368683	4.376653
1.692419	186.220253	4.381658
2.143482	192.926597	4.386662
1.728142	197.157803	4.391667
2.175097	190.229325	4.396672
2.218951	185.059344	4.401677
1.810662	185.470889	4.406682
1.736836	185.789232	4.411686
1.700959	188.619955	4.416691
1.981442	190.287806	4.421696
1.675997	188.532037	4.426701
2.084126	190.271761	4.431706
2.138833	192.746703	4.436710
2.215012	198.764789	4.441715
2.132315	181.478635	4.446720
2.032691	182.620387	4.451725
1.962281	186.604902	4.456730
1.983015	182.900140	4.461734
1.887033	186.186300	4.466739
2.052527	186.245923	4.471744
2.204305	187.386497	4.476749
1.967774	191.767028	4.481754
1.950754	180.450005	4.486758
1.854011	188.469146	4.491763
2.094457	189.659189	4.496768
2.188441	189.631872	4.501773
1.764347	192.089615	4.506778
1.946467	185.034699	4.511782
2.024554	191.950971	4.516787
2.108159	198.970787	4.521792
2.308018	202.925880	4.526797
2.335360	206.999580	4.531802
2.542799	191.082410	4.536806
2.055975	196.672473	4.541811
1.981780	196.016460	4.546816
2.048436	194.515959	4.551821
2.128650	216.886495	4.556826
2.264573	203.894202	4.561830
2.171586	206.328868	4.566835
2.322907	206.457136	4.571840
2.442391	209.845790	4.576845
2.172443	212.077061	4.581850
2.135182	205.249278	4.586854
2.136553	210.064161	4.591859
2.402237	205.982743	4.596864
2.468804	207.231496	4.601869
2.430383	214.292463	4.606874
2.679420	207.942111	4.611878
2.295665	211.984909	4.616883
2.226395	207.905023	4.621888
2.439336	210.333186	4.626893
2.191267	206.296957	4.631898
2.848491	211.797483	4.636902
2.541404	213.537838	4.641907
2.652689	215.330109	4.646912
2.743670	207.169430	4.651917
2.555444	213.057849	4.656922
2.812894	216.016909	4.661926
2.481495	220.965862	4.666931
2.826388	216.783525	4.671936
2.762512	204.701844	4.676941
2.665033	215.049582	4.681946
2.181670	214.786297	4.686950
2.353234	218.132044	4.691955
2.101352	225.577420	4.696960
2.589285	222.388355	4.701965
2.685858	243.962293	4.706970
2.957947	232.856482	4.711974
2.503849	221.408173	4.716979
2.869002	221.269036	4.721984
2.562421	227.780151	4.726989
2.799535	227.281306	4.731994
2.905135	228.660021	4.736998
2.481888	230.064130	4.742003
2.599104	230.061670	4.747008
2.732562	232.922981	4.752013
2.649030	237.229082	4.757018
2.816666	236.649308	4.762022
2.759338	239.106899	4.767027
2.599927	242.206796	4.772032
2.746057	239.007672	4.777037
2.798318	236.519174	4.782042
2.882701	233.199954	4.787046
2.941468	239.980050	4.792051
2.994991	237.111713	4.797056
3.021753	233.991285	4.802061
2.666514	245.271333	4.807066
2.842513	233.104829	4.812070
2.861926	238.043458	4.817075
2.869146	233.087970	4.822080
3.077951	243.147597	4.827085
2.626364	241.885966	4.832090
2.986844	244.237379	4.837094
2.872679	239.968327	4.842099
2.557125	245.576031	4.847104
3.131181	247.527203	4.852109
3.337093	257.802419	4.857114
3.107082	242.070369	4.862118
2.869006	245.040148	4.867123
3.197672	248.462679	4.872128
3.066786	248.929109	4.877133
2.953720	260.244225	4.882138
3.397981	263.636106	4.887142
3.349302	252.222729	4.892147
3.173824	244.609710	4.897152
3.353303	243.695904	4.902157
3.221116	243.121683	4.907162
3.042227	236.119791	4.912166
3.121377	234.911564	4.917171
3.302282	226.002900	4.922176
3.297377	238.228122	4.927181
3.250062	238.441100	4.932186
3.112531	232.059181	4.937190
3.078153	236.604396	4.942195
3.313380	248.877658	4.947200
3.448943	249.887885	4.952205
3.271697	255.451912	4.957210
3.456027	249.548210	4.962214
3.304161	260.910496	4.967219
3.212941	262.168001	4.972224
3.667260	252.944676	4.977229
3.339141	247.471931	4.982234
3.490734	235.489555	4.987238
3.063855	242.440176	4.992243
3.126157	248.577496	4.997248
3.567179	253.735219	5.002253
3.687562	263.466945	5.007258
3.856357	261.213396	5.012262
3.474873	252.354316	5.017267
3.237656	240.536876	5.022272
3.688383	239.995281	5.027277
3.220869	244.449752	5.032282
3.408749	258.869046	5.037286
3.339577	260.591345	5.042291
3.543873	258.673947	5.047296
3.791431	259.998926	5.052301
3.619110	263.423532	5.057306
3.493788	257.261161	5.062310
3.613629	264.006448	5.067315
3.372682	263.933205	5.072320
3.349813	266.455036	5.077325
3.481270	268.392866	5.082330
3.613527	265.733725	5.087334
3.457394	262.920173	5.092339
3.566250	272.783411	5.097344
3.579019	263.799668	5.102349
3.415335	267.305187	5.107354
3.639477	258.260063	5.112358
3.869145	264.728827	5.117363
3.678716	267.950614	5.122368
4.001246	263.939425	5.127373
3.791323	268.015280	5.132378
3.913797	264.354772	5.137382
3.623450	275.245092	5.142387
3.816026	256.277212	5.147392
4.072620	269.736709	5.152397
3.445030	267.420496	5.157402
3.544276	266.939952	5.162406
3.198738	263.529479	5.167411
3.772447	264.250030	5.172416
3.985274	275.694747	5.177421
3.692326	269.719819	5.182426
3.924901	289.655990	5.187430
4.178145	292.248728	5.192435
3.964612	284.477105	5.197440
4.106135	272.496272	5.202445
3.868283	271.587332	5.207450
4.103676	261.464799	5.212454
3.986892	269.287784	5.217459
3.544508	273.826933	5.222464
3.904484	268.620363	5.227469
4.179141	290.514637	5.232474
4.253980	279.290815	5.237478
3.845300	274.906261	5.242483
3.598324	276.605625	5.247488
4.395853	283.868653	5.252493
4.324136	291.535938	5.257498
4.291487	278.484416	5.262502
4.420460	279.179302	5.267507
3.966615	273.643868	5.272512
4.151889	263.497500	5.277517
3.784136	262.953628	5.282522
3.882979	264.779479	5.287526
3.772108	271.703055	5.292531
3.928238	296.921852	5.297536
4.520926	291.609441	5.302541
4.138690	296.677060	5.307546
4.632633	290.905469	5.312550
4.392912	292.660652	5.317555
4.173002	284.146553	5.322560
4.039823	275.270947	5.327565
3.955606	294.228246	5.332570
4.019205	285.989538	5.337574
4.183973	285.150785	5.342579
4.219867	296.328839	5.347584
4.569243	292.186915	5.352589
4.122352	293.525109	5.357594
4.478004	286.471607	5.362598
4.091755	289.923200	5.367603
4.209190	289.057016	5.372608
4.425248	292.326248	5.377613
4.515034	292.770976	5.382618
4.540580	289.084425	5.387622
4.309620	287.244284	5.392627
4.727236	297.230302	5.397632
4.776753	294.017737	5.402637
4.056239	298.230044	5.407642
4.515068	279.774331	5.412646
4.637435	296.896162	5.417651
4.677173	293.960361	5.422656
4.426159	285.954132	5.427661
4.416390	289.698278	5.432666
4.588907	293.926562	5.437670
4.585101	286.600002	5.442675
4.355318	284.762842	5.447680
4.593757	279.261986	5.452685
4.348953	290.113587	5.457690
4.318241	285.825203	5.462694
4.346592	296.881047	5.467699
4.391029	291.404066	5.472704
4.550105	286.522994	5.477709
4.126848	294.365234	5.482714
4.274264	289.881439	5.487718
4.338736	300.890533	5.492723
4.455831	310.774656	5.497728
4.760276	301.802427	5.502733
4.727006	314.414926	5.507738
5.141612	306.855536	5.512742
4.777055	307.412132	5.517747
4.414700	308.708692	5.522752
4.797793	306.118056	5.527757
4.808007	324.310887	5.532762
4.818952	314.049266	5.537766
4.939180	319.165207	5.542771
4.971242	313.800875	5.547776
4.789177	299.649487	5.552781
4.870061	296.476330	5.557786
4.676340	286.784420	5.562790
4.984454	292.541803	5.567795
4.743973	298.387767	5.572800
4.817171	300.945266	5.577805
4.937754	305.994710	5.582810
5.000055	302.495420	5.587814
4.805969	308.100049	5.592819
4.783692	317.793907	5.597824
5.107433	313.077012	5.602829
4.966216	311.279842	5.607834
5.313229	311.222621	5.612838
5.076753	305.846319	5.617843
4.891491	294.659820	5.622848
5.097980	281.077527	5.627853
4.772190	284.867712	5.632858
4.706971	280.394880	5.637862
4.516681	296.192346	5.642867
4.569346	299.752770	5.647872
4.974497	307.674839	5.652877
4.617040	310.530340	5.657882
4.935050	307.848599	5.662886
5.408863	309.989390	5.667891
5.054852	307.665376	5.672896
5.382919	306.510137	5.677901
4.809453	315.049641	5.682906
5.135952	310.389264	5.687910
4.849176	304.277324	5.692915
4.824747	312.275771	5.697920
5.086290	304.271986	5.702925
5.057236	311.451754	5.707930
5.198547	318.535398	5.712934
5.260388	330.095405	5.717939
5.028518	337.572513	5.722944
5.005719	332.026894	5.727949
5.008101	330.748358	5.732954
5.252861	335.101443	5.737958
5.166607	332.637663	5.742963
5.415615	331.494731	5.747968
5.619036	331.333319	5.752973
5.495409	331.630944	5.757978
5.540245	336.068941	5.762982
5.279485	331.053910	5.767987
5.337431	330.266588	5.772992
5.604211	322.929521	5.777997
5.248445	323.256963	5.783002
5.542785	321.214809	5.788006
5.580733	326.144250	5.793011
5.239782	320.407729	5.798016
5.214893	323.540477	5.803021
5.264806	322.109011	5.808026
5.596054	326.375863	5.813030
5.468390	331.748699	5.818035
5.485439	333.058954	5.823040
5.337813	334.866240	5.828045
5.385228	333.501599	5.833050
5.396754	331.718610	5.838054
5.634111	326.670317	5.843059
5.491421	339.385290	5.848064
5.522815	337.501132	5.853069
5.557905	340.861823	5.858074
5.364860	330.888214	5.863078
5.866530	331.949010	5.868083
5.633264	336.645438	5.873088
6.000718	322.060467	5.878093
5.533140	339.913260	5.883098
5.872810	339.335170	5.888102
6.023781	336.527574	5.893107
5.673353	334.743993	5.898112
5.858854	327.362633	5.903117
5.403662	344.223262	5.908122
5.533382	333.357851	5.913126
5.810810	338.360738	5.918131
5.261986	344.533131	5.923136
5.654970	336.088094	5.928141
5.624845	333.197965	5.933146
5.477172	341.310525	5.938150
5.375462	334.195338	5.943155
5.558499	335.381674	5.948160
5.539034	331.524956	5.953165
5.185025	332.620904	5.958170
5.744286	343.397967	5.963174
6.252262	353.271873	5.968179
6.103682	355.272296	5.973184
5.975053	345.222211	5.978189
5.864574	341.075945	5.983194
5.537476	333.340964	5.988198
6.016372	332.601994	5.993203
6.309080	338.969223	5.998208
6.188927	332.745911	6.003213
5.914802	336.037688	6.008218
5.839517	333.271647	6.013222
5.751580	329.460391	6.018227
5.701314	325.504067	6.023232
6.000903	323.249128	6.028237
5.661788	334.833601	6.033242
5.857928	327.380982	6.038246
6.439034	333.035765	6.043251
5.477417	333.979547	6.048256
5.696719	333.334779	6.053261
5.705749	349.825747	6.058266
5.893590	349.546539	6.063270
6.252144	352.334858	6.068275
5.883108	347.276571	6.073280
6.004089	335.463408	6.078285
5.739823	332.533805	6.083290
5.783101	344.156822	6.088294
5.985412	351.357530	6.093299
5.945079	355.815119	6.098304
6.092395	355.175230	6.103309
5.783935	341.011852	6.108314
5.875081	341.737940	6.113318
5.927358	341.574750	6.118323
5.772193	346.891762	6.123328
6.017060	343.961980	6.128333
6.040955	349.576975	6.133338
5.869538	338.122542	6.138342
5.750592	330.772763	6.143347
5.780181	353.277901	6.148352
6.040590	352.256578	6.153357
5.987637	357.959470	6.158362
5.721345	347.298076	6.163366
6.120187	348.776674	6.168371
5.770164	355.395838	6.173376
6.277161	333.806826	6.178381
5.833843	337.631139	6.183386
5.740019	332.953943	6.188390
5.869995	332.715382	6.193395
5.698732	339.164341	6.198400
5.811601	341.861199	6.203405
5.845981	351.571564	6.208410
5.614130	355.581252	6.213414
6.094337	357.790654	6.218419
6.149689	355.978693	6.223424
6.270629	355.175234	6.228429
5.623366	348.698632	6.233434
5.825713	350.900677	6.238438
6.021852	349.449605	6.243443
5.962161	357.915464	6.248448
6.140652	340.129751	6.253453
5.445661	339.345765	6.258458
6.097524	358.163217	6.263462
5.913685	353.768946	6.268467
5.389219	351.930204	6.273472
5.692521	359.172138	6.278477
6.143125	356.748151	6.283482
5.878595	358.630588	6.288486
6.223329	346.852181	6.293491
6.105729	363.160400	6.298496
5.662234	353.415595	6.303501
5.821514	348.556620	6.308506
5.900348	367.263987	6.313510
6.156716	355.258891	6.318515
6.031164	355.765621	6.323520
6.016708	342.746021	6.328525
5.509524	340.619855	6.333530
5.732254	352.828697	6.338534
5.844003	350.909880	6.343539
5.784760	357.195874	6.348544
5.853173	359.254259	6.353549
5.768418	360.004571	6.358554
6.183840	360.243579	6.363558
6.053929	360.042317	6.368563
6.193030	351.193882	6.373568
5.988372	346.663651	6.378573
5.745230	341.332667	6.383578
5.627932	349.753708	6.388582
6.028922	356.148376	6.393587
5.749485	355.280707	6.398592
5.991087	361.238291	6.403597
5.725161	363.127273	6.408602
5.701825	354.585698	6.413606
6.037427	358.500708	6.418611
5.789598	361.902289	6.423616
6.164490	357.294476	6.428621
6.033796	371.725499	6.433626
5.812867	355.817930	6.438630
5.378143	363.238048	6.443635
5.984978	361.776814	6.448640
6.588952	364.757875	6.453645
6.120633	372.306613	6.458650
5.703600	358.697956	6.463654
5.852546	355.011161	6.468659
5.892572	362.426964	6.473664
6.040166	363.160082	6.478669
5.707184	362.262784	6.483674
5.585974	360.297981	6.488678
5.293052	367.120228	6.493683
5.493040	362.254911	6.498688
5.866749	360.867939	6.503693
5.866514	360.326952	6.508698
5.841990	359.302536	6.513702
6.352331	351.377050	6.518707
6.264441	353.042161	6.523712
6.387448	352.602208	6.528717
6.217888	364.214084	6.533722
6.078409	363.223384	6.538726
6.074179	349.246746	6.543731
5.848794	352.107001	6.548736
5.460958	340.945686	6.553741
5.795938	346.319260	6.558746
5.455972	359.605956	6.563750
6.043690	358.460906	6.568755
6.046969	362.244164	6.573760
6.162115	356.961794	6.578765
6.356251	362.945752	6.583770
5.611099	349.793144	6.588774
5.894061	351.441643	6.593779
5.757128	348.144204	6.598784
6.211828	353.166950	6.603789
5.886171	351.116923	6.608794
5.937947	355.171035	6.613798
6.048972	341.632032	6.618803
5.925227	332.954242	6.623808
5.509232	335.692314	6.628813
5.816194	344.613600	6.633818
6.021345	355.132597	6.638822
6.126634	353.708324	6.643827
5.870062	345.459327	6.648832
5.853271	339.251556	6.653837
5.716591	343.161004	6.658842
6.024889	361.193569	6.663846
6.491117	350.446595	6.668851
5.862718	339.019020	6.673856
5.701019	334.263808	6.678861
5.615968	337.535638	6.683866
5.664031	348.373313	6.688870
6.543050	351.852543	6.693875
5.552543	336.662753	6.698880
5.807807	342.504310	6.703885
6.243457	337.210009	6.708890
5.709496	339.362180	6.713894
5.733209	335.270952	6.718899
6.047213	356.460002	6.723904
5.884464	348.879757	6.728909
6.074236	358.875974	6.733914
5.620325	344.254356	6.738918
5.869666	346.730653	6.743923
6.074355	361.387856	6.748928
5.567153	352.225601	6.753933
5.730692	361.558362	6.758938
5.538441	358.351791	6.763942
6.107327	354.166185	6.768947
5.566847	360.786531	6.773952
6.203712	356.685252	6.778957
6.150577	362.963969	6.783962
5.754201	364.598019	6.788966
6.293319	358.034773	6.793971
5.851236	372.030230	6.798976
6.085656	358.288508	6.803981
6.201404	360.583129	6.808986
5.835236	352.575816	6.813990
5.704249	345.313326	6.818995
5.456582	350.103747	6.824000
5.886952	349.369169	6.829005
6.035912	354.654651	6.834010
5.858533	364.549850	6.839014
6.088648	354.491361	6.844019
5.685862	360.375270	6.849024
5.674260	360.073331	6.854029
5.727066	360.995212	6.859034
5.491747	362.300469	6.864038
5.881049	356.934286	6.869043
5.756231	353.831110	6.874048
5.848800	367.562989	6.879053
5.901430	361.126105	6.884058
5.734068	367.912984	6.889062
6.175356	358.625196	6.894067
6.013323	366.964626	6.899072
5.903276	356.598434	6.904077
5.909884	363.579685	6.909082
5.921282	360.768506	6.914086
6.507896	361.189665	6.919091
6.094779	365.455365	6.924096
5.990462	361.624506	6.929101
6.176403	363.003378	6.934106
5.820200	361.416843	6.939110
6.160320	354.795997	6.944115
6.077133	346.197306	6.949120
6.051878	340.636249	6.954125
5.250331	339.157020	6.959130
5.884749	345.088239	6.964134
6.140947	350.562664	6.969139
5.865520	362.026509	6.974144
5.812754	357.713068	6.979149
6.010559	361.500839	6.984154
6.053935	351.075962	6.989158
5.702920	341.041522	6.994163
5.881802	346.467873	6.999168
5.650042	347.725120	7.004173
5.970249	365.933003	7.009178
5.726478	360.788770	7.014182
6.202288	357.870485	7.019187
5.844678	366.809833	7.024192
5.970124	356.350029	7.029197
6.173418	361.585925	7.034202
5.890667	357.276655	7.039206
5.954373	339.613217	7.044211
5.765156	351.332548	7.049216
5.664993	348.620997	7.054221
6.061022	351.868547	7.059226
6.101224	353.576989	7.064230
5.832239	330.305485	7.069235
5.846019	339.652061	7.074240
6.032436	355.504821	7.079245
5.764174	344.068626	7.084250
5.686182	353.359896	7.089254
5.797905	347.208042	7.094259
5.461557	362.044394	7.099264
5.965638	352.069798	7.104269
6.059471	364.131039	7.109274
5.880399	368.629215	7.114278
5.606077	364.388233	7.119283
5.751808	366.488364	7.124288
5.861418	361.564354	7.129293
6.066303	363.402178	7.134298
5.884201	363.677272	7.139302
5.818791	360.871725	7.144307
5.643363	367.296033	7.149312
5.886650	357.672083	7.154317
6.278263	359.683311	7.159322
6.113486	367.298679	7.164326
6.331981	360.127300	7.169331
6.060248	364.203310	7.174336
5.961113	362.649516	7.179341
6.026815	365.844096	7.184346
5.556265	365.860384	7.189350
6.016539	358.021783	7.194355
6.082636	361.070771	7.199360
6.009452	357.102190	7.204365
5.626703	348.192640	7.209370
5.737609	367.243021	7.214374
5.914238	364.962929	7.219379
5.505089	367.722086	7.224384
5.784664	367.574125	7.229389
6.194855	358.781554	7.234394
6.045986	363.072548	7.239398
6.372963	355.317977	7.244403
5.945492	356.798682	7.249408
5.537149	341.018381	7.254413
6.155107	354.592520	7.259418
5.876017	362.026370	7.264422
5.914284	351.750983	7.269427
6.024591	366.214079	7.274432
5.854225	357.799797	7.279437
5.615090	346.384376	7.284442
5.903088	363.240040	7.289446
5.957947	359.628004	7.294451
5.888969	369.101374	7.299456
5.862936	367.881042	7.304461
6.142766	372.152748	7.309466
6.015363	357.078491	7.314470
5.965466	346.813669	7.319475
5.744921	338.707761	7.324480
5.964277	343.311573	7.329485
5.999171	352.851018	7.334490
5.734244	349.098951	7.339494
5.872653	348.919187	7.344499
6.119050	357.498738	7.349504
5.821632	349.746474	7.354509
5.995292	345.264906	7.359514
5.522688	341.462919	7.364518
5.889492	346.173487	7.369523
6.174623	362.336745	7.374528
6.046071	363.486176	7.379533
5.775622	353.426530	7.384538
5.541662	350.941453	7.389542
5.909622	358.483363	7.394547
5.710478	367.347420	7.399552
5.693589	370.333401	7.404557
6.138009	355.211243	7.409562
5.864218	365.545391	7.414566
6.317189	375.956214	7.419571
5.946688	374.469979	7.424576
6.003835	373.995987	7.429581
5.694650	366.852980	7.434586
5.461086	365.076510	7.439590
6.113730	364.120665	7.444595
5.564411	376.209286	7.449600
5.986849	370.986634	7.454605
5.964590	373.786792	7.459610
5.585171	368.714297	7.464614
5.694367	360.120447	7.469619
5.968518	365.250400	7.474624
5.777939	367.697119	7.479629
5.989197	366.215219	7.484634
6.035662	368.466845	7.489638
6.268289	360.239750	7.494643
5.686643	375.709083	7.499648
5.820199	374.524014	7.504653
6.233871	361.124534	7.509658
6.217768	370.466287	7.514662
6.066088	369.455341	7.519667
6.131632	367.610154	7.524672
5.937996	354.533023	7.529677
6.152179	345.701374	7.534682
5.725230	352.566629	7.539686
5.836853	345.544771	7.544691
5.494958	347.907481	7.549696
5.449817	357.266403	7.554701
5.870583	364.170516	7.559706
6.007117	365.813341	7.564710
6.269046	362.396851	7.569715
6.352061	369.957822	7.574720
6.015181	354.362533	7.579725
5.733446	349.948704	7.584730
5.666578	353.916886	7.589734
5.949959	361.582695	7.594739
6.054561	369.674972	7.599744
5.803654	352.022541	7.604749
5.844179	347.729378	7.609754
5.990597	360.453136	7.614758
6.204003	357.461812	7.619763
5.592000	352.662812	7.624768
5.684345	345.849597	7.629773
5.781918	355.787403	7.634778
5.905334	361.814008	7.639782
6.138465	371.003063	7.644787
5.891186	363.875729	7.649792
5.874856	363.603000	7.654797
5.934573	366.558070	7.659802
5.939336	366.089071	7.664806
6.047405	366.388587	7.669811
5.548458	354.216358	7.674816
5.673617	355.256685	7.679821
5.926434	363.635925	7.684826
5.511636	368.692815	7.689830
5.661084	369.359207	7.694835
5.844666	364.100980	7.699840
6.389612	376.088829	7.704845
6.014534	371.547161	7.709850
6.350077	373.652541	7.714854
6.462935	359.875961	7.719859
5.899606	348.995062	7.724864
5.487538	344.092169	7.729869
5.746796	344.516840	7.734874
5.490669	362.586666	7.739878
5.749827	352.498346	7.744883
5.782029	363.566287	7.749888
5.638449	361.136738	7.754893
5.912516	361.508484	7.759898
5.948728	354.485709	7.764902
6.034252	364.311502	7.769907
6.108449	362.515588	7.774912
5.954970	360.603265	7.779917
6.049234	358.734625	7.784922
5.858434	366.335063	7.789926
5.839690	356.321646	7.794931
5.853800	361.795802	7.799936
6.357345	362.751906	7.804941
6.085795	359.820269	7.809946
5.735366	363.823111	7.814950
6.072384	358.265754	7.819955
6.073481	363.843176	7.824960
5.942952	350.952372	7.829965
5.657628	343.005241	7.834970
5.800375	361.357807	7.839974
6.192414	358.019135	7.844979
5.973546	359.198446	7.849984
5.718126	349.288321	7.854989
5.824374	351.729951	7.859994
5.471043	366.467712	7.864998
6.018218	364.784816	7.870003
5.937537	374.952864	7.875008
5.782776	366.820881	7.880013
5.926245	363.805644	7.885018
6.036298	364.851488	7.890022
5.767531	368.139273	7.895027
5.726941	360.897502	7.900032
5.861471	364.834329	7.905037
6.052933	366.952650	7.910042
5.860220	375.382282	7.915046
6.104531	369.709643	7.920051
5.914971	371.188108	7.925056
6.047070	378.915444	7.930061
6.437759	363.067664	7.935066
5.657863	355.131094	7.940070
5.520228	347.667160	7.945075
5.712566	359.817464	7.950080
5.692253	363.866983	7.955085
6.085075	365.175680	7.960090
6.096897	371.583490	7.965094
5.809791	365.057134	7.970099
5.863024	366.412377	7.975104
5.560929	365.870933	7.980109
5.938046	371.807422	7.985114
5.679399	366.637031	7.990118
5.797511	360.000468	7.995136
6.084227	370.855380	8.000154
5.797718	365.898269	8.005171
5.766281	360.661617	8.010189
6.030180	373.344043	8.015206
6.107682	364.562421	8.020224
6.011090	365.053933	8.025242
5.986039	369.270585	8.030259
5.933574	360.786897	8.035277
6.355141	378.455934	8.040294
5.947473	379.260954	8.045312
6.044831	379.914763	8.050330
5.839042	373.143210	8.055347
5.770082	368.802289	8.060365
5.674499	370.909332	8.065382
5.934492	365.548413	8.070400
5.964197	371.798239	8.075418
5.837367	372.505887	8.080435
6.305575	362.281264	8.085453
5.941488	375.503256	8.090470
5.755340	373.897587	8.095488
5.818230	380.236919	8.100506
5.598412	379.299177	8.105523
5.845346	369.711729	8.110541
5.969322	369.484126	8.115558
5.729190	370.711161	8.120576
6.258681	373.828513	8.125594
5.814027	366.333644	8.130611
6.027465	364.331264	8.135629
5.839387	377.910841	8.140646
5.922080	382.893320	8.145664
5.868623	390.926417	8.150682
5.941973	395.575856	8.155699
6.212985	391.039993	8.160717
6.232774	404.729231	8.165734
5.948027	396.887576	8.170752
6.177447	399.890714	8.175770
6.171277	403.952963	8.180787
6.159613	399.558934	8.185805
6.199035	406.034466	8.190822
6.288340	399.930135	8.195840
6.131528	380.253832	8.200858
5.616508	379.081200	8.205875
6.249859	385.603099	8.210893
6.146953	399.365083	8.215910
6.113942	396.848832	8.220928
6.200090	391.716934	8.225946
5.910323	400.326443	8.230963
6.112864	400.884985	8.235981
5.819771	393.710472	8.240998
6.254908	400.266394	8.246016
6.334155	398.464776	8.251034
6.417001	402.500542	8.256051
6.161110	403.190418	8.261069
6.105341	405.376469	8.266086
6.250510	396.953507	8.271104
6.176434	396.220279	8.276122
5.766800	399.032596	8.281139
6.365451	391.403678	8.286157
6.052606	398.088680	8.291174
6.174333	392.957553	8.296192
6.635775	386.224114	8.301210
6.126739	402.782120	8.306227
6.050397	390.767812	8.311245
6.022751	393.549055	8.316262
6.223959	398.699269	8.321280
6.642780	392.158646	8.326298
6.223378	396.127450	8.331315
6.550506	387.489979	8.336333
6.570271	393.747672	8.341350
6.168959	388.675892	8.346368
6.223610	390.977286	8.351386
6.245632	397.849979	8.356403
6.370029	393.147604	8.361421
6.343748	404.310032	8.366438
6.528890	398.853465	8.371456
6.487016	394.404184	8.376474
6.085971	389.654238	8.381491
6.450093	387.590527	8.386509
6.374886	388.050309	8.391526
6.336688	384.581863	8.396544
6.392986	382.521901	8.401562
6.385379	384.971836	8.406579
6.125569	363.156284	8.411597
6.075319	383.151913	8.416614
6.560246	391.845917	8.421632
6.677720	393.083545	8.426650
6.305363	397.199651	8.431667
6.377401	384.815123	8.436685
6.302659	380.071177	8.441702
6.162452	382.958302	8.446720
6.669606	387.158363	8.451738
6.146864	386.255163	8.456755
6.345468	384.431806	8.461773
6.653032	406.587013	8.466790
6.546992	394.350119	8.471808
6.224331	383.910966	8.476826
5.940629	392.144005	8.481843
6.237866	398.197560	8.486861
6.739954	397.144263	8.491878
6.483408	397.648058	8.496896
6.653353	401.215850	8.501914
6.587091	404.728906	8.506931
6.305197	395.454143	8.511949
6.753452	405.264652	8.516966
6.463652	374.621100	8.521984
6.400515	374.659302	8.527002
6.255479	382.716121	8.532019
6.671273	390.136542	8.537037
6.631626	385.721629	8.542054
6.256829	391.299176	8.547072
6.481623	383.255123	8.552090
6.090790	398.254768	8.557107
6.403939	393.854347	8.562125
6.443234	393.958648	8.567143
6.341588	397.294184	8.572160
6.904205	397.629414	8.577178
6.176324	399.279514	8.582195
6.449537	394.617081	8.587213
6.610163	397.163895	8.592231
6.206180	398.930813	8.597248
6.457973	397.575677	8.602266
6.587651	399.833834	8.607283
6.655765	397.434376	8.612301
6.666200	404.829558	8.617319
6.507333	403.579383	8.622336
6.573036	399.375270	8.627354
6.129209	393.858851	8.632371
6.301145	390.881524	8.637389
6.319655	398.578388	8.642407
6.353165	393.587221	8.647424
6.411576	390.078488	8.652442
6.434483	405.436577	8.657459
6.579506	419.958353	8.662477
6.974718	419.180459	8.667495
6.832997	412.272690	8.672512
6.560472	396.013019	8.677530
6.045623	409.880172	8.682547
6.327406	415.431235	8.687565
6.863594	416.909770	8.692583
6.612864	430.357138	8.697600
6.769080	428.048096	8.702618
6.865957	420.904368	8.707635
6.432062	424.155947	8.712653
7.066627	425.051148	8.717671
6.881249	435.578835	8.722688
6.962083	422.697474	8.727706
6.803444	408.812043	8.732723
6.672747	400.798086	8.737741
6.371285	398.178473	8.742759
6.432431	404.798937	8.747776
6.736534	411.012366	8.752794
6.755121	421.760740	8.757811
6.355119	416.420518	8.762829
6.520815	418.871875	8.767847
6.956813	422.852662	8.772864
6.907496	424.100482	8.777882
6.761353	418.771225	8.782899
6.955798	418.857681	8.787917
6.672088	424.111803	8.792935
6.772362	430.688317	8.797952
6.757796	423.763902	8.802970
6.743773	424.513946	8.807987
7.090639	419.994666	8.813005
7.064221	424.807961	8.818023
6.859301	414.157963	8.823040
6.581672	404.901465	8.828058
6.686734	420.918929	8.833075
6.605814	422.976361	8.838093
6.897243	423.338036	8.843111
6.571761	423.028940	8.848128
6.668620	425.749780	8.853146
6.813679	426.522390	8.858163
6.504287	429.719872	8.863181
6.772821	424.158800	8.868199
6.208844	428.153276	8.873216
6.706894	427.271012	8.878234
6.751138	421.325160	8.883251
6.463814	424.405602	8.888269
6.989301	437.672164	8.893287
7.069548	434.084286	8.898304
7.339693	443.253548	8.903322
6.645105	430.669629	8.908339
6.450217	436.926045	8.913357
6.718695	443.870832	8.918375
6.885696	451.620335	8.923392
7.212376	449.862234	8.928410
7.266711	451.942789	8.933427
7.082210	442.125844	8.938445
6.868900	432.871940	8.943463
6.699985	436.331561	8.948480
7.212744	439.795495	8.953498
6.982959	431.437207	8.958515
6.800472	432.125122	8.963533
6.982618	434.797972	8.968551
7.032403	449.823727	8.973568
7.148767	453.283113	8.978586
6.914829	438.913945	8.983603
6.976826	442.978212	8.988621
7.002970	448.442862	8.993639
6.891431	442.073155	8.998656
7.593385	441.752405	9.003674
6.860903	439.777379	9.008691
6.639980	437.416606	9.013709
7.053654	439.034132	9.018727
7.488466	445.391316	9.023744
6.931816	432.164255	9.028762
6.908777	432.142568	9.033779
6.869467	439.873697	9.038797
7.175711	446.721091	9.043815
7.101451	460.459728	9.048832
7.302255	449.749694	9.053850
7.454529	433.957155	9.058867
6.775846	433.583135	9.063885
6.877139	434.914799	9.068903
6.830747	444.843368	9.073920
6.893350	452.612281	9.078938
7.384998	452.355832	9.083955
7.252435	461.963327	9.088973
7.257042	455.796428	9.093991
7.403248	453.422672	9.099008
7.268843	440.644234	9.104026
7.233026	436.474852	9.109043
7.018727	434.539062	9.114061
6.790894	426.338255	9.119079
7.304068	433.248095	9.124096
7.571192	441.834031	9.129114
7.158918	433.254858	9.134131
7.096051	437.240740	9.139149
7.213419	434.631646	9.144167
7.117730	424.554742	9.149184
7.036385	428.101708	9.154202
7.173110	437.850290	9.159219
7.404666	441.070843	9.164237
7.531806	439.006156	9.169255
7.164990	440.158251	9.174272
7.152703	432.094286	9.179290
7.103490	429.927676	9.184307
6.857289	437.735196	9.189325
7.167095	443.654272	9.194343
7.361268	451.551016	9.199360
7.218943	448.414336	9.204378
7.384959	455.996744	9.209395
7.179042	452.043183	9.214413
7.563949	451.150132	9.219431
7.229671	457.317811	9.224448
7.265039	458.012831	9.229466
7.346895	455.481844	9.234483
7.459583	458.171823	9.239501
7.387666	451.836967	9.244519
7.440774	451.241717	9.249536
7.251416	451.779231	9.254554
7.365063	442.509128	9.259571
7.196636	459.951386	9.264589
7.387020	450.208605	9.269607
7.449879	471.354315	9.274624
7.254346	459.882356	9.279642
7.595870	455.363899	9.284659
7.376810	471.498142	9.289677
7.723814	461.576343	9.294695
7.284460	450.527343	9.299712
7.226254	440.062760	9.304730
7.712280	437.162749	9.309747
7.585376	443.358092	9.314765
7.383701	435.620245	9.319783
7.370905	434.773338	9.324800
7.007530	435.880718	9.329818
7.177725	443.011212	9.334835
7.321950	457.634124	9.339853
7.654232	456.427390	9.344871
7.503315	461.499909	9.349888
7.540099	458.294317	9.354906
7.930316	457.895877	9.359923
7.312701	449.064659	9.364941
7.273062	442.068404	9.369959
7.413214	449.023706	9.374976
7.669097	455.945214	9.379994
7.567043	452.616079	9.385011
7.404590	464.519236	9.390029
7.659297	454.775905	9.395047
7.827656	455.535421	9.400064
7.216781	440.489671	9.405082
7.469632	436.594066	9.410099
7.248869	456.777265	9.415117
7.573725	448.411504	9.420135
7.757773	453.267774	9.425152
7.399465	453.216240	9.430170
7.542079	446.485084	9.435187
7.302166	456.244983	9.440205
7.470752	448.430548	9.445223
7.963452	453.339743	9.450240
7.643543	455.768887	9.455258
7.572452	453.552034	9.460275
7.473381	467.120977	9.465293
7.601303	449.173746	9.470311
7.743729	447.949237	9.475328
7.544663	458.927173	9.480346
7.643331	455.894974	9.485363
7.573607	456.499064	9.490381
7.791624	454.104660	9.495399
7.805409	453.304104	9.500416
7.751182	461.592961	9.505434
7.731358	458.986290	9.510451
7.750623	462.823697	9.515469
7.879850	454.661953	9.520487
8.061904	452.178479	9.525504
7.585462	449.914290	9.530522
7.547628	436.956725	9.535539
7.274211	439.574279	9.540557
7.695579	448.672664	9.545575
7.678113	450.325762	9.550592
7.835954	449.682650	9.555610
7.875415	453.516910	9.560627
7.981706	462.377194	9.565645
7.622869	459.110128	9.570663
7.619740	452.389038	9.575680
7.615807	460.098890	9.580698
7.648225	451.734481	9.585715
7.642897	453.474048	9.590733
7.931380	454.388422	9.595751
7.804354	456.554017	9.600768
7.883206	452.552962	9.605786
7.865242	453.063791	9.610803
7.937829	461.165653	9.615821
7.152373	462.777388	9.620839
7.688305	459.645551	9.625856
7.646428	461.611706	9.630874
7.712581	455.015522	9.635891
7.792782	463.914581	9.640909
7.742040	457.967727	9.645927
7.809063	458.818757	9.650944
8.051524	465.874896	9.655962
7.827199	451.510532	9.660979
7.587956	461.639542	9.665997
7.982617	465.386944	9.671015
7.456232	461.931380	9.676032
7.853932	465.798224	9.681050
8.029934	477.342594	9.686067
7.957505	480.367498	9.691085
7.747345	480.409657	9.696103
8.273709	479.321019	9.701120
7.767471	475.530971	9.706138
8.019258	469.278247	9.711155
7.873880	463.270390	9.716173
7.847289	468.642276	9.721191
7.983810	474.954399	9.726208
7.764662	483.571887	9.731226
8.153743	480.103166	9.736243
7.993326	484.729067	9.741261
8.023628	485.939250	9.746279
8.088475	490.287094	9.751296
7.729813	493.934052	9.756314
7.748560	486.628901	9.761331
7.844893	479.504169	9.766349
7.636889	482.073677	9.771367
7.920595	483.354854	9.776384
7.824845	486.863050	9.781402
8.026317	478.238788	9.786419
8.008142	474.685160	9.791437
7.770135	479.136957	9.796455
7.876349	489.433092	9.801472
7.850833	487.953874	9.806490
8.028733	478.822065	9.811507
8.099142	497.902829	9.816525
8.006007	483.145645	9.821543
8.441221	495.754150	9.826560
8.194858	494.905738	9.831578
8.348967	482.495741	9.836595
8.082333	492.272443	9.841613
8.168100	481.706527	9.846631
8.001995	492.792955	9.851648
8.014660	482.907422	9.856666
8.265287	474.912951	9.861683
8.077713	479.574636	9.866701
8.313661	478.288229	9.871719
8.624801	480.262535	9.876736
8.640901	478.464429	9.881754
8.761979	486.388347	9.886771
8.608536	486.680440	9.891789
8.314173	488.660664	9.896807
8.522868	484.610984	9.901824
8.325534	492.123754	9.906842
8.322129	482.537355	9.911859
8.175563	481.897457	9.916877
8.215443	489.594189	9.921895
8.157473	481.650919	9.926912
7.901760	492.022340	9.931930
8.301774	485.068065	9.936947
8.327881	486.547132	9.941965
8.260244	491.739231	9.946983
8.504020	476.506738	9.952000
8.236068	480.799103	9.957018
8.197961	482.704715	9.962035
8.441553	480.019160	9.967053
8.237859	489.353736	9.972071
8.049653	483.526102	9.977088
8.534971	487.603362	9.982106
8.273453	481.591492	9.987123
7.976921	480.432170	9.992141
7.866842	485.457314	9.997159
8.159153	478.504031	10.002176
8.472584	492.352736	10.007194
8.469784	488.607371	10.012211
8.161696	494.745740	10.017229
8.129004	487.104631	10.022247
8.340583	481.132705	10.027264
8.326861	487.477692	10.032282
8.404982	496.904087	10.037299
8.756172	501.907909	10.042317
8.706581	499.214352	10.047335
8.428452	480.907451	10.052352
8.132097	484.308031	10.057370
8.161125	486.998418	10.062387
8.464009	486.894429	10.067405
8.491506	503.545710	10.072423
8.594144	508.600854	10.077440
8.694247	515.521394	10.082458
8.553080	500.449796	10.087475
8.403870	483.943638	10.092493
8.237148	496.049442	10.097511
8.274968	508.293815	10.102528
8.639750	511.970143	10.107546
8.336906	521.724098	10.112563
8.350765	504.747582	10.117581
8.283844	512.353659	10.122599
8.600587	506.756654	10.127616
8.536754	509.467814	10.132634
8.579232	506.201369	10.137651
8.534474	511.579252	10.142669
8.322517	510.940067	10.147687
8.539299	506.103363	10.152704
8.418427	509.848994	10.157722
8.598441	512.089862	10.162739
8.711327	503.059676	10.167757
8.409604	515.486302	10.172775
8.733776	512.125506	10.177792
8.737055	508.830451	10.182810
8.493123	522.993167	10.187827
8.597229	512.077255	10.192845
8.446093	521.432065	10.197863
8.723791	506.096439	10.202880
8.528106	517.790220	10.207898
8.684293	523.663817	10.212915
8.638825	502.467945	10.217933
8.416075	510.808308	10.222951
8.608498	519.428002	10.227968
8.925672	528.141881	10.232986
8.864316	534.020951	10.238003
9.280533	519.878680	10.243021
8.862172	511.710653	10.248039
8.741595	506.961187	10.253056
8.899591	510.070135	10.258074
8.828595	515.783449	10.263091
8.502016	505.051357	10.268109
8.383094	511.308594	10.273127
8.731797	499.915969	10.278144
8.724337	512.757504	10.283162
8.899173	516.804219	10.288179
8.963600	518.788541	10.293197
8.523818	516.281960	10.298215
9.024675	528.387984	10.303232
8.867706	526.544239	10.308250
8.647559	521.983833	10.313267
8.857057	531.288810	10.318285
8.436951	536.441130	10.323303
8.728922	536.796413	10.328320
8.768040	524.861862	10.333338
8.811302	528.146460	10.338355
8.948992	529.983683	10.343373
8.928752	529.491365	10.348391
9.235831	532.113222	10.353408
9.086481	531.697808	10.358426
8.713773	536.934263	10.363443
9.462554	532.939333	10.368461
9.174977	540.576622	10.373479
9.112041	532.520499	10.378496
8.913136	514.964899	10.383514
8.864281	524.477348	10.388531
9.111871	525.338135	10.393549
9.244363	527.955617	10.398567
8.981677	510.602448	10.403584
8.867020	504.267917	10.408602
8.680481	509.636317	10.413619
9.078240	519.801874	10.418637
9.232502	531.021475	10.423655
8.953002	531.055496	10.428672
9.321494	530.518432	10.433690
8.918221	523.159059	10.438707
8.718225	512.703886	10.443725
8.843190	515.202623	10.448743
9.059491	523.080175	10.453760
9.022689	532.420345	10.458778
8.953820	538.366855	10.463795
9.198401	522.379992	10.468813
9.026020	526.783714	10.473831
8.910213	523.819610	10.478848
9.076388	529.376086	10.483866
8.937072	530.262401	10.488883
9.097870	535.248541	10.493901
9.228735	531.504446	10.498919
9.274042	539.247690	10.503936
9.377336	539.786976	10.508954
9.430430	534.092162	10.513971
9.346276	525.304074	10.518989
9.293601	533.693704	10.524007
9.393564	532.346419	10.529024
9.233253	529.278794	10.534042
9.012804	535.580249	10.539059
9.285814	531.760376	10.544077
9.462934	536.797621	10.549095
9.232649	533.280162	10.554112
9.476216	535.135612	10.559130
9.256266	532.531689	10.564147
9.406614	528.500551	10.569165
9.077721	532.439515	10.574183
9.364325	529.425377	10.579200
9.219707	534.503248	10.584218
9.140227	530.899196	10.589235
9.073685	534.541704	10.594253
8.810272	531.890901	10.599271
9.268027	534.041193	10.604288
9.454217	529.486945	10.609306
9.153548	533.178527	10.614323
9.216146	525.999072	10.619341
9.133448	529.044516	10.624359
8.920734	528.850398	10.629376
8.907383	524.623852	10.634394
9.270622	543.567558	10.639411
9.717951	540.929165	10.644429
9.393331	549.995433	10.649447
9.440214	551.808928	10.654464
9.010661	539.953650	10.659482
9.031271	557.985082	10.664499
9.597432	554.239478	10.669517
9.749837	564.686248	10.674535
9.643800	559.489554	10.679552
9.743981	555.784944	10.684570
9.452156	550.121738	10.689587
9.345072	540.822838	10.694605
9.787719	552.461434	10.699623
9.578736	546.513943	10.704640
9.626072	524.341116	10.709658
9.062832	530.052184	10.714675
9.665455	531.381535	10.719693
9.366032	542.624445	10.724711
9.257004	541.060400	10.729728
9.588664	553.713471	10.734746
9.520281	553.130822	10.739763
9.693136	554.517622	10.744781
9.750574	557.658013	10.749799
9.598536	550.010213	10.754816
9.827822	557.778466	10.759834
9.440227	554.320208	10.764851
9.716013	551.787414	10.769869
9.590250	543.731600	10.774887
9.479487	547.772299	10.779904
9.795011	555.303071	10.784922
9.863539	568.530429	10.789939
9.871596	549.910666	10.794957
9.582106	541.072493	10.799975
9.345905	538.916048	10.804992
9.678292	543.275896	10.810010
9.541701	555.594791	10.815027
9.652710	556.517870	10.820045
9.983699	557.050107	10.825063
9.832924	558.203284	10.830080
9.926295	549.311808	10.835098
9.437198	542.429673	10.840115
9.812112	541.872675	10.845133
9.630669	550.294984	10.850151
9.577590	558.851940	10.855168
9.699266	549.981302	10.860186
9.939161	558.113961	10.865203
9.634019	551.089577	10.870221
9.867812	553.476705	10.875239
9.558221	565.607956	10.880256
9.847210	554.193037	10.885274
9.439290	561.467236	10.890291
9.709515	553.602217	10.895309
10.011787	554.940466	10.900327
9.860099	554.926187	10.905344
9.936766	553.159667	10.910362
9.599790	559.371980	10.915379
9.771740	556.587119	10.920397
9.845937	548.859917	10.925415
9.730349	561.055630	10.930432
