Fri Aug 26 14:21:04 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.197389	103.007752	0.000000
0.091078	88.161402	0.005005
-0.365538	88.286268	0.010010
-0.295119	85.086322	0.015014
-0.422917	88.361617	0.020019
-0.642775	77.563462	0.025024
-0.737288	77.261801	0.030029
-0.964958	73.519828	0.035034
-0.957688	66.773765	0.040038
-1.747108	53.517558	0.045043
-1.846286	46.050944	0.050048
-1.943135	45.708520	0.055053
-2.484784	42.572242	0.060058
-2.516212	33.089329	0.065062
-2.550510	42.414781	0.070067
-3.333694	28.486928	0.075072
-3.500824	18.939732	0.080077
-3.691465	17.422379	0.085082
-3.645306	0.603556	0.090086
-4.295924	5.228860	0.095091
-4.414531	2.339924	0.100096
-4.292628	1.583805	0.105101
-4.909083	-1.692673	0.110106
-5.143550	-2.330034	0.115110
-5.351302	-4.331923	0.120115
-6.036650	3.130251	0.125120
-6.320454	-0.172711	0.130125
-6.466783	-4.607515	0.135130
-6.659170	-5.412774	0.140134
-7.103138	-1.626377	0.145139
-6.936102	-6.094152	0.150144
-7.293117	-4.380827	0.155149
-8.180611	-1.408031	0.160154
-8.430057	10.352109	0.165158
-8.276866	10.432648	0.170163
-8.653790	6.331126	0.175168
-8.164720	4.195435	0.180173
-8.805609	3.320806	0.185178
-9.618927	-3.639142	0.190182
-10.156851	-1.967249	0.195187
-9.651328	1.332807	0.200192
-9.610652	-6.664906	0.205197
-9.852388	-3.463634	0.210202
-10.172786	-4.913327	0.215206
-10.819054	-1.231469	0.220211
-11.752169	-5.967702	0.225216
-11.501157	-6.566759	0.230221
-11.515947	6.596302	0.235226
-11.269220	-3.429755	0.240230
-11.512357	-1.281759	0.245235
-12.223087	-6.213962	0.250240
-12.699615	-5.412140	0.255245
-12.730256	2.387844	0.260250
-12.974583	3.492024	0.265254
-12.869603	7.003135	0.270259
-13.371809	1.744244	0.275264
-13.691985	-2.280693	0.280269
-14.653544	2.124113	0.285274
-14.158498	3.002446	0.290278
-14.463394	9.127274	0.295283
-14.737270	-0.295727	0.300288
-14.831750	-1.935614	0.305293
-14.876007	5.031289	0.310298
-15.630032	-0.697741	0.315302
-15.910952	2.898761	0.320307
-15.855968	10.846763	0.325312
-16.040367	-0.345993	0.330317
-16.722221	5.989379	0.335322
-16.925291	1.933555	0.340326
-17.327774	2.065810	0.345331
-17.296709	-0.210535	0.350336
-17.252613	-3.052038	0.355341
-17.427615	3.384746	0.360346
-17.733686	-1.841408	0.365350
-18.263823	-3.274264	0.370355
-19.004738	4.009906	0.375360
-18.820710	-4.468856	0.380365
-18.691588	9.883476	0.385370
-18.986131	1.314714	0.390374
-19.444010	3.629019	0.395379
-19.848911	3.894524	0.400384
-20.081758	-8.087922	0.405389
-20.405556	-0.131569	0.410394
-20.100497	2.557478	0.415398
-20.342348	-1.913073	0.420403
-21.400154	-5.478323	0.425408
-21.733333	-3.607363	0.430413
-22.022219	10.797397	0.435418
-21.945487	-7.187235	0.440422
-22.353282	-2.194794	0.445427
-22.275348	3.554061	0.450432
-22.111385	-2.934806	0.455437
-22.353754	2.417844	0.460442
-22.472825	-6.589508	0.465446
-22.669204	-3.664207	0.470451
-23.256570	-5.442481	0.475456
-23.759992	-3.500723	0.480461
-24.603408	-3.695271	0.485466
-24.692854	1.105241	0.490470
-24.540194	-0.136542	0.495475
-24.618875	-2.512854	0.500480
-24.412245	3.351999	0.505485
-25.305549	4.819805	0.510490
-26.156461	1.206522	0.515494
-26.082296	-1.791517	0.520499
-26.364390	7.183367	0.525504
-25.996585	4.332591	0.530509
-26.373788	-4.068279	0.535514
-26.600132	4.167121	0.540518
-26.759179	7.203666	0.545523
-27.535041	-2.960558	0.550528
-27.483690	-3.607620	0.555533
-27.944740	-0.267801	0.560538
-27.870935	-4.689424	0.565542
-27.892493	-4.126113	0.570547
-28.577816	-1.909269	0.575552
-28.681474	-2.959289	0.580557
-29.102427	-0.970261	0.585562
-29.041789	-3.055064	0.590566
-29.177373	4.691659	0.595571
-29.635365	4.494046	0.600576
-29.829780	0.506475	0.605581
-30.403071	10.042374	0.610586
-30.239762	0.775925	0.615590
-30.399919	0.898923	0.620595
-31.157893	2.975224	0.625600
-31.442345	-4.956048	0.630605
-31.988322	7.587387	0.635610
-32.019911	2.078059	0.640614
-31.577712	5.732811	0.645619
-31.914855	3.567576	0.650624
-32.670272	-7.384412	0.655629
-33.006142	-1.378149	0.660634
-33.005593	-3.039159	0.665638
-33.440632	0.363048	0.670643
-33.202017	-1.635575	0.675648
-33.563510	-1.794430	0.680653
-34.074383	6.320763	0.685658
-34.354661	-6.309173	0.690662
-34.550228	-6.481208	0.695667
-34.879865	-5.866766	0.700672
-34.677088	-8.600100	0.705677
-35.572431	-5.312882	0.710682
-35.856640	-1.722196	0.715686
-36.100302	-7.242792	0.720691
-36.300733	4.243964	0.725696
-36.145096	-8.324132	0.730701
-36.859177	-5.302409	0.735706
-36.512572	-1.354374	0.740710
-36.530489	5.640062	0.745715
-37.025836	-5.928203	0.750720
-37.526522	-2.104502	0.755725
-37.763740	4.769060	0.760730
-37.660087	1.266573	0.765734
-38.396418	0.172695	0.770739
-39.125384	4.278705	0.775744
-39.163751	-4.380557	0.780749
-39.576034	-5.119942	0.785754
-39.394179	2.491937	0.790758
-39.403040	-0.913940	0.795763
-39.282070	-3.919266	0.800768
-39.443887	-1.534003	0.805773
-40.311992	-1.054014	0.810778
-40.876436	-1.010433	0.815782
-40.662542	-5.640522	0.820787
-40.912265	3.329319	0.825792
-40.823415	-5.058694	0.830797
-41.779816	-1.916987	0.835802
-42.064857	-2.641383	0.840806
-42.324711	1.530786	0.845811
-42.514071	-0.116473	0.850816
-42.197827	-8.729708	0.855821
-42.445710	-7.719885	0.860826
-42.784526	1.213209	0.865830
-43.588071	-2.938940	0.870835
-43.913600	1.487055	0.875840
-43.641966	-5.736722	0.880845
-44.209038	-2.133631	0.885850
-44.101450	0.627288	0.890854
-44.492705	-4.016145	0.895859
-45.432895	-0.272706	0.900864
-45.194542	2.936073	0.905869
-45.578649	-0.360760	0.910874
-45.624987	-7.427465	0.915878
-45.422947	-9.350792	0.920883
-45.799567	-4.059496	0.925888
-45.739686	-6.352981	0.930893
-46.776937	4.305481	0.935898
-47.088998	-4.912259	0.940902
-46.995158	0.277315	0.945907
-47.108591	-7.550872	0.950912
-47.483559	-7.483010	0.955917
-48.296167	-4.180200	0.960922
-48.241395	1.600732	0.965926
-48.193453	-2.734609	0.970931
-48.505729	-9.161978	0.975936
-48.418050	-2.791407	0.980941
-48.897087	9.634041	0.985946
-49.078302	-5.719399	0.990950
-49.425353	-3.213549	0.995955
-49.637612	-2.747092	1.000960
-49.969180	-7.213162	1.005965
-50.800987	-1.262556	1.010970
-50.922197	-2.316170	1.015974
-50.968447	-12.983113	1.020979
-51.463297	0.020573	1.025984
-51.343693	-0.482097	1.030989
-51.449776	1.413615	1.035994
-51.482812	-3.763302	1.040998
-52.391093	-2.293164	1.046003
-52.892735	1.166867	1.051008
-52.452332	-11.818873	1.056013
-52.756327	1.835282	1.061018
-52.871730	-0.975059	1.066022
-52.905610	4.746913	1.071027
-53.595554	0.105694	1.076032
-53.640373	-2.712473	1.081037
-53.944595	9.900884	1.086042
-54.125857	4.933698	1.091046
-54.098577	-2.849964	1.096051
-54.911265	8.380956	1.101056
-55.258250	0.063964	1.106061
-55.687830	5.287581	1.111066
-55.546265	2.839012	1.116070
-55.472176	2.112483	1.121075
-56.152031	6.441792	1.126080
-56.325991	3.368494	1.131085
-56.981526	2.546765	1.136090
-57.148080	3.512289	1.141094
-57.159603	2.435270	1.146099
-57.355532	8.815203	1.151104
-57.478939	-0.257911	1.156109
-57.830666	1.347028	1.161114
-58.616435	-2.671850	1.166118
-58.568580	-2.771058	1.171123
-58.799234	4.949339	1.176128
-58.528377	-4.833707	1.181133
-58.707679	8.778893	1.186138
-58.663748	4.532756	1.191142
-59.496171	4.937590	1.196147
-59.743964	3.881540	1.201152
-60.067996	0.015388	1.206157
-60.166455	4.023228	1.211162
-60.809184	-3.962987	1.216166
-61.206502	0.160984	1.221171
-61.690043	4.734964	1.226176
-61.805227	17.132237	1.231181
-61.805563	2.462450	1.236186
-62.019773	10.287852	1.241190
-61.549228	2.732555	1.246195
-61.847621	2.854932	1.251200
-61.899561	12.784203	1.256205
-62.782816	1.358588	1.261210
-63.019038	2.872779	1.266214
-63.211000	1.760581	1.271219
-64.087728	17.345162	1.276224
-64.079294	2.699319	1.281229
-64.197470	4.378622	1.286234
-64.421040	-1.629141	1.291238
-64.416900	1.736322	1.296243
-64.847687	9.842209	1.301248
-64.752192	7.204667	1.306253
-65.440542	-0.752300	1.311258
-65.754784	9.660720	1.316262
-65.709371	-2.478942	1.321267
-66.079993	1.821201	1.326272
-66.102783	3.359107	1.331277
-66.877300	4.533182	1.336282
-67.572338	11.465373	1.341286
-67.522267	6.288168	1.346291
-67.732653	9.047978	1.351296
-67.615875	5.821848	1.356301
-67.532509	6.451078	1.361306
-67.276396	10.925714	1.366310
-67.833121	2.113049	1.371315
-68.666075	2.802694	1.376320
-68.918586	1.355086	1.381325
-69.067512	3.282778	1.386330
-69.445757	11.488048	1.391334
-69.888417	7.592911	1.396339
-70.438488	12.047541	1.401344
-70.480098	-0.176644	1.406349
-70.656896	3.735829	1.411354
-71.155813	9.552352	1.416358
-71.246267	4.843102	1.421363
-71.097200	13.928020	1.426368
-70.609453	1.697340	1.431373
-70.612152	-2.247315	1.436378
-71.633858	-2.278065	1.441382
-71.876142	8.598296	1.446387
-72.431698	6.258269	1.451392
-72.470060	3.385314	1.456397
-73.310296	5.828752	1.461402
-73.666216	7.095835	1.466406
-73.636605	5.354372	1.471411
-73.489531	11.355045	1.476416
-73.358684	-0.310718	1.481421
-73.427493	0.740825	1.486426
-74.259874	3.758823	1.491430
-74.511103	4.259821	1.496435
-75.059796	7.698706	1.501440
-74.985472	3.700930	1.506445
-76.136231	1.811068	1.511450
-76.154542	-0.251951	1.516454
-75.476586	-3.764763	1.521459
-76.568846	4.788948	1.526464
-76.635741	5.441573	1.531469
-76.542830	0.251374	1.536474
-77.138781	-1.803962	1.541478
-76.757619	-1.148335	1.546483
-77.207357	5.290095	1.551488
-77.635118	-7.807237	1.556493
-78.049480	-6.578511	1.561498
-77.935651	-5.201077	1.566502
-77.981112	-12.935443	1.571507
-78.545218	2.502375	1.576512
-78.860129	-3.266546	1.581517
-79.590758	10.254730	1.586522
-79.523241	3.375933	1.591526
-79.518847	-5.115983	1.596531
-79.870432	4.211390	1.601536
-79.983391	-3.240398	1.606541
-80.651490	-0.402997	1.611546
-81.123039	0.417033	1.616550
-81.058398	-6.277821	1.621555
-81.163137	6.026070	1.626560
-81.051814	-16.288632	1.631565
-81.152000	-12.445037	1.636570
-81.931203	-0.706828	1.641574
-82.205344	-10.689740	1.646579
-82.789149	-2.303780	1.651584
-82.581723	-7.581407	1.656589
-82.663335	-6.404490	1.661594
-82.874434	-12.895063	1.666598
-83.435827	-7.353546	1.671603
-84.140326	-5.579790	1.676608
-84.187717	3.399673	1.681613
-83.791995	-8.816670	1.686618
-84.320342	1.528443	1.691622
-84.348159	-9.793080	1.696627
-85.051650	-0.391937	1.701632
-85.256611	-7.158705	1.706637
-85.466109	-5.923912	1.711642
-85.754317	-1.680894	1.716646
-85.483561	1.513347	1.721651
-86.194033	-6.598353	1.726656
-86.635193	-9.560445	1.731661
-86.992243	-16.689493	1.736666
-87.259884	-12.886262	1.741670
-86.915208	-16.185835	1.746675
-87.477317	-4.905359	1.751680
-87.232191	-9.350490	1.756685
-87.635082	-7.250384	1.761690
-88.389196	-6.873560	1.766694
-88.259574	-11.395616	1.771699
-88.958974	-4.152716	1.776704
-88.427442	-8.525385	1.781709
-89.165288	-6.626219	1.786714
-89.451018	1.665878	1.791718
-89.341769	-13.084228	1.796723
-89.794684	-0.017475	1.801728
-90.250351	-7.143827	1.806733
-90.708739	-8.613160	1.811738
-91.079721	-1.570085	1.816742
-91.240993	-16.249595	1.821747
-91.230222	-7.943559	1.826752
-91.133015	-6.747029	1.831757
-91.620970	-3.902877	1.836762
-91.546517	-0.247817	1.841766
-92.274546	-8.749074	1.846771
-92.822441	0.475988	1.851776
-92.742498	-14.772572	1.856781
-92.677859	0.159237	1.861786
-93.313989	-1.102095	1.866790
-92.929158	-10.849098	1.871795
-93.575139	-0.118689	1.876800
-94.219608	-11.894670	1.881805
-94.456182	-1.246988	1.886810
-94.602019	-1.388801	1.891814
-94.245047	-11.318122	1.896819
-94.806474	-8.639695	1.901824
-95.736427	-10.525970	1.906829
-95.807586	2.734437	1.911834
-96.130608	-4.529623	1.916838
-96.061503	-14.379320	1.921843
-96.270630	-9.152070	1.926848
-96.171315	-7.038412	1.931853
-95.788172	-6.139495	1.936858
-96.602519	-3.874088	1.941862
-96.717439	-17.447211	1.946867
-97.393805	-2.884067	1.951872
-97.576997	-16.114379	1.956877
-98.480117	-12.107803	1.961882
-98.976955	-15.659153	1.966886
-98.766205	-15.628704	1.971891
-99.110095	-3.417294	1.976896
-98.528810	-6.272835	1.981901
-98.767845	-12.107347	1.986906
-98.848930	-7.045560	1.991910
-99.557140	-13.797241	1.996915
-100.274638	-9.143271	2.006912
-99.843512	-6.673096	2.016909
-99.092523	-4.721542	2.026906
-98.916081	-12.003052	2.036902
-97.912617	-3.156729	2.046899
-97.915074	-1.512334	2.056896
-97.336708	-0.816818	2.066893
-96.513597	-5.427285	2.076890
-96.324437	-3.188689	2.086886
-95.793078	-8.393603	2.096883
-95.137641	-10.009833	2.106880
-94.896697	-6.265143	2.116877
-93.925298	-7.654979	2.126874
-93.522724	-6.805385	2.136870
-93.481991	-2.123561	2.146867
-92.729880	-4.939561	2.156864
-92.342828	-3.276621	2.166861
-91.834101	-9.083040	2.176858
-91.255028	-11.910110	2.186854
-90.876721	-5.187002	2.196851
-89.968992	-8.071578	2.206848
-89.714094	-10.350846	2.216845
-89.526063	-10.557534	2.226842
-88.599780	-11.081900	2.236838
-88.352359	-15.770617	2.246835
-87.483905	-9.345565	2.256832
-87.239987	-4.882271	2.266829
-86.764230	-13.344419	2.276826
-85.593453	-5.968614	2.286822
-85.614962	-7.821554	2.296819
-85.449443	-2.883570	2.306816
-84.948584	-2.568780	2.316813
-84.013792	-8.058248	2.326810
-83.543771	-9.534739	2.336806
-83.646491	-9.369885	2.346803
-82.566144	-6.804396	2.356800
-82.123364	-11.479184	2.366797
-81.467346	-9.446321	2.376794
-81.074038	-6.523612	2.386790
-81.001700	-9.290790	2.396787
-80.297656	-5.298266	2.406784
-79.560850	-5.923007	2.416781
-79.288851	-2.059610	2.426778
-78.597675	0.873740	2.436774
-78.401479	-2.131294	2.446771
-78.026451	-2.953121	2.456768
-77.125543	-3.869498	2.466765
-76.203307	-6.259006	2.476762
-75.917660	-5.875863	2.486758
-75.997263	-3.060080	2.496755
-75.499319	-2.656141	2.506752
-74.698039	-4.162035	2.516749
-74.194296	-1.408569	2.526746
-72.924717	-5.122404	2.536742
-73.217044	-5.555232	2.546739
-72.954408	3.970295	2.556736
-72.546020	-1.142619	2.566733
-71.541822	-1.207129	2.576730
-71.013874	-0.525937	2.586726
-70.281025	-9.249855	2.596723
-69.994905	0.069280	2.606720
-70.043211	-2.451040	2.616717
-69.153623	0.045953	2.626714
-68.508329	-7.051977	2.636710
-68.213962	-7.572984	2.646707
-67.410029	5.191175	2.656704
-66.896453	-0.318240	2.666701
-66.906168	-0.456127	2.676698
-66.122229	-0.666902	2.686694
-65.485927	-2.413196	2.696691
-65.437119	0.715202	2.706688
-64.521598	-0.783138	2.716685
-64.063245	-2.419365	2.726682
-63.826915	-0.736124	2.736678
-63.053004	1.978446	2.746675
-62.737864	0.462715	2.756672
-62.057661	-3.919601	2.766669
-61.140045	5.865065	2.776666
-60.978200	0.822214	2.786662
-61.111656	-2.549630	2.796659
-60.465988	4.027322	2.806656
-59.928503	1.567844	2.816653
-58.724684	-1.907678	2.826650
-58.268422	3.453860	2.836646
-58.328667	-3.290308	2.846643
-57.860218	-2.783578	2.856640
-57.136379	-3.897291	2.866637
-56.839478	-5.806144	2.876634
-55.723464	-0.921117	2.886630
-55.426772	-6.482290	2.896627
-55.112418	-1.684682	2.906624
-54.879651	-1.001877	2.916621
-54.028645	-2.699240	2.926618
-53.579545	-9.158425	2.936614
-52.641801	2.704281	2.946611
-52.276950	-1.470551	2.956608
-52.397520	-0.815092	2.966605
-51.945647	-4.661362	2.976602
-51.148473	-1.833210	2.986598
-50.482209	-3.349759	2.996595
-49.716735	-8.318704	3.006592
-49.628157	0.641565	3.016589
-49.416258	-4.969760	3.026586
-48.277113	-4.437580	3.036582
-48.147823	-4.403881	3.046579
-47.821387	-4.442056	3.056576
-46.657852	2.453395	3.066573
-46.252775	-3.650492	3.076570
-46.058372	-3.645936	3.086566
-46.163434	-1.627615	3.096563
-45.236517	-1.927173	3.106560
-44.723641	-5.488344	3.116557
-43.798340	2.822147	3.126554
-43.339791	-5.542296	3.136550
-43.502893	0.805798	3.146547
-42.692771	-1.816502	3.156544
-41.998867	1.287482	3.166541
-41.302149	-4.019206	3.176538
-40.847270	-4.172410	3.186534
-40.659348	0.866623	3.196531
-40.313533	-2.940960	3.206528
-39.529345	-4.932018	3.216525
-38.895148	-5.509104	3.226522
-38.760875	-3.417178	3.236518
-37.692260	-2.192961	3.246515
-37.335398	-1.700533	3.256512
-37.465646	-2.297976	3.266509
-36.365483	-11.174115	3.276506
-35.795398	-5.770115	3.286502
-35.711622	-9.929692	3.296499
-35.323528	0.605803	3.306496
-34.647668	-1.330376	3.316493
-33.768051	0.845067	3.326490
-33.057120	3.423731	3.336486
-33.023774	0.383865	3.346483
-33.062039	-3.360751	3.356480
-32.607054	-2.829749	3.366477
-31.651052	-3.038804	3.376474
-30.639810	-5.394653	3.386470
-30.446585	-11.155119	3.396467
-30.313095	-5.768669	3.406464
-29.409318	-4.895743	3.416461
-29.178786	-6.328610	3.426458
-28.580448	-4.834776	3.436454
-28.159485	-12.388770	3.446451
-27.493769	-8.789406	3.456448
-27.114132	-0.824762	3.466445
-26.230053	-6.645279	3.476442
-26.055474	-4.493106	3.486438
-25.950333	-5.253906	3.496435
-24.760538	-0.846015	3.506432
-24.765935	2.385855	3.516429
-23.696530	2.403057	3.526426
-23.241383	-3.996887	3.536422
-22.930892	-1.875378	3.546419
-22.868063	-4.672754	3.556416
-21.922783	-7.794418	3.566413
-21.468026	-6.753382	3.576410
-21.015885	-6.057218	3.586406
-20.326174	-0.630660	3.596403
-20.117840	-4.625906	3.606400
-19.770180	-3.469996	3.616397
-19.017683	3.388090	3.626394
-18.522920	-2.634731	3.636390
-17.872801	-6.172924	3.646387
-17.498319	1.412401	3.656384
-17.312766	-2.278368	3.666381
-16.104002	3.127564	3.676378
-15.595566	-2.555275	3.686374
-15.764064	-1.119436	3.696371
-15.046734	-0.695803	3.706368
-14.005422	-2.305590	3.716365
-14.350454	-2.410275	3.726362
-13.851956	-4.508901	3.736358
-12.958377	-1.318800	3.746355
-12.656189	-0.580282	3.756352
-11.321860	-5.549101	3.766349
-11.578239	-1.052256	3.776346
-11.420173	-1.672414	3.786342
-10.750764	-2.125106	3.796339
-9.794838	4.042427	3.806336
-9.518564	-4.518546	3.816333
-8.792172	-6.725511	3.826330
-8.603595	-9.152838	3.836326
-8.221490	-5.192546	3.846323
-7.241605	-7.229910	3.856320
-7.119261	-6.121280	3.866317
-6.581125	-2.289814	3.876314
-5.602080	-4.561458	3.886310
-5.603560	-3.370194	3.896307
-5.297178	1.875304	3.906304
-4.661174	4.776069	3.916301
-4.297766	8.387662	3.926298
-3.767230	20.570372	3.936294
-3.074490	32.721500	3.946291
-3.052138	36.234150	3.956288
-2.366099	46.989374	3.966285
-1.594970	58.554961	3.976282
-1.375316	69.503187	3.986278
-0.914959	85.399921	3.996275
-0.673958	103.427851	4.006272
0.000000	110.948775	4.011277
-0.144368	112.224054	4.016282
0.345555	136.280228	4.021286
0.445235	141.835923	4.026291
0.544363	138.210730	4.031296
0.897658	141.556659	4.036301
0.970361	138.074782	4.041306
0.911138	136.397756	4.046310
0.875394	140.044696	4.051315
1.126798	141.694943	4.056320
0.862219	139.771487	4.061325
0.780094	133.333538	4.066330
1.040420	133.637836	4.071334
0.869998	138.596522	4.076339
1.070852	129.928420	4.081344
1.209024	150.420142	4.086349
0.955811	136.479289	4.091354
0.984701	131.703966	4.096358
1.122206	134.245119	4.101363
0.902327	143.627992	4.106368
1.100606	142.894775	4.111373
0.928211	143.013352	4.116378
1.124606	134.693945	4.121382
0.596539	144.871428	4.126387
0.978619	147.213156	4.131392
1.045922	142.317957	4.136397
0.818330	142.913352	4.141402
0.986390	134.269335	4.146406
0.746484	142.782152	4.151411
0.791238	140.345474	4.156416
0.774242	142.705045	4.161421
0.829816	150.554944	4.166426
1.048424	139.160150	4.171430
0.910302	145.512152	4.176435
1.277282	144.202190	4.181440
1.205792	142.204379	4.186445
0.936008	144.264796	4.191450
1.359440	151.538579	4.196454
1.296620	146.128978	4.201459
1.391309	144.526061	4.206464
1.309821	143.241633	4.211469
1.235193	149.662842	4.216474
1.077808	139.690132	4.221478
0.976187	145.245532	4.226483
1.112127	157.774649	4.231488
1.343748	164.493023	4.236493
1.345354	170.146252	4.241498
2.023007	160.717380	4.246502
1.529358	163.549790	4.251507
1.296782	149.472840	4.256512
1.042667	145.690678	4.261517
1.018759	145.378022	4.266522
1.451589	151.853097	4.271526
1.359970	156.688791	4.276531
1.644233	160.757299	4.281536
1.669802	156.624712	4.286541
0.970877	151.551424	4.291546
1.400182	148.792286	4.296550
1.068009	165.070480	4.301555
1.816114	163.435428	4.306560
1.738902	172.881522	4.311565
1.426520	166.501557	4.316570
1.592113	154.007721	4.321574
1.409022	165.020497	4.326579
1.666558	173.905121	4.331584
1.535004	165.405811	4.336589
1.339102	157.900428	4.341594
1.602290	162.981430	4.346598
1.662919	167.790258	4.351603
1.633646	165.994674	4.356608
1.770933	175.616175	4.361613
1.798946	160.808961	4.366618
1.542462	141.623241	4.371622
1.235825	148.824036	4.376627
1.446332	153.204575	4.381632
1.583483	160.741229	4.386637
1.498765	166.129493	4.391642
1.562645	171.722408	4.396646
1.620249	172.083579	4.401651
1.799540	165.405606	4.406656
1.591189	167.155911	4.411661
1.474909	168.603987	4.416666
1.566358	166.840225	4.421670
1.413650	172.580754	4.426675
1.797400	170.515224	4.431680
1.810055	167.782991	4.436685
1.414957	174.064284	4.441690
1.684314	166.163763	4.446694
1.473058	176.725361	4.451699
1.692200	183.119826	4.456704
2.383314	188.339848	4.461709
2.170171	187.888980	4.466714
2.012895	177.909904	4.471718
1.935623	176.333758	4.476723
1.728539	173.623081	4.481728
1.794285	170.341592	4.486733
1.747105	178.862384	4.491738
1.891586	171.737422	4.496742
2.051830	190.941301	4.501747
2.003408	192.945113	4.506752
1.719914	179.568912	4.511757
2.034416	193.655256	4.516762
2.108173	192.349816	4.521766
2.139848	199.789016	4.526771
1.970511	183.933694	4.531776
1.860729	182.669486	4.536781
1.743200	194.972345	4.541786
2.065517	195.143608	4.546790
1.929996	206.576100	4.551795
2.167092	192.919523	4.556800
2.669174	195.669671	4.561805
1.945254	194.298606	4.566810
2.207402	183.890400	4.571814
2.062740	194.963648	4.576819
2.250994	194.143407	4.581824
2.277423	198.359633	4.586829
1.946609	199.059683	4.591834
2.699457	195.873686	4.596838
2.527458	190.484234	4.601843
1.851979	188.865187	4.606848
1.849272	188.574540	4.611853
1.925045	196.522552	4.616858
2.410104	197.320196	4.621862
2.059584	192.651385	4.626867
2.318004	197.840704	4.631872
2.314706	198.518235	4.636877
2.275478	198.204800	4.641882
2.303244	201.889320	4.646886
2.389348	204.818129	4.651891
2.439916	195.894989	4.656896
2.169688	189.840639	4.661901
2.059014	196.574354	4.666906
2.581217	188.865404	4.671910
2.206358	198.161706	4.676915
2.140944	202.224557	4.681920
2.090483	197.167349	4.686925
2.358492	203.962327	4.691930
2.541982	193.601163	4.696934
2.406553	204.850146	4.701939
2.105339	201.628949	4.706944
2.531358	191.305954	4.711949
2.142707	197.760254	4.716954
2.076735	199.083444	4.721958
2.314622	216.842115	4.726963
2.590868	214.878737	4.731968
2.813001	214.866287	4.736973
2.564205	225.297720	4.741978
2.819443	216.070627	4.746982
3.157246	224.053784	4.751987
2.881105	214.824005	4.756992
2.596058	200.910204	4.761997
2.545749	192.546925	4.767002
2.668463	203.461493	4.772006
2.317640	194.252843	4.777011
2.274529	201.276591	4.782016
2.687163	204.012194	4.787021
2.433398	219.025411	4.792026
2.876357	211.034567	4.797030
3.051800	223.839148	4.802035
2.637606	216.026048	4.807040
3.036742	205.691412	4.812045
2.680080	201.732219	4.817050
2.875353	199.945962	4.822054
2.762860	195.746279	4.827059
2.306379	198.588726	4.832064
2.504641	203.891815	4.837069
2.367185	216.836854	4.842074
2.868518	214.658102	4.847078
3.173303	219.042960	4.852083
3.046890	220.827968	4.857088
3.080947	219.430634	4.862093
2.927266	221.330616	4.867098
3.044828	221.764709	4.872102
3.080441	223.255577	4.877107
2.793582	215.748512	4.882112
2.895353	211.341463	4.887117
2.797426	219.791083	4.892122
3.194080	218.492314	4.897126
2.808927	219.447593	4.902131
3.066161	223.156500	4.907136
3.378129	216.815347	4.912141
2.950668	211.753558	4.917146
2.616770	198.049840	4.922150
2.807743	213.218430	4.927155
2.969133	214.917499	4.932160
3.129655	224.567047	4.937165
3.104465	227.244274	4.942170
2.900775	215.813943	4.947174
2.968460	222.798303	4.952179
2.547955	225.679444	4.957184
3.003430	223.941255	4.962189
2.703045	223.345785	4.967194
2.790977	214.904026	4.972198
2.768585	218.843126	4.977203
3.047169	225.275807	4.982208
3.297334	228.979488	4.987213
3.214230	239.495861	4.992218
3.186735	232.644419	4.997222
3.249112	236.102099	5.002227
3.120727	242.901863	5.007232
3.436126	230.558652	5.012237
3.300790	236.476828	5.017242
2.946037	220.128333	5.022246
3.309564	240.515471	5.027251
3.267527	233.821313	5.032256
3.625539	236.527462	5.037261
3.107588	225.816756	5.042266
3.398087	228.346757	5.047270
3.412305	227.417573	5.052275
3.195528	226.733157	5.057280
3.340096	228.438011	5.062285
3.516427	234.323478	5.067290
3.458675	233.990781	5.072294
3.302937	229.503600	5.077299
3.270847	237.411479	5.082304
3.617120	241.312166	5.087309
3.395920	237.689371	5.092314
3.553050	236.766408	5.097318
3.540739	234.686608	5.102323
3.237282	238.305649	5.107328
3.653573	226.016334	5.112333
3.455635	238.863241	5.117338
3.425931	238.570469	5.122342
3.556036	246.703030	5.127347
3.695171	232.061949	5.132352
3.571162	212.754288	5.137357
3.544106	235.021351	5.142362
3.619933	227.220536	5.147366
3.485054	230.724745	5.152371
3.350201	238.892228	5.157376
3.448309	239.667865	5.162381
3.242824	241.683481	5.167386
3.409008	241.936001	5.172390
3.534643	249.366920	5.177395
3.387424	248.839349	5.182400
3.320803	239.459879	5.187405
3.395044	241.688202	5.192410
3.625676	240.535500	5.197414
3.706251	241.880168	5.202419
3.689712	245.682324	5.207424
3.735098	249.054068	5.212429
3.668883	243.790495	5.217434
3.652570	237.715578	5.222438
3.608751	239.513038	5.227443
4.105800	255.121216	5.232448
3.897168	248.430845	5.237453
3.709416	246.476433	5.242458
3.607842	235.008045	5.247462
3.820750	255.162392	5.252467
3.944659	263.261125	5.257472
3.973326	253.787719	5.262477
3.612118	251.847658	5.267482
4.264080	258.247526	5.272486
3.800281	252.362496	5.277491
3.724121	249.634587	5.282496
4.250490	254.171612	5.287501
3.918855	252.220619	5.292506
4.029744	240.934279	5.297510
3.869961	252.677455	5.302515
3.412969	248.822456	5.307520
3.773183	249.696486	5.312525
4.084352	274.097048	5.317530
3.963960	275.197766	5.322534
4.363582	278.036645	5.327539
4.154365	282.798935	5.332544
4.280899	271.291844	5.337549
3.994604	274.009731	5.342554
4.171475	257.818871	5.347558
4.058862	264.144798	5.352563
3.861512	270.243479	5.357568
4.384035	268.760597	5.362573
4.313265	273.678496	5.367578
4.205416	263.403780	5.372582
3.873406	249.775657	5.377587
4.300578	251.082180	5.382592
4.086897	254.060835	5.387597
4.083612	275.495360	5.392602
4.277470	263.898700	5.397606
4.367862	263.394243	5.402611
4.397441	264.525394	5.407616
4.325722	254.842995	5.412621
3.933021	255.033838	5.417626
4.027290	255.775273	5.422630
4.458686	261.061063	5.427635
4.136115	261.766160	5.432640
4.315481	255.584841	5.437645
4.260498	270.282419	5.442650
4.333691	263.250776	5.447654
4.511931	273.248762	5.452659
4.316409	277.404652	5.457664
4.516411	264.876908	5.462669
4.495447	269.603557	5.467674
4.620981	266.736676	5.472678
4.358647	254.315724	5.477683
3.873736	252.730274	5.482688
4.392249	264.193847	5.487693
4.430047	276.314393	5.492698
3.992070	274.708979	5.497702
4.353930	276.364188	5.502707
4.241764	271.509550	5.507712
4.255961	273.835809	5.512717
4.019081	274.359889	5.517722
4.626160	269.823531	5.522726
4.515471	267.157942	5.527731
4.495411	277.360807	5.532736
4.236535	271.307825	5.537741
4.306585	266.276126	5.542746
4.660704	273.345620	5.547750
4.462187	278.134716	5.552755
4.541319	278.508356	5.557760
4.640736	277.524776	5.562765
4.793220	291.038484	5.567770
4.848930	284.904881	5.572774
4.685841	269.190876	5.577779
4.470532	264.497830	5.582784
4.624048	266.305696	5.587789
4.241236	290.428360	5.592794
4.626028	279.004439	5.597798
4.837475	282.799580	5.602803
4.747059	281.798100	5.607808
5.289884	281.498443	5.612813
4.728902	277.988652	5.617818
4.320930	272.724498	5.622822
4.757595	278.401772	5.627827
4.598966	286.550832	5.632832
4.705554	290.722963	5.637837
4.589384	286.805399	5.642842
4.945755	283.586206	5.647846
4.851748	289.551747	5.652851
4.869308	295.651777	5.657856
4.849109	290.061492	5.662861
4.813602	293.018741	5.667866
4.617343	292.435530	5.672870
4.956794	296.701117	5.677875
4.801570	298.253341	5.682880
5.028757	279.783091	5.687885
5.262326	294.828061	5.692890
5.074047	294.354337	5.697894
4.819460	293.650496	5.702899
5.007650	296.604553	5.707904
5.177438	283.654400	5.712909
4.868616	290.070995	5.717914
4.704160	299.160587	5.722918
4.960985	290.834863	5.727923
4.846598	294.921178	5.732928
4.544410	287.856223	5.737933
4.688765	290.203347	5.742938
4.641359	289.103423	5.747942
5.143207	300.904967	5.752947
5.046025	310.221368	5.757952
5.608207	304.635315	5.762957
5.451491	306.814185	5.767962
4.770759	303.038301	5.772966
5.167311	290.381862	5.777971
4.969684	294.247024	5.782976
5.213287	290.725854	5.787981
5.273924	305.376986	5.792986
5.488969	304.119142	5.797990
4.883161	288.056441	5.802995
4.892528	299.615128	5.808000
5.382270	298.776415	5.813005
5.369021	307.570391	5.818010
5.526286	306.166521	5.823014
5.452074	293.111985	5.828019
5.010631	306.360679	5.833024
5.531995	297.775468	5.838029
5.302071	299.595582	5.843034
5.147289	286.123333	5.848038
5.395386	295.683355	5.853043
5.556119	294.630117	5.858048
5.317744	284.856593	5.863053
5.045998	297.041166	5.868058
5.419943	300.029577	5.873062
5.399655	308.973343	5.878067
5.540984	302.589126	5.883072
5.738722	310.018335	5.888077
5.398320	305.670616	5.893082
5.175257	293.983827	5.898086
5.204135	298.446464	5.903091
5.254195	311.969808	5.908096
5.688986	316.470488	5.913101
5.604351	312.905508	5.918106
5.702420	310.333957	5.923110
5.690458	315.695120	5.928115
5.440235	325.759845	5.933120
5.671159	313.958068	5.938125
5.363571	315.546671	5.943130
5.310391	307.996857	5.948134
5.182425	315.884897	5.953139
5.108383	321.347475	5.958144
5.394150	312.561660	5.963149
5.315143	319.812503	5.968154
5.224275	318.213152	5.973158
5.522590	318.831072	5.978163
5.464421	331.115291	5.983168
5.825130	340.221213	5.988173
5.901682	342.113836	5.993178
5.763466	335.576981	5.998182
5.585956	319.134361	6.003187
5.690287	331.462881	6.008192
5.823362	329.588220	6.013197
5.474707	331.673593	6.018202
5.580707	329.524741	6.023206
5.968493	333.757502	6.028211
5.817697	353.452904	6.033216
5.986240	330.350571	6.038221
6.085601	331.837851	6.043226
5.880803	322.831022	6.048230
5.733664	321.711824	6.053235
5.561094	318.315554	6.058240
5.731877	317.089910	6.063245
5.502762	315.578522	6.068250
5.571169	315.975978	6.073254
5.521796	325.879719	6.078259
5.696656	339.855045	6.083264
6.128708	336.124194	6.088269
5.820198	333.986097	6.093274
5.661963	319.704450	6.098278
5.876073	317.959540	6.103283
5.195871	324.263130	6.108288
5.635529	324.172521	6.113293
5.791340	341.105713	6.118298
6.047750	344.327563	6.123302
5.873295	325.631902	6.128307
5.640866	321.106019	6.133312
5.922420	315.392816	6.138317
5.442839	312.136095	6.143322
5.543832	321.500740	6.148326
5.835711	320.635886	6.153331
5.495707	333.274030	6.158336
5.995559	333.003208	6.163341
5.939305	338.241563	6.168346
5.756266	322.786877	6.173350
5.521674	323.443478	6.178355
5.447810	326.406704	6.183360
5.969302	328.922901	6.188365
5.912570	339.188458	6.193370
5.822721	333.194558	6.198374
5.662528	317.900832	6.203379
5.549851	324.138207	6.208384
5.678333	328.234172	6.213389
5.901338	331.840865	6.218394
5.651509	334.473990	6.223398
5.805688	326.388854	6.228403
5.615322	335.229402	6.233408
5.835335	323.821617	6.238413
5.607803	317.001287	6.243418
5.626349	323.914244	6.248422
6.089751	331.406502	6.253427
5.465752	339.292691	6.258432
5.939125	331.341350	6.263437
5.825140	327.980249	6.268442
5.653670	327.098953	6.273446
5.816887	317.433724	6.278451
5.522648	323.395651	6.283456
5.880903	318.338047	6.288461
5.580007	312.756657	6.293466
5.839877	322.985566	6.298470
5.832539	320.601266	6.303475
5.310214	320.125768	6.308480
5.960909	326.500548	6.313485
5.756895	333.068517	6.318490
5.743972	335.424316	6.323494
5.974620	334.031165	6.328499
5.714044	323.232872	6.333504
5.832201	316.266972	6.338509
5.635822	328.563217	6.343514
5.531492	314.463004	6.348518
5.850046	321.743696	6.353523
5.412580	329.822297	6.358528
5.936438	322.464204	6.363533
5.943688	335.684188	6.368538
5.968174	329.647179	6.373542
5.685555	315.365920	6.378547
5.625587	322.677073	6.383552
5.600741	318.881323	6.388557
5.512607	319.100675	6.393562
5.892486	325.650497	6.398566
5.588105	318.895914	6.403571
5.734527	340.465394	6.408576
5.816258	333.929095	6.413581
5.563800	329.178542	6.418586
5.482584	340.631137	6.423590
6.115580	344.265747	6.428595
5.649043	349.419289	6.433600
6.143598	335.314400	6.438605
5.984931	321.469411	6.443610
5.504331	320.892505	6.448614
5.500884	322.082584	6.453619
5.266545	325.662408	6.458624
5.657163	329.587848	6.463629
5.496154	343.783147	6.468634
5.694688	338.478326	6.473638
6.010493	337.543308	6.478643
5.565588	336.286974	6.483648
5.807171	336.379062	6.488653
6.139291	343.097675	6.493658
5.532634	340.297326	6.498662
5.644293	339.685154	6.503667
5.212067	350.357188	6.508672
5.508083	343.572391	6.513677
5.781357	343.276736	6.518682
5.714375	352.401798	6.523686
6.172534	341.668758	6.528691
5.991186	344.256422	6.533696
6.305165	337.547923	6.538701
5.927550	339.270815	6.543706
5.682100	333.146120	6.548710
5.628525	330.455810	6.553715
5.714424	335.295550	6.558720
5.684298	327.277074	6.563725
5.719770	329.049542	6.568730
5.635308	331.995437	6.573734
5.777398	325.804079	6.578739
5.628324	346.552719	6.583744
5.985209	338.666967	6.588749
5.477125	345.706219	6.593754
5.781976	337.537508	6.598758
6.102938	332.074424	6.603763
5.544108	337.327753	6.608768
5.570273	337.573602	6.613773
5.853796	339.278978	6.618778
5.734656	332.514531	6.623782
5.640316	337.217821	6.628787
5.737170	342.217206	6.633792
5.950087	333.218101	6.638797
5.528387	333.334367	6.643802
5.575460	336.332548	6.648806
5.738495	341.603199	6.653811
5.890117	346.344126	6.658816
5.858370	340.281067	6.663821
5.860582	331.223021	6.668826
5.736800	329.242821	6.673830
5.498277	319.978658	6.678835
5.912764	332.091212	6.683840
5.889765	334.030970	6.688845
5.635344	325.920867	6.693850
5.498407	326.467352	6.698854
5.809324	329.737660	6.703859
5.914214	336.020257	6.708864
5.900515	325.787792	6.713869
5.662002	322.072764	6.718874
5.723560	319.886541	6.723878
5.585168	323.770960	6.728883
5.832232	319.543739	6.733888
5.739342	308.703529	6.738893
5.580552	321.458980	6.743898
5.801869	326.299780	6.748902
5.809051	325.086952	6.753907
5.613139	336.019573	6.758912
5.722002	323.214917	6.763917
5.908981	321.736818	6.768922
5.823717	324.787239	6.773926
5.494445	319.390597	6.778931
5.557087	318.463359	6.783936
5.779470	328.027402	6.788941
6.011539	337.292555	6.793946
5.758782	330.567894	6.798950
5.574170	318.900412	6.803955
5.374969	324.198983	6.808960
5.889119	336.042927	6.813965
5.829037	343.581894	6.818970
5.999278	337.439931	6.823974
5.845912	318.990927	6.828979
5.338197	327.007699	6.833984
5.835656	333.877733	6.838989
5.803457	337.717147	6.843994
5.702862	334.360288	6.848998
5.747161	328.336013	6.854003
5.602314	329.060897	6.859008
5.955120	334.691135	6.864013
5.693590	321.298753	6.869018
5.682174	324.499025	6.874022
5.786885	312.498604	6.879027
5.404273	318.006060	6.884032
5.718062	327.315430	6.889037
5.861080	331.051634	6.894042
5.993908	335.241835	6.899046
5.961613	319.561205	6.904051
5.875264	320.922376	6.909056
5.581504	314.783064	6.914061
5.357577	308.895468	6.919066
5.624969	322.078102	6.924070
5.965098	330.775942	6.929075
5.702663	318.766242	6.934080
5.657042	314.524482	6.939085
5.524769	329.955467	6.944090
5.537920	340.159525	6.949094
6.024978	338.906782	6.954099
5.914465	332.887627	6.959104
6.091557	332.328541	6.964109
5.942666	326.356491	6.969114
5.462570	321.989389	6.974118
5.271048	325.214539	6.979123
5.724460	331.898444	6.984128
6.121593	331.368374	6.989133
5.783376	329.503817	6.994138
5.539832	325.568112	6.999142
5.400195	324.229450	7.004147
5.785110	335.919511	7.009152
5.964418	337.571511	7.014157
5.711607	338.667540	7.019162
5.603571	338.409108	7.024166
6.014376	338.601397	7.029171
6.019491	328.881686	7.034176
5.921157	325.072066	7.039181
5.647848	317.028183	7.044186
5.779564	317.656224	7.049190
5.592648	325.382607	7.054195
5.526402	329.606965	7.059200
5.788277	324.469454	7.064205
5.725538	320.179738	7.069210
5.524383	321.242414	7.074214
5.730390	311.279466	7.079219
5.794854	320.633979	7.084224
5.921218	321.038230	7.089229
5.859095	320.446788	7.094234
5.692926	326.961407	7.099238
5.588866	319.391036	7.104243
5.642519	320.157779	7.109248
5.570023	312.240817	7.114253
5.783269	316.083141	7.119258
5.869820	320.476693	7.124262
6.022486	320.130215	7.129267
6.083937	321.585432	7.134272
5.999037	318.548830	7.139277
6.378311	325.453080	7.144282
6.222542	317.166273	7.149286
6.150897	313.118387	7.154291
6.070194	310.046332	7.159296
5.505035	302.459176	7.164301
5.705520	294.110585	7.169306
5.587131	305.771422	7.174310
5.725998	312.668806	7.179315
5.857257	328.995216	7.184320
5.825005	311.514438	7.189325
5.819659	303.859103	7.194330
5.427234	303.062828	7.199334
5.517909	307.778433	7.204339
5.704331	308.486540	7.209344
5.632746	317.390842	7.214349
5.875385	313.012453	7.219354
5.439496	316.009897	7.224358
5.512092	307.602119	7.229363
5.391919	318.760215	7.234368
5.379499	315.395958	7.239373
5.653223	312.271884	7.244378
5.492914	316.922166	7.249382
5.820146	317.560894	7.254387
5.492324	324.477161	7.259392
5.288166	314.407232	7.264397
5.516563	321.800036	7.269402
5.721410	330.439846	7.274406
5.927540	339.297756	7.279411
5.808615	327.177123	7.284416
5.889759	319.884795	7.289421
5.610296	324.575777	7.294426
5.394186	322.553006	7.299430
5.768552	329.628862	7.304435
5.860125	340.905862	7.309440
6.082515	335.673256	7.314445
5.488533	330.450700	7.319450
5.510848	326.397673	7.324454
5.970763	326.721519	7.329459
5.890933	326.186617	7.334464
5.509046	318.887290	7.339469
5.576621	317.949793	7.344474
5.702985	333.138035	7.349478
6.228402	329.519197	7.354483
5.823497	329.256367	7.359488
6.100623	320.614261	7.364493
6.058322	315.732915	7.369498
5.516052	323.862631	7.374502
5.474822	310.410648	7.379507
5.890238	311.238123	7.384512
5.488956	325.799842	7.389517
6.025235	321.669958	7.394522
5.529308	328.821204	7.399526
5.940994	318.253598	7.404531
5.745552	324.817066	7.409536
6.070331	315.148830	7.414541
5.579865	317.806765	7.419546
5.573042	316.963108	7.424550
5.663736	316.284599	7.429555
5.655482	321.730607	7.434560
5.544802	314.974341	7.439565
5.672316	317.577186	7.444570
5.420038	326.180601	7.449574
5.829108	318.058946	7.454579
5.769406	320.766870	7.459584
5.635635	323.979864	7.464589
5.776888	323.745893	7.469594
5.432101	318.740803	7.474598
6.015359	331.001083	7.479603
5.826583	327.445986	7.484608
6.075391	316.944869	7.489613
5.620587	316.844830	7.494618
5.645589	316.847254	7.499622
5.801182	319.217941	7.504627
5.633734	318.861194	7.509632
5.740847	312.985329	7.514637
5.845014	320.928977	7.519642
5.660339	318.388792	7.524646
5.974955	309.332737	7.529651
6.137201	316.824422	7.534656
5.669254	316.011432	7.539661
5.834774	316.741776	7.544666
5.746521	315.698829	7.549670
5.543036	319.065043	7.554675
5.611528	322.936233	7.559680
5.618465	324.355646	7.564685
5.809399	319.896723	7.569690
5.425119	319.953379	7.574694
5.569938	324.799761	7.579699
5.321379	324.680265	7.584704
5.855678	327.937939	7.589709
5.815960	342.743930	7.594714
5.758101	335.122067	7.599718
5.743396	329.043704	7.604723
5.350470	333.322090	7.609728
6.102148	335.289928	7.614733
5.761341	330.891646	7.619738
5.543013	328.805946	7.624742
6.328271	332.179568	7.629747
5.846154	324.993919	7.634752
5.483242	328.596925	7.639757
5.711027	322.215058	7.644762
5.158873	323.332384	7.649766
5.745859	331.349557	7.654771
5.872857	340.770273	7.659776
5.465459	348.065929	7.664781
5.805263	347.342306	7.669786
5.776890	353.386233	7.674790
6.105306	346.729266	7.679795
5.702186	340.752502	7.684800
5.688934	328.555304	7.689805
5.681652	326.914465	7.694810
5.658140	332.021171	7.699814
5.868552	341.103039	7.704819
5.754808	326.760677	7.709824
5.463326	328.707435	7.714829
5.834702	330.620591	7.719834
5.749603	344.696506	7.724838
6.133264	333.184143	7.729843
5.844226	330.454565	7.734848
5.636393	328.803822	7.739853
5.740479	324.696936	7.744858
5.433683	328.129856	7.749862
5.801159	318.989637	7.754867
5.844274	327.331928	7.759872
5.507959	321.879435	7.764877
5.547630	317.611740	7.769882
5.668777	339.378139	7.774886
6.180859	331.360661	7.779891
5.887216	334.842154	7.784896
5.494811	325.864534	7.789901
5.741754	320.163045	7.794906
5.515041	323.918849	7.799910
6.134409	325.454876	7.804915
5.569933	324.002029	7.809920
6.019705	324.469820	7.814925
5.971099	327.267765	7.819930
5.671833	322.068927	7.824934
6.121390	314.611676	7.829939
5.847475	327.704590	7.834944
5.663508	327.388379	7.839949
5.461948	314.049940	7.844954
5.504573	318.444003	7.849958
5.712623	310.821878	7.854963
5.817843	311.732450	7.859968
5.846330	318.691313	7.864973
5.908675	318.570866	7.869978
5.436614	323.630351	7.874982
5.502896	313.923270	7.879987
5.543286	322.787995	7.884992
5.337149	317.960631	7.889997
5.499751	327.739622	7.895002
6.109177	346.373869	7.900006
6.027503	337.958458	7.905011
5.673476	330.860429	7.910016
5.622748	324.620000	7.915021
5.905544	332.706681	7.920026
5.283544	326.953823	7.925030
