Fri Aug 26 14:26:28 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.582109	102.125110	0.000000
0.794001	91.224905	0.005005
0.694192	98.883821	0.010010
0.892521	107.825061	0.015014
0.549263	93.097837	0.020019
0.326058	84.660272	0.025024
0.484953	74.552917	0.030029
-0.187510	69.475513	0.035034
-0.140453	56.364288	0.040038
-0.377561	58.378457	0.045043
-1.125092	53.252636	0.050048
-0.471330	36.832691	0.055053
-1.574202	32.784060	0.060058
-1.641858	27.131627	0.065062
-1.967778	21.231514	0.070067
-2.741161	22.187098	0.075072
-2.574666	10.373390	0.080077
-3.125164	19.560884	0.085082
-3.093072	6.167298	0.090086
-3.541939	0.422371	0.095091
-3.841830	2.247000	0.100096
-3.877704	1.376223	0.105101
-4.827088	1.267752	0.110106
-5.224410	-3.007777	0.115110
-5.313764	-3.610807	0.120115
-5.753424	2.876650	0.125120
-5.228322	-4.139849	0.130125
-5.159053	-6.403181	0.135130
-5.553203	-3.950130	0.140134
-5.749140	-0.923684	0.145139
-6.602827	2.771465	0.150144
-6.854545	2.313932	0.155149
-7.182970	3.583038	0.160154
-7.115950	3.246715	0.165158
-6.592289	5.316430	0.170163
-7.621628	-0.467828	0.175168
-7.866884	3.293936	0.180173
-8.178565	0.858970	0.185178
-8.351645	9.168311	0.190182
-8.306484	2.843446	0.195187
-9.114506	-0.570899	0.200192
-9.043946	-11.417399	0.205197
-9.862510	-6.168044	0.210202
-9.934140	-7.722928	0.215206
-9.748043	-7.334334	0.220211
-10.143820	-1.609821	0.225216
-10.338016	-8.909781	0.230221
-10.973025	-2.265365	0.235226
-11.348754	-7.708475	0.240230
-11.378852	1.938968	0.245235
-11.496812	-7.647523	0.250240
-11.641460	-6.492450	0.255245
-11.402574	0.790998	0.260250
-11.947109	7.959151	0.265254
-12.644329	1.708746	0.270259
-12.775348	4.744067	0.275264
-12.952209	-5.728567	0.280269
-12.878753	5.269449	0.285274
-13.493552	1.932584	0.290278
-13.831173	5.120291	0.295283
-14.232628	-7.560397	0.300288
-14.185753	-6.817944	0.305293
-14.844853	0.687572	0.310298
-14.661090	7.663240	0.315302
-14.658870	-5.760485	0.320307
-14.829952	2.206868	0.325312
-15.502453	-0.330101	0.330317
-15.902349	3.800577	0.335322
-15.883045	-0.514510	0.340326
-16.154194	1.492299	0.345331
-15.957576	3.106749	0.350336
-16.757944	-2.912467	0.355341
-17.324001	5.768095	0.360346
-17.400969	4.824626	0.365350
-17.548037	5.473893	0.370355
-17.856218	16.850864	0.375360
-17.360748	8.190713	0.380365
-18.174167	7.719399	0.385370
-18.483808	2.095160	0.390374
-18.643956	1.696134	0.395379
-18.774693	5.462213	0.400384
-19.261956	3.529132	0.405389
-19.956049	1.574471	0.410394
-20.157900	3.178198	0.415398
-19.680717	1.300592	0.420403
-20.316513	11.295436	0.425408
-20.116766	1.931548	0.430413
-20.212047	2.911262	0.435418
-20.943112	5.499026	0.440422
-21.429465	10.753607	0.445427
-22.229053	13.503895	0.450432
-21.773612	8.826682	0.455437
-22.022498	5.100662	0.460442
-21.928832	4.589354	0.465446
-21.853681	4.261256	0.470451
-22.477482	3.349145	0.475456
-22.668976	0.095064	0.480461
-22.989417	3.232641	0.485466
-23.647410	4.299969	0.490470
-23.863896	7.759871	0.495475
-24.393357	13.340693	0.500480
-24.267665	11.331157	0.505485
-24.530820	9.584637	0.510490
-24.614445	4.396590	0.515494
-24.236009	-0.097794	0.520499
-25.403675	7.464761	0.525504
-25.521690	-6.278752	0.530509
-25.736666	-1.550465	0.535514
-25.897738	7.623844	0.540518
-26.045446	-3.074784	0.545523
-26.511946	8.557776	0.550528
-26.763885	-0.830693	0.555533
-26.913852	5.200386	0.560538
-27.148800	4.031586	0.565542
-27.143401	6.529993	0.570547
-28.019755	-0.379031	0.575552
-28.512603	-6.734017	0.580557
-28.581523	-1.269196	0.585562
-28.686809	-6.833503	0.590566
-28.490867	-2.393815	0.595571
-29.011817	4.185391	0.600576
-28.981226	-9.853330	0.605581
-28.961679	-3.304500	0.610586
-29.775043	1.567573	0.615590
-29.900674	-7.435612	0.620595
-30.583164	3.471300	0.625600
-30.510536	1.327663	0.630605
-30.387861	0.631510	0.635610
-30.610947	0.596612	0.640614
-31.247212	-4.679387	0.645619
-31.977185	-3.550234	0.650624
-32.046917	-1.173004	0.655629
-31.989958	-6.253226	0.660634
-32.222218	3.065037	0.665638
-31.927627	-8.784419	0.670643
-33.048266	-3.070430	0.675648
-32.936771	-8.614707	0.680653
-33.002219	2.974388	0.685658
-33.213357	0.042894	0.690662
-33.776671	-1.593617	0.695667
-34.471534	4.095209	0.700672
-34.755794	-6.180373	0.705677
-34.492256	-2.845830	0.710682
-34.842214	-4.256141	0.715686
-34.564676	0.639063	0.720691
-34.860318	-1.010652	0.725696
-35.221544	-8.376350	0.730701
-35.974073	3.193176	0.735706
-36.396330	5.432313	0.740710
-36.295093	-3.163286	0.745715
-37.069046	-2.935252	0.750720
-36.295885	-0.053365	0.755725
-36.573818	-5.413628	0.760730
-36.861663	3.483034	0.765734
-37.602087	-5.288393	0.770739
-37.603975	-4.070128	0.775744
-37.901481	-2.840637	0.780749
-39.024321	8.631531	0.785754
-39.153151	6.253514	0.790758
-38.840776	-6.484532	0.795763
-39.206908	-2.308494	0.800768
-39.387345	-1.935596	0.805773
-39.420824	-6.296244	0.810778
-39.693760	-2.362499	0.815782
-39.735647	-2.972920	0.820787
-39.898573	-0.135105	0.825792
-40.505966	-4.184941	0.830797
-40.960842	-1.165634	0.835802
-40.800881	0.024268	0.840806
-40.921091	-5.452298	0.845811
-42.040114	-7.793196	0.850816
-42.223493	-10.314573	0.855821
-42.420429	-3.070836	0.860826
-42.857824	2.482993	0.865830
-41.954920	-3.118070	0.870835
-42.173655	8.950459	0.875840
-42.211547	-0.721264	0.880845
-43.351029	5.312026	0.885850
-43.678602	-3.564809	0.890854
-43.658570	-5.700256	0.895859
-43.741918	7.853088	0.900864
-44.155750	2.485510	0.905869
-44.595904	14.851100	0.910874
-45.363456	-0.439543	0.915878
-45.348954	-1.368781	0.920883
-45.522576	10.445961	0.925888
-45.511457	2.788175	0.930893
-45.702870	-0.152716	0.935898
-45.431390	-3.735135	0.940902
-46.050748	-0.313745	0.945907
-46.662739	6.798473	0.950912
-46.606186	5.517850	0.955917
-46.670739	4.831867	0.960922
-47.463332	11.579914	0.965926
-47.561392	5.293167	0.970931
-48.266518	12.546435	0.975936
-48.532223	-1.813141	0.980941
-48.424156	9.761596	0.985946
-48.661872	8.612209	0.990950
-48.350477	6.159322	0.995955
-48.512490	3.542871	1.000960
-49.079126	-2.284951	1.005965
-49.516759	6.774233	1.010970
-49.727487	3.273219	1.015974
-49.650493	4.593094	1.020979
-50.496064	2.083072	1.025984
-50.506042	-2.578618	1.030989
-50.870052	4.036260	1.035994
-51.167111	17.265393	1.040998
-50.992294	1.151003	1.046003
-51.401816	0.262476	1.051008
-52.003344	2.760470	1.056013
-52.777016	-0.871184	1.061018
-52.868865	6.343539	1.066022
-52.933308	-3.770121	1.071027
-53.309518	5.836301	1.076032
-53.184757	0.081155	1.081037
-53.137331	-9.936028	1.086042
-53.484014	-3.478869	1.091046
-53.033973	3.781191	1.096051
-53.249247	3.811513	1.101056
-54.053998	-0.625195	1.106061
-54.323950	7.449297	1.111066
-54.469250	5.260500	1.116070
-55.192079	-2.580390	1.121075
-55.515897	2.705826	1.126080
-55.404496	-5.461097	1.131085
-55.645442	-0.134003	1.136090
-55.795089	3.160473	1.141094
-56.445658	-7.396582	1.146099
-57.075750	5.783158	1.151104
-57.168787	-0.257604	1.156109
-57.120534	-0.578350	1.161114
-56.893668	6.640532	1.166118
-56.717799	-2.593088	1.171123
-57.592307	-3.282671	1.176128
-57.932800	4.733203	1.181133
-58.205637	-6.686230	1.186138
-58.832615	-0.365756	1.191142
-58.833090	2.310728	1.196147
-59.667471	8.774225	1.201152
-59.877142	-0.244349	1.206157
-59.741220	7.868186	1.211162
-60.500999	5.427062	1.216166
-60.133702	-3.918617	1.221171
-60.200412	2.289316	1.226176
-60.046418	2.315925	1.231181
-60.329907	-4.071656	1.236186
-60.986979	-3.732110	1.241190
-61.179222	-9.909277	1.246195
-62.031123	-4.154876	1.251200
-61.851452	-5.366085	1.256205
-61.911914	-1.158549	1.261210
-62.078820	7.105536	1.266214
-62.536533	-10.014470	1.271219
-63.063260	-4.547972	1.276224
-62.723055	1.729477	1.281229
-62.781846	1.308343	1.286234
-63.778096	-0.653052	1.291238
-64.022067	-10.245227	1.296243
-64.554563	11.907230	1.301248
-64.398391	-1.853663	1.306253
-64.905816	3.571868	1.311258
-65.348911	2.849915	1.316262
-64.922738	6.171791	1.321267
-64.989589	-5.542297	1.326272
-65.373268	0.414441	1.331277
-65.631971	-5.837798	1.336282
-66.439871	8.549666	1.341286
-65.985911	-4.726098	1.346291
-66.301643	5.199925	1.351296
-66.672553	-2.809649	1.356301
-67.434639	4.344919	1.361306
-68.182884	11.022788	1.366310
-67.673721	-4.507759	1.371315
-68.244485	10.456531	1.376320
-67.843844	4.645776	1.381325
-67.769805	11.432889	1.386330
-67.983042	-1.359357	1.391334
-68.752771	-1.397725	1.396339
-69.196872	9.763126	1.401344
-69.437310	13.894287	1.406349
-69.213927	4.919013	1.411354
-69.512493	7.297073	1.416358
-69.642037	5.317787	1.421363
-70.161104	5.781374	1.426368
-70.372715	0.451913	1.431373
-71.008502	7.763982	1.436378
-71.587493	4.934054	1.441382
-71.814575	5.491380	1.446387
-71.787600	15.164738	1.451392
-71.645022	9.732673	1.456397
-71.525345	8.768077	1.461402
-72.161010	6.848612	1.466406
-72.591208	1.569002	1.471411
-73.268782	6.587608	1.476416
-73.231519	9.175962	1.481421
-73.216715	6.566781	1.486426
-73.296850	9.220870	1.491430
-73.584988	-1.534981	1.496435
-74.270847	9.350311	1.501440
-75.170454	3.118767	1.506445
-75.303174	6.214461	1.511450
-75.482492	7.628025	1.516454
-74.723818	4.048840	1.521459
-75.023768	7.069336	1.526464
-74.860888	13.073851	1.531469
-75.537273	11.230326	1.536474
-76.239476	4.487172	1.541478
-76.270044	-0.968550	1.546483
-76.490682	10.056271	1.551488
-76.585105	1.238045	1.556493
-77.121086	5.370929	1.561498
-77.804114	8.476379	1.566502
-77.756102	6.058175	1.571507
-78.153053	4.341979	1.576512
-78.239210	4.266780	1.581517
-78.058045	7.531894	1.586522
-77.943935	1.844844	1.591526
-78.594512	-1.476956	1.596531
-78.972901	0.809132	1.601536
-79.326701	1.246987	1.606541
-79.214396	7.306830	1.611546
-80.229355	13.592807	1.616550
-80.589400	4.252808	1.621555
-80.769346	5.005268	1.626560
-80.923554	9.964532	1.631565
-80.881682	-3.734271	1.636570
-80.920692	4.696553	1.641574
-80.665785	-1.392055	1.646579
-81.488070	3.127080	1.651584
-81.767679	3.180074	1.656589
-81.949176	0.826077	1.661594
-82.466555	5.905158	1.666598
-82.389431	0.084667	1.671603
-83.171975	12.301089	1.676608
-83.558754	5.897952	1.681613
-83.624519	8.303039	1.686618
-83.789529	8.528008	1.691622
-83.953963	-1.820010	1.696627
-83.720243	6.618969	1.701632
-83.940358	6.333680	1.706637
-84.301565	-0.668201	1.711642
-84.947443	3.146447	1.716646
-85.006722	0.289384	1.721651
-85.338716	-2.601145	1.726656
-85.851084	-2.170237	1.731661
-86.031714	-4.109931	1.736666
-86.774652	6.875991	1.741670
-86.718771	3.706778	1.746675
-86.762303	3.621777	1.751680
-86.940609	8.173519	1.756685
-87.065680	6.051173	1.761690
-87.065179	12.773808	1.766694
-87.223348	-1.532906	1.771699
-87.980971	5.636785	1.776704
-88.234523	1.136403	1.781709
-88.282917	-0.143697	1.786714
-88.385611	3.950196	1.791718
-88.431204	-0.149147	1.796723
-89.080341	2.501789	1.801728
-89.637643	9.513745	1.806733
-89.770788	5.554579	1.811738
-90.235906	7.449225	1.816742
-90.059187	2.236465	1.821747
-90.155256	6.576092	1.826752
-90.976418	2.720887	1.831757
-91.118093	5.757866	1.836762
-91.904244	-3.009600	1.841766
-91.266974	7.160331	1.846771
-91.431009	8.663261	1.851776
-91.680702	7.588503	1.856781
-91.427633	0.867453	1.861786
-92.360136	5.767568	1.866790
-92.558608	-1.806961	1.871795
-93.041305	2.921882	1.876800
-93.027267	-1.797328	1.881805
-93.582701	11.994026	1.886810
-94.151477	6.644248	1.891814
-94.351514	2.847352	1.896819
-94.296689	6.280828	1.901824
-94.514919	2.037528	1.906829
-94.254113	10.029380	1.911834
-94.902674	5.998610	1.916838
-94.579871	4.562641	1.921843
-95.341389	0.951242	1.926848
-95.936108	4.027123	1.931853
-95.705391	7.306667	1.936858
-96.032093	12.928681	1.941862
-96.254637	7.037792	1.946867
-97.243052	7.742131	1.951872
-97.469255	8.100010	1.956877
-97.183858	-0.334441	1.961882
-97.723924	3.732642	1.966886
-97.657466	11.308681	1.971891
-97.736034	8.277456	1.976896
-97.843648	5.304535	1.981901
-97.749635	-3.682226	1.986906
-98.573065	6.057097	1.991910
-98.807533	2.819201	1.996915
-99.134052	9.894185	2.006912
-99.116014	9.226096	2.016909
-98.580745	10.162687	2.026906
-97.794886	4.588661	2.036902
-97.772778	13.790476	2.046899
-96.942100	5.209664	2.056896
-96.460971	10.231509	2.066893
-95.653789	8.341359	2.076890
-95.286446	2.075418	2.086886
-95.027471	6.701045	2.096883
-94.667784	0.740394	2.106880
-94.074183	4.471313	2.116877
-93.571192	4.807900	2.126874
-92.804918	10.140130	2.136870
-92.620431	8.505319	2.146867
-91.831002	6.773151	2.156864
-91.207952	5.874650	2.166861
-91.129626	4.281711	2.176858
-90.319022	2.242148	2.186854
-89.981395	-1.180912	2.196851
-89.624119	6.489402	2.206848
-88.350655	3.576344	2.216845
-88.005818	3.323024	2.226842
-87.942306	3.056487	2.236838
-87.797984	8.853007	2.246835
-86.974028	2.009140	2.256832
-86.679565	1.082608	2.266829
-85.576571	3.346764	2.276826
-84.927673	4.186472	2.286822
-84.871323	7.738123	2.296819
-85.073871	1.795322	2.306816
-84.193688	2.174548	2.316813
-83.476840	-3.357054	2.326810
-82.900661	3.981413	2.336806
-82.232672	1.824676	2.346803
-81.607707	1.017741	2.356800
-81.453135	7.984712	2.366797
-81.117516	4.105816	2.376794
-80.221913	5.632514	2.386790
-79.752483	8.831588	2.396787
-79.469215	2.870164	2.406784
-78.939604	7.298437	2.416781
-78.397024	1.876327	2.426778
-78.099530	3.277579	2.436774
-77.302518	6.229252	2.446771
-77.293845	8.857024	2.456768
-76.291491	5.140404	2.466765
-75.331265	7.420455	2.476762
-75.330247	-0.375465	2.486758
-75.004187	11.667963	2.496755
-74.022729	11.597446	2.506752
-73.821527	3.158990	2.516749
-73.841177	-5.546005	2.526746
-72.583169	1.002079	2.536742
-72.431464	2.565409	2.546739
-72.281388	-2.048011	2.556736
-71.418775	-2.438968	2.566733
-71.192266	0.490662	2.576730
-70.558003	3.249104	2.586726
-69.410701	5.864312	2.596723
-69.266987	6.260007	2.606720
-68.687616	9.229729	2.616717
-68.393229	6.367747	2.626714
-68.094160	2.934852	2.636710
-67.252329	4.473090	2.646707
-66.818456	7.009317	2.656704
-66.458417	4.951211	2.666701
-65.560266	2.163112	2.676698
-65.729413	7.438255	2.686694
-64.732998	5.857586	2.696691
-64.086236	5.750486	2.706688
-63.937116	7.349064	2.716685
-63.263362	6.449005	2.726682
-62.452641	-2.451803	2.736678
-62.502158	12.757613	2.746675
-62.063544	4.332874	2.756672
-61.150796	1.558341	2.766669
-60.948177	2.321820	2.776666
