Fri Aug 26 14:23:47 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.001129	93.982062	0.000000
0.363978	91.464205	0.005005
0.247207	90.191579	0.010010
-0.043054	82.144086	0.015014
0.044814	72.917788	0.020019
-0.316458	65.260999	0.025024
-0.824005	55.966067	0.030029
-0.772704	48.738579	0.035034
-0.890668	45.783077	0.040038
-1.109644	27.369863	0.045043
-1.219838	38.228834	0.050048
-1.938011	21.658670	0.055053
-2.320542	17.959778	0.060058
-2.784373	8.449263	0.065062
-2.736243	5.847545	0.070067
-3.132455	8.516050	0.075072
-3.542887	4.059066	0.080077
-4.032139	2.543893	0.085082
-3.978686	-4.490925	0.090086
-3.859126	-6.825362	0.095091
-4.668150	-6.012919	0.100096
-4.754916	-14.152160	0.105101
-5.346693	-5.587807	0.110106
-5.704604	-6.019315	0.115110
-5.336685	-19.556928	0.120115
-5.928305	-9.375978	0.125120
-6.105238	-18.228818	0.130125
-6.437714	-22.391059	0.135130
-6.513394	-18.418424	0.140134
-6.656288	-27.643541	0.145139
-7.153600	-18.806010	0.150144
-7.618977	-12.346183	0.155149
-7.523192	-15.771538	0.160154
-8.008561	-7.676155	0.165158
-7.705419	-15.509119	0.170163
-8.602482	-16.634939	0.175168
-8.734689	-15.092673	0.180173
-9.368227	-11.257798	0.185178
-9.815239	-17.303560	0.190182
-9.508536	-15.981485	0.195187
-9.411256	-15.971354	0.200192
-9.675148	-22.520171	0.205197
-9.879454	-17.973871	0.210202
-10.421815	-18.224805	0.215206
-10.707542	-16.668127	0.220211
-11.096627	-8.508644	0.225216
-11.290397	-16.245259	0.230221
-11.119635	-8.081196	0.235226
-11.993394	-14.003570	0.240230
-12.028099	-21.271419	0.245235
-12.741212	-11.884612	0.250240
-12.931210	-13.879795	0.255245
-12.755498	-16.688029	0.260250
-13.083535	-15.349382	0.265254
-12.970485	-14.316685	0.270259
-13.110294	-10.846574	0.275264
-13.778324	-14.915445	0.280269
-13.843098	-16.465069	0.285274
-14.138696	-11.439497	0.290278
-14.269439	-12.175284	0.295283
-14.959295	-10.720194	0.300288
-15.079773	-19.129420	0.305293
-15.468108	-15.237814	0.310298
-15.610042	-10.299440	0.315302
-15.371472	-11.779239	0.320307
-15.542486	-10.813041	0.325312
-16.160631	-15.652118	0.330317
-16.612689	-18.859302	0.335322
-17.080576	-13.547488	0.340326
-17.084865	-16.299223	0.345331
-16.995644	-4.250161	0.350336
-17.197736	-11.400207	0.355341
-17.520721	-10.508420	0.360346
-18.164659	-16.023664	0.365350
-18.352785	-13.824144	0.370355
-18.703276	-9.337336	0.375360
-18.465523	-11.974903	0.380365
-18.443283	-7.796056	0.385370
-19.631379	-17.003970	0.390374
-19.643164	-19.548901	0.395379
-20.164012	-14.564188	0.400384
-20.192602	-7.065089	0.405389
-20.294096	-14.869853	0.410394
-20.174237	-16.321677	0.415398
-20.413885	-20.767281	0.420403
-21.147076	-12.297969	0.425408
-21.140903	-11.979434	0.430413
-21.653339	-11.814262	0.435418
-21.535043	-10.785545	0.440422
-21.680051	-14.258828	0.445427
-22.690452	-16.104131	0.450432
-22.772819	-16.097665	0.455437
-22.895612	-20.937937	0.460442
-22.729308	-19.087820	0.465446
-23.125664	-15.622058	0.470451
-23.580873	-10.995564	0.475456
-23.355037	-15.304843	0.480461
-23.979545	-13.581527	0.485466
-24.525720	-11.051022	0.490470
-24.625812	-20.156259	0.495475
-24.778661	-9.227405	0.500480
-24.274438	-9.217361	0.505485
-24.853241	-15.128711	0.510490
-25.523468	-10.652231	0.515494
-25.606135	-21.183822	0.520499
-26.003474	-14.668153	0.525504
-26.284758	-15.953121	0.530509
-26.637625	-13.968388	0.535514
-27.112462	-12.916922	0.540518
-26.885007	-12.547421	0.545523
-27.374653	-9.940298	0.550528
-27.286371	-16.161149	0.555533
-27.167962	-15.793651	0.560538
-27.916158	-20.966805	0.565542
-28.584103	-24.459903	0.570547
-28.684916	-14.766648	0.575552
-28.504401	-19.711090	0.580557
-28.367358	-16.122740	0.585562
-29.691423	-10.351765	0.590566
-29.758684	-16.557888	0.595571
-30.270881	-17.253265	0.600576
-30.508148	-17.222682	0.605581
-30.367629	-17.804557	0.610586
-30.296681	-15.496683	0.615590
-30.142183	-23.252717	0.620595
-30.675208	-22.565502	0.625600
-30.994863	-20.576449	0.630605
-31.384775	-22.252613	0.635610
-31.613077	-19.796911	0.640614
-31.866334	-18.419289	0.645619
-32.567178	-25.928256	0.650624
-32.657786	-29.783316	0.655629
-33.095246	-25.475954	0.660634
-33.559414	-21.521924	0.665638
-33.228505	-20.485184	0.670643
-33.192218	-18.697079	0.675648
-33.199045	-21.299727	0.680653
-33.998505	-24.158600	0.685658
-34.599962	-20.692542	0.690662
-34.158290	-20.957486	0.695667
-34.500730	-16.231497	0.700672
-34.881036	-26.821143	0.705677
-35.351966	-23.688608	0.710682
-35.727113	-27.670203	0.715686
-35.606894	-20.649845	0.720691
-35.941411	-15.697307	0.725696
-36.278823	-21.880348	0.730701
-36.991273	-24.566113	0.735706
-37.320691	-19.740916	0.740710
-36.936654	-21.929874	0.745715
-37.293068	-11.741258	0.750720
-37.486505	-23.517894	0.755725
-37.542803	-23.793888	0.760730
-37.993481	-17.665371	0.765734
-38.165331	-24.200044	0.770739
-38.651083	-19.040469	0.775744
-38.968081	-18.269833	0.780749
-38.834946	-21.875003	0.785754
-39.005038	-16.071736	0.790758
-39.014281	-18.126698	0.795763
-40.198498	-8.274248	0.800768
-40.349911	-18.190879	0.805773
-40.613031	-13.344367	0.810778
-40.992330	-9.428858	0.815782
-40.692168	-30.469568	0.820787
-40.398963	-20.246064	0.825792
-41.356253	-26.361062	0.830797
-41.630932	-26.884619	0.835802
-42.140390	-23.568922	0.840806
-41.937703	-24.255385	0.845811
-42.330492	-19.701886	0.850816
-42.281110	-22.471467	0.855821
-42.850349	-28.121718	0.860826
-43.412208	-29.891328	0.865830
-43.315385	-28.144285	0.870835
-43.772702	-23.704122	0.875840
-43.159472	-32.088377	0.880845
-43.601401	-20.722231	0.885850
-44.908590	-22.144849	0.890854
-44.832681	-24.200413	0.895859
-45.031543	-23.612681	0.900864
-44.719324	-19.510623	0.905869
-44.971898	-22.891228	0.910874
-45.083057	-21.621150	0.915878
-45.737354	-21.443381	0.920883
-46.147226	-14.201286	0.925888
-46.400679	-27.816143	0.930893
-46.214521	-22.871912	0.935898
-46.867788	-24.532380	0.940902
-47.421344	-29.602962	0.945907
-47.924780	-19.663533	0.950912
-47.878432	-17.652376	0.955917
-47.890990	-25.929708	0.960922
-48.479668	-19.874615	0.965926
-48.381934	-17.384257	0.970931
-48.369864	-23.504656	0.975936
-48.386605	-25.558449	0.980941
-48.339868	-23.468261	0.985946
-49.434488	-27.322017	0.990950
-49.445685	-17.329518	0.995955
-49.542524	-18.988039	1.000960
-49.982101	-26.436447	1.005965
-50.417335	-25.859367	1.010970
-50.895882	-23.696885	1.015974
-50.981782	-27.739332	1.020979
-51.098663	-14.376915	1.025984
-51.119655	-13.924441	1.030989
-51.245485	-19.507695	1.035994
-52.022815	-26.419477	1.040998
-52.084810	-36.713838	1.046003
-52.844681	-20.913383	1.051008
-52.260568	-24.459059	1.056013
-52.262366	-29.191620	1.061018
-52.883335	-22.147608	1.066022
-53.522097	-28.995545	1.071027
-53.516032	-26.962299	1.076032
-53.697191	-27.060670	1.081037
-53.892885	-30.219183	1.086042
-54.268884	-25.355099	1.091046
-55.036093	-26.134152	1.096051
-55.157596	-23.872243	1.101056
-55.588436	-25.848906	1.106061
-55.425289	-24.169136	1.111066
-55.513322	-18.372320	1.116070
-55.443277	-27.342696	1.121075
-55.344209	-17.674239	1.126080
-55.815935	-12.206809	1.131085
-56.269849	-14.515228	1.136090
-56.869250	-28.304002	1.141094
-57.910175	-26.136213	1.146099
-57.582904	-22.833739	1.151104
-57.613471	-26.150836	1.156109
-58.195379	-29.720600	1.161114
-58.462762	-28.723580	1.166118
-58.359033	-33.950280	1.171123
-58.630293	-21.557216	1.176128
-58.185472	-32.942855	1.181133
-58.534887	-33.891358	1.186138
-59.315790	-21.172179	1.191142
-59.573264	-36.564369	1.196147
-59.962025	-14.291934	1.201152
-60.175812	-27.305546	1.206157
-60.060332	-25.403227	1.211162
-60.822051	-23.408619	1.216166
-61.017561	-23.495265	1.221171
-61.502074	-14.058635	1.226176
-61.618317	-25.521431	1.231181
-61.876082	-19.976590	1.236186
-61.723051	-19.494265	1.241190
-61.261145	-16.440534	1.246195
-62.203912	-12.623950	1.251200
-62.697295	-25.711085	1.256205
-62.923005	-19.797924	1.261210
-63.122012	-22.095412	1.266214
-62.814429	-21.418860	1.271219
-63.397711	-14.924859	1.276224
-64.159259	-20.529351	1.281229
-64.275359	-26.063499	1.286234
-64.347933	-17.975449	1.291238
-64.224778	-26.074601	1.296243
-64.907284	-16.044017	1.301248
-65.309374	-18.284577	1.306253
-65.498301	-26.816011	1.311258
-65.694512	-22.489266	1.316262
-65.603199	-26.239777	1.321267
-65.572808	-20.167182	1.326272
-66.316211	-20.276085	1.331277
-66.927944	-29.899581	1.336282
-67.150512	-26.834189	1.341286
-66.791113	-24.846465	1.346291
-67.268297	-23.829434	1.351296
-66.991142	-20.784903	1.356301
-68.045498	-36.198546	1.361306
-68.433654	-26.027143	1.366310
-68.887776	-29.357384	1.371315
-69.214406	-18.860210	1.376320
-68.830736	-22.371514	1.381325
-68.954746	-25.357698	1.386330
-69.006637	-28.219074	1.391334
-69.368341	-29.608572	1.396339
-70.165736	-22.372582	1.401344
-70.491020	-29.557217	1.406349
-70.317866	-22.643177	1.411354
-70.368479	-28.272939	1.416358
-70.306309	-29.000797	1.421363
-71.198962	-29.795118	1.426368
-71.744568	-24.278225	1.431373
-71.581193	-26.508753	1.436378
-72.085913	-13.876862	1.441382
-71.766993	-28.833636	1.446387
-71.992807	-26.334032	1.451392
-72.612543	-24.412149	1.456397
-72.889999	-21.221156	1.461402
-73.666643	-18.404840	1.466406
-73.212100	-27.669190	1.471411
-73.392728	-22.152178	1.476416
-73.535426	-18.387401	1.481421
-73.943160	-15.729760	1.486426
-75.029099	-13.950417	1.491430
-74.879301	-25.872235	1.496435
-74.762308	-20.161125	1.501440
-74.735495	-25.999088	1.506445
-75.035822	-20.327402	1.511450
-76.144067	-19.329170	1.516454
-76.047331	-20.226919	1.521459
-76.179599	-18.896608	1.526464
-76.361456	-22.054114	1.531469
-76.318408	-18.596658	1.536474
-77.041896	-13.260867	1.541478
-77.530809	-19.575335	1.546483
-77.822914	-20.270179	1.551488
-77.830168	-25.014545	1.556493
-77.506391	-23.359785	1.561498
-77.763992	-15.957910	1.566502
-78.227233	-18.998841	1.571507
-78.401523	-16.510420	1.576512
-79.146581	-17.707359	1.581517
-78.842254	-23.205731	1.586522
-79.231878	-19.693564	1.591526
-79.106763	-25.733488	1.596531
-79.681772	-14.697785	1.601536
-80.220724	-27.369711	1.606541
-80.290279	-25.308873	1.611546
-80.439760	-24.887011	1.616550
-81.103096	-32.733993	1.621555
-81.720679	-17.496674	1.626560
-81.921080	-22.536824	1.631565
-82.108136	-28.135850	1.636570
-82.086878	-12.798686	1.641574
-81.666224	-33.358291	1.646579
-82.167183	-22.410049	1.651584
-82.125535	-25.580208	1.656589
-82.689075	-18.617901	1.661594
-83.247180	-27.661308	1.666598
-83.403594	-28.361460	1.671603
-83.076673	-17.165643	1.676608
-83.738244	-23.168499	1.681613
-84.302577	-27.462309	1.686618
-84.822967	-16.833731	1.691622
-84.629934	-24.216124	1.696627
-84.671062	-18.394976	1.701632
-84.988471	-21.790794	1.706637
-85.062937	-23.610980	1.711642
-85.849039	-24.054908	1.716646
-86.072783	-24.162466	1.721651
-86.481397	-14.766129	1.726656
-86.354458	-21.037285	1.731661
-86.054036	-24.959554	1.736666
-87.468286	-15.144057	1.741670
-87.362636	-18.887311	1.746675
-87.749654	-27.191754	1.751680
-87.957726	-23.514873	1.756685
-87.870636	-23.550610	1.761690
-87.856840	-17.279285	1.766694
-87.667238	-26.372674	1.771699
-88.665525	-22.623375	1.776704
-88.922577	-26.999828	1.781709
-89.300784	-22.720674	1.786714
-89.490599	-18.290524	1.791718
-89.152147	-16.470375	1.796723
-89.978905	-18.448667	1.801728
-90.426092	-20.128566	1.806733
-90.516351	-19.915235	1.811738
-90.926763	-19.968420	1.816742
-90.959885	-23.304101	1.821747
-91.373395	-21.442800	1.826752
-91.341690	-21.435113	1.831757
-91.365019	-25.082356	1.836762
-92.280551	-19.112409	1.841766
-92.147198	-23.657213	1.846771
-92.534163	-16.412361	1.851776
-92.824128	-16.844955	1.856781
-92.324585	-19.826990	1.861786
-93.132800	-15.389136	1.866790
-93.433174	-27.769188	1.871795
-93.614978	-24.358979	1.876800
-93.505068	-23.566231	1.881805
-93.826494	-21.039084	1.886810
-95.031898	-22.964747	1.891814
-95.072239	-23.853808	1.896819
-95.614576	-19.172625	1.901824
-95.625560	-14.099626	1.906829
-95.484425	-23.074742	1.911834
-95.627758	-18.221574	1.916838
-95.882916	-15.872418	1.921843
-95.683211	-21.629737	1.926848
-95.853050	-15.589239	1.931853
-96.380207	-20.705058	1.936858
-97.014991	-12.516817	1.941862
-96.969489	-25.327197	1.946867
-97.312843	-21.123069	1.951872
-97.678802	-20.534629	1.956877
-98.218299	-24.303977	1.961882
-98.509304	-22.208658	1.966886
-98.450415	-25.602956	1.971891
-98.560939	-22.115263	1.976896
-98.660110	-14.991148	1.981901
-98.925235	-31.891203	1.986906
-99.788398	-23.509227	1.991910
-99.831118	-27.134467	1.996915
-99.856596	-17.379270	2.006912
-99.902945	-19.193540	2.016909
-99.272289	-15.097769	2.026906
-98.833642	-15.742650	2.036902
-98.089987	-19.773770	2.046899
-97.561568	-15.117237	2.056896
-97.319287	-16.938435	2.066893
-96.617001	-16.702566	2.076890
-95.888033	-17.288115	2.086886
-96.116682	-17.971644	2.096883
-95.620262	-16.854779	2.106880
-94.834338	-15.333177	2.116877
-93.904077	-14.920567	2.126874
-93.410353	-20.407925	2.136870
-93.454899	-19.827699	2.146867
-92.744146	-15.266077	2.156864
-92.054955	-20.115485	2.166861
-91.928803	-19.115193	2.176858
-91.234411	-14.630216	2.186854
-90.832772	-12.633812	2.196851
-90.119647	-17.943095	2.206848
-89.231315	-18.116316	2.216845
-89.249627	-17.682721	2.226842
-88.906365	-19.225046	2.236838
-88.102530	-19.375608	2.246835
-87.775437	-21.171998	2.256832
-87.447299	-14.976459	2.266829
-86.430535	-20.659291	2.276826
-86.173931	-18.931733	2.286822
-85.617606	-19.411210	2.296819
-84.754684	-22.120965	2.306816
-84.518652	-18.058782	2.316813
-84.358832	-17.047892	2.326810
-84.077545	-18.789636	2.336806
-83.300712	-19.363631	2.346803
-82.519370	-14.369522	2.356800
-81.989996	-20.971124	2.366797
-81.929078	-19.447507	2.376794
-80.655322	-17.507700	2.386790
-80.524549	-19.729672	2.396787
-80.595266	-22.142010	2.406784
-80.342270	-16.400422	2.416781
-79.277013	-24.203655	2.426778
-78.306777	-20.810134	2.436774
-78.131859	-20.603022	2.446771
-77.795496	-27.823947	2.456768
-76.804272	-25.643753	2.466765
-76.766257	-25.275947	2.476762
-76.583768	-20.480026	2.486758
-75.474976	-23.095019	2.496755
-75.415583	-16.800617	2.506752
-74.530336	-21.604526	2.516749
-73.995688	-22.413235	2.526746
-73.820767	-23.707611	2.536742
-73.137083	-16.332029	2.546739
-72.822750	-20.866489	2.556736
-71.888750	-23.213522	2.566733
-71.223365	-12.040191	2.576730
-71.042856	-16.569654	2.586726
-70.820596	-15.384760	2.596723
-70.321268	-13.945242	2.606720
-69.552509	-14.774564	2.616717
-69.328584	-18.417496	2.626714
-68.703897	-18.264574	2.636710
-67.836842	-14.931011	2.646707
-67.918173	-17.572939	2.656704
-67.026201	-22.032616	2.666701
-66.498200	-18.725455	2.676698
-66.537743	-16.368932	2.686694
-65.506703	-14.350152	2.696691
-64.977226	-14.416815	2.706688
-64.644368	-19.942481	2.716685
-63.906025	-21.875759	2.726682
-63.833534	-16.464016	2.736678
-63.250899	-13.884427	2.746675
-62.567792	-16.648545	2.756672
-62.319241	-18.695626	2.766669
-61.550819	-23.075880	2.776666
-61.370123	-18.095952	2.786662
-60.485893	-17.305553	2.796659
-59.515868	-22.090985	2.806656
-59.135493	-20.756486	2.816653
-59.398613	-22.720732	2.826650
-59.244739	-17.926690	2.836646
-58.252954	-27.828167	2.846643
-57.119303	-26.329028	2.856640
-56.794614	-23.639589	2.866637
-56.614105	-26.426818	2.876634
-56.198205	-27.283560	2.886630
-55.749666	-24.781292	2.896627
-55.178783	-26.102473	2.906624
-54.838703	-23.947604	2.916621
-53.737740	-23.735794	2.926618
-53.381663	-23.113411	2.936614
-53.277261	-18.026572	2.946611
-52.310068	-22.222372	2.956608
-52.023422	-16.356146	2.966605
-51.794317	-20.880504	2.976602
-50.906919	-20.974386	2.986598
-50.377303	-25.098887	2.996595
-50.418901	-13.061567	3.006592
-49.592901	-14.964147	3.016589
-48.887637	-18.187862	3.026586
-48.665981	-23.464972	3.036582
-47.871154	-23.921396	3.046579
-47.579415	-22.436885	3.056576
-47.368120	-23.502515	3.066573
-46.503541	-27.894572	3.076570
-45.720895	-20.271478	3.086566
-45.801871	-19.137569	3.096563
-45.366815	-12.999854	3.106560
-44.783910	-18.570787	3.116557
-43.830482	-18.532403	3.126554
-43.408583	-16.529650	3.136550
-43.233756	-16.721653	3.146547
-42.482077	-15.777573	3.156544
-41.944742	-24.569291	3.166541
-41.756031	-13.701864	3.176538
-40.746009	-25.364254	3.186534
-40.286825	-19.626259	3.196531
-40.095342	-21.163958	3.206528
-39.938697	-23.380455	3.216525
-39.037105	-25.370827	3.226522
-38.720842	-27.647021	3.236518
-37.564077	-21.951116	3.246515
-37.183136	-26.809548	3.256512
-36.956995	-19.578129	3.266509
-37.071785	-21.609818	3.276506
-36.004563	-19.134187	3.286502
-35.676024	-26.005449	3.296499
-35.004564	-14.285050	3.306496
-34.404181	-19.785848	3.316493
-34.072010	-20.613715	3.326490
-33.736096	-24.422965	3.336486
-32.993976	-19.730013	3.346483
-32.926989	-24.735960	3.356480
-32.124450	-23.324645	3.366477
-31.714878	-19.140598	3.376474
-30.466654	-24.457169	3.386470
-30.170617	-21.003021	3.396467
-30.084072	-30.158525	3.406464
-30.116642	-22.240616	3.416461
-28.941713	-25.740189	3.426458
-28.509796	-21.613472	3.436454
-27.681087	-24.241874	3.446451
-27.257710	-24.266676	3.456448
-27.064209	-20.159856	3.466445
-26.834572	-22.257842	3.476442
-26.128981	-24.895584	3.486438
-25.692515	-31.140607	3.496435
-24.568688	-22.265544	3.506432
-24.090856	-24.785465	3.516429
-24.083921	-22.946176	3.526426
-24.052519	-27.351056	3.536422
-22.998078	-20.406985	3.546419
-22.815985	-28.227929	3.556416
-21.738936	-17.790242	3.566413
-21.494766	-21.911481	3.576410
-21.103710	-18.833244	3.586406
-20.389084	-20.835686	3.596403
-19.874373	-22.870356	3.606400
-19.728982	-20.780203	3.616397
-18.855573	-21.990102	3.626394
-18.318281	-18.120535	3.636390
-18.381889	-23.213852	3.646387
-17.458192	-16.867123	3.656384
-17.013881	-21.814615	3.666381
-16.479979	-20.380479	3.676378
-15.743829	-24.207697	3.686374
-15.684470	-19.094838	3.696371
-15.081782	-23.290903	3.706368
-13.928220	-22.273183	3.716365
-13.925321	-23.515434	3.726362
-13.594443	-26.836075	3.736358
-12.980597	-25.018424	3.746355
-12.200337	-22.646994	3.756352
-12.424774	-24.661612	3.766349
-11.389411	-23.625489	3.776346
-10.813835	-31.495025	3.786342
-10.679282	-20.802893	3.796339
-10.056713	-26.756956	3.806336
-9.536964	-23.793787	3.816333
-9.140667	-19.994131	3.826330
-8.287413	-15.549721	3.836326
-8.019036	-23.428450	3.846323
-7.783890	-18.048364	3.856320
-7.010916	-16.936542	3.866317
-6.615311	-16.032052	3.876314
-5.966375	-16.126816	3.886310
-5.729551	-14.526053	3.896307
-4.908153	-11.774567	3.906304
-4.539684	3.078360	3.916301
-4.098416	11.353317	3.926298
-3.938179	15.313275	3.936294
-3.543893	23.373815	3.946291
-2.720979	42.635153	3.956288
-2.173974	43.902535	3.966285
-2.052351	59.658726	3.976282
-1.628942	68.265934	3.986278
-1.019649	90.636433	3.996275
-0.518379	110.226684	4.006272
0.000000	124.233335	4.011277
0.048766	136.216028	4.016282
0.660573	133.102597	4.021286
0.278912	134.936809	4.026291
0.301036	132.924401	4.031296
1.024476	146.956518	4.036301
0.796723	153.806505	4.041306
0.648305	144.904853	4.046310
0.443229	158.040697	4.051315
0.973359	163.795111	4.056320
0.959320	163.398642	4.061325
0.630410	160.865096	4.066330
1.127439	157.399380	4.071334
0.871412	167.230795	4.076339
0.713356	156.821562	4.081344
1.096784	160.074203	4.086349
1.202238	164.316063	4.091354
1.114976	161.450671	4.096358
0.702447	170.594626	4.101363
0.889404	164.605115	4.106368
0.863262	171.059895	4.111373
1.057797	171.342780	4.116378
0.882755	161.477178	4.121382
0.655367	170.383505	4.126387
0.569898	169.716590	4.131392
0.558170	168.984411	4.136397
0.446953	160.032667	4.141402
0.814742	164.992966	4.146406
1.114766	188.708626	4.151411
1.422457	194.304699	4.156416
1.177344	187.449165	4.161421
0.877516	179.032967	4.166426
1.195244	194.124850	4.171430
0.805945	196.662595	4.176435
1.031635	188.629633	4.181440
1.185009	201.168710	4.186445
1.344389	198.695172	4.191450
1.643054	194.703525	4.196454
1.325858	196.167047	4.201459
1.226220	191.696425	4.206464
1.396996	188.287828	4.211469
1.450409	190.547841	4.216474
1.455296	177.585444	4.221478
1.089974	182.950949	4.226483
1.210711	175.696781	4.231488
1.037832	180.791883	4.236493
1.253571	189.233765	4.241498
1.202439	193.601250	4.246502
1.210242	200.303850	4.251507
1.363018	203.753758	4.256512
1.495600	195.308192	4.261517
1.185926	192.227493	4.266522
1.727145	188.663145	4.271526
1.367479	192.572478	4.276531
1.440132	193.636787	4.281536
1.819407	192.128737	4.286541
1.396699	189.701537	4.291546
1.541392	175.676523	4.296550
1.262133	183.116657	4.301555
1.552970	189.639148	4.306560
1.741703	191.027061	4.311565
1.163246	177.193730	4.316570
1.532352	182.093718	4.321574
1.550694	196.431804	4.326579
1.835214	196.947446	4.331584
1.435494	179.397429	4.336589
1.519151	191.880917	4.341594
1.692969	190.531403	4.346598
1.637673	192.941217	4.351603
1.808924	189.867895	4.356608
1.561840	176.881456	4.361613
1.300028	184.568805	4.366618
1.859348	185.728181	4.371622
1.638229	193.665456	4.376627
1.465074	189.883310	4.381632
1.587369	189.155573	4.386637
1.782567	201.827340	4.391642
1.900054	192.504621	4.396646
1.658310	199.265057	4.401651
1.902518	196.196194	4.406656
1.624632	189.747550	4.411661
1.396460	197.005733	4.416666
1.402214	190.664784	4.421670
1.476968	193.098641	4.426675
1.382348	192.091471	4.431680
1.813258	192.733014	4.436685
1.573824	194.016753	4.441690
2.150820	184.255507	4.446694
1.732969	199.968111	4.451699
1.604330	196.716858	4.456704
2.321240	200.249771	4.461709
1.707132	197.289235	4.466714
1.748229	187.114727	4.471718
2.021684	197.547075	4.476723
2.064926	188.868654	4.481728
1.915631	189.217727	4.486733
1.838715	195.228014	4.491738
1.817874	198.793536	4.496742
1.739200	197.821848	4.501747
1.608828	200.607175	4.506752
1.930691	200.360882	4.511757
2.113060	221.121041	4.516762
2.212562	220.127938	4.521766
1.867445	199.864446	4.526771
1.606711	201.964568	4.531776
2.101662	216.373994	4.536781
2.165882	218.233703	4.541786
2.345806	219.885577	4.546790
2.108595	213.079422	4.551795
2.312099	212.781956	4.556800
2.062666	201.279634	4.561805
1.836738	202.763747	4.566810
2.115191	207.915133	4.571814
2.116209	219.402291	4.576819
2.417049	218.776465	4.581824
2.187263	220.903408	4.586829
2.201942	227.782114	4.591834
2.335583	220.222205	4.596838
2.143543	215.639417	4.601843
2.205500	217.097690	4.606848
2.336949	204.707178	4.611853
2.256425	214.932063	4.616858
2.101124	214.437367	4.621862
2.035213	226.077315	4.626867
2.460883	220.275241	4.631872
2.281709	218.458676	4.636877
1.825793	226.521106	4.641882
2.062163	216.629383	4.646886
2.142752	219.821620	4.651891
2.259278	217.993817	4.656896
2.287368	218.834116	4.661901
2.572628	220.014018	4.666906
2.264039	217.758868	4.671910
2.202320	220.372161	4.676915
2.232394	214.672809	4.681920
2.272492	219.567087	4.686925
2.208195	228.194955	4.691930
2.180556	221.786429	4.696934
2.352581	234.737069	4.701939
2.530393	238.898080	4.706944
2.891580	242.071942	4.711949
2.692099	240.157299	4.716954
2.665904	225.503968	4.721958
2.728713	228.259222	4.726963
2.570284	219.662805	4.731968
2.596409	221.863797	4.736973
2.311767	221.424039	4.741978
2.081019	210.690742	4.746982
2.636287	229.175107	4.751987
2.566909	227.822327	4.756992
2.538421	229.326320	4.761997
2.479532	249.206604	4.767002
2.844043	242.303588	4.772006
2.561627	247.055102	4.777011
3.113259	244.957075	4.782016
2.997507	230.716309	4.787021
2.368900	230.608509	4.792026
2.367447	228.397285	4.797030
2.558501	246.786518	4.802035
2.820552	241.247189	4.807040
2.736191	251.431564	4.812045
2.554697	243.968166	4.817050
2.809442	242.112512	4.822054
2.694214	251.678446	4.827059
3.024964	241.803652	4.832064
2.905474	244.467071	4.837069
2.658446	257.078020	4.842074
2.929718	250.667236	4.847078
2.675642	255.518742	4.852083
2.815337	257.493252	4.857088
3.044550	247.561498	4.862093
3.053036	246.683802	4.867098
3.320605	241.466311	4.872102
2.751590	245.164645	4.877107
2.883934	242.340977	4.882112
3.122886	245.717366	4.887117
2.768093	240.944780	4.892122
3.042352	238.630517	4.897126
2.902522	242.761892	4.902131
2.943626	244.786551	4.907136
2.837266	246.473509	4.912141
2.532528	256.442268	4.917146
2.772052	252.671784	4.922150
2.688126	258.559801	4.927155
2.831017	258.211661	4.932160
3.118132	248.612571	4.937165
2.960024	257.587246	4.942170
3.025960	244.232489	4.947174
2.834501	249.627890	4.952179
2.958307	255.524691	4.957184
2.717301	247.092975	4.962189
2.573097	254.401382	4.967194
3.397546	254.991145	4.972198
2.966334	269.136697	4.977203
3.255216	271.432824	4.982208
3.153238	263.925399	4.987213
3.079525	267.385274	4.992218
3.305226	263.623267	4.997222
3.208653	275.090855	5.002227
2.885696	267.285646	5.007232
3.228563	271.316564	5.012237
3.170050	274.802547	5.017242
3.391473	268.668432	5.022246
3.284422	267.451227	5.027251
3.335906	271.002338	5.032256
3.461964	264.465465	5.037261
3.306942	271.338973	5.042266
3.540355	263.722383	5.047270
3.335251	267.696251	5.052275
3.182131	266.479891	5.057280
3.272652	266.307581	5.062285
3.171542	265.421638	5.067290
3.293230	270.841055	5.072294
3.228971	264.821023	5.077299
3.367468	269.617738	5.082304
3.387605	274.366445	5.087309
3.285605	275.046671	5.092314
3.503582	264.233985	5.097318
3.472025	269.088814	5.102323
3.371418	271.268415	5.107328
3.439943	272.877528	5.112333
3.345164	276.685527	5.117338
3.251509	266.462353	5.122342
3.444483	273.085531	5.127347
3.252082	283.577806	5.132352
3.599409	292.619336	5.137357
3.438968	301.974041	5.142362
3.517545	306.618747	5.147366
3.529174	300.526776	5.152371
3.696626	296.055672	5.157376
3.595438	295.755025	5.162381
3.413364	295.878253	5.167386
3.934338	297.891478	5.172390
3.605564	294.646058	5.177395
3.696100	297.444461	5.182400
3.810657	293.557387	5.187405
3.475500	297.507219	5.192410
3.735352	298.295619	5.197414
4.001287	308.346395	5.202419
4.058509	301.064101	5.207424
4.098790	293.164361	5.212429
3.666768	287.714100	5.217434
3.573924	270.723644	5.222438
3.585768	289.485666	5.227443
3.644936	293.095696	5.232448
3.707323	299.694924	5.237453
3.730237	297.176182	5.242458
3.839429	297.374281	5.247462
3.754019	304.300238	5.252467
3.893797	299.251320	5.257472
3.859233	298.551164	5.262477
3.713119	292.964639	5.267482
4.099938	296.305361	5.272486
4.040662	300.674140	5.277491
3.878432	289.607429	5.282496
4.124533	301.186193	5.287501
3.952375	298.403598	5.292506
4.080120	291.923399	5.297510
3.866594	306.095198	5.302515
3.578409	311.239926	5.307520
3.958976	297.513445	5.312525
3.884954	315.516920	5.317530
3.961453	303.536686	5.322534
4.057158	297.282932	5.327539
3.838385	294.308282	5.332544
3.816080	296.943923	5.337549
3.696302	308.538530	5.342554
3.762273	302.185002	5.347558
3.892462	301.959060	5.352563
4.147680	313.944530	5.357568
4.130087	318.515628	5.362573
4.265609	330.978483	5.367578
4.281756	322.494039	5.372582
3.954149	313.057062	5.377587
3.950985	311.909098	5.382592
4.336313	318.018297	5.387597
4.152130	323.643538	5.392602
4.548325	318.946991	5.397606
3.853069	311.993819	5.402611
4.503877	317.897171	5.407616
4.364279	321.133200	5.412621
3.982159	320.442865	5.417626
4.417679	322.377650	5.422630
4.356330	322.962965	5.427635
4.306145	331.006564	5.432640
4.580814	320.805104	5.437645
4.363130	315.865620	5.442650
4.002411	301.514243	5.447654
4.318553	313.787616	5.452659
4.540696	321.643279	5.457664
4.227615	315.079849	5.462669
4.208204	327.785120	5.467674
4.377240	329.574738	5.472678
4.483757	324.841035	5.477683
4.342410	322.575651	5.482688
4.420942	319.383868	5.487693
4.607034	330.987812	5.492698
4.601813	327.527498	5.497702
4.136391	326.948207	5.502707
3.943433	325.912049	5.507712
4.456768	326.920409	5.512717
4.249370	336.121094	5.517722
3.915722	326.767306	5.522726
4.370645	325.035499	5.527731
4.354383	329.729777	5.532736
4.561963	329.855612	5.537741
4.388722	329.667421	5.542746
4.423794	323.616085	5.547750
4.271989	346.124166	5.552755
4.234466	343.412349	5.557760
5.064476	349.610510	5.562765
5.086572	343.583333	5.567770
4.962145	342.833893	5.572774
4.871425	345.163822	5.577779
4.456634	335.246868	5.582784
4.745885	326.093487	5.587789
4.338986	339.817700	5.592794
4.739557	345.870753	5.597798
4.878690	347.256910	5.602803
4.631210	348.124302	5.607808
4.746946	342.522302	5.612813
4.198083	347.691809	5.617818
4.862365	339.077972	5.622822
4.880869	350.306231	5.627827
4.875329	355.410129	5.632832
5.303366	353.673014	5.637837
4.803513	362.384580	5.642842
5.193331	346.018083	5.647846
4.934075	342.796632	5.652851
4.475596	326.616013	5.657856
4.709656	335.921969	5.662861
4.625224	351.177838	5.667866
5.157099	345.109255	5.672870
4.754793	362.929776	5.677875
4.642437	355.822557	5.682880
4.993474	360.235033	5.687885
4.874994	359.589068	5.692890
4.769360	354.679583	5.697894
4.830369	362.535043	5.702899
5.074486	359.871121	5.707904
5.178994	354.868807	5.712909
4.951669	358.710116	5.717914
5.027332	350.330285	5.722918
5.209578	351.200373	5.727923
4.860583	357.322678	5.732928
5.219827	350.464733	5.737933
4.774636	354.419054	5.742938
5.158853	345.611540	5.747942
5.281388	346.123934	5.752947
5.043668	351.469621	5.757952
5.255340	357.128152	5.762957
4.971532	354.799524	5.767962
5.255090	350.819686	5.772966
5.312361	354.797014	5.777971
4.906143	349.801455	5.782976
5.062433	358.442496	5.787981
4.830933	362.920362	5.792986
5.175103	350.638996	5.797990
4.940234	356.284794	5.802995
5.016740	362.502201	5.808000
5.000825	354.930719	5.813005
5.067648	356.729927	5.818010
5.516505	368.849799	5.823014
5.179927	364.495117	5.828019
4.809728	376.169885	5.833024
5.456539	369.504439	5.838029
4.964941	385.918377	5.843034
4.897536	377.190655	5.848038
5.180896	377.893142	5.853043
4.949083	384.066814	5.858048
5.224613	381.144901	5.863053
5.281802	377.785589	5.868058
5.445179	372.682357	5.873062
5.422194	379.892849	5.878067
5.275681	381.959390	5.883072
5.722420	385.246507	5.888077
5.476144	377.489422	5.893082
5.484403	373.852995	5.898086
5.342287	378.266328	5.903091
5.123953	379.553122	5.908096
5.233447	377.650468	5.913101
5.552635	399.692984	5.918106
5.523663	403.022533	5.923110
5.482626	410.125118	5.928115
5.781127	412.688682	5.933120
5.614900	402.112901	5.938125
5.125919	398.506431	5.943130
5.628700	402.202437	5.948134
5.854281	409.614683	5.953139
5.918835	401.382090	5.958144
6.168591	396.869672	5.963149
5.948518	383.420138	5.968154
5.847606	381.063030	5.973158
5.602409	375.007857	5.978163
5.287528	374.825900	5.983168
5.649784	370.302301	5.988173
5.826986	373.118860	5.993178
5.756005	374.540897	5.998182
5.962228	374.385372	6.003187
5.358976	376.687538	6.008192
5.617412	363.815242	6.013197
5.501277	373.049193	6.018202
5.842714	363.666207	6.023206
5.816467	376.328285	6.028211
5.622025	379.329257	6.033216
5.568337	374.449643	6.038221
5.350482	373.705257	6.043226
5.936672	405.361871	6.048230
6.027379	397.106225	6.053235
5.461922	394.100116	6.058240
5.879732	393.750298	6.063245
5.745925	410.899483	6.068250
6.052759	404.084479	6.073254
5.662894	389.949538	6.078259
5.589798	381.887079	6.083264
5.682602	384.865475	6.088269
5.586806	397.990809	6.093274
5.680736	395.717257	6.098278
6.215866	400.072607	6.103283
5.671160	390.277089	6.108288
5.572858	380.130502	6.113293
5.702358	395.213897	6.118298
5.809301	397.769319	6.123302
5.648279	404.210383	6.128307
5.698038	403.069992	6.133312
6.085427	400.348957	6.138317
5.588994	387.432824	6.143322
5.476349	391.828917	6.148326
5.671616	407.370313	6.153331
5.870564	405.694171	6.158336
5.729320	401.293249	6.163341
5.925621	404.695292	6.168346
6.095412	404.763736	6.173350
5.561410	387.702651	6.178355
5.326402	397.053197	6.183360
5.828585	396.804137	6.188365
5.410911	409.574638	6.193370
5.600106	406.403574	6.198374
5.642401	408.621054	6.203379
5.476538	409.959791	6.208384
5.886095	404.685344	6.213389
5.550838	406.686363	6.218394
5.877669	411.944170	6.223398
5.875686	405.863774	6.228403
5.624410	414.751796	6.233408
5.991693	404.244807	6.238413
5.601394	411.762435	6.243418
5.974646	397.676351	6.248422
5.889986	409.528144	6.253427
5.793532	411.327469	6.258432
5.770137	411.644289	6.263437
5.653747	414.316742	6.268442
5.491383	402.443233	6.273446
5.882517	409.589260	6.278451
5.782908	406.770043	6.283456
6.312672	406.858370	6.288461
6.012505	405.532019	6.293466
5.752922	396.533654	6.298470
5.502539	391.849174	6.303475
5.850062	402.007521	6.308480
5.953870	403.547878	6.313485
5.807544	390.668980	6.318490
5.603249	393.016599	6.323494
5.610674	390.620476	6.328499
5.808083	399.520888	6.333504
5.998989	392.072212	6.338509
5.721473	396.013090	6.343514
5.819579	387.101407	6.348518
5.919680	390.271655	6.353523
5.792031	387.605501	6.358528
5.932664	386.422489	6.363533
5.969755	387.261395	6.368538
5.510118	384.105935	6.373542
5.369842	389.768653	6.378547
5.417869	399.160554	6.383552
5.965555	395.544539	6.388557
5.819778	394.637071	6.393562
5.781884	392.026544	6.398566
5.566991	391.142492	6.403571
5.577605	396.724772	6.408576
5.688312	394.110090	6.413581
6.078290	412.139496	6.418586
5.883747	401.840204	6.423590
5.870752	393.784201	6.428595
5.558308	383.800666	6.433600
5.782605	385.423500	6.438605
5.384791	386.330119	6.443610
5.812574	394.530280	6.448614
5.982260	396.737415	6.453619
5.635086	397.073008	6.458624
6.054440	390.420822	6.463629
5.896064	391.141467	6.468634
5.653538	381.241959	6.473638
5.691329	388.822638	6.478643
5.825293	383.834712	6.483648
5.957012	384.836053	6.488653
5.317199	382.265460	6.493658
5.516535	389.026895	6.498662
5.715210	392.608897	6.503667
5.380764	393.417066	6.508672
6.062191	401.305659	6.513677
6.043163	408.316232	6.518682
5.943398	401.308273	6.523686
5.974722	394.396964	6.528691
5.707691	396.437979	6.533696
6.049155	392.357369	6.538701
5.972080	391.398076	6.543706
5.651190	380.520525	6.548710
5.913800	381.798876	6.553715
5.713636	382.956293	6.558720
5.601645	386.903035	6.563725
5.515599	395.312909	6.568730
5.605046	391.505652	6.573734
5.894487	393.548611	6.578739
5.808445	395.308349	6.583744
5.553311	390.055139	6.588749
5.551277	387.932569	6.593754
5.644085	394.761211	6.598758
5.834572	387.078486	6.603763
5.684793	390.746378	6.608768
5.666814	388.803459	6.613773
5.824815	387.380464	6.618778
5.650429	382.624043	6.623782
5.787129	384.377574	6.628787
5.484521	386.218485	6.633792
5.837890	389.399919	6.638797
5.999770	386.647558	6.643802
5.755825	386.657035	6.648806
5.828013	388.442756	6.653811
5.704540	381.710575	6.658816
5.968405	389.265547	6.663821
5.799049	390.089141	6.668826
5.561279	390.391881	6.673830
6.027636	381.441848	6.678835
5.522292	382.703727	6.683840
5.629425	382.737635	6.688845
5.619513	395.087139	6.693850
5.598578	384.270450	6.698854
5.948631	387.439745	6.703859
5.788784	397.958657	6.708864
5.550609	387.286520	6.713869
5.531913	397.489228	6.718874
5.542023	390.793193	6.723878
5.957121	396.723780	6.728883
6.028131	407.934410	6.733888
5.799859	393.312403	6.738893
5.396366	395.719510	6.743898
5.484048	397.800209	6.748902
5.728506	400.884708	6.753907
5.908926	410.550228	6.758912
5.989007	411.762089	6.763917
5.890273	401.621884	6.768922
5.939961	396.979267	6.773926
6.041967	395.482733	6.778931
5.588928	388.558255	6.783936
5.712976	395.046679	6.788941
5.471892	399.832927	6.793946
5.897697	395.492414	6.798950
5.786819	387.141610	6.803955
5.715200	406.979760	6.808960
5.797387	391.338156	6.813965
5.706532	385.796781	6.818970
5.812402	386.640797	6.823974
5.812899	380.958652	6.828979
5.468260	379.867014	6.833984
5.839812	392.321637	6.838989
5.672951	388.155658	6.843994
5.665964	388.226317	6.848998
5.821175	384.241145	6.854003
5.381894	399.729473	6.859008
5.850337	397.963917	6.864013
5.628344	405.281333	6.869018
5.892907	403.082452	6.874022
5.780872	393.830165	6.879027
5.590940	399.380396	6.884032
6.013657	394.787266	6.889037
6.111164	403.573522	6.894042
5.850116	389.149610	6.899046
5.766183	376.191406	6.904051
5.926965	379.064306	6.909056
5.935585	385.418839	6.914061
5.618151	383.057479	6.919066
5.908874	392.392607	6.924070
5.798735	392.634347	6.929075
5.401213	395.527737	6.934080
5.860299	387.192595	6.939085
5.450600	395.798392	6.944090
5.692115	396.197351	6.949094
5.879408	393.187935	6.954099
5.760192	397.227552	6.959104
5.733032	391.575020	6.964109
5.496481	394.582551	6.969114
5.699218	392.826727	6.974118
5.619338	388.906630	6.979123
5.419628	392.585460	6.984128
5.731616	398.601704	6.989133
5.933447	408.728955	6.994138
5.676426	403.178646	6.999142
5.650787	402.840924	7.004147
6.076145	408.393435	7.009152
6.140817	407.424727	7.014157
5.861220	401.384392	7.019162
5.450551	386.860391	7.024166
5.646762	391.942379	7.029171
5.653816	399.929641	7.034176
5.643835	384.131552	7.039181
5.532392	393.839341	7.044186
5.933070	405.466871	7.049190
5.893834	393.754530	7.054195
5.465688	393.827486	7.059200
5.674943	392.535714	7.064205
5.897046	405.402752	7.069210
5.954893	395.155916	7.074214
6.045130	393.841546	7.079219
5.919491	390.798596	7.084224
5.775700	388.919558	7.089229
5.931790	393.463634	7.094234
5.795403	400.131812	7.099238
5.765201	386.848863	7.104243
5.654556	389.817808	7.109248
5.858663	389.608829	7.114253
5.737602	393.265923	7.119258
5.520141	396.020548	7.124262
5.644065	393.970114	7.129267
5.723119	392.736579	7.134272
5.820607	389.560814	7.139277
5.616179	402.889724	7.144282
5.711924	404.700252	7.149286
5.919205	390.428046	7.154291
5.575767	392.933368	7.159296
5.776131	390.567316	7.164301
5.732895	391.782557	7.169306
5.919050	394.692637	7.174310
5.709244	384.708939	7.179315
5.572582	401.355528	7.184320
5.480636	393.710447	7.189325
5.446993	398.666875	7.194330
5.612937	399.786273	7.199334
5.814810	406.186655	7.204339
6.007916	416.837284	7.209344
5.578441	403.711399	7.214349
5.598279	408.415896	7.219354
5.772228	410.881794	7.224358
5.713113	411.071299	7.229363
5.576737	417.717336	7.234368
5.793529	419.350833	7.239373
5.652279	420.103614	7.244378
5.584035	423.122910	7.249382
5.817005	424.326786	7.254387
5.901149	426.841469	7.259392
5.967400	409.857747	7.264397
5.691740	418.442686	7.269402
5.649630	415.478474	7.274406
6.246491	411.222055	7.279411
6.085069	408.820582	7.284416
5.969488	394.661914	7.289421
5.775183	400.386831	7.294426
5.912716	394.689673	7.299430
5.975256	390.699946	7.304435
5.473863	383.631141	7.309440
5.667830	387.201220	7.314445
5.578796	387.661135	7.319450
5.363438	392.636362	7.324454
5.811411	385.100208	7.329459
5.729665	384.695294	7.334464
5.761664	379.862448	7.339469
5.500213	388.100315	7.344474
5.353805	384.383564	7.349478
5.870703	400.988507	7.354483
5.670567	413.446734	7.359488
6.281825	399.896225	7.364493
6.138552	400.408877	7.369498
5.891037	391.702862	7.374502
5.898119	383.991747	7.379507
5.914111	388.244426	7.384512
6.035656	373.811577	7.389517
6.213904	382.465031	7.394522
5.820996	388.986485	7.399526
5.957598	374.864498	7.404531
5.783662	385.920264	7.409536
6.029255	383.948964	7.414541
5.794308	382.033499	7.419546
5.713239	386.060847	7.424550
5.808195	379.164947	7.429555
5.903927	382.073284	7.434560
5.805732	370.427085	7.439565
5.379499	360.888380	7.444570
5.491212	371.475725	7.449574
5.879946	376.350566	7.454579
5.434690	377.644217	7.459584
5.641665	368.484641	7.464589
5.804488	381.632971	7.469594
5.364035	384.036340	7.474598
5.804304	375.191610	7.479603
5.506481	385.035979	7.484608
5.607656	380.271456	7.489613
5.737382	385.901626	7.494618
5.641103	383.923442	7.499622
5.669446	386.614485	7.504627
5.841985	388.688299	7.509632
5.969199	381.771557	7.514637
5.385863	382.384362	7.519642
5.524405	387.095681	7.524646
5.729392	384.055038	7.529651
5.506514	383.286124	7.534656
5.563163	380.578622	7.539661
5.593234	379.814617	7.544666
5.725455	378.740481	7.549670
5.322369	386.336019	7.554675
5.380371	400.206192	7.559680
6.041216	401.903426	7.564685
6.190671	417.575350	7.569690
5.893569	407.118018	7.574694
5.734252	399.220834	7.579699
5.636627	397.147948	7.584704
5.947407	391.654769	7.589709
5.919469	385.413907	7.594714
5.527676	386.920695	7.599718
5.547283	381.801880	7.604723
5.461528	401.629571	7.609728
5.631096	401.929001	7.614733
5.521273	410.323603	7.619738
5.812096	415.387703	7.624742
5.977787	408.442813	7.629747
5.997732	423.217426	7.634752
5.849143	412.078914	7.639757
5.878771	399.558589	7.644762
5.753040	387.059297	7.649766
5.695727	389.643456	7.654771
5.918551	378.140256	7.659776
6.152691	386.433837	7.664781
5.870344	386.322744	7.669786
5.465915	383.532007	7.674790
5.553920	384.321858	7.679795
5.606669	391.128262	7.684800
5.825523	383.494905	7.689805
5.589938	388.856090	7.694810
5.570673	394.411385	7.699814
5.775657	393.091804	7.704819
5.967130	402.078562	7.709824
5.819810	388.187431	7.714829
5.957323	388.314684	7.719834
5.819810	395.736001	7.724838
5.814681	394.661103	7.729843
5.417635	398.532009	7.734848
5.683647	391.077966	7.739853
5.786589	388.350600	7.744858
5.486129	384.825512	7.749862
5.815917	397.027216	7.754867
5.651407	402.943645	7.759872
6.074806	406.629865	7.764877
5.737842	398.114942	7.769882
5.647766	400.014512	7.774886
5.866645	382.260414	7.779891
5.642215	392.308493	7.784896
6.047921	387.882527	7.789901
5.651348	390.377140	7.794906
5.736866	394.214039	7.799910
5.505963	388.068052	7.804915
5.744290	389.701358	7.809920
6.208641	386.477965	7.814925
5.884400	383.159058	7.819930