5.983996	331.093610	7.930035
6.076393	338.365229	7.935040
5.473935	325.883289	7.940045
5.539574	322.389821	7.945050
5.653904	329.506163	7.950054
5.798631	331.324896	7.955059
6.062195	338.879908	7.960064
5.876791	318.297227	7.965069
5.569707	309.878960	7.970074
5.851566	313.840312	7.975078
5.604400	311.575609	7.980083
5.839422	311.719338	7.985088
5.708404	323.353680	7.990093
5.782343	315.474028	7.995098
5.632991	322.852881	8.000102
5.648313	312.859511	8.005107
5.459362	327.011691	8.010112
5.615986	346.610240	8.015130
5.849481	340.272069	8.020147
5.774403	337.266959	8.025165
6.009764	338.312687	8.030182
6.008785	342.058570	8.035200
5.613458	325.133326	8.040218
5.618302	319.799541	8.045235
5.835216	335.509217	8.050253
6.276010	328.554981	8.055270
5.949457	326.466294	8.060288
5.650937	324.732984	8.065306
5.910176	317.560881	8.070323
5.548045	311.182919	8.075341
5.257058	316.400295	8.080358
5.726367	333.200388	8.085376
5.899816	333.681429	8.090394
6.009650	330.808468	8.095411
5.882479	332.822619	8.100429
5.868843	327.901942	8.105446
5.846745	326.441158	8.110464
5.323220	327.396769	8.115482
5.773893	332.741659	8.120499
5.752679	336.992437	8.125517
5.881045	345.356966	8.130534
5.844537	340.443002	8.135552
5.556288	343.817068	8.140570
5.956562	328.137496	8.145587
5.997292	331.605497	8.150605
6.002316	335.741742	8.155622
6.252648	335.055851	8.160640
5.641514	345.592992	8.165658
6.187084	336.612299	8.170675
5.969421	339.442072	8.175693
6.030403	334.036429	8.180710
5.494210	327.202751	8.185728
5.691574	337.557206	8.190746
6.189269	330.288014	8.195763
6.060218	347.389554	8.200781
6.320698	341.369056	8.205798
5.992845	335.039395	8.210816
5.694325	329.459366	8.215834
5.620920	329.735858	8.220851
5.576125	346.739077	8.225869
5.844365	340.584834	8.230886
6.050240	338.406937	8.235904
6.193500	336.645866	8.240922
6.135591	344.827970	8.245939
5.868815	343.509416	8.250957
6.280672	346.982750	8.255974
6.139803	346.900537	8.260992
5.807516	347.087954	8.266010
5.920002	345.107624	8.271027
6.097835	346.440005	8.276045
6.131764	345.768873	8.281062
6.245506	345.126337	8.286080
5.886671	341.559524	8.291098
5.965084	334.204140	8.296115
6.158967	340.409480	8.301133
5.942425	341.424587	8.306150
5.975924	340.119238	8.311168
6.023736	347.802071	8.316186
5.756322	345.410700	8.321203
5.745630	346.355889	8.326221
6.073404	351.719920	8.331238
6.320874	353.123507	8.336256
5.978203	348.859936	8.341274
6.196204	338.033705	8.346291
6.184635	349.282186	8.351309
5.973659	345.149582	8.356326
6.165090	346.000189	8.361344
5.697967	343.150788	8.366362
6.072783	342.909393	8.371379
6.068094	348.520836	8.376397
5.924119	339.047930	8.381414
6.307447	341.661061	8.386432
5.852938	344.997900	8.391450
6.296439	354.430464	8.396467
6.740240	353.648182	8.401485
6.208196	351.547306	8.406502
6.669139	351.317747	8.411520
6.295509	346.563561	8.416538
6.255862	343.439332	8.421555
5.805105	333.076970	8.426573
6.191320	340.388392	8.431590
6.230292	343.951339	8.436608
6.061137	346.795649	8.441626
6.129521	347.103711	8.446643
6.518228	347.936226	8.451661
5.881236	349.490142	8.456678
6.030754	344.402054	8.461696
6.363270	348.190683	8.466714
6.171655	347.437908	8.471731
6.297937	347.361434	8.476749
6.337419	350.974793	8.481766
6.360942	347.607210	8.486784
6.213864	349.040669	8.491802
6.344071	347.739197	8.496819
6.145888	349.010209	8.501837
6.100431	343.614824	8.506854
6.218390	349.282907	8.511872
6.006042	351.313477	8.516890
6.096131	344.972387	8.521907
6.021754	349.114686	8.526925
6.272280	349.110381	8.531942
6.453127	348.473176	8.536960
6.071086	347.292482	8.541978
6.093414	349.734614	8.546995
6.275724	348.308271	8.552013
5.776167	351.125134	8.557030
6.055530	340.251480	8.562048
6.023910	346.078543	8.567066
6.143402	350.178035	8.572083
6.196556	359.573553	8.577101
6.189461	373.415289	8.582119
6.817377	364.311313	8.587136
6.482470	361.188873	8.592154
6.328061	355.700001	8.597171
6.415457	351.110707	8.602189
6.386612	354.807285	8.607207
6.139340	352.097212	8.612224
6.156552	351.734779	8.617242
6.540059	362.539924	8.622259
6.429513	372.125029	8.627277
6.622303	368.548061	8.632295
6.661407	360.520324	8.637312
6.231720	356.743645	8.642330
6.237606	355.310058	8.647347
6.345022	355.350125	8.652365
6.390760	367.608966	8.657383
6.664754	360.207342	8.662400
6.004836	362.089859	8.667418
6.222218	362.119116	8.672435
6.427308	366.000168	8.677453
6.589922	375.328161	8.682471
6.954021	360.193808	8.687488
6.562519	368.954854	8.692506
6.140940	345.542525	8.697523
6.289543	353.613589	8.702541
6.309426	360.732761	8.707559
6.757152	365.778335	8.712576
6.824922	372.015943	8.717594
6.604694	366.723498	8.722611
6.310341	348.962044	8.727629
6.512119	361.818247	8.732647
6.649174	363.491477	8.737664
6.223392	352.973744	8.742682
6.373364	358.946097	8.747699
6.633487	356.418943	8.752717
6.621741	370.371848	8.757735
6.845376	359.178673	8.762752
6.475595	354.206147	8.767770
6.605435	361.974039	8.772787
6.390988	347.043378	8.777805
6.087709	352.903272	8.782823
6.621901	358.774781	8.787840
6.511507	362.711263	8.792858
6.651592	363.453107	8.797875
6.938338	366.668228	8.802893
6.795634	369.827144	8.807911
6.591640	356.002477	8.812928
6.600175	363.590452	8.817946
6.907889	349.660874	8.822963
6.828023	351.743397	8.827981
6.388101	350.697941	8.832999
6.745171	339.360933	8.838016
6.269182	346.118671	8.843034
6.528605	345.844752	8.848051
7.077034	363.850631	8.853069
6.777586	352.429650	8.858087
6.635924	347.734016	8.863104
6.705475	343.784942	8.868122
5.999280	347.173590	8.873139
6.614891	348.147493	8.878157
6.631783	364.027184	8.883175
7.161696	368.413056	8.888192
7.071688	354.659001	8.893210
6.662052	341.128282	8.898227
6.667097	335.819707	8.903245
6.179759	344.330589	8.908263
6.354492	360.624335	8.913280
6.644303	367.540545	8.918298
6.524634	369.509353	8.923315
6.659842	366.114911	8.928333
6.444010	377.035469	8.933351
6.729915	364.620829	8.938368
6.676681	365.373838	8.943386
6.535989	372.843046	8.948403
6.735181	365.866456	8.953421
6.773136	367.618228	8.958439
6.924468	368.307830	8.963456
6.819054	363.994693	8.968474
6.773819	360.079265	8.973491
6.912830	366.602409	8.978509
6.914088	370.578311	8.983527
6.969889	373.611651	8.988544
6.941268	371.517595	8.993562
6.516523	367.686498	8.998579
6.680340	370.548394	9.003597
6.674094	369.015715	9.008615
6.916257	359.662549	9.013632
6.459417	368.941826	9.018650
6.715830	362.508565	9.023667
7.001807	368.756377	9.028685
6.943729	365.947421	9.033703
6.918104	371.325458	9.038720
6.799647	368.734175	9.043738
6.766237	368.524783	9.048755
7.154969	364.822639	9.053773
7.000726	371.609182	9.058791
6.938372	367.519702	9.063808
7.079940	370.426085	9.068826
6.937589	367.320997	9.073843
7.107412	357.745579	9.078861
6.727067	360.007423	9.083879
6.670845	371.225002	9.088896
7.127494	365.480050	9.093914
6.922866	361.898691	9.098931
7.218003	361.369916	9.103949
7.013611	362.875413	9.108967
6.886788	363.551521	9.113984
6.974697	362.853050	9.119002
6.880349	370.176193	9.124019
7.321840	367.175854	9.129037
7.030935	365.384553	9.134055
6.782359	370.194574	9.139072
7.087466	363.618039	9.144090
6.966517	368.360854	9.149107
6.999362	361.738351	9.154125
6.787277	360.890938	9.159143
6.878148	366.664224	9.164160
7.044090	367.200081	9.169178
7.140998	355.556448	9.174195
6.846316	363.027539	9.179213
6.804439	361.800193	9.184231
6.718127	355.615945	9.189248
7.257066	364.604488	9.194266
7.031216	366.921170	9.199283
7.263304	366.607328	9.204301
7.024225	361.614450	9.209319
6.938555	365.259921	9.214336
6.840211	359.629781	9.219354
6.872919	383.629646	9.224371
7.160385	371.299961	9.229389
7.276329	391.045694	9.234407
7.358771	382.900751	9.239424
7.603168	384.898080	9.244442
7.011105	376.946516	9.249459
7.145640	367.417609	9.254477
6.717348	362.987494	9.259495
7.148040	379.446523	9.264512
7.761874	377.782586	9.269530
7.150030	368.145837	9.274547
6.946532	359.098733	9.279565
7.069882	365.955657	9.284583
6.957550	369.494832	9.289600
7.094971	376.207566	9.294618
7.011867	385.406573	9.299635
7.173769	380.985543	9.304653
7.162549	387.475284	9.309671
6.944725	383.359515	9.314688
7.000792	384.578321	9.319706
6.803374	389.446651	9.324723
7.709435	391.498744	9.329741
7.380668	386.778586	9.334759
7.086372	389.844348	9.339776
7.412408	383.299259	9.344794
7.107937	386.839951	9.349811
7.423343	384.029645	9.354829
7.171814	389.401836	9.359847
7.347925	383.921452	9.364864
7.694497	385.035070	9.369882
7.462757	396.352572	9.374899
7.277384	391.663733	9.379917
7.213435	384.993179	9.384935
7.144393	394.922111	9.389952
7.582579	387.207748	9.394970
7.007155	390.860052	9.399987
7.259539	394.194131	9.405005
7.753932	388.623167	9.410023
7.539097	382.799729	9.415040
7.834221	377.597448	9.420058
7.300332	380.463839	9.425075
7.300174	385.774802	9.430093
7.278430	390.656804	9.435111
6.895209	384.566108	9.440128
7.684040	378.927215	9.445146
7.287959	387.865699	9.450163
7.098870	385.481061	9.455181
7.574094	381.270010	9.460199
7.568726	387.597902	9.465216
7.502386	390.839601	9.470234
7.411908	377.385389	9.475251
7.481775	383.704721	9.480269
7.513045	385.788878	9.485287
7.547505	395.171547	9.490304
7.432826	380.108566	9.495322
7.510907	386.029009	9.500339
7.471472	386.114030	9.505357
7.511181	380.509724	9.510375
7.437130	395.112944	9.515392
7.318664	385.913739	9.520410
7.148961	388.997970	9.525427
7.303365	384.612819	9.530445
7.473539	383.737445	9.535463
7.572137	387.095467	9.540480
7.606245	374.527529	9.545498
7.486427	378.077338	9.550515
7.644756	376.528501	9.555533
7.911011	376.701619	9.560551
7.439713	383.474419	9.565568
7.395150	379.710353	9.570586
7.283176	387.661065	9.575603
7.431671	379.064050	9.580621
7.380003	381.602910	9.585639
7.076716	379.996563	9.590656
7.257027	382.142717	9.595674
7.199129	395.430675	9.600691
7.565340	401.079056	9.605709
7.695741	411.573362	9.610727
7.440217	417.883411	9.615744
7.903229	404.544964	9.620762
7.749562	414.237786	9.625779
7.853366	414.022808	9.630797
7.761284	409.546645	9.635815
7.491961	397.931605	9.640832
7.709900	394.069864	9.645850
7.607063	389.945657	9.650867
7.564833	401.176855	9.655885
7.570489	404.691356	9.660903
7.661667	413.484564	9.665920
7.690508	412.091578	9.670938
7.854392	416.745879	9.675955
7.784420	413.146700	9.680973
7.633310	411.314695	9.685991
7.626597	417.125280	9.691008
8.099043	404.369159	9.696026
7.557315	421.415108	9.701043
7.496643	415.031197	9.706061
7.748398	410.435232	9.711079
7.578632	408.300034	9.716096
7.685211	405.099381	9.721114
7.872316	411.826482	9.726131
7.993917	409.144171	9.731149
7.896790	406.637920	9.736167
7.520026	413.702110	9.741184
7.748566	409.586263	9.746202
7.768778	408.137819	9.751219
7.805451	410.530391	9.756237
7.945027	412.080163	9.761255
7.992408	419.557976	9.766272
7.987192	403.995117	9.771290
7.983453	419.032356	9.776307
7.744548	415.184937	9.781325
8.136942	406.726651	9.786343
7.881619	419.685621	9.791360
8.051493	409.154005	9.796378
7.942386	395.768947	9.801395
7.535075	389.978631	9.806413
7.822688	394.026712	9.811431
7.660205	407.674928	9.816448
7.992552	409.456605	9.821466
7.992071	403.230576	9.826483
7.925875	402.764369	9.831501
7.983808	404.954825	9.836519
7.868882	406.200255	9.841536
8.108969	398.652423	9.846554
7.858454	400.285018	9.851571
7.845031	407.333659	9.856589
8.111685	400.510645	9.861607
7.766679	411.811080	9.866624
8.060828	397.870954	9.871642
8.124577	403.389712	9.876659
7.993014	402.002767	9.881677
8.040873	406.602551	9.886695
8.108319	410.069564	9.891712
8.145779	410.246748	9.896730
8.251995	413.329048	9.901747
7.974501	412.924140	9.906765
8.298835	403.375130	9.911783
7.689374	398.370485	9.916800
7.812945	404.785599	9.921818
7.770091	409.784497	9.926835
7.835793	410.115067	9.931853
7.885566	406.610848	9.936871
7.713515	416.953442	9.941888
7.699521	409.542990	9.946906
8.105273	407.709487	9.951923
7.852058	400.636071	9.956941
7.591764	405.586775	9.961959
8.052026	425.105377	9.966976
8.097549	431.595766	9.971994
8.168201	435.706038	9.977011
8.242687	434.709866	9.982029
8.215747	426.263214	9.987047
8.451752	439.489667	9.992064
8.137472	431.012013	9.997082
8.043329	426.810709	10.002099
8.101281	433.236051	10.007117
8.341194	428.815486	10.012135
8.198227	439.336592	10.017152
8.251586	432.294323	10.022170
7.892211	425.313162	10.027187
8.023742	438.675795	10.032205
8.590808	432.026892	10.037223
8.231971	435.935803	10.042240
8.050420	439.630929	10.047258
8.487138	433.573493	10.052275
8.189693	429.255526	10.057293
8.667725	429.266290	10.062311
8.098610	426.707297	10.067328
8.458115	417.345299	10.072346
8.412970	409.188652	10.077363
7.679801	420.776735	10.082381
8.362192	424.558241	10.087399
8.659364	435.351628	10.092416
8.210106	421.763903	10.097434
8.490103	425.658551	10.102451
8.566375	433.488461	10.107469
8.417224	415.126848	10.112487
8.225155	412.288257	10.117504
8.130767	409.431302	10.122522
8.098884	410.013739	10.127539
8.286272	433.273256	10.132557
8.287236	425.655351	10.137575
8.438949	434.133046	10.142592
8.280193	424.510925	10.147610
8.526058	420.155704	10.152627
8.255299	430.217043	10.157645
8.597681	432.233833	10.162663
8.622766	435.145740	10.167680
8.659006	429.428356	10.172698
8.847839	427.571822	10.177715
8.032828	423.952948	10.182733
8.461021	426.824181	10.187751
8.284911	430.108223	10.192768
8.362538	440.998908	10.197786
8.442601	430.774738	10.202803
8.269420	436.109499	10.207821
8.304543	429.631776	10.212839
8.451302	439.470332	10.217856
8.493689	440.053829	10.222874
8.282991	421.894287	10.227891
8.152804	443.401386	10.232909
8.267189	425.017666	10.237927
8.409858	429.356553	10.242944
8.415148	428.046123	10.247962
8.729297	423.481464	10.252979
8.527746	431.910024	10.257997
8.630633	436.094168	10.263015
8.562551	432.346375	10.268032
8.280125	440.737041	10.273050
8.826779	437.938056	10.278067
8.240967	441.415271	10.283085
8.526431	435.229912	10.288103
8.506039	447.880939	10.293120
8.715412	451.322707	10.298138
9.016184	450.644737	10.303155
8.536529	452.540220	10.308173
8.295356	442.968789	10.313191
8.347103	455.820018	10.318208
8.501319	463.994395	10.323226
9.001983	460.419964	10.328243
8.707031	473.770134	10.333261
8.663765	468.478508	10.338279
9.162757	476.157418	10.343296
8.869510	462.160382	10.348314
8.753717	449.962852	10.353331
8.654298	442.635111	10.358349
8.874709	426.352326	10.363367
8.401730	434.346644	10.368384
8.553189	448.034369	10.373402
8.832229	440.379474	10.378419
8.380433	457.301007	10.383437
8.577992	462.357158	10.388455
9.064339	457.923462	10.393472
8.742698	462.028550	10.398490
9.184277	463.777446	10.403507
8.869475	470.876191	10.408525
9.068342	463.912235	10.413543
8.874253	445.661725	10.418560
8.360924	454.208262	10.423578
8.547936	448.085563	10.428595
8.531678	467.003092	10.433613
8.926699	446.455054	10.438631
9.255254	460.525451	10.443648
9.134015	473.753905	10.448666
9.117418	454.024147	10.453683
9.225772	454.755157	10.458701
9.011674	442.752810	10.463719
8.802013	438.335971	10.468736
8.826549	436.789026	10.473754
8.808110	423.948381	10.478771
8.792897	435.219573	10.483789
8.868368	442.087138	10.488807
8.793486	460.701378	10.493824
8.825497	454.678546	10.498842
9.010348	456.726177	10.503859
9.214082	458.837137	10.508877
9.010341	464.378627	10.513895
9.261762	455.538342	10.518912
8.663372	444.416298	10.523930
8.911480	448.612547	10.528947
8.873629	453.222532	10.533965
8.925320	466.187382	10.538983
8.658787	459.889152	10.544000
8.577514	455.165154	10.549018
8.922941	452.375408	10.554035
9.007046	455.013054	10.559053
8.992085	468.985471	10.564071
9.051023	455.700431	10.569088
9.222053	456.323857	10.574106
9.236351	452.812530	10.579123
8.887237	460.569834	10.584141
8.698840	460.857920	10.589159
9.094848	459.707551	10.594176
9.065316	461.359392	10.599194
8.941852	463.436093	10.604211
9.359720	459.603167	10.609229
9.072316	462.131407	10.614247
9.073722	455.551632	10.619264
8.862354	471.643675	10.624282
9.165981	470.170033	10.629299
9.476927	474.151387	10.634317
9.331298	468.194076	10.639335
9.255467	457.716464	10.644352
9.180456	467.400225	10.649370
9.315671	461.856759	10.654387
9.198284	458.403802	10.659405
9.299765	457.706370	10.664423
9.653613	451.541915	10.669440
9.430592	456.531009	10.674458
9.054264	458.445118	10.679475
9.258691	459.170637	10.684493
9.334833	455.504520	10.689511
9.357729	459.805261	10.694528
9.293411	460.926056	10.699546
9.444784	457.690018	10.704563
9.051364	459.376425	10.709581
9.408044	461.867497	10.714599
9.241601	457.999320	10.719616
9.036003	459.132644	10.724634
9.560769	459.934514	10.729651
9.348956	460.459765	10.734669
9.229903	454.996914	10.739687
9.689491	450.438004	10.744704
9.347713	453.779401	10.749722
9.350435	449.269534	10.754739
9.344994	459.803952	10.759757
9.316660	457.135512	10.764775
9.968828	454.477879	10.769792
9.678080	452.576097	10.774810
9.578611	445.560773	10.779827
9.740332	447.492089	10.784845
9.108958	456.382039	10.789863
9.563734	453.325971	10.794880
9.512921	459.708299	10.799898
9.902478	460.565932	10.804915
9.548849	454.694656	10.809933
9.040211	462.404218	10.814951
9.476305	454.393520	10.819968
9.239850	453.335312	10.824986
9.386326	447.070608	10.830003
9.567268	446.679526	10.835021
9.470903	453.760032	10.840039
9.605666	448.693146	10.845056
9.506993	455.259640	10.850074
9.478808	456.567305	10.855091
9.604287	455.749376	10.860109
9.424520	451.813850	10.865127
9.569369	445.596736	10.870144
9.360741	459.842283	10.875162
9.259691	453.852791	10.880179
9.626044	450.674797	10.885197
9.557147	455.611493	10.890215
9.675916	446.413187	10.895232
9.469582	442.819455	10.900250
9.479887	455.203788	10.905267
9.508969	469.999286	10.910285
9.495883	473.381024	10.915303
9.887696	470.795483	10.920320
9.797795	474.350120	10.925338
9.668393	485.310934	10.930355
10.014975	476.582049	10.935373
9.567738	463.861784	10.940391
9.731840	458.465294	10.945408
9.687716	476.049173	10.950426
9.641953	478.530326	10.955443
10.105070	470.761555	10.960461
9.929448	467.724743	10.965479
9.881773	453.512761	10.970496
9.409242	456.117159	10.975514
9.459597	469.830110	10.980531
9.825254	471.038587	10.985549
9.611460	481.936803	10.990567
9.904945	478.950022	10.995584
9.662505	487.296615	11.000602
9.703302	477.381476	11.005619
9.890862	476.790555	11.010637
9.793078	482.006299	11.015655
9.835928	479.740163	11.020672
9.807477	484.998759	11.025690
9.428182	480.235952	11.030707
9.802528	475.179091	11.035725
9.658472	486.808032	11.040743
9.524405	472.473793	11.045760
9.896615	474.255581	11.050778
9.659184	481.774609	11.055795
9.782310	476.472852	11.060813
9.501385	489.123448	11.065831
9.800381	490.714674	11.070848
9.825672	502.834788	11.075866
9.834258	505.831323	11.080883
10.187932	502.368128	11.085901
9.926775	500.701564	11.090919
10.252526	494.522535	11.095936
10.501516	508.286637	11.100954
10.363299	501.397238	11.105971
10.254001	481.337916	11.110989
10.106336	482.017274	11.116007
9.735442	474.129057	11.121024
9.944313	477.722380	11.126042
9.793742	478.228628	11.131059
9.818439	477.003532	11.136077
9.718429	490.304429	11.141095
10.080061	499.137619	11.146112
10.005320	496.738317	11.151130
10.102637	502.232945	11.156147
10.309328	506.126402	11.161165
10.287371	509.938699	11.166183
10.431666	508.679201	11.171200
10.316158	506.810086	11.176218
9.931388	504.872447	11.181235
10.202849	500.838254	11.186253
10.209963	505.924069	11.191271
10.278859	506.493974	11.196288
10.520769	513.259916	11.201306
10.150664	498.018862	11.206323
10.162707	492.393584	11.211341
9.919638	493.021527	11.216359
10.246716	499.578552	11.221376
10.263049	505.675900	11.226394
10.409000	510.506580	11.231411
10.650825	493.718648	11.236429
9.975128	497.424453	11.241447
9.871590	500.255416	11.246464
10.429169	502.973979	11.251482
10.615786	512.178392	11.256499
10.144066	492.639367	11.261517
10.389036	502.901304	11.266535
10.703251	493.508450	11.271552
10.183184	494.147964	11.276570
9.986454	498.489221	11.281587
10.332317	501.458488	11.286605
10.195953	509.883246	11.291623
10.331846	496.573571	11.296640
10.477967	509.400679	11.301658
10.146858	510.424166	11.306675
10.438895	504.136780	11.311693
10.263603	500.225791	11.316711
10.396849	505.673803	11.321728
10.422842	510.191815	11.326746
10.593754	506.993750	11.331763
10.473873	505.961567	11.336781
10.219829	508.235322	11.341799
10.301742	504.571453	11.346816
10.153710	507.052754	11.351834
10.063435	503.661835	11.356851
10.436829	489.826060	11.361869
10.190462	510.941092	11.366887
10.417271	505.591627	11.371904
10.367803	507.145595	11.376922
10.283381	531.375325	11.381939
10.911770	526.269429	11.386957
10.766013	535.954775	11.391975
10.413028	518.748210	11.396992
10.559879	513.231319	11.402010
10.644000	522.035147	11.407027
10.658571	519.047605	11.412045
10.338958	519.946232	11.417063
10.550700	525.921647	11.422080
11.045092	525.926710	11.427098
10.653505	528.000985	11.432115
10.663526	510.176201	11.437133
10.284218	516.120566	11.442151
11.034027	525.076360	11.447168
10.910455	513.902434	11.452186
10.562375	506.332528	11.457203
10.588755	510.932527	11.462221
10.767463	510.308272	11.467239
10.864991	504.694925	11.472256
10.635835	508.700421	11.477274
10.370091	516.204938	11.482291
10.834741	520.976534	11.487309
10.853262	520.989418	11.492327
10.927053	524.594315	11.497344
10.923007	519.085137	11.502362
10.567622	511.380673	11.507379
10.851935	501.519119	11.512397
10.759879	507.033766	11.517415
10.755571	517.653246	11.522432
10.962119	518.627735	11.527450
10.744924	530.984428	11.532467
10.939001	527.192642	11.537485
11.208282	523.247143	11.542503
11.138905	519.521623	11.547520
10.908391	505.082459	11.552538
10.534048	509.647023	11.557555
10.721789	510.832714	11.562573
10.680878	498.907501	11.567591
10.938167	518.943781	11.572608
11.261773	525.394064	11.577626
10.672004	522.450124	11.582643
11.170870	515.644558	11.587661
10.771783	529.512734	11.592679
10.833731	529.872292	11.597696
11.219315	529.275784	11.602714
10.997592	531.664425	11.607731
10.896404	530.436835	11.612749
11.049414	527.778017	11.617767
11.172386	533.899795	11.622784
11.231135	525.909948	11.627802
10.753876	512.102461	11.632819
10.969488	518.459107	11.637837
11.399099	525.347301	11.642855
11.021236	527.116495	11.647872
11.245689	520.281072	11.652890
10.372708	525.929934	11.657907
10.925423	529.188878	11.662925
11.033981	524.384815	11.667943
11.023067	528.981159	11.672960
11.381767	523.163048	11.677978
10.819690	532.373591	11.682995
10.994247	528.297678	11.688013
11.072474	522.172957	11.693031
11.152117	532.454341	11.698048
11.008412	530.554901	11.703066
10.533838	536.170137	11.708083
11.080357	525.106460	11.713101
10.977209	532.285880	11.718119
11.293790	550.220753	11.723136
11.755492	551.490019	11.728154
11.447038	548.234044	11.733171
11.145966	541.543548	11.738189
11.043906	525.175186	11.743207
11.105697	536.320849	11.748224
11.423725	544.737990	11.753242
11.332354	553.370350	11.758259
11.435699	541.252243	11.763277
11.649846	535.153690	11.768295
11.190057	524.234068	11.773312
10.926662	522.978087	11.778330
11.378775	538.294732	11.783347
11.702395	547.496767	11.788365
11.558559	538.591754	11.793383
10.960492	530.442248	11.798400
11.466406	545.873594	11.803418
11.406028	557.281278	11.808435
11.228516	546.052617	11.813453
11.565574	555.094779	11.818471
11.202777	551.522229	11.823488
11.708939	558.767732	11.828506
11.768141	555.429267	11.833523
11.432124	549.378500	11.838541
11.362649	534.737521	11.843559
11.169165	546.689763	11.848576
11.620081	539.607643	11.853594
11.803306	554.745270	11.858611
11.296179	555.786698	11.863629
11.595444	548.725030	11.868647
11.481910	560.219884	11.873664
11.637333	553.376261	11.878682
11.549410	564.942867	11.883699
11.310101	555.055517	11.888717
11.461423	549.361200	11.893735
11.735439	549.624627	11.898752
11.807398	552.832200	11.903770
11.720537	559.068704	11.908787
11.514150	556.860298	11.913805
11.564513	548.543556	11.918823
11.739122	554.837174	11.923840
11.743660	553.747750	11.928858
11.551479	554.973662	11.933875
11.656616	549.744108	11.938893
11.820954	547.512696	11.943911
11.523567	558.244099	11.948928
11.795709	547.507138	11.953946
11.492863	551.416824	11.958963
11.695206	550.331314	11.963981
11.632289	549.075675	11.968999
11.708401	558.297317	11.974016
11.783773	552.113072	11.979034
11.747064	551.446618	11.984051
11.774644	558.776101	11.989069
11.702506	554.801705	11.994087
11.879717	555.465197	11.999104
11.783957	556.202745	12.004122
11.671305	552.682763	12.009139
11.342267	553.406141	12.014157
11.353198	558.339904	12.019175
11.661851	577.812853	12.024192
11.970058	568.256800	12.029210
12.354395	579.989718	12.034227
11.780981	579.381580	12.039245
12.060659	572.382911	12.044263
11.787759	577.739551	12.049280
11.929444	576.786556	12.054298
12.127486	580.242736	12.059315
12.235943	568.802285	12.064333
12.041653	555.222096	12.069351
11.850046	559.357451	12.074368
12.278134	560.960141	12.079386
11.788440	555.132106	12.084403
11.819057	559.807194	12.089421
12.269378	563.962520	12.094439
12.035045	570.837346	12.099456
12.148853	564.511418	12.104474
12.021787	562.246482	12.109491
12.023682	573.925336	12.114509
12.356933	565.362579	12.119527
11.744967	563.204696	12.124544
11.770634	572.437355	12.129562
12.150507	571.510389	12.134579
12.275044	571.083906	12.139597
12.456087	574.129338	12.144615
12.027382	571.781982	12.149632
12.310294	576.910079	12.154650
12.234119	571.607767	12.159667
12.030068	572.204393	12.164685
12.376294	572.532314	12.169703
12.301837	575.974118	12.174720
12.398739	567.981467	12.179738
12.164451	564.934839	12.184755
12.385997	566.266742	12.189773
12.176164	560.688610	12.194791
12.330257	565.483325	12.199808
11.888456	567.101538	12.204826
12.297879	577.180130	12.209843
12.206038	579.911458	12.214861
12.058749	572.139855	12.219879
12.221141	581.922409	12.224896
12.086587	578.390053	12.229914
12.223336	575.768473	12.234931
12.254420	574.592866	12.239949
12.072497	569.193415	12.244967
11.865157	568.032841	12.249984
12.049788	568.603662	12.255002
12.777786	588.708739	12.260019
12.343593	590.496176	12.265037
12.510670	577.017491	12.270055
12.384950	582.960264	12.275072
12.361676	584.491226	12.280090
12.685773	591.032971	12.285107
12.519098	591.898322	12.290125
12.535530	580.058798	12.295143
12.288180	594.799613	12.300160
12.249225	586.869130	12.305178
12.810356	593.610647	12.310195
12.639601	600.712261	12.315213
12.916542	598.333927	12.320231
12.786444	594.011954	12.325248
12.611922	581.501599	12.330266
12.534182	590.655697	12.335283
12.517311	577.669536	12.340301
12.702916	565.608030	12.345319
12.592927	579.200869	12.350336
12.538454	571.102403	12.355354
12.647608	574.297877	12.360371
12.173169	584.977971	12.365389
12.897416	595.061203	12.370407
12.594813	596.556764	12.375424
12.816000	593.480239	12.380442
12.774635	590.583442	12.385459
12.684568	599.597458	12.390477
13.169796	592.506820	12.395495
13.025915	589.673320	12.400512
12.814785	575.145877	12.405530
12.964623	566.223527	12.410547
12.468192	574.934742	12.415565
12.676874	570.578962	12.420583
12.823084	583.658564	12.425600
12.625652	588.757315	12.430618
13.079298	589.687025	12.435635
12.930362	594.399545	12.440653
13.185723	589.017208	12.445671
12.871355	577.279680	12.450688
12.595325	575.429240	12.455706
12.709861	567.863016	12.460723
12.601087	590.995288	12.465741
12.974126	591.344280	12.470759
13.232152	593.241684	12.475776
12.823505	600.146817	12.480794
12.883819	599.288537	12.485811
13.172140	591.250295	12.490829
13.258770	596.535185	12.495847
13.060248	593.126391	12.500864
13.244309	590.349125	12.505882
13.461829	562.333849	12.510899
13.125673	570.019758	12.515917
13.080064	565.993893	12.520935
13.081774	575.476427	12.525952
12.681956	571.351082	12.530970
13.007702	570.748111	12.535987
12.989813	569.416034	12.541005
12.903308	575.368477	12.546023
12.916669	575.442123	12.551040
12.874707	596.822066	12.556058
13.226627	588.114385	12.561075
13.109973	596.230015	12.566093
13.243336	589.266742	12.571111
13.128780	592.115213	12.576128
13.217667	589.040353	12.581146
12.921299	601.788104	12.586163
12.918437	599.683699	12.591181
13.316601	594.241259	12.596199
13.036238	596.351871	12.601216
12.960000	595.663169	12.606234
13.142519	596.183830	12.611251
12.900872	597.808751	12.616269
12.927241	587.255193	12.621287
13.154767	603.985894	12.626304
13.287769	611.851230	12.631322
13.484716	623.057951	12.636339
13.534197	619.926108	12.641357
13.398734	613.935607	12.646375
13.475873	596.311718	12.651392
13.052097	592.650828	12.656410
13.711448	609.210164	12.661427
13.225618	613.814202	12.666445
13.623158	603.635173	12.671463
13.426597	598.654543	12.676480
13.036557	604.464914	12.681498
13.532906	610.399201	12.686515
13.593195	617.284975	12.691533
13.643520	618.451045	12.696551
13.499543	616.236070	12.701568
13.282375	616.134177	12.706586
13.897269	609.613456	12.711603
13.489772	617.635528	12.716621
13.532373	608.600471	12.721639
13.538953	609.413603	12.726656
13.314562	613.711858	12.731674
13.216058	621.433369	12.736691
13.502178	611.173857	12.741709
13.451437	620.188072	12.746727
13.688622	621.236689	12.751744
13.704171	624.415190	12.756762
13.999552	621.068342	12.761779
13.663249	623.276026	12.766797
14.034772	616.190459	12.771815
13.677673	622.800406	12.776832
13.194142	618.959473	12.781850
13.842813	616.482236	12.786867
13.632985	624.142188	12.791885
13.743762	625.377738	12.796903
13.719956	618.353721	12.801920
13.576544	630.610636	12.806938
13.765567	615.560128	12.811955
13.842225	619.631639	12.816973
13.486235	620.390773	12.821991
13.801953	610.139277	12.827008
13.744033	619.192477	12.832026
14.102325	618.903161	12.837043
13.566367	620.315141	12.842061
13.837339	615.558347	12.847079
14.069986	622.691833	12.852096
13.814593	626.799266	12.857114
13.905408	616.021071	12.862131
13.825093	618.567580	12.867149
13.807746	620.425814	12.872167
13.861278	619.881002	12.877184
13.829046	612.609000	12.882202
13.784346	617.024441	12.887219
13.928923	617.983339	12.892237
13.986800	634.822530	12.897255
14.270460	633.544481	12.902272
13.851063	627.320483	12.907290
14.012316	629.125665	12.912307
14.181042	638.213013	12.917325
14.109437	636.592660	12.922343
13.833120	627.616714	12.927360
13.734987	647.847327	12.932378
14.140092	638.358197	12.937395
14.498602	651.313279	12.942413
14.287126	658.635844	12.947431
14.354454	650.802390	12.952448
14.286667	641.544670	12.957466
14.190458	636.980734	12.962483
14.141836	635.773353	12.967501
13.966588	641.171611	12.972519
14.090734	642.812165	12.977536
14.122516	643.233224	12.982554
14.251544	645.153874	12.987571
14.211395	649.871561	12.992589
14.178898	647.831722	12.997607
14.314085	644.276290	13.002624
13.972577	646.847692	13.007642
14.154365	647.336911	13.012659
14.469415	646.117088	13.017677
14.386800	652.835784	13.022695
14.508842	647.998031	13.027712
14.484816	652.101005	13.032730
14.739118	647.132211	13.037747
14.543347	642.492259	13.042765
14.635529	646.078539	13.047783
14.588144	651.160257	13.052800
14.322889	652.975045	13.057818
14.117620	644.461382	13.062835
14.503094	657.778331	13.067853
14.456585	651.704544	13.072871
14.452150	639.492701	13.077888
14.119218	647.354860	13.082906
14.519039	639.671607	13.087923
14.600256	642.959803	13.092941
14.395292	644.096196	13.097959
14.518069	640.138769	13.102976
14.231022	653.263788	13.107994
14.405797	652.390841	13.113011
14.336886	644.098937	13.118029
14.128020	651.544164	13.123047
14.767296	657.178513	13.128064
14.849259	670.943500	13.133082
14.884909	655.506598	13.138099
14.242469	651.444255	13.143117
14.625759	652.242916	13.148135
15.104654	648.851712	13.153152
14.624998	663.969567	13.158170
14.571651	655.968714	13.163187
14.888964	656.850228	13.168205
14.727323	657.474966	13.173223
14.802344	652.849653	13.178240
15.005346	661.354185	13.183258
14.965434	657.901749	13.188275
14.558922	650.056867	13.193293
14.519088	650.722597	13.198311
15.183412	655.422118	13.203328
14.991691	656.786815	13.208346
14.821802	658.731917	13.213363
14.749195	642.229478	13.218381
14.812436	657.745622	13.223399
15.097694	651.992551	13.228416
15.008934	662.880877	13.233434
14.779469	659.584181	13.238451
15.346591	655.642772	13.243469
14.995271	649.408167	13.248487
14.975623	649.669982	13.253504
14.845285	656.295127	13.258522
15.106491	655.471837	13.263539
15.006383	659.561412	13.268557
14.758531	664.399800	13.273575
15.148392	661.035079	13.278592
14.868225	659.115848	13.283610
14.675011	663.469220	13.288627
14.833858	658.117668	13.293645
14.943340	671.133627	13.298663
15.196403	658.171650	13.303680
15.250693	655.468225	13.308698
15.371239	657.257658	13.313715
15.085919	658.589593	13.318733
15.011184	666.648237	13.323751
15.053735	656.858952	13.328768
15.377936	669.614270	13.333786
15.124941	668.921528	13.338803
15.489281	665.519756	13.343821
15.234670	665.493117	13.348839
15.369969	657.226215	13.353856
15.126261	665.958084	13.358874
15.326479	664.642533	13.363891
15.304442	664.125264	13.368909
15.094945	661.500777	13.373927
15.338291	660.705513	13.378944
15.589452	657.318207	13.383962
15.527103	658.129450	13.388979
15.292289	660.400230	13.393997
15.140226	668.584519	13.399015
15.670100	653.433575	13.404032
15.266378	658.813764	13.409050
15.291281	661.451191	13.414067
15.177470	655.757096	13.419085
14.827423	666.212752	13.424103
15.413544	671.934274	13.429120
15.359788	678.430744	13.434138
15.524591	683.182799	13.439155
15.485421	686.581262	13.444173
15.508837	686.637564	13.449191
15.625816	687.010647	13.454208
15.539580	684.300696	13.459226
15.721211	688.311699	13.464243
15.774166	678.662789	13.469261
15.398517	683.038259	13.474279
15.399447	682.328072	13.479296
15.410114	680.521342	13.484314
15.326257	687.801958	13.489331
15.395432	680.548852	13.494349
15.494843	684.212907	13.499367
15.427612	680.682672	13.504384
15.595418	697.170303	13.509402
15.727382	710.747661	13.514419
15.721912	692.271877	13.519437
15.862416	704.800209	13.524455
16.215662	700.292506	13.529472
16.195948	701.112891	13.534490
15.892581	683.608117	13.539507
15.888656	678.499645	13.544525
15.663287	677.054701	13.549543
15.684545	672.021202	13.554560
16.266192	684.559729	13.559578
16.100516	678.504485	13.564595
15.715007	673.745749	13.569613
15.848200	668.836830	13.574631
15.719504	667.048644	13.579648
16.236824	685.984313	13.584666
16.142349	681.584191	13.589683
16.083231	667.597875	13.594701
15.779935	680.087994	13.599719
15.730572	685.062736	13.604736
16.193439	692.573802	13.609754
16.296635	695.934322	13.614771
16.255397	689.790275	13.619789
15.802685	688.844615	13.624807
16.406447	678.955317	13.629824
16.007759	677.897108	13.634842
16.067947	679.216275	13.639859
16.283710	669.680872	13.644877
16.084535	682.748052	13.649895
16.021966	684.853166	13.654912
16.477774	687.887395	13.659930
15.825676	694.366580	13.664947
16.331535	693.905970	13.669965
16.642396	710.904655	13.674983
16.113136	683.516682	13.680000
16.355202	688.275643	13.685018
16.200546	690.956810	13.690035
16.004674	693.997833	13.695053
16.430618	696.273034	13.700071
16.425997	698.754123	13.705088
16.651256	701.432942	13.710106
16.193299	709.481846	13.715123
16.714173	701.221161	13.720141
16.379664	690.641681	13.725159
16.306998	698.621124	13.730176
16.604880	700.111561	13.735194
16.417433	695.277802	13.740211
16.465908	691.382423	13.745229
16.358914	701.759232	13.750247
16.539220	707.569196	13.755264
16.737794	696.505939	13.760282
16.456414	695.085494	13.765299
16.551525	700.296514	13.770317
16.518216	697.742417	13.775335
16.570463	700.410305	13.780352
16.870377	704.462855	13.785370
16.268000	699.128827	13.790387
16.572230	697.326880	13.795405
16.591417	700.069341	13.800423
16.709463	703.654761	13.805440
16.666697	691.161683	13.810458
16.415282	702.693875	13.815475
16.559592	696.924866	13.820493
16.458093	703.365664	13.825511
16.832673	701.502272	13.830528
16.934954	703.275619	13.835546
16.984894	705.426333	13.840563
17.011925	697.397168	13.845581
17.296978	699.968851	13.850599
16.658995	689.326171	13.855616
16.764509	689.546410	13.860634
16.391502	704.452042	13.865651
16.849595	700.139447	13.870669
16.499362	703.908226	13.875687
16.615267	703.653492	13.880704
16.849259	701.692073	13.885722
16.558331	711.456918	13.890739
16.798402	701.611610	13.895757
16.543439	704.210570	13.900775
16.691580	707.665077	13.905792
17.105508	706.830629	13.910810
16.915475	724.052475	13.915827
16.886996	724.236774	13.920845
17.219229	724.781464	13.925863
17.282325	730.758002	13.930880
17.330213	724.615845	13.935898
17.077453	715.112340	13.940915
17.126767	703.340196	13.945933
16.989965	706.005962	13.950951
16.988685	713.134881	13.955968
17.074007	717.833051	13.960986
17.277132	725.883173	13.966003
17.242716	725.970569	13.971021
17.393330	728.326510	13.976039
17.018297	725.267055	13.981056
17.418497	722.822178	13.986074
17.240402	724.503485	13.991091
17.120089	724.115121	13.996109
17.399831	723.203737	14.001127
16.919740	738.110291	14.006144
17.372598	739.781723	14.011162
17.475548	737.225339	14.016179
17.192097	737.591343	14.021197
17.241051	734.020918	14.026215
17.147192	732.662789	14.031232
17.401216	721.843340	14.036250
17.182641	728.608479	14.041267
17.393658	730.920303	14.046285
17.408419	731.186229	14.051303
17.216976	731.137133	14.056320
17.469253	731.719518	14.061338
17.561605	732.405695	14.066355
17.319993	735.870400	14.071373
17.280804	734.390153	14.076391
17.019973	742.310553	14.081408
17.486963	746.283452	14.086426
17.322330	747.972133	14.091443
17.848256	749.704770	14.096461
17.760290	748.743342	14.101479
17.302718	758.792927	14.106496
17.660721	752.043917	14.111514
17.489748	757.006056	14.116531
17.603055	755.322189	14.121549
17.755540	746.670729	14.126567
17.438446	754.476821	14.131584
17.940311	751.325011	14.136602
17.904873	749.610657	14.141619
17.759893	763.502566	14.146637
17.755157	752.108022	14.151655
17.549866	759.448599	14.156672
17.822551	753.628027	14.161690
17.780912	758.330197	14.166707
17.815784	753.641683	14.171725
17.971497	751.572529	14.176743
17.843355	751.665051	14.181760
18.133402	752.374096	14.186778
17.783865	748.546985	14.191795
17.693793	755.216389	14.196813
18.006146	738.669703	14.201831
17.418351	753.110215	14.206848
17.921939	743.305904	14.211866
18.016802	742.817768	14.216883
17.780538	746.272174	14.221901
18.039812	757.444031	14.226919
18.087497	779.921046	14.231936
18.284237	775.308308	14.236954
18.284778	762.123647	14.241971
17.973927	764.280050	14.246989
18.396813	767.123764	14.252007
18.063793	761.681510	14.257024
18.144117	765.903958	14.262042
18.024223	767.241702	14.267059
18.475712	771.015055	14.272077
18.279357	766.466677	14.277095
18.067336	776.793613	14.282112
17.791008	777.660266	14.287130
18.289852	778.844874	14.292147
18.378760	782.355954	14.297165
18.504732	768.167176	14.302183
18.436696	785.054516	14.307200
18.015513	775.116467	14.312218
18.794426	781.069933	14.317235
18.501249	787.420688	14.322253
18.423687	776.977870	14.327271
18.430003	771.265036	14.332288
18.406210	775.541565	14.337306
18.636724	779.683830	14.342323
18.188003	777.800296	14.347341
18.543820	782.263869	14.352359
18.823424	784.624981	14.357376
19.036580	772.615848	14.362394
18.456787	771.472225	14.367411
18.219794	756.506861	14.372429
18.478537	767.031886	14.377447
18.535511	780.762980	14.382464
18.822996	779.758873	14.387482
18.781124	775.950123	14.392499
18.435731	779.434150	14.397517
18.713852	771.722453	14.402535
18.656562	764.978138	14.407552
18.738651	772.084634	14.412570
19.034474	775.563497	14.417587
18.771813	774.742872	14.422605
18.759510	773.138519	14.427623
18.452455	774.114095	14.432640
18.512115	773.498899	14.437658
18.709227	777.119360	14.442675
18.682217	775.006071	14.447693
18.885715	773.977171	14.452711
18.487425	779.593229	14.457728
18.814624	771.403690	14.462746
18.694791	772.403763	14.467763
18.719691	772.270492	14.472781
19.035424	767.989513	14.477799
18.779155	781.529544	14.482816
18.664018	775.703077	14.487834
18.867613	785.166913	14.492851
18.987904	794.523806	14.497869
19.414060	797.243943	14.502887
18.926774	796.821198	14.507904
19.075382	788.444868	14.512922
19.121622	797.141124	14.517939
19.091306	796.511535	14.522957
19.180634	805.810140	14.527975
19.109250	802.245815	14.532992
19.224342	796.781116	14.538010
19.219430	790.868057	14.543027
18.855127	796.264240	14.548045
19.321020	798.804626	14.553063
19.037160	802.335880	14.558080
19.214633	796.075695	14.563098
19.477255	796.280941	14.568115
19.264557	803.897237	14.573133
19.331588	797.089374	14.578151
19.010530	800.635886	14.583168
19.007025	789.556699	14.588186
19.157354	799.110883	14.593203
18.994964	791.395182	14.598221
19.122525	789.418767	14.603239
19.335042	806.259290	14.608256
19.490036	801.782429	14.613274
19.214463	809.045609	14.618291
19.261433	815.854640	14.623309
19.612912	820.236850	14.628327
19.555781	830.700643	14.633344
19.582904	819.067573	14.638362
19.635396	822.956706	14.643379
19.607463	823.970875	14.648397
19.732003	812.433093	14.653415
19.321920	799.526926	14.658432
19.524963	816.081763	14.663450
19.692947	828.372380	14.668467