9.876191	551.505914	10.935450
10.266460	560.202117	10.940467
9.739416	552.495943	10.945485
9.509166	559.164991	10.950503
9.471378	561.928905	10.955520
9.568820	552.374102	10.960538
9.700752	572.354200	10.965555
10.031261	579.191556	10.970573
10.337168	577.534503	10.975591
10.026817	582.423605	10.980608
10.236008	574.394518	10.985626
9.809690	572.305538	10.990643
9.844713	575.187501	10.995661
10.050606	576.316705	11.000679
9.889982	576.224924	11.005696
9.990536	578.184694	11.010714
10.164125	578.959180	11.015731
10.162598	575.873136	11.020749
10.185467	581.906359	11.025767
10.058313	578.126691	11.030784
10.539313	572.472534	11.035802
10.133054	572.576782	11.040819
9.649978	554.077662	11.045837
9.946876	564.669186	11.050855
10.104476	583.531348	11.055872
10.542833	583.027584	11.060890
10.106068	585.377114	11.065907
10.172406	579.052244	11.070925
10.228411	578.219863	11.075943
10.237494	583.191770	11.080960
10.152857	569.812222	11.085978
9.983254	574.856127	11.090995
9.995584	582.733906	11.096013
10.256699	581.550867	11.101031
10.063878	578.964802	11.106048
10.234937	576.467244	11.111066
10.326056	584.689349	11.116083
10.195126	581.408866	11.121101
10.398257	581.225737	11.126119
10.108899	588.790744	11.131136
10.312377	584.707142	11.136154
10.085757	574.073049	11.141171
10.244470	580.025163	11.146189
10.393392	583.974947	11.151207
10.321303	586.529619	11.156224
10.441579	586.870612	11.161242
10.441475	587.135676	11.166259
10.146516	582.182976	11.171277
10.491725	584.622185	11.176295
10.466563	587.349425	11.181312
10.348952	585.212379	11.186330
10.064871	586.711349	11.191347
10.040658	581.984727	11.196365
10.329472	581.390643	11.201383
10.246102	592.189707	11.206400
10.438727	573.698966	11.211418
10.657875	584.435146	11.216435
10.313682	582.213462	11.221453
10.448099	572.435149	11.226471
10.528238	579.538696	11.231488
10.352331	572.828684	11.236506
10.247270	575.508404	11.241523
10.317593	580.019513	11.246541
10.233495	579.025916	11.251559
10.168621	583.390824	11.256576
10.107456	574.356146	11.261594
10.885836	597.934078	11.266611
10.761082	603.456982	11.271629
10.389184	585.697882	11.276647
10.555131	591.500556	11.281664
10.452810	597.461761	11.286682
10.644566	590.325284	11.291699
10.635573	601.743909	11.296717
10.809864	602.612958	11.301735
10.800908	591.304362	11.306752
10.431013	578.729741	11.311770
10.819393	580.092453	11.316787
10.728328	583.416910	11.321805
10.649331	579.273152	11.326823
10.743518	580.930968	11.331840
10.866520	581.375673	11.336858
10.747456	585.136817	11.341875
10.462901	572.836080	11.346893
10.585028	576.954129	11.351911
10.282105	583.227418	11.356928
10.454522	581.218778	11.361946
10.983184	589.653616	11.366963
10.928347	599.375311	11.371981
10.925776	582.562218	11.376999
10.759813	576.478636	11.382016
10.571918	573.869716	11.387034
10.716130	576.128788	11.392051
10.570768	587.183644	11.397069
10.903408	597.454055	11.402087
10.487827	610.643215	11.407104
10.753579	604.675436	11.412122
10.960041	595.693748	11.417139
10.758649	599.350953	11.422157
11.116631	604.669315	11.427175
11.449835	597.785355	11.432192
10.794667	586.466927	11.437210
10.697745	577.141179	11.442227
10.410685	577.760178	11.447245
10.963955	586.342656	11.452263
11.080817	600.562864	11.457280
10.925619	596.027039	11.462298
10.939369	581.193174	11.467315
10.572225	587.261877	11.472333
11.146233	599.886715	11.477351
11.059240	597.631295	11.482368
10.994369	603.485689	11.487386
11.135518	591.999094	11.492403
10.859456	589.637418	11.497421
10.820799	580.460382	11.502439
11.435561	599.409166	11.507456
10.797873	585.825392	11.512474
10.753840	576.715464	11.517491
10.857771	587.949248	11.522509
11.050889	588.988927	11.527527
11.048750	590.974154	11.532544
11.127053	605.594828	11.537562
11.148770	604.957126	11.542579
11.158951	604.740926	11.547597
11.165670	598.624139	11.552615
11.005580	597.462499	11.557632
11.006905	596.578673	11.562650
11.295632	604.284045	11.567667
10.525386	610.705841	11.572685
10.853456	603.832145	11.577703
11.239701	607.972193	11.582720
10.925584	608.636430	11.587738
11.196415	601.913653	11.592755
10.896775	602.900671	11.597773
10.711580	604.936490	11.602791
10.971548	607.543603	11.607808
10.927287	605.729636	11.612826
11.226830	607.402817	11.617843
11.513238	619.318239	11.622861
11.144172	601.019060	11.627879
11.252505	612.425737	11.632896
10.897429	620.427006	11.637914
11.172893	619.610946	11.642931
11.297917	626.483469	11.647949
11.391695	622.764064	11.652967
11.383189	624.447340	11.657984
11.093727	623.668745	11.663002
11.850269	619.770414	11.668019
11.370080	621.987860	11.673037
11.486816	622.143218	11.678055
11.365059	615.689836	11.683072
10.897867	608.368780	11.688090
11.401654	609.072923	11.693107
11.613034	618.892029	11.698125
11.264032	618.378315	11.703143
11.490900	623.079648	11.708160
11.259536	623.210312	11.713178
11.378775	621.137367	11.718195
11.507290	628.722533	11.723213
11.317186	625.615350	11.728231
11.309551	624.701361	11.733248
11.578495	625.814439	11.738266
11.678049	624.432498	11.743283
11.823501	618.230990	11.748301
11.831153	614.310410	11.753319
11.559241	613.690023	11.758336
11.095649	606.434677	11.763354
11.234298	607.214604	11.768371
11.200740	619.252424	11.773389
11.702833	626.552214	11.778407
11.257749	619.890406	11.783424
11.313937	623.823080	11.788442
11.591295	624.988495	11.793459
11.397271	624.166640	11.798477
11.275506	621.146644	11.803495
11.822369	630.796763	11.808512
11.477144	628.496342	11.813530
11.857783	620.986474	11.818547
11.457355	625.662403	11.823565
11.689786	631.846045	11.828583
11.573636	617.597243	11.833600
11.553628	620.913798	11.838618
11.451184	623.914998	11.843635
11.612730	629.118790	11.848653
11.929837	633.916525	11.853671
11.970333	631.196299	11.858688
11.368930	636.499948	11.863706
11.275962	633.585915	11.868723
11.769620	650.701220	11.873741
12.015758	655.330136	11.878759
12.118630	646.244635	11.883776
11.982115	646.654011	11.888794
11.664302	633.124535	11.893811
11.739979	630.133755	11.898829
11.541417	639.881005	11.903847
12.021931	641.188353	11.908864
11.889360	658.498995	11.913882
11.998503	643.924771	11.918899
12.038291	642.618403	11.923917
11.933893	632.432288	11.928935
11.855224	623.356129	11.933952
11.429334	627.243946	11.938970
11.651107	647.689806	11.943987
11.864407	642.130954	11.949005
11.759608	648.133586	11.954023
12.009844	651.616347	11.959040
12.033375	653.547093	11.964058
11.663130	648.290527	11.969075
11.669271	656.153524	11.974093
11.914310	650.157398	11.979111
12.126048	652.424901	11.984128
11.625236	652.932021	11.989146
11.912313	649.835742	11.994163
11.903324	640.944379	11.999181
12.031866	654.244505	12.004199
12.331737	651.417624	12.009216
12.036248	654.357370	12.014234
11.877635	654.940594	12.019251
12.032393	647.648914	12.024269
11.971422	646.986216	12.029287
12.175923	655.392665	12.034304
11.930102	651.953337	12.039322
12.307316	657.492774	12.044339
12.245573	659.013935	12.049357
12.003250	658.622461	12.054375
12.299692	646.840262	12.059392
11.858410	660.352184	12.064410
12.216540	670.722807	12.069427
12.149557	673.961483	12.074445
12.456320	678.293797	12.079463
12.649139	672.668699	12.084480
12.411295	665.027898	12.089498
12.112421	645.673211	12.094515
12.261732	650.986207	12.099533
11.872021	654.530738	12.104551
12.399277	658.734047	12.109568
12.099016	676.985966	12.114586
12.091835	683.926431	12.119603
12.346756	676.972581	12.124621
12.530236	677.843358	12.129639
12.677313	676.939991	12.134656
12.220638	676.787011	12.139674
12.252536	677.372131	12.144691
12.422391	672.583712	12.149709
12.162728	677.808919	12.154727
12.417446	668.911196	12.159744
12.547293	675.328567	12.164762
12.395858	671.385408	12.169779
12.222515	663.816613	12.174797
11.914481	679.665107	12.179815
12.448537	665.567487	12.184832
12.587272	672.800798	12.189850
12.274274	665.452555	12.194867
12.412054	672.244218	12.199885
12.620437	674.171431	12.204903
12.535454	675.800350	12.209920
12.551636	669.350717	12.214938
12.538694	667.938953	12.219955
12.504327	673.902226	12.224973
12.340841	682.520610	12.229991
12.305129	675.148125	12.235008
12.487004	679.443082	12.240026
12.378733	672.940244	12.245043
12.647998	670.209640	12.250061
12.398946	681.564710	12.255079
12.336187	680.630900	12.260096
12.635220	689.524402	12.265114
12.879605	692.531571	12.270131
12.686833	698.819307	12.275149
12.741976	698.858028	12.280167
12.662739	685.789968	12.285184
12.972385	682.219970	12.290202
12.634482	685.147392	12.295219
12.845454	678.474930	12.300237
12.500392	681.829484	12.305255
12.692679	689.022907	12.310272
13.239739	692.942284	12.315290
12.651126	682.916734	12.320307
12.572949	679.908876	12.325325
12.795713	696.454198	12.330343
13.104709	690.978258	12.335360
12.553995	692.130600	12.340378
13.021913	695.342799	12.345395
12.918180	697.501641	12.350413
12.950079	699.579407	12.355431
12.814316	686.516991	12.360448
12.836015	690.830578	12.365466
12.738070	698.081816	12.370483
13.133472	689.256850	12.375501
12.789495	704.546092	12.380519
13.194384	695.981568	12.385536
13.291754	685.934415	12.390554
12.856561	679.356248	12.395571
13.294545	666.362301	12.400589
12.792665	682.676464	12.405607
12.653254	679.902194	12.410624
13.103396	680.627315	12.415642
12.570667	688.334394	12.420659
13.002505	691.476474	12.425677
13.105814	695.837314	12.430695
13.416074	694.460429	12.435712
12.953086	691.544040	12.440730
13.144121	695.897533	12.445747
13.323565	688.601992	12.450765
12.797450	690.346930	12.455783
13.132554	688.644297	12.460800
13.112124	700.071078	12.465818
12.906789	701.993283	12.470835
13.112346	694.826214	12.475853
13.216577	709.310398	12.480871
12.915353	702.345302	12.485888
13.153010	700.859804	12.490906
13.263811	699.851634	12.495923
13.081986	694.499448	12.500941
12.987018	707.764989	12.505959
13.219920	696.768952	12.510976
13.526985	697.080864	12.515994
13.305704	700.548689	12.521011
13.057425	699.672163	12.526029
13.031889	705.283789	12.531047
13.313293	702.636494	12.536064
13.327543	694.710285	12.541082
13.355456	698.562175	12.546099
13.711568	696.518610	12.551117
13.088948	694.453867	12.556135
13.197265	697.131941	12.561152
13.381380	690.324806	12.566170
13.257905	697.561084	12.571187
13.224606	695.619173	12.576205
12.900942	693.359566	12.581223
13.276364	693.723949	12.586240
13.521891	691.883789	12.591258
13.213441	698.729160	12.596275
13.772046	707.345579	12.601293
13.481090	714.248190	12.606311
13.552908	702.308430	12.611328
13.494002	697.514598	12.616346
13.522173	695.509470	12.621363
13.369576	693.459906	12.626381
13.522237	710.880817	12.631399
13.511971	713.946573	12.636416
13.721764	720.749132	12.641434
13.479557	719.694941	12.646451
13.827135	718.905516	12.651469
13.855363	709.948366	12.656487
13.684753	703.748703	12.661504
13.284308	697.982445	12.666522
12.972187	717.725741	12.671539
13.644603	704.723667	12.676557
13.804924	719.221216	12.681575
13.619593	718.530543	12.686592
13.532028	719.550816	12.691610
13.372348	716.924859	12.696627
13.768628	712.757562	12.701645
13.636051	723.453918	12.706663
13.832187	721.454192	12.711680
13.811005	723.057403	12.716698
13.799025	735.107720	12.721715
13.993904	719.595463	12.726733
13.766590	725.939078	12.731751
13.724883	721.578049	12.736768
13.781623	711.373111	12.741786
13.896327	721.579699	12.746803
13.787766	703.902553	12.751821
13.765553	716.329979	12.756839
13.702247	714.566302	12.761856
14.015517	714.224018	12.766874
13.675921	729.080267	12.771891
13.761204	720.341439	12.776909
13.788966	712.744467	12.781927
13.862347	722.039180	12.786944
13.967642	721.786080	12.791962
13.712642	728.582116	12.796979
13.933808	717.553181	12.801997
13.879537	723.361784	12.807015
14.084490	725.311627	12.812032
14.286654	723.651779	12.817050
14.136380	724.435671	12.822067
13.940014	717.179697	12.827085
13.788368	719.424894	12.832103
13.493014	727.432691	12.837120
14.404831	735.902615	12.842138
14.351276	737.289968	12.847155
14.302627	731.213313	12.852173
14.470762	723.884806	12.857191
13.721582	720.845719	12.862208
14.306307	717.826158	12.867226
13.909936	720.791089	12.872243
14.091127	730.091111	12.877261
14.675930	740.167714	12.882279
14.168725	726.093317	12.887296
14.188336	717.061767	12.892314
13.651462	728.991839	12.897331
14.032756	734.284520	12.902349
14.004813	740.006981	12.907367
14.123406	746.924733	12.912384
14.417442	734.189827	12.917402
13.928268	740.687823	12.922419
14.109123	742.751869	12.927437
14.250100	743.152755	12.932455
14.015706	751.472954	12.937472
14.198093	747.695546	12.942490
14.200020	759.071548	12.947507
14.061809	750.689385	12.952525
14.428177	766.388773	12.957543
14.624234	769.248851	12.962560
14.579286	759.832868	12.967578
14.172155	753.114608	12.972595
14.484630	756.499339	12.977613
14.590225	758.641375	12.982631
14.509060	756.265111	12.987648
14.438871	751.170073	12.992666
14.393070	763.758990	12.997683
14.712958	771.980276	13.002701
14.598851	763.471280	13.007719
14.485856	759.790352	13.012736
14.862880	752.041158	13.017754
14.627279	749.098822	13.022771
14.762242	739.089967	13.027789
14.490923	735.566233	13.032807
14.436051	742.151240	13.037824
14.732569	741.549640	13.042842
14.434058	745.610148	13.047859
14.545292	758.909891	13.052877
14.731076	757.315705	13.057895
14.654361	775.744351	13.062912
14.984958	770.239778	13.067930
14.635565	758.315070	13.072947
14.369853	754.904066	13.077965
14.787366	762.769331	13.082983
14.869045	766.155285	13.088000
14.978769	764.311016	13.093018
15.060126	765.349172	13.098035
14.651935	754.339310	13.103053
14.857610	742.025243	13.108071
14.522974	745.677978	13.113088
14.833286	758.306116	13.118106
15.187282	772.038273	13.123123
14.752268	762.316958	13.128141
14.852837	759.123470	13.133159
14.900414	770.662781	13.138176
14.690381	759.110838	13.143194
14.922807	760.182275	13.148211
14.983463	778.046754	13.153229
15.100877	767.876517	13.158247
14.642052	773.293702	13.163264
14.861501	769.762977	13.168282
14.791963	766.570728	13.173299
14.984402	768.762358	13.178317
14.871858	769.306855	13.183335
15.113130	763.800414	13.188352
14.934769	763.058162	13.193370
14.944573	768.509675	13.198387
14.753188	763.256784	13.203405
15.043994	760.617483	13.208423
14.868474	769.152579	13.213440
14.972698	772.752769	13.218458
14.814734	776.520010	13.223475
14.569099	769.284309	13.228493
14.887757	776.331863	13.233511
15.332631	796.367628	13.238528
15.505691	790.944380	13.243546
15.598147	794.360219	13.248563
15.153269	781.071314	13.253581
15.331899	771.560556	13.258599
15.256493	773.692906	13.263616
15.219900	767.440798	13.268634
15.142782	769.150549	13.273651
15.339483	765.168944	13.278669
15.313242	761.932086	13.283687
15.282159	774.790110	13.288704
15.463135	772.982082	13.293722
15.385584	770.857710	13.298739
15.536314	774.406480	13.303757
15.484109	766.679929	13.308775
15.167382	772.336913	13.313792
14.952072	767.917698	13.318810
15.316815	781.528272	13.323827
15.325082	785.780859	13.328845
15.454259	785.849077	13.333863
15.396204	795.378881	13.338880
15.807568	784.774715	13.343898
15.724531	786.141416	13.348915
15.258621	788.842638	13.353933
15.469710	790.491740	13.358951
15.551295	790.220240	13.363968
15.794066	786.632233	13.368986
15.717061	787.048125	13.374003
14.880305	794.815208	13.379021
15.340393	795.106453	13.384039
15.414115	792.182220	13.389056
15.421922	792.439744	13.394074
15.771992	787.954586	13.399091
15.563702	787.232771	13.404109
15.684125	785.790766	13.409127
15.837266	799.904501	13.414144
16.007829	790.928304	13.419162
15.555514	789.092647	13.424179
15.519552	789.268626	13.429197
16.043396	780.871729	13.434215
15.925429	785.421672	13.439232
16.059191	782.519650	13.444250
16.079376	784.731790	13.449267
15.768612	790.428876	13.454285
16.125602	785.781699	13.459303
16.031836	785.528034	13.464320
15.794456	790.626731	13.469338
15.601639	794.434116	13.474355
15.570043	791.649353	13.479373
15.611750	783.942886	13.484391
15.725016	789.760139	13.489408
15.476636	795.706282	13.494426
16.011423	793.628576	13.499443
15.497471	795.393720	13.504461
15.921191	794.055966	13.509479
15.999424	796.855500	13.514496
15.982445	794.327230	13.519514
15.562405	792.480236	13.524531
15.736778	806.442352	13.529549
16.274406	817.491994	13.534567
16.004088	825.211922	13.539584
16.356241	814.639047	13.544602
16.317617	807.532041	13.549619
16.099479	801.929863	13.554637
16.219857	789.250357	13.559655
15.952147	793.463866	13.564672
16.007956	809.697626	13.569690
16.275727	819.366056	13.574707
16.217512	822.164748	13.579725
16.285105	813.759979	13.584743
16.728130	806.300279	13.589760
16.535652	795.108487	13.594778
16.333506	789.147227	13.599795
16.098713	783.516091	13.604813
15.720548	787.885648	13.609831
16.211897	794.685422	13.614848
16.119136	807.594097	13.619866
16.234319	807.014417	13.624883
15.862520	813.610926	13.629901
16.110484	808.400066	13.634919
16.480660	803.242762	13.639936
16.455122	807.147177	13.644954
16.581594	804.079033	13.649971
16.343071	810.607454	13.654989
16.411327	802.802173	13.660007
16.527693	814.176172	13.665024
16.616160	806.550774	13.670042
16.385193	810.790124	13.675059
16.560939	816.452494	13.680077
16.518938	808.620198	13.685095
16.130474	806.231814	13.690112
16.061767	812.916828	13.695130
16.658416	804.230881	13.700147
16.526646	813.734303	13.705165
16.872194	808.896403	13.710183
16.875815	813.250703	13.715200
16.559615	815.070264	13.720218
16.676721	813.423651	13.725235
16.529149	809.441991	13.730253
16.439154	803.993425	13.735271
16.152747	805.852527	13.740288
16.529717	809.545955	13.745306
16.770990	808.100910	13.750323
16.526943	811.146279	13.755341
16.871377	812.168723	13.760359
16.644322	812.216669	13.765376
16.436474	825.354709	13.770394
17.050430	822.444185	13.775411
17.103568	834.831561	13.780429
16.776124	831.998183	13.785447
16.608329	826.574346	13.790464
16.564725	831.778581	13.795482
16.921002	828.775636	13.800499
16.797936	836.898665	13.805517
16.651560	831.165387	13.810535
16.784536	830.475642	13.815552
16.842855	834.209220	13.820570
17.031949	827.495929	13.825587
16.994969	826.930472	13.830605
17.134543	825.867324	13.835623
16.891001	823.841372	13.840640
16.915927	836.447730	13.845658
16.821669	834.824556	13.850675
16.367577	835.469569	13.855693
16.447246	839.244005	13.860711
17.003549	835.600861	13.865728
17.012527	862.577735	13.870746
17.186613	867.716530	13.875763
17.350161	868.284314	13.880781
17.190739	856.800166	13.885799
17.194440	844.754154	13.890816
16.755693	854.668301	13.895834
17.245077	855.147485	13.900851
17.010101	865.907205	13.905869
16.968756	864.881690	13.910887
17.231546	862.505507	13.915904
17.300414	863.520367	13.920922
17.467250	855.803854	13.925939
17.254124	860.475927	13.930957
17.338815	865.745402	13.935975
17.661307	860.434563	13.940992
17.357124	861.510661	13.946010
17.433684	861.246254	13.951027
17.468583	865.447378	13.956045
17.059341	870.632815	13.961063
17.495616	864.922416	13.966080
17.331351	861.413547	13.971098
17.412984	855.704720	13.976115
17.456277	858.288802	13.981133
17.312470	860.879926	13.986151
17.363759	857.517373	13.991168
17.125696	861.202431	13.996186
17.724162	857.435957	14.001203
17.293221	860.712399	14.006221
17.265634	859.738389	14.011239
17.700212	854.217602	14.016256
17.515834	866.998576	14.021274
17.770082	866.106915	14.026291
17.549139	858.630653	14.031309
17.526582	855.077632	14.036327
17.784191	853.447008	14.041344
17.353734	860.885779	14.046362
17.927076	856.719282	14.051379
17.744503	864.182575	14.056397
17.391664	856.360785	14.061415
17.728044	852.549912	14.066432
17.455745	864.868060	14.071450
17.759509	880.558362	14.076467
17.562749	880.705730	14.081485
17.435005	880.447886	14.086503
17.951551	876.612113	14.091520
18.162507	877.892023	14.096538
18.145349	882.988016	14.101555
18.105395	873.410253	14.106573
18.160095	870.706714	14.111591
17.975770	859.873365	14.116608
17.662464	863.380795	14.121626
17.786223	862.749286	14.126643
18.073278	867.621189	14.131661
17.947205	874.491879	14.136679
18.407811	873.549154	14.141696
17.989212	867.738331	14.146714
18.060820	862.419217	14.151731
17.944737	859.994728	14.156749
17.969455	877.079126	14.161767
18.193099	873.926414	14.166784
18.383379	872.962663	14.171802
18.045170	852.332649	14.176819
17.717445	861.598369	14.181837
17.991887	865.197322	14.186855
18.530710	866.388314	14.191872
18.068081	870.423912	14.196890
18.286915	871.547964	14.201907
18.328521	874.943334	14.206925
18.253045	868.665687	14.211943
18.232515	865.973862	14.216960
18.256886	871.997482	14.221978
18.238110	869.428457	14.226995
18.457874	867.197824	14.232013
17.981864	881.112941	14.237031
18.090953	873.490616	14.242048
17.737774	881.946132	14.247066
18.036876	879.608473	14.252083
18.082221	876.379383	14.257101
18.124792	877.417273	14.262119
18.357018	883.386444	14.267136
18.240770	888.772416	14.272154
18.467227	895.594537	14.277171
18.781823	895.179462	14.282189
18.498587	894.535582	14.287207
18.638374	887.492282	14.292224
18.504333	879.951989	14.297242
18.483154	888.601964	14.302259
18.735499	890.449774	14.307277
18.583567	888.131846	14.312295
18.601997	888.513948	14.317312
18.724732	894.203531	14.322330
18.737939	885.371705	14.327347
18.348777	879.026131	14.332365
18.418727	888.564457	14.337383
18.428452	887.335334	14.342400
18.662244	895.301844	14.347418
18.826005	899.508158	14.352435
18.718879	892.418095	14.357453
18.706072	892.659896	14.362471
18.703248	895.800262	14.367488
18.795075	906.032608	14.372506
18.723603	891.533639	14.377523
18.848453	882.308899	14.382541
18.812669	894.523973	14.387559
18.705295	894.341850	14.392576
18.720681	890.126522	14.397594
18.521337	884.969505	14.402611
18.668075	893.088421	14.407629
18.675648	895.523440	14.412647
18.985627	907.548991	14.417664
19.135828	915.152993	14.422682
19.154790	909.343456	14.427699
19.312591	898.542020	14.432717
18.923645	901.808776	14.437735
19.159260	891.812565	14.442752
19.067125	892.779913	14.447770
18.663168	894.439580	14.452787
18.988178	892.432393	14.457805
19.087248	914.892088	14.462823
19.266322	909.202786	14.467840
19.558952	910.195433	14.472858
19.329237	912.351825	14.477875
19.502129	910.904796	14.482893
19.264324	904.024419	14.487911
19.205930	889.867390	14.492928
19.255412	896.104854	14.497946
18.954114	884.781629	14.502963
19.326123	902.679805	14.507981
19.279532	912.147928	14.512999
19.432848	901.981492	14.518016
19.397767	910.441142	14.523034
19.375132	896.998048	14.528051
19.283959	894.332996	14.533069
19.399236	907.032632	14.538087
19.709173	915.511148	14.543104
19.463588	901.537886	14.548122
19.337929	890.909974	14.553139
19.566868	897.898964	14.558157
19.748591	902.938752	14.563175
19.280827	898.217991	14.568192
19.356344	895.766822	14.573210
19.567851	907.915000	14.578227
19.563135	911.847754	14.583245
19.366664	920.603930	14.588263
19.854687	914.841278	14.593280
20.218349	919.092210	14.598298
19.420870	909.171634	14.603315
19.392339	902.820395	14.608333
19.426371	914.311415	14.613351
19.691858	909.325011	14.618368
19.755806	919.328181	14.623386
19.695372	918.012151	14.628403
19.764769	916.688530	14.633421
19.494351	927.804093	14.638439
19.635561	924.541133	14.643456
19.643035	923.328137	14.648474
19.419251	916.186801	14.653491
19.888471	911.698840	14.658509
19.812883	927.871117	14.663527
19.584982	916.568001	14.668544
19.475660	925.623029	14.673562
19.842321	943.108677	14.678579
20.184956	949.237402	14.683597
20.141825	940.029319	14.688615
20.075940	929.098594	14.693632
20.284605	924.708000	14.698650
20.093694	923.197695	14.703667
19.725273	920.885068	14.708685
20.209957	926.076504	14.713703
19.977780	917.554261	14.718720
20.143391	928.106484	14.723738
20.337037	932.809916	14.728755
20.496693	924.072031	14.733773
19.748969	914.440344	14.738791
19.933002	924.478468	14.743808
20.320713	921.877704	14.748826
20.294901	937.228058	14.753843
20.481105	935.873627	14.758861
20.105258	929.604856	14.763879
20.178500	930.849408	14.768896
20.144460	942.139610	14.773914
20.022322	940.924703	14.778931
19.964794	936.360961	14.783949
20.305803	939.545629	14.788967
20.250319	946.922898	14.793984
20.340881	928.914730	14.799002
19.755233	939.624953	14.804019
19.712187	943.712001	14.809037
20.231529	952.246292	14.814055
21.008016	950.847291	14.819072
20.805951	936.592675	14.824090
20.750637	940.852043	14.829107
20.527877	938.926982	14.834125
20.366698	934.369911	14.839143
20.869872	928.014772	14.844160
20.601811	926.292421	14.849178
20.441248	930.120058	14.854195
20.759253	931.228673	14.859213
20.546093	930.192037	14.864231
20.588662	928.241444	14.869248
20.640179	926.349418	14.874266
20.748328	923.602836	14.879283
20.797615	927.236856	14.884301
21.117016	929.187837	14.889319
20.733981	924.258221	14.894336
20.776211	927.688218	14.899354
20.582638	932.783291	14.904371
20.923471	928.413142	14.909389
20.456302	928.264948	14.914407
20.862360	938.552528	14.919424
21.228572	945.614836	14.924442
21.013769	955.768722	14.929459
21.260355	942.643432	14.934477
20.669661	929.033143	14.939495
20.734401	926.766680	14.944512
20.779009	933.563482	14.949530
20.596240	945.044097	14.954547
21.088533	946.990252	14.959565
21.001104	955.000491	14.964583
21.057450	962.041624	14.969600
21.324828	947.079605	14.974618
21.358571	949.106621	14.979635
21.263932	949.951288	14.984653
21.291992	944.108765	14.989671
21.378744	945.262854	14.994688
21.524719	952.346832	14.999706
21.020663	942.197519	15.004723
21.492608	950.862263	15.009741
20.990061	949.447812	15.014759
21.004364	946.971453	15.019776
21.489691	936.563960	15.024794
21.235349	944.587559	15.029811
21.154417	943.022260	15.034829
21.140250	952.605274	15.039847
21.117835	960.094162	15.044864
21.319225	947.389308	15.049882
21.223505	945.479179	15.054899
21.243213	952.283020	15.059917
21.362030	946.151817	15.064935
21.377298	941.958584	15.069952
21.631704	944.607638	15.074970
21.255259	947.866144	15.079987
21.413502	943.451839	15.085005
21.886333	945.644015	15.090023
21.846806	945.041082	15.095040
21.668939	945.434813	15.100058
21.489397	947.255200	15.105075
21.144359	938.135149	15.110093
21.770878	958.215397	15.115111
21.735442	959.902898	15.120128
21.924185	955.395480	15.125146
21.749872	962.784945	15.130163
22.083044	953.013348	15.135181
21.678979	948.465688	15.140199
21.518812	941.667880	15.145216
21.716843	946.793503	15.150234
21.590968	957.965472	15.155251
21.869521	964.467091	15.160269
21.737114	957.286265	15.165287
21.817299	966.444350	15.170304
21.575992	962.073314	15.175322
21.582997	971.842387	15.180339
21.951337	959.477597	15.185357
21.857775	956.244873	15.190375
21.775447	964.522561	15.195392
22.064855	961.495292	15.200410
21.615167	964.206637	15.205427
21.451056	962.947771	15.210445
21.935276	975.274438	15.215463
22.000997	982.585514	15.220480
22.463404	976.564903	15.225498
22.410656	982.742576	15.230515
22.511440	986.393838	15.235533
22.327386	966.247765	15.240551
22.085997	967.168929	15.245568
22.277681	963.620398	15.250586
22.255587	965.763405	15.255603
21.984758	954.400679	15.260621
22.342953	971.089269	15.265639
22.447662	984.841469	15.270656
22.367826	981.082750	15.275674
22.620485	981.245351	15.280691
22.838759	968.541008	15.285709
22.425333	969.889738	15.290727
22.208740	963.959070	15.295744
22.708519	959.917610	15.300762
22.391346	964.517550	15.305779
22.085605	961.642903	15.310797
22.545304	970.227514	15.315815
22.432007	980.605447	15.320832
22.439198	981.453195	15.325850
22.670017	988.751191	15.330867
22.604289	984.772528	15.335885
22.805457	978.499106	15.340903
22.654559	990.132575	15.345920
22.951043	975.948626	15.350938
22.748873	978.570944	15.355955
22.688994	983.197099	15.360973
22.858778	977.499754	15.365991
22.707649	978.056577	15.371008
22.614046	981.744414	15.376026
22.812496	975.988959	15.381043
22.636772	980.431182	15.386061
23.147429	976.432206	15.391079
22.574919	985.000813	15.396096
22.798991	971.172119	15.401114
22.923216	976.025224	15.406131
22.824696	980.143008	15.411149
23.156908	978.917316	15.416167
23.022715	975.520504	15.421184
23.193272	971.486121	15.426202
23.528629	980.427761	15.431219
23.202336	978.689225	15.436237
23.018380	971.169288	15.441255
22.976482	977.446254	15.446272
23.167348	979.593975	15.451290
23.016324	974.170638	15.456307
22.989181	978.933704	15.461325
23.128096	980.051272	15.466343
22.772173	985.215817	15.471360
22.943222	978.271754	15.476378
23.074438	974.701078	15.481395
22.793367	979.330114	15.486413
22.919622	972.216305	15.491431
23.246197	983.762807	15.496448
23.061333	999.857490	15.501466
23.676621	1003.517010	15.506483
23.405844	1003.584386	15.511501
23.710431	1002.688036	15.516519
23.294406	990.637848	15.521536
23.534220	1001.105980	15.526554
23.687381	996.600936	15.531571
22.966208	992.396122	15.536589
23.505454	996.405145	15.541607
23.044026	1005.918971	15.546624
23.237770	1002.953927	15.551642
23.738272	998.754559	15.556659
23.566358	1003.480212	15.561677
23.266714	1001.014857	15.566695
23.685499	996.332759	15.571712
23.730505	997.846796	15.576730
23.678346	989.381695	15.581747
23.652366	1004.855208	15.586765
23.869122	995.830692	15.591783
23.767055	1001.056702	15.596800
23.660075	997.087614	15.601818
24.119351	997.978582	15.606835
23.858958	997.365854	15.611853
23.850599	990.847344	15.616871
23.588183	1005.821193	15.621888
23.611163	1000.736823	15.626906
23.719651	998.170055	15.631923
23.577716	998.075362	15.636941
24.101646	1014.340564	15.641959
24.164235	1019.155941	15.646976
23.678288	1026.843258	15.651994
24.088244	1026.141937	15.657011
23.879115	1019.812463	15.662029
24.414337	1014.992313	15.667047
24.400260	1022.044435	15.672064
24.122165	1014.094175	15.677082
24.566994	1013.747181	15.682099
24.604991	1013.678121	15.687117
24.498553	998.793195	15.692135
24.272373	1001.775855	15.697152
24.097964	1003.582825	15.702170
24.074527	1002.857467	15.707187
24.139996	998.066279	15.712205
24.010317	998.676566	15.717223
24.438601	1005.773415	15.722240
24.599040	1015.991986	15.727258
24.656501	1010.974827	15.732275
24.475152	1007.001537	15.737293
24.516503	1000.437415	15.742311
24.536950	995.075735	15.747328
24.332998	993.138272	15.752346
24.491957	990.929714	15.757363
24.518700	1002.469262	15.762381
24.725086	1007.988071	15.767399
24.887255	1000.856036	15.772416
24.567496	993.739079	15.777434
24.323720	998.359157	15.782451
23.974430	1008.631841	15.787469
24.583811	1012.784579	15.792487
24.257600	1012.160009	15.797504
24.566842	1021.620124	15.802522
24.614500	1011.631020	15.807539
24.422105	1020.130994	15.812557
24.395005	1012.413051	15.817575
24.848237	1020.692585	15.822592
24.756913	1033.497060	15.827610
24.899097	1030.644178	15.832627
24.693273	1038.007023	15.837645
24.775097	1038.546513	15.842663
24.907681	1041.003112	15.847680
25.015851	1035.226981	15.852698
25.246069	1040.101470	15.857715
25.065440	1040.028580	15.862733
25.261902	1040.177841	15.867751
25.169534	1035.408062	15.872768
25.089738	1036.909975	15.877786
24.962550	1034.247354	15.882803
25.052084	1041.807208	15.887821
25.194917	1038.512418	15.892839
24.760213	1035.604189	15.897856
24.878419	1036.469369	15.902874
25.330928	1023.971511	15.907891
24.918959	1030.943577	15.912909
24.975874	1036.637143	15.917927
25.389083	1038.838614	15.922944
25.061244	1031.852286	15.927962
25.423598	1031.259362	15.932979
25.383593	1034.175171	15.937997
25.267672	1027.143227	15.943015
25.269011	1028.796606	15.948032
25.428630	1037.238626	15.953050
25.567026	1042.603931	15.958067
25.643968	1050.131036	15.963085
25.663203	1041.424424	15.968103
25.709092	1038.608624	15.973120
25.318771	1038.827154	15.978138
25.611692	1043.745530	15.983155
25.787295	1054.839063	15.988173
25.744696	1040.291297	15.993191
25.881692	1031.146639	15.998208
25.484692	1029.977675	16.003226
25.954783	1029.336419	16.008243
25.373234	1030.746042	16.013261
25.729457	1046.264224	16.018279
25.419932	1042.610680	16.023296
25.776975	1054.991916	16.028314
25.845674	1055.924764	16.033331
25.948501	1058.483828	16.038349
25.998394	1057.491433	16.043367
25.868645	1056.530163	16.048384
25.811906	1058.719601	16.053402
26.144466	1055.527810	16.058419
26.136877	1048.750386	16.063437
26.491734	1049.477736	16.068455
26.601230	1051.309935	16.073472
26.131104	1062.390404	16.078490
26.282367	1045.016443	16.083507
26.009134	1038.021611	16.088525
26.232548	1040.262100	16.093543
26.273164	1036.023874	16.098560
25.778682	1047.947557	16.103578
26.140399	1046.067181	16.108595
26.239256	1053.575096	16.113613
26.232963	1048.479492	16.118631
26.244211	1055.319403	16.123648
26.246020	1049.408351	16.128666
26.578297	1057.896080	16.133683
26.281796	1055.120964	16.138701
26.213733	1046.620442	16.143719
26.524982	1053.139093	16.148736
26.730195	1057.162268	16.153754
26.604054	1050.479040	16.158771
26.174928	1050.940295	16.163789
26.280689	1052.549017	16.168807
26.724906	1053.650613	16.173824
26.492296	1057.091868	16.178842
26.547755	1049.667163	16.183859
26.817517	1053.462540	16.188877
26.755369	1054.930150	16.193895
26.944149	1055.702292	16.198912
26.367554	1060.235351	16.203930
26.689859	1044.213829	16.208947
26.750991	1057.717255	16.213965
26.871952	1061.409570	16.218983
27.082599	1049.435339	16.224000
26.594871	1053.831486	16.229018
26.669850	1052.033621	16.234035
26.679498	1047.541442	16.239053
26.650511	1053.639702	16.244071
27.094558	1052.305076	16.249088
26.602241	1061.388246	16.254106
26.679116	1068.195855	16.259123
27.242307	1072.848099	16.264141
26.953938	1079.665242	16.269159
27.505959	1073.106789	16.274176
27.202451	1080.068299	16.279194
26.963244	1081.528765	16.284211
26.945118	1072.316721	16.289229
26.644674	1080.631577	16.294247
27.278046	1069.304719	16.299264
27.069639	1079.476615	16.304282
27.240580	1071.901378	16.309299
27.066301	1075.153677	16.314317
26.763666	1081.865746	16.319335
27.024975	1073.929305	16.324352
27.178335	1081.640182	16.329370
27.237108	1093.234762	16.334387
27.500201	1093.487257	16.339405
27.768453	1098.595679	16.344423
27.778280	1104.429140	16.349440
27.754568	1101.261253	16.354458
27.431337	1075.645686	16.359475
27.698121	1068.301679	16.364493
27.444772	1075.817104	16.369511
27.625237	1079.329747	16.374528
27.773293	1092.093838	16.379546
27.627973	1087.221838	16.384563
27.861272	1096.198362	16.389581
28.008027	1089.336932	16.394599
28.200236	1074.919834	16.399616
27.651425	1068.542245	16.404634
27.760707	1063.750530	16.409651
27.764898	1059.701003	16.414669
27.376705	1058.647430	16.419687
27.866774	1078.755372	16.424704
27.805595	1088.326844	16.429722
28.054997	1084.974428	16.434739
28.332331	1092.435637	16.439757
28.189578	1090.977778	16.444775
28.282018	1083.540990	16.449792
27.594319	1074.758238	16.454810
28.151789	1078.890673	16.459827
28.574904	1083.735141	16.464845
28.141635	1081.574599	16.469863
28.071460	1068.747839	16.474880
27.955606	1073.546833	16.479898
28.042492	1081.488964	16.484915
28.208333	1086.894190	16.489933
28.133256	1082.162732	16.494951
28.448968	1093.439600	16.499968
27.994737	1095.375353	16.504986
28.325823	1093.215722	16.510003
28.420841	1102.633496	16.515021
28.000536	1096.343185	16.520039
28.096324	1089.262475	16.525056
28.394513	1093.056590	16.530074
28.311947	1087.698298	16.535091
28.488861	1090.406776	16.540109
28.259314	1108.875342	16.545127
28.218104	1103.302325	16.550144
28.379169	1115.480590	16.555162
28.487121	1117.410865	16.560179
28.786754	1119.387036	16.565197
28.467269	1128.591652	16.570215
28.539641	1117.689777	16.575232
29.027365	1130.312649	16.580250
28.581124	1115.622541	16.585267
29.154270	1116.407425	16.590285
29.008206	1113.662524	16.595303
29.200863	1116.302284	16.600320
28.942416	1116.484504	16.605338
28.809916	1120.165802	16.610355
29.033671	1117.672588	16.615373
28.448359	1105.430931	16.620391
29.063656	1110.390649	16.625408
28.914493	1114.058762	16.630426
28.908399	1118.395714	16.635443
28.904554	1110.756158	16.640461
28.607830	1115.043686	16.645479
28.348861	1107.724716	16.650496
28.843133	1119.216794	16.655514
28.965108	1137.980950	16.660531
29.259992	1131.077507	16.665549
29.501401	1129.607169	16.670567
29.356669	1138.304904	16.675584
29.540291	1144.909731	16.680602
29.189895	1140.277927	16.685619
29.428753	1135.787908	16.690637
29.770938	1132.380012	16.695655
29.503757	1131.863009	16.700672
29.442382	1136.057096	16.705690
29.344114	1140.304264	16.710707
29.659786	1131.791293	16.715725
29.720782	1137.231794	16.720743
29.437895	1128.591113	16.725760
29.954578	1126.683445	16.730778
29.785127	1127.113738	16.735795
29.925986	1112.171279	16.740813
29.716525	1109.272150	16.745831
29.540490	1107.481804	16.750848
29.883802	1100.965303	16.755866
29.667056	1100.453073	16.760883
29.857577	1096.040016	16.765901
29.600169	1102.265374	16.770919
29.630690	1101.547389	16.775936
29.816058	1110.004369	16.780954
29.602150	1123.478084	16.785971
29.913913	1123.637796	16.790989
30.081721	1121.907522	16.796007
29.868308	1119.431880	16.801024
30.116577	1122.410117	16.806042
29.767554	1129.776360	16.811059
29.950089	1120.817068	16.816077
30.023467	1120.515284	16.821095
30.374386	1129.987903	16.826112
30.388211	1119.707363	16.831130
30.157465	1127.531712	16.836147
30.325848	1117.810927	16.841165
30.194710	1126.033174	16.846183
30.219888	1122.753531	16.851200
30.088117	1123.906941	16.856218
30.053927	1128.440773	16.861235
30.346408	1122.926248	16.866253
30.138929	1124.397556	16.871271
30.284215	1138.216140	16.876288
30.781605	1139.208478	16.881306
30.348276	1150.409503	16.886323
30.496738	1146.548932	16.891341
30.735896	1151.936452	16.896359
30.221032	1141.981209	16.901376
30.706804	1144.837265	16.906394
30.573024	1153.640599	16.911411
30.515123	1149.389282	16.916429
30.484261	1152.183768	16.921447
30.570417	1149.409018	16.926464
30.505786	1147.718087	16.931482
30.220335	1154.888252	16.936499
30.519530	1142.998000	16.941517
30.523669	1153.584966	16.946535
30.484938	1168.912285	16.951552
30.898006	1170.138659	16.956570
30.851729	1177.047533	16.961587
31.335702	1164.270125	16.966605
31.458291	1173.904550	16.971623
31.274530	1167.047213	16.976640
30.926637	1152.912958	16.981658
30.693276	1158.487657	16.986675
31.087500	1156.368680	16.991693
31.291748	1160.836994	16.996711
31.295636	1166.153852	17.001728
31.353404	1162.664002	17.006746
31.307650	1164.681330	17.011763
31.408450	1159.546929	17.016781
31.491432	1157.561617	17.021799
31.248400	1156.829417	17.026816
31.273243	1156.143872	17.031834
31.206135	1159.193308	17.036851
31.228561	1153.080197	17.041869
31.520172	1161.492257	17.046887
31.303583	1166.433191	17.051904
31.611554	1157.085125	17.056922