5.643702	387.388428	7.824934
5.832646	380.648734	7.829939
5.577466	382.773322	7.834944
6.008188	383.383265	7.839949
5.994341	397.388007	7.844954
6.042991	398.250424	7.849958
5.737865	383.485369	7.854963
5.677588	394.355767	7.859968
5.472644	391.575099	7.864973
5.969357	391.766647	7.869978
5.619650	389.239469	7.874982
5.820406	392.732563	7.879987
5.843443	387.610049	7.884992
5.549355	385.267199	7.889997
5.463802	387.764006	7.895002
5.617733	392.767157	7.900006
5.655650	384.026196	7.905011
5.937816	393.119050	7.910016
5.577320	398.670527	7.915021
5.904953	392.469214	7.920026
5.464589	392.765534	7.925030
6.172925	388.191210	7.930035
5.894300	382.992280	7.935040
5.778135	394.858459	7.940045
5.658493	389.679066	7.945050
5.503569	393.781189	7.950054
5.671367	381.979673	7.955059
5.401378	392.079137	7.960064
5.528298	388.107860	7.965069
5.340714	397.106178	7.970074
5.888061	414.095530	7.975078
6.014056	404.904252	7.980083
5.992161	407.362677	7.985088
6.055863	398.048225	7.990093
5.835017	391.929144	7.995098
6.012484	395.074692	8.000102
5.876180	391.077960	8.005107
5.688899	397.754061	8.010112
5.733952	404.542670	8.015130
5.446688	396.041866	8.020147
5.233957	392.146173	8.025165
5.503533	389.901527	8.030182
5.596198	406.353245	8.035200
5.962814	406.233020	8.040218
6.319342	417.954370	8.045235
5.737469	406.428981	8.050253
6.008311	396.951387	8.055270
5.696108	393.658133	8.060288
5.742862	385.449294	8.065306
5.556252	386.163092	8.070323
5.622913	390.718903	8.075341
5.930569	393.533144	8.080358
5.985174	397.835227	8.085376
6.159158	388.221247	8.090394
5.755334	392.272828	8.095411
5.629160	396.076064	8.100429
5.994925	397.871450	8.105446
5.655091	396.835630	8.110464
5.896537	396.993657	8.115482
5.798082	397.722131	8.120499
5.632073	393.140700	8.125517
5.869292	394.056740	8.130534
6.063945	402.309980	8.135552
5.859072	401.291015	8.140570
5.773556	392.386435	8.145587
5.402553	402.608512	8.150605
6.156029	422.128788	8.155622
6.123429	420.881037	8.160640
5.877037	408.432453	8.165658
5.908451	406.111283	8.170675
5.915252	408.562133	8.175693
6.164708	399.539126	8.180710
5.806520	392.037084	8.185728
5.615386	395.815722	8.190746
6.113884	406.786006	8.195763
6.119125	410.218506	8.200781
6.055152	391.783663	8.205798
6.098378	396.829095	8.210816
5.782635	399.333318	8.215834
5.985197	386.638132	8.220851
5.757065	399.864230	8.225869
5.613144	390.432283	8.230886
6.050211	408.638567	8.235904
6.214472	423.173140	8.240922
6.252503	415.741936	8.245939
5.620508	407.212753	8.250957
6.000351	407.140959	8.255974
6.251600	412.485350	8.260992
6.048226	415.735748	8.266010
6.213843	403.835215	8.271027
6.156485	405.295713	8.276045
6.144517	392.280491	8.281062
5.978673	390.144662	8.286080
5.901677	394.549281	8.291098
5.989210	402.030287	8.296115
5.773147	404.156092	8.301133
5.946426	401.939061	8.306150
6.220942	404.562812	8.311168
5.850458	411.181062	8.316186
5.897134	411.464083	8.321203
6.000319	427.608084	8.326221
6.190985	417.546545	8.331238
6.388908	413.915098	8.336256
5.913263	414.560295	8.341274
6.408460	406.060731	8.346291
5.881890	399.553687	8.351309
6.206514	405.407333	8.356326
6.151398	410.720532	8.361344
6.007564	411.588610	8.366362
6.077299	412.559128	8.371379
5.609700	418.059622	8.376397
6.487720	409.916997	8.381414
6.735204	417.663427	8.386432
5.959860	412.211231	8.391450
5.882735	396.356599	8.396467
5.695331	410.412610	8.401485
6.071825	414.901254	8.406502
6.388350	414.940299	8.411520
6.422629	424.414512	8.416538
6.473404	419.493222	8.421555
6.082506	417.139978	8.426573
6.316707	406.566761	8.431590
6.196499	397.156364	8.436608
5.832316	398.866595	8.441626
6.410201	413.286270	8.446643
6.309744	417.590410	8.451661
6.383560	402.706302	8.456678
6.405121	401.071442	8.461696
6.136533	402.022056	8.466714
6.066670	396.863948	8.471731
5.779628	409.717391	8.476749
6.135946	418.866919	8.481766
6.146245	419.023067	8.486784
6.065781	427.584229	8.491802
6.375856	412.309894	8.496819
6.119620	421.898762	8.501837
6.187100	421.825111	8.506854
6.361798	425.531018	8.511872
6.222253	423.589896	8.516890
6.540093	419.289714	8.521907
5.966844	424.282820	8.526925
6.579358	411.119865	8.531942
6.502382	419.759371	8.536960
6.363557	425.139254	8.541978
6.600113	419.049848	8.546995
6.465683	429.746324	8.552013
6.289007	415.507091	8.557030
6.291227	405.746284	8.562048
6.111126	407.118601	8.567066
6.283612	407.555594	8.572083
6.606434	420.648591	8.577101
6.831471	419.641581	8.582119
6.620366	402.873729	8.587136
6.225444	407.072243	8.592154
6.388230	395.276293	8.597171
6.409312	394.597671	8.602189
6.307139	391.435809	8.607207
6.510855	397.377702	8.612224
6.135968	406.388618	8.617242
6.499424	398.057884	8.622259
6.426932	401.360481	8.627277
6.330451	392.583833	8.632295
6.200897	400.155441	8.637312
6.210499	402.561675	8.642330
6.502567	404.280178	8.647347
6.249601	398.352199	8.652365
6.350517	408.989930	8.657383
6.555374	407.093013	8.662400
6.400266	407.423229	8.667418
6.339134	413.441076	8.672435
6.454529	419.914255	8.677453
6.451678	420.722514	8.682471
6.607735	415.759589	8.687488
6.445417	414.481545	8.692506
6.527346	411.369908	8.697523
6.410146	419.024802	8.702541
6.249092	418.851040	8.707559
6.707640	415.898503	8.712576
6.078133	427.823872	8.717594
6.388679	420.157742	8.722611
6.515806	418.553779	8.727629
6.639625	425.704114	8.732647
6.836763	421.507926	8.737664
6.386210	427.535918	8.742682
6.550980	417.970692	8.747699
6.830248	417.933491	8.752717
6.417065	424.028244	8.757735
6.671815	426.645609	8.762752
6.620387	423.087696	8.767770
6.947079	419.250016	8.772787
6.608927	422.754918	8.777805
6.321953	413.884848	8.782823
6.631615	413.972297	8.787840
6.546547	422.764536	8.792858
6.686147	422.932108	8.797875
6.830733	423.386069	8.802893
6.186411	403.599438	8.807911
6.516872	410.177977	8.812928
6.741244	413.494314	8.817946
7.041271	421.737468	8.822963
6.767034	405.986096	8.827981
6.324572	401.390904	8.832999
6.736393	401.484536	8.838016
6.557865	415.526546	8.843034
6.668362	404.010118	8.848051
6.492229	402.576444	8.853069
6.528070	417.478128	8.858087
6.838601	417.963053	8.863104
6.263340	415.436552	8.868122
6.690064	417.569571	8.873139
6.584798	413.325798	8.878157
6.877699	422.570405	8.883175
6.770100	408.459271	8.888192
6.441149	424.339208	8.893210
6.634925	413.614499	8.898227
6.497327	416.542246	8.903245
6.364524	410.734403	8.908263
6.751726	413.258564	8.913280
6.467645	422.753942	8.918298
6.583080	421.451587	8.923315
6.681569	427.753840	8.928333
6.488307	422.532891	8.933351
6.582298	416.030203	8.938368
6.580473	418.848453	8.943386
6.384943	428.210133	8.948403
6.771988	446.651451	8.953421
6.639289	444.267470	8.958439
6.931100	441.372446	8.963456
6.771358	442.634303	8.968474
6.975352	440.541867	8.973491
6.924693	442.070749	8.978509
6.816830	441.096635	8.983527
7.040822	439.616438	8.988544
6.899323	440.727139	8.993562
7.056423	434.107326	8.998579
6.911947	422.791523	9.003597
6.651270	420.743035	9.008615
6.834386	414.027665	9.013632
6.673896	419.136377	9.018650
7.193616	431.911562	9.023667
6.927944	422.328149	9.028685
6.896163	422.219462	9.033703
6.958616	417.239553	9.038720
6.799884	413.490076	9.043738
6.848848	412.403188	9.048755
6.957980	414.730814	9.053773
6.760809	414.764637	9.058791
7.162006	414.093100	9.063808
6.783343	420.823074	9.068826
6.808067	412.646053	9.073843
6.955565	422.878928	9.078861
6.883127	427.999179	9.083879
7.111970	428.998572	9.088896
6.853716	432.364810	9.093914
7.080247	424.737003	9.098931
6.913294	427.385314	9.103949
6.774529	423.667438	9.108967
6.769218	433.671658	9.113984
6.938856	442.796618	9.119002
7.010119	443.706943	9.124019
7.220714	445.725300	9.129037
7.053454	441.718380	9.134055
7.271340	438.131155	9.139072
6.666833	435.959482	9.144090
6.828640	441.084289	9.149107
6.668507	429.023028	9.154125
6.867304	442.239487	9.159143
7.228048	438.907718	9.164160
7.227078	446.213183	9.169178
6.980776	436.787685	9.174195
7.116591	437.258790	9.179213
6.883657	442.132647	9.184231
6.880471	432.284309	9.189248
6.945029	444.253097	9.194266
7.061876	438.845011	9.199283
7.259775	440.606580	9.204301
7.119275	441.215376	9.209319
7.208509	432.898921	9.214336
7.065187	437.654687	9.219354
7.200676	428.946041	9.224371
7.030984	438.139609	9.229389
6.979248	439.043839	9.234407
7.102662	438.668003	9.239424
6.943240	443.779712	9.244442
6.588291	439.843039	9.249459
6.841639	438.853709	9.254477
7.104118	454.013614	9.259495
7.163723	440.195143	9.264512
6.871498	446.741264	9.269530
7.234750	456.132717	9.274547
7.321484	459.442091	9.279565
7.286136	461.337803	9.284583
7.430237	448.443402	9.289600
7.336744	445.873444	9.294618
7.133116	445.567461	9.299635
7.013904	440.148793	9.304653
6.774509	441.915334	9.309671
7.088685	453.065816	9.314688
7.326268	461.807839	9.319706
7.619679	464.049979	9.324723
7.497761	456.347029	9.329741
7.231245	455.930922	9.334759
7.165519	442.709449	9.339776
7.351414	447.748460	9.344794
7.130973	443.024019	9.349811
7.526655	452.530336	9.354829
7.042515	451.352887	9.359847
7.273083	444.200948	9.364864
6.905800	460.443475	9.369882
7.135705	464.450049	9.374899
7.554030	462.011829	9.379917
7.323977	461.552177	9.384935
7.782911	462.320097	9.389952
7.738033	458.057445	9.394970
7.087378	447.296940	9.399987
7.388994	441.891642	9.405005
6.910453	435.500178	9.410023
7.196834	459.495359	9.415040
7.395871	463.683457	9.420058
7.210794	469.023219	9.425075
7.202423	461.848517	9.430093
7.123092	468.358343	9.435111
7.487403	466.868920	9.440128
7.410199	468.909999	9.445146
7.213829	463.919884	9.450163
7.375212	461.344952	9.455181
7.697549	465.365536	9.460199
7.695661	460.187360	9.465216
7.856380	461.718046	9.470234
7.413494	459.675833	9.475251
7.785942	454.524578	9.480269
7.504271	452.570870	9.485287
7.392862	452.061189	9.490304
7.314459	452.439421	9.495322
7.343446	464.164464	9.500339
7.714934	466.703702	9.505357
7.527114	474.962880	9.510375
7.603753	466.402227	9.515392
7.555067	465.267427	9.520410
7.344268	460.708730	9.525427
7.371244	454.655098	9.530445
8.027904	467.983318	9.535463
7.768469	453.618090	9.540480
7.470109	449.136142	9.545498
7.159284	447.783393	9.550515
7.642957	451.438043	9.555533
7.568308	458.414174	9.560551
7.702614	461.476312	9.565568
7.364447	446.627909	9.570586
7.596074	451.678735	9.575603
7.591757	455.848002	9.580621
7.660000	464.505943	9.585639
7.550272	463.415359	9.590656
7.860558	468.242514	9.595674
7.419351	456.856128	9.600691
7.724019	449.194056	9.605709
7.547714	457.719664	9.610727
7.550460	464.219865	9.615744
7.854811	464.459613	9.620762
7.734927	454.184484	9.625779
7.556088	443.413635	9.630797
7.178277	446.725910	9.635815
7.655461	459.510893	9.640832
7.509499	464.203964	9.645850
7.473817	468.264513	9.650867
7.569987	469.372923	9.655885
8.035943	468.710236	9.660903
7.463868	463.437806	9.665920
7.782012	464.943981	9.670938
7.456354	466.755512	9.675955
7.676566	467.279747	9.680973
7.434874	472.142352	9.685991
7.804244	468.231748	9.691008
7.886440	472.709426	9.696026
7.621320	473.987692	9.701043
7.813375	458.371948	9.706061
7.918914	476.222839	9.711079
7.509878	462.048147	9.716096
7.581271	468.042223	9.721114
7.618864	468.752674	9.726131
7.822221	461.737502	9.731149
7.714420	464.913071	9.736167
7.247833	466.244794	9.741184
7.598740	472.542475	9.746202
7.645069	484.208029	9.751219
7.543104	492.595853	9.756237
7.947486	491.330552	9.761255
7.860932	498.390599	9.766272
8.279741	491.354494	9.771290
8.068939	498.982972	9.776307
8.076260	477.952448	9.781325
7.725386	470.777423	9.786343
7.677373	462.737931	9.791360
7.779510	472.217382	9.796378
8.040696	488.469377	9.801395
8.233997	486.179793	9.806413
7.800459	473.346909	9.811431
7.564471	475.778768	9.816448
7.766949	477.574340	9.821466
8.004040	486.875004	9.826483
7.669715	480.798726	9.831501
8.124044	492.915135	9.836519
7.441462	493.217030	9.841536
7.880850	491.614934	9.846554
7.854256	496.734377	9.851571
7.855980	490.744623	9.856589
7.773987	492.530842	9.861607
7.926844	492.260869	9.866624
8.020162	487.960915	9.871642
7.844357	501.898432	9.876659
8.200170	492.186662	9.881677
8.307046	493.684710	9.886695
7.532108	503.865599	9.891712
8.072479	491.373353	9.896730
7.930640	497.649935	9.901747
8.255281	479.324902	9.906765
8.325790	488.156064	9.911783
7.744621	490.168318	9.916800
7.838430	490.870017	9.921818
7.880613	490.737191	9.926835
8.077432	489.318023	9.931853
8.091440	494.879249	9.936871
8.115803	501.104710	9.941888
8.172996	494.247977	9.946906
7.978415	495.723536	9.951923
7.949999	492.733202	9.956941
8.257785	499.356328	9.961959
8.140885	489.951678	9.966976
8.142442	491.775379	9.971994
7.973604	504.175004	9.977011
8.047497	504.740955	9.982029
8.373090	511.228775	9.987047
8.087022	505.886557	9.992064
8.169144	497.047338	9.997082
7.953331	507.002326	10.002099
8.167636	519.556894	10.007117
8.215107	506.283037	10.012135
8.360469	515.661111	10.017152
8.464707	507.686253	10.022170
7.901120	505.953149	10.027187
8.423118	506.272614	10.032205
8.367295	507.227974	10.037223
8.289696	504.286319	10.042240
8.565463	493.302655	10.047258
8.297240	495.654332	10.052275
8.191091	491.038310	10.057293
8.345617	486.362769	10.062311
7.893045	494.925097	10.067328
7.921206	495.050063	10.072346
7.882812	496.842116	10.077363
8.344346	513.785588	10.082381
8.427269	507.833677	10.087399
8.260962	519.017986	10.092416
8.415221	511.884213	10.097434
8.363000	517.818660	10.102451
8.378980	506.613514	10.107469
8.524803	508.443156	10.112487
8.547140	509.742938	10.117504
8.741910	504.515195	10.122522
8.540835	506.367291	10.127539
8.035187	487.928535	10.132557
8.311502	490.167028	10.137575
8.083451	501.944738	10.142592
8.496655	504.622648	10.147610
8.267464	511.840602	10.152627
8.477759	516.598135	10.157645
8.647951	514.359481	10.162663
8.367804	517.691275	10.167680
8.662468	505.461326	10.172698
8.481145	514.189705	10.177715
8.855405	515.892267	10.182733
8.338220	503.425820	10.187751
7.892737	504.009522	10.192768
8.391102	501.580924	10.197786
8.617969	504.612880	10.202803
8.158646	515.135938	10.207821
8.129060	507.860384	10.212839
8.253531	515.203149	10.217856
8.626241	512.311297	10.222874
8.093347	519.081100	10.227891
8.244480	513.068076	10.232909
8.343953	514.838666	10.237927
8.581906	508.095789	10.242944
8.455964	518.914067	10.247962
8.460225	521.740853	10.252979
8.324752	535.590070	10.257997
8.427927	538.505595	10.263015
8.278977	547.677056	10.268032
8.636145	538.678232	10.273050
8.822013	534.370168	10.278067
8.564242	543.817335	10.283085
8.793178	542.926471	10.288103
8.703836	533.334479	10.293120
8.907345	533.927585	10.298138
8.917375	538.040990	10.303155
8.619771	543.799065	10.308173
8.602511	535.808398	10.313191
8.617204	529.100274	10.318208
8.513120	533.818400	10.323226
8.563702	539.115181	10.328243
8.402185	529.818438	10.333261
8.904378	534.483193	10.338279
8.732596	536.311797	10.343296
9.076754	536.876693	10.348314
8.673119	542.887952	10.353331
8.582578	540.396412	10.358349
9.134424	534.027514	10.363367
8.988287	538.212569	10.368384
8.698851	529.342824	10.373402
8.570956	532.739275	10.378419
8.475697	536.903786	10.383437
8.757762	538.759553	10.388455
8.866115	543.715995	10.393472
8.994232	537.785438	10.398490
9.165592	537.272752	10.403507
8.894957	531.410593	10.408525
8.840041	511.528917	10.413543
8.328582	519.456669	10.418560
8.688315	519.220755	10.423578
9.021953	534.413829	10.428595
9.031743	531.954004	10.433613
8.699415	537.054791	10.438631
8.445099	544.936207	10.443648
8.495189	538.392975	10.448666
8.899882	537.364298	10.453683
8.534798	537.446354	10.458701
8.597797	539.708599	10.463719
8.466542	545.977239	10.468736
8.862376	542.147702	10.473754
8.911364	531.183544	10.478771
8.788778	545.119121	10.483789
9.364119	540.706237	10.488807
8.900516	544.397945	10.493824
8.769765	539.397593	10.498842
9.000050	536.237590	10.503859
8.618917	543.409789	10.508877
9.075859	548.595968	10.513895
9.266013	560.510567	10.518912
9.341273	550.861380	10.523930
9.341152	546.209901	10.528947
8.864801	542.910619	10.533965
8.968845	544.942421	10.538983
8.937119	542.801471	10.544000
8.761805	539.512121	10.549018
8.987812	533.793533	10.554035
8.774110	550.211036	10.559053
9.247211	559.844207	10.564071
9.222148	562.328441	10.569088
9.158023	560.438675	10.574106
9.089439	559.130248	10.579123
8.948069	556.772847	10.584141
9.256322	556.907851	10.589159
9.022257	558.910249	10.594176
9.178116	561.615612	10.599194
9.507388	559.465789	10.604211
9.169133	564.236161	10.609229
9.203848	544.842246	10.614247
8.900079	550.746444	10.619264
8.843119	543.503539	10.624282
9.015457	550.438095	10.629299
9.049370	564.494481	10.634317
9.405380	564.013004	10.639335
9.116994	565.010888	10.644352
9.329564	563.084353	10.649370
9.470446	568.600603	10.654387
9.233846	569.044492	10.659405
9.441320	567.478497	10.664423
9.320211	576.749775	10.669440
9.070307	560.416989	10.674458
9.414880	558.015484	10.679475
9.212154	564.238457	10.684493
9.409221	557.410412	10.689511
9.566329	559.967264	10.694528
9.171752	551.921732	10.699546
9.348356	538.570943	10.704563
9.095125	547.272666	10.709581
9.383468	552.601857	10.714599
9.606035	559.964080	10.719616
9.237923	546.862190	10.724634
9.113873	543.634283	10.729651
9.238689	555.634788	10.734669
9.713894	558.280963	10.739687
9.416527	568.264461	10.744704
9.359578	562.495249	10.749722
9.515332	550.021821	10.754739
9.217133	547.562611	10.759757
9.547479	546.898945	10.764775
9.437864	543.441581	10.769792
8.954443	542.525935	10.774810
9.456928	548.746396	10.779827
9.401193	550.594802	10.784845
9.493626	567.087728	10.789863
9.421586	558.584893	10.794880
9.354810	563.278284	10.799898
9.727496	559.581730	10.804915
9.328879	555.124832	10.809933
9.148150	558.816680	10.814951
9.198670	560.604363	10.819968
9.174127	555.852547	10.824986
9.487115	554.213324	10.830003
9.292580	568.204300	10.835021
9.566551	567.653548	10.840039
9.352790	559.396831	10.845056
9.358666	549.376610	10.850074
9.229950	555.054747	10.855091
9.280308	566.356825	10.860109
9.459949	571.939622	10.865127
9.903393	578.263957	10.870144
9.589407	581.089811	10.875162
9.836602	578.094419	10.880179
9.715334	586.829261	10.885197
9.715009	569.760202	10.890215
9.794011	559.040652	10.895232
9.734200	561.987869	10.900250
9.786337	552.632604	10.905267
9.703280	562.317655	10.910285
9.688274	550.886942	10.915303
9.653569	551.498203	10.920320
9.626088	556.254900	10.925338
9.387598	547.869500	10.930355
9.728248	568.918446	10.935373
9.902248	570.822599	10.940391
9.996405	558.219906	10.945408
9.299464	558.798581	10.950426
9.772970	563.988498	10.955443
10.026273	573.785280	10.960461
10.073119	566.892262	10.965479
9.595104	558.793449	10.970496
9.275446	561.206789	10.975514
9.623669	567.965651	10.980531
9.855375	573.720216	10.985549
9.543748	576.100751	10.990567
10.246972	582.024893	10.995584
10.083616	581.106747	11.000602
10.428372	576.420498	11.005619
10.010240	573.374067	11.010637
9.528912	562.710200	11.015655
9.463494	559.772951	11.020672
9.922751	570.806248	11.025690
10.099583	573.887030	11.030707
9.731427	574.550209	11.035725
9.858594	578.642230	11.040743
9.976978	578.712126	11.045760
9.960562	585.278468	11.050778
10.326756	572.980534	11.055795
10.003067	563.791071	11.060813
9.513179	562.554550	11.065831
9.765929	567.258152	11.070848
9.811286	568.898323	11.075866
9.947628	576.441229	11.080883
10.000931	581.854358	11.085901
10.091460	575.866527	11.090919
10.297430	574.105114	11.095936
10.425429	579.310961	11.100954
9.864944	558.539154	11.105971
9.783899	567.403419	11.110989
10.082103	575.883605	11.116007
10.407028	570.036000	11.121024
9.934060	571.292987	11.126042
9.811822	564.653504	11.131059
9.913839	578.008204	11.136077
9.743379	574.626578	11.141095
10.153150	583.752090	11.146112
10.041431	587.922331	11.151130
10.505351	587.922650	11.156147
10.270674	584.304876	11.161165
10.101131	579.944844	11.166183
10.499029	576.055021	11.171200
9.996249	579.225837	11.176218
10.105830	571.467860	11.181235
10.409146	582.762120	11.186253
10.160257	572.945648	11.191271
10.252245	566.178140	11.196288
9.892159	575.066920	11.201306
10.257400	578.140457	11.206323
10.152943	585.525206	11.211341
10.484142	579.954321	11.216359
10.691020	571.247113	11.221376
10.026598	570.902423	11.226394
10.246664	556.550815	11.231411
9.705579	566.868892	11.236429
9.813709	582.318014	11.241447
10.204516	582.777823	11.246464
9.990421	584.590930	11.251482
10.292261	589.006039	11.256499
10.208124	584.178290	11.261517
10.427588	578.296611	11.266535
10.563891	582.712246	11.271552
10.314963	583.659807	11.276570
10.549252	577.624348	11.281587
10.561338	585.107711	11.286605
10.465808	580.196534	11.291623
10.479991	573.652568	11.296640
10.180282	578.912384	11.301658
10.321958	577.284053	11.306675
10.770197	582.572579	11.311693
10.528552	589.685211	11.316711
10.787742	581.298045	11.321728
10.272103	589.239100	11.326746
10.487681	587.283694	11.331763
10.476849	584.817605	11.336781
10.344919	587.091272	11.341799
10.722685	582.002266	11.346816
10.316365	579.480994	11.351834
10.378204	577.653662	11.356851
10.608041	583.515814	11.361869
10.492961	583.079282	11.366887
10.836072	587.882425	11.371904
10.436607	575.498580	11.376922
10.420435	581.575752	11.381939
10.291452	581.160319	11.386957
10.908370	591.708353	11.391975
10.408140	581.867894	11.396992
10.281041	585.377836	11.402010
10.427194	580.567880	11.407027
10.306771	574.145853	11.412045
10.550260	584.120887	11.417063
10.505164	579.438534	11.422080
10.354609	591.601853	11.427098
10.347199	579.513557	11.432115
10.508593	585.471569	11.437133
10.586328	598.445072	11.442151
10.883558	603.533063	11.447168
10.866687	605.451159	11.452186
10.894454	594.610183	11.457203
10.765949	584.045998	11.462221
10.760986	581.597930	11.467239
10.944820	577.728812	11.472256
10.331077	578.616414	11.477274
10.791296	581.318572	11.482291
10.992624	577.086983	11.487309
10.726280	584.010961	11.492327
11.061453	570.064282	11.497344
10.157413	576.816156	11.502362
10.552690	585.221275	11.507379
10.854739	592.425975	11.512397
10.825254	594.778363	11.517415
11.138632	598.775127	11.522432
10.919397	594.624792	11.527450
10.731523	588.449938	11.532467
10.692074	594.915732	11.537485
10.684955	603.191015	11.542503
10.769167	607.914556	11.547520
10.802723	608.792892	11.552538
10.835770	613.467599	11.557555
11.048028	604.046353	11.562573
11.038541	613.852516	11.567591
10.977986	606.742683	11.572608
11.076175	613.862372	11.577626
10.993479	612.136432	11.582643
11.257745	604.499519	11.587661
10.950618	605.784334	11.592679
10.845848	609.306582	11.597696
10.914939	613.707444	11.602714
10.759579	604.703182	11.607731
11.108741	612.153010	11.612749
10.741387	608.644248	11.617767
10.949072	610.934466	11.622784
11.047782	612.736741	11.627802
10.815866	613.214614	11.632819
10.814436	609.898178	11.637837
10.825259	614.992896	11.642855
11.179972	607.278786	11.647872
11.118288	611.832547	11.652890
11.150030	609.713263	11.657907
11.194385	603.742079	11.662925
11.019145	608.420812	11.667943
11.361822	596.568320	11.672960
11.276202	603.041306	11.677978
11.164157	612.349060	11.682995
11.442307	607.935095	11.688013
10.963531	614.175819	11.693031
11.131808	608.078046	11.698048
10.992789	610.848263	11.703066
10.946865	610.170597	11.708083
11.005197	608.091353	11.713101
11.244052	613.873220	11.718119
11.317297	604.621934	11.723136
11.128145	615.753058	11.728154
11.042533	617.079122	11.733171
11.263505	599.208747	11.738189
11.038684	615.845785	11.743207
11.297298	625.496608	11.748224
11.348312	632.068247	11.753242
11.487184	633.056415	11.758259
11.634615	629.325493	11.763277
10.951156	617.673775	11.768295
11.484708	619.695516	11.773312
11.336893	619.964642	11.778330
11.250713	632.259972	11.783347
11.601111	621.636980	11.788365
11.147209	619.807895	11.793383
11.621122	617.995293	11.798400
11.542521	623.681427	11.803418
11.476611	614.672701	11.808435
11.493154	599.989841	11.813453
11.183800	605.087071	11.818471
11.708233	616.583603	11.823488
11.438792	610.036447	11.828506
11.245250	610.281136	11.833523
11.623256	611.342519	11.838541
11.628422	625.397118	11.843559
11.524606	605.425125	11.848576
11.701991	604.835763	11.853594
11.261319	602.408195	11.858611
11.485335	604.736894	11.863629
11.432601	621.956191	11.868647
11.477305	631.529873	11.873664
11.794296	626.806911	11.878682
11.421419	624.081616	11.883699
11.887581	617.681850	11.888717
11.722719	624.473283	11.893735
11.402715	611.329143	11.898752
11.550506	619.914817	11.903770
11.382491	622.967250	11.908787
11.588970	623.395801	11.913805
11.778856	632.217915	11.918823
11.681894	625.467181	11.923840
11.349529	625.288532	11.928858
11.480307	634.984509	11.933875
12.040942	621.315100	11.938893
11.747164	631.806141	11.943911
11.554482	631.615211	11.948928
11.843030	625.214694	11.953946
11.688639	628.164025	11.958963
11.779628	630.661756	11.963981
11.617130	634.221398	11.968999
11.854361	636.412349	11.974016
11.875220	642.594226	11.979034
11.674566	639.536012	11.984051
11.754322	633.508815	11.989069
11.472451	640.492035	11.994087
11.998522	635.035954	11.999104
11.872734	628.441180	12.004122
11.650418	634.724029	12.009139
12.037472	629.018205	12.014157
12.177710	627.276488	12.019175
12.016900	624.467684	12.024192
12.081547	627.925690	12.029210
12.007030	631.642041	12.034227
11.800379	618.776882	12.039245
12.202843	632.479306	12.044263
12.288396	632.383906	12.049280
11.846882	627.147901	12.054298
11.526559	627.680563	12.059315
12.088445	626.255036	12.064333
11.791920	627.279436	12.069351
11.936669	632.331217	12.074368
11.681985	634.740763	12.079386
11.254599	640.579033	12.084403
11.517536	636.028580	12.089421
11.877019	650.839046	12.094439
12.208684	664.432602	12.099456
12.040048	656.970360	12.104474
11.759434	660.371679	12.109491
12.153559	659.117431	12.114509
12.501654	657.166630	12.119527
12.184204	660.497947	12.124544
12.505869	650.917635	12.129562
12.238066	657.122371	12.134579
12.165501	643.040309	12.139597
11.984897	636.217389	12.144615
12.190290	640.316180	12.149632
12.244262	646.742202	12.154650
12.138722	656.932560	12.159667
12.548978	656.549929	12.164685
12.144300	638.126852	12.169703
11.949361	637.532345	12.174720
12.512229	642.055143	12.179738
12.056727	645.985444	12.184755
12.290672	649.193041	12.189773
12.394350	652.389363	12.194791
12.298470	651.381815	12.199808
12.460548	651.271345	12.204826
12.075268	656.465615	12.209843
12.587157	644.750841	12.214861
12.392453	659.287850	12.219879
12.290332	652.380124	12.224896
12.366510	642.607672	12.229914
11.849235	654.881778	12.234931
12.274158	648.674607	12.239949
12.184321	655.457527	12.244967
12.095501	654.010237	12.249984
11.971682	653.736004	12.255002
11.856206	665.417402	12.260019
12.258271	652.132408	12.265037
12.251577	654.001589	12.270055
12.434496	666.072015	12.275072
12.722281	672.742500	12.280090
12.950931	668.800115	12.285107
12.354187	662.821434	12.290125
12.378946	652.867641	12.295143
12.219928	650.961083	12.300160
12.859955	662.326042	12.305178
12.279325	666.225337	12.310195
12.657256	660.599815	12.315213
12.816006	676.337774	12.320231
12.312449	673.784292	12.325248
12.647839	671.592478	12.330266
12.867814	685.001474	12.335283
12.995414	669.850001	12.340301
12.594336	656.194605	12.345319
12.432828	661.622270	12.350336
12.895509	655.563847	12.355354
12.347613	671.153055	12.360371
12.662546	666.061186	12.365389
12.788745	667.818163	12.370407
12.788929	676.448936	12.375424
12.574905	673.626321	12.380442
12.790297	669.910054	12.385459
12.654186	667.930503	12.390477
13.146756	682.461507	12.395495
12.879723	670.451439	12.400512
12.845560	655.441925	12.405530
12.467225	656.147716	12.410547
12.673209	657.141214	12.415565
12.839263	664.256668	12.420583
12.743533	673.849082	12.425600
13.092122	670.910469	12.430618
12.910341	680.759273	12.435635
12.768733	668.827505	12.440653
13.077480	668.842517	12.445671
12.890274	669.023106	12.450688
12.971140	660.777272	12.455706
12.869303	655.652469	12.460723
12.692975	648.611136	12.465741
12.899737	660.873498	12.470759
12.741496	674.940956	12.475776
13.108866	664.791806	12.480794
13.133110	673.393586	12.485811
13.140790	673.016831	12.490829
13.085012	667.894320	12.495847
12.793556	666.046249	12.500864
13.034944	664.841026	12.505882
12.919727	673.865293	12.510899
13.139150	669.141732	12.515917
13.182876	677.465935	12.520935
12.691662	678.864621	12.525952
13.058830	676.387002	12.530970
12.959207	671.962414	12.535987
13.179686	672.180511	12.541005
13.265542	675.329122	12.546023
12.617776	681.836013	12.551040
13.248533	674.337662	12.556058
13.430487	680.431356	12.561075
12.953435	681.076781	12.566093
13.203059	677.935832	12.571111
13.112368	673.601368	12.576128
13.327464	673.044001	12.581146
13.301257	676.535097	12.586163
13.211477	679.569047	12.591181
13.544682	680.470158	12.596199
13.350935	677.701187	12.601216
13.256478	674.916758	12.606234
13.217574	676.014655	12.611251
13.091024	682.269988	12.616269
13.308251	676.167726	12.621287
13.104823	679.938870	12.626304
13.182068	681.712938	12.631322
13.443663	674.720173	12.636339
13.162221	679.986642	12.641357
13.348668	671.109003	12.646375
13.050558	677.864400	12.651392
13.480871	668.791009	12.656410
12.916373	670.131679	12.661427
12.703793	675.961762	12.666445
13.394361	690.124286	12.671463
13.516918	700.020388	12.676480
13.711565	690.989989	12.681498
13.780514	694.393691	12.686515
13.625972	684.818079	12.691533
13.581479	674.651001	12.696551
13.392058	670.925182	12.701568
13.432984	671.171234	12.706586
13.276335	683.550152	12.711603
13.156487	703.332939	12.716621
13.327317	699.399549	12.721639
13.437630	708.991459	12.726656
13.607289	700.561374	12.731674
13.557220	707.104600	12.736691
13.523796	705.579256	12.741709
13.543306	700.779518	12.746727
13.701237	701.913040	12.751744
13.477684	702.329655	12.756762
13.699542	695.942652	12.761779
13.877173	697.218269	12.766797
13.660414	687.680744	12.771815
13.693673	694.068984	12.776832
13.615380	696.144972	12.781850
13.892356	696.224889	12.786867
13.489069	693.182437	12.791885
13.687703	687.717362	12.796903
13.200569	695.701362	12.801920
13.586257	690.169294	12.806938
13.775019	694.188638	12.811955
13.607800	697.569153	12.816973
14.026650	706.507129	12.821991
13.975132	713.596519	12.827008
13.896809	705.473276	12.832026
13.954413	692.027295	12.837043
13.614951	701.332635	12.842061
14.152004	700.854523	12.847079
13.645378	700.157069	12.852096
13.901901	705.661668	12.857114
14.281442	705.372177	12.862131
13.835677	697.514424	12.867149
13.946250	697.396194	12.872167
13.732889	705.855109	12.877184
13.933250	714.464200	12.882202
14.093019	712.135629	12.887219
13.858657	716.643721	12.892237
14.576471	715.222311	12.897255
13.905651	705.629243	12.902272
14.005457	699.472674	12.907290
14.126583	709.454208	12.912307
13.881828	705.465605	12.917325
14.220563	713.475659	12.922343
14.126100	718.823477	12.927360
14.130693	715.430347	12.932378
13.854318	705.431894	12.937395
14.189691	719.097495	12.942413
14.255397	713.384874	12.947431
14.138904	720.686348	12.952448
14.571149	710.959404	12.957466
14.468153	710.502053	12.962483
14.145685	703.130012	12.967501
14.178356	691.672851	12.972519
13.647148	698.887412	12.977536
13.979085	708.309121	12.982554
14.520968	710.783997	12.987571
14.413476	712.264948	12.992589
14.396905	712.728229	12.997607
14.492940	704.281204	13.002624
14.192860	707.278477	13.007642
14.582206	701.061049	13.012659
14.144849	713.789796	13.017677
14.428606	708.216790	13.022695
14.158984	717.839458	13.027712
14.140948	710.331656	13.032730
14.529780	709.841909	13.037747
14.226485	723.329249	13.042765
14.629863	702.085323	13.047783
14.767721	712.802688	13.052800
14.572007	713.751438	13.057818
14.546700	715.229061	13.062835
15.085950	716.988003	13.067853
14.459529	699.173726	13.072871
14.131503	708.688721	13.077888
14.257794	706.630442	13.082906
14.389158	704.899566	13.087923
14.232897	718.853144	13.092941
14.580482	712.796843	13.097959
14.431971	719.585767	13.102976
14.191583	725.884085	13.107994
14.606742	715.276200	13.113011
14.392860	726.698413	13.118029
14.339002	724.362077	13.123047
14.246949	724.461582	13.128064
14.360420	727.953030	13.133082
14.949115	727.217577	13.138099
14.598816	736.177494	13.143117
14.894319	728.702916	13.148135
14.642988	729.953808	13.153152
14.884870	732.469084	13.158170
14.842464	716.419418	13.163187
14.713650	709.033003	13.168205
14.515245	716.861609	13.173223
14.606868	733.695632	13.178240
14.914025	733.477370	13.183258
14.979148	737.695849	13.188275
14.810811	740.745196	13.193293
14.794706	742.199299	13.198311
15.124388	743.738415	13.203328
15.229970	740.566235	13.208346
15.091744	730.202286	13.213363
14.848374	729.851994	13.218381
14.896381	715.722701	13.223399
14.344125	719.074809	13.228416
14.337324	729.492825	13.233434
14.713101	729.680431	13.238451
14.534851	739.519251	13.243469
14.888434	737.072141	13.248487
14.840157	746.016596	13.253504
14.784445	748.029115	13.258522
15.370334	746.281115	13.263539
15.144592	745.088659	13.268557
15.219322	748.901714	13.273575
15.098076	748.608145	13.278592
14.800170	752.599135	13.283610
15.417934	745.453062	13.288627
14.922214	744.949561	13.293645
14.726980	749.855500	13.298663
14.963375	742.825607	13.303680
14.801382	745.583643	13.308698
15.355844	745.774986	13.313715
15.318412	754.831364	13.318733
15.141369	751.993510	13.323751
15.046615	751.509629	13.328768
15.239906	763.146173	13.333786
15.737236	763.254897	13.338803
15.454275	754.024280	13.343821
15.219790	745.095381	13.348839
15.400271	740.459912	13.353856
15.241658	747.572302	13.358874
15.521377	733.192330	13.363891
15.259164	742.100667	13.368909
15.121664	739.048382	13.373927
15.058817	733.955354	13.378944
15.272832	755.655380	13.383962
15.686383	758.954950	13.388979
15.441664	764.294619	13.393997
15.416961	763.067705	13.399015
15.237632	760.100822	13.404032
15.375258	759.097936	13.409050
15.456597	762.304068	13.414067
15.824240	770.429564	13.419085
15.445455	765.824361	13.424103
15.581410	756.623191	13.429120
15.628842	765.660050	13.434138
15.432209	766.094564	13.439155
15.565178	759.658264	13.444173
15.680453	757.406040	13.449191
15.972324	757.837078	13.454208
15.700066	745.155606	13.459226
15.851706	735.361887	13.464243
15.547837	743.797043	13.469261
15.654890	736.399139	13.474279
15.673116	733.313142	13.479296
15.606783	738.612407	13.484314
15.580406	736.243388	13.489331
15.339156	734.646261	13.494349
15.456401	751.536271	13.499367
15.624783	756.991495	13.504384
15.784374	756.733093	13.509402
16.331087	761.741262	13.514419
15.888730	762.232969	13.519437
15.757806	753.934862	13.524455
15.835065	738.371459	13.529472
15.475751	747.831388	13.534490
16.073073	752.721225	13.539507
15.808898	758.710842	13.544525
15.644222	759.780991	13.549543
16.007210	759.689731	13.554560
16.278725	759.795744	13.559578
15.748960	747.441533	13.564595
15.669211	750.076314	13.569613
16.059692	761.044702	13.574631
16.309212	751.065326	13.579648
15.690135	758.309371	13.584666
16.260563	756.286074	13.589683
16.018280	761.240366	13.594701
15.722836	758.165333	13.599719
15.973185	762.130924	13.604736
15.648328	762.310855	13.609754
15.998023	766.361962	13.614771
15.895845	756.787625	13.619789
15.698091	754.120249	13.624807
15.916270	760.012677	13.629824
15.715301	768.690591	13.634842
15.988139	761.020719	13.639859
16.156136	766.179369	13.644877
15.740511	761.513633	13.649895
15.929167	771.733989	13.654912
15.995115	781.358092	13.659930
16.288667	781.208217	13.664947
16.258237	788.013495	13.669965
15.919211	800.285193	13.674983
16.177330	788.284797	13.680000
16.152701	787.550162	13.685018
16.117449	788.609629	13.690035
16.384891	799.215355	13.695053
16.221221	786.087769	13.700071
16.579421	782.750021	13.705088
16.335163	791.226410	13.710106
16.544850	780.975516	13.715123
16.599920	784.567584	13.720141
16.324368	781.890226	13.725159
16.461531	776.687152	13.730176
16.269514	787.339161	13.735194
16.328797	781.864196	13.740211
16.429351	788.961497	13.745229
16.499266	776.116278	13.750247
16.530853	775.805224	13.755264
16.698326	780.515848	13.760282
17.053909	783.695064	13.765299
16.778631	781.323768	13.770317
16.605542	782.761291	13.775335
16.787131	783.177943	13.780352
16.467184	787.857164	13.785370
16.372605	783.387583	13.790387
16.557952	783.128326	13.795405
16.526634	785.512582	13.800423
16.505456	780.867476	13.805440
16.388857	783.889841	13.810458
16.455043	777.432375	13.815475
16.810873	782.255681	13.820493
16.443470	784.165258	13.825511
16.436154	777.018667	13.830528
16.570366	809.564761	13.835546
17.292056	796.564401	13.840563
16.949295	791.937805	13.845581
16.501573	786.484974	13.850599
16.941531	790.196993	13.855616
16.796319	801.924135	13.860634
16.868680	806.630640	13.865651
17.198714	796.572434	13.870669
16.754805	795.890456	13.875687
16.631430	793.227272	13.880704
16.850991	804.266477	13.885722
17.111150	812.553890	13.890739
17.177532	805.064462	13.895757
16.957225	803.896402	13.900775
17.107771	799.713691	13.905792
16.538085	786.829196	13.910810
17.102649	799.957416	13.915827
17.280763	796.852826	13.920845
17.188388	806.571018	13.925863
17.184058	798.581375	13.930880
17.016192	787.218489	13.935898
16.915779	801.684131	13.940915
17.178607	796.297388	13.945933
17.033702	804.206063	13.950951
17.206517	795.027536	13.955968
16.961942	804.990324	13.960986
17.332245	799.252341	13.966003
17.332320	793.994868	13.971021
16.932633	802.760542	13.976039
17.360582	799.500292	13.981056
17.200945	792.626712	13.986074
17.281172	791.859973	13.991091
17.587551	800.045512	13.996109
17.262817	802.323979	14.001127
17.679176	802.581005	14.006144
17.394988	798.364998	14.011162
17.506209	797.596589	14.016179
17.505303	781.688721	14.021197
17.143220	774.026182	14.026215
17.023028	788.507515	14.031232
17.427515	797.545600	14.036250
17.344334	800.417602	14.041267
17.235108	792.324377	14.046285
17.031753	805.344951	14.051303
17.416118	794.779682	14.056320
17.199771	794.027561	14.061338
17.087406	798.412540	14.066355
17.431477	795.976370	14.071373
17.196693	802.816626	14.076391
17.585673	816.578095	14.081408
17.456582	816.796973	14.086426
17.463991	814.397438	14.091443
17.757911	816.080981	14.096461
17.726660	817.903512	14.101479
17.720396	813.139313	14.106496
17.975637	817.372391	14.111514
17.780256	820.214529	14.116531
17.891319	798.388011	14.121549
17.472623	796.222074	14.126567
17.168951	794.852405	14.131584
17.747647	814.346679	14.136602
17.698006	811.694102	14.141619
17.855894	809.286918	14.146637
17.939347	818.741061	14.151655
18.423786	818.782367	14.156672
18.305785	815.629205	14.161690
17.852394	801.202379	14.166707
17.741077	785.535754	14.171725
17.693569	792.084924	14.176743
17.681430	789.240324	14.181760
17.842120	802.816425	14.186778
17.575832	812.814156	14.191795
18.324625	811.236441	14.196813
17.946135	816.931460	14.201831
17.839248	815.275537	14.206848
17.813364	818.760298	14.211866
17.877859	811.839191	14.216883
18.171906	809.423431	14.221901
18.060278	815.326202	14.226919
18.085780	816.925307	14.231936
18.101205	819.441141	14.236954
17.946186	817.010093	14.241971
18.089953	806.081501	14.246989
17.835337	821.375875	14.252007
17.885547	814.384410	14.257024
18.094986	809.119582	14.262042
18.057053	803.785976	14.267059
18.181985	807.016886	14.272077
18.322204	812.160940	14.277095
18.385334	816.307167	14.282112
18.114347	817.747312	14.287130
18.162988	821.375101	14.292147
18.303792	809.746397	14.297165
18.189620	814.109572	14.302183
18.196311	818.491798	14.307200
18.034935	821.934541	14.312218
18.343089	833.411240	14.317235
18.574381	836.168015	14.322253
18.399749	848.808618	14.327271
18.422599	833.269381	14.332288
18.455364	840.434060	14.337306
18.334188	837.003685	14.342323
18.374721	831.626296	14.347341
18.572535	838.711629	14.352359
18.536317	835.719296	14.357376
18.707903	838.406475	14.362394
18.727305	832.328649	14.367411
18.648585	827.985972	14.372429
18.134600	833.859878	14.377447
18.526491	842.230934	14.382464
18.838606	832.964429	14.387482
18.791291	830.361979	14.392499
19.050802	830.974778	14.397517
18.280535	838.349688	14.402535
18.637683	831.992064	14.407552
18.897362	826.709942	14.412570
19.193860	827.304359	14.417587
18.930428	826.670018	14.422605
18.627011	830.128566	14.427623
18.663496	825.364020	14.432640
18.728274	823.649812	14.437658
18.584361	824.227594	14.442675
18.899802	824.124803	14.447693
18.725536	833.467605	14.452711
18.700736	837.349823	14.457728
19.047935	829.090846	14.462746
18.497458	836.128586	14.467763
18.679849	829.602517	14.472781
18.543466	831.577113	14.477799
18.894924	837.029104	14.482816
18.973807	832.967994	14.487834
18.947266	841.186452	14.492851
19.091098	847.229336	14.497869
18.802507	843.477895	14.502887
19.103267	856.921780	14.507904
19.318039	854.032373	14.512922
19.224694	857.139491	14.517939
19.637960	844.994983	14.522957
19.215025	835.483168	14.527975
19.074129	840.926612	14.532992
18.928848	823.078324	14.538010
18.929396	834.615539	14.543027
19.293037	847.765611	14.548045
19.083241	839.249376	14.553063
19.277476	847.083177	14.558080
19.096155	846.811582	14.563098
19.362349	859.279419	14.568115
19.024874	854.973867	14.573133
19.315234	857.582596	14.578151
19.399745	856.158795	14.583168