19.645162	824.633967	14.673485
19.559037	825.543591	14.678503
19.539288	823.870967	14.683520
20.060800	824.824836	14.688538
19.835682	827.570641	14.693555
20.006622	824.760669	14.698573
19.904005	818.686092	14.703591
19.750646	824.538577	14.708608
19.586102	819.420359	14.713626
19.601864	820.677027	14.718643
19.455470	825.423925	14.723661
19.694534	820.807741	14.728679
20.022863	819.765715	14.733696
19.922925	812.608311	14.738714
19.835221	816.462467	14.743731
19.868243	823.169535	14.748749
20.024192	819.134322	14.753767
19.529662	815.885178	14.758784
19.462338	820.446199	14.763802
20.293197	827.038515	14.768819
20.392058	827.105162	14.773837
20.239981	818.851370	14.778855
19.663971	822.958275	14.783872
19.681172	821.980469	14.788890
20.359619	829.461184	14.793907
20.139596	836.977651	14.798925
20.210381	843.609421	14.803943
20.741683	843.798082	14.808960
20.628861	821.368975	14.813978
20.402023	816.866354	14.818995
20.299691	817.488175	14.824013
20.099265	820.223823	14.829031
20.248935	818.916131	14.834048
20.040314	819.018028	14.839066
20.366829	811.346115	14.844083
20.024073	803.140953	14.849101
20.385754	811.699744	14.854119
20.309599	830.289324	14.859136
20.005435	837.020493	14.864154
20.461943	834.399582	14.869171
20.046515	842.224178	14.874189
20.514617	836.079672	14.879207
20.304443	841.638059	14.884224
20.063257	835.269479	14.889242
20.189032	829.383395	14.894259
20.259527	836.381272	14.899277
20.505722	834.815559	14.904295
20.261649	842.342084	14.909312
20.355652	856.184233	14.914330
20.972667	856.795040	14.919347
20.636965	858.204260	14.924365
21.040736	854.831025	14.929383
20.327679	845.121413	14.934400
20.398230	854.997310	14.939418
20.601321	857.351409	14.944435
20.556789	868.479121	14.949453
20.985704	863.337918	14.954471
20.726016	870.245207	14.959488
20.675590	867.084695	14.964506
20.813325	863.784437	14.969523
20.909366	858.376333	14.974541
20.936003	859.473524	14.979559
21.072749	854.945844	14.984576
20.868731	862.084298	14.989594
21.424872	864.108881	14.994611
20.988084	863.993845	14.999629
21.150074	867.329465	15.004647
20.905119	848.830846	15.009664
20.832335	869.868786	15.014682
21.037632	854.559928	15.019699
21.206464	864.089176	15.024717
21.173969	869.525236	15.029735
21.236442	865.633951	15.034752
20.982546	864.591056	15.039770
21.362775	862.777260	15.044787
21.470187	861.132170	15.049805
20.919919	844.953215	15.054823
20.852715	856.112851	15.059840
20.769909	850.170876	15.064858
21.191543	858.095521	15.069875
21.034382	854.023845	15.074893
21.143409	860.690692	15.079911
21.297102	862.023715	15.084928
21.332760	853.627072	15.089946
21.437002	848.063063	15.094963
21.317661	845.938896	15.099981
21.398763	854.806473	15.104999
21.294433	854.507134	15.110016
21.347327	856.950888	15.115034
21.174171	853.235144	15.120051
21.073259	855.933214	15.125069
21.085195	859.926497	15.130087
21.387886	854.808104	15.135104
21.377664	865.712727	15.140122
21.688368	864.872253	15.145139
22.174297	882.288803	15.150157
22.141723	868.645326	15.155175
21.959637	848.161432	15.160192
21.937465	840.859368	15.165210
21.814637	844.214084	15.170227
21.861831	853.355176	15.175245
22.079631	843.393340	15.180263
22.113768	838.679673	15.185280
21.708711	849.481662	15.190298
21.932375	843.608735	15.195315
21.882058	846.213721	15.200333
21.851015	840.408853	15.205351
21.651386	838.981979	15.210368
21.437012	849.946780	15.215386
21.624825	836.691882	15.220403
21.578491	848.002894	15.225421
21.478433	843.007169	15.230439
21.837118	839.183377	15.235456
21.609102	852.851604	15.240474
21.791862	838.373069	15.245491
21.783348	845.007719	15.250509
22.109879	852.057254	15.255527
22.129815	849.242387	15.260544
21.763182	855.011325	15.265562
22.481544	857.061143	15.270579
22.100863	853.734307	15.275597
21.948106	850.043789	15.280615
22.077403	852.936384	15.285632
22.243202	866.394987	15.290650
22.200510	866.149165	15.295667
22.201624	872.548802	15.300685
21.911562	876.933083	15.305703
22.306798	869.903683	15.310720
22.246106	871.030250	15.315738
22.375188	866.229211	15.320755
22.153685	873.282032	15.325773
22.342388	873.208461	15.330791
22.540683	865.922553	15.335808
22.142350	875.028884	15.340826
22.051788	865.361193	15.345843
22.629551	864.119387	15.350861
22.197341	863.820605	15.355879
22.279986	870.886029	15.360896
21.967413	875.191765	15.365914
22.035652	865.969553	15.370931
22.351750	878.925094	15.375949
22.426940	889.144263	15.380967
22.709130	884.846388	15.385984
22.584189	892.212378	15.391002
22.808776	897.532682	15.396019
22.815380	894.663081	15.401037
22.561101	879.845468	15.406055
22.588393	882.409974	15.411072
22.503432	895.311208	15.416090
22.479836	891.925612	15.421107
22.506650	895.446382	15.426125
22.755708	890.727641	15.431143
22.940973	880.859209	15.436160
22.747079	894.676787	15.441178
23.108616	878.529403	15.446195
23.160210	897.039203	15.451213
22.828685	897.781916	15.456231
22.547577	892.164285	15.461248
22.455393	894.075223	15.466266
22.679147	900.635862	15.471283
22.743637	892.925817	15.476301
22.421947	892.168024	15.481319
23.151914	893.240917	15.486336
22.982933	895.492009	15.491354
22.834699	910.328103	15.496371
23.480220	905.667548	15.501389
23.068663	901.461904	15.506407
23.451567	891.527983	15.511424
23.170963	890.672277	15.516442
23.224091	877.473031	15.521459
22.985816	881.517899	15.526477
23.372057	882.650619	15.531495
23.543769	874.882864	15.536512
23.226834	881.496121	15.541530
23.060307	880.335482	15.546547
23.490765	881.950457	15.551565
23.756911	888.797974	15.556583
23.260399	886.072977	15.561600
23.211658	892.366777	15.566618
23.379151	884.700657	15.571635
23.383226	890.736931	15.576653
23.226623	884.904261	15.581671
23.519180	884.669357	15.586688
23.219788	876.930769	15.591706
23.665731	890.752863	15.596723
23.787204	891.339841	15.601741
23.622590	896.613446	15.606759
23.349104	883.016935	15.611776
23.492887	897.334193	15.616794
23.834600	901.812615	15.621811
23.861235	892.439080	15.626829
23.493397	895.055641	15.631847
23.680060	889.661820	15.636864
23.974813	898.717057	15.641882
23.566238	889.187226	15.646899
24.122028	890.646991	15.651917
23.470308	890.331894	15.656935
23.536486	895.919853	15.661952
24.033118	895.145101	15.666970
23.799553	906.011941	15.671987
23.946064	897.348715	15.677005
23.649074	914.514815	15.682023
23.656426	915.280505	15.687040
23.874680	911.254505	15.692058
23.666326	905.470910	15.697075
23.713583	903.159855	15.702093
23.685457	905.414263	15.707111
23.799016	908.362965	15.712128
24.334529	906.348267	15.717146
24.182076	904.611091	15.722163
24.086148	899.046675	15.727181
23.964956	906.393153	15.732199
23.865188	895.470896	15.737216
23.844018	902.836512	15.742234
23.744119	926.374928	15.747251
24.354570	927.737825	15.752269
24.136724	934.098993	15.757287
24.242736	930.339768	15.762304
24.387907	926.280963	15.767322
24.210861	923.499909	15.772339
24.473073	931.376826	15.777357
24.282613	933.836390	15.782375
24.635522	929.391798	15.787392
24.765063	933.294205	15.792410
24.480442	925.079935	15.797427
24.573552	925.109608	15.802445
24.120565	924.034592	15.807463
24.386062	923.204310	15.812480
24.420097	927.459249	15.817498
24.453058	927.662386	15.822515
24.684382	919.727542	15.827533
24.425489	929.951413	15.832551
24.728251	913.371345	15.837568
24.668201	921.121711	15.842586
24.481855	919.841082	15.847603
24.821363	920.182679	15.852621
24.409665	930.575506	15.857639
24.479656	924.903200	15.862656
24.351351	931.726942	15.867674
25.019425	932.200417	15.872691
24.758915	940.313354	15.877709
24.566934	948.592348	15.882727
24.917301	944.103967	15.887744
25.191956	940.990656	15.892762
25.306498	945.608599	15.897779
25.410931	933.682556	15.902797
25.071436	920.645392	15.907815
24.885444	918.869257	15.912832
25.005956	913.043924	15.917850
24.914645	915.772065	15.922867
25.119211	910.482745	15.927885
24.942583	923.322534	15.932903
25.080836	921.344440	15.937920
25.131013	918.322886	15.942938
24.998220	937.113895	15.947955
25.309016	933.751967	15.952973
25.191303	945.465466	15.957991
25.489120	938.779403	15.963008
25.176611	920.502661	15.968026
25.257140	933.084673	15.973043
25.540883	928.896997	15.978061
25.253224	931.456899	15.983079
25.229876	942.111154	15.988096
25.546365	941.897769	15.993114
25.323541	947.735863	15.998131
25.285276	953.810307	16.003149
24.931538	948.525852	16.008167
25.377583	938.427442	16.013184
25.459534	946.455506	16.018202
25.327813	953.910938	16.023219
25.582654	942.974465	16.028237
25.371958	945.506608	16.033255
25.392215	945.683321	16.038272
25.537779	944.900113	16.043290
25.073125	956.894850	16.048307
25.919927	961.360918	16.053325
25.389813	955.292895	16.058343
25.646470	960.390479	16.063360
26.039658	970.509691	16.068378
25.841293	975.523492	16.073395
26.103481	976.827010	16.078413
26.200530	964.280413	16.083431
25.833409	956.262007	16.088448
25.632442	943.821784	16.093466
25.705321	951.826017	16.098483
25.859225	957.021647	16.103501
25.933524	968.812561	16.108519
26.184456	960.994565	16.113536
26.541882	960.134190	16.118554
26.050194	959.074664	16.123571
26.253425	942.563713	16.128589
25.911008	943.705747	16.133607
26.070198	935.122577	16.138624
26.313738	939.310188	16.143642
26.056330	954.040242	16.148659
26.540734	954.008993	16.153677
25.896251	949.249478	16.158695
26.232317	953.274366	16.163712
26.224581	959.419797	16.168730
25.907400	967.159725	16.173747
26.316502	969.819430	16.178765
26.222996	968.814671	16.183783
26.123248	965.330467	16.188800
26.356635	957.335327	16.193818
26.265638	958.151043	16.198835
26.283995	956.570302	16.203853
26.340437	958.975649	16.208871
26.585464	963.396559	16.213888
26.570060	966.283300	16.218906
26.465085	965.558033	16.223923
26.830413	971.765302	16.228941
26.813501	967.621272	16.233959
26.722796	965.716689	16.238976
26.574764	960.690531	16.243994
26.464901	969.742530	16.249011
26.733651	969.467152	16.254029
26.587122	971.481232	16.259047
26.379978	954.295718	16.264064
26.511541	955.010513	16.269082
26.555626	968.664866	16.274099
26.868040	974.681562	16.279117
26.836892	974.001604	16.284135
26.683692	981.662359	16.289152
26.813316	972.364264	16.294170
27.087100	982.754534	16.299187
27.018386	980.044966	16.304205
26.975871	976.876891	16.309223
27.022811	977.125188	16.314240
26.771694	965.162964	16.319258
26.938861	975.468846	16.324275
27.110600	959.956843	16.329293
27.206056	970.901881	16.334311
27.074170	974.409506	16.339328
27.364461	971.451543	16.344346
26.848678	979.676826	16.349363
26.883331	981.198803	16.354381
26.757173	977.740798	16.359399
27.021614	982.663610	16.364416
27.478974	999.532467	16.369434
27.159943	1001.349350	16.374451
27.479134	995.310023	16.379469
28.012376	987.810973	16.384487
27.554715	989.441159	16.389504
27.618661	968.716852	16.394522
27.702201	972.285609	16.399539
27.586370	957.575760	16.404557
27.545512	967.125090	16.409575
27.407128	963.321859	16.414592
27.395103	962.228677	16.419610
27.193756	968.287492	16.424627
27.901049	976.697881	16.429645
28.232997	982.768342	16.434663
27.605159	981.900423	16.439680
27.710172	968.386925	16.444698
27.450768	971.501001	16.449715
27.851768	971.135605	16.454733
27.681542	975.867319	16.459751
27.593231	983.921908	16.464768
27.979740	976.628742	16.469786
28.146158	986.082694	16.474803
27.807078	994.009077	16.479821
27.676750	977.512158	16.484839
27.644386	982.471714	16.489856
28.051137	978.725614	16.494874
27.966789	985.694010	16.499891
27.651859	985.717786	16.504909
27.846444	989.496471	16.509927
27.819876	993.975453	16.514944
28.274270	982.581861	16.519962
27.813528	984.174657	16.524979
27.854560	992.177555	16.529997
28.431215	1000.668254	16.535015
28.319217	1012.491359	16.540032
28.540978	1007.660073	16.545050
28.477062	995.138516	16.550067
28.206308	989.317274	16.555085
28.034319	989.239901	16.560103
28.042137	996.553707	16.565120
28.287902	996.723712	16.570138
28.574695	1008.674070	16.575155
28.341734	1006.352981	16.580173
28.539587	1005.520604	16.585191
28.457832	1015.638051	16.590208
28.579320	1007.436252	16.595226
28.879095	1009.241996	16.600243
28.747195	1009.354038	16.605261
28.917913	1014.913135	16.610279
28.356485	1009.468497	16.615296
28.706054	1004.664650	16.620314
28.852029	1005.844254	16.625331
28.423486	1014.428349	16.630349
28.680290	1008.764799	16.635367
28.806517	1009.896986	16.640384
28.845364	1007.950138	16.645402
28.671970	1007.475359	16.650419
28.745595	1008.218111	16.655437
28.868903	1008.561814	16.660455
28.345490	1006.816115	16.665472
28.530476	1006.067791	16.670490
28.792809	1013.714356	16.675507
28.817173	1021.495803	16.680525
29.070528	1027.007324	16.685543
28.868585	1035.751806	16.690560
29.322818	1031.524938	16.695578
29.409162	1023.076143	16.700595
29.129377	1028.471859	16.705613
29.647015	1026.112797	16.710631
29.074010	1013.894549	16.715648
29.545279	1005.306937	16.720666
29.466229	1007.234777	16.725683
29.108463	996.311602	16.730701
29.143240	997.161386	16.735719
29.218926	1021.783416	16.740736
29.345870	1026.399449	16.745754
29.565855	1027.046831	16.750771
29.468616	1032.862245	16.755789
29.968586	1023.733677	16.760807
29.788758	1022.231122	16.765824
29.502970	1000.516674	16.770842
29.406830	991.310523	16.775859
29.543505	1007.456157	16.780877
29.797119	1012.024062	16.785895
29.654626	1023.703602	16.790912
29.739060	1020.357966	16.795930
29.783511	1015.538506	16.800947
29.677127	1018.483601	16.805965
29.478715	1022.942009	16.810983
29.426343	1026.020705	16.816000
29.678073	1011.057928	16.821018
29.740841	1013.639020	16.826035
29.358086	1017.422395	16.831053
29.536864	1017.763773	16.836071
29.526480	1018.090423	16.841088
29.750130	1024.019972	16.846106
30.309048	1036.789502	16.851123
30.068896	1045.211738	16.856141
30.324560	1039.482085	16.861159
30.141690	1043.849718	16.866176
30.036997	1044.481381	16.871194
30.294394	1039.133305	16.876211
30.072740	1049.035870	16.881229
30.176668	1046.886384	16.886247
30.412992	1049.699232	16.891264
30.151226	1045.987776	16.896282
30.241420	1037.535219	16.901299
30.433311	1040.291868	16.906317
30.292639	1041.916886	16.911335
30.271845	1044.040784	16.916352
30.281721	1043.177714	16.921370
30.119542	1041.003388	16.926387
30.167849	1046.215486	16.931405
30.556633	1038.656855	16.936423
30.008138	1043.245513	16.941440
30.193814	1044.112830	16.946458
30.662517	1046.435068	16.951475
30.542223	1047.700312	16.956493
30.851580	1030.134511	16.961511
30.508319	1032.305459	16.966528
30.384783	1030.222947	16.971546
30.776092	1051.602250	16.976563
30.510901	1061.792463	16.981581
30.840838	1061.633787	16.986599
30.710959	1068.176964	16.991616
30.855287	1064.957693	16.996634
31.006931	1058.862381	17.001651
30.900596	1071.113827	17.006669
31.035036	1056.677352	17.011687
30.726258	1060.846844	17.016704
30.986247	1062.501000	17.021722
31.061658	1055.398247	17.026739
30.924249	1056.694559	17.031757
30.819391	1064.281553	17.036775
31.006800	1061.683571	17.041792
30.930461	1063.746693	17.046810
31.083883	1051.102897	17.051827
30.675496	1064.464858	17.056845
31.084432	1076.882233	17.061863
31.361453	1085.728889	17.066880
31.558925	1083.312373	17.071898
31.969882	1077.583775	17.076915
31.688390	1069.286901	17.081933
31.309213	1052.229062	17.086951
31.011284	1050.088494	17.091968
31.253172	1066.356654	17.096986
31.468423	1068.996063	17.102003
31.666719	1082.673830	17.107021
31.733270	1082.818091	17.112039
31.830385	1083.396244	17.117056
31.478856	1086.281689	17.122074
31.192799	1077.070349	17.127091
31.321217	1074.891800	17.132109
31.803956	1080.140409	17.137127
31.763036	1080.620135	17.142144
31.684945	1084.690600	17.147162
31.702181	1078.941253	17.152179
31.506599	1082.651319	17.157197
31.343424	1073.275683	17.162215
31.735285	1083.723367	17.167232
31.872024	1103.592885	17.172250
32.478776	1100.008123	17.177267
32.439930	1103.179400	17.182285
32.195464	1081.963342	17.187303
32.119239	1082.514836	17.192320
32.395033	1076.930358	17.197338
32.192093	1070.988078	17.202355
31.913868	1078.387478	17.207373
32.054613	1076.992795	17.212391
32.170783	1063.827777	17.217408
32.087125	1080.954512	17.222426
32.381561	1099.006996	17.227443
32.314526	1096.994574	17.232461
32.874230	1084.480000	17.237479
32.030419	1084.816492	17.242496
32.438220	1087.324940	17.247514
32.475332	1095.262224	17.252531
32.445518	1095.973748	17.257549
32.648116	1103.399281	17.262567
32.845811	1105.243019	17.267584
32.289055	1090.216706	17.272602
32.281570	1093.083300	17.277619
32.192599	1099.673767	17.282637
32.401499	1098.558803	17.287655
32.338702	1099.613130	17.292672
32.191373	1106.853308	17.297690
32.609853	1100.404016	17.302707
32.348037	1113.244581	17.307725
32.886553	1123.013054	17.312743
33.204947	1127.779184	17.317760
32.978135	1125.974670	17.322778
33.146692	1104.653255	17.327795
33.364678	1110.590026	17.332813
33.023380	1101.772279	17.337831
33.012271	1094.357936	17.342848
32.805611	1102.692935	17.347866
33.007500	1097.217786	17.352883
33.088072	1106.514757	17.357901
33.139182	1120.657277	17.362919
33.390604	1126.626718	17.367936
33.152645	1127.234952	17.372954
32.694427	1122.900821	17.377971
33.225521	1128.063021	17.382989
33.122950	1120.599793	17.388007
33.547112	1123.096231	17.393024
33.326388	1125.143971	17.398042
33.492507	1126.014337	17.403059
33.099064	1130.212806	17.408077
33.396789	1128.222483	17.413095
33.423052	1119.596806	17.418112
33.331060	1124.319534	17.423130
33.538095	1120.096420	17.428147
33.241387	1124.699545	17.433165
33.395379	1122.248767	17.438183
33.660723	1125.811340	17.443200
33.955521	1141.648457	17.448218
33.960662	1132.514825	17.453235
34.146793	1140.387902	17.458253
33.903324	1126.363656	17.463271
33.910754	1121.202796	17.468288
33.561483	1129.395911	17.473306
33.965449	1130.604783	17.478323
33.871788	1130.543616	17.483341
34.179965	1129.028188	17.488359
34.042453	1125.180606	17.493376
33.934372	1134.506964	17.498394
34.252158	1132.371507	17.503411
34.223540	1131.116797	17.508429
34.178861	1137.618333	17.513447
34.320553	1126.636249	17.518464
33.832452	1137.814256	17.523482
34.390288	1133.107335	17.528499
34.171325	1142.747604	17.533517
34.102237	1138.854652	17.538535
34.392792	1136.887535	17.543552
34.604596	1139.587452	17.548570
34.361997	1131.303428	17.553587
34.123370	1141.795661	17.558605
34.013432	1133.033394	17.563623
34.284853	1136.200550	17.568640
33.858069	1136.752977	17.573658
34.275606	1140.531696	17.578675
34.404875	1156.962639	17.583693
34.916899	1169.708008	17.588711
34.730519	1165.909051	17.593728
34.399681	1174.427518	17.598746
34.550178	1161.014088	17.603763
34.657035	1169.899903	17.608781
34.868267	1164.552667	17.613799
34.843639	1160.021632	17.618816
34.710428	1167.237545	17.623834
34.845207	1159.607959	17.628851
34.917048	1168.628613	17.633869
34.602066	1167.450044	17.638887
34.858078	1166.595982	17.643904
34.803224	1172.070329	17.648922
35.433195	1171.230626	17.653939
35.204621	1174.866953	17.658957
34.986486	1172.161684	17.663975
35.390841	1176.232795	17.668992
35.337004	1176.465227	17.674010
34.977856	1164.008453	17.679027
35.112928	1173.110782	17.684045
34.996140	1189.589531	17.689063
35.580226	1188.820088	17.694080
35.509817	1187.783318	17.699098
35.475685	1184.090040	17.704115
35.844887	1190.707036	17.709133
35.817546	1181.556346	17.714151
35.948884	1171.405818	17.719168
35.521932	1172.927098	17.724186
35.018661	1160.786253	17.729203
35.506053	1172.781228	17.734221
35.517197	1176.437036	17.739239
35.830377	1180.951530	17.744256
35.927869	1195.528699	17.749274
36.074202	1181.894997	17.754291
35.913592	1182.131430	17.759309
35.774597	1190.866186	17.764327
35.981838	1174.266035	17.769344
35.670958	1180.698579	17.774362
35.612521	1183.292255	17.779379
35.318395	1181.870599	17.784397
35.540990	1181.801218	17.789415
35.930868	1186.183852	17.794432
36.294833	1197.718381	17.799450
36.412685	1202.357966	17.804467
36.429125	1200.979472	17.809485
36.528900	1187.905277	17.814503
36.769704	1171.514495	17.819520
36.351653	1174.467116	17.824538
36.037820	1178.255572	17.829555
36.000212	1165.269055	17.834573
36.027510	1181.293022	17.839591
36.411178	1186.983118	17.844608
36.469908	1192.726964	17.849626
36.635938	1200.192944	17.854643
36.367277	1202.772017	17.859661
36.405175	1189.473927	17.864679
36.718200	1196.225902	17.869696
36.484059	1201.160130	17.874714
36.935984	1198.164341	17.879731
36.979657	1192.982039	17.884749
36.728950	1192.784378	17.889767
36.923148	1196.714646	17.894784
36.959424	1205.469458	17.899802
36.849227	1195.511155	17.904819
36.967433	1193.457258	17.909837
36.595145	1199.151448	17.914855
36.590420	1194.787718	17.919872
36.608565	1193.418427	17.924890
36.636116	1198.248794	17.929907
36.953213	1195.788391	17.934925
36.875723	1204.851248	17.939943
37.085177	1211.401605	17.944960
36.798153	1219.496707	17.949978
37.105725	1221.124535	17.954995
37.116973	1225.641869	17.960013
37.046512	1224.920684	17.965031
37.184720	1223.264455	17.970048
36.989437	1223.373744	17.975066
37.085395	1223.276742	17.980083
37.566329	1226.395516	17.985101
36.881260	1240.315081	17.990119
37.673590	1237.761746	17.995136
38.000055	1248.633118	18.000154
37.524511	1239.167174	18.005171
37.756274	1239.576047	18.010189
37.603115	1245.428638	18.015207
37.783975	1244.185487	18.020224
38.038503	1243.315873	18.025242
37.864711	1242.550816	18.030259
37.993277	1230.680778	18.035277
37.509503	1226.773476	18.040295
37.860811	1227.289968	18.045312
37.826107	1233.931996	18.050330
37.753168	1237.525169	18.055347
37.699732	1232.253833	18.060365
37.611222	1240.911327	18.065383
37.882765	1232.515648	18.070400
37.668227	1235.007404	18.075418
37.828784	1241.237183	18.080435
38.032278	1246.456735	18.085453
38.055405	1257.997033	18.090471
38.152596	1261.421711	18.095488
38.523967	1267.773311	18.100506
38.412030	1255.950168	18.105523
38.519077	1262.320828	18.110541
38.427646	1269.552369	18.115559
38.370474	1263.202322	18.120576
38.779225	1262.769442	18.125594
38.643685	1257.965317	18.130611
38.694611	1258.582226	18.135629
38.869368	1261.852817	18.140647
38.799571	1255.956018	18.145664
39.102085	1252.099859	18.150682
38.518581	1259.111363	18.155699
38.629488	1249.213280	18.160717
38.738275	1257.663339	18.165735
38.707112	1254.657549	18.170752
38.727755	1263.042438	18.175770
38.636047	1266.979366	18.180787
38.939899	1265.152176	18.185805
38.648722	1263.165165	18.190823
38.493201	1254.286859	18.195840
38.786827	1259.230450	18.200858
39.060932	1272.221219	18.205875
39.311173	1275.224440	18.210893
39.201482	1285.841851	18.215911
39.212919	1281.857435	18.220928
39.340599	1279.669509	18.225946
38.791080	1284.974755	18.230963
39.095831	1271.729729	18.235981
39.405331	1281.906331	18.240999
39.147146	1277.206503	18.246016
39.475423	1278.474507	18.251034
39.151180	1287.468526	18.256051
39.282763	1277.687129	18.261069
39.228582	1285.660802	18.266087
39.380415	1295.233954	18.271104
39.864570	1301.754198	18.276122
39.555316	1296.585789	18.281139
39.806860	1297.199867	18.286157
39.825412	1299.292423	18.291175
40.036679	1288.542404	18.296192
39.934088	1295.005676	18.301210
39.972559	1298.518400	18.306227
40.122752	1283.369232	18.311245
39.840911	1294.130215	18.316263
39.893157	1291.253443	18.321280
40.365367	1298.365681	18.326298
39.756841	1295.345635	18.331315
40.332471	1292.706111	18.336333
40.349460	1292.368940	18.341351
40.486655	1286.544044	18.346368
40.346822	1284.763841	18.351386
39.715878	1276.133114	18.356403
40.371579	1281.582071	18.361421
40.001490	1291.201768	18.366439
40.194094	1288.918526	18.371456
40.381106	1295.043218	18.376474
40.392513	1289.622914	18.381491
40.422622	1284.635201	18.386509
40.030002	1286.091185	18.391527
40.099404	1286.951371	18.396544
40.334415	1305.455130	18.401562
40.321756	1312.469296	18.406579
40.270688	1311.650415	18.411597
40.386786	1318.306865	18.416615
40.218915	1312.964959	18.421632
41.312708	1320.583189	18.426650
40.915670	1331.084418	18.431667
41.293834	1321.081569	18.436685
41.087804	1304.413096	18.441703
41.105703	1303.750735	18.446720
41.443320	1307.081185	18.451738
41.096361	1313.402630	18.456755
41.124999	1315.632473	18.461773
41.208384	1312.255388	18.466791
41.632027	1313.047799	18.471808
41.115343	1311.881689	18.476826
41.180805	1314.639130	18.481843
41.294053	1312.459759	18.486861
41.177147	1310.142652	18.491879
40.955234	1320.323118	18.496896
41.166876	1318.017973	18.501914
41.124886	1334.314798	18.506931
41.136499	1332.757163	18.511949
41.304999	1340.210195	18.516967
41.120467	1338.260220	18.521984
41.371515	1333.670441	18.527002
41.667482	1342.062995	18.532019
41.797813	1346.546039	18.537037
41.838414	1354.990981	18.542055
42.018965	1353.091461	18.547072
42.174063	1346.948177	18.552090
41.982366	1345.646259	18.557107
41.774925	1334.361798	18.562125
41.970126	1336.508907	18.567143
42.079494	1344.015328	18.572160
42.224656	1351.544582	18.577178
42.304674	1360.459918	18.582195
42.380449	1340.882053	18.587213
41.989887	1336.076587	18.592231
42.009091	1342.637679	18.597248
42.610958	1341.833903	18.602266
42.402798	1343.744011	18.607283
42.058665	1333.080438	18.612301
42.168351	1342.729606	18.617319
41.855345	1353.609086	18.622336
42.271583	1348.905221	18.627354
42.014600	1355.903795	18.632371
42.551286	1350.575260	18.637389
42.337912	1350.302356	18.642407
42.527867	1344.772185	18.647424
42.585295	1350.986501	18.652442
42.687212	1365.913415	18.657459
42.732715	1368.187977	18.662477
43.407776	1361.657618	18.667495
43.180383	1350.729705	18.672512
43.268302	1335.508137	18.677530
42.940169	1335.167894	18.682547
43.132523	1327.406196	18.687565
43.139452	1335.004302	18.692583
43.090605	1329.315656	18.697600
42.829170	1324.906655	18.702618
43.058532	1332.697347	18.707635
43.186087	1325.848301	18.712653
43.316428	1323.688357	18.717671
43.072491	1333.020191	18.722688
43.218456	1337.021116	18.727706
43.319049	1352.244872	18.732723
43.231874	1348.607155	18.737741
43.606013	1353.932715	18.742759
43.608581	1352.723627	18.747776
43.754706	1346.143082	18.752794
43.575231	1352.886590	18.757811
43.634702	1357.153451	18.762829
43.649609	1349.223710	18.767847
43.613073	1347.556806	18.772864
43.941354	1348.190496	18.777882
43.181521	1353.834620	18.782899
43.470959	1361.395064	18.787917
43.913427	1357.466599	18.792935
44.149412	1360.778169	18.797952
43.648819	1359.268722	18.802970
43.689959	1361.076902	18.807987
43.818673	1363.881308	18.813005
44.295487	1370.569979	18.818023
44.338228	1377.086393	18.823040
44.509555	1373.118089	18.828058
44.305342	1365.206677	18.833075
44.022310	1367.434560	18.838093
44.471271	1374.679837	18.843111
44.328111	1370.997184	18.848128
44.475506	1368.932410	18.853146
44.613251	1379.328314	18.858163
44.647444	1377.931263	18.863181
44.870651	1364.900837	18.868199
44.670507	1370.868083	18.873216
44.841670	1354.617365	18.878234
44.675727	1357.167844	18.883251
44.565427	1358.523073	18.888269
44.707670	1365.907620	18.893287
44.618983	1365.293410	18.898304
45.071321	1361.082540	18.903322
44.868670	1375.271083	18.908339
44.833754	1371.218125	18.913357
44.742030	1360.859221	18.918375
44.965741	1364.778620	18.923392
44.661785	1360.754928	18.928410
44.980555	1366.947495	18.933427
45.052576	1362.574931	18.938445
44.742664	1359.988064	18.943463
44.828539	1363.177838	18.948480
45.281654	1382.212611	18.953498
45.343070	1387.078783	18.958515
45.024398	1392.392300	18.963533
45.101746	1394.680842	18.968551
45.348022	1393.872467	18.973568
45.579964	1389.456062	18.978586
45.259710	1390.449504	18.983603
45.373753	1390.106688	18.988621
45.683824	1378.640639	18.993639
45.640643	1381.071022	18.998656
45.848971	1377.279994	19.003674
45.757737	1385.821217	19.008691
45.965915	1393.874011	19.013709
46.213596	1379.997159	19.018727
45.576077	1394.950861	19.023744
45.657422	1389.674273	19.028762
45.669971	1399.284946	19.033779
45.479827	1407.911007	19.038797
46.084021	1410.597210	19.043815
45.758302	1418.887776	19.048832
45.990609	1414.808982	19.053850
45.959482	1412.371208	19.058867
45.876476	1415.997542	19.063885
46.120119	1426.443259	19.068903
46.322873	1433.588037	19.073920
47.272887	1424.001029	19.078938
47.173277	1424.067021	19.083955
47.064649	1411.173433	19.088973
46.888298	1400.332217	19.093991
46.886650	1408.411376	19.099008
46.796825	1397.244263	19.104026
46.846545	1397.072409	19.109043
46.431595	1397.414716	19.114061
46.722483	1389.473546	19.119079
46.747437	1396.507136	19.124096
46.680841	1384.629511	19.129114
46.852553	1385.880873	19.134131
47.010687	1386.926066	19.139149
47.108479	1391.508863	19.144167
46.999291	1398.118367	19.149184
46.707911	1394.802771	19.154202
47.032423	1406.832732	19.159219
46.932470	1424.688174	19.164237
47.142539	1418.700409	19.169255
46.922956	1417.153517	19.174272
46.809817	1421.617683	19.179290
47.392947	1411.289379	19.184307
46.960035	1431.519356	19.189325
47.621099	1429.926870	19.194343
47.729818	1447.074498	19.199360
47.752845	1444.066550	19.204378
47.451098	1436.684693	19.209395
47.534615	1445.022009	19.214413
47.955960	1436.757548	19.219431
47.784921	1440.943552	19.224448
47.975467	1438.304002	19.229466
48.118071	1435.138582	19.234483
48.228578	1445.718648	19.239501
47.995391	1436.959641	19.244519
47.950989	1442.044276	19.249536
47.913937	1431.575832	19.254554
48.036340	1432.257358	19.259571
47.943002	1441.796177	19.264589
47.994882	1445.215323	19.269607
48.121988	1431.574956	19.274624
48.344293	1440.237803	19.279642
48.545807	1437.896350	19.284659
48.198893	1431.490367	19.289677
48.253092	1424.712664	19.294695
47.975722	1436.340889	19.299712
48.529931	1444.526026	19.304730
48.608452	1431.858908	19.309747
47.865166	1440.072484	19.314765
48.575927	1442.985099	19.319783
48.426441	1465.629380	19.324800
48.382433	1459.024746	19.329818
48.632980	1455.668945	19.334835
48.394620	1466.233912	19.339853
48.373428	1450.123509	19.344871
48.594125	1467.348397	19.349888
48.780233	1479.144333	19.354906
49.230660	1489.251775	19.359923
49.327409	1486.945562	19.364941
49.549536	1475.871844	19.369959
49.510987	1477.802896	19.374976
49.605638	1480.975546	19.379994
49.315572	1474.380814	19.385011
49.370694	1474.309104	19.390029
49.457451	1481.298391	19.395047
49.855562	1476.114471	19.400064
49.707594	1473.915789	19.405082
49.631949	1458.757452	19.410099
49.376401	1466.926661	19.415117
49.732131	1476.386114	19.420135
49.752161	1476.809023	19.425152
49.566175	1484.591865	19.430170
49.662544	1483.472307	19.435187
49.321132	1479.097810	19.440205
49.703013	1480.720405	19.445223
49.806134	1479.994276	19.450240
49.352286	1481.160003	19.455258
49.747127	1486.791652	19.460275
50.058737	1490.217705	19.465293
49.973309	1497.830260	19.470311
50.348575	1506.485104	19.475328
50.127356	1502.003525	19.480346
50.019154	1504.500853	19.485363
49.928958	1508.396573	19.490381
50.009700	1499.837969	19.495399
50.229782	1499.484953	19.500416
49.823628	1513.430732	19.505434
50.363379	1515.057153	19.510451
50.652507	1523.902144	19.515469
50.562812	1513.328238	19.520487
50.861608	1516.945642	19.525504
50.641961	1521.931351	19.530522
51.181717	1514.147041	19.535539
51.140088	1514.327084	19.540557
51.157885	1504.891485	19.545575
50.855155	1511.651087	19.550592
51.272252	1520.233152	19.555610
51.324745	1506.822098	19.560627
51.072746	1516.653906	19.565645
50.963465	1519.170339	19.570663
50.965706	1517.973915	19.575680
50.924645	1511.031127	19.580698
50.990126	1520.598911	19.585715
51.304308	1516.961788	19.590733
51.287688	1515.862975	19.595751
51.365910	1526.669025	19.600768
50.984018	1542.965312	19.605786
51.555364	1535.920855	19.610803
51.775017	1537.925324	19.615821
51.904020	1537.169916	19.620839
51.994840	1539.456379	19.625856
51.916083	1539.497033	19.630874
52.217299	1533.577091	19.635891
51.903813	1531.489380	19.640909
51.716289	1526.311418	19.645927
51.663678	1512.752619	19.650944
51.969273	1538.904867	19.655962
52.424791	1535.851659	19.660979
52.067101	1527.468602	19.665997
51.789274	1542.350645	19.671015
51.969709	1541.344229	19.676032
51.925468	1552.090465	19.681050
52.090091	1544.869484	19.686067
52.129826	1535.383117	19.691085
52.341147	1534.599113	19.696103
52.186555	1540.729739	19.701120
52.053705	1546.771774	19.706138
52.521612	1548.870138	19.711155
52.572311	1560.210676	19.716173
52.479902	1552.710970	19.721191
52.550450	1561.763583	19.726208
52.630574	1563.209101	19.731226
52.464810	1553.417043	19.736243
52.224191	1565.926425	19.741261
52.412169	1570.141771	19.746279
52.651743	1582.115646	19.751296
52.598595	1592.077484	19.756314
53.049820	1581.580268	19.761331
53.044327	1580.675382	19.766349
52.946146	1585.787367	19.771367
53.304153	1583.222710	19.776384
53.273940	1594.774687	19.781402
53.700521	1591.239972	19.786419
53.727854	1590.525638	19.791437
53.844389	1580.503417	19.796455
53.887623	1574.923434	19.801472
53.611733	1567.114612	19.806490
53.499620	1562.679147	19.811507
53.480992	1569.230433	19.816525
53.967357	1577.388324	19.821543
53.880410	1567.085362	19.826560
53.880879	1569.433234	19.831578
54.013408	1577.021356	19.836595
54.123345	1579.128120	19.841613
54.072028	1570.889849	19.846631
54.184460	1570.572527	19.851648
54.088564	1578.808450	19.856666
54.115669	1589.881277	19.861683
53.949575	1592.715840	19.866701
53.942172	1589.217136	19.871719
54.466802	1581.561387	19.876736
54.196643	1589.650874	19.881754
54.365168	1585.105437	19.886771
54.420045	1581.464492	19.891789
54.228098	1579.569294	19.896807
54.523420	1580.526866	19.901824
54.481913	1583.881682	19.906842
54.868665	1579.630479	19.911859
54.235835	1585.362200	19.916877
54.486115	1601.156165	19.921895
54.741175	1596.057600	19.926912
54.589320	1611.888937	19.931930
54.711322	1598.416498	19.936947
54.775593	1611.048858	19.941965
54.994612	1614.969043	19.946983
55.189979	1609.756690	19.952000
54.899853	1619.727037	19.957018
55.152130	1621.265680	19.962035
55.100047	1625.890808	19.967053
55.024756	1631.182281	19.972071
55.287865	1630.084091	19.977088
54.989630	1639.598112	19.982106
55.094231	1629.716579	19.987123
55.456197	1623.518901	19.992141
55.266893	1629.162646	19.997159
55.717243	1643.088785	20.002176
55.854242	1650.717269	20.007194
55.867309	1651.813466	20.012211
56.150922	1655.243911	20.017229
55.930783	1653.719175	20.022247
56.215738	1649.976120	20.027264
56.171780	1654.170792	20.032282
56.469073	1646.275850	20.037299
56.281210	1636.850111	20.042317
56.233264	1632.344677	20.047335
56.055724	1620.657740	20.052352
56.037495	1627.480390	20.057370
55.984721	1634.769177	20.062387
56.048132	1648.907046	20.067405
56.032766	1658.768363	20.072423
56.253597	1650.730686	20.077440
56.172749	1650.673834	20.082458
56.390316	1650.021399	20.087475
56.615617	1663.187314	20.092493
56.495869	1673.803364	20.097511
56.590903	1673.438256	20.102528
56.711490	1682.467360	20.107546
56.786891	1677.756514	20.112563
56.779077	1671.657418	20.117581
56.821292	1680.301083	20.122599
57.086772	1677.245879	20.127616
57.050940	1681.221537	20.132634
56.989229	1692.273541	20.137651
56.976594	1693.465263	20.142669
57.559992	1694.633616	20.147687
57.603607	1694.705711	20.152704
57.227513	1693.823805	20.157722
57.397102	1704.255968	20.162739
57.642165	1700.134097	20.167757
57.735756	1695.814899	20.172775
57.852564	1695.301229	20.177792
58.004264	1696.404248	20.182810
57.776516	1697.051936	20.187827
57.841451	1693.393623	20.192845
57.926807	1691.007104	20.197863
58.112245	1678.509362	20.202880
57.930093	1686.089718	20.207898
57.820449	1697.448996	20.212915
58.372843	1689.012533	20.217933
57.871526	1691.227103	20.222951
58.174813	1685.032227	20.227968
58.096094	1694.183888	20.232986
57.909344	1692.789653	20.238003
58.106100	1695.495154	20.243021
57.905199	1717.273581	20.248039
58.738297	1711.816737	20.253056
58.500338	1716.208890	20.258074
58.502119	1720.636302	20.263091
58.124262	1712.158466	20.268109
58.429870	1724.197897	20.273127
58.622721	1724.451890	20.278144
59.001255	1729.385549	20.283162
59.007653	1749.162469	20.288179
58.859368	1732.620308	20.293197
58.917683	1743.057194	20.298215
59.248856	1740.310497	20.303232
59.463032	1741.100826	20.308250
59.256522	1738.819705	20.313267
59.345573	1738.023170	20.318285
59.299426	1739.753458	20.323303
59.500114	1732.245913	20.328320
59.212001	1741.597461	20.333338
59.207428	1744.410056	20.338355
59.675708	1740.666843	20.343373
59.351702	1746.552510	20.348391
59.503735	1728.180520	20.353408
59.470268	1735.548395	20.358426
59.418577	1736.392742	20.363443
59.645541	1737.048533	20.368461
59.425044	1759.959869	20.373479
60.168821	1759.566339	20.378496
60.186538	1764.190102	20.383514
59.736879	1769.969104	20.388531
60.040535	1764.752470	20.393549
59.654376	1771.376832	20.398567
59.935901	1757.188297	20.403584
59.941083	1763.792753	20.408602
59.714277	1772.172226	20.413619
60.277685	1775.499170	20.418637
59.868031	1788.278028	20.423655
60.501866	1790.779789	20.428672
60.235664	1792.437042	20.433690
60.306066	1800.079115	20.438707
60.624875	1799.830646	20.443725
60.501198	1814.026177	20.448743
60.849249	1810.238551	20.453760
60.898985	1803.628662	20.458778
60.746864	1808.651275	20.463795
61.214916	1802.806258	20.468813
61.480555	1804.787818	20.473831
61.758012	1791.259472	20.478848
61.637372	1790.612351	20.483866
61.733664	1793.936284	20.488883
61.911434	1785.450802	20.493901
61.893934	1797.013554	20.498919
61.745909	1788.925943	20.503936
61.863472	1777.713680	20.508954
61.417999	1775.327743	20.513971
61.688064	1773.161771	20.518989
61.699934	1787.983135	20.524007
61.881057	1796.520020	20.529024
62.109577	1775.898544	20.534042
61.391821	1785.108719	20.539059
61.825923	1785.811159	20.544077
61.952576	1792.548197	20.549095
61.899762	1786.872645	20.554112
62.193341	1787.492820	20.559130
61.956018	1798.300824	20.564147
61.924462	1788.591886	20.569165
61.991849	1798.629750	20.574183
62.110207	1810.199761	20.579200
62.335064	1810.373031	20.584218
62.293004	1808.202000	20.589235
62.702739	1794.359558	20.594253
62.576701	1808.142030	20.599271
62.586887	1813.290857	20.604288
62.855115	1817.367532	20.609306
62.593159	1813.946287	20.614323
62.872795	1821.076095	20.619341
63.055685	1827.365720	20.624359
62.923505	1838.466657	20.629376
63.011775	1835.388523	20.634394
62.957500	1838.833739	20.639411
63.261836	1833.336104	20.644429
63.182107	1839.373123	20.649447
62.930818	1838.989346	20.654464
63.349527	1837.131593	20.659482
62.902517	1842.089671	20.664499
63.230161	1840.643740	20.669517
63.017464	1833.623405	20.674535
63.779565	1848.346948	20.679552
63.636942	1858.098796	20.684570
63.579193	1865.498909	20.689587
64.044767	1862.914310	20.694605
64.145821	1856.501545	20.699623
64.416494	1852.700711	20.704640
64.622864	1850.942290	20.709658
64.376591	1844.583606	20.714675
64.251814	1834.463110	20.719693
64.263717	1832.757060	20.724711
63.932123	1830.927759	20.729728
64.307946	1831.683458	20.734746
64.249596	1848.623947	20.739763
64.577371	1842.431517	20.744781
64.225388	1837.979680	20.749799
64.323618	1838.071676	20.754816
64.388454	1839.958268	20.759834
63.956454	1847.173637	20.764851
64.671997	1855.819855	20.769869
64.625243	1857.906865	20.774887
64.675000	1857.883328	20.779904
64.836242	1859.369892	20.784922
65.013234	1858.218823	20.789939
65.006063	1854.467558	20.794957
65.000726	1861.799546	20.799975
64.944212	1861.170842	20.804992
65.219172	1866.114354	20.810010
65.140340	1881.903001	20.815027
65.497432	1875.655501	20.820045
65.318303	1885.087989	20.825063
65.531852	1884.581344	20.830080
65.851643	1885.595085	20.835098
65.387874	1892.203172	20.840115
65.701562	1884.684282	20.845133
65.702762	1883.860392	20.850151
65.890682	1884.585386	20.855168
65.730445	1890.439290	20.860186
65.935551	1895.273761	20.865203
65.777822	1899.744989	20.870221
66.198412	1906.325848	20.875239
66.294542	1909.978043	20.880256
66.566082	1901.455816	20.885274
65.944842	1916.640954	20.890291
66.232168	1906.689793	20.895309
66.534769	1903.174320	20.900327
66.594709	1911.007424	20.905344
66.620129	1905.142923	20.910362
66.456929	1904.735961	20.915379
66.710954	1929.318855	20.920397
66.707697	1930.139890	20.925415
66.697400	1943.118622	20.930432
66.923562	1934.063782	20.935450
66.666900	1945.698581	20.940467
66.940152	1932.470595	20.945485
66.951359	1937.928580	20.950503
66.768990	1936.306417	20.955520
67.032150	1939.415042	20.960538
67.133060	1958.306444	20.965555
67.266470	1959.876248	20.970573
67.334010	1948.873645	20.975591
67.293355	1955.649417	20.980608
67.513631	1954.949211	20.985626
67.392081	1959.749348	20.990643
67.329798	1963.173744	20.995661
67.809172	1961.868288	21.000679
67.780676	1979.388098	21.005696
67.837344	1974.310848	21.010714
67.793875	1986.288035	21.015731
68.174051	1981.987267	21.020749
67.969972	1975.893377	21.025767
67.750065	1981.573557	21.030784
68.134514	1975.782528	21.035802
68.293282	1979.443921	21.040819
68.251784	1968.878020	21.045837
68.386138	1982.241373	21.050855
68.275835	1997.258664	21.055872
68.691723	1997.219150	21.060890
69.065566	2003.021498	21.065907
68.712192	2004.970064	21.070925
68.985022	1998.792446	21.075943
68.925655	2000.875125	21.080960
69.086280	1989.277313	21.085978
69.109097	1998.668952	21.090995
68.920479	1998.849792	21.096013