-60.537797	4.047608	2.786662
-59.710356	-0.310161	2.796659
-59.471075	1.337732	2.806656
-58.916241	4.542515	2.816653
-58.259686	7.192954	2.826650
-57.701005	3.570755	2.836646
-56.927203	6.573558	2.846643
-56.917869	12.384763	2.856640
-56.488990	12.729723	2.866637
-56.067975	12.721125	2.876634
-55.328385	6.739334	2.886630
-54.645232	-1.102609	2.896627
-53.908724	9.384930	2.906624
-53.615953	3.795814	2.916621
-53.694151	4.302085	2.926618
-53.072270	0.413463	2.936614
-52.401414	0.882300	2.946611
-51.521773	2.430490	2.956608
-50.929985	-1.523135	2.966605
-51.019802	-0.514559	2.976602
-50.534496	0.030683	2.986598
-49.770697	-3.496743	2.996595
-49.572843	4.892120	3.006592
-48.670739	2.505703	3.016589
-47.855808	-2.895457	3.026586
-47.800177	-1.314000	3.036582
-47.815699	4.665793	3.046579
-46.911074	4.116247	3.056576
-46.272636	9.839004	3.066573
-45.221300	6.073577	3.076570
-45.080417	1.227177	3.086566
-44.978071	5.037754	3.096563
-44.735748	4.927103	3.106560
-43.563188	5.381179	3.116557
-43.406166	6.867658	3.126554
-42.939637	9.829609	3.136550
-42.438779	6.552188	3.146547
-41.573487	10.725467	3.156544
-40.947256	6.579583	3.166541
-40.695842	0.737155	3.176538
-40.517815	3.972098	3.186534
-39.913332	2.579162	3.196531
-39.165546	9.713525	3.206528
-39.064267	3.653727	3.216525
-37.914904	3.382845	3.226522
-37.678453	3.881306	3.236518
-37.583309	1.943637	3.246515
-36.798009	2.917325	3.256512
-36.151952	12.560506	3.266509
-36.013198	5.550898	3.276506
-35.219614	-1.234390	3.286502
-34.578383	3.914579	3.296499
-34.338022	-4.042148	3.306496
-33.679184	-3.001254	3.316493
-33.427952	7.840600	3.326490
-32.762020	5.855240	3.336486
-31.979138	5.486202	3.346483
-31.749021	4.724906	3.356480
-31.506905	2.488763	3.366477
-30.505021	9.631081	3.376474
-30.200134	0.042445	3.386470
-29.987496	-0.503894	3.396467
-29.139531	3.472517	3.406464
-29.025041	-1.974804	3.416461
-27.675504	7.004498	3.426458
-27.634019	5.144871	3.436454
-27.349471	8.787703	3.446451
-26.975752	5.257655	3.456448
-25.962375	8.552600	3.466445
-25.739175	4.478970	3.476442
-25.495909	-0.899706	3.486438
-24.972380	-0.737370	3.496435
-24.541762	4.425386	3.506432
-23.751611	9.319928	3.516429
-23.398372	13.946723	3.526426
-22.374103	6.004149	3.536422
-22.052925	7.189480	3.546419
-21.941061	1.213562	3.556416
-21.566384	3.939566	3.566413
-20.549812	-1.458146	3.576410
-20.192474	-1.586704	3.586406
-19.402522	6.101777	3.596403
-18.874197	6.358397	3.606400
-18.824622	11.273216	3.616397
-18.570358	4.508542	3.626394
-17.457472	-5.576516	3.636390
-17.458985	-1.233435	3.646387
-17.050351	-1.620227	3.656384
-15.846262	8.620292	3.666381
-15.532611	4.073263	3.676378
-15.358750	5.389232	3.686374
-14.532919	5.070526	3.696371
-14.399878	11.233093	3.706368
-13.783233	4.342308	3.716365
-12.886480	4.414857	3.726362
-12.820000	8.560460	3.736358
-12.436617	1.205499	3.746355
-11.700338	4.325016	3.756352
-11.339361	11.326378	3.766349
-10.483986	-0.210575	3.776346
-10.110946	5.192388	3.786342
-9.870053	4.812706	3.796339
-9.049200	4.843222	3.806336
-8.390523	2.089241	3.816333
-8.329590	9.609306	3.826330
-7.885567	0.908134	3.836326
-7.054881	8.533256	3.846323
-6.772298	3.724978	3.856320
-6.034339	3.100016	3.866317
-5.599339	5.376319	3.876314
-5.317313	2.544771	3.886310
-4.962163	6.635926	3.896307
-4.407991	19.419938	3.906304
-4.091587	18.413965	3.916301
-3.475844	24.548897	3.926298
-2.861516	34.805232	3.936294
-2.627364	43.207472	3.946291
-2.162808	60.183668	3.956288
-1.669009	61.582872	3.966285
-1.125404	75.784536	3.976282
-0.656711	86.855504	3.986278
-0.172103	112.219898	3.996275
0.000000	124.424169	4.001280
0.439227	128.069897	4.006285
0.508184	131.792257	4.011290
0.621895	135.137501	4.016294
0.736328	135.752386	4.021299
1.056399	142.675249	4.026304
1.078872	145.307056	4.031309
1.164872	139.368078	4.036314
1.005776	140.047696	4.041318
0.988373	148.086098	4.046323
1.346967	155.094714	4.051328
1.117499	153.823813	4.056333
1.107351	150.778744	4.061338
1.110112	158.769720	4.066342
1.096088	147.407958	4.071347
1.116504	156.297831	4.076352
1.184583	155.562718	4.081357
0.964443	152.990094	4.086362
1.188787	156.609174	4.091366
1.555888	154.533562	4.096371
1.453689	157.972536	4.101376
1.220326	157.635524	4.106381
1.462993	155.031971	4.111386
1.345526	159.441406	4.116390
1.312198	159.478200	4.121395
1.362608	164.513216	4.126400
1.310753	167.751369	4.131405
1.308521	162.588567	4.136410
1.418761	163.232579	4.141414
1.534956	156.039243	4.146419
1.502846	162.425340	4.151424
1.562596	151.352639	4.156429
1.506507	155.986629	4.161434
1.088812	148.509435	4.166438
1.359241	144.588637	4.171443
1.558042	165.013962	4.176448
1.381455	155.895242	4.181453
1.830446	164.658281	4.186458
1.412988	152.419719	4.191462
1.645301	142.459078	4.196467
1.358054	139.975996	4.201472
1.380808	152.544852	4.206477
1.848496	158.837312	4.211482
1.584470	158.976462	4.216486
1.624939	138.899793	4.221491
1.383260	140.196531	4.226496
1.456630	153.519951	4.231501
1.424196	159.267035	4.236506
1.790162	168.887704	4.241510
1.699395	161.248875	4.246515
1.818335	172.347478	4.251520
1.788089	160.434591	4.256525
1.521474	162.323656	4.261530
1.410577	170.303860	4.266534
1.785919	164.601391	4.271539
1.362976	174.259474	4.276544
1.776584	166.159308	4.281549
1.872009	162.582121	4.286554
2.042674	168.360860	4.291558
1.593821	174.131657	4.296563
2.071251	172.298286	4.301568
2.061742	162.834018	4.306573
1.596890	160.536770	4.311578
1.842715	170.473530	4.316582
1.244942	163.628629	4.321587
1.358102	166.148246	4.326592
2.092470	170.222581	4.331597
2.034163	170.510031	4.336602
1.703605	176.657869	4.341606
1.950630	170.696974	4.346611
1.745645	172.307531	4.351616
1.464807	172.218350	4.356621
1.741471	167.828352	4.361626
1.242435	174.764867	4.366630
1.828508	164.758626	4.371635
1.692717	174.318218	4.376640
1.552043	170.290582	4.381645
2.207261	184.402936	4.386650
1.873237	191.696571	4.391654
2.169064	187.120091	4.396659
2.098835	194.752297	4.401664
2.186029	196.067434	4.406669
2.372994	185.316583	4.411674
1.812601	190.481506	4.416678
1.934926	184.527367	4.421683
2.072172	201.010884	4.426688
2.057609	199.725500	4.431693
2.189587	199.318951	4.436698
1.980440	200.041164	4.441702
2.104781	192.840218	4.446707
1.947740	195.405071	4.451712
2.099707	199.801040	4.456717
2.060366	197.507137	4.461722
2.026835	194.734614	4.466726
1.815807	199.433867	4.471731
2.405373	197.655799	4.476736
2.218549	196.153634	4.481741
2.492564	197.920563	4.486746
1.837833	198.073089	4.491750
2.277236	188.735062	4.496755
2.187138	197.325793	4.501760
2.219613	198.380538	4.506765
2.486952	185.431069	4.511770
1.798797	199.939250	4.516774
2.423274	196.687799	4.521779
2.313390	195.142017	4.526784
2.163746	197.911359	4.531789
2.387357	201.071829	4.536794
1.896681	200.284508	4.541798
2.631691	191.080784	4.546803
2.223326	195.791778	4.551808
2.318308	201.886025	4.556813
2.407756	200.837543	4.561818
1.825907	209.061928	4.566822
2.279961	195.703739	4.571827
2.366775	218.348483	4.576832
2.296342	213.961896	4.581837
2.581891	213.015755	4.586842
2.608544	217.358475	4.591846
2.875107	221.176635	4.596851
2.745316	223.449354	4.601856
2.804565	218.520567	4.606861
3.038345	207.556773	4.611866
2.617441	206.704807	4.616870
2.746978	198.753256	4.621875
2.669434	198.518530	4.626880
2.414792	192.313040	4.631885
2.699821	190.693117	4.636890
2.627631	200.533879	4.641894
2.500777	191.790203	4.646899
2.374384	194.337630	4.651904
2.636885	194.065778	4.656909
2.688399	192.181664	4.661914
2.474662	193.296888	4.666918
2.650214	191.016983	4.671923
2.409340	207.840945	4.676928
2.385183	215.244528	4.681933
2.735506	214.592016	4.686938
2.740346	223.993700	4.691942
2.795097	219.277580	4.696947
2.537747	226.844024	4.701952
2.763046	223.844540	4.706957
3.177661	215.019711	4.711962
2.693433	221.257928	4.716966
2.422519	213.102971	4.721971
2.507292	221.403902	4.726976
2.643864	223.378891	4.731981
2.874277	220.650688	4.736986
2.539234	230.193877	4.741990
2.860225	223.069867	4.746995
2.467317	222.789331	4.752000
2.694814	222.677949	4.757005
2.957784	216.540554	4.762010
3.002787	239.891009	4.767014
2.980824	227.695219	4.772019
2.768632	230.433176	4.777024
2.707757	238.854866	4.782029
3.265514	237.923288	4.787034
3.201233	252.084445	4.792038
2.941806	242.592608	4.797043
2.593788	236.948959	4.802048
3.128432	247.748773	4.807053
2.926540	248.741937	4.812058
2.979978	247.936334	4.817062
3.151549	252.977821	4.822067
2.987094	254.515637	4.827072
2.624177	248.244730	4.832077
3.129380	245.505376	4.837082
2.925181	245.328334	4.842086
3.077235	244.836401	4.847091
3.224189	258.616669	4.852096
3.343396	247.759273	4.857101
3.140858	241.688019	4.862106
2.997467	253.805097	4.867110
3.289281	252.329643	4.872115
3.093398	250.303710	4.877120
3.044286	241.196736	4.882125
3.085866	245.467537	4.887130
2.890089	247.301289	4.892134
3.385072	248.505484	4.897139
3.376143	245.165986	4.902144
3.138871	247.499734	4.907149
3.335503	246.554781	4.912154
3.257767	243.276615	4.917158
3.187903	243.107130	4.922163
3.246284	242.272286	4.927168
3.188082	254.989857	4.932173
3.266622	248.545814	4.937178
3.553116	255.783991	4.942182
3.398348	252.944915	4.947187
3.292923	247.193890	4.952192
3.148550	254.632026	4.957197
3.631059	258.290024	4.962202
3.527290	267.009466	4.967206
3.819223	255.441814	4.972211
3.745242	248.293869	4.977216
3.432087	253.483591	4.982221
3.521814	246.734092	4.987226
3.157214	250.255067	4.992230
3.208598	249.060651	4.997235
3.419597	250.236296	5.002240
3.884776	257.057519	5.007245
3.873569	251.203240	5.012250
3.734949	249.279121	5.017254
3.787457	239.406531	5.022259
3.490876	243.157355	5.027264
3.434967	247.645811	5.032269
3.748112	250.646820	5.037274
3.183475	248.007599	5.042278
3.496559	234.203104	5.047283
3.808748	236.331082	5.052288
3.431074	242.002235	5.057293
3.877178	252.265355	5.062298
3.496239	252.039902	5.067302
3.467321	251.610946	5.072307
4.139776	262.114072	5.077312
3.862431	260.388717	5.082317
3.839086	249.885702	5.087322
3.697836	243.577119	5.092326
3.848255	245.714467	5.097331
3.760923	250.271090	5.102336
3.570697	257.713203	5.107341
3.859031	245.630437	5.112346
4.033676	245.166624	5.117350
3.989549	245.160807	5.122355
3.845662	249.912893	5.127360
3.488986	250.439784	5.132365
3.546545	246.321157	5.137370
3.329794	267.390255	5.142374
3.691846	265.350217	5.147379
4.050921	279.122784	5.152384
3.945242	273.020620	5.157389
3.809519	273.443509	5.162394
3.801448	271.388332	5.167398
4.062937	272.072073	5.172403
4.350303	273.710384	5.177408
3.945364	278.202571	5.182413
4.081269	278.728698	5.187418
3.885578	282.103161	5.192422
4.151155	268.182651	5.197427
4.224209	268.427504	5.202432
4.086755	273.811334	5.207437
4.130098	276.914465	5.212442
4.310961	274.513502	5.217446
4.345045	268.066882	5.222451
3.779333	258.575269	5.227456
3.819554	260.207766	5.232461
3.905851	266.534338	5.237466
3.841667	270.002215	5.242470
3.852807	270.019431	5.247475
3.645163	265.160658	5.252480
3.694250	267.487789	5.257485
4.001959	266.576159	5.262490
4.018745	277.156069	5.267494
3.932440	269.801230	5.272499
4.003428	282.748639	5.277504
4.111255	291.438311	5.282509
4.589199	299.301583	5.287514
4.097256	304.465373	5.292518
4.447621	297.520253	5.297523
4.400763	294.404947	5.302528
3.994313	295.490072	5.307533
4.350129	290.284140	5.312538
4.426056	293.568859	5.317542
4.629151	297.270370	5.322547
4.243657	286.225780	5.327552
3.963655	294.526592	5.332557
4.474659	294.548237	5.337562
4.533335	302.337586	5.342566
4.197518	294.354044	5.347571
4.490844	295.643423	5.352576
4.293630	295.205869	5.357581
4.301301	294.233387	5.362586
4.264660	302.822174	5.367590
4.236758	307.859932	5.372595
4.867909	301.133681	5.377600
4.673481	311.835081	5.382605
4.484192	300.044937	5.387610
4.514548	310.695520	5.392614
4.394068	303.985055	5.397619
4.485257	306.527095	5.402624
4.377421	306.667236	5.407629
4.259302	295.878399	5.412634
4.371511	296.661312	5.417638
4.569090	300.468083	5.422643
4.670468	297.199985	5.427648
4.403630	294.599810	5.432653
4.554413	293.867633	5.437658
4.753652	298.211975	5.442662
4.678526	298.922817	5.447667
4.673894	303.058460	5.452672
4.640834	291.845101	5.457677
4.789369	297.538744	5.462682
4.216652	297.982216	5.467686
4.750343	299.341737	5.472691
4.339457	300.940072	5.477696
4.286278	301.255198	5.482701
4.857951	297.353901	5.487706
4.463544	298.563699	5.492710
4.822433	304.996536	5.497715
4.638828	317.834915	5.502720
4.699373	325.529073	5.507725
4.933742	325.391311	5.512730
4.987506	330.577710	5.517734
4.839991	317.730701	5.522739
4.998121	313.659674	5.527744
4.600257	321.997832	5.532749
5.046371	297.536210	5.537754
4.816648	303.836069	5.542758
4.613137	305.063601	5.547763
4.857679	308.575166	5.552768
4.638658	324.753604	5.557773
5.403006	323.103334	5.562778
5.027250	337.145378	5.567782
5.473232	325.591661	5.572787
4.807777	299.819326	5.577792
4.697309	301.794823	5.582797
4.660493	305.163535	5.587802
5.247423	326.031643	5.592806
4.920308	325.924356	5.597811
5.419970	324.637994	5.602816
4.810330	319.863942	5.607821
4.823572	318.890591	5.612826
4.897335	329.929889	5.617830
5.032345	328.605390	5.622835
5.096678	329.367285	5.627840
4.864638	326.802816	5.632845
5.156416	329.474977	5.637850
5.013072	325.640708	5.642854
4.951673	320.325723	5.647859
5.231670	319.563936	5.652864
4.879579	326.556723	5.657869
4.971622	321.606984	5.662874
4.831719	334.457553	5.667878
4.983139	328.166646	5.672883
4.748426	335.020941	5.677888
5.200171	333.792658	5.682893
5.213928	332.860354	5.687898
5.335300	340.386862	5.692902
4.994324	335.434937	5.697907
5.136207	340.076116	5.702912
5.228011	350.172997	5.707917
5.375611	352.380398	5.712922
5.355698	353.867245	5.717926
5.362480	359.386829	5.722931
5.853493	359.332494	5.727936
5.197293	352.971172	5.732941
5.203492	353.441567	5.737946
5.454869	362.355693	5.742950
5.457080	367.160993	5.747955
5.940089	354.402446	5.752960
5.362497	356.662647	5.757965
5.250415	340.440755	5.762970
5.453043	335.008729	5.767974
5.457469	328.740708	5.772979
5.543083	326.579192	5.777984
5.269953	328.845768	5.782989
5.300964	330.043115	5.787994
5.259798	334.826686	5.792998
5.550349	343.598665	5.798003
5.798270	345.926485	5.803008
5.568460	344.256995	5.808013
5.684402	349.572921	5.813018
5.716102	355.607472	5.818022