19.419746	849.951485	14.588186
19.418957	859.245201	14.593203
19.333071	857.052686	14.598221
19.662991	854.284204	14.603239
19.144449	851.739340	14.608256
19.442259	846.716356	14.613274
19.154118	850.399742	14.618291
19.452772	852.880951	14.623309
19.195647	854.167466	14.628327
19.213251	851.898879	14.633344
19.552844	852.868431	14.638362
19.419254	851.822562	14.643379
19.657169	846.894108	14.648397
19.741449	849.992504	14.653415
19.529252	850.981696	14.658432
19.546090	844.045907	14.663450
19.476082	852.845480	14.668467
19.586056	856.924464	14.673485
19.675826	855.241074	14.678503
19.638839	873.237628	14.683520
20.054259	877.306929	14.688538
19.597240	874.187606	14.693555
19.951118	878.010875	14.698573
19.966373	862.700008	14.703591
19.960336	863.467759	14.708608
20.194362	854.775121	14.713626
19.720103	856.426795	14.718643
19.619109	855.593596	14.723661
19.413539	859.999413	14.728679
19.927614	868.105311	14.733696
20.174277	872.614286	14.738714
19.925736	876.395651	14.743731
20.137605	870.764361	14.748749
20.043333	881.281290	14.753767
19.976439	878.508315	14.758784
20.076806	862.044978	14.763802
20.241308	876.766073	14.768819
19.751610	868.896149	14.773837
20.456847	870.231641	14.778855
20.229404	864.091253	14.783872
20.114883	847.348968	14.788890
19.924704	865.217890	14.793907
20.096237	862.669722	14.798925
20.364247	867.661355	14.803943
20.078845	877.191893	14.808960
20.258698	875.746935	14.813978
20.649380	881.842914	14.818995
20.408487	866.051229	14.824013
20.456176	852.988514	14.829031
20.049681	856.333731	14.834048
20.306174	843.320562	14.839066
20.229104	856.624461	14.844083
19.950135	868.893168	14.849101
20.406433	875.638477	14.854119
19.988688	871.986032	14.859136
20.267007	879.443847	14.864154
20.193491	880.723866	14.869171
20.378229	878.912082	14.874189
19.963964	874.287129	14.879207
19.683796	878.054484	14.884224
20.021002	876.745969	14.889242
20.296546	904.716509	14.894259
20.375857	896.593882	14.899277
21.047973	894.706214	14.904295
20.843402	894.119508	14.909312
20.957089	886.714197	14.914330
21.124166	890.301471	14.919347
20.747864	878.144176	14.924365
21.025359	873.572462	14.929383
20.647286	873.934245	14.934400
20.865610	871.855306	14.939418
20.768009	866.158595	14.944435
20.186571	860.082791	14.949453
20.691039	859.193193	14.954471
20.169096	871.566002	14.959488
20.653501	881.730907	14.964506
21.026899	889.909209	14.969523
20.894982	890.216889	14.974541
21.103483	886.836158	14.979559
21.179055	893.886899	14.984576
21.159193	893.233566	14.989594
21.053638	891.902470	14.994611
20.705102	882.353799	14.999629
20.830373	874.220871	15.004647
20.902502	889.653776	15.009664
21.183402	883.402677	15.014682
20.899944	898.875175	15.019699
21.339961	898.857126	15.024717
21.238854	895.041771	15.029735
20.984446	892.171761	15.034752
21.327384	889.451738	15.039770
21.232915	882.407034	15.044787
20.763856	893.531420	15.049805
21.043125	882.417586	15.054823
21.079182	887.274929	15.059840
21.404292	883.446864	15.064858
20.987106	889.788545	15.069875
20.972786	888.954473	15.074893
21.048428	886.459100	15.079911
21.006956	893.117817	15.084928
20.835074	882.942053	15.089946
21.311830	895.156229	15.094963
21.073715	901.381673	15.099981
21.833766	902.749658	15.104999
21.401340	908.576177	15.110016
21.421826	893.062502	15.115034
21.435741	902.874648	15.120051
21.438410	902.261988	15.125069
21.761912	911.909176	15.130087
21.662919	902.368978	15.135104
21.421979	890.089617	15.140122
21.190233	890.415995	15.145139
21.716375	906.245275	15.150157
21.785870	900.229053	15.155175
21.700526	907.636205	15.160192
21.822062	901.419380	15.165210
21.547209	888.779234	15.170227
21.613138	891.176764	15.175245
21.857043	900.564945	15.180263
21.593218	900.495539	15.185280
21.887167	895.722446	15.190298
21.863546	903.441872	15.195315
21.811488	902.418019	15.200333
21.794679	885.827739	15.205351
21.794257	882.845603	15.210368
21.601207	899.187631	15.215386
21.649961	898.100746	15.220403
21.804237	911.901987	15.225421
22.246444	902.163920	15.230439
22.175163	909.445810	15.235456
21.949631	905.678227	15.240474
21.510808	904.632542	15.245491
21.678383	909.791300	15.250509
22.200228	903.010385	15.255527
21.849448	910.342103	15.260544
21.736868	910.021935	15.265562
22.213975	913.630369	15.270579
21.659042	907.118086	15.275597
22.059135	904.657400	15.280615
21.690477	909.486245	15.285632
21.976117	899.955589	15.290650
22.116150	903.127362	15.295667
21.757613	922.979113	15.300685
22.338608	929.140150	15.305703
22.513225	925.559565	15.310720
22.287000	921.467044	15.315738
22.605234	926.264685	15.320755
22.266277	923.628735	15.325773
22.411549	911.191400	15.330791
22.064993	918.197422	15.335808
22.191576	916.419934	15.340826
22.332928	920.588720	15.345843
22.057993	935.898979	15.350861
22.539753	927.637941	15.355879
22.462562	930.922433	15.360896
22.389355	934.149503	15.365914
22.582623	923.831657	15.370931
22.444811	935.071750	15.375949
22.657405	929.279386	15.380967
22.282051	929.968944	15.385984
22.052348	932.406197	15.391002
22.628261	925.219232	15.396019
22.238088	928.400978	15.401037
22.782225	931.333118	15.406055
22.852381	942.376737	15.411072
22.642044	934.507469	15.416090
23.037265	933.246720	15.421107
22.547838	937.646260	15.426125
22.609476	938.365609	15.431143
22.438931	937.268685	15.436160
23.039063	949.832912	15.441178
22.857954	948.488329	15.446195
22.717296	954.304149	15.451213
23.178012	940.684766	15.456231
23.056641	947.898733	15.461248
23.281767	951.028864	15.466266
23.171753	940.871835	15.471283
22.746222	933.114966	15.476301
22.815839	932.412987	15.481319
23.032258	939.918334	15.486336
22.877778	947.516144	15.491354
23.153109	948.561978	15.496371
23.326922	948.512794	15.501389
22.918977	943.416632	15.506407
23.207995	947.013333	15.511424
23.202928	950.756806	15.516442
23.166227	952.147862	15.521459
23.210517	946.312270	15.526477
23.202818	939.288748	15.531495
22.831174	951.152225	15.536512
22.933057	947.690256	15.541530
23.492034	953.220424	15.546547
23.273172	949.148841	15.551565
23.105588	951.532244	15.556583
23.102737	947.423874	15.561600
23.278258	942.249493	15.566618
23.439962	941.624693	15.571635
23.738267	944.604578	15.576653
23.377878	942.719873	15.581671
23.613869	954.687560	15.586688
23.171627	945.295454	15.591706
23.749389	945.107639	15.596723
23.334934	940.845609	15.601741
23.486387	941.699294	15.606759
23.413668	946.299039	15.611776
23.322445	952.211301	15.616794
23.982739	949.621736	15.621811
23.329746	959.455699	15.626829
23.729587	960.927108	15.631847
24.007690	965.194531	15.636864
23.529224	960.705781	15.641882
23.733446	959.689359	15.646899
23.726300	974.430948	15.651917
23.693415	969.046014	15.656935
23.565167	967.996151	15.661952
23.552357	974.615723	15.666970
23.846013	964.234888	15.671987
23.802510	977.306438	15.677005
23.669030	971.971878	15.682023
23.725861	975.895065	15.687040
23.428647	976.550368	15.692058
23.844589	968.476280	15.697075
23.740437	976.520695	15.702093
24.056602	990.164250	15.707111
24.026815	994.826750	15.712128
24.286055	988.727307	15.717146
24.146228	976.634111	15.722163
24.265676	979.297871	15.727181
24.361600	968.518638	15.732199
24.476702	961.706356	15.737216
24.136113	968.099254	15.742234
24.450785	966.131533	15.747251
24.579535	967.720889	15.752269
24.336813	971.179481	15.757287
24.289756	963.571951	15.762304
24.526661	962.171751	15.767322
24.538131	960.200746	15.772339
24.219735	964.744074	15.777357
24.069409	969.160252	15.782375
24.364068	964.043053	15.787392
24.186344	971.956912	15.792410
24.589072	968.085187	15.797427
24.358270	961.172130	15.802445
24.411317	969.457149	15.807463
24.740867	965.309645	15.812480
24.522756	971.487818	15.817498
24.836184	964.957076	15.822515
24.478052	969.670691	15.827533
24.565013	966.769608	15.832551
24.471130	966.885178	15.837568
24.629216	980.553338	15.842586
24.975014	981.531398	15.847603
24.769290	980.462039	15.852621
24.408138	970.694383	15.857639
24.434319	969.869780	15.862656
24.461440	988.323520	15.867674
24.361598	978.556199	15.872691
24.599594	988.440800	15.877709
24.507175	985.627603	15.882727
24.463747	986.151876	15.887744
24.263247	993.018425	15.892762
24.754339	1002.658504	15.897779
24.939850	1008.073269	15.902797
25.221242	1007.047986	15.907815
25.355202	1003.988104	15.912832
25.388931	994.906867	15.917850
25.625012	987.248932	15.922867
25.347223	977.048578	15.927885
25.428553	967.243589	15.932903
25.278901	969.456948	15.937920
25.131376	971.048293	15.942938
25.476180	963.969878	15.947955
25.622263	966.162438	15.952973
25.284130	974.905989	15.957991
25.691180	967.738987	15.963008
25.589750	970.121561	15.968026
25.599551	968.497947	15.973043
25.261741	963.769550	15.978061
25.435363	965.389788	15.983079
25.249721	951.517588	15.988096
25.421705	961.115811	15.993114
25.763562	960.573413	15.998131
25.403274	961.472061	16.003149
25.262447	959.073496	16.008167
25.823056	957.291544	16.013184
25.311494	960.205022	16.018202
25.110393	964.423980	16.023219
25.425799	971.894994	16.028237
25.456647	970.072448	16.033255
25.675617	958.374673	16.038272
25.354423	969.577069	16.043290
25.609616	964.308227	16.048307
25.384898	964.674537	16.053325
25.276045	978.485240	16.058343
25.466779	972.172411	16.063360
25.456988	983.654529	16.068378
25.545669	990.141543	16.073395
25.837296	984.251651	16.078413
25.953957	994.843101	16.083431
25.647983	992.918361	16.088448
25.610506	997.358000	16.093466
25.933547	1003.025903	16.098483
25.908456	995.304488	16.103501
25.514621	1000.452852	16.108519
26.012838	996.701951	16.113536
25.755230	995.517595	16.118554
25.790205	993.135835	16.123571
25.841095	1004.239295	16.128589
26.383410	1024.727217	16.133607
26.583758	1006.029680	16.138624
26.001130	1003.153950	16.143642
25.977777	999.862945	16.148659
26.258250	1001.106793	16.153677
26.187670	1002.922843	16.158695
26.310471	1006.150966	16.163712
26.137545	1008.099714	16.168730
26.291742	1017.363071	16.173747
26.346014	1002.891752	16.178765
26.319931	1012.757523	16.183783
26.766970	1003.637178	16.188800
26.585528	1009.790720	16.193818
26.330514	1007.690790	16.198835
26.799124	1008.438295	16.203853
26.324529	997.047293	16.208871
26.544926	998.316273	16.213888
26.223490	1007.221340	16.218906
26.597492	1007.800541	16.223923
26.758836	1005.976608	16.228941
26.455937	1008.800802	16.233959
26.783389	1006.506045	16.238976
26.617188	1013.812223	16.243994
26.415020	1009.905282	16.249011
26.714293	1009.031847	16.254029
26.755308	1011.884546	16.259047
26.480504	1010.248437	16.264064
26.620576	1010.996602	16.269082
26.412845	1011.587482	16.274099
26.846023	1010.096760	16.279117
26.563531	1012.933557	16.284135
26.754309	1003.543846	16.289152
26.448699	1002.385897	16.294170
27.035104	1009.726373	16.299187
26.851312	1023.785461	16.304205
26.766439	1028.964623	16.309223
27.276760	1024.738468	16.314240
27.198576	1030.860162	16.319258
26.958302	1030.272699	16.324275
27.107642	1025.954426	16.329293
26.959462	1026.930505	16.334311
27.201843	1027.195689	16.339328
27.298917	1035.066791	16.344346
27.221065	1030.477780	16.349363
27.562591	1030.819045	16.354381
26.654363	1033.816384	16.359399
27.288564	1033.632405	16.364416
27.447011	1027.558110	16.369434
27.341634	1026.290090	16.374451
27.654344	1022.489173	16.379469
27.206831	1033.452503	16.384487
27.735219	1022.807872	16.389504
27.744034	1036.622391	16.394522
27.528075	1041.055116	16.399539
27.884853	1025.429008	16.404557
27.572332	1035.951606	16.409575
27.721278	1028.572304	16.414592
27.433693	1031.760186	16.419610
27.590602	1026.411956	16.424627
27.635617	1026.821476	16.429645
27.611248	1026.418145	16.434663
27.593554	1028.696172	16.439680
27.569256	1033.282089	16.444698
27.491877	1032.662953	16.449715
27.724553	1028.186539	16.454733
27.357657	1030.963897	16.459751
27.238322	1027.047212	16.464768
27.487744	1046.577229	16.469786
28.048644	1051.709503	16.474803
28.080390	1053.433888	16.479821
28.001569	1052.067059	16.484839
28.512185	1050.251856	16.489856
28.074976	1042.313722	16.494874
27.925793	1032.468849	16.499891
28.037580	1035.922750	16.504909
27.995225	1041.780098	16.509927
28.166005	1045.029159	16.514944
28.184021	1050.274359	16.519962
28.120112	1053.708282	16.524979
28.142531	1052.713850	16.529997
27.951767	1058.483857	16.535015
28.115852	1050.540463	16.540032
27.938989	1050.097759	16.545050
28.090025	1046.662831	16.550067
28.620868	1049.496076	16.555085
28.061779	1044.417106	16.560103
28.105959	1055.688899	16.565120
28.460196	1046.428348	16.570138
28.483259	1050.770213	16.575155
28.646074	1055.200773	16.580173
28.295051	1048.457876	16.585191
28.392642	1052.731334	16.590208
28.397333	1053.418529	16.595226
28.387235	1053.757737	16.600243
29.106085	1048.451395	16.605261
28.783474	1057.347202	16.610279
28.534000	1058.055035	16.615296
28.915668	1045.448258	16.620314
28.567606	1058.434743	16.625331
28.891885	1054.370089	16.630349
28.858103	1057.616289	16.635367
28.667569	1062.925520	16.640384
28.511222	1047.527604	16.645402
28.399665	1050.069553	16.650419
28.445103	1063.528100	16.655437
28.744005	1075.375621	16.660455
28.892387	1072.547009	16.665472
28.675515	1077.093493	16.670490
28.915955	1070.772890	16.675507
29.171616	1074.409524	16.680525
28.813518	1065.569136	16.685543
29.114081	1068.965251	16.690560
29.043334	1069.616855	16.695578
28.933345	1076.289464	16.700595
29.048730	1069.129963	16.705613
28.971853	1074.774948	16.710631
29.153270	1087.530696	16.715648
29.442745	1087.024852	16.720666
29.446185	1090.214770	16.725683
29.495903	1075.447459	16.730701
29.324955	1082.839610	16.735719
29.312695	1079.594200	16.740736
29.544630	1073.183403	16.745754
29.015674	1072.814452	16.750771
29.942681	1086.192565	16.755789
29.694371	1083.501452	16.760807
29.339368	1068.468959	16.765824
29.701429	1078.621469	16.770842
29.490658	1084.643906	16.775859
29.883179	1074.916637	16.780877
29.551273	1075.466893	16.785895
29.755120	1069.656911	16.790912
29.727315	1079.330485	16.795930
29.921900	1076.441030	16.800947
30.005338	1062.422709	16.805965
29.921428	1060.971466	16.810983
29.898346	1059.062634	16.816000
29.896215	1054.796338	16.821018
29.389456	1058.340237	16.826035
30.003028	1061.384664	16.831053
29.772504	1078.909791	16.836071
29.875051	1079.685892	16.841088
30.127387	1080.142029	16.846106
30.190968	1081.470145	16.851123
29.927307	1076.988946	16.856141
29.865961	1085.556914	16.861159
29.826369	1082.467236	16.866176
30.271573	1077.888293	16.871194
29.932150	1088.127935	16.876211
30.389615	1085.532062	16.881229
30.404879	1088.373004	16.886247
30.300411	1086.779794	16.891264
30.341682	1080.572247	16.896282
30.179248	1080.553325	16.901299
30.139445	1081.518845	16.906317
30.298013	1086.322454	16.911335
29.935610	1083.096845	16.916352
30.202984	1077.204387	16.921370
30.090061	1083.116916	16.926387
29.950090	1082.419161	16.931405
30.229353	1086.736925	16.936423
30.042998	1102.708872	16.941440
30.201886	1103.454111	16.946458
30.629665	1094.393522	16.951475
30.591229	1092.840523	16.956493
30.917849	1099.063315	16.961511
30.517567	1108.321532	16.966528
30.936941	1103.462584	16.971546
30.467267	1109.354927	16.976563
30.727795	1100.910505	16.981581
30.816397	1105.422059	16.986599
30.747355	1104.587029	16.991616
30.766238	1108.740213	16.996634
30.612315	1110.080105	17.001651
30.722212	1122.449386	17.006669
31.053310	1123.991472	17.011687
31.282222	1129.402673	17.016704
31.535844	1123.016884	17.021722
30.929009	1112.946576	17.026739
30.862955	1100.362132	17.031757
31.134002	1119.832059	17.036775
30.749590	1130.053484	17.041792
31.384065	1122.936217	17.046810
31.234034	1112.857903	17.051827
31.708720	1125.419696	17.056845
31.653427	1117.819694	17.061863
31.265674	1106.932647	17.066880
31.453198	1094.867298	17.071898
30.909899	1097.523810	17.076915
31.184355	1109.962135	17.081933
31.576644	1112.889545	17.086951
31.559390	1118.348538	17.091968
31.586674	1119.379353	17.096986
31.592113	1125.412321	17.102003
31.647435	1122.737044	17.107021
31.726397	1122.162990	17.112039
31.434124	1115.262599	17.117056
31.677153	1121.511037	17.122074
31.771234	1130.670204	17.127091
31.454304	1130.975135	17.132109
31.678669	1128.166242	17.137127
31.604945	1125.151297	17.142144
31.713966	1115.758478	17.147162
31.470497	1124.755604	17.152179
31.530729	1122.950557	17.157197
31.584540	1113.039320	17.162215
31.365490	1122.790030	17.167232
31.839121	1127.200617	17.172250
31.726996	1141.349625	17.177267
31.806279	1144.407824	17.182285
32.003817	1145.661440	17.187303
32.113248	1153.193002	17.192320
31.990418	1154.976177	17.197338
32.189165	1154.241462	17.202355
31.819990	1153.008194	17.207373
32.193020	1155.768198	17.212391
32.143400	1150.928609	17.217408
32.335762	1144.795346	17.222426
32.165290	1152.723934	17.227443
31.795245	1145.109810	17.232461
32.283715	1162.810253	17.237479
32.589178	1164.753963	17.242496
32.858890	1157.399986	17.247514
32.591023	1145.077303	17.252531
32.481004	1145.179607	17.257549
32.566403	1143.701997	17.262567
32.348845	1145.765006	17.267584
32.553446	1138.238139	17.272602
32.591978	1147.128255	17.277619
32.600806	1155.786317	17.282637
32.758160	1161.098217	17.287655
32.665817	1169.241865	17.292672
32.970218	1170.958524	17.297690
32.719520	1167.904855	17.302707
32.598791	1165.913385	17.307725
32.567558	1165.984488	17.312743
32.553782	1159.570891	17.317760
33.162766	1157.917086	17.322778
33.161859	1165.525792	17.327795
33.001113	1160.627764	17.332813
32.954104	1167.454703	17.337831
32.689305	1166.097886	17.342848
32.959875	1163.439582	17.347866
32.960241	1171.922246	17.352883
32.915481	1171.257000	17.357901
32.949105	1164.097568	17.362919
32.758582	1169.378427	17.367936
33.329672	1163.353447	17.372954
33.173079	1169.174974	17.377971
32.958736	1176.349859	17.382989
33.156239	1184.943846	17.388007
33.231319	1193.844074	17.393024
33.181360	1181.345429	17.398042
33.558529	1188.658596	17.403059
33.389905	1189.256016	17.408077
33.680755	1189.860794	17.413095
33.779395	1181.782364	17.418112
34.115230	1179.420008	17.423130
33.752825	1183.878725	17.428147
33.750086	1185.958785	17.433165
34.001948	1179.677391	17.438183
33.668016	1187.899687	17.443200
34.231817	1180.638767	17.448218
34.027169	1171.840706	17.453235
33.923591	1159.915309	17.458253
33.973513	1156.499259	17.463271
33.784670	1164.402311	17.468288
34.016753	1156.852223	17.473306
33.932870	1154.485790	17.478323
33.851232	1150.197138	17.483341
33.787270	1150.954985	17.488359
33.637708	1158.318591	17.493376
33.861402	1171.392863	17.498394
33.941924	1179.455954	17.503411
33.985643	1186.095205	17.508429
34.167140	1179.891038	17.513447
34.124612	1181.175722	17.518464
34.244001	1190.596067	17.523482
34.262642	1187.752922	17.528499
33.995957	1188.880004	17.533517
33.849866	1171.773101	17.538535
33.767547	1184.235468	17.543552
34.348914	1192.719200	17.548570
34.628120	1207.637304	17.553587
33.972470	1215.231207	17.558605
34.436238	1212.662737	17.563623
34.331498	1213.105045	17.568640
34.786632	1210.064550	17.573658
34.681984	1201.560172	17.578675
34.545997	1212.339410	17.583693
34.861456	1206.269010	17.588711
35.005493	1206.155035	17.593728
34.839135	1201.576604	17.598746
34.936641	1202.179926	17.603763
34.968775	1198.214373	17.608781
35.002449	1198.865503	17.613799
34.866451	1203.039668	17.618816
35.153143	1208.331444	17.623834
34.689263	1181.882374	17.628851
34.614079	1196.319161	17.633869
35.109908	1199.104234	17.638887
34.696188	1207.645074	17.643904
35.074603	1195.370056	17.648922
34.862875	1200.089339	17.653939
34.935450	1201.387661	17.658957
34.803690	1200.294149	17.663975
34.628754	1203.253085	17.668992
34.698043	1208.130588	17.674010
35.154321	1223.964719	17.679027
35.122593	1223.742410	17.684045
35.437999	1218.849126	17.689063
35.413225	1218.613111	17.694080
35.459020	1227.300166	17.699098
35.219635	1224.913754	17.704115
35.231528	1226.373004	17.709133
35.326881	1218.029983	17.714151
35.133882	1220.773984	17.719168
35.392642	1215.236271	17.724186
35.895835	1234.506078	17.729203
35.583954	1228.331373	17.734221
35.752870	1224.205664	17.739239
35.736296	1244.765077	17.744256
35.645422	1247.401663	17.749274
36.226535	1239.945521	17.754291
36.100187	1230.377848	17.759309
36.248552	1212.417177	17.764327
35.990296	1201.598272	17.769344
35.883292	1215.759165	17.774362
35.924116	1207.882228	17.779379
35.678498	1208.554752	17.784397
36.316434	1219.346042	17.789415
36.320972	1216.277872	17.794432
36.033883	1207.331683	17.799450
36.284676	1210.890208	17.804467
36.141134	1210.057305	17.809485
36.182672	1210.372698	17.814503
36.211621	1222.183452	17.819520
36.314486	1233.017033	17.824538
36.590261	1228.511768	17.829555
36.556538	1233.559950	17.834573
36.728813	1217.160828	17.839591
36.225682	1204.862109	17.844608
36.140269	1216.027949	17.849626
36.427812	1218.340527	17.854643
36.322192	1231.444025	17.859661
36.466680	1230.430578	17.864679
36.415296	1234.462188	17.869696
36.291640	1227.844768	17.874714
36.562864	1224.529948	17.879731
36.157930	1232.807500	17.884749
36.852490	1234.242514	17.889767
36.479373	1237.456373	17.894784
36.592876	1249.673702	17.899802
36.895409	1254.713719	17.904819
36.801346	1254.321234	17.909837
37.024968	1257.502147	17.914855
37.137021	1257.869677	17.919872
36.813567	1256.241119	17.924890
37.367642	1248.356838	17.929907
37.087466	1258.502147	17.934925
37.209075	1257.501727	17.939943
37.215228	1259.753980	17.944960
36.854851	1244.968327	17.949978
37.213379	1242.334187	17.954995
37.039497	1249.808914	17.960013
37.302265	1247.375875	17.965031
37.291368	1249.312045	17.970048
37.272842	1255.819003	17.975066
37.255680	1253.824022	17.980083
36.985427	1253.957585	17.985101
37.246847	1247.381190	17.990119
37.495123	1254.480923	17.995136
37.771996	1262.743854	18.000154
37.660765	1262.271991	18.005171
37.501143	1263.884181	18.010189
37.743987	1261.328010	18.015207
37.905066	1269.031460	18.020224
37.731179	1265.612365	18.025242
38.031057	1269.336829	18.030259
37.871409	1270.999516	18.035277
38.094482	1263.308774	18.040295
37.553361	1265.419018	18.045312
37.519867	1265.948064	18.050330
38.324920	1259.103987	18.055347
37.948542	1262.633938	18.060365
38.106310	1267.554486	18.065383
37.991039	1266.398442	18.070400
37.893357	1266.189557	18.075418
38.161031	1264.636221	18.080435
37.822812	1263.032052	18.085453
38.406797	1258.611337	18.090471
38.278983	1254.964164	18.095488
38.080169	1262.064082	18.100506
38.546531	1257.106259	18.105523
38.161642	1262.265929	18.110541
38.122184	1258.904800	18.115559
38.478906	1260.102082	18.120576
38.368099	1276.737764	18.125594
38.716573	1270.703227	18.130611
38.555822	1278.418919	18.135629
38.724572	1278.263226	18.140647
38.680807	1270.904361	18.145664
38.551323	1272.092137	18.150682
38.807628	1274.680985	18.155699
38.691765	1273.853237	18.160717
38.730563	1272.594311	18.165735
38.975031	1274.272974	18.170752
38.689768	1275.134710	18.175770
38.626564	1269.457760	18.180787
38.809593	1272.383064	18.185805
38.828730	1276.457353	18.190823
38.924128	1275.293755	18.195840
38.881371	1276.392289	18.200858
39.128722	1275.299708	18.205875
39.181050	1281.398012	18.210893
38.831109	1283.140821	18.215911
39.223244	1292.821712	18.220928
39.292878	1297.869599	18.225946
39.500770	1296.174089	18.230963
39.690034	1298.173775	18.235981
39.344669	1299.527708	18.240999
39.499026	1307.210131	18.246016
39.701823	1302.665717	18.251034
39.817744	1291.027950	18.256051
39.356671	1276.040198	18.261069
39.473641	1274.273639	18.266087
39.744468	1279.672049	18.271104
39.713516	1296.494132	18.276122
39.854308	1287.913630	18.281139
39.662635	1288.852313	18.286157
39.538061	1287.274839	18.291175
39.737377	1294.394834	18.296192
39.365307	1308.114230	18.301210
39.760772	1294.463712	18.306227
39.635289	1305.392850	18.311245
39.617022	1305.181067	18.316263
39.899950	1303.265590	18.321280
39.759037	1304.650808	18.326298
40.243500	1300.908297	18.331315
40.043711	1306.534623	18.336333
39.658286	1308.699525	18.341351
39.865094	1316.654653	18.346368
40.348076	1323.143514	18.351386
40.434472	1322.243248	18.356403
40.018034	1314.178681	18.361421
40.256736	1320.980130	18.366439
40.219006	1308.176533	18.371456
40.166350	1321.805183	18.376474
40.581886	1305.854100	18.381491
40.597524	1321.842130	18.386509
40.376253	1323.403963	18.391527
40.687568	1310.249374	18.396544
40.627855	1317.469669	18.401562
40.503694	1321.263320	18.406579
40.663438	1333.565027	18.411597
40.725623	1343.249979	18.416615
40.995439	1342.336934	18.421632
41.056078	1341.434365	18.426650
40.934840	1328.905688	18.431667
40.793760	1347.297625	18.436685
41.000973	1345.895707	18.441703
41.151199	1335.978802	18.446720
41.089965	1342.606051	18.451738
40.862676	1337.390129	18.456755
40.831608	1340.547594	18.461773
40.955134	1339.565807	18.466791
41.343491	1341.206295	18.471808
41.003959	1342.433091	18.476826
41.069315	1345.133730	18.481843
41.444757	1336.478801	18.486861
40.892454	1345.328462	18.491879
41.532901	1335.953772	18.496896
41.298947	1342.999233	18.501914
41.496557	1339.853644	18.506931
41.271066	1339.162883	18.511949
41.197186	1359.112810	18.516967
41.665974	1355.088706	18.521984
41.677402	1356.838374	18.527002
42.091758	1354.583692	18.532019
42.085034	1358.220210	18.537037
42.208374	1351.412809	18.542055
42.406851	1336.274981	18.547072
42.130572	1327.708902	18.552090
42.217318	1327.392406	18.557107
42.015145	1324.100780	18.562125
41.965529	1323.739243	18.567143
42.053026	1320.639204	18.572160
42.221241	1328.186934	18.577178
41.973999	1314.989918	18.582195
42.210092	1313.334196	18.587213
42.183017	1318.766377	18.592231
42.592861	1315.275323	18.597248
42.200365	1315.326933	18.602266
42.449693	1315.846662	18.607283
42.258064	1321.181386	18.612301
42.035543	1318.823894	18.617319
42.427645	1312.766772	18.622336
42.247567	1321.293379	18.627354
42.292635	1334.430296	18.632371
42.601402	1338.134456	18.637389
42.706095	1347.244746	18.642407
42.817896	1345.987072	18.647424
42.631853	1350.623500	18.652442
42.611039	1334.128100	18.657459
43.066180	1346.718340	18.662477
42.716791	1348.839767	18.667495
42.933653	1339.685660	18.672512
42.905745	1346.998846	18.677530
42.793701	1345.154327	18.682547
42.778584	1347.406746	18.687565
42.591567	1344.156938	18.692583
42.897887	1357.887516	18.697600
42.979101	1352.175431	18.702618
42.759510	1351.654165	18.707635
43.132694	1359.491890	18.712653
42.840000	1368.575699	18.717671
43.133720	1371.594239	18.722688
43.263869	1378.532533	18.727706
43.462273	1377.438098	18.732723
43.226330	1376.698469	18.737741
43.200279	1374.310380	18.742759
43.456527	1373.178538	18.747776
43.562544	1373.013677	18.752794
42.894722	1373.679358	18.757811
43.370922	1378.569293	18.762829
43.452015	1396.614264	18.767847
43.896911	1399.555623	18.772864
43.529144	1404.867303	18.777882
43.757594	1403.752410	18.782899
43.701832	1395.158277	18.787917
43.750904	1399.433061	18.792935
44.022296	1398.797480	18.797952
44.031564	1399.951038	18.802970
43.814055	1395.904388	18.807987
44.040997	1392.886768	18.813005
43.709245	1389.659486	18.818023
43.709978	1394.629765	18.823040
43.975862	1407.789161	18.828058
44.090017	1409.519685	18.833075
44.307139	1410.751336	18.838093
44.045395	1429.117963	18.843111
44.225099	1422.456395	18.848128
44.434557	1422.344857	18.853146
44.042771	1414.339522	18.858163
44.759969	1411.172985	18.863181
44.602114	1423.562072	18.868199
44.522102	1424.133080	18.873216
44.358726	1423.195956	18.878234
44.742205	1428.621054	18.883251
44.850982	1428.282192	18.888269
44.811923	1440.794807	18.893287
44.936647	1433.573745	18.898304
44.943914	1434.027022	18.903322
44.891573	1439.968106	18.908339
44.926297	1426.550380	18.913357
44.912834	1424.425414	18.918375
44.870131	1427.764589	18.923392
44.979135	1427.615041	18.928410
45.206450	1435.399771	18.933427
45.396790	1435.045054	18.938445
45.294592	1433.170590	18.943463
45.239161	1429.045048	18.948480
45.192847	1429.345720	18.953498
45.020223	1432.578890	18.958515
45.328255	1432.205849	18.963533
45.046470	1433.145947	18.968551
45.126588	1434.118061	18.973568
45.247588	1424.511773	18.978586
45.161059	1429.139039	18.983603
45.575771	1439.867388	18.988621
45.732417	1452.175970	18.993639
46.135227	1452.507703	18.998656
46.093611	1447.900319	19.003674
45.551764	1444.361751	19.008691
45.707355	1441.036493	19.013709
45.990858	1454.663399	19.018727
45.768374	1450.727966	19.023744
46.023698	1443.540215	19.028762
45.967282	1440.743431	19.033779
46.068432	1443.476382	19.038797
46.077227	1447.927864	19.043815
45.984366	1448.115862	19.048832
46.158705	1442.354535	19.053850
45.939386	1436.364163	19.058867
46.034287	1433.849936	19.063885
46.016004	1447.779447	19.068903
46.065636	1443.239909	19.073920
46.315255	1456.228303	19.078938
46.434639	1460.971842	19.083955
46.195705	1464.281615	19.088973
46.388250	1469.139999	19.093991
46.765325	1466.644952	19.099008
46.924591	1471.577946	19.104026
46.772163	1468.833976	19.109043
47.100451	1457.453374	19.114061
47.033454	1459.357276	19.119079
46.947650	1459.326421	19.124096
47.189585	1453.267386	19.129114
47.635499	1469.794478	19.134131
47.179673	1454.537512	19.139149
46.885814	1442.638396	19.144167
47.044359	1446.874056	19.149184
47.339883	1448.008296	19.154202
47.395587	1462.749972	19.159219
47.530442	1452.586084	19.164237
47.335718	1445.929154	19.169255
46.983707	1440.025714	19.174272
47.233821	1440.267610	19.179290
46.892571	1456.453339	19.184307
46.961253	1459.989775	19.189325
47.079782	1467.939781	19.194343
47.077014	1465.589080	19.199360
47.306989	1471.265311	19.204378
47.541715	1484.114031	19.209395
47.789325	1480.174828	19.214413
47.576498	1488.132251	19.219431
47.828166	1492.751060	19.224448
47.998490	1483.692489	19.229466
47.714917	1495.684629	19.234483
48.056123	1480.489742	19.239501
48.327559	1484.269173	19.244519
48.000509	1475.041889	19.249536
48.425243	1479.633750	19.254554
48.011026	1489.752721	19.259571
48.129415	1480.670679	19.264589
47.780814	1488.251606	19.269607
48.026226	1483.362836	19.274624
48.000246	1484.253641	19.279642
48.002334	1492.284903	19.284659
48.140971	1494.011623	19.289677
48.223868	1498.407399	19.294695
47.964089	1524.805444	19.299712
48.141228	1510.453440	19.304730
48.247382	1521.138359	19.309747
48.455864	1502.675724	19.314765
48.852239	1511.614452	19.319783
48.948041	1510.507581	19.324800
48.940629	1514.879552	19.329818
48.198645	1515.683017	19.334835
48.769425	1514.006728	19.339853
48.871802	1532.244185	19.344871
49.235367	1536.899233	19.349888
49.287412	1526.252728	19.354906
49.061288	1534.291138	19.359923
49.213293	1531.089499	19.364941
49.163661	1530.327167	19.369959
49.033042	1530.565226	19.374976
49.512587	1526.444733	19.379994
49.419238	1528.674642	19.385011
49.568771	1525.072596	19.390029
49.596724	1532.894719	19.395047
49.440577	1524.117334	19.400064
49.873169	1510.435625	19.405082
49.267799	1512.921977	19.410099
49.672997	1513.622574	19.415117
49.195421	1522.400726	19.420135
49.182427	1532.163759	19.425152
49.758409	1526.715418	19.430170
49.638540	1522.555705	19.435187
49.709661	1513.948072	19.440205
49.484962	1528.114912	19.445223
49.626550	1522.873062	19.450240
50.200534	1532.752993	19.455258
49.789661	1545.582351	19.460275
49.512497	1540.475122	19.465293
50.201645	1546.417562	19.470311
50.186861	1547.363433	19.475328
50.513819	1539.082033	19.480346
50.303953	1547.739621	19.485363
50.397393	1546.229167	19.490381
50.626738	1547.187521	19.495399
50.235503	1548.315081	19.500416
50.730063	1539.824547	19.505434
50.409985	1538.236463	19.510451
50.771980	1544.753710	19.515469
50.693196	1542.222328	19.520487
50.173137	1543.395192	19.525504
50.559238	1538.257281	19.530522
50.287080	1549.001118	19.535539
50.581402	1552.975819	19.540557
50.615918	1555.798059	19.545575
50.542974	1564.248141	19.550592
51.094761	1555.035467	19.555610
51.122406	1556.419707	19.560627
51.031593	1555.070485	19.565645
50.991071	1553.404160	19.570663
50.841391	1562.475269	19.575680
50.934189	1566.951572	19.580698
51.290017	1579.604778	19.585715
51.195155	1589.134432	19.590733
51.609385	1574.773866	19.595751
51.266037	1587.655858	19.600768
51.672313	1584.070632	19.605786
51.670435	1585.071301	19.610803
51.550881	1586.904502	19.615821
51.812807	1582.776852	19.620839
51.269815	1578.929161	19.625856
51.777824	1586.301019	19.630874
51.796923	1582.971738	19.635891
51.488280	1586.516453	19.640909
51.849400	1579.608827	19.645927
51.452853	1589.005567	19.650944
52.294236	1592.992935	19.655962
52.003854	1597.639360	19.660979
51.843426	1603.404820	19.665997
51.974833	1594.371187	19.671015
51.478389	1604.746027	19.676032
51.559119	1603.215456	19.681050
51.911187	1607.357908	19.686067
52.076036	1619.090961	19.691085
52.508708	1622.791669	19.696103
52.605022	1627.078088	19.701120
53.019626	1610.050729	19.706138
53.340153	1614.213872	19.711155
53.276684	1601.789620	19.716173
52.959829	1584.768868	19.721191
52.812856	1584.785408	19.726208
53.007032	1585.966994	19.731226
53.113197	1586.587917	19.736243
52.878167	1585.280082	19.741261
53.003453	1574.808341	19.746279
52.695537	1583.093040	19.751296
52.803185	1572.194849	19.756314
52.819165	1587.930597	19.761331
52.681591	1597.157631	19.766349
53.004607	1606.603298	19.771367
52.919120	1603.580636	19.776384
53.277142	1600.738236	19.781402
53.104397	1609.756154	19.786419
52.971305	1616.003364	19.791437
53.478719	1610.464686	19.796455
53.400811	1630.980445	19.801472
53.543236	1633.476621	19.806490
53.706770	1640.144725	19.811507
53.624012	1622.686695	19.816525
53.833378	1629.404466	19.821543
53.937962	1638.745300	19.826560
54.162578	1633.137034	19.831578
54.060829	1631.211985	19.836595
53.902833	1631.681530	19.841613
54.142950	1632.483574	19.846631
54.210008	1635.638438	19.851648
54.371958	1639.277156	19.856666
54.381453	1627.365400	19.861683
54.158959	1630.697890	19.866701
54.579301	1630.420971	19.871719
54.362435	1631.903247	19.876736
54.704893	1624.919613	19.881754
54.655780	1628.247200	19.886771
54.334602	1625.639934	19.891789
54.439418	1623.827895	19.896807
54.257521	1628.274397	19.901824
54.357173	1631.660876	19.906842
54.476292	1619.627914	19.911859
54.410852	1632.308876	19.916877
54.547950	1627.288605	19.921895
54.653179	1647.952598	19.926912
54.740140	1648.715371	19.931930
54.983303	1647.487718	19.936947
54.981510	1648.958601	19.941965
54.916074	1652.651659	19.946983
54.811032	1654.318503	19.952000
54.562993	1652.302617	19.957018
54.910681	1664.146092	19.962035
54.994569	1669.557947	19.967053
55.118513	1671.394272	19.972071
55.165342	1679.734240	19.977088
55.605910	1679.627745	19.982106
55.424965	1677.891750	19.987123
55.514974	1679.613437	19.992141
55.488960	1670.948266	19.997159
55.389313	1688.333691	20.002176
55.786142	1675.228638	20.007194
55.864754	1675.159561	20.012211
55.625663	1680.684823	20.017229
55.907689	1668.863155	20.022247
56.012273	1683.764664	20.027264
55.853625	1698.363179	20.032282
56.188332	1698.333127	20.037299
55.976262	1708.606945	20.042317
56.385845	1699.498391	20.047335
56.459688	1710.036971	20.052352
56.127745	1700.519991	20.057370
56.414393	1702.116387	20.062387
56.425529	1700.817555	20.067405
56.459059	1702.191423	20.072423
56.546272	1699.031401	20.077440
56.385339	1692.971891	20.082458
56.301774	1692.943843	20.087475
56.464368	1691.021814	20.092493
57.054441	1677.104014	20.097511
57.220836	1688.959952	20.102528
56.901862	1684.929033	20.107546
57.051542	1680.616861	20.112563
57.149673	1684.268680	20.117581
57.308933	1682.817396	20.122599
57.339529	1697.970284	20.127616
57.003932	1676.303753	20.132634
57.242968	1679.059455	20.137651
57.072798	1689.121607	20.142669
57.326222	1678.282708	20.147687
57.366026	1680.577113	20.152704
57.149298	1680.282614	20.157722
57.589181	1686.257599	20.162739
57.449553	1705.785796	20.167757
58.000148	1700.707438	20.172775
57.702769	1709.280896	20.177792
57.842614	1713.737288	20.182810
57.772863	1699.975851	20.187827
57.732289	1711.239164	20.192845
57.918485	1704.232489	20.197863
57.666539	1699.332732	20.202880
57.537774	1697.774808	20.207898
57.794111	1700.351091	20.212915
57.578290	1696.957376	20.217933
57.719539	1714.639845	20.222951
57.785477	1722.815908	20.227968
57.955058	1727.447559	20.232986
58.189651	1722.203794	20.238003
58.030571	1727.186424	20.243021
58.239237	1719.068530	20.248039
58.605824	1729.043978	20.253056
58.769891	1743.636468	20.258074
58.877245	1744.664321	20.263091
58.668303	1740.979185	20.268109
59.011014	1730.296771	20.273127
58.872542	1738.103869	20.278144
58.993960	1746.277617	20.283162
59.095356	1729.933242	20.288179
59.037803	1728.758714	20.293197
59.129942	1733.493944	20.298215
59.096032	1733.350866	20.303232
59.093883	1736.175687	20.308250
59.419143	1741.370098	20.313267
59.209245	1747.506233	20.318285
59.309343	1747.225522	20.323303
59.349626	1744.072799	20.328320
59.407270	1750.454466	20.333338
59.465403	1745.380183	20.338355
59.184395	1744.511851	20.343373
59.464367	1742.366408	20.348391
59.732735	1739.272851	20.353408
59.363094	1739.507100	20.358426
59.391131	1742.033724	20.363443
59.557968	1741.679505	20.368461
59.534424	1756.080302	20.373479
59.863541	1764.464725	20.378496
59.782757	1767.850919	20.383514
60.391717	1763.855394	20.388531
59.757226	1772.992623	20.393549
60.035554	1760.669684	20.398567
59.933031	1762.850555	20.403584
59.829830	1766.603167	20.408602
60.235210	1775.108268	20.413619
60.224989	1782.317889	20.418637
60.511799	1783.175789	20.423655
60.681979	1790.676071	20.428672
60.515858	1792.633312	20.433690
60.551491	1784.886321	20.438707
60.393770	1786.293128	20.443725
60.440872	1785.323215	20.448743
60.736458	1788.511955	20.453760
60.606914	1807.322304	20.458778
61.246392	1799.377147	20.463795
61.491038	1813.587908	20.468813
61.607292	1806.652046	20.473831
61.498102	1803.566766	20.478848
61.207487	1810.573894	20.483866
61.334566	1802.512847	20.488883
61.045434	1803.561407	20.493901
61.335051	1813.132309	20.498919
61.425539	1810.909059	20.503936
61.258796	1821.377862	20.508954
61.323322	1804.376420	20.513971
61.571766	1810.775741	20.518989
61.610415	1805.120633	20.524007
61.730244	1808.352521	20.529024
61.799555	1826.248278	20.534042
61.805533	1827.143592	20.539059
61.772376	1829.982723	20.544077
61.728081	1830.298866	20.549095
62.186697	1831.328841	20.554112
61.778004	1830.552970	20.559130
62.168430	1830.066105	20.564147
62.436680	1825.719658	20.569165
61.936297	1824.247985	20.574183
62.063746	1832.550225	20.579200
62.331630	1843.901301	20.584218
62.263915	1850.864272	20.589235
62.369566	1855.300776	20.594253
62.322392	1856.030792	20.599271
62.902358	1841.196070	20.604288
62.412766	1849.569141	20.609306
62.717636	1845.311664	20.614323
63.217304	1850.400056	20.619341
62.966859	1851.464687	20.624359
63.205758	1856.861932	20.629376
63.285230	1860.636617	20.634394
63.207546	1851.619629	20.639411
63.277034	1847.783820	20.644429
63.270194	1857.211547	20.649447
63.531243	1859.357916	20.654464
63.208688	1855.627327	20.659482
63.498211	1856.197620	20.664499
63.352539	1865.356623	20.669517
63.644088	1865.724624	20.674535
63.841083	1853.808772	20.679552
63.595196	1856.015131	20.684570
63.729005	1861.864255	20.689587
63.714673	1865.107573	20.694605
63.894771	1869.453592	20.699623
64.076431	1859.345304	20.704640
63.648869	1867.437317	20.709658
64.082188	1859.634688	20.714675
64.022891	1859.596551	20.719693
63.790717	1864.521169	20.724711
64.019552	1869.310895	20.729728
64.028393	1875.810662	20.734746
64.438696	1886.035022	20.739763
64.483294	1889.007228	20.744781
64.393977	1892.779796	20.749799
64.489980	1889.148140	20.754816
64.354183	1889.244993	20.759834
64.311964	1880.490722	20.764851
64.356989	1899.072010	20.769869
64.711490	1907.162204	20.774887
64.959838	1907.776781	20.779904
64.567900	1910.252047	20.784922
65.236752	1913.710911	20.789939
65.076898	1900.133768	20.794957
65.094367	1903.059706	20.799975
65.351989	1906.721454	20.804992
64.814277	1908.272642	20.810010
64.763494	1918.783410	20.815027
65.222997	1914.205186	20.820045
65.346461	1931.123750	20.825063
65.813441	1922.069265	20.830080
65.578265	1927.221594	20.835098
65.618416	1926.688273	20.840115
65.604533	1921.767169	20.845133
65.622829	1923.894534	20.850151
65.654172	1926.865655	20.855168
65.807903	1951.240122	20.860186
65.926850	1952.177816	20.865203
66.004161	1945.740287	20.870221
66.046587	1950.278180	20.875239
66.327788	1943.130384	20.880256
66.499438	1949.838368	20.885274
66.305296	1940.268245	20.890291
66.319157	1939.079428	20.895309
65.968405	1947.689713	20.900327
66.555740	1949.782137	20.905344
66.656349	1958.107550	20.910362
66.563391	1963.174629	20.915379
66.610164	1964.363411	20.920397
67.198562	1969.677873	20.925415
67.051519	1959.551275	20.930432
67.074801	1974.371008	20.935450
67.128976	1975.508143	20.940467
67.501005	1969.289818	20.945485
67.339615	1971.609273	20.950503
67.690520	1970.011360	20.955520
67.334026	1968.507804	20.960538
67.270886	1966.958575	20.965555
67.664665	1964.918468	20.970573
67.388802	1957.156782	20.975591
67.827128	1961.592012	20.980608
67.548129	1957.321268	20.985626
67.598015	1959.980227	20.990643
67.752919	1959.561587	20.995661
67.371312	1965.311104	21.000679
67.526242	1965.053412	21.005696
67.460064	1958.890693	21.010714