69.346193	1987.927105	21.101031
69.042639	1995.422348	21.106048
69.173301	1989.020706	21.111066
69.116124	2000.403567	21.116083
69.279222	2003.316334	21.121101
69.253881	1995.285271	21.126119
69.224801	2012.047782	21.131136
69.742764	2021.658999	21.136154
69.365069	2013.667007	21.141171
69.797491	2017.336296	21.146189
70.203489	2016.130626	21.151207
69.639916	2022.855289	21.156224
69.976899	2019.003068	21.161242
69.951120	2019.758184	21.166259
70.025955	2020.892126	21.171277
70.132964	2019.038701	21.176295
70.005813	2039.742488	21.181312
70.510430	2044.192683	21.186330
70.289786	2042.361866	21.191347
70.561919	2032.876923	21.196365
70.458991	2041.265638	21.201383
70.252948	2041.019985	21.206400
70.499844	2040.747995	21.211418
70.632139	2044.763831	21.216435
70.390629	2050.671468	21.221453
70.493082	2053.012993	21.226471
70.635757	2064.491017	21.231488
71.043514	2073.242069	21.236506
70.956123	2058.037713	21.241523
70.834177	2065.978101	21.246541
71.207593	2074.996443	21.251559
71.223863	2085.294902	21.256576
71.696833	2099.596590	21.261594
71.717967	2095.891363	21.266611
71.441050	2093.289783	21.271629
71.658780	2084.435004	21.276647
71.555490	2095.257035	21.281664
71.538785	2094.110861	21.286682
71.722471	2090.058420	21.291699
71.665717	2089.265635	21.296717
71.766012	2088.227483	21.301735
71.551602	2097.870712	21.306752
72.061538	2100.884137	21.311770
72.426097	2107.524290	21.316787
72.222406	2120.100896	21.321805
72.254320	2117.498569	21.326823
72.355222	2116.744356	21.331840
72.714090	2105.689987	21.336858
72.617801	2111.060614	21.341875
72.525360	2111.513673	21.346893
72.558720	2102.599224	21.351911
72.511484	2107.141666	21.356928
72.702434	2103.315320	21.361946
72.758509	2110.117117	21.366963
72.394012	2112.490323	21.371981
72.616435	2120.121488	21.376999
72.536244	2140.972722	21.382016
72.674922	2138.426356	21.387034
72.827108	2134.306223	21.392051
72.683077	2150.711201	21.397069
73.088289	2147.668879	21.402087
73.204737	2162.859298	21.407104
73.477327	2162.731636	21.412122
73.814506	2172.184880	21.417139
73.699236	2163.561799	21.422157
74.002492	2158.761699	21.427175
73.517739	2167.531829	21.432192
73.977332	2167.122575	21.437210
74.095495	2183.587753	21.442227
74.241134	2184.224663	21.447245
74.447992	2180.872374	21.452263
74.059627	2186.932315	21.457280
74.299979	2185.859727	21.462298
74.727252	2185.739542	21.467315
74.805067	2187.759856	21.472333
74.809507	2187.083778	21.477351
74.353938	2181.739065	21.482368
74.653574	2182.042715	21.487386
74.442431	2177.234332	21.492403
74.396139	2180.315436	21.497421
74.695579	2181.439667	21.502439
74.542560	2176.691666	21.507456
74.592355	2197.336526	21.512474
74.853615	2206.618562	21.517491
75.022762	2205.566528	21.522509
75.343311	2205.096866	21.527527
74.966118	2201.851286	21.532544
75.076051	2200.997829	21.537562
75.370305	2205.865844	21.542579
75.348465	2217.555782	21.547597
75.664911	2222.085814	21.552615
76.031881	2220.924079	21.557632
75.881499	2224.583159	21.562650
75.567921	2222.599526	21.567667
75.774407	2226.619633	21.572685
76.028898	2213.523756	21.577703
75.922566	2206.480402	21.582720
76.027048	2220.804842	21.587738
76.059420	2218.142466	21.592755
76.257478	2231.322509	21.597773
76.707165	2241.758716	21.602791
76.601593	2243.883333	21.607808
76.479782	2239.146236	21.612826
76.698816	2227.479213	21.617843
76.416463	2235.949606	21.622861
76.639991	2241.166331	21.627879
76.384728	2234.796284	21.632896
76.376049	2234.062284	21.637914
76.846205	2253.802273	21.642931
76.511876	2261.889430	21.647949
76.909337	2261.966400	21.652967
76.778840	2257.495753	21.657984
77.136258	2268.388178	21.663002
77.260904	2273.601373	21.668019
77.189195	2289.244095	21.673037
77.300490	2280.964400	21.678055
77.282907	2295.257409	21.683072
77.242734	2290.375037	21.688090
77.312261	2288.663128	21.693107
77.258090	2300.017307	21.698125
77.649542	2305.700240	21.703143
77.562095	2304.713398	21.708160
77.768353	2312.615420	21.713178
78.020071	2312.554127	21.718195
78.183174	2305.209994	21.723213
78.516011	2312.887170	21.728231
78.406330	2324.938012	21.733248
78.492553	2337.084601	21.738266
78.730404	2326.702228	21.743283
78.736726	2331.883366	21.748301
79.131149	2334.409857	21.753319
79.108169	2323.790368	21.758336
78.786739	2316.976131	21.763354
78.927252	2316.540810	21.768371
78.947899	2320.652991	21.773389
78.716899	2317.065873	21.778407
78.997725	2324.429241	21.783424
78.868065	2318.068012	21.788442
79.285151	2316.961589	21.793459
79.406184	2322.134332	21.798477
79.245410	2325.618315	21.803495
79.424792	2341.736416	21.808512
79.691744	2348.413948	21.813530
79.568190	2343.737059	21.818547
79.720208	2347.446918	21.823565
79.670492	2338.772518	21.828583
79.676368	2342.066446	21.833600
79.688449	2345.779156	21.838618
80.044916	2347.465754	21.843635
79.999865	2363.669313	21.848653
80.289087	2366.859167	21.853671
80.291556	2364.138305	21.858688
80.237194	2371.383455	21.863706
80.405194	2364.511934	21.868723
80.325017	2363.950016	21.873741
80.464261	2357.502723	21.878759
80.772691	2375.516450	21.883776
80.806676	2371.127470	21.888794
81.183826	2382.764864	21.893811
80.873111	2382.522878	21.898829
81.138847	2382.014406	21.903847
81.208520	2387.709593	21.908864
81.314500	2383.435640	21.913882
81.339866	2382.601653	21.918899
81.130820	2377.218499	21.923917
81.525871	2379.568163	21.928935
81.111373	2385.483907	21.933952
81.243024	2395.294336	21.938970
81.740394	2396.337269	21.943987
81.767109	2409.910216	21.949005
81.489926	2402.038109	21.954023
81.602800	2403.649021	21.959040
81.817566	2406.515939	21.964058
82.014168	2420.696801	21.969075
81.990432	2426.343423	21.974093
81.949957	2424.200474	21.979111
82.350069	2424.128701	21.984128
82.322990	2427.907489	21.989146
82.162901	2429.374698	21.994163
82.419346	2439.115226	21.999181
82.657785	2457.070500	22.004199
82.843755	2456.385085	22.009216
82.496901	2461.491851	22.014234
82.881395	2465.077172	22.019251
83.011950	2450.141527	22.024269
82.644937	2447.885303	22.029287
82.906330	2453.288712	22.034304
83.053542	2462.553922	22.039322
83.290799	2473.682945	22.044339
83.230630	2479.070151	22.049357
83.449990	2482.375051	22.054375
83.697091	2479.590836	22.059392
83.446456	2488.106905	22.064410
83.790840	2483.398153	22.069427
83.853799	2481.355867	22.074445
83.668100	2483.155293	22.079463
83.875388	2482.381346	22.084480
83.792420	2503.646872	22.089498
83.942483	2497.163128	22.094515
84.081032	2503.229506	22.099533
84.065226	2501.354125	22.104551
83.995977	2507.367644	22.109568
84.193880	2514.889178	22.114586
84.928318	2521.607608	22.119603
84.595512	2527.261353	22.124621
84.843363	2527.254314	22.129639
85.112997	2513.616181	22.134656
84.856510	2525.708951	22.139674
85.025553	2529.801232	22.144691
85.069138	2519.897149	22.149709
84.934147	2522.692298	22.154727
84.741098	2509.896274	22.159744
85.112637	2534.483795	22.164762
85.394548	2539.483221	22.169779
85.811252	2540.879572	22.174797
85.702798	2545.122366	22.179815
86.085397	2540.966266	22.184832
85.349499	2551.214830	22.189850
85.239623	2547.185900	22.194867
85.742056	2549.670359	22.199885
85.746317	2568.381779	22.204903
85.916438	2564.334499	22.209920
86.136436	2565.086088	22.214938
85.902485	2568.452114	22.219955
86.488264	2568.458739	22.224973
86.179734	2570.668645	22.229991
86.372211	2576.003920	22.235008
86.127663	2590.086331	22.240026
86.614719	2594.678264	22.245043
87.049754	2597.479358	22.250061
86.815771	2593.422400	22.255079
86.850592	2586.079188	22.260096
87.014513	2603.841070	22.265114
87.322730	2610.969901	22.270131
87.429947	2612.995154	22.275149
87.363344	2616.496092	22.280167
87.777658	2615.412175	22.285184
87.639796	2613.896638	22.290202
87.803505	2608.991905	22.295219
87.746727	2612.298794	22.300237
87.815474	2614.077553	22.305255
87.838552	2610.977876	22.310272
87.458169	2617.055654	22.315290
87.486797	2610.767514	22.320307
87.964179	2619.747853	22.325325
87.946550	2639.475844	22.330343
88.497648	2642.574479	22.335360
88.477994	2637.916053	22.340378
88.574165	2632.314875	22.345395
88.868398	2627.004779	22.350413
89.197389	2622.099557	22.355431
88.928138	2618.868654	22.360448
88.830250	2625.069722	22.365466
88.836518	2617.102891	22.370483
89.210617	2621.191672	22.375501
88.659079	2627.040461	22.380519
88.578942	2617.622681	22.385536
89.028523	2631.537088	22.390554
89.322281	2646.207969	22.395571
89.481927	2645.583454	22.400589
89.688733	2658.402661	22.405607
89.936725	2650.003676	22.410624
89.474024	2644.095001	22.415642
89.816531	2651.928619	22.420659
89.522716	2660.192697	22.425677
89.461537	2663.105774	22.430695
89.603157	2659.832986	22.435712
89.795978	2669.618262	22.440730
89.523373	2671.383897	22.445747
89.930086	2671.614077	22.450765
89.928932	2681.271757	22.455783
89.976936	2686.263456	22.460800
90.202450	2703.362544	22.465818
90.474697	2700.763743	22.470835
90.848360	2714.071448	22.475853
90.570044	2726.186688	22.480871
91.004710	2726.747058	22.485888
90.815376	2724.684059	22.490906
91.015512	2731.387918	22.495923
90.850311	2724.678599	22.500941
90.813309	2734.187242	22.505959
91.026281	2745.796781	22.510976
91.357898	2752.110917	22.515994
91.035141	2761.376862	22.521011
91.541374	2753.085958	22.526029
91.791728	2770.114965	22.531047
91.983198	2774.055475	22.536064
91.921136	2778.306881	22.541082
92.001563	2775.545415	22.546099
92.660465	2775.168240	22.551117
92.445553	2778.499780	22.556135
92.470018	2766.212551	22.561152
91.971915	2773.792060	22.566170
91.984483	2773.111538	22.571187
92.587378	2773.560505	22.576205
92.432204	2797.040554	22.581223
92.643342	2794.148272	22.586240
92.565938	2798.932291	22.591258
92.605030	2800.797744	22.596275
93.074267	2815.403570	22.601293
92.959010	2827.471397	22.606311
93.039261	2819.717040	22.611328
93.372599	2817.250735	22.616346
93.425017	2814.058085	22.621363
93.719567	2806.633317	22.626381
93.501108	2803.157767	22.631399
94.048516	2809.605598	22.636416
94.029323	2814.715103	22.641434
94.105018	2805.168811	22.646451
94.049206	2805.256392	22.651469
93.532601	2820.965688	22.656487
94.214720	2819.496052	22.661504
94.593693	2832.888233	22.666522
94.372675	2825.335427	22.671539
94.436130	2827.010881	22.676557
94.303531	2834.419890	22.681575
94.625095	2825.996744	22.686592
94.580301	2819.230771	22.691610
94.562135	2847.944420	22.696627
94.848565	2848.209111	22.701645
95.002433	2855.728176	22.706663
94.726745	2839.482562	22.711680
94.938944	2850.508414	22.716698
94.898284	2855.359317	22.721715
95.119180	2853.481764	22.726733
95.159365	2882.454651	22.731751
95.612072	2884.590261	22.736768
95.687546	2885.108722	22.741786
95.619412	2879.476239	22.746803
95.734178	2867.269564	22.751821
95.585750	2884.095656	22.756839
95.777635	2889.137601	22.761856
96.394727	2903.127134	22.766874
96.024532	2903.976939	22.771891
96.074550	2904.303686	22.776909
96.249154	2913.545928	22.781927
96.118472	2907.708560	22.786944
96.237907	2924.224717	22.791962
96.476164	2932.317708	22.796979
96.793153	2925.997187	22.801997
96.751439	2930.602099	22.807015
96.737985	2931.503670	22.812032
96.975395	2935.089893	22.817050
97.214575	2955.879725	22.822067
97.254330	2945.515214	22.827085
97.301106	2955.105613	22.832103
97.283412	2945.457011	22.837120
97.518024	2951.006765	22.842138
97.777700	2976.136220	22.847155
97.930038	2977.097196	22.852173
97.513282	2984.891367	22.857191
97.917141	2973.542256	22.862208
97.910708	2973.230793	22.867226
98.070964	2976.532363	22.872243
98.385608	2973.409322	22.877261
97.918701	2981.217612	22.882279
98.502478	2981.025717	22.887296
99.740265	2972.466166	22.892314
99.592093	2979.366371	22.897331
99.994036	2957.959072	22.902349
99.436193	2950.909976	22.907367
99.607069	2942.380836	22.912384
99.348734	2940.596823	22.917402
99.297717	2950.764231	22.922419
99.337076	2937.770756	22.927437
99.005205	2941.931651	22.932455
99.040528	2945.991193	22.937472
99.579042	2954.009043	22.942490
99.325676	2967.304096	22.947507
99.600434	2965.695882	22.952525
99.644500	2970.445255	22.957543
99.789840	2977.280824	22.962560
100.040342	2971.797537	22.967578
100.404395	2998.375204	22.972595
100.477299	2990.779723	22.977613
100.337543	2996.027981	22.982631
100.412365	2995.716491	22.987648
100.286569	3002.553255	22.992666
99.965414	2999.604945	22.997683
100.248653	3014.394541	23.002701
100.471740	3021.833464	23.007719
100.626551	3025.123267	23.012736
100.926125	3026.916628	23.017754
101.086455	3042.905769	23.022771
101.346690	3032.715183	23.027789
101.325761	3043.218818	23.032807
101.090860	3044.170653	23.037824
101.590276	3042.723134	23.042842
101.312766	3049.346828	23.047859
101.943420	3034.752600	23.052877
101.885498	3045.684915	23.057895
101.800926	3045.767507	23.062912
102.073553	3055.486914	23.067930
102.041349	3072.503390	23.072947
102.310866	3072.404608	23.077965
102.358761	3070.137360	23.082983
102.104879	3071.199459	23.088000
102.579989	3069.616853	23.093018
102.142649	3074.296022	23.098035
102.402925	3083.269367	23.103053
102.618915	3088.228713	23.108071
102.865421	3102.291880	23.113088
103.035053	3092.623503	23.118106
102.770730	3103.445963	23.123123
103.161005	3113.301735	23.128141
103.458484	3104.323575	23.133159
103.614229	3102.759127	23.138176
103.865242	3104.175010	23.143194
103.485903	3099.547215	23.148211
103.938921	3104.949392	23.153229
103.878068	3099.931151	23.158247
104.061755	3119.461050	23.163264
104.390947	3118.696503	23.168282
104.115906	3132.133922	23.173299
104.424470	3130.072260	23.178317
104.374507	3130.430359	23.183335
104.329472	3136.115237	23.188352
104.889463	3125.799026	23.193370
104.294145	3134.867732	23.198387
104.641014	3147.075286	23.203405
104.640511	3153.292934	23.208423
104.734297	3158.463849	23.213440
105.041508	3154.193102	23.218458
105.221007	3162.427904	23.223475
105.435389	3177.452440	23.228493
105.572340	3176.055032	23.233511
105.604754	3182.728362	23.238528
105.756402	3173.962240	23.243546
105.767371	3179.903528	23.248563
105.836902	3177.134228	23.253581
105.931377	3173.445766	23.258599
105.769079	3196.611832	23.263616
106.171851	3191.107927	23.268634
106.048766	3199.143677	23.273651
106.282901	3198.185620	23.278669
106.749965	3189.193640	23.283687
106.520251	3192.587526	23.288704
106.683281	3195.058640	23.293722
106.787041	3214.070855	23.298739
107.107169	3211.770673	23.303757
107.184834	3218.181324	23.308775
107.166607	3219.860064	23.313792
107.587893	3218.175360	23.318810
106.946110	3224.357162	23.323827
107.353536	3224.732422	23.328845
107.523168	3241.799694	23.333863
107.496556	3241.857481	23.338880
107.779742	3236.034474	23.343898
107.602602	3245.473677	23.348915
107.682184	3248.049319	23.353933
107.876808	3253.627486	23.358951
108.099733	3267.180001	23.363968
108.514041	3255.507160	23.368986
108.043854	3271.323241	23.374003
108.341186	3265.434899	23.379021
108.375258	3276.917983	23.384039
108.347505	3285.674313	23.389056
108.758271	3284.720313	23.394074
108.798522	3290.688640	23.399091
108.700034	3286.522056	23.404109
109.483205	3294.757616	23.409127
109.136462	3310.238897	23.414144
109.403777	3302.161685	23.419162
109.346891	3311.872567	23.424179
109.546858	3305.910998	23.429197
109.695406	3304.420245	23.434215
109.837230	3306.329724	23.439232
110.052827	3323.210015	23.444250
110.236811	3331.466289	23.449267
110.008130	3327.654519	23.454285
110.417923	3330.579594	23.459303
110.236478	3328.736228	23.464320
110.460470	3327.972270	23.469338
110.353159	3329.475520	23.474355
110.703185	3341.379722	23.479373
110.974876	3355.988340	23.484391
110.818305	3360.421874	23.489408
110.996229	3350.436451	23.494426
110.964452	3351.628107	23.499443
111.158268	3356.474201	23.504461
111.710329	3363.341280	23.509479
111.441132	3372.555013	23.514496
111.645242	3371.784680	23.519514
111.700957	3376.762747	23.524531
111.603437	3372.368748	23.529549
111.668066	3370.853181	23.534567
111.680093	3393.496840	23.539584
112.373975	3400.922590	23.544602
112.244321	3396.640897	23.549619
112.378005	3396.869411	23.554637
112.326187	3390.028569	23.559655
112.583734	3405.772496	23.564672
112.851700	3412.226179	23.569690
112.975430	3416.325718	23.574707
113.060618	3423.091919	23.579725
113.338645	3421.615716	23.584743
113.260144	3427.722512	23.589760
113.328705	3417.918200	23.594778
113.045160	3417.331099	23.599795
113.430038	3421.557258	23.604813
113.539492	3434.963445	23.609831
113.838699	3446.512669	23.614848
113.619385	3442.989784	23.619866
113.741364	3446.957043	23.624883
114.016623	3452.301785	23.629901
113.834013	3459.624151	23.634919
113.737569	3467.188756	23.639936
114.118832	3480.356975	23.644954
114.311030	3486.522644	23.649971
114.207450	3496.382923	23.654989
114.232303	3483.751119	23.660007
114.242103	3509.352621	23.665024
114.663456	3515.050223	23.670042
114.890839	3514.143701	23.675059
115.240136	3530.731938	23.680077
115.856320	3538.968361	23.685095
115.611987	3540.783332	23.690112
115.680774	3535.874189	23.695130
115.979798	3543.519284	23.700147
115.807319	3538.704515	23.705165
116.092246	3535.838501	23.710183
116.244904	3538.541679	23.715200
116.451526	3529.763670	23.720218
116.419911	3525.709711	23.725235
116.179242	3527.681920	23.730253
116.530875	3525.487261	23.735271
116.781886	3532.716896	23.740288
116.735727	3547.274157	23.745306
116.751915	3542.136487	23.750323
116.750037	3553.884153	23.755341
117.036702	3556.525440	23.760359
116.865623	3562.807662	23.765376
117.108019	3559.468523	23.770394
117.394027	3569.413372	23.775411
117.278128	3580.171978	23.780429
117.348990	3570.256758	23.785447
117.779111	3583.881408	23.790464
117.818656	3575.441854	23.795482
117.606493	3568.726906	23.800499
118.109362	3598.954516	23.805517
118.389286	3598.617397	23.810535
118.093866	3597.814360	23.815552
117.941161	3604.128454	23.820570
118.480499	3617.874999	23.825587
118.680349	3618.582428	23.830605
118.667224	3613.689173	23.835623
118.952260	3616.387534	23.840640
118.845830	3626.169423	23.845658
119.185164	3636.393223	23.850675
119.355871	3640.214064	23.855693
119.280992	3643.991081	23.860711
119.498777	3644.544220	23.865728
119.651116	3643.400034	23.870746
119.494991	3654.199665	23.875763
119.517831	3663.131362	23.880781
119.437569	3673.183793	23.885799
119.485311	3680.426197	23.890816
119.709357	3687.275033	23.895834
120.117547	3707.348207	23.900851
120.077890	3717.239686	23.905869
120.549667	3725.621771	23.910887
120.349211	3726.495684	23.915904
120.661254	3741.480237	23.920922
120.687406	3747.422504	23.925939
120.834617	3752.260180	23.930957
121.325572	3749.661898	23.935975
121.447421	3759.888066	23.940992
121.213662	3771.763507	23.946010
121.885832	3774.780368	23.951027
121.864843	3779.839925	23.956045
121.960173	3776.596237	23.961063
121.855653	3776.779780	23.966080
122.006630	3776.226015	23.971098
122.384538	3777.959913	23.976115
122.375696	3791.233283	23.981133
122.233904	3804.584174	23.986151
122.380875	3804.343501	23.991168
122.335556	3796.901805	23.996186
122.925047	3807.033099	24.001203
122.942471	3824.017307	24.006221
123.185991	3818.657945	24.011239
123.683903	3817.769258	24.016256
123.210304	3815.100202	24.021274
123.354565	3814.721076	24.026291
123.387385	3828.287830	24.031309
123.538087	3832.989265	24.036327
123.570756	3848.140496	24.041344
123.620486	3844.140082	24.046362
123.777737	3850.074597	24.051379
123.716871	3862.390305	24.056397
123.997829	3868.984161	24.061415
124.503525	3871.136893	24.066432
124.086744	3873.518466	24.071450
124.662176	3875.849717	24.076467
124.644963	3884.263819	24.081485
125.213050	3886.318464	24.086503
125.049199	3888.607003	24.091520
125.194635	3896.361380	24.096538
125.141727	3895.754135	24.101555
125.450932	3889.699617	24.106573
125.462891	3887.459955	24.111591
125.365577	3895.255282	24.116608
125.817204	3908.463360	24.121626
125.959775	3918.096170	24.126643
126.069427	3915.083791	24.131661
126.200697	3912.247953	24.136679
126.205677	3912.417606	24.141696
126.355636	3925.454881	24.146714
126.688283	3936.248020	24.151731
126.520469	3930.637040	24.156749
126.689856	3928.555926	24.161767
126.772573	3926.163211	24.166784
126.741005	3946.819590	24.171802
127.392504	3952.080654	24.176819
127.403386	3960.765014	24.181837
127.424630	3964.123128	24.186855
127.397552	3964.465055	24.191872
127.295422	3959.863316	24.196890
127.718817	3969.234648	24.201907
127.827405	3976.051070	24.206925
128.092704	3978.686278	24.211943
128.119263	3982.535947	24.216960
127.859562	3994.952140	24.221978
128.220471	3997.133743	24.226995
128.334962	4013.528573	24.232013
128.538332	4011.707287	24.237031
128.846577	4024.050858	24.242048
128.555031	4039.205382	24.247066
128.980029	4032.545719	24.252083
129.006609	4046.189360	24.257101
129.322119	4060.899041	24.262119
129.641712	4058.459960	24.267136
129.626164	4067.394677	24.272154
130.050204	4059.447386	24.277171
129.953279	4060.257851	24.282189
129.955163	4061.273873	24.287207
129.966182	4065.621518	24.292224
130.348805	4071.858741	24.297242
130.504200	4081.088793	24.302259
130.254952	4088.633259	24.307277
130.396902	4078.343719	24.312295
130.721820	4094.772144	24.317312
130.742895	4102.318718	24.322330
130.935170	4110.716092	24.327347
131.112318	4104.669437	24.332365
130.998274	4111.489009	24.337383
131.384844	4122.668403	24.342400
131.570974	4130.738487	24.347418
131.592006	4125.325298	24.352435
131.799453	4129.686565	24.357453
131.959535	4138.739163	24.362471
132.228216	4144.460735	24.367488
131.977731	4146.990049	24.372506
132.012356	4146.899427	24.377523
132.419056	4158.242993	24.382541
132.421324	4171.537007	24.387559
132.886221	4177.701488	24.392576
132.647988	4180.746534	24.397594
132.923939	4179.415785	24.402611
133.235757	4180.989572	24.407629
132.997816	4187.942089	24.412647
133.417237	4195.663406	24.417664
133.328068	4204.271927	24.422682
133.346920	4204.928652	24.427699
133.719831	4204.299289	24.432717
133.403212	4214.407758	24.437735
133.916555	4223.345428	24.442752
133.919590	4231.683945	24.447770
134.268887	4232.090375	24.452787
134.321591	4240.537947	24.457805
134.216142	4252.191720	24.462823
134.565176	4255.262131	24.467840
134.170200	4262.109716	24.472858
134.560989	4274.487951	24.477875
134.866685	4285.105585	24.482893
134.641771	4278.616457	24.487911
135.423605	4294.235345	24.492928
135.601055	4294.864224	24.497946
135.675037	4299.041149	24.502963
135.470755	4307.749706	24.507981
135.864945	4312.476484	24.512999
136.349768	4322.005723	24.518016
136.492521	4328.299319	24.523034
136.400934	4332.543062	24.528051
136.657544	4329.056378	24.533069
136.402576	4330.273377	24.538087
136.948421	4341.592239	24.543104
136.971648	4351.894068	24.548122
137.164492	4349.755596	24.553139
137.310591	4358.340187	24.558157
137.094932	4350.018913	24.563175
137.586034	4354.695894	24.568192
137.529840	4370.281192	24.573210
137.502381	4370.954602	24.578227
137.762545	4371.911491	24.583245
137.645559	4373.911880	24.588263
137.889046	4380.420224	24.593280
138.299668	4390.147276	24.598298
138.156704	4392.347405	24.603315
138.355353	4398.064180	24.608333
138.762277	4420.537171	24.613351
139.121072	4415.011339	24.618368
139.000269	4417.372150	24.623386
139.134518	4420.999984	24.628403
139.175859	4421.807877	24.633421
138.968072	4437.517837	24.638439
139.370251	4436.334704	24.643456
139.197521	4440.531134	24.648474
139.728055	4451.691475	24.653491
139.715910	4468.147466	24.658509
139.567937	4476.512762	24.663527
139.731347	4478.068649	24.668544
139.734061	4495.604985	24.673562
140.018088	4513.217482	24.678579
140.667424	4519.047198	24.683597
140.800762	4523.429566	24.688615
141.004634	4522.984330	24.693632
140.817121	4533.432702	24.698650
141.670864	4536.389862	24.703667
142.127781	4529.898649	24.708685
141.930662	4545.869021	24.713703
142.345199	4531.102077	24.718720
142.094838	4536.137585	24.723738
142.364728	4528.349814	24.728755
142.504013	4529.609606	24.733773
142.510403	4531.666556	24.738791
142.118145	4527.056184	24.743808
142.079959	4533.570561	24.748826
142.462063	4531.699302	24.753843
142.742915	4531.930170	24.758861
142.432234	4552.804296	24.763879
142.538676	4555.372787	24.768896
142.684644	4558.026659	24.773914
143.103238	4570.438645	24.778931
143.203841	4590.462843	24.783949
143.263269	4589.746550	24.788967
143.127173	4590.607326	24.793984
143.783878	4612.303074	24.799002
143.883914	4608.651331	24.804019
143.881890	4607.433270	24.809037
144.059539	4631.848678	24.814055
144.512676	4623.947114	24.819072
144.575500	4631.411655	24.824090
144.798880	4624.467528	24.829107
144.920754	4635.101362	24.834125
145.041288	4658.253672	24.839143
145.262950	4657.527900	24.844160
145.283086	4661.609131	24.849178
145.514442	4653.685268	24.854195
145.530867	4658.344696	24.859213
145.438767	4682.855829	24.864231
145.583901	4676.485703	24.869248
145.970891	4686.030367	24.874266
146.314662	4696.247765	24.879283
146.255817	4698.093942	24.884301
146.358708	4707.341957	24.889319
146.473727	4702.602059	24.894336
146.879686	4714.208072	24.899354
146.874107	4725.445737	24.904371
146.905890	4734.250314	24.909389
146.728859	4740.192977	24.914407
147.600514	4739.675333	24.919424
147.396669	4744.918293	24.924442
147.495254	4749.091491	24.929459
147.680717	4745.480079	24.934477
147.617600	4764.425214	24.939495
147.584691	4770.007712	24.944512
147.907618	4782.993425	24.949530
148.058957	4793.518602	24.954547
148.709650	4793.054297	24.959565
148.745823	4802.918781	24.964583
148.755923	4809.962331	24.969600
149.245203	4823.903820	24.974618
149.261082	4829.870137	24.979635
149.501802	4830.605974	24.984653
149.141679	4835.058932	24.989671
149.608412	4847.899201	24.994688
150.011059	4848.818152	24.999706
150.022245	4855.186075	25.004723
150.450570	4851.379009	25.009741
150.306971	4847.986100	25.014759
150.617349	4861.908125	25.019776
150.802774	4873.138240	25.024794
150.437733	4874.375568	25.029811
150.955360	4879.117999	25.034829
150.803108	4872.708881	25.039847
151.121896	4884.145502	25.044864
151.015019	4898.849030	25.049882
150.935772	4898.933955	25.054899
151.436121	4903.369752	25.059917
151.652141	4918.218722	25.064935
151.686288	4929.144154	25.069952
151.916765	4928.555883	25.074970
152.084027	4927.134684	25.079987
152.604534	4937.886549	25.085005
152.405813	4943.138238	25.090023
152.551494	4945.523914	25.095040
152.682982	4946.137878	25.100058
152.839232	4946.422873	25.105075
152.870443	4953.166485	25.110093
152.991105	4971.795988	25.115111
153.010240	4970.609329	25.120128
153.379817	4971.590252	25.125146
153.011640	4989.784535	25.130163
153.385856	4996.032858	25.135181
153.426821	5012.143333	25.140199
153.805404	5013.296461	25.145216
153.852690	5020.615227	25.150234
153.975018	5041.476158	25.155251
154.382635	5053.221015	25.160269
154.352171	5059.046269	25.165287
154.416780	5070.219560	25.170304
154.789508	5080.732532	25.175322
154.802264	5084.388883	25.180339
155.058821	5094.531704	25.185357
155.080899	5100.291974	25.190375
155.501738	5104.206756	25.195392
155.872508	5123.132060	25.200410
156.105022	5133.666893	25.205427
156.359575	5126.859762	25.210445
156.303768	5133.746406	25.215463
156.380924	5139.933707	25.220480
156.554182	5151.554135	25.225498
156.574731	5166.361143	25.230515
156.944636	5157.717907	25.235533
156.971605	5171.876840	25.240551
157.127779	5177.240636	25.245568
157.388961	5167.231782	25.250586
157.396531	5182.116579	25.255603
157.371430	5196.463558	25.260621
157.717168	5198.297300	25.265639
157.750555	5206.252760	25.270656
157.975399	5209.885587	25.275674
158.376752	5219.844953	25.280691
158.393291	5212.301507	25.285709
158.217606	5229.004604	25.290727
158.681617	5247.120084	25.295744
158.942140	5249.983491	25.300762
158.679107	5273.688717	25.305779
159.103222	5278.767776	25.310797
159.183256	5280.485069	25.315815
159.550337	5299.531079	25.320832
159.671057	5293.028809	25.325850
159.937108	5311.790693	25.330867
159.765288	5316.697398	25.335885
160.223774	5331.966651	25.340903
160.222183	5333.946022	25.345920
160.739670	5336.453785	25.350938
160.494467	5358.502332	25.355955
160.452470	5355.948925	25.360973
160.517159	5373.811050	25.365991
160.765465	5387.424335	25.371008
161.402695	5385.522740	25.376026
161.341795	5398.101486	25.381043
161.502149	5410.298576	25.386061
161.854548	5418.718976	25.391079
162.009470	5410.980293	25.396096
162.692768	5418.339087	25.401114
162.956372	5422.111122	25.406131
162.784760	5413.334274	25.411149
163.299420	5425.574065	25.416167
163.040366	5414.358208	25.421184
163.332523	5411.291915	25.426202
163.406981	5422.025132	25.431219
163.602984	5424.532455	25.436237
163.634523	5423.350149	25.441255
163.713690	5415.468589	25.446272
163.899194	5422.074719	25.451290
164.226808	5443.282933	25.456307
164.158561	5440.392696	25.461325
164.133921	5439.698928	25.466343
164.028391	5439.503860	25.471360
164.347442	5450.887137	25.476378
164.489021	5473.260702	25.481395
164.601446	5466.456634	25.486413
165.193322	5481.064469	25.491431
165.031525	5489.018876	25.496448
165.309412	5489.256533	25.501466
165.487203	5497.603145	25.506483
165.738707	5502.052581	25.511501
166.101308	5512.971418	25.516519
165.976500	5513.470633	25.521536
166.447510	5510.139738	25.526554
166.786127	5526.463165	25.531571
167.218481	5531.143288	25.536589
167.038812	5534.195222	25.541607
166.920267	5537.995213	25.546624
167.418167	5533.296498	25.551642
167.361436	5539.028142	25.556659
167.715377	5536.899174	25.561677
167.470717	5551.428974	25.566695
167.528757	5549.226125	25.571712
167.891980	5547.786995	25.576730
167.901476	5570.799928	25.581747
168.008834	5581.405011	25.586765
168.204337	5585.348667	25.591783
168.216477	5597.512140	25.596800
168.897136	5603.564606	25.601818
168.707859	5615.349097	25.606835
168.903110	5623.434210	25.611853
168.822064	5634.586333	25.616871
169.230779	5644.415368	25.621888
169.982498	5643.543903	25.626906
169.727444	5657.251541	25.631923
169.878454	5654.140896	25.636941
170.192210	5660.304165	25.641959
170.306826	5682.922085	25.646976
170.298659	5682.222587	25.651994
170.482554	5690.776671	25.657011
170.628571	5700.861283	25.662029
171.061859	5713.745253	25.667047
170.829842	5721.376096	25.672064
171.329474	5729.063487	25.677082
171.212011	5743.100148	25.682100
171.324726	5748.129968	25.687117
171.611065	5758.435822	25.692135
171.820554	5767.143787	25.697152
172.455297	5775.425697	25.702170
172.149943	5788.759317	25.707188
172.193728	5785.977846	25.712205
172.806894	5800.409012	25.717223
172.973101	5810.973500	25.722240
172.729537	5803.404016	25.727258
172.840207	5812.098978	25.732276
173.445321	5827.879286	25.737293
173.504994	5837.601781	25.742311
173.668304	5840.272082	25.747328
174.328114	5852.123397	25.752346
174.180564	5860.445069	25.757364
174.519531	5857.699702	25.762381
174.711710	5851.192422	25.767399
174.718266	5861.049463	25.772416
174.652224	5855.879748	25.777434
174.889274	5870.865113	25.782452
174.818559	5875.898274	25.787469
174.841731	5867.283434	25.792487
175.145278	5898.372947	25.797504
175.390965	5902.504569	25.802522
175.444003	5906.031707	25.807540
175.709016	5924.560795	25.812557
175.983593	5933.590151	25.817575
175.813571	5944.712123	25.822592
176.116956	5948.534894	25.827610
176.310677	5966.970957	25.832628
176.543776	5971.679060	25.837645
176.982104	5982.425402	25.842663
176.910980	5988.487717	25.847680
177.341092	5995.346382	25.852698
177.400874	6006.135890	25.857716
177.243100	6009.231844	25.862733
177.695898	6029.546866	25.867751
177.801819	6034.909269	25.872768
178.080769	6039.692324	25.877786
178.055886	6055.738215	25.882804
178.367612	6065.134336	25.887821
178.939082	6066.734156	25.892839
178.923279	6081.733808	25.897856
179.373936	6080.239990	25.902874
179.553643	6094.622079	25.907892
179.721790	6107.096207	25.912909
179.977535	6112.084919	25.917927
179.866529	6119.829666	25.922944
180.018394	6103.688169	25.927962
180.213009	6137.456103	25.932980
180.251957	6147.131483	25.937997
180.677464	6144.391540	25.943015
180.739372	6173.606212	25.948032
180.762557	6158.763146	25.953050
180.838332	6174.364165	25.958068
181.082752	6196.018671	25.963085
181.561418	6196.275587	25.968103
181.322242	6211.568969	25.973120
181.622280	6216.326691	25.978138
181.600798	6229.635376	25.983156
181.569655	6246.648349	25.988173
182.193720	6258.597039	25.993191
182.339780	6274.603882	25.998208
182.360321	6278.739076	26.003226
182.594991	6302.570176	26.008244
183.064023	6314.615644	26.013261
183.325204	6316.873036	26.018279
183.832727	6332.375404	26.023296
184.041345	6334.937710	26.028314
184.269714	6329.873544	26.033332
183.929655	6338.133861	26.038349
184.611010	6347.614631	26.043367
184.547831	6358.319321	26.048384
184.471524	6353.564589	26.053402
184.994354	6369.263477	26.058420
185.106668	6386.664616	26.063437
185.061770	6378.562047	26.068455
185.306006	6383.053868	26.073472
185.604637	6397.913282	26.078490
186.032881	6402.556392	26.083508
186.018500	6412.786324	26.088525
186.576817	6405.868293	26.093543
186.650336	6424.276182	26.098560
186.794691	6421.665201	26.103578
186.879170	6429.063975	26.108596
186.830746	6429.510285	26.113613
187.222253	6429.550336	26.118631
187.146071	6435.452594	26.123648
187.164223	6445.008258	26.128666
187.442785	6455.729247	26.133684
187.417570	6453.611855	26.138701
187.928309	6464.416656	26.143719
187.958096	6481.079437	26.148736
187.819395	6479.598426	26.153754
188.242666	6490.347413	26.158772
188.193125	6502.012861	26.163789
188.987134	6517.900098	26.168807
189.100088	6538.091820	26.173824
189.047655	6537.354987	26.178842
189.494442	6545.574968	26.183860
189.807466	6556.050740	26.188877
189.996460	6552.305841	26.193895
190.356265	6550.513615	26.198912
190.365615	6571.898962	26.203930
190.367822	6578.903387	26.208948
190.291291	6585.714886	26.213965
190.951204	6591.060650	26.218983
190.952405	6601.572368	26.224000
190.916718	6604.996655	26.229018
191.618864	6622.363010	26.234036
191.072678	6631.889833	26.239053
191.349416	6632.149785	26.244071
191.368154	6654.439750	26.249088
191.555160	6663.874538	26.254106
191.759636	6678.161685	26.259124
192.077179	6696.291942	26.264141
192.557256	6708.544296	26.269159
192.774215	6719.473906	26.274176
192.826692	6735.685127	26.279194
193.146362	6751.277077	26.284212
193.148945	6757.315543	26.289229
193.856903	6768.424437	26.294247
193.980957	6768.774454	26.299264
193.778277	6782.926196	26.304282
194.129330	6788.168580	26.309300
193.969987	6799.295721	26.314317
194.173903	6812.140417	26.319335
194.516977	6830.348909	26.324352
194.766708	6838.849087	26.329370
194.797289	6844.943202	26.334388
194.975947	6871.722722	26.339405
195.453378	6876.232024	26.344423
195.485866	6899.476651	26.349440
195.116365	6911.387894	26.354458
195.801034	6926.301280	26.359476
196.136184	6938.541627	26.364493
196.618192	6959.146718	26.369511
196.796201	6966.262819	26.374528
196.810460	6975.263770	26.379546
197.207055	6984.637682	26.384564
197.806320	6985.529294	26.389581
197.945697	6991.395014	26.394599
198.258271	6997.022265	26.399616
198.399983	7008.273129	26.404634
199.001829	7002.512959	26.409652
198.518594	7005.902824	26.414669
198.950239	7009.579579	26.419687
199.146899	7010.631734	26.424704
199.008541	7023.637198	26.429722
199.580101	7025.824259	26.434740
199.344286	7029.431309	26.439757
199.635815	7033.934869	26.444775
199.868504	7038.024578	26.449792
199.546980	7054.303779	26.454810
199.740629	7059.668609	26.459828
199.810726	7082.149978	26.464845
200.223974	7075.986664	26.469863
200.261987	7097.598609	26.474880
200.123324	7107.362129	26.479898
200.345585	7121.182799	26.484916
200.832369	7147.021369	26.489933
201.588314	7160.841059	26.494951
202.113987	7155.547285	26.499968
201.900948	7160.662935	26.504986
202.042907	7171.639217	26.510004
202.401991	7185.028246	26.515021
202.940125	7186.267168	26.520039
203.151690	7191.749207	26.525056
202.921674	7204.715403	26.530074
203.387332	7207.992298	26.535092
203.400202	7217.205092	26.540109
203.461036	7219.490632	26.545127
203.871017	7235.068934	26.550144
203.929335	7244.097883	26.555162
203.991124	7250.679741	26.560180
203.994475	7264.809248	26.565197
204.405371	7274.922941	26.570215
204.833995	7288.948374	26.575232
204.747088	7298.100978	26.580250
205.361317	7302.061895	26.585268
205.717015	7303.193483	26.590285
206.123451	7299.768148	26.595303
206.396188	7312.782421	26.600320
206.360487	7324.357845	26.605338
206.439249	7326.091314	26.610356
206.596006	7327.803169	26.615373
206.961434	7339.647621	26.620391
207.285188	7341.342950	26.625408
207.464299	7349.911184	26.630426
207.446547	7349.336232	26.635444
207.659137	7363.477434	26.640461
207.864385	7377.967046	26.645479
207.950391	7377.622175	26.650496
207.962998	7383.510914	26.655514
208.104312	7405.201844	26.660532
208.224169	7418.243151	26.665549
208.969062	7433.472734	26.670567
208.899315	7429.698490	26.675584
208.982153	7447.888130	26.680602
209.258450	7453.360170	26.685620
209.360414	7466.246453	26.690637
209.239181	7469.378002	26.695655
210.011283	7480.477344	26.700672
210.161631	7509.563571	26.705690
210.293435	7515.402226	26.710708
210.770129	7521.891174	26.715725
211.042181	7535.218245	26.720743
211.495026	7538.487725	26.725760
211.419304	7548.585780	26.730778
211.520971	7559.072934	26.735796
211.686576	7572.410290	26.740813
211.708215	7576.709765	26.745831
212.055789	7588.550844	26.750848
211.986053	7604.434600	26.755866
212.284671	7604.858477	26.760884
212.377717	7620.391742	26.765901
212.806689	7639.105398	26.770919
213.121989	7650.026566	26.775936
213.187605	7664.579183	26.780954
213.593666	7663.006949	26.785972
213.843768	7672.100957	26.790989
213.810109	7676.380651	26.796007
214.190414	7692.090239	26.801024
214.479469	7711.217209	26.806042
215.009210	7700.852630	26.811060
214.874474	7707.664135	26.816077
215.117546	7717.769475	26.821095
215.178530	7718.694420	26.826112
215.461483	7725.636632	26.831130
215.444010	7740.764177	26.836148
215.902822	7743.887547	26.841165
215.932283	7769.772939	26.846183
216.563374	7767.256465	26.851200
216.207509	7775.134739	26.856218
216.490123	7786.395712	26.861236
216.770984	7814.215112	26.866253
216.709257	7829.270696	26.871271
216.954417	7829.857592	26.876288
217.116479	7855.640380	26.881306
217.550037	7864.990047	26.886324
217.745567	7880.109801	26.891341
218.098482	7895.624939	26.896359
218.574195	7908.822707	26.901376
218.590814	7919.954699	26.906394
218.597840	7920.531318	26.911412
219.034612	7934.372874	26.916429
219.250475	7950.553416	26.921447
219.687548	7959.302761	26.926464
219.671843	7977.312535	26.931482
219.465978	7993.287272	26.936500
220.044268	7999.470132	26.941517
220.503758	8019.874719	26.946535
220.620193	8020.948894	26.951552
221.018152	8033.259120	26.956570
221.173141	8043.880312	26.961588
221.264531	8056.317207	26.966605
221.326349	8084.035366	26.971623
221.840115	8086.616708	26.976640
221.687408	8095.767325	26.981658
222.162477	8118.186910	26.986676
222.407326	8132.888784	26.991693
222.350352	8133.087064	26.996711
222.665066	8150.347869	27.001728
223.187627	8168.725479	27.006746
223.602240	8178.978001	27.011764
224.067422	8173.039858	27.016781
224.075105	8182.572799	27.021799
224.493877	8199.059769	27.026816
224.613020	8214.835719	27.031834
225.015390	8204.004510	27.036852
225.079202	8223.242848	27.041869
224.941790	8238.815671	27.046887
225.236320	8235.685405	27.051904
225.294035	8258.987805	27.056922
225.507593	8262.247315	27.061940
225.622681	8279.286759	27.066957
225.668069	8294.720674	27.071975
226.111441	8301.600245	27.076992
226.387512	8321.484399	27.082010
226.704052	8331.041944	27.087028
226.939917	8348.744567	27.092045
226.869131	8372.070273	27.097063
227.150630	8377.462853	27.102080
227.659924	8394.797776	27.107098
227.502344	8406.623318	27.112116
227.914820	8421.810766	27.117133
227.858222	8436.872361	27.122151
228.239029	8443.717527	27.127168
228.621614	8474.824359	27.132186
228.758611	8472.230021	27.137204
229.047912	8484.920527	27.142221
229.073236	8488.487204	27.147239
229.237299	8504.726810	27.152256
229.357110	8518.529754	27.157274
229.766183	8545.667313	27.162292
230.109922	8548.126812	27.167309
230.184863	8565.226440	27.172327
230.582103	8582.436916	27.177344
230.877516	8601.525936	27.182362
230.879679	8604.982587	27.187380
231.219087	8625.523351	27.192397
231.594670	8638.550965	27.197415
231.846948	8658.533900	27.202432
231.890664	8662.978574	27.207450
232.529065	8675.261266	27.212468
232.889932	8682.419020	27.217485
232.663402	8699.897202	27.222503
232.845475	8703.875196	27.227520
233.018079	8725.079773	27.232538
233.037362	8739.874076	27.237556
233.590442	8747.772263	27.242573
233.874646	8773.237391	27.247591
234.093191	8785.800207	27.252608
234.396717	8799.158021	27.257626
234.663743	8826.245494	27.262644
235.041959	8823.749309	27.267661
235.385232	8841.495667	27.272679
236.191452	8834.860167	27.277696
236.585280	8832.816175	27.282714
236.540933	8843.058437	27.287732
236.972925	8854.132638	27.292749
236.896517	8862.375132	27.297767
237.435450	8857.075656	27.302784
237.604916	8856.319968	27.307802
237.764319	8867.985955	27.312820
238.251577	8875.098850	27.317837
237.786538	8880.626747	27.322855
238.315792	8882.921652	27.327872