31.418487	1161.571118	17.061939
31.585301	1157.985396	17.066957
31.550845	1162.197388	17.071975
31.362261	1164.129658	17.076992
31.462429	1153.848278	17.082010
31.484809	1164.284088	17.087027
31.386620	1148.495198	17.092045
31.405009	1160.288612	17.097063
31.506559	1173.744807	17.102080
31.995700	1161.534638	17.107098
32.000409	1172.263536	17.112115
32.056806	1176.003797	17.117133
31.871382	1174.394786	17.122151
32.031727	1173.700766	17.127168
31.959803	1172.490647	17.132186
31.722095	1176.923635	17.137203
31.843664	1169.362356	17.142221
31.969381	1169.320663	17.147239
31.970439	1174.956699	17.152256
31.925998	1172.849214	17.157274
31.939558	1177.845836	17.162291
32.003942	1181.641659	17.167309
32.328448	1179.618740	17.172327
32.402211	1178.120852	17.177344
32.493288	1175.121271	17.182362
32.360610	1174.024753	17.187379
32.267975	1170.637212	17.192397
32.470282	1171.508239	17.197415
32.431068	1180.748140	17.202432
32.373057	1183.982355	17.207450
32.319625	1203.064222	17.212467
32.670240	1193.491748	17.217485
32.870639	1194.120077	17.222503
32.639856	1186.197087	17.227520
32.618074	1175.319304	17.232538
32.502705	1172.945153	17.237555
32.454908	1179.260978	17.242573
32.883691	1188.390148	17.247591
32.607294	1196.038600	17.252608
32.707718	1194.864761	17.257626
32.361301	1190.169209	17.262643
32.680483	1188.964467	17.267661
32.911245	1195.975381	17.272679
32.840196	1206.050224	17.277696
32.870721	1200.412359	17.282714
32.706894	1197.496643	17.287731
32.263185	1194.182694	17.292749
32.703006	1203.461631	17.297767
33.201481	1220.037097	17.302784
33.376366	1220.827189	17.307802
33.219760	1214.369548	17.312819
33.142399	1198.810899	17.317837
33.230239	1195.448903	17.322855
33.120375	1210.487534	17.327872
33.680410	1211.018845	17.332890
33.434903	1211.811274	17.337907
33.111109	1203.972185	17.342925
33.284419	1196.585874	17.347943
33.174361	1210.516854	17.352960
33.664008	1209.272947	17.357978
33.866795	1216.452326	17.362995
33.334544	1203.852047	17.368013
33.438799	1203.778982	17.373031
33.681754	1210.128444	17.378048
33.907417	1219.857297	17.383066
33.468761	1204.724123	17.388083
33.570623	1193.833389	17.393101
33.977347	1204.982550	17.398119
33.661891	1198.846291	17.403136
33.550149	1208.665540	17.408154
33.531711	1216.532611	17.413171
33.513052	1223.345686	17.418189
33.919092	1213.635184	17.423207
33.658159	1220.700573	17.428224
33.439618	1223.129816	17.433242
33.699147	1220.053508	17.438259
33.649608	1217.243070	17.443277
33.682582	1218.247761	17.448295
33.607752	1237.380333	17.453312
34.071542	1244.465438	17.458330
33.937883	1246.824664	17.463347
34.159130	1245.512091	17.468365
34.093747	1251.521411	17.473383
34.185682	1242.105951	17.478400
34.346950	1239.783394	17.483418
34.151696	1237.740408	17.488435
34.095678	1249.169927	17.493453
34.977610	1238.107219	17.498471
34.393726	1241.779926	17.503488
34.580373	1237.215960	17.508506
34.719853	1232.520483	17.513523
34.586069	1242.182237	17.518541
34.555344	1228.244692	17.523559
34.470778	1234.790323	17.528576
34.703676	1233.472780	17.533594
34.471981	1237.201105	17.538611
34.607223	1237.132683	17.543629
34.797149	1233.278260	17.548647
34.778769	1231.838895	17.553664
34.883999	1227.038300	17.558682
34.812000	1230.675487	17.563699
34.610260	1229.848493	17.568717
34.694987	1230.362290	17.573735
34.750483	1230.350465	17.578752
34.676559	1233.991109	17.583770
34.889193	1234.945737	17.588787
34.678051	1225.350256	17.593805
34.757548	1243.590964	17.598823
34.966383	1251.716155	17.603840
34.878028	1247.886122	17.608858
35.135608	1245.507544	17.613875
34.695637	1257.574358	17.618893
35.069475	1248.796655	17.623911
35.025823	1247.036177	17.628928
34.912537	1252.248228	17.633946
35.150090	1247.603749	17.638963
35.124058	1249.286658	17.643981
35.064993	1240.522712	17.648999
35.356027	1258.648449	17.654016
35.503595	1262.570193	17.659034
35.809488	1266.366302	17.664051
35.327396	1258.375110	17.669069
35.660075	1265.237641	17.674087
35.629631	1270.828118	17.679104
35.666496	1271.958438	17.684122
35.780784	1272.338246	17.689139
35.645530	1277.244456	17.694157
35.726887	1269.323323	17.699175
35.764412	1270.204231	17.704192
35.861341	1266.616745	17.709210
36.201434	1267.415831	17.714227
35.943109	1258.787042	17.719245
35.848863	1252.206069	17.724263
35.624569	1254.165998	17.729280
35.908311	1264.438098	17.734298
35.997525	1266.664796	17.739315
36.011606	1270.190760	17.744333
36.185802	1264.883956	17.749351
36.087224	1266.751730	17.754368
35.890826	1264.642647	17.759386
35.808550	1261.477538	17.764403
35.652728	1272.682770	17.769421
35.642333	1264.248905	17.774439
35.730411	1273.235506	17.779456
36.085345	1283.035785	17.784474
36.154678	1287.622967	17.789491
36.222737	1294.971677	17.794509
36.335588	1288.181722	17.799527
36.333401	1292.612782	17.804544
36.609429	1299.291642	17.809562
36.819671	1283.874333	17.814579
36.505277	1292.702700	17.819597
36.476637	1284.426301	17.824615
36.506736	1275.579028	17.829632
36.511035	1280.930570	17.834650
36.585023	1276.207409	17.839667
36.714505	1289.372165	17.844685
36.929351	1294.883434	17.849703
36.950638	1286.990580	17.854720
36.849751	1287.918286	17.859738
36.801559	1285.833463	17.864755
37.116993	1290.215071	17.869773
37.349435	1286.824232	17.874791
36.864447	1285.899324	17.879808
36.602408	1290.039483	17.884826
36.697652	1296.449843	17.889843
37.061973	1307.570957	17.894861
37.222977	1302.360870	17.899879
37.408542	1303.600584	17.904896
37.250057	1304.098601	17.909914
37.297909	1306.338057	17.914931
36.908965	1303.542580	17.919949
37.148570	1309.974650	17.924967
37.398087	1311.545234	17.929984
37.373919	1317.406149	17.935002
37.471531	1309.248937	17.940019
37.168594	1309.693706	17.945037
37.235283	1305.463980	17.950055
37.439266	1310.475172	17.955072
36.946125	1315.809499	17.960090
37.675187	1318.349994	17.965107
37.455465	1334.885908	17.970125
37.601293	1330.962592	17.975143
38.020128	1330.944689	17.980160
37.929508	1330.573760	17.985178
37.937091	1330.853418	17.990195
37.892069	1335.250133	17.995213
38.160312	1331.001643	18.000231
37.878491	1319.776094	18.005248
37.823677	1331.574707	18.010266
38.131378	1323.854994	18.015283
37.873551	1343.719918	18.020301
38.231155	1336.645684	18.025319
38.125742	1332.092452	18.030336
37.921915	1337.141899	18.035354
38.074885	1322.569764	18.040371
38.470540	1330.871031	18.045389
38.114738	1330.604507	18.050407
38.054830	1333.141610	18.055424
37.967836	1337.488056	18.060442
38.458935	1329.515724	18.065459
38.407404	1332.184067	18.070477
38.373601	1335.515527	18.075495
38.682510	1317.687566	18.080512
38.288926	1339.766909	18.085530
38.380503	1321.455228	18.090547
38.363999	1331.865633	18.095565
38.367757	1326.970356	18.100583
38.672069	1332.442461	18.105600
38.651088	1351.806613	18.110618
38.815602	1346.848432	18.115635
38.820265	1358.524194	18.120653
38.762943	1357.598968	18.125671
39.044733	1348.273813	18.130688
38.970417	1347.565829	18.135706
39.235747	1346.795497	18.140723
38.980353	1350.035227	18.145741
39.165628	1341.384668	18.150759
39.271949	1341.459604	18.155776
38.908964	1332.903878	18.160794
39.587307	1328.534733	18.165811
38.969701	1325.033239	18.170829
39.374145	1331.575352	18.175847
38.998983	1331.128804	18.180864
38.977450	1334.499379	18.185882
39.314201	1336.435082	18.190899
39.427996	1338.020488	18.195917
39.169063	1344.918356	18.200935
39.301127	1339.886334	18.205952
38.902090	1341.024566	18.210970
39.223153	1340.141414	18.215987
39.276615	1335.863247	18.221005
39.189085	1338.073292	18.226023
39.525688	1348.002694	18.231040
39.367743	1358.959001	18.236058
39.729148	1353.051820	18.241075
39.514968	1365.124577	18.246093
39.577102	1357.610342	18.251111
39.694779	1365.749778	18.256128
39.698449	1359.109339	18.261146
39.815839	1366.541917	18.266163
39.553635	1358.393367	18.271181
39.538501	1368.841450	18.276199
39.776282	1372.944833	18.281216
39.538494	1389.701363	18.286234
40.101384	1390.118626	18.291251
40.145901	1389.411074	18.296269
40.111941	1384.720470	18.301287
40.096060	1385.975775	18.306304
40.453926	1383.089257	18.311322
40.388020	1389.714090	18.316339
40.623657	1381.008334	18.321357
40.667429	1382.860268	18.326375
40.857378	1389.871302	18.331392
40.707589	1388.146269	18.336410
40.518469	1377.455363	18.341427
40.615934	1374.085524	18.346445
40.619736	1371.452950	18.351463
40.718663	1365.372036	18.356480
40.791647	1375.058474	18.361498
40.758200	1361.645114	18.366515
40.193619	1356.172440	18.371533
40.755537	1368.581958	18.376551
40.968965	1374.800376	18.381568
40.717020	1374.344110	18.386586
40.840946	1375.331493	18.391603
40.964241	1368.391558	18.396621
40.687187	1377.756954	18.401639
41.055932	1374.701485	18.406656
40.975070	1378.535743	18.411674
40.859085	1377.382963	18.416691
40.714558	1371.119045	18.421709
40.885634	1376.337352	18.426727
40.857668	1383.382312	18.431744
41.027936	1393.634284	18.436762
41.276483	1396.085501	18.441779
41.311827	1400.261436	18.446797
41.124503	1403.288605	18.451815
41.431632	1395.013526	18.456832
41.176709	1403.719079	18.461850
41.227418	1397.039743	18.466867
41.014099	1399.906857	18.471885
41.203911	1408.902933	18.476903
41.275296	1413.022765	18.481920
41.501708	1421.060090	18.486938
41.761553	1418.870486	18.491955
42.002146	1424.194749	18.496973
41.742723	1438.691964	18.501991
41.841410	1423.045749	18.507008
41.891061	1436.011602	18.512026
41.799235	1419.880651	18.517043
41.817000	1418.391462	18.522061
41.929381	1429.431957	18.527079
42.071017	1420.434701	18.532096
41.868243	1419.737247	18.537114
42.289963	1417.175299	18.542131
42.283142	1416.125442	18.547149
42.074109	1408.495614	18.552167
42.397877	1413.112642	18.557184
42.584353	1419.164857	18.562202
42.335926	1418.935262	18.567219
42.372192	1405.236459	18.572237
42.230175	1419.384017	18.577255
42.194418	1416.148522	18.582272
42.193498	1416.764022	18.587290
42.312137	1414.220861	18.592307
42.488491	1418.930270	18.597325
42.476838	1430.965228	18.602343
42.786464	1439.715445	18.607360
42.911361	1437.695174	18.612378
42.759027	1434.859681	18.617395
42.987298	1438.327083	18.622413
42.470760	1439.559355	18.627431
43.039933	1428.709329	18.632448
43.439884	1454.729973	18.637466
42.952867	1426.198165	18.642483
43.129294	1415.589178	18.647501
42.754275	1420.397057	18.652519
43.017781	1426.064894	18.657536
42.982349	1431.369018	18.662554
42.958562	1435.184935	18.667571
43.280853	1435.705932	18.672589
43.390421	1438.696350	18.677607
42.945368	1430.967559	18.682624
43.179392	1446.227404	18.687642
43.157872	1439.950621	18.692659
43.122545	1431.580520	18.697677
43.305624	1436.948455	18.702695
43.319110	1428.201524	18.707712
43.316855	1437.470517	18.712730
43.245600	1452.011030	18.717747
43.611819	1452.522033	18.722765
43.618796	1467.479572	18.727783
43.688193	1461.043458	18.732800
43.289678	1456.630504	18.737818
43.847071	1458.872697	18.742835
43.821388	1456.434051	18.747853
43.510762	1458.344328	18.752871
43.759104	1445.395121	18.757888
44.115790	1448.517481	18.762906
43.816211	1455.689966	18.767923
43.846089	1455.407571	18.772941
43.913694	1455.122459	18.777959
43.922580	1472.244607	18.782976
44.319773	1474.716874	18.787994
44.459326	1480.148404	18.793011
44.485700	1479.822374	18.798029
44.478475	1482.360764	18.803047
44.808390	1471.058809	18.808064
44.482666	1455.712176	18.813082
44.201286	1457.475886	18.818099
44.365867	1453.675855	18.823117
44.221722	1472.503889	18.828135
44.617413	1471.353489	18.833152
44.572643	1475.671304	18.838170
44.603315	1481.069293	18.843187
44.664521	1473.277440	18.848205
44.455712	1475.238138	18.853223
44.785685	1474.079035	18.858240
45.105209	1473.514857	18.863258
44.507162	1478.736176	18.868275
44.871016	1468.378846	18.873293
44.362489	1473.456837	18.878311
44.546720	1486.139839	18.883328
44.691525	1490.472323	18.888346
45.254366	1493.581528	18.893363
45.195671	1497.535438	18.898381
44.888007	1496.081131	18.903399
44.849094	1497.661926	18.908416
45.214881	1496.904349	18.913434
44.872146	1499.974666	18.918451
45.323840	1508.652305	18.923469
45.310876	1519.889098	18.928487
45.458212	1523.009352	18.933504
45.776289	1524.913268	18.938522
45.473675	1530.028644	18.943539
45.790633	1509.803950	18.948557
45.495266	1517.524921	18.953575
45.499618	1523.624463	18.958592
45.743229	1513.945399	18.963610
45.843924	1515.662251	18.968627
46.061841	1504.365090	18.973645
46.055475	1511.384646	18.978663
46.114024	1516.813020	18.983680
46.234980	1499.809413	18.988698
45.969654	1499.383630	18.993715
46.114229	1496.912159	18.998733
46.182293	1511.311108	19.003751
46.176325	1515.610267	19.008768
46.335913	1506.408199	19.013786
45.897548	1514.571159	19.018803
46.541739	1510.374548	19.023821
46.208797	1518.006694	19.028839
46.090473	1516.611269	19.033856
46.111793	1509.721870	19.038874
46.427126	1510.275511	19.043891
46.680095	1513.729615	19.048909
46.628343	1514.911618	19.053927
46.453141	1507.150246	19.058944
46.524928	1502.348472	19.063962
46.304616	1508.716520	19.068979
46.625278	1503.743451	19.073997
46.561731	1520.820118	19.079015
46.542826	1514.015876	19.084032
46.825707	1518.348960	19.089050
46.532638	1532.797841	19.094067
46.896492	1534.416917	19.099085
46.824271	1535.497965	19.104103
46.616134	1536.111018	19.109120
46.745350	1542.128009	19.114138
46.552811	1545.957599	19.119155
47.644471	1548.801441	19.124173
47.326380	1551.306189	19.129191
47.187677	1552.407056	19.134208
47.704755	1547.027848	19.139226
47.732338	1552.622003	19.144243
47.440280	1536.190758	19.149261
47.207344	1541.516198	19.154279
47.262986	1540.576530	19.159296
47.562140	1551.266124	19.164314
47.533347	1562.527500	19.169331
47.661266	1552.759130	19.174349
47.661258	1554.327560	19.179367
47.856292	1547.764555	19.184384
47.846813	1548.397172	19.189402
47.596787	1555.839697	19.194419
47.893539	1550.172895	19.199437
47.861426	1554.608680	19.204455
47.705814	1547.207163	19.209472
48.178766	1554.205759	19.214490
47.635827	1557.556569	19.219507
47.581560	1556.927507	19.224525
47.678740	1566.102189	19.229543
48.215192	1575.199016	19.234560
48.148863	1575.610108	19.239578
48.232784	1574.328360	19.244595
48.569567	1575.380445	19.249613
48.482783	1577.372649	19.254631
49.042047	1581.246144	19.259648
49.044944	1577.218792	19.264666
48.448506	1577.914394	19.269683
48.468898	1571.173441	19.274701
48.718320	1580.229752	19.279719
48.305520	1576.579552	19.284736
48.488448	1571.571104	19.289754
48.524280	1575.841679	19.294771
48.501448	1576.892949	19.299789
48.849939	1575.901373	19.304807
48.800596	1581.668462	19.309824
48.684661	1575.062344	19.314842
48.873447	1591.897817	19.319859
49.046260	1587.455838	19.324877
48.912468	1592.412401	19.329895
49.095615	1588.035085	19.334912
49.170250	1591.220320	19.339930
49.161127	1600.332674	19.344947
49.375776	1592.586307	19.349965
49.316729	1599.806608	19.354983
49.281251	1594.728015	19.360000
49.460702	1585.134643	19.365018
49.556786	1599.709185	19.370035
49.254758	1595.306420	19.375053
49.538278	1597.512375	19.380071
49.259413	1609.620615	19.385088
49.452719	1613.355432	19.390106
49.568628	1623.120530	19.395123
49.548885	1613.504507	19.400141
49.780492	1612.026189	19.405159
49.542678	1624.109113	19.410176
49.900606	1617.287187	19.415194
49.845515	1615.525297	19.420211
50.107106	1616.920457	19.425229
50.321644	1620.298512	19.430247
50.260832	1622.712719	19.435264
50.303507	1617.360015	19.440282
50.400204	1628.358893	19.445299
50.633493	1620.527560	19.450317
50.921142	1617.472053	19.455335
50.504000	1615.870676	19.460352
50.792707	1610.271381	19.465370
50.501047	1614.195315	19.470387
50.469308	1607.197373	19.475405
50.547518	1604.941350	19.480423
50.301605	1608.211210	19.485440
50.358794	1608.883943	19.490458
50.431945	1618.456876	19.495475
50.718453	1632.645184	19.500493
50.949328	1626.862380	19.505511
50.586977	1640.290167	19.510528
51.073203	1631.870327	19.515546
50.901857	1619.166223	19.520563
51.181593	1625.740485	19.525581
51.404147	1624.632812	19.530599
50.947303	1631.255485	19.535616
51.169605	1619.108641	19.540634
50.905989	1623.372200	19.545651
50.905093	1624.366408	19.550669
51.287061	1627.178744	19.555687
51.558636	1646.229419	19.560704
51.675832	1644.232415	19.565722
52.004402	1649.751335	19.570739
51.772952	1640.124077	19.575757
51.698125	1635.512355	19.580775
51.363627	1625.292068	19.585792
51.662466	1634.700481	19.590810
51.500494	1643.218105	19.595827
51.658962	1646.952041	19.600845
51.817079	1642.625948	19.605863
51.598110	1642.448568	19.610880
51.851733	1638.195970	19.615898
51.573248	1645.690301	19.620915
51.340755	1650.760079	19.625933
52.155675	1655.253362	19.630951
52.269811	1669.209755	19.635968
52.692895	1662.043146	19.640986
52.320737	1649.335570	19.646003
52.278016	1642.926315	19.651021
52.222313	1635.761675	19.656039
52.556421	1659.063046	19.661056
52.667237	1660.636322	19.666074
52.318150	1652.873557	19.671091
52.443829	1663.621787	19.676109
52.969697	1666.553739	19.681127
52.627689	1670.065794	19.686144
52.572400	1661.859642	19.691162
52.906548	1659.005176	19.696179
52.494900	1660.300028	19.701197
53.182602	1664.456507	19.706215
52.776501	1674.747885	19.711232
52.669287	1668.863069	19.716250
52.899535	1663.913501	19.721267
52.822157	1667.608421	19.726285
52.708436	1666.401620	19.731303
52.816758	1673.819959	19.736320
53.057278	1678.677241	19.741338
53.466858	1684.839981	19.746355
53.357311	1684.904346	19.751373
53.387678	1686.212433	19.756391
53.629921	1680.999055	19.761408
53.726605	1683.906312	19.766426
53.878817	1678.568093	19.771443
53.571312	1680.187566	19.776461
53.472285	1679.088932	19.781479
53.528948	1688.295233	19.786496
53.401997	1681.914857	19.791514
53.586917	1683.833211	19.796531
53.511469	1698.630204	19.801549
53.912548	1706.410084	19.806567
54.317258	1704.791196	19.811584
54.184187	1700.387346	19.816602
54.487962	1701.428799	19.821619
54.042457	1698.825105	19.826637
53.911362	1702.654630	19.831655
54.253620	1699.830454	19.836672
54.032858	1694.042205	19.841690
54.577681	1698.403980	19.846707
54.204721	1695.201999	19.851725
54.392419	1695.627192	19.856743
53.970555	1691.271464	19.861760
54.203495	1705.307220	19.866778
54.599743	1710.566308	19.871795
54.203797	1718.069489	19.876813
54.565134	1705.515922	19.881831
54.279902	1719.228414	19.886848
54.510668	1716.238552	19.891866
54.973166	1730.071326	19.896883
54.837297	1751.997441	19.901901
54.758933	1737.786042	19.906919
55.158115	1750.647209	19.911936
54.814251	1756.154089	19.916954
55.326066	1745.738848	19.921971
55.184210	1752.277809	19.926989
55.335207	1744.670678	19.932007
55.347541	1748.916550	19.937024
55.389372	1740.335470	19.942042
55.725455	1739.393156	19.947059
55.209480	1745.201391	19.952077
55.660435	1729.970287	19.957095
55.647378	1742.674721	19.962112
55.414762	1731.949347	19.967130
55.464599	1728.946627	19.972147
55.754400	1740.840183	19.977165
55.865398	1747.611180	19.982183
56.003999	1765.865311	19.987200
55.987691	1764.337216	19.992218
56.277575	1756.402335	19.997235
56.192366	1760.581344	20.002253
55.990502	1739.222152	20.007271
56.150307	1738.367245	20.012288
56.130498	1755.172232	20.017306
56.612522	1763.734818	20.022323
56.559423	1759.908653	20.027341
56.554338	1758.593411	20.032359
56.414121	1764.204290	20.037376
56.484427	1762.372367	20.042394
56.920327	1758.874021	20.047411
56.572560	1760.638629	20.052429
56.641870	1757.591845	20.057447
56.557587	1760.132805	20.062464
56.276397	1756.780821	20.067482
56.780099	1756.614004	20.072499
56.550457	1757.893148	20.077517
56.928364	1751.323688	20.082535
57.053974	1757.514887	20.087552
56.836139	1761.042341	20.092570
57.345078	1755.320347	20.097587
57.153661	1770.350055	20.102605
57.473797	1775.444283	20.107623
57.437977	1774.894395	20.112640
57.008759	1756.802211	20.117658
57.335891	1763.293404	20.122675
57.310197	1782.248492	20.127693
57.523463	1772.157437	20.132711
57.688830	1777.493518	20.137728
57.332814	1775.447096	20.142746
57.772321	1773.289439	20.147763
56.923342	1775.633871	20.152781
57.078778	1774.968996	20.157799
57.281740	1791.041880	20.162816
57.511415	1797.081187	20.167834
57.529359	1800.152205	20.172851
57.467513	1805.056598	20.177869
58.265209	1810.278460	20.182887
58.539414	1811.690607	20.187904
58.687728	1819.074377	20.192922
58.706583	1808.780033	20.197939
58.326742	1797.736705	20.202957
58.486213	1790.286030	20.207975
58.416314	1791.417226	20.212992
58.452259	1795.892969	20.218010
58.940653	1805.833709	20.223027
58.920299	1798.291105	20.228045
58.650841	1793.911623	20.233063
58.736841	1788.694137	20.238080
58.753169	1802.479665	20.243098
59.214547	1800.833011	20.248115
58.945861	1804.526185	20.253133
59.024111	1805.403936	20.258151
59.216404	1811.183972	20.263168
59.134107	1811.032650	20.268186
58.899578	1805.407459	20.273203
59.007869	1818.878871	20.278221
58.942670	1809.326626	20.283239
59.021549	1804.671994	20.288256
59.013797	1814.674207	20.293274
59.109480	1805.267333	20.298291
59.280991	1811.785929	20.303309
58.830547	1812.840672	20.308327
59.352898	1820.491264	20.313344
59.406455	1838.907039	20.318362
59.557675	1838.555252	20.323379
59.493068	1830.596634	20.328397
59.626896	1838.951529	20.333415
59.541807	1837.329991	20.338432
59.496918	1847.650438	20.343450
59.781558	1858.976814	20.348467
59.881272	1862.243401	20.353485
59.867294	1862.681064	20.358503
60.043610	1860.659051	20.363520
60.129809	1850.556176	20.368538
60.616270	1854.968103	20.373555
60.456586	1861.244783	20.378573
60.400255	1850.201548	20.383591
60.554559	1855.867590	20.388608
60.005663	1851.610497	20.393626
60.647592	1862.294249	20.398643
60.821275	1879.861360	20.403661
61.122834	1881.079899	20.408679
61.118507	1880.171642	20.413696
61.353869	1862.449266	20.418714
61.327298	1847.033627	20.423731
60.969041	1843.469557	20.428749
61.101084	1846.844720	20.433767
61.389481	1837.410982	20.438784
61.158731	1843.244271	20.443802
61.344563	1847.630416	20.448819
61.131526	1841.979776	20.453837
61.085839	1843.848843	20.458855
61.351699	1845.072938	20.463872
61.458738	1859.769066	20.468890
61.424738	1862.845027	20.473907
61.383967	1863.217431	20.478925
61.457004	1868.324910	20.483943
61.487259	1862.592202	20.488960
61.567454	1869.841427	20.493978
61.836512	1857.832313	20.498995
61.709806	1854.367893	20.504013
61.596720	1863.423982	20.509031
61.874297	1868.149310	20.514048
61.940066	1883.303178	20.519066
62.229177	1886.549750	20.524083
61.870517	1881.650785	20.529101
61.984779	1885.962874	20.534119
62.032259	1882.332469	20.539136
61.905650	1885.728975	20.544154
62.118840	1901.450061	20.549171
62.247578	1908.660185	20.554189
62.645178	1908.042811	20.559207
62.665010	1905.417131	20.564224
62.918466	1919.910625	20.569242
62.746948	1913.300412	20.574259
62.427102	1913.921402	20.579277
62.546936	1911.365360	20.584295
62.964644	1909.864356	20.589312
62.675681	1916.053882	20.594330
62.452520	1932.571949	20.599347
62.942726	1930.359042	20.604365
62.989156	1935.884108	20.609383
63.406881	1928.793969	20.614400
63.316338	1928.457730	20.619418
63.273262	1925.103357	20.624435
63.453763	1920.489679	20.629453
63.498786	1926.049676	20.634471
63.782509	1921.694492	20.639488
63.406701	1926.931833	20.644506
63.567186	1929.431551	20.649523
63.698836	1928.682008	20.654541
63.509230	1926.824262	20.659559
63.516360	1945.111670	20.664576
63.855965	1944.635873	20.669594
63.960809	1945.553673	20.674611
64.016318	1945.106329	20.679629
63.922768	1951.211792	20.684647
64.424782	1939.926930	20.689664
63.998975	1950.464539	20.694682
63.951906	1942.269602	20.699699
64.068506	1946.398298	20.704717
64.105888	1963.178797	20.709735
64.413732	1965.090667	20.714752
64.500397	1974.153583	20.719770
64.384604	1975.579125	20.724787
64.677255	1971.112081	20.729805
64.501385	1974.058665	20.734823
64.960203	1963.452726	20.739840
64.672397	1969.670493	20.744858
64.765082	1977.381739	20.749875
65.085958	1968.836001	20.754893
64.955071	1986.343335	20.759911
65.302753	1984.465048	20.764928
65.179322	1985.348961	20.769946
65.212408	1988.493397	20.774963
65.747179	1987.797857	20.779981
65.651415	1990.848740	20.784999
65.798163	1994.748683	20.790016
66.017172	1992.426507	20.795034
65.563283	1977.254019	20.800051
65.633516	1977.924735	20.805069
65.138613	1986.639531	20.810087
65.812722	1977.672705	20.815104
65.556715	1989.335814	20.820122
65.427268	1990.921279	20.825139
65.938294	1988.127589	20.830157
65.584928	1993.146852	20.835175
65.842790	1999.693099	20.840192
65.928665	2016.106321	20.845210
65.891583	2020.429382	20.850227
66.114310	2010.245197	20.855245
65.928014	2016.724899	20.860263
66.082621	2022.649733	20.865280
66.176460	2034.252089	20.870298
66.387312	2030.504696	20.875315
66.578712	2032.955432	20.880333
66.750599	2035.529133	20.885351
66.935326	2026.531175	20.890368
66.884758	2032.601571	20.895386
66.740555	2029.496462	20.900403
66.605344	2028.501273	20.905421
67.063740	2045.254170	20.910439
67.107189	2041.352950	20.915456
67.329006	2057.145417	20.920474
67.558340	2054.057888	20.925491
67.855419	2051.433204	20.930509
67.896929	2048.204499	20.935527
67.718945	2029.719457	20.940544
67.212154	2026.074330	20.945562
67.241140	2036.134066	20.950579
68.056272	2036.493140	20.955597
67.604776	2049.228182	20.960615
67.967732	2047.382226	20.965632
67.747070	2046.277260	20.970650
67.777632	2043.353230	20.975667
68.142541	2045.937907	20.980685
67.464835	2052.576185	20.985703
67.619089	2041.679934	20.990720
68.338066	2038.333129	20.995738
68.138527	2047.996088	21.000755
68.128248	2043.601438	21.005773
68.277092	2048.656139	21.010791
68.408279	2052.044099	21.015808
68.032789	2058.979324	21.020826
68.104312	2072.462964	21.025843
68.352664	2066.399575	21.030861
68.577961	2076.091083	21.035879
68.759522	2065.733388	21.040896
68.664266	2078.880066	21.045914
68.551118	2079.285835	21.050931
68.902082	2084.754065	21.055949
68.658628	2092.037991	21.060967
68.910899	2090.534326	21.065984
69.200465	2092.464836	21.071002
69.158053	2088.207728	21.076019
69.357597	2099.171947	21.081037
69.325504	2091.804624	21.086055
69.198375	2090.461020	21.091072
69.434793	2096.723451	21.096090
69.576433	2115.974747	21.101107
69.791425	2103.740346	21.106125
70.136546	2120.899132	21.111143
70.068901	2120.720278	21.116160
70.178253	2114.340828	21.121178
70.212523	2099.511973	21.126195
70.689335	2098.904352	21.131213
70.207631	2094.232778	21.136231
70.173403	2088.784604	21.141248
69.896793	2084.352512	21.146266
69.749154	2093.246832	21.151283
70.227256	2098.606905	21.156301
70.489667	2105.685839	21.161319
70.512648	2101.036676	21.166336
70.369725	2101.778456	21.171354
70.212989	2098.296572	21.176371
70.484964	2110.189994	21.181389
70.551699	2122.778129	21.186407
70.627716	2126.635461	21.191424
71.048581	2122.703865	21.196442
70.477386	2133.911188	21.201459
70.991819	2127.323491	21.206477
70.782957	2125.699106	21.211495
71.117078	2145.406481	21.216512
71.777099	2143.709934	21.221530
71.570333	2141.526617	21.226547
71.714296	2137.111086	21.231565
71.730205	2144.682871	21.236583
71.592269	2135.877113	21.241600
71.808692	2128.906604	21.246618
71.460135	2141.603593	21.251635
71.667167	2152.774973	21.256653
71.990004	2138.620716	21.261671
71.792419	2151.849655	21.266688
72.244438	2139.912857	21.271706
71.882162	2144.772596	21.276723
71.966180	2142.247346	21.281741
71.860072	2142.465818	21.286759
72.165902	2147.363555	21.291776
72.383405	2138.663410	21.296794
72.430097	2153.501726	21.301811
72.577765	2155.571106	21.306829
72.664685	2160.711223	21.311847
72.401584	2165.808003	21.316864
72.561376	2155.387370	21.321882
72.655648	2152.235642	21.326899
72.685042	2157.207981	21.331917
72.516318	2151.190564	21.336935
72.805519	2159.205823	21.341952
72.532932	2152.279881	21.346970
72.589107	2168.246565	21.351987
72.910295	2174.495825	21.357005
72.949645	2181.145592	21.362023
73.061088	2189.611439	21.367040
72.927931	2181.934749	21.372058
72.979456	2206.132941	21.377075
73.209376	2210.865780	21.382093
73.516763	2205.812531	21.387111
73.609566	2210.516223	21.392128
73.974315	2207.243475	21.397146
73.778415	2199.996290	21.402163
73.996119	2198.166622	21.407181
74.059411	2202.893842	21.412199
73.966447	2205.893831	21.417216
74.087062	2214.613895	21.422234
74.253562	2224.128435	21.427251
74.304201	2230.432462	21.432269
74.863312	2225.573556	21.437287
74.271744	2222.566469	21.442304
74.637456	2222.929245	21.447322
74.573662	2221.244394	21.452339
74.741388	2218.687164	21.457357
74.906149	2218.639391	21.462375
74.878275	2229.339282	21.467392
74.942067	2221.310003	21.472410
74.835373	2220.771135	21.477427
74.990609	2217.543629	21.482445
74.572212	2216.207492	21.487463
74.839775	2228.385717	21.492480
75.196675	2227.989276	21.497498
75.339127	2234.938607	21.502515
75.388882	2247.286463	21.507533
75.431258	2253.658060	21.512551
75.516787	2245.335036	21.517568
75.747419	2240.953325	21.522586
75.699285	2239.373336	21.527603
75.633525	2241.406524	21.532621
75.618798	2241.203650	21.537639
75.780691	2262.070963	21.542656
76.035817	2266.206569	21.547674
75.981866	2268.562987	21.552691
76.196466	2266.746420	21.557709
76.188492	2263.512756	21.562727
75.843483	2261.186838	21.567744
76.204365	2264.160359	21.572762
76.188989	2276.158593	21.577779
76.186394	2281.833419	21.582797
76.630089	2279.936997	21.587815
76.385720	2287.322136	21.592832
76.595055	2290.050998	21.597850
76.647843	2293.555357	21.602867
76.850826	2291.030500	21.607885
77.034950	2303.994983	21.612903
77.094943	2313.396758	21.617920
77.352482	2312.709655	21.622938
77.151900	2312.469441	21.627955
77.329124	2313.366523	21.632973
77.705252	2311.505866	21.637991
77.537410	2311.412041	21.643008
77.505491	2304.549561	21.648026
77.464729	2311.950349	21.653043
77.651733	2315.092970	21.658061
77.862735	2307.009173	21.663079
78.069121	2319.487335	21.668096
78.071321	2314.503663	21.673114
77.882962	2309.694836	21.678131
77.719112	2308.243317	21.683149
77.768251	2301.945762	21.688167
77.864392	2319.430698	21.693184
78.227080	2317.303875	21.698202
78.160959	2327.110322	21.703219
78.147050	2337.243181	21.708237
78.470124	2330.546340	21.713255
78.163815	2343.375757	21.718272
78.369565	2338.101596	21.723290
78.359285	2352.945791	21.728307
78.336465	2349.903783	21.733325
78.498871	2352.434822	21.738343
78.621286	2364.616802	21.743360
78.864201	2378.004556	21.748378
79.238145	2383.724937	21.753395
79.224196	2376.193716	21.758413
79.244326	2378.317694	21.763431
79.352485	2377.969446	21.768448
79.553165	2378.133844	21.773466
79.711184	2381.744921	21.778483
79.471037	2383.884176	21.783501
79.552470	2375.419709	21.788519
79.341972	2391.371304	21.793536
79.971218	2384.156530	21.798554
79.888656	2392.213995	21.803571
79.657613	2404.362665	21.808589
79.966345	2398.349728	21.813607
80.135133	2395.173732	21.818624
80.023499	2399.167644	21.823642
80.463263	2398.310146	21.828659
80.607544	2411.441866	21.833677
80.750425	2414.976407	21.838695
80.891575	2419.618974	21.843712
80.556426	2402.259462	21.848730
80.696103	2403.222359	21.853747
80.785484	2405.584883	21.858765
81.102615	2403.941698	21.863783
81.078631	2407.716825	21.868800
81.304198	2415.615866	21.873818
81.430473	2407.469472	21.878835
81.101501	2404.689729	21.883853
81.730763	2408.997505	21.888871
81.269074	2412.768193	21.893888
81.193534	2406.565758	21.898906
81.396443	2404.627913	21.903923
81.143117	2408.751191	21.908941
81.600321	2414.064118	21.913959
81.697685	2429.535442	21.918976
81.925544	2421.095496	21.923994
81.887313	2425.144261	21.929011
81.819241	2425.811280	21.934029
81.842410	2419.719712	21.939047
81.939989	2440.748735	21.944064
82.006215	2442.392143	21.949082
82.349238	2448.612852	21.954099
82.357830	2454.787796	21.959117
82.457088	2447.658668	21.964135
82.548551	2450.989769	21.969152
82.701040	2444.076432	21.974170
83.077020	2436.973657	21.979187
82.751612	2445.873737	21.984205
82.949597	2433.263039	21.989223
82.915681	2442.363902	21.994240
82.974764	2454.019282	21.999258
83.056688	2467.236496	22.004275
82.925493	2468.232101	22.009293
82.803995	2467.578758	22.014311
82.774692	2473.652304	22.019328
83.166685	2477.924451	22.024346
83.445840	2482.763314	22.029363
83.397293	2487.347065	22.034381
83.462885	2484.060880	22.039399
83.627719	2482.813810	22.044416
83.770998	2494.535008	22.049434
84.027414	2489.912521	22.054451
84.047005	2496.963139	22.059469
84.078184	2501.790119	22.064487
83.825181	2507.182089	22.069504
83.698679	2507.343776	22.074522
84.131311	2501.314671	22.079539
84.100802	2522.840291	22.084557
84.569184	2526.122190	22.089575
84.886382	2531.838829	22.094592
84.870740	2534.962543	22.099610
84.933659	2529.325528	22.104627
84.674847	2529.873915	22.109645
85.259153	2523.426684	22.114663
85.185672	2532.344392	22.119680
85.297844	2526.327299	22.124698
85.430940	2520.363758	22.129715
85.203444	2524.763927	22.134733
85.500762	2528.984550	22.139751
85.665081	2517.013396	22.144768
85.805823	2525.260231	22.149786
85.735013	2522.847401	22.154803
85.665676	2539.938566	22.159821
85.975861	2535.528618	22.164839
86.012157	2550.002782	22.169856
85.799469	2553.646362	22.174874
86.168257	2543.625340	22.179891
85.954314	2552.770069	22.184909
86.264941	2547.690971	22.189927
86.248826	2546.415260	22.194944
86.154449	2547.954286	22.199962
86.518634	2557.829573	22.204979
86.836835	2568.602026	22.209997
86.983155	2564.839321	22.215015
87.021502	2579.060707	22.220032
87.067492	2577.781637	22.225050
87.250622	2566.672273	22.230067
86.899125	2561.888777	22.235085
86.960344	2557.729040	22.240103
87.363585	2562.823179	22.245120
87.095370	2567.419060	22.250138
87.363876	2565.991730	22.255155
87.154800	2575.233549	22.260173
87.781152	2582.196044	22.265191
87.694638	2583.399309	22.270208
87.532131	2589.720867	22.275226
87.605928	2588.197609	22.280243
87.580441	2591.127191	22.285261
87.975494	2597.421908	22.290279
88.013418	2606.076137	22.295296
87.624280	2613.506041	22.300314
88.190013	2611.729451	22.305331
87.926511	2616.517129	22.310349
88.278039	2602.115025	22.315367
88.668827	2619.507039	22.320384
88.551463	2630.246350	22.325402
88.871557	2638.736733	22.330419
88.727810	2638.320395	22.335437
88.859536	2642.156541	22.340455
89.146140	2633.612668	22.345472
89.191508	2623.316884	22.350490
89.246327	2625.972018	22.355507
89.064796	2628.222105	22.360525
89.285343	2629.506963	22.365543
89.144062	2633.991573	22.370560
89.540315	2635.113365	22.375578
89.326006	2627.881497	22.380595
89.641914	2644.960122	22.385613
89.500048	2657.028802	22.390631
89.901567	2660.232767	22.395648
89.967325	2657.044362	22.400666
89.596439	2657.894245	22.405683
89.870140	2661.260132	22.410701
90.254353	2665.514600	22.415719
90.290596	2668.551357	22.420736
90.263622	2687.709590	22.425754
90.386717	2679.948605	22.430771
90.294771	2685.599597	22.435789
90.520720	2685.062577	22.440807
90.335485	2683.601733	22.445824
90.315806	2697.361995	22.450842
90.480523	2716.029630	22.455859
90.847010	2715.972541	22.460877
90.981760	2706.922059	22.465895
91.286240	2709.023898	22.470912
90.890614	2724.285031	22.475930
91.040728	2726.410905	22.480947
91.206675	2735.777469	22.485965
91.312347	2727.375341	22.490983
91.931742	2731.176608	22.496000
91.418179	2740.301803	22.501018
91.875823	2749.275792	22.506035
92.392897	2751.843194	22.511053
92.105698	2750.354035	22.516071
91.956131	2753.662753	22.521088
92.133066	2751.530083	22.526106
92.664258	2749.809355	22.531123
92.358363	2749.364606	22.536141
92.430311	2744.275273	22.541159
92.549569	2747.611570	22.546176
92.853137	2748.548969	22.551194
92.879450	2739.805711	22.556211
92.903925	2757.829295	22.561229
93.084985	2767.332389	22.566247
92.939761	2773.070605	22.571264
92.704078	2771.592359	22.576282
93.101628	2772.486722	22.581299
93.102801	2778.322077	22.586317
92.970658	2772.863691	22.591335
93.120892	2788.005174	22.596352
93.430966	2802.228616	22.601370
93.454618	2790.257088	22.606387
93.239911	2792.575481	22.611405
93.580223	2811.957553	22.616423
93.736521	2813.047283	22.621440
93.626221	2819.701649	22.626458
93.834420	2812.555416	22.631475
94.130416	2834.412460	22.636493
94.051676	2832.246998	22.641511
94.639866	2833.698713	22.646528
94.779895	2839.108491	22.651546
95.006339	2834.171819	22.656563
94.866565	2836.061950	22.661581
94.897424	2844.950943	22.666599
95.106929	2832.417074	22.671616
95.214488	2827.726150	22.676634
95.551069	2830.204891	22.681651
95.498576	2820.441827	22.686669
95.276911	2834.107399	22.691687
95.274123	2824.560675	22.696704
95.382010	2827.766202	22.701722
95.311205	2831.539239	22.706739
95.527227	2823.927840	22.711757
95.505483	2840.964540	22.716775
95.686393	2839.440364	22.721792
95.272553	2845.362448	22.726810
95.683357	2855.461035	22.731827
95.790379	2847.999152	22.736845
96.115244	2865.572097	22.741863
96.380474	2874.569795	22.746880
96.172196	2878.133852	22.751898
96.415297	2868.106970	22.756915
96.531431	2869.998290	22.761933
96.341110	2863.946122	22.766951
96.903406	2867.813119	22.771968
97.025529	2890.224368	22.776986
97.228544	2889.605699	22.782003
97.031962	2887.736313	22.787021
97.160176	2890.910281	22.792039
97.359246	2888.133463	22.797056
97.300400	2892.570586	22.802074
97.246682	2892.954495	22.807091
97.541022	2897.181981	22.812109
97.732078	2898.461983	22.817127
98.092790	2905.705826	22.822144
97.839498	2915.062011	22.827162
97.916815	2918.692073	22.832179
98.279786	2911.799439	22.837197
98.214318	2912.806928	22.842215
97.908770	2903.954298	22.847232
97.985990	2916.118442	22.852250
98.284836	2918.606226	22.857267
98.440388	2926.541643	22.862285
98.501470	2938.698845	22.867303
99.046557	2930.600627	22.872320
98.953093	2933.294674	22.877338
98.834753	2919.249520	22.882355
99.227957	2919.882613	22.887373
98.849890	2924.580902	22.892391
99.181065	2926.978439	22.897408
99.530386	2943.114787	22.902426
99.707478	2951.375095	22.907443
99.674025	2941.157679	22.912461
99.526052	2939.769914	22.917479
99.615287	2942.227214	22.922496
99.490258	2944.979831	22.927514
99.574013	2953.055838	22.932531
100.247300	2956.880324	22.937549
100.149520	2973.335642	22.942567
100.394863	2968.241342	22.947584
100.373321	2974.181292	22.952602
100.355233	2967.228034	22.957619
100.402697	2974.552237	22.962637
100.145798	2970.375654	22.967655
100.408813	2979.752482	22.972672
100.826868	2995.041808	22.977690
100.428596	2992.894514	22.982707
101.068630	2993.533365	22.987725
100.836181	2996.684603	22.992743
101.080162	3012.061011	22.997760
101.126400	3017.775808	23.002778
101.389813	3017.378127	23.007795
101.872865	2996.964938	23.012813
101.907373	3014.595860	23.017831
101.748426	3014.841506	23.022848
102.000830	3017.863605	23.027866
101.595175	3016.793691	23.032883