67.438869	1969.873430	21.015731
67.743475	1995.026072	21.020749
67.689249	1997.029032	21.025767
67.894119	1986.901279	21.030784
67.722194	1989.550593	21.035802
68.015439	2002.362173	21.040819
68.436191	2002.179863	21.045837
68.374686	2012.755475	21.050855
68.365679	2006.845781	21.055872
68.352069	2018.695248	21.060890
68.338860	2012.637877	21.065907
68.769382	2014.726320	21.070925
68.348787	2022.119856	21.075943
68.641055	2015.932868	21.080960
69.058676	2032.493292	21.085978
69.068965	2032.248652	21.090995
69.089959	2030.478026	21.096013
69.205786	2033.385516	21.101031
69.199995	2025.534412	21.106048
69.206136	2028.455823	21.111066
69.218060	2034.775279	21.116083
69.316963	2024.067531	21.121101
69.317208	2031.083111	21.126119
69.559705	2032.080472	21.131136
69.565881	2050.753177	21.136154
69.787035	2050.179047	21.141171
70.174971	2044.015026	21.146189
70.457802	2040.887606	21.151207
70.587170	2042.798868	21.156224
70.622379	2022.219791	21.161242
70.065792	2016.591016	21.166259
69.960114	2018.444193	21.171277
70.171306	2019.837763	21.176295
70.298103	2013.420908	21.181312
70.345771	2024.367710	21.186330
70.319802	2037.415214	21.191347
70.645724	2036.834241	21.196365
70.517567	2041.098902	21.201383
70.656080	2042.680522	21.206400
70.744023	2031.444278	21.211418
70.657837	2031.940524	21.216435
70.625298	2035.038378	21.221453
70.612347	2039.155708	21.226471
70.759956	2037.510542	21.231488
70.923819	2052.532524	21.236506
70.737837	2064.689738	21.241523
70.933403	2065.265199	21.246541
71.219588	2068.048337	21.251559
71.289090	2066.541567	21.256576
71.277978	2067.407994	21.261594
71.093183	2065.218105	21.266611
71.422429	2074.880811	21.271629
71.261693	2092.348727	21.276647
71.504540	2090.085942	21.281664
71.551278	2097.119557	21.286682
71.417068	2093.176548	21.291699
71.479593	2086.381492	21.296717
71.989948	2105.206140	21.301735
72.156239	2104.470130	21.306752
72.358454	2104.366028	21.311770
72.201573	2105.141538	21.316787
72.332508	2099.860151	21.321805
72.515665	2106.228715	21.326823
72.869991	2105.078403	21.331840
72.940080	2101.116208	21.336858
72.578066	2089.893175	21.341875
72.626747	2074.225754	21.346893
72.503346	2085.224474	21.351911
72.516839	2088.195245	21.356928
72.736641	2099.954775	21.361946
72.600908	2102.904598	21.366963
72.740645	2101.184909	21.371981
72.651848	2106.901507	21.376999
73.009321	2099.457738	21.382016
73.198141	2098.992787	21.387034
72.875580	2117.688340	21.392051
73.502139	2118.559635	21.397069
73.376484	2121.236481	21.402087
73.264932	2123.074803	21.407104
73.166612	2113.628530	21.412122
73.246913	2119.817444	21.417139
73.391531	2116.462210	21.422157
73.189012	2130.045378	21.427175
73.559287	2141.898278	21.432192
73.882831	2147.582249	21.437210
73.650456	2151.175163	21.442227
74.205465	2148.907952	21.447245
73.827871	2140.189989	21.452263
73.557017	2142.703243	21.457280
73.855379	2169.031118	21.462298
74.272132	2165.541982	21.467315
74.391486	2165.463405	21.472333
74.563993	2167.266973	21.477351
74.860089	2159.431928	21.482368
74.500363	2164.149258	21.487386
74.409179	2170.790945	21.492403
74.357663	2175.709613	21.497421
74.759579	2187.999452	21.502439
75.024846	2182.170080	21.507456
75.040962	2181.176566	21.512474
75.039006	2187.889577	21.517491
75.126502	2180.759222	21.522509
75.301054	2180.182876	21.527527
75.253036	2180.029366	21.532544
75.592030	2176.198866	21.537562
75.550738	2182.476165	21.542579
75.796959	2188.228995	21.547597
75.453174	2188.216213	21.552615
75.678491	2208.407699	21.557632
75.653759	2200.594183	21.562650
75.494123	2204.522939	21.567667
75.837805	2207.139348	21.572685
75.947389	2205.863023	21.577703
75.994734	2204.631105	21.582720
75.777990	2206.249115	21.587738
75.970244	2225.432702	21.592755
75.953564	2230.592127	21.597773
76.261889	2239.355571	21.602791
76.150500	2226.966749	21.607808
76.387739	2219.895119	21.612826
76.139841	2227.375466	21.617843
76.849718	2241.873916	21.622861
76.831636	2247.484869	21.627879
76.669124	2258.660207	21.632896
76.696911	2255.064347	21.637914
77.075119	2257.694324	21.642931
76.975631	2255.497441	21.647949
77.066910	2249.568897	21.652967
77.004721	2258.298514	21.657984
77.328822	2261.596515	21.663002
77.230509	2273.727597	21.668019
77.321880	2274.669602	21.673037
77.640634	2275.834996	21.678055
77.979371	2280.651905	21.683072
77.616902	2272.029358	21.688090
77.607515	2274.148452	21.693107
77.809851	2278.945570	21.698125
78.190306	2278.794780	21.703143
78.029228	2283.250827	21.708160
78.245451	2274.386693	21.713178
78.133055	2271.065133	21.718195
78.500188	2265.702739	21.723213
78.292639	2264.106536	21.728231
78.106502	2277.201244	21.733248
78.212635	2281.760862	21.738266
77.766291	2271.551292	21.743283
78.425890	2281.421467	21.748301
78.500531	2288.671731	21.753319
78.098035	2295.958414	21.758336
78.395843	2287.488693	21.763354
78.636629	2297.490359	21.768371
79.005232	2306.294948	21.773389
79.147860	2306.714548	21.778407
79.287231	2304.666674	21.783424
79.595965	2303.214161	21.788442
79.244013	2311.395592	21.793459
79.199125	2308.186598	21.798477
79.482022	2300.678614	21.803495
79.331188	2306.881487	21.808512
79.590628	2300.103032	21.813530
79.533261	2308.595224	21.818547
79.730153	2321.718697	21.823565
79.744593	2325.146978	21.828583
79.927098	2326.633407	21.833600
80.002378	2329.828142	21.838618
80.020717	2333.369433	21.843635
80.487024	2327.657045	21.848653
80.501474	2331.277841	21.853671
80.284942	2336.310613	21.858688
80.298840	2332.697963	21.863706
80.052131	2334.797205	21.868723
80.114353	2342.939414	21.873741
80.318943	2345.586968	21.878759
80.434419	2355.838564	21.883776
80.458546	2342.885731	21.888794
80.685496	2363.888228	21.893811
80.935796	2374.753200	21.898829
81.396683	2373.898724	21.903847
81.299224	2383.675372	21.908864
81.281646	2377.160938	21.913882
81.395776	2377.275689	21.918899
81.190578	2381.233669	21.923917
81.429498	2368.676592	21.928935
81.385693	2368.645508	21.933952
81.298281	2373.935915	21.938970
81.630094	2393.470361	21.943987
81.815378	2399.665120	21.949005
81.976072	2395.814994	21.954023
81.937424	2397.443165	21.959040
81.968909	2395.219561	21.964058
81.911907	2401.483603	21.969075
81.938499	2393.437936	21.974093
82.384352	2392.506899	21.979111
82.398520	2401.183670	21.984128
82.508587	2408.144426	21.989146
82.378144	2417.178256	21.994163
82.461178	2420.261339	21.999181
82.322845	2420.914046	22.004199
82.188946	2424.030905	22.009216
82.809195	2416.416697	22.014234
82.786368	2422.536560	22.019251
83.112606	2423.290518	22.024269
83.177963	2435.001726	22.029287
83.137963	2443.822658	22.034304
83.484130	2441.925621	22.039322
83.539319	2444.463897	22.044339
83.373085	2444.256203	22.049357
83.666049	2437.794389	22.054375
83.545489	2435.827998	22.059392
83.399960	2434.834389	22.064410
83.612570	2438.124534	22.069427
83.529342	2438.039624	22.074445
84.005888	2432.180433	22.079463
84.054971	2430.253906	22.084480
84.141827	2435.744431	22.089498
84.327946	2432.363741	22.094515
84.357288	2444.049002	22.099533
84.356966	2448.136055	22.104551
83.861000	2444.770033	22.109568
84.343872	2451.063654	22.114586
84.501713	2455.915087	22.119603
84.447397	2457.447867	22.124621
84.881111	2447.025432	22.129639
84.763630	2450.871934	22.134656
84.985170	2466.667975	22.139674
85.282194	2476.039250	22.144691
85.288400	2475.836267	22.149709
85.647461	2478.093693	22.154727
84.942377	2480.501018	22.159744
85.173444	2468.263852	22.164762
85.199816	2475.625856	22.169779
85.088201	2484.631539	22.174797
85.271998	2474.352148	22.179815
85.409617	2493.778073	22.184832
85.669878	2501.198354	22.189850
85.714665	2500.380251	22.194867
85.597398	2503.156840	22.199885
85.822763	2500.401231	22.204903
85.894695	2511.152035	22.209920
86.123092	2512.167399	22.214938
86.359818	2513.203559	22.219955
86.152496	2521.185830	22.224973
86.094703	2516.413420	22.229991
86.127892	2524.039488	22.235008
86.621534	2535.744045	22.240026
86.901284	2545.670351	22.245043
86.801508	2547.888763	22.250061
86.632519	2539.501069	22.255079
87.019308	2544.250605	22.260096
87.148069	2538.846342	22.265114
86.950675	2531.245770	22.270131
87.111583	2546.647349	22.275149
87.511835	2547.140463	22.280167
87.390946	2566.139622	22.285184
87.300704	2561.476401	22.290202
87.786045	2559.854350	22.295219
87.831963	2563.833238	22.300237
87.977698	2551.423095	22.305255
88.084006	2566.549150	22.310272
87.902557	2565.759956	22.315290
88.423423	2564.507941	22.320307
88.198392	2562.358971	22.325325
88.351079	2555.716970	22.330343
88.273830	2553.718574	22.335360
88.144277	2560.966024	22.340378
88.686898	2564.315273	22.345395
88.557194	2558.392628	22.350413
88.244234	2561.041892	22.355431
88.294404	2571.057608	22.360448
88.439999	2577.530027	22.365466
88.937794	2577.733379	22.370483
88.723353	2579.849717	22.375501
88.703666	2572.631745	22.380519
89.065787	2591.233814	22.385536
88.802033	2595.538653	22.390554
89.300073	2605.519376	22.395571
89.788462	2602.514501	22.400589
89.953548	2585.831201	22.405607
90.137521	2584.615857	22.410624
89.961891	2582.020504	22.415642
90.487774	2584.643319	22.420659
90.084981	2582.424186	22.425677
90.404917	2583.832431	22.430695
90.356693	2595.201640	22.435712
90.278814	2586.765023	22.440730
90.613062	2579.864354	22.445747
90.392471	2586.150773	22.450765
90.574873	2578.456333	22.455783
90.496364	2588.384789	22.460800
90.354401	2590.511936	22.465818
90.505374	2583.238984	22.470835
90.329675	2579.498001	22.475853
90.814793	2582.613192	22.480871
90.478304	2595.109802	22.485888
90.717124	2607.791424	22.490906
90.676803	2611.906834	22.495923
90.565012	2608.430471	22.500941
91.021794	2618.184077	22.505959
90.901020	2625.616393	22.510976
90.810740	2636.635542	22.515994
91.077387	2647.548631	22.521011
91.486332	2661.677678	22.526029
91.783106	2655.316188	22.531047
91.725229	2660.759883	22.536064
91.856607	2666.590713	22.541082
91.915358	2662.226186	22.546099
92.173239	2671.430075	22.551117
92.484286	2676.939423	22.556135
92.416608	2681.882838	22.561152
92.242577	2688.487117	22.566170
92.702842	2677.170409	22.571187
92.516924	2689.372220	22.576205
92.222593	2680.625249	22.581223
92.273506	2690.012862	22.586240
92.396750	2696.930651	22.591258
92.602224	2703.182336	22.596275
92.505537	2720.170638	22.601293
93.055540	2721.397897	22.606311
93.233768	2735.098982	22.611328
92.922846	2736.652800	22.616346
93.342195	2730.193298	22.621363
93.447649	2728.431546	22.626381
93.454553	2733.035133	22.631399
93.930739	2745.477909	22.636416
93.949174	2754.605502	22.641434
94.248081	2753.608958	22.646451
93.826436	2755.079022	22.651469
94.306168	2747.388715	22.656487
94.335108	2752.181396	22.661504
94.632276	2753.381744	22.666522
94.802369	2747.219840	22.671539
94.512999	2744.367594	22.676557
94.648355	2740.751733	22.681575
94.644614	2744.407005	22.686592
94.699093	2748.586589	22.691610
95.172066	2737.526662	22.696627
94.863635	2740.292020	22.701645
94.741235	2738.568899	22.706663
95.017125	2736.139930	22.711680
95.268637	2757.662971	22.716698
95.173816	2763.860437	22.721715
95.033671	2762.774446	22.726733
95.195044	2760.581072	22.731751
95.409420	2764.215013	22.736768
95.125850	2769.861152	22.741786
95.523697	2775.625282	22.746803
95.327513	2793.812671	22.751821
95.515665	2778.261787	22.756839
95.821298	2789.907414	22.761856
96.001594	2810.810392	22.766874
96.169713	2811.806754	22.771891
96.452214	2821.177316	22.776909
96.513703	2813.690965	22.781927
96.641591	2805.768210	22.786944
96.471525	2803.793705	22.791962
96.738431	2806.078145	22.796979
96.681105	2813.838360	22.801997
96.715496	2823.982917	22.807015
96.884949	2828.725338	22.812032
96.698161	2835.603079	22.817050
97.253588	2830.924477	22.822067
96.821013	2842.479925	22.827085
97.418089	2854.575723	22.832103
97.803034	2853.436378	22.837120
97.704617	2859.555535	22.842138
97.906986	2849.361408	22.847155
97.887768	2856.386653	22.852173
97.765784	2851.901883	22.857191
98.027451	2850.343036	22.862208
98.014535	2857.809152	22.867226
97.663589	2852.577320	22.872243
98.025599	2865.662861	22.877261
98.179857	2870.006835	22.882279
98.754213	2871.526984	22.887296
98.268813	2878.817340	22.892314
98.408100	2874.184579	22.897331
98.834858	2891.637551	22.902349
98.637512	2902.518884	22.907367
98.919240	2892.059890	22.912384
99.016521	2899.594081	22.917402
99.181429	2893.972626	22.922419
99.425866	2899.293580	22.927437
99.476281	2892.787308	22.932455
99.754933	2891.904373	22.937472
99.702319	2889.381349	22.942490
99.673118	2901.618871	22.947507
100.065310	2913.364720	22.952525
99.831191	2914.180694	22.957543
100.305688	2909.719817	22.962560
99.861527	2908.296106	22.967578
100.179279	2897.427521	22.972595
100.549511	2906.052255	22.977613
100.511168	2907.491059	22.982631
100.326503	2904.556208	22.987648
100.114440	2910.014516	22.992666
100.355165	2918.056605	22.997683
100.484480	2928.454711	23.002701
100.546886	2931.967167	23.007719
101.032593	2942.297169	23.012736
100.807496	2937.683250	23.017754
101.000412	2948.327109	23.022771
101.148574	2951.823061	23.027789
101.107665	2960.745384	23.032807
101.361568	2959.541221	23.037824
101.243911	2967.355080	23.042842
101.323502	2972.423984	23.047859
101.838361	2979.410311	23.052877
102.054072	2982.955718	23.057895
102.318965	2981.371109	23.062912
102.044750	2986.674999	23.067930
102.272402	2985.800000	23.072947
102.014779	2977.807790	23.077965
101.895104	2977.895825	23.082983
102.177530	2983.157235	23.088000
102.278021	2999.244016	23.093018
102.656334	3002.833546	23.098035
102.648608	2998.848552	23.103053
102.593206	3009.171312	23.108071
102.806883	3005.240217	23.113088
103.013082	3022.465698	23.118106
103.071862	3022.327114	23.123123
103.196681	3025.681534	23.128141
103.005326	3025.430401	23.133159
103.244802	3025.071161	23.138176
103.360232	3035.657701	23.143194
103.630259	3043.483825	23.148211
103.988980	3049.055300	23.153229
103.876478	3052.970589	23.158247
104.272241	3043.693078	23.163264
104.230055	3043.194636	23.168282
104.159515	3054.068943	23.173299
104.252382	3045.630775	23.178317
104.269431	3066.512126	23.183335
104.555972	3066.543229	23.188352
104.511090	3083.410188	23.193370
104.348550	3076.634018	23.198387
104.484785	3074.693854	23.203405
104.773723	3080.197300	23.208423
105.049191	3090.616931	23.213440
105.234917	3099.822806	23.218458
105.264448	3104.937414	23.223475
105.427087	3097.236362	23.228493
105.176687	3098.739758	23.233511
105.716560	3110.462744	23.238528
105.566348	3119.869270	23.243546
105.803392	3132.081276	23.248563
105.791714	3133.433888	23.253581
105.728058	3130.751586	23.258599
105.968072	3114.996658	23.263616
105.721047	3131.134507	23.268634
105.903685	3134.757685	23.273651
106.298977	3136.908558	23.278669
106.106953	3156.591672	23.283687
106.499115	3162.438872	23.288704
106.825647	3173.377675	23.293722
106.687977	3167.538129	23.298739
107.039844	3165.444449	23.303757
106.951911	3169.617898	23.308775
107.135606	3174.124638	23.313792
106.913582	3179.174280	23.318810
107.458990	3192.881670	23.323827
107.870739	3187.786643	23.328845
107.677096	3189.962936	23.333863
107.897211	3187.921328	23.338880
107.854690	3184.882240	23.343898
107.840725	3183.751328	23.348915
108.195005	3176.197149	23.353933
108.196385	3188.000869	23.358951
108.679110	3199.628658	23.363968
108.776623	3200.721251	23.368986
108.501533	3204.551422	23.374003
109.046829	3200.101545	23.379021
108.870299	3200.551921	23.384039
108.690510	3190.843180	23.389056
108.699295	3200.026157	23.394074
108.803236	3191.469419	23.399091
108.845202	3190.746410	23.404109
108.874189	3203.363282	23.409127
109.413058	3204.926861	23.414144
109.189745	3219.820732	23.419162
109.214176	3219.097295	23.424179
109.886024	3220.087846	23.429197
109.465682	3224.442463	23.434215
109.401625	3217.641438	23.439232
109.606297	3230.451907	23.444250
109.796660	3243.867438	23.449267
110.288233	3233.104147	23.454285
109.946151	3245.169684	23.459303
110.319916	3238.000652	23.464320
110.556439	3253.403691	23.469338
110.515433	3264.440802	23.474355
110.989280	3259.194059	23.479373
110.833649	3267.244360	23.484391
111.015757	3265.735739	23.489408
110.882324	3267.025256	23.494426
110.958602	3268.462024	23.499443
111.187904	3268.798719	23.504461
111.193889	3279.304601	23.509479
111.413861	3282.262359	23.514496
111.751826	3285.750919	23.519514
111.423893	3294.535038	23.524531
111.710997	3284.267506	23.529549
111.985631	3302.789251	23.534567
112.228897	3302.786062	23.539584
111.909546	3304.669481	23.544602
112.183430	3306.088112	23.549619
112.440164	3308.232173	23.554637
112.498387	3329.101106	23.559655
112.705263	3329.169863	23.564672
113.019034	3328.016321	23.569690
112.783280	3332.926116	23.574707
113.248496	3319.506229	23.579725
113.100260	3327.302912	23.584743
113.507417	3319.225985	23.589760
113.693083	3323.653552	23.594778
113.359249	3325.412981	23.599795
113.138245	3327.981760	23.604813
113.707281	3337.667783	23.609831
114.008706	3345.811080	23.614848
114.036404	3344.970352	23.619866
113.877750	3354.141602	23.624883
114.048508	3348.822087	23.629901
114.045223	3364.609736	23.634919
114.129644	3370.078833	23.639936
114.633260	3370.751562	23.644954
114.205262	3377.780687	23.649971
114.344968	3370.622794	23.654989
114.428713	3387.924501	23.660007
114.731974	3391.970816	23.665024
114.928787	3394.635519	23.670042
114.749833	3402.490671	23.675059
115.136912	3409.127789	23.680077
115.165453	3426.062542	23.685095
115.250033	3427.365470	23.690112
115.389435	3421.245989	23.695130
115.374597	3432.979802	23.700147
115.992067	3436.699464	23.705165
115.769749	3447.449297	23.710183
115.997958	3447.416892	23.715200
116.107745	3450.701139	23.720218
116.105823	3450.076482	23.725235
116.538477	3447.048586	23.730253
116.177288	3458.599626	23.735271
116.445603	3470.955335	23.740288
116.700504	3471.003991	23.745306
116.594302	3473.210891	23.750323
117.129983	3471.356835	23.755341
117.002362	3469.782796	23.760359
117.236196	3482.667809	23.765376
117.156723	3494.291790	23.770394
117.352645	3489.119814	23.775411
117.269579	3484.404736	23.780429
117.269036	3484.657285	23.785447
117.664064	3498.290480	23.790464
117.962556	3507.608412	23.795482
117.995534	3517.166528	23.800499
117.994675	3508.641737	23.805517
118.369746	3515.145047	23.810535
118.490148	3510.032166	23.815552
118.836045	3510.300213	23.820570
118.631754	3522.628540	23.825587
118.774542	3521.504764	23.830605
118.854586	3539.795084	23.835623
118.683892	3545.237673	23.840640
119.134430	3537.463204	23.845658
118.898929	3534.154263	23.850675
119.409533	3548.889955	23.855693
119.266258	3555.739103	23.860711
119.285159	3567.360439	23.865728
119.580562	3559.979390	23.870746
119.396973	3572.604367	23.875763
119.464711	3576.371772	23.880781
119.449682	3587.846906	23.885799
119.848689	3588.185592	23.890816
120.488207	3598.735054	23.895834
120.331347	3609.440074	23.900851
120.695245	3607.502283	23.905869
120.853322	3609.806927	23.910887
120.813616	3618.240175	23.915904
121.465473	3610.535330	23.920922
120.842151	3606.980603	23.925939
120.703133	3619.428238	23.930957
120.873690	3629.706704	23.935975
120.799225	3627.461570	23.940992
121.408502	3641.399233	23.946010
121.486287	3647.314475	23.951027
121.713180	3653.563157	23.956045
121.962008	3655.935740	23.961063
121.651173	3657.862056	23.966080
121.925134	3667.067110	23.971098
121.811112	3670.581929	23.976115
122.329675	3683.103977	23.981133
122.643736	3677.765211	23.986151
122.514387	3687.979935	23.991168
122.992569	3690.806030	23.996186
122.968915	3704.132131	24.001203
122.986589	3698.318726	24.006221
123.331648	3700.493271	24.011239
123.253958	3704.482187	24.016256
123.148409	3704.735306	24.021274
123.466487	3709.972442	24.026291
123.427578	3718.307769	24.031309
123.633564	3723.388768	24.036327
123.675043	3733.911483	24.041344
123.712049	3721.728931	24.046362
123.599152	3730.688093	24.051379
123.579010	3745.118360	24.056397
124.329909	3749.574812	24.061415
124.056583	3752.824075	24.066432
124.439074	3754.563550	24.071450
124.343707	3763.750404	24.076467
124.806805	3768.949198	24.081485
124.928585	3781.192216	24.086503
124.914627	3777.694082	24.091520
124.987629	3770.082449	24.096538
125.314042	3792.873346	24.101555
125.230901	3794.076165	24.106573
125.332266	3805.444940	24.111591
125.005536	3801.512591	24.116608
125.525544	3810.092348	24.121626
125.906733	3825.561728	24.126643
126.111193	3825.359427	24.131661
126.121732	3821.627063	24.136679
126.188438	3830.671937	24.141696
126.334663	3815.840001	24.146714
126.499306	3834.748699	24.151731
126.315703	3843.753644	24.156749
126.678592	3848.775531	24.161767
126.852385	3852.166669	24.166784
127.038801	3852.124989	24.171802
127.354485	3861.307865	24.176819
127.380384	3871.766804	24.181837
127.560270	3864.255272	24.186855
127.773726	3864.244101	24.191872
128.179962	3863.631633	24.196890
128.185687	3878.938577	24.201907
127.741494	3867.181190	24.206925
127.957153	3866.399549	24.211943
128.123386	3887.050310	24.216960
128.383529	3894.824688	24.221978
128.612928	3893.939906	24.226995
128.700193	3893.307660	24.232013
128.913750	3903.147179	24.237031
128.768085	3894.657377	24.242048
128.990373	3899.868451	24.247066
129.055207	3919.502937	24.252083
128.760005	3923.718298	24.257101
128.705068	3921.975090	24.262119
129.125046	3937.299651	24.267136
129.032410	3937.812733	24.272154
129.384305	3940.879469	24.277171
129.555355	3955.961893	24.282189
129.850910	3967.556196	24.287207
129.638348	3971.383105	24.292224
130.480629	3980.045333	24.297242
130.579282	3985.509245	24.302259
130.691284	3992.722817	24.307277
130.413016	3989.369950	24.312295
130.361203	3986.082827	24.317312
130.626883	3996.264630	24.322330
130.924802	4002.492907	24.327347
131.004830	4000.081640	24.332365
131.168161	4009.859599	24.337383
131.039010	4027.794760	24.342400
131.453676	4033.436739	24.347418
131.845265	4039.464224	24.352435
131.744091	4038.444681	24.357453
132.142176	4050.515456	24.362471
132.158114	4058.015452	24.367488
132.181882	4060.975480	24.372506
132.269433	4057.635084	24.377523
132.404004	4056.496773	24.382541
132.481854	4075.125700	24.387559
132.751053	4085.332255	24.392576
133.243617	4071.206856	24.397594
133.132491	4081.747220	24.402611
133.497172	4082.141762	24.407629
133.571372	4075.991180	24.412647
133.410370	4073.358613	24.417664
133.621204	4077.962357	24.422682
133.717797	4075.788379	24.427699
133.403852	4079.618470	24.432717
133.542097	4086.745930	24.437735
133.811009	4098.385498	24.442752
134.278555	4090.030542	24.447770
134.148106	4099.649129	24.452787
134.428307	4115.446955	24.457805
134.399713	4125.819836	24.462823
134.272103	4128.689817	24.467840
134.663235	4129.013959	24.472858
134.776464	4136.344181	24.477875
134.931102	4148.544457	24.482893
135.067868	4145.373135	24.487911
135.045835	4161.016052	24.492928
135.330755	4172.081882	24.497946
135.542007	4166.872607	24.502963
135.593691	4177.949503	24.507981
135.873223	4190.812126	24.512999
135.921564	4201.517111	24.518016
136.105896	4208.656382	24.523034
136.162621	4202.167595	24.528051
136.448890	4216.313810	24.533069
136.783038	4223.035222	24.538087
136.446094	4232.859626	24.543104
137.007051	4229.543340	24.548122
137.239731	4234.307851	24.553139
137.065708	4242.525577	24.558157
137.533453	4252.824413	24.563175
137.662772	4253.214570	24.568192
137.913891	4248.478826	24.573210
138.100378	4249.813294	24.578227
137.565323	4252.481597	24.583245
137.805010	4243.448717	24.588263
138.090547	4268.260316	24.593280
138.108044	4276.066323	24.598298
138.200286	4274.041347	24.603315
138.176900	4291.108093	24.608333
138.954424	4284.993130	24.613351
138.844913	4293.794226	24.618368
138.677811	4303.352345	24.623386
138.893035	4300.897895	24.628403
138.998154	4308.197886	24.633421
139.140851	4318.623118	24.638439
139.464498	4322.827443	24.643456
139.669707	4335.701741	24.648474
139.864517	4336.435215	24.653491
139.266914	4339.498343	24.658509
139.840562	4341.400652	24.663527
140.280341	4355.030686	24.668544
140.814750	4355.212585	24.673562
140.696912	4363.983448	24.678579
140.589029	4355.623270	24.683597
140.568544	4358.331416	24.688615
140.395374	4372.536658	24.693632
140.972535	4385.387802	24.698650
141.042419	4370.977623	24.703667
141.126535	4388.845218	24.708685
141.608595	4395.130183	24.713703
141.827833	4401.765393	24.718720
141.676054	4403.771182	24.723738
141.765412	4401.958117	24.728755
141.758573	4421.648495	24.733773
141.979052	4429.653381	24.738791
142.116531	4428.700819	24.743808
142.159329	4434.669112	24.748826
142.866275	4447.828356	24.753843
142.775210	4458.233248	24.758861
143.019841	4451.087001	24.763879
142.815977	4461.013907	24.768896
143.103010	4454.833217	24.773914
143.120080	4462.421582	24.778931
143.133637	4480.461227	24.783949
143.457805	4478.933546	24.788967
143.645504	4484.484749	24.793984
143.379311	4493.947923	24.799002
143.861766	4508.865540	24.804019
143.653622	4511.950127	24.809037
144.165105	4508.168038	24.814055
144.640135	4529.169158	24.819072
144.800897	4527.427029	24.824090
144.727769	4523.559198	24.829107
145.062494	4527.872320	24.834125
144.833333	4532.137511	24.839143
145.279649	4545.334247	24.844160
145.268478	4559.785862	24.849178
145.760734	4555.110344	24.854195
145.246444	4555.988947	24.859213
145.872679	4561.623405	24.864231
146.334869	4572.166329	24.869248
146.193135	4580.811606	24.874266
146.552525	4576.866955	24.879283
146.108304	4582.617577	24.884301
146.624816	4573.067976	24.889319
146.710937	4584.578496	24.894336
146.633156	4600.066339	24.899354
147.278283	4597.870026	24.904371
146.926187	4607.375040	24.909389
147.366125	4596.978811	24.914407
147.290950	4606.185044	24.919424
147.428817	4630.559297	24.924442
148.045689	4616.862330	24.929459
147.740930	4627.726702	24.934477
147.748811	4630.168492	24.939495
148.450810	4648.129528	24.944512
147.948359	4655.259114	24.949530
148.369108	4649.022820	24.954547
148.229360	4652.623900	24.959565
148.572619	4663.194863	24.964583
149.313501	4669.275496	24.969600
149.255200	4664.196425	24.974618
149.063246	4666.760868	24.979635
149.088193	4676.137775	24.984653
149.454665	4683.491920	24.989671
149.644433	4688.768257	24.994688
149.442323	4709.291076	24.999706
150.099437	4710.517586	25.004723
149.763748	4726.768508	25.009741
150.149054	4724.691543	25.014759
150.581708	4723.743513	25.019776
150.419811	4732.925434	25.024794
150.745509	4737.132694	25.029811
150.430039	4746.310124	25.034829
150.729899	4750.859146	25.039847
151.033673	4761.909777	25.044864
151.186008	4771.686704	25.049882
151.256098	4775.049971	25.054899
151.268128	4783.311573	25.059917
151.580788	4798.410530	25.064935
151.481069	4800.020017	25.069952
151.539177	4805.531523	25.074970
152.338105	4815.109956	25.079987
152.145000	4828.097121	25.085005
152.415142	4830.914755	25.090023
152.945223	4825.703000	25.095040
152.733072	4825.019489	25.100058
152.997020	4835.732315	25.105075
153.334371	4848.513807	25.110093
153.359306	4846.363520	25.115111
153.765625	4849.333560	25.120128
153.240946	4841.855563	25.125146
153.586092	4839.901625	25.130163
153.942290	4848.359031	25.135181
154.488492	4850.057345	25.140199
154.530711	4858.686739	25.145216
154.913287	4857.383510	25.150234
154.809110	4852.718708	25.155251
155.145272	4854.194053	25.160269
155.136137	4839.331809	25.165287
155.440537	4832.034067	25.170304
155.177956	4836.806404	25.175322
155.529869	4837.581724	25.180339
155.342854	4842.661097	25.185357
155.355751	4850.471225	25.190375
155.808185	4866.672168	25.195392
155.574534	4864.489540	25.200410
155.667004	4870.797451	25.205427
155.837028	4888.838393	25.210445
155.828059	4900.594339	25.215463
156.097289	4905.886776	25.220480
156.367472	4917.403572	25.225498
156.586894	4927.555225	25.230515
156.681384	4932.177301	25.235533
156.629719	4942.696281	25.240551
156.847697	4940.765288	25.245568
157.215249	4965.883875	25.250586
157.669610	4975.029946	25.255603
157.480863	4972.445757	25.260621
158.043017	4972.206694	25.265639
158.162366	4977.806568	25.270656
158.045690	4987.439263	25.275674
158.313646	4991.223139	25.280691
158.885140	4999.688130	25.285709
158.610623	5006.289958	25.290727
158.781301	5005.060743	25.295744
158.883150	5015.928327	25.300762
159.079032	5014.130181	25.305779
159.022123	5035.565075	25.310797
159.239214	5041.616908	25.315815
159.693874	5036.912401	25.320832
159.570684	5043.317077	25.325850
160.087791	5053.826481	25.330867
160.184463	5056.011457	25.335885
160.279074	5048.629501	25.340903
160.729758	5049.742978	25.345920
160.637009	5072.269319	25.350938
160.638019	5067.919515	25.355955
160.865009	5073.426905	25.360973
161.113149	5075.995485	25.365991
161.495856	5085.364252	25.371008
161.446756	5095.245314	25.376026
161.336412	5085.581557	25.381043
161.914866	5099.610374	25.386061
161.682466	5104.965186	25.391079
161.997154	5112.621121	25.396096
162.182960	5123.920762	25.401114
162.350487	5126.861739	25.406131
162.715881	5141.984338	25.411149
162.473804	5151.718712	25.416167
162.952069	5149.232666	25.421184
162.694243	5139.553964	25.426202
162.771153	5158.591338	25.431219
162.897531	5167.251967	25.436237
162.950329	5180.611442	25.441255
163.498737	5186.078295	25.446272
163.562812	5199.770616	25.451290
163.513996	5207.798834	25.456307
163.830017	5223.917170	25.461325
164.029695	5226.944696	25.466343
164.551113	5227.573697	25.471360
164.037505	5246.450580	25.476378
164.550198	5255.117393	25.481395
164.919964	5255.517486	25.486413
164.851982	5276.635580	25.491431
165.105372	5276.198379	25.496448
165.070996	5286.149852	25.501466
165.448240	5299.616727	25.506483
165.623557	5307.730041	25.511501
165.625393	5314.563572	25.516519
166.139946	5318.021880	25.521536
165.979758	5326.111681	25.526554
166.118254	5332.358925	25.531571
166.243665	5342.102474	25.536589
166.682295	5352.163418	25.541607
167.421236	5356.066591	25.546624
167.221682	5359.888608	25.551642
167.549492	5360.999140	25.556659
167.841236	5371.780555	25.561677
167.846920	5382.682270	25.566695
167.692604	5380.736593	25.571712
167.923528	5390.372200	25.576730
168.061926	5385.268616	25.581747
168.642252	5391.743807	25.586765
168.122523	5402.092873	25.591783
168.813083	5400.302899	25.596800
168.781687	5415.414902	25.601818
168.873911	5422.013443	25.606835
168.867861	5436.060922	25.611853
169.363826	5438.209030	25.616871
169.790490	5439.061123	25.621888
169.623168	5453.285237	25.626906
169.630754	5447.548599	25.631923
170.041781	5453.791334	25.636941
170.030504	5467.170465	25.641959
170.560205	5474.155456	25.646976
170.309765	5474.282799	25.651994
170.493294	5482.454887	25.657011
171.005608	5492.769587	25.662029
170.988973	5498.681196	25.667047
171.380642	5498.938997	25.672064
171.553148	5521.030028	25.677082
171.648534	5526.655898	25.682100
171.837370	5521.433944	25.687117
171.789618	5525.617461	25.692135
172.154523	5528.281563	25.697152
172.472816	5543.307663	25.702170
172.963814	5538.508987	25.707188
173.103798	5535.586291	25.712205
173.111381	5535.632428	25.717223
173.635340	5533.795779	25.722240
173.342524	5538.235255	25.727258
173.431931	5526.513659	25.732276
173.369852	5540.099615	25.737293
173.331965	5560.490503	25.742311
173.635806	5563.138865	25.747328
173.873073	5573.796307	25.752346
174.210022	5582.534831	25.757364
174.722104	5579.216445	25.762381
174.654906	5588.920668	25.767399
174.666440	5578.495883	25.772416
174.873845	5584.274785	25.777434
174.680710	5585.725274	25.782452
175.172014	5588.669580	25.787469
174.916015	5603.538929	25.792487
174.788821	5605.739885	25.797504
175.194190	5625.247443	25.802522
175.436777	5635.320127	25.807540
175.802145	5649.691890	25.812557
175.719745	5657.068968	25.817575
175.994683	5665.978171	25.822592
176.123322	5675.696143	25.827610
176.367171	5680.894906	25.832628
176.815483	5699.878179	25.837645
176.601556	5709.324375	25.842663
177.295469	5713.938555	25.847680
177.388308	5731.938689	25.852698
177.168625	5740.915467	25.857716
177.212142	5748.029920	25.862733
177.654441	5761.928932	25.867751
177.849308	5761.343002	25.872768
178.042287	5779.296027	25.877786
178.084364	5788.007956	25.882804
178.723604	5781.112256	25.887821
178.643799	5794.849522	25.892839
179.100258	5798.190705	25.897856
179.379557	5803.734365	25.902874
179.090116	5808.252295	25.907892
179.388622	5820.734331	25.912909
179.459695	5826.004227	25.917927
179.880289	5842.252035	25.922944
179.951461	5844.115946	25.927962
180.060646	5845.683530	25.932980
180.579111	5864.286731	25.937997
180.634045	5877.021376	25.943015
180.931540	5871.207903	25.948032
181.443678	5880.648472	25.953050
181.597435	5886.773580	25.958068
181.956436	5883.740972	25.963085
182.147627	5881.744605	25.968103
182.280150	5879.852071	25.973120
182.239505	5883.510566	25.978138
181.922139	5888.247513	25.983156
182.648798	5884.100199	25.988173
182.876670	5905.867417	25.993191
182.479788	5911.970937	25.998208
183.037890	5912.496399	26.003226
182.673660	5915.119403	26.008244
183.011746	5935.521621	26.013261
183.046747	5947.691227	26.018279
183.168152	5951.349759	26.023296
183.523771	5960.647437	26.028314
183.868571	5979.391432	26.033332
184.124386	5985.494371	26.038349
184.400529	5998.863867	26.043367
184.561139	5992.358268	26.048384
184.716459	6005.203639	26.053402
184.845197	6003.611562	26.058420
185.095702	6017.556414	26.063437
185.585792	6013.569011	26.068455
185.524704	6034.150282	26.073472
185.930919	6036.609161	26.078490
185.924853	6046.411436	26.083508
186.206747	6037.371097	26.088525
186.145434	6047.705976	26.093543
186.271537	6065.505549	26.098560
186.945342	6066.978935	26.103578
186.574442	6072.658630	26.108596
187.048853	6067.518326	26.113613
187.215474	6073.597302	26.118631
187.167687	6091.108308	26.123648
187.275121	6096.401031	26.128666
186.993184	6101.716497	26.133684
187.502786	6116.905842	26.138701
187.624862	6115.377926	26.143719
187.605932	6126.091361	26.148736
187.911525	6131.485823	26.153754
188.262133	6147.400724	26.158772
188.597320	6159.501640	26.163789
189.021695	6163.734908	26.168807
189.156445	6166.169778	26.173824
189.723871	6177.824183	26.178842
189.707090	6181.886232	26.183860
190.013746	6176.604712	26.188877
189.991070	6180.904428	26.193895
189.941870	6184.766341	26.198912
190.349022	6197.992477	26.203930
190.409961	6205.142277	26.208948
190.624305	6211.198085	26.213965
190.974574	6219.884335	26.218983
190.965224	6221.921811	26.224000
190.931917	6224.161887	26.229018
191.234049	6247.186932	26.234036
191.366690	6257.052955	26.239053
191.442375	6273.859915	26.244071
191.924149	6277.124643	26.249088
192.276272	6276.975089	26.254106
192.374670	6297.778048	26.259124
192.565731	6300.983870	26.264141
192.672582	6304.881491	26.269159
192.864990	6319.299651	26.274176
193.358098	6321.082137	26.279194
192.928532	6336.885073	26.284212
193.446730	6339.190821	26.289229
193.659819	6357.390663	26.294247
193.553617	6360.156646	26.299264
193.891819	6368.598624	26.304282
193.927029	6394.048715	26.309300
194.259539	6401.468824	26.314317
194.609143	6406.793381	26.319335
194.543352	6417.735253	26.324352
194.657614	6433.128463	26.329370
194.754116	6441.251397	26.334388
195.469895	6451.260334	26.339405
195.784317	6462.985879	26.344423
195.772884	6465.977033	26.349440
196.011906	6473.822099	26.354458
195.914934	6485.936849	26.359476
196.193949	6502.368281	26.364493
196.660007	6508.419724	26.369511
196.551865	6521.265438	26.374528
197.039574	6518.888227	26.379546
196.962720	6543.396329	26.384564
197.277495	6551.425352	26.389581
197.521277	6562.375934	26.394599
197.415259	6572.898002	26.399616
198.083237	6588.246174	26.404634
198.342995	6600.621135	26.409652
198.530490	6601.772532	26.414669
198.630153	6601.011994	26.419687
198.341553	6618.977687	26.424704
198.864692	6618.706804	26.429722
199.082028	6641.047908	26.434740
199.010391	6640.572891	26.439757
199.692226	6651.752061	26.444775
199.666728	6659.553157	26.449792
200.086289	6663.408483	26.454810
200.178662	6661.825167	26.459828
199.992721	6684.352222	26.464845
200.506081	6682.895924	26.469863
200.356616	6696.654182	26.474880
200.652848	6706.479195	26.479898
201.110461	6725.376857	26.484916
201.462695	6734.025166	26.489933
201.811687	6741.884794	26.494951
201.623601	6749.016754	26.499968
202.133856	6753.350434	26.504986
202.260519	6772.192339	26.510004
202.455475	6768.910488	26.515021
202.892807	6768.902348	26.520039
202.581879	6784.444127	26.525056
203.009426	6792.878706	26.530074
202.708445	6810.777064	26.535092
202.900894	6816.148307	26.540109
203.615309	6837.506267	26.545127
203.239458	6845.320950	26.550144
203.701028	6843.481263	26.555162
203.988469	6867.686854	26.560180
204.141984	6873.051548	26.565197
204.821087	6878.176576	26.570215
204.826596	6902.271424	26.575232
205.366334	6899.860810	26.580250
205.412005	6904.607789	26.585268
205.586001	6909.663096	26.590285
206.124741	6915.457129	26.595303
206.045369	6923.812850	26.600320
206.187110	6928.765854	26.605338
206.128717	6939.239679	26.610356
206.439685	6950.419950	26.615373
206.393020	6955.623269	26.620391
206.782672	6979.528983	26.625408
207.198035	6981.756122	26.630426
207.556046	6989.999583	26.635444
207.293521	7016.339757	26.640461
207.712761	7010.601675	26.645479
207.675523	7028.617025	26.650496
208.019922	7032.847164	26.655514
208.238390	7043.533647	26.660532
208.886341	7042.952902	26.665549
209.174248	7044.634822	26.670567
209.272856	7053.698430	26.675584
209.721142	7063.477864	26.680602
209.932257	7072.397693	26.685620
210.117342	7064.912448	26.690637
210.237614	7064.881064	26.695655
209.965281	7080.663316	26.700672
210.389518	7090.616978	26.705690
210.646590	7101.767850	26.710708
210.612527	7101.662633	26.715725
211.022694	7102.103835	26.720743
210.702041	7119.737227	26.725760
211.289934	7129.315023	26.730778
211.547407	7145.014846	26.735796
211.670611	7150.889433	26.740813
211.834496	7162.913508	26.745831
212.221111	7172.592114	26.750848
212.264776	7177.288966	26.755866
212.362995	7195.049784	26.760884
212.215927	7203.782365	26.765901
212.922072	7211.583434	26.770919
212.961451	7231.484315	26.775936
213.123789	7238.688182	26.780954
213.338353	7254.839895	26.785972
213.545178	7260.793046	26.790989
214.005552	7264.818930	26.796007
214.210363	7281.650907	26.801024
214.153962	7276.794949	26.806042
214.507571	7300.501498	26.811060
214.502007	7308.656492	26.816077
214.982451	7320.688210	26.821095
215.225245	7331.522603	26.826112
215.578636	7338.336882	26.831130
215.577271	7342.160023	26.836148
215.660637	7361.388098	26.841165
216.147744	7370.798614	26.846183
216.188124	7395.119131	26.851200
216.429990	7397.755314	26.856218
216.675397	7415.133546	26.861236
216.634906	7406.486827	26.866253
217.059861	7419.957313	26.871271
217.285533	7432.303418	26.876288
217.415999	7437.356177	26.881306
217.999820	7454.905899	26.886324
218.093140	7465.994095	26.891341
218.439423	7470.776498	26.896359
218.385493	7481.088936	26.901376
218.743747	7487.391099	26.906394
219.215023	7497.239795	26.911412
219.352198	7505.779891	26.916429
219.946829	7504.718118	26.921447
219.795140	7524.393355	26.926464
220.171205	7525.035605	26.931482
220.330083	7530.825838	26.936500
220.133193	7550.179822	26.941517
220.660812	7558.185621	26.946535
220.580936	7562.617685	26.951552
221.112551	7578.041588	26.956570
221.123884	7584.284147	26.961588
221.131597	7596.484352	26.966605
221.434033	7602.953090	26.971623
221.627534	7627.442647	26.976640
221.938061	7645.975859	26.981658
222.225642	7640.646381	26.986676
222.625441	7665.296442	26.991693
222.728545	7666.451575	26.996711
223.322430	7684.448232	27.001728
223.283134	7701.009219	27.006746
223.382102	7702.092389	27.011764
223.140476	7717.191667	27.016781
224.047966	7715.241432	27.021799
224.339534	7727.621673	27.026816
224.640385	7735.988019	27.031834
224.533171	7739.673033	27.036852
224.853133	7764.379853	27.041869
225.341025	7761.355286	27.046887
225.397570	7775.817843	27.051904
225.624142	7792.590076	27.056922
225.770886	7796.554414	27.061940
225.706351	7804.750377	27.066957
226.152671	7809.552021	27.071975
225.895301	7821.683153	27.076992
226.655051	7847.552824	27.082010
226.749599	7850.846555	27.087028
226.773995	7866.270745	27.092045
227.324930	7878.396035	27.097063
227.347059	7889.366134	27.102080
227.503269	7900.719456	27.107098
227.959346	7899.069941	27.112116
228.072493	7923.155682	27.117133
228.420959	7929.813102	27.122151
228.572579	7943.285487	27.127168
228.822754	7956.297406	27.132186
229.482133	7964.030313	27.137204
228.764074	7959.223517	27.142221
229.367140	7973.446452	27.147239
229.818628	7984.409745	27.152256
229.718630	8004.254236	27.157274
229.957344	8007.238266	27.162292
229.988165	8029.928953	27.167309
230.588582	8034.479363	27.172327
230.776166	8049.423694	27.177344
230.908820	8054.185841	27.182362
231.526562	8064.106749	27.187380
231.090906	8077.582268	27.192397
231.810836	8084.488139	27.197415
232.321294	8086.867931	27.202432
232.442889	8103.476843	27.207450
232.955295	8106.244644	27.212468
233.117469	8109.316375	27.217485
233.169546	8122.021454	27.222503
233.509077	8127.521719	27.227520
233.527904	8132.045891	27.232538
233.812106	8142.069281	27.237556
234.167795	8166.827906	27.242573
234.301158	8163.968965	27.247591
234.562159	8169.468841	27.252608