5.697318	345.622539	5.823027
5.739553	338.728542	5.828032
5.355583	332.774089	5.833037
5.407458	333.382902	5.838042
5.421018	340.771175	5.843046
5.552079	351.845857	5.848051
5.562128	348.474912	5.853056
5.151793	362.038312	5.858061
5.305581	352.940818	5.863066
5.463365	354.491746	5.868070
5.419013	346.149594	5.873075
5.681828	346.972335	5.878080
5.606731	346.126630	5.883085
5.594689	341.727757	5.888090
5.609939	349.378357	5.893094
5.736054	347.419337	5.898099
5.708096	345.927224	5.903104
5.533257	350.873978	5.908109
5.814939	355.101095	5.913114
6.027835	365.558777	5.918118
6.077053	366.981079	5.923123
6.105065	361.108003	5.928128
5.623006	352.280348	5.933133
5.758181	337.557524	5.938138
5.790766	351.463237	5.943142
6.030828	365.868161	5.948147
5.848022	359.322401	5.953152
5.686222	352.330455	5.958157
6.105172	365.489498	5.963162
6.172062	365.637237	5.968166
5.920910	360.370767	5.973171
5.813329	349.286031	5.978176
5.997503	361.478730	5.983181
6.254674	366.092475	5.988186
5.954949	355.553336	5.993190
5.953060	345.847342	5.998195
6.235392	342.775684	6.003200
5.927494	350.084299	6.008205
5.679799	340.688657	6.013210
6.188585	360.154796	6.018214
5.664146	376.092936	6.023219
6.485203	373.734651	6.028224
6.151916	362.185183	6.033229
5.960151	354.486066	6.038234
5.811530	350.491264	6.043238
5.868860	362.045661	6.048243
5.732836	370.779667	6.053248
5.850034	374.440784	6.058253
6.190235	373.046369	6.063258
6.143197	374.575406	6.068262
6.356624	379.686341	6.073267
6.291276	368.769021	6.078272
5.842862	365.285959	6.083277
5.718435	344.399513	6.088282
5.806428	363.833096	6.093286
5.720012	372.768183	6.098291
6.345096	372.613881	6.103296
5.978234	378.292885	6.108301
6.176947	386.047812	6.113306
6.139518	380.786024	6.118310
6.203358	375.891280	6.123315
6.011844	360.836491	6.128320
5.623427	369.344041	6.133325
6.296349	370.144059	6.138330
6.131189	374.801415	6.143334
6.126500	370.265350	6.148339
5.962683	365.807845	6.153344
5.726127	371.415939	6.158349
6.255485	369.451079	6.163354
5.970634	373.301342	6.168358
6.221042	372.158187	6.173363
6.007811	350.184589	6.178368
6.010766	360.143452	6.183373
5.773058	351.986424	6.188378
5.800668	366.199802	6.193382
6.032006	368.697884	6.198387
6.375067	367.584595	6.203392
6.037451	374.334706	6.208397
5.843588	372.975988	6.213402
6.415378	382.349594	6.218406
6.409162	370.584683	6.223411
6.262904	351.792841	6.228416
5.952288	355.321250	6.233421
5.667971	346.750708	6.238426
5.729508	347.747153	6.243430
5.818044	352.811087	6.248435
6.393637	356.293264	6.253440
5.706979	346.994438	6.258445
5.889681	365.989341	6.263450
6.379199	358.212623	6.268454
6.112428	355.258094	6.273459
5.784694	345.030202	6.278464
5.695369	361.498524	6.283469
6.169108	362.354863	6.288474
6.315119	369.026509	6.293478
6.031499	364.416817	6.298483
6.175525	346.133433	6.303488
6.029254	352.651267	6.308493
6.213974	347.468794	6.313498
6.221899	349.201240	6.318502
5.926144	354.078238	6.323507
5.868406	345.295251	6.328512
6.072075	348.281685	6.333517
6.033408	344.639919	6.338522
5.984376	345.441611	6.343526
6.138446	345.423918	6.348531
6.090651	347.395990	6.353536
5.859785	348.694222	6.358541
6.103058	353.461985	6.363546
5.803645	348.085975	6.368550
6.003339	342.094427	6.373555
5.889761	342.362011	6.378560
5.978912	348.552128	6.383565
5.885225	334.320513	6.388570
5.891645	352.776546	6.393574
6.018907	370.163430	6.398579
6.199913	367.480862	6.403584
5.928021	365.128234	6.408589
6.226191	365.733502	6.413594
5.979034	355.904341	6.418598
5.626574	350.777031	6.423603
6.417516	351.011351	6.428608
6.013450	358.034389	6.433613
6.021502	349.870735	6.438618
6.101061	354.034410	6.443622
5.991937	358.676711	6.448627
5.906404	353.634389	6.453632
5.826659	355.013495	6.458637
6.131453	368.082748	6.463642
6.301909	373.216190	6.468646
5.953020	371.872117	6.473651
6.081570	351.759349	6.478656
5.928027	362.321538	6.483661
5.966541	345.301085	6.488666
6.120883	352.452311	6.493670
6.008635	357.556999	6.498675
5.896364	345.783307	6.503680
5.658687	365.204323	6.508685
6.076382	369.944934	6.513690
6.181740	366.220629	6.518694
6.428237	369.684446	6.523699
6.119005	362.089035	6.528704
5.819484	358.642902	6.533709
5.798864	358.329709	6.538714
6.157711	368.922854	6.543718
6.029086	369.287692	6.548723
6.151389	352.026400	6.553728
6.228955	365.317689	6.558733
6.188376	354.570526	6.563738
6.140889	355.283394	6.568742
6.050272	359.337527	6.573747
6.039329	348.240910	6.578752
5.768689	355.167244	6.583757
5.920883	348.616786	6.588762
5.866257	349.251672	6.593766
5.740806	355.266399	6.598771
6.172004	359.571477	6.603776
6.255364	363.845293	6.608781
6.037162	362.313197	6.613786
5.841359	347.692516	6.618790
5.808824	355.141754	6.623795
6.140225	356.349280	6.628800
5.988692	366.746645	6.633805
6.292132	350.814384	6.638810
5.482856	353.850965	6.643814
5.682196	365.493984	6.648819
6.549182	362.552754	6.653824
6.031604	373.339305	6.658829
6.478370	371.361994	6.663834
6.097713	361.347974	6.668838
5.949738	356.489377	6.673843
6.144935	359.708083	6.678848
5.980990	359.790523	6.683853
6.088794	349.460016	6.688858
6.288097	351.535983	6.693862
6.105882	362.447479	6.698867
6.348836	357.999409	6.703872
6.112525	362.044589	6.708877
5.871822	350.664208	6.713882
6.178293	358.022701	6.718886
6.068862	363.493943	6.723891
6.174405	350.613837	6.728896
6.121255	363.938131	6.733901
6.059918	357.854344	6.738906
5.516907	350.301664	6.743910
5.365668	362.470658	6.748915
5.369899	352.308133	6.753920
5.916055	364.096467	6.758925
6.023333	371.100006	6.763930
6.549170	381.534283	6.768934
6.155852	369.203228	6.773939
5.827349	359.440513	6.778944
5.565686	368.554742	6.783949
6.032823	376.827850	6.788954
6.237539	372.793848	6.793958
6.350207	371.801851	6.798963
6.243919	355.560060	6.803968
5.621660	361.019398	6.808973
5.874406	346.199169	6.813978
6.299030	361.938912	6.818982
6.009015	363.477305	6.823987
6.126949	353.667231	6.828992
5.765342	351.192533	6.833997
5.922943	347.969454	6.839002
6.096018	363.077657	6.844006
5.877880	362.488337	6.849011
6.221334	368.300350	6.854016
5.663910	364.505233	6.859021
6.138823	371.154145	6.864026
6.130273	369.412238	6.869030
6.153493	363.052696	6.874035
6.216810	353.633934	6.879040
6.099183	348.501700	6.884045
6.059344	352.557416	6.889050
6.153504	352.802148	6.894054
6.089924	355.918776	6.899059
6.490373	339.446246	6.904064
5.983038	353.100671	6.909069
5.985342	349.575909	6.914074
6.030963	359.265540	6.919078
5.871066	354.680879	6.924083
6.287581	341.214533	6.929088
5.969717	344.029070	6.934093
6.052022	348.271409	6.939098
6.031975	352.596123	6.944102
6.121673	344.837369	6.949107
6.528560	343.986223	6.954112
6.161413	351.088930	6.959117
5.995625	345.432692	6.964122
6.191521	342.966105	6.969126
5.776666	355.068572	6.974131
6.071868	342.756884	6.979136
6.112156	355.611050	6.984141
6.031288	350.450945	6.989146
6.190181	345.073181	6.994150
6.188630	351.831070	6.999155
6.268123	349.483844	7.004160
6.265662	343.707266	7.009165
5.923463	333.054532	7.014170
5.917035	337.782077	7.019174
5.358208	351.577393	7.024179
5.926618	343.712469	7.029184
5.875398	359.390257	7.034189
5.861451	357.943418	7.039194
6.000149	351.173600	7.044198
5.832723	358.004773	7.049203
5.934065	353.313000	7.054208
5.960047	353.214011	7.059213
6.136862	352.914371	7.064218
6.040319	356.178499	7.069222
5.800262	356.146241	7.074227
6.390215	363.049317	7.079232
6.337403	353.414521	7.084237
6.143440	356.753927	7.089242
6.192436	358.192082	7.094246
6.255135	350.652661	7.099251
6.277830	348.127620	7.104256
5.884116	358.872731	7.109261
6.276924	356.182498	7.114266
6.175352	363.718417	7.119270
6.436930	352.446490	7.124275
5.900341	340.618646	7.129280
5.832728	341.087878	7.134285
5.831678	337.202978	7.139290
6.123555	341.823968	7.144294
6.037815	343.194515	7.149299
6.171327	327.298223	7.154304
5.634892	328.232748	7.159309
6.194395	348.038985	7.164314
6.149194	342.895475	7.169318
5.726732	332.502008	7.174323
6.054103	345.197576	7.179328
6.053036	349.487697	7.184333
6.105670	353.291738	7.189338
6.187972	350.254386	7.194342
5.894307	334.668203	7.199347
5.984353	334.353599	7.204352
6.023517	345.600771	7.209357
6.098858	351.343792	7.214362
5.790442	342.118954	7.219366
6.158399	344.133860	7.224371
6.157401	338.429820	7.229376
6.047920	337.573651	7.234381
5.808839	332.805175	7.239386
5.998987	342.048358	7.244390
6.093696	355.979203	7.249395
5.951753	347.411803	7.254400
5.813381	344.772637	7.259405
6.182868	350.156654	7.264410
6.266169	351.763470	7.269414
6.162547	347.758499	7.274419
6.015696	336.581811	7.279424
5.926276	335.883867	7.284429
5.518570	337.760116	7.289434
5.992483	345.339303	7.294438
6.203900	357.682779	7.299443
6.250671	340.002995	7.304448
5.942567	353.079079	7.309453
6.031112	357.481798	7.314458
6.274279	352.179494	7.319462
6.092928	341.865539	7.324467
6.199116	327.909689	7.329472
5.775742	330.481228	7.334477
5.882856	331.385156	7.339482
5.919738	334.555741	7.344486
6.131223	349.335255	7.349491
5.974558	338.501773	7.354496
5.685259	344.393313	7.359501
6.140733	351.782387	7.364506
6.239863	354.513019	7.369510
5.866713	356.912230	7.374515
6.258478	353.092715	7.379520
6.276994	346.284664	7.384525
5.725354	341.204187	7.389530
6.096711	329.564012	7.394534
5.788097	323.733868	7.399539
6.030071	339.884837	7.404544
6.137718	354.721651	7.409549
6.048883	357.782101	7.414554
5.955744	349.953737	7.419558
6.053716	352.001189	7.424563
5.782022	341.751919	7.429568
6.286006	344.897235	7.434573
6.208045	340.992672	7.439578
6.084067	338.920733	7.444582
5.998021	328.259758	7.449587
5.937868	328.164689	7.454592
5.752239	327.908825	7.459597
5.636061	336.162004	7.464602
6.029733	351.881247	7.469606
5.872160	359.147478	7.474611
6.148434	351.052792	7.479616
6.167316	356.583146	7.484621
6.273405	349.252103	7.489626
6.317106	348.425866	7.494630
5.770929	343.989934	7.499635
6.254182	343.601454	7.504640
5.900630	341.941740	7.509645
5.978224	344.678887	7.514650
5.929369	344.699116	7.519654
5.873264	343.578376	7.524659
5.924842	349.280805	7.529664
6.066321	354.304859	7.534669
6.008271	348.075033	7.539674
6.326679	357.700045	7.544678
6.227373	354.276523	7.549683
5.858913	336.582299	7.554688
5.892923	345.710591	7.559693
6.044291	348.309705	7.564698
6.075481	346.150332	7.569702
5.542433	352.310775	7.574707
5.968643	348.378333	7.579712
6.172321	357.774439	7.584717
5.816067	347.807247	7.589722
6.543172	344.375278	7.594726
6.121804	348.075951	7.599731
6.109358	350.270306	7.604736
6.067283	341.874018	7.609741
5.675702	333.782084	7.614746
5.958867	345.329783	7.619750
5.686582	351.474936	7.624755
5.991185	348.640252	7.629760
6.130702	353.303949	7.634765
6.245857	354.624236	7.639770
6.078334	350.720961	7.644774
5.932799	356.194657	7.649779
6.029911	343.891664	7.654784
5.874162	349.224582	7.659789
5.988945	356.217456	7.664794
5.913267	352.461229	7.669798
6.040678	356.481415	7.674803
6.155931	358.462903	7.679808
6.162334	354.883719	7.684813
6.182698	357.449447	7.689818
6.214215	349.924373	7.694822
6.130101	357.039962	7.699827
6.174702	349.699510	7.704832
6.040229	338.191867	7.709837
5.779040	339.928248	7.714842
5.775290	334.800432	7.719846
5.793732	346.139415	7.724851
6.081625	345.657967	7.729856
5.930266	354.853090	7.734861
5.774217	360.141766	7.739866
5.985608	359.039487	7.744870
5.957290	364.267149	7.749875
6.341170	353.292551	7.754880
6.365304	353.674733	7.759885
5.958285	357.819257	7.764890
5.825751	355.717011	7.769894
5.729640	356.617781	7.774899
6.027953	352.651467	7.779904
6.370686	353.907848	7.784909
6.190398	356.893954	7.789914
6.305838	353.145935	7.794918
6.182082	343.556992	7.799923
6.126014	337.649559	7.804928
5.729226	338.043494	7.809933
5.611368	334.015433	7.814938
6.069579	335.715733	7.819942
5.829306	351.543170	7.824947
5.927014	341.691960	7.829952
5.969742	348.167710	7.834957
5.916661	352.997433	7.839962
6.223768	341.727916	7.844966
5.753168	353.690366	7.849971
6.395172	347.981122	7.854976
5.982027	356.233092	7.859981
6.001479	346.482647	7.864986
5.903995	349.057232	7.869990
6.039619	348.434979	7.874995
6.288425	349.209281	7.880000
6.256360	349.290170	7.885005
6.209808	351.559437	7.890010
6.161052	342.382754	7.895014
5.825346	332.671794	7.900019
5.956586	337.175427	7.905024
5.968904	344.263342	7.910029
5.905123	348.854288	7.915034
6.214868	348.594061	7.920038
6.069059	348.828699	7.925043
6.270533	342.707162	7.930048
5.880752	339.158029	7.935053
5.671953	323.748464	7.940058
6.239538	337.460139	7.945062
6.331068	346.392818	7.950067
5.841440	329.131912	7.955072
5.912168	327.817421	7.960077
5.813745	341.268968	7.965082
5.954493	340.041650	7.970086
6.074519	353.686982	7.975091
5.948475	341.390261	7.980096
6.100289	353.812617	7.985101
5.935411	355.761790	7.990106
5.717143	352.647852	7.995110
5.582012	360.454746	8.000115
6.285507	344.235056	8.005133
6.168182	353.641310	8.010150
5.951775	351.557539	8.015168
6.071121	353.306082	8.020186
6.169615	352.091572	8.025203
6.219192	354.037160	8.030221
6.229881	356.607309	8.035238
5.942554	352.959916	8.040256
6.008184	349.298593	8.045274
6.002155	355.172140	8.050291
5.854079	352.134194	8.055309
5.733413	350.483617	8.060326
5.903520	352.653423	8.065344
6.406556	355.112203	8.070362
5.764475	358.494004	8.075379
5.995678	348.533493	8.080397
6.228532	353.650362	8.085414
6.036381	348.789009	8.090432
6.006565	351.797786	8.095450
5.878139	362.035706	8.100467
5.845526	353.754044	8.105485
6.217069	357.186300	8.110502
6.232483	355.861655	8.115520
6.231270	351.033686	8.120538
5.926442	356.956912	8.125555
6.194947	348.047733	8.130573
6.029080	351.740375	8.135590
5.827996	359.190556	8.140608
6.204308	350.946208	8.145626
6.125007	361.028164	8.150643
6.062980	360.498175	8.155661
6.126911	354.038064	8.160678
6.052679	365.094325	8.165696
6.544974	376.428441	8.170714
6.137079	372.417983	8.175731
5.904087	365.675911	8.180749
6.384986	382.063985	8.185766
5.905244	377.490386	8.190784
6.057925	374.547613	8.195802
6.040232	376.819242	8.200819
6.290774	384.173871	8.205837
6.691286	386.090069	8.210854
6.284686	390.176789	8.215872
6.752367	377.434033	8.220890
5.830464	367.274370	8.225907
5.951684	375.532710	8.230925
6.303332	380.927721	8.235942
6.094726	383.330055	8.240960
6.393690	377.404514	8.245978
6.157087	388.142104	8.250995