102.323285	3003.134287	23.037901
101.828935	3012.903630	23.042919
102.138733	3019.369576	23.047936
102.361593	3027.603857	23.052954
102.260383	3036.807026	23.057971
102.698482	3034.466387	23.062989
102.462961	3037.984219	23.068007
102.525474	3037.662002	23.073024
102.794341	3039.188701	23.078042
102.432573	3052.109315	23.083059
102.706355	3056.207484	23.088077
102.747413	3065.012939	23.093095
102.783762	3061.431371	23.098112
103.184247	3078.090102	23.103130
103.574708	3080.165974	23.108147
103.860627	3079.875252	23.113165
103.965815	3083.785060	23.118183
103.822979	3079.600161	23.123200
103.801161	3083.526587	23.128218
103.981318	3078.180447	23.133235
104.395189	3084.964762	23.138253
103.904460	3084.059582	23.143271
104.164121	3080.484272	23.148288
104.655770	3085.223936	23.153306
104.388526	3098.732687	23.158323
104.868982	3104.692362	23.163341
104.275219	3099.258406	23.168359
104.775700	3099.376135	23.173376
104.638982	3100.057022	23.178394
104.969748	3104.578719	23.183411
105.436405	3119.109426	23.188429
104.914180	3127.955270	23.193447
105.249837	3125.046686	23.198464
105.498199	3131.885192	23.203482
105.388843	3124.879804	23.208499
105.339790	3126.831587	23.213517
105.650172	3141.762223	23.218535
105.939947	3150.869859	23.223552
105.908994	3145.698594	23.228570
106.145250	3153.447959	23.233587
106.493940	3148.637351	23.238605
106.281523	3153.616053	23.243623
106.236468	3153.985994	23.248640
106.409164	3151.380517	23.253658
106.211550	3153.478522	23.258675
106.218969	3163.071984	23.263693
106.602736	3171.278123	23.268711
106.607256	3178.757433	23.273728
106.875138	3182.907048	23.278746
106.749738	3196.015051	23.283763
107.100441	3198.510581	23.288781
106.908930	3195.030741	23.293799
107.298146	3205.170761	23.298816
107.676961	3207.889158	23.303834
107.699956	3218.401818	23.308851
108.005535	3214.724648	23.313869
107.994620	3208.603401	23.318887
107.978773	3211.490554	23.323904
108.191513	3213.038631	23.328922
108.128384	3208.718203	23.333939
108.126767	3208.589024	23.338957
108.676888	3218.700844	23.343975
108.373268	3226.698415	23.348992
108.664086	3226.031347	23.354010
108.641169	3225.741365	23.359027
108.806786	3228.745450	23.364045
109.168177	3225.267894	23.369063
108.877177	3231.328785	23.374080
109.019193	3224.233723	23.379098
108.935325	3238.727151	23.384115
109.161130	3245.149445	23.389133
108.929018	3249.531571	23.394151
108.974054	3255.088823	23.399168
109.458128	3254.262264	23.404186
109.459291	3277.652298	23.409203
109.527161	3282.012977	23.414221
109.786236	3286.466977	23.419239
110.080411	3288.071817	23.424256
109.994634	3304.244670	23.429274
110.036879	3302.981913	23.434291
110.232481	3300.540125	23.439309
110.326053	3303.956272	23.444327
110.393357	3316.933363	23.449344
111.075835	3331.531639	23.454362
111.039328	3329.343760	23.459379
110.977163	3323.091583	23.464397
111.144410	3325.833469	23.469415
111.227215	3333.253313	23.474432
111.395244	3327.375596	23.479450
111.549925	3330.873763	23.484467
111.462658	3340.617776	23.489485
111.641566	3355.101947	23.494503
111.664303	3352.876436	23.499520
111.931398	3358.613766	23.504538
111.879666	3358.864816	23.509555
112.094041	3353.731043	23.514573
112.205223	3363.409454	23.519591
111.926943	3370.105958	23.524608
112.012258	3374.429224	23.529626
112.035159	3372.516147	23.534643
112.726710	3384.588116	23.539661
113.006567	3398.160251	23.544679
112.834600	3394.494272	23.549696
113.346950	3394.010483	23.554714
113.250367	3390.313831	23.559731
113.428273	3390.983618	23.564749
113.153098	3386.762441	23.569767
113.350201	3398.643127	23.574784
113.966037	3397.732924	23.579802
113.854771	3417.413202	23.584819
113.886976	3409.079005	23.589837
114.218507	3410.605448	23.594855
114.233096	3408.640005	23.599872
114.192305	3403.470197	23.604890
114.334819	3405.436371	23.609907
114.218837	3395.850157	23.614925
114.201704	3413.281202	23.619943
114.342782	3429.879650	23.624960
114.906437	3430.281073	23.629978
114.534768	3432.810200	23.634995
114.860519	3428.580670	23.640013
114.998885	3437.775149	23.645031
114.876305	3455.708705	23.650048
115.190930	3450.852822	23.655066
114.988258	3456.634917	23.660083
115.193769	3458.758566	23.665101
115.382650	3473.831487	23.670119
115.230851	3480.713491	23.675136
115.600537	3482.906268	23.680154
115.592679	3493.976226	23.685171
116.158163	3511.679619	23.690189
116.200705	3508.545178	23.695207
116.110366	3516.730604	23.700224
116.287771	3511.779289	23.705242
116.371302	3520.104925	23.710259
116.679535	3522.692331	23.715277
116.754950	3520.521722	23.720295
116.770589	3523.511333	23.725312
116.961104	3524.201256	23.730330
117.111787	3530.786846	23.735347
117.058214	3519.537001	23.740365
117.507909	3524.005569	23.745383
117.488532	3543.573836	23.750400
117.884394	3537.256585	23.755418
117.903921	3528.409847	23.760435
118.082671	3529.966400	23.765453
118.503230	3530.065015	23.770471
118.470883	3535.160972	23.775488
118.858661	3535.394095	23.780506
118.541836	3536.412347	23.785523
118.626383	3536.291844	23.790541
119.041227	3526.654476	23.795559
118.828492	3524.973753	23.800576
118.744960	3521.682191	23.805594
118.833492	3518.509025	23.810611
118.865468	3535.010934	23.815629
119.009709	3526.046937	23.820647
118.986744	3543.381174	23.825664
119.469828	3546.083390	23.830682
119.343094	3549.868441	23.835699
119.447960	3556.151866	23.840717
119.328403	3555.845362	23.845735
119.569874	3574.366222	23.850752
119.638875	3573.692647	23.855770
119.725644	3581.317129	23.860787
119.618708	3590.407848	23.865805
120.258743	3596.734214	23.870823
120.422247	3600.136373	23.875840
120.547429	3592.728167	23.880858
120.602781	3603.318075	23.885875
120.505444	3619.938036	23.890893
121.055672	3621.783944	23.895911
120.757722	3628.878132	23.900928
120.992575	3629.848372	23.905946
121.203734	3641.004256	23.910963
121.329359	3644.472290	23.915981
120.989401	3643.638292	23.920999
121.129253	3654.360260	23.926016
121.268531	3655.326444	23.931034
121.344663	3670.114085	23.936051
121.394330	3681.168889	23.941069
122.187648	3689.699718	23.946087
122.061326	3700.781933	23.951104
122.372152	3695.850827	23.956122
122.710195	3700.418885	23.961139
122.386483	3706.005281	23.966157
122.867579	3716.977155	23.971175
122.898813	3724.272627	23.976192
123.159852	3709.227234	23.981210
123.213244	3711.977437	23.986227
123.347664	3720.311024	23.991245
123.464488	3715.511116	23.996263
123.317189	3733.691826	24.001280
123.723934	3733.003536	24.006298
123.928459	3741.395655	24.011315
124.044485	3748.242376	24.016333
123.942980	3735.560615	24.021351
123.680357	3749.397380	24.026368
123.904233	3748.595530	24.031386
124.670140	3754.236389	24.036403
124.101137	3767.155060	24.041421
124.640162	3757.643423	24.046439
124.480769	3769.434671	24.051456
124.495854	3765.622711	24.056474
124.931182	3771.491793	24.061491
124.895231	3792.347500	24.066509
125.123043	3794.152093	24.071527
125.004643	3787.463480	24.076544
125.062847	3787.006203	24.081562
125.473341	3793.153751	24.086579
125.230182	3808.256342	24.091597
125.575656	3809.518680	24.096615
125.529412	3813.755224	24.101632
125.661155	3833.218213	24.106650
126.316526	3839.917872	24.111667
126.121793	3838.565723	24.116685
126.551885	3830.538665	24.121703
126.641011	3840.725766	24.126720
126.905058	3856.453274	24.131738
126.973639	3852.348904	24.136755
126.751972	3857.606990	24.141773
126.934833	3858.228680	24.146791
127.140057	3854.538599	24.151808
127.147252	3860.092460	24.156826
127.482638	3867.425855	24.161843
127.319400	3868.085649	24.166861
127.570579	3864.003348	24.171879
127.812205	3871.332405	24.176896
127.831770	3877.376722	24.181914
127.916927	3886.948997	24.186931
128.133283	3896.279912	24.191949
128.350069	3891.278175	24.196967
128.476845	3898.868156	24.201984
128.587524	3906.365959	24.207002
128.858993	3911.957598	24.212019
128.888729	3909.636241	24.217037
129.024003	3897.450910	24.222055
128.947544	3905.236662	24.227072
129.152526	3918.498909	24.232090
129.665996	3919.283754	24.237107
129.610469	3937.807039	24.242125
129.629984	3935.398895	24.247143
129.857875	3930.430137	24.252160
129.903519	3932.856485	24.257178
130.225354	3931.379715	24.262195
129.996582	3945.066172	24.267213
130.174608	3947.452973	24.272231
130.525062	3956.523165	24.277248
130.553686	3958.990041	24.282266
130.571832	3962.528527	24.287283
130.625422	3976.862269	24.292301
130.691011	3975.109764	24.297319
130.828525	3978.121508	24.302336
131.145404	3991.902954	24.307354
131.504854	4007.574708	24.312371
131.372893	4014.955675	24.317389
131.405907	4013.135644	24.322407
131.949446	4009.818957	24.327424
131.388884	4016.717462	24.332442
131.554351	4023.054740	24.337459
132.133288	4044.528325	24.342477
132.005080	4041.193123	24.347495
131.813126	4038.975703	24.352512
132.276438	4061.616199	24.357530
132.631776	4063.277869	24.362547
132.401466	4068.275389	24.367565
132.726174	4085.650705	24.372583
132.834131	4088.332502	24.377600
132.914947	4095.686687	24.382618
133.145225	4078.894031	24.387635
133.160973	4092.574092	24.392653
133.604732	4103.005976	24.397671
133.720948	4104.566002	24.402688
133.509434	4109.819424	24.407706
134.016745	4106.053853	24.412723
133.761447	4119.324783	24.417741
134.206733	4127.133557	24.422759
134.512929	4134.922957	24.427776
134.634279	4142.040441	24.432794
134.735949	4132.707171	24.437811
134.608071	4137.477290	24.442829
134.915699	4147.750485	24.447847
135.162013	4158.336238	24.452864
134.942556	4149.961973	24.457882
135.180581	4155.530488	24.462899
135.490043	4157.218248	24.467917
135.371744	4164.426708	24.472935
135.637220	4174.539197	24.477952
135.489948	4188.800222	24.482970
135.697852	4182.761361	24.487987
135.568342	4190.580745	24.493005
136.176863	4201.665642	24.498023
135.974168	4204.241162	24.503040
136.236776	4220.306936	24.508058
136.725028	4220.887405	24.513075
136.744815	4226.704549	24.518093
136.860314	4233.125432	24.523111
136.841573	4228.965134	24.528128
137.119779	4243.560812	24.533146
137.631713	4250.241925	24.538163
137.667436	4247.282015	24.543181
137.430943	4252.230046	24.548199
137.790243	4251.760599	24.553216
137.568055	4269.584217	24.558234
137.872519	4275.076142	24.563251
138.041961	4282.883741	24.568269
138.084477	4291.998889	24.573287
138.446112	4300.761349	24.578304
138.423632	4295.954569	24.583322
138.767682	4290.491022	24.588339
138.631028	4306.606410	24.593357
138.852412	4316.381802	24.598375
139.385320	4327.955156	24.603392
139.274650	4326.744542	24.608410
139.421845	4328.795310	24.613427
139.442535	4327.674717	24.618445
139.517970	4341.307797	24.623463
139.484464	4344.223130	24.628480
139.590896	4347.612223	24.633498
140.034684	4360.367319	24.638515
140.362940	4377.089001	24.643533
140.203740	4374.995849	24.648551
140.716859	4372.482390	24.653568
140.448499	4374.866151	24.658586
140.646053	4394.029115	24.663603
141.130711	4402.033885	24.668621
140.988980	4409.694293	24.673639
141.403973	4408.196670	24.678656
140.879353	4406.880056	24.683674
141.300572	4426.503778	24.688691
141.328195	4423.920707	24.693709
141.613433	4435.371716	24.698727
142.296910	4447.985397	24.703744
142.019069	4463.766237	24.708762
142.456757	4455.160108	24.713779
142.656180	4441.720819	24.718797
142.984340	4435.334890	24.723815
143.062371	4432.229483	24.728832
143.008891	4440.665253	24.733850
143.123690	4440.366435	24.738867
143.629058	4435.619473	24.743885
143.313677	4439.655025	24.748903
143.165900	4429.681823	24.753920
143.092551	4444.922636	24.758938
143.374060	4448.653784	24.763955
143.610946	4463.363388	24.768973
143.440642	4458.238693	24.773991
144.145274	4473.891831	24.779008
143.808329	4486.411900	24.784026
144.130643	4490.651191	24.789043
144.118670	4507.170298	24.794061
144.389913	4506.629333	24.799079
144.724465	4517.832833	24.804096
144.923825	4520.989700	24.809114
145.167253	4523.688346	24.814131
145.470216	4538.621296	24.819149
145.146507	4541.985859	24.824167
145.422770	4533.976130	24.829184
145.383843	4541.743686	24.834202
145.440399	4556.784455	24.839219
145.897013	4558.458812	24.844237
145.653169	4566.542357	24.849255
145.893413	4573.044943	24.854272
146.043418	4591.940915	24.859290
146.472660	4591.905621	24.864307
146.656264	4599.206131	24.869325
146.445380	4617.924744	24.874343
146.247333	4626.367326	24.879360
146.644753	4630.525516	24.884378
146.885150	4636.939723	24.889395
146.966159	4641.781613	24.894413
146.550038	4660.595351	24.899431
147.461097	4664.389504	24.904448
147.371147	4689.945057	24.909466
147.503901	4695.444906	24.914483
147.664505	4705.334133	24.919501
147.940263	4721.865453	24.924519
148.410588	4715.589862	24.929536
148.596850	4730.623206	24.934554
148.733771	4735.914095	24.939571
149.028307	4735.849271	24.944589
148.573089	4747.949193	24.949607
149.164938	4738.359381	24.954624
149.035224	4755.335786	24.959642
149.257042	4764.268591	24.964659
149.714035	4766.700449	24.969677
149.956315	4777.268254	24.974695
149.807165	4785.640169	24.979712
150.215500	4802.201424	24.984730
150.291016	4797.931628	24.989747
150.527500	4802.342176	24.994765
150.290914	4811.081235	24.999783
150.616897	4824.044385	25.004800
150.904624	4821.777438	25.009818
150.854087	4827.744606	25.014835
150.806067	4831.669177	25.019853
150.996501	4847.131242	25.024871
150.925950	4839.020710	25.029888
151.110096	4862.567377	25.034906
151.598709	4872.768618	25.039923
151.956971	4876.140697	25.044941
151.686933	4889.547053	25.049959
152.207271	4892.117419	25.054976
152.245820	4904.468839	25.059994
152.417850	4903.491939	25.065011
152.413196	4899.812229	25.070029
152.304649	4920.642659	25.075047
152.580079	4914.318432	25.080064
152.759725	4930.830186	25.085082
153.189175	4937.252943	25.090099
153.550848	4942.149066	25.095117
153.031361	4956.162468	25.100135
153.733735	4950.955425	25.105152
153.926035	4956.916393	25.110170
154.265945	4974.545869	25.115187
154.376279	4966.937401	25.120205
154.264699	4982.285623	25.125223
154.199049	4985.540648	25.130240
154.251385	4991.277215	25.135258
154.464675	5005.302826	25.140275
154.740003	5002.397026	25.145293
154.421032	5015.501761	25.150311
154.923484	5025.202213	25.155328
155.337519	5032.523838	25.160346
155.059641	5037.863614	25.165363
155.316811	5052.027627	25.170381
155.454117	5056.131720	25.175399
155.722552	5063.592815	25.180416
156.080411	5074.628895	25.185434
156.082403	5071.557313	25.190451
156.167984	5085.015767	25.195469
156.570272	5103.004963	25.200487
156.692499	5104.122235	25.205504
157.103405	5110.866745	25.210522
156.929004	5121.395461	25.215539
157.264222	5128.104414	25.220557
157.055330	5132.123538	25.225575
157.472099	5134.842636	25.230592
157.738316	5151.877714	25.235610
157.941265	5160.930443	25.240627
157.829128	5152.365398	25.245645
157.833301	5159.687757	25.250663
158.418881	5182.796720	25.255680
158.319279	5186.158074	25.260698
158.391540	5187.762916	25.265715
158.996771	5200.442967	25.270733
158.815879	5211.976509	25.275751
158.972691	5217.494866	25.280768
158.996139	5212.144089	25.285786
159.564123	5222.973938	25.290803
159.873199	5225.514113	25.295821
159.933487	5229.036815	25.300839
159.933620	5225.406797	25.305856
160.421693	5244.219249	25.310874
160.522103	5256.466583	25.315891
160.483724	5247.949983	25.320909
160.575920	5258.232099	25.325927
160.693289	5259.874115	25.330944
160.864394	5271.668543	25.335962
160.984942	5278.073228	25.340979
161.629559	5278.938728	25.345997
161.441556	5279.239429	25.351015
161.639095	5298.049822	25.356032
161.596262	5300.578511	25.361050
161.487670	5305.450097	25.366067
162.018300	5311.658375	25.371085
162.070153	5312.376270	25.376103
162.257366	5332.592953	25.381120
162.599639	5327.776459	25.386138
162.742746	5342.318300	25.391155
162.529006	5345.113499	25.396173
162.555293	5354.190672	25.401191
162.709378	5354.690635	25.406208
163.282090	5363.357619	25.411226
163.260163	5372.407586	25.416243
163.565325	5370.169422	25.421261
163.481265	5382.865378	25.426279
164.175777	5387.469907	25.431296
164.363305	5394.871136	25.436314
164.040697	5402.598000	25.441331
164.312120	5403.253305	25.446349
164.445093	5421.811887	25.451367
164.690966	5423.948426	25.456384
164.843622	5430.089331	25.461402
164.699586	5435.269497	25.466419
165.256252	5440.110145	25.471437
165.268485	5445.856255	25.476455
165.283657	5457.703489	25.481472
165.474986	5479.532684	25.486490
165.394349	5475.328076	25.491507
165.476211	5482.758418	25.496525
165.276008	5500.178937	25.501543
165.822291	5523.436496	25.506560
166.317383	5529.309475	25.511578
166.194162	5545.682705	25.516595
166.894639	5559.980115	25.521613
166.595090	5564.783647	25.526631
166.935028	5568.928909	25.531648
167.535614	5583.898453	25.536666
167.506247	5590.718002	25.541683
167.612315	5601.067596	25.546701
168.092062	5612.618485	25.551719
168.043426	5605.362783	25.556736
168.246094	5610.081824	25.561754
168.261876	5627.765555	25.566771
168.512523	5624.001758	25.571789
168.770023	5635.404183	25.576807
168.917722	5652.107804	25.581824
169.728031	5662.133142	25.586842
169.448194	5659.159001	25.591859
169.517662	5655.663305	25.596877
169.644527	5661.849339	25.601895
169.545552	5679.560457	25.606912
169.991194	5685.542196	25.611930
170.074774	5685.478650	25.616947
170.153785	5690.699919	25.621965
170.534990	5695.738409	25.626983
170.452274	5704.242448	25.632000
170.955507	5716.957680	25.637018
170.947154	5732.864960	25.642035
171.380526	5728.318271	25.647053
171.248496	5731.719496	25.652071
171.456177	5748.019293	25.657088
171.351668	5756.905540	25.662106
171.699289	5769.872311	25.667123
171.719710	5781.059211	25.672141
172.043844	5791.807416	25.677159
171.977905	5799.693351	25.682176
172.467068	5811.684825	25.687194
172.746626	5818.336411	25.692212
172.707750	5823.213064	25.697229
172.919144	5824.392257	25.702247
172.820994	5842.586363	25.707264
173.359395	5840.374962	25.712282
173.442246	5862.729717	25.717300
173.791143	5862.672212	25.722317
173.979221	5870.916363	25.727335
173.687473	5880.841934	25.732352
174.325326	5893.397441	25.737370
173.950929	5900.296076	25.742388
174.357151	5894.026907	25.747405
174.723675	5899.354991	25.752423
174.908910	5911.791582	25.757440
175.295860	5913.697879	25.762458
175.099165	5925.366909	25.767476
174.913568	5935.370682	25.772493
175.552297	5930.356358	25.777511
175.443999	5951.734022	25.782528
175.690306	5962.443938	25.787546
175.888054	5967.179621	25.792564
176.140977	5965.299904	25.797581
176.109693	5991.564702	25.802599
176.549827	5994.693812	25.807616
176.712360	5991.151996	25.812634
176.960238	6014.977486	25.817652
176.742751	6018.392069	25.822669
177.083140	6022.742546	25.827687
177.211632	6044.721093	25.832704
177.263355	6046.348148	25.837722
177.931082	6068.694169	25.842740
177.491109	6080.751562	25.847757
178.397229	6091.728155	25.852775
178.246001	6103.784801	25.857792
178.614017	6101.009604	25.862810
178.479034	6115.226030	25.867828
178.580324	6115.039772	25.872845
179.099021	6130.451821	25.877863
179.062621	6142.992522	25.882880
179.337293	6162.644096	25.887898
179.547143	6160.938368	25.892916
179.874753	6167.756218	25.897933
180.195974	6182.861294	25.902951
180.235281	6174.032284	25.907968
180.486912	6189.934209	25.912986
180.890531	6203.230333	25.918004
180.857604	6201.338277	25.923021
181.124007	6201.814464	25.928039
181.175205	6214.976066	25.933056
181.211193	6212.786022	25.938074
181.365242	6227.503639	25.943092
181.510476	6234.611912	25.948109
181.973931	6244.382222	25.953127
181.908091	6252.063154	25.958144
182.150245	6257.407550	25.963162
182.334292	6270.308601	25.968180
182.605045	6278.559005	25.973197
182.908353	6279.878595	25.978215
182.668759	6296.049648	25.983232
183.155294	6296.882994	25.988250
183.110595	6302.278376	25.993268
183.466119	6317.021518	25.998285
183.940722	6321.401678	26.003303
183.914739	6320.809082	26.008320
184.415784	6339.898436	26.013338
184.540978	6346.665794	26.018356
184.402039	6347.182996	26.023373
184.919441	6347.036123	26.028391
185.004819	6350.447808	26.033408
185.311614	6363.408732	26.038426
185.001553	6373.135392	26.043444
185.096692	6374.563160	26.048461
185.267472	6384.701095	26.053479
185.495629	6401.579121	26.058496
185.688927	6409.459682	26.063514
186.180095	6419.651927	26.068532
186.008569	6437.640237	26.073549
186.748648	6443.895214	26.078567
186.345420	6456.003952	26.083584
186.540986	6457.210905	26.088602
186.943503	6463.111228	26.093620
186.562506	6487.439302	26.098637
187.099208	6481.001255	26.103655
186.994806	6499.282218	26.108672
187.133480	6511.606512	26.113690
187.355784	6517.733784	26.118708
187.462297	6540.050960	26.123725
188.027305	6543.530061	26.128743
188.100429	6563.964745	26.133760
188.233125	6574.556970	26.138778
188.843614	6592.531009	26.143796
188.715216	6593.775781	26.148813
189.189321	6602.174605	26.153831
189.309911	6622.649316	26.158848
189.528460	6621.532501	26.163866
189.220564	6630.340351	26.168884
189.447830	6652.430519	26.173901
190.032536	6656.310638	26.178919
190.132919	6679.339205	26.183936
190.566118	6680.360809	26.188954
191.128534	6692.249913	26.193972
190.779096	6700.073045	26.198989
191.447692	6700.669721	26.204007
191.117802	6714.743336	26.209024
191.419441	6726.912976	26.214042
191.647857	6727.672887	26.219060
191.477236	6748.335130	26.224077
191.995025	6755.366662	26.229095
192.026842	6763.875458	26.234112
192.192063	6773.594626	26.239130
192.580918	6792.083195	26.244148
192.616650	6792.333301	26.249165
192.921829	6800.638560	26.254183
193.241878	6809.364514	26.259200
193.484639	6824.646489	26.264218
193.697575	6833.695338	26.269236
193.979363	6837.234374	26.274253
194.101956	6847.935661	26.279271
194.274416	6856.226883	26.284288
194.492103	6860.483021	26.289306
194.509691	6871.781516	26.294324
195.103017	6888.186444	26.299341
195.137283	6882.814553	26.304359
195.051600	6905.787140	26.309376
195.074323	6910.667119	26.314394
195.413620	6918.550424	26.319412
195.346446	6937.018592	26.324429
195.708483	6951.830682	26.329447
195.823823	6962.280621	26.334464
196.299555	6964.037466	26.339482
196.661945	6974.297423	26.344500
196.706071	6990.061883	26.349517
196.884351	6999.340342	26.354535
197.443670	7019.813484	26.359552
197.593493	7018.839932	26.364570
197.563610	7019.412780	26.369588
197.545525	7033.820067	26.374605
197.625171	7048.278443	26.379623
198.199431	7055.989484	26.384640
198.217672	7067.906733	26.389658
198.632162	7074.083191	26.394676
198.547524	7082.771263	26.399693
198.631821	7105.897575	26.404711
198.706472	7111.094675	26.409728
199.161529	7124.484481	26.414746
199.500255	7126.679373	26.419764
199.325380	7138.724596	26.424781
199.552450	7156.954608	26.429799
199.847782	7156.952795	26.434816
199.973347	7172.840476	26.439834
200.279818	7176.019014	26.444852
200.571539	7187.091927	26.449869
200.639164	7201.637530	26.454887
201.045260	7213.702840	26.459904
201.103587	7222.671777	26.464922
201.734738	7232.776390	26.469940
201.488065	7245.732560	26.474957
201.100335	7254.161688	26.479975
201.579864	7266.534441	26.484992
201.998961	7290.679031	26.490010
202.230563	7305.199187	26.495028
202.191926	7311.727232	26.500045
202.530390	7326.650628	26.505063
202.700840	7334.273127	26.510080
202.890821	7354.172773	26.515098
203.438047	7361.433564	26.520116
203.733269	7386.907665	26.525133
203.828761	7379.947664	26.530151
204.287881	7395.931980	26.535168
204.200810	7407.982650	26.540186
204.615814	7402.462939	26.545204
204.867231	7428.698409	26.550221
205.191125	7429.989625	26.555239
205.164555	7438.050078	26.560256
205.551772	7448.748398	26.565274
205.984193	7452.466143	26.570292
205.861731	7461.283401	26.575309
206.070429	7464.505623	26.580327
206.439857	7474.632176	26.585344
206.379142	7481.886645	26.590362
206.685402	7487.218264	26.595380
206.507645	7512.500999	26.600397
206.636037	7510.122785	26.605415
206.969362	7521.435661	26.610432
207.410218	7535.244689	26.615450
207.718769	7542.842617	26.620468
207.786246	7561.754511	26.625485
207.818644	7562.475525	26.630503
208.260771	7577.809168	26.635520
208.279997	7597.814585	26.640538
208.532953	7595.956798	26.645556
208.336334	7613.179880	26.650573
208.666356	7630.677716	26.655591
208.860283	7647.833713	26.660608
208.929922	7667.127366	26.665626
209.730562	7678.225522	26.670644
209.742278	7686.299063	26.675661
210.068284	7698.999076	26.680679
210.767418	7705.614441	26.685696
210.525676	7726.869729	26.690714
210.811259	7722.014085	26.695732
210.716661	7739.701254	26.700749
211.358819	7747.323094	26.705767
211.950246	7737.255096	26.710784
212.071101	7754.236310	26.715802
212.322063	7764.289916	26.720820
212.337328	7772.110388	26.725837
212.345954	7772.670950	26.730855
212.791671	7778.066180	26.735872
212.985499	7788.368622	26.740890
213.118538	7794.674380	26.745908
213.111480	7800.932500	26.750925
213.527244	7817.034426	26.755943
213.593221	7816.702118	26.760960
213.566752	7826.912601	26.765978
214.074172	7829.990515	26.770996
214.198310	7855.810753	26.776013
214.391954	7851.509228	26.781031
214.541156	7852.445681	26.786048
214.695379	7874.788622	26.791066
215.011672	7879.547385	26.796084
215.056621	7890.681243	26.801101
215.121391	7899.182277	26.806119
215.725982	7903.028000	26.811136
216.149677	7914.832163	26.816154
216.090042	7933.827369	26.821172
216.354932	7928.870713	26.826189
216.367276	7941.465035	26.831207
216.727541	7954.554511	26.836224
216.471165	7971.048501	26.841242
216.892205	7974.474527	26.846260
216.718275	7984.812235	26.851277
217.076242	8004.639078	26.856295
217.928897	8010.826561	26.861312
217.635109	8036.251200	26.866330
217.512140	8035.370577	26.871348
218.095961	8055.528521	26.876365
218.358696	8077.779045	26.881383
218.283727	8081.017127	26.886400
218.580333	8105.696449	26.891418
219.123028	8117.832640	26.896436
219.526225	8137.917772	26.901453
219.387919	8148.455230	26.906471
219.946037	8156.491265	26.911488
219.807680	8172.907077	26.916506
220.352947	8193.598394	26.921524
220.418050	8208.284093	26.926541
220.147892	8224.306903	26.931559
220.574527	8236.240251	26.936576
221.143298	8255.068498	26.941594
221.298423	8266.848402	26.946612
221.879575	8277.605410	26.951629
222.064913	8295.066421	26.956647
222.365662	8294.997470	26.961664
222.622982	8318.249904	26.966682
222.494307	8326.421352	26.971700
223.174745	8340.143173	26.976717
223.336509	8337.365030	26.981735
223.887440	8334.340033	26.986752
224.183166	8354.378993	26.991770
224.365151	8355.872321	26.996788
224.378605	8357.047770	27.001805
224.739985	8358.311119	27.006823
224.912168	8358.871491	27.011840
224.708338	8373.157207	27.016858
224.915187	8384.184073	27.021876
225.164003	8387.867454	27.026893
225.309572	8401.009615	27.031911
225.353373	8409.523621	27.036928
225.623878	8424.171199	27.041946
225.909000	8436.540283	27.046964
226.754300	8451.101551	27.051981
226.777556	8469.042576	27.056999
226.390222	8470.801344	27.062016
226.649922	8483.528007	27.067034
226.761188	8503.021262	27.072052
227.252069	8519.992929	27.077069
227.488560	8520.306515	27.082087
227.552774	8538.913685	27.087104
227.597755	8552.128442	27.092122
228.010673	8584.471439	27.097140
228.521096	8594.671372	27.102157
228.487662	8607.683695	27.107175
228.632123	8616.412591	27.112192
228.796821	8639.010549	27.117210
228.902683	8651.770750	27.122228
229.228220	8656.490392	27.127245
229.250002	8678.877025	27.132263
229.658142	8690.188444	27.137280
229.707772	8702.237618	27.142298
230.208974	8713.345137	27.147316
230.334048	8739.671601	27.152333
230.540516	8759.175561	27.157351
230.785039	8769.107592	27.162368
230.906857	8784.829920	27.167386
231.655359	8796.842964	27.172404
232.212165	8808.005026	27.177421
231.737797	8827.842368	27.182439
232.372812	8840.908641	27.187456
232.579881	8849.801542	27.192474
232.631170	8869.658118	27.197492
233.324643	8872.359961	27.202509
233.114013	8886.962843	27.207527
233.477052	8893.072156	27.212544
233.807949	8909.980690	27.217562
233.509219	8924.916187	27.222580
234.203601	8932.224151	27.227597
234.134641	8958.306464	27.232615
234.368428	8976.455146	27.237632
234.816335	8981.853548	27.242650
235.113699	9000.364898	27.247668
235.362636	9011.748658	27.252685
235.130807	9029.164810	27.257703
235.877817	9038.204211	27.262720
236.326778	9050.702899	27.267738
236.518107	9060.062453	27.272756
236.864485	9065.059942	27.277773
236.952792	9090.047681	27.282791
237.077161	9100.677386	27.287808
237.302079	9107.900651	27.292826
237.897006	9123.729569	27.297844
237.901264	9128.748768	27.302861
237.620642	9152.600620	27.307879
238.166179	9158.949968	27.312896
238.448013	9174.726645	27.317914
238.615572	9191.834511	27.322932
238.777580	9208.706468	27.327949
238.699131	9228.087950	27.332967
239.417927	9230.681718	27.337984
239.520556	9253.558450	27.343002
239.739104	9267.109771	27.348020
240.330867	9287.356228	27.353037
240.496839	9298.655208	27.358055
240.668032	9306.145806	27.363072
241.445009	9311.350999	27.368090
241.326417	9321.371432	27.373108
241.504751	9338.329367	27.378125
241.359015	9338.449901	27.383143
241.713157	9354.682739	27.388160
242.176330	9375.157687	27.393178
242.060283	9388.644372	27.398196
242.517097	9395.522241	27.403213
242.734864	9420.913336	27.408231
242.539103	9438.920970	27.413248
243.182179	9450.701434	27.418266
243.492608	9465.788790	27.423284
243.876811	9470.477408	27.428301
243.904719	9477.835679	27.433319
244.255334	9493.216737	27.438336
244.890756	9511.972747	27.443354
244.782329	9521.556007	27.448372
245.155715	9528.626876	27.453389
245.185617	9540.556534	27.458407
245.241110	9552.229636	27.463424
245.760848	9548.385266	27.468442
245.832851	9566.193474	27.473460
245.884291	9586.398090	27.478477
246.165812	9594.051590	27.483495
246.091336	9614.256897	27.488512
246.492750	9635.029057	27.493530
246.859491	9651.759039	27.498548
247.395199	9671.402137	27.503565
247.298537	9688.690516	27.508583
247.619730	9705.159271	27.513600
247.846305	9717.011064	27.518618
248.148152	9742.645247	27.523636
248.225726	9752.307015	27.528653
248.632819	9762.372133	27.533671
248.671443	9781.038207	27.538688
249.290715	9786.763782	27.543706
249.685328	9808.313886	27.548724
249.835566	9821.784686	27.553741
250.057465	9838.287961	27.558759
250.400173	9849.392426	27.563776
250.815012	9871.362529	27.568794
250.519460	9884.170287	27.573812
251.172847	9896.994495	27.578829
251.366870	9918.326529	27.583847
251.239455	9933.356140	27.588864
251.861218	9946.740991	27.593882
251.857950	9963.389939	27.598900
252.239691	9979.028611	27.603917
252.318947	10004.587304	27.608935
252.525297	10017.746409	27.613952
253.136526	10027.599923	27.618970
253.114643	10051.523150	27.623988
253.577424	10064.923366	27.629005
253.739951	10089.556745	27.634023
253.814938	10107.393423	27.639040
254.354022	10123.320296	27.644058
254.866438	10138.664070	27.649076
255.130804	10151.340636	27.654093
255.025115	10177.048338	27.659111
255.364633	10189.416440	27.664128
255.793959	10181.579348	27.669146
256.132225	10218.066623	27.674164
256.350180	10224.498914	27.679181
256.375274	10237.275937	27.684199
256.899614	10256.173131	27.689216
257.272858	10272.350123	27.694234
257.267687	10284.247830	27.699252
257.745896	10301.475694	27.704269
258.023277	10306.531623	27.709287
258.326185	10328.579684	27.714304
258.617065	10336.383587	27.719322
258.732242	10349.591852	27.724340
258.652399	10372.391018	27.729357
259.223332	10387.129143	27.734375
259.312661	10388.697053	27.739392
259.458255	10413.185100	27.744410
259.669163	10434.575087	27.749428
260.061049	10447.500379	27.754445
260.344680	10465.099686	27.759463
260.132795	10485.150515	27.764480
261.011399	10497.820096	27.769498
260.843447	10513.026984	27.774516
261.392978	10533.136136	27.779533
261.572362	10551.244309	27.784551
261.903135	10567.216624	27.789568
262.463936	10578.701191	27.794586
262.423034	10590.592026	27.799604
263.336938	10594.737481	27.804621
263.433132	10604.406264	27.809639
263.403818	10619.440099	27.814656
263.803859	10626.343053	27.819674
263.756945	10636.346717	27.824692
263.862045	10650.030376	27.829709
264.301168	10657.517695	27.834727
264.141880	10673.579026	27.839744
264.269476	10681.215893	27.844762
264.805407	10703.082877	27.849780
264.888284	10717.774108	27.854797
265.339716	10742.161296	27.859815
265.381664	10758.895480	27.864832
265.585276	10772.421806	27.869850
265.698203	10795.491434	27.874868
265.989883	10817.551293	27.879885
266.532686	10850.506350	27.884903
266.562325	10866.393190	27.889920
267.091101	10880.115253	27.894938
267.240141	10898.364258	27.899956
267.877980	10911.160015	27.904973
268.555589	10929.370963	27.909991
268.785823	10946.369646	27.915008
269.150592	10964.777735	27.920026
269.288244	10973.281461	27.925044
269.487133	10994.550819	27.930061
270.070179	11002.464233	27.935079
270.145882	11012.676348	27.940096
270.731686	11015.076372	27.945114
270.605357	11028.979473	27.950132
271.004809	11042.870192	27.955149
271.117592	11051.680945	27.960167
271.566933	11072.791416	27.965184
271.804068	11070.430553	27.970202
271.697262	11102.419957	27.975220
271.764830	11109.005425	27.980237
272.504713	11128.738261	27.985255
272.448250	11148.421435	27.990272
272.902728	11161.403786	27.995290
273.276353	11187.155083	28.000308
273.210614	11203.991683	28.005325
273.974513	11217.434261	28.010343
273.788319	11232.294088	28.015360
273.982713	11249.939603	28.020378
274.171147	11263.241307	28.025396
274.759267	11292.063202	28.030413
275.025017	11302.883708	28.035431
274.972062	11322.184457	28.040448
275.530672	11335.561198	28.045466
275.411107	11364.177627	28.050484
275.674458	11386.646734	28.055501
276.210384	11400.456479	28.060519
276.081467	11430.441683	28.065536
276.501680	11451.838139	28.070554
277.169794	11481.184657	28.075572
277.381274	11500.618086	28.080589
277.866512	11515.660943	28.085607
278.212538	11528.793053	28.090624
278.713108	11546.346974	28.095642
278.779221	11561.625630	28.100660
278.791470	11587.260071	28.105677
279.226638	11591.385560	28.110695
279.382921	11606.085006	28.115712
279.872093	11623.328173	28.120730
280.086484	11638.015440	28.125748
280.486836	11640.302329	28.130765
280.545466	11659.203983	28.135783
280.674490	11680.058722	28.140800
281.050202	11684.547139	28.145818
281.536789	11709.539533	28.150836
281.277073	11724.196478	28.155853
281.681702	11734.411456	28.160871
281.763857	11763.619137	28.165888
282.339874	11781.385723	28.170906
282.616874	11801.829173	28.175924
282.605950	11817.742081	28.180941
283.258081	11831.805609	28.185959
283.215665	11856.773197	28.190976
283.771684	11870.460172	28.195994
284.311135	11896.527651	28.201012
284.320520	11910.129246	28.206029
284.205023	11930.599209	28.211047
284.776687	11953.876716	28.216064
285.176248	11971.462550	28.221082
285.475501	11987.428356	28.226100
285.879060	12007.293423	28.231117
285.985273	12024.126091	28.236135
286.472565	12048.591498	28.241152
286.922925	12060.675184	28.246170
287.086840	12072.535071	28.251188
287.477532	12100.593217	28.256205
287.864502	12102.923296	28.261223
287.843594	12132.599142	28.266240
288.255131	12152.141038	28.271258
288.218443	12168.219295	28.276276
288.240370	12185.415731	28.281293
288.678912	12203.595674	28.286311
288.961197	12232.109811	28.291328
289.692237	12246.767643	28.296346
290.036972	12271.299743	28.301364
290.420625	12289.049394	28.306381
290.814421	12298.287480	28.311399
290.999281	12306.143449	28.316416
291.767267	12324.398527	28.321434
292.025932	12337.026941	28.326452
292.558381	12355.315562	28.331469
292.492673	12357.738253	28.336487
292.562883	12385.164652	28.341504
293.067733	12391.455137	28.346522
293.220641	12409.073466	28.351540
293.179819	12419.080289	28.356557
293.870656	12440.770461	28.361575
293.931424	12462.040882	28.366592
294.533370	12471.041396	28.371610
294.831055	12481.185015	28.376628
294.823433	12505.049156	28.381645
295.160464	12522.749447	28.386663
295.371195	12531.523542	28.391680
295.320793	12556.408043	28.396698
295.904505	12568.499715	28.401716
295.855159	12594.482997	28.406733
296.189069	12610.939704	28.411751
296.449427	12639.669442	28.416768
297.038347	12653.550806	28.421786
297.332753	12674.541947	28.426804
297.111861	12700.754178	28.431821
297.543380	12719.753576	28.436839
297.898271	12742.197422	28.441856
298.556917	12764.309805	28.446874
298.792690	12779.079896	28.451892
298.955033	12803.950548	28.456909
299.231657	12829.905509	28.461927
299.429184	12847.545722	28.466944
299.630714	12863.173813	28.471962
299.987112	12884.322899	28.476980
300.297050	12899.940459	28.481997
300.703486	12920.964957	28.487015
300.942955	12937.338760	28.492032
301.158369	12952.168996	28.497050
301.867526	12975.802144	28.502068
301.851737	12998.019801	28.507085
302.353915	13010.774963	28.512103
302.111052	13032.762756	28.517120
302.669502	13051.973249	28.522138
303.581168	13068.905659	28.527156
303.548720	13093.409132	28.532173
304.050990	13098.282390	28.537191
304.492197	13119.983789	28.542208
305.079014	13127.205954	28.547226
305.584177	13146.206948	28.552244
305.561254	13164.500715	28.557261
305.565718	13176.392438	28.562279
305.676060	13191.412902	28.567296
306.089084	13210.200940	28.572314
306.173880	13227.514852	28.577332
306.438490	13252.051230	28.582349
306.682430	13266.987798	28.587367
307.258081	13285.854802	28.592384
307.421502	13305.802837	28.597402
308.023643	13321.135256	28.602420
308.266702	13338.907786	28.607437
308.861845	13350.906605	28.612455
309.003931	13375.642217	28.617472
309.396123	13394.799997	28.622490
309.911117	13411.500789	28.627508
310.075839	13427.567709	28.632525
310.350126	13441.321797	28.637543
310.810040	13451.750157	28.642560
310.804743	13471.604633	28.647578
311.357628	13485.302749	28.652596
311.435593	13500.445342	28.657613
311.759080	13518.543415	28.662631
312.251249	13530.605748	28.667648
311.971537	13558.419909	28.672666
312.584720	13576.097145	28.677684
312.542761	13595.433245	28.682701
312.805853	13610.610262	28.687719
313.097899	13643.861893	28.692736
313.359935	13664.578119	28.697754
314.187380	13690.382192	28.702772
314.321587	13721.896407	28.707789
314.469955	13741.569346	28.712807
314.964803	13767.125300	28.717824
314.983399	13789.278531	28.722842
315.757082	13813.676382	28.727860
315.815306	13841.548874	28.732877
316.210601	13852.176993	28.737895
317.051590	13881.955090	28.742912
317.207671	13902.688072	28.747930
317.477744	13923.179113	28.752948
317.635633	13945.648744	28.757965
317.952665	13968.115732	28.762983
318.249877	13987.841545	28.768000
318.132689	13997.100017	28.773018
318.948608	14028.663351	28.778036
319.064525	14048.389031	28.783053
319.386487	14073.416507	28.788071
319.738101	14085.801087	28.793088