234.418801	8185.512931	27.257626
234.800385	8195.076051	27.262644
235.294602	8209.196149	27.267661
235.424424	8216.203414	27.272679
235.771030	8230.460162	27.277696
235.510896	8235.681291	27.282714
235.702625	8246.199002	27.287732
236.469872	8265.927698	27.292749
236.598678	8273.898034	27.297767
236.579964	8272.830686	27.302784
236.672628	8294.454468	27.307802
237.062742	8301.945307	27.312820
237.519403	8313.296306	27.317837
237.456416	8326.092051	27.322855
237.727379	8341.421424	27.327872
238.200885	8355.036577	27.332890
238.599131	8349.907502	27.337908
238.839117	8362.993907	27.342925
239.091602	8376.122574	27.347943
239.750817	8376.550294	27.352960
239.547800	8395.921904	27.357978
239.830558	8409.279502	27.362996
239.651225	8417.020053	27.368013
240.283566	8434.607357	27.373031
240.155217	8446.519917	27.378048
240.400898	8461.490265	27.383066
240.912729	8466.518662	27.388084
240.867631	8483.766337	27.393101
241.154987	8493.710502	27.398119
241.433406	8504.407444	27.403136
241.415770	8528.789001	27.408154
241.791645	8541.879634	27.413172
242.183198	8552.934682	27.418189
242.770500	8578.870116	27.423207
242.847541	8577.819413	27.428224
242.809229	8594.759898	27.433242
243.337670	8595.258497	27.438260
243.475174	8616.231631	27.443277
243.843556	8634.258013	27.448295
244.163850	8641.036889	27.453312
244.175660	8643.333377	27.458330
244.760449	8659.112975	27.463348
244.309371	8661.431017	27.468365
244.758716	8681.029698	27.473383
245.227664	8678.759322	27.478400
245.079525	8690.441495	27.483418
245.049623	8708.324746	27.488436
245.815113	8721.799999	27.493453
245.961826	8735.273727	27.498471
246.488925	8738.901227	27.503488
246.222141	8761.244508	27.508506
246.829753	8759.855466	27.513524
247.085167	8779.771741	27.518541
247.538690	8786.747770	27.523559
247.762315	8801.336660	27.528576
248.026118	8813.895596	27.533594
248.334583	8814.598934	27.538612
248.647821	8822.663921	27.543629
248.961072	8833.914442	27.548647
249.743860	8828.447542	27.553664
249.918603	8835.729031	27.558682
250.072123	8822.539922	27.563700
249.858773	8837.518898	27.568717
249.912268	8843.117581	27.573735
250.157281	8846.823748	27.578752
250.443863	8875.035343	27.583770
250.944751	8877.179946	27.588788
250.880718	8880.719550	27.593805
250.928161	8902.916210	27.598823
251.464697	8908.670180	27.603840
251.275099	8932.425516	27.608858
251.381095	8949.871101	27.613876
251.684848	8964.075103	27.618893
251.887589	8976.785728	27.623911
252.135764	8987.225616	27.628928
252.322084	9012.447430	27.633946
252.633464	9031.089246	27.638964
253.048840	9039.056341	27.643981
253.379303	9070.898443	27.648999
253.516729	9084.765359	27.654016
254.009611	9102.940146	27.659034
254.471431	9120.106336	27.664052
254.378584	9124.130361	27.669069
254.857595	9142.228416	27.674087
255.794209	9150.603771	27.679104
255.826944	9150.857531	27.684122
256.087910	9166.972125	27.689140
256.617260	9164.442872	27.694157
256.759252	9176.459042	27.699175
257.112947	9177.900446	27.704192
256.874633	9186.720783	27.709210
257.425550	9196.917912	27.714228
257.560935	9210.166433	27.719245
257.406351	9219.096880	27.724263
257.705173	9225.206835	27.729280
257.883886	9254.739720	27.734298
258.172633	9263.023401	27.739316
258.429982	9275.678372	27.744333
258.512083	9295.978949	27.749351
258.750591	9312.930666	27.754368
258.858437	9326.470862	27.759386
259.396013	9333.613973	27.764404
259.658854	9353.479195	27.769421
259.842452	9376.457154	27.774439
260.216492	9392.008143	27.779456
260.394278	9400.287061	27.784474
261.014801	9421.533202	27.789492
261.258734	9434.916530	27.794509
261.119489	9451.901927	27.799527
261.697379	9455.262772	27.804544
261.719127	9477.277843	27.809562
262.094018	9485.570314	27.814580
262.100052	9488.720257	27.819597
262.361943	9509.210925	27.824615
262.968940	9516.002318	27.829632
263.255852	9537.174241	27.834650
263.176581	9539.077736	27.839668
263.859594	9552.430678	27.844685
263.715690	9559.253746	27.849703
264.090367	9578.681884	27.854720
264.259412	9594.605940	27.859738
264.333545	9605.164833	27.864756
264.841032	9626.289889	27.869773
264.865050	9640.556904	27.874791
265.496490	9662.685654	27.879808
265.673810	9674.046251	27.884826
265.594908	9693.614586	27.889844
266.199187	9703.080674	27.894861
266.428109	9736.442586	27.899879
266.458928	9748.021788	27.904896
266.510537	9762.755035	27.909914
266.915831	9776.820719	27.914932
267.585400	9787.981616	27.919949
267.397317	9815.097190	27.924967
268.122587	9820.162192	27.929984
268.870525	9839.608267	27.935002
269.164799	9832.591130	27.940020
269.778580	9846.832789	27.945037
269.571726	9863.330236	27.950055
270.191455	9850.269882	27.955072
270.139908	9874.838455	27.960090
270.539704	9872.521873	27.965108
271.190167	9879.114038	27.970125
271.189515	9896.065635	27.975143
271.474994	9903.008261	27.980160
271.705139	9905.469823	27.985178
271.719835	9919.549066	27.990196
272.465263	9924.781453	27.995213
272.563455	9936.242935	28.000231
272.670272	9935.376958	28.005248
272.833146	9956.167693	28.010266
272.800626	9957.662974	28.015284
273.325927	9965.250265	28.020301
273.460994	9981.940855	28.025319
273.678135	9999.288033	28.030336
273.659106	10008.046202	28.035354
274.008107	10030.923445	28.040372
274.058925	10048.527048	28.045389
273.809675	10064.194581	28.050407
274.506235	10086.275811	28.055424
275.079096	10113.686962	28.060442
275.370217	10137.182713	28.065460
276.055099	10145.174632	28.070477
275.695870	10170.827103	28.075495
276.449790	10182.865479	28.080512
276.444490	10207.187331	28.085530
276.541156	10217.638871	28.090548
277.041836	10237.032295	28.095565
277.526840	10241.121309	28.100583
278.149745	10247.657908	28.105600
278.584700	10271.586095	28.110618
278.946381	10276.616266	28.115636
279.428839	10274.248878	28.120653
279.158349	10294.498088	28.125671
279.521569	10297.093696	28.130688
280.254367	10307.098940	28.135706
279.967301	10321.114958	28.140724
280.465971	10330.420998	28.145741
280.444023	10342.662361	28.150759
280.775974	10347.012029	28.155776
280.652172	10365.189342	28.160794
280.705257	10382.543474	28.165812
281.275828	10390.174411	28.170829
281.344080	10406.945246	28.175847
281.523708	10421.210735	28.180864
281.902198	10440.364489	28.185882
282.048616	10445.709227	28.190900
282.661702	10466.348348	28.195917
282.585389	10489.289212	28.200935
283.255930	10508.249171	28.205952
283.629859	10527.542651	28.210970
283.710863	10540.642716	28.215988
284.335481	10546.790794	28.221005
284.438501	10572.798102	28.226023
284.586761	10589.231431	28.231040
285.139338	10607.830967	28.236058
285.500820	10613.495902	28.241076
285.600394	10613.003598	28.246093
285.726611	10638.423263	28.251111
286.062613	10646.463401	28.256128
286.630577	10663.191400	28.261146
286.612143	10678.037314	28.266164
286.986577	10695.689026	28.271181
287.032361	10715.876822	28.276199
287.381644	10733.961897	28.281216
287.585047	10750.989855	28.286234
287.755389	10776.563869	28.291252
288.147772	10791.715336	28.296269
288.197443	10817.829172	28.301287
288.545827	10831.080419	28.306304
288.737694	10859.410812	28.311322
289.169081	10883.034066	28.316340
289.487042	10905.336242	28.321357
290.082196	10924.857762	28.326375
290.612001	10939.801665	28.331392
291.023512	10954.596649	28.336410
290.833093	10979.061996	28.341428
291.448414	10991.864484	28.346445
291.762521	11013.962154	28.351463
292.159685	11020.638369	28.356480
292.317545	11039.719733	28.361498
292.650176	11048.745707	28.366516
292.590649	11055.016253	28.371533
293.436479	11087.147842	28.376551
293.210335	11097.653290	28.381568
294.341431	11099.958960	28.386586
294.249176	11106.828229	28.391604
294.593172	11120.528731	28.396621
294.697079	11137.282041	28.401639
295.478447	11157.722066	28.406656
295.634781	11165.089432	28.411674
295.674488	11181.167596	28.416692
296.360693	11196.936728	28.421709
296.740089	11220.116978	28.426727
296.799917	11232.343034	28.431744
296.943345	11233.845758	28.436762
296.665792	11254.046583	28.441780
297.342689	11259.754179	28.446797
297.204914	11284.022276	28.451815
297.624469	11299.454103	28.456832
298.453374	11330.376254	28.461850
298.291339	11344.297790	28.466868
298.634595	11360.565666	28.471885
298.533547	11376.880623	28.476903
298.777421	11393.694468	28.481920
299.318210	11416.259373	28.486938
299.381741	11446.340975	28.491956
299.924566	11462.053714	28.496973
300.199233	11484.928526	28.501991
300.563454	11499.301876	28.507008
300.802575	11512.141188	28.512026
301.453516	11543.675548	28.517044
301.771207	11542.584057	28.522061
301.927857	11570.093723	28.527079
301.947111	11583.627249	28.532096
302.313677	11594.602748	28.537114
302.706745	11628.138257	28.542132
303.047052	11635.549791	28.547149
303.388342	11654.053804	28.552167
303.636507	11677.068753	28.557184
304.358227	11693.363252	28.562202
304.253971	11718.015076	28.567220
305.037695	11719.481307	28.572237
304.833491	11736.813599	28.577255
304.977702	11760.309002	28.582272
305.408768	11770.523051	28.587290
305.603281	11799.163900	28.592308
305.793817	11815.209653	28.597325
306.429320	11838.909697	28.602343
306.655020	11843.497293	28.607360
307.462803	11869.434573	28.612378
307.654843	11886.329556	28.617396
308.196208	11906.937230	28.622413
308.626145	11911.931958	28.627431
308.507519	11936.633670	28.632448
309.039848	11944.921676	28.637466
308.719719	11967.823367	28.642484
309.632607	11988.648007	28.647501
309.864576	12008.321931	28.652519
309.902706	12030.129054	28.657536
310.337063	12043.629862	28.662554
310.457879	12069.825938	28.667572
310.758865	12086.334692	28.672589
311.139475	12108.003330	28.677607
311.367809	12127.030622	28.682624
312.189405	12141.437463	28.687642
312.174471	12168.759997	28.692660
312.644407	12177.048346	28.697677
312.943998	12208.341702	28.702695
313.160486	12214.670710	28.707712
313.763557	12228.356951	28.712730
314.132829	12253.662025	28.717748
314.279902	12259.247165	28.722765
314.640294	12271.272378	28.727783
314.728920	12292.279361	28.732800
315.279778	12300.580429	28.737818
315.426177	12316.077725	28.742836
315.837729	12332.398967	28.747853
316.093732	12358.609133	28.752871
316.334720	12375.032750	28.757888
316.645226	12387.934176	28.762906
317.162990	12408.912372	28.767924
317.281777	12425.904503	28.772941
317.657628	12446.841680	28.777959
318.042593	12453.191905	28.782976
318.564546	12474.365302	28.787994
318.397234	12490.887321	28.793012
318.811696	12511.035440	28.798029
319.130310	12535.344619	28.803047
319.467375	12550.796637	28.808064
320.054351	12560.961583	28.813082
320.266866	12585.745219	28.818100
320.472999	12603.810178	28.823117
321.160766	12613.211073	28.828135
321.106241	12625.304267	28.833152
321.787274	12628.267551	28.838170
322.144447	12643.334425	28.843188
322.627788	12648.627340	28.848205
322.688174	12667.889738	28.853223
322.942606	12673.714067	28.858240
323.358333	12683.858375	28.863258
323.404814	12699.248389	28.868276
322.992425	12721.865369	28.873293
324.088002	12735.405836	28.878311
324.029620	12757.781437	28.883328
324.483838	12777.655242	28.888346
324.760271	12795.785227	28.893364
325.110783	12810.483812	28.898381
325.211343	12836.750421	28.903399
325.629934	12856.377232	28.908416
325.780021	12873.721724	28.913434
325.776299	12895.533206	28.918452
326.508025	12927.739401	28.923469
327.185764	12942.039786	28.928487
327.255743	12971.664939	28.933504
327.487297	12986.647437	28.938522
327.991943	13013.798729	28.943540
328.378698	13031.384409	28.948557
328.933083	13045.129352	28.953575
328.701701	13080.157270	28.958592
329.505899	13097.611709	28.963610
329.818401	13114.700615	28.968628
330.296526	13136.885774	28.973645
330.553829	13153.045429	28.978663
330.814184	13168.453055	28.983680
331.113316	13194.945034	28.988698
331.178886	13212.410362	28.993716
331.611221	13228.555464	28.998733
332.371074	13247.801137	29.003751
332.553773	13267.802992	29.008768
332.828826	13283.151581	29.013786
333.213203	13319.644066	29.018804
333.514140	13336.539186	29.023821
333.641344	13350.846643	29.028839
334.136190	13385.001015	29.033856
334.393685	13395.647181	29.038874
334.973308	13420.611602	29.043892
335.233681	13448.843653	29.048909
335.556865	13457.003838	29.053927
335.689966	13480.717853	29.058944
336.065704	13499.603583	29.063962
336.616959	13527.146253	29.068980
336.495798	13554.531540	29.073997
337.088055	13565.375161	29.079015
337.479818	13597.177528	29.084032
338.300944	13607.612908	29.089050
338.623772	13622.063801	29.094068
339.018289	13634.447734	29.099085
339.252345	13662.441041	29.104103
339.333550	13676.689590	29.109120
339.904477	13685.891318	29.114138
340.348698	13708.707698	29.119156
340.249196	13730.241365	29.124173
340.842053	13744.618734	29.129191
341.019327	13760.497679	29.134208
341.627956	13775.024197	29.139226
342.060373	13803.043674	29.144244
341.722573	13819.214439	29.149261
342.026754	13830.289380	29.154279
342.335388	13865.218887	29.159296
342.735704	13895.138276	29.164314
343.352401	13909.812067	29.169332
343.372614	13927.433540	29.174349
343.657730	13944.956946	29.179367
343.998535	13966.937084	29.184384
344.416977	13985.447166	29.189402
344.604717	14008.237520	29.194420
344.573010	14028.210397	29.199437
345.097660	14045.636603	29.204455
345.512144	14081.276368	29.209472
346.146202	14108.137497	29.214490
346.305375	14119.762570	29.219508
346.364236	14155.154669	29.224525
346.859297	14179.526918	29.229543
347.522930	14212.121709	29.234560
347.626523	14234.704372	29.239578
347.994576	14256.589021	29.244596
348.212020	14283.998437	29.249613
348.631462	14302.669734	29.254631
349.284869	14339.030716	29.259648
349.344096	14366.199607	29.264666
350.428516	14388.658178	29.269684
350.629922	14413.676476	29.274701
351.423671	14422.884929	29.279719
351.532897	14448.978731	29.284736
352.081387	14467.156390	29.289754
352.457367	14471.490694	29.294772
352.629866	14492.019668	29.299789
353.006168	14496.353928	29.304807
353.200236	14503.508293	29.309824
353.665456	14524.004363	29.314842
354.486335	14531.007468	29.319860
354.734420	14557.534564	29.324877
355.296662	14563.857905	29.329895
355.528291	14579.189042	29.334912
355.564034	14592.090537	29.339930
355.882475	14610.664170	29.344948
356.009641	14636.430153	29.349965
356.243395	14652.436850	29.354983
356.473518	14672.281215	29.360000
356.667122	14704.567897	29.365018
357.166928	14722.715483	29.370036
357.391782	14750.958159	29.375053
358.011441	14773.293741	29.380071
358.431731	14799.522767	29.385088
359.057069	14822.498620	29.390106
359.150007	14837.497847	29.395124
359.605830	14859.685339	29.400141
360.285699	14882.813841	29.405159
360.089921	14912.300225	29.410176
360.049831	14936.829397	29.415194
360.342529	14953.158775	29.420212
360.648499	14988.984517	29.425229
361.554696	15010.634664	29.430247
362.187492	15046.125399	29.435264
362.276146	15068.196597	29.440282
362.648881	15092.124812	29.445300
363.029478	15120.672240	29.450317
363.149097	15137.129782	29.455335
363.521489	15166.029112	29.460352
364.106260	15194.371164	29.465370
364.374216	15210.518282	29.470388
364.609358	15255.463767	29.475405
364.949622	15268.109871	29.480423
365.541674	15301.598811	29.485440
365.754752	15317.441901	29.490458
365.949707	15337.624045	29.495476
366.352014	15371.373197	29.500493
366.927120	15399.148579	29.505511
367.371416	15426.012691	29.510528
367.486721	15451.320520	29.515546
368.077734	15461.849602	29.520564
368.473615	15492.615442	29.525581
368.385361	15515.393718	29.530599
368.771278	15532.040694	29.535616
368.891670	15558.096376	29.540634
369.971569	15579.331665	29.545652
370.202514	15610.628693	29.550669
370.765304	15643.573253	29.555687
370.786557	15670.257224	29.560704
371.195412	15686.651261	29.565722
371.670498	15705.706898	29.570740
371.779874	15741.593082	29.575757
372.377988	15760.645412	29.580775
372.958544	15789.977546	29.585792
372.840213	15816.803467	29.590810
373.613679	15837.853037	29.595828
373.468517	15869.300631	29.600845
374.473555	15882.270019	29.605863
374.937351	15911.074131	29.610880
375.220025	15935.721726	29.615898
376.039838	15951.470884	29.620916
376.404967	15972.249392	29.625933
377.001444	15988.181791	29.630951
377.196394	15999.830866	29.635968
377.484936	16023.457524	29.640986
378.170482	16032.576227	29.646004
378.602815	16055.798381	29.651021
378.937330	16072.498048	29.656039
379.411733	16077.970190	29.661056
379.302909	16098.408880	29.666074
380.050091	16112.546095	29.671092
379.839044	16132.915460	29.676109
380.088096	16158.433961	29.681127
380.587977	16177.843102	29.686144
381.084980	16205.366516	29.691162
381.461252	16229.150320	29.696180
381.435782	16264.050960	29.701197
381.930810	16285.463367	29.706215
382.618279	16314.113246	29.711232
382.816174	16339.801030	29.716250
383.401242	16355.678660	29.721268
383.764370	16374.063868	29.726285
384.392472	16397.249642	29.731303
384.676043	16416.705334	29.736320
384.891993	16445.264580	29.741338
385.802649	16461.660122	29.746356
385.957377	16483.530003	29.751373
386.065091	16502.627836	29.756391
386.912465	16528.881183	29.761408
386.783410	16542.659261	29.766426
387.057000	16560.666944	29.771444
387.520460	16586.781160	29.776461
387.740150	16614.721026	29.781479
388.008116	16640.126679	29.786496
388.560909	16668.971768	29.791514
389.223554	16701.915238	29.796532
389.472264	16726.644940	29.801549
389.769209	16755.776349	29.806567
390.262949	16769.100728	29.811584
390.365323	16800.170196	29.816602
390.921594	16833.209413	29.821620
391.390038	16858.798919	29.826637
392.053316	16873.148743	29.831655
392.234021	16902.399541	29.836672
392.625305	16929.185578	29.841690
392.975536	16960.121964	29.846708
393.058532	16977.907031	29.851725
393.277276	17003.684052	29.856743
394.227614	17023.251333	29.861760
394.151967	17056.348250	29.866778
394.753516	17081.310900	29.871796
395.441599	17105.186221	29.876813
395.811554	17123.027821	29.881831
396.419255	17138.267719	29.886848
396.672301	17158.414310	29.891866
396.987128	17170.222310	29.896884
397.373029	17189.375430	29.901901
397.526643	17216.277830	29.906919
397.966786	17229.538227	29.911936
398.327323	17254.447026	29.916954
398.785758	17282.527571	29.921972
398.979542	17316.047293	29.926989
398.996802	17345.159965	29.932007
400.105314	17363.057370	29.937024
400.100298	17398.171662	29.942042
400.635172	17420.735161	29.947060
400.790149	17453.484159	29.952077
401.618725	17472.274898	29.957095
401.782818	17502.429383	29.962112
402.380962	17525.684357	29.967130
402.476928	17552.662530	29.972148
403.200571	17595.001108	29.977165
403.584901	17610.683613	29.982183
404.119269	17641.775624	29.987200
404.341873	17675.923201	29.992218
404.943720	17703.138689	29.997236
405.218443	17722.363342	30.002253
405.694335	17757.115986	30.007271
406.056867	17785.348014	30.012288
406.188557	17809.421380	30.017306
406.823399	17839.626290	30.022324
407.150672	17868.129253	30.027341
407.513097	17902.577642	30.032359
408.388522	17928.184177	30.037376
408.392580	17956.289061	30.042394
408.737652	17980.683188	30.047412
409.471184	18017.430356	30.052429
409.743250	18044.337579	30.057447
410.099740	18057.895849	30.062464
410.749212	18101.062017	30.067482
411.102951	18117.128735	30.072500
411.734344	18149.766840	30.077517
412.211207	18173.616355	30.082535
413.067069	18188.272001	30.087552
412.855792	18208.817318	30.092570
413.222522	18233.821177	30.097588
413.512402	18257.883108	30.102605
413.919774	18288.995932	30.107623
414.703383	18313.233764	30.112640
414.759811	18348.621338	30.117658
415.321616	18371.169122	30.122676
415.844161	18400.059417	30.127693
416.146272	18423.014101	30.132711
416.493228	18451.167399	30.137728
416.718921	18476.597844	30.142746
417.125542	18502.372885	30.147764
417.894943	18533.631900	30.152781
418.247961	18574.728926	30.157799
418.628269	18598.518186	30.162816
419.111830	18624.641508	30.167834
419.027557	18650.985934	30.172852
419.298662	18683.270391	30.177869
419.995054	18710.200925	30.182887
420.284287	18738.578422	30.187904
420.978172	18779.313256	30.192922
421.472958	18802.705891	30.197940
421.767207	18822.339239	30.202957
422.092997	18848.506378	30.207975
422.846897	18864.757805	30.212992
422.564886	18897.160313	30.218010
422.993692	18917.789941	30.223028
423.527283	18954.190959	30.228045
424.001996	18990.967633	30.233063
424.377440	19016.154355	30.238080
425.034141	19041.107795	30.243098
425.189993	19077.504673	30.248116
425.690578	19098.533965	30.253133
425.987524	19138.920701	30.258151
426.478122	19168.360433	30.263168
426.832066	19202.711370	30.268186
427.506677	19238.345480	30.273204
428.034360	19257.671266	30.278221
428.507003	19288.971380	30.283239
429.024462	19317.825927	30.288256
429.505707	19345.637412	30.293274
429.587465	19381.572565	30.298292
430.183460	19400.306626	30.303309
430.800183	19429.000577	30.308327
431.568139	19454.910163	30.313344
431.474697	19493.797922	30.318362
431.851202	19520.962597	30.323380
432.499654	19545.545220	30.328397
432.714545	19588.763399	30.333415
432.985398	19610.669278	30.338432
433.516614	19654.021573	30.343450
434.182357	19678.949153	30.348468
434.687112	19711.179987	30.353485
434.936079	19744.088798	30.358503
435.692528	19771.839095	30.363520
436.196143	19808.928708	30.368538
436.537412	19828.182996	30.373556
437.026001	19862.552042	30.378573
437.258545	19890.826322	30.383591
437.534887	19913.123396	30.388608
438.236458	19952.324237	30.393626
438.595261	19973.363911	30.398644
439.070103	20001.392139	30.403661
439.685297	20046.697112	30.408679
440.011243	20074.116829	30.413696
440.074532	20107.156246	30.418714
440.922853	20145.715467	30.423732
441.598051	20171.495134	30.428749
441.939621	20201.092306	30.433767
442.348157	20216.937418	30.438784
442.926217	20255.557885	30.443802
443.489718	20285.809299	30.448820
444.022280	20310.676287	30.453837
444.306775	20340.250964	30.458855
444.702245	20357.387107	30.463872
445.151508	20383.050594	30.468890
445.222278	20407.130339	30.473908
446.153444	20440.502746	30.478925
446.456459	20464.963400	30.483943
446.707167	20489.925039	30.488960
447.293679	20518.094576	30.493978
448.154837	20554.611858	30.498996
448.598966	20577.490109	30.504013
448.660408	20606.089012	30.509031
449.105832	20628.095217	30.514048
449.309456	20658.542232	30.519066
449.762707	20682.676498	30.524084
449.933316	20710.601470	30.529101
450.700278	20750.867821	30.534119
451.157818	20779.714904	30.539136
451.213580	20805.964615	30.544154
451.980872	20841.511406	30.549172
452.492567	20862.957875	30.554189
452.645191	20899.649286	30.559207
452.784159	20923.163043	30.564224
453.455981	20960.494020	30.569242
453.848270	20988.959837	30.574260
454.419110	21008.242730	30.579277
455.023601	21058.132454	30.584295
455.539010	21070.240153	30.589312
455.996615	21108.622005	30.594330
456.149715	21140.726709	30.599348
456.751789	21165.040586	30.604365
457.042286	21206.430889	30.609383
457.750761	21227.474340	30.614400
458.491408	21267.948038	30.619418
458.839997	21301.779072	30.624436
459.317903	21320.571272	30.629453
459.599641	21360.421581	30.634471
459.982731	21382.886943	30.639488
460.578369	21418.170857	30.644506
460.673699	21449.488940	30.649524
461.109704	21483.534141	30.654541
461.594957	21525.994202	30.659559
461.900829	21559.788101	30.664576
462.506797	21607.631813	30.669594
463.402420	21646.275084	30.674612
463.902041	21676.506997	30.679629
464.496033	21708.038510	30.684647
464.787449	21738.189198	30.689664
465.156534	21770.476133	30.694682
465.426046	21812.085805	30.699700
466.326561	21834.332123	30.704717
466.667506	21870.199891	30.709735
466.886772	21904.753452	30.714752
467.756273	21942.978030	30.719770
468.157085	21979.525400	30.724788
468.834161	22005.389330	30.729805
468.536107	22045.539798	30.734823
469.321850	22080.536241	30.739840
469.839352	22118.746453	30.744858
470.135093	22165.546694	30.749876
471.000697	22204.953971	30.754893
471.263841	22236.607341	30.759911
471.704636	22267.550689	30.764928
472.527027	22302.554458	30.769946
473.033885	22337.860159	30.774964
473.486628	22368.271035	30.779981
473.581853	22404.955227	30.784999
474.335376	22430.731989	30.790016
475.326079	22453.735853	30.795034
475.616298	22489.530499	30.800052
476.220201	22514.597690	30.805069
476.663473	22540.397620	30.810087
476.965462	22572.152899	30.815104
477.707862	22600.275877	30.820122
477.879107	22632.980467	30.825140
478.567567	22659.930315	30.830157
479.165712	22697.174953	30.835175
479.237984	22730.280559	30.840192
479.958138	22753.630194	30.845210
479.925889	22795.440564	30.850228
480.238308	22822.632421	30.855245
481.047069	22855.402421	30.860263
481.529550	22892.583289	30.865280
481.983499	22922.337666	30.870298
482.218734	22952.846491	30.875316
482.978296	22984.613343	30.880333
483.283826	23017.664158	30.885351
483.420765	23051.284701	30.890368
484.221340	23077.099215	30.895386
484.518006	23116.312529	30.900404
484.790731	23147.700468	30.905421
485.442034	23184.305852	30.910439
485.844910	23215.945352	30.915456
486.514053	23250.090001	30.920474
486.591926	23295.783093	30.925492
487.228380	23323.316969	30.930509
488.098775	23364.014887	30.935527
488.007774	23398.404509	30.940544
489.001617	23427.487926	30.945562
488.873211	23475.406248	30.950580
489.646314	23508.429323	30.955597
490.068669	23541.841967	30.960615
490.353280	23586.543042	30.965632
491.003757	23628.697535	30.970650
490.997000	23670.733263	30.975668
491.790394	23710.761416	30.980685
492.895348	23762.583218	30.985703
493.160136	23804.084062	30.990720
494.142183	23846.528632	30.995738
494.312685	23880.966844	31.000756
495.080945	23911.293053	31.005773
495.298198	23953.585187	31.010791
495.703259	23994.186220	31.015808
496.249445	24027.890043	31.020826
496.715510	24078.485091	31.025844
497.420151	24113.712608	31.030861
498.094097	24152.907145	31.035879
498.600886	24184.847973	31.040896
499.024751	24224.713511	31.045914
499.580989	24269.190571	31.050932
500.286928	24303.343939	31.055949
500.930226	24337.639823	31.060967
501.009328	24376.175403	31.065984
501.564054	24410.188191	31.071002
502.137999	24448.198201	31.076020
502.756932	24480.020934	31.081037
502.972836	24515.173579	31.086055
503.434559	24565.915884	31.091072
504.064304	24592.839580	31.096090
504.608981	24635.398156	31.101108
505.157826	24675.409442	31.106125
505.727960	24710.134438	31.111143
506.152501	24752.964744	31.116160
506.774921	24789.628132	31.121178
507.728732	24814.542643	31.126196
508.343086	24838.416760	31.131213
508.789350	24882.602651	31.136231
509.169559	24915.107829	31.141248
509.906896	24929.610040	31.146266
510.231488	24965.346910	31.151284
510.346761	25003.555770	31.156301
511.025360	25033.322566	31.161319
511.334924	25078.332752	31.166336
511.607420	25112.188445	31.171354
512.266744	25156.942132	31.176372
512.868534	25190.544468	31.181389
513.296616	25226.114021	31.186407
513.335951	25276.904923	31.191424
514.439757	25315.636686	31.196442
515.598707	25334.099164	31.201460
517.117476	25327.290272	31.206477
517.717936	25353.511753	31.211495
518.347766	25375.431332	31.216512
518.805888	25374.304600	31.221530
519.018208	25381.305290	31.226548
519.283314	25408.748186	31.231565
519.736457	25410.510314	31.236583
519.842841	25439.722189	31.241600
520.218558	25445.894867	31.246618
520.361988	25472.592111	31.251636
520.585696	25506.967961	31.256653
521.090047	25533.836609	31.261671
521.501516	25580.810126	31.266688
521.876840	25603.205635	31.271706
522.346662	25642.991006	31.276724
522.553353	25690.615992	31.281741
523.229178	25730.950885	31.286759
523.475348	25776.345371	31.291776
523.920900	25814.314763	31.296794
524.654710	25863.204213	31.301812
524.750495	25905.904886	31.306829
525.518012	25952.754324	31.311847
525.670050	26007.251908	31.316864
526.515141	26058.627170	31.321882
527.396230	26108.309550	31.326900
527.781642	26153.202897	31.331917
528.249839	26193.697438	31.336935
528.624052	26244.489208	31.341952
529.169270	26289.326380	31.346970
529.563344	26334.907656	31.351988
530.341922	26378.962944	31.357005
531.113687	26435.153757	31.362023
531.675103	26485.329231	31.367040
532.174723	26523.222022	31.372058
532.863903	26565.420911	31.377076
533.506057	26610.161545	31.382093
534.250213	26646.581850	31.387111
534.418146	26693.311468	31.392128
534.820155	26740.832685	31.397146
535.465788	26791.703659	31.402164
536.063770	26844.219087	31.407181
536.697670	26878.697740	31.412199
537.091884	26930.676304	31.417216
537.944977	26964.223520	31.422234
538.365000	27006.168183	31.427252
538.909690	27052.549251	31.432269
539.448151	27080.312117	31.437287
539.699355	27148.050772	31.442304
540.192357	27188.075748	31.447322
541.011545	27230.736124	31.452340
541.341460	27284.014931	31.457357
542.065725	27325.344070	31.462375
542.537146	27374.037856	31.467392
543.053379	27416.056874	31.472410
543.757231	27456.858554	31.477428
543.886083	27506.964853	31.482445
545.042807	27541.388526	31.487463
545.661348	27598.718801	31.492480
546.366992	27635.526103	31.497498
546.855741	27675.521102	31.502516
547.287463	27715.329125	31.507533
547.977875	27750.249212	31.512551
548.399048	27798.300837	31.517568
549.251662	27839.124370	31.522586
549.621615	27883.094856	31.527604
550.105052	27914.653372	31.532621
550.855926	27957.920035	31.537639
551.340700	28002.030915	31.542656
551.812785	28040.227891	31.547674
552.592879	28070.722869	31.552692
552.684969	28115.489252	31.557709
553.465814	28148.348100	31.562727
554.008666	28186.919887	31.567744
554.192802	28220.358425	31.572762
554.991669	28253.840372	31.577780
555.394671	28301.826487	31.582797
555.980262	28324.381894	31.587815
556.284591	28385.163769	31.592832
556.748258	28416.643974	31.597850
557.327938	28459.603361	31.602868
558.123411	28502.257459	31.607885
558.908516	28539.717695	31.612903
559.155270	28587.261078	31.617920
559.582747	28621.256533	31.622938
559.884907	28659.379991	31.627956
560.432311	28710.106723	31.632973
560.738815	28761.623247	31.637991
561.072287	28820.511988	31.643008
561.896695	28862.561866	31.648026
562.940551	28903.654838	31.653044
563.409838	28961.012182	31.658061
564.096857	29003.267040	31.663079
564.634585	29059.868154	31.668096
565.654614	29100.200414	31.673114
566.567905	29134.942800	31.678132
566.972937	29168.632939	31.683149
567.894587	29209.176676	31.688167
568.341279	29254.086296	31.693184
568.788274	29287.460376	31.698202
570.027540	29318.309239	31.703220
570.295708	29370.003926	31.708237
570.701310	29387.563417	31.713255
571.136072	29433.195870	31.718272
571.593271	29469.539488	31.723290
572.602105	29507.472344	31.728308
572.811814	29545.327403	31.733325
573.605229	29583.654229	31.738343
573.876928	29624.224118	31.743360
574.474101	29670.678826	31.748378
574.743340	29705.452913	31.753396
575.129743	29754.785072	31.758413
575.902567	29781.364712	31.763431
576.724651	29832.266378	31.768448
577.364770	29867.450760	31.773466
578.252304	29902.369127	31.778484
578.480142	29950.285239	31.783501
578.962326	29986.859764	31.788519
579.719407	30037.241086	31.793536
580.489819	30075.970643	31.798554
581.137340	30121.672642	31.803572
581.419773	30167.595927	31.808589
582.030428	30197.210215	31.813607
582.519183	30241.243127	31.818624
582.855787	30284.515993	31.823642
583.607267	30332.838209	31.828660
583.912582	30388.101145	31.833677
584.397688	30436.654707	31.838695
584.893016	30473.986598	31.843712
585.169558	30537.061139	31.848730
585.978437	30573.509993	31.853748
586.158817	30635.967680	31.858765
587.104325	30686.441362	31.863783
587.310502	30745.760000	31.868800
588.200851	30806.660097	31.873818
588.933374	30859.923462	31.878836
589.309572	30904.430450	31.883853
589.935933	30956.711816	31.888871
590.547904	31020.412002	31.893888
591.012874	31073.256106	31.898906
591.543248	31114.281729	31.903924
592.422800	31167.017283	31.908941
593.066798	31210.414915	31.913959
593.518600	31256.807329	31.918976
594.264014	31303.413320	31.923994
595.085586	31346.714058	31.929012
595.641137	31387.363335	31.934029
596.218433	31430.190232	31.939047
596.780750	31483.898922	31.944064
597.447864	31499.750619	31.949082
598.709517	31549.880084	31.954100
599.007939	31587.465894	31.959117
599.715547	31623.325496	31.964135
600.523867	31667.020907	31.969152
600.850045	31712.346582	31.974170
601.555678	31739.950669	31.979188
601.906525	31788.041540	31.984205
602.771342	31826.393031	31.989223
603.447404	31869.199140	31.994240
603.688147	31907.237024	31.999258
604.619492	31949.124845	32.004276
605.109729	31991.814735	32.009293
605.420762	32030.998774	32.014311
606.387808	32078.046134	32.019328
606.820234	32128.521026	32.024346
607.616281	32174.311912	32.029364
607.908607	32220.901995	32.034381
608.621063	32262.356712	32.039399
608.907181	32303.997994	32.044416
609.216193	32361.389739	32.049434
609.859761	32411.339347	32.054452
610.200268	32459.989700	32.059469
610.818920	32525.046339	32.064487
611.685019	32574.209394	32.069504
612.272217	32639.359791	32.074522
613.511673	32691.202382	32.079540
613.887069	32742.775008	32.084557
614.214341	32799.899596	32.089575
615.088547	32846.602796	32.094592
615.696169	32895.585578	32.099610
616.672055	32946.072678	32.104628
617.267304	32995.367398	32.109645
617.724428	33043.672214	32.114663
618.742246	33089.221961	32.119680
619.369728	33135.818811	32.124698
619.936944	33180.300935	32.129716
620.076132	33232.802951	32.134733
620.889215	33276.798139	32.139751
621.905823	33323.303220	32.144768
622.124047	33374.693243	32.149786
623.277296	33408.242197	32.154804
623.543811	33464.050411	32.159821
623.940550	33514.578465	32.164839
624.913635	33560.673587	32.169856
625.128923	33613.442886	32.174874
625.858360	33660.094575	32.179892
626.435675	33720.015096	32.184909
627.269225	33768.806697	32.189927
628.459264	33797.242185	32.194944
629.424155	33834.898994	32.199962
630.035357	33874.886947	32.204980
630.943189	33908.095573	32.209997
631.567015	33944.718243	32.215015
631.557592	33982.457446	32.220032
632.042372	34021.839451	32.225050
632.764901	34050.411285	32.230068
633.413872	34085.860657	32.235085
634.317699	34132.903526	32.240103
634.701288	34162.388115	32.245120
635.224099	34208.712817	32.250138
635.736814	34235.774908	32.255156
636.431621	34280.574591	32.260173
636.683046	34320.714236	32.265191
637.410962	34352.269816	32.270208
638.238066	34404.402132	32.275226
638.688647	34439.307644	32.280244
639.036965	34487.885623	32.285261
639.569017	34533.767031	32.290279
639.860994	34576.227516	32.295296
640.254018	34640.048705	32.300314
640.973913	34691.534560	32.305332
641.427101	34743.542571	32.310349
641.693162	34817.683460	32.315367
642.613143	34871.313563	32.320384
643.038519	34939.923127	32.325402
644.116981	34998.492113	32.330420
644.947129	35064.541643	32.335437
645.026878	35124.663749	32.340455
646.111474	35182.998354	32.345472
646.673589	35243.210096	32.350490
648.461074	35277.510550	32.355508
648.984096	35338.076395	32.360525
649.530130	35380.928893	32.365543
650.384032	35431.042629	32.370560
650.871784	35481.738270	32.375578
651.872417	35519.771899	32.380596
652.403318	35568.886665	32.385613
652.742508	35623.336209	32.390631
653.610669	35667.694548	32.395648
654.079987	35719.032231	32.400666
654.911873	35776.117958	32.405684
655.698395	35827.861769	32.410701
655.971968	35875.872869	32.415719
656.895902	35926.027458	32.420736
657.322406	35983.227432	32.425754
658.063515	36043.249188	32.430772
658.574962	36093.563229	32.435789
659.052578	36152.349080	32.440807
659.865718	36181.560961	32.445824
660.845605	36238.877812	32.450842
661.516855	36293.663085	32.455860
662.397304	36343.768524	32.460877
662.770839	36406.991061	32.465895
663.355690	36458.508559	32.470912
663.971995	36505.886009	32.475930
664.881297	36556.860040	32.480948
665.205894	36607.514214	32.485965
665.606160	36676.696058	32.490983
666.497972	36725.131327	32.496000
667.188693	36784.985974	32.501018
668.003455	36831.612417	32.506036
668.642938	36892.721003	32.511053
669.055793	36945.961063	32.516071
670.353502	37001.516911	32.521088
670.979416	37057.177483	32.526106
671.763371	37108.614973	32.531124
672.355306	37152.671635	32.536141
672.888301	37216.377607	32.541159
673.537354	37262.670364	32.546176
674.156274	37314.323738	32.551194
674.713172	37367.985057	32.556212
675.418038	37427.921507	32.561229
675.969118	37480.572282	32.566247
676.518134	37529.416848	32.571264
677.183937	37594.355295	32.576282
677.899015	37653.620510	32.581300
678.430167	37699.812421	32.586317
679.299496	37758.377309	32.591335
680.248520	37801.696791	32.596352
680.833630	37847.874299	32.601370
680.846988	37894.324291	32.606388
681.200758	37947.177661	32.611405
681.693063	38018.746114	32.616423
683.134884	38073.460262	32.621440
683.829889	38134.095809	32.626458
684.408719	38186.206496	32.631476
685.732978	38228.557838	32.636493
686.301090	38290.320203	32.641511
687.135874	38335.037087	32.646528
688.048921	38384.111493	32.651546
688.618718	38427.503921	32.656564
689.379391	38473.958979	32.661581
690.194055	38524.838610	32.666599
691.223640	38566.951929	32.671616
691.529952	38608.368491	32.676634
691.762912	38663.499980	32.681652
692.487951	38707.033222	32.686669
692.978562	38771.755877	32.691687
694.012868	38822.260539	32.696704
694.726930	38871.246881	32.701722
695.639123	38928.967230	32.706740
696.279976	38977.231653	32.711757
696.880714	39032.585080	32.716775
697.688288	39081.835591	32.721792
698.006030	39133.021671	32.726810
698.541869	39198.699788	32.731828
699.588312	39258.670381	32.736845
700.244754	39321.263024	32.741863
700.668526	39357.964097	32.746880
701.460183	39424.709759	32.751898
702.312162	39480.651290	32.756916
703.530132	39513.592738	32.761933
704.291807	39583.050201	32.766951
704.937265	39625.813515	32.771968
705.677889	39676.890785	32.776986
706.282405	39732.043047	32.782004
707.187024	39782.070548	32.787021
707.538743	39842.992003	32.792039
708.411011	39893.378943	32.797056
709.016015	39948.000459	32.802074
709.740062	40002.875516	32.807092
710.619371	40054.646709	32.812109
710.708405	40111.505473	32.817127
711.799981	40175.095297	32.822144
712.258026	40226.540381	32.827162
713.011396	40278.572030	32.832180
713.940590	40342.801067	32.837197
714.358196	40395.758001	32.842215
715.299959	40450.739431	32.847232
715.958721	40517.597684	32.852250
716.630446	40572.482326	32.857268
716.947066	40630.698351	32.862285
717.771227	40691.788963	32.867303
718.315106	40759.310917	32.872320
719.393392	40825.972000	32.877338
720.092442	40887.588582	32.882356
720.597199	40931.894211	32.887373
721.169070	41007.596286	32.892391
721.611198	41074.616458	32.897408
723.075594	41138.644365	32.902426
723.686595	41194.457065	32.907444
724.502056	41248.119392	32.912461
724.890272	41315.711570	32.917479
725.643458	41374.222114	32.922496
726.614319	41417.463228	32.927514
727.476381	41479.644283	32.932532
728.360930	41523.031857	32.937549
728.703736	41577.622381	32.942567
729.322095	41624.764098	32.947584
730.066768	41690.037755	32.952602
730.282454	41750.429153	32.957620
731.408197	41807.491452	32.962637
731.883511	41864.832239	32.967655
732.624684	41931.979249	32.972672
733.385657	41986.992694	32.977690
733.816847	42051.063944	32.982708
734.819151	42111.744989	32.987725
735.121646	42193.343435	32.992743
735.963243	42252.765971	32.997760
737.406274	42315.548355	33.002778
738.158567	42373.802392	33.007796
738.722051	42435.495032	33.012813
739.315637	42513.798415	33.017831
739.829069	42578.193614	33.022848
740.900025	42638.523887	33.027866
741.899259	42704.134098	33.032884
742.408185	42757.816214	33.037901
743.134738	42833.690259	33.042919
743.468604	42889.910932	33.047936
744.692274	42957.257935	33.052954
745.821802	43021.084152	33.057972
746.615177	43081.351325	33.062989
747.528227	43149.455666	33.068007
748.144254	43209.542072	33.073024
749.031542	43263.527045	33.078042
749.639257	43338.959600	33.083060
750.457313	43396.674800	33.088077
751.232912	43457.774351	33.093095
751.904061	43521.793547	33.098112
752.562822	43585.701005	33.103130
753.206172	43653.829908	33.108148
753.879834	43714.553878	33.113165
754.883495	43791.191367	33.118183
755.577091	43849.825299	33.123200
756.675677	43898.421498	33.128218
757.422964	43968.989368	33.133236
757.857312	44026.860821	33.138253
758.421971	44089.329575	33.143271
759.266118	44162.748325	33.148288
760.101080	44223.214543	33.153306
760.869445	44288.991903	33.158324
761.100554	44356.383822	33.163341
762.259552	44445.586803	33.168359
763.075146	44510.054442	33.173376
763.932002	44561.529817	33.178394
764.537292	44641.913634	33.183412
765.362887	44698.416569	33.188429
766.691532	44760.388756	33.193447
767.443128	44835.297962	33.198464
768.160796	44893.519744	33.203482
768.468188	44957.719888	33.208500
769.455328	45017.772396	33.213517
770.201821	45087.888502	33.218535
770.788860	45146.447556	33.223552
771.294898	45211.648572	33.228570
772.239091	45285.093402	33.233588
773.274630	45351.395287	33.238605
773.622900	45416.260899	33.243623
774.322787	45490.351694	33.248640
775.604949	45552.282713	33.253658
775.907247	45629.699906	33.258676
776.958653	45684.911376	33.263693
778.019285	45747.003933	33.268711
778.800332	45803.877168	33.273728
779.709305	45852.127607	33.278746
780.288455	45921.804271	33.283764