6.362112	374.758626	8.256013
6.751697	374.593801	8.261030
5.984438	382.769582	8.266048
6.334372	378.126762	8.271066
6.150325	382.062071	8.276083
6.178298	376.137698	8.281101
6.353082	381.989414	8.286118
6.248313	390.645846	8.291136
6.386567	376.805727	8.296154
6.147223	381.484909	8.301171
5.961198	385.530974	8.306189
6.486923	386.424182	8.311206
6.501941	382.900113	8.316224
6.832085	372.747469	8.321242
6.094256	385.749957	8.326259
6.466824	389.696429	8.331277
6.431036	384.132257	8.336294
6.187732	387.114322	8.341312
6.510959	382.030713	8.346330
6.412670	382.856984	8.351347
6.452301	385.460498	8.356365
6.411833	387.546336	8.361382
6.280859	389.415903	8.366400
6.736422	376.760237	8.371418
6.538968	376.734146	8.376435
6.220464	395.689164	8.381453
6.469298	383.166661	8.386470
6.556379	390.246957	8.391488
6.691255	382.093832	8.396506
6.387051	380.569653	8.401523
6.019590	368.354543	8.406541
6.842497	373.076607	8.411558
6.436316	374.613500	8.416576
6.158023	372.558296	8.421594
6.748235	381.257988	8.426611
6.495495	384.945229	8.431629
6.415624	369.024797	8.436646
6.168304	375.125257	8.441664
6.780489	388.605485	8.446682
6.544377	388.102599	8.451699
6.386648	386.205338	8.456717
6.652421	383.188154	8.461734
6.617301	383.341905	8.466752
6.531704	365.835078	8.471770
6.236866	367.165297	8.476787
6.445164	379.720686	8.481805
6.673785	383.260401	8.486822
6.627779	390.440310	8.491840
6.339059	383.593304	8.496858
6.349383	378.772998	8.501875
6.553956	386.169498	8.506893
6.560185	388.468960	8.511910
6.386169	391.790514	8.516928
6.411348	376.920326	8.521946
6.298483	381.680797	8.526963
6.515658	389.946293	8.531981
6.503013	378.701517	8.536998
6.238875	382.532537	8.542016
6.563307	384.015634	8.547034
6.435993	385.616402	8.552051
6.581794	377.199659	8.557069
6.783456	376.098466	8.562087
6.721271	386.783655	8.567104
6.532634	378.740858	8.572122
6.361462	386.845922	8.577139
6.565940	383.532184	8.582157
6.528668	379.441931	8.587175
6.834626	378.763134	8.592192
6.728429	376.169920	8.597210
6.473884	379.194757	8.602227
6.451021	389.454124	8.607245
6.859364	378.702351	8.612263
6.787874	384.488275	8.617280
6.810046	382.471491	8.622298
6.524660	384.343009	8.627315
6.770973	393.105718	8.632333
6.726700	385.277114	8.637351
6.371846	388.667847	8.642368
6.620727	375.624661	8.647386
6.539470	378.076591	8.652403
6.223513	393.648362	8.657421
6.938688	396.913520	8.662439
7.100682	408.043475	8.667456
6.915719	407.611517	8.672474
7.029100	386.028151	8.677491
6.776849	386.171529	8.682509
6.653025	376.518731	8.687527
6.742579	387.628396	8.692544
6.694833	390.592636	8.697562
6.781529	374.292833	8.702579
6.713178	383.205509	8.707597
6.538030	392.851149	8.712615
6.343633	396.327348	8.717632
6.678031	396.685485	8.722650
7.063361	401.611378	8.727667
6.632584	405.963784	8.732685
7.246576	404.934084	8.737703
6.901890	409.358290	8.742720
6.732814	391.899147	8.747738
6.881151	394.864414	8.752755
6.971054	401.644490	8.757773
6.728000	383.609923	8.762791
6.903087	388.855711	8.767808
6.804572	388.637499	8.772826
7.133327	386.819120	8.777843
6.480247	392.316921	8.782861
6.992073	393.657240	8.787879
6.787253	400.454801	8.792896
7.035512	404.256537	8.797914
6.847253	395.670903	8.802931
6.778057	398.578526	8.807949
7.158182	393.397698	8.812967
6.942297	390.054738	8.817984
6.689572	388.367917	8.823002
6.635143	392.516564	8.828019
6.595422	400.803129	8.833037
6.923000	398.347492	8.838055
6.757971	411.689984	8.843072
6.543991	407.314828	8.848090
7.236695	414.704763	8.853107
6.887106	414.187988	8.858125
6.943581	408.748293	8.863143
6.777743	405.757282	8.868160
6.687737	410.533135	8.873178
6.730532	405.098726	8.878195
6.839091	409.187289	8.883213
6.886127	400.186340	8.888231
6.980819	409.143068	8.893248
6.758279	411.629623	8.898266
6.992958	416.730447	8.903283
6.784648	413.411549	8.908301
6.836762	408.786690	8.913319
7.008323	429.634566	8.918336
6.799326	430.894623	8.923354
7.099183	431.305473	8.928371
7.075070	433.593887	8.933389
7.257898	428.061933	8.938407
7.273792	433.045355	8.943424
7.134529	428.835277	8.948442
6.980166	422.768872	8.953459
6.968520	425.557093	8.958477
7.287355	418.574456	8.963495
7.066782	421.612944	8.968512
6.992232	414.284479	8.973530
7.144521	422.597961	8.978547
7.263009	420.080206	8.983565
7.065758	416.440865	8.988583
7.211759	413.609574	8.993600
6.547062	414.770174	8.998618
7.150239	416.137295	9.003635
6.930283	429.056028	9.008653
7.568102	426.536305	9.013671
7.771922	435.015330	9.018688
7.232013	423.821063	9.023706
6.991301	412.854759	9.028723
6.987529	419.769341	9.033741
7.289436	397.916779	9.038759
6.763503	406.859687	9.043776
6.900702	426.759905	9.048794
7.188036	430.205285	9.053811
7.234338	438.913955	9.058829
7.325003	430.919162	9.063847
7.470382	434.888394	9.068864
7.424832	436.665775	9.073882
7.280757	422.632904	9.078899
7.011507	420.229164	9.083917
7.099128	422.383421	9.088935
7.247296	432.313242	9.093952
7.300767	433.952135	9.098970
7.661904	426.997621	9.103987
7.141795	419.375626	9.109005
7.393433	413.003027	9.114023
6.800151	415.376900	9.119040
7.050091	429.068186	9.124058
7.450727	423.899933	9.129075
7.539909	432.336849	9.134093
7.603175	432.336433	9.139111
7.346608	415.465218	9.144128
7.071509	414.286781	9.149146
7.096957	415.122189	9.154163
6.914384	422.304440	9.159181
6.991374	429.692421	9.164199
7.630248	429.337310	9.169216
7.203587	433.575479	9.174234
7.446455	422.514944	9.179251
7.258151	434.961717	9.184269
7.331175	433.612318	9.189287
7.636844	425.394714	9.194304
7.552881	433.899612	9.199322
7.922867	426.132718	9.204339
7.488257	426.604276	9.209357
7.081426	414.265883	9.214375
7.316781	423.573084	9.219392
7.635984	429.534867	9.224410
7.330453	415.915285	9.229427
7.203419	424.007183	9.234445
7.552367	424.975251	9.239463
7.573763	428.783913	9.244480
7.211991	434.252150	9.249498
7.406616	431.413285	9.254515
7.192473	429.073544	9.259533
7.292227	423.204249	9.264551
7.603025	423.534504	9.269568
6.984227	431.844976	9.274586
7.548102	429.964740	9.279603
7.397443	435.510555	9.284621
6.918228	438.854391	9.289639
7.423010	426.288852	9.294656
7.458687	437.012480	9.299674
7.210923	429.464837	9.304691
7.287823	432.971383	9.309709
7.221465	427.850593	9.314727
7.391416	438.455491	9.319744
7.565562	462.042110	9.324762
7.809520	453.291327	9.329779
7.615832	448.935091	9.334797
7.612931	449.405703	9.339815
7.465534	439.665027	9.344832
7.365100	437.727282	9.349850
7.782587	443.954621	9.354867
7.375707	438.123178	9.359885
7.462652	448.895633	9.364903
7.716348	458.067459	9.369920
7.434543	457.906185	9.374938
7.659852	452.897760	9.379955
7.724784	452.130260	9.384973
7.673390	464.527336	9.389991
7.863274	454.074607	9.395008
7.278950	453.490241	9.400026
7.421358	457.844931	9.405043
7.624696	466.216754	9.410061
7.838504	463.482190	9.415079
7.697416	453.945641	9.420096
7.602872	466.087517	9.425114
7.650756	463.085311	9.430131
7.766093	457.680615	9.435149
7.229115	458.149178	9.440167
7.770159	450.425065	9.445184
7.609261	457.856407	9.450202
7.392627	465.198605	9.455219
7.698488	457.451149	9.460237
7.542664	456.228894	9.465255
7.955604	458.300947	9.470272
7.590595	464.684837	9.475290
7.646908	456.364038	9.480307
7.400088	458.040220	9.485325
7.238359	458.156882	9.490343
7.543452	460.706453	9.495360
7.179058	461.160768	9.500378
7.576051	474.608297	9.505395
7.908304	481.398004	9.510413
8.305303	481.585458	9.515431
8.221436	468.098573	9.520448
7.846961	459.646038	9.525466
7.664840	462.290400	9.530483
8.040068	455.794407	9.535501
7.854130	457.738808	9.540519
7.771954	456.899543	9.545536
7.863197	453.092206	9.550554
7.825026	464.688843	9.555571
8.176861	464.801281	9.560589
7.732586	461.093099	9.565607
8.134495	461.933009	9.570624
7.710184	455.056596	9.575642
7.727710	456.988252	9.580659
8.073899	451.509748	9.585677
7.908415	466.827791	9.590695
7.865973	454.268542	9.595712
7.817219	459.034830	9.600730
7.675949	451.145564	9.605747
8.062130	452.877817	9.610765
7.826492	455.271747	9.615783
7.898580	456.219810	9.620800
7.748904	456.167346	9.625818
8.168888	462.529996	9.630835
8.478470	458.029131	9.635853
8.153978	454.330702	9.640871
8.212373	455.953052	9.645888
8.008839	459.960836	9.650906
7.961552	451.321669	9.655923
8.053759	451.783784	9.660941
7.772024	460.884349	9.665959
8.165717	464.262686	9.670976
8.160602	465.314284	9.675994
8.122335	460.006084	9.681011
8.045418	463.609164	9.686029
8.131437	460.847162	9.691047
8.285677	452.649966	9.696064
7.891696	461.411419	9.701082
8.048581	457.328786	9.706099
8.004480	453.858087	9.711117
7.788083	459.657130	9.716135
8.084911	462.709738	9.721152
7.932495	461.083027	9.726170
7.820948	457.007476	9.731187
8.099782	452.666028	9.736205
7.998035	460.832896	9.741223
7.924035	445.138689	9.746240
7.887018	454.213772	9.751258
8.114632	459.129525	9.756275
8.066515	458.562655	9.761293
7.691069	464.020406	9.766311
8.129224	466.527172	9.771328
8.262061	476.986399	9.776346
8.126680	468.004351	9.781363
7.987283	471.541425	9.786381
8.033632	475.456661	9.791399
8.257954	474.774792	9.796416
8.013106	487.678509	9.801434
7.944482	488.159354	9.806451
8.144762	481.491784	9.811469
8.006317	486.332001	9.816487
8.284085	483.480183	9.821504
8.515973	488.613020	9.826522
8.055956	478.132081	9.831539
8.292962	481.790426	9.836557
8.135165	479.385103	9.841575
8.177990	482.865408	9.846592
8.443095	481.404052	9.851610
7.945432	482.529183	9.856627
8.366160	485.269028	9.861645
8.454330	486.965636	9.866663
8.275255	476.037032	9.871680
8.478768	485.986667	9.876698
8.236855	475.708446	9.881715
8.295121	482.076931	9.886733
8.310304	479.931841	9.891751
8.336121	472.335273	9.896768
8.062748	485.442235	9.901786
8.032711	479.488993	9.906803
8.113459	484.061563	9.911821
7.972115	483.799527	9.916839
8.139767	475.281511	9.921856
8.380614	473.180179	9.926874
8.164514	482.873267	9.931891
8.636095	485.422165	9.936909
8.076720	484.732933	9.941927
8.410808	475.886059	9.946944
8.510455	479.849799	9.951962
8.337996	476.418015	9.956979
8.371016	479.634770	9.961997
8.440523	478.907581	9.967015
8.565282	487.357917	9.972032
8.749282	481.835231	9.977050
8.532422	485.567398	9.982067
8.528798	482.140882	9.987085
8.093412	482.240194	9.992103
8.449271	480.502789	9.997120
8.373427	479.820320	10.002138
8.413957	482.549935	10.007155
8.938508	488.798488	10.012173
8.505759	483.835709	10.017191
8.288498	478.325008	10.022208
8.187163	480.966262	10.027226
8.344626	509.923321	10.032243
8.933305	503.965253	10.037261
8.763387	501.221003	10.042279
8.407827	488.063570	10.047296
8.676428	481.107664	10.052314
8.414469	487.412405	10.057331
8.508267	481.916385	10.062349
8.326939	490.452248	10.067367
8.674821	502.105561	10.072384
8.927465	509.112792	10.077402
8.752741	495.677901	10.082419
8.792880	491.282092	10.087437
8.614025	486.538546	10.092455
8.542086	483.602327	10.097472
8.784362	479.500083	10.102490
8.399326	485.543132	10.107507
8.572508	471.520784	10.112525
8.475460	477.771444	10.117543
8.481949	483.826113	10.122560
8.739100	487.374030	10.127578
8.686324	498.474368	10.132595
9.028320	496.682318	10.137613
8.733213	490.634648	10.142631
8.676661	485.136792	10.147648
8.731765	492.698612	10.152666
8.509809	479.693945	10.157683
8.707908	480.593989	10.162701
8.600292	486.395039	10.167719
8.722056	496.133355	10.172736
8.925665	503.968691	10.177754
8.580870	496.420348	10.182771
9.077636	496.904680	10.187789
8.522474	490.348414	10.192807
8.820793	493.842588	10.197824
8.859612	498.712011	10.202842
8.698487	501.037544	10.207859
8.951144	497.757307	10.212877
8.637832	503.543053	10.217895
8.900008	504.306895	10.222912
9.263173	494.587677	10.227930
8.511508	495.275851	10.232947
8.778252	490.538662	10.237965
8.822320	496.448636	10.242983
8.487514	503.547329	10.248000
9.040888	503.016189	10.253018
8.815113	509.829677	10.258035
9.013461	506.172904	10.263053
9.021752	505.631962	10.268071
8.689926	508.050342	10.273088
8.974531	502.000768	10.278106
8.996391	506.591980	10.283123
9.206170	509.781220	10.288141
8.628760	495.572773	10.293159
8.799128	499.575997	10.298176
9.076731	500.476287	10.303194
8.958439	503.691360	10.308211
9.059959	499.421686	10.313229
9.206626	506.587421	10.318247
9.003791	495.517344	10.323264
8.909180	483.856093	10.328282
8.930136	488.759852	10.333299
9.123935	487.363244	10.338317
9.019914	494.735256	10.343335
9.109936	491.234200	10.348352
9.131254	481.094865	10.353370
8.948675	488.072025	10.358387
9.057928	483.296245	10.363405
8.856255	488.282000	10.368423
8.564964	490.845539	10.373440
9.141515	504.441851	10.378458
8.890260	513.701792	10.383475
8.940937	494.854553	10.388493
9.045687	511.481185	10.393511
9.082035	516.376243	10.398528
9.088916	512.884972	10.403546
8.853228	511.741416	10.408563
9.269875	512.601124	10.413581
9.459519	513.956902	10.418599
8.973454	519.450828	10.423616
9.338907	507.932516	10.428634
9.119970	505.558799	10.433651
8.917159	512.393958	10.438669
9.236103	516.099510	10.443687
8.859065	508.707654	10.448704
9.390764	504.509851	10.453722
9.299885	513.381921	10.458739
8.864109	509.555646	10.463757
9.291582	514.408740	10.468775
9.080933	512.983587	10.473792
9.290703	504.436910	10.478810
8.908138	514.083353	10.483827
8.838286	502.913674	10.488845
9.177315	508.979690	10.493863
9.085669	510.622250	10.498880
9.483641	513.570760	10.503898
8.910835	506.610155	10.508915
9.367225	509.625305	10.513933
9.119381	521.251468	10.518951
9.058028	516.379171	10.523968
9.525853	524.949673	10.528986
9.220981	525.820737	10.534003
9.159471	524.255604	10.539021
9.172557	526.304718	10.544039
8.984550	534.948934	10.549056
9.385796	532.204110	10.554074
9.520810	539.166554	10.559091
9.454992	537.239188	10.564109
9.644751	533.451208	10.569127
9.418579	534.433091	10.574144
9.624803	530.841355	10.579162
8.988125	531.300197	10.584179
9.572787	532.951064	10.589197
9.824880	534.650556	10.594215
9.250598	530.640723	10.599232
9.476051	522.356671	10.604250
9.297105	520.999162	10.609267
9.169942	526.995763	10.614285
9.334963	526.518777	10.619303
9.107450	528.687400	10.624320
9.578706	536.380097	10.629338
9.204392	535.081406	10.634355
9.763492	539.131407	10.639373
9.599598	533.101162	10.644391
9.536687	537.541485	10.649408
9.648195	533.813023	10.654426
9.634669	539.719356	10.659443
9.470044	537.930444	10.664461