320.259517	14108.122734	28.798106
320.634674	14125.865963	28.803124
321.044200	14145.081806	28.808141
321.325015	14156.943752	28.813159
321.832547	14170.652585	28.818176
321.930367	14173.280583	28.823194
322.189703	14188.502861	28.828212
322.425192	14218.243118	28.833229
322.845905	14233.073977	28.838247
323.300318	14243.648900	28.843264
323.084713	14265.652825	28.848282
323.686256	14278.646018	28.853300
324.060010	14298.139176	28.858317
324.392547	14319.157787	28.863335
324.720333	14334.480056	28.868352
324.858890	14357.524789	28.873370
325.158480	14374.872629	28.878388
325.382446	14393.419684	28.883405
325.776499	14415.559406	28.888423
325.972365	14428.660072	28.893440
326.347755	14453.667100	28.898458
326.599398	14469.948751	28.903476
326.715048	14504.132557	28.908493
327.184178	14534.099054	28.913511
327.650435	14555.469761	28.918528
327.962761	14588.669361	28.923546
328.366671	14600.954552	28.928564
328.631920	14633.694164	28.933581
328.758381	14659.532897	28.938599
329.255070	14671.421561	28.943616
329.597432	14697.425693	28.948634
330.033652	14721.517229	28.953652
330.534365	14750.838055	28.958669
330.755077	14773.551533	28.963687
331.223793	14793.662038	28.968704
331.417882	14812.255209	28.973722
331.802594	14839.832002	28.978740
332.256855	14864.243038	28.983757
332.757149	14876.860797	28.988775
333.785079	14877.976621	28.993792
333.764373	14893.972590	28.998810
333.996525	14916.074937	29.003828
334.841991	14931.923457	29.008845
334.542614	14949.554559	29.013863
335.101208	14959.466244	29.018880
335.558832	14979.092319	29.023898
335.860526	15002.541943	29.028916
335.790100	15012.017857	29.033933
335.978800	15033.691281	29.038951
336.787901	15055.283934	29.043968
336.495246	15067.813672	29.048986
337.500129	15084.452307	29.054004
337.345679	15105.276000	29.059021
337.445697	15128.782443	29.064039
338.058934	15139.885821	29.069056
338.090564	15172.372177	29.074074
338.644040	15193.824768	29.079092
339.488925	15216.015246	29.084109
339.673951	15235.197663	29.089127
340.100093	15245.670169	29.094144
340.052363	15281.889415	29.099162
340.543571	15294.098301	29.104180
340.962913	15308.112240	29.109197
340.901702	15334.903301	29.114215
341.276405	15350.857043	29.119232
341.186976	15379.923311	29.124250
342.301788	15394.893360	29.129268
342.586225	15413.488842	29.134285
342.744052	15442.977812	29.139303
343.059825	15463.981348	29.144320
342.953263	15487.495127	29.149338
343.649930	15500.035355	29.154356
344.236374	15515.741511	29.159373
344.314378	15543.468136	29.164391
344.491657	15552.678360	29.169408
344.395610	15577.210725	29.174426
345.119690	15605.152680	29.179444
345.467140	15626.391489	29.184461
345.775737	15659.830404	29.189479
346.521131	15680.476734	29.194496
346.610232	15707.633381	29.199514
346.988200	15726.498851	29.204532
347.615593	15740.607050	29.209549
347.774513	15761.496369	29.214567
348.104857	15775.852969	29.219584
348.413816	15811.146001	29.224602
348.705569	15827.975268	29.229620
349.323177	15847.536272	29.234637
349.522503	15874.960243	29.239655
349.714848	15890.658580	29.244672
349.719350	15918.962526	29.249690
350.374104	15942.377290	29.254708
350.852517	15966.956526	29.259725
350.967086	15994.561254	29.264743
351.383007	16026.382835	29.269760
351.733372	16055.943841	29.274778
352.608248	16079.071837	29.279796
353.074552	16091.272478	29.284813
353.403878	16114.535983	29.289831
353.973636	16118.502553	29.294848
354.422079	16147.593632	29.299866
354.453607	16161.239041	29.304884
355.124276	16174.478596	29.309901
354.877288	16202.661038	29.314919
355.684586	16217.963864	29.319936
356.292549	16241.016751	29.324954
356.212829	16252.367629	29.329972
356.169644	16280.777442	29.334989
356.705129	16301.283413	29.340007
357.327355	16319.369226	29.345024
357.719801	16346.789073	29.350042
357.824293	16366.724222	29.355060
358.643251	16379.710273	29.360077
358.483980	16414.426686	29.365095
358.885776	16426.577575	29.370112
359.265687	16449.100866	29.375130
359.442664	16477.141904	29.380148
359.938693	16498.222740	29.385165
360.297671	16523.866715	29.390183
360.369017	16549.293356	29.395200
360.961656	16583.116047	29.400218
360.836205	16613.775314	29.405236
362.250754	16629.609298	29.410253
361.990584	16654.380204	29.415271
362.825631	16680.828314	29.420288
363.136635	16697.952241	29.425306
363.225005	16716.952209	29.430324
363.917371	16736.319296	29.435341
364.218996	16764.710886	29.440359
364.307677	16778.167804	29.445376
364.882988	16798.285936	29.450394
365.106405	16827.018271	29.455412
365.327099	16829.728578	29.460429
365.491074	16864.945050	29.465447
366.228083	16877.255655	29.470464
366.413826	16910.046283	29.475482
366.817721	16941.369060	29.480500
367.669618	16969.915329	29.485517
367.743384	16995.007384	29.490535
367.874737	17007.049137	29.495552
368.573506	17033.983248	29.500570
368.438916	17059.360503	29.505588
368.849760	17073.797140	29.510605
368.917158	17105.415774	29.515623
369.343543	17118.532932	29.520640
370.145402	17137.558054	29.525658
369.838972	17170.469966	29.530676
370.308121	17190.984058	29.535693
370.648962	17217.828858	29.540711
370.912241	17246.072361	29.545728
371.225745	17281.774837	29.550746
371.854514	17319.629795	29.555764
372.614216	17344.198590	29.560781
372.554059	17375.717501	29.565799
372.881070	17395.116864	29.570816
373.622815	17415.999368	29.575834
373.827583	17443.727950	29.580852
374.340914	17472.460334	29.585869
374.426226	17504.869631	29.590887
374.883124	17530.638680	29.595904
375.352025	17560.881590	29.600922
375.579222	17601.351744	29.605940
375.862540	17617.580604	29.610957
376.317421	17659.809508	29.615975
377.144200	17681.083361	29.620992
377.571391	17709.753702	29.626010
377.792240	17740.016558	29.631028
378.489217	17756.478045	29.636045
378.962414	17782.216467	29.641063
379.347749	17805.536470	29.646080
379.987593	17830.718365	29.651098
380.059409	17840.663112	29.656116
380.729629	17870.830946	29.661133
380.806566	17896.871265	29.666151
381.216517	17912.720577	29.671168
381.946083	17937.686492	29.676186
381.930914	17960.374135	29.681204
382.800095	17976.758463	29.686221
382.791866	18002.054110	29.691239
383.140161	18018.961777	29.696256
383.600026	18044.835287	29.701274
383.751144	18076.682533	29.706292
384.150393	18089.324463	29.711309
384.736289	18119.872218	29.716327
384.545131	18146.807449	29.721344
384.952938	18175.525721	29.726362
385.199896	18215.469744	29.731380
386.108831	18233.528519	29.736397
386.318553	18267.009469	29.741415
386.564479	18301.527208	29.746432
386.909765	18318.473510	29.751450
387.232184	18350.319807	29.756468
387.755853	18381.149310	29.761485
388.329499	18408.167996	29.766503
388.265576	18440.144078	29.771520
389.043262	18463.782840	29.776538
389.435282	18497.115775	29.781556
389.953452	18517.971107	29.786573
390.205413	18552.418861	29.791591
390.517077	18574.525673	29.796608
391.021666	18598.137623	29.801626
391.490498	18642.091170	29.806644
392.153227	18655.204168	29.811661
392.358562	18689.337232	29.816679
392.907731	18708.166339	29.821696
393.456596	18733.174049	29.826714
393.723790	18746.373957	29.831732
394.332705	18762.850014	29.836749
394.565537	18785.247310	29.841767
394.922933	18800.701210	29.846784
395.680019	18813.559559	29.851802
395.797424	18839.834912	29.856820
396.033580	18856.659688	29.861837
396.390509	18882.474532	29.866855
396.738498	18897.904703	29.871872
396.881366	18919.722308	29.876890
397.075798	18951.046204	29.881908
397.164259	18971.400338	29.886925
397.740801	18995.254274	29.891943
398.505549	19026.647445	29.896960
398.814509	19054.403177	29.901978
398.963042	19082.025983	29.906996
399.660345	19107.415396	29.912013
400.143573	19138.681999	29.917031
400.319285	19164.411712	29.922048
400.736566	19190.097533	29.927066
401.322428	19230.881676	29.932084
401.473811	19253.879737	29.937101
401.966840	19273.476257	29.942119
402.362700	19303.467916	29.947136
402.953778	19334.686456	29.952154
403.160103	19361.510947	29.957172
403.779004	19389.983350	29.962189
403.738190	19423.915950	29.967207
404.030106	19453.014266	29.972224
404.420057	19484.125366	29.977242
405.073670	19524.343613	29.982260
405.859154	19547.514968	29.987277
406.230782	19566.454680	29.992295
406.551419	19581.592716	29.997312
407.521799	19599.674793	30.002330
408.090881	19633.588622	30.007348
408.368602	19667.535233	30.012365
408.713718	19675.265040	30.017383
409.167000	19702.228452	30.022400
409.740600	19715.337092	30.027418
409.875542	19739.109062	30.032436
410.471038	19764.325648	30.037453
410.701182	19788.714643	30.042471
410.839833	19813.421170	30.047488
411.399133	19841.006375	30.052506
411.636600	19868.098383	30.057524
411.990613	19897.023430	30.062541
412.796747	19923.496281	30.067559
412.686183	19950.876348	30.072576
413.275740	19978.779251	30.077594
413.597871	20016.864117	30.082612
413.873068	20044.740238	30.087629
415.003329	20061.370000	30.092647
414.757614	20101.849487	30.097664
415.272239	20126.295703	30.102682
415.575646	20166.285485	30.107700
415.779792	20191.500368	30.112717
416.302804	20218.024014	30.117735
416.650895	20263.522657	30.122752
417.481781	20281.437546	30.127770
417.609223	20321.290770	30.132788
418.022426	20351.142344	30.137805
418.492176	20385.047670	30.142823
418.552265	20420.191993	30.147840
419.352677	20442.749237	30.152858
419.481568	20481.635897	30.157876
419.922775	20510.099692	30.162893
420.650786	20533.338031	30.167911
420.903535	20577.007358	30.172928
421.271535	20602.835392	30.177946
421.843935	20636.624084	30.182964
421.868797	20661.058762	30.187981
422.528723	20684.061472	30.192999
422.919863	20721.012333	30.198016
423.306704	20737.221365	30.203034
423.681862	20775.514269	30.208052
423.882071	20800.913777	30.213069
424.477231	20829.676297	30.218087
424.719657	20864.230708	30.223104
425.285425	20898.242021	30.228122
425.732124	20934.167400	30.233140
426.199037	20969.931741	30.238157
426.320658	21001.737810	30.243175
426.901626	21035.342626	30.248192
427.313754	21060.747388	30.253210
427.897031	21098.307193	30.258228
428.245168	21131.550369	30.263245
429.475992	21163.752666	30.268263
429.768655	21192.512265	30.273280
430.407031	21208.341339	30.278298
430.527422	21238.972775	30.283316
431.100409	21273.786043	30.288333
431.402731	21295.227648	30.293351
431.730812	21322.762481	30.298368
432.475639	21352.513406	30.303386
432.862436	21382.130562	30.308404
432.994111	21410.757582	30.313421
433.599141	21432.474449	30.318439
433.987122	21476.863976	30.323456
434.549513	21499.693276	30.328474
434.902135	21535.128926	30.333492
434.694648	21573.425633	30.338509
435.918333	21605.642406	30.343527
435.668103	21639.895769	30.348544
436.539314	21661.501947	30.353562
437.206246	21697.154333	30.358580
437.446157	21723.281795	30.363597
438.382119	21748.195195	30.368615
438.416292	21778.215361	30.373632
438.964111	21808.585267	30.378650
439.309749	21837.444975	30.383668
439.656870	21869.337392	30.388685
440.041973	21893.376315	30.393703
440.415529	21930.231089	30.398720
440.984792	21969.557617	30.403738
441.167062	22008.596948	30.408756
441.335982	22039.853931	30.413773
442.092521	22069.389285	30.418791
442.538487	22117.145358	30.423808
442.714824	22139.567924	30.428826
443.718057	22178.208082	30.433844
444.250952	22218.109444	30.438861
444.424878	22248.784663	30.443879
444.877862	22287.656027	30.448896
445.362539	22317.335175	30.453914
445.775519	22339.620029	30.458932
446.049080	22373.009602	30.463949
446.851366	22399.334750	30.468967
447.076046	22431.961150	30.473984
447.782734	22460.790837	30.479002
448.609395	22495.143418	30.484020
449.013367	22519.395003	30.489037
449.381591	22544.246147	30.494055
449.677295	22576.198259	30.499072
450.415090	22601.093040	30.504090
451.058601	22638.279915	30.509108
450.979759	22659.365303	30.514125
451.413905	22675.758133	30.519143
451.621758	22715.489944	30.524160
452.173039	22739.870518	30.529178
452.545518	22754.724905	30.534196
452.946795	22783.526783	30.539213
453.537997	22813.967309	30.544231
453.810825	22841.348573	30.549248
454.035919	22871.877777	30.554266
454.873669	22903.815541	30.559284
455.221337	22924.177649	30.564301
455.622182	22957.282999	30.569319
455.963529	22994.144770	30.574336
456.228286	23025.893902	30.579354
456.658331	23060.580923	30.584372
457.150248	23109.684485	30.589389
457.528696	23140.468261	30.594407
458.112079	23165.368834	30.599424
458.490636	23206.433627	30.604442
459.249136	23243.540548	30.609460
459.549895	23282.766151	30.614477
459.819861	23312.461260	30.619495
460.159390	23353.191205	30.624512
460.840609	23390.430494	30.629530
461.287536	23426.076016	30.634548
461.936387	23471.295113	30.639565
462.536221	23505.735313	30.644583
462.588052	23534.725384	30.649600
463.136423	23573.988841	30.654618
463.568569	23614.572203	30.659636
464.039325	23652.697825	30.664653
465.002509	23688.339277	30.669671
465.541097	23722.334411	30.674688
466.080707	23751.931326	30.679706
466.843249	23782.302430	30.684724
467.136089	23809.757744	30.689741
467.725698	23843.903122	30.694759
468.004615	23881.641983	30.699776
468.472304	23907.073351	30.704794
469.090751	23936.677226	30.709812
469.109399	23970.557832	30.714829
469.501079	24002.560489	30.719847
470.123981	24042.539978	30.724864
470.402641	24071.160597	30.729882
470.980378	24102.508846	30.734900
471.288951	24149.494974	30.739917
472.277240	24169.063509	30.744935
473.099752	24203.362823	30.749952
473.544161	24235.749441	30.754970
473.986102	24267.504567	30.759988
474.086663	24301.012782	30.765005
474.739589	24324.248323	30.770023
474.910519	24354.762957	30.775040
475.175081	24391.885724	30.780058
476.088590	24427.807967	30.785076
476.671101	24454.997896	30.790093
477.174341	24489.063035	30.795111
477.608627	24519.435811	30.800128
478.079074	24552.254927	30.805146
478.598706	24576.036022	30.810164
478.860440	24611.971592	30.815181
479.368633	24638.926885	30.820199
480.107011	24678.959186	30.825216
480.179953	24706.228787	30.830234
481.074498	24736.852533	30.835252
481.136207	24776.307872	30.840269
481.698897	24812.323339	30.845287
481.942362	24834.675299	30.850304
482.217534	24884.019198	30.855322
482.949320	24904.051795	30.860340
483.186806	24929.153774	30.865357
483.880603	24964.972159	30.870375
484.231625	25001.874053	30.875392
484.470783	25028.562098	30.880410
485.204479	25069.644953	30.885428
485.552347	25116.715709	30.890445
485.931757	25142.478373	30.895463
486.618943	25188.327352	30.900480
486.663554	25223.419397	30.905498
487.650323	25255.186067	30.910516
487.986497	25293.519042	30.915533
488.422787	25328.076323	30.920551
488.857865	25358.633519	30.925568
489.184674	25405.202658	30.930586
489.855772	25444.475967	30.935604
490.248000	25491.325826	30.940621
490.662844	25523.794967	30.945639
491.187231	25576.059387	30.950656
491.087907	25613.013554	30.955674
491.667118	25660.182283	30.960692
492.424440	25719.413080	30.965709
492.976799	25762.661662	30.970727
493.481707	25811.049387	30.975744
494.078945	25853.886713	30.980762
494.769074	25891.767578	30.985780
495.358745	25945.463710	30.990797
496.093972	25983.141812	30.995815
496.536911	26015.582094	31.000832
497.042440	26068.103521	31.005850
497.615447	26103.291797	31.010868
497.810613	26138.728551	31.015885
498.210711	26172.231177	31.020903
499.218354	26220.219306	31.025920
499.387554	26254.244646	31.030938
500.279294	26294.091978	31.035956
500.767856	26339.216111	31.040973
501.210089	26368.806775	31.045991
501.903220	26397.524189	31.051008
502.686205	26434.652184	31.056026
503.287042	26471.208205	31.061044
503.658677	26504.026934	31.066061
504.338974	26532.076617	31.071079
504.970769	26570.574562	31.076096
505.186954	26608.340957	31.081114
505.387274	26632.844124	31.086132
506.238995	26666.656465	31.091149
506.336470	26706.805223	31.096167
506.623017	26733.475510	31.101184
507.322581	26781.506617	31.106202
508.256900	26796.693672	31.111220
508.572199	26835.930284	31.116237
509.209187	26871.571307	31.121255
509.853971	26904.480886	31.126272
510.210519	26945.645248	31.131290
510.758500	26973.545500	31.136308
511.391376	27003.284380	31.141325
511.806956	27043.377964	31.146343
512.325870	27082.071421	31.151360
512.741396	27121.634273	31.156378
513.221672	27145.045326	31.161396
513.111103	27182.187398	31.166413
514.141894	27216.396238	31.171431
515.008636	27247.457917	31.176448
515.042001	27287.921179	31.181466
516.247179	27311.921121	31.186484
516.862750	27336.240410	31.191501
517.470904	27352.256054	31.196519
518.177421	27378.962937	31.201536
518.582778	27405.463927	31.206554
519.047065	27423.600357	31.211572
519.069690	27444.188310	31.216589
519.346164	27468.547907	31.221607
520.106089	27492.162319	31.226624
520.218778	27531.039959	31.231642
520.649736	27558.845471	31.236660
521.468857	27596.071101	31.241677
521.442077	27637.903296	31.246695
521.861213	27671.146307	31.251712
521.950021	27720.077407	31.256730
522.467635	27759.284310	31.261748
523.189968	27806.037583	31.266765
523.646781	27852.857581	31.271783
524.172046	27891.557915	31.276800
524.543029	27944.193642	31.281818
525.056971	27988.830825	31.286836
525.313432	28033.520831	31.291853
525.977420	28076.775946	31.296871
526.436403	28127.198916	31.301888
527.039969	28188.881635	31.306906
527.266454	28239.315795	31.311924
528.423019	28288.486550	31.316941
528.746545	28341.769068	31.321959
529.854388	28379.545321	31.326976
529.842765	28430.920866	31.331994
530.236419	28485.381114	31.337012
531.021804	28517.734169	31.342029
531.918408	28577.943985	31.347047
532.471702	28619.991281	31.352064
533.052463	28664.752277	31.357082
533.915372	28706.441838	31.362100
534.654364	28742.683374	31.367117
535.107950	28784.872946	31.372135
535.548152	28825.332811	31.377152
536.392178	28867.524979	31.382170
536.377037	28901.077790	31.387188
537.245851	28936.559933	31.392205
537.574074	28989.053314	31.397223
538.344439	29020.651013	31.402240
538.800012	29063.814252	31.407258
539.358501	29104.085593	31.412276
540.034889	29132.499767	31.417293
540.311619	29184.698267	31.422311
541.302458	29222.822981	31.427328
541.912531	29254.875815	31.432346
542.063624	29294.123764	31.437364
542.685154	29335.839546	31.442381
543.214844	29380.799686	31.447399
543.981698	29406.608593	31.452416
544.502184	29463.984600	31.457434
544.813086	29493.714037	31.462452
545.786559	29530.615769	31.467469
546.000110	29572.465076	31.472487
546.563328	29604.178098	31.477504
546.771360	29642.924816	31.482522
547.443682	29681.239032	31.487540
548.114015	29730.609055	31.492557
548.279232	29773.553508	31.497575
548.505270	29811.223167	31.502592
549.145325	29862.007808	31.507610
549.779227	29913.103264	31.512628
550.293952	29957.175728	31.517645
550.911891	30008.058989	31.522663
551.768018	30042.261844	31.527680
552.194774	30090.191514	31.532698
552.585696	30137.785533	31.537716
552.928578	30171.303647	31.542733
553.598154	30221.370292	31.547751
554.020543	30253.611933	31.552768
554.271459	30305.406422	31.557786
555.216868	30343.028278	31.562804
555.972992	30381.823808	31.567821
556.338610	30432.462944	31.572839
556.743980	30472.609098	31.577856
557.431248	30517.111028	31.582874
557.846722	30570.486161	31.587892
558.760227	30598.441930	31.592909
559.257502	30649.389809	31.597927
559.867239	30694.447822	31.602944
560.131683	30729.274920	31.607962
560.956181	30785.886657	31.612980
561.568243	30809.161291	31.617997
562.428826	30854.484027	31.623015
563.190697	30895.131783	31.628032
563.908421	30932.992447	31.633050
564.251570	30964.090724	31.638068
565.402608	30992.199692	31.643085
565.866712	31032.154471	31.648103
566.476202	31068.319133	31.653120
566.715885	31108.536567	31.658138
567.123393	31144.239735	31.663156
567.917749	31176.753628	31.668173
567.970854	31219.130648	31.673191
568.753352	31257.790970	31.678208
569.455267	31300.522300	31.683226
569.824199	31342.660762	31.688244
570.560291	31398.276501	31.693261
570.880166	31425.364937	31.698279
571.319576	31479.800706	31.703296
571.822783	31520.666963	31.708314
572.224539	31574.539904	31.713332
573.369248	31619.048856	31.718349
573.727540	31669.622625	31.723367
574.087594	31713.672344	31.728384
574.649827	31761.888238	31.733402
575.277812	31811.920962	31.738420
575.651083	31854.407478	31.743437
576.047683	31909.179764	31.748455
576.752987	31964.049535	31.753472
577.260618	32002.956332	31.758490
577.709778	32063.214394	31.763508
578.649143	32125.166403	31.768525
579.221544	32173.223626	31.773543
579.899444	32214.765768	31.778560
580.633900	32263.019232	31.783578
581.166276	32305.614659	31.788596
582.238675	32344.383601	31.793613
582.814301	32393.515537	31.798631
583.181938	32432.938033	31.803648
583.905908	32479.682717	31.808666
584.366361	32530.678883	31.813684
585.220006	32563.508137	31.818701
585.524282	32603.414960	31.823719
586.390471	32649.107418	31.828736
587.324094	32690.907831	31.833754
587.782645	32729.861559	31.838772
588.404248	32765.097973	31.843789
588.801599	32804.491258	31.848807
589.524396	32842.051166	31.853824
590.175510	32869.292220	31.858842
590.628494	32908.032201	31.863860
591.689416	32939.426304	31.868877
592.057514	32977.749735	31.873895
592.472914	33013.214650	31.878912
593.414876	33044.829736	31.883930
593.623135	33078.089016	31.888948
593.978756	33102.790671	31.893965
594.687504	33143.406847	31.898983
595.189150	33171.019277	31.904000
595.845901	33205.245757	31.909018
596.126455	33249.759967	31.914036
596.889911	33271.009701	31.919053
597.020773	33327.881758	31.924071
597.426573	33378.711484	31.929088
598.198522	33405.921785	31.934106
598.736492	33468.300634	31.939124
599.236202	33508.810976	31.944141
599.633147	33557.423440	31.949159
599.880234	33605.218496	31.954176
601.078534	33654.996162	31.959194
601.555284	33710.354983	31.964212
602.077927	33758.177036	31.969229
602.918246	33808.175171	31.974247
603.529118	33866.902248	31.979264
603.977963	33906.485582	31.984282
604.189160	33964.763047	31.989300
604.915327	34024.642239	31.994317
605.435769	34079.672795	31.999335
605.675468	34126.395392	32.004352
607.045918	34194.450709	32.009370
607.590099	34250.034383	32.014388
607.681985	34309.633785	32.019405
608.833598	34366.065241	32.024423
609.420102	34418.690207	32.029440
610.084903	34465.429572	32.034458
610.790546	34527.817077	32.039476
611.498811	34572.318086	32.044493
612.331587	34623.767183	32.049511
613.089191	34672.933041	32.054528
613.856787	34713.694839	32.059546
614.275944	34762.540564	32.064564
614.534338	34812.201747	32.069581
615.301336	34868.966296	32.074599
616.282972	34920.291783	32.079616
617.239952	34950.408959	32.084634
617.782288	34988.519258	32.089652
618.419000	35024.395699	32.094669
619.180937	35074.377435	32.099687
619.999210	35117.597947	32.104704
620.630718	35148.676533	32.109722
620.895840	35203.123828	32.114740
621.672549	35243.733489	32.119757
622.336653	35290.025881	32.124775
622.350492	35329.723867	32.129792
623.305044	35366.474525	32.134810
623.686276	35421.321605	32.139828
624.255377	35474.331278	32.144845
624.873538	35515.623707	32.149863
625.258422	35570.679256	32.154880
626.023647	35618.214855	32.159898
626.436288	35679.291977	32.164916
627.114643	35733.777472	32.169933
627.856046	35784.807349	32.174951
628.225840	35839.398055	32.179968
629.016164	35893.360701	32.184986
629.668729	35952.706733	32.190004
630.072817	35999.818869	32.195021
630.664734	36046.686890	32.200039
631.054816	36104.449220	32.205056
631.679909	36156.579317	32.210074
632.521995	36224.110108	32.215092
633.085376	36275.750591	32.220109
633.998771	36323.315288	32.225127
634.512073	36375.425388	32.230144
635.179903	36417.148128	32.235162
635.414056	36473.544669	32.240180
635.956629	36512.789497	32.245197
636.950592	36576.130874	32.250215
637.397953	36620.348007	32.255232
638.408689	36667.310275	32.260250
638.783724	36724.969139	32.265268
639.616806	36779.913786	32.270285
640.150059	36827.317479	32.275303
640.518773	36879.615722	32.280320
641.375171	36940.045652	32.285338
642.137397	36984.922721	32.290356
643.004975	37037.801304	32.295373
643.589191	37086.645654	32.300391
644.357222	37136.011622	32.305408
644.774552	37185.223631	32.310426
645.656487	37242.861893	32.315444
646.426358	37297.786098	32.320461
647.497499	37339.390951	32.325479
647.758509	37389.924041	32.330496
648.642137	37437.129109	32.335514
649.334870	37489.612367	32.340532
649.609389	37530.070612	32.345549
650.476891	37579.099629	32.350567
651.000207	37637.863431	32.355584
651.630583	37673.131966	32.360602
652.102270	37722.159693	32.365620
652.579033	37780.981722	32.370637
653.367499	37834.152822	32.375655
653.918404	37893.077438	32.380672
654.545587	37948.259493	32.385690
655.167073	38016.127497	32.390708
655.662864	38064.785493	32.395725
656.588602	38125.410331	32.400743
657.051253	38186.961108	32.405760
658.310930	38241.451043	32.410778
658.760201	38301.037603	32.415796
659.307046	38352.034349	32.420813
660.196656	38399.822378	32.425831
660.897081	38456.094643	32.430848
661.199065	38523.786338	32.435866
662.311547	38572.943905	32.440884
662.474136	38631.874084	32.445901
664.188745	38670.554673	32.450919
664.721570	38720.030466	32.455936
665.968757	38759.074870	32.460954
666.583822	38810.270765	32.465972
666.729754	38849.986342	32.470989
667.720836	38886.395905	32.476007
667.922756	38937.871424	32.481024
668.596335	38980.129463	32.486042
669.374148	39035.872647	32.491060
669.699546	39079.070412	32.496077
670.771358	39135.255020	32.501095
671.072901	39186.924310	32.506112
671.524988	39243.515540	32.511130
671.834606	39299.838199	32.516148
672.641775	39349.222136	32.521165
673.731132	39410.881212	32.526183
674.090455	39460.012601	32.531200
674.637190	39518.183442	32.536218
675.495161	39582.218882	32.541236
676.031209	39632.176883	32.546253
676.677028	39689.700365	32.551271
676.982173	39752.627135	32.556288
677.929771	39806.632073	32.561306
678.524970	39863.114108	32.566324
679.139650	39919.239111	32.571341
680.123209	39963.107717	32.576359
680.675602	40020.077454	32.581376
681.578381	40064.679786	32.586394
682.398487	40110.363854	32.591412
683.513163	40146.806897	32.596429
685.178447	40179.433055	32.601447
685.756853	40218.293303	32.606464
685.953696	40247.366323	32.611482
686.443488	40285.456292	32.616500
687.140371	40331.640644	32.621517
687.570377	40371.352733	32.626535
688.300510	40414.098055	32.631552
688.862756	40461.492591	32.636570
689.361637	40510.370638	32.641588
689.557623	40566.258929	32.646605
690.452763	40618.933319	32.651623
691.002101	40681.217637	32.656640
691.458255	40740.930005	32.661658
692.172849	40786.043761	32.666676
692.984877	40855.269712	32.671693
693.569408	40914.956248	32.676711
694.167294	40985.683196	32.681728
694.647638	41047.644109	32.686746
695.549944	41104.910056	32.691764
695.882017	41174.958015	32.696781
696.760588	41240.886136	32.701799
697.320583	41318.785643	32.706816
698.121827	41377.238060	32.711834
698.818061	41442.183258	32.716852
699.545045	41504.397999	32.721869
700.369071	41576.286986	32.726887
701.153432	41641.725020	32.731904
701.759190	41709.626011	32.736922
702.701242	41765.110297	32.741940
703.188462	41835.458771	32.746957
704.274154	41900.091716	32.751975
704.782897	41967.724001	32.756992
705.317961	42031.620847	32.762010
706.514299	42100.835188	32.767028
706.826210	42163.419999	32.772045
707.749412	42225.770684	32.777063
708.320977	42292.609925	32.782080
709.512114	42354.463886	32.787098
710.808824	42418.818846	32.792116
711.512979	42472.950508	32.797133
712.338577	42513.920462	32.802151
712.716599	42580.506092	32.807168
713.258119	42632.822942	32.812186
714.138263	42682.044952	32.817204
714.906071	42745.313106	32.822221
715.777131	42792.557094	32.827239
716.336442	42854.782790	32.832256
716.706596	42918.031118	32.837274
717.633906	42963.040346	32.842292
717.978931	43033.009990	32.847309
718.909194	43090.574044	32.852327
719.571252	43152.171062	32.857344
720.380619	43208.944646	32.862362
721.450655	43263.476694	32.867380
722.166806	43322.870988	32.872397
722.993722	43383.608085	32.877415
723.797319	43432.002455	32.882432
724.154306	43493.515089	32.887450
725.055110	43538.415767	32.892468
725.438745	43598.975781	32.897485
726.083132	43650.918501	32.902503
726.680021	43711.198945	32.907520
727.073125	43769.133017	32.912538
728.417849	43822.004444	32.917556
728.843420	43879.579541	32.922573
729.615482	43922.236622	32.927591
730.311614	43985.051418	32.932608
730.578828	44041.013354	32.937626
731.134339	44097.847713	32.942644
731.528749	44160.697325	32.947661
732.530872	44236.419355	32.952679
733.281992	44298.682504	32.957696
734.249346	44366.737793	32.962714
734.964190	44427.343389	32.967732
735.390869	44493.028997	32.972749
736.478858	44558.807941	32.977767
737.342452	44625.906067	32.982784
737.865114	44692.918308	32.987802
738.607879	44754.987947	32.992820
739.173740	44833.645347	32.997837
739.855292	44895.446586	33.002855
740.814955	44962.220822	33.007872
741.020628	45032.534734	33.012890
742.426699	45106.001887	33.017908
742.622384	45187.716463	33.022925
743.732309	45249.825208	33.027943
744.519406	45327.323954	33.032960
745.187522	45405.739729	33.037978
746.196795	45466.023987	33.042996
746.882513	45539.927312	33.048013
747.688658	45610.035703	33.053031
748.454439	45675.709957	33.058048
748.990192	45744.709584	33.063066
750.022002	45818.958474	33.068084
750.817316	45896.382002	33.073101
751.765804	45969.531028	33.078119
752.867439	46025.374370	33.083136
753.358922	46111.069473	33.088154
754.273863	46167.239544	33.093172
754.700576	46233.594472	33.098189
754.945977	46300.863441	33.103207
756.158700	46375.712274	33.108224
756.926604	46446.436518	33.113242
758.091507	46509.678864	33.118260
758.699068	46577.575485	33.123277
759.416868	46655.848722	33.128295
760.268023	46713.282631	33.133312
760.552461	46782.090502	33.138330
761.748620	46846.802891	33.143348
762.483719	46922.252953	33.148365
763.476969	46991.602708	33.153383
764.086630	47062.201693	33.158400
764.629924	47134.664779	33.163418
765.842481	47181.649830	33.168436
766.590054	47259.218327	33.173453
767.210271	47322.029000	33.178471
768.298263	47383.457512	33.183488
768.943760	47454.937811	33.188506
769.495391	47510.326403	33.193524
770.234579	47582.811041	33.198541
771.042243	47648.800843	33.203559
771.741683	47709.392397	33.208576
772.460436	47789.295265	33.213594
773.492391	47848.285488	33.218612
774.327506	47911.753913	33.223629
775.395159	47978.754374	33.228647
776.198356	48033.554693	33.233664
776.320008	48101.854176	33.238682
777.692722	48156.958374	33.243700
778.636749	48202.614522	33.248717
779.211997	48258.032897	33.253735
780.183302	48299.787920	33.258752
780.756547	48355.788877	33.263770
781.917690	48407.965842	33.268788
782.872180	48464.496081	33.273805
783.152322	48511.502512	33.278823
783.631068	48558.686899	33.283840
784.328782	48618.964825	33.288858
785.177434	48673.481246	33.293876
785.665164	48734.892984	33.298893
786.385212	48810.598410	33.303911
786.999425	48871.389801	33.308928
787.965903	48939.187015	33.313946
788.930716	49009.034517	33.318964
789.174346	49076.729558	33.323981
790.073888	49141.519981	33.328999
791.014020	49199.382879	33.334016
791.405884	49277.032617	33.339034
792.377491	49356.933260	33.344052
792.888263	49428.092760	33.349069
793.847577	49509.419367	33.354087
794.697556	49580.254487	33.359104
795.555990	49660.793833	33.364122
796.150453	49738.400943	33.369140
797.342341	49809.537850	33.374157
797.605913	49895.738250	33.379175
798.635376	49964.711825	33.384192
799.360670	50051.916509	33.389210
800.358778	50119.244104	33.394228
800.914772	50204.723160	33.399245
801.440141	50281.071141	33.404263
802.836606	50367.584134	33.409280
803.240967	50448.190598	33.414298
804.041233	50524.116971	33.419316
805.260466	50603.755635	33.424333
805.773962	50680.271291	33.429351
807.345857	50754.623077	33.434368
808.415017	50838.733873	33.439386
808.852017	50902.588931	33.444404
809.758624	50973.185424	33.449421
810.812846	51047.713648	33.454439
811.579222	51105.646362	33.459456
812.266108	51185.648302	33.464474
812.953566	51264.511524	33.469492
814.066522	51335.349074	33.474509
814.892758	51399.347386	33.479527
816.162503	51460.942060	33.484544
817.124094	51538.390519	33.489562
817.964296	51589.935013	33.494580
818.515816	51644.555362	33.499597
819.728098	51715.536799	33.504615
820.760863	51771.714997	33.509632
821.433990	51843.248980	33.514650
822.329792	51896.519212	33.519668
823.374552	51957.922445	33.524685
823.934683	52012.523338	33.529703
824.660316	52059.765062	33.534720
825.409792	52122.853511	33.539738
826.368301	52179.088548	33.544756
827.132588	52236.176531	33.549773
827.496321	52310.158242	33.554791
828.505252	52358.716895	33.559808
829.281467	52433.602904	33.564826
829.771347	52498.681673	33.569844
830.913162	52568.233998	33.574861
831.361646	52632.408410	33.579879
832.217449	52698.810199	33.584896
832.833658	52762.788014	33.589914
833.282602	52831.632713	33.594932
834.503710	52889.018191	33.599949
835.341697	52967.471445	33.604967
836.018416	53016.905787	33.609984
837.438926	53077.740939	33.615002
838.008236	53141.113301	33.620020
838.755505	53200.566550	33.625037
839.433953	53274.470688	33.630055
840.328726	53324.820907	33.635072
841.279990	53397.417404	33.640090
841.929577	53462.524620	33.645108
842.717726	53532.115888	33.650125
843.148022	53614.697265	33.655143
844.240008	53678.470638	33.660160
844.992106	53756.648823	33.665178
845.699526	53841.769654	33.670196
846.608524	53910.950901	33.675213
847.046067	54001.809493	33.680231
848.069454	54065.885685	33.685248
848.982688	54155.810214	33.690266
849.675091	54237.081042	33.695284
850.866338	54325.640380	33.700301
851.362364	54412.030156	33.705319
852.596941	54494.229970	33.710336
853.235242	54576.408984	33.715354
853.978321	54658.964320	33.720372
855.007570	54748.740161	33.725389
855.718956	54835.452342	33.730407
856.647280	54916.739413	33.735424
857.585323	55000.062950	33.740442
858.313533	55088.779499	33.745460
859.502286	55164.837692	33.750477
860.381678	55256.448684	33.755495
860.980291	55343.787802	33.760512
862.024434	55432.190667	33.765530
862.991728	55509.872865	33.770548
864.419489	55595.685267	33.775565
865.398454	55671.087947	33.780583
866.446365	55741.702148	33.785600
867.098299	55811.739023	33.790618
868.104427	55889.517675	33.795636
869.050803	55961.015338	33.800653
870.061003	56039.686169	33.805671
871.039185	56118.862199	33.810688
871.811791	56187.160029	33.815706
872.538127	56262.565939	33.820724
873.675439	56337.357524	33.825741
874.731703	56411.965773	33.830759
875.088252	56477.329427	33.835776
876.097762	56558.305708	33.840794
876.692674	56638.125363	33.845812
877.620909	56699.622404	33.850829
878.595121	56781.237807	33.855847
879.357384	56851.393467	33.860864
880.443288	56927.327752	33.865882
881.492890	57004.603303	33.870900
882.561834	57075.838408	33.875917
883.056395	57155.890593	33.880935
883.854689	57229.161866	33.885952
884.640355	57303.220109	33.890970
885.611950	57377.262297	33.895988
887.011794	57442.826932	33.901005
887.604596	57525.649777	33.906023
888.602391	57598.846823	33.911040
889.917156	57660.716535	33.916058
890.107063	57738.678897	33.921076
891.311260	57808.300221	33.926093
892.097542	57871.316014	33.931111
892.853861	57930.286053	33.936128
893.916848	58004.119748	33.941146
894.022148	58070.533175	33.946164
894.980935	58132.503818	33.951181
895.712323	58211.731518	33.956199
896.543578	58290.469249	33.961216
897.168475	58368.422898	33.966234
897.957031	58449.269071	33.971252
898.915264	58532.139760	33.976269
899.570549	58617.178179	33.981287
900.556298	58690.981696	33.986304
901.657223	58784.356558	33.991322
902.244814	58869.969707	33.996340
903.488964	58955.170821	34.001357
904.411989	59054.840430	34.006375
905.158212	59143.980608	34.011392
906.019731	59219.387413	34.016410
907.174471	59314.699060	34.021428
907.862099	59399.956721	34.026445
909.057235	59489.648573	34.031463
909.925478	59576.980115	34.036480
911.233430	59653.204901	34.041498
911.706271	59741.642949	34.046516
913.166244	59828.193367	34.051533
914.077981	59912.316601	34.056551
915.150092	59995.630294	34.061568
916.160322	60078.612106	34.066586
916.623496	60170.091420	34.071604
917.479454	60258.446387	34.076621
918.355903	60345.766749	34.081639
919.350944	60432.106851	34.086656
920.220790	60518.048985	34.091674
921.008808	60613.055676	34.096692
922.277717	60692.796465	34.101709
923.032055	60786.036739	34.106727
923.968304	60877.065270	34.111744
925.277410	60961.054303	34.116762
926.187085	61052.859862	34.121780
927.470669	61129.517154	34.126797
928.198531	61223.788653	34.131815
929.347438	61299.695194	34.136832
930.016594	61377.398390	34.141850
931.070352	61466.682746	34.146868
931.771752	61550.344286	34.151885
932.938754	61640.352252	34.156903
934.084425	61709.905247	34.161920
935.242254	61805.833813	34.166938
935.862243	61880.128027	34.171956
937.075955	61961.375425	34.176973
938.062050	62034.885158	34.181991
938.571724	62127.111477	34.187008
940.237790	62203.041586	34.192026
940.936354	62289.440698	34.197044
941.582692	62366.910019	34.202061
942.736795	62449.339386	34.207079
943.573540	62540.718730	34.212096
944.496995	62619.316797	34.217114
945.070190	62701.362660	34.222132
946.154880	62786.937441	34.227149
947.198226	62873.177306	34.232167
948.029077	62956.196755	34.237184
949.494631	63033.015221	34.242202
950.012837	63108.671004	34.247220
950.888584	63193.412450	34.252237
951.541318	63275.770680	34.257255
952.471893	63375.431338	34.262272
953.495398	63446.875716	34.267290
954.497870	63532.478525	34.272308
955.533111	63608.821334	34.277325
956.118653	63686.430846	34.282343
956.713999	63771.496450	34.287360
957.855042	63842.436215	34.292378
958.692752	63935.029670	34.297396
959.693642	64022.134755	34.302413
960.747661	64104.363622	34.307431
961.461744	64192.526846	34.312448
962.455235	64274.271902	34.317466
963.210315	64365.506059	34.322484
963.994969	64456.875220	34.327501
965.152584	64548.883041	34.332519
966.243360	64644.858329	34.337536
967.655849	64726.286410	34.342554
968.823724	64827.030136	34.347572
969.935581	64908.378988	34.352589
971.024431	64988.073003	34.357607
971.763652	65092.195552	34.362624
972.974698	65161.203572	34.367642
973.758712	65247.922506	34.372660
974.762346	65333.999783	34.377677
975.760624	65420.059195	34.382695
976.120236	65510.637339	34.387712
977.760399	65601.238062	34.392730
978.666206	65685.407142	34.397748
979.916734	65767.041073	34.402765
980.919300	65865.199965	34.407783
981.636002	65957.306893	34.412800
982.953925	66037.791613	34.417818