780.543522	45973.952227	33.288781
782.166700	46017.923151	33.293799
782.739037	46078.492211	33.298816
783.305061	46133.666481	33.303834
784.329383	46196.771745	33.308852
785.007685	46254.883007	33.313869
786.096531	46308.711148	33.318887
786.413444	46371.958653	33.323904
787.261765	46430.847294	33.328922
788.183568	46493.868137	33.333940
788.714569	46554.735908	33.338957
789.662044	46619.220727	33.343975
789.658241	46681.791541	33.348992
790.947137	46750.208959	33.354010
791.472321	46830.454947	33.359028
792.640759	46899.872106	33.364045
793.420877	46964.308052	33.369063
794.086144	47037.397168	33.374080
794.833900	47091.881257	33.379098
795.663622	47169.588560	33.384116
796.143383	47243.700421	33.389133
797.068329	47314.257509	33.394151
797.735250	47399.088900	33.399168
799.228954	47459.777622	33.404186
799.775507	47541.117239	33.409204
800.622514	47600.610131	33.414221
801.657861	47663.749419	33.419239
802.720219	47734.261121	33.424256
803.421469	47800.698181	33.429274
804.638810	47861.317128	33.434292
805.890320	47914.567067	33.439309
806.795599	47972.615789	33.444327
807.279962	48032.862166	33.449344
808.100558	48084.718193	33.454362
808.917689	48148.664620	33.459380
809.622758	48198.925661	33.464397
810.266276	48268.409755	33.469415
810.845388	48328.914204	33.474432
811.555724	48390.119604	33.479450
812.448582	48466.625825	33.484468
813.085770	48528.614816	33.489485
814.184108	48582.244451	33.494503
814.617591	48663.156506	33.499520
815.592040	48728.048033	33.504538
816.204941	48801.283842	33.509556
816.991284	48871.500406	33.514573
818.367739	48933.887876	33.519591
818.923150	49004.925299	33.524608
820.051515	49073.697386	33.529626
820.652126	49132.049559	33.534644
821.326151	49198.982093	33.539661
822.492821	49260.719832	33.544679
823.447594	49329.842374	33.549696
824.267071	49393.095990	33.554714
825.317589	49462.646902	33.559732
825.518359	49529.502231	33.564749
826.307163	49592.729539	33.569767
826.681626	49659.513921	33.574784
827.896128	49732.981734	33.579802
828.424462	49807.575219	33.584820
829.325700	49879.934453	33.589837
830.139929	49952.876880	33.594855
830.445031	50029.176135	33.599872
831.312296	50099.523063	33.604890
831.875384	50178.041368	33.609908
832.693638	50249.826278	33.614925
833.949833	50320.701750	33.619943
834.320478	50381.845145	33.624960
835.479242	50456.121154	33.629978
836.864628	50523.244190	33.634996
837.724071	50587.399645	33.640013
838.910518	50647.568928	33.645031
838.986529	50721.830855	33.650048
840.023548	50784.200280	33.655066
841.229953	50847.416653	33.660084
842.133671	50914.084328	33.665101
842.878622	50982.725681	33.670119
843.337752	51050.266508	33.675136
844.459865	51116.381941	33.680154
845.421547	51190.374635	33.685172
845.572268	51264.209077	33.690189
846.796716	51328.765338	33.695207
847.281875	51418.119635	33.700224
848.359783	51493.259428	33.705242
849.216155	51573.540113	33.710260
849.991123	51647.038162	33.715277
850.926807	51724.997540	33.720295
851.420255	51798.653785	33.725312
852.470448	51876.032707	33.730330
853.550248	51952.173427	33.735348
854.479527	52033.102408	33.740365
855.386653	52108.112592	33.745383
856.228769	52187.771200	33.750400
857.172777	52264.604798	33.755418
858.282135	52340.508071	33.760436
858.596449	52419.952239	33.765453
859.592771	52487.932490	33.770471
860.451040	52571.823055	33.775488
861.170198	52649.262408	33.780506
862.368014	52732.936180	33.785524
863.048660	52822.145215	33.790541
863.914997	52887.356358	33.795559
864.973736	52968.394991	33.800576
865.443840	53066.059926	33.805594
866.291904	53138.209824	33.810612
867.081517	53218.633130	33.815629
868.524402	53307.775988	33.820647
869.110380	53378.107046	33.825664
870.403277	53463.666984	33.830682
871.407537	53540.375173	33.835700
872.047196	53625.746306	33.840717
872.902629	53690.948731	33.845735
873.739454	53784.357840	33.850752
875.017721	53845.565226	33.855770
876.142017	53920.579066	33.860788
876.642673	54001.860020	33.865805
877.637034	54069.661663	33.870823
878.503019	54146.450310	33.875840
879.493920	54226.345823	33.880858
880.488605	54291.382694	33.885876
881.174893	54366.010516	33.890893
882.309509	54445.365498	33.895911
883.091476	54515.023984	33.900928
884.027533	54582.266647	33.905946
884.821122	54648.019247	33.910964
885.280052	54727.771455	33.915981
886.419576	54796.932142	33.920999
887.357237	54877.319094	33.926016
887.953286	54962.417090	33.931034
889.048664	55029.288173	33.936052
889.577316	55115.631225	33.941069
890.620289	55183.403192	33.946087
891.366077	55253.341604	33.951104
892.092938	55330.219043	33.956122
893.008778	55400.625031	33.961140
893.459174	55482.456816	33.966157
894.755133	55542.906452	33.971175
895.680087	55619.589455	33.976192
896.854146	55686.804541	33.981210
897.975424	55763.394164	33.986228
898.699554	55833.761668	33.991245
899.182965	55900.698829	33.996263
900.074547	55980.179063	34.001280
901.081031	56061.350384	34.006298
901.855651	56139.849447	34.011316
902.928619	56207.037441	34.016333
903.673231	56282.864655	34.021351
904.439737	56366.017252	34.026368
905.475260	56449.716828	34.031386
906.493515	56518.572325	34.036404
907.957660	56595.440347	34.041421
909.065546	56675.325910	34.046439
910.107838	56757.133227	34.051456
910.864940	56817.916807	34.056474
911.544472	56888.674093	34.061492
912.255047	56969.508512	34.066509
912.774417	57041.911352	34.071527
913.958666	57124.609178	34.076544
915.277178	57208.526844	34.081562
916.212264	57274.600115	34.086580
916.972875	57365.351750	34.091597
918.358656	57434.177990	34.096615
918.942360	57511.097404	34.101632
920.034985	57588.994780	34.106650
921.156580	57661.362707	34.111668
921.799809	57744.672193	34.116685
923.049266	57806.596808	34.121703
923.776417	57892.596229	34.126720
924.284276	57981.642723	34.131738
925.497577	58047.617853	34.136756
926.979055	58123.190624	34.141773
928.062139	58191.053499	34.146791
929.103373	58258.011686	34.151808
930.100110	58321.192157	34.156826
931.108909	58391.187423	34.161844
931.579808	58470.437606	34.166861
932.156991	58542.443556	34.171879
933.279233	58614.092719	34.176896
934.116936	58693.843509	34.181914
934.991295	58766.012731	34.186932
936.033411	58853.618488	34.191949
936.552004	58925.565076	34.196967
937.673149	59016.216173	34.201984
938.324309	59095.377049	34.207002
939.147548	59178.328007	34.212020
940.086982	59266.444931	34.217037
940.843161	59346.071312	34.222055
941.478783	59426.691452	34.227072
942.481822	59524.654341	34.232090
943.619717	59607.652727	34.237108
944.616963	59713.358232	34.242125
945.012329	59799.409747	34.247143
946.573881	59891.698202	34.252160
947.099710	59988.325749	34.257178
948.094750	60071.417580	34.262196
949.240521	60164.506023	34.267213
950.327944	60257.458323	34.272231
951.360656	60344.716459	34.277248
952.343146	60424.602304	34.282266
953.581858	60511.860620	34.287284
954.313799	60590.671978	34.292301
954.797626	60672.971929	34.297319
956.290291	60744.677321	34.302336
957.003086	60827.005446	34.307354
957.817062	60906.311435	34.312372
958.708819	60988.586926	34.317389
959.778736	61073.702387	34.322407
960.938017	61160.108188	34.327424
961.380112	61246.860137	34.332442
962.718985	61332.827147	34.337460
963.398478	61422.524158	34.342477
964.212404	61506.712485	34.347495
964.854588	61596.283007	34.352512
965.820651	61696.279618	34.357530
966.747106	61780.983088	34.362548
968.019427	61863.942886	34.367565
968.856552	61964.929157	34.372583
970.429518	62051.545889	34.377600
970.980336	62159.774860	34.382618
972.055403	62240.316865	34.387636
973.196996	62344.637600	34.392653
974.214315	62436.729164	34.397671
975.055488	62530.108206	34.402688
975.891929	62626.083742	34.407706
977.156204	62724.829018	34.412724
978.209812	62810.123931	34.417741
979.424865	62913.251861	34.422759
980.261274	62999.448489	34.427776
981.190633	63098.684181	34.432794
982.223068	63178.248335	34.437812
983.448517	63274.817858	34.442829
984.084866	63366.744281	34.447847
985.298161	63453.269974	34.452864
986.136443	63555.541300	34.457882
987.228016	63639.339153	34.462900
988.425873	63738.307704	34.467917
989.236234	63841.021353	34.472935
990.780240	63923.597574	34.477952
991.638354	64015.903359	34.482970
992.665952	64097.952802	34.487988
993.522366	64188.518566	34.493005
994.617964	64278.104155	34.498023
995.673610	64368.114111	34.503040
996.187511	64463.539185	34.508058
997.665758	64550.128730	34.513076
998.374758	64654.551806	34.518093
999.151738	64746.341128	34.523111
1000.338188	64842.068124	34.528128
1001.266242	64948.414546	34.533146
1002.331701	65028.758147	34.538164
1003.435894	65128.329211	34.543181
1004.148237	65232.127407	34.548199
1005.602135	65326.719370	34.553216
1006.414987	65425.893795	34.558234
1007.300145	65520.980199	34.563252
1008.624744	65608.654584	34.568269
1009.451960	65703.193565	34.573287
1010.617588	65797.294027	34.578304
1011.313564	65904.661923	34.583322
1012.407065	65987.479669	34.588340
1013.669731	66086.073849	34.593357
1014.682743	66180.351440	34.598375
1015.750498	66279.464212	34.603392
1015.927476	66384.914277	34.608410
1017.415374	66477.010761	34.613428
1018.667924	66571.410801	34.618445
1019.248926	66673.722187	34.623463
1020.673932	66762.733504	34.628480
1021.847947	66851.803196	34.633498
1022.366936	66928.179520	34.638516
1023.708380	67005.586690	34.643533
1024.386949	67100.597212	34.648551
1025.573381	67191.097052	34.653568
1026.364284	67274.181365	34.658586
1027.718709	67369.087685	34.663604
1028.269948	67457.066122	34.668621
1029.626243	67554.277495	34.673639
1030.347636	67642.761930	34.678656
1031.443866	67743.123278	34.683674
1032.494772	67839.167615	34.688692
1033.392806	67938.838783	34.693709
1034.429736	68047.384637	34.698727
1035.684437	68133.843949	34.703744
1036.365321	68229.903026	34.708762
1037.489365	68331.870593	34.713780
1038.690200	68429.831301	34.718797
1039.817404	68528.943557	34.723815
1040.910863	68619.488246	34.728832
1042.103464	68736.972222	34.733850
1043.065704	68829.956820	34.738868
1044.178134	68935.031172	34.743885
1045.088190	69033.121752	34.748903
1046.617307	69126.196472	34.753920
1047.285621	69228.137216	34.758938
1048.074274	69327.944766	34.763956
1049.123083	69432.670126	34.768973
1049.756340	69541.133144	34.773991
1051.338861	69640.514392	34.779008
1052.665782	69749.959416	34.784026
1053.573925	69863.997513	34.789044
1054.338356	69970.611943	34.794061
1055.646911	70075.141167	34.799079
1056.973983	70176.609506	34.804096
1057.733979	70284.815283	34.809114
1059.212643	70389.167319	34.814132
1060.601037	70480.229846	34.819149
1061.442624	70589.481668	34.824167
1062.263200	70686.604602	34.829184
1063.550256	70793.407008	34.834202
1064.302270	70890.554038	34.839220
1065.749461	70992.190496	34.844237
1066.308403	71098.955511	34.849255
1068.130854	71197.608805	34.854272
1069.831055	71291.481536	34.859290
1070.987710	71391.391696	34.864308
1072.122440	71464.240745	34.869325
1072.891691	71567.390768	34.874343
1074.012010	71649.741291	34.879360
1075.244786	71744.904244	34.884378
1076.297234	71846.960087	34.889396
1077.509094	71919.507099	34.894413
1078.135418	72021.401975	34.899431
1078.879700	72113.070723	34.904448
1080.101705	72205.336686	34.909466
1081.068577	72300.631698	34.914484
1082.552754	72401.634597	34.919501
1083.149323	72512.351088	34.924519
1084.598554	72591.284365	34.929536
1085.462377	72691.966978	34.934554
1086.552197	72793.336733	34.939572
1087.867260	72879.283132	34.944589
1088.905884	72985.917810	34.949607
1090.172450	73079.471788	34.954624
1091.212927	73170.819457	34.959642
1091.852421	73267.106175	34.964660
1093.229708	73362.379128	34.969677
1094.139649	73456.889222	34.974695
1095.320268	73536.259772	34.979712
1096.341919	73618.885115	34.984730
1096.726587	73707.246224	34.989748
1098.030876	73795.109833	34.994765
1099.022582	73895.093142	34.999783
1100.027245	73992.389595	35.004800
1100.912262	74093.821527	35.009818
1101.864178	74197.320690	35.014836
1102.946619	74298.165356	35.019853
1104.188923	74406.471304	35.024871
1105.235956	74506.790284	35.029888
1106.393471	74614.020965	35.034906
1107.228534	74722.556245	35.039924
1108.369317	74830.601051	35.044941
1109.306187	74945.783972	35.049959
1110.337326	75046.132779	35.054976
1111.568897	75169.985416	35.059994
1112.728860	75284.007729	35.065012
1114.319066	75384.992783	35.070029
1115.205703	75504.391284	35.075047
1116.894430	75611.745934	35.080064
1118.114014	75715.373960	35.085082
1119.207365	75817.375327	35.090100
1120.591063	75923.017988	35.095117
1121.448470	76028.274302	35.100135
1122.659545	76141.240919	35.105152
1123.920839	76236.770165	35.110170
1124.604698	76347.324275	35.115188
1126.389218	76444.280210	35.120205
1127.269670	76563.697022	35.125223
1128.297063	76655.831312	35.130240
1129.933098	76781.515823	35.135258
1130.591723	76875.507033	35.140276
1131.802182	76992.404207	35.145293
1132.978633	77108.965153	35.150311
1134.204588	77211.242481	35.155328
1135.514768	77320.955673	35.160346
1136.252844	77434.102636	35.165364
1137.328910	77542.079677	35.170381
1138.541356	77648.642456	35.175399
1139.894195	77759.959587	35.180416
1141.943475	77857.031365	35.185434
1142.993725	77957.793355	35.190452
1144.356717	78042.418665	35.195469
1145.593097	78146.357383	35.200487
1146.733868	78248.449166	35.205504
1147.099229	78339.526725	35.210522
1148.516752	78441.576149	35.215540
1149.665311	78538.448505	35.220557
1150.767815	78644.449533	35.225575
1151.610094	78753.151824	35.230592
1152.815798	78862.203364	35.235610
1153.856244	78968.937399	35.240628
1154.832440	79071.729282	35.245645
1156.264521	79192.946641	35.250663
1157.205313	79293.033792	35.255680
1158.179500	79414.931490	35.260698
1159.340504	79533.050714	35.265716
1160.622389	79633.478735	35.270733
1161.258289	79749.058186	35.275751
1162.837628	79863.997184	35.280768
1164.127076	79964.830631	35.285786
1165.517098	80075.695256	35.290804
1166.813798	80178.403353	35.295821
1168.065873	80286.085037	35.300839
1169.377386	80394.898103	35.305856
1170.543379	80488.125880	35.310874
1171.475909	80583.379367	35.315892
1172.484043	80678.393367	35.320909
1173.608816	80777.545049	35.325927
1174.524888	80875.640010	35.330944
1175.661237	80973.168915	35.335962
1176.746545	81082.475970	35.340980
1177.914414	81187.095577	35.345997
1178.706986	81291.812000	35.351015
1179.641248	81400.028890	35.356032
1181.075198	81511.867939	35.361050
1182.017306	81632.374007	35.366068
1183.459295	81743.655264	35.371085
1184.177519	81857.760944	35.376103
1185.435635	81965.638200	35.381120
1186.979071	82083.974758	35.386138
1188.332473	82213.364207	35.391156
1189.395807	82314.292001	35.396173
1190.569676	82434.600718	35.401191
1191.660171	82555.645118	35.406208
1193.000569	82660.357381	35.411226
1194.272946	82782.413389	35.416244
1195.559513	82890.733208	35.421261
1197.219814	83009.068123	35.426279
1198.397467	83125.350046	35.431296
1199.581303	83230.139466	35.436314
1201.149049	83341.382105	35.441332
1202.326549	83456.727798	35.446349
1203.658224	83566.563631	35.451367
1204.866815	83664.065257	35.456384
1206.145650	83775.519281	35.461402
1207.015147	83888.798675	35.466420
1208.265501	84003.045564	35.471437
1209.759069	84108.790993	35.476455
1210.301770	84233.462942	35.481472
1212.105302	84337.463083	35.486490
1212.858298	84460.113962	35.491508
1214.372078	84572.826958	35.496525
1215.808434	84691.571175	35.501543
1216.950050	84808.321721	35.506560
1218.510332	84913.274131	35.511578
1219.647501	85026.047528	35.516596
1220.876402	85137.768050	35.521613
1222.005294	85255.079922	35.526631
1223.122683	85363.574837	35.531648
1224.696705	85470.833319	35.536666
1225.688049	85583.656939	35.541684
1227.212707	85693.318826	35.546701
1228.836159	85806.323699	35.551719
1230.293125	85888.373019	35.556736
1231.889119	85990.954219	35.561754
1232.965324	86092.881736	35.566772
1233.923865	86191.381233	35.571789
1235.124369	86299.423214	35.576807
1236.325674	86395.554023	35.581824
1237.769217	86489.505913	35.586842
1238.847992	86592.816010	35.591860
1240.260182	86695.301593	35.596877
1241.528055	86796.897622	35.601895
1242.617721	86909.444984	35.606912
1243.939542	87006.864268	35.611930
1244.761515	87111.863540	35.616948
1245.718103	87218.261513	35.621965
1247.362369	87316.201885	35.626983
1248.644336	87417.671160	35.632000
1249.869179	87527.994903	35.637018
1250.598775	87648.711393	35.642036
1251.727284	87749.939586	35.647053
1252.621174	87865.207634	35.652071
1253.774349	87973.491280	35.657088
1255.055471	88068.563359	35.662106
1256.098527	88181.553729	35.667124
1256.995964	88284.175689	35.672141
1257.939724	88400.008334	35.677159
1259.344468	88520.255807	35.682176
1260.462614	88638.013834	35.687194
1261.419390	88760.980612	35.692212
1262.785806	88879.626071	35.697229
1264.074241	89010.107938	35.702247
1265.312139	89145.299905	35.707264
1266.441131	89268.546135	35.712282
1267.617636	89400.910073	35.717300
1268.894197	89535.844340	35.722317
1270.268237	89661.297197	35.727335
1271.217333	89797.145393	35.732352
1272.835502	89933.954622	35.737370
1273.553837	90068.775419	35.742388
1275.118952	90208.889232	35.747405
1276.606313	90351.778616	35.752423
1277.749954	90483.734252	35.757440
1279.371277	90622.954111	35.762458
1280.902403	90755.839171	35.767476
1282.298212	90890.862387	35.772493
1283.462338	91017.202743	35.777511
1284.723619	91163.122183	35.782528
1285.915916	91292.969952	35.787546
1287.518114	91431.423429	35.792564
1289.166686	91567.525641	35.797581
1290.797960	91698.662945	35.802599
1291.647677	91826.487794	35.807616
1293.069314	91947.456183	35.812634
1294.771691	92079.762766	35.817652
1296.130152	92212.224851	35.822669
1297.439615	92345.442924	35.827687
1299.151112	92469.055226	35.832704
1300.318027	92593.475237	35.837722
1301.471866	92716.516277	35.842740
1302.762208	92848.459411	35.847757
1304.463367	92970.034765	35.852775
1305.611463	93087.400000	35.857792
1307.293296	93201.197084	35.862810
1308.606941	93318.892331	35.867828
1310.057562	93446.706504	35.872845
1311.619556	93559.674367	35.877863
1312.674785	93680.377128	35.882880
1314.171264	93789.705683	35.887898
1315.249713	93908.757992	35.892916
1316.695946	94027.373267	35.897933
1318.352881	94148.985538	35.902951
1319.322184	94272.898108	35.907968
1320.574938	94384.282052	35.912986
1321.744716	94501.522570	35.918004
1323.001898	94622.590522	35.923021
1324.215839	94737.619573	35.928039
1325.911616	94861.307352	35.933056
1327.023889	94982.145761	35.938074
1328.443703	95105.573260	35.943092
1329.513459	95233.999173	35.948109
1330.753637	95348.291230	35.953127
1332.317112	95466.817729	35.958144
1333.797886	95586.346251	35.963162
1335.214529	95708.040078	35.968180
1336.558932	95820.568405	35.973197
1337.966809	95941.757481	35.978215
1338.901778	96068.686725	35.983232
1339.901402	96192.437453	35.988250
1341.427959	96303.595527	35.993268
1342.642492	96427.579929	35.998285
1344.155349	96534.760706	36.003303
1345.642137	96637.712106	36.008320
1346.721540	96750.487843	36.013338
1348.015360	96857.158742	36.018356
1349.114484	96970.553330	36.023373
1350.567686	97084.793226	36.028391
1351.663342	97209.889375	36.033408
1352.756446	97325.466497	36.038426
1354.015083	97450.500203	36.043444
1355.337020	97587.136157	36.048461
1356.881944	97712.177044	36.053479
1358.130008	97839.470347	36.058496
1359.518868	97968.453585	36.063514
1361.120990	98096.263257	36.068532
1362.065477	98230.222581	36.073549
1363.646549	98357.985876	36.078567
1364.985351	98492.455383	36.083584
1366.650983	98614.311840	36.088602
1368.504180	98739.917281	36.093620
1369.420651	98879.182634	36.098637
1370.760558	99001.623701	36.103655
1372.139946	99144.570547	36.108672
1373.736059	99268.684159	36.113690
1374.802811	99415.268493	36.118708
1375.878482	99564.260778	36.123725
1377.688034	99689.940128	36.128743
1378.961864	99829.699110	36.133760
1380.709114	99975.850471	36.138778
1381.842068	100099.037869	36.143796
1382.828701	100247.083687	36.148813
1384.526713	100388.021459	36.153831
1385.966461	100534.882446	36.158848
1387.217108	100662.566896	36.163866
1388.798727	100805.591058	36.168884
1390.288873	100955.919799	36.173901
1391.661822	101089.646863	36.178919
1392.867984	101239.640782	36.183936
1394.428884	101372.959421	36.188954
1395.451976	101519.268491	36.193972
1397.091901	101665.520243	36.198989
1398.474613	101810.823793	36.204007
1399.857618	101958.574825	36.209024
1401.558426	102101.979147	36.214042
1402.944560	102244.380780	36.219060
1404.657865	102385.236066	36.224077
1406.274520	102520.059420	36.229095
1407.292744	102651.261695	36.234112
1408.608419	102786.969764	36.239130
1410.399391	102928.905638	36.244148
1411.718170	103079.118656	36.249165
1413.392718	103211.526898	36.254183
1415.083710	103352.846223	36.259200
1416.253672	103495.020651	36.264218
1418.067140	103614.933008	36.269236
1419.513008	103754.808783	36.274253
1421.334581	103887.425060	36.279271
1422.567025	104023.569554	36.284288
1424.047384	104146.210933	36.289306
1425.687674	104265.962409	36.294324
1427.019779	104398.352608	36.299341
1428.282108	104524.756964	36.304359
1429.517242	104663.794493	36.309376
1430.943042	104793.597799	36.314394
1432.408568	104904.262398	36.319412
1433.505590	105034.916606	36.324429
1435.190893	105177.208178	36.329447
1436.529918	105308.814776	36.334464
1437.619151	105431.407623	36.339482
1438.745918	105543.116050	36.344500
1439.899805	105683.286239	36.349517
1441.397327	105797.714627	36.354535
1442.527695	105933.705244	36.359552
1443.828671	106067.007114	36.364570
1445.159866	106194.586234	36.369588
1446.170550	106340.436604	36.374605
1447.742751	106489.940762	36.379623
1449.131949	106631.206753	36.384640
1450.050871	106779.736071	36.389658
1451.737626	106930.188010	36.394676
1453.213122	107080.242372	36.399693
1454.699853	107232.831672	36.404711
1456.501247	107390.115071	36.409728
1457.924292	107541.346197	36.414746
1459.620477	107683.849464	36.419764
1461.048199	107838.695060	36.424781
1463.001185	107991.405370	36.429799
1464.429503	108145.542150	36.434816
1465.785618	108295.937418	36.439834
1467.316548	108436.136302	36.444852
1468.931991	108588.242401	36.449869
1471.045133	108741.273479	36.454887
1472.417279	108873.915794	36.459904
1473.640342	109032.945200	36.464922
1475.375673	109168.512102	36.469940
1476.653720	109323.146703	36.474957
1478.335382	109470.909491	36.479975
1479.850008	109629.274873	36.484992
1480.723742	109768.554260	36.490010
1482.385764	109911.731423	36.495028
1483.671585	110070.730428	36.500045
1485.295831	110225.758978	36.505063
1486.791726	110388.962262	36.510080
1488.009151	110554.289386	36.515098
1489.755490	110702.567237	36.520116
1490.935723	110858.745603	36.525133
1492.465860	111024.634971	36.530151
1494.294551	111189.223171	36.535168
1495.550732	111346.926343	36.540186
1496.931492	111510.520496	36.545204
1498.380654	111678.200963	36.550221
1500.021065	111837.342957	36.555239
1501.497728	111994.875186	36.560256
1502.530380	112169.788050	36.565274
1504.408548	112335.997145	36.570292
1506.429971	112507.397037	36.575309
1508.057900	112665.365232	36.580327
1509.732214	112828.387085	36.585344
1510.792646	112984.885107	36.590362
1512.853483	113143.942109	36.595380
1514.444636	113310.086246	36.600397
1515.822406	113464.000490	36.605415
1517.431765	113624.803957	36.610432
1518.444310	113784.534239	36.615450
1520.326701	113938.739753	36.620468
1521.947075	114093.532057	36.625485
1523.266006	114263.984296	36.630503
1525.201842	114419.540578	36.635520
1526.504711	114580.370614	36.640538
1528.499820	114723.870334	36.645556
1529.989532	114869.541955	36.650573
1531.473703	115034.505755	36.655591
1533.278371	115175.081764	36.660608
1534.844902	115328.340359	36.665626
1536.718179	115473.523457	36.670644
1537.687573	115610.755973	36.675661
1539.502120	115754.960039	36.680679
1541.114505	115894.604804	36.685696
1541.902636	116029.444593	36.690714
1543.590699	116158.247060	36.695732
1544.820963	116298.219174	36.700749
1546.142850	116442.832370	36.705767
1547.785480	116589.755332	36.710784
1548.980789	116741.948739	36.715802
1550.452301	116886.426220	36.720820
1551.845365	117050.791703	36.725837
1553.216625	117198.888147	36.730855
1554.789368	117360.309781	36.735872
1555.911888	117533.636156	36.740890
1557.485544	117702.326932	36.745908
1558.905260	117879.426483	36.750925
1559.952867	118050.940421	36.755943
1561.726143	118212.613553	36.760960
1563.021753	118402.266686	36.765978
1564.722737	118574.556510	36.770996
1566.369673	118764.905142	36.776013
1568.040704	118951.052488	36.781031
1569.890734	119122.700074	36.786048
1571.715001	119308.850690	36.791066
1573.157810	119489.112582	36.796084
1575.128972	119672.007573	36.801101
1576.200943	119848.422050	36.806119
1578.277184	120022.486593	36.811136
1580.135847	120205.515802	36.816154
1581.955038	120372.277510	36.821172
1583.401222	120551.123176	36.826189
1585.385941	120726.942967	36.831207
1587.951261	120886.322352	36.836224
1589.125296	121058.743426	36.841242
1590.728257	121224.553041	36.846260
1592.214188	121381.793789	36.851277
1594.067721	121553.806861	36.856295
1595.822170	121706.795671	36.861312
1597.567998	121887.833451	36.866330
1598.656303	122049.946483	36.871348
1600.389650	122213.761107	36.876365
1601.580836	122395.141265	36.881383
1603.325962	122556.139328	36.886400
1604.490142	122738.984100	36.891418
1606.081188	122918.972458	36.896436
1607.596239	123102.271725	36.901453
1609.088116	123293.580111	36.906471
1611.108608	123464.345052	36.911488
1612.455229	123644.920239	36.916506
1613.982917	123818.998281	36.921524
1615.796753	124011.350996	36.926541
1617.370884	124189.584406	36.931559
1619.201006	124365.381109	36.936576
1620.769532	124555.744860	36.941594
1622.096808	124739.372663	36.946612
1623.725165	124918.323983	36.951629
1625.277623	125115.035979	36.956647
1627.035659	125292.903133	36.961664
1628.520467	125484.007419	36.966682
1630.062218	125681.091741	36.971700
1631.364414	125860.694257	36.976717
1632.983957	126053.556363	36.981735
1634.643269	126239.765410	36.986752
1635.816209	126438.255579	36.991770
1637.612551	126647.915502	36.996788
1639.319923	126837.672076	37.001805
1640.580887	127045.552399	37.006823
1642.475610	127247.372280	37.011840
1643.727309	127445.372953	37.016858
1645.172709	127634.082888	37.021876
1646.833296	127833.049427	37.026893
1648.470726	128018.432579	37.031911
1650.043341	128211.032982	37.036928
1651.483847	128409.199176	37.041946
1652.860759	128606.526157	37.046964
1655.058055	128806.187738	37.051981
1656.541165	129002.434315	37.056999
1658.632663	129191.735863	37.062016
1660.053437	129388.539508	37.067034
1661.599394	129584.639455	37.072052
1663.600882	129781.176921	37.077069
1665.397798	129985.486666	37.082087
1666.653986	130180.860522	37.087104
1668.122222	130398.418729	37.092122
1670.267069	130611.064011	37.097140
1671.978091	130810.506230	37.102157
1673.115433	131013.845082	37.107175
1674.956121	131232.554929	37.112192
1676.399666	131443.575222	37.117210
1678.408370	131654.457834	37.122228
1679.913604	131877.118454	37.127245
1681.485785	132103.893520	37.132263
1683.335606	132314.423425	37.137280
1684.758741	132535.349195	37.142298
1686.683850	132756.642058	37.147316
1688.164987	132979.337446	37.152333
1689.676120	133205.023830	37.157351
1691.701423	133433.448252	37.162368
1693.706135	133665.582202	37.167386
1694.979826	133887.147102	37.172404
1696.973462	134114.767891	37.177421
1698.727070	134348.987429	37.182439
1700.829519	134564.335995	37.187456
1702.085814	134799.231690	37.192474
1703.517413	135038.022303	37.197492
1705.580604	135252.644321	37.202509
1707.005431	135494.255436	37.207527
1709.142846	135720.935707	37.212544
1711.167562	135951.390741	37.217562
1712.911351	136178.350291	37.222580
1715.144480	136409.105144	37.227597
1716.780953	136634.700510	37.232615
1718.280980	136859.785259	37.237632
1719.992861	137076.513641	37.242650
1721.516526	137311.736073	37.247668
1723.683802	137532.507244	37.252685
1725.266005	137771.910589	37.257703
1727.121425	137988.938178	37.262720
1728.835421	138209.795824	37.267738
1730.511271	138433.223870	37.272756
1732.433651	138653.162879	37.277773
1734.053170	138884.507863	37.282791
1736.015034	139113.541827	37.287808
1737.685902	139345.769419	37.292826
1739.178983	139573.876045	37.297844
1741.083218	139798.797913	37.302861
1742.744592	140018.187480	37.307879
1744.491576	140244.963385	37.312896
1746.267313	140473.791792	37.317914
1747.913011	140701.765873	37.322932
1750.200868	140912.762297	37.327949
1751.859656	141144.391407	37.332967
1753.936716	141357.364300	37.337984
1755.326359	141579.087694	37.343002
1756.861490	141794.989649	37.348020
1759.248770	142017.003968	37.353037
1760.548485	142233.172953	37.358055
1762.271299	142436.585822	37.363072
1764.040263	142642.632142	37.368090
1765.169620	142858.360832	37.373108
1766.662636	143062.890834	37.378125
1769.373357	143268.970893	37.383143
1771.250519	143462.375833	37.388160
1772.998021	143669.673565	37.393178
1773.994866	143883.498250	37.398196
1775.740997	144090.569506	37.403213
1777.707217	144312.634346	37.408231
1779.313990	144533.601167	37.413248
1780.910765	144754.748206	37.418266
1782.428767	144979.449511	37.423284
1784.149802	145206.239771	37.428301
1785.602747	145452.821514	37.433319
1787.166166	145685.565616	37.438336
1788.507689	145924.221767	37.443354
1789.976524	146171.020288	37.448372
1791.920622	146432.024796	37.453389
1793.140544	146685.286807	37.458407
1795.086551	146960.661389	37.463424
1796.858696	147223.537068	37.468442
1798.301311	147492.710076	37.473460
1800.777885	147754.653798	37.478477
1802.205917	148027.601532	37.483495
1804.149384	148299.188506	37.488512
1805.968369	148562.190569	37.493530
1807.788982	148850.020852	37.498548
1810.117916	149111.499303	37.503565
1811.857062	149390.180935	37.508583
1813.856333	149665.574127	37.513600
1816.121735	149933.451092	37.518618
1817.936196	150202.288097	37.523636
1819.423828	150477.561997	37.528653
1821.194753	150754.570266	37.533671
1822.951410	151028.650008	37.538688
1824.822032	151300.949010	37.543706
1826.502559	151587.546413	37.548724
1828.543978	151887.709311	37.553741
1830.457614	152180.683764	37.558759
1831.992742	152458.270479	37.563776
1833.839075	152749.125876	37.568794
1836.164831	153024.091699	37.573812
1838.417101	153296.341132	37.578829
1839.839733	153577.238629	37.583847
1841.644546	153861.530808	37.588864
1843.560061	154147.571660	37.593882
1845.472352	154424.131950	37.598900
1847.584297	154699.761221	37.603917
1849.099781	154988.013862	37.608935
1850.804099	155275.388039	37.613952
1852.947998	155559.305837	37.618970
1854.386876	155846.787637	37.623988
1856.369689	156126.252145	37.629005
1858.115173	156416.024817	37.634023
1859.907657	156713.256037	37.639040
1862.043027	157005.814528	37.644058
1863.422720	157307.797320	37.649076
1865.212387	157593.938197	37.654093
1867.333750	157896.506757	37.659111
1869.242570	158181.806735	37.664128
1871.679784	158473.436798	37.669146
1873.432584	158772.182453	37.674164
1875.426896	159042.873882	37.679181
1877.039948	159332.427389	37.684199
1878.879316	159628.205789	37.689216
1880.580491	159918.979784	37.694234
1882.190705	160211.711691	37.699252
1884.075533	160487.034924	37.704269
1886.018042	160765.740084	37.709287
1887.565181	161042.705254	37.714304
1889.565719	161322.406800	37.719322
1891.245139	161603.365647	37.724340
1893.075956	161877.687725	37.729357
1895.127608	162164.494613	37.734375
1897.053210	162450.916139	37.739392
1899.333352	162727.190560	37.744410
1900.735621	163020.437564	37.749428
1902.383404	163311.349713	37.754445
1903.857680	163610.859979	37.759463
1905.206501	163920.421045	37.764480
1907.501359	164229.201523	37.769498
1909.099775	164544.719251	37.774516
1910.997154	164850.326951	37.779533
1913.093836	165169.655146	37.784551
1914.751134	165496.163217	37.789568
1916.861438	165815.530442	37.794586
1918.028090	166147.704449	37.799604
1920.313906	166469.713694	37.804621
1922.507542	166802.150028	37.809639
1924.101619	167131.367439	37.814656
1925.912735	167472.093976	37.819674
1928.302820	167804.656897	37.824692
1930.231656	168134.537959	37.829709
1931.872619	168481.517339	37.834727
1933.801812	168834.510020	37.839744
1935.579165	169177.332339	37.844762
1937.381435	169532.963803	37.849780
1939.684037	169881.040508	37.854797
1941.503512	170238.183711	37.859815
1943.321505	170590.986407	37.864832
1945.029854	170943.769763	37.869850
1946.934628	171304.866428	37.874868
1949.226554	171658.997154	37.879885
1951.850918	172015.439551	37.884903
1953.569323	172371.161187	37.889920
1955.626746	172731.136226	37.894938
1957.633005	173085.533919	37.899956
1959.699193	173451.390004	37.904973
1961.379364	173808.165443	37.909991
1963.459262	174174.759257	37.915008
1965.674425	174536.876741	37.920026
1967.829675	174901.417822	37.925044
1969.506065	175254.683015	37.930061
1971.557696	175617.541931	37.935079
1973.344087	175987.097596	37.940096
1975.561978	176336.664240	37.945114
1977.094039	176709.259522	37.950132
1979.080222	177076.223922	37.955149
1981.331224	177442.628083	37.960167
1983.417789	177820.970586	37.965184
1985.507437	178183.695119	37.970202
1987.352430	178546.891018	37.975220
1989.748631	178910.307428	37.980237
1991.805347	179272.533722	37.985255
1993.592830	179633.838313	37.990272
1995.913131	180002.375957	37.995290
1997.853739	180371.075810	38.000308
1999.430562	180752.583476	38.005325
2001.576210	181089.634141	38.010343
2003.554281	181464.732886	38.015360
2005.542918	181841.203014	38.020378
2007.241072	182209.973436	38.025396
2008.950409	182576.711710	38.030413
2011.449926	182941.829929	38.035431
2013.619924	183315.128345	38.040448
2015.430462	183660.139360	38.045466
2017.244702	184001.239637	38.050484
2019.308622	184350.988618	38.055501
2021.615267	184703.444142	38.060519
2023.486772	185060.591245	38.065536
2025.372548	185396.148244	38.070554
2027.539198	185746.673511	38.075572
2029.350881	186110.412007	38.080589
2031.705259	186454.052705	38.085607
2033.557797	186818.244528	38.090624
2035.917110	187172.427566	38.095642
2037.590070	187536.014839	38.100660
2039.366418	187913.176061	38.105677
2041.149236	188334.025107	38.110695
2042.980220	188706.964240	38.115712
2045.352871	189070.574778	38.120730
2047.263842	189459.455136	38.125748
2049.137371	189842.475256	38.130765
2050.776033	190220.478592	38.135783
2052.567753	190616.849126	38.140800
2054.492780	191011.041241	38.145818
2056.547372	191402.776080	38.150836
2058.444920	191809.675349	38.155853
2060.386545	192210.549202	38.160871
2062.792197	192622.249048	38.165888
2064.778733	193035.361741	38.170906
2066.868891	193449.094700	38.175924
2068.367220	193862.260702	38.180941
2070.475696	194280.489486	38.185959
2073.183969	194699.896331	38.190976
2075.786235	195114.926617	38.195994
2077.894744	195523.760939	38.201012
2079.724683	195958.320587	38.206029
2081.718658	196353.483928	38.211047
2084.373983	196772.397448	38.216064
2087.011408	197177.928392	38.221082
2089.354866	197594.606747	38.226100
2091.341671	198012.103862	38.231117
2093.372214	198409.578774	38.236135
2095.404693	198824.835724	38.241152
2097.291418	199238.236760	38.246170
2099.829687	199658.370639	38.251188
2101.570528	200078.426539	38.256205
2103.872517	200483.358180	38.261223
2105.824288	200906.863520	38.266240
2107.776496	201318.735669	38.271258
2109.756100	201751.053417	38.276276
2111.786174	202173.660714	38.281293
2113.910018	202591.580411	38.286311
2115.692810	203018.775279	38.291328
2117.890549	203452.790678	38.296346
2120.372237	203881.656998	38.301364
2122.557216	204307.598374	38.306381
2124.504696	204739.674322	38.311399
2126.330404	205183.684084	38.316416
2128.150292	205619.490639	38.321434
2130.849100	206044.441334	38.326452
2133.331537	206473.033797	38.331469
2135.649714	206893.955593	38.336487
2137.938159	207343.715279	38.341504
2139.426882	207773.455698	38.346522
2141.686231	208209.326174	38.351540
2143.944132	208643.394070	38.356557
2145.964499	209061.140054	38.361575
2147.845195	209520.976302	38.366592
2149.929756	209955.657792	38.371610
2152.249555	210393.656651	38.376628
2154.167332	210830.474037	38.381645
2156.361139	211249.974831	38.386663
2157.976601	211666.467039	38.391680
2160.006052	212079.770789	38.396698
2162.452027	212499.970865	38.401716
2164.550102	212917.482075	38.406733
2166.840290	213336.843807	38.411751
2169.023615	213768.111614	38.416768
2171.191690	214187.137775	38.421786
2173.082201	214608.875023	38.426804
2175.186922	215047.498312	38.431821
2177.559543	215468.272380	38.436839
2180.088473	215911.962195	38.441856
2182.014795	216353.053467	38.446874
2184.191032	216782.877801	38.451892
2186.095710	217230.603727	38.456909
2188.453641	217664.617648	38.461927
2190.312019	218122.462349	38.466944
2192.295127	218577.315776	38.471962
2194.472184	219040.776733	38.476980
2196.253462	219503.791563	38.481997
2198.167752	219961.959269	38.487015
2200.185721	220441.094852	38.492032
2202.512300	220917.439078	38.497050
2205.012656	221389.158404	38.502068
2207.204407	221875.863581	38.507085
2209.802514	222346.348768	38.512103
2211.704751	222836.706808	38.517120
2214.093703	223319.190229	38.522138
2216.521853	223810.254275	38.527156
2218.901707	224280.799453	38.532173
2221.365687	224750.061421	38.537191
2223.444336	225243.720542	38.542208
2225.294467	225741.302090	38.547226
2227.414764	226228.730770	38.552244
2229.712657	226730.739146	38.557261
2232.022363	227219.129036	38.562279
2234.126892	227721.396006	38.567296
2236.732419	228216.751194	38.572314
2239.420302	228704.878668	38.577332
2241.441622	229214.169681	38.582349
2244.052525	229693.798408	38.587367
2246.263424	230192.059525	38.592384
2248.281683	230682.119455	38.597402
2251.178390	231177.199406	38.602420
2253.357043	231673.533965	38.607437
2255.738795	232162.037547	38.612455
2257.846492	232669.356934	38.617472
2259.972252	233157.467708	38.622490
2262.429120	233656.373997	38.627508
2264.752535	234154.106597	38.632525
2267.127140	234641.211916	38.637543
2269.310223	235143.792059	38.642560
2271.253712	235641.201137	38.647578
2274.049176	236142.719463	38.652596
2276.046588	236643.980298	38.657613
2277.741220	237147.040445	38.662631
2279.977709	237649.913952	38.667648
2282.131410	238161.411444	38.672666
2284.424106	238668.771135	38.677684
2286.578410	239196.474395	38.682701
2288.686772	239707.544601	38.687719
2291.326645	240227.092171	38.692736
2293.630171	240742.880624	38.697754
2296.791356	241218.752967	38.702772
2299.293616	241725.236388	38.707789
2302.293879	242217.313870	38.712807
2304.812110	242694.604515	38.717824
2307.399557	243184.076970	38.722842
2309.661757	243633.258879	38.727860
2311.977368	244099.400846	38.732877
2313.820471	244560.179133	38.737895
2316.156616	245016.510409	38.742912
2317.890162	245475.855822	38.747930
2320.923444	245913.761170	38.752948
2323.378516	246373.398739	38.757965
2325.144891	246845.107112	38.762983
2327.833220	247305.595299	38.768000
2329.868971	247764.735982	38.773018
2332.626342	248218.809735	38.778036
2334.904030	248687.411022	38.783053
2337.001852	249143.718903	38.788071
2339.839078	249612.662505	38.793088
2342.045111	250084.573514	38.798106
2344.212378	250551.434196	38.803124
2346.399073	251024.056822	38.808141
2349.163618	251485.919279	38.813159
2351.615404	251955.932304	38.818176
2353.678754	252433.116900	38.823194
2355.803884	252910.976249	38.828212
2357.799619	253405.797186	38.833229
2360.129122	253886.085584	38.838247
2362.229189	254381.344230	38.843264
2363.984505	254888.949131	38.848282
2366.618623	255389.353853	38.853300
2369.209331	255893.573714	38.858317
2371.439244	256405.010992	38.863335
2373.745278	256915.723237	38.868352
2375.505150	257437.390122	38.873370
2377.863009	257959.673069	38.878388
2379.936049	258481.718787	38.883405
2382.205402	259029.234062	38.888423
2384.367493	259566.298562	38.893440
2386.901761	260116.841204	38.898458
2389.323834	260648.627915	38.903476
2391.910114	261199.157424	38.908493
2394.258462	261740.907505	38.913511
2396.886779	262294.066827	38.918528
2398.939756	262851.503929	38.923546
2401.592877	263400.208916	38.928564
2404.248210	263954.955893	38.933581
2406.673121	264522.664180	38.938599
2409.059229	265061.140838	38.943616
2411.412266	265617.780279	38.948634
2414.394276	266174.344219	38.953652
2416.781871	266736.458369	38.958669
2419.021477	267283.403926	38.963687
2421.611627	267845.683461	38.968704
2423.825993	268407.307068	38.973722
2426.637701	268966.396190	38.978740
2429.184512	269528.139246	38.983757
2431.002985	270086.131775	38.988775
2433.584413	270642.833897	38.993792
2435.857308	271213.244601	38.998810
2438.019763	271782.957747	39.003828
2440.588818	272355.956420	39.008845
2443.313883	272920.038050	39.013863
2445.737033	273494.093243	39.018880
2447.363365	274067.024147	39.023898
2449.833705	274632.530976	39.028916
2452.666149	275221.113870	39.033933
2454.566266	275807.678978	39.038951
2457.614922	276382.201129	39.043968
2459.880447	276968.853367	39.048986
2462.564597	277553.023549	39.054004
2465.058266	278128.584545	39.059021
2467.528057	278703.484736	39.064039