9.771543	530.363509	10.669479
9.582991	540.951705	10.674496
9.495757	536.121300	10.679514
9.573815	529.191887	10.684531
9.247238	531.584208	10.689549
9.795249	530.668912	10.694567
9.327045	530.145355	10.699584
9.388837	532.881134	10.704602
9.450489	526.919911	10.709619
9.162486	530.170879	10.714637
9.522219	535.438452	10.719655
9.253407	540.914338	10.724672
9.374878	538.629621	10.729690
9.534015	524.489503	10.734707
9.448150	547.697014	10.739725
9.930232	551.263570	10.744743
9.756988	556.667778	10.749760
9.848679	549.401733	10.754778
9.830431	535.686839	10.759795
9.416783	528.635176	10.764813
9.701069	525.788647	10.769831
9.554160	540.286544	10.774848
9.632960	552.818039	10.779866
9.845178	552.412595	10.784883
9.662132	553.056419	10.789901
9.781573	551.841790	10.794919
9.677390	556.758739	10.799936
9.923802	562.126011	10.804954
10.009556	555.406820	10.809971
9.848975	547.025077	10.814989
9.823688	536.915056	10.820007
9.969820	555.838925	10.825024
9.990573	540.631633	10.830042
9.767537	534.698954	10.835059
9.590981	536.253755	10.840077
9.673771	537.386341	10.845095
10.061434	550.696531	10.850112
9.870125	545.424755	10.855130
9.960854	540.724425	10.860147
9.797948	548.534798	10.865165
9.953095	542.802000	10.870183
9.788973	542.142740	10.875200
10.232166	539.713262	10.880218
10.350714	533.446546	10.885235
9.561560	535.156683	10.890253
9.835990	536.849542	10.895271
9.596613	528.549501	10.900288
9.977216	547.856559	10.905306
10.150997	551.234440	10.910323
10.116790	556.399260	10.915341
10.114566	535.212393	10.920359
9.760815	543.222884	10.925376
10.028299	550.685393	10.930394
10.228229	541.089392	10.935411
9.920089	540.799679	10.940429
9.787336	534.253365	10.945447
9.887126	555.241946	10.950464
10.120279	559.131271	10.955482
10.516130	553.929014	10.960499
10.121679	548.660465	10.965517
10.043235	541.424068	10.970535
10.280914	536.688236	10.975552
9.870043	529.850726	10.980570
9.956122	531.244720	10.985587
9.408610	547.212423	10.990605
10.072102	543.801943	10.995623
9.819188	549.966448	11.000640
10.040102	555.037899	11.005658
10.465292	548.007096	11.010675
10.128837	555.405855	11.015693
10.204744	550.856146	11.020711
10.186990	554.958097	11.025728
10.255114	563.196391	11.030746
9.698259	554.677535	11.035763
9.937609	560.490856	11.040781
9.844282	562.288311	11.045799
10.227335	555.112593	11.050816
9.974557	569.980433	11.055834
9.842394	561.398607	11.060851
10.409642	581.853710	11.065869
10.281484	576.587871	11.070887
10.126065	573.055589	11.075904
10.147396	573.364647	11.080922
10.410281	584.469538	11.085939
10.339780	584.426836	11.090957
10.533161	585.580074	11.095975
10.395775	566.496963	11.100992
10.316117	565.108213	11.106010
10.242601	561.907150	11.111027
10.177967	561.885624	11.116045
10.197000	568.285493	11.121063
10.439200	578.658329	11.126080
10.458614	580.447699	11.131098
10.431651	576.895416	11.136115
10.308797	571.067042	11.141133
10.431671	569.397460	11.146151
10.497418	573.413834	11.151168
10.263244	565.819837	11.156186
10.475528	572.763953	11.161203
10.559795	585.903665	11.166221
10.259247	580.260739	11.171239
10.203581	576.835996	11.176256
10.217693	590.939649	11.181274
10.204098	581.809199	11.186291
10.327090	589.095413	11.191309
10.445916	585.905423	11.196327
10.494616	590.890093	11.201344
10.006276	586.178927	11.206362
10.534862	582.016304	11.211379
10.376085	588.620583	11.216397
10.521527	588.619995	11.221415
10.845737	592.485683	11.226432
10.654320	584.436915	11.231450
10.743900	581.608070	11.236467
10.438556	587.906978	11.241485
10.607327	581.215875	11.246503
10.302981	581.458880	11.251520
10.746698	589.095931	11.256538
10.490939	583.635370	11.261555
10.389284	583.496537	11.266573
10.797934	585.610298	11.271591
10.817621	587.068279	11.276608
10.269968	594.124411	11.281626
10.466231	589.297188	11.286643
10.345846	588.148298	11.291661
10.707145	594.346570	11.296679
10.492067	588.952255	11.301696
10.650959	609.499369	11.306714
10.917246	602.474352	11.311731
10.545823	621.033921	11.316749
10.516420	614.667139	11.321767
10.767825	616.890590	11.326784
11.079559	611.941244	11.331802
11.213694	614.466965	11.336819
10.522864	605.246292	11.341837
10.770882	602.702033	11.346855
10.799756	597.111949	11.351872
10.753093	609.237001	11.356890
10.900595	606.613720	11.361907
10.609964	613.834961	11.366925
10.780580	616.490696	11.371943
10.971368	616.202193	11.376960
11.077649	624.425106	11.381978
11.100836	607.557487	11.386995
10.825106	600.149820	11.392013
10.602794	592.979981	11.397031
10.869059	606.517389	11.402048
10.877034	619.858346	11.407066
11.064041	619.226462	11.412083
10.948896	604.175968	11.417101
11.114263	609.423335	11.422119
10.718058	596.972711	11.427136
10.486219	607.362567	11.432154
10.909411	607.321890	11.437171
11.065764	620.765973	11.442189
10.821044	624.215339	11.447207
11.147405	616.300526	11.452224
10.796667	621.486246	11.457242
11.306894	623.912387	11.462259
11.053984	622.370734	11.467277
11.049009	613.737523	11.472295
11.291999	612.702462	11.477312
10.764277	614.513908	11.482330
10.686837	611.038903	11.487347
10.880902	612.747437	11.492365
10.870858	612.543849	11.497383
10.783485	609.272354	11.502400
10.945890	620.228816	11.507418
10.833221	611.340985	11.512435
10.729282	621.111355	11.517453
10.749602	618.952826	11.522471
11.242994	622.347228	11.527488
10.793817	637.406643	11.532506
11.403613	633.468040	11.537523
11.223626	629.914326	11.542541
11.127488	637.976265	11.547559
11.010050	636.700685	11.552576
11.048304	641.418762	11.557594
10.979079	633.694916	11.562611
11.107088	640.992994	11.567629
11.224767	643.732711	11.572647
11.408954	638.695924	11.577664
11.433001	647.035789	11.582682
11.413128	639.774455	11.587699
11.663393	640.003691	11.592717
11.537907	637.729011	11.597735
11.232061	620.877896	11.602752
11.004897	627.044729	11.607770
11.228328	639.266598	11.612787
11.536654	640.493459	11.617805
11.407079	641.693829	11.622823
11.538607	632.979398	11.627840
11.152154	634.790941	11.632858
11.148826	640.389617	11.637875
11.235967	640.088850	11.642893
11.472365	638.559370	11.647911
11.235971	637.538988	11.652928
11.244080	645.054544	11.657946
11.084853	640.588757	11.662963
11.310153	646.934449	11.667981
11.306201	646.089308	11.672999
11.376456	646.431774	11.678016
11.533663	650.260363	11.683034
11.348605	651.933258	11.688051
11.154078	645.828851	11.693069
10.846821	643.342639	11.698087
11.177107	645.102548	11.703104
11.376485	666.747916	11.708122
11.656289	664.321771	11.713139
11.703302	673.535356	11.718157
11.699871	677.417362	11.723175
11.781093	654.330257	11.728192
11.478598	656.425365	11.733210
11.191209	645.617659	11.738227
11.769875	660.558085	11.743245
11.492551	671.084444	11.748263
11.779730	674.640346	11.753280
11.660971	678.786453	11.758298
11.455686	667.268541	11.763315
11.492190	663.517018	11.768333
11.557799	670.802733	11.773351
11.822428	656.838583	11.778368
11.499087	670.915947	11.783386
11.600436	675.112987	11.788403
11.571819	670.806732	11.793421
11.578423	669.363519	11.798439
11.671821	668.730429	11.803456
11.935789	671.904950	11.808474
11.787290	680.603044	11.813491
11.926741	679.552543	11.818509
11.331684	682.027709	11.823527
11.828064	674.319921	11.828544
11.847728	671.978457	11.833562
11.645008	668.579749	11.838579
11.814118	673.823395	11.843597
11.961289	668.016062	11.848615
12.011504	663.773271	11.853632
11.646531	673.915660	11.858650
11.795037	666.508183	11.863667
11.598488	664.020510	11.868685
11.418319	668.737889	11.873703
11.700313	665.778090	11.878720
11.686788	661.636739	11.883738
11.571584	657.817322	11.888755
11.955255	663.090673	11.893773
11.766560	664.770448	11.898791
11.859866	659.833008	11.903808
11.673162	670.995329	11.908826
11.938078	680.607321	11.913843
12.228913	684.973669	11.918861
11.968253	688.457086	11.923879
12.191437	681.514485	11.928896
12.114515	672.299177	11.933914
11.488934	669.569044	11.938931
11.994080	672.756505	11.943949
11.904646	688.138635	11.948967
12.260936	685.981435	11.953984
12.199018	694.205324	11.959002
11.893478	689.778083	11.964019
12.107710	691.761187	11.969037
12.487219	693.819539	11.974055
12.016683	678.070105	11.979072
11.872565	678.647914	11.984090
12.050169	689.128697	11.989107
12.419652	690.936155	11.994125
12.196155	687.414449	11.999143
12.099604	666.592396	12.004160
12.185409	679.435302	12.009178
11.948769	684.249837	12.014195
12.262290	694.965074	12.019213
12.126187	706.656008	12.024231
12.351048	697.854433	12.029248
12.558748	696.872197	12.034266
12.154197	677.600197	12.039283
12.294193	673.961942	12.044301
12.081634	674.638766	12.049319
12.056540	683.803624	12.054336
12.102198	689.530384	12.059354
12.457762	697.373703	12.064371
12.507258	696.491836	12.069389
12.235156	702.769830	12.074407
12.320944	694.488510	12.079424
12.149170	696.733678	12.084442
11.811300	697.553086	12.089459
12.269308	693.499252	12.094477
11.925469	699.201454	12.099495
12.330876	699.901981	12.104512
11.897012	697.151460	12.109530
12.246963	702.758266	12.114547
12.508156	704.216524	12.119565
12.158985	704.980889	12.124583
12.439461	698.862466	12.129600
12.334503	691.434483	12.134618
12.502666	696.220708	12.139635
12.733208	691.233491	12.144653
12.183316	698.053335	12.149671
12.203252	702.859484	12.154688
12.446584	700.502126	12.159706
12.439151	718.585417	12.164723
12.629382	717.706882	12.169741
12.107412	729.593604	12.174759
12.390570	724.096429	12.179776
12.669818	718.511505	12.184794
12.625429	725.230564	12.189811
12.873809	718.549105	12.194829
12.575098	722.688527	12.199847
12.471912	718.769399	12.204864
12.827424	714.750453	12.209882
12.944735	720.579672	12.214899
12.806783	711.175037	12.219917
12.573737	709.011765	12.224935
12.491175	701.245787	12.229952
12.849364	716.024935	12.234970
12.691295	715.222719	12.239987
13.063895	699.471376	12.245005
12.505792	695.354848	12.250023
12.571763	694.221115	12.255040
12.907594	696.652330	12.260058
12.650070	705.190691	12.265075
12.760457	690.029274	12.270093
12.619772	704.898708	12.275111
12.724031	712.891611	12.280128
13.161923	718.727719	12.285146
12.645477	709.732297	12.290163
13.061088	703.491851	12.295181
12.745581	708.949811	12.300199
12.945950	698.908703	12.305216
12.906579	698.372020	12.310234
12.194065	699.805161	12.315251
12.710784	698.017445	12.320269
12.943280	713.699756	12.325287
12.993495	716.080771	12.330304
13.362886	717.648413	12.335322
13.004819	720.171889	12.340339
13.538001	720.511707	12.345357
13.428443	713.734506	12.350375
12.949448	702.287588	12.355392
12.902064	691.275234	12.360410
13.171692	700.015530	12.365427
12.871296	691.709135	12.370445
12.870313	699.671082	12.375463
12.745125	707.911139	12.380480
12.948204	690.526300	12.385498
12.390366	692.077364	12.390515
12.879626	702.036277	12.395533
13.357619	716.579029	12.400551
12.983781	712.601059	12.405568
13.618312	715.418101	12.410586
13.073524	715.016912	12.415603
13.154098	701.135031	12.420621
12.728337	695.855534	12.425639
13.155186	706.035598	12.430656
13.099757	708.120647	12.435674
13.086365	723.374207	12.440691
12.787317	716.434010	12.445709
12.969055	715.228604	12.450727
12.931276	721.552170	12.455744
12.967618	711.927900	12.460762
12.779653	723.472290	12.465779
13.118877	720.614022	12.470797
13.028842	725.869631	12.475815
12.890506	719.371454	12.480832
13.503589	729.819172	12.485850
13.235569	735.408599	12.490867
13.265552	734.015388	12.495885
13.300387	741.511044	12.500903
13.342018	741.611824	12.505920
13.389550	746.795529	12.510938
12.844686	755.097794	12.515955
12.841272	745.479695	12.520973
13.474511	749.171074	12.525991
13.157354	751.088601	12.531008
13.189523	742.544216	12.536026
13.415190	751.367119	12.541043
13.194861	747.920645	12.546061
13.291278	747.662612	12.551079
13.322570	759.466369	12.556096
13.310474	747.978285	12.561114
13.633099	757.161624	12.566131
13.649814	749.175046	12.571149
13.301501	745.868416	12.576167
13.388576	748.265787	12.581184
13.590293	747.499068	12.586202
13.079351	740.957915	12.591219
13.699067	749.896184	12.596237
13.499067	747.891860	12.601255
12.962981	762.573603	12.606272
13.481823	772.146109	12.611290
13.462542	766.478265	12.616307
13.957470	770.875973	12.621325
13.777884	767.584093	12.626343
13.621426	771.467856	12.631360
13.727738	764.884236	12.636378
13.452776	769.184068	12.641395
13.461966	768.769207	12.646413
13.804654	773.944833	12.651431
13.530439	778.459140	12.656448
13.728615	770.027746	12.661466
13.730987	771.065574	12.666483
13.685233	768.118919	12.671501
13.875790	766.590255	12.676519
13.710933	775.944174	12.681536
13.820411	769.227520	12.686554
13.752496	777.048449	12.691571
13.766808	768.740355	12.696589
14.007425	768.611343	12.701607
13.714518	767.549261	12.706624
13.793822	766.041074	12.711642
13.828228	764.991145	12.716659
13.860180	765.857114	12.721677
13.931027	764.804666	12.726695
13.655402	764.017596	12.731712
13.829412	770.150419	12.736730
13.737375	771.928759	12.741747
13.785115	776.055276	12.746765
13.844219	766.430588	12.751783
13.492264	773.399518	12.756800
13.953213	775.012868	12.761818
14.004668	782.184071	12.766835
13.835051	771.563073	12.771853
13.964664	779.075546	12.776871
14.057809	799.254430	12.781888
14.118311	800.513576	12.786906
14.008439	793.080004	12.791923
14.219604	797.569235	12.796941
13.721251	782.729730	12.801959
13.763819	801.688919	12.806976
14.436141	802.878053	12.811994
14.407953	802.415363	12.817011
14.399012	793.378751	12.822029
14.139709	779.395096	12.827047
14.009139	782.154553	12.832064
14.169843	782.198925	12.837082
14.119037	778.883837	12.842099
14.042297	782.341791	12.847117
14.458960	791.314852	12.852135
13.987610	788.724784	12.857152
14.443808	791.080468	12.862170
14.345390	789.590483	12.867187
14.150443	783.678593	12.872205
14.186207	777.134354	12.877223
14.239127	791.206878	12.882240
14.504190	788.991289	12.887258
14.297743	790.904206	12.892275
14.287373	790.069523	12.897293
14.460883	791.860168	12.902311
14.156020	796.543348	12.907328
14.476040	795.979108	12.912346
14.604669	796.697486	12.917363
13.925382	785.524690	12.922381
14.554860	783.492198	12.927399
14.150338	794.287734	12.932416
14.329522	791.782567	12.937434
14.643487	794.993505	12.942451
14.489211	804.128047	12.947469
14.637667	794.473654	12.952487
14.389510	791.965596	12.957504