238.732439	8891.526238	27.332890
238.313260	8904.194734	27.337908
238.892800	8906.279757	27.342925
238.434250	8927.500743	27.347943
238.767533	8934.640790	27.352960
239.034886	8949.958610	27.357978
239.321881	8969.005121	27.362996
239.818859	8986.001547	27.368013
239.637026	9012.717175	27.373031
239.616887	9019.265063	27.378048
240.257314	9044.454106	27.383066
240.142494	9057.618352	27.388084
240.597122	9071.158053	27.393101
241.260514	9092.150884	27.398119
241.555155	9103.616007	27.403136
241.820271	9116.566442	27.408154
241.839840	9130.578037	27.413172
242.632750	9134.568368	27.418189
242.795538	9143.752469	27.423207
243.190133	9156.035555	27.428224
243.198590	9156.962436	27.433242
243.251512	9170.820481	27.438260
243.654619	9184.485102	27.443277
243.635387	9192.428381	27.448295
243.692130	9206.775221	27.453312
244.257275	9219.066525	27.458330
244.391649	9241.641548	27.463348
244.682733	9251.026732	27.468365
244.595686	9257.430418	27.473383
244.924414	9262.575960	27.478400
245.324197	9270.911830	27.483418
245.468387	9292.475087	27.488436
245.896736	9287.978847	27.493453
246.215428	9310.203224	27.498471
246.075215	9324.501888	27.503488
246.289262	9324.474868	27.508506
246.168847	9346.467718	27.513524
247.199258	9361.903871	27.518541
247.178069	9370.122208	27.523559
247.452416	9379.607936	27.528576
247.953737	9381.114795	27.533594
248.301730	9393.534740	27.538612
248.925366	9404.216356	27.543629
249.435134	9405.744003	27.548647
249.501879	9415.069480	27.553664
249.723951	9417.191273	27.558682
249.672102	9410.758619	27.563700
249.869067	9429.497585	27.568717
249.914132	9449.014794	27.573735
249.781365	9445.417280	27.578752
249.665084	9456.570887	27.583770
249.888861	9483.959678	27.588788
250.598481	9501.801182	27.593805
250.828114	9530.104725	27.598823
251.132640	9544.299589	27.603840
251.624300	9559.582992	27.608858
251.579895	9573.358616	27.613876
251.963636	9583.847207	27.618893
251.958442	9596.669571	27.623911
252.067286	9618.099790	27.628928
252.441178	9639.728720	27.633946
252.877210	9654.139988	27.638964
252.936896	9670.737851	27.643981
253.168679	9697.743682	27.648999
253.226336	9714.120891	27.654016
253.634383	9731.217094	27.659034
253.721568	9751.883623	27.664052
254.818426	9761.626680	27.669069
255.059334	9773.810970	27.674087
255.149514	9783.139298	27.679104
255.746844	9798.327515	27.684122
255.324821	9814.040688	27.689140
255.770827	9825.208009	27.694157
256.105437	9843.237675	27.699175
256.270878	9870.680320	27.704192
256.765653	9880.832906	27.709210
256.823262	9896.023140	27.714228
257.110830	9908.200254	27.719245
257.242200	9925.889081	27.724263
257.406000	9955.974767	27.729280
258.090415	9958.368789	27.734298
258.348112	9976.574739	27.739316
258.385758	9978.406422	27.744333
258.688867	9996.529546	27.749351
258.790906	10014.030427	27.754368
259.227143	10028.915552	27.759386
259.225527	10043.568911	27.764404
259.809031	10066.747523	27.769421
260.211522	10079.361512	27.774439
260.051898	10089.230899	27.779456
260.713795	10095.805591	27.784474
261.025946	10118.537128	27.789492
261.011904	10124.658216	27.794509
261.659298	10135.633347	27.799527
261.627129	10153.609910	27.804544
261.889791	10156.331678	27.809562
261.962781	10175.649547	27.814580
262.320538	10189.997642	27.819597
262.463980	10194.250346	27.824615
262.722579	10219.011044	27.829632
263.114608	10228.166307	27.834650
262.919461	10243.159374	27.839668
263.005265	10245.624528	27.844685
263.356130	10268.195510	27.849703
263.556819	10288.503969	27.854720
264.156198	10300.718045	27.859738
263.903112	10320.301529	27.864756
264.533199	10340.227457	27.869773
265.033958	10358.787453	27.874791
265.026112	10388.682703	27.879808
265.265458	10399.952007	27.884826
265.828511	10429.827904	27.889844
266.699229	10429.285033	27.894861
267.715567	10415.092219	27.899879
267.405959	10410.524316	27.904896
268.307768	10406.241422	27.909914
268.757252	10414.794245	27.914932
268.562322	10413.293252	27.919949
269.063817	10422.482087	27.924967
268.994889	10426.439539	27.929984
269.036159	10430.016736	27.935002
269.419958	10434.683581	27.940020
269.268982	10432.806329	27.945037
269.663696	10449.671623	27.950055
269.565158	10466.193792	27.955072
270.007381	10476.007573	27.960090
269.787737	10490.543673	27.965108
270.034484	10504.786155	27.970125
270.430191	10526.305370	27.975143
270.316425	10550.167788	27.980160
270.778052	10557.560019	27.985178
270.739138	10590.308410	27.990196
271.241873	10607.302271	27.995213
271.643113	10632.101302	28.000231
271.681550	10653.969926	28.005248
272.201903	10659.275470	28.010266
272.597944	10681.419982	28.015284
272.857870	10711.476136	28.020301
273.589228	10723.256320	28.025319
273.647098	10743.287553	28.030336
273.653952	10746.781761	28.035354
273.736437	10774.513349	28.040372
274.339333	10788.747963	28.045389
274.498133	10807.247978	28.050407
274.710600	10828.211941	28.055424
274.973147	10839.332656	28.060442
275.376160	10865.524159	28.065460
275.570582	10890.261008	28.070477
275.675007	10907.718152	28.075495
275.872690	10921.438137	28.080512
276.553802	10948.549489	28.085530
276.587740	10966.364983	28.090548
276.647898	10988.457955	28.095565
276.860602	10999.962266	28.100583
277.439746	11021.055651	28.105600
277.704547	11039.662534	28.110618
278.107957	11066.997269	28.115636
278.318710	11084.974798	28.120653
279.130350	11104.462806	28.125671
279.110334	11114.825671	28.130688
279.535407	11129.874449	28.135706
279.895277	11130.645678	28.140724
279.883780	11154.148776	28.145741
280.297992	11154.965223	28.150759
280.319633	11176.186626	28.155776
280.702454	11173.651527	28.160794
281.159602	11191.552909	28.165812
281.275606	11211.970283	28.170829
281.351137	11226.006316	28.175847
281.789381	11239.338598	28.180864
281.965866	11253.090545	28.185882
282.435796	11277.750281	28.190900
282.542372	11292.198324	28.195917
283.175886	11300.902884	28.200935
283.203236	11326.758828	28.205952
283.268010	11329.779969	28.210970
283.757160	11354.319985	28.215988
284.071612	11366.749629	28.221005
284.470491	11375.778090	28.226023
284.600607	11398.583733	28.231040
284.647029	11414.121116	28.236058
284.810557	11435.813302	28.241076
285.459212	11458.557234	28.246093
286.051091	11473.283509	28.251111
285.892266	11504.842822	28.256128
286.045492	11508.184923	28.261146
286.804361	11529.257217	28.266164
286.850800	11556.108298	28.271181
287.199374	11564.731040	28.276199
286.938101	11587.998858	28.281216
287.405926	11600.414252	28.286234
287.904775	11631.691406	28.291252
287.907849	11652.379448	28.296269
288.565627	11677.446214	28.301287
288.917103	11692.257453	28.306304
290.069807	11684.897606	28.311322
290.461624	11684.745026	28.316340
290.523546	11707.599552	28.321357
291.091128	11712.304417	28.326375
291.024920	11713.160952	28.331392
291.336323	11729.573048	28.336410
291.819097	11742.721932	28.341428
291.806538	11755.076440	28.346445
292.314847	11763.819656	28.351463
292.114057	11775.271987	28.356480
292.398428	11792.026211	28.361498
292.376862	11811.265762	28.366516
293.072217	11829.705357	28.371533
293.442464	11837.172319	28.376551
293.555841	11857.508707	28.381568
293.480206	11867.586988	28.386586
293.864811	11884.439364	28.391604
294.080786	11915.770505	28.396621
294.439340	11927.148477	28.401639
294.871752	11950.495049	28.406656
295.252929	11974.209597	28.411674
295.485832	11987.527018	28.416692
295.389578	12001.596690	28.421709
295.817960	12014.170067	28.426727
296.055191	12036.170395	28.431744
296.383646	12059.593282	28.436762
296.892558	12079.142070	28.441780
296.706996	12102.297691	28.446797
297.427694	12108.399770	28.451815
297.673260	12134.068127	28.456832
297.982828	12152.675462	28.461850
298.367924	12174.772924	28.466868
298.808630	12189.895906	28.471885
299.035266	12200.344120	28.476903
299.293762	12229.484046	28.481920
299.675082	12246.081487	28.486938
300.005815	12255.544114	28.491956
300.317063	12270.583111	28.496973
300.270069	12289.517655	28.501991
300.441645	12311.196968	28.507008
301.097376	12326.747609	28.512026
301.569752	12335.054609	28.517044
301.462465	12355.773237	28.522061
301.942885	12362.335941	28.527079
302.257765	12384.245645	28.532096
302.502882	12404.833678	28.537114
302.887431	12418.411990	28.542132
303.127909	12435.006262	28.547149
303.680013	12451.476249	28.552167
304.146208	12474.515071	28.557184
304.198391	12476.186849	28.562202
304.475266	12487.849443	28.567220
304.757337	12507.958177	28.572237
305.244189	12508.523392	28.577255
305.197317	12539.628085	28.582272
305.653695	12553.406881	28.587290
306.162374	12568.121710	28.592308
306.232631	12584.594201	28.597325
306.655931	12594.964651	28.602343
306.873546	12613.413082	28.607360
307.042335	12640.464547	28.612378
307.236807	12650.400147	28.617396
307.585919	12674.505818	28.622413
308.113327	12694.156573	28.627431
308.631470	12706.864856	28.632448
308.872532	12726.588644	28.637466
309.444303	12730.090005	28.642484
309.553493	12763.744357	28.647501
310.191506	12774.763559	28.652519
310.268208	12787.341682	28.657536
310.311063	12801.680810	28.662554
310.907315	12825.798724	28.667572
310.674479	12842.864925	28.672589
310.994097	12854.473726	28.677607
311.419977	12887.535854	28.682624
311.333302	12914.542223	28.687642
311.428441	12933.701594	28.692660
311.751723	12958.108484	28.697677
312.485974	12980.032537	28.702695
313.215521	13008.159305	28.707712
313.175339	13027.377732	28.712730
313.677885	13035.775081	28.717748
314.188433	13058.782451	28.722765
314.520712	13066.701069	28.727783
315.106944	13085.840980	28.732800
315.044671	13103.645058	28.737818
315.759598	13118.217684	28.742836
315.963107	13143.278185	28.747853
315.978209	13150.829383	28.752871
316.730648	13172.589780	28.757888
316.720711	13185.478493	28.762906
317.331122	13194.380165	28.767924
317.271408	13223.334330	28.772941
317.544024	13244.623201	28.777959
318.137236	13246.823443	28.782976
318.171333	13266.267389	28.787994
318.717724	13290.185241	28.793012
318.760629	13323.266704	28.798029
318.876494	13329.883345	28.803047
319.572254	13351.564352	28.808064
319.563228	13383.397170	28.813082
319.734882	13398.960905	28.818100
319.925024	13422.293336	28.823117
320.607995	13433.166979	28.828135
321.079066	13449.533614	28.833152
321.079177	13482.574649	28.838170
321.433964	13488.532044	28.843188
321.736100	13504.956606	28.848205
322.511587	13533.329638	28.853223
322.611237	13543.908894	28.858240
322.789142	13561.963380	28.863258
323.340191	13575.308184	28.868276
323.288692	13589.968917	28.873293
323.963656	13620.091425	28.878311
324.135551	13635.825845	28.883328
324.299093	13650.282619	28.888346
324.567026	13675.179057	28.893364
324.617435	13692.400875	28.898381
325.079680	13714.023915	28.903399
325.865994	13740.895554	28.908416
326.174347	13758.601493	28.913434
326.380404	13776.234952	28.918452
326.290742	13794.861851	28.923469
326.611240	13812.041730	28.928487
327.090647	13842.810839	28.933504
327.358637	13870.170731	28.938522
327.752662	13890.803520	28.943540
328.153635	13916.810115	28.948557
328.505972	13937.114700	28.953575
329.168410	13974.986236	28.958592
329.177063	13997.580241	28.963610
329.869529	14006.229518	28.968628
329.875173	14027.349248	28.973645
330.140527	14057.848863	28.978663
330.852625	14075.839622	28.983680
330.877452	14105.906219	28.988698
331.262109	14123.240608	28.993716
331.470886	14144.865705	28.998733
331.807981	14164.623413	29.003751
332.309988	14184.901804	29.008768
332.706970	14205.209200	29.013786
333.474597	14224.132545	29.018804
333.711174	14238.546817	29.023821
333.964700	14273.659336	29.028839
334.380805	14285.058198	29.033856
334.246444	14300.373460	29.038874
335.046565	14321.331934	29.043892
335.173102	14341.094184	29.048909
335.594134	14364.909748	29.053927
336.440136	14379.115560	29.058944
336.347449	14389.652597	29.063962
337.247797	14397.297011	29.068980
337.541678	14415.937443	29.073997
337.926692	14434.083680	29.079015
337.942118	14440.135264	29.084032
338.226084	14457.412999	29.089050
338.484698	14477.439054	29.094068
338.916431	14495.710716	29.099085
338.759383	14522.566110	29.104103
339.233585	14538.330009	29.109120
339.464870	14567.411455	29.114138
339.706568	14593.225867	29.119156
340.217781	14609.265132	29.124173
340.346110	14629.946406	29.129191
340.658583	14652.307563	29.134208
340.713227	14680.551365	29.139226
341.453866	14700.846845	29.144244
342.113118	14723.131991	29.149261
342.359683	14744.142373	29.154279
342.498667	14760.432360	29.159296
342.951372	14785.595193	29.164314
343.155119	14800.820322	29.169332
343.778343	14823.019609	29.174349
343.627710	14835.324986	29.179367
344.286750	14856.763945	29.184384
344.211195	14878.206757	29.189402
344.690940	14894.901737	29.194420
345.164283	14928.686410	29.199437
344.870899	14947.295622	29.204455
345.312368	14966.681045	29.209472
345.723907	14993.685444	29.214490
345.908758	15020.374618	29.219508
346.515570	15051.008998	29.224525
347.256127	15084.575490	29.229543
347.475971	15102.302778	29.234560
347.664788	15125.346957	29.239578
348.159538	15147.377133	29.244596
349.140006	15166.612526	29.249613
348.732472	15198.115649	29.254631
349.170721	15212.824555	29.259648
349.251924	15246.623468	29.264666
349.776389	15270.897793	29.269684
350.192857	15297.058617	29.274701
350.348809	15317.534211	29.279719
351.080616	15351.288869	29.284736
351.256361	15375.860800	29.289754
351.681970	15398.947400	29.294772
352.085060	15424.892564	29.299789
352.196915	15448.564967	29.304807
352.750183	15475.844858	29.309824
352.850195	15515.708277	29.314842
353.625646	15523.858963	29.319860
354.143841	15552.562472	29.324877
355.065472	15572.410661	29.329895
355.292580	15582.266919	29.334912
355.737235	15601.324035	29.339930
356.180975	15612.365668	29.344948
356.611303	15631.816668	29.349965
356.609914	15645.381583	29.354983
357.097931	15659.514601	29.360000
356.974162	15678.881365	29.365018
357.575670	15709.059681	29.370036
357.750921	15723.070892	29.375053
357.908617	15754.846976	29.380071
358.283627	15783.449951	29.385088
358.484376	15804.279137	29.390106
358.844693	15825.869917	29.395124
359.318463	15855.660932	29.400141
359.549478	15882.552570	29.405159
360.144239	15905.900854	29.410176
360.168584	15930.307569	29.415194
360.502105	15970.808301	29.420212
360.597518	15984.121512	29.425229
360.792855	16021.776116	29.430247
361.580787	16051.281653	29.435264
361.749244	16087.023467	29.440282
362.072828	16110.790060	29.445300
362.790300	16133.693144	29.450317
362.979679	16166.137703	29.455335
363.518183	16190.035169	29.460352
364.186492	16220.699753	29.465370
364.694808	16232.603397	29.470388
365.056681	16265.239197	29.475405
365.001661	16279.214021	29.480423
365.733395	16295.886791	29.485440
366.429693	16325.192247	29.490458
366.599768	16335.010397	29.495476
367.058959	16353.102697	29.500493
367.316482	16380.957370	29.505511
367.453390	16394.371791	29.510528
368.267718	16411.183405	29.515546
368.811981	16433.444237	29.520564
369.267912	16445.431971	29.525581
369.555126	16451.599798	29.530599
369.888678	16460.167107	29.535616
370.177401	16484.732347	29.540634
370.060370	16503.884124	29.545652
370.433153	16510.010223	29.550669
370.439854	16540.370886	29.555687
370.884470	16552.726824	29.560704
371.233854	16583.170016	29.565722
371.999314	16597.320546	29.570740
372.528762	16614.113522	29.575757
372.748884	16643.338834	29.580775
373.004657	16659.293257	29.585792
373.440492	16681.299632	29.590810
373.511406	16705.507418	29.595828
374.171516	16725.018510	29.600845
374.471739	16745.656360	29.605863
375.317780	16762.273841	29.610880
375.456943	16788.107179	29.615898
375.889570	16809.046645	29.620916
376.250997	16829.769811	29.625933
376.358451	16854.351110	29.630951
376.785297	16877.006593	29.635968
377.656326	16889.924897	29.640986
377.562771	16924.218267	29.646004
377.763677	16933.425498	29.651021
377.928449	16968.004051	29.656039
378.329129	16981.538900	29.661056
378.781324	17020.962124	29.666074
378.692969	17045.495189	29.671092
378.804901	17077.612228	29.676109
379.195482	17118.845585	29.681127
379.904313	17162.587875	29.686144
380.627572	17197.825302	29.691162
381.106400	17224.465461	29.696180
381.271927	17242.980181	29.701197
381.563784	17280.372702	29.706215
382.200827	17309.240376	29.711232
382.657391	17333.947973	29.716250
383.012643	17362.550060	29.721268
383.633475	17382.949169	29.726285
383.657295	17408.412794	29.731303
384.082239	17437.048362	29.736320
384.700134	17469.750580	29.741338
385.143625	17501.342924	29.746356
385.610168	17526.879917	29.751373
385.752418	17551.052391	29.756391
386.293037	17584.986043	29.761408
386.865514	17610.885685	29.766426
387.095151	17640.603767	29.771444
387.618243	17653.061906	29.776461
388.383740	17670.700304	29.781479
388.594794	17688.974630	29.786496
388.935720	17699.351218	29.791514
389.204104	17735.102647	29.796532
389.734252	17746.738512	29.801549
389.905373	17778.064168	29.806567
390.472363	17803.611159	29.811584
390.514237	17835.373967	29.816602
390.944469	17858.175373	29.821620
391.066007	17879.237083	29.826637
391.871039	17911.847745	29.831655
392.090662	17939.975898	29.836672
392.362213	17973.042435	29.841690
392.222694	17993.671115	29.846708
392.702712	18023.559277	29.851725
393.251011	18057.378853	29.856743
393.849578	18086.395821	29.861760
394.140947	18112.598909	29.866778
394.270526	18145.852094	29.871796
394.655053	18181.055609	29.876813
394.927797	18202.106765	29.881831
395.508198	18224.847321	29.886848
395.955601	18254.450319	29.891866
396.230360	18296.746588	29.896884
396.658715	18311.121434	29.901901
397.128581	18349.559107	29.906919
397.301318	18377.240342	29.911936
398.089887	18407.068426	29.916954
398.109217	18442.803077	29.921972
398.583533	18469.136102	29.926989
399.242222	18505.586283	29.932007
399.414145	18533.830121	29.937024
400.056705	18565.064703	29.942042
400.511718	18606.670252	29.947060
401.284574	18624.687427	29.952077
401.673315	18648.923978	29.957095
401.742145	18680.109079	29.962112
402.630091	18704.400650	29.967130
403.028246	18726.519465	29.972148
403.766493	18740.100918	29.977165
404.045009	18762.484782	29.982183
405.015111	18771.980624	29.987200
405.449500	18779.039171	29.992218
406.078798	18808.355679	29.997236
406.294627	18821.190921	30.002253
406.630084	18831.006708	30.007271
407.112171	18848.052232	30.012288
406.880923	18869.852236	30.017306
407.171007	18890.528704	30.022324
407.784876	18913.662868	30.027341
408.329578	18932.063316	30.032359
408.200281	18956.854719	30.037376
408.939039	18979.091372	30.042394
409.101242	19001.518890	30.047412
409.959771	19015.321881	30.052429
410.260337	19050.382106	30.057447
410.278600	19078.619070	30.062464
410.764993	19095.424071	30.067482
411.075151	19126.509143	30.072500
411.558501	19149.834484	30.077517
411.896383	19173.024558	30.082535
412.168284	19195.169879	30.087552
412.469004	19231.215963	30.092570
412.990577	19262.059854	30.097588
413.619648	19287.169536	30.102605
414.020462	19318.367155	30.107623
414.702417	19338.382910	30.112640
414.982492	19365.821404	30.117658
415.184140	19394.188219	30.122676
415.926781	19411.926534	30.127693
416.332256	19441.095628	30.132711
416.333652	19470.940496	30.137728
416.779271	19506.781316	30.142746
416.809355	19534.082069	30.147764
417.353187	19571.411351	30.152781
417.966276	19603.024943	30.157799
418.020483	19632.842883	30.162816
418.769956	19659.002012	30.167834
419.129526	19688.747227	30.172852
419.676945	19718.273708	30.177869
420.225267	19753.277673	30.182887
420.505336	19784.817047	30.187904
421.084158	19803.592082	30.192922
421.235753	19832.908690	30.197940
422.045128	19851.098223	30.202957
422.502238	19882.193212	30.207975
422.510682	19899.654563	30.212992
422.978928	19924.973324	30.218010
422.930085	19959.337748	30.223028
423.529292	19994.334224	30.228045
423.557170	20018.982465	30.233063
424.052209	20045.339672	30.238080
424.904418	20077.915044	30.243098
425.106115	20121.414429	30.248116
425.792484	20153.674575	30.253133
426.005792	20178.452099	30.258151
426.387533	20215.934208	30.263168
426.669076	20234.263134	30.268186
427.327976	20276.276452	30.273204
427.647225	20303.160498	30.278221
428.135117	20336.551182	30.283239
428.659659	20379.539663	30.288256
429.224736	20403.580359	30.293274
429.797961	20431.676019	30.298292
431.076785	20438.755346	30.303309
432.470620	20452.096942	30.308327
432.822770	20468.033179	30.313344
433.642126	20464.860295	30.318362
433.694425	20475.586572	30.323380
433.875962	20493.021506	30.328397
434.366508	20510.212487	30.333415
434.130882	20526.354002	30.338432
434.624754	20535.823765	30.343450
435.126929	20562.104741	30.348468
435.285882	20582.727601	30.353485
435.430597	20604.193011	30.358503
435.815222	20632.735318	30.363520
436.082679	20662.982854	30.368538
436.479733	20692.161446	30.373556
436.639569	20714.660801	30.378573
436.934060	20743.754346	30.383591
437.031818	20790.373622	30.388608
437.787133	20820.425405	30.393626
438.419236	20858.059314	30.398644
438.601191	20900.160859	30.403661
438.957899	20929.282903	30.408679
439.330705	20972.694357	30.413696
439.649444	21016.708241	30.418714
440.066763	21047.141540	30.423732
440.589958	21090.965804	30.428749
441.218566	21129.396882	30.433767
441.822164	21175.439177	30.438784
442.155416	21200.502599	30.443802
442.736810	21250.687028	30.448820
443.126555	21289.370428	30.453837
443.739578	21309.076703	30.458855
444.223649	21351.694514	30.463872
444.606259	21378.519623	30.468890
445.095476	21410.420794	30.473908
445.580733	21443.605267	30.478925
446.075024	21480.358292	30.483943
446.418538	21517.476054	30.488960
447.122786	21542.197827	30.493978
447.878797	21578.651236	30.498996
448.109508	21606.163740	30.504013
449.024440	21626.196121	30.509031
449.437930	21657.047979	30.514048
449.958833	21668.662364	30.519066
450.314194	21684.883421	30.524084
450.432255	21719.623004	30.529101
451.278387	21735.887753	30.534119
451.679781	21763.734059	30.539136
452.322588	21768.701417	30.544154
452.140015	21797.377947	30.549172
452.245133	21812.374365	30.554189
452.525278	21838.931720	30.559207
453.480764	21879.442720	30.564224
454.221163	21902.826108	30.569242
454.477008	21928.717601	30.574260
454.146265	21957.449022	30.579277
454.996701	21985.705947	30.584295
455.303760	22019.285610	30.589312
455.923397	22050.908453	30.594330
456.651311	22083.001023	30.599348
456.662231	22115.868720	30.604365
457.210498	22139.421309	30.609383
457.630467	22178.133343	30.614400
457.915257	22208.058304	30.619418
458.691190	22245.887312	30.624436
458.837500	22277.912776	30.629453
459.417918	22319.443508	30.634471
459.630383	22355.414292	30.639488
460.066314	22392.633050	30.644506
460.547896	22424.676062	30.649524
461.075893	22471.011178	30.654541
461.769030	22499.855695	30.659559
462.242783	22545.851900	30.664576
462.231783	22577.144087	30.669594
463.432742	22615.274124	30.674612
463.516425	22655.587544	30.679629
464.239631	22690.727491	30.684647
464.291301	22726.079463	30.689664
464.744808	22757.735620	30.694682
465.159622	22793.081729	30.699700
465.344634	22842.194524	30.704717
466.113920	22885.668522	30.709735
466.640991	22924.245283	30.714752
467.176286	22964.375285	30.719770
467.633626	22995.664730	30.724788
467.834435	23042.968359	30.729805
468.743985	23081.454288	30.734823
469.220130	23119.919299	30.739840
469.769339	23156.230886	30.744858
470.560804	23192.662801	30.749876
470.950678	23228.209455	30.754893
471.598057	23262.515480	30.759911
472.167037	23300.435593	30.764928
472.447875	23328.884219	30.769946
472.888119	23354.325496	30.774964
473.408059	23395.634097	30.779981
474.168711	23426.662156	30.784999
474.305419	23461.420847	30.790016
475.084697	23488.414553	30.795034
475.420010	23521.689050	30.800052
475.858168	23554.960229	30.805069
476.189369	23585.107531	30.810087
476.820002	23624.446778	30.815104
476.818668	23653.761278	30.820122
477.998642	23690.557005	30.825140
478.193301	23722.975377	30.830157
478.724028	23756.023951	30.835175
479.150859	23786.896010	30.840192
479.523884	23821.681732	30.845210
480.118789	23847.011095	30.850228
480.882387	23886.557651	30.855245
481.006496	23911.385344	30.860263
481.029632	23940.184601	30.865280
481.841001	23985.114191	30.870298
482.782710	24009.555636	30.875316
483.174107	24038.038618	30.880333
483.789245	24050.777196	30.885351
484.819578	24080.759537	30.890368
484.797937	24092.409257	30.895386
485.699833	24103.731953	30.900404
485.904636	24130.019740	30.905421
486.750066	24158.508043	30.910439
487.247748	24166.203251	30.915456
487.303215	24193.980441	30.920474
487.506020	24219.769434	30.925492
487.841371	24253.443262	30.930509
488.295451	24276.355848	30.935527
488.528355	24306.228856	30.940544
489.333533	24330.180087	30.945562
490.072028	24359.797526	30.950580
490.437725	24383.355927	30.955597
491.000903	24414.997650	30.960615
491.420938	24449.233686	30.965632
491.451181	24487.606454	30.970650
492.097475	24509.655228	30.975668
492.196274	24553.622736	30.980685
492.981369	24583.486028	30.985703
493.317244	24625.988604	30.990720
493.872807	24667.306935	30.995738
494.949687	24694.729908	31.000756
495.052137	24735.897739	31.005773
495.533706	24764.936471	31.010791
496.265827	24800.066122	31.015808
496.369294	24842.200891	31.020826
496.830947	24870.794194	31.025844
497.806042	24923.113171	31.030861
498.074316	24955.983408	31.035879
498.666599	24979.816894	31.040896
498.918497	25019.514872	31.045914
499.722571	25055.189889	31.050932
500.028060	25097.635001	31.055949
500.485972	25136.940924	31.060967
500.775902	25169.150904	31.065984
501.470939	25210.562396	31.071002
502.331905	25239.403722	31.076020
502.843951	25282.524865	31.081037
502.873568	25317.012752	31.086055
503.509827	25366.067829	31.091072
503.958587	25398.626310	31.096090
504.563806	25432.841518	31.101108
504.879814	25473.977618	31.106125
505.559181	25518.261319	31.111143
506.241443	25552.685927	31.116160
506.761034	25589.954511	31.121178
507.124323	25628.467204	31.126196
507.789427	25666.364209	31.131213
508.312086	25705.218783	31.136231
508.628568	25732.350773	31.141248
509.217702	25774.121182	31.146266
509.580261	25804.247988	31.151284
510.143108	25847.811141	31.156301
510.235260	25887.737935	31.161319
511.072974	25933.590492	31.166336
511.369133	25984.020867	31.171354
512.122047	26023.333158	31.176372
512.575390	26059.412154	31.181389
513.162403	26087.020735	31.186407
513.861049	26136.523011	31.191424
513.933521	26166.954635	31.196442
514.847815	26210.546019	31.201460
515.682093	26245.099826	31.206477
516.116640	26274.855894	31.211495
516.787140	26307.381327	31.216512
517.246019	26336.267866	31.221530
518.243012	26358.719119	31.226548
518.230418	26386.345616	31.231565
518.727234	26403.439615	31.236583
519.397113	26436.584710	31.241600
520.162868	26469.139816	31.246618
520.341220	26487.332582	31.251636
520.408110	26528.933057	31.256653
520.860789	26559.950725	31.261671
521.516852	26592.453586	31.266688
521.767218	26629.709126	31.271706
522.470363	26669.207388	31.276724
522.723216	26716.277745	31.281741
523.014255	26757.268669	31.286759
523.691281	26783.435854	31.291776
524.103287	26826.379954	31.296794
524.960344	26861.961450	31.301812
525.481314	26906.222300	31.306829
525.942228	26949.512975	31.311847
526.285110	26993.985026	31.316864
526.549570	27038.425141	31.321882
527.435596	27082.743310	31.326900
527.827975	27127.024662	31.331917
528.561589	27165.210869	31.336935
529.278286	27205.731943	31.341952
529.407269	27249.599511	31.346970
530.662671	27292.438584	31.351988
531.091774	27329.724470	31.357005
531.101040	27369.995747	31.362023
532.384222	27400.158584	31.367040
532.231807	27448.317617	31.372058
532.895666	27488.025843	31.377076
533.888466	27535.962560	31.382093
533.928128	27589.167245	31.387111
535.000359	27619.919440	31.392128
535.224800	27664.910707	31.397146
535.459488	27708.484714	31.402164
536.429704	27742.463728	31.407181
536.861924	27787.473484	31.412199
537.455558	27826.213642	31.417216
537.970055	27869.346248	31.422234
538.877565	27899.524070	31.427252
539.356515	27941.531006	31.432269
539.184587	27974.910797	31.437287
540.031967	28017.125993	31.442304
540.323168	28070.924826	31.447322
540.841577	28107.964379	31.452340
541.734268	28156.234170	31.457357
542.459808	28195.889934	31.462375
543.141110	28238.295777	31.467392
543.657884	28282.478115	31.472410
544.211765	28323.393359	31.477428
544.584541	28358.945424	31.482445
545.213295	28402.725035	31.487463
545.542646	28438.966623	31.492480
546.046790	28485.489991	31.497498
546.713235	28525.914071	31.502516
547.240878	28558.882521	31.507533
547.628603	28611.700696	31.512551
548.261244	28654.159224	31.517568
549.077866	28697.316078	31.522586
549.501653	28743.606037	31.527604
549.935427	28778.068497	31.532621
550.496218	28835.423860	31.537639
551.273659	28858.367163	31.542656
551.443246	28905.512435	31.547674
552.090805	28944.309532	31.552692
552.963508	28975.006350	31.557709
553.594473	29020.424021	31.562727
554.349857	29057.712843	31.567744
554.567303	29085.667478	31.572762
555.120318	29119.378739	31.577780
555.350891	29151.730707	31.582797
555.701881	29200.890045	31.587815
556.310588	29226.110248	31.592832
556.914656	29282.474075	31.597850
557.221784	29319.694098	31.602868
558.227393	29363.707862	31.607885
558.449205	29408.874045	31.612903
558.812988	29445.750469	31.617920
559.104460	29491.354774	31.622938
559.719464	29527.794019	31.627956
560.551119	29576.569705	31.632973
561.427218	29631.849187	31.637991
561.987422	29667.943237	31.643008
562.463490	29722.267560	31.648026
563.222431	29764.304186	31.653044
563.785689	29805.018663	31.658061
564.463655	29853.825254	31.663079
565.053289	29888.524483	31.668096
565.703966	29935.970171	31.673114
565.850010	29971.497123	31.678132
566.412171	30023.210877	31.683149
566.911356	30066.906760	31.688167
567.491379	30106.911261	31.693184
568.423808	30160.634724	31.698202
568.980634	30198.809886	31.703220
569.489959	30249.894000	31.708237
570.190765	30297.218937	31.713255
570.694642	30338.626401	31.718272
570.984523	30387.020584	31.723290
571.805772	30427.127222	31.728308
572.515606	30470.993449	31.733325
573.060092	30524.228308	31.738343
574.156162	30554.266919	31.743360
574.516604	30596.816093	31.748378
574.821338	30637.812671	31.753396
575.634854	30675.196525	31.758413
576.256396	30713.033859	31.763431
577.046990	30752.545379	31.768448
577.389568	30794.819605	31.773466
578.144988	30844.235978	31.778484
578.413396	30877.292760	31.783501
578.781115	30925.884694	31.788519
579.182650	30968.586271	31.793536
580.021660	31008.185565	31.798554
580.407858	31065.700758	31.803572
581.326363	31104.099436	31.808589
581.605459	31151.163268	31.813607
582.475283	31190.252399	31.818624
582.895697	31231.655684	31.823642
583.634618	31278.528115	31.828660
585.037257	31315.100770	31.833677
585.173260	31347.591018	31.838695
586.106320	31385.652914	31.843712
587.123308	31423.512169	31.848730
587.319434	31458.597698	31.853748
588.159741	31486.243696	31.858765
588.448960	31522.086068	31.863783
589.051639	31543.283226	31.868800
589.440789	31578.427411	31.873818
590.177229	31610.590701	31.878836
591.398460	31632.545072	31.883853
591.760001	31665.462184	31.888871
592.141485	31691.296048	31.893888
592.471774	31727.334673	31.898906
592.708839	31768.666428	31.903924
593.336605	31793.526480	31.908941
593.784693	31823.794250	31.913959
594.085881	31866.374224	31.918976
594.727509	31904.254863	31.923994
595.169359	31945.289580	31.929012
596.043461	31986.667998	31.934029
595.914604	32032.431853	31.939047
596.731989	32077.055994	31.944064
597.271312	32112.247243	31.949082
597.373320	32166.010371	31.954100
597.931098	32217.464783	31.959117
598.115302	32274.060186	31.964135
599.461305	32320.783572	31.969152
599.947354	32391.145425	31.974170
600.250580	32438.031407	31.979188
601.032455	32494.970575	31.984205
601.340981	32560.846838	31.989223
602.081621	32607.646143	31.994240
602.314956	32663.324603	31.999258
602.865664	32727.450458	32.004276
604.234569	32779.892645	32.009293
604.398366	32841.942271	32.014311
605.205242	32899.940740	32.019328
605.910137	32958.656987	32.024346
606.635181	33024.678499	32.029364
607.370970	33068.571470	32.034381
607.505367	33136.683041	32.039399
607.572171	33197.832125	32.044416
608.697323	33263.589800	32.049434
609.205366	33318.746763	32.054452
610.056046	33374.514353	32.059469
610.400076	33443.384551	32.064487
611.142303	33507.451372	32.069504
612.488721	33571.114548	32.074522
612.881524	33628.642114	32.079540
613.700584	33673.711964	32.084557
614.471594	33718.618691	32.089575
615.240922	33767.325436	32.094592
616.619745	33810.405450	32.099610
616.931607	33864.949522	32.104628
617.441708	33910.889872	32.109645
618.183129	33955.827003	32.114663
618.113456	34001.554336	32.119680
619.118838	34055.257554	32.124698
619.956192	34113.109227	32.129716
620.929399	34147.129953	32.134733
621.319294	34191.856774	32.139751
621.670582	34233.820502	32.144768
622.604660	34280.289961	32.149786
622.999113	34336.061586	32.154804
623.860337	34367.008448	32.159821
624.645905	34408.614088	32.164839
625.269105	34445.395781	32.169856
626.147649	34493.613027	32.174874
626.476962	34536.231992	32.179892
627.193616	34578.670617	32.184909
628.090360	34613.450054	32.189927
628.950182	34641.242620	32.194944
629.818454	34683.664178	32.199962
630.368988	34711.852722	32.204980
631.000158	34750.315497	32.209997
631.471214	34779.218304	32.215015
631.910180	34810.332714	32.220032
632.669360	34847.100264	32.225050
632.781350	34883.089791	32.230068
633.674993	34918.976665	32.235085
633.696766	34969.003858	32.240103
634.093246	35009.621708	32.245120
634.583569	35050.610706	32.250138
634.803654	35100.929792	32.255156
635.574660	35146.661513	32.260173
635.827373	35197.772403	32.265191
636.345163	35249.670422	32.270208
637.014522	35297.782974	32.275226
637.550431	35343.899468	32.280244
638.225344	35411.365211	32.285261
638.561192	35470.765554	32.290279
639.642029	35531.820462	32.295296
640.763832	35580.862220	32.300314
641.290170	35631.988468	32.305332
641.963350	35683.863362	32.310349
642.943338	35729.639685	32.315367
643.869729	35764.675643	32.320384
644.875069	35809.733714	32.325402
645.211387	35863.501434	32.330420
645.973232	35897.406144	32.335437
646.569665	35947.763498	32.340455
647.187106	35991.491307	32.345472
647.734888	36038.796169	32.350490
647.971055	36091.081527	32.355508
649.035598	36148.163630	32.360525
649.298167	36190.967037	32.365543
649.467900	36244.451829	32.370560
650.230082	36298.091124	32.375578
650.849044	36358.316127	32.380596
651.823400	36408.160484	32.385613
652.453745	36465.146632	32.390631
653.637057	36519.353232	32.395648
654.424217	36562.315999	32.400666
655.372420	36600.808660	32.405684
655.715084	36652.003894	32.410701
656.280783	36710.063041	32.415719
656.958729	36768.598076	32.420736
657.845698	36805.842339	32.425754
658.201862	36849.562000	32.430772
658.770600	36899.628731	32.435789
659.046530	36948.552404	32.440807
659.693579	37004.993602	32.445824
660.753779	37065.961287	32.450842
661.052817	37121.647598	32.455860
661.691198	37181.283843	32.460877
662.203645	37236.507250	32.465895
662.979902	37294.914606	32.470912
663.558320	37354.819924	32.475930
664.292550	37420.727276	32.480948
665.736139	37456.172407	32.485965
667.237227	37491.166013	32.490983
667.771290	37530.641708	32.496000
668.842189	37567.517209	32.501018
669.021669	37609.697737	32.506036
669.730780	37653.610711	32.511053
669.960505	37696.536071	32.516071
670.592530	37744.280565	32.521088
671.114029	37786.812898	32.526106
671.634640	37839.918244	32.531124
672.564285	37877.309497	32.536141
673.486041	37921.695796	32.541159
674.032012	37975.568994	32.546176
675.047052	38021.711553	32.551194
675.506507	38059.884551	32.556212
676.210419	38103.091024	32.561229
676.784995	38154.677428	32.566247
677.445164	38190.365883	32.571264
677.848773	38236.648351	32.576282
678.341852	38294.451189	32.581300
678.377096	38341.151669	32.586317
679.069755	38392.087902	32.591335
679.445728	38446.033008	32.596352
680.233259	38497.909590	32.601370
680.878434	38556.960507	32.606388
681.558566	38608.733926	32.611405
682.098538	38670.362616	32.616423
682.451735	38727.834267	32.621440
682.899800	38790.970003	32.626458
683.336732	38857.927195	32.631476
683.692930	38935.356665	32.636493
684.648495	39006.609628	32.641511
685.080937	39085.558122	32.646528
686.333445	39156.651527	32.651546
686.903914	39230.886786	32.656564
688.021902	39307.003793	32.661581
688.820189	39360.392181	32.666599
689.379306	39434.395922	32.671616
690.150214	39490.647302	32.676634
691.057249	39559.930256	32.681652
691.948535	39618.680159	32.686669
693.033499	39673.175655	32.691687
693.721836	39734.796933	32.696704
694.774302	39791.245576	32.701722
694.875728	39842.871728	32.706740
695.414022	39900.216495	32.711757
696.481062	39956.707569	32.716775
697.076398	40021.386013	32.721792
697.912402	40081.790040	32.726810
698.711197	40146.260109	32.731828
699.230118	40201.831612	32.736845
700.092019	40259.797312	32.741863
700.444682	40327.417229	32.746880
701.622869	40378.971898	32.751898
702.643967	40429.387491	32.756916
703.285306	40497.987521	32.761933
704.271290	40552.152803	32.766951
704.774290	40602.700044	32.771968
705.663158	40653.332793	32.776986
706.303253	40701.487323	32.782004
707.076318	40749.918502	32.787021
708.179686	40791.164556	32.792039
708.617850	40848.489467	32.797056
709.491329	40889.177007	32.802074
710.441329	40943.513299	32.807092
710.785500	40992.764381	32.812109
711.402740	41032.391639	32.817127
711.576163	41101.363653	32.822144
712.134388	41149.835490	32.827162
713.207665	41209.706085	32.832180
714.389161	41263.596049	32.837197
715.151510	41315.293565	32.842215
715.454816	41370.566418	32.847232
716.161493	41424.423179	32.852250
716.609560	41478.927482	32.857268
717.730430	41531.834600	32.862285
718.433823	41586.482835	32.867303
718.636942	41639.842982	32.872320
719.367810	41710.557935	32.877338
719.897993	41764.961623	32.882356
720.617858	41827.444058	32.887373
721.379508	41896.036075	32.892391
722.033516	41966.675274	32.897408
722.457431	42030.469286	32.902426
723.028564	42090.091577	32.907444
723.797588	42161.548356	32.912461
724.444697	42229.912584	32.917479
725.109876	42304.617925	32.922496
725.682076	42365.556343	32.927514
726.487191	42428.141063	32.932532
727.084249	42491.289631	32.937549
728.165384	42549.777537	32.942567
728.431970	42612.029174	32.947584
729.190056	42682.021987	32.952602
730.184671	42747.949262	32.957620
730.416730	42819.188172	32.962637
731.466270	42894.993138	32.967655
732.283188	42963.630482	32.972672
732.956957	43029.368197	32.977690
733.663942	43093.899193	32.982708
734.421143	43161.844378	32.987725
736.132359	43208.060356	32.992743
737.337107	43273.880593	32.997760
737.973451	43332.117241	33.002778
738.525093	43378.684862	33.007796
739.497789	43449.930688	33.012813
739.659483	43498.867914	33.017831
740.847485	43562.610667	33.022848
741.691662	43606.849869	33.027866
742.545004	43658.943540	33.032884
743.250403	43715.563866	33.037901
744.097070	43766.431751	33.042919
744.922135	43819.314521	33.047936
745.426256	43882.007147	33.052954
745.755733	43934.391746	33.057972
746.445562	43996.859706	33.062989
747.205899	44060.784322	33.068007
748.070874	44132.143991	33.073024
748.816184	44185.368964	33.078042
749.680112	44249.828298	33.083060
750.492706	44313.543098	33.088077
751.430630	44375.068982	33.093095
751.786485	44441.663695	33.098112
752.276986	44496.447163	33.103130
753.092052	44554.811010	33.108148
754.058531	44620.621739	33.113165
754.950770	44687.298151	33.118183
755.584249	44756.108763	33.123200
756.446431	44812.106562	33.128218
757.453367	44875.571328	33.133236
758.092693	44941.288446	33.138253
758.827588	44999.545755	33.143271
759.294244	45059.571841	33.148288
759.841244	45131.857137	33.153306
761.006994	45193.583863	33.158324
762.113865	45238.329422	33.163341
763.261069	45306.277390	33.168359
764.427199	45362.994656	33.173376
764.836203	45408.747428	33.178394
765.386376	45461.417545	33.183412
766.120995	45523.288204	33.188429
766.908119	45568.564949	33.193447
767.988035	45629.521860	33.198464
768.486150	45685.901136	33.203482
769.892695	45728.361730	33.208500
770.700427	45777.943504	33.213517
771.522626	45822.633337	33.218535
772.311587	45872.863469	33.223552
772.673700	45927.885510	33.228570
773.613952	45976.397016	33.233588
773.837487	46027.898435	33.238605
774.906564	46083.146073	33.243623
775.557659	46140.040372	33.248640
775.660020	46198.272751	33.253658
776.315266	46255.881517	33.258676
776.753730	46328.174918	33.263693
777.772023	46393.179414	33.268711
778.022411	46455.792244	33.273728
778.726978	46519.498521	33.278746
779.859044	46565.995099	33.283764
780.502401	46639.687270	33.288781
781.093476	46699.919789	33.293799
781.436193	46769.306904	33.298816
782.335359	46844.282059	33.303834
783.168272	46904.559717	33.308852
783.851169	46979.455118	33.313869
785.467541	47044.570829	33.318887
786.172239	47114.940137	33.323904
787.065703	47173.039233	33.328922
787.796080	47246.144163	33.333940