2470.081528	279260.032266	39.069056
2471.898802	279813.515932	39.074074
2473.996513	280365.555189	39.079092
2476.754570	280925.309173	39.084109
2479.203147	281503.137172	39.089127
2481.612904	282064.282619	39.094144
2484.183134	282626.693855	39.099162
2486.800712	283194.070524	39.104180
2489.485371	283758.994438	39.109197
2491.600322	284323.748548	39.114215
2494.061721	284895.401931	39.119232
2496.733962	285466.332162	39.124250
2499.170589	286046.105614	39.129268
2501.431118	286629.989725	39.134285
2503.933304	287221.677404	39.139303
2506.343647	287801.389006	39.144320
2508.346178	288400.863122	39.149338
2510.677375	288997.817588	39.154356
2513.190532	289604.209242	39.159373
2515.727093	290220.164002	39.164391
2518.465397	290832.856728	39.169408
2521.072741	291458.106874	39.174426
2523.301490	292076.681179	39.179444
2525.886112	292694.686090	39.184461
2528.034842	293328.773638	39.189479
2530.192446	293956.429569	39.194496
2532.992973	294605.382148	39.199514
2535.536963	295238.245453	39.204532
2538.614687	295876.959881	39.209549
2541.259657	296520.253818	39.214567
2543.827791	297151.848541	39.219584
2546.373791	297793.137958	39.224602
2549.284342	298433.931801	39.229620
2552.333226	299080.561307	39.234637
2555.173041	299719.218893	39.239655
2557.576166	300352.047303	39.244672
2560.194941	300990.267562	39.249690
2562.972160	301623.556114	39.254708
2565.524719	302261.822438	39.259725
2567.933076	302894.874128	39.264743
2571.102006	303521.250469	39.269760
2573.781040	304158.052672	39.274778
2576.608392	304798.073252	39.279796
2579.464592	305425.541513	39.284813
2581.821252	306059.273551	39.289831
2584.511968	306692.971090	39.294848
2587.364776	307325.747021	39.299866
2590.239428	307946.987604	39.304884
2592.755920	308567.210074	39.309901
2595.274128	309190.140402	39.314919
2597.803905	309810.801986	39.319936
2600.417759	310440.148531	39.324954
2602.573850	311081.335122	39.329972
2605.539902	311718.706803	39.334989
2607.955423	312348.947443	39.340007
2610.212897	312981.666161	39.345024
2613.124015	313615.645132	39.350042
2615.507974	314245.966655	39.355060
2618.414102	314890.969147	39.360077
2620.885178	315533.517723	39.365095
2623.461171	316163.021596	39.370112
2625.845009	316810.336839	39.375130
2628.920837	317447.333085	39.380148
2631.544791	318079.949440	39.385165
2633.781866	318729.822746	39.390183
2636.350647	319372.402390	39.395200
2639.522185	320010.742384	39.400218
2641.717269	320639.074452	39.405236
2644.294447	321256.426285	39.410253
2646.814901	321865.099623	39.415271
2649.813205	322472.395740	39.420288
2652.345059	323083.561905	39.425306
2654.882140	323693.880990	39.430324
2657.470126	324321.209132	39.435341
2659.685662	324937.700464	39.440359
2662.305095	325562.086880	39.445376
2664.554194	326195.655591	39.450394
2666.809360	326835.353592	39.455412
2669.670699	327482.355738	39.460429
2671.743521	328129.749236	39.465447
2674.246236	328781.632121	39.470464
2677.018767	329449.598065	39.475482
2679.108636	330115.959087	39.480500
2682.182680	330789.588957	39.485517
2684.711609	331469.101560	39.490535
2687.149320	332143.009843	39.495552
2690.204688	332830.001784	39.500570
2692.897832	333521.147318	39.505588
2695.802031	334201.187111	39.510605
2698.475147	334894.416097	39.515623
2701.319793	335579.310626	39.520640
2704.221520	336272.376908	39.525658
2706.731757	336969.980814	39.530676
2709.581940	337670.080425	39.535693
2712.359241	338374.718200	39.540711
2715.053795	339072.405331	39.545728
2717.488739	339791.729222	39.550746
2720.384676	340506.452242	39.555764
2722.788021	341205.893092	39.560781
2725.588670	341940.562428	39.565799
2728.185428	342665.179523	39.570816
2731.129530	343391.452052	39.575834
2733.619351	344122.877521	39.580852
2736.965560	344849.792246	39.585869
2739.657345	345585.872060	39.590887
2742.316959	346310.072946	39.595904
2745.507515	347041.656416	39.600922
2748.199827	347759.608230	39.605940
2751.741186	348481.799290	39.610957
2754.520035	349206.375394	39.615975
2757.555340	349934.978018	39.620992
2760.536749	350643.998276	39.626010
2762.597089	351381.037045	39.631028
2766.127873	352099.803172	39.636045
2768.505256	352813.433772	39.641063
2771.619346	353544.529077	39.646080
2774.873008	354265.444762	39.651098
2777.627246	354978.410449	39.656116
2780.177076	355697.856474	39.661133
2782.991364	356418.385617	39.666151
2785.883734	357138.961988	39.671168
2789.010569	357841.714834	39.676186
2791.250428	358574.299057	39.681204
2793.953460	359296.527467	39.686221
2796.929534	360020.065062	39.691239
2800.694916	360698.622815	39.696256
2805.877365	361363.130675	39.701274
2808.485773	362048.656321	39.706292
2811.345081	362732.099511	39.711309
2814.260650	363418.483602	39.716327
2816.680772	364091.344123	39.721344
2819.180781	364765.849520	39.726362
2821.809393	365446.933994	39.731380
2824.238841	366129.984925	39.736397
2826.499829	366827.313656	39.741415
2828.649845	367502.012695	39.746432
2831.181477	368171.745653	39.751450
2833.353146	368839.694400	39.756468
2835.848717	369505.347132	39.761485
2838.741378	370191.523225	39.766503
2841.278753	370875.229347	39.771520
2844.026133	371559.772928	39.776538
2845.966762	372277.161140	39.781556
2848.861325	372978.090843	39.786573
2851.611886	373690.350379	39.791591
2854.479677	374402.497195	39.796608
2857.059677	375132.429896	39.801626
2859.328724	375864.848801	39.806644
2862.189384	376601.057161	39.811661
2864.724590	377362.679362	39.816679
2867.853468	378111.876211	39.821696
2870.441450	378867.899611	39.826714
2872.782641	379641.215260	39.831732
2875.921437	380411.648520	39.836749
2878.852639	381191.285899	39.841767
2881.660187	381967.550598	39.846784
2884.730551	382743.269993	39.851802
2887.558227	383538.480116	39.856820
2890.634243	384330.005412	39.861837
2894.000034	385116.573390	39.866855
2897.086491	385915.214926	39.871872
2899.979647	386709.176519	39.876890
2902.566242	387520.152370	39.881908
2905.446220	388324.168795	39.886925
2908.774367	389131.052148	39.891943
2911.357545	389943.924831	39.896960
2914.298515	390756.436586	39.901978
2917.231737	391574.999157	39.906996
2920.453961	392387.615651	39.912013
2923.240923	393210.753939	39.917031
2926.152556	394027.667745	39.922048
2929.620045	394838.746135	39.927066
2932.684975	395668.693575	39.932084
2936.016044	396495.077485	39.937101
2938.901875	397322.362546	39.942119
2941.535867	398148.240384	39.947136
2944.623879	398968.905795	39.952154
2947.915730	399799.533412	39.957172
2950.948561	400621.414807	39.962189
2954.036447	401434.856211	39.967207
2957.145283	402269.877989	39.972224
2960.572293	403081.538134	39.977242
2963.368986	403904.756160	39.982260
2966.461974	404717.118591	39.987277
2969.070843	405532.462414	39.992295
2971.812726	406374.424972	39.997312
2975.020995	407190.931100	40.002330
2977.751002	408021.245376	40.007348
2981.172938	408840.390251	40.012365
2984.599859	409670.534298	40.017383
2987.249507	410487.360117	40.022400
2990.294125	411313.099743	40.027418
2993.050314	412141.028453	40.032436
2996.090416	412966.453101	40.037453
2999.462452	413798.421619	40.042471
3002.271342	414620.227210	40.047488
3005.698569	415447.115232	40.052506
3009.470578	416248.828749	40.057524
3012.311152	417061.430555	40.062541
3015.531850	417870.199183	40.067559
3018.282197	418689.782719	40.072576
3021.130893	419499.456894	40.077594
3024.356359	420310.305349	40.082612
3027.182348	421109.148546	40.087629
3030.134051	421893.731572	40.092647
3032.972781	422676.835882	40.097664
3035.871401	423455.754691	40.102682
3038.180423	424240.701995	40.107700
3040.767297	425026.688154	40.112717
3043.480601	425823.039322	40.117735
3046.026769	426619.385108	40.122752
3048.811550	427442.304662	40.127770
3051.527253	428272.329106	40.132788
3054.158083	429103.697096	40.137805
3057.466778	429929.971061	40.142823
3060.705051	430772.143586	40.147840
3063.895891	431615.500552	40.152858
3066.442987	432471.405315	40.157876
3069.551594	433327.437907	40.162893
3072.804641	434181.338312	40.167911
3075.592826	435059.126072	40.172928
3078.703138	435924.241053	40.177946
3081.675040	436802.223933	40.182964
3085.041926	437676.467003	40.187981
3087.912312	438550.090361	40.192999
3090.952253	439446.938506	40.198016
3094.446995	440331.649224	40.203034
3097.657878	441236.064840	40.208052
3100.412736	442137.022096	40.213069
3103.997415	443024.673049	40.218087
3107.192382	443931.738629	40.223104
3110.522180	444826.414506	40.228122
3113.487378	445742.366902	40.233140
3116.847586	446647.707216	40.238157
3119.581870	447546.130804	40.243175
3122.680644	448470.662264	40.248192
3125.364112	449398.796367	40.253210
3128.566079	450330.891984	40.258228
3131.487027	451257.782322	40.263245
3135.019647	452191.749256	40.268263
3137.484805	453138.101330	40.273280
3140.491097	454070.132886	40.278298
3144.231124	455011.945679	40.283316
3147.423157	455962.879238	40.288333
3151.328820	456907.391148	40.293351
3154.852832	457847.217295	40.298368
3157.886539	458778.034759	40.303386
3161.325124	459728.219253	40.308404
3164.145004	460667.194058	40.313421
3167.637202	461603.388792	40.318439
3170.896868	462552.889367	40.323456
3174.585223	463490.715820	40.328474
3177.870981	464426.534819	40.333492
3181.311332	465362.681389	40.338509
3184.961137	466290.268004	40.343527
3188.112283	467216.720514	40.348544
3191.257809	468138.885248	40.353562
3194.641089	469071.503428	40.358580
3197.839531	469994.111385	40.363597
3201.404240	470910.054299	40.368615
3204.135440	471844.331510	40.373632
3207.379170	472761.027608	40.378650
3210.332690	473690.676321	40.383668
3213.658455	474621.726414	40.388685
3216.998917	475539.157841	40.393703
3220.487427	476463.118357	40.398720
3223.777224	477370.873897	40.403738
3226.832453	478294.997590	40.408756
3229.642846	479213.409639	40.413773
3233.703316	480128.398425	40.418791
3236.933883	481056.013204	40.423808
3239.855926	481959.228416	40.428826
3243.063704	482849.193830	40.433844
3245.868756	483724.053330	40.438861
3249.321771	484606.270864	40.443879
3252.167931	485503.447131	40.448896
3255.129555	486381.054660	40.453914
3258.177728	487269.984799	40.458932
3260.885287	488175.138173	40.463949
3263.882873	489083.719043	40.468967
3266.580502	490005.439477	40.473984
3269.984512	490919.539344	40.479002
3273.260817	491846.598205	40.484020
3275.978866	492788.644616	40.489037
3279.482459	493729.149914	40.494055
3282.475680	494673.200388	40.499072
3285.590875	495632.529775	40.504090
3288.929101	496603.292557	40.509108
3292.205090	497576.921360	40.514125
3295.440824	498532.922224	40.519143
3298.609040	499519.729718	40.524160
3301.721648	500501.344906	40.529178
3305.106980	501496.793761	40.534196
3308.310471	502496.027649	40.539213
3311.809474	503491.371994	40.544231
3314.643281	504507.534290	40.549248
3318.034544	505519.462005	40.554266
3321.567767	506523.295790	40.559284
3324.494459	507567.100810	40.564301
3327.826256	508589.636532	40.569319
3332.675998	509588.319468	40.574336
3336.837278	510589.956093	40.579354
3340.657532	511600.627751	40.584372
3344.461616	512600.315038	40.589389
3348.153050	513586.269099	40.594407
3351.725787	514581.876847	40.599424
3355.468779	515565.921831	40.604442
3358.703761	516563.199015	40.609460
3361.794084	517555.901400	40.614477
3365.279949	518540.527155	40.619495
3368.309752	519550.990684	40.624512
3371.218253	520549.284082	40.629530
3374.458883	521551.523257	40.634548
3377.995893	522563.994759	40.639565
3381.059531	523572.493561	40.644583
3384.225487	524588.739370	40.649600
3387.416442	525613.395360	40.654618
3391.058047	526641.670330	40.659636
3394.157966	527670.301371	40.664653
3397.774560	528698.420156	40.669671
3401.021963	529732.493329	40.674688
3404.313981	530761.857106	40.679706
3408.139434	531786.838013	40.684724
3411.082565	532840.801037	40.689741
3414.617985	533880.576459	40.694759
3418.116678	534926.951765	40.699776
3421.265522	535977.061827	40.704794
3424.693582	537027.494225	40.709812
3427.646750	538087.200673	40.714829
3431.069855	539145.189765	40.719847
3434.201964	540212.721992	40.724864
3437.534967	541281.487758	40.729882
3441.197191	542348.957410	40.734900
3444.587320	543422.098662	40.739917
3448.259769	544489.434411	40.744935
3451.580470	545564.208415	40.749952
3454.880365	546631.117263	40.754970
3458.661843	547701.019151	40.759988
3462.016056	548782.279736	40.765005
3465.329239	549841.269058	40.770010
3468.973438	550857.493274	40.775015
3472.066228	551833.602939	40.780020
3475.194921	552768.561003	40.785024
3478.038574	553648.051526	40.790029
3481.225360	554460.931590	40.795034
3483.821942	555230.025309	40.800039
3486.609347	555938.686110	40.805044
3489.348852	556588.770750	40.810048
3491.389130	557196.620150	40.815053
3493.971349	557724.212552	40.820058
3496.353291	558218.702226	40.825063
3497.988943	558671.637127	40.830068
3500.073703	559058.067602	40.835072
3501.636390	559416.131706	40.840077
3503.336045	559720.208904	40.845082
3505.031701	559987.807486	40.850087
3506.338536	560212.710398	40.855092
3507.622577	560406.417040	40.860096
3508.454158	560574.722448	40.865101
3509.631758	560695.953432	40.870106
3511.122955	560793.072891	40.875111
3511.741955	560848.081773	40.880116
3512.849898	560889.602276	40.885120
3513.496707	560907.334073	40.890125
3514.478997	560892.965436	40.895130
3515.512177	560857.993554	40.900135
3516.128278	560814.094824	40.905140
3516.806161	560729.547848	40.910144
3517.326580	560636.133455	40.915149
3517.961055	560511.856958	40.920154
3518.409557	560386.854579	40.925159
3518.480740	560255.429275	40.930164
3518.820912	560095.728204	40.935168
3519.218768	559949.831011	40.940173
3519.617283	559770.323338	40.945178
3519.908161	559581.786877	40.950183
3519.630855	559389.768890	40.955188
3519.871463	559186.564260	40.960192
3519.574567	558989.217447	40.965197
3520.202682	558772.933171	40.970202
3519.832582	558555.293033	40.975207
3519.991367	558343.796766	40.980212
3519.885916	558123.143201	40.985216
3519.876481	557895.486554	40.990221
3519.898697	557667.368423	40.995226
3519.931756	557437.636345	41.000231
3519.562783	557209.017618	41.005236
3519.832022	556966.878745	41.010240
3519.735830	556734.691078	41.015245
3519.533471	556501.007902	41.020250
3519.740416	556256.904586	41.025255
3519.234750	556013.660989	41.030260
3519.327525	555768.359431	41.035264
3519.098686	555539.636792	41.040269
3519.128317	555292.325147	41.045274
3518.933087	555053.989150	41.050279
3518.681929	554814.048884	41.055284
3518.700443	554570.644265	41.060288
3518.337400	554338.904159	41.065293
3518.134750	554087.482616	41.070298
3518.182542	553849.235771	41.075303
3517.949582	553614.797641	41.080308
3517.695695	553372.466786	41.085312
3517.368482	553145.875410	41.090317
3517.193669	552915.586673	41.095322
3517.119480	552689.148446	41.100327
3517.059329	552476.527423	41.105332
3517.111138	552235.483495	41.110336
3516.771590	552016.111620	41.115341
3516.726583	551790.657492	41.120346
3516.502976	551561.959337	41.125351
3516.535879	551355.236256	41.130356
3516.226775	551117.745409	41.135360
3516.131393	550897.913204	41.140365
3515.706386	550681.898963	41.145370
3515.739344	550482.048759	41.150375
3515.572743	550275.489259	41.155380
3515.376140	550054.752649	41.160384
3515.144072	549844.726904	41.165389
3515.017719	549637.094515	41.170394
3514.675220	549439.347162	41.175399
3514.289859	549234.815353	41.180404
3514.388373	549033.020620	41.185408
3514.150416	548847.868199	41.190413
3514.125758	548645.432592	41.195418
3514.149592	548455.104606	41.200423
3513.694973	548266.909812	41.205428
3513.985768	548072.410996	41.210432
3514.037843	547877.091387	41.215437
3513.787532	547687.850220	41.220442
3512.979712	547508.750522	41.225447
3512.925201	547325.005004	41.230452
3513.193034	547133.663155	41.235456
3512.893755	546962.070114	41.240461
3513.139864	546787.120906	41.245466
3512.883280	546603.446397	41.250471
3512.316477	546430.177686	41.255476
3512.457023	546254.281818	41.260480
3512.471908	546085.343563	41.265485
3512.063873	545908.723456	41.270490
3511.675678	545746.532484	41.275495
3511.659823	545585.840624	41.280500
3511.308219	545419.414829	41.285504
3511.429575	545268.807119	41.290509
3511.451025	545105.940470	41.295514
3511.759539	544942.322839	41.300519
3511.465408	544790.114140	41.305524
3510.930293	544628.535029	41.310528
3510.653104	544480.846889	41.315533
3510.512111	544332.180086	41.320538
3510.805150	544178.564719	41.325543
3510.130682	544034.756033	41.330548
3510.555663	543898.269705	41.335552
3510.154003	543760.401425	41.340557
3510.098579	543607.285985	41.345562
3510.332573	543467.907054	41.350567
3510.058558	543346.162051	41.355572
3510.139913	543196.139199	41.360576
3509.718060	543061.133763	41.365581
3509.792859	542922.477817	41.370586
3509.728788	542789.275120	41.375591
3509.384001	542649.373458	41.380596
3509.037197	542520.488056	41.385600
3509.073782	542405.024407	41.390605
3509.035696	542269.598565	41.395610
3508.926777	542145.803838	41.400615
3508.698600	542019.661868	41.405620
3508.882318	541911.012973	41.410624
3508.824437	541795.105622	41.415629
3508.671250	541662.106078	41.420634
3508.582025	541543.434144	41.425639
3508.410160	541439.062726	41.430644
3508.357382	541317.313922	41.435648
3508.175347	541209.722150	41.440653
3508.222767	541081.314092	41.445658
3508.027389	540968.992825	41.450663
3507.864550	540865.772485	41.455668
3507.948426	540760.449983	41.460672
3507.615407	540655.493370	41.465677
3508.007368	540544.888295	41.470682
3508.046415	540435.846667	41.475687
3507.263319	540329.548517	41.480692
3507.658220	540222.663622	41.485696
3507.166624	540128.545544	41.490701
3507.439398	540025.049275	41.495706
3507.276512	539916.688730	41.500711
3506.932768	539824.457488	41.505716
3507.450210	539722.078006	41.510720
3507.195656	539628.623793	41.515725
3506.689826	539542.906972	41.520730
3506.658154	539448.762587	41.525735
3506.622162	539358.895447	41.530740
3506.717567	539255.823063	41.535744
3507.138767	539167.896276	41.540749
3506.486910	539077.519119	41.545754
3506.483882	538985.430038	41.550759
3506.572136	538903.642232	41.555764
3506.623547	538813.506017	41.560768
3506.760799	538723.607420	41.565773
3506.446735	538628.746046	41.570778
3506.542199	538549.118757	41.575783
3506.570307	538461.952793	41.580788
3506.269657	538378.662071	41.585792
3506.402782	538286.546740	41.590797
3506.315412	538205.184371	41.595802
3506.567838	538119.692221	41.600807
3506.183287	538034.902531	41.605812
3506.272658	537946.515679	41.610816
3506.342990	537869.152737	41.615821
3506.056212	537773.827801	41.620826
3506.056799	537691.089629	41.625831
3505.781508	537622.535946	41.630836
3505.794506	537533.302542	41.635840
3505.653460	537466.790582	41.640845
3505.476336	537393.892156	41.645850
3505.832059	537316.481452	41.650855
3505.651647	537245.797165	41.655860
3505.585605	537163.669892	41.660864
3505.369426	537086.850088	41.665869
3505.219485	537013.693612	41.670874
3505.233772	536940.209179	41.675879
3505.038468	536881.856138	41.680884
3505.234243	536801.447367	41.685888
3505.139708	536739.655491	41.690893
3505.130433	536679.259329	41.695898
3505.502397	536608.636556	41.700903
3504.972419	536542.431964	41.705908
3505.125844	536475.164372	41.710912
3505.151773	536408.067263	41.715917
3505.251256	536336.982069	41.720922
3505.141892	536268.193967	41.725927
3505.018206	536214.960709	41.730932
3505.124126	536145.836450	41.735936
3504.880353	536086.681989	41.740941
3504.796527	536020.052932	41.745946
3504.913054	535948.912599	41.750951
3504.568539	535895.762714	41.755956
3504.441957	535824.760192	41.760960
3504.299835	535765.638766	41.765965
3504.482693	535712.808737	41.770970
3504.779721	535651.554704	41.775975
3504.458654	535602.124776	41.780980
3504.297677	535546.679779	41.785984
3504.598942	535483.058497	41.790989
3504.378190	535418.008042	41.795994
3504.329093	535369.189268	41.800999
3504.276797	535311.058502	41.806004
3504.521881	535255.951756	41.811008
3504.414091	535192.745052	41.816013
3504.210652	535139.318394	41.821018
3504.497610	535069.405108	41.826023
3504.373240	535027.140654	41.831028
3504.277326	534978.579373	41.836032
3504.425267	534922.278200	41.841037
3504.267440	534881.478286	41.846042
3504.484227	534822.749718	41.851047
3504.166393	534767.728479	41.856052
3504.264344	534702.322776	41.861056
3504.165074	534649.129569	41.866061
3503.766246	534600.765017	41.871066
3504.236153	534552.416117	41.876071
3504.178355	534500.927396	41.881076
3503.873530	534439.962615	41.886080
3504.227355	534398.628490	41.891085
3503.877962	534344.768183	41.896090
3504.006159	534290.430606	41.901095
3503.729489	534242.096039	41.906100
3504.302221	534198.411523	41.911104
3503.879787	534151.005438	41.916109
3503.927617	534096.830576	41.921114
3504.164478	534045.948627	41.926119
3503.829185	534008.395435	41.931124
3503.846427	533949.945655	41.936128
3503.870290	533888.725752	41.941133
3503.756194	533849.476378	41.946138
3504.110640	533800.790236	41.951143
3503.765974	533749.695557	41.956148
3503.700063	533700.470335	41.961152
3504.067199	533670.912090	41.966157
3504.044380	533621.025398	41.971162
3504.173811	533561.599880	41.976167
3503.641407	533526.442109	41.981172
3503.701649	533476.239871	41.986176
3503.726789	533429.919400	41.991181
3503.647326	533388.599128	41.996186
3503.785049	533337.024997	42.001191
3503.541143	533289.487277	42.006196
3503.892737	533248.250514	42.011200
3503.720253	533209.713112	42.016205
3503.541593	533156.475765	42.021210
3503.472906	533111.930839	42.026215
3503.672266	533066.236446	42.031220
3503.752817	533029.521918	42.036224
3503.669529	532987.999579	42.041229
3503.678164	532933.674908	42.046234
3503.763775	532886.839624	42.051239
3503.502776	532849.926005	42.056244
3503.563498	532796.146462	42.061248
3503.458828	532752.008671	42.066253
3503.300452	532725.399813	42.071258
3503.308609	532669.412662	42.076263
3503.264317	532636.291091	42.081268
3503.332550	532586.688330	42.086272
3503.150980	532558.471621	42.091277
3503.064067	532508.489923	42.096282
3503.268883	532469.337781	42.101287
3503.197948	532441.506385	42.106292
3503.024132	532389.926618	42.111296
3502.931765	532367.435304	42.116301
3503.056734	532337.005436	42.121306
3503.390923	532300.903906	42.126311
3503.158189	532264.185615	42.131316
3503.196422	532223.095056	42.136320
3503.366983	532190.492751	42.141325
3503.199654	532151.246515	42.146330
3503.455877	532111.380408	42.151335
3503.119238	532069.542110	42.156340
3502.929076	532031.457101	42.161344
3503.005357	531998.919337	42.166349
3503.285680	531961.465806	42.171354
3503.252098	531915.652565	42.176359
3503.301333	531876.120047	42.181364
3503.285574	531839.165390	42.186368
3503.272929	531805.583624	42.191373
3502.986951	531768.016258	42.196378
3503.183929	531730.575032	42.201383
3503.022887	531693.592219	42.206388
3503.262620	531655.288159	42.211392
3502.974780	531626.683154	42.216397
3502.976401	531584.639603	42.221402
3503.010514	531555.279423	42.226407
3503.209338	531520.254174	42.231412
3503.309603	531483.381155	42.236416
3503.070418	531440.367578	42.241421
3503.067768	531405.121611	42.246426
3503.162829	531371.673021	42.251431
3503.328675	531331.919297	42.256436
3503.067052	531285.786860	42.261440
3503.132802	531247.256913	42.266445
3503.094932	531214.382483	42.271450
3503.496608	531181.187808	42.276455
3503.205596	531151.071665	42.281460
3502.744311	531103.710828	42.286464
3502.793639	531076.210268	42.291469
3502.738138	531046.309000	42.296474
3503.055394	531005.674714	42.301479
3502.819792	530990.403862	42.306484
3502.769495	530951.840747	42.311488
3502.792255	530916.388090	42.316493
3502.293695	530889.475933	42.321498
3502.630988	530868.979682	42.326503
3502.681172	530831.911198	42.331508
3502.699803	530807.335392	42.336512
3503.111305	530763.211239	42.341517
3503.269925	530740.526993	42.346522
3503.373515	530689.149092	42.351527
3503.093934	530654.498094	42.356532
3503.061990	530613.262314	42.361536
3502.939743	530585.082448	42.366541
3503.166957	530549.999823	42.371546
3502.965638	530504.560212	42.376551
3502.981264	530485.120524	42.381556
3502.455272	530461.585572	42.386560
3502.919281	530418.912401	42.391565
3502.804721	530391.939461	42.396570
3502.998646	530351.876250	42.401575
3503.037954	530328.706296	42.406580
3502.691787	530288.475154	42.411584
3502.898869	530255.258055	42.416589
3502.723370	530225.373581	42.421594
3502.909407	530189.742477	42.426599
3502.760324	530162.875150	42.431604
3503.115435	530126.814710	42.436608
3503.170974	530088.635433	42.441613
3503.074708	530058.234678	42.446618
3503.124542	530014.013208	42.451623
3503.030703	529977.015071	42.456628
3503.063073	529939.795759	42.461632
3503.078851	529914.815858	42.466637
3502.872338	529878.892489	42.471642
3502.775619	529852.016376	42.476647
3503.051899	529818.283821	42.481652
3502.803015	529793.798097	42.486656
3503.000608	529755.998612	42.491661
3502.587804	529723.380210	42.496666
3502.601301	529693.364394	42.501671
3502.449207	529660.302396	42.506676
3502.712597	529628.787143	42.511680
3502.446369	529602.339765	42.516685
3502.140390	529574.236671	42.521690
3502.637637	529539.260397	42.526695
3502.694290	529523.287680	42.531700
3502.401688	529492.865804	42.536704
3502.693088	529464.669516	42.541709
3502.771486	529433.132221	42.546714
3503.176905	529396.810149	42.551719
3502.740645	529377.942734	42.556724
3502.893637	529335.969115	42.561728
3502.903335	529297.845030	42.566733
3502.640984	529266.259638	42.571738
3502.637228	529238.461316	42.576743
3502.530383	529204.786804	42.581748
3502.277388	529182.415716	42.586752
3502.652788	529158.133821	42.591757
3502.136895	529132.731559	42.596762
3502.656244	529100.671602	42.601767
3502.274362	529090.860263	42.606772
3502.222045	529058.083385	42.611776
3502.435328	529031.660960	42.616781
3502.345818	529009.566304	42.621786
3502.581465	528983.794999	42.626791
3502.525345	528966.479398	42.631796
3502.250788	528920.038457	42.636800
3502.292613	528907.542246	42.641805
3502.390580	528879.626612	42.646810
3502.681923	528842.817144	42.651815
3502.668809	528829.372532	42.656820
3502.568417	528796.753570	42.661824
3503.001855	528764.605439	42.666829
3502.562476	528736.269497	42.671834
3502.357887	528702.608908	42.676839
3502.354190	528675.564821	42.681844
3502.304221	528657.290968	42.686848
3502.343892	528626.412477	42.691853
3502.264093	528599.732616	42.696858
3502.267729	528579.838705	42.701863
3502.323848	528550.971991	42.706868
3502.366187	528525.229869	42.711872
3502.226008	528511.099622	42.716877
3502.348351	528490.280567	42.721882
3502.000125	528456.792789	42.726887
3502.177934	528448.958770	42.731892
3501.937228	528412.482709	42.736896
3502.135690	528398.249281	42.741901
3502.372870	528387.736718	42.746906
3502.583798	528351.190208	42.751911
3502.351128	528330.929783	42.756916
3502.340393	528295.273796	42.761920
3502.581948	528269.903086	42.766925
3502.534890	528255.405525	42.771930
3502.668413	528222.698375	42.776935
3502.371726	528194.339059	42.781940
3502.603093	528171.890877	42.786945
3502.588396	528143.286112	42.791949
3502.296418	528110.745626	42.796954
3502.459074	528091.329878	42.801959
3502.228596	528069.305943	42.806964
3502.189169	528042.165386	42.811969
3502.248335	528009.821833	42.816973
3502.455163	527995.435574	42.821978
3502.356315	527971.074197	42.826983
3502.161755	527939.172875	42.831988
3502.378595	527922.216346	42.836993
3502.254363	527892.771871	42.841997
3502.435371	527878.540599	42.847002
3502.440277	527849.126296	42.852007
3502.274935	527823.364755	42.857012
3502.399107	527808.487497	42.862017
3502.513439	527776.638446	42.867021
3502.637520	527752.342706	42.872026
3502.287698	527729.027257	42.877031
3502.180847	527694.492657	42.882036
3502.198114	527666.536645	42.887041
3502.199384	527646.138029	42.892045
3501.780550	527626.459519	42.897050
3501.673210	527605.120777	42.902055
3502.192763	527599.701038	42.907060
3502.104708	527571.207181	42.912065
3502.405632	527551.013622	42.917069
3502.215099	527521.528269	42.922074
3502.481821	527492.072429	42.927079
3502.505110	527479.124445	42.932084
3502.247606	527443.957860	42.937089
3502.309265	527411.864290	42.942093
3502.168467	527394.610167	42.947098
3502.500022	527364.640281	42.952103
3502.129757	527350.796430	42.957108
3502.356745	527321.396761	42.962113
3502.242766	527303.735404	42.967117
3502.064096	527290.667559	42.972122
3502.026469	527250.328728	42.977127
3502.102591	527235.559038	42.982132
3502.021374	527213.460078	42.987137
3502.313965	527191.605121	42.992141
3501.993319	527180.624355	42.997146
3502.270202	527156.152637	43.002151
3502.348339	527139.972215	43.007156
3502.070399	527117.752602	43.012161
3502.237600	527079.647957	43.017165
3502.095323	527071.459983	43.022170
3502.332498	527046.994243	43.027175
3502.088074	527024.064096	43.032180
3501.841677	527009.445079	43.037185
3501.832981	526982.801251	43.042189
3501.590804	526974.578394	43.047194
3501.872578	526951.666976	43.052199
3502.007996	526934.369268	43.057204
3501.604954	526920.630804	43.062209
3501.984431	526898.661105	43.067213
3502.023464	526878.658383	43.072218
3502.009778	526872.465050	43.077223
3502.246183	526839.939945	43.082228
3502.277185	526820.290970	43.087233
3502.650523	526787.039253	43.092237
3502.253481	526775.264122	43.097242
3502.438119	526738.062436	43.102247
3502.562764	526713.512851	43.107252
3502.131526	526701.188905	43.112257
3502.224227	526664.605760	43.117261
3502.046271	526653.602350	43.122266
3502.178253	526615.249998	43.127271
3502.248650	526611.058272	43.132276
3502.151996	526577.073239	43.137281
3502.394272	526554.620616	43.142285
3502.337515	526540.324164	43.147290
3502.276287	526520.135020	43.152295
3502.397078	526500.673082	43.157300
3502.181885	526471.642561	43.162305
3502.285620	526437.424503	43.167309
3502.509030	526425.653252	43.172314
3502.198333	526397.392996	43.177319
3502.108296	526378.971110	43.182324
3502.206253	526363.290368	43.187329
3502.445460	526336.505920	43.192333
3502.043824	526308.612226	43.197338
3502.428188	526276.868661	43.202343
3502.258448	526258.156780	43.207348
3501.967420	526233.318389	43.212353
3502.106573	526214.659123	43.217357
3502.244037	526199.375014	43.222362
3502.579629	526170.056636	43.227367
3502.131519	526148.718200	43.232372
3501.889887	526111.480345	43.237377
3502.282168	526097.063167	43.242381
3502.328494	526074.690597	43.247386
3502.098226	526060.974725	43.252391
3501.990334	526038.122367	43.257396
3502.005214	526028.901841	43.262401
3502.038166	526000.990244	43.267405
3502.057992	525980.132820	43.272410
3502.114171	525954.635403	43.277415
3501.945294	525948.163550	43.282420
3501.869158	525915.029967	43.287425
3502.168109	525897.906953	43.292429
3502.067379	525888.653947	43.297434
3502.219330	525866.214217	43.302439
3502.074892	525844.022064	43.307444
3502.238550	525819.112142	43.312449
3502.247645	525792.664647	43.317453
3502.219076	525776.096178	43.322458
3502.168471	525758.221403	43.327463
3502.009491	525737.189927	43.332468
3502.121233	525702.666488	43.337473
3502.507816	525688.300128	43.342477
3501.924077	525661.592008	43.347482
3502.045767	525642.078298	43.352487
3502.300212	525617.103496	43.357492
3501.885517	525603.113604	43.362497
3502.129281	525572.448095	43.367501
3502.039839	525559.818024	43.372506
3502.136827	525531.240609	43.377511
3502.145006	525508.369278	43.382516
3501.757777	525491.805891	43.387521
3502.435673	525467.268660	43.392525
3501.905069	525443.372815	43.397530
3501.959557	525434.347212	43.402535
3502.009704	525406.079066	43.407540
3502.071409	525394.835817	43.412545
3502.421301	525363.095436	43.417549
3502.031571	525348.043512	43.422554
3502.082648	525323.150181	43.427559
3502.066919	525304.463365	43.432564
3501.746184	525291.919407	43.437569
3502.236321	525262.423854	43.442573
3501.771915	525249.247332	43.447578
3501.942326	525230.027690	43.452583
3502.083537	525203.759968	43.457588
3501.866677	525196.388452	43.462593
3502.051667	525168.955207	43.467597
3501.887127	525165.152216	43.472602
3501.883123	525140.468617	43.477607
3501.946989	525116.177420	43.482612
3502.069151	525092.229740	43.487617
3502.179644	525080.273367	43.492621
3501.969374	525066.704482	43.497626
3502.035113	525036.921840	43.502631
3501.857287	525017.806459	43.507636
3501.718740	524999.541338	43.512641
3502.138939	524984.262214	43.517645
3501.715283	524967.250452	43.522650
3502.168009	524947.130069	43.527655
3502.097788	524920.491677	43.532660
3501.813514	524909.201102	43.537665
3501.767931	524882.155785	43.542669
3502.137092	524868.597286	43.547674
3502.198674	524849.746670	43.552679
3502.375446	524830.021692	43.557684
3502.009536	524801.363613	43.562689
3501.944694	524776.185034	43.567693
3502.268555	524746.764595	43.572698
3502.351132	524730.429416	43.577703
3502.424669	524694.649872	43.582708
3502.355661	524682.166921	43.587713
3502.365210	524654.810297	43.592717
3502.099423	524638.831482	43.597722
3502.131354	524608.599743	43.602727
3502.154276	524589.402130	43.607732
3502.221817	524570.852462	43.612737
3502.411286	524547.548246	43.617741
3502.341256	524530.128249	43.622746
3502.090569	524504.020889	43.627751
3502.539344	524481.331125	43.632756
3502.113439	524465.326639	43.637761
3502.434020	524433.739746	43.642765
3502.201523	524414.883900	43.647770
3502.181669	524388.740395	43.652775
3502.119128	524359.832642	43.657780
3502.081843	524338.880777	43.662785
3502.220937	524319.463182	43.667789
3501.843967	524293.727715	43.672794
3502.280363	524273.105070	43.677799
3502.055301	524255.960735	43.682804
3502.301546	524235.166103	43.687809
3502.509136	524206.165603	43.692813
3502.429801	524184.665865	43.697818
3502.378629	524160.945006	43.702823
3502.563124	524135.373761	43.707828
3502.417364	524108.846263	43.712833
3502.205101	524085.301476	43.717837
3502.239205	524056.831448	43.722842
3502.417455	524035.895948	43.727847
3502.367687	524003.257306	43.732852
3502.064055	523988.795008	43.737857
3501.979385	523964.877492	43.742861
3501.871579	523940.107065	43.747866
3502.043278	523913.076353	43.752871
3501.867321	523901.566545	43.757876
3501.416177	523884.557676	43.762881
3501.559824	523876.978186	43.767885
3501.548030	523861.765006	43.772890
3501.424481	523844.050157	43.777895
3501.472456	523838.450386	43.782900
3501.728303	523834.228930	43.787905
3501.832398	523810.634430	43.792909
3501.971155	523798.874037	43.797914
3501.738644	523775.684522	43.802919
3501.919394	523755.856579	43.807924
3501.815159	523742.269845	43.812929
3501.835564	523725.489681	43.817933
3501.958377	523713.328644	43.822938
3501.931439	523692.626062	43.827943
3501.708378	523667.117343	43.832948
3501.598178	523652.372671	43.837953
3501.743356	523633.003516	43.842957
3501.886958	523634.240679	43.847962
3501.761319	523615.467838	43.852967
3501.837010	523590.214774	43.857972
3501.586321	523574.585006	43.862977
3502.001528	523555.324864	43.867981
3501.914829	523547.680269	43.872986
3501.907060	523520.928603	43.877991
3501.947327	523506.311502	43.882996
3501.422549	523489.968555	43.888001
3502.229285	523464.299201	43.893005
3501.960661	523454.869101	43.898010
3501.969621	523438.291888	43.903015
3501.974444	523418.641970	43.908020
3501.907372	523390.942006	43.913025
3501.857763	523364.095772	43.918029
3501.879034	523365.654293	43.923034
3501.624280	523338.084190	43.928039
3501.876361	523331.797471	43.933044
3501.545521	523306.304836	43.938049
3502.011644	523294.291527	43.943053
3501.846129	523276.733606	43.948058
3501.758925	523253.520574	43.953063
3502.072626	523240.926340	43.958068
3501.878143	523224.582053	43.963073
3501.990693	523212.875607	43.968077
3501.846485	523192.845483	43.973082
3501.756215	523176.636070	43.978087
3501.782151	523158.393219	43.983092
3501.772383	523137.384806	43.988097
3502.393680	523126.556405	43.993101
3501.860211	523103.160639	43.998106
3502.126915	523082.461804	44.003111
3502.005488	523066.609792	44.008116
3502.237215	523049.543979	44.013121
3502.184335	523018.767624	44.018125
3501.918886	523002.988333	44.023130
3501.678265	522971.586093	44.028135
3501.796153	522957.057083	44.033140
3501.690508	522946.291273	44.038145
3501.853964	522927.019023	44.043149
3501.947967	522919.245182	44.048154
3501.799036	522896.444212	44.053159
3501.980043	522884.827597	44.058164
3501.969024	522864.574718	44.063169
3501.965020	522845.126871	44.068173
3501.623297	522819.584619	44.073178
3501.783755	522803.688432	44.078183
3502.082235	522788.375366	44.083188
3501.786109	522769.375945	44.088193
3501.735877	522747.264751	44.093197
3501.356910	522732.510505	44.098202
3501.739861	522708.820289	44.103207
3501.828355	522710.318040	44.108212
3501.522263	522685.072297	44.113217
3501.911654	522672.062671	44.118221
3501.591085	522671.407130	44.123226
3501.882454	522645.010250	44.128231
3501.894005	522631.102059	44.133236
3501.499205	522611.361988	44.138241
3501.803271	522581.385638	44.143245
3501.753048	522579.327613	44.148250
3501.551146	522568.223780	44.153255
3501.559212	522543.835826	44.158260
3501.838247	522551.702929	44.163265
3501.822735	522520.365374	44.168269
3501.677045	522514.644030	44.173274
3501.835923	522505.398665	44.178279
3501.800832	522480.059979	44.183284
3501.741856	522480.673756	44.188289
3501.889172	522448.302976	44.193293
3501.736697	522433.462770	44.198298
3501.563930	522422.555827	44.203303
3501.631669	522392.263128	44.208308
3501.423152	522387.408073	44.213313
3501.301843	522373.066813	44.218317
3501.289303	522379.417413	44.223322
3501.501582	522352.377243	44.228327
3501.935365	522337.848794	44.233332
3501.644990	522332.653752	44.238337
3501.919753	522303.689074	44.243341
3501.461670	522293.582224	44.248346
3501.322388	522275.918137	44.253351
3501.790333	522258.512243	44.258356
3501.854368	522254.824010	44.263361
3501.846523	522230.841059	44.268365
3501.900493	522218.487834	44.273370
3502.153885	522206.960144	44.278375
3502.389014	522183.090459	44.283380
3501.548368	522166.694272	44.288385
3501.630473	522135.592565	44.293389
3501.525513	522134.802671	44.298394
3501.506462	522120.142905	44.303399
3501.781340	522097.929664	44.308404
3501.577253	522094.686210	44.313409
3501.939600	522079.916663	44.318413
3501.600286	522056.539243	44.323418
3501.736009	522052.587863	44.328423
3501.926292	522033.763647	44.333428
3501.366140	522013.998040	44.338433
3501.996612	521990.923085	44.343437
3502.099612	521981.736444	44.348442
3501.790074	521969.489945	44.353447
3501.779419	521944.146447	44.358452
3501.671048	521932.725206	44.363457
3501.421156	521922.484903	44.368461
3501.848768	521895.863801	44.373466
3501.785903	521886.803683	44.378471
3501.848364	521876.665903	44.383476
3501.767055	521866.096994	44.388481
3501.758075	521847.001195	44.393485
3501.776236	521823.366190	44.398490
3501.649886	521802.524998	44.403495
3502.341754	521792.793097	44.408500
3501.776275	521785.423555	44.413505
3501.880132	521755.325358	44.418509
3501.826788	521732.457149	44.423514
3501.912440	521729.168520	44.428519
3501.938873	521709.059240	44.433524
3501.787341	521687.969845	44.438529
3501.900439	521671.676581	44.443533
3501.849790	521648.656645	44.448538
3501.691684	521635.479273	44.453543
3502.201293	521618.519573	44.458548
3502.355760	521601.514339	44.463553
3502.575745	521574.773747	44.468557
3502.412833	521555.499932	44.473562
3501.924791	521528.516699	44.478567
3501.888713	521496.424118	44.483572
3502.173774	521484.386988	44.488577
3502.260664	521454.189979	44.493581
3502.085860	521439.503320	44.498586
3501.960317	521417.048931	44.503591
3502.175789	521401.948769	44.508596
3501.917537	521378.759118	44.513601
3501.679960	521356.977133	44.518605
3501.819490	521342.795746	44.523610
3501.964895	521325.590013	44.528615
3502.514185	521313.914737	44.533620
3501.832194	521283.887384	44.538625
3502.003672	521266.022443	44.543629
3501.702127	521246.517806	44.548634
3501.784669	521234.612749	44.553639
3501.958880	521204.300813	44.558644
3501.604478	521200.627015	44.563649
3501.717261	521175.363646	44.568653
3501.867603	521153.520968	44.573658
3501.486219	521140.982548	44.578663
3502.037297	521125.729072	44.583668
3501.654565	521106.287258	44.588673
3501.761911	521098.006379	44.593677
3501.904259	521086.041494	44.598682
3501.772010	521068.273946	44.603687
3502.134956	521046.196446	44.608692
3501.993398	521034.829999	44.613697
3501.625447	521006.768814	44.618701
3501.749560	520996.368823	44.623706
3501.770939	520982.003877	44.628711
3501.799402	520964.815883	44.633716
3501.618340	520947.811647	44.638721
3502.416473	520924.507219	44.643725
3502.055129	520908.538823	44.648730
3501.922271	520883.262741	44.653735
3502.202322	520854.193348	44.658740
3502.000154	520839.258333	44.663745
3502.029776	520819.751937	44.668749
3502.091797	520800.895571	44.673754
3501.749315	520773.384253	44.678759
3501.778203	520760.580066	44.683764
3501.332262	520736.662631	44.688769
3501.911310	520717.826478	44.693773
3501.807693	520715.222158	44.698778
3501.714540	520697.800787	44.703783
3502.005269	520677.044132	44.708788
3501.998755	520663.489471	44.713793
3501.827182	520631.869456	44.718797
3501.748885	520624.876998	44.723802
3501.674822	520606.797431	44.728807