983.735781	66131.921322	34.422836
984.443186	66216.439610	34.427853
985.787118	66308.956675	34.432871
986.831068	66400.450801	34.437888
988.127008	66481.586136	34.442906
988.945089	66571.615538	34.447924
990.046628	66653.649066	34.452941
990.689766	66749.898310	34.457959
991.324746	66837.551265	34.462976
992.717086	66927.435557	34.467994
993.589635	67020.699714	34.473012
994.428922	67107.891266	34.478029
995.522275	67211.517877	34.483047
996.530955	67309.649746	34.488064
997.859257	67400.090177	34.493082
999.176716	67488.177309	34.498100
1000.068743	67581.643093	34.503117
1000.936197	67679.152553	34.508135
1001.610311	67765.941520	34.513152
1002.999488	67855.861235	34.518170
1003.776520	67938.759852	34.523188
1004.691840	68043.683867	34.528205
1005.885584	68120.655137	34.533223
1007.004520	68214.068914	34.538240
1007.687646	68305.220813	34.543258
1008.659369	68397.917369	34.548276
1010.111431	68485.911002	34.553293
1011.829334	68561.263397	34.558311
1012.571291	68646.499839	34.563328
1013.534394	68730.277489	34.568346
1014.243789	68823.079730	34.573364
1015.468396	68910.198442	34.578381
1015.929434	68984.994235	34.583399
1016.930210	69080.253122	34.588416
1018.323023	69175.160070	34.593434
1019.578067	69263.332664	34.598452
1020.637620	69339.043092	34.603469
1021.382020	69414.739479	34.608487
1022.421084	69495.354481	34.613504
1023.270847	69575.606618	34.618522
1024.249310	69655.845302	34.623540
1024.935015	69737.674820	34.628557
1025.752616	69813.525611	34.633575
1026.795890	69906.393746	34.638592
1027.507663	69989.815683	34.643610
1028.630084	70081.677988	34.648628
1029.571693	70175.525392	34.653645
1030.877517	70268.423608	34.658663
1031.670002	70355.886736	34.663680
1032.707400	70455.419199	34.668698
1033.895649	70549.324543	34.673716
1034.526603	70649.199631	34.678733
1035.627722	70751.522160	34.683751
1036.428758	70840.404012	34.688768
1037.554036	70942.558890	34.693786
1039.199732	71042.936092	34.698804
1040.129623	71133.255322	34.703821
1041.303928	71234.086577	34.708839
1041.703518	71327.490576	34.713856
1042.740167	71440.666929	34.718874
1044.289738	71527.978141	34.723892
1045.796062	71614.143865	34.728909
1046.919471	71700.812752	34.733927
1048.283224	71802.287950	34.738944
1049.231777	71888.465407	34.743962
1050.415416	71983.636797	34.748980
1051.131399	72086.328455	34.753997
1052.251662	72177.634864	34.759015
1053.722473	72268.773037	34.764032
1054.731743	72352.612153	34.769050
1055.164083	72445.039795	34.774068
1056.582202	72544.482936	34.779085
1057.826748	72637.836056	34.784103
1059.006892	72729.793660	34.789120
1060.761206	72813.150969	34.794138
1062.390742	72889.954530	34.799156
1063.299260	72964.375422	34.804173
1064.577913	73038.168955	34.809191
1065.688379	73113.559418	34.814208
1066.225485	73186.468203	34.819226
1067.227236	73276.884930	34.824244
1068.012713	73363.206579	34.829261
1069.554542	73444.496432	34.834279
1069.963687	73538.261414	34.839296
1070.542413	73626.376658	34.844314
1071.449355	73710.046015	34.849332
1072.458524	73811.900778	34.854349
1073.400559	73918.668146	34.859367
1074.265308	74023.142739	34.864384
1075.282521	74110.228706	34.869402
1076.346657	74207.491277	34.874420
1077.704238	74320.883328	34.879437
1078.738956	74418.556567	34.884455
1079.536173	74519.750378	34.889472
1080.601803	74632.986536	34.894490
1082.031122	74739.643338	34.899508
1082.982422	74851.188244	34.904525
1084.089816	74946.268130	34.909543
1084.890840	75048.919999	34.914560
1085.807763	75158.330878	34.919578
1086.778154	75269.557884	34.924596
1087.928356	75387.382076	34.929613
1088.867181	75486.974147	34.934631
1090.228689	75600.003659	34.939648
1091.549077	75714.914750	34.944666
1092.285889	75803.354555	34.949684
1093.352927	75913.923164	34.954701
1094.663700	75999.107519	34.959719
1095.746284	76101.820911	34.964736
1096.699880	76199.031898	34.969754
1098.063802	76286.716981	34.974772
1099.016187	76386.373596	34.979789
1100.126240	76481.914507	34.984807
1101.123459	76586.923137	34.989824
1102.219845	76693.918181	34.994842
1103.603651	76793.496472	34.999860
1104.089370	76903.209550	35.004877
1105.391121	76986.814984	35.009895
1106.846888	77092.970276	35.014912
1108.008681	77215.804310	35.019930
1109.057103	77304.466528	35.024948
1110.295886	77408.756678	35.029965
1111.564023	77516.260267	35.034983
1112.698198	77618.730679	35.040000
1113.881441	77721.953909	35.045018
1115.159840	77825.745440	35.050036
1115.828464	77938.981224	35.055053
1116.675776	78041.763900	35.060071
1118.071312	78143.460853	35.065088
1119.054884	78257.903067	35.070106
1120.398526	78356.809240	35.075124
1121.397341	78477.761423	35.080141
1122.866551	78578.346387	35.085159
1123.823379	78691.299717	35.090176
1125.119347	78794.053379	35.095194
1126.793661	78895.912420	35.100212
1127.382518	78998.954269	35.105229
1128.581659	79102.382912	35.110247
1130.260841	79209.183062	35.115264
1131.007690	79306.234588	35.120282
1132.421471	79407.768685	35.125300
1133.961698	79513.958213	35.130317
1134.787979	79609.959610	35.135335
1135.980117	79718.028398	35.140352
1136.778528	79814.756963	35.145370
1138.392300	79922.684906	35.150388
1139.505056	80017.160867	35.155405
1140.581399	80110.097206	35.160423
1141.800514	80213.729596	35.165440
1142.751318	80332.911043	35.170458
1143.810327	80426.585942	35.175476
1145.284725	80526.607080	35.180493
1146.388283	80620.643103	35.185511
1147.778864	80715.065521	35.190528
1148.963534	80822.759689	35.195546
1150.186874	80916.334641	35.200564
1150.939858	81021.486893	35.205581
1151.755934	81128.593477	35.210599
1153.018128	81224.469243	35.215616
1153.813726	81343.311747	35.220634
1154.934959	81449.396507	35.225652
1155.850849	81572.756958	35.230669
1156.928544	81677.797781	35.235687
1158.433554	81784.736286	35.240704
1159.428216	81908.820794	35.245722
1160.474364	82013.360991	35.250740
1161.674601	82133.942966	35.255757
1163.035010	82239.917461	35.260775
1164.191907	82360.355112	35.265792
1165.261621	82469.416507	35.270810
1166.609918	82578.168890	35.275828
1167.876510	82703.291520	35.280845
1169.159348	82810.129127	35.285863
1170.677106	82912.838094	35.290880
1171.160641	83015.683075	35.295898
1172.790143	83106.503327	35.300916
1173.578021	83210.860089	35.305933
1174.877816	83301.922342	35.310951
1175.737232	83403.405170	35.315968
1177.261358	83503.378473	35.320986
1178.529981	83593.192136	35.326004
1179.449509	83700.482431	35.331021
1180.163563	83799.455186	35.336039
1181.584919	83906.794852	35.341056
1182.605641	84022.015103	35.346074
1183.912143	84122.151159	35.351092
1185.274663	84222.937728	35.356109
1186.437055	84332.663400	35.361127
1188.039781	84438.595713	35.366144
1188.596442	84556.551236	35.371162
1189.961785	84664.662723	35.376180
1191.245880	84775.739615	35.381197
1192.112342	84883.498764	35.386215
1193.584366	84983.865490	35.391232
1194.933245	85104.766365	35.396250
1196.250753	85205.424010	35.401268
1197.512662	85319.674263	35.406285
1198.495643	85431.852273	35.411303
1199.572365	85544.066814	35.416320
1200.742710	85663.870071	35.421338
1202.076932	85772.472078	35.426356
1203.592133	85894.161347	35.431373
1204.789513	85997.792920	35.436391
1206.254238	86101.345236	35.441408
1207.388463	86220.788944	35.446426
1208.518242	86332.795537	35.451444
1209.919969	86451.869094	35.456461
1211.030317	86558.037897	35.461479
1212.296206	86652.486754	35.466496
1213.401195	86769.402897	35.471514
1214.663842	86885.420604	35.476532
1216.082378	87002.795757	35.481549
1217.290638	87110.205861	35.486567
1218.739579	87215.411969	35.491584
1219.333441	87330.559792	35.496602
1220.848681	87440.837924	35.501620
1222.091219	87562.335839	35.506637
1223.241575	87673.799473	35.511655
1224.553931	87791.612506	35.516672
1225.499136	87908.659453	35.521690
1226.920489	88014.544364	35.526708
1227.971043	88134.693235	35.531725
1229.425506	88262.142477	35.536743
1230.436052	88370.715830	35.541760
1231.639364	88496.811195	35.546778
1233.057709	88607.945186	35.551796
1234.263728	88723.066541	35.556813
1235.325486	88846.701574	35.561831
1237.273168	88952.229128	35.566848
1238.061571	89067.277425	35.571866
1239.302850	89180.342063	35.576884
1240.703002	89288.832800	35.581901
1241.765363	89413.914827	35.586919
1243.438251	89518.549366	35.591936
1244.563719	89639.617825	35.596954
1245.837411	89755.049483	35.601972
1247.594888	89861.357598	35.606989
1248.612714	89967.616467	35.612007
1250.069070	90068.370602	35.617024
1251.224925	90176.927950	35.622042
1252.494499	90282.616475	35.627060
1253.580289	90380.767928	35.632077
1255.184241	90477.216842	35.637095
1256.232205	90567.162372	35.642112
1257.138166	90666.229899	35.647130
1258.406888	90770.690943	35.652148
1259.334910	90860.073034	35.657165
1260.455114	90965.622462	35.662183
1261.620907	91074.650445	35.667200
1262.490485	91184.586746	35.672218
1263.565884	91299.763730	35.677236
1264.701203	91411.699986	35.682253
1265.643116	91536.175937	35.687271
1267.199340	91650.417592	35.692288
1268.393057	91784.563649	35.697306
1269.597625	91906.059863	35.702324
1271.007308	92026.916280	35.707341
1271.988657	92154.759962	35.712359
1273.233950	92278.748149	35.717376
1274.767615	92408.547486	35.722394
1275.881547	92532.848666	35.727412
1276.949607	92661.999119	35.732429
1278.331531	92795.892214	35.737447
1280.033789	92930.635927	35.742464
1280.971108	93064.029050	35.747482
1282.556478	93190.363512	35.752500
1284.175923	93319.139408	35.757517
1285.895933	93428.381106	35.762535
1287.524294	93543.252385	35.767552
1289.137012	93676.530378	35.772570
1290.469824	93786.632137	35.777588
1291.924842	93901.899313	35.782605
1292.698357	94030.416945	35.787623
1294.326253	94134.288634	35.792640
1295.144486	94247.400068	35.797658
1296.343478	94384.269195	35.802676
1298.167544	94502.485183	35.807693
1299.183300	94631.081691	35.812711
1300.350321	94742.873130	35.817728
1301.794921	94866.219682	35.822746
1302.797099	95000.498382	35.827764
1304.341498	95115.768858	35.832781
1305.652339	95246.362734	35.837799
1307.324533	95355.238447	35.842816
1308.949672	95477.786125	35.847834
1310.062449	95603.519562	35.852852
1311.557571	95715.047951	35.857869
1311.963183	95844.986672	35.862887
1313.856830	95956.022919	35.867904
1314.872671	96082.901520	35.872922
1316.198859	96209.199945	35.877940
1317.794957	96335.330109	35.882957
1319.251577	96455.993798	35.887975
1320.339084	96591.939300	35.892992
1321.540095	96703.149389	35.898010
1322.700944	96829.285907	35.903028
1324.374996	96946.368328	35.908045
1325.435062	97085.185047	35.913063
1326.926273	97212.526627	35.918080
1328.287332	97344.135547	35.923098
1329.509084	97463.457941	35.928116
1331.161381	97583.715209	35.933133
1332.138658	97714.751588	35.938151
1334.224783	97836.311352	35.943168
1335.172632	97957.376896	35.948186
1336.442741	98085.085997	35.953204
1337.943349	98194.239126	35.958221
1338.930097	98319.318498	35.963239
1339.949053	98447.131529	35.968256
1341.692857	98570.484104	35.973274
1342.554512	98694.874521	35.978292
1344.129757	98796.450014	35.983309
1345.091895	98912.712424	35.988327
1346.623810	99029.114757	35.993344
1347.632932	99157.743492	35.998362
1348.699943	99281.647855	36.003380
1350.534453	99395.912704	36.008397
1351.556584	99517.505047	36.013415
1352.999557	99641.022673	36.018432
1354.415457	99761.033381	36.023450
1355.276609	99900.324365	36.028468
1356.733300	100027.885412	36.033485
1357.782614	100167.490552	36.038503
1359.390664	100289.362259	36.043520
1361.013097	100430.704890	36.048538
1362.102003	100564.778175	36.053556
1363.991421	100700.768518	36.058573
1365.287817	100836.129107	36.063591
1366.491405	100960.411670	36.068608
1367.883474	101100.740827	36.073626
1369.203993	101232.676306	36.078644
1370.898662	101368.319422	36.083661
1372.229033	101500.824959	36.088679
1373.456603	101640.941167	36.093696
1374.811851	101783.129984	36.098714
1375.844269	101919.284167	36.103732
1377.576759	102058.613599	36.108749
1378.912478	102204.192358	36.113767
1380.595913	102341.819068	36.118784
1381.983165	102473.051858	36.123802
1383.361070	102624.293131	36.128820
1384.982432	102758.723614	36.133837
1386.119693	102901.838697	36.138855
1387.536077	103042.045601	36.143872
1389.216424	103186.002920	36.148890
1390.353479	103333.887064	36.153908
1391.402040	103476.245040	36.158925
1393.110275	103616.155376	36.163943
1394.574410	103759.984019	36.168960
1396.128197	103893.719617	36.173978
1397.087675	104033.925759	36.178996
1399.070621	104175.139658	36.184013
1400.528464	104318.299706	36.189031
1401.977807	104472.885559	36.194048
1403.297801	104605.925015	36.199066
1404.547100	104762.838271	36.204084
1406.165181	104901.614226	36.209101
1407.619538	105045.399211	36.214119
1408.982936	105180.399486	36.219136
1410.450298	105329.217370	36.224154
1411.270823	105473.660734	36.229172
1413.012894	105625.911348	36.234189
1414.600339	105760.232418	36.239207
1416.138715	105897.997841	36.244224
1417.915426	106034.446081	36.249242
1419.220476	106170.042663	36.254260
1420.781199	106315.718466	36.259277
1422.015230	106456.475242	36.264295
1423.239440	106589.765671	36.269312
1424.724809	106724.753126	36.274330
1426.366449	106867.565711	36.279348
1427.867989	107014.179356	36.284365
1429.285625	107146.490852	36.289383
1430.490399	107276.122438	36.294400
1432.138242	107431.603889	36.299418
1433.121977	107567.167278	36.304436
1435.068067	107703.621200	36.309453
1436.440364	107835.004069	36.314471
1437.686751	107953.840758	36.319488
1439.242547	108076.091460	36.324506
1440.194776	108209.722177	36.329524
1441.697707	108330.523754	36.334541
1443.344505	108467.192134	36.339559
1444.206965	108591.797043	36.344576
1445.955682	108720.601250	36.349594
1447.046468	108864.408201	36.354612
1448.293084	108991.110477	36.359629
1449.544048	109136.263146	36.364647
1450.804594	109283.798936	36.369664
1452.762822	109426.915240	36.374682
1454.007647	109572.349663	36.379700
1455.384883	109710.066689	36.384717
1456.769117	109863.951564	36.389735
1458.385623	110014.529226	36.394752
1460.017441	110160.349700	36.399770
1461.324952	110315.301039	36.404788
1462.824228	110460.547370	36.409805
1464.374740	110617.465866	36.414823
1465.775308	110775.854080	36.419840
1467.375153	110922.443576	36.424858
1468.972727	111074.892901	36.429876
1470.112564	111224.231050	36.434893
1471.571401	111372.543691	36.439911
1473.228075	111533.913669	36.444928
1474.898721	111678.567657	36.449946
1476.494379	111836.701979	36.454964
1477.992280	111988.815654	36.459981
1479.792496	112140.147373	36.464999
1481.305149	112283.915313	36.470016
1483.085787	112443.456596	36.475034
1484.563183	112587.155150	36.480052
1486.275334	112733.417577	36.485069
1488.358722	112868.145454	36.490087
1489.617838	113008.303298	36.495104
1491.925823	113137.543874	36.500122
1493.240268	113279.507726	36.505140
1494.941760	113412.356689	36.510157
1496.340320	113539.038910	36.515175
1497.417729	113675.739969	36.520192
1499.086634	113807.073560	36.525210
1500.335652	113961.111331	36.530228
1501.581277	114101.706723	36.535245
1503.012910	114249.781837	36.540263
1504.102781	114395.665909	36.545280
1505.779114	114534.661329	36.550298
1506.894243	114695.964902	36.555316
1508.314204	114842.484255	36.560333
1510.408334	114997.992912	36.565351
1511.526288	115151.117573	36.570368
1513.070658	115293.992040	36.575386
1514.560176	115450.535265	36.580404
1515.737847	115615.232209	36.585421
1517.666787	115758.822297	36.590439
1519.013730	115917.571203	36.595456
1520.512763	116079.734289	36.600474
1522.079219	116226.401236	36.605492
1523.208748	116390.119827	36.610509
1524.813896	116553.790478	36.615527
1526.079255	116711.680326	36.620544
1527.484539	116870.614484	36.625562
1529.340870	117038.180073	36.630580
1530.796799	117200.557697	36.635597
1532.197085	117362.665644	36.640615
1533.759256	117528.440076	36.645632
1535.501036	117683.545551	36.650650
1537.366838	117842.234586	36.655668
1538.850324	117986.245064	36.660685
1539.903237	118134.952763	36.665703
1541.625387	118276.441143	36.670720
1542.999326	118422.905674	36.675738
1544.911489	118566.141337	36.680756
1546.578670	118711.673455	36.685773
1548.102494	118854.425232	36.690791
1549.116392	119008.457125	36.695808
1550.649222	119162.966983	36.700826
1552.448527	119317.080831	36.705844
1553.502560	119467.150807	36.710861
1554.892445	119612.488527	36.715879
1555.596646	119793.995638	36.720896
1557.536110	119955.269693	36.725914
1559.224272	120129.724830	36.730932
1560.824069	120308.164825	36.735949
1561.902254	120483.705914	36.740967
1563.207981	120663.055886	36.745984
1564.825849	120847.647703	36.751002
1566.270246	121031.493619	36.756020
1567.517601	121222.512731	36.761037
1569.190326	121412.946489	36.766055
1570.882276	121607.615019	36.771072
1572.890976	121806.966799	36.776090
1574.129729	122003.217377	36.781108
1575.992183	122198.674172	36.786125
1577.900499	122380.005974	36.791143
1579.234327	122573.618736	36.796160
1580.970691	122767.981670	36.801178
1582.659522	122959.625565	36.806196
1584.226880	123146.037445	36.811213
1586.104126	123333.657856	36.816231
1587.570353	123530.197778	36.821248
1589.346651	123723.277929	36.826266
1591.298113	123906.068885	36.831284
1592.449700	124095.049047	36.836301
1593.903811	124296.960785	36.841319
1595.590555	124493.014434	36.846336
1597.218873	124686.578971	36.851354
1599.053518	124884.248021	36.856372
1601.023548	125068.462244	36.861389
1602.608334	125256.099138	36.866407
1604.413587	125446.290604	36.871424
1606.132298	125629.024138	36.876442
1608.139799	125808.262828	36.881460
1609.917223	126008.102977	36.886477
1611.443204	126184.639922	36.891495
1612.709797	126374.006135	36.896512
1614.493241	126543.793327	36.901530
1616.535713	126733.002384	36.906548
1618.148812	126914.705117	36.911565
1619.618034	127085.939009	36.916583
1621.149791	127278.668208	36.921600
1622.138722	127458.021909	36.926618
1623.896401	127649.778841	36.931636
1625.282666	127841.772088	36.936653
1626.905196	128037.091547	36.941671
1627.844669	128230.945020	36.946688
1630.022559	128430.201734	36.951706
1631.796414	128632.427683	36.956724
1632.614256	128832.963734	36.961741
1634.156687	129021.372947	36.966759
1635.827940	129231.039914	36.971776
1637.268561	129442.951461	36.976794
1638.760433	129653.676143	36.981812
1640.295354	129866.260269	36.986829
1642.193251	130075.350582	36.991847
1643.249763	130285.296084	36.996864
1645.074270	130482.600142	37.001882
1646.693533	130678.769765	37.006900
1648.116770	130892.429499	37.011917
1650.071819	131089.107015	37.016935
1651.564828	131291.731948	37.021952
1652.931485	131479.392753	37.026970
1655.343300	131667.894076	37.031988
1656.892189	131863.597911	37.037005
1659.123964	132061.378744	37.042023
1660.851269	132265.443630	37.047040
1661.998230	132466.288108	37.052058
1663.808667	132669.682150	37.057076
1665.409437	132864.798747	37.062093
1667.221205	133070.338819	37.067111
1668.525517	133275.578175	37.072128
1670.708838	133465.785070	37.077146
1672.670014	133662.321017	37.082164
1674.060820	133871.407089	37.087181
1675.636187	134085.173021	37.092199
1677.172030	134292.652391	37.097216
1678.662599	134503.185150	37.102234
1680.254944	134705.924635	37.107252
1681.869322	134932.745671	37.112269
1683.550121	135154.799053	37.117287
1684.772303	135387.431660	37.122304
1686.022548	135610.518692	37.127322
1688.031009	135839.135618	37.132340
1689.476942	136084.794429	37.137357
1691.238295	136309.290032	37.142375
1693.067050	136552.074706	37.147392
1694.656630	136795.951144	37.152410
1696.376292	137024.162151	37.157428
1698.030935	137268.183257	37.162445
1699.603792	137508.081480	37.167463
1701.340933	137749.719288	37.172480
1703.108699	137992.660668	37.177498
1705.144628	138242.604591	37.182516
1706.817977	138491.629148	37.187533
1708.585194	138731.033917	37.192551
1710.018377	138966.735575	37.197568
1712.753909	139206.093591	37.202586
1714.198772	139447.392297	37.207604
1715.945781	139692.858456	37.212621
1718.046267	139924.793503	37.217639
1719.824762	140165.574400	37.222656
1721.296570	140403.980330	37.227674
1723.218129	140640.286934	37.232692
1724.834814	140889.129917	37.237709
1726.611004	141121.717735	37.242727
1728.263235	141366.369672	37.247744
1729.854404	141595.181295	37.252762
1731.493762	141847.528421	37.257780
1733.032070	142095.869500	37.262797
1734.991839	142337.508758	37.267815
1736.666392	142587.265245	37.272832
1738.117967	142823.287628	37.277850
1740.419583	143069.205039	37.282868
1742.290795	143313.883449	37.287885
1744.231247	143549.071742	37.292903
1745.720453	143791.895558	37.297920
1747.391024	144036.875296	37.302938
1749.401513	144279.163463	37.307956
1751.237893	144512.608371	37.312973
1752.667961	144760.827415	37.317991
1754.613173	145001.809293	37.323008
1755.991720	145256.943185	37.328026
1757.988007	145482.968311	37.333044
1759.467476	145734.281304	37.338061
1760.952219	145968.599972	37.343079
1763.031496	146198.258003	37.348096
1764.821046	146416.082231	37.353114
1766.115002	146650.344873	37.358132
1767.730758	146889.305434	37.363149
1769.353592	147110.255484	37.368167
1771.447360	147345.627966	37.373184
1772.902552	147588.348330	37.378202
1774.625345	147831.612035	37.383220
1776.092150	148083.078080	37.388237
1777.702986	148322.134845	37.393255
1779.797424	148580.943513	37.398272
1781.144806	148834.957602	37.403290
1783.114886	149080.295611	37.408308
1784.563030	149357.143703	37.413325
1786.282576	149617.475472	37.418343
1788.059965	149879.919249	37.423360
1789.464660	150148.845040	37.428378
1791.322871	150417.511192	37.433396
1792.860982	150702.209312	37.438413
1794.538844	150971.007828	37.443431
1796.510038	151259.703331	37.448448
1798.477193	151548.756405	37.453466
1800.410211	151825.452827	37.458484
1802.292167	152109.838207	37.463501
1803.916354	152388.235685	37.468519
1805.795704	152678.768120	37.473536
1807.671512	152981.602899	37.478554
1809.793160	153273.395488	37.483572
1811.481062	153556.510993	37.488589
1813.250157	153841.214725	37.493607
1815.682031	154141.278082	37.498624
1818.853541	154389.753309	37.503642
1821.288412	154646.862049	37.508660
1823.037094	154912.177651	37.513677
1824.800484	155172.706448	37.518695
1826.471843	155434.824844	37.523712
1828.096277	155713.594077	37.528730
1829.905803	155968.673384	37.533748
1831.569351	156234.858831	37.538765
1833.169933	156508.786277	37.543783
1835.000921	156777.994825	37.548800
1836.814146	157053.859380	37.553818
1838.132631	157337.622181	37.558836
1839.963449	157627.120818	37.563853
1842.001779	157908.095697	37.568871
1843.930667	158194.839727	37.573888
1845.602850	158468.612718	37.578906
1847.817549	158734.406198	37.583924
1850.199501	159009.658049	37.588941
1852.486246	159277.321565	37.593959
1854.727502	159542.809756	37.598976
1856.488878	159813.591535	37.603994
1858.070895	160081.939525	37.609012
1859.790797	160340.364828	37.614029
1861.709544	160618.857115	37.619047
1863.385999	160879.233815	37.624064
1865.087911	161153.458461	37.629082
1866.739522	161430.358204	37.634100
1868.234058	161715.040645	37.639117
1869.910741	161988.891969	37.644135
1871.862646	162271.626752	37.649152
1873.712567	162565.030444	37.654170
1875.403763	162855.705171	37.659188
1876.931189	163142.940704	37.664205
1878.556843	163432.269752	37.669223
1880.457216	163718.561060	37.674240
1882.055625	164021.875297	37.679258
1883.868411	164292.223741	37.684276
1885.203672	164584.573955	37.689293
1886.490804	164879.116700	37.694311
1888.398817	165175.760576	37.699328
1889.986365	165475.909051	37.704346
1891.894312	165774.485424	37.709364
1893.797066	166082.192695	37.714381
1895.740680	166394.541931	37.719399
1897.805950	166704.892986	37.724416
1899.207518	167016.339074	37.729434
1901.250926	167330.784669	37.734452
1903.157546	167654.699375	37.739469
1904.710172	167976.182092	37.744487
1906.455454	168305.165551	37.749504
1908.393093	168634.488812	37.754522
1910.331837	168970.276203	37.759540
1912.247367	169302.031112	37.764557
1914.136712	169636.127895	37.769575
1915.810924	169986.143884	37.774592
1917.656736	170324.935870	37.779610
1919.820224	170660.365980	37.784628
1921.906455	171008.341938	37.789645
1923.587519	171356.458769	37.794663
1926.116358	171695.607826	37.799680
1928.206267	172038.534408	37.804698
1931.112167	172366.619030	37.809716
1933.508580	172701.882347	37.814733
1935.158234	173032.742967	37.819751
1937.413173	173352.324076	37.824768
1939.355853	173693.820733	37.829786
1941.136180	174027.217513	37.834804
1943.367643	174361.954963	37.839821
1945.183920	174691.311015	37.844839
1947.228887	175030.016679	37.849856
1948.727689	175351.996515	37.854874
1951.322540	175688.905132	37.859892
1953.179545	176031.085443	37.864909
1954.851867	176363.607172	37.869927
1956.841286	176709.579173	37.874944
1958.545929	177047.038256	37.879962
1960.524974	177397.433753	37.884980
1962.453928	177725.870195	37.889997
1964.251040	178077.541278	37.895015
1966.382801	178425.301369	37.900032
1968.462401	178772.080493	37.905050
1970.688293	179110.431734	37.910068
1972.682913	179465.785742	37.915085
1974.216412	179803.434703	37.920103
1976.205381	180157.217731	37.925120
1977.963739	180522.340028	37.930138
1979.900955	180886.013695	37.935156
1981.991847	181232.114952	37.940173
1983.361761	181599.587854	37.945191
1985.473218	181956.025628	37.950208
1986.833150	182332.722504	37.955226
1988.593466	182695.440311	37.960244
1990.967235	183083.564032	37.965261
1992.923529	183469.824018	37.970279
1994.823485	183840.118602	37.975296
1996.843838	184220.987118	37.980314
1998.832750	184604.325692	37.985332
2000.967289	184981.039375	37.990349
2002.687097	185371.509084	37.995367
2004.731836	185733.584351	38.000384
2006.638498	186130.885663	38.005402
2008.646649	186523.905638	38.010420
2010.915826	186889.836145	38.015437
2013.296565	187283.613779	38.020455
2015.006623	187694.692764	38.025472
2017.018510	188061.861149	38.030490
2019.037875	188421.892294	38.035508
2020.544803	188786.296950	38.040525
2022.471522	189146.421095	38.045543
2024.704053	189503.501616	38.050560
2026.638008	189875.158580	38.055578
2028.447953	190243.076839	38.060596
2030.965425	190615.229607	38.065613
2032.972599	190996.505503	38.070631
2035.360162	191343.966317	38.075648
2037.987713	191719.890129	38.080666
2039.783250	192088.781657	38.085684
2041.653878	192465.181210	38.090701
2043.475434	192834.807572	38.095719
2045.379783	193215.979510	38.100736
2047.384701	193588.272061	38.105754
2049.089541	193972.881059	38.110772
2050.983940	194365.437629	38.115789
2053.110504	194761.083591	38.120807
2055.131645	195142.141485	38.125824
2057.109535	195539.336988	38.130842
2058.925193	195948.294318	38.135860
2061.287463	196349.191770	38.140877
2062.787565	196761.680623	38.145895
2065.255284	197157.407494	38.150912
2068.087769	197563.671169	38.155930
2069.969117	197969.779195	38.160948
2072.047261	198359.473596	38.165965
2074.143542	198773.856759	38.170983
2076.460072	199176.775939	38.176000
2078.656485	199581.950246	38.181018
2080.608014	199988.332215	38.186036
2082.648821	200390.738613	38.191053
2084.673934	200801.683584	38.196071
2086.652791	201226.557201	38.201088
2088.988519	201632.451677	38.206106
2090.514202	202059.074490	38.211124
2092.802085	202472.192681	38.216141
2094.424017	202902.104907	38.221159
2096.428768	203325.531757	38.226176
2098.806810	203755.506173	38.231194
2101.101882	204188.593625	38.236212
2103.496695	204611.505474	38.241229
2105.752172	205034.033497	38.246247
2107.705690	205451.300240	38.251264
2109.884367	205878.033480	38.256282
2111.935634	206310.757124	38.261300
2113.993289	206732.049340	38.266317
2115.985122	207166.638407	38.271335
2118.908031	207595.875809	38.276352
2121.094544	208016.286748	38.281370
2122.883814	208439.605437	38.286388
2125.309549	208864.350030	38.291405
2127.347978	209297.614932	38.296423
2129.527364	209722.119929	38.301440
2131.687656	210136.035423	38.306458
2133.402462	210571.512158	38.311476
2136.117010	211000.584777	38.316493
2138.047959	211423.048104	38.321511
2140.045893	211845.120586	38.326528
2142.442105	212277.089877	38.331546
2144.525436	212703.926158	38.336564
2146.827102	213125.876962	38.341581
2148.984403	213548.790724	38.346599
2151.279100	213978.313998	38.351616
2153.089815	214395.668554	38.356634
2155.338009	214817.172533	38.361652
2157.653205	215216.666923	38.366669
2159.406318	215625.750216	38.371687
2161.168343	216022.664124	38.376704
2163.702057	216414.021899	38.381722
2165.625270	216826.204576	38.386740
2167.660578	217226.887637	38.391757
2169.655971	217645.207549	38.396775
2171.190844	218065.708008	38.401792
2173.489078	218487.868279	38.406810
2175.281430	218920.370798	38.411828
2177.391036	219353.789614	38.416845
2179.088137	219786.688635	38.421863
2181.451517	220230.916044	38.426880
2183.446563	220687.852249	38.431898
2185.437890	221135.415211	38.436916
2187.754007	221582.267355	38.441933
2190.025239	222042.870288	38.446951
2192.110165	222503.095949	38.451968
2194.322229	222967.595288	38.456986
2196.344667	223442.235116	38.462004
2198.674084	223909.028250	38.467021
2200.825492	224377.856115	38.472039
2203.569183	224831.095389	38.477056
2206.580325	225279.517122	38.482074
2209.116087	225740.689513	38.487092
2211.165144	226209.990755	38.492109
2213.566890	226668.694391	38.497127
2215.649394	227115.736384	38.502144
2217.899220	227586.149442	38.507162
2219.964442	228057.048411	38.512180
2222.192413	228528.048955	38.517197
2224.260187	228989.192103	38.522215
2226.134778	229454.124956	38.527232
2228.675853	229930.309506	38.532250
2230.895326	230424.148877	38.537268
2233.376690	230888.453152	38.542285
2235.183019	231367.748965	38.547303
2237.859804	231836.518771	38.552320
2240.097026	232314.552902	38.557338
2241.950517	232808.193610	38.562356
2244.391183	233286.754207	38.567373
2246.024656	233780.352103	38.572391
2248.242575	234277.745365	38.577408
2250.984687	234759.814229	38.582426
2253.128166	235261.790736	38.587444
2255.632171	235753.218789	38.592461
2257.874197	236242.426094	38.597479
2260.002542	236732.463404	38.602496
2262.934187	237227.608223	38.607514
2265.195720	237720.798951	38.612532
2267.528253	238206.534663	38.617549
2269.688327	238697.783678	38.622567
2272.307434	239191.272220	38.627584
2275.103783	239662.910773	38.632602
2277.441990	240141.885265	38.637620
2279.567881	240615.684297	38.642637
2282.777007	241089.313940	38.647655
2284.758100	241549.238236	38.652672
2287.201340	242018.641436	38.657690
2289.271608	242510.507468	38.662708
2291.170361	242977.834324	38.667725
2293.294098	243458.004644	38.672743
2295.546119	243934.241933	38.677760
2297.937505	244421.151206	38.682778
2300.346794	244902.163127	38.687796
2302.707655	245378.024716	38.692813
2304.720486	245861.433229	38.697831
2307.001295	246339.642126	38.702848
2309.210534	246787.606356	38.707866
2310.875837	247256.865446	38.712884
2312.985619	247718.281011	38.717901
2315.016492	248175.363882	38.722919
2316.968482	248650.544461	38.727936
2319.262137	249123.714623	38.732954
2321.435835	249606.301049	38.737972
2323.442009	250090.918973	38.742989
2325.800243	250590.823646	38.748007
2327.256884	251078.902717	38.753024
2330.283844	251572.502203	38.758042
2332.220273	252091.697237	38.763060
2334.324251	252595.953564	38.768077
2336.639486	253122.020894	38.773095
2338.761499	253640.064108	38.778112
2341.021974	254161.563972	38.783130
2343.044804	254694.224802	38.788148
2345.407764	255220.251729	38.793165
2347.938391	255767.486083	38.798183
2350.028938	256311.103555	38.803200
2352.588498	256847.330315	38.808218
2355.211713	257399.522224	38.813236
2357.617130	257950.856644	38.818253
2360.052772	258507.568940	38.823271
2361.720132	259065.871564	38.828288
2364.047003	259624.348426	38.833306
2366.309540	260197.768182	38.838324
2368.789091	260768.154165	38.843341
2371.550056	261342.583004	38.848359
2373.900320	261915.980691	38.853376
2376.101251	262486.096725	38.858394
2378.704270	263065.545198	38.863412
2381.239229	263647.058578	38.868429
2383.760434	264220.671718	38.873447
2386.211334	264796.070667	38.878464
2388.748542	265362.918880	38.883482
2390.955244	265952.166639	38.888500
2393.475773	266540.828774	38.893517
2396.471042	267106.986425	38.898535
2399.066193	267696.290496	38.903552
2401.743099	268271.024939	38.908570
2404.241245	268844.615447	38.913588
2406.818912	269422.380823	38.918605
2409.284966	269982.838536	38.923623
2411.829468	270564.767269	38.928640
2414.384970	271136.887059	38.933658
2417.030237	271693.572924	38.938676
2419.731811	272260.634091	38.943693
2422.072251	272825.563642	38.948711
2424.014270	273387.173715	38.953728
2426.716927	273956.179232	38.958746
2429.264811	274523.198681	38.963764
2431.863212	275080.581134	38.968781
2434.663602	275649.128223	38.973799
2437.077047	276210.417475	38.978816
2439.617997	276756.546953	38.983834
2441.999720	277324.283988	38.988852
2444.045874	277889.301053	38.993869
2446.464019	278453.570483	38.998887
2448.959108	279013.785981	39.003904
2451.781904	279575.724054	39.008922
2454.197581	280142.546370	39.013940
2456.519214	280697.545094	39.018957
2458.907655	281258.370034	39.023975
2461.298593	281812.536993	39.028992
2463.925671	282368.059674	39.034010
2466.810259	282913.380414	39.039028
2469.015726	283456.898150	39.044045
2471.985855	283994.071287	39.049063
2473.728029	284523.178555	39.054080
2476.271037	285046.342125	39.059098
2479.045503	285568.145270	39.064116
2481.193778	286091.286130	39.069133
2483.988294	286614.703271	39.074151
2486.163654	287153.930604	39.079168
2488.338771	287689.370168	39.084186
2490.551873	288229.420825	39.089204
2492.735010	288782.700819	39.094221
2494.964832	289332.718706	39.099239
2497.153233	289898.963417	39.104256
2500.018683	290447.273155	39.109274
2502.023309	291014.907630	39.114292
2504.475436	291585.564984	39.119309
2507.041327	292163.435666	39.124327
2508.913355	292749.635328	39.129344
2511.574534	293321.513565	39.134362
2513.818536	293925.061509	39.139380
2516.279627	294516.230322	39.144397
2518.912725	295109.854628	39.149415
2521.466680	295718.083911	39.154432
2524.358525	296307.923654	39.159450
2527.401528	296912.509924	39.164468
2529.564684	297515.348029	39.169485
2531.824972	298113.645595	39.174503
2534.372047	298734.284060	39.179520
2536.876865	299356.369298	39.184538
2539.515609	299986.956765	39.189556
2542.025364	300594.988270	39.194573
2544.155089	301221.756575	39.199591
2546.660148	301855.770428	39.204608
2548.922367	302475.776207	39.209626
2551.871542	303117.296357	39.214644
2554.105281	303767.551032	39.219661
2556.670341	304411.780615	39.224679
2559.236168	305062.348238	39.229696
2562.697456	305689.110133	39.234714
2565.653227	306323.964344	39.239732
2568.482786	306963.602372	39.244749
2571.224061	307584.995381	39.249767
2573.712972	308243.428365	39.254784
2576.229641	308878.470829	39.259802
2578.970292	309516.084610	39.264820
2581.324292	310153.496402	39.269837
2584.267806	310775.375990	39.274855
2586.891163	311426.054421	39.279872
2589.441067	312066.049996	39.284890
2591.819977	312692.916340	39.289908
2594.871655	313341.395174	39.294925
2597.867995	313967.234665	39.299943
2601.130149	314595.232352	39.304960
2603.981417	315212.524579	39.309978
2606.973737	315828.517556	39.314996
2609.089414	316448.623021	39.320013
2611.803757	317067.104083	39.325031
2614.243577	317695.795840	39.330048
2616.933727	318316.902612	39.335066
2619.216434	318928.116187	39.340084
2621.769812	319556.915999	39.345101
2624.441975	320180.435312	39.350119
2627.126031	320801.913691	39.355136
2629.394208	321429.461835	39.360154
2632.438852	322054.317002	39.365172
2634.727119	322688.618644	39.370189
2637.311638	323308.451865	39.375207
2639.761203	323940.907877	39.380224
2641.976870	324572.426457	39.385242
2644.569858	325185.937647	39.390260
2646.763907	325806.225602	39.395277
2649.250494	326409.103693	39.400295
2651.549855	327026.870111	39.405312
2653.725765	327655.886012	39.410330
2656.383783	328283.548428	39.415348
2658.887759	328918.658639	39.420365
2661.122125	329557.479350	39.425383
2663.695771	330208.516077	39.430400
2666.424938	330854.519890	39.435418
2669.416174	331510.340858	39.440436
2671.282739	332181.293376	39.445453
2674.174130	332849.766129	39.450471
2676.938376	333518.678186	39.455488
2678.932782	334200.204449	39.460506
2681.580098	334873.448532	39.465524
2683.855074	335565.991740	39.470541
2686.910656	336262.738173	39.475559
2689.491848	336964.466216	39.480576
2692.338168	337669.081932	39.485594
2695.277540	338369.712634	39.490612
2698.077400	339069.489097	39.495629
2701.215320	339769.351516	39.500647
2704.125256	340468.474810	39.505664
2706.664242	341184.051769	39.510682
2709.445178	341893.438911	39.515700
2712.246110	342594.997186	39.520717
2715.484585	343306.643100	39.525735
2717.910416	344018.274058	39.530752
2720.707558	344735.487847	39.535770
2723.549994	345444.564484	39.540788
2726.109219	346167.922228	39.545805
2729.038240	346880.860670	39.550823
2732.129157	347597.816082	39.555840
2735.105614	348325.322629	39.560858
2737.961938	349028.768234	39.565876
2740.692082	349749.714389	39.570893
2743.621102	350470.081295	39.575911
2746.706470	351171.771866	39.580928
2749.571924	351878.146756	39.585946
2752.647675	352586.273606	39.590964
2755.522327	353294.390772	39.595981
2758.553393	353995.850747	39.600999
2761.820818	354692.923163	39.606016
2764.547594	355390.140373	39.611034
2767.243241	356091.605970	39.616052
2769.616058	356795.412967	39.621069
2772.421984	357500.201325	39.626087
2775.355770	358207.767510	39.631104
2777.860322	358922.355175	39.636122
2780.233091	359638.695679	39.641140
2782.974536	360351.387884	39.646157
2785.545145	361068.500287	39.651175
2788.172728	361791.416443	39.656192
2790.782159	362517.765004	39.661210
2793.517358	363251.958667	39.666228
2796.724390	363971.386075	39.671245
2799.289677	364700.425150	39.676263
2802.252589	365435.644032	39.681280
2804.467863	366168.451751	39.686298
2807.723226	366905.235196	39.691316
2810.385797	367645.589177	39.696333
2812.693610	368386.080601	39.701351
2815.821387	369117.277366	39.706368
2818.063987	369873.856579	39.711386
2821.477371	370607.352290	39.716404
2823.872923	371355.683391	39.721421
2826.300365	372094.082490	39.726439
2829.186760	372817.593799	39.731456
2831.663266	373539.553767	39.736474
2834.998558	374258.016846	39.741492
2837.648048	374975.073019	39.746509
2840.338548	375697.804130	39.751527
2842.989407	376412.288729	39.756544
2845.755023	377152.373408	39.761562
2848.898040	377882.904715	39.766580
2851.525381	378622.134314	39.771597
2854.118058	379357.903758	39.776615
2857.131246	380105.492418	39.781632