788.585958	47307.125471	33.338957
789.350763	47374.481306	33.343975
790.217636	47437.291897	33.348992
790.561256	47509.629152	33.354010
791.837451	47569.320832	33.359028
792.548868	47645.188239	33.364045
793.128067	47715.515689	33.369063
794.014758	47777.356220	33.374080
794.812423	47850.288143	33.379098
795.764299	47915.693270	33.384116
796.210010	48000.630899	33.389133
796.610331	48070.759547	33.394151
797.538063	48150.991801	33.399168
797.947067	48235.094610	33.404186
799.000385	48307.975554	33.409204
800.103330	48394.501505	33.414221
801.272928	48471.356869	33.419239
801.986660	48551.680789	33.424256
802.625859	48626.120272	33.429274
803.662931	48696.347849	33.434292
804.326268	48775.320195	33.439309
805.526431	48846.902041	33.444327
806.221534	48921.593176	33.449344
806.971995	48996.750436	33.454362
807.848712	49064.935304	33.459380
809.039457	49143.377632	33.464397
809.647213	49208.637590	33.469415
810.750723	49269.265336	33.474432
811.277163	49347.356252	33.479450
812.141222	49419.865303	33.484468
813.409452	49483.333992	33.489485
814.203089	49547.749830	33.494503
815.118194	49600.613192	33.499520
816.746088	49642.793625	33.504538
817.920762	49695.110656	33.509556
818.676464	49760.741422	33.514573
819.513306	49805.759509	33.519591
820.355027	49863.348407	33.524608
820.626623	49918.014601	33.529626
821.630689	49961.298706	33.534644
822.460998	50033.574532	33.539661
823.115558	50085.593805	33.544679
823.849664	50137.790620	33.549696
823.872089	50200.987034	33.554714
825.121199	50257.779578	33.559732
825.983196	50329.817306	33.564749
826.298059	50395.417278	33.569767
827.108765	50459.288896	33.574784
827.643279	50529.486445	33.579802
828.522021	50599.826762	33.584820
829.054168	50666.608480	33.589837
829.963953	50750.864023	33.594855
830.791622	50820.770067	33.599872
831.559115	50889.540477	33.604890
832.606088	50955.312799	33.609908
833.496082	51029.815953	33.614925
834.180341	51097.214284	33.619943
834.799239	51154.954991	33.624960
835.427143	51224.311249	33.629978
836.213450	51294.130257	33.634996
837.185485	51360.858161	33.640013
837.820939	51436.167848	33.645031
838.484544	51510.132007	33.650048
839.081245	51598.128202	33.655066
839.695783	51673.638064	33.660084
840.951413	51755.812350	33.665101
841.875981	51836.380682	33.670119
843.144679	51913.054976	33.675136
843.334073	52003.824251	33.680154
844.657046	52083.597439	33.685172
845.333439	52167.242739	33.690189
846.167041	52245.169100	33.695207
847.143647	52325.186860	33.700224
847.882500	52409.297872	33.705242
848.754987	52491.914059	33.710260
849.822316	52569.121743	33.715277
850.404309	52653.549124	33.720295
851.089413	52735.271508	33.725312
852.245121	52832.822370	33.730330
853.454871	52914.615578	33.735348
853.927992	52991.398285	33.740365
854.809686	53075.837490	33.745383
855.706452	53152.896479	33.750400
856.764096	53235.815521	33.755418
857.229928	53325.047217	33.760436
858.518153	53411.398627	33.765453
859.462337	53495.848604	33.770471
860.781777	53565.743304	33.775488
861.484366	53648.212845	33.780506
862.362586	53718.632292	33.785524
863.520708	53799.044488	33.790541
864.408003	53860.781020	33.795559
865.430363	53935.361459	33.800576
866.354463	54016.253786	33.805594
866.958605	54092.988066	33.810612
868.195687	54164.106021	33.815629
868.446721	54248.881759	33.820647
869.642978	54317.937259	33.825664
870.943216	54392.026598	33.830682
872.160110	54456.769861	33.835700
872.892701	54521.405174	33.840717
873.406357	54590.219683	33.845735
874.713697	54652.734552	33.850752
875.685658	54721.300914	33.855770
876.192949	54791.268730	33.860788
877.132840	54862.156615	33.865805
877.356761	54929.903448	33.870823
878.470079	55005.637514	33.875840
879.296215	55083.770649	33.880858
879.983483	55159.666454	33.885876
880.811463	55243.140915	33.890893
881.571921	55321.677415	33.895911
882.542100	55402.042069	33.900928
883.129298	55483.143749	33.905946
884.053576	55564.288162	33.910964
884.985489	55643.052173	33.915981
885.589324	55727.398583	33.920999
886.783892	55817.659063	33.926016
887.849368	55899.440804	33.931034
888.179531	55982.761205	33.936052
889.390008	56065.717037	33.941069
890.366535	56143.342953	33.946087
891.178023	56211.799379	33.951104
892.167631	56298.498955	33.956122
892.929024	56366.242162	33.961140
893.851925	56431.770711	33.966157
894.224256	56513.662459	33.971175
895.569338	56590.738827	33.976192
896.318664	56663.319871	33.981210
897.257394	56738.023418	33.986228
898.730995	56808.909983	33.991245
899.675867	56895.403514	33.996263
900.368181	56951.912926	34.001280
901.954712	57018.592883	34.006298
902.686769	57090.545034	34.011316
903.836389	57161.407131	34.016333
904.283731	57220.872904	34.021351
905.393968	57286.773356	34.026368
906.341108	57359.781400	34.031386
907.174644	57431.952949	34.036404
908.200314	57496.519085	34.041421
908.842993	57568.613163	34.046439
909.976928	57640.428460	34.051456
910.885039	57722.823206	34.056474
911.558459	57786.710793	34.061492
912.604862	57856.242935	34.066509
913.377743	57947.134056	34.071527
914.453575	58014.092483	34.076544
915.043427	58090.095047	34.081562
915.725026	58172.444315	34.086580
916.812111	58246.559850	34.091597
917.845111	58331.361292	34.096615
918.948423	58413.848272	34.101632
919.552908	58485.526987	34.106650
920.599144	58572.662685	34.111668
921.439632	58656.830672	34.116685
921.686569	58745.667391	34.121703
923.039959	58831.863788	34.126720
924.114318	58922.926850	34.131738
924.708183	59011.583956	34.136756
925.775750	59102.933572	34.141773
926.249856	59183.286862	34.146791
927.483176	59292.352605	34.151808
928.377192	59384.211329	34.156826
929.379701	59463.976943	34.161844
930.669256	59558.116647	34.166861
931.227926	59647.623373	34.171879
932.687531	59735.009051	34.176896
933.486020	59824.681641	34.181914
933.985399	59910.369195	34.186932
935.148711	60003.201068	34.191949
935.862697	60102.970855	34.196967
937.008613	60187.235854	34.201984
937.975008	60278.757548	34.207002
938.722325	60375.890128	34.212020
939.610873	60452.594169	34.217037
940.597753	60550.424397	34.222055
941.774439	60639.787924	34.227072
942.508388	60730.182818	34.232090
943.468443	60831.866844	34.237108
944.910624	60907.897464	34.242125
945.618396	60998.265773	34.247143
946.951975	61074.174557	34.252160
948.324389	61165.218595	34.257178
949.065245	61244.859852	34.262196
950.087003	61331.028098	34.267213
950.952008	61409.821346	34.272231
951.920447	61490.529383	34.277248
953.062919	61577.154449	34.282266
953.878179	61651.075796	34.287284
954.934606	61728.960398	34.292301
955.579799	61803.231506	34.297319
956.220249	61867.660333	34.302336
957.448576	61939.859773	34.307354
957.971052	62018.581685	34.312372
959.187032	62096.594536	34.317389
959.696584	62180.123535	34.322407
960.600456	62247.430543	34.327424
961.539770	62338.375424	34.332442
961.898007	62430.271998	34.337460
962.890722	62523.975547	34.342477
963.975230	62617.975345	34.347495
964.997131	62716.910199	34.352512
966.030998	62803.955284	34.357530
966.984364	62898.641242	34.362548
967.982370	62985.255753	34.367565
968.607189	63085.760510	34.372583
969.290429	63190.149772	34.377600
970.184004	63285.017430	34.382618
971.473304	63393.985059	34.387636
972.819831	63489.048868	34.392653
973.865124	63594.143124	34.397671
974.593333	63698.426229	34.402688
975.854084	63797.530781	34.407706
976.620902	63901.947999	34.412724
977.646689	63996.259685	34.417741
978.785409	64107.463252	34.422759
980.335850	64195.660936	34.427776
981.297337	64285.425654	34.432794
981.900457	64379.583006	34.437812
983.087155	64498.428325	34.442829
983.729972	64586.673707	34.447847
984.987558	64682.350993	34.452864
985.900968	64766.921025	34.457882
986.535142	64885.790877	34.462900
987.733329	64979.142466	34.467917
989.003890	65083.296268	34.472935
989.977877	65175.221052	34.477952
991.315353	65273.616772	34.482970
991.759889	65377.368572	34.487988
993.618332	65470.220360	34.493005
994.665227	65550.866040	34.498023
996.254496	65625.691657	34.503040
997.745282	65707.161415	34.508058
998.758991	65791.060848	34.513076
1000.052487	65864.534052	34.518093
1001.007577	65938.079139	34.523111
1001.409785	66024.271421	34.528128
1002.933389	66084.015257	34.533146
1004.125267	66157.106269	34.538164
1005.288005	66223.180771	34.543181
1006.550902	66295.203824	34.548199
1007.281441	66365.872766	34.553216
1008.537586	66432.522077	34.558234
1009.304208	66496.784913	34.563252
1010.290523	66573.720525	34.568269
1011.378203	66649.469308	34.573287
1011.933265	66721.774699	34.578304
1012.147935	66801.078719	34.583322
1013.324349	66874.275507	34.588340
1014.573991	66952.291921	34.593357
1015.240625	67046.841874	34.598375
1016.020392	67137.297154	34.603392
1017.127573	67216.653482	34.608410
1017.563237	67304.763316	34.613428
1019.015710	67388.852993	34.618445
1019.531271	67489.069423	34.623463
1020.640156	67566.349851	34.628480
1021.954939	67654.703938	34.633498
1022.735424	67730.459433	34.638516
1023.837045	67808.982707	34.643533
1024.724274	67900.747258	34.648551
1025.756527	67974.925714	34.653568
1026.856557	68068.272298	34.658586
1027.202335	68158.716434	34.663604
1028.067654	68253.936404	34.668621
1029.038066	68347.836041	34.673639
1030.113529	68446.949662	34.678656
1031.175231	68537.498971	34.683674
1031.940516	68635.566210	34.688692
1032.976087	68738.859794	34.693709
1034.430037	68829.260429	34.698727
1035.290669	68932.202110	34.703744
1036.584529	69030.809097	34.708762
1037.505415	69137.895918	34.713780
1038.243410	69226.991050	34.718797
1039.613260	69333.533904	34.723815
1040.451713	69451.658746	34.728832
1041.442773	69550.808744	34.733850
1042.332363	69649.196080	34.738868
1043.243214	69753.633901	34.743885
1044.518008	69875.010738	34.748903
1045.630729	69990.904452	34.753920
1046.781632	70085.890431	34.758938
1047.872919	70194.823069	34.763956
1049.181553	70304.456864	34.768973
1049.969674	70409.011407	34.773991
1050.754224	70515.555241	34.779008
1052.524978	70616.038020	34.784026
1054.068874	70724.129889	34.789044
1054.784873	70823.827810	34.794061
1056.428825	70913.224637	34.799079
1058.037773	71002.171292	34.804096
1059.056513	71074.948635	34.809114
1060.220320	71176.528562	34.814132
1061.111522	71266.715003	34.819149
1062.289779	71349.308830	34.824167
1063.477837	71449.708213	34.829184
1064.673149	71534.326350	34.834202
1065.381009	71631.470301	34.839220
1066.660555	71723.016341	34.844237
1067.456559	71806.798296	34.849255
1067.931377	71917.860486	34.854272
1069.330201	71999.130185	34.859290
1070.096893	72114.479255	34.864308
1071.175479	72211.263677	34.869325
1072.360900	72304.586864	34.874343
1073.711363	72406.991074	34.879360
1074.503198	72504.758444	34.884378
1075.544306	72604.336530	34.889396
1076.317981	72701.043556	34.894413
1077.560029	72799.818506	34.899431
1078.601031	72909.099557	34.904448
1079.622226	73003.413362	34.909466
1080.686914	73114.350771	34.914484
1081.422844	73230.279455	34.919501
1082.343838	73329.866302	34.924519
1083.464962	73438.871084	34.929536
1084.611801	73543.743230	34.934554
1085.774761	73658.087405	34.939572
1086.579095	73763.634364	34.944589
1087.809957	73875.461037	34.949607
1089.160453	73992.639985	34.954624
1090.308412	74100.934001	34.959642
1091.559385	74197.952169	34.964660
1092.731154	74308.092586	34.969677
1094.058132	74391.128754	34.974695
1094.363227	74490.131828	34.979712
1095.765678	74577.868707	34.984730
1097.582211	74652.127685	34.989748
1098.925066	74736.150436	34.994765
1099.803138	74822.019106	34.999783
1100.822738	74918.467913	35.004800
1102.240180	74996.095934	35.009818
1103.144721	75089.675287	35.014836
1103.954592	75172.693040	35.019853
1105.220552	75254.538054	35.024871
1105.972832	75357.312730	35.029888
1107.671128	75438.229670	35.034906
1108.758744	75539.749502	35.039924
1109.734356	75624.528875	35.044941
1111.015237	75722.611926	35.049959
1111.574575	75809.331379	35.054976
1113.061082	75900.327575	35.059994
1114.114701	76004.983201	35.065012
1115.135388	76103.285475	35.070029
1116.465363	76190.532220	35.075047
1117.325454	76279.853802	35.080064
1118.079216	76377.615931	35.085082
1119.564605	76474.390490	35.090100
1120.785576	76577.628883	35.095117
1122.306746	76679.845554	35.100135
1122.779210	76780.870434	35.105152
1123.997492	76881.361572	35.110170
1125.015512	76994.995126	35.115188
1125.882100	77096.770553	35.120205
1127.416330	77199.607858	35.125223
1128.372568	77306.133133	35.130240
1129.184752	77413.555319	35.135258
1130.235631	77528.174064	35.140276
1131.166258	77651.983505	35.145293
1132.520262	77767.936865	35.150311
1133.256713	77880.667846	35.155328
1134.145493	77979.846186	35.160346
1135.596328	78105.565578	35.165364
1136.521557	78234.205011	35.170381
1138.161397	78341.426003	35.175399
1139.416408	78468.849736	35.180416
1140.504223	78579.375304	35.185434
1141.968233	78692.173726	35.190452
1143.041590	78805.844192	35.195469
1144.569257	78913.920990	35.200487
1145.806511	79029.644486	35.205504
1146.708873	79125.860431	35.210522
1147.923352	79238.142516	35.215540
1149.109866	79358.207931	35.220557
1150.644711	79463.207294	35.225575
1151.922044	79579.699645	35.230592
1153.326813	79667.959343	35.235610
1154.340981	79766.402482	35.240628
1155.626796	79865.551149	35.245645
1156.942842	79959.729264	35.250663
1157.623314	80066.358829	35.255680
1158.965335	80168.819090	35.260698
1160.488022	80272.493171	35.265716
1161.547328	80365.027644	35.270733
1162.555227	80471.367084	35.275751
1163.921356	80573.419672	35.280768
1165.535911	80653.845652	35.285786
1167.096461	80741.248349	35.290804
1167.473594	80835.778284	35.295821
1168.979867	80929.841390	35.300839
1170.206579	81021.389118	35.305856
1170.932131	81106.338379	35.310874
1172.166307	81196.314512	35.315892
1172.939561	81284.360901	35.320909
1174.051809	81366.197416	35.325927
1175.401879	81457.955423	35.330944
1176.097251	81547.826508	35.335962
1177.127180	81640.369779	35.340980
1177.860151	81743.222020	35.345997
1179.098080	81839.547147	35.351015
1180.267727	81945.144836	35.356032
1181.311518	82046.999575	35.361050
1182.406805	82152.964373	35.366068
1183.295253	82274.355718	35.371085
1184.453618	82378.056297	35.376103
1185.914905	82488.387207	35.381120
1187.358828	82596.478648	35.386138
1188.887801	82691.050924	35.391156
1190.028351	82808.515600	35.396173
1191.384139	82900.252076	35.401191
1192.870328	83007.337563	35.406208
1194.027783	83110.825578	35.411226
1194.752719	83210.529508	35.416244
1196.136922	83328.085115	35.421261
1197.480697	83434.472169	35.426279
1198.650136	83538.568058	35.431296
1199.592495	83650.365347	35.436314
1201.089374	83758.567010	35.441332
1201.881375	83872.593257	35.446349
1203.176869	83981.853435	35.451367
1204.512192	84087.179905	35.456384
1205.616849	84201.348860	35.461402
1206.990639	84315.375012	35.466420
1207.896812	84432.097277	35.471437
1209.325517	84546.014434	35.476455
1210.261247	84667.738077	35.481472
1211.631579	84780.144731	35.486490
1213.058999	84891.529252	35.491508
1214.174710	85018.104735	35.496525
1215.480716	85123.718343	35.501543
1216.895756	85237.982494	35.506560
1217.911418	85354.349339	35.511578
1219.476200	85468.134929	35.516596
1220.505320	85593.319897	35.521613
1222.099415	85698.852757	35.526631
1223.220947	85819.487946	35.531648
1224.444561	85932.137347	35.536666
1225.038798	86044.834463	35.541684
1226.256923	86161.173043	35.546701
1227.637310	86280.806816	35.551719
1229.121075	86409.662697	35.556736
1230.262669	86526.394804	35.561754
1231.565143	86630.696598	35.566772
1232.624737	86754.006400	35.571789
1233.554310	86877.957888	35.576807
1235.140593	87000.198339	35.581824
1236.339419	87118.267143	35.586842
1237.985271	87230.691116	35.591860
1238.877176	87359.047730	35.596877
1240.535229	87471.204614	35.601895
1241.547136	87591.902228	35.606912
1242.978319	87706.541073	35.611930
1244.466508	87814.315746	35.616948
1245.042057	87932.256744	35.621965
1246.717721	88045.439550	35.626983
1248.165147	88161.230836	35.632000
1249.134163	88272.281472	35.637018
1250.499599	88390.316792	35.642036
1251.757347	88503.895898	35.647053
1253.040360	88613.428917	35.652071
1254.549585	88711.990551	35.657088
1255.896260	88804.380823	35.662106
1257.245040	88895.592484	35.667124
1258.401397	88992.182326	35.672141
1259.168541	89088.009325	35.677159
1260.223746	89184.704250	35.682176
1261.425125	89289.386067	35.687194
1262.731196	89393.380288	35.692212
1263.937408	89505.209708	35.697229
1265.336641	89613.955280	35.702247
1266.356771	89728.374476	35.707264
1267.596575	89850.515935	35.712282
1269.396513	89953.928316	35.717300
1270.555537	90059.531913	35.722317
1271.555983	90164.324125	35.727335
1272.987857	90280.620376	35.732352
1273.879985	90408.014333	35.737370
1275.150681	90514.083746	35.742388
1276.374113	90637.244852	35.747405
1277.364882	90751.127571	35.752423
1278.893139	90875.268770	35.757440
1279.925229	91003.784102	35.762458
1281.443250	91133.377660	35.767476
1282.735087	91252.779206	35.772493
1284.156878	91382.097317	35.777511
1285.706086	91496.719740	35.782528
1286.707659	91625.242473	35.787546
1288.762682	91724.907786	35.792564
1290.306930	91855.552312	35.797581
1291.650326	91962.325264	35.802599
1292.976307	92072.105081	35.807616
1293.960415	92196.044910	35.812634
1295.436827	92305.802160	35.817652
1296.777228	92421.651971	35.822669
1297.364733	92542.701832	35.827687
1299.249691	92651.788372	35.832704
1300.467221	92774.591555	35.837722
1302.146865	92891.125471	35.842740
1303.075594	93016.610879	35.847757
1304.348375	93134.831398	35.852775
1305.696082	93255.993907	35.857792
1306.831922	93376.999754	35.862810
1307.931487	93501.281812	35.867828
1309.107651	93633.765731	35.872845
1310.181751	93761.665132	35.877863
1311.718547	93886.907362	35.882880
1312.530425	94026.699732	35.887898
1314.020876	94161.608629	35.892916
1315.570330	94296.889187	35.897933
1317.164701	94421.554254	35.902951
1318.102681	94557.526863	35.907968
1319.053997	94692.230468	35.912986
1320.497244	94829.545256	35.918004
1322.057986	94975.499639	35.923021
1323.486472	95100.205939	35.928039
1325.268721	95220.687450	35.933056
1326.528996	95367.235489	35.938074
1327.919828	95488.552171	35.943092
1329.266951	95624.136209	35.948109
1330.774001	95742.038721	35.953127
1332.266933	95870.984436	35.958144
1333.637416	96002.522927	35.963162
1334.808642	96118.527062	35.968180
1336.001484	96237.798641	35.973197
1337.334316	96368.507924	35.978215
1338.884129	96485.379837	35.983232
1340.420584	96612.635932	35.988250
1341.799484	96730.904374	35.993268
1342.668594	96848.618803	35.998285
1343.502426	96959.417974	36.003303
1345.008847	97068.477616	36.008320
1346.104289	97191.989160	36.013338
1347.650347	97310.918283	36.018356
1348.981844	97429.830546	36.023373
1350.051326	97554.944772	36.028391
1351.163907	97673.080734	36.033408
1352.594901	97807.418858	36.038426
1353.777952	97947.361155	36.043444
1354.721090	98072.104116	36.048461
1356.147878	98203.288095	36.053479
1357.620636	98349.740911	36.058496
1358.687704	98496.143455	36.063514
1360.186628	98633.783142	36.068532
1361.293818	98780.472314	36.073549
1362.646574	98922.065833	36.078567
1364.184448	99058.496978	36.083584
1365.548967	99212.335943	36.088602
1366.636796	99358.206769	36.093620
1368.233507	99507.041575	36.098637
1369.533677	99660.918062	36.103655
1371.235537	99803.995087	36.108672
1372.706219	99954.410889	36.113690
1373.839152	100108.315544	36.118708
1375.472715	100258.048185	36.123725
1376.626342	100416.667111	36.128743
1378.444783	100556.610654	36.133760
1379.941108	100703.641036	36.138778
1381.678391	100838.920378	36.143796
1383.803646	100980.567522	36.148813
1385.227159	101115.300999	36.153831
1386.734774	101245.026865	36.158848
1388.282785	101388.705348	36.163866
1389.367433	101521.401393	36.168884
1390.984689	101642.021669	36.173901
1392.575397	101779.597102	36.178919
1394.248412	101906.295152	36.183936
1395.857224	102037.428367	36.188954
1397.337666	102158.376121	36.193972
1398.650962	102284.687886	36.198989
1399.872201	102409.987523	36.204007
1401.143195	102534.823471	36.209024
1402.781123	102666.829477	36.214042
1403.832092	102794.718120	36.219060
1405.341569	102923.600889	36.224077
1406.482319	103058.399049	36.229095
1407.558782	103191.749724	36.234112
1409.016069	103332.496719	36.239130
1410.361966	103464.817621	36.244148
1411.843153	103610.773033	36.249165
1413.699480	103739.351418	36.254183
1415.633645	103864.723110	36.259200
1416.429237	103997.550191	36.264218
1417.697724	104134.944702	36.269236
1419.687145	104264.429967	36.274253
1420.816669	104390.423361	36.279271
1422.076051	104521.113650	36.284288
1423.699228	104656.286971	36.289306
1424.764678	104791.623720	36.294324
1426.458341	104916.783215	36.299341
1427.779902	105059.270330	36.304359
1429.281604	105192.892485	36.309376
1429.979224	105338.330756	36.314394
1431.533385	105469.993214	36.319412
1432.840273	105616.922791	36.324429
1434.090125	105761.237210	36.329447
1435.667948	105896.460614	36.334464
1436.404165	106038.396310	36.339482
1437.910856	106171.653853	36.344500
1439.292022	106310.079453	36.349517
1440.775160	106434.072764	36.354535
1443.254193	106553.815919	36.359552
1445.013278	106686.275405	36.364570
1446.358737	106807.933043	36.369588
1447.695882	106928.578006	36.374605
1449.069232	107057.371047	36.379623
1450.520620	107173.091906	36.384640
1451.685309	107310.959302	36.389658
1452.967118	107444.586512	36.394676
1454.288856	107587.959153	36.399693
1455.464572	107733.536135	36.404711
1456.579375	107863.564398	36.409728
1458.231141	108019.250833	36.414746
1459.096742	108174.375588	36.419764
1460.654722	108322.571144	36.424781
1461.998908	108483.608014	36.429799
1463.680286	108635.729373	36.434816
1465.010061	108801.081384	36.439834
1466.450481	108963.107280	36.444852
1468.138670	109124.512049	36.449869
1469.229653	109292.427051	36.454887
1470.779748	109449.670128	36.459904
1472.530358	109616.824615	36.464922
1474.161859	109781.018390	36.469940
1475.791706	109934.763945	36.474957
1477.444769	110096.381575	36.479975
1478.939724	110259.368770	36.484992
1480.593102	110415.674382	36.490010
1482.034051	110576.021060	36.495028
1483.740243	110736.593494	36.500045
1484.901877	110903.389250	36.505063
1486.339941	111059.667823	36.510080
1488.347975	111223.581460	36.515098
1489.707608	111380.837459	36.520116
1491.423185	111533.118255	36.525133
1492.354756	111705.241862	36.530151
1493.973643	111863.994141	36.535168
1495.984632	112017.854307	36.540186
1497.689027	112181.413803	36.545204
1499.271276	112340.731912	36.550221
1500.072352	112499.512850	36.555239
1501.960911	112663.578532	36.560256
1503.480472	112821.691055	36.565274
1505.109794	112978.721886	36.570292
1506.528986	113141.176070	36.575309
1507.867167	113300.675932	36.580327
1509.555853	113465.714875	36.585344
1511.234187	113618.314712	36.590362
1512.786593	113785.418197	36.595380
1514.544142	113942.496674	36.600397
1515.923343	114100.636645	36.605415
1517.490385	114256.211536	36.610432
1518.753230	114410.147637	36.615450
1519.825459	114573.955884	36.620468
1521.319937	114731.256271	36.625485
1523.182122	114901.106885	36.630503
1524.779562	115057.187774	36.635520
1526.578180	115227.569797	36.640538
1527.737614	115388.108583	36.645556
1529.762183	115548.703664	36.650573
1531.383337	115709.603215	36.655591
1532.680678	115858.936044	36.660608
1534.274850	116017.837191	36.665626
1535.978062	116171.965805	36.670644
1537.272145	116324.002566	36.675661
1538.626306	116470.944547	36.680679
1540.083963	116607.394456	36.685696
1541.401015	116754.914092	36.690714
1542.470715	116908.104316	36.695732
1544.022114	117058.784940	36.700749
1545.574107	117213.905365	36.705767
1547.001017	117367.574590	36.710784
1548.547473	117529.939596	36.715802
1549.834990	117691.838253	36.720820
1551.578511	117848.364768	36.725837
1552.878554	118017.137544	36.730855
1554.379821	118181.212045	36.735872
1555.913052	118346.017959	36.740890
1557.390376	118537.774353	36.745908
1558.919775	118696.937960	36.750925
1560.454093	118880.759611	36.755943
1561.350367	119056.969409	36.760960
1563.418533	119244.857495	36.765978
1564.563529	119429.566876	36.770996
1566.815059	119613.217012	36.776013
1567.941198	119790.434546	36.781031
1569.530805	119974.582661	36.786048
1571.322798	120152.180246	36.791066
1572.709919	120344.454459	36.796084
1574.531825	120524.776323	36.801101
1576.304430	120723.144545	36.806119
1577.741143	120905.088373	36.811136
1579.909180	121091.840996	36.816154
1581.340480	121276.045331	36.821172
1583.107439	121471.183580	36.826189
1584.500407	121646.769779	36.831207
1585.715354	121832.342359	36.836224
1587.259913	122024.575024	36.841242
1589.045455	122218.001603	36.846260
1590.991203	122411.708651	36.851277
1592.375693	122595.748896	36.856295
1593.791275	122790.035056	36.861312
1595.684097	122985.820906	36.866330
1597.269703	123180.171321	36.871348
1599.239718	123370.771323	36.876365
1600.641433	123558.416109	36.881383
1602.469089	123751.488447	36.886400
1604.365115	123930.266780	36.891418
1605.910290	124115.544977	36.896436
1608.543065	124279.063201	36.901453
1610.674750	124450.436627	36.906471
1612.518641	124608.218029	36.911488
1614.383114	124763.662597	36.916506
1615.585799	124940.536260	36.921524
1617.386962	125104.555183	36.926541
1619.009077	125267.638482	36.931559
1620.292617	125432.437048	36.936576
1621.983371	125594.508761	36.941594
1623.524907	125766.664704	36.946612
1624.845061	125939.337920	36.951629
1626.200420	126099.814605	36.956647
1627.720534	126281.262622	36.961664
1629.610065	126451.553113	36.966682
1630.863425	126630.735226	36.971700
1632.238519	126810.888745	36.976717
1634.312536	126986.481194	36.981735
1635.805720	127160.705803	36.986752
1637.145769	127342.046983	36.991770
1638.621983	127522.669982	36.996788
1640.240132	127703.969468	37.001805
1642.067331	127887.952251	37.006823
1643.103191	128074.647197	37.011840
1644.611648	128248.645640	37.016858
1646.693921	128423.951100	37.021876
1648.053864	128593.685799	37.026893
1649.307208	128767.117118	37.031911
1650.740571	128946.547666	37.036928
1652.476605	129125.094499	37.041946
1653.834220	129312.937518	37.046964
1655.637577	129487.960964	37.051981
1657.546155	129667.713941	37.056999
1658.864187	129858.915090	37.062016
1660.574885	130046.896734	37.067034
1661.848508	130238.144567	37.072052
1663.282233	130435.585402	37.077069
1664.909882	130633.669429	37.082087
1666.287591	130845.318680	37.087104
1667.798762	131040.999315	37.092122
1669.104206	131263.560921	37.097140
1670.671832	131475.297913	37.102157
1672.538044	131693.955322	37.107175
1673.826639	131926.140664	37.112192
1675.820153	132143.790845	37.117210
1677.409673	132379.979375	37.122228
1678.873551	132594.110724	37.127245
1680.992603	132836.322485	37.132263
1682.512698	133062.260451	37.137280
1684.639863	133281.430835	37.142298
1686.119402	133526.448639	37.147316
1687.631192	133754.421660	37.152333
1689.194520	133987.577601	37.157351
1690.812827	134236.714331	37.162368
1692.547628	134464.186803	37.167386
1694.345026	134698.883490	37.172404
1696.169131	134946.177616	37.177421
1698.015338	135184.231890	37.182439
1699.851411	135418.444140	37.187456
1702.162927	135638.879077	37.192474
1704.106135	135870.640644	37.197492
1705.905326	136092.489926	37.202509
1708.115626	136314.542791	37.207527
1710.077512	136537.967816	37.212544
1711.847722	136763.987088	37.217562
1713.445528	136978.194768	37.222580
1715.392628	137195.508850	37.227597
1717.061367	137421.445642	37.232615
1718.869781	137641.486363	37.237632
1720.360720	137856.933005	37.242650
1721.786015	138079.053148	37.247668
1723.316007	138311.754311	37.252685
1724.832003	138531.502139	37.257703
1726.801068	138763.350431	37.262720
1728.767662	138989.832259	37.267738
1729.910307	139222.306371	37.272756
1731.933658	139458.261333	37.277773
1733.722871	139688.961982	37.282791
1735.644744	139927.397042	37.287808
1737.056319	140151.318510	37.292826
1739.300795	140379.083585	37.297844
1740.565215	140613.563398	37.302861
1742.673245	140842.570235	37.307879
1744.328952	141076.521859	37.312896
1745.759823	141312.019836	37.317914
1747.137805	141555.408300	37.322932
1748.640959	141790.453178	37.327949
1750.576108	142027.665598	37.332967
1752.154956	142274.859131	37.337984
1753.856433	142516.653747	37.343002
1755.493259	142769.158391	37.348020
1757.238063	143014.946487	37.353037
1759.144734	143243.729486	37.358055
1760.564095	143486.524646	37.363072
1762.292631	143714.474530	37.368090
1764.019716	143951.398656	37.373108
1765.492711	144182.766430	37.378125
1767.115543	144428.961282	37.383143
1768.288987	144674.097718	37.388160
1770.534147	144912.900311	37.393178
1772.094351	145161.494575	37.398196
1773.510633	145428.338147	37.403213
1775.243593	145672.275461	37.408231
1776.714343	145941.537437	37.413248
1778.607630	146187.140318	37.418266
1780.493027	146457.190855	37.423284
1781.890155	146719.766886	37.428301
1784.461623	146979.293009	37.433319
1786.417819	147241.175451	37.438336
1788.240105	147503.435448	37.443354
1790.138992	147775.610430	37.448372
1792.084763	148047.677994	37.453389
1793.734414	148309.740446	37.458407
1795.306680	148575.598692	37.463424
1797.247638	148843.165198	37.468442
1798.889973	149114.777794	37.473460
1800.951497	149393.688450	37.478477
1802.700836	149659.753049	37.483495
1804.235559	149944.333500	37.488512
1806.510443	150211.715287	37.493530
1808.499115	150482.036999	37.498548
1810.377703	150758.558821	37.503565
1812.071662	151013.024383	37.508583
1814.040306	151305.833216	37.513600
1815.854051	151566.743661	37.518618
1817.985102	151843.333240	37.523636
1819.502942	152146.409625	37.528653
1821.530873	152417.458338	37.533671
1823.399685	152692.227013	37.538688
1825.117495	152961.803402	37.543706
1827.065555	153244.280282	37.548724
1828.983148	153526.890266	37.553741
1831.101605	153787.979515	37.558759
1832.551291	154075.691882	37.563776
1834.565730	154351.575773	37.568794
1836.322895	154632.845281	37.573812
1837.791928	154918.629381	37.578829
1839.639360	155199.811458	37.583847
1841.260334	155479.963825	37.588864
1843.378019	155773.090091	37.593882
1846.092810	156045.877228	37.598900
1848.946486	156300.770136	37.603917
1853.032647	156511.866483	37.608935
1855.350787	156756.942964	37.613952
1857.359339	156970.433532	37.618970
1859.212537	157201.201165	37.623988
1860.586028	157418.194369	37.629005
1862.237715	157647.217830	37.634023
1863.542015	157894.310242	37.639040
1865.225136	158113.606332	37.644058
1866.864111	158364.685574	37.649076
1868.270912	158610.558954	37.654093
1870.136835	158855.803293	37.659111
1871.074549	159107.197873	37.664128
1872.564727	159373.271989	37.669146
1873.867506	159630.464376	37.674164
1875.448861	159917.524565	37.679181
1877.067586	160188.571444	37.684199
1878.628363	160466.776035	37.689216
1880.298757	160753.673888	37.694234
1881.997014	161033.218018	37.699252
1883.533183	161304.612672	37.704269
1885.306949	161591.180870	37.709287
1886.829503	161868.712049	37.714304
1888.723276	162157.485867	37.719322
1890.414189	162437.634030	37.724340
1891.843312	162739.813368	37.729357
1893.743287	163020.604409	37.734375
1895.136967	163334.586537	37.739392
1896.717525	163636.568738	37.744410
1898.651515	163945.696005	37.749428
1901.008383	164270.298994	37.754445
1902.831664	164580.779561	37.759463
1904.827053	164896.744972	37.764480
1906.681900	165216.695003	37.769498
1908.251250	165539.573071	37.774516
1909.773156	165871.893527	37.779533
1911.952398	166198.907733	37.784551
1913.547405	166539.637855	37.789568
1915.218781	166883.074861	37.794586
1917.420862	167228.005369	37.799604
1919.326992	167578.189320	37.804621
1921.196361	167928.977498	37.809639
1924.060081	168262.789290	37.814656
1926.166732	168601.062839	37.819674
1929.032520	168927.005327	37.824692
1930.589888	169256.543050	37.829709
1932.734984	169592.339372	37.834727
1934.515723	169929.400189	37.839744
1936.283191	170274.476589	37.844762
1938.271561	170616.447486	37.849780
1939.880126	170958.606051	37.854797
1941.833294	171317.955657	37.859815
1943.706230	171662.945928	37.864832
1945.327785	172023.696457	37.869850
1947.399549	172378.702810	37.874868
1949.118303	172743.314395	37.879885
1950.952672	173092.621665	37.884903
1953.063886	173465.149754	37.889920
1954.629597	173836.723302	37.894938
1956.947205	174202.873869	37.899956
1958.494820	174579.190055	37.904973
1960.356473	174957.033701	37.909991
1962.432326	175329.690373	37.915008
1964.560292	175701.807333	37.920026
1966.782351	176080.539810	37.925044
1968.501459	176453.892065	37.930061
1970.861896	176831.908063	37.935079
1972.833374	177201.097457	37.940096
1974.933624	177583.550986	37.945114
1976.953518	177958.780619	37.950132
1979.284796	178342.217493	37.955149
1980.748872	178708.520960	37.960167
1983.114786	179075.472939	37.965184
1984.553338	179458.774329	37.970202
1986.873025	179838.384605	37.975220
1988.813873	180219.528530	37.980237
1990.892050	180598.570094	37.985255
1992.790943	180981.654012	37.990272
1994.290855	181370.236797	37.995290
1995.903447	181758.067149	38.000308
1998.817952	182139.067590	38.005325
2002.259264	182484.531645	38.010343
2005.003984	182849.408121	38.015360
2006.782127	183215.147588	38.020378
2008.907063	183561.556995	38.025396
2010.624275	183921.390777	38.030413
2013.078764	184274.812265	38.035431
2015.562503	184609.968733	38.040448
2017.379645	184942.842585	38.045466
2019.270162	185258.587224	38.050484
2020.927638	185592.097660	38.055501
2022.529008	185917.769594	38.060519
2024.317635	186265.485343	38.065536
2026.085352	186596.746771	38.070554
2027.875395	186924.856258	38.075572
2029.816628	187309.584054	38.080589
2031.605096	187705.284237	38.085607
2032.788171	188056.071912	38.090624
2034.761396	188421.850596	38.095642
2036.672751	188787.436939	38.100660
2038.235441	189163.543521	38.105677
2039.879559	189558.688699	38.110695
2041.997197	189934.305107	38.115712
2043.226818	190315.699798	38.120730
2045.713165	190725.526256	38.125748
2047.560882	191136.977572	38.130765
2049.265538	191548.173189	38.135783
2051.339798	191960.658933	38.140800
2053.428267	192391.000509	38.145818
2055.686410	192789.210716	38.150836
2057.650761	193209.109395	38.155853
2060.326409	193617.468396	38.160871
2062.908945	194019.442170	38.165888
2064.999186	194446.513830	38.170906
2067.145794	194852.495203	38.175924
2068.959181	195272.144723	38.180941
2070.874063	195692.770417	38.185959
2073.309268	196109.303029	38.190976
2074.713235	196547.309192	38.195994
2077.022104	196971.205076	38.201012
2078.848432	197406.658843	38.206029
2080.755986	197827.038111	38.211047
2083.252233	198262.618814	38.216064
2084.979826	198710.741909	38.221082
2087.364707	199147.942845	38.226100
2089.003246	199595.371163	38.231117
2091.479044	200037.513856	38.236135
2093.759932	200482.380742	38.241152
2095.168023	200937.977395	38.246170
2097.393352	201385.598839	38.251188
2099.693448	201844.488471	38.256205
2101.868576	202292.806003	38.261223
2104.585351	202724.376404	38.266240
2106.781995	203175.588731	38.271258
2109.285415	203613.545116	38.276276
2111.138928	204064.889262	38.281293
2112.899200	204518.662261	38.286311
2115.119052	204960.831970	38.291328
2116.953486	205417.618465	38.296346
2119.302541	205864.240983	38.301364
2121.823872	206312.107813	38.306381
2124.118191	206761.585918	38.311399
2126.310206	207211.309517	38.316416
2128.495344	207658.850448	38.321434
2130.438007	208103.457845	38.326452
2133.018252	208551.802754	38.331469
2134.886034	208994.137221	38.336487
2136.985655	209435.725126	38.341504
2138.899687	209897.157276	38.346522
2140.969571	210344.289322	38.351540
2142.812921	210801.517127	38.356557
2145.215183	211258.684124	38.361575
2147.077243	211717.053694	38.366592
2148.972429	212176.638206	38.371610
2151.450853	212632.499950	38.376628
2154.102669	213066.691526	38.381645
2156.587125	213490.316429	38.386663
2158.681946	213911.335133	38.391680
2160.573392	214341.912388	38.396698
2162.262580	214765.103760	38.401716
2164.484443	215199.746019	38.406733
2165.940282	215631.942206	38.411751
2168.108930	216067.203404	38.416768
2170.169092	216524.964327	38.421786
2172.064164	216964.104995	38.426804
2174.238391	217421.645853	38.431821
2176.190000	217883.540454	38.436839
2178.373632	218329.725143	38.441856
2180.352326	218801.523865	38.446874
2182.460388	219273.582283	38.451892
2184.451542	219749.088793	38.456909
2186.270557	220226.527732	38.461927
2188.405581	220711.818455	38.466944
2190.408752	221201.474086	38.471962
2193.246224	221685.741515	38.476980
2195.222697	222179.618892	38.481997
2197.055137	222673.239462	38.487015
2199.498576	223177.079189	38.492032
2201.629474	223680.027773	38.497050
2203.741414	224185.494449	38.502068
2206.235296	224691.536893	38.507085
2208.216126	225202.079570	38.512103
2210.454457	225703.970226	38.517120
2212.885272	226220.895568	38.522138
2215.235091	226732.549441	38.527156
2217.748126	227259.852184	38.532173
2219.543862	227772.024012	38.537191
2222.116713	228283.592101	38.542208
2224.527070	228792.467089	38.547226
2227.061360	229312.551200	38.552244
2230.058959	229806.803275	38.557261
2232.112313	230321.601506	38.562279
2234.783442	230815.573625	38.567296
2237.218869	231332.598160	38.572314
2239.145260	231837.710877	38.577332
2241.353294	232352.128050	38.582349
2243.568806	232860.726137	38.587367
2246.084857	233349.512757	38.592384
2248.162811	233858.741048	38.597402
2250.325029	234375.068804	38.602420
2252.591477	234884.520746	38.607437
2254.660610	235399.007376	38.612455
2256.774329	235913.029182	38.617472
2259.164514	236429.471477	38.622490
2261.519142	236949.627561	38.627508
2264.119059	237458.033641	38.632525
2266.100968	237979.872080	38.637543
2268.766371	238492.813696	38.642560
2270.909508	239001.110715	38.647578
2273.597320	239509.169717	38.652596
2275.950861	240013.291533	38.657613
2277.870249	240529.394246	38.662631
2280.288090	241042.141394	38.667648
2282.546098	241558.875361	38.672666
2284.424124	242074.371871	38.677684
2286.848602	242592.195592	38.682701
2289.215157	243121.255434	38.687719
2291.394662	243630.859013	38.692736
2293.494167	244140.042061	38.697754
2295.954379	244664.943080	38.702772
2298.224816	245187.509892	38.707789
2300.384236	245716.316396	38.712807
2302.776349	246227.506583	38.717824
2305.454697	246741.191198	38.722842
2307.956708	247229.118187	38.727860
2310.155717	247720.952283	38.732877
2312.347843	248211.897068	38.737895
2314.459179	248696.629501	38.742912
2316.881727	249197.950767	38.747930
2318.865022	249687.095031	38.752948
2322.019183	250163.329150	38.757965
2324.322436	250637.814580	38.762983
2326.837946	251132.587307	38.768000
2329.328845	251615.652010	38.773018
2331.444646	252105.708352	38.778036
2333.666213	252595.848300	38.783053
2335.345473	253105.046216	38.788071
2337.812741	253607.058095	38.793088
2339.828129	254113.837886	38.798106
2341.796573	254639.699756	38.803124
2343.578662	255151.084463	38.808141
2345.517162	255695.820313	38.813159
2347.551691	256234.163343	38.818176
2349.886648	256783.075138	38.823194
2351.658734	257344.061533	38.828212
2354.022327	257897.688790	38.833229
2355.988135	258462.043886	38.838247
2358.809904	259029.311314	38.843264
2361.267680	259605.497574	38.848282
2363.865343	260179.347882	38.853300
2365.925435	260746.192393	38.858317
2368.636144	261318.673355	38.863335
2371.263140	261887.303689	38.868352
2373.886097	262461.494387	38.873370
2376.061672	263048.604057	38.878388
2378.637733	263621.094254	38.883405
2380.958167	264210.715090	38.888423
2383.051988	264796.202430	38.893440
2385.552051	265380.251722	38.898458
2388.259361	265975.720458	38.903476
2390.494032	266564.020564	38.908493
2393.148981	267152.708995	38.913511
2395.411099	267749.862010	38.918528
2397.580131	268348.448171	38.923546
2400.144289	268948.416821	38.928564
2402.767586	269531.025516	38.933581
2405.120305	270119.057070	38.938599
2407.689192	270721.908980	38.943616
2410.063572	271318.691725	38.948634
2412.545044	271927.289081	38.953652
2414.665826	272533.652630	38.958669
2417.190114	273136.825334	38.963687
2419.667787	273745.004286	38.968704
2421.790164	274348.789754	38.973722
2424.499325	274959.006507	38.978740
2427.255938	275554.913210	38.983757
2429.572600	276162.490141	38.988775
2432.248297	276769.752691	38.993792
2434.708222	277377.501348	38.998810
2437.360608	277981.329858	39.003828
2439.945087	278579.932816	39.008845
2442.289425	279178.390753	39.013863
2444.936176	279780.733186	39.018880
2447.481352	280378.515560	39.023898
2450.045741	280982.968968	39.028916
2452.734761	281572.009009	39.033933
2455.181972	282162.478630	39.038951
2458.284809	282755.253846	39.043968
2461.220324	283330.376094	39.048986
2463.378269	283918.616231	39.054004
2466.139188	284499.342733	39.059021
2468.506978	285060.268082	39.064039
2470.420668	285633.245033	39.069056
2472.746274	286164.356536	39.074074
2474.720273	286731.982357	39.079092
2477.050893	287296.475398	39.084109
2479.705495	287865.991656	39.089127
2481.342810	288429.973506	39.094144
2484.242987	288998.603770	39.099162
2486.243843	289576.002092	39.104180