3501.985488	520588.053255	44.733812
3501.740300	520586.730766	44.738817
3501.764004	520571.205983	44.743821
3501.677545	520558.721913	44.748826
3501.719407	520527.824338	44.753831
3502.110450	520518.491093	44.758836
3501.609059	520510.354976	44.763841
3501.479540	520488.000447	44.768845
3501.673955	520480.108789	44.773850
3501.656037	520465.799804	44.778855
3501.711917	520443.517139	44.783860
3501.987665	520429.162417	44.788865
3501.627431	520410.975939	44.793869
3501.907466	520396.771697	44.798874
3501.708466	520374.629368	44.803879
3501.609143	520361.693573	44.808884
3501.319037	520360.327657	44.813889
3501.474178	520338.482918	44.818893
3501.662672	520323.234570	44.823898
3501.307700	520304.996737	44.828903
3501.729084	520298.682265	44.833908
3501.773379	520286.479962	44.838913
3501.792127	520265.160270	44.843917
3502.037172	520264.215011	44.848922
3501.553892	520235.565439	44.853927
3502.118565	520233.260187	44.858932
3502.326485	520203.595891	44.863937
3501.703906	520177.789963	44.868941
3501.883823	520148.281087	44.873946
3501.699933	520133.443236	44.878951
3502.154240	520120.622639	44.883956
3502.091851	520099.264917	44.888961
3502.128737	520071.340372	44.893965
3501.882421	520059.183086	44.898970
3501.913309	520043.253420	44.903975
3501.980663	520015.475203	44.908980
3501.957503	520014.269292	44.913985
3501.865164	519979.510922	44.918989
3501.843421	519965.000422	44.923994
3501.923328	519954.001766	44.928999
3501.863814	519924.277684	44.934004
3501.750349	519916.937565	44.939009
3502.043739	519895.221785	44.944013
3501.910548	519883.701881	44.949018
3501.930173	519854.519684	44.954023
3501.928288	519847.414142	44.959028
3501.802154	519819.161675	44.964033
3501.938734	519796.915785	44.969037
3502.212165	519784.576582	44.974042
3502.179230	519764.524046	44.979047
3502.123534	519734.143805	44.984052
3501.931086	519718.097322	44.989057
3501.905290	519701.218546	44.994061
3501.783315	519681.230139	44.999066
3501.786466	519671.906280	45.004071
3501.912838	519642.152654	45.009076
3501.962286	519629.243406	45.014081
3501.919441	519608.940200	45.019085
3501.869222	519601.640464	45.024090
3502.044065	519584.024767	45.029095
3502.276537	519555.867138	45.034100
3501.934665	519535.862339	45.039105
3502.016365	519516.043582	45.044109
3502.067985	519488.317132	45.049114
3501.891600	519468.941645	45.054119
3501.920675	519454.019513	45.059124
3502.063522	519434.947082	45.064129
3501.922591	519413.600503	45.069133
3501.722974	519402.292116	45.074138
3501.735005	519390.043630	45.079143
3501.875071	519361.698389	45.084148
3501.872745	519348.494546	45.089153
3501.657893	519330.132799	45.094157
3502.241880	519301.415966	45.099162
3501.601708	519290.730418	45.104167
3502.038212	519268.134604	45.109172
3501.430407	519271.253030	45.114177
3501.821295	519250.881794	45.119181
3501.873782	519236.258168	45.124186
3501.881346	519229.453221	45.129191
3501.821738	519203.406635	45.134196
3501.694959	519191.280367	45.139201
3501.538186	519169.331091	45.144205
3501.611983	519146.993111	45.149210
3501.616643	519139.886181	45.154215
3501.586800	519129.357522	45.159220
3501.732174	519108.721888	45.164225
3501.834707	519093.485539	45.169229
3501.758731	519079.234525	45.174234
3501.885900	519066.211851	45.179239
3501.806774	519055.640405	45.184244
3501.476533	519021.974978	45.189249
3501.723518	519017.148622	45.194253
3501.925523	519000.183128	45.199258
3501.627742	518979.263466	45.204263
3501.984298	518962.979461	45.209268
3502.195515	518951.153176	45.214273
3501.869681	518930.489800	45.219277
3501.933899	518899.383444	45.224282
3502.142534	518897.082977	45.229287
3502.426524	518863.623972	45.234292
3502.068170	518848.660667	45.239297
3501.867212	518819.964169	45.244301
3502.059114	518804.007995	45.249306
3501.815306	518782.474835	45.254311
3501.893306	518762.201959	45.259316
3501.949568	518747.879620	45.264321
3501.849683	518737.815157	45.269325
3501.971007	518717.283473	45.274330
3501.922792	518698.995742	45.279335
3502.023063	518677.812074	45.284340
3501.797142	518661.517551	45.289345
3501.967231	518637.702146	45.294349
3502.129160	518619.734410	45.299354
3501.761854	518602.605012	45.304359
3501.886019	518589.481549	45.309364
3501.831383	518573.563470	45.314369
3501.667823	518550.354238	45.319373
3501.860087	518515.346234	45.324378
3501.683684	518516.079263	45.329383
3501.726401	518505.286827	45.334388
3501.622331	518489.628346	45.339393
3501.556090	518473.359150	45.344397
3501.620341	518459.640075	45.349402
3501.389633	518438.961149	45.354407
3501.722440	518424.797041	45.359412
3501.510484	518422.461143	45.364417
3501.581403	518399.769579	45.369421
3501.628008	518384.692344	45.374426
3501.387261	518383.217740	45.379431
3501.813971	518364.502848	45.384436
3501.539563	518353.558035	45.389441
3501.506459	518337.333921	45.394445
3501.778761	518316.778140	45.399450
3501.435980	518306.448746	45.404455
3501.513879	518300.338011	45.409460
3501.486504	518290.110729	45.414465
3501.389431	518262.203315	45.419469
3501.378109	518250.411053	45.424474
3501.670318	518253.742464	45.429479
3501.485690	518225.546189	45.434484
3501.775285	518207.054026	45.439489
3501.687199	518210.041411	45.444493
3501.854230	518177.506158	45.449498
3501.556894	518171.403354	45.454503
3501.658952	518151.881857	45.459508
3501.520156	518141.974214	45.464513
3501.253899	518126.945380	45.469517
3501.822735	518117.179614	45.474522
3501.776428	518108.164793	45.479527
3501.449441	518081.956062	45.484532
3501.752161	518075.608632	45.489537
3501.778332	518049.042467	45.494541
3501.975090	518036.461604	45.499546
3501.776514	518026.563180	45.504551
3501.739553	518006.710291	45.509556
3501.763012	517995.164410	45.514561
3501.683768	517974.360404	45.519565
3501.960198	517953.400213	45.524570
3501.771239	517942.592981	45.529575
3501.951209	517926.940056	45.534580
3501.518480	517918.489271	45.539585
3501.923842	517900.583514	45.544589
3502.121788	517880.391470	45.549594
3501.734526	517867.397301	45.554599
3502.011776	517837.817871	45.559604
3501.919605	517823.668871	45.564609
3501.247305	517799.579865	45.569613
3501.748868	517789.975546	45.574618
3501.927607	517782.891223	45.579623
3501.715931	517746.835233	45.584628
3501.851950	517752.761653	45.589633
3501.387074	517731.815672	45.594637
3501.800543	517710.783382	45.599642
3501.690881	517703.693493	45.604647
3501.783344	517676.309829	45.609652
3502.024057	517662.209668	45.614657
3501.715912	517644.565818	45.619661
3501.803428	517623.584116	45.624666
3501.466554	517616.277519	45.629671
3501.549461	517599.278415	45.634676
3501.391254	517580.199836	45.639681
3501.464583	517582.355772	45.644685
3501.661283	517569.018427	45.649690
3501.469849	517545.711015	45.654695
3501.561218	517536.220754	45.659700
3501.725610	517526.416698	45.664705
3501.711901	517506.307442	45.669709
3502.096632	517483.414310	45.674714
3501.864601	517472.361386	45.679719
3501.741581	517447.480619	45.684724
3501.454777	517442.131918	45.689729
3501.876586	517423.618123	45.694733
3502.018392	517405.752733	45.699738
3501.682940	517391.237903	45.704743
3501.791218	517369.748533	45.709748
3501.789374	517364.305053	45.714753
3501.905129	517340.949490	45.719757
3501.965950	517325.364825	45.724762
3501.494238	517314.601095	45.729767
3501.543038	517292.515997	45.734772
3501.790551	517286.630442	45.739777
3501.745539	517273.280017	45.744781
3501.998714	517243.854267	45.749786
3501.692243	517235.080976	45.754791
3501.938283	517208.579776	45.759796
3501.876945	517189.485577	45.764801
3501.328546	517176.767853	45.769805
3501.904854	517161.657248	45.774810
3501.271114	517138.115535	45.779815
3501.555925	517065.486643	45.784820
3501.791747	516954.707343	45.789825
3501.599024	516804.827635	45.794829
3501.381065	516595.469151	45.799834
3500.696437	516345.601141	45.804839
3500.695032	516039.969927	45.809844
3500.279163	515695.882400	45.814849
3499.890869	515295.773749	45.819853
3499.602977	514857.171919	45.824858
3498.842923	514370.734586	45.829863
3498.131096	513828.863480	45.834868
3497.171634	513248.236792	45.839873
3496.643819	512623.701775	45.844877
3495.658427	511946.617065	45.849882
3494.884044	511255.901757	45.854887
3494.165556	510501.400371	45.859892
3493.458216	509704.543638	45.864897
3492.012867	508868.921136	45.869901
3490.897629	507976.050563	45.874906
3489.814510	507065.211733	45.879911
3488.789074	506089.634364	45.884916
3487.758338	505089.775506	45.889921
3486.161224	504049.118662	45.894925
3485.237348	502959.490185	45.899930
3483.888567	501834.069053	45.904935
3482.610335	500653.088962	45.909940
3481.282888	499447.543349	45.914945
3479.457579	498196.852897	45.919949
3478.044205	496906.720377	45.924954
3476.663569	495581.687930	45.929959
3474.951881	494219.935406	45.934964
3473.031410	492823.857943	45.939969
3471.054036	491389.837780	45.944973
3469.740429	489922.196798	45.949978
3467.700813	488424.324234	45.954983
3465.706807	486885.029997	45.959988
3464.053194	485311.480527	45.964993
3461.994017	483715.958145	45.969997
3460.191711	482083.094943	45.975002
3458.108889	480412.862919	45.980007
3455.908453	478714.474402	45.985012
3453.582969	477001.063959	45.990017
3451.462139	475244.825602	45.995021
3449.626767	473453.367806	46.000026
3446.982866	471648.641903	46.005031
3444.431793	469797.940571	46.010036
3442.121071	467937.688818	46.015041
3439.629589	466042.156434	46.020045
3437.717977	464126.187269	46.025050
3435.192642	462188.646638	46.030055
3432.547965	460215.133888	46.035060
3429.843213	458225.818799	46.040065
3427.433703	456210.470849	46.045069
3424.771034	454164.259117	46.050074
3422.299920	452112.718418	46.055079
3419.672144	450040.564383	46.060084
3416.800431	447931.351134	46.065089
3414.224599	445814.859009	46.070093
3411.490954	443663.508398	46.075098
3408.610935	441498.914235	46.080103
3405.876442	439307.656665	46.085108
3403.260280	437105.741556	46.090113
3400.372369	434898.903111	46.095117
3397.694155	432639.082375	46.100122
3394.782624	430381.215504	46.105127
3391.726321	428085.151932	46.110132
3389.016003	425800.124748	46.115137
3385.803932	423477.555904	46.120141
3382.864880	421146.264672	46.125146
3379.845614	418795.049710	46.130151
3376.750512	416429.992228	46.135156
3374.018803	414044.581561	46.140161
3370.598109	411644.811198	46.145165
3367.502820	409237.015162	46.150170
3364.309852	406814.614124	46.155175
3360.921090	404372.446806	46.160180
3358.050874	401917.807985	46.165185
3354.729653	399458.613002	46.170189
3351.506510	396979.552167	46.175194
3348.072238	394491.381619	46.180199
3344.901905	391988.139643	46.185204
3341.447747	389477.348704	46.190209
3338.038367	386968.733702	46.195213
3334.835872	384435.334727	46.200218
3331.509171	381902.085134	46.205223
3328.110594	379348.893090	46.210228
3324.757524	376783.332658	46.215233
3321.155188	374217.032925	46.220237
3318.001337	371632.590097	46.225242
3314.024740	369042.954572	46.230247
3310.529262	366449.222102	46.235252
3307.327931	363847.003780	46.240257
3303.558002	361245.635085	46.245261
3300.146095	358634.404191	46.250266
3296.546256	356015.761665	46.255271
3292.952169	353381.469849	46.260276
3289.406363	350762.383073	46.265281
3285.911321	348125.638008	46.270285
3282.252566	345486.243308	46.275290
3278.209218	342844.161004	46.280295
3274.846393	340191.982247	46.285300
3271.329840	337540.723321	46.290305
3267.413334	334887.909597	46.295309
3263.751056	332232.273601	46.300314
3259.951894	329564.825220	46.305319
3256.394760	326903.237461	46.310324
3252.661136	324234.124156	46.315329
3248.616898	321565.243295	46.320333
3245.066662	318893.141495	46.325338
3241.472114	316232.333150	46.330343
3237.671257	313549.618927	46.335348
3234.360393	310882.068706	46.340353
3229.643255	308202.882844	46.345357
3226.273527	305527.185102	46.350362
3222.234689	302852.698629	46.355367
3218.407803	300190.999030	46.360372
3214.892878	297517.998730	46.365377
3210.963238	294841.882871	46.370381
3207.198470	292167.274768	46.375386
3202.998410	289500.280433	46.380391
3198.795691	286831.037049	46.385396
3195.360294	284170.834572	46.390401
3191.279160	281521.095172	46.395405
3187.362981	278845.672117	46.400410
3183.350279	276196.319642	46.405415
3179.427891	273549.489020	46.410420
3175.451717	270906.837075	46.415425
3171.557589	268264.069713	46.420429
3167.658523	265617.487221	46.425434
3163.436408	262993.728537	46.430439
3159.373754	260364.814687	46.435444
3155.364491	257733.873106	46.440449
3151.242925	255115.322414	46.445453
3147.361918	252498.314886	46.450458
3143.185102	249896.741710	46.455463
3139.034631	247301.083856	46.460468
3134.752541	244722.525402	46.465473
3130.789416	242146.254976	46.470477
3127.041748	239564.193969	46.475482
3122.901195	236998.496968	46.480487
3118.689408	234440.586375	46.485492
3114.510800	231898.421961	46.490497
3110.366367	229357.821560	46.495501
3106.353492	226822.492523	46.500506
3102.156957	224300.434260	46.505511
3098.194493	221792.757259	46.510516
3094.279910	219288.797323	46.515521
3089.687235	216793.790461	46.520525
3086.023410	214304.994353	46.525530
3081.342349	211833.259437	46.530535
3077.119926	209371.533863	46.535540
3073.187822	206908.233802	46.540545
3068.512001	204475.638594	46.545549
3064.340612	202047.554296	46.550554
3059.883534	199629.760844	46.555559
3055.428433	197240.501456	46.560564
3051.652825	194855.378010	46.565569
3046.663585	192487.166364	46.570573
3042.533378	190129.485599	46.575578
3038.192627	187800.686450	46.580583
3033.728023	185479.697955	46.585588
3028.775018	183177.757834	46.590593
3024.365762	180897.202487	46.595597
3019.658057	178632.588095	46.600602
3014.873711	176405.842313	46.605607
3010.252345	174183.204743	46.610612
3005.912214	171991.761585	46.615617
3000.899470	169824.252543	46.620621
2996.313671	167674.053179	46.625626
2991.203922	165557.656249	46.630631
2985.773510	163462.657247	46.635636
2981.342014	161404.952109	46.640641
2975.767314	159384.363637	46.645645
2970.626189	157389.508550	46.650650
2964.736045	155436.033396	46.655655
2959.402665	153522.841854	46.660660
2953.474683	151563.230516	46.665665
2946.822818	149761.954482	46.670669
2940.726170	147991.854446	46.675674
2934.456566	146297.629328	46.680679
2926.838390	144663.270544	46.685684
2920.050448	143079.680318	46.690689
2912.967322	141595.646426	46.695693
2906.320793	140141.603877	46.700698
2899.313710	138757.865916	46.705703
2893.108442	137436.180148	46.710708
2887.212892	136170.219243	46.715713
2881.593117	134978.252734	46.720717
2876.031227	133810.848371	46.725722
2870.655327	132720.433579	46.730727
2865.586558	131658.568921	46.735732
2860.232188	130636.996772	46.740737
2855.330464	129651.096714	46.745741
2851.076220	128702.337134	46.750746
2846.175415	127788.118798	46.755751
2841.777940	126900.234805	46.760756
2837.620323	126043.990318	46.765761
2833.087821	125217.952923	46.770765
2828.905643	124407.750583	46.775770
2825.214631	123622.848399	46.780775
2821.034136	122853.973538	46.785780
2817.264873	122098.123512	46.790785
2812.912409	121370.204801	46.795789
2809.286805	120634.187363	46.800794
2805.517992	119943.110230	46.805799
2801.432216	119247.300574	46.810804
2797.932591	118564.841133	46.815809
2793.427269	117908.021433	46.820813
2789.741682	117242.336857	46.825818
2786.089102	116597.691169	46.830823
2782.161903	115973.177540	46.835828
2778.039611	115343.605858	46.840833
2774.423587	114732.327080	46.845837
2770.715800	114128.307678	46.850842
2766.583440	113553.265362	46.855847
2762.615841	112979.083841	46.860852
2758.904380	112402.862705	46.865857
2754.976854	111838.356183	46.870861
2751.394881	111278.038611	46.875866
2747.482716	110731.779282	46.880871
2743.939449	110199.468796	46.885876
2740.330712	109662.688670	46.890881
2736.864638	109133.522571	46.895885
2733.352317	108604.880223	46.900890
2730.107401	108086.311113	46.905895
2726.346116	107569.317532	46.910900
2723.052642	107049.932517	46.915905
2719.612908	106534.747799	46.920909
2716.348343	106012.513759	46.925914
2713.104030	105495.064307	46.930919
2709.521707	104971.789809	46.935924
2706.053100	104454.035297	46.940929
2702.746428	103937.433030	46.945933
2699.500777	103410.101001	46.950938
2696.077424	102901.235956	46.955943
2692.635549	102374.815274	46.960948
2689.833997	101861.293596	46.965953
2686.171308	101324.170919	46.970957
2682.896629	100788.585465	46.975962
2679.447799	100269.609756	46.980967
2676.326632	99734.716847	46.985972
2673.087005	99201.465357	46.990977
2669.702666	98671.994501	46.995981
2665.858481	98126.908172	47.000986
2662.192996	97592.834717	47.005991
2658.643055	97053.630663	47.010996
2655.590131	96502.806447	47.016001
2652.178746	95969.000500	47.021005
2648.733543	95429.134464	47.026010
2645.335666	94890.274329	47.031015
2641.531888	94336.580679	47.036020
2638.723867	93787.176863	47.041025
2635.162195	93243.669181	47.046029
2631.983989	92687.137679	47.051034
2628.278138	92138.729067	47.056039
2624.818484	91583.494073	47.061044
2621.320650	91030.066780	47.066049
2617.897940	90480.221047	47.071053
2614.713201	89912.166394	47.076058
2610.959501	89349.865030	47.081063
2607.731871	88800.972728	47.086068
2604.441358	88237.298984	47.091073
2600.914576	87678.284610	47.096077
2597.250013	87103.231030	47.101082
2593.671115	86541.057581	47.106087
2590.243224	85976.546623	47.111092
2586.873377	85401.125018	47.116097
2583.276510	84832.749852	47.121101
2579.629729	84268.839826	47.126106
2576.769243	83705.593405	47.131111
2572.852026	83125.462650	47.136116
2569.661882	82550.679967	47.141121
2566.248699	81982.815588	47.146125
2562.827536	81401.525112	47.151130
2559.148545	80818.635545	47.156135
2555.762559	80242.774551	47.161140
2552.237987	79655.147553	47.166145
2548.948301	79070.100131	47.171149
2545.457278	78491.154648	47.176154
2542.123672	77906.519733	47.181159
2538.490283	77327.862201	47.186164
2535.054999	76740.258057	47.191169
2531.272760	76161.864318	47.196173
2528.094607	75561.076140	47.201178
2524.411679	74977.028355	47.206183
2520.808812	74395.304669	47.211188
2517.469851	73789.730120	47.216193
2514.057828	73212.802488	47.221197
2510.729596	72614.656047	47.226202
2507.238398	72022.757630	47.231207
2503.744162	71427.520856	47.236212
2500.547561	70825.102782	47.241217
2496.978141	70232.095083	47.246221
2493.327758	69628.023068	47.251226
2489.962100	69031.290944	47.256231
2486.152424	68433.689486	47.261236
2482.690396	67823.434682	47.266241
2479.500911	67228.786258	47.271245
2476.037048	66633.737335	47.276250
2472.452097	66029.358789	47.281255
2468.928304	65434.258398	47.286260
2465.638716	64827.285595	47.291265
2462.494969	64225.490145	47.296269
2458.810644	63613.022804	47.301274
2455.358400	62994.219486	47.306279
2451.688304	62392.626230	47.311284
2447.955055	61770.425607	47.316289
2444.441925	61173.597258	47.321293
2440.984662	60555.832962	47.326298
2437.832323	59952.993857	47.331303
2434.167945	59338.497146	47.336308
2430.791989	58723.774349	47.341313
2427.359834	58110.966787	47.346317
2423.936027	57491.136667	47.351322
2420.613033	56878.007147	47.356327
2416.853156	56253.515182	47.361332
2413.596174	55630.496688	47.366337
2409.939389	55022.174483	47.371341
2406.449267	54396.414003	47.376346
2403.070967	53777.003217	47.381351
2399.476220	53159.088846	47.386356
2396.219781	52530.410651	47.391361
2392.541154	51911.825391	47.396365
2389.217039	51289.515811	47.401370
2385.612668	50656.704875	47.406375
2381.988029	50038.554440	47.411380
2378.830963	49406.038030	47.416385
2375.323842	48790.757197	47.421389
2371.837841	48145.082975	47.426394
2368.475152	47523.934178	47.431399
2365.161692	46892.044519	47.436404
2361.514326	46253.825277	47.441409
2357.801827	45619.838944	47.446413
2354.381072	44984.835790	47.451418
2350.921229	44355.729034	47.456423
2347.346567	43723.125734	47.461428
2343.649835	43082.468047	47.466433
2340.119665	42450.483849	47.471437
2336.684784	41812.320592	47.476442
2333.239349	41179.357823	47.481447
2329.612644	40540.988732	47.486452
2326.432645	39912.402590	47.491457
2322.734999	39281.366438	47.496461
2319.445218	38636.755766	47.501466
2315.986099	37998.441659	47.506471
2312.202727	37367.183123	47.511476
2309.099374	36724.210934	47.516481
2305.573540	36083.612263	47.521485
2302.125171	35443.838522	47.526490
2298.693890	34800.366862	47.531495
2294.748824	34161.621900	47.536500
2291.217291	33516.512537	47.541505
2287.487446	32885.429594	47.546509
2283.857782	32253.088807	47.551514
2280.657010	31608.734601	47.556519
2276.887159	30985.719985	47.561524
2273.561760	30343.389085	47.566529
2269.788800	29708.251847	47.571533
2266.242948	29064.157270	47.576538
2262.614947	28446.247877	47.581543
2258.639582	27814.198061	47.586548
2255.706273	27184.476880	47.591553
2251.790411	26559.401514	47.596557
2248.157000	25944.223768	47.601562
2244.396393	25321.842633	47.606567
2240.568415	24719.087509	47.611572
2236.847397	24105.373418	47.616577
2232.505858	23500.042294	47.621581
2228.441054	22922.085868	47.626586
2224.445291	22337.084705	47.631591
2220.122487	21780.221000	47.636596
2215.770420	21212.323691	47.641601
2211.694793	20679.276935	47.646605
2207.760894	20127.245213	47.651610
2203.833680	19594.939565	47.656615
2199.798693	19090.312606	47.661620
2196.246346	18558.990273	47.666625
2192.531642	18065.715373	47.671629
2188.568337	17560.743248	47.676634
2184.525169	17062.737945	47.681639
2180.755859	16577.334178	47.686644
2177.300431	16101.564153	47.691649
2173.715927	15623.720348	47.696653
2170.077145	15142.375971	47.701658
2166.652979	14679.418719	47.706663
2163.216683	14223.519261	47.711668
2159.273375	13757.331239	47.716673
2155.628951	13303.427024	47.721677
2152.462158	12851.665988	47.726682
2149.212945	12385.530310	47.731687
2145.529694	11935.172717	47.736692
2141.797642	11480.775073	47.741697
2138.336217	11043.997766	47.746701
2134.746035	10586.370762	47.751706
2131.571321	10139.902358	47.756711
2127.797570	9704.493265	47.761716
2124.487984	9259.057697	47.766721
2120.806017	8828.754126	47.771725
2117.445931	8387.990711	47.776730
2113.642867	7936.852435	47.781735
2110.171438	7501.201114	47.786740
2106.698952	7061.730673	47.791745
2103.111943	6637.945134	47.796749
2099.877534	6205.417649	47.801754
2096.237798	5766.963150	47.806759
2092.594232	5352.764077	47.811764
2089.281274	4919.649453	47.816769
2085.457016	4492.121424	47.821773
2081.717917	4071.956968	47.826778
2078.450653	3650.456742	47.831783
2074.681320	3228.256557	47.836788
2071.098211	2809.147662	47.841793
2067.202823	2402.516310	47.846797
2063.107032	1998.529353	47.851802
2059.277395	1600.565933	47.856807
2055.212609	1220.628498	47.861812
2051.101684	838.763704	47.866817
2045.721562	513.527661	47.871821
2039.505884	217.239791	47.876826
2029.440893	50.869134	47.881831
2013.864670	105.912253	47.886836
2004.609599	103.726994	47.891841
2000.152434	112.152787	47.896845
1997.660682	109.120571	47.901850
1996.981121	107.483090	47.906855
1995.726582	103.644561	47.911860
1994.462097	105.429515	47.916865
1992.051855	110.904520	47.921869
1989.123782	111.635440	47.926874
1986.079069	104.225271	47.931879
1982.804691	98.774392	47.936884
1979.575946	99.969718	47.941889
1976.163325	101.585963	47.946893
1972.729846	101.319877	47.951898
1969.848928	96.563894	47.956903
1966.144838	105.435624	47.961908
1963.240705	87.136204	47.966913
1959.815012	99.416220	47.971917
1956.501162	104.057431	47.976922
1953.571965	92.880283	47.981927
1949.793741	100.004520	47.986932
1946.653462	102.695175	47.991937
1943.007219	94.049872	47.996941
1939.542921	102.849480	48.001946
1936.025537	98.081826	48.006951
1932.801866	100.949974	48.011956
1929.936186	93.205073	48.016961
1925.853907	97.921585	48.021965
1921.990899	100.383042	48.026970
1919.298313	90.279542	48.031975
1915.861513	99.812015	48.036980
1912.340000	92.846223	48.041985
1909.507732	91.521639	48.046989
1906.293318	97.457153	48.051994
1902.173661	98.680412	48.056999
1898.908237	100.004837	48.062004
1895.807375	90.274928	48.067009
1891.913766	98.372566	48.072013
1888.270950	105.542171	48.077018
1884.668398	95.469567	48.082023
1881.076811	103.387326	48.087028
1877.955498	91.831972	48.092033
1874.438133	96.878177	48.097037
1871.621977	97.231022	48.102042
1868.086042	97.240315	48.107047
1864.416299	99.833046	48.112052
1861.229098	99.440055	48.117057
1857.498774	94.541040	48.122061
1854.145581	102.380568	48.127066
1850.790557	93.661482	48.132071
1847.342907	99.892724	48.137076
1843.710702	97.338573	48.142081
1840.085295	96.020377	48.147085
1836.201045	91.363619	48.152090
1833.259114	88.698874	48.157095
1829.563174	85.227678	48.162100
1826.331351	86.917032	48.167105
1822.675564	96.363365	48.172109
1818.928246	91.802354	48.177114
1815.644771	98.526894	48.182119
1812.149713	99.542219	48.187124
1808.962927	89.968065	48.192129
1805.911091	96.855866	48.197133
1802.277619	96.981584	48.202138
1798.600401	86.999714	48.207143
1795.247272	95.734562	48.212148
1791.470270	89.694393	48.217153
1788.314519	93.918701	48.222157
1784.194620	100.273554	48.227162
1780.882852	92.038125	48.232167
1777.444633	99.441639	48.237172
1774.226381	104.571008	48.242177
1770.655975	97.268000	48.247181
1767.088358	99.642365	48.252186
1763.768199	93.600698	48.257191
1760.056227	91.369015	48.262196
1757.223715	86.877604	48.267201
1753.387608	92.780169	48.272205
1749.638376	96.701383	48.277210
1746.268932	96.842960	48.282215
1742.697156	93.671983	48.287220
1739.480207	92.081421	48.292225
1735.745292	83.430976	48.297229
1732.330203	93.614955	48.302234
1728.967229	96.074529	48.307239
1725.383458	104.519416	48.312244
1721.810580	90.006697	48.317249
1718.378158	96.409575	48.322253
1714.766674	95.810552	48.327258
1711.568785	90.246567	48.332263
1707.697777	83.784452	48.337268
1704.267691	85.548963	48.342273
1700.612518	94.156817	48.347277
1696.972552	91.929753	48.352282
1694.082817	87.346016	48.357287
1690.775989	95.440916	48.362292
1687.488459	83.629901	48.367297
1683.849911	85.509116	48.372301
1679.884589	96.275438	48.377306
1676.507539	78.021226	48.382311
1672.536076	89.250401	48.387316
1669.101023	89.579364	48.392321
1666.005452	86.916403	48.397325
1662.580353	86.136518	48.402330
1659.017770	88.200062	48.407335
1655.153966	87.441003	48.412340
1652.085183	91.680254	48.417345
1648.563604	85.122634	48.422349
1645.053933	85.115204	48.427354
1641.898735	83.170197	48.432359
1638.076041	93.724497	48.437364
1634.479016	89.472310	48.442369
1631.076600	78.932019	48.447373
1627.512566	98.377214	48.452378
1624.028106	81.063532	48.457383
1620.356622	91.853720	48.462388
1616.653314	83.903884	48.467393
1613.702855	89.387039	48.472397
1610.155978	85.051123	48.477402
1606.978913	87.295109	48.482407
1603.148935	95.129754	48.487412
1599.687338	81.729193	48.492417
1595.867836	86.594647	48.497421
1592.246285	83.184667	48.502426
1588.591254	86.385721	48.507431
1585.738634	85.330083	48.512436
1582.283273	82.071406	48.517441
1579.020606	89.643748	48.522445
1575.233444	78.970364	48.527450
1571.857021	83.187897	48.532455
1568.371467	76.855635	48.537460
1564.508070	80.829429	48.542465
1561.027999	85.806566	48.547469
1557.707438	83.719629	48.552474
1554.148235	81.340810	48.557479
1550.608438	87.782550	48.562484
1547.121242	78.543099	48.567489
1543.471690	82.315934	48.572493
1540.103771	83.523461	48.577498
1536.910867	78.572486	48.582503
1533.173904	84.355225	48.587508
1529.726512	78.583332	48.592513
1526.026456	71.268916	48.597517
1522.335186	76.747153	48.602522
1519.080533	64.570404	48.607527
1515.319165	75.333445	48.612532
1512.135442	76.540778	48.617537
1508.886318	73.060190	48.622541
1505.129865	73.932730	48.627546
1501.875066	80.728737	48.632551
1498.365856	81.331845	48.637556
1494.740894	79.535899	48.642561
1491.069828	83.720204	48.647565
1487.592962	85.200953	48.652570
1484.035267	82.230295	48.657575
1480.741633	83.173168	48.662580
1477.246592	78.607743	48.667585
1473.429893	84.561081	48.672589
1470.152841	81.173427	48.677594
1466.739245	80.290533	48.682599
1463.016468	85.719898	48.687604
1459.587005	83.567665	48.692609
1456.120581	74.293363	48.697613
1452.526757	78.623832	48.702618
1449.355870	85.457401	48.707623
1445.747857	79.118908	48.712628
1442.086554	82.795504	48.717633
1438.499528	78.769577	48.722637
1434.811152	88.505716	48.727642
1431.863580	82.194140	48.732647
1428.041997	91.830794	48.737652
1424.678440	76.440863	48.742657
1421.170550	76.176919	48.747661
1417.769838	77.917898	48.752666
1414.348106	74.764739	48.757671
1410.442969	88.153892	48.762676
1406.744171	81.763096	48.767681
1403.659990	83.622486	48.772685
1400.340090	80.118125	48.777690
1396.761896	80.172004	48.782695
1393.491047	79.345993	48.787700
1389.717045	81.129258	48.792705
1386.185035	77.224487	48.797709
1382.400246	84.884426	48.802714
1379.027339	64.234735	48.807719
1375.664553	75.669717	48.812724
1372.299618	76.841993	48.817729
1368.651079	69.263325	48.822733
1364.777088	86.396613	48.827738
1361.596991	79.842834	48.832743
1358.112934	80.245891	48.837748
1354.733363	83.650856	48.842753
1351.355879	75.659845	48.847757
1347.655786	77.017166	48.852762
1344.341629	78.947156	48.857767
1340.568363	78.053821	48.862772
1337.086592	89.270053	48.867777
1333.647709	79.975665	48.872781
1329.554364	90.179794	48.877786
1326.797648	77.077698	48.882791
1323.060727	82.227702	48.887796
1319.615660	70.245139	48.892801
1316.164827	70.342477	48.897805
1312.628387	73.094828	48.902810
1309.315565	73.059956	48.907815
1305.327847	81.773358	48.912820
1302.399622	77.170352	48.917825
1299.311026	81.086841	48.922829
1294.922805	86.717867	48.927834
1291.536455	78.598534	48.932839
1287.802792	80.248982	48.937844
1284.767853	80.813090	48.942849
1281.272941	67.591798	48.947853
1277.477136	80.467227	48.952858
1273.923310	73.183874	48.957863
1270.334496	85.106452	48.962868
1266.819443	80.746648	48.967873
1263.598820	70.750765	48.972877
1260.054092	78.964952	48.977882
1256.636368	79.984106	48.982887
1252.945948	76.645003	48.987892
1249.669586	73.769789	48.992897
1246.232110	82.729735	48.997901
1242.557974	77.385478	49.002906
1239.401681	78.357613	49.007911
1235.224424	78.621812	49.012916
1232.225835	80.069266	49.017921
1228.735120	71.472655	49.022925
1224.883713	85.394435	49.027930
1221.632134	82.154703	49.032935
1218.423369	76.611466	49.037940
1214.639135	88.950435	49.042945
1211.035313	77.356425	49.047949
1207.093732	88.618920	49.052954
1204.012569	72.368854	49.057959
1200.672357	85.379013	49.062964
1197.273549	78.587224	49.067969
1193.450523	79.191753	49.072973
1190.083537	87.463700	49.077978
1186.371003	73.861853	49.082983
1182.897078	82.413031	49.087988
1179.489046	80.437827	49.092993
1176.473426	67.584871	49.097997
1172.433668	80.393871	49.103002
1168.927434	76.013728	49.108007
1165.293923	80.160573	49.113012
1161.869533	66.662580	49.118017
1158.841221	69.373815	49.123021
1154.849023	70.960116	49.128026
1151.541825	73.872947	49.133031
1148.171820	72.761845	49.138036
1144.453117	84.676168	49.143041
1141.108836	77.613315	49.148045
1137.507628	77.632840	49.153050
1133.916066	81.333405	49.158055
1130.312858	83.023673	49.163060
1127.056594	76.671608	49.168065
1123.811841	68.954204	49.173069
1119.920354	75.216589	49.178074
1116.795569	75.171450	49.183079
1113.112398	72.337430	49.188084
1109.422645	77.628798	49.193089
1105.963245	71.403270	49.198093
1102.394735	74.075211	49.203098
1098.753890	68.561285	49.208103
1095.514596	70.226547	49.213108
1092.088319	68.472490	49.218113
1088.432066	70.446260	49.223117
1084.627887	77.539764	49.228122
1081.359542	67.522871	49.233127
1077.701767	79.823169	49.238132
1074.313773	72.343199	49.243137
1070.938848	76.323252	49.248141
1067.286028	80.384527	49.253146
1064.037018	66.729546	49.258151
1060.648375	73.068683	49.263156
1057.143679	72.076632	49.268161
1053.511133	70.987426	49.273165
1049.692529	73.780557	49.278170
1046.253940	71.927184	49.283175
1043.055161	72.225757	49.288180
1039.493611	75.697034	49.293185
1036.494104	70.561006	49.298189
1032.474582	73.040571	49.303194
1028.660496	72.333959	49.308199
1025.254737	76.616202	49.313204
1021.571375	80.954312	49.318209
1018.693301	69.978192	49.323213
1014.758245	70.078171	49.328218
1011.475818	74.126086	49.333223
1007.575914	75.277267	49.338228
1004.126976	74.023447	49.343233
1001.387174	72.576988	49.348237
997.016560	78.290717	49.353242
994.033925	70.396494	49.358247
990.776345	75.819911	49.363252
987.038836	73.854891	49.368257
983.525411	73.073011	49.373261
979.737516	83.859178	49.378266
975.984963	83.968718	49.383271
973.028957	73.400197	49.388276
969.184834	80.759349	49.393281
965.797143	64.699428	49.398285
962.330785	74.742693	49.403290
958.865962	72.361915	49.408295
955.524231	69.376695	49.413300
951.761498	75.248899	49.418305
948.457155	72.219895	49.423309
944.921293	72.877826	49.428314
941.230370	69.443938	49.433319
937.772730	70.219405	49.438324
934.476531	69.017748	49.443329
930.743676	68.883786	49.448333
927.052270	74.257681	49.453338
923.948688	66.211459	49.458343
920.563076	78.956601	49.463348
916.794024	75.958811	49.468353
913.666540	67.381648	49.473357
909.346969	67.392802	49.478362
906.364011	63.614603	49.483367
903.147965	65.877364	49.488372
899.317781	72.576301	49.493377
895.871379	74.707246	49.498381
892.181091	78.698439	49.503386
888.641995	73.175035	49.508391
885.552424	75.750298	49.513396
882.019176	71.247857	49.518401
878.318407	70.454025	49.523405
874.949966	69.769809	49.528410
871.199673	71.865805	49.533415
867.489579	66.878379	49.538420
863.933319	64.704834	49.543425
860.828995	63.115821	49.548429
857.337480	68.563005	49.553434
853.769138	68.533156	49.558439
850.593692	73.064292	49.563444
846.975805	70.362514	49.568449
843.247599	73.663603	49.573453
839.703695	67.008359	49.578458
836.173110	70.424214	49.583463
832.390775	67.479125	49.588468
829.282759	70.379958	49.593473
826.147299	68.878052	49.598477
822.204229	68.897048	49.603482
818.809092	64.540795	49.608487
815.387234	62.963253	49.613492
811.659377	68.899638	49.618497
808.200210	57.412923	49.623501
804.146690	63.890372	49.628506
801.035554	62.723197	49.633511
798.017193	68.014475	49.638516
794.052984	75.281601	49.643521
790.882974	64.385774	49.648525
787.014807	72.612364	49.653530
783.676845	62.672807	49.658535
780.422382	60.958483	49.663540
776.456666	65.916354	49.668545
773.495478	63.444549	49.673549
769.718041	74.165817	49.678554
766.833465	62.795302	49.683559
763.127282	64.197923	49.688564
758.861180	73.916445	49.693569
755.664931	56.393636	49.698573
752.174162	64.890498	49.703578
748.808950	64.591765	49.708583
745.512857	62.747888	49.713588
741.782998	55.514187	49.718593
738.186157	55.324277	49.723597
734.255745	57.169922	49.728602
730.912690	67.361670	49.733607
727.665439	66.500424	49.738612
724.389871	66.893240	49.743617
720.732106	61.002373	49.748621
716.594473	64.854415	49.753626
713.102112	59.842615	49.758631
710.076422	60.522393	49.763636
706.505508	66.399553	49.768641
703.482810	63.231832	49.773645
699.395598	75.554692	49.778650
695.983676	61.010856	49.783655
692.652332	64.550728	49.788660
688.892283	71.732297	49.793665
685.993675	64.546368	49.798669
682.640262	64.824760	49.803674
678.650179	61.136935	49.808679
675.092157	65.582108	49.813684
671.773687	70.091229	49.818689
668.177711	58.666969	49.823693
664.449488	59.886376	49.828698
661.141418	56.636539	49.833703
657.228498	60.304912	49.838708
653.864035	63.663286	49.843713
650.760114	65.889634	49.848717
647.069741	62.363960	49.853722
643.687515	65.044910	49.858727
640.365327	55.039658	49.863732
636.689658	60.974257	49.868737
633.045145	63.420799	49.873741
629.726762	58.416730	49.878746
625.644847	60.605504	49.883751
622.568023	51.223270	49.888756
618.825913	70.544242	49.893761
616.038546	58.737858	49.898765
612.338830	67.672206	49.903770
608.536732	60.551013	49.908775
604.925908	62.210885	49.913780
601.294387	61.766970	49.918785
598.134790	62.651099	49.923789
594.610755	64.560047	49.928794
591.017738	57.766969	49.933799
587.532456	63.017054	49.938804
583.993476	61.236319	49.943809
580.499671	54.769476	49.948813
576.878420	67.133690	49.953818
573.246942	56.246479	49.958823
570.121438	62.908502	49.963828
566.520562	67.569159	49.968833
563.275603	56.988765	49.973837
559.592476	62.655620	49.978842
555.685778	62.842993	49.983847
552.383858	55.450964	49.988852
548.655746	62.320691	49.993857
545.875257	57.011443	49.998861
542.035635	54.445471	50.003866
538.352089	53.794535	50.008871
535.053206	62.179280	50.013876
531.166867	61.727589	50.018881
528.330843	54.753405	50.023885
524.355230	51.136122	50.028890
521.264134	55.847131	50.033895
517.540921	58.179390	50.038900
513.716806	53.633713	50.043905
510.612869	53.424047	50.048909
507.041881	55.049255	50.053914
503.501936	47.994842	50.058919
499.977396	50.217082	50.063924
496.125569	55.163576	50.068929
492.896709	48.006954	50.073933
489.677085	55.136036	50.078938
486.199687	46.483727	50.083943
482.397681	51.567994	50.088948
478.596897	48.125978	50.093953
475.238164	54.061868	50.098957
471.600888	58.955983	50.103962
468.396838	56.898504	50.108967
465.296451	50.591895	50.113972
461.491276	52.512988	50.118977
458.003752	57.810887	50.123981
454.503651	52.303641	50.128986
451.073289	48.547706	50.133991
447.720386	51.496185	50.138996
443.522100	51.719478	50.144001
440.221762	44.934653	50.149005
436.587580	56.535269	50.154010
433.153425	49.609929	50.159015
429.755756	44.137363	50.164020
426.357668	54.005497	50.169025
423.088519	57.788804	50.174029
419.849519	59.574306	50.179034
416.179897	64.862595	50.184039
412.370705	52.459217	50.189044
408.806729	60.385378	50.194049
405.522721	52.601458	50.199053
401.692251	54.611915	50.204058
398.624227	45.810474	50.209063
394.631725	56.967016	50.214068
390.958127	61.275187	50.219073
387.737701	55.531429	50.224077
384.050435	58.879973	50.229082
380.381161	67.173699	50.234087
377.130749	56.701759	50.239092
373.461917	64.372172	50.244097
370.703872	57.569367	50.249101
366.706238	56.942044	50.254106
363.676992	50.469358	50.259111
359.922298	53.910657	50.264116
356.265787	52.395021	50.269121
352.595803	53.064414	50.274125
349.228910	59.245188	50.279130
345.617303	51.395225	50.284135
342.600876	45.695648	50.289140
339.037302	63.299411	50.294145
335.268824	57.479637	50.299149
331.750606	60.833506	50.304154
328.153649	58.887834	50.309159
324.772107	54.858569	50.314164
321.189789	57.801651	50.319169
317.852357	52.718347	50.324173
314.070837	40.105057	50.329178
311.051991	56.102285	50.334183
307.396658	58.572694	50.339188
303.532475	58.032170	50.344193
300.603618	48.892713	50.349197
296.807898	45.823254	50.354202
293.404518	51.794581	50.359207
290.135761	53.230399	50.364212
285.963250	53.737599	50.369217
282.430990	49.617915	50.374221
279.150858	57.866879	50.379226
275.746460	39.025738	50.384231
272.402761	46.531642	50.389236
268.851069	52.159076	50.394241
265.325889	43.941348	50.399245
261.388143	45.655322	50.404250
257.831496	52.583795	50.409255
254.647401	43.588488	50.414260
251.184431	51.138273	50.419265
247.738873	38.577098	50.424269
244.398385	49.420170	50.429274
240.512488	45.254314	50.434279
237.416125	45.432633	50.439284
233.541097	54.561968	50.444289
230.662356	44.481443	50.449293
226.763206	47.635208	50.454298
223.078642	46.946514	50.459303
219.561203	47.864251	50.464308
216.035173	43.139352	50.469313
212.616558	48.299995	50.474317
208.975357	60.952053	50.479322
205.686391	52.450792	50.484327
202.335159	50.191646	50.489332
198.611198	54.153348	50.494337
195.097725	45.022676	50.499341
191.585191	51.086934	50.504346
187.912337	60.488510	50.509351
184.673922	59.480431	50.514356
180.847331	44.400205	50.519361
177.623140	39.416355	50.524365
174.389315	43.728843	50.529370
170.503537	48.348472	50.534375
167.241276	46.720868	50.539380
163.549036	48.206814	50.544385
160.283679	47.857812	50.549389
156.784377	44.587210	50.554394
152.902035	46.903161	50.559399
149.855179	46.074066	50.564404
145.962855	50.833919	50.569409
142.594926	44.151420	50.574413
138.907070	54.320939	50.579418
135.601885	45.474218	50.584423
132.328493	48.416679	50.589428
128.131540	46.700492	50.594433
124.839236	49.554152	50.599437
121.337730	50.260621	50.604442
117.752131	46.899060	50.609447
114.872448	39.577421	50.614452
111.650528	52.189507	50.619457
107.679876	45.559726	50.624461
104.265976	47.258602	50.629466
100.899760	49.538495	50.634471
97.384360	40.525203	50.639476
93.593744	41.207088	50.644481
89.921002	40.380537	50.649485
86.064471	47.779642	50.654490
82.676563	46.276014	50.659495
79.855092	44.475394	50.664500
75.637041	53.155125	50.669505
72.749857	49.017301	50.674509
69.018119	53.372523	50.679514
65.393096	43.996665	50.684519
62.161201	48.416429	50.689524
58.895631	48.491404	50.694529
55.176699	48.345909	50.699533
51.413487	61.890140	50.704538
47.926420	56.529633	50.709543
44.617771	48.942607	50.714548
40.644492	44.328501	50.719553
37.421045	48.326185	50.724557
33.612913	48.893750	50.729562
30.501705	48.954188	50.734567
27.532114	48.543337	50.739572
23.732567	49.046294	50.744577
20.318016	42.804500	50.749581
16.588925	47.969211	50.754586
12.189548	49.214110	50.759591
9.150448	48.032660	50.764596
5.660291	52.527441	50.769601
2.514159	44.272899	50.774605