2859.665934	380857.642919	39.786650
2862.467511	381613.098986	39.791668
2865.361697	382375.154634	39.796685
2868.036113	383136.994139	39.801703
2870.823740	383904.137391	39.806720
2873.226532	384684.512235	39.811738
2876.192277	385464.319792	39.816756
2878.873545	386252.707212	39.821773
2881.691946	387049.759905	39.826791
2884.947242	387839.882313	39.831808
2887.223752	388639.830278	39.836826
2890.357802	389463.547257	39.841844
2893.050983	390271.075390	39.846861
2895.753570	391090.247730	39.851879
2899.034661	391916.948815	39.856896
2901.507400	392733.519471	39.861914
2904.629392	393561.050296	39.866932
2908.520007	394383.876360	39.871949
2911.512906	395200.839670	39.876967
2914.848020	396021.620187	39.881984
2917.756876	396838.540535	39.887002
2921.110836	397662.653373	39.892020
2923.944411	398501.043338	39.897037
2926.726457	399326.300595	39.902055
2930.332420	400142.289059	39.907072
2933.406563	400970.226678	39.912090
2936.643128	401779.786608	39.917108
2939.414890	402603.460991	39.922125
2942.169768	403422.806395	39.927143
2945.215486	404232.511817	39.932160
2948.446664	405054.153639	39.937178
2951.551130	405868.093136	39.942196
2954.687025	406700.873761	39.947213
2957.162381	407518.191197	39.952231
2960.641391	408335.018872	39.957248
2963.171215	409162.488739	39.962266
2966.135787	409989.404575	39.967284
2968.936389	410817.124337	39.972301
2972.399809	411649.111246	39.977319
2975.286744	412477.108780	39.982336
2977.759709	413300.687258	39.987354
2981.007011	414132.966600	39.992372
2983.805305	414970.999718	39.997389
2986.272939	415807.230459	40.002407
2989.514040	416639.210909	40.007424
2992.218815	417493.547668	40.012442
2995.319743	418330.035556	40.017460
2998.590250	419177.337438	40.022477
3001.601245	420026.364863	40.027495
3004.544904	420861.713924	40.032512
3007.217726	421720.535549	40.037530
3010.425034	422566.191973	40.042548
3013.691063	423418.681282	40.047565
3016.439742	424275.412281	40.052583
3019.528646	425115.116463	40.057600
3022.690141	425967.768136	40.062618
3025.765415	426800.225179	40.067636
3028.685597	427615.635041	40.072653
3031.624466	428436.316784	40.077671
3034.823266	429250.403306	40.082688
3037.839566	430052.757652	40.087706
3040.799825	430850.943374	40.092724
3044.183695	431661.666866	40.097741
3047.250521	432468.362819	40.102759
3050.320507	433279.270328	40.107776
3053.096468	434086.096233	40.112794
3056.416358	434902.809987	40.117812
3059.746573	435715.495424	40.122829
3062.239432	436536.513439	40.127847
3065.354718	437359.824808	40.132864
3068.088621	438201.753942	40.137882
3070.810210	439027.580798	40.142900
3074.092501	439870.664132	40.147917
3076.247887	440726.111019	40.152935
3079.478176	441586.555008	40.157952
3082.234264	442454.054849	40.162970
3085.360725	443318.274297	40.167988
3088.771990	444187.106651	40.173005
3091.402364	445063.141331	40.178023
3094.623238	445951.668905	40.183040
3098.024413	446848.862424	40.188058
3101.063923	447745.108556	40.193076
3103.983900	448621.685099	40.198093
3107.314011	449513.708153	40.203111
3110.694474	450424.159852	40.208128
3113.539872	451318.188519	40.213146
3116.419315	452231.958641	40.218164
3119.819101	453131.919180	40.223181
3122.523064	454055.467504	40.228199
3125.764945	454970.907841	40.233216
3128.771110	455898.350927	40.238234
3132.373345	456824.794020	40.243252
3135.262580	457746.554377	40.248269
3138.148707	458690.271146	40.253287
3141.558366	459610.438153	40.258304
3144.697484	460553.155675	40.263322
3147.766424	461498.203965	40.268340
3151.542872	462434.965960	40.273357
3154.732073	463379.537943	40.278375
3158.256835	464303.874151	40.283392
3161.765211	465248.090178	40.288410
3164.676761	466187.048983	40.293428
3168.213045	467106.991493	40.298445
3171.032247	468058.823703	40.303463
3174.270804	469001.860533	40.308480
3177.668964	469941.237738	40.313498
3180.312453	470888.546364	40.318516
3183.504261	471838.539036	40.323533
3186.465565	472786.495208	40.328551
3189.943974	473724.886270	40.333568
3192.633131	474685.531290	40.338586
3195.820488	475655.318608	40.343604
3199.007126	476615.367739	40.348621
3201.485300	477590.694096	40.353639
3204.697799	478554.857285	40.358656
3208.068698	479536.932324	40.363674
3211.267368	480522.047770	40.368692
3214.419719	481494.760821	40.373709
3217.418212	482481.548627	40.378727
3220.908018	483461.848071	40.383744
3224.080002	484446.065685	40.388762
3227.264718	485431.881618	40.393780
3230.431618	486416.075488	40.398797
3233.521914	487407.573904	40.403815
3236.968999	488380.967854	40.408832
3240.293384	489330.441345	40.413850
3243.343260	490278.840462	40.418868
3246.799643	491229.685721	40.423885
3249.405524	492191.834796	40.428903
3252.895728	493137.870397	40.433920
3256.064899	494099.356270	40.438938
3259.010327	495054.671672	40.443956
3262.386942	496005.729733	40.448973
3265.470133	496986.528510	40.453991
3268.737243	497944.729094	40.459008
3271.990593	498926.228116	40.464026
3275.096593	499907.835320	40.469044
3278.275269	500887.653794	40.474061
3281.866727	501880.126306	40.479079
3285.211907	502870.606326	40.484096
3288.724379	503857.016658	40.489114
3292.221116	504851.564163	40.494132
3295.315761	505834.884265	40.499149
3298.566695	506835.269552	40.504167
3301.696786	507839.225647	40.509184
3304.762224	508859.571154	40.514202
3307.859354	509884.465899	40.519220
3311.176321	510901.958225	40.524237
3314.043084	511943.488328	40.529255
3317.326671	512964.507353	40.534272
3320.562264	514011.206738	40.539290
3323.802214	515058.882318	40.544308
3327.247187	516116.653504	40.549325
3330.822269	517169.144470	40.554343
3333.799758	518236.880342	40.559360
3337.467327	519295.125406	40.564378
3340.558230	520376.298827	40.569396
3343.944206	521434.471015	40.574413
3347.857525	522510.420025	40.579431
3351.097153	523583.271958	40.584448
3354.306091	524668.052258	40.589466
3357.589829	525743.387023	40.594484
3361.163738	526824.718991	40.599501
3364.802932	527914.794140	40.604519
3368.102548	529002.270088	40.609536
3371.979853	530080.022606	40.614554
3375.600324	531169.729963	40.619572
3379.060247	532235.365807	40.624589
3382.913765	533311.599233	40.629607
3386.738808	534382.324626	40.634624
3390.325553	535454.855831	40.639642
3393.656709	536522.869086	40.644660
3397.344966	537597.966360	40.649677
3400.839664	538677.570851	40.654695
3404.081065	539748.038411	40.659712
3407.636167	540821.076701	40.664730
3411.087368	541888.921226	40.669748
3414.410653	542966.529841	40.674765
3417.697884	544040.689662	40.679783
3420.977402	545113.002259	40.684800
3424.375349	546191.324089	40.689818
3427.711219	547281.700630	40.694836
3430.827751	548361.933532	40.699853
3434.131057	549454.179273	40.704871
3437.286975	550542.890419	40.709888
3440.829585	551633.600474	40.714906
3444.121087	552728.964843	40.719924
3448.092634	553826.129785	40.724941
3451.347673	554916.388703	40.729959
3454.773011	556014.241611	40.734976
3458.636483	557113.980791	40.739994
3461.863816	558222.638347	40.745012
3465.108580	559303.794929	40.750016
3468.566978	560352.054213	40.755021
3471.628710	561354.472203	40.760026
3475.294029	562306.735857	40.765031
3478.269484	563201.876521	40.770036
3481.411579	564033.446201	40.775040
3484.295088	564818.647996	40.780045
3487.792945	565533.102634	40.785050
3490.509118	566184.621926	40.790055
3492.830196	566787.013422	40.795060
3495.261808	567327.202994	40.800064
3497.629721	567820.337428	40.805069
3499.775226	568260.975524	40.810074
3501.962851	568641.853439	40.815079
3503.268464	568977.025640	40.820084
3505.038950	569283.001912	40.825088
3506.536131	569532.643463	40.830093
3508.072645	569752.508304	40.835098
3509.423636	569923.710190	40.840103
3510.568771	570066.833567	40.845108
3511.811930	570179.724117	40.850112
3512.828010	570249.383388	40.855117
3513.281802	570304.825064	40.860122
3514.011021	570326.896337	40.865127
3514.684203	570321.421034	40.870132
3515.455370	570296.255279	40.875136
3516.288741	570262.747915	40.880141
3516.426510	570205.005466	40.885146
3517.136973	570127.598502	40.890151
3517.490432	570031.173231	40.895156
3517.900320	569926.607027	40.900160
3517.976807	569797.697464	40.905165
3518.741415	569661.752515	40.910170
3518.922591	569522.433278	40.915175
3519.095237	569368.757653	40.920180
3519.685870	569196.793552	40.925184
3519.635061	569028.390323	40.930189
3519.379170	568838.180328	40.935194
3519.822768	568642.637640	40.940199
3519.612052	568440.617264	40.945204
3519.599958	568242.779313	40.950208
3519.870581	568033.648793	40.955213
3519.497374	567830.237374	40.960218
3519.679357	567613.381838	40.965223
3519.621419	567392.041167	40.970228
3519.918310	567167.026253	40.975232
3520.053635	566945.747392	40.980237
3519.520222	566715.430619	40.985242
3519.890402	566483.462408	40.990247
3519.785133	566259.044758	40.995252
3519.624230	566014.999147	41.000256
3519.795241	565788.671636	41.005261
3519.532279	565553.268588	41.010266
3519.324535	565304.294536	41.015271
3518.862809	565076.344381	41.020276
3518.944198	564836.404171	41.025280
3519.188299	564600.902985	41.030285
3518.570897	564363.170886	41.035290
3518.371423	564124.716072	41.040295
3518.191355	563895.443569	41.045300
3517.937639	563653.773541	41.050304
3518.139911	563439.097026	41.055309
3517.897028	563213.286233	41.060314
3517.675786	562971.245523	41.065319
3517.660458	562743.230661	41.070324
3517.352867	562509.832496	41.075328
3517.492248	562289.167902	41.080333
3517.102518	562062.102168	41.085338
3517.028001	561845.129139	41.090343
3516.736560	561620.450555	41.095348
3516.854079	561390.279176	41.100352
3516.772166	561179.372913	41.105357
3516.288941	560949.939436	41.110362
3516.277176	560738.361363	41.115367
3515.718219	560532.993198	41.120372
3515.621994	560317.552724	41.125376
3515.769362	560107.094001	41.130381
3516.053873	559898.971323	41.135386
3515.698753	559672.507339	41.140391
3514.989401	559481.713244	41.145396
3515.293949	559267.547760	41.150400
3515.101610	559063.704741	41.155405
3514.664096	558876.375430	41.160410
3514.676728	558673.599128	41.165415
3514.313049	558472.988122	41.170420
3514.238233	558272.328785	41.175424
3514.182891	558085.078279	41.180429
3513.892288	557900.624922	41.185434
3513.807566	557706.690448	41.190439
3513.573578	557525.940685	41.195444
3513.714154	557340.406641	41.200448
3513.490848	557147.891589	41.205453
3513.392497	556972.488912	41.210458
3513.609845	556791.356316	41.215463
3512.992514	556612.009135	41.220468
3512.752418	556430.389508	41.225472
3513.064067	556256.118569	41.230477
3512.668022	556072.256445	41.235482
3512.907232	555906.735683	41.240487
3512.583429	555740.697204	41.245492
3512.188904	555571.250103	41.250496
3512.326452	555398.752736	41.255501
3511.990692	555237.433187	41.260506
3511.893481	555071.098916	41.265511
3511.965922	554913.631548	41.270516
3511.565111	554753.270527	41.275520
3511.660876	554590.166374	41.280525
3511.487469	554421.774379	41.285530
3511.586336	554262.937389	41.290535
3511.187360	554122.470765	41.295540
3510.855993	553962.842341	41.300544
3511.301544	553808.720279	41.305549
3510.797703	553661.579737	41.310554
3510.830894	553507.568269	41.315559
3510.587465	553362.293574	41.320564
3510.415263	553219.418755	41.325568
3510.599180	553080.709114	41.330573
3510.369674	552933.768359	41.335578
3510.144121	552786.774940	41.340583
3509.880775	552660.395099	41.345588
3509.858453	552523.168917	41.350592
3510.002984	552392.550609	41.355597
3509.753418	552253.446554	41.360602
3509.846649	552113.734601	41.365607
3509.736032	551988.178574	41.370612
3509.886391	551847.650358	41.375616
3509.758629	551717.117437	41.380621
3509.353339	551589.290687	41.385626
3509.621282	551461.408103	41.390631
3509.101649	551343.248771	41.395636
3509.029754	551206.568446	41.400640
3509.133795	551086.248377	41.405645
3509.032500	550962.992910	41.410650
3508.981118	550831.533684	41.415655
3508.644986	550718.970491	41.420660
3508.551818	550599.530987	41.425664
3508.808332	550490.141368	41.430669
3508.557539	550364.841813	41.435674
3508.360089	550255.017968	41.440679
3507.799124	550137.506988	41.445684
3507.797425	550024.483136	41.450688
3507.770241	549936.249390	41.455693
3507.521514	549833.870916	41.460698
3508.178658	549719.886992	41.465703
3508.014133	549616.638855	41.470708
3507.507816	549513.744715	41.475712
3507.706258	549414.913311	41.480717
3507.658218	549300.331299	41.485722
3507.600697	549199.476477	41.490727
3507.256607	549102.838796	41.495732
3506.923582	549001.522402	41.500736
3507.186339	548911.928833	41.505741
3507.099116	548825.104343	41.510746
3506.973780	548721.138612	41.515751
3507.050892	548633.734082	41.520756
3507.070289	548539.599867	41.525760
3506.913250	548442.324474	41.530765
3506.710707	548357.526000	41.535770
3506.920204	548260.141844	41.540775
3506.618607	548171.887834	41.545780
3506.816506	548084.611464	41.550784
3506.852157	548005.958653	41.555789
3506.969224	547910.195271	41.560794
3506.753675	547806.034702	41.565799
3506.464956	547726.927718	41.570804
3506.342453	547635.624760	41.575808
3506.787430	547567.264701	41.580813
3506.297221	547481.901509	41.585818
3506.084720	547391.717092	41.590823
3506.327623	547307.797561	41.595828
3505.926572	547231.722218	41.600832
3506.105536	547144.794172	41.605837
3505.841253	547063.064067	41.610842
3506.137148	546985.722086	41.615847
3506.082910	546918.441929	41.620852
3505.940418	546834.830612	41.625856
3506.082346	546762.640865	41.630861
3505.895545	546683.008419	41.635866
3506.166324	546599.180325	41.640871
3505.677620	546524.773899	41.645876
3505.865270	546453.631371	41.650880
3505.971826	546371.034306	41.655885
3505.699977	546304.438480	41.660890
3506.119717	546220.232591	41.665895
3505.862361	546157.808072	41.670900
3505.837300	546072.312467	41.675904
3505.967548	545997.303615	41.680909
3505.739439	545926.122168	41.685914
3506.026428	545836.049863	41.690919
3505.677755	545771.273745	41.695924
3505.673518	545696.485183	41.700928
3505.818948	545625.143291	41.705933
3505.642527	545556.164693	41.710938
3505.719459	545472.610633	41.715943
3505.556851	545406.546246	41.720948
3505.638630	545335.112000	41.725952
3505.553069	545256.309685	41.730957
3505.401435	545184.005543	41.735962
3505.169782	545117.296494	41.740967
3505.643923	545056.915414	41.745972
3505.259548	544984.143345	41.750976
3505.237454	544919.764651	41.755981
3505.229809	544855.282778	41.760986
3505.136366	544783.520540	41.765991
3504.883613	544721.490476	41.770996
3505.095637	544659.186580	41.776000
3504.940751	544589.897472	41.781005
3504.636540	544530.439763	41.786010
3504.845409	544465.720980	41.791015
3504.359654	544415.093551	41.796020
3504.378174	544356.741708	41.801024
3504.460373	544301.045643	41.806029
3504.437068	544248.685638	41.811034
3504.376072	544192.307152	41.816039
3504.379354	544129.530076	41.821044
3504.396308	544076.056441	41.826048
3504.467424	544023.328683	41.831053
3504.109487	543977.961325	41.836058
3504.361754	543915.446243	41.841063
3504.216455	543874.975085	41.846068
3504.362390	543820.071803	41.851072
3504.424041	543765.332305	41.856077
3504.238404	543713.045617	41.861082
3504.677896	543662.623278	41.866087
3504.382014	543609.196325	41.871092
3504.570514	543550.311224	41.876096
3504.339591	543491.742634	41.881101
3504.422181	543446.606620	41.886106
3504.688706	543387.859526	41.891111
3504.506653	543337.130158	41.896116
3504.279472	543275.441061	41.901120
3504.642910	543219.193358	41.906125
3504.371709	543174.866001	41.911130
3504.651550	543115.662808	41.916135
3504.376940	543061.576228	41.921140
3504.526201	543010.492142	41.926144
3504.345721	542942.656763	41.931149
3504.233492	542903.233753	41.936154
3504.471671	542835.735100	41.941159
3504.173848	542790.555305	41.946164
3504.224518	542735.963936	41.951168
3504.562685	542683.138668	41.956173
3503.930461	542632.275265	41.961178
3504.103626	542577.010140	41.966183
3504.140302	542526.847149	41.971188
3504.082392	542480.874280	41.976192
3504.359687	542433.742290	41.981197
3504.220332	542391.856769	41.986202
3504.060859	542335.233695	41.991207
3503.807358	542292.158186	41.996212
3503.542737	542240.783207	42.001216
3503.826474	542188.618351	42.006221
3503.994191	542152.972951	42.011226
3503.896226	542107.709285	42.016231
3504.084808	542061.746834	42.021236
3503.833167	542009.714858	42.026240
3504.291377	541952.390215	42.031245
3503.932341	541914.461511	42.036250
3504.125727	541856.272048	42.041255
3503.829594	541810.333794	42.046260
3503.780883	541770.394230	42.051264
3504.152674	541725.357955	42.056269
3503.779157	541686.726456	42.061274
3503.932672	541629.749629	42.066279
3503.874151	541581.509529	42.071284
3503.338075	541543.406006	42.076288
3503.754119	541504.097645	42.081293
3503.865979	541462.371183	42.086298
3504.111339	541409.303444	42.091303
3503.744593	541370.217103	42.096308
3504.019540	541324.288834	42.101312
3503.741057	541259.629338	42.106317
3503.957441	541226.992544	42.111322
3503.835428	541171.364670	42.116327
3503.945134	541134.819769	42.121332
3503.845685	541089.904869	42.126336
3504.061195	541046.802424	42.131341
3503.755910	541004.334331	42.136346
3503.925992	540958.722935	42.141351
3503.571974	540911.633173	42.146356
3503.783110	540862.442694	42.151360
3504.054534	540815.708083	42.156365
3503.859687	540775.737790	42.161370
3503.561843	540722.751692	42.166375
3503.515760	540678.430809	42.171380
3503.687286	540636.038224	42.176384
3503.783946	540603.770661	42.181389
3503.602868	540562.439019	42.186394
3503.263039	540509.659824	42.191399
3503.568413	540472.680028	42.196404
3503.289115	540428.847407	42.201408
3503.831741	540397.264669	42.206413
3503.770145	540356.920097	42.211418
3503.760719	540300.365158	42.216423
3503.748210	540271.786889	42.221428
3503.473242	540224.531310	42.226432
3504.034197	540172.868472	42.231437
3503.676140	540137.349511	42.236442
3503.932343	540090.513952	42.241447
3503.826420	540044.589981	42.246452
3503.513528	540005.994212	42.251456
3503.703310	539948.903519	42.256461
3503.449355	539913.719959	42.261466
3503.664597	539872.022474	42.266471
3503.348493	539835.489758	42.271476
3503.319664	539796.798828	42.276480
3503.580897	539767.824589	42.281485
3503.301843	539717.397634	42.286490
3503.560440	539678.862895	42.291495
3503.845123	539641.380695	42.296500
3503.472306	539595.245026	42.301504
3503.707132	539553.644086	42.306509
3503.075873	539518.316859	42.311514
3503.728906	539465.731047	42.316519
3503.477981	539433.212666	42.321524
3503.229782	539393.497907	42.326528
3503.379990	539351.859153	42.331533
3503.077673	539315.675037	42.336538
3503.223911	539269.759338	42.341543
3503.541672	539242.033134	42.346548
3503.309273	539206.492004	42.351552
3503.116159	539167.422145	42.356557
3502.991948	539132.769764	42.361562
3503.303508	539103.484246	42.366567
3502.893683	539062.434909	42.371572
3502.884188	539029.575990	42.376576
3503.548401	538999.128266	42.381581
3503.105671	538973.281099	42.386586
3503.107518	538932.569860	42.391591
3503.126887	538903.933222	42.396596
3502.615555	538859.980307	42.401600
3503.136576	538836.700326	42.406605
3502.851209	538798.901762	42.411610
3503.383698	538762.284223	42.416615
3503.181581	538721.151136	42.421620
3503.047956	538684.385411	42.426624
3503.154392	538646.525425	42.431629
3502.888378	538637.206572	42.436634
3503.046616	538592.594976	42.441639
3503.204386	538557.645526	42.446644
3502.985900	538522.200963	42.451648
3503.070126	538480.770918	42.456653
3503.099389	538461.139807	42.461658
3502.949446	538427.345021	42.466663
3502.935942	538396.397423	42.471668
3503.127072	538361.039644	42.476672
3503.326106	538322.962986	42.481677
3502.797276	538305.280506	42.486682
3503.165199	538250.519735	42.491687
3503.243528	538214.776501	42.496692
3503.262042	538187.849449	42.501696
3502.999449	538150.749971	42.506701
3502.933512	538122.577779	42.511706
3503.144737	538081.931887	42.516711
3503.230282	538046.589666	42.521716
3502.908318	538013.927725	42.526720
3503.008891	537979.941788	42.531725
3502.828132	537957.172020	42.536730
3502.951014	537918.703393	42.541735
3502.820202	537885.910724	42.546740
3502.821524	537856.720943	42.551744
3503.317137	537820.559381	42.556749
3503.128407	537798.897764	42.561754
3502.861737	537762.099750	42.566759
3502.851127	537727.979462	42.571764
3502.948059	537702.146383	42.576768
3503.231309	537662.293185	42.581773
3503.108896	537630.152810	42.586778
3502.986450	537594.590063	42.591783
3503.175206	537555.254515	42.596788
3503.182680	537532.957978	42.601792
3503.025018	537489.297584	42.606797
3502.802978	537462.708403	42.611802
3503.045827	537419.891360	42.616807
3503.547306	537392.937802	42.621812
3503.081597	537352.847886	42.626816
3503.066893	537309.466604	42.631821
3502.906339	537284.679329	42.636826
3502.550462	537250.913467	42.641831
3502.742459	537227.782415	42.646836
3502.704271	537202.573303	42.651840
3502.532247	537167.570705	42.656845
3502.621377	537149.488475	42.661850
3502.758692	537114.437594	42.666855
3502.944622	537090.350971	42.671860
3503.111313	537056.754927	42.676864
3503.270804	537019.234164	42.681869
3503.189758	536994.232632	42.686874
3502.979456	536958.128150	42.691879
3502.636183	536924.460124	42.696884
3502.763673	536892.480326	42.701888
3502.751009	536863.340782	42.706893
3502.870555	536840.270634	42.711898
3502.907529	536806.090147	42.716903
3502.954286	536777.645795	42.721908
3502.977249	536746.185208	42.726912
3503.124037	536706.148941	42.731917
3503.016570	536687.744332	42.736922
3502.771223	536658.036551	42.741927
3503.054709	536626.434466	42.746932
3502.697793	536591.257734	42.751936
3502.924794	536552.215140	42.756941
3502.961710	536527.747992	42.761946
3503.123518	536496.063856	42.766951
3502.926088	536461.264606	42.771956
3502.825056	536423.883303	42.776960
3502.916821	536397.041741	42.781965
3502.848630	536374.251631	42.786970
3503.099259	536331.580734	42.791975
3503.145858	536305.199005	42.796980
3503.325277	536268.830600	42.801985
3503.120187	536238.008250	42.806989
3503.093722	536201.571027	42.811994
3502.973686	536168.168271	42.816999
3502.776282	536138.552489	42.822004
3502.490259	536109.051097	42.827009
3502.685243	536071.220032	42.832013
3502.633296	536048.225478	42.837018
3502.992960	536024.814494	42.842023
3503.051993	535986.651996	42.847028
3502.863702	535957.135046	42.852033
3502.892143	535913.842989	42.857037
3502.764918	535895.691988	42.862042
3502.727588	535866.151337	42.867047
3502.857613	535836.081227	42.872052
3502.710511	535808.822592	42.877057
3502.771139	535778.813482	42.882061
3502.752377	535760.997758	42.887066
3502.778101	535720.524237	42.892071
3502.771765	535682.220001	42.897076
3502.487983	535666.559473	42.902081
3502.924779	535636.340487	42.907085
3503.014170	535605.521127	42.912090
3503.125695	535567.953245	42.917095
3503.238285	535534.361632	42.922100
3503.114978	535507.501342	42.927105
3503.017648	535473.187194	42.932109
3502.829148	535435.363594	42.937114
3502.659065	535399.097450	42.942119
3502.739402	535363.698294	42.947124
3502.981130	535342.317887	42.952129
3502.913695	535310.163131	42.957133
3502.558067	535288.120536	42.962138
3502.764496	535257.936511	42.967143
3502.971076	535222.215299	42.972148
3502.418281	535196.629285	42.977153
3502.778783	535164.558585	42.982157
3502.775863	535142.108491	42.987162
3502.688795	535115.191405	42.992167
3502.699862	535076.983332	42.997172
3502.875666	535056.569127	43.002177
3502.682745	535020.607495	43.007181
3502.302684	534988.097878	43.012186
3502.685664	534973.893230	43.017191
3502.862593	534942.504939	43.022196
3502.353991	534919.277396	43.027201
3503.138939	534889.908575	43.032205
3502.687048	534868.433963	43.037210
3502.331748	534832.648090	43.042215
3502.843160	534803.271299	43.047220
3502.867081	534775.128097	43.052225
3502.640649	534739.875641	43.057229
3502.567736	534719.549945	43.062234
3502.650206	534689.484556	43.067239
3502.832269	534663.531430	43.072244
3502.970661	534633.306190	43.077249
3503.058047	534602.132363	43.082253
3502.759559	534575.750444	43.087258
3502.311612	534545.515560	43.092263
3502.529872	534520.462631	43.097268
3502.670856	534498.140042	43.102273
3502.895744	534476.408440	43.107277
3502.503401	534442.288469	43.112282
3502.716652	534406.312257	43.117287
3502.851436	534385.047586	43.122292
3502.510333	534357.514019	43.127297
3502.773137	534336.732753	43.132301
3502.588818	534301.019476	43.137306
3502.621172	534263.862837	43.142311
3502.806936	534243.596819	43.147316
3502.409659	534219.343865	43.152321
3502.584373	534189.766369	43.157325
3502.572224	534170.940589	43.162330
3502.420770	534141.917152	43.167335
3502.473681	534112.509457	43.172340
3502.452865	534091.822273	43.177345
3502.776836	534063.882536	43.182349
3502.380952	534042.951588	43.187354
3502.670875	534008.069856	43.192359
3502.561607	533991.524315	43.197364
3502.373462	533968.698265	43.202369
3502.265563	533934.583030	43.207373
3502.306912	533909.103365	43.212378
3502.712647	533880.798113	43.217383
3502.621410	533860.473914	43.222388
3502.392722	533843.695055	43.227393
3502.349950	533805.843992	43.232397
3502.441498	533777.688091	43.237402
3502.409490	533748.846554	43.242407
3502.756064	533733.286950	43.247412
3502.331210	533704.858848	43.252417
3502.370050	533682.651431	43.257421
3502.140096	533667.533866	43.262426
3502.382528	533639.505215	43.267431
3502.431495	533618.856758	43.272436
3502.196667	533598.655178	43.277441
3502.466167	533572.333850	43.282445
3502.448112	533545.251716	43.287450
3502.151950	533520.327244	43.292455
3502.741535	533493.402164	43.297460
3502.392983	533470.298130	43.302465
3502.426453	533444.869121	43.307469
3502.340620	533431.188833	43.312474
3502.139455	533402.121124	43.317479
3502.212268	533376.534826	43.322484
3502.241391	533363.289676	43.327489
3502.317342	533335.789719	43.332493
3502.374507	533316.196740	43.337498
3502.266826	533296.478349	43.342503
3502.686842	533271.895054	43.347508
3502.309746	533250.909552	43.352513
3502.459759	533225.361287	43.357517
3502.525574	533200.681940	43.362522
3502.387722	533176.739072	43.367527
3502.628603	533155.304834	43.372532
3502.240659	533135.076011	43.377537
3502.178429	533107.345345	43.382541
3502.414762	533085.408244	43.387546
3502.683054	533064.120626	43.392551
3502.855889	533036.554612	43.397556
3502.576240	533015.251489	43.402561
3502.622053	532981.713970	43.407565
3502.713594	532957.936386	43.412570
3502.313594	532925.172939	43.417575
3502.774688	532907.429640	43.422580
3502.313548	532873.920384	43.427585
3502.805947	532847.663592	43.432589
3502.341919	532828.654445	43.437594
3502.728080	532795.869028	43.442599
3502.894639	532777.365838	43.447604
3502.338946	532751.473335	43.452609
3502.765726	532712.488723	43.457613
3502.906275	532687.545035	43.462618
3502.359327	532652.890577	43.467623
3502.497006	532633.686815	43.472628
3502.430707	532614.967893	43.477633
3502.361179	532575.657323	43.482637
3502.147294	532558.068930	43.487642
3502.246588	532524.018430	43.492647
3502.401903	532518.405633	43.497652
3502.168962	532507.516386	43.502657
3502.249352	532485.099060	43.507661
3502.538402	532458.067560	43.512666
3502.247814	532428.105317	43.517671
3502.473122	532404.658339	43.522676
3502.165382	532392.421234	43.527681
3502.161231	532364.579245	43.532685
3502.382849	532333.681156	43.537690
3502.428242	532320.180668	43.542695
3502.471127	532294.244452	43.547700
3502.332050	532278.859378	43.552705
3502.192187	532240.616061	43.557709
3502.712734	532229.609329	43.562714
3502.432096	532201.558271	43.567719
3502.624096	532173.181859	43.572724
3502.661360	532149.763684	43.577729
3502.476104	532122.905993	43.582733
3502.554967	532101.797326	43.587738
3502.406192	532076.142246	43.592743
3502.567567	532041.829075	43.597748
3502.177519	532018.829606	43.602753
3502.164442	531988.772814	43.607757
3502.402560	531992.058818	43.612762
3502.274292	531958.545746	43.617767
3502.287836	531937.195226	43.622772
3502.421045	531909.481937	43.627777
3502.456177	531891.199339	43.632781
3502.184694	531859.671954	43.637786
3501.951832	531838.158214	43.642791
3502.102256	531817.893907	43.647796
3501.896442	531809.467024	43.652801
3502.138295	531793.065438	43.657805
3502.052036	531775.002968	43.662810
3501.919781	531759.062360	43.667815
3502.043088	531737.190925	43.672820
3502.083455	531726.762000	43.677825
3502.342166	531701.949087	43.682829
3502.256243	531681.469591	43.687834
3502.361336	531652.400653	43.692839
3502.561976	531633.789832	43.697844
3502.196144	531606.858472	43.702849
3502.380089	531578.884829	43.707853
3502.335287	531559.053309	43.712858
3502.234489	531534.296021	43.717863
3502.179944	531528.715456	43.722868
3501.986416	531506.188014	43.727873
3502.265138	531472.761412	43.732877
3501.961250	531463.292179	43.737882
3501.926769	531443.760989	43.742887
3502.180243	531421.566656	43.747892
3502.077522	531410.253408	43.752897
3502.432478	531385.777381	43.757901
3502.233666	531350.259634	43.762906
3502.631580	531333.228958	43.767911
3502.404498	531317.604680	43.772916
3502.148303	531285.167180	43.777921
3502.365112	531269.121301	43.782925
3502.262350	531245.672937	43.787930
3502.336935	531225.268452	43.792935
3502.036523	531195.758070	43.797940
3502.261133	531187.666628	43.802945
3502.573341	531164.052837	43.807949
3502.230330	531145.576271	43.812954
3502.061680	531121.281934	43.817959
3502.192470	531106.256303	43.822964
3501.923430	531082.934228	43.827969
3502.462587	531059.133872	43.832973
3502.220176	531040.137967	43.837978
3502.017453	531016.805454	43.842983
3502.444248	530987.382852	43.847988
3502.235397	530980.667929	43.852993
3502.183920	530944.521905	43.857997
3502.250657	530935.447796	43.863002
3502.196780	530903.229633	43.868007
3502.325917	530889.764984	43.873012
3502.415412	530866.588145	43.878017
3502.292280	530841.128058	43.883021
3502.227862	530823.010515	43.888026
3501.996401	530803.055829	43.893031
3502.112325	530779.371179	43.898036
3502.183955	530769.238750	43.903041
3502.738040	530741.759614	43.908045
3502.716448	530714.772841	43.913050
3502.378725	530683.101851	43.918055
3501.925695	530654.318960	43.923060
3502.147806	530639.882842	43.928065
3502.379943	530627.207576	43.933069
3502.048109	530607.318565	43.938074
3501.985900	530576.057637	43.943079
3502.426840	530552.372355	43.948084
3502.423025	530540.438697	43.953089
3502.436714	530510.072198	43.958093
3502.266873	530487.287531	43.963098
3502.283621	530481.342934	43.968103
3502.431095	530447.783068	43.973108
3502.263024	530424.947661	43.978113
3502.426120	530395.917255	43.983117
3502.422415	530374.164013	43.988122
3502.163754	530354.515010	43.993127
3502.384749	530338.819831	43.998132
3502.147483	530315.642507	44.003137
3502.275449	530289.689065	44.008141
3502.210075	530268.247381	44.013146
3502.431826	530248.422747	44.018151
3502.694498	530224.412118	44.023156
3502.269845	530192.098828	44.028161
3502.283230	530175.428625	44.033165
3502.145467	530144.329494	44.038170
3501.977940	530132.622366	44.043175
3502.344147	530111.818264	44.048180
3502.219277	530095.068759	44.053185
3502.305645	530061.567769	44.058189
3502.273253	530048.328820	44.063194
3502.158150	530027.750554	44.068199
3502.315063	529996.252714	44.073204
3502.414700	529984.201735	44.078209
3502.493189	529953.370643	44.083213
3502.425257	529932.684172	44.088218
3502.397564	529911.789976	44.093223
3502.278871	529888.794875	44.098228
3502.400804	529862.690452	44.103233
3502.468410	529834.429031	44.108237
3502.673028	529818.332914	44.113242
3502.522939	529791.817455	44.118247
3502.483259	529762.615768	44.123252
3502.088751	529739.814401	44.128257
3502.160191	529715.228295	44.133261
3502.218357	529695.377923	44.138266
3502.211112	529671.106131	44.143271
3502.212408	529651.566695	44.148276
3501.836603	529630.625503	44.153281
3502.276113	529623.758628	44.158285
3502.392451	529594.884801	44.163290
3502.007968	529579.081497	44.168295
3502.317182	529548.364627	44.173300
3502.264023	529540.013238	44.178305
3502.411062	529503.832341	44.183309
3502.407491	529490.537985	44.188314
3502.223118	529469.768184	44.193319
3502.661886	529446.937357	44.198324
3502.677589	529423.014052	44.203329
3502.236670	529383.096978	44.208333
3502.320124	529366.767363	44.213338
3502.390986	529335.482766	44.218343
3502.273602	529315.105176	44.223348
3502.105013	529291.562830	44.228353
3502.391588	529271.223032	44.233357
3502.221028	529242.896678	44.238362
3502.211557	529235.293703	44.243367
3502.328543	529196.397173	44.248372
3502.282599	529191.066073	44.253377
3502.367621	529172.469745	44.258381
3502.421727	529149.396097	44.263386
3502.220867	529135.427030	44.268391
3502.544043	529102.088182	44.273396
3502.366969	529087.662115	44.278401
3502.235031	529056.257329	44.283405
3501.905760	529030.372546	44.288410
3502.189279	529015.270391	44.293415
3502.171446	528994.725728	44.298420
3502.163069	528972.719081	44.303425
3502.216294	528948.789073	44.308429
3502.349470	528928.120085	44.313434
3501.953579	528908.087371	44.318439
3502.311599	528881.843536	44.323444
3501.733303	528863.652163	44.328449
3501.647977	528851.578565	44.333453
3501.937039	528812.301588	44.338458
3501.586847	528809.938675	44.343463
3502.148779	528798.167204	44.348468
3502.006980	528776.886059	44.353473
3502.200881	528772.625435	44.358477
3501.988897	528752.110605	44.363482
3502.063036	528741.321510	44.368487
3502.234794	528702.817895	44.373492
3502.445595	528689.187193	44.378497
3502.209297	528662.330329	44.383501
3502.891987	528642.884810	44.388506
3502.215959	528629.946037	44.393511
3502.049150	528601.970257	44.398516
3502.203487	528574.750249	44.403521
3502.264118	528563.056577	44.408525
3502.005721	528538.519597	44.413530
3501.852417	528527.161362	44.418535
3502.051383	528494.444662	44.423540
3501.725179	528488.602893	44.428545
3501.752358	528478.374886	44.433549
3501.644912	528447.720283	44.438554
3501.956411	528438.606361	44.443559
3502.157476	528434.848147	44.448564
3501.865409	528407.848351	44.453569
3501.683283	528401.782668	44.458573
3502.056328	528382.133132	44.463578
3502.171665	528363.984217	44.468583
3502.127227	528344.298863	44.473588
3502.076253	528322.851758	44.478593
3502.249389	528313.003822	44.483597
3502.240193	528280.419711	44.488602
3501.819332	528268.448155	44.493607
3502.328293	528240.467176	44.498612
3502.056593	528231.192042	44.503617
3501.944605	528208.746962	44.508621
3502.234176	528187.649560	44.513626
3501.729984	528170.452980	44.518631
3502.159406	528139.260836	44.523636
3502.041951	528138.221428	44.528641
3502.269618	528117.032816	44.533645
3502.154634	528100.581415	44.538650
3501.972369	528079.960182	44.543655
3502.247636	528052.569184	44.548660
3502.280000	528039.821783	44.553665
3501.842555	528016.520450	44.558669
3501.997219	527993.882414	44.563674
3501.753142	527977.350216	44.568679
3502.176442	527966.254327	44.573684
3501.623737	527953.597886	44.578689
3501.419299	527927.590775	44.583693
3501.741743	527933.231861	44.588698
3501.722687	527908.152806	44.593703
3502.144346	527883.760607	44.598708
3502.132568	527876.409033	44.603713
3501.836274	527850.013138	44.608717
3502.071475	527830.333865	44.613722
3502.130748	527813.502428	44.618727
3501.931014	527796.409079	44.623732
3502.036096	527787.427562	44.628737
3502.181021	527758.091963	44.633741
3502.252658	527754.051501	44.638746
3501.671262	527730.721696	44.643751
3501.899717	527711.446226	44.648756
3501.844076	527701.079406	44.653761
3502.159011	527675.494639	44.658765
3502.059439	527663.119969	44.663770
3501.975784	527648.577053	44.668775
3502.030337	527618.499710	44.673780
3501.969199	527613.019234	44.678785
3501.808775	527592.343473	44.683789
3502.219558	527576.615469	44.688794
3502.103067	527550.090260	44.693799
3502.033903	527529.249098	44.698804
3501.892781	527524.939472	44.703809
3502.135407	527506.114800	44.708813
3502.273198	527484.939161	44.713818
3502.200526	527467.624145	44.718823
3502.036326	527449.265636	44.723828
3501.901516	527434.075669	44.728833
3501.880528	527418.968707	44.733837
3502.117157	527392.942273	44.738842
3501.752461	527384.688363	44.743847
3502.008001	527360.975827	44.748852
3501.902406	527344.068713	44.753857
3501.710533	527333.068023	44.758861
3501.696027	527300.633421	44.763866
3501.803543	527291.147510	44.768871
3501.797538	527280.974107	44.773876
3502.016847	527266.031049	44.778881
3501.568612	527246.860203	44.783885
3501.562582	527239.356276	44.788890
3501.582542	527239.202037	44.793895
3501.740672	527213.993356	44.798900
3501.855402	527207.528350	44.803905
3501.625506	527192.302533	44.808909
3501.868828	527173.829858	44.813914
3502.075195	527174.301399	44.818919
3502.223173	527147.583122	44.823924
3502.253386	527121.689012	44.828929
3501.863968	527099.184478	44.833933
3502.411111	527075.980110	44.838938
3501.756441	527063.086834	44.843943
3501.913183	527048.505848	44.848948
3501.984125	527041.493518	44.853953
3501.829331	527021.772994	44.858957
3502.111009	526991.155192	44.863962
3501.901379	526991.238154	44.868967
3502.178902	526968.931827	44.873972
3502.370248	526947.092196	44.878977
3501.954107	526923.936723	44.883981
3502.253571	526898.755817	44.888986
3502.117323	526869.864957	44.893991
3502.170605	526857.163530	44.898996
3502.078842	526850.982330	44.904001
3502.016789	526822.029451	44.909005
3501.982847	526804.909018	44.914010
3501.709139	526786.566629	44.919015
3502.103275	526769.228427	44.924020
3502.101628	526752.959188	44.929025
3501.762683	526740.318684	44.934029
3501.964950	526728.047278	44.939034
3501.951609	526704.627260	44.944039
3501.971154	526690.470190	44.949044
3501.597399	526676.777269	44.954049
3501.639165	526651.333773	44.959053
3501.858420	526646.967780	44.964058
3501.919369	526638.999758	44.969063
3501.514319	526624.203504	44.974068
3502.105146	526612.224120	44.979073
3501.860192	526589.595496	44.984077
3502.100907	526564.120874	44.989082
3501.983076	526561.217685	44.994087
3502.069304	526528.866258	44.999092
3501.914430	526525.011782	45.004097
3501.722056	526507.160056	45.009101
3501.871554	526480.893536	45.014106
3501.877689	526476.107313	45.019111
3501.999915	526456.393209	45.024116
3501.839836	526436.773378	45.029121
3501.878845	526429.060499	45.034125
3502.244287	526411.524810	45.039130
3502.009473	526402.645618	45.044135
3502.266299	526373.742879	45.049140
3502.154816	526355.525763	45.054145
3502.001743	526333.235002	45.059149
3502.395089	526324.459494	45.064154
3501.887944	526290.487190	45.069159
3501.749995	526279.829833	45.074164
3501.899205	526261.118674	45.079169
3501.704825	526248.152971	45.084173