2488.575668	290143.593461	39.109197
2490.890036	290740.102854	39.114215
2493.002119	291335.952519	39.119232
2495.597085	291930.832675	39.124250
2497.313464	292540.519415	39.129268
2499.897771	293148.186154	39.134285
2502.525760	293765.564290	39.139303
2504.951953	294387.359874	39.144320
2507.561246	295002.443099	39.149338
2510.061108	295619.948898	39.154356
2512.750018	296250.036945	39.159373
2515.613079	296875.749622	39.164391
2518.242013	297500.374840	39.169408
2520.666907	298114.819034	39.174426
2523.298058	298757.683939	39.179444
2526.158719	299390.274663	39.184461
2528.340000	300023.573188	39.189479
2530.834037	300662.857791	39.194496
2533.395809	301301.870496	39.199514
2535.666017	301951.532418	39.204532
2538.123853	302597.603259	39.209549
2540.745030	303247.956362	39.214567
2543.698950	303892.106448	39.219584
2546.854359	304524.920973	39.224602
2549.237373	305179.754845	39.229620
2552.049731	305827.507517	39.234637
2554.794896	306482.395296	39.239655
2557.171242	307136.925857	39.244672
2559.566742	307787.002833	39.249690
2561.632361	308447.174289	39.254708
2564.219894	309112.687569	39.259725
2567.058689	309778.228854	39.264743
2569.387613	310437.850249	39.269760
2571.924538	311095.653545	39.274778
2574.326374	311776.794111	39.279796
2576.991249	312448.290028	39.284813
2579.869727	313119.793889	39.289831
2582.621519	313796.104648	39.294848
2586.005433	314457.637705	39.299866
2588.151756	315130.343095	39.304884
2590.815306	315797.983813	39.309901
2593.587219	316454.329741	39.314919
2596.064667	317125.228259	39.319936
2599.263515	317783.087120	39.324954
2601.745313	318461.045239	39.329972
2603.973079	319125.506479	39.334989
2606.100386	319791.648113	39.340007
2608.583571	320485.232025	39.345024
2611.400499	321164.770732	39.350042
2613.467037	321853.855088	39.355060
2615.776364	322520.154435	39.360077
2618.521417	323221.493954	39.365095
2620.922018	323918.561710	39.370112
2623.654173	324617.266223	39.375130
2626.042399	325310.633276	39.380148
2628.444691	326017.535548	39.385165
2631.080080	326721.090842	39.390183
2633.339567	327434.688961	39.395200
2636.004580	328145.014461	39.400218
2638.833370	328836.400319	39.405236
2641.505625	329528.077530	39.410253
2643.870104	330219.181578	39.415271
2646.556801	330899.466456	39.420288
2649.652953	331572.166352	39.425306
2652.397398	332243.742264	39.430324
2655.585408	332923.608962	39.435341
2658.383179	333595.330369	39.440359
2660.919921	334277.810936	39.445376
2663.548695	334955.724074	39.450394
2665.925124	335633.943203	39.455412
2668.346301	336318.078653	39.460429
2671.106690	337005.167138	39.465447
2673.207744	337714.260879	39.470464
2675.703848	338416.050393	39.475482
2678.496837	339123.994324	39.480500
2680.819376	339833.265708	39.485517
2683.637535	340558.652967	39.490535
2685.870674	341287.362862	39.495552
2688.931832	341998.505052	39.500570
2691.654857	342728.909549	39.505588
2694.572383	343450.975384	39.510605
2697.646288	344176.805904	39.515623
2700.014038	344914.954530	39.520640
2702.756542	345651.837007	39.525658
2705.372257	346388.368207	39.530676
2708.297020	347125.900299	39.535693
2712.372493	347834.481342	39.540711
2716.091920	348540.922007	39.545728
2719.319973	349257.465356	39.550746
2722.347454	349958.227432	39.555764
2725.363946	350656.795651	39.560781
2728.256493	351349.308313	39.565799
2731.059546	352053.559274	39.570816
2733.856988	352739.642242	39.575834
2736.720871	353438.605108	39.580852
2739.308556	354143.781740	39.585869
2742.274314	354826.472372	39.590887
2744.252534	355535.895943	39.595904
2746.922726	356235.841186	39.600922
2749.844561	356939.001797	39.605940
2752.472800	357649.315527	39.610957
2754.702407	358358.306066	39.615975
2757.349588	359088.989944	39.620992
2759.997287	359797.907419	39.626010
2762.775011	360518.295957	39.631028
2765.610279	361249.430858	39.636045
2768.354794	361965.303507	39.641063
2770.604842	362714.489693	39.646080
2773.082539	363455.080228	39.651098
2776.027806	364192.918256	39.656116
2778.510240	364936.334753	39.661133
2781.287609	365683.183813	39.666151
2783.901876	366437.160338	39.671168
2786.533543	367176.365471	39.676186
2789.109005	367953.470921	39.681204
2791.680289	368709.523210	39.686221
2794.533772	369475.444738	39.691239
2796.847288	370253.668402	39.696256
2799.386572	371034.926710	39.701274
2802.291838	371810.303893	39.706292
2804.902074	372605.088264	39.711309
2808.166053	373397.062427	39.716327
2810.493520	374176.390376	39.721344
2813.589851	374956.893914	39.726362
2816.667426	375739.455405	39.731380
2819.446222	376535.011511	39.736397
2822.704337	377310.634031	39.741415
2825.856105	378082.197538	39.746432
2828.647071	378837.228225	39.751450
2831.483211	379582.680781	39.756468
2834.284885	380328.624251	39.761485
2837.400926	381058.413631	39.766503
2839.746032	381816.290501	39.771520
2842.330439	382568.459994	39.776538
2844.909002	383317.645299	39.781556
2848.205673	384070.901222	39.786573
2851.460614	384817.506244	39.791591
2854.420254	385570.922394	39.796608
2857.083185	386316.587916	39.801626
2860.175356	387072.369897	39.806644
2863.923907	387796.171390	39.811661
2868.024472	388527.594982	39.816679
2871.029878	389271.600126	39.821696
2874.195992	389994.516853	39.826714
2877.472050	390717.192758	39.831732
2879.506656	391451.585957	39.836749
2882.528227	392185.347823	39.841767
2885.080843	392935.566117	39.846784
2887.972898	393663.885646	39.851802
2890.835492	394407.832873	39.856820
2893.311746	395165.234077	39.861837
2895.821257	395909.999749	39.866855
2898.700781	396670.682547	39.871872
2900.999760	397447.884374	39.876890
2904.034520	398226.312954	39.881908
2906.469367	399007.036457	39.886925
2909.294996	399789.950993	39.891943
2911.683223	400592.901413	39.896960
2915.254314	401388.249978	39.901978
2918.119579	402185.047554	39.906996
2920.748377	402987.067406	39.912013
2923.664300	403799.035421	39.917031
2926.449710	404612.614272	39.922048
2929.461294	405413.122618	39.927066
2932.551129	406227.355079	39.932084
2935.692384	407060.374569	39.937101
2938.604069	407867.440001	39.942119
2941.039722	408695.296209	39.947136
2943.734034	409527.584439	39.952154
2947.119410	410358.873562	39.957172
2949.790140	411198.590428	39.962189
2952.971497	412023.220234	39.967207
2955.500085	412874.834378	39.972224
2958.460616	413728.118377	39.977242
2961.367074	414579.404114	39.982260
2964.179582	415436.386685	39.987277
2967.302529	416287.216661	39.992295
2970.566148	417153.721096	39.997312
2973.056777	418010.599307	40.002330
2976.570090	418873.656069	40.007348
2979.442493	419741.581526	40.012365
2982.361617	420598.641217	40.017383
2985.533308	421462.908264	40.022400
2988.259127	422330.849415	40.027418
2991.267889	423202.552897	40.032436
2994.398437	424068.688920	40.037453
2998.145360	424937.725898	40.042471
3000.954219	425788.468149	40.047488
3004.217835	426650.175780	40.052506
3007.256352	427508.949355	40.057524
3009.891707	428377.909911	40.062541
3013.040027	429239.574640	40.067559
3016.499192	430092.712061	40.072576
3018.831994	430960.090267	40.077594
3022.289761	431824.070949	40.082612
3025.253070	432685.411790	40.087629
3028.350807	433518.543314	40.092647
3030.891803	434352.837580	40.097664
3033.439861	435183.506813	40.102682
3036.428202	436009.068996	40.107700
3038.924359	436855.996196	40.112717
3041.946262	437689.313004	40.117735
3045.263113	438542.505278	40.122752
3047.740142	439411.452242	40.127770
3050.803554	440265.414669	40.132788
3053.750797	441136.431891	40.137805
3056.506090	441996.274265	40.142823
3059.605730	442875.370477	40.147840
3062.208424	443768.746821	40.152858
3065.368271	444651.840900	40.157876
3067.985189	445547.351394	40.162893
3071.108595	446451.426172	40.167911
3073.972410	447361.455860	40.172928
3076.977806	448282.881406	40.177946
3080.380784	449208.389467	40.182964
3083.312127	450131.348215	40.187981
3086.857863	451050.427537	40.192999
3090.224772	451984.179809	40.198016
3093.050687	452904.638861	40.203034
3096.898137	453824.436826	40.208052
3100.296629	454747.538027	40.213069
3103.477136	455681.931910	40.218087
3106.659790	456602.596632	40.223104
3110.013071	457543.526929	40.228122
3113.501344	458463.944686	40.233140
3116.717020	459397.124248	40.238157
3119.649407	460322.727580	40.243175
3123.058417	461238.719882	40.248192
3125.926057	462181.087267	40.253210
3129.479851	463106.644940	40.258228
3132.236573	464035.606071	40.263245
3135.183583	464979.420063	40.268263
3138.474240	465926.810336	40.273280
3141.644225	466874.115336	40.278298
3145.038660	467800.145647	40.283316
3148.466402	468747.455229	40.288333
3151.766496	469691.250272	40.293351
3155.039287	470635.903316	40.298368
3158.058001	471577.011335	40.303386
3161.360927	472503.346304	40.308404
3164.492880	473458.044693	40.313421
3167.416071	474407.172902	40.318439
3170.648909	475358.466038	40.323456
3173.560948	476319.684892	40.328474
3176.495707	477265.113570	40.333492
3179.348734	478230.713565	40.338509
3182.847776	479193.230771	40.343527
3186.282139	480159.227840	40.348544
3189.615373	481122.510225	40.353562
3192.968902	482068.796626	40.358580
3196.114397	483035.820958	40.363597
3199.431672	483994.897445	40.368615
3202.915047	484954.795859	40.373632
3206.421871	485912.262937	40.378650
3209.459087	486863.395405	40.383668
3212.618265	487821.049684	40.388685
3215.764534	488770.736940	40.393703
3218.957919	489738.441629	40.398720
3222.197650	490699.630073	40.403738
3225.357436	491656.539064	40.408756
3228.696519	492615.726463	40.413773
3231.816463	493568.239108	40.418791
3235.423968	494524.593422	40.423808
3238.354628	495475.150620	40.428826
3241.399441	496399.195089	40.433844
3244.843590	497321.005091	40.438861
3248.179322	498234.618508	40.443879
3251.408050	499145.020237	40.448896
3254.180274	500062.634730	40.453914
3257.595149	500967.860086	40.458932
3260.664799	501895.077801	40.463949
3264.146729	502809.036235	40.468967
3267.643325	503740.749706	40.473984
3271.054248	504660.489800	40.479002
3274.015590	505575.259258	40.484020
3277.370847	506514.412576	40.489037
3280.804119	507442.875889	40.494055
3283.703113	508382.681100	40.499072
3286.707570	509329.047772	40.504090
3290.287253	510273.752292	40.509108
3293.558483	511225.935758	40.514125
3296.630884	512177.632692	40.519143
3299.703519	513140.278562	40.524160
3302.565940	514115.613411	40.529178
3305.540267	515077.687493	40.534196
3308.960473	516068.184898	40.539213
3311.521571	517069.906247	40.544231
3314.967763	518066.942230	40.549248
3318.076707	519079.390810	40.554266
3321.374142	520093.292935	40.559284
3324.738989	521113.391526	40.564301
3327.244840	522150.433669	40.569319
3331.040167	523183.024048	40.574336
3334.144423	524241.973921	40.579354
3337.679314	525277.357676	40.584372
3340.660115	526337.315934	40.589389
3344.359288	527394.063293	40.594407
3347.626813	528447.929838	40.599424
3351.932005	529502.002562	40.604442
3355.831144	530531.593128	40.609460
3359.659188	531570.455065	40.614477
3363.317651	532629.398261	40.619495
3367.090208	533659.514284	40.624512
3370.096299	534699.508778	40.629530
3374.033019	535746.956096	40.634548
3377.418173	536793.751067	40.639565
3380.373454	537828.730529	40.644583
3384.079940	538875.154142	40.649600
3387.616311	539925.282225	40.654618
3391.099286	540957.063636	40.659636
3394.236450	542000.255916	40.664653
3397.412430	543060.767247	40.669671
3400.684049	544108.479909	40.674688
3404.037960	545154.436163	40.679706
3407.468481	546208.268736	40.684724
3410.850237	547264.928561	40.689741
3414.217742	548328.471904	40.694759
3417.635278	549390.410926	40.699776
3420.874973	550454.893299	40.704794
3424.437167	551516.675396	40.709812
3427.733740	552577.303135	40.714829
3431.438552	553660.435485	40.719847
3434.787982	554711.342468	40.724864
3437.969690	555779.326912	40.729882
3441.301714	556854.861521	40.734900
3445.263115	557925.791214	40.739917
3448.819248	558998.090898	40.744935
3452.855105	560062.302111	40.749952
3456.186986	561131.737947	40.754970
3459.810835	562189.158017	40.759988
3463.425756	563242.827511	40.765005
3466.629624	564294.291245	40.770010
3470.397572	565291.994498	40.775015
3473.458939	566245.788975	40.780020
3476.716479	567159.008967	40.785024
3479.826753	568016.957949	40.790029
3482.342839	568805.059672	40.795034
3485.604344	569548.368062	40.800039
3488.205894	570228.539261	40.805044
3490.870893	570844.719003	40.810048
3493.135287	571416.562694	40.815053
3495.457357	571950.780554	40.820058
3497.447856	572405.535970	40.825063
3499.598388	572820.404832	40.830068
3501.853370	573192.238841	40.835072
3503.636138	573520.630162	40.840077
3504.792589	573790.854653	40.845082
3506.642007	574043.604196	40.850087
3507.515675	574241.458617	40.855092
3508.770438	574399.763552	40.860096
3510.241119	574537.311154	40.865101
3511.116019	574651.569335	40.870106
3512.132481	574733.192359	40.875111
3512.894465	574774.817084	40.880116
3513.746410	574797.111431	40.885120
3514.688497	574777.899424	40.890125
3515.001651	574744.937712	40.895130
3515.878207	574704.061331	40.900135
3516.139699	574643.512474	40.905140
3516.731132	574559.330616	40.910144
3517.489408	574461.776017	40.915149
3517.008168	574361.954939	40.920154
3517.806209	574235.491958	40.925159
3518.198776	574105.678758	40.930164
3517.908191	573956.201142	40.935168
3518.573849	573801.254049	40.940173
3518.552420	573637.128988	40.945178
3519.023718	573455.462954	40.950183
3519.124249	573292.668745	40.955188
3519.191087	573102.128192	40.960192
3519.546123	572905.116511	40.965197
3519.129643	572710.680361	40.970202
3519.734898	572495.005381	40.975207
3519.427811	572289.504925	40.980212
3519.482920	572076.165875	40.985216
3519.257321	571859.554308	40.990221
3519.259215	571646.165317	40.995226
3519.239947	571418.371988	41.000231
3519.304787	571197.788096	41.005236
3519.354851	570962.245953	41.010240
3519.178222	570732.355519	41.015245
3518.832617	570501.784092	41.020250
3518.601387	570269.383318	41.025255
3518.704218	570045.257888	41.030260
3518.592882	569817.447059	41.035264
3518.832382	569580.943583	41.040269
3518.161861	569356.975267	41.045274
3518.382004	569115.546029	41.050279
3518.174382	568894.408105	41.055284
3517.828754	568662.143239	41.060288
3517.803365	568439.612859	41.065293
3517.685102	568215.185004	41.070298
3518.083117	567976.716306	41.075303
3517.811602	567752.453917	41.080308
3517.520585	567528.792660	41.085312
3517.306118	567297.785249	41.090317
3517.095455	567078.370202	41.095322
3517.141309	566843.397163	41.100327
3516.481310	566627.206531	41.105332
3516.262881	566405.872069	41.110336
3516.571731	566183.396932	41.115341
3516.415608	565970.981821	41.120346
3516.067947	565753.270207	41.125351
3516.087419	565536.150151	41.130356
3515.556530	565319.212117	41.135360
3515.945746	565101.825577	41.140365
3515.543725	564900.325722	41.145370
3515.419506	564693.054514	41.150375
3515.622931	564485.929509	41.155380
3515.157084	564278.553455	41.160384
3515.022159	564075.240170	41.165389
3514.730392	563879.279833	41.170394
3514.969445	563668.970978	41.175399
3514.603274	563485.671208	41.180404
3514.297481	563276.745853	41.185408
3514.431031	563087.184751	41.190413
3514.039893	562892.730070	41.195418
3514.289071	562684.862967	41.200423
3513.869074	562496.634091	41.205428
3513.873380	562300.249721	41.210432
3513.626160	562103.348713	41.215437
3513.457384	561926.724343	41.220442
3513.476963	561746.049711	41.225447
3512.736866	561562.677668	41.230452
3512.832702	561376.108638	41.235456
3512.712652	561201.525263	41.240461
3512.694964	561032.549343	41.245466
3512.300975	560856.898401	41.250471
3512.205353	560683.207749	41.255476
3512.223631	560523.461880	41.260480
3512.241140	560349.547790	41.265485
3511.947977	560184.319985	41.270490
3511.786380	560009.926423	41.275495
3511.785889	559849.320366	41.280500
3511.377223	559694.301777	41.285504
3511.591012	559531.899764	41.290509
3511.165587	559374.618887	41.295514
3511.135489	559210.391590	41.300519
3510.804626	559063.843140	41.305524
3510.897450	558921.698382	41.310528
3510.654234	558763.928898	41.315533
3510.663968	558622.145180	41.320538
3510.946347	558470.921970	41.325543
3510.684327	558328.071700	41.330548
3509.976997	558179.561209	41.335552
3510.604702	558031.494296	41.340557
3510.305644	557891.156779	41.345562
3510.030552	557754.381326	41.350567
3509.696964	557622.889265	41.355572
3509.768718	557475.756159	41.360576
3509.969601	557343.524644	41.365581
3509.941621	557209.970584	41.370586
3509.753866	557068.701616	41.375591
3509.320331	556935.509092	41.380596
3509.118653	556816.851408	41.385600
3508.945071	556680.399614	41.390605
3508.793397	556563.842150	41.395610
3508.446238	556429.826545	41.400615
3508.522733	556326.447340	41.405620
3508.613515	556200.602299	41.410624
3508.838907	556083.931241	41.415629
3508.101381	555970.524589	41.420634
3508.604427	555847.476123	41.425639
3509.049534	555740.818278	41.430644
3508.486865	555617.179481	41.435648
3508.190958	555495.859892	41.440653
3508.021054	555387.837219	41.445658
3507.932985	555274.976256	41.450663
3507.603473	555165.016430	41.455668
3507.984133	555061.579011	41.460672
3508.050277	554957.083984	41.465677
3508.031088	554849.585857	41.470682
3507.716182	554741.831239	41.475687
3507.752260	554638.996657	41.480692
3507.526138	554525.597308	41.485696
3507.328907	554418.123039	41.490701
3507.288828	554322.736040	41.495706
3507.256992	554220.461318	41.500711
3507.434462	554120.213857	41.505716
3507.100394	554032.459707	41.510720
3507.070177	553937.419958	41.515725
3506.940770	553834.805322	41.520730
3507.083934	553733.353701	41.525735
3507.551831	553637.831984	41.530740
3507.440773	553539.534598	41.535744
3507.209525	553450.352848	41.540749
3506.508679	553349.129870	41.545754
3506.587354	553258.842933	41.550759
3506.528191	553166.716974	41.555764
3506.599601	553078.742010	41.560768
3506.764320	552988.288873	41.565773
3506.389113	552891.183436	41.570778
3506.684186	552813.174673	41.575783
3506.604536	552727.985319	41.580788
3506.316077	552638.907031	41.585792
3506.254737	552539.789523	41.590797
3506.409001	552460.644255	41.595802
3506.452499	552378.750960	41.600807
3506.446008	552288.620860	41.605812
3506.346911	552206.547520	41.610816
3506.127650	552123.939364	41.615821
3506.119012	552044.213503	41.620826
3505.919812	551955.518467	41.625831
3506.195919	551875.294760	41.630836
3505.940479	551798.722448	41.635840
3505.803346	551709.814879	41.640845
3506.183979	551634.349054	41.645850
3505.715273	551564.544795	41.650855
3505.892620	551488.104268	41.655860
3505.260844	551406.711684	41.660864
3505.447878	551333.586641	41.665869
3505.299994	551261.820369	41.670874
3505.167545	551193.218474	41.675879
3505.512938	551125.396481	41.680884
3505.115374	551056.432884	41.685888
3505.259406	550980.295999	41.690893
3504.521127	550922.545466	41.695898
3504.826726	550856.638590	41.700903
3505.256763	550794.935067	41.705908
3504.969449	550733.242312	41.710912
3505.111468	550668.113997	41.715917
3504.876797	550605.859379	41.720922
3505.097009	550526.590733	41.725927
3504.932934	550457.537141	41.730932
3504.766314	550397.935504	41.735936
3505.086992	550328.051603	41.740941
3505.038185	550267.576295	41.745946
3504.926711	550198.915272	41.750951
3504.814003	550142.320626	41.755956
3504.790103	550080.030531	41.760960
3504.696003	550015.890760	41.765965
3504.513462	549962.825603	41.770970
3504.455313	549897.472943	41.775975
3504.737784	549841.167359	41.780980
3504.484639	549781.827577	41.785984
3504.526039	549724.201440	41.790989
3504.485809	549673.626837	41.795994
3504.892734	549608.401382	41.800999
3504.572836	549555.154713	41.806004
3504.470182	549495.035927	41.811008
3504.613627	549438.398168	41.816013
3504.739853	549382.165070	41.821018
3504.504363	549319.803474	41.826023
3504.141258	549253.489221	41.831028
3504.507340	549200.134263	41.836032
3504.559710	549143.257908	41.841037
3504.349924	549091.450252	41.846042
3504.142083	549024.406655	41.851047
3504.135124	548981.466873	41.856052
3503.778336	548934.810206	41.861056
3504.234342	548879.629701	41.866061
3504.043522	548827.415719	41.871066
3504.317825	548775.229702	41.876071
3504.415942	548723.724562	41.881076
3504.266225	548657.373881	41.886080
3504.673611	548601.696861	41.891085
3504.227162	548550.225452	41.896090
3504.255757	548490.282457	41.901095
3504.336027	548440.438284	41.906100
3503.879611	548390.576855	41.911104
3503.942766	548333.946500	41.916109
3503.803536	548303.344694	41.921114
3504.158534	548250.339337	41.926119
3504.055734	548193.130737	41.931124
3503.789608	548141.428413	41.936128
3503.977650	548085.481479	41.941133
3504.311095	548040.675154	41.946138
3503.863774	547986.586650	41.951143
3503.753362	547928.020276	41.956148
3503.655447	547883.733083	41.961152
3503.970195	547840.538112	41.966157
3503.865721	547802.386633	41.971162
3503.764518	547748.092360	41.976167
3503.734191	547706.509519	41.981172
3503.720039	547657.883769	41.986176
3503.764068	547610.707118	41.991181
3503.391118	547571.942964	41.996186
3503.620077	547528.408235	42.001191
3503.976512	547477.762874	42.006196
3503.725146	547433.196212	42.011200
3504.039763	547379.791092	42.016205
3504.130916	547339.596194	42.021210
3503.992301	547293.804551	42.026215
3503.967675	547242.563767	42.031220
3503.524131	547198.378186	42.036224
3504.086956	547138.999252	42.041229
3503.944117	547104.271280	42.046234
3503.715962	547042.953089	42.051239
3503.631604	547003.840500	42.056244
3503.431599	546963.890848	42.061248
3504.352270	546916.625421	42.066253
3503.729726	546863.917103	42.071258
3503.746952	546813.623551	42.076263
3503.773932	546768.256811	42.081268
3503.837242	546728.768336	42.086272
3503.862298	546663.687304	42.091277
3503.869940	546627.325244	42.096282
3503.597259	546579.137813	42.101287
3503.559650	546520.704312	42.106292
3503.448743	546485.818756	42.111296
3503.544686	546439.534819	42.116301
3503.583094	546407.090138	42.121306
3503.030230	546370.361911	42.126311
3503.406935	546326.297035	42.131316
3503.017438	546283.105629	42.136320
3503.011961	546241.564286	42.141325
3503.178545	546210.205596	42.146330
3503.111962	546172.194068	42.151335
3503.464808	546141.812092	42.156340
3503.108512	546104.650139	42.161344
3503.630683	546053.269048	42.166349
3503.443908	546019.148395	42.171354
3503.083976	545977.912797	42.176359
3503.175297	545933.890937	42.181364
3503.142342	545898.438357	42.186368
3503.359791	545856.106613	42.191373
3503.118755	545819.680292	42.196378
3502.919472	545774.797779	42.201383
3503.201776	545741.508681	42.206388
3503.214870	545713.441816	42.211392
3503.556042	545678.483639	42.216397
3502.952220	545648.551100	42.221402
3502.715933	545606.993253	42.226407
3503.193523	545563.614114	42.231412
3502.903506	545529.156107	42.236416
3503.278737	545488.910998	42.241421
3502.816755	545463.281423	42.246426
3503.127573	545427.069852	42.251431
3503.276027	545387.463264	42.256436
3503.583397	545352.911806	42.261440
3503.478499	545312.992327	42.266445
3503.184807	545278.031224	42.271450
3503.277727	545224.701619	42.276455
3503.341688	545188.276280	42.281460
3503.239124	545150.669604	42.286464
3503.196895	545111.946872	42.291469
3503.151982	545074.230397	42.296474
3503.278012	545030.602320	42.301479
3502.779130	544998.489058	42.306484
3502.763456	544965.998730	42.311488
3502.889169	544926.494810	42.316493
3503.220032	544899.935917	42.321498
3502.988109	544858.374887	42.326503
3503.335373	544824.318744	42.331508
3503.072142	544783.416223	42.336512
3503.306005	544739.669749	42.341517
3503.178399	544715.495577	42.346522
3503.134901	544670.584834	42.351527
3503.306745	544633.939887	42.356532
3503.266887	544600.949372	42.361536
3503.396810	544553.898625	42.366541
3502.827342	544511.986563	42.371546
3502.633817	544480.025645	42.376551
3502.963534	544444.411884	42.381556
3503.033321	544412.912825	42.386560
3503.213523	544392.714182	42.391565
3502.927915	544359.912172	42.396570
3502.696548	544317.242630	42.401575
3502.836909	544286.838894	42.406580
3502.684521	544256.380036	42.411584
3503.241280	544216.102571	42.416589
3503.164214	544184.223376	42.421594
3502.750558	544150.082596	42.426599
3502.604430	544119.320619	42.431604
3502.615478	544091.854039	42.436608
3502.950999	544048.994760	42.441613
3502.937636	544021.481522	42.446618
3503.062099	543997.568546	42.451623
3503.171366	543958.667748	42.456628
3502.700463	543921.215283	42.461632
3503.122198	543875.223227	42.466637
3502.843738	543853.435091	42.471642
3503.048890	543818.241353	42.476647
3503.069165	543781.919310	42.481652
3502.810653	543742.924162	42.486656
3503.012258	543712.207678	42.491661
3502.949806	543688.625018	42.496666
3502.565068	543650.755903	42.501671
3503.089242	543609.324570	42.506676
3502.599945	543592.951307	42.511680
3502.681167	543552.544490	42.516685
3502.784183	543532.255860	42.521690
3502.690339	543491.171828	42.526695
3502.530416	543459.203066	42.531700
3502.351860	543440.064802	42.536704
3502.632402	543405.059387	42.541709
3502.802010	543375.504065	42.546714
3502.861504	543348.883496	42.551719
3502.932112	543309.634561	42.556724
3502.832356	543275.140709	42.561728
3502.780563	543234.602648	42.566733
3502.906521	543211.190991	42.571738
3503.141705	543170.909901	42.576743
3503.177284	543144.996899	42.581748
3502.609786	543107.003659	42.586752
3502.590054	543076.521281	42.591757
3502.780387	543043.038076	42.596762
3502.819096	543016.973404	42.601767
3502.824497	542986.839042	42.606772
3503.174677	542959.166282	42.611776
3502.734476	542911.795620	42.616781
3502.598322	542887.267091	42.621786
3502.697466	542859.884711	42.626791
3502.749229	542825.164813	42.631796
3502.637779	542799.223669	42.636800
3502.964547	542751.179671	42.641805
3502.945336	542724.016641	42.646810
3502.879487	542699.376189	42.651815
3503.454464	542655.820883	42.656820
3503.165184	542622.511805	42.661824
3503.008202	542579.422291	42.666829
3502.782995	542551.486013	42.671834
3502.786996	542522.407224	42.676839
3502.775754	542486.287561	42.681844
3502.681447	542457.475461	42.686848
3502.750931	542413.494891	42.691853
3503.147352	542397.183464	42.696858
3503.098998	542368.967716	42.701863
3503.126295	542321.220219	42.706868
3503.001801	542284.715127	42.711872
3502.880034	542246.247438	42.716877
3502.735653	542212.864413	42.721882
3502.594544	542178.172739	42.726887
3503.064127	542147.310102	42.731892
3502.753690	542128.391595	42.736896
3502.739359	542086.234076	42.741901
3502.643232	542057.572272	42.746906
3502.684928	542029.895160	42.751911
3502.919880	541991.823974	42.756916
3502.763594	541963.925974	42.761920
3502.564362	541920.689841	42.766925
3502.755722	541889.517693	42.771930
3502.767375	541858.222499	42.776935
3502.691179	541830.714228	42.781940
3502.362845	541816.175095	42.786945
3502.322026	541784.233838	42.791949
3502.324781	541766.372895	42.796954
3502.517175	541743.602211	42.801959
3502.417206	541718.260783	42.806964
3502.322658	541690.805372	42.811969
3502.435171	541662.864875	42.816973
3502.353992	541640.086264	42.821978
3502.546022	541606.699591	42.826983
3502.514812	541575.611612	42.831988
3502.355247	541553.398474	42.836993
3502.354742	541522.859020	42.841997
3502.406431	541510.977261	42.847002
3502.195429	541473.829214	42.852007
3502.459089	541436.808445	42.857012
3502.590021	541433.115237	42.862017
3502.550023	541393.424710	42.867021
3502.694315	541365.629547	42.872026
3502.632688	541339.526696	42.877031
3502.741618	541310.026271	42.882036
3502.240917	541279.815630	42.887041
3502.462606	541255.177915	42.892045
3502.673132	541223.196122	42.897050
3502.582333	541190.858628	42.902055
3502.751985	541162.958445	42.907060
3502.465272	541141.971896	42.912065
3502.293656	541113.319687	42.917069
3502.629957	541088.965696	42.922074
3502.442673	541056.743501	42.927079
3502.537695	541017.533921	42.932084
3502.113606	541001.650259	42.937089
3502.304371	540972.538824	42.942093
3502.142160	540965.218139	42.947098
3502.408751	540936.296079	42.952103
3502.449482	540904.440530	42.957108
3501.856487	540882.545229	42.962113
3502.064069	540853.833422	42.967117
3502.000489	540837.742509	42.972122
3502.017225	540818.972376	42.977127
3502.508633	540786.341987	42.982132
3502.019192	540772.883336	42.987137
3502.448428	540745.042465	42.992141
3502.427343	540725.120825	42.997146
3502.007866	540695.650874	43.002151
3502.482209	540676.205533	43.007156
3502.485133	540659.751834	43.012161
3502.635774	540617.513413	43.017165
3502.145300	540598.268405	43.022170
3502.178831	540565.104905	43.027175
3502.861975	540549.551534	43.032180
3502.063712	540522.806879	43.037185
3502.451317	540490.091246	43.042189
3502.608768	540463.902175	43.047194
3502.515331	540442.079320	43.052199
3502.656252	540418.408557	43.057204
3502.277910	540387.824517	43.062209
3502.164164	540360.369196	43.067213
3502.213898	540350.650276	43.072218
3501.942575	540323.320030	43.077223
3502.552288	540295.802306	43.082228
3502.391373	540269.310154	43.087233
3502.125595	540234.380939	43.092237
3502.038512	540219.047656	43.097242
3502.347229	540190.519875	43.102247
3502.088635	540160.419827	43.107252
3502.135282	540152.512673	43.112257
3502.279851	540118.928181	43.117261
3502.123018	540105.215786	43.122266
3502.555796	540079.888799	43.127271
3502.653291	540056.676979	43.132276
3502.299750	540036.705351	43.137281
3502.411013	540001.666503	43.142285
3502.150355	539970.459319	43.147290
3502.057035	539944.912019	43.152295
3502.185749	539932.563921	43.157300
3502.243519	539910.263750	43.162305
3501.873462	539881.438350	43.167309
3502.074886	539858.059037	43.172314
3502.025322	539844.480623	43.177319
3502.568022	539820.092073	43.182324
3502.166943	539797.460553	43.187329
3502.079699	539776.340052	43.192333
3502.237948	539750.300339	43.197338
3502.179688	539727.061833	43.202343
3502.278778	539704.151036	43.207348
3501.951616	539698.616466	43.212353
3502.242902	539662.190037	43.217357
3502.103941	539638.913608	43.222362
3501.943322	539616.194025	43.227367
3502.316270	539598.825927	43.232372
3502.192196	539575.446425	43.237377
3501.857919	539538.764746	43.242381
3502.287570	539524.054693	43.247386
3502.222145	539505.546998	43.252391
3502.543066	539485.771467	43.257396
3502.224839	539470.221643	43.262401
3502.385570	539435.727057	43.267405
3502.726008	539409.205407	43.272410
3502.538123	539380.803404	43.277415
3502.268387	539350.300594	43.282420
3502.285728	539330.320457	43.287425
3502.214207	539295.207457	43.292429
3501.945408	539286.392748	43.297434
3502.354472	539263.986453	43.302439
3502.012704	539232.689430	43.307444
3501.780623	539209.778952	43.312449
3502.144482	539187.027306	43.317453
3502.111474	539170.879192	43.322458
3502.128413	539154.320712	43.327463
3502.312929	539131.596875	43.332468
3501.971265	539118.415389	43.337473
3502.297210	539087.718609	43.342477
3502.129301	539075.214548	43.347482
3502.336004	539050.876809	43.352487
3502.483419	539016.836056	43.357492
3502.232710	539002.382239	43.362497
3502.241373	538977.068730	43.367501
3502.223567	538940.990265	43.372506
3502.262483	538922.364837	43.377511
3502.220804	538893.888669	43.382516
3501.710336	538871.876388	43.387521
3502.314235	538853.364232	43.392525
3502.169988	538830.187786	43.397530
3501.910041	538815.886164	43.402535
3502.255690	538786.795929	43.407540
3502.070639	538779.779469	43.412545
3502.269603	538746.484818	43.417549
3502.288638	538723.987296	43.422554
3502.332185	538701.334950	43.427559
3502.313952	538666.111270	43.432564
3502.313898	538652.121286	43.437569
3502.534590	538625.113399	43.442573
3502.431343	538597.602299	43.447578
3501.999024	538572.004337	43.452583
3502.235903	538546.654457	43.457588
3501.685593	538526.660741	43.462593
3502.101178	538509.536144	43.467597
3502.132751	538488.143388	43.472602
3501.736433	538463.848038	43.477607
3502.408614	538451.011336	43.482612
3501.978632	538440.812034	43.487617
3502.041402	538410.255222	43.492621
3502.089860	538393.489547	43.497626
3502.008181	538371.711620	43.502631
3501.806143	538349.801411	43.507636
3501.984863	538335.179360	43.512641
3502.000819	538315.348817	43.517645
3502.261562	538281.540087	43.522650
3502.091321	538266.720634	43.527655
3502.455508	538245.929940	43.532660
3501.886466	538216.276185	43.537665
3501.788559	538196.412849	43.542669
3502.364776	538187.012950	43.547674
3502.525244	538169.625644	43.552679
3502.447346	538128.068731	43.557684
3502.122820	538119.010252	43.562689
3502.322270	538082.996196	43.567693
3502.216262	538043.557071	43.572698
3501.757396	538032.657369	43.577703
3502.278479	538010.483070	43.582708
3501.936145	537996.897912	43.587713
3502.059402	537967.538457	43.592717
3501.914982	537952.563640	43.597722
3501.796358	537937.484138	43.602727
3501.977703	537918.482792	43.607732
3501.830211	537901.797289	43.612737
3501.987967	537877.615904	43.617741
3501.903278	537867.966329	43.622746
3501.852883	537845.578713	43.627751
3502.025895	537824.917736	43.632756
3502.198934	537812.057414	43.637761
3501.936453	537793.225600	43.642765
3501.946939	537770.375433	43.647770
3501.840760	537760.074867	43.652775
3502.044893	537725.166272	43.657780
3502.062901	537723.049710	43.662785
3502.016465	537688.381315	43.667789
3502.192430	537662.686864	43.672794
3501.904205	537643.858835	43.677799
3502.108718	537621.280175	43.682804
3502.175453	537604.611274	43.687809
3502.133952	537575.779834	43.692813
3502.078348	537563.810416	43.697818
3502.236163	537537.766242	43.702823
3502.593326	537515.314625	43.707828
3502.176417	537492.933095	43.712833
3502.012535	537467.140150	43.717837
3502.337945	537447.109117	43.722842
3502.504957	537419.251445	43.727847
3502.553581	537390.808192	43.732852
3502.511579	537373.451308	43.737857
3502.370438	537344.936824	43.742861
3502.301572	537310.623196	43.747866
3502.107903	537299.027317	43.752871
3502.610514	537259.692375	43.757876
3502.685658	537249.765815	43.762881
3502.395307	537215.989690	43.767885
3502.471773	537178.985635	43.772890
3502.070170	537157.406406	43.777895
3502.099628	537127.153681	43.782900
3502.103723	537124.938525	43.787905
3502.092365	537091.672284	43.792909
3502.081906	537068.824121	43.797914
3501.998005	537050.617709	43.802919
3502.392694	537022.925065	43.807924
3502.247344	537012.428670	43.812929
3502.090082	536970.779676	43.817933
3502.299095	536959.271817	43.822938
3502.359569	536935.053457	43.827943
3502.039833	536906.817438	43.832948
3502.122336	536890.900112	43.837953
3502.156846	536860.142663	43.842957
3502.280887	536844.923446	43.847962
3502.115094	536830.806262	43.852967
3502.241885	536800.487287	43.857972
3502.164437	536772.867573	43.862977
3502.129811	536751.230550	43.867981
3502.659930	536724.069829	43.872986
3502.499004	536698.476197	43.877991
3502.308581	536672.534783	43.882996
3502.309459	536651.445713	43.888001
3502.461736	536623.387275	43.893005
3502.005463	536596.832765	43.898010
3501.988670	536582.289465	43.903015
3502.389333	536548.756369	43.908020
3502.440099	536529.118962	43.913025
3502.176285	536507.718520	43.918029
3502.459503	536483.061986	43.923034
3501.952892	536469.047770	43.928039
3502.747551	536434.647748	43.933044
3502.409230	536413.913065	43.938049
3502.297350	536377.489659	43.943053
3502.208632	536349.719787	43.948058
3502.127670	536335.236525	43.953063
3502.087706	536298.097043	43.958068
3501.719799	536293.775312	43.963073
3501.972647	536271.388082	43.968077
3502.131244	536254.250129	43.973082
3501.963127	536233.438335	43.978087
3501.961766	536216.828555	43.983092
3501.831159	536196.916864	43.988097
3502.019083	536170.865224	43.993101
3502.451090	536147.946564	43.998106
3502.229848	536135.649250	44.003111
3502.151963	536102.793459	44.008116
3502.464131	536077.829639	44.013121
3502.264486	536045.898660	44.018125
3502.087795	536037.872706	44.023130
3502.033987	536012.714039	44.028135
3502.271571	535980.714859	44.033140
3501.837195	535972.326289	44.038145
3501.803719	535950.134057	44.043149
3502.002610	535916.983049	44.048154
3501.455940	535906.296523	44.053159
3502.202566	535873.714519	44.058164
3502.113306	535879.315543	44.063169
3502.473305	535842.464845	44.068173
3502.467916	535828.673937	44.073178
3501.717399	535803.321267	44.078183
3502.511892	535783.214641	44.083188
3502.350060	535756.813907	44.088193
3502.394784	535730.934664	44.093197
3501.929258	535708.054217	44.098202
3501.927929	535679.161917	44.103207
3502.489081	535664.980661	44.108212
3502.066578	535642.445750	44.113217
3501.836113	535618.924539	44.118221
3502.083499	535589.137627	44.123226
3502.083347	535580.580557	44.128231
3502.345830	535558.995960	44.133236
3502.113125	535542.572315	44.138241
3502.298440	535517.375467	44.143245
3502.327271	535493.612333	44.148250
3501.878553	535470.275821	44.153255
3502.321107	535441.968285	44.158260
3502.299943	535421.333650	44.163265
3501.973698	535393.900689	44.168269
3501.944889	535373.720195	44.173274
3501.757866	535343.597621	44.178279
3502.277380	535336.771645	44.183284
3502.008408	535323.071548	44.188289
3501.903429	535293.791816	44.193293
3502.065382	535273.430469	44.198298
3501.851534	535258.563974	44.203303
3502.082230	535241.212103	44.208308
3501.704899	535220.833918	44.213313
3501.815639	535197.309176	44.218317
3502.186010	535165.891353	44.223322
3501.748774	535161.479350	44.228327
3501.976265	535144.429872	44.233332
3502.120043	535131.621754	44.238337
3501.985636	535108.839724	44.243341
3502.219042	535082.577451	44.248346
3501.948105	535049.245628	44.253351
3502.253419	535034.499437	44.258356
3502.067958	535006.490024	44.263361
3502.114076	534994.401699	44.268365
3501.833675	534969.527940	44.273370
3501.780448	534964.150025	44.278375
3501.941528	534928.082736	44.283380
3502.118855	534923.222648	44.288385
3501.688374	534906.174566	44.293389
3502.376571	534880.495510	44.298394
3501.598231	534857.561546	44.303399
3502.219556	534833.856010	44.308404
3502.162560	534810.709034	44.313409
3502.203534	534792.328967	44.318413
3502.385611	534771.863019	44.323418
3502.037784	534747.452373	44.328423
3502.013834	534720.172289	44.333428
3501.888365	534718.782306	44.338433
3502.033805	534700.033477	44.343437
3501.997636	534662.284604	44.348442
3501.775312	534641.680021	44.353447
3501.410755	534622.809084	44.358452
3501.685566	534625.434305	44.363457
3501.965930	534597.754230	44.368461
3501.847056	534575.321216	44.373466
3501.909311	534559.756530	44.378471
3501.792351	534541.350342	44.383476
3501.719488	534525.504601	44.388481
3501.790637	534495.641907	44.393485
3501.868442	534489.991702	44.398490
3501.866713	534480.225984	44.403495
3502.020972	534452.565221	44.408500
3501.997668	534436.208257	44.413505
3502.095948	534419.278609	44.418509
3502.456384	534392.894483	44.423514
3501.908843	534382.206817	44.428519
3502.278383	534347.212955	44.433524
3501.845562	534332.228441	44.438529
3501.726848	534307.730967	44.443533
3501.958878	534277.238643	44.448538
3501.813110	534271.069384	44.453543
3502.587411	534246.835558	44.458548
3502.138864	534232.759514	44.463553
3502.012849	534201.919999	44.468557
3502.251207	534180.588555	44.473562
3501.968802	534171.067645	44.478567
3502.130713	534141.190006	44.483572
3501.967550	534122.689727	44.488577
3502.255073	534097.272833	44.493581
3502.376597	534071.378303	44.498586
3502.258109	534046.427223	44.503591
3502.387211	534023.702952	44.508596
3502.374078	534000.094619	44.513601
3502.138077	533977.175370	44.518605
3502.375394	533951.816345	44.523610
3502.104418	533929.909298	44.528615
3502.004090	533895.692123	44.533620
3501.932510	533872.042308	44.538625
3502.275165	533864.638973	44.543629
3501.782967	533833.150764	44.548634
3501.721021	533820.776100	44.553639
3501.993104	533796.569242	44.558644
3501.927131	533789.632194	44.563649
3501.807460	533759.193376	44.568653
3501.849669	533738.344813	44.573658
3502.078679	533729.599824	44.578663
3501.860451	533697.313505	44.583668
3502.218815	533687.289779	44.588673
3501.849047	533663.132208	44.593677
3501.956071	533645.294006	44.598682
3501.693596	533623.838207	44.603687
3502.367057	533613.664705	44.608692
3502.104314	533596.236380	44.613697
3501.696198	533577.219657	44.618701
3502.356215	533554.663663	44.623706
3502.365068	533529.842800	44.628711
3502.146304	533497.757441	44.633716
3501.755592	533481.456441	44.638721
3501.812192	533467.603016	44.643725
3502.122523	533441.073715	44.648730
3502.241379	533415.278976	44.653735
3502.137560	533399.386326	44.658740
3502.291643	533372.075690	44.663745
3502.249351	533350.937585	44.668749
3502.428566	533321.357427	44.673754
3502.195260	533306.139293	44.678759
3502.038702	533280.538177	44.683764
3502.167216	533263.350587	44.688769
3501.886608	533240.638352	44.693773
3502.239467	533216.317150	44.698778
3502.101848	533195.596386	44.703783
3502.317037	533172.605499	44.708788
3502.226855	533154.746964	44.713793
3501.936437	533121.111117	44.718797
3501.990789	533108.264565	44.723802
3501.924816	533083.001381	44.728807
3502.198208	533066.646859	44.733812
3501.707480	533035.710278	44.738817
3501.739376	533028.505863	44.743821
3502.001162	533006.564691	44.748826
3502.355892	532992.462982	44.753831