14.565240	793.162621	12.962522
14.631036	791.741739	12.967539
14.598516	792.674550	12.972557
14.675069	784.271554	12.977575
14.600713	799.632498	12.982592
14.736727	798.831826	12.987610
14.500469	784.068274	12.992627
14.493224	796.644894	12.997645
14.951137	788.520181	13.002663
14.385242	785.657663	13.007680
14.472585	793.075740	13.012698
14.809888	790.646937	13.017715
14.795665	797.945134	13.022733
14.725614	797.214415	13.027751
14.582753	798.265389	13.032768
14.380152	799.754842	13.037786
14.551806	805.682922	13.042803
14.478851	800.288505	13.047821
14.801568	795.185925	13.052839
14.435037	802.021439	13.057856
14.264519	792.561873	13.062874
14.317410	793.866383	13.067891
14.237920	796.198178	13.072909
14.666588	808.091572	13.077927
14.706857	813.910726	13.082944
14.977136	821.142547	13.087962
15.009120	819.805821	13.092979
14.597614	816.783564	13.097997
14.810151	817.460477	13.103015
14.571882	823.174684	13.108032
14.550544	820.337825	13.113050
14.799615	815.912562	13.118067
14.746336	824.595901	13.123085
14.888629	819.575052	13.128103
14.895196	820.984604	13.133120
14.984479	824.953191	13.138138
14.703810	819.502748	13.143155
14.830102	827.675304	13.148173
14.875615	821.722806	13.153191
14.947897	828.275420	13.158208
14.953730	828.801485	13.163226
15.563337	834.888600	13.168243
15.532534	830.036706	13.173261
15.473765	825.122898	13.178279
15.115721	823.531325	13.183296
15.026091	820.067644	13.188314
15.046605	822.652108	13.193331
15.037054	831.934540	13.198349
15.393699	822.026817	13.203367
14.885609	833.494892	13.208384
14.954952	818.352379	13.213402
15.114951	824.083470	13.218419
14.854211	828.788190	13.223437
15.331602	828.300430	13.228455
15.176952	833.054904	13.233472
15.235562	843.011521	13.238490
15.489036	838.544543	13.243507
15.143363	847.049360	13.248525
15.625419	832.104503	13.253543
15.343600	837.074432	13.258560
15.077554	824.391950	13.263578
15.298876	829.943086	13.268595
15.407001	840.466334	13.273613
15.525195	841.539780	13.278631
15.307971	827.603183	13.283648
15.353036	849.048743	13.288666
15.609985	842.974959	13.293683
15.325820	839.386931	13.298701
15.517285	837.968570	13.303719
15.494489	848.307084	13.308736
15.395847	842.777802	13.313754
15.439669	844.695938	13.318771
15.527891	846.297901	13.323789
15.760776	841.332368	13.328807
15.527875	846.780665	13.333824
15.559666	844.976920	13.338842
15.700558	844.254380	13.343859
15.341683	845.178047	13.348877
15.427306	845.994640	13.353895
15.779813	845.646241	13.358912
15.347911	844.940301	13.363930
15.932290	846.985709	13.368947
15.589428	849.011387	13.373965
15.337217	845.203794	13.378983
15.441743	845.828100	13.384000
15.584491	849.302386	13.389018
15.690775	844.485947	13.394035
15.427219	841.784625	13.399053
15.746759	843.038156	13.404071
15.537656	843.635555	13.409088
15.671290	849.948256	13.414106
15.587272	839.534791	13.419123
15.287126	850.809558	13.424141
15.708947	859.731359	13.429159
15.643836	867.501400	13.434176
15.939188	871.822911	13.439194
16.116301	866.408474	13.444211
15.918949	873.211363	13.449229
16.016700	862.166839	13.454247
16.289080	869.474090	13.459264
16.045911	861.688867	13.464282
15.788704	848.850361	13.469299
15.407908	845.955858	13.474317
15.928635	854.764430	13.479335
15.687658	858.623502	13.484352
15.695199	861.292041	13.489370
15.873645	866.464865	13.494387
15.857193	873.946472	13.499405
16.218407	868.582264	13.504423
16.126142	870.815074	13.509440
15.922320	865.551463	13.514458
16.234207	868.008520	13.519475
16.019639	875.259048	13.524493
16.016616	867.638400	13.529511
16.320504	866.644334	13.534528
16.076393	876.556587	13.539546
15.963473	870.515134	13.544563
15.817045	871.434127	13.549581
15.851456	867.809116	13.554599
16.159398	868.537448	13.559616
15.759128	869.966166	13.564634
16.493811	869.340519	13.569651
16.141179	870.600878	13.574669
16.287492	867.586434	13.579687
16.347874	870.366665	13.584704
16.190715	869.450695	13.589722
16.455778	877.286094	13.594739
16.332851	875.443320	13.599757
16.229250	877.479086	13.604775
16.539952	878.244857	13.609792
16.106137	879.864987	13.614810
16.319252	889.649255	13.619827
16.374529	898.580809	13.624845
16.595162	899.527858	13.629863
16.667864	888.354678	13.634880
16.403774	881.374260	13.639898
16.794973	877.381279	13.644915
16.628131	872.534776	13.649933
16.264166	867.179336	13.654951
16.576067	867.042381	13.659968
16.085899	870.659394	13.664986
16.213526	874.240178	13.670003
16.399163	900.937139	13.675021
16.691832	896.520848	13.680039
17.074186	891.412111	13.685056
16.647846	897.101975	13.690074
16.734797	884.361334	13.695091
16.704655	886.950539	13.700109
16.570717	894.945897	13.705127
16.699406	890.419442	13.710144
16.573641	888.053257	13.715162
16.648137	888.253060	13.720179
16.670757	894.747159	13.725197
16.909036	884.125701	13.730215
16.519832	885.861960	13.735232
16.567223	887.268317	13.740250
16.814818	888.791822	13.745267
16.683505	889.399201	13.750285
16.361408	889.218949	13.755303
16.869191	891.860099	13.760320
16.285334	899.048216	13.765338
16.734759	888.245561	13.770355
16.794606	889.104037	13.775373
16.515749	895.414707	13.780391
16.828071	899.995509	13.785408
16.348884	912.210199	13.790426
16.879607	912.357904	13.795443
16.979645	920.465164	13.800461
17.268401	921.739272	13.805479
16.859109	920.903580	13.810496
16.871560	924.865216	13.815514
17.023970	916.497683	13.820531
17.162129	920.815279	13.825549
16.954403	916.303326	13.830567
16.721440	910.331042	13.835584
16.998150	911.332476	13.840602
17.218169	908.164542	13.845619
16.834492	908.890106	13.850637
16.544496	909.051988	13.855655
16.992361	915.262140	13.860672
17.090294	915.609770	13.865690
17.346184	914.010962	13.870707
17.402090	922.323906	13.875725
17.341252	914.920518	13.880743
17.299252	917.716697	13.885760
17.147225	907.174928	13.890778
17.268990	910.939665	13.895795
17.233139	912.762918	13.900813
17.124850	908.999174	13.905831
17.433746	910.816088	13.910848
17.009789	904.472764	13.915866
17.359177	916.138738	13.920883
17.574500	927.494241	13.925901
17.436321	936.061466	13.930919
17.613385	919.422054	13.935936
17.283377	915.396189	13.940954
17.677043	908.824580	13.945971
17.720374	904.459730	13.950989
17.445502	908.567082	13.956007
17.304243	911.328222	13.961024
17.069216	910.124578	13.966042
17.361283	918.668988	13.971059
16.938569	921.593869	13.976077
16.813152	933.491567	13.981095
17.675915	928.273309	13.986112
17.553816	936.740203	13.991130
17.531140	938.930630	13.996147
17.611236	930.710045	14.001165
17.888036	939.228441	14.006183
18.250856	934.293143	14.011200
18.023395	940.397016	14.016218
18.141413	934.130241	14.021235
18.197239	935.125043	14.026253
17.894807	931.514594	14.031271
17.642199	916.100240	14.036288
17.502047	917.286496	14.041306
17.316150	915.068522	14.046323
17.892398	915.007172	14.051341
17.378553	936.262151	14.056359
17.994551	929.154156	14.061376
17.858707	931.128677	14.066394
17.917452	928.850521	14.071411
17.902564	923.800468	14.076429
17.953138	933.161953	14.081447
18.055645	930.132228	14.086464
17.827069	933.976763	14.091482
18.028683	935.349644	14.096499
18.356410	936.055964	14.101517
17.967115	924.500265	14.106535
17.964914	916.305124	14.111552
18.000703	914.626978	14.116570
17.938166	927.505783	14.121587
17.899249	926.912219	14.126605
17.728493	929.248774	14.131623
18.160149	933.473341	14.136640
18.103539	936.634708	14.141658
18.018514	931.437786	14.146675
18.043724	932.752928	14.151693
17.806800	935.554212	14.156711
18.163160	933.920826	14.161728
18.162034	944.947129	14.166746
18.046812	931.111333	14.171763
18.201479	939.389973	14.176781
18.279598	941.110280	14.181799
18.254359	942.868770	14.186816
17.937654	933.608611	14.191834
17.835277	936.827595	14.196851
18.113239	937.036744	14.201869
18.164298	937.306467	14.206887
18.098968	936.748573	14.211904
18.480753	944.325993	14.216922
18.236571	949.031322	14.221939
18.035355	944.748718	14.226957
18.145005	963.555627	14.231975
18.351580	965.050813	14.236992
18.331973	963.453870	14.242010
18.512794	966.660324	14.247027
18.651855	959.131122	14.252045
18.611865	969.232546	14.257063
18.699360	960.963460	14.262080
18.604325	955.910098	14.267098
18.438736	962.872175	14.272115
18.668777	957.831314	14.277133
18.596740	968.549942	14.282151
18.647292	958.932793	14.287168
18.620733	957.134966	14.292186
18.746939	951.592732	14.297203
18.550922	949.306903	14.302221
18.459200	956.648788	14.307239
18.813830	948.647379	14.312256
18.786827	952.223852	14.317274
18.780996	965.822833	14.322291
18.657254	957.056471	14.327309
18.628288	956.224676	14.332327
18.840714	950.293485	14.337344
19.025684	956.528805	14.342362
18.615008	960.376451	14.347379
18.959157	956.879919	14.352397
18.637291	951.312775	14.357415
18.962404	958.103777	14.362432
18.692156	949.540108	14.367450
18.612143	957.189433	14.372467
18.688237	955.050582	14.377485
18.749226	958.543930	14.382503
19.090742	949.840831	14.387520
18.715931	962.105574	14.392538
18.674468	966.605779	14.397555
18.565000	958.357893	14.402573
18.865427	953.394436	14.407591
19.053104	956.139082	14.412608
19.038931	965.261360	14.417626
19.125026	969.624943	14.422643
19.100125	975.836143	14.427661
18.880571	977.665915	14.432679
19.395002	986.046351	14.437696
19.199082	982.498202	14.442714
18.851709	991.823848	14.447731
19.540101	985.487185	14.452749
19.340983	987.051848	14.457767
19.090916	972.107256	14.462784
19.390947	967.724514	14.467802
19.205931	971.432889	14.472819
19.368316	960.857914	14.477837
19.409810	963.161427	14.482855
19.305036	966.043125	14.487872
18.778393	958.813226	14.492890
18.898404	979.553011	14.497907
19.258282	978.581780	14.502925
19.222555	984.646348	14.507943
19.355894	989.630574	14.512960
19.347175	983.569704	14.517978
19.533180	986.882650	14.522995
19.437625	987.569670	14.528013
19.651099	985.958526	14.533031
19.497506	980.895340	14.538048
19.607774	980.726663	14.543066
19.358421	992.353367	14.548083
19.564263	984.630723	14.553101
19.346207	983.676891	14.558119
19.031574	983.732158	14.563136
19.040262	977.908416	14.568154
18.837065	993.403194	14.573171
19.499458	1005.724225	14.578189
19.551194	1004.854617	14.583207
19.569674	1010.651983	14.588224
19.781492	1012.351480	14.593242
19.874448	1014.533380	14.598259
19.749881	1005.066546	14.603277
19.928557	1011.280775	14.608295
19.672359	1015.009709	14.613312
19.914403	1015.461133	14.618330
19.438685	1017.516982	14.623347
19.798460	1008.205107	14.628365
20.043505	1010.991322	14.633383
19.732590	1014.081845	14.638400
20.163044	1006.825985	14.643418
19.806762	1014.944376	14.648435
19.988028	1009.781709	14.653453
19.849855	1013.205092	14.658471
19.875014	1002.440023	14.663488
20.025361	1001.406742	14.668506
19.748841	1013.933923	14.673523
20.035753	1019.758924	14.678541
19.919643	1021.162347	14.683559
19.566961	1009.256914	14.688576
19.910168	1002.945588	14.693594
19.507526	1013.163460	14.698611
19.927753	1029.567890	14.703629
19.713536	1032.261514	14.708647
20.094589	1030.621119	14.713664
20.109521	1034.752804	14.718682
20.080950	1038.686140	14.723699
20.674187	1036.936970	14.728717
20.459159	1038.687149	14.733735
20.633396	1039.676143	14.738752
20.565370	1037.240989	14.743770
20.266109	1036.899392	14.748787
20.323069	1041.826098	14.753805
20.299752	1035.038503	14.758823
20.277609	1040.864293	14.763840
20.541405	1041.201880	14.768858
20.748700	1040.620471	14.773875
20.453883	1028.611344	14.778893
20.362078	1030.774676	14.783911
20.153652	1034.070148	14.788928
20.806650	1045.098809	14.793946
20.328103	1043.617495	14.798963
20.208122	1033.739683	14.803981
20.284589	1038.123716	14.808999
20.552048	1040.751814	14.814016
20.490187	1036.460114	14.819034
20.471096	1048.578015	14.824051
20.701739	1040.842018	14.829069
20.700299	1034.757907	14.834087
20.774351	1031.574808	14.839104
20.741558	1028.351541	14.844122
20.690497	1034.519498	14.849139
20.508294	1033.455942	14.854157
20.589568	1030.363236	14.859175
20.377093	1036.625751	14.864192
20.828054	1030.035710	14.869210
20.616714	1037.446745	14.874227
20.531860	1026.563092	14.879245
20.862829	1035.754744	14.884263
20.669003	1036.990389	14.889280
21.045399	1034.410302	14.894298
20.504241	1034.185261	14.899315
20.824723	1031.863186	14.904333
20.761828	1019.167869	14.909351
20.845238	1030.824838	14.914368
21.024319	1038.796771	14.919386
20.786174	1037.836597	14.924403
21.198884	1045.554411	14.929421
21.199280	1044.560252	14.934439
21.014112	1042.373706	14.939456
20.958590	1023.693919	14.944474
21.040291	1035.777185	14.949491
20.701475	1040.806536	14.954509
21.245534	1045.512240	14.959527
21.202712	1046.957901	14.964544
21.185616	1045.467856	14.969562
20.977185	1057.318601	14.974579
21.053371	1053.930042	14.979597
21.494981	1053.009197	14.984615
21.419543	1060.910316	14.989632
21.300560	1056.728489	14.994650
21.329750	1057.563344	14.999667
21.405349	1059.410286	15.004685
21.152013	1054.845439	15.009703
20.742708	1057.010871	15.014720
21.318031	1052.193933	15.019738
21.451692	1059.103143	15.024755
21.217296	1055.557815	15.029773
21.053339	1047.709686	15.034791
20.891616	1055.911410	15.039808
21.489842	1045.259060	15.044826
21.034345	1048.757103	15.049843
21.443498	1057.179210	15.054861
22.072349	1065.216825	15.059879
21.335132	1062.980530	15.064896
21.503169	1056.494489	15.069914
21.350598	1066.054927	15.074931
21.335498	1068.695464	15.079949
21.966989	1074.015560	15.084967
21.502085	1086.493228	15.089984
21.545515	1079.367024	15.095002
21.617769	1079.996363	15.100019
21.866360	1078.900444	15.105037
21.806192	1074.640029	15.110055
21.616503	1081.280860	15.115072
21.645251	1079.793141	15.120090
21.949927	1072.967087	15.125107
21.523033	1071.193710	15.130125
21.944761	1073.917712	15.135143
21.796187	1077.194406	15.140160
21.830670	1077.917987	15.145178
22.218301	1081.297388	15.150195
21.696574	1077.257155	15.155213
22.030259	1072.042337	15.160231
22.012199	1077.611887	15.165248
21.644727	1072.622999	15.170266
21.343065	1072.591040	15.175283
21.807419	1074.273316	15.180301
21.922097	1077.471154	15.185319
21.740875	1070.168494	15.190336
21.978770	1088.112978	15.195354
22.196653	1092.863167	15.200371
21.981480	1102.379723	15.205389
22.193720	1101.103272	15.210407
21.916415	1101.301048	15.215424