3501.878097	526231.049924	45.089178
3501.661471	526226.801994	45.094183
3501.811238	526196.505117	45.099188
3502.131918	526181.242831	45.104193
3501.929819	526166.263367	45.109197
3502.151075	526150.915773	45.114202
3501.849565	526145.421722	45.119207
3501.786735	526110.170881	45.124212
3502.146747	526096.514292	45.129217
3501.964012	526085.561514	45.134221
3502.032171	526069.280574	45.139226
3501.837880	526065.734332	45.144231
3501.789084	526035.568731	45.149236
3501.853897	526015.510299	45.154241
3502.161923	526005.488540	45.159245
3501.532423	525975.413167	45.164250
3501.759875	525972.103509	45.169255
3501.903175	525960.848028	45.174260
3501.948951	525938.727153	45.179265
3502.118322	525924.193340	45.184269
3502.102427	525910.242444	45.189274
3502.117759	525901.021750	45.194279
3502.098421	525873.017241	45.199284
3501.890299	525856.124180	45.204289
3501.920317	525839.345160	45.209293
3502.129730	525811.909406	45.214298
3501.982357	525806.139360	45.219303
3501.836505	525773.771834	45.224308
3501.964826	525768.915969	45.229313
3502.036543	525754.246046	45.234317
3501.910507	525724.998486	45.239322
3501.690223	525721.959934	45.244327
3502.187301	525699.415816	45.249332
3502.165659	525685.616700	45.254337
3501.663211	525662.321327	45.259341
3501.864601	525638.714890	45.264346
3501.666851	525643.833419	45.269351
3502.038152	525618.941154	45.274356
3501.961286	525603.034830	45.279361
3501.660105	525596.885634	45.284365
3501.924849	525574.830827	45.289370
3501.867206	525558.871085	45.294375
3501.953333	525553.769836	45.299380
3501.946785	525518.508667	45.304385
3501.577205	525517.407534	45.309389
3501.901477	525496.703449	45.314394
3501.968286	525481.379117	45.319399
3501.925125	525463.502767	45.324404
3501.812388	525456.518184	45.329409
3501.753865	525437.082570	45.334413
3502.086066	525416.226001	45.339418
3501.652766	525404.707152	45.344423
3501.831945	525388.005101	45.349428
3502.077220	525377.841511	45.354433
3502.089068	525352.903935	45.359437
3502.025569	525336.441084	45.364442
3502.086204	525314.266483	45.369447
3502.041953	525295.080317	45.374452
3502.085572	525278.147347	45.379457
3502.085418	525262.379804	45.384461
3502.231532	525244.624833	45.389466
3501.597728	525220.543114	45.394471
3501.766464	525217.746164	45.399476
3501.893851	525200.800060	45.404481
3501.678014	525176.653221	45.409485
3501.995766	525158.518795	45.414490
3501.868128	525152.543890	45.419495
3502.026143	525123.200428	45.424500
3501.766811	525121.477592	45.429505
3502.111113	525096.487801	45.434509
3502.141796	525074.015204	45.439514
3501.898163	525068.813955	45.444519
3502.213215	525047.354963	45.449524
3501.920536	525033.798854	45.454529
3502.095808	525010.951016	45.459533
3502.274395	524985.835676	45.464538
3501.813661	524971.600382	45.469543
3501.994882	524945.577777	45.474548
3501.977566	524941.449549	45.479553
3502.133033	524908.478884	45.484557
3502.036800	524901.642572	45.489562
3501.745627	524878.967845	45.494567
3501.815260	524871.954576	45.499572
3501.850117	524859.455615	45.504577
3501.539275	524843.836678	45.509581
3501.694140	524826.029411	45.514586
3502.185420	524825.549916	45.519591
3501.888360	524793.707306	45.524596
3501.890117	524784.588706	45.529601
3501.374823	524770.412064	45.534605
3501.669916	524744.371346	45.539610
3501.909487	524749.976317	45.544615
3501.875261	524735.170625	45.549620
3502.104381	524712.817672	45.554625
3502.025223	524704.114629	45.559629
3502.225352	524669.070939	45.564634
3501.957987	524653.747280	45.569639
3501.842329	524630.792929	45.574644
3501.959557	524608.860238	45.579649
3501.582873	524602.772706	45.584653
3501.842720	524575.679205	45.589658
3501.613003	524579.291771	45.594663
3501.768924	524564.607435	45.599668
3502.008517	524537.013226	45.604673
3502.002106	524518.928376	45.609677
3502.331444	524504.670394	45.614682
3502.023327	524492.325217	45.619687
3502.353398	524471.366748	45.624692
3501.888399	524442.975174	45.629697
3501.997283	524431.623002	45.634701
3502.006639	524409.051845	45.639706
3502.091319	524394.630302	45.644711
3502.153054	524374.620257	45.649716
3501.776784	524360.723817	45.654721
3501.990546	524348.146158	45.659725
3502.269041	524330.873162	45.664730
3502.138277	524317.190368	45.669735
3502.326011	524287.739687	45.674740
3502.368318	524259.470297	45.679745
3502.019847	524240.581850	45.684749
3502.251859	524225.532645	45.689754
3501.736524	524207.073152	45.694759
3501.877382	524178.889014	45.699764
3501.967582	524167.388386	45.704769
3501.856647	524147.203352	45.709773
3502.079883	524129.636416	45.714778
3501.803347	524118.696613	45.719783
3501.748353	524089.585546	45.724788
3502.178595	524085.538548	45.729793
3501.903942	524067.343688	45.734797
3502.100380	524049.277017	45.739802
3502.133351	524035.316554	45.744807
3501.951512	524012.976002	45.749812
3502.297699	523994.684433	45.754817
3501.912242	523961.644465	45.759821
3502.009239	523889.433948	45.764826
3501.749198	523781.810326	45.769831
3501.657586	523610.426826	45.774836
3501.685984	523409.296792	45.779841
3500.706556	523161.212105	45.784845
3500.526854	522861.505417	45.789850
3500.008578	522518.261004	45.794855
3499.938538	522112.659383	45.799860
3499.365744	521678.654005	45.804865
3498.552928	521186.369895	45.809869
3498.162530	520661.549159	45.814874
3497.559787	520090.277044	45.819879
3496.801662	519465.080058	45.824884
3496.010406	518801.454915	45.829889
3494.927241	518085.626092	45.834893
3494.229547	517334.365786	45.839898
3493.186744	516543.950955	45.844903
3492.437850	515695.320929	45.849908
3491.118888	514802.917252	45.854913
3489.924522	513889.059420	45.859917
3488.774431	512922.444322	45.864922
3487.812266	511919.376506	45.869927
3486.395783	510867.038582	45.874932
3484.991883	509771.247688	45.879937
3483.355594	508650.845000	45.884941
3482.175140	507472.023492	45.889946
3480.623692	506277.977841	45.894951
3478.994850	505027.643603	45.899956
3477.394136	503750.757966	45.904961
3475.284088	502436.145783	45.909965
3473.877845	501072.254306	45.914970
3472.212133	499695.204009	45.919975
3470.453093	498272.814747	45.924980
3468.822547	496819.425779	45.929985
3467.119287	495326.578916	45.934989
3465.052885	493795.923928	45.939994
3462.947956	492242.951573	45.944999
3460.998514	490656.465494	45.950004
3459.091012	489031.524443	45.955009
3457.042173	487385.773588	45.960013
3454.689280	485698.369956	45.965018
3452.735889	483990.966046	45.970023
3450.088071	482247.255220	45.975028
3448.150587	480481.157035	45.980033
3445.869361	478682.165982	45.985037
3443.655069	476863.653031	45.990042
3441.428291	475012.634257	45.995047
3438.771816	473118.396729	46.000052
3436.317922	471221.176497	46.005057
3433.314311	469302.786117	46.010061
3431.248083	467344.731726	46.015066
3428.845549	465382.604800	46.020071
3426.270791	463383.044862	46.025076
3423.711615	461363.768883	46.030081
3421.162402	459320.320323	46.035085
3418.277323	457251.936933	46.040090
3415.852155	455169.925874	46.045095
3413.103962	453063.473619	46.050100
3410.623004	450934.557433	46.055105
3407.189707	448780.678311	46.060109
3404.892674	446608.542829	46.065114
3401.875960	444430.133632	46.070119
3398.905036	442229.176158	46.075124
3396.383587	439996.130518	46.080129
3393.049922	437757.121020	46.085133
3390.213393	435495.327091	46.090138
3387.127622	433227.327303	46.095143
3384.297437	430933.077900	46.100148
3381.244336	428628.814483	46.105153
3377.798090	426303.665483	46.110157
3374.411296	423958.316786	46.115162
3371.537126	421614.900147	46.120167
3368.790843	419249.496274	46.125172
3365.664490	416876.328193	46.130177
3362.330587	414486.900288	46.135181
3358.954667	412077.076361	46.140186
3356.029826	409667.523748	46.145191
3352.549838	407233.442298	46.150196
3349.235440	404800.490343	46.155201
3345.824923	402349.886807	46.160205
3342.621871	399888.991816	46.165210
3339.452960	397423.618816	46.170215
3335.779441	394940.859588	46.175220
3332.439228	392445.404790	46.180225
3328.872234	389952.217173	46.185229
3325.636048	387439.965210	46.190234
3322.103519	384927.050958	46.195239
3318.504687	382407.500550	46.200244
3315.334583	379871.715901	46.205249
3311.979771	377340.363765	46.210253
3308.748953	374787.798441	46.215258
3305.030913	372237.305390	46.220263
3301.344017	369667.443489	46.225268
3297.818348	367086.448621	46.230273
3294.397406	364527.997838	46.235277
3290.734763	361944.255038	46.240282
3287.366657	359354.601138	46.245287
3283.282217	356757.468006	46.250292
3279.755259	354166.156648	46.255297
3275.919328	351578.723276	46.260301
3272.824263	348978.790694	46.265306
3268.736462	346361.443648	46.270311
3265.221166	343762.467086	46.275316
3261.410467	341149.864205	46.280321
3257.810069	338535.077204	46.285325
3254.065496	335912.646622	46.290330
3249.996955	333294.582220	46.295335
3246.707036	330684.126028	46.300340
3243.173829	328057.787149	46.305345
3239.356953	325429.284309	46.310349
3235.638932	322806.270278	46.315354
3231.523546	320180.304947	46.320359
3227.541210	317548.078453	46.325364
3223.913891	314924.673551	46.330369
3220.204010	312307.212630	46.335373
3216.260663	309685.698432	46.340378
3212.245058	307055.656155	46.345383
3208.751675	304433.538774	46.350388
3204.806191	301807.439780	46.355393
3200.624347	299193.593459	46.360397
3196.699182	296574.391809	46.365402
3193.125216	293963.671096	46.370407
3188.942179	291358.200660	46.375412
3185.304129	288747.215928	46.380417
3181.090801	286143.623788	46.385421
3177.713909	283528.039373	46.390426
3173.808469	280937.874606	46.395431
3169.442584	278348.454696	46.400436
3165.963318	275744.093886	46.405441
3161.415427	273166.577043	46.410445
3158.059932	270582.431864	46.415450
3153.644000	267991.426926	46.420455
3149.622093	265426.723106	46.425460
3145.870087	262845.717839	46.430465
3141.697382	260279.258316	46.435469
3137.880685	257718.417587	46.440474
3133.727547	255165.574380	46.445479
3129.525601	252611.367607	46.450484
3125.460024	250081.545293	46.455489
3121.490876	247554.980677	46.460493
3117.541047	245028.328078	46.465498
3113.520149	242510.875929	46.470503
3109.041971	239997.747662	46.475508
3105.216316	237492.467529	46.480513
3101.265301	235018.795668	46.485517
3097.160578	232526.388725	46.490522
3092.870902	230051.650295	46.495527
3088.761015	227586.632094	46.500532
3085.032795	225121.806458	46.505537
3080.778492	222685.894575	46.510541
3076.609165	220233.470015	46.515546
3072.192514	217802.536845	46.520551
3068.396267	215385.959385	46.525556
3064.022480	212966.430369	46.530561
3060.069121	210582.611792	46.535565
3055.983144	208182.331590	46.540570
3051.228035	205810.118475	46.545575
3046.662343	203455.297641	46.550580
3042.860934	201103.596970	46.555585
3038.345765	198764.875972	46.560589
3034.248188	196438.706486	46.565594
3030.079326	194137.900043	46.570599
3025.337276	191843.997548	46.575604
3021.257939	189570.000119	46.580609
3016.788050	187316.990094	46.585613
3012.577612	185069.945974	46.590618
3008.190676	182842.968286	46.595623
3003.569837	180620.407723	46.600628
2998.904444	178424.618374	46.605633
2994.405273	176260.291139	46.610637
2989.932418	174105.373369	46.615642
2985.317928	171973.055753	46.620647
2980.716670	169860.666937	46.625652
2975.782677	167770.399899	46.630657
2971.124508	165705.457042	46.635661
2966.634831	163658.676069	46.640666
2961.099974	161642.185276	46.645671
2956.351729	159673.950377	46.650676
2951.590133	157716.191189	46.655681
2946.150800	155800.180147	46.660685
2941.047074	153886.406913	46.665690
2935.422927	151977.258710	46.670695
2929.850990	150166.690061	46.675700
2923.939111	148404.234526	46.680705
2918.044288	146687.211831	46.685709
2911.742152	145023.561175	46.690714
2904.921155	143427.788458	46.695719
2897.866358	141882.819687	46.700724
2891.037638	140398.325379	46.705729
2884.445125	138982.683510	46.710733
2877.569122	137620.728002	46.715738
2871.274749	136336.530271	46.720743
2865.237297	135103.088429	46.725748
2859.396614	133920.700744	46.730753
2853.367049	132793.099979	46.735757
2848.443137	131710.171367	46.740762
2843.412195	130678.168255	46.745767
2837.886747	129681.120159	46.750772
2833.205034	128728.254768	46.755777
2828.354013	127810.924987	46.760781
2824.017509	126912.080125	46.765786
2819.828688	126057.888441	46.770791
2815.259726	125222.864668	46.775796
2811.104393	124414.210124	46.780801
2806.749317	123636.762726	46.785805
2802.904443	122868.891363	46.790810
2798.799266	122122.988168	46.795815
2794.980502	121395.342416	46.800820
2791.135267	120680.825919	46.805825
2787.691611	119980.986504	46.810829
2783.652122	119280.782010	46.815834
2780.102945	118610.665193	46.820839
2776.084174	117946.686290	46.825844
2772.600119	117284.772173	46.830849
2768.513707	116648.662463	46.835853
2764.784983	116003.721345	46.840858
2761.270092	115389.135610	46.845863
2757.119125	114774.900696	46.850868
2753.537117	114155.832074	46.855873
2749.295154	113561.467307	46.860877
2746.137074	112970.554588	46.865882
2742.075634	112386.429097	46.870887
2738.080289	111824.921571	46.875892
2734.605713	111256.679645	46.880897
2730.739981	110702.950671	46.885901
2726.930182	110147.835872	46.890906
2723.225759	109607.105122	46.895911
2719.437437	109078.829401	46.900916
2715.768398	108543.194939	46.905921
2712.183854	108034.151046	46.910925
2709.065545	107510.015636	46.915930
2705.271472	106994.676046	46.920935
2701.482143	106480.424026	46.925940
2698.276377	105966.533876	46.930945
2694.389155	105463.346631	46.935949
2691.444785	104955.837974	46.940954
2687.819187	104443.841383	46.945959
2684.316156	103946.527922	46.950964
2680.858585	103440.062724	46.955969
2677.574047	102936.781494	46.960973
2674.021891	102430.409989	46.965978
2670.697247	101922.472872	46.970983
2667.113506	101421.345887	46.975988
2663.812291	100918.898883	46.980993
2660.314669	100420.341341	46.985997
2657.374084	99911.549611	46.991002
2654.100078	99408.867573	46.996007
2650.410805	98898.873827	47.001012
2647.128989	98378.187159	47.006017
2643.693363	97868.272056	47.011021
2640.253477	97354.845454	47.016026
2637.001277	96843.011969	47.021031
2633.442099	96326.163909	47.026036
2630.234316	95802.140373	47.031041
2626.690897	95280.948193	47.036045
2623.683143	94752.145665	47.041050
2620.027781	94234.559340	47.046055
2616.504908	93708.256539	47.051060
2613.344278	93186.010771	47.056065
2609.741386	92648.098869	47.061069
2606.582401	92120.191060	47.066074
2603.090642	91593.805449	47.071079
2599.617362	91054.897761	47.076084
2596.395895	90525.553557	47.081089
2592.896064	89980.100239	47.086093
2589.808297	89444.884240	47.091098
2586.026479	88894.196430	47.096103
2582.144162	88361.499479	47.101108
2578.939216	87801.454796	47.106113
2575.489805	87262.586586	47.111117
2571.936340	86715.816937	47.116122
2568.433311	86166.394511	47.121127
2565.273883	85623.420687	47.126132
2561.919250	85070.832630	47.131137
2558.380171	84517.508948	47.136141
2554.702636	83966.097536	47.141146
2551.150171	83414.651876	47.146151
2547.382223	82862.958252	47.151156
2544.346673	82311.618653	47.156161
2540.939360	81754.060067	47.161165
2537.525796	81192.207526	47.166170
2534.089135	80640.658186	47.171175
2530.640717	80084.980886	47.176180
2527.139979	79519.085664	47.181185
2523.588682	78957.248742	47.186189
2519.747623	78385.409414	47.191194
2516.299077	77826.183171	47.196199
2512.831533	77262.996144	47.201204
2509.410789	76694.847794	47.206209
2505.754020	76137.682395	47.211213
2502.511460	75571.358554	47.216218
2498.805462	75006.629898	47.221223
2495.104769	74449.226785	47.226228
2492.227875	73888.595917	47.231233
2488.884730	73319.592319	47.236237
2485.627682	72747.705041	47.241242
2482.225578	72168.449899	47.246247
2478.868680	71593.047756	47.251252
2475.133157	71011.101895	47.256257
2471.626609	70429.438050	47.261261
2467.969798	69850.426050	47.266266
2464.671998	69277.071721	47.271271
2461.207788	68699.185399	47.276276
2458.201533	68119.882299	47.281281
2454.614489	67524.622865	47.286285
2450.980946	66944.428274	47.291290
2447.646440	66352.279841	47.296295
2443.751215	65772.216146	47.301300
2440.394658	65174.557432	47.306305
2436.994133	64597.731515	47.311309
2433.556771	64007.532702	47.316314
2429.762989	63424.245004	47.321319
2426.072267	62825.380458	47.326324
2422.991128	62230.046568	47.331329
2419.374663	61655.111936	47.336333
2415.801698	61054.031647	47.341338
2412.623764	60456.191767	47.346343
2408.897270	59872.755245	47.351348
2405.547917	59276.284451	47.356353
2401.817226	58674.646257	47.361357
2398.604232	58077.168413	47.366362
2395.119534	57487.260305	47.371367
2391.321369	56892.212530	47.376372
2388.187752	56295.921336	47.381377
2384.511435	55694.209594	47.386381
2381.250803	55092.898828	47.391386
2378.049285	54494.449067	47.396391
2374.400136	53894.307735	47.401396
2371.080811	53285.883103	47.406401
2367.600206	52682.339720	47.411405
2363.978909	52086.744424	47.416410
2360.821263	51476.165802	47.421415
2356.957181	50865.243757	47.426420
2353.815186	50250.489309	47.431425
2350.069924	49646.729807	47.436429
2346.429874	49042.950767	47.441434
2342.963779	48428.676062	47.446439
2339.286179	47813.581878	47.451444
2336.031532	47198.470223	47.456449
2332.509627	46595.213352	47.461453
2329.177347	45979.563438	47.466458
2325.601435	45364.082434	47.471463
2321.943251	44757.243134	47.476468
2318.781316	44144.153767	47.481473
2315.165767	43540.308761	47.486477
2311.427207	42915.199357	47.491482
2308.024121	42295.876434	47.496487
2304.562612	41684.740619	47.501492
2301.024109	41063.894581	47.506497
2297.298801	40451.439251	47.511501
2293.533155	39838.766463	47.516506
2290.209561	39219.321643	47.521511
2286.569848	38618.139274	47.526516
2283.391905	38003.214282	47.531521
2279.901854	37398.536749	47.536525
2276.674346	36773.771273	47.541530
2272.975507	36166.580882	47.546535
2269.201058	35553.891940	47.551540
2265.404405	34941.566420	47.556545
2261.813281	34338.233836	47.561549
2257.994535	33738.769679	47.566554
2254.741650	33121.785248	47.571559
2250.724539	32520.276092	47.576564
2247.400862	31909.518045	47.581569
2244.134200	31319.170176	47.586573
2240.261162	30727.646930	47.591578
2236.746827	30142.441143	47.596583
2232.356948	29545.949575	47.601588
2228.368540	28974.234890	47.606593
2223.846750	28418.841460	47.611597
2219.802848	27867.932136	47.616602
2215.677218	27322.962369	47.621607
2211.655016	26792.691408	47.626612
2207.724204	26259.163298	47.631617
2203.605886	25736.056820	47.636621
2199.854984	25227.719934	47.641626
2196.446340	24719.881160	47.646631
2192.339136	24223.992383	47.651636
2188.584746	23725.685223	47.656641
2184.915263	23244.837144	47.661645
2181.080287	22763.760359	47.666650
2178.107845	22280.812552	47.671655
2174.219415	21809.903075	47.676660
2171.051044	21322.289744	47.681665
2167.201893	20859.739491	47.686669
2163.376547	20395.644503	47.691674
2160.159724	19928.216361	47.696679
2156.462621	19465.181243	47.701684
2153.498328	19000.947293	47.706689
2149.971623	18539.516414	47.711693
2146.424224	18073.267200	47.716698
2142.706024	17613.129503	47.721703
2139.012982	17148.727048	47.726708
2135.330314	16686.240407	47.731713
2132.124803	16232.670728	47.736717
2128.799064	15782.366518	47.741722
2125.122107	15320.985231	47.746727
2121.776397	14878.830150	47.751732
2118.538773	14413.745354	47.756737
2114.729319	13970.518339	47.761741
2111.268234	13510.945565	47.766746
2108.044656	13056.672083	47.771751
2104.489948	12604.474527	47.776756
2101.309777	12161.476803	47.781761
2097.548200	11704.593799	47.786765
2093.763174	11253.626309	47.791770
2090.525944	10797.392862	47.796775
2086.987276	10350.150464	47.801780
2083.830481	9895.635851	47.806785
2079.786388	9445.575266	47.811789
2076.457840	8998.433871	47.816794
2072.887025	8548.916409	47.821799
2069.388573	8100.265831	47.826804
2065.351547	7656.172657	47.831809
2061.629442	7217.025975	47.836813
2058.025022	6778.577221	47.841818
2054.762698	6339.582482	47.846823
2050.976251	5909.202452	47.851828
2047.346979	5474.118056	47.856833
2043.903686	5044.230318	47.861837
2040.282992	4630.354789	47.866842
2036.322295	4198.029614	47.871847
2032.584698	3783.659940	47.876852
2029.297008	3363.825108	47.881857
2025.087336	2960.312685	47.886861
2021.185194	2559.099734	47.891866
2017.286152	2161.366238	47.896871
2012.255394	1801.422009	47.901876
2006.574183	1465.100778	47.906881
2001.201107	1152.884825	47.911885
1996.133750	871.287649	47.916890
1991.134755	607.711655	47.921895
1986.360610	362.463889	47.926900
1981.382820	151.299207	47.931905
1971.184770	98.622174	47.936909
1960.709207	122.132795	47.941914
1954.506684	111.404984	47.946919
1950.513405	117.661036	47.951924
1948.271622	119.892321	47.956929
1946.399120	111.315812	47.961933
1944.646706	120.019835	47.966938
1942.864446	116.193843	47.971943
1940.131548	115.714326	47.976948
1936.959295	103.673357	47.981953
1934.287055	114.845868	47.986957
1930.788379	116.858324	47.991962
1927.316053	104.788129	47.996967
1923.941847	107.701855	48.001972
1921.192012	114.770445	48.006977
1917.779198	112.473207	48.011981
1913.972281	116.393904	48.016986
1910.931925	113.871022	48.021991
1907.512617	116.677876	48.026996
1904.517446	115.676038	48.032001
1900.705873	122.036689	48.037005
1897.654998	122.337483	48.042010
1894.758761	116.229823	48.047015
1891.140805	119.364984	48.052020
1887.704340	123.829135	48.057025
1884.553513	115.508532	48.062029
1880.525961	120.748040	48.067034
1876.792139	115.637601	48.072039
1873.503015	125.175572	48.077044
1870.509873	115.900296	48.082049
1867.109933	113.297343	48.087053
1863.106163	121.810763	48.092058
1860.758173	117.335679	48.097063
1857.144796	125.032213	48.102068
1853.561421	121.284069	48.107073
1850.210647	121.660015	48.112077
1846.403353	124.467147	48.117082
1842.906510	109.752748	48.122087
1839.523371	109.472515	48.127092
1836.401535	110.353826	48.132097
1833.022616	113.951654	48.137101
1829.366705	120.762638	48.142106
1825.917957	110.314940	48.147111
1822.202677	115.907640	48.152116
1818.715443	115.216509	48.157121
1815.343528	113.162850	48.162125
1812.074692	119.081533	48.167130
1808.395300	116.949180	48.172135
1804.982569	124.225349	48.177140
1801.758952	122.177083	48.182145
1798.286562	115.396651	48.187149
1794.734534	115.395805	48.192154
1791.202957	116.116267	48.197159
1787.855508	116.602431	48.202164
1784.313890	123.373483	48.207169
1781.033980	119.125706	48.212173
1777.178503	114.913728	48.217178
1774.236970	108.075991	48.222183
1770.173442	119.926941	48.227188
1766.630876	123.575553	48.232193
1763.672361	111.662694	48.237197
1760.061436	113.926746	48.242202
1756.861660	104.490667	48.247207
1753.154724	114.014568	48.252212
1749.611246	108.827067	48.257217
1745.925272	110.830722	48.262221
1742.494142	111.570355	48.267226
1738.959827	94.473219	48.272231
1735.381669	102.512273	48.277236
1732.381490	114.311613	48.282241
1728.529674	108.042660	48.287245
1725.328130	114.352662	48.292250
1721.898441	103.813436	48.297255
1718.480346	109.097298	48.302260
1714.875484	99.942572	48.307265
1711.381388	113.982764	48.312269
1707.718730	114.790072	48.317274
1704.403517	97.573420	48.322279
1700.921468	103.860640	48.327284
1697.156089	106.515726	48.332289
1693.810750	106.675706	48.337293
1690.360799	111.347604	48.342298
1687.325630	103.682906	48.347303
1683.404437	109.510137	48.352308
1679.942021	105.322419	48.357313
1676.397777	105.899332	48.362317
1672.776731	105.950367	48.367322
1669.296052	107.102673	48.372327
1665.673097	97.827389	48.377332
1662.185329	101.730062	48.382337
1659.142465	104.234733	48.387341
1655.694742	96.533015	48.392346
1652.259410	101.316530	48.397351
1648.706410	103.505136	48.402356
1645.165368	96.156461	48.407361
1641.650915	107.032942	48.412365
1637.719489	106.974104	48.417370
1634.645633	102.197576	48.422375
1631.054791	98.165893	48.427380
1627.439058	96.953787	48.432385
1624.242585	99.700663	48.437389
1620.501987	104.825918	48.442394
1617.108781	108.169720	48.447399
1613.626431	103.738343	48.452404
1609.929292	106.129718	48.457409
1606.682727	103.344738	48.462413
1602.712495	107.936268	48.467418
1599.586199	100.238312	48.472423
1596.042287	108.521975	48.477428
1592.892272	96.635799	48.482433
1589.560711	100.688168	48.487437
1585.738043	102.339792	48.492442
1582.148743	100.380105	48.497447
1578.869388	99.267506	48.502452
1575.147647	95.964876	48.507457
1571.500520	103.790045	48.512461
1567.782757	103.593557	48.517466
1564.714769	97.803739	48.522471
1560.779816	99.093197	48.527476
1557.487385	96.312199	48.532481
1554.182682	93.134485	48.537485
1550.848195	101.265328	48.542490
1547.602213	89.675672	48.547495
1544.057988	103.824892	48.552500
1540.412659	94.474021	48.557505
1536.610234	92.870210	48.562509
1532.537856	97.629499	48.567514
1529.440095	98.896221	48.572519
1526.258683	96.145402	48.577524
1523.076208	96.052262	48.582529
1519.594140	98.555699	48.587533
1515.363582	97.401335	48.592538
1512.230303	103.302088	48.597543
1508.458547	101.845363	48.602548
1505.265459	96.761549	48.607553
1501.486802	95.979769	48.612557
1498.496279	96.109851	48.617562
1495.006203	92.581352	48.622567
1491.349192	98.405436	48.627572
1487.756958	96.110864	48.632577
1484.282470	102.782887	48.637581
1480.436332	103.916162	48.642586
1477.290732	94.515995	48.647591
1473.653430	95.221304	48.652596
1470.068567	87.869990	48.657601
1466.548865	88.446265	48.662605
1463.127457	88.520032	48.667610
1459.639743	93.988741	48.672615
1456.115922	97.982458	48.677620
1452.802533	92.132778	48.682625
1449.420503	93.323531	48.687629
1445.452702	103.005091	48.692634
1442.487883	91.773482	48.697639
1438.831353	107.569489	48.702644
1435.409203	102.284058	48.707649
1431.862923	99.378072	48.712653
1428.012829	109.525361	48.717658
1424.761041	100.492899	48.722663
1421.381876	97.310971	48.727668
1417.845358	103.416858	48.732673
1414.236095	99.350107	48.737677
1410.689887	98.759944	48.742682
1407.373019	87.529357	48.747687
1403.530229	99.526270	48.752692
1399.806474	101.861694	48.757697
1396.691643	103.305087	48.762701
1392.987682	103.840447	48.767706
1389.605940	89.604951	48.772711
1386.280215	93.754497	48.777716
1383.130123	90.625504	48.782721
1379.605149	94.812391	48.787725
1375.741230	107.394718	48.792730
1372.192483	86.468683	48.797735
1368.655808	101.059639	48.802740
1365.030285	96.305740	48.807745
1361.897602	97.410234	48.812749
1358.379913	92.506677	48.817754
1355.037523	83.545285	48.822759
1351.260158	87.018497	48.827764
1347.586697	89.893416	48.832769
1343.954264	90.218335	48.837773
1340.510883	98.220601	48.842778
1337.570699	83.903738	48.847783
1333.971077	93.157837	48.852788
1330.215359	95.526714	48.857793
1327.018118	94.825297	48.862797
1322.890302	94.993211	48.867802
1319.536775	94.806493	48.872807
1316.027883	97.494452	48.877812
1312.822446	98.100919	48.882817
1309.649826	90.109672	48.887821
1305.408816	93.522180	48.892826
1302.511195	88.256367	48.897831
1298.649603	93.495383	48.902836
1295.041370	92.449822	48.907841
1291.959339	91.009153	48.912845
1288.278306	100.813756	48.917850
1284.828140	88.901599	48.922855
1281.027728	99.670730	48.927860
1277.678203	99.328372	48.932865
1274.212482	85.251507	48.937869
1270.825593	93.453785	48.942874
1267.082951	92.698063	48.947879
1263.975585	94.478820	48.952884
1260.129067	102.078776	48.957889
1256.742914	105.826458	48.962893
1253.024120	106.186974	48.967898
1249.737370	93.759012	48.972903
1246.392738	95.440662	48.977908
1242.691646	93.545872	48.982913
1239.475024	95.552441	48.987917
1235.616449	94.564837	48.992922
1232.647042	87.839088	48.997927
1228.508014	92.706848	49.002932
1225.019031	87.602696	49.007937
1221.996997	83.833706	49.012941
1218.314061	90.924153	49.017946
1214.556438	94.476560	49.022951
1210.778462	100.936410	49.027956
1207.750193	101.009118	49.032961
1204.259189	90.315030	49.037965
1200.334680	96.658485	49.042970
1197.066608	95.572644	49.047975
1193.676272	86.511176	49.052980
1190.155400	93.364432	49.057985
1186.654383	95.114721	49.062989
1183.130846	92.024898	49.067994
1179.768598	92.342580	49.072999
1176.308567	92.219911	49.078004
1172.672079	102.466829	49.083009
1169.572526	96.685144	49.088013
1165.614493	96.424861	49.093018
1162.459261	92.312786	49.098023
1158.784605	95.349256	49.103028
1154.859640	94.023989	49.108033
1151.385098	93.606194	49.113037
1147.840310	94.597686	49.118042
1144.501349	88.302790	49.123047
1141.056240	99.190622	49.128052
1137.883988	82.480207	49.133057
1133.982628	83.884701	49.138061
1130.116673	97.365829	49.143066
1126.823886	94.974073	49.148071
1123.732442	87.308738	49.153076
1120.328990	94.877697	49.158081
1116.599479	97.552558	49.163085
1112.975714	100.011646	49.168090
1110.147132	91.008281	49.173095
1106.176862	99.022968	49.178100
1102.471487	94.018953	49.183105
1098.954518	96.670222	49.188109
1095.213009	100.865526	49.193114
1091.922933	93.759449	49.198119
1088.711719	96.635204	49.203124
1085.525911	99.209618	49.208129
1081.843163	97.963715	49.213133
1077.944245	98.804697	49.218138
1074.652271	86.580066	49.223143
1070.899420	100.575091	49.228148
1067.727267	91.909945	49.233153
1064.134641	84.249869	49.238157
1060.331736	86.309748	49.243162
1056.686167	81.843752	49.248167
1053.635036	87.029394	49.253172
1049.949321	95.471180	49.258177
1046.845987	89.392717	49.263181
1043.124935	96.391034	49.268186
1040.175622	92.613910	49.273191
1036.080368	93.621498	49.278196
1032.375627	98.114797	49.283201
1029.018853	89.924477	49.288205
1025.186245	94.570555	49.293210
1022.128867	81.765267	49.298215
1018.971528	90.665796	49.303220
1014.597275	96.244057	49.308225
1011.416634	90.399091	49.313229
1007.982659	101.218755	49.318234
1004.879672	84.117948	49.323239
1001.247592	88.277241	49.328244
997.652960	88.729189	49.333249
994.282889	90.639444	49.338253
990.376051	93.487449	49.343258
986.654426	89.941281	49.348263
983.246765	85.150367	49.353268
979.634632	85.510131	49.358273
976.770657	82.149996	49.363277
973.215892	87.711425	49.368282
969.737234	78.973793	49.373287
966.237613	81.280695	49.378292
962.690443	90.539293	49.383297
959.189683	88.910745	49.388301
955.096757	98.469433	49.393306
951.741963	88.475516	49.398311
948.286227	87.596082	49.403316
944.671776	88.683859	49.408321
941.493858	81.765993	49.413325
938.123868	85.830711	49.418330
934.813386	78.190017	49.423335
931.102051	83.250648	49.428340
927.517136	80.129290	49.433345
923.833933	81.284717	49.438349
920.091961	83.452182	49.443354
917.208840	80.484168	49.448359
913.780272	81.561995	49.453364
910.125365	87.325675	49.458369
906.618735	76.032988	49.463373
903.085475	86.700426	49.468378
899.057800	89.431212	49.473383
895.733074	96.076785	49.478388
892.081815	84.012524	49.483393
889.124805	78.126443	49.488397
885.520595	84.973703	49.493402
881.674763	87.122539	49.498407
878.478950	87.439655	49.503412
875.245984	83.836420	49.508417
871.333026	82.480852	49.513421
867.961484	89.000837	49.518426
864.650464	87.776191	49.523431
861.064319	89.932061	49.528436
857.411023	79.339242	49.533441
853.719761	86.715736	49.538445
849.891080	86.770710	49.543450
847.286625	80.174872	49.548455
843.681428	84.051589	49.553460
839.847608	81.430887	49.558465
836.604638	74.991394	49.563469
832.859124	88.801775	49.568474
829.497645	77.787060	49.573479
825.734817	87.768916	49.578484
822.341328	82.928367	49.583489
818.882365	71.897196	49.588493
815.581847	79.696907	49.593498
812.123531	83.955714	49.598503
808.201179	84.506155	49.603508
804.678922	79.660345	49.608513
801.573791	76.185917	49.613517
797.703989	79.607129	49.618522
794.164230	74.858958	49.623527
790.772274	77.063697	49.628532
787.533095	80.991006	49.633537
783.994863	83.016041	49.638541
780.271124	83.216037	49.643546
776.996893	79.296545	49.648551
773.307706	75.609326	49.653556
769.512352	90.607521	49.658561
766.224971	81.295998	49.663565
762.690431	88.739849	49.668570
759.545435	77.912906	49.673575
756.135763	80.816417	49.678580
752.409209	78.656748	49.683585
749.029270	75.028957	49.688589
744.894952	79.424638	49.693594
741.588473	76.225165	49.698599
738.373604	78.937004	49.703604
735.047993	81.533209	49.708609
731.721261	74.654366	49.713613
727.798335	85.762108	49.718618
724.130711	78.192866	49.723623
720.726811	71.414623	49.728628
717.298295	74.634274	49.733633
714.027751	71.656996	49.738637
710.081664	76.032869	49.743642
706.881844	77.837556	49.748647
703.144583	83.462214	49.753652
699.484476	79.618622	49.758657
695.993085	78.175309	49.763661
692.524798	78.376677	49.768666
689.656150	65.956535	49.773671
686.040495	75.181507	49.778676
682.232224	72.050667	49.783681
678.825476	71.119352	49.788685
675.173663	82.542386	49.793690
672.295296	73.942315	49.798695
668.483308	71.897198	49.803700
664.494654	79.386434	49.808705
661.308702	77.927214	49.813709
657.653058	82.827342	49.818714
653.898505	78.251833	49.823719
650.412365	81.243186	49.828724
647.430041	74.930824	49.833729
644.041109	72.667995	49.838733
640.239462	80.045866	49.843738
636.726011	79.248222	49.848743
632.973536	79.908280	49.853748
629.524379	70.925687	49.858753
626.651872	78.158917	49.863757
622.712528	89.082565	49.868762
619.275891	78.199814	49.873767
615.983001	76.089712	49.878772
611.734944	81.635711	49.883777
608.170551	69.194182	49.888781
604.828704	78.550538	49.893786
601.937894	76.045659	49.898791
598.126766	79.723508	49.903796
594.623602	82.844064	49.908801
591.516931	78.721350	49.913805
587.874286	84.919732	49.918810
584.353746	79.750998	49.923815
580.651374	74.379624	49.928820
576.965367	81.109926	49.933825
573.735121	72.871530	49.938829
569.889681	78.797769	49.943834
566.744596	74.291908	49.948839
563.232130	75.218324	49.953844
559.704633	77.542261	49.958849
556.509843	84.898432	49.963853
552.312630	81.552920	49.968858
548.971040	80.472276	49.973863
545.237694	81.448899	49.978868
542.166275	79.490986	49.983873
539.059601	81.328645	49.988877
535.230224	80.972493	49.993882
531.836215	72.958910	49.998887
527.977691	79.194066	50.003892
524.655439	72.915662	50.008897
521.010323	72.565628	50.013901
516.849002	83.583945	50.018906
513.815897	78.918293	50.023911
510.614333	73.389876	50.028916
507.221327	85.057358	50.033921
503.861392	78.813295	50.038925
500.152119	73.737232	50.043930
496.466463	76.765988	50.048935
493.223835	80.478729	50.053940
489.632810	80.499919	50.058945
486.314436	68.624382	50.063949
482.377392	83.135280	50.068954
478.682964	77.746868	50.073959
475.533716	76.756511	50.078964
472.352841	87.365940	50.083969
468.873580	77.869221	50.088973
465.017709	77.406476	50.093978
461.963239	74.341814	50.098983
457.998258	77.632353	50.103988
454.328762	78.270025	50.108993
451.077334	73.274551	50.113997
447.560459	81.357894	50.119002
444.038067	69.896932	50.124007
440.471243	76.355596	50.129012
437.030331	77.397435	50.134017
433.449632	74.930379	50.139021
429.570115	79.998255	50.144026
426.519593	74.651976	50.149031
423.407128	85.291884	50.154036
419.453062	88.495311	50.159041
415.896191	71.218564	50.164045
412.350403	86.652456	50.169050
409.195605	77.643062	50.174055
405.557849	73.951062	50.179060
401.601494	83.956739	50.184065
398.273340	76.812430	50.189069
394.691468	82.403432	50.194074
391.347946	85.837670	50.199079
388.631539	78.050809	50.204084
384.793944	82.406665	50.209089
381.418647	79.537489	50.214093
377.519161	86.253590	50.219098
373.943183	88.974229	50.224103
370.384180	83.204094	50.229108
366.904124	74.210547	50.234113
363.516531	75.946429	50.239117
359.661957	76.831221	50.244122
356.330005	75.923105	50.249127
352.698611	79.936822	50.254132
349.035043	85.765170	50.259137
346.243147	77.759120	50.264141
342.600654	82.239626	50.269146
338.995686	73.616700	50.274151
335.692719	70.385106	50.279156
331.884630	80.045009	50.284161
328.372285	82.069229	50.289165
324.469967	74.036749	50.294170
321.337841	76.390907	50.299175
317.965824	80.531922	50.304180
314.261207	82.000799	50.309185
311.143250	72.223248	50.314189
307.464765	79.192840	50.319194
303.974834	74.604671	50.324199
300.438831	80.321415	50.329204
296.886943	87.040353	50.334209
293.367126	72.228698	50.339213
289.686783	75.433816	50.344218
286.441314	68.944193	50.349223
283.156011	76.795345	50.354228
279.416109	81.506153	50.359233
276.075520	77.021284	50.364237
272.362945	80.554117	50.369242
268.950108	74.925760	50.374247
265.214703	77.196681	50.379252
261.449942	81.901869	50.384257
258.200213	70.933160	50.389261
254.936902	75.440060	50.394266
251.565554	80.545895	50.399271
247.857317	67.329607	50.404276
244.057094	70.917215	50.409281
240.598606	69.857978	50.414285
237.225763	81.025631	50.419290
234.031298	74.021887	50.424295
230.344051	76.981322	50.429300
226.846427	76.396402	50.434305
223.461661	73.281961	50.439309
219.825185	76.119600	50.444314
216.433227	69.617996	50.449319
213.038878	73.379693	50.454324
209.118138	75.303000	50.459329
205.749525	75.030182	50.464333
202.169126	87.761369	50.469338
198.858006	86.403954	50.474343
195.272476	77.053551	50.479348
191.873536	79.158206	50.484353
188.556443	73.802851	50.489357
184.822562	77.835706	50.494362
181.349203	69.821896	50.499367
177.745205	74.685555	50.504372
174.070061	73.378493	50.509377
170.850041	73.041418	50.514381
167.273056	75.730600	50.519386
163.812018	70.078132	50.524391
160.374715	68.753025	50.529396
156.344850	82.228047	50.534401
153.431893	73.829606	50.539405
149.746041	75.352530	50.544410
146.197409	78.932618	50.549415
142.605973	73.702240	50.554420
139.167875	63.787917	50.559425
135.875975	72.241200	50.564429
132.265827	71.806687	50.569434
128.658378	75.326333	50.574439
125.632812	68.748721	50.579444
121.790137	71.574184	50.584449
118.276099	65.942632	50.589453
114.814879	68.199357	50.594458
110.936264	73.668911	50.599463
107.555366	72.879179	50.604468
104.241074	80.250818	50.609473
100.846570	68.969339	50.614477
97.304343	78.040551	50.619482
93.671719	66.774003	50.624487
90.066649	63.548358	50.629492
86.565109	73.087784	50.634497
83.147196	64.666742	50.639501
79.603407	80.941856	50.644506
76.079882	77.820570	50.649511
72.944540	73.632803	50.654516
68.715354	77.496023	50.659521
65.764743	70.764386	50.664525
62.373753	81.242030	50.669530
58.280405	72.764805	50.674535
55.161938	78.267871	50.679540
51.091484	77.237506	50.684545
47.782971	75.209013	50.689549
44.551418	78.154467	50.694554
41.369091	75.540033	50.699559
38.336259	73.168072	50.704564
34.272935	71.877179	50.709569
30.647774	68.208596	50.714573
27.278060	79.581408	50.719578
23.824813	74.092263	50.724583
19.935387	76.994620	50.729588
16.035100	77.139957	50.734593
13.119785	68.707114	50.739597
9.861662	77.325986	50.744602
6.235783	77.298890	50.749607
2.758829	74.562661	50.754612