3501.763645	532956.003958	44.758836
3501.744051	532946.189514	44.763841
3501.673321	532927.824178	44.768845
3501.959157	532908.396406	44.773850
3501.642911	532897.621164	44.778855
3501.628671	532878.844197	44.783860
3501.604010	532859.968133	44.788865
3502.066300	532847.158535	44.793869
3501.799589	532820.214295	44.798874
3501.629731	532807.251296	44.803879
3502.113872	532800.479845	44.808884
3501.714400	532778.137721	44.813889
3501.575146	532765.925118	44.818893
3502.082171	532736.947125	44.823898
3501.782523	532727.880952	44.828903
3501.876415	532705.764011	44.833908
3502.077247	532687.053994	44.838913
3502.242835	532665.529992	44.843917
3502.338741	532647.239023	44.848922
3501.639143	532617.794014	44.853927
3501.687394	532605.803820	44.858932
3501.259183	532599.929449	44.863937
3501.273222	532580.442786	44.868941
3501.554922	532547.471634	44.873946
3501.400756	532548.502566	44.878951
3502.066343	532536.617633	44.883956
3501.634230	532514.985001	44.888961
3501.865766	532502.059929	44.893965
3501.887458	532480.356622	44.898970
3501.542976	532469.333677	44.903975
3501.694542	532449.674373	44.908980
3501.520866	532442.602318	44.913985
3501.380705	532432.202071	44.918989
3501.812576	532416.526944	44.923994
3501.503732	532406.656407	44.928999
3501.625005	532389.116349	44.934004
3501.663605	532392.936797	44.939009
3501.694235	532366.448826	44.944013
3501.859127	532339.335727	44.949018
3501.534196	532335.459101	44.954023
3501.684974	532306.032100	44.959028
3501.705642	532297.721358	44.964033
3501.458676	532289.754349	44.969037
3501.751218	532260.405882	44.974042
3501.281117	532262.392277	44.979047
3501.445605	532243.939021	44.984052
3501.448392	532231.250672	44.989057
3501.227389	532216.734226	44.994061
3501.909482	532207.615615	44.999066
3501.462650	532205.822226	45.004071
3501.695932	532169.333222	45.009076
3501.583974	532166.228989	45.014081
3501.687264	532168.075823	45.019085
3501.949614	532130.172411	45.024090
3501.756688	532128.440198	45.029095
3501.768186	532093.093176	45.034100
3501.995676	532094.366849	45.039105
3501.668187	532080.773110	45.044109
3502.265663	532038.436879	45.049114
3501.879266	532032.706792	45.054119
3501.685729	532005.145276	45.059124
3501.703880	531996.633334	45.064129
3501.904024	531973.189518	45.069133
3501.920221	531945.897339	45.074138
3501.568363	531944.391233	45.079143
3501.393556	531916.021013	45.084148
3501.983352	531904.751502	45.089153
3501.978242	531890.402496	45.094157
3501.743244	531867.227603	45.099162
3501.720478	531863.756967	45.104167
3501.873026	531836.896493	45.109172
3501.670191	531827.059368	45.114177
3501.830744	531815.604824	45.119181
3501.942921	531794.440146	45.124186
3501.665872	531786.427158	45.129191
3501.546667	531758.551449	45.134196
3501.710248	531749.764961	45.139201
3501.919605	531741.928009	45.144205
3501.841005	531719.232022	45.149210
3501.603396	531707.386184	45.154215
3501.657338	531678.778448	45.159220
3501.976957	531665.083575	45.164225
3501.638468	531649.930213	45.169229
3501.808051	531622.160326	45.174234
3501.732915	531615.223538	45.179239
3501.739679	531605.051521	45.184244
3502.040343	531592.618304	45.189249
3501.946538	531563.680847	45.194253
3502.114267	531535.256495	45.199258
3501.749830	531530.982961	45.204263
3501.694768	531505.715010	45.209268
3501.954876	531495.855946	45.214273
3501.924660	531473.252705	45.219277
3501.984517	531458.993817	45.224282
3502.106848	531439.337537	45.229287
3501.975013	531414.031003	45.234292
3501.897068	531387.406878	45.239297
3501.591389	531370.334704	45.244301
3501.677343	531352.748393	45.249306
3501.358323	531330.945131	45.254311
3501.653523	531324.202321	45.259316
3501.930565	531311.017226	45.264321
3501.752653	531285.365145	45.269325
3501.726306	531269.860652	45.274330
3501.525996	531266.316779	45.279335
3501.677949	531244.137966	45.284340
3501.894145	531232.221077	45.289345
3501.312098	531204.164440	45.294349
3501.869965	531182.576945	45.299354
3501.980639	531186.235474	45.304359
3502.003424	531160.602269	45.309364
3501.922046	531142.588538	45.314369
3501.485429	531122.112404	45.319373
3501.908356	531094.654443	45.324378
3501.915102	531095.861860	45.329383
3501.824503	531074.475802	45.334388
3501.982286	531068.559898	45.339393
3501.686845	531051.082884	45.344397
3501.752879	531027.960360	45.349402
3501.621613	531029.441027	45.354407
3501.550516	531002.210808	45.359412
3501.647940	530992.225620	45.364417
3501.650233	530978.780823	45.369421
3501.694450	530947.806372	45.374426
3501.451756	530943.513699	45.379431
3501.499504	530929.910716	45.384436
3501.412723	530907.869190	45.389441
3501.387499	530902.334167	45.394445
3501.836790	530885.848830	45.399450
3501.027934	530875.098207	45.404455
3501.276067	530861.262554	45.409460
3501.815505	530855.589289	45.414465
3501.527069	530851.152641	45.419469
3501.672780	530823.132997	45.424474
3501.283180	530809.849718	45.429479
3501.293980	530802.949479	45.434484
3501.531984	530803.264913	45.439489
3501.660969	530781.642787	45.444493
3501.705404	530762.450800	45.449498
3501.275565	530771.178654	45.454503
3501.376979	530730.526720	45.459508
3501.706440	530725.943522	45.464513
3501.456832	530715.407869	45.469517
3501.796045	530702.665679	45.474522
3501.753251	530687.767310	45.479527
3501.634659	530662.155127	45.484532
3501.614615	530634.916197	45.489537
3501.425399	530637.110896	45.494541
3501.900149	530622.937598	45.499546
3501.666241	530614.161846	45.504551
3501.992130	530590.544915	45.509556
3501.569544	530576.914044	45.514561
3501.694469	530549.450956	45.519565
3501.843718	530539.658779	45.524570
3501.838450	530527.372868	45.529575
3501.788088	530504.922151	45.534580
3501.801608	530495.201417	45.539585
3501.675455	530470.748212	45.544589
3501.581918	530463.964742	45.549594
3501.539853	530458.079661	45.554599
3501.621487	530431.680533	45.559604
3501.639353	530422.865473	45.564609
3501.895727	530409.128773	45.569613
3501.860872	530387.078287	45.574618
3502.050492	530384.682038	45.579623
3502.058635	530355.172120	45.584628
3501.805806	530335.371134	45.589633
3502.163816	530320.812827	45.594637
3501.984151	530304.777127	45.599642
3501.969931	530282.471472	45.604647
3501.825275	530260.991780	45.609652
3501.398848	530234.973454	45.614657
3501.475278	530219.854572	45.619661
3501.839320	530210.683361	45.624666
3501.345516	530205.976309	45.629671
3501.337800	530176.770596	45.634676
3501.540578	530162.890907	45.639681
3501.383929	530167.145247	45.644685
3501.531660	530151.662694	45.649690
3501.583873	530137.856766	45.654695
3501.290648	530126.420998	45.659700
3501.782516	530109.424491	45.664705
3501.538708	530093.398513	45.669709
3501.542403	530076.276500	45.674714
3501.494782	530079.758544	45.679719
3501.737203	530048.549691	45.684724
3501.644984	530034.766129	45.689729
3501.299380	530026.863438	45.694733
3501.576078	530007.382414	45.699738
3501.462966	529990.882755	45.704743
3501.210791	529982.864783	45.709748
3501.485817	529976.325852	45.714753
3501.184119	529959.150494	45.719757
3501.696303	529932.935149	45.724762
3501.338916	529940.745839	45.729767
3501.770442	529924.010271	45.734772
3502.001131	529905.795199	45.739777
3501.359077	529907.002972	45.744781
3501.748814	529887.453821	45.749786
3501.652358	529873.418959	45.754791
3501.825926	529859.493137	45.759796
3501.974189	529827.240892	45.764801
3501.787837	529812.363865	45.769805
3501.882914	529787.874957	45.774810
3501.825151	529769.754942	45.779815
3501.907261	529702.261790	45.784820
3501.640645	529580.888096	45.789825
3501.484187	529429.431455	45.794829
3501.229686	529227.980508	45.799834
3500.451380	528969.397528	45.804839
3499.921795	528673.250699	45.809844
3499.927980	528327.405497	45.814849
3499.535545	527942.831982	45.819853
3499.002142	527498.131066	45.824858
3498.301262	527020.147454	45.829863
3498.089654	526487.720346	45.834868
3497.287780	525918.541049	45.839873
3496.486475	525301.984478	45.844877
3495.948278	524626.063681	45.849882
3495.177884	523921.528613	45.854887
3494.100418	523165.361270	45.859892
3493.238343	522372.839581	45.864897
3492.276984	521529.342854	45.869901
3491.237107	520631.734080	45.874906
3490.176561	519706.552572	45.879911
3489.069004	518733.183421	45.884916
3487.596497	517716.655972	45.889921
3485.917768	516668.479490	45.894925
3484.951612	515580.791068	45.899930
3483.759252	514450.803675	45.904935
3482.440355	513272.895178	45.909940
3481.251929	512052.207514	45.914945
3479.273072	510814.844119	45.919949
3477.669455	509522.441538	45.924954
3476.087543	508202.377733	45.929959
3474.821939	506835.179146	45.934964
3473.112317	505438.204397	45.939969
3470.659762	504012.551472	45.944973
3468.989931	502536.984548	45.949978
3467.313613	501043.908610	45.954983
3465.296688	499511.467728	45.959988
3463.671262	497938.527024	45.964993
3461.213176	496345.456850	45.969997
3459.491977	494715.549344	45.975002
3457.348355	493049.428381	45.980007
3455.440628	491357.382868	45.985012
3453.326248	489638.161162	45.990017
3451.062793	487896.140564	45.995021
3448.918255	486108.289188	46.000026
3446.531318	484301.979937	46.005031
3444.305255	482465.372655	46.010036
3441.731099	480590.553463	46.015041
3439.268973	478711.602287	46.020045
3437.042201	476797.314748	46.025050
3434.402681	474844.191776	46.030055
3431.794164	472878.896244	46.035060
3429.650068	470895.493051	46.040065
3426.925231	468879.576628	46.045069
3424.362098	466841.288246	46.050074
3421.880169	464782.000096	46.055079
3419.160009	462703.881078	46.060084
3416.348094	460603.564625	46.065089
3413.724484	458483.480737	46.070093
3410.991238	456343.822779	46.075098
3408.389906	454180.297071	46.080103
3405.443752	451991.402444	46.085108
3402.756901	449792.478624	46.090113
3399.863504	447567.243498	46.095117
3397.002004	445315.855631	46.100122
3394.060668	443062.077276	46.105127
3391.148854	440779.049431	46.110132
3388.437089	438479.756328	46.115137
3385.503812	436183.258816	46.120141
3382.269876	433839.463119	46.125146
3379.341292	431501.620443	46.130151
3376.090380	429138.919280	46.135156
3372.830466	426755.157431	46.140161
3369.700530	424358.369197	46.145165
3366.643982	421956.217635	46.150170
3363.683328	419542.920688	46.155175
3360.025650	417112.262760	46.160180
3357.384992	414669.604117	46.165185
3353.746496	412223.626905	46.170189
3350.294655	409746.300346	46.175194
3347.300654	407273.240399	46.180199
3343.624122	404779.260783	46.185204
3340.818890	402282.942529	46.190209
3336.800110	399775.579938	46.195213
3333.698309	397258.161425	46.200218
3330.386181	394728.325257	46.205223
3326.923958	392194.641517	46.210228
3323.751292	389654.734614	46.215233
3320.055714	387100.888346	46.220237
3316.881767	384532.533812	46.225242
3313.162143	381961.822455	46.230247
3309.811004	379391.739200	46.235252
3306.404864	376794.137334	46.240257
3302.788012	374196.317435	46.245261
3299.333542	371596.422169	46.250266
3296.119395	368991.064354	46.255271
3292.633552	366371.510211	46.260276
3288.914083	363746.190425	46.265281
3285.261891	361124.234839	46.270285
3281.743556	358485.764626	46.275290
3277.832407	355851.449239	46.280295
3274.257158	353208.725852	46.285300
3270.430342	350561.323516	46.290305
3266.576291	347920.701775	46.295309
3262.833563	345258.954542	46.300314
3259.489731	342615.219026	46.305319
3255.760568	339951.178245	46.310324
3252.021946	337297.569887	46.315329
3248.616778	334641.199120	46.320333
3244.540474	331972.485142	46.325338
3240.966281	329310.451384	46.330343
3237.454658	326655.045114	46.335348
3233.411581	323970.266780	46.340353
3229.645118	321297.915806	46.345357
3225.971843	318631.947142	46.350362
3221.890116	315959.875512	46.355367
3217.939356	313291.824101	46.360372
3214.321040	310622.041452	46.365377
3209.865733	307952.240834	46.370381
3206.035634	305291.004855	46.375386
3202.659720	302632.741542	46.380391
3198.670301	299977.902105	46.385396
3194.887746	297318.957117	46.390401
3190.318134	294663.981574	46.395405
3186.547440	292012.301061	46.400410
3182.859572	289371.999918	46.405415
3178.967648	286727.217812	46.410420
3175.210781	284081.673825	46.415425
3170.960665	281453.571830	46.420429
3166.773888	278820.986644	46.425434
3163.008043	276197.615646	46.430439
3158.970797	273571.273805	46.435444
3155.048284	270951.708332	46.440449
3151.084011	268352.342351	46.445453
3147.138641	265738.057441	46.450458
3142.865811	263126.761468	46.455463
3138.689820	260538.001267	46.460468
3134.607020	257944.229160	46.465473
3130.455368	255367.400838	46.470477
3126.727654	252795.322599	46.475482
3122.586329	250237.526598	46.480487
3118.514401	247684.850531	46.485492
3114.794555	245132.568607	46.490497
3110.681484	242592.159702	46.495501
3106.598286	240052.330806	46.500506
3102.483736	237528.453060	46.505511
3098.073332	235004.603001	46.510516
3094.259852	232484.975350	46.515521
3090.288356	229991.747727	46.520525
3086.248024	227484.108875	46.525530
3081.809785	225004.825406	46.530535
3077.231708	222528.722973	46.535540
3073.132926	220070.022491	46.540545
3068.745977	217625.663276	46.545549
3064.577223	215185.586185	46.550554
3060.616915	212769.254183	46.555559
3056.266879	210354.580393	46.560564
3052.395592	207945.202344	46.565569
3048.025891	205569.519155	46.570573
3043.679362	203177.357276	46.575578
3039.693903	200816.062426	46.580583
3035.242320	198459.636388	46.585588
3030.818750	196119.694301	46.590593
3026.268852	193800.362522	46.595597
3022.379407	191495.179703	46.600602
3017.786337	189201.839290	46.605607
3013.385820	186938.716683	46.610612
3008.792622	184671.445690	46.615617
3004.639891	182438.813262	46.620621
3000.038380	180213.967731	46.625626
2995.226307	178014.697550	46.630631
2990.817700	175820.487878	46.635636
2986.057701	173658.612121	46.640641
2981.570647	171524.428392	46.645645
2976.316679	169409.862539	46.650650
2971.742191	167314.575564	46.655655
2966.983630	165256.306378	46.660660
2962.099789	163215.786507	46.665665
2956.737287	161209.172377	46.670669
2951.893788	159233.876574	46.675674
2946.771534	157285.847618	46.680679
2941.557301	155386.436698	46.685684
2935.762971	153503.900725	46.690689
2930.120880	151608.639628	46.695693
2924.344268	149821.059192	46.700698
2918.293543	148082.941663	46.705703
2911.659052	146411.013799	46.710708
2904.937700	144792.443274	46.715713
2897.938999	143246.494277	46.720717
2891.161994	141746.363869	46.725722
2884.865311	140314.693828	46.730727
2877.921033	138951.870582	46.735732
2871.770057	137631.392749	46.740737
2866.122842	136376.647385	46.745741
2860.040315	135183.501217	46.750746
2854.274750	134034.925954	46.755751
2849.155003	132935.574173	46.760756
2844.286665	131869.183105	46.765761
2838.885646	130846.150818	46.770765
2834.125355	129874.547318	46.775770
2829.553708	128915.325881	46.780775
2825.019767	128012.175912	46.785780
2821.055997	127117.122623	46.790785
2816.480258	126255.406267	46.795789
2812.385533	125414.911823	46.800794
2808.194132	124599.340104	46.805799
2804.061807	123813.562062	46.810804
2800.173740	123019.202187	46.815809
2796.183259	122263.841632	46.820813
2792.079651	121528.937657	46.825818
2788.285176	120795.589070	46.830823
2784.565488	120084.891920	46.835828
2780.978628	119380.698262	46.840833
2776.941708	118692.114652	46.845837
2773.216598	118008.365387	46.850842
2769.363617	117337.199301	46.855847
2765.252490	116680.225569	46.860852
2761.341191	116030.442152	46.865857
2757.395789	115403.843165	46.870861
2753.422490	114779.331768	46.875866
2749.848824	114177.694197	46.880871
2745.554883	113569.198146	46.885876
2742.403685	112982.225771	46.890881
2738.597018	112395.212374	46.895885
2734.593272	111815.015970	46.900890
2730.702377	111246.470261	46.905895
2726.921732	110693.897865	46.910900
2723.333803	110148.728920	46.915905
2719.619622	109606.868155	46.920909
2716.089007	109059.418778	46.925914
2712.340061	108520.478909	46.930919
2708.665254	107999.333963	46.935924
2705.322233	107453.253733	46.940929
2701.805103	106941.914464	46.945933
2698.561895	106411.014058	46.950938
2695.016958	105886.919022	46.955943
2691.322133	105377.817368	46.960948
2688.559046	104846.002322	46.965953
2684.664606	104335.955956	46.970957
2681.403331	103810.514354	46.975962
2678.072682	103296.252223	46.980967
2674.886806	102771.374589	46.985972
2671.691123	102242.769853	46.990977
2668.168194	101720.834018	46.995981
2664.932039	101190.892480	47.000986
2661.258579	100660.214152	47.005991
2657.695249	100134.357128	47.010996
2654.799402	99604.185147	47.016001
2651.285770	99075.579623	47.021005
2647.820317	98543.670892	47.026010
2644.634348	98012.197760	47.031015
2641.061958	97479.039815	47.036020
2637.996480	96943.892950	47.041025
2634.232608	96402.306286	47.046029
2630.627439	95855.214310	47.051034
2627.341810	95316.977778	47.056039
2624.006623	94785.061321	47.061044
2620.547219	94239.461849	47.066049
2617.594017	93694.047384	47.071053
2613.870246	93153.832642	47.076058
2610.443492	92588.459689	47.081063
2607.052405	92023.078956	47.086068
2603.753703	91477.961099	47.091073
2600.364956	90917.695890	47.096077
2596.608630	90359.925141	47.101082
2593.355077	89803.890732	47.106087
2589.673478	89252.354789	47.111092
2586.341866	88692.935474	47.116097
2583.097816	88131.277013	47.121101
2579.482413	87565.824788	47.126106
2576.295382	86997.153357	47.131111
2572.678571	86435.648835	47.136116
2569.400118	85866.886595	47.141121
2565.807515	85291.959544	47.146125
2562.138775	84724.474627	47.151130
2558.759098	84147.593611	47.156135
2555.256372	83576.485108	47.161140
2551.838300	82996.787796	47.166145
2548.292115	82440.812387	47.171149
2544.602379	81867.404647	47.176154
2541.773037	81287.637994	47.181159
2538.153782	80701.121899	47.186164
2534.791108	80127.571752	47.191169
2531.490135	79547.914534	47.196173
2527.533611	78961.957474	47.201178
2524.172648	78374.523081	47.206183
2520.747732	77796.649158	47.211188
2517.259472	77191.542837	47.216193
2513.886718	76621.559672	47.221197
2510.242181	76028.555634	47.226202
2507.242576	75447.160248	47.231207
2502.908761	74853.133619	47.236212
2499.986688	74257.935317	47.241217
2496.755932	73680.550710	47.246221
2493.120544	73081.641980	47.251226
2489.558492	72478.519644	47.256231
2485.933594	71894.060900	47.261236
2482.406323	71293.677494	47.266241
2478.882660	70690.552004	47.271245
2475.620716	70103.403916	47.276250
2472.082778	69500.022478	47.281255
2468.471098	68903.700209	47.286260
2465.370767	68293.473644	47.291265
2461.979609	67707.548948	47.296269
2458.242461	67091.425987	47.301274
2455.005318	66493.590617	47.306279
2451.237838	65893.738160	47.311284
2447.966699	65288.230791	47.316289
2444.380085	64686.106524	47.321293
2440.757544	64075.294351	47.326298
2437.657512	63470.629179	47.331303
2433.714806	62856.278965	47.336308
2430.569550	62244.275879	47.341313
2426.931814	61628.836033	47.346317
2423.489317	61025.571982	47.351322
2419.709817	60415.921358	47.356327
2416.480403	59802.703774	47.361332
2412.919886	59191.260090	47.366337
2409.437899	58587.269122	47.371341
2406.311641	57965.007812	47.376346
2402.824266	57359.906178	47.381351
2398.956567	56740.590077	47.386356
2395.911133	56114.906039	47.391361
2392.234085	55501.848321	47.396365
2388.840901	54889.307854	47.401370
2385.216476	54259.321592	47.406375
2381.822294	53640.367803	47.411380
2378.703797	53010.919836	47.416385
2375.122910	52405.273877	47.421389
2371.799478	51773.987935	47.426394
2368.088307	51142.995139	47.431399
2364.676915	50510.976968	47.436404
2361.049895	49889.317217	47.441409
2357.671026	49261.026287	47.446413
2353.834934	48631.142892	47.451418
2350.546288	47991.772909	47.456423
2346.704923	47377.071096	47.461428
2343.563490	46732.722137	47.466433
2339.706879	46110.655683	47.471437
2336.133200	45490.832781	47.476442
2332.965818	44864.070318	47.481447
2329.330346	44235.007505	47.486452
2325.795963	43603.765291	47.491457
2322.173710	42970.227483	47.496461
2318.605921	42346.686410	47.501466
2315.527643	41723.974503	47.506471
2311.945639	41096.184670	47.511476
2308.354202	40456.189906	47.516481
2304.571358	39831.130653	47.521485
2300.995269	39202.779366	47.526490
2298.050006	38565.186964	47.531495
2294.158577	37945.771765	47.536500
2291.082208	37314.887102	47.541505
2287.243863	36683.657784	47.546509
2283.740938	36061.802222	47.551514
2280.451741	35439.113820	47.556519
2276.819720	34806.564146	47.561524
2273.107916	34172.499179	47.566529
2269.681313	33544.170502	47.571533
2265.872309	32917.574393	47.576538
2262.301089	32285.357204	47.581543
2258.787922	31662.853351	47.586548
2254.837354	31038.154636	47.591553
2251.509709	30417.585865	47.596557
2247.507830	29801.354932	47.601562
2244.191281	29189.199234	47.606567
2240.280076	28580.874077	47.611572
2236.816673	27965.431877	47.616577
2232.828541	27364.815954	47.621581
2229.265526	26767.326103	47.626586
2225.654900	26164.671957	47.631591
2221.877126	25576.254323	47.636596
2217.862414	24995.652061	47.641601
2213.614052	24424.986462	47.646605
2209.267540	23861.042590	47.651610
2205.284470	23302.620415	47.656615
2200.583655	22771.369993	47.661620
2197.142828	22237.492419	47.666625
2192.959111	21719.569001	47.671629
2188.661699	21206.978887	47.676634
2185.242887	20691.896303	47.681639
2181.458922	20208.485581	47.686644
2177.588291	19717.917402	47.691649
2173.784190	19239.132287	47.696653
2169.904821	18760.725323	47.701658
2166.448179	18281.276279	47.706663
2162.209657	17810.656605	47.711668
2159.101086	17345.293829	47.716673
2155.390197	16884.849195	47.721677
2151.384655	16439.945641	47.726682
2148.024013	15993.546109	47.731687
2143.985410	15566.998420	47.736692
2140.608500	15111.388818	47.741697
2136.740022	14692.692875	47.746701
2132.782683	14268.241720	47.751706
2129.779460	13850.857542	47.756711
2125.914519	13435.490917	47.761716
2122.083648	13029.227016	47.766721
2118.235620	12631.880123	47.771725
2114.471058	12239.682545	47.776730
2110.374523	11850.739033	47.781735
2106.098282	11483.177744	47.786740
2102.224952	11117.156423	47.791745
2098.218847	10766.550723	47.796749
2094.255402	10411.332812	47.801754
2090.432900	10074.899314	47.806759
2086.407936	9752.108255	47.811764
2082.820101	9423.807216	47.816769
2078.805185	9113.709189	47.821773
2075.037428	8808.677070	47.826778
2071.730615	8498.931750	47.831783
2068.070432	8206.331977	47.836788
2064.215977	7909.291649	47.841793
2060.625354	7627.650898	47.846797
2056.732964	7337.936907	47.851802
2052.912192	7058.831518	47.856807
2049.464356	6788.151062	47.861812
2046.020529	6517.366370	47.866817
2042.137632	6242.147346	47.871821
2038.599804	5989.060476	47.876826
2035.028546	5721.579743	47.881831
2031.412457	5468.999624	47.886836
2028.172706	5205.395879	47.891841
2024.443503	4964.593738	47.896845
2021.277737	4710.811641	47.901850
2017.837309	4466.252840	47.906855
2014.124034	4213.464783	47.911860
2010.770533	3973.633103	47.916865
2007.238442	3722.323628	47.921869
2003.723602	3485.979000	47.926874
2000.852816	3238.465439	47.931879
1996.811986	3001.304038	47.936884
1993.222434	2750.292327	47.941889
1989.779804	2510.686971	47.946893
1986.057734	2282.174181	47.951898
1982.412323	2040.271550	47.956903
1978.842522	1814.765859	47.961908
1975.673675	1589.827072	47.966913
1971.970347	1360.715629	47.971917
1968.052769	1132.251101	47.976922
1964.802865	911.389586	47.981927
1960.714724	690.265786	47.986932
1957.132992	481.186376	47.991937
1953.202836	278.032405	47.996941
1948.193659	108.046254	48.001946
1937.593341	97.797278	48.006951
1928.264158	113.780176	48.011956
1922.634192	113.602869	48.016961
1918.925511	106.985763	48.021965
1916.101162	114.743004	48.026970
1914.595608	105.464008	48.031975
1912.433638	109.407116	48.036980
1909.699929	113.436044	48.041985
1906.622499	110.621560	48.046989
1903.210505	118.153889	48.051994
1900.147423	115.818057	48.056999
1896.891923	116.422795	48.062004
1893.313186	110.383410	48.067009
1890.250948	107.515944	48.072013
1886.897073	109.651414	48.077018
1883.477493	107.475472	48.082023
1879.529250	112.468537	48.087028
1876.054679	110.212569	48.092033
1873.561392	111.885075	48.097037
1869.924265	113.558435	48.102042
1866.896729	110.312251	48.107047
1863.051113	110.505804	48.112052
1859.242009	107.454028	48.117057
1855.750500	105.146916	48.122061
1852.874578	111.355634	48.127066
1849.534422	106.712289	48.132071
1846.185845	103.449636	48.137076
1843.152130	112.384727	48.142081
1839.276333	108.508111	48.147085
1835.657054	110.276771	48.152090
1832.722250	109.819212	48.157095
1829.231261	101.738241	48.162100
1825.362602	105.725514	48.167105
1822.092402	101.732503	48.172109
1818.857727	99.872635	48.177114
1815.171808	100.278615	48.182119
1811.239712	108.853659	48.187124
1807.899141	104.643813	48.192129
1804.530485	104.389820	48.197133
1800.860325	106.647286	48.202138
1798.107443	107.401592	48.207143
1794.366577	108.607055	48.212148
1791.077784	109.046142	48.217153
1787.928445	109.561599	48.222157
1784.060524	106.256398	48.227162
1780.831411	103.965402	48.232167
1777.085822	106.588946	48.237172
1773.563322	107.190956	48.242177
1769.891274	108.259162	48.247181
1766.692623	107.308004	48.252186
1763.418676	98.383354	48.257191
1759.559773	108.645921	48.262196
1755.886826	97.309347	48.267201
1752.872891	96.541412	48.272205
1749.189076	108.042213	48.277210
1746.052011	106.027955	48.282215
1742.219494	107.390055	48.287220
1739.032159	105.405768	48.292225
1735.468255	101.920381	48.297229
1732.004463	107.546725	48.302234
1728.849898	100.419469	48.307239
1724.681951	106.753349	48.312244
1721.353997	102.566861	48.317249
1718.140302	101.209931	48.322253
1714.393072	100.730133	48.327258
1711.432730	93.389159	48.332263
1707.359095	98.945904	48.337268
1703.951562	98.878302	48.342273
1700.322003	96.953357	48.347277
1697.188544	93.524367	48.352282
1693.873226	96.928822	48.357287
1689.986377	89.599179	48.362292
1686.518357	103.901074	48.367297
1683.129320	103.827431	48.372301
1679.212565	96.214544	48.377306
1676.067009	96.441523	48.382311
1673.125901	100.129418	48.387316
1669.479047	98.868384	48.392321
1665.665942	102.691999	48.397325
1661.882705	105.254972	48.402330
1658.621637	106.287695	48.407335
1654.906133	100.677754	48.412340
1651.631554	91.794351	48.417345
1648.601032	99.574184	48.422349
1645.178857	96.588763	48.427354
1641.673706	89.433834	48.432359
1637.968701	97.135149	48.437364
1634.249024	94.996451	48.442369
1630.974176	98.970407	48.447373
1627.241021	102.870164	48.452378
1624.064339	89.162692	48.457383
1620.319539	94.136758	48.462388
1616.814279	87.608265	48.467393
1613.478963	95.131820	48.472397
1609.844816	97.775994	48.477402
1606.540929	91.912175	48.482407
1602.754208	94.099213	48.487412
1599.497069	98.643045	48.492417
1595.901989	91.033891	48.497421
1592.133819	101.864455	48.502426
1588.916671	93.282167	48.507431
1585.278864	96.335031	48.512436
1582.029902	91.123882	48.517441
1578.444773	86.249790	48.522445
1575.096878	93.819595	48.527450
1571.348472	92.659798	48.532455
1567.716802	99.175967	48.537460
1564.513213	95.767397	48.542465
1561.345802	88.775046	48.547469
1557.334250	87.928287	48.552474
1554.037710	83.736935	48.557479
1550.570544	91.379086	48.562484
1546.727860	95.691358	48.567489
1543.510032	87.295845	48.572493
1539.903032	96.408740	48.577498
1536.486336	89.955058	48.582503
1532.931532	89.065684	48.587508
1529.431625	91.214414	48.592513
1526.123993	95.418100	48.597517
1522.334889	102.730720	48.602522
1519.008068	96.747097	48.607527
1515.553118	95.383445	48.612532
1511.870558	92.511333	48.617537
1508.597041	89.499627	48.622541
1505.078655	100.503282	48.627546
1501.608765	89.764736	48.632551
1498.018370	91.747221	48.637556
1494.040447	96.055237	48.642561
1490.874947	84.820073	48.647565
1487.569610	96.467598	48.652570
1483.759013	86.446465	48.657575
1480.660807	93.774933	48.662580
1477.298789	92.615117	48.667585
1474.024084	86.174146	48.672589
1469.940173	87.100842	48.677594
1466.424810	86.471087	48.682599
1462.960935	93.502136	48.687604
1459.511076	90.748832	48.692609
1455.931984	82.817683	48.697613
1452.385395	87.276859	48.702618
1448.809032	90.111364	48.707623
1445.629272	95.842202	48.712628
1442.216297	83.788203	48.717633
1439.043780	85.598086	48.722637
1435.240903	96.041752	48.727642
1431.507077	85.496160	48.732647
1427.543781	83.844653	48.737652
1424.114160	83.672949	48.742657
1420.879602	83.663871	48.747661
1417.855630	88.142944	48.752666
1414.697381	83.319490	48.757671
1410.883587	81.540314	48.762676
1406.825762	87.186361	48.767681
1403.551066	79.527377	48.772685
1399.479336	87.380687	48.777690
1396.813761	88.630786	48.782695
1393.357866	95.859909	48.787700
1389.858882	86.245865	48.792705
1385.866309	89.955065	48.797709
1382.258088	92.800861	48.802714
1379.091865	91.648545	48.807719
1375.336689	91.331369	48.812724
1371.991372	91.725505	48.817729
1368.737304	90.526753	48.822733
1364.866470	90.629370	48.827738
1361.300745	86.891221	48.832743
1358.148474	95.158235	48.837748
1354.333365	85.172631	48.842753
1351.796214	86.608384	48.847757
1347.645316	89.177988	48.852762
1344.141452	86.575472	48.857767
1340.501580	83.873906	48.862772
1336.931479	87.150363	48.867777
1333.602316	87.124380	48.872781
1330.214017	91.153974	48.877786
1326.696188	82.567916	48.882791
1323.025212	87.476725	48.887796
1319.303120	86.467883	48.892801
1315.800585	88.651840	48.897805
1312.518009	92.339118	48.902810
1309.041242	82.044602	48.907815
1305.759285	86.437288	48.912820
1301.918207	95.412619	48.917825
1298.474416	85.093989	48.922829
1294.956169	93.968451	48.927834
1291.489286	95.561577	48.932839
1288.221245	92.526898	48.937844
1284.676179	91.126680	48.942849
1280.909908	82.402134	48.947853
1276.913733	100.595314	48.952858
1274.338933	89.973750	48.957863
1270.695820	96.678371	48.962868
1267.017283	86.377302	48.967873
1263.433383	93.085361	48.972877
1260.169802	95.402969	48.977882
1256.678819	94.630239	48.982887
1252.876415	93.225788	48.987892
1249.510841	94.164082	48.992897
1246.131017	96.113814	48.997901
1242.017980	87.636232	49.002906
1239.127706	94.786811	49.007911
1235.514905	86.111149	49.012916
1231.872997	92.223972	49.017921
1228.675804	86.103161	49.022925
1225.024545	89.173964	49.027930
1221.701527	83.104378	49.032935
1217.939230	86.875823	49.037940
1214.322192	83.547471	49.042945
1211.099276	81.995881	49.047949
1207.655254	83.841715	49.052954
1203.946351	87.838963	49.057959
1200.377608	86.290584	49.062964
1196.948855	91.158535	49.067969
1193.536679	88.424710	49.072973
1189.921094	82.631617	49.077978
1186.735385	79.005183	49.082983
1182.822166	78.972052	49.087988
1179.284241	79.468953	49.092993
1175.863042	86.325692	49.097997
1172.500959	88.006917	49.103002
1169.099171	76.960456	49.108007
1165.725208	75.900610	49.113012
1161.834942	86.810287	49.118017
1158.679672	86.124516	49.123021
1154.880668	83.318033	49.128026
1151.696983	86.660904	49.133031
1148.199296	89.666682	49.138036
1144.419887	78.666349	49.143041
1140.806348	81.310515	49.148045
1136.963755	84.461726	49.153050
1133.811385	88.233151	49.158055
1130.526815	80.237233	49.163060
1126.980300	89.400831	49.168065
1123.494148	83.979900	49.173069
1119.924707	89.249397	49.178074
1116.209927	82.785236	49.183079
1112.804132	83.802568	49.188084
1109.449062	89.930859	49.193089
1106.188945	85.534584	49.198093
1102.440846	86.744401	49.203098
1099.039129	87.397275	49.208103
1095.841097	90.166592	49.213108
1091.944812	86.065492	49.218113
1088.370824	73.963871	49.223117
1084.816298	83.821562	49.228122
1081.454027	89.337220	49.233127
1077.729551	95.064280	49.238132
1074.055927	97.894974	49.243137
1071.092336	87.137815	49.248141
1067.577847	94.221051	49.253146
1063.809020	86.189791	49.258151
1060.195031	86.154389	49.263156
1056.487777	95.273411	49.268161
1053.405297	84.563237	49.273165
1049.846784	92.425265	49.278170
1046.247498	86.746715	49.283175
1043.165885	89.263801	49.288180
1039.338757	88.464328	49.293185
1036.068637	86.094382	49.298189
1032.676091	90.460008	49.303194
1028.798281	86.745176	49.308199
1025.057712	87.833609	49.313204
1021.628122	85.675146	49.318209
1018.298680	85.361344	49.323213
1014.864076	84.845617	49.328218
1011.669157	86.643202	49.333223
1008.278010	87.310259	49.338228
1004.496944	92.195100	49.343233
1000.847046	87.717146	49.348237
997.336020	84.726657	49.353242
993.979062	85.549741	49.358247
990.690075	79.319875	49.363252
987.025910	90.526551	49.368257
983.234431	85.596086	49.373261
979.359775	86.955328	49.378266
976.168805	90.166472	49.383271
972.833802	84.393013	49.388276
968.972713	91.318237	49.393281
965.991221	78.982045	49.398285
962.197074	85.782955	49.403290
958.750445	84.968556	49.408295
955.400007	85.667245	49.413300
951.586629	91.715030	49.418305
948.697756	82.401564	49.423309
945.178390	86.720499	49.428314
941.351882	82.383941	49.433319
937.498168	84.812418	49.438324
934.071618	89.468076	49.443329
930.797366	78.123407	49.448333
926.904083	91.207016	49.453338
923.782708	81.325482	49.458343
920.313674	80.141261	49.463348
916.671457	85.324026	49.468353
913.657655	79.753674	49.473357
910.242306	92.959037	49.478362
906.464359	81.521937	49.483367
903.011336	84.650494	49.488372
899.260085	81.656286	49.493377
895.750835	80.823169	49.498381
891.643379	84.091562	49.503386
888.375663	93.781235	49.508391
885.322216	83.984044	49.513396
881.724484	86.268278	49.518401
878.179470	80.097266	49.523405
874.894042	86.050217	49.528410
871.728524	81.712016	49.533415
868.006702	87.321620	49.538420
864.040763	81.583120	49.543425
860.614494	72.695006	49.548429
857.134345	84.312790	49.553434
854.050060	80.765522	49.558439
850.417704	76.382939	49.563444
846.653041	78.085735	49.568449
843.406549	73.912001	49.573453
839.566043	79.948195	49.578458
836.065750	77.930475	49.583463
832.596603	85.183827	49.588468
828.905741	80.250382	49.593473
825.696112	76.513828	49.598477
822.116335	75.590462	49.603482
818.451687	80.583741	49.608487
815.335936	81.780575	49.613492
811.727156	79.422249	49.618497
808.414628	83.667870	49.623501
804.677802	84.208429	49.628506
801.522622	72.614306	49.633511
798.084195	66.958219	49.638516
794.198105	78.133002	49.643521
790.938008	71.038153	49.648525
786.738655	76.111505	49.653530
783.158822	71.537265	49.658535
780.180325	72.532407	49.663540
776.468140	78.200625	49.668545
773.652300	80.192316	49.673549
769.642882	79.123872	49.678554
766.153045	80.163813	49.683559
762.648205	73.904314	49.688564
758.790049	82.214786	49.693569
755.819487	74.954650	49.698573
752.065068	76.089562	49.703578
748.667208	75.754805	49.708583
745.433169	76.970060	49.713588
741.400286	72.997850	49.718593
738.322773	72.179803	49.723597
734.591966	81.381591	49.728602
731.167886	74.511590	49.733607
727.865359	77.566115	49.738612
724.311547	82.858516	49.743617
720.812501	73.583135	49.748621
717.049169	78.816405	49.753626
713.287312	73.068313	49.758631
709.968369	67.618262	49.763636
706.124685	76.125793	49.768641
703.351795	72.916043	49.773645
699.455354	78.603459	49.778650
695.857742	79.834189	49.783655
692.588974	80.624595	49.788660
689.309153	88.145871	49.793665
685.661419	69.579770	49.798669
682.316226	79.711762	49.803674
678.814129	73.723928	49.808679
675.148200	71.937654	49.813684
671.371865	73.949164	49.818689
668.195030	77.224567	49.823693
664.518149	80.966947	49.828698
660.917753	81.081335	49.833703
657.559149	66.197051	49.838708
653.932955	81.181578	49.843713
650.814083	71.638227	49.848717
647.322338	78.736923	49.853722
643.453841	73.517960	49.858727
639.823139	69.230067	49.863732
636.404558	80.863578	49.868737
633.158112	76.376665	49.873741
629.567676	74.477408	49.878746
625.817927	78.794269	49.883751
622.116701	65.092765	49.888756
618.863853	78.608171	49.893761
616.126728	77.028484	49.898765
612.338465	77.422055	49.903770
608.687886	71.903427	49.908775
605.102899	75.900419	49.913780
601.126247	76.513139	49.918785
598.136977	73.789492	49.923789
594.405318	76.860215	49.928794
590.816633	79.317074	49.933799
587.743746	74.787331	49.938804
584.250097	79.757173	49.943809
580.691107	74.338183	49.948813
576.798479	82.385121	49.953818
573.401796	74.106211	49.958823
569.716459	70.136875	49.963828
566.330462	78.766151	49.968833
562.883690	74.329417	49.973837
559.382098	81.666927	49.978842
555.735389	83.477943	49.983847
552.637889	67.170510	49.988852
549.234016	81.196635	49.993857
545.933083	75.104743	49.998861
541.762415	71.865847	50.003866
538.402969	82.066501	50.008871
535.410526	73.411466	50.013876
531.291808	71.350861	50.018881
528.014792	76.679279	50.023885
524.460008	74.764996	50.028890
521.054357	68.183226	50.033895
517.411769	75.419303	50.038900
513.551543	67.778869	50.043905
510.147464	67.669731	50.048909
506.539562	71.885429	50.053914
503.781610	77.275408	50.058919
500.269785	75.601208	50.063924
496.527092	80.173241	50.068929
492.974730	73.911698	50.073933
489.107824	85.747884	50.078938
485.707424	81.275469	50.083943
482.286025	73.595196	50.088948
478.988985	78.075707	50.093953
475.238765	76.391168	50.098957
471.788308	68.126980	50.103962
468.424027	64.183610	50.108967
464.813952	64.612735	50.113972
461.757516	71.928403	50.118977
458.192802	69.079230	50.123981
454.331955	70.379442	50.128986
450.950401	74.091684	50.133991
447.319040	73.711061	50.138996
443.631932	72.643110	50.144001
440.608993	63.875789	50.149005
436.638482	66.373124	50.154010
433.200185	64.140173	50.159015
429.640841	73.492447	50.164020
426.342161	68.418931	50.169025
423.220880	63.827150	50.174029
419.151649	74.647655	50.179034
415.616664	71.221236	50.184039
412.447002	67.108374	50.189044
408.669612	77.003948	50.194049
405.298847	67.585282	50.199053
401.681748	76.873786	50.204058
398.162327	69.145519	50.209063
394.966868	65.878213	50.214068
391.052680	78.025471	50.219073
387.731993	72.537782	50.224077
384.525539	74.428970	50.229082
380.352807	68.226067	50.234087
377.169837	67.184042	50.239092
373.677495	73.590004	50.244097
370.709110	72.729702	50.249101
366.934384	75.686936	50.254106
363.310227	81.189631	50.259111
359.851489	76.479554	50.264116
356.073872	88.001298	50.269121
352.557636	75.330886	50.274125
349.000140	84.777793	50.279130
345.471303	73.526671	50.284135
342.597409	77.289601	50.289140
339.058577	81.108597	50.294145
335.583537	68.222979	50.299149
331.943597	74.905017	50.304154
328.309653	66.296112	50.309159
324.845162	67.253069	50.314164
321.073199	74.613704	50.319169
317.546469	70.246407	50.324173
314.181308	78.736415	50.329178
310.777693	70.253001	50.334183
307.432764	75.209204	50.339188
303.368629	65.420795	50.344193
300.249077	67.311117	50.349197
296.607460	70.940479	50.354202
292.909424	77.030469	50.359207
289.992845	72.653604	50.364212
286.149046	67.747234	50.369217
282.730302	67.542336	50.374221
279.486152	71.457824	50.379226
275.667059	69.053233	50.384231
272.039009	67.280108	50.389236
268.879556	71.233029	50.394241
265.569353	65.892423	50.399245
261.423670	71.406718	50.404250
257.990879	78.496263	50.409255
254.717712	68.967524	50.414260
250.772219	87.342601	50.419265
247.835407	74.493425	50.424269
244.601350	75.692920	50.429274
240.786172	66.827520	50.434279
237.559864	73.571715	50.439284
233.489265	67.406726	50.444289
230.048310	58.989258	50.449293
226.318016	73.562894	50.454298
222.971643	67.794505	50.459303
219.734666	69.225404	50.464308
216.240315	73.062796	50.469313
212.521824	72.281332	50.474317
208.789129	68.091650	50.479322
205.560909	70.071666	50.484327
202.333012	68.293198	50.489332
198.617329	75.300243	50.494337
195.129404	74.767615	50.499341
191.679783	71.960677	50.504346
188.064396	73.096164	50.509351
184.921810	65.777496	50.514356
181.337303	77.035066	50.519361
177.504955	67.900279	50.524365
173.848747	67.782985	50.529370
170.324592	68.331648	50.534375
167.127501	56.725218	50.539380
163.531220	73.318554	50.544385
159.845048	71.253947	50.549389
156.497687	69.544704	50.554394
153.131553	79.765397	50.559399
149.620790	71.437899	50.564404
145.929564	72.079014	50.569409
142.273303	69.399166	50.574413
138.964588	59.834864	50.579418
135.565417	64.910255	50.584423
132.159233	68.692800	50.589428
128.833456	72.586211	50.594433
125.217559	72.586032	50.599437
121.605462	71.553907	50.604442
117.691441	65.193728	50.609447
114.809822	63.060814	50.614452
111.167484	78.307278	50.619457
107.624120	74.537376	50.624461
104.012303	74.460637	50.629466
100.106259	77.944536	50.634471
97.371925	71.166581	50.639476
93.628310	73.970313	50.644481
90.119813	66.705469	50.649485
86.392610	69.120680	50.654490
82.808536	77.372709	50.659495
79.630349	67.300890	50.664500
75.893145	67.616989	50.669505
72.586937	65.819097	50.674509
69.386787	66.573585	50.679514
65.222690	67.370590	50.684519
61.922548	68.811343	50.689524
58.256117	66.079312	50.694529
55.105601	61.488980	50.699533
51.738353	64.607431	50.704538
48.035058	67.411218	50.709543
44.555158	61.622526	50.714548
40.605616	64.287489	50.719553
37.400634	57.981448	50.724557
33.899896	59.965948	50.729562
30.262871	62.066578	50.734567
27.285144	67.041563	50.739572
23.398211	69.054557	50.744577
19.896745	67.647731	50.749581
16.350655	68.832563	50.754586
12.714679	64.782880	50.759591
9.293233	51.145554	50.764596
5.880201	61.300782	50.769601
2.538242	64.845559	50.774605