22.040563	1110.991993	15.220442
22.319410	1105.170328	15.225459
22.095211	1100.465236	15.230477
22.209991	1094.908957	15.235495
21.985291	1107.450227	15.240512
22.008149	1109.194933	15.245530
22.199742	1116.297115	15.250547
22.011747	1101.806648	15.255565
22.363298	1107.457514	15.260583
22.280229	1105.826259	15.265600
22.341629	1098.454255	15.270618
22.528971	1098.456612	15.275635
22.341656	1108.041416	15.280653
22.501819	1102.342371	15.285671
22.283342	1102.010286	15.290688
22.410071	1104.830715	15.295706
22.650770	1107.551351	15.300723
22.667648	1111.850007	15.305741
22.649045	1108.671854	15.310759
22.317679	1107.773526	15.315776
22.594894	1121.672535	15.320794
22.852323	1116.583185	15.325811
22.768703	1124.387777	15.330829
22.623085	1101.660455	15.335847
22.844679	1103.478359	15.340864
22.703676	1111.916722	15.345882
22.761326	1112.043412	15.350899
22.447120	1123.203776	15.355917
22.591280	1127.069213	15.360935
22.822200	1124.555944	15.365952
22.953031	1116.608239	15.370970
22.836730	1117.320584	15.375987
22.630840	1123.657844	15.381005
23.118355	1121.344464	15.386023
22.894446	1119.905547	15.391040
23.144167	1125.742685	15.396058
23.055556	1112.110886	15.401075
22.767694	1121.878608	15.406093
23.328240	1114.567737	15.411111
22.837154	1122.763969	15.416128
22.978882	1118.456329	15.421146
23.168213	1119.184205	15.426163
22.991236	1116.428335	15.431181
23.399204	1110.984192	15.436199
22.984017	1116.568248	15.441216
23.107624	1128.411524	15.446234
23.340287	1118.352529	15.451251
23.215524	1115.042582	15.456269
23.161834	1112.573627	15.461287
23.378986	1130.117445	15.466304
23.110388	1118.454465	15.471322
23.159882	1114.375780	15.476339
23.015090	1118.421902	15.481357
22.907583	1118.858325	15.486375
23.158986	1117.058229	15.491392
22.761275	1121.033278	15.496410
23.461200	1130.773442	15.501427
23.136473	1150.149947	15.506445
23.261297	1129.636864	15.511463
23.033245	1151.229451	15.516480
23.526440	1141.619025	15.521498
23.767115	1146.100594	15.526515
23.556871	1147.894220	15.531533
23.431862	1146.357853	15.536551
23.604650	1144.693069	15.541568
23.453118	1151.959141	15.546586
24.067612	1146.829968	15.551603
23.667929	1145.768707	15.556621
23.856834	1143.931003	15.561639
23.850065	1142.092206	15.566656
23.623027	1138.359525	15.571674
23.973326	1143.313171	15.576691
23.957224	1146.673393	15.581709
23.521155	1140.584332	15.586727
23.447141	1136.231384	15.591744
23.420787	1135.089909	15.596762
23.729712	1134.091889	15.601779
23.400641	1151.039124	15.606797
23.684848	1144.973617	15.611815
23.981386	1164.688906	15.616832
23.962827	1172.751631	15.621850
23.882452	1173.423671	15.626867
24.093193	1170.235045	15.631885
24.091998	1168.575257	15.636903
24.393936	1166.164534	15.641920
24.183155	1163.899910	15.646938
24.100020	1145.940657	15.651955
24.141962	1140.294720	15.656973
24.268789	1144.633070	15.661991
24.176838	1137.038775	15.667008
24.154903	1151.637630	15.672026
24.038441	1151.387489	15.677043
24.145167	1162.583326	15.682061
24.157240	1162.388911	15.687079
24.009047	1166.394548	15.692096
24.163946	1173.578205	15.697114
24.414530	1160.168111	15.702131
24.339606	1157.206999	15.707149
24.349438	1161.064955	15.712167
24.335281	1156.690059	15.717184
24.683891	1157.115428	15.722202
24.838233	1157.078743	15.727219
24.758255	1155.888810	15.732237
24.697875	1155.257555	15.737255
24.565405	1159.024059	15.742272
24.260158	1156.748898	15.747290
24.499309	1156.799993	15.752307
24.447111	1158.613194	15.757325
24.615444	1155.601585	15.762343
25.108923	1156.973223	15.767360
24.904412	1153.281212	15.772378
24.733307	1150.745327	15.777395
24.715837	1151.499090	15.782413
24.873407	1152.272937	15.787431
25.217563	1148.785834	15.792448
24.448535	1148.163928	15.797466
24.804057	1143.103478	15.802483
25.079121	1151.694829	15.807501
24.730563	1148.192503	15.812519
24.697324	1139.875860	15.817536
24.665879	1150.196961	15.822554
24.866920	1145.248925	15.827571
24.545669	1155.529945	15.832589
25.093544	1154.122339	15.837607
25.041952	1146.603807	15.842624
24.771379	1160.685964	15.847642
25.028960	1148.243614	15.852659
25.032161	1150.830822	15.857677
24.874101	1151.915740	15.862695
24.918678	1154.038919	15.867712
24.835506	1157.740942	15.872730
24.925754	1148.458335	15.877747
24.795090	1155.452918	15.882765
25.141416	1172.203499	15.887783
25.290942	1165.982230	15.892800
25.181042	1184.668922	15.897818
25.441384	1179.102577	15.902835
25.649807	1173.711574	15.907853
25.233633	1166.726320	15.912871
24.937277	1163.764970	15.917888
25.123524	1164.894111	15.922906
25.406732	1170.022311	15.927923
25.615714	1175.269366	15.932941
25.381357	1175.697139	15.937959
25.276877	1174.138638	15.942976
25.360104	1174.409668	15.947994
25.271957	1176.092769	15.953011
25.583624	1180.089926	15.958029
25.314277	1179.535386	15.963047
25.586180	1170.726254	15.968064
25.593844	1191.316521	15.973082
25.489044	1175.863149	15.978099
25.149513	1175.467859	15.983117
24.810459	1173.690261	15.988135
25.560373	1192.902651	15.993152
25.468732	1190.458530	15.998170
25.587774	1193.267547	16.003187
25.693379	1191.960356	16.008205
25.611473	1197.830216	16.013223
26.078234	1188.094493	16.018240
25.652793	1194.724735	16.023258
25.673330	1185.935798	16.028275
25.821517	1192.868045	16.033293
25.616997	1190.902243	16.038311
25.847081	1210.586905	16.043328
26.062534	1212.939104	16.048346
26.387218	1210.139827	16.053363
26.213343	1210.577119	16.058381
25.998013	1209.285181	16.063399
26.524817	1211.768784	16.068416
26.061592	1197.141212	16.073434
26.094852	1190.265854	16.078451
26.186658	1197.961114	16.083469
26.139070	1203.377511	16.088487
26.167008	1210.353734	16.093504
26.181964	1217.855842	16.098522
26.297455	1220.501315	16.103539
26.553684	1223.165903	16.108557
26.229876	1219.318883	16.113575
26.774120	1212.786835	16.118592
26.309380	1212.729773	16.123610
26.379016	1207.268851	16.128627
26.467514	1213.030134	16.133645
26.676628	1211.817278	16.138663
26.531527	1200.873472	16.143680
26.654690	1197.152525	16.148698
26.397228	1195.056110	16.153715
26.480543	1190.022250	16.158733
26.301722	1205.481859	16.163751
26.905306	1200.818270	16.168768
26.525857	1210.360461	16.173786
26.789535	1207.744251	16.178803
26.958309	1218.602260	16.183821
26.836221	1211.646940	16.188839
26.707187	1189.727962	16.193856
26.828849	1192.214681	16.198874
26.655312	1185.564025	16.203891
26.763025	1194.146739	16.208909
26.499042	1200.388929	16.213927
26.857479	1197.413986	16.218944
26.814071	1209.005611	16.223962
27.130248	1200.994297	16.228979
26.929231	1205.699284	16.233997
27.051187	1211.445890	16.239015
27.038630	1201.305108	16.244032
27.036923	1201.737684	16.249050
26.907829	1203.878441	16.254067
26.887787	1195.455576	16.259085
26.833057	1194.211218	16.264103
26.919226	1189.454623	16.269120
26.852981	1201.620995	16.274138
26.785509	1196.579052	16.279155
27.587711	1201.642235	16.284173
27.016836	1206.739322	16.289191
27.230114	1202.969629	16.294208
26.976135	1201.813097	16.299226
26.936653	1200.635791	16.304243
27.036076	1215.755443	16.309261
26.885380	1225.618631	16.314279
27.256999	1220.647171	16.319296
27.552258	1227.114723	16.324314
27.491918	1226.616002	16.329331
27.398496	1224.740196	16.334349
27.765779	1224.809211	16.339367
27.474103	1227.868373	16.344384
27.365178	1238.618153	16.349402
27.501994	1228.324711	16.354419
27.589850	1225.325621	16.359437
27.328675	1228.941765	16.364455
27.375206	1220.530614	16.369472
27.588851	1227.998635	16.374490
27.777878	1223.573153	16.379507
27.958264	1234.508260	16.384525
27.761574	1237.609439	16.389543
27.645945	1236.330378	16.394560
27.842864	1230.868565	16.399578
27.838598	1234.924392	16.404595
27.772478	1231.024626	16.409613
27.622913	1258.074112	16.414631
28.256054	1253.298611	16.419648
28.102223	1253.612863	16.424666
27.776651	1249.441064	16.429683
28.052469	1250.975987	16.434701
27.886447	1259.216344	16.439719
28.154429	1258.041656	16.444736
27.905189	1251.891911	16.449754
28.147883	1251.705770	16.454771
28.179554	1253.139850	16.459789
27.892491	1252.102073	16.464807
27.938989	1255.941718	16.469824
28.352674	1255.116730	16.474842
28.230081	1252.803651	16.479859
28.347016	1241.449793	16.484877
28.139113	1250.731767	16.489895
28.073812	1248.185707	16.494912
28.310812	1249.770854	16.499930
28.320815	1253.714010	16.504947
28.428510	1250.367845	16.509965
28.151447	1258.183678	16.514983
28.333630	1252.272875	16.520000
28.436268	1251.985464	16.525018
28.498228	1261.023456	16.530035
28.502060	1266.835808	16.535053
28.467072	1274.626582	16.540071
28.371773	1266.884431	16.545088
28.458347	1262.815718	16.550106
28.591083	1273.723553	16.555123
28.596273	1275.537298	16.560141
28.561875	1274.665309	16.565159
28.780623	1274.280924	16.570176
28.827304	1272.840891	16.575194
28.835098	1274.789929	16.580211
29.062726	1270.967496	16.585229
28.756008	1275.038864	16.590247
28.407448	1273.452084	16.595264
28.964382	1270.193760	16.600282
28.764919	1277.129675	16.605299
28.950917	1274.916870	16.610317
28.438266	1274.273976	16.615335
28.516447	1264.977408	16.620352
29.010149	1279.388788	16.625370
28.904704	1288.093097	16.630387
29.234437	1290.380177	16.635405
29.144207	1287.677046	16.640423
29.314227	1290.702204	16.645440
29.908276	1292.304348	16.650458
29.469928	1283.050322	16.655475
29.321175	1267.651051	16.660493
29.399045	1266.884658	16.665511
29.478391	1262.526737	16.670528
29.388011	1261.404689	16.675546
29.501766	1261.541579	16.680563
29.665730	1266.420130	16.685581
29.359314	1261.977103	16.690599
29.558579	1256.530697	16.695616
29.464666	1254.137413	16.700634
29.465189	1258.874151	16.705651
29.441680	1251.827728	16.710669
29.272100	1266.326588	16.715687
29.287064	1262.912807	16.720704
29.519756	1262.643017	16.725722
29.374058	1280.461226	16.730739
29.741426	1279.940094	16.735757
29.429708	1282.895088	16.740775
29.472768	1276.725070	16.745792
29.593015	1289.954374	16.750810
29.654145	1295.524286	16.755827
29.876319	1280.168238	16.760845
29.767666	1287.377196	16.765863
29.468612	1284.883304	16.770880
29.766749	1283.464079	16.775898
29.695457	1284.349303	16.780915
29.856837	1301.236098	16.785933
29.817719	1301.895408	16.790951
29.888739	1314.829438	16.795968
30.183521	1308.367753	16.800986
30.316301	1309.356906	16.806003
30.115657	1304.758544	16.811021
30.308427	1308.240911	16.816039
30.161825	1303.927626	16.821056
30.068009	1309.035672	16.826074
30.419726	1308.611649	16.831091
30.354712	1310.619365	16.836109
30.442502	1306.260119	16.841127
30.251701	1309.120551	16.846144
30.683742	1301.946377	16.851162
30.221418	1308.793842	16.856179
30.436301	1306.096853	16.861197
30.274825	1308.447791	16.866215
30.072317	1306.936098	16.871232
30.453214	1304.153301	16.876250
30.258288	1309.280245	16.881267
30.656736	1302.818201	16.886285
30.577705	1307.210733	16.891303
30.095376	1311.318918	16.896320
30.494081	1302.417395	16.901338
30.498911	1304.739284	16.906355
30.721337	1300.851382	16.911373
30.485762	1308.831192	16.916391
30.565378	1322.316154	16.921408
31.022812	1325.485918	16.926426
30.773792	1329.576717	16.931443
30.919458	1325.741787	16.936461
30.929042	1328.814021	16.941479
30.739949	1333.602392	16.946496
31.322180	1331.062800	16.951514
31.519703	1323.117242	16.956531
30.855082	1300.442071	16.961549
30.584829	1311.731409	16.966567
30.755535	1318.732783	16.971584
30.973013	1316.833808	16.976602
31.199264	1322.182359	16.981619
31.191195	1319.734675	16.986637
31.265253	1315.267111	16.991655
31.214349	1317.054880	16.996672
31.204456	1324.027570	17.001690
31.245454	1319.846018	17.006707
31.496878	1320.804076	17.011725
31.634885	1331.859450	17.016743
31.226343	1332.667797	17.021760
31.901455	1321.776094	17.026778
31.200539	1318.893484	17.031795
31.522749	1328.755683	17.036813
31.390656	1325.771885	17.041831
31.297079	1326.338689	17.046848
31.497364	1335.314157	17.051866
31.101617	1327.845976	17.056883
31.683024	1322.466284	17.061901
31.295861	1319.418059	17.066919
31.597016	1325.007414	17.071936
31.486090	1326.072381	17.076954
31.660077	1326.086285	17.081971
31.405562	1322.569282	17.086989
32.008116	1336.029641	17.092007
31.740200	1346.488659	17.097024
31.753060	1347.925675	17.102042
31.849457	1360.338233	17.107059
31.978566	1357.556761	17.112077
31.910278	1348.797351	17.117095
31.984356	1358.183802	17.122112
31.999460	1343.803528	17.127130
31.843111	1347.867279	17.132147
31.710967	1350.115826	17.137165
31.974731	1346.060532	17.142183
31.771856	1352.119691	17.147200
31.997929	1341.367317	17.152218
31.987869	1349.955819	17.157235
32.005539	1347.330554	17.162253
32.293331	1358.274260	17.167271
31.829022	1370.367024	17.172288
32.082895	1367.711292	17.177306
32.148743	1372.396865	17.182323
32.195004	1376.283909	17.187341
32.322937	1373.291178	17.192359
32.612742	1375.505590	17.197376
33.016004	1368.616737	17.202394
32.714522	1379.731099	17.207411
32.943319	1360.539631	17.212429
33.089379	1364.041904	17.217447
32.575564	1368.483210	17.222464
32.936879	1361.698721	17.227482
32.645406	1356.215080	17.232499
32.744787	1351.759343	17.237517
32.819585	1340.468788	17.242535
32.309781	1346.080270	17.247552
32.988332	1356.533945	17.252570
32.564247	1370.252003	17.257587
32.400512	1367.497188	17.262605
33.063717	1370.597053	17.267623
32.775535	1377.553131	17.272640
32.954200	1373.129226	17.277658
32.626093	1369.308090	17.282675
32.388262	1366.192425	17.287693
32.389816	1372.500630	17.292711
33.079837	1390.365558	17.297728
33.380212	1382.987787	17.302746
33.318486	1394.661280	17.307763
33.035224	1391.350711	17.312781
33.551948	1383.895074	17.317799
32.733930	1385.000708	17.322816
32.900375	1385.350303	17.327834
33.184835	1386.716634	17.332851
33.359840	1390.896063	17.337869
33.432734	1386.406572	17.342887
33.528373	1398.412173	17.347904
33.298824	1384.287710	17.352922
33.502529	1394.550250	17.357939
33.418066	1393.345221	17.362957
33.500506	1390.069234	17.367975
33.373810	1392.320093	17.372992
33.472029	1385.059003	17.378010
33.847390	1386.736230	17.383027
33.405767	1387.862156	17.388045
33.612389	1383.313975	17.393063
33.567393	1378.413649	17.398080
33.837684	1372.637411	17.403098
33.719373	1380.990317	17.408115
33.522304	1391.678173	17.413133
34.027644	1399.940300	17.418151
34.082628	1405.621657	17.423168
34.350549	1396.677333	17.428186
34.466248	1382.672687	17.433203
34.177453	1383.156278	17.438221
34.237456	1366.187535	17.443239
34.034537	1368.696412	17.448256
34.161146	1364.078642	17.453274
34.191627	1365.541319	17.458291
34.144068	1379.020879	17.463309
34.342667	1371.709452	17.468327
34.149551	1370.000631	17.473344
34.301762	1362.699586	17.478362
34.426097	1365.836012	17.483379
34.070042	1371.735990	17.488397
34.209870	1366.330362	17.493415
33.970092	1376.721901	17.498432
34.587898	1394.108924	17.503450
34.654845	1390.611285	17.508467
34.308359	1399.176451	17.513485
34.409095	1389.447115	17.518503
34.476081	1390.361309	17.523520
34.389290	1397.232390	17.528538
34.428431	1386.720534	17.533555
34.281848	1399.246689	17.538573
34.886677	1387.655829	17.543591
34.662031	1393.219772	17.548608
34.696183	1395.464523	17.553626
34.656398	1391.898295	17.558643
34.801155	1390.954225	17.563661
35.065698	1392.617148	17.568679
35.103246	1382.938679	17.573696
35.174305	1385.326006	17.578714
35.069424	1376.436580	17.583731
34.869385	1380.664933	17.588749
35.001723	1383.825362	17.593767
35.401249	1390.402972	17.598784
35.151539	1389.876927	17.603802
35.254587	1389.204439	17.608819
35.032226	1394.685976	17.613837
35.341225	1388.446112	17.618855
35.086327	1386.541780	17.623872
35.230528	1383.290892	17.628890
35.359735	1386.303486	17.633907
35.133980	1388.525587	17.638925
35.016721	1388.360773	17.643943
35.098852	1395.322319	17.648960
35.132555	1405.731256	17.653978
35.341950	1410.388177	17.658995
35.377901	1424.211377	17.664013
35.753602	1408.329538	17.669031
35.834419	1410.440793	17.674048
35.197136	1414.282791	17.679066
35.567690	1406.771007	17.684083
35.392560	1414.403780	17.689101
35.743467	1410.704135	17.694119
35.488128	1417.374247	17.699136
35.665488	1413.427065	17.704154
35.625693	1413.300684	17.709171
35.625224	1428.571770	17.714189
35.985167	1441.855386	17.719207
35.966343	1445.957709	17.724224
36.077078	1441.026807	17.729242
36.296074	1441.873155	17.734259
36.197039	1447.581661	17.739277
36.097946	1435.876302	17.744295
36.060354	1424.931398	17.749312
36.224220	1436.645535	17.754330
36.203600	1440.703954	17.759347
36.107585	1439.301903	17.764365
36.399939	1436.431885	17.769383
36.417189	1446.830784	17.774400
36.332496	1440.099928	17.779418
36.197186	1438.628255	17.784435
36.163338	1436.440191	17.789453
36.461426	1431.079332	17.794471
36.327930	1439.873289	17.799488
36.208681	1435.135988	17.804506
36.471330	1431.825624	17.809523
36.453365	1441.690356	17.814541
36.537037	1431.891069	17.819559
36.638973	1434.513438	17.824576
36.423788	1434.616337	17.829594
36.370213	1431.484597	17.834611
36.464559	1443.086484	17.839629
36.599785	1450.734068	17.844647
36.501751	1456.148928	17.849664
37.015168	1456.182569	17.854682
37.107210	1457.859733	17.859699
37.069840	1466.133804	17.864717
36.763615	1465.774346	17.869735
37.223773	1458.396914	17.874752
36.963307	1463.347912	17.879770
37.199929	1458.870781	17.884787
37.179073	1461.262962	17.889805
37.208048	1461.037510	17.894823
37.127071	1461.835888	17.899840
37.311599	1457.878112	17.904858
37.706381	1462.837546	17.909875
37.548565	1462.129931	17.914893
37.742696	1455.210489	17.919911
37.718428	1457.587422	17.924928
36.999193	1449.831880	17.929946
37.411766	1442.935238	17.934963
37.249398	1447.271350	17.939981
37.574625	1451.332730	17.944999
37.786594	1449.778585	17.950016
37.543927	1457.390332	17.955034
37.632449	1441.953967	17.960051
37.400260	1447.847308	17.965069
37.295969	1456.371637	17.970087
37.413340	1454.201052	17.975104
37.461257	1454.995141	17.980122
37.815904	1453.655468	17.985139
37.444866	1449.752635	17.990157
36.959520	1460.930389	17.995175
37.757452	1475.048406	18.000192
37.597368	1482.082411	18.005210
37.883005	1479.185030	18.010227
38.177666	1485.384523	18.015245
37.712866	1481.117580	18.020263
38.080930	1478.810130	18.025280
37.724965	1490.075056	18.030298
37.930826	1490.904517	18.035315
37.985741	1496.724770	18.040333
38.408402	1497.015541	18.045351
38.152036	1496.755619	18.050368
38.099519	1497.489606	18.055386
38.318536	1499.582511	18.060403
37.942386	1498.634330	18.065421
37.945897	1507.227106	18.070439
38.272846	1499.299190	18.075456
37.920912	1499.508588	18.080474
38.438835	1513.408297	18.085491
38.558058	1520.146363	18.090509
38.607236	1523.761584	18.095527
38.882762	1526.767200	18.100544
38.890092	1523.234635	18.105562
38.865455	1522.288530	18.110579
38.753075	1526.039359	18.115597
38.833326	1530.353496	18.120615
39.167268	1518.274546	18.125632
38.938596	1520.976805	18.130650
38.959285	1512.528513	18.135667
39.128055	1522.989073	18.140685
38.917983	1511.793256	18.145703
39.285897	1510.858617	18.150720
39.264463	1522.529076	18.155738
39.051621	1516.231559	18.160755
38.975212	1517.723513	18.165773
38.709626	1518.373909	18.170791
39.085904	1521.231292	18.175808
38.763543	1521.287762	18.180826
39.321074	1519.888093	18.185843
39.534498	1527.397301	18.190861
39.231927	1522.713766	18.195879
39.343463	1523.239173	18.200896
39.463816	1530.712379	18.205914
39.639697	1529.302703	18.210931
39.729085	1542.489661	18.215949
39.298157	1534.809117	18.220967
39.889752	1539.671656	18.225984
39.878694	1546.622523	18.231002
39.820913	1538.006554	18.236019
39.641430	1521.418937	18.241037
39.895402	1532.052432	18.246055
39.661597	1528.775164	18.251072
39.735989	1546.303748	18.256090
39.878068	1537.044428	18.261107
40.021642	1535.267390	18.266125
39.838126	1536.365763	18.271143
40.260888	1535.394180	18.276160
39.946243	1537.756373	18.281178
39.964535	1537.093920	18.286195
40.123873	1532.862336	18.291213
39.865751	1541.666280	18.296231
40.074007	1531.298424	18.301248
39.797424	1534.273235	18.306266
40.078067	1547.354679	18.311283
39.722681	1538.431591	18.316301
39.663081	1545.421574	18.321319
40.223175	1559.422052	18.326336
40.512156	1562.027941	18.331354
40.359040	1557.901804	18.336371
40.718041	1560.689299	18.341389
40.701762	1559.700864	18.346407
40.925087	1554.465219	18.351424
40.568540	1558.547565	18.356442
40.687542	1552.905278	18.361459
40.793158	1555.012689	18.366477
40.627524	1555.827408	18.371495
41.009956	1552.583580	18.376512
40.999567	1557.555630	18.381530
40.803388	1558.113168	18.386547
40.831531	1549.291309	18.391565
40.756867	1553.064674	18.396583
40.805860	1552.776143	18.401600
40.623643	1547.426914	18.406618
40.787961	1549.907042	18.411635
41.103368	1554.383391	18.416653
41.007143	1578.408066	18.421671
41.324868	1572.690651	18.426688
41.365205	1589.287292	18.431706
40.863852	1584.792482	18.436723
41.373833	1579.322848	18.441741
40.754373	1583.392484	18.446759
41.384685	1567.688617	18.451776
41.335379	1574.825334	18.456794
41.154044	1580.108032	18.461811
41.386686	1578.257162	18.466829
41.098553	1584.234998	18.471847
41.356612	1594.609113	18.476864
41.772466	1595.061895	18.481882
41.816783	1594.935040	18.486899
41.931119	1598.199298	18.491917
41.823664	1601.075204	18.496935
41.945535	1594.185894	18.501952
41.872552	1601.222164	18.506970
41.890905	1598.514704	18.511987
41.843367	1589.291191	18.517005
41.858642	1603.641621	18.522023
41.786269	1595.349794	18.527040
41.837095	1594.174181	18.532058
41.759456	1595.559034	18.537075
41.884462	1598.218862	18.542093
42.037100	1605.892204	18.547111
42.155562	1608.174350	18.552128
42.366246	1617.321913	18.557146
42.451008	1619.669269	18.562163
42.495754	1618.257911	18.567181
42.599106	1614.634638	18.572199
42.758238	1607.398689	18.577216
42.484403	1601.662913	18.582234
42.284075	1592.561018	18.587251
42.557747	1596.718822	18.592269
42.233668	1620.078428	18.597287
42.841436	1616.127307	18.602304
42.747487	1614.219982	18.607322
42.681724	1628.832363	18.612339
42.988679	1627.563220	18.617357
42.793428	1617.494828	18.622375
42.795742	1629.123789	18.627392
42.739928	1624.266105	18.632410
42.443038	1613.553965	18.637427
42.876800	1611.756986	18.642445
42.768117	1615.592467	18.647463
42.940773	1615.723346	18.652480
42.857465	1622.672868	18.657498
42.598075	1628.876622	18.662515
42.852369	1626.261813	18.667533
43.200703	1644.410574	18.672551
43.272997	1634.928534	18.677568
43.510212	1651.510358	18.682586
43.382905	1651.337639	18.687603
43.241528	1646.385972	18.692621
43.442920	1643.340732	18.697639
43.940409	1633.584204	18.702656
43.823214	1642.684998	18.707674
43.534262	1634.688810	18.712691
44.046358	1637.831185	18.717709
43.602575	1641.090827	18.722727
43.636381	1630.563878	18.727744
43.601791	1637.553159	18.732762
43.684522	1640.756073	18.737779
43.780241	1639.147425	18.742797
43.706690	1636.630997	18.747815
43.885576	1631.784108	18.752832
43.848963	1639.398565	18.757850
43.629125	1634.257142	18.762867
43.875618	1629.077830	18.767885
43.956498	1631.280621	18.772903
44.290368	1630.692110	18.777920
44.181661	1637.781295	18.782938
44.089637	1632.023514	18.787955
44.068480	1640.361415	18.792973
43.750659	1649.061095	18.797991
44.118732	1657.874900	18.803008
44.263560	1661.506815	18.808026
44.233550	1654.631661	18.813043
44.413683	1664.822287	18.818061
43.957437	1657.095137	18.823079
44.208641	1651.473263	18.828096
44.180535	1663.662415	18.833114
44.627107	1676.011205	18.838131
44.706901	1667.777705	18.843149
44.794139	1676.931895	18.848167
45.005818	1670.202147	18.853184
45.183640	1674.327555	18.858202
45.000948	1676.116943	18.863219
45.164885	1673.383649	18.868237
45.113102	1683.761875	18.873255
44.859364	1679.083318	18.878272
45.140675	1673.314736	18.883290
44.978947	1669.944166	18.888307
44.713128	1670.616695	18.893325
45.062761	1672.064421	18.898343
45.163917	1675.614774	18.903360
45.166330	1675.289311	18.908378
45.010520	1678.466254	18.913395
45.395265	1669.759231	18.918413
45.074641	1672.946054	18.923431
45.173073	1667.622521	18.928448
45.255210	1682.704235	18.933466
45.336466	1691.853053	18.938483
45.890286	1689.791216	18.943501
45.935726	1698.749950	18.948519
45.886371	1690.590197	18.953536
45.947821	1676.505403	18.958554
45.450868	1675.156290	18.963571
45.841556	1680.428853	18.968589
46.135058	1690.043253	18.973607
45.840346	1691.209441	18.978624
46.409205	1685.579125	18.983642
46.009011	1682.024770	18.988659
45.853908	1664.975623	18.993677
45.833009	1677.072141	18.998695
46.070525	1680.235184	19.003712
46.171326	1676.587048	19.008730
46.186629	1685.752444	19.013747
46.491255	1684.234346	19.018765
46.070946	1687.133727	19.023783
46.277151	1683.232489	19.028800
46.129446	1683.665717	19.033818
46.120258	1685.166155	19.038835
46.645246	1684.124999	19.043853
46.507243	1674.558913	19.048871
46.348389	1681.684326	19.053888
46.463593	1683.004447	19.058906
46.357874	1684.327406	19.063923
46.869689	1680.135584	19.068941
46.748192	1688.217725	19.073959
46.713534	1686.149679	19.078976
46.936752	1698.457519	19.083994
46.823701	1714.229227	19.089011
46.987380	1710.517645	19.094029
47.281918	1711.008254	19.099047
46.732377	1715.215359	19.104064
46.992967	1717.762575	19.109082
46.744597	1710.463795	19.114099
47.183292	1714.425516	19.119117
47.353793	1713.957115	19.124135
46.994437	1713.372389	19.129152
46.870383	1712.886731	19.134170
47.129816	1718.817229	19.139187
46.863451	1712.666834	19.144205
47.264491	1734.222141	19.149223
47.240106	1732.982488	19.154240
47.430025	1727.881384	19.159258
47.427873	1742.884751	19.164275
47.610437	1733.896744	19.169293
47.930422	1738.432388	19.174311
47.627872	1731.542832	19.179328
47.663671	1728.573854	19.184346
47.635335	1739.084164	19.189363
47.873900	1729.465731	19.194381
47.939819	1732.308352	19.199399
47.417886	1738.584579	19.204416
48.068744	1741.471832	19.209434
48.256375	1753.561183	19.214451
48.629711	1751.224475	19.219469
48.523341	1734.820941	19.224487
48.577883	1736.478723	19.229504
48.617888	1732.792704	19.234522
48.568995	1720.931016	19.239539
48.620410	1707.892355	19.244557
48.631428	1710.879224	19.249575
48.677422	1720.226055	19.254592
48.750332	1712.081971	19.259610
48.652491	1716.029397	19.264627
48.664080	1718.728993	19.269645
48.866303	1719.161390	19.274663
48.765652	1719.965998	19.279680
49.075149	1718.974171	19.284698
48.761704	1719.120772	19.289715
48.896486	1713.352899	19.294733
48.962705	1706.620537	19.299751
48.677816	1719.768068	19.304768
48.761388	1716.592833	19.309786
48.671681	1713.037468	19.314803
48.579161	1713.610431	19.319821
48.803515	1708.260970	19.324839
48.625995	1708.250706	19.329856
49.167643	1722.642358	19.334874
49.344304	1735.938951	19.339891
49.397423	1733.387007	19.344909
49.275130	1732.370886	19.349927
49.101204	1733.508803	19.354944
49.242240	1734.471448	19.359962
49.439374	1737.817517	19.364979
49.123051	1744.572986	19.369997
48.759058	1729.528727	19.375015
49.032875	1742.608222	19.380032
49.397715	1753.846297	19.385050
49.066302	1760.641993	19.390067
48.942757	1765.975710	19.395085
49.748973	1775.172649	19.400103
49.720807	1791.114250	19.405120
50.164155	1790.057397	19.410138
50.226900	1800.320026	19.415155
50.396695	1793.574661	19.420173
50.497439	1769.309081	19.425191
50.634019	1761.871448	19.430208
50.760525	1742.089566	19.435226
50.677786	1745.330885	19.440243
50.208426	1750.336577	19.445261
50.393476	1750.916819	19.450279
50.483398	1752.572250	19.455296
50.755670	1752.072222	19.460314
50.703068	1742.495959	19.465331
50.482281	1746.718160	19.470349
50.719951	1733.764093	19.475367
50.550849	1745.773278	19.480384
50.405979	1735.611765	19.485402
50.380649	1740.538854	19.490419
50.344727	1738.859173	19.495437
50.538912	1743.827826	19.500455
50.915854	1762.720199	19.505472
50.929149	1761.152776	19.510490
50.843576	1767.067577	19.515507
50.654620	1773.254102	19.520525
51.138626	1760.144896	19.525543
51.053444	1772.333541	19.530560
51.128819	1767.812008	19.535578
50.924387	1774.379650	19.540595
51.030549	1773.482596	19.545613
50.875247	1763.663528	19.550631
50.757723	1778.542873	19.555648
51.026980	1780.227191	19.560666
51.055529	1782.996741	19.565683
51.132836	1794.917100	19.570701
51.564358	1783.103652	19.575719
51.496755	1799.038777	19.580736
51.568972	1809.170546	19.585754
51.539625	1813.151511	19.590771
51.705209	1809.912996	19.595789
51.835474	1807.197548	19.600807
51.923405	1810.270291	19.605824
52.011391	1808.104239	19.610842
51.905847	1808.855963	19.615859
51.701473	1805.473072	19.620877
51.973041	1799.118970	19.625895
51.879600	1799.821470	19.630912
51.994909	1799.014512	19.635930
51.935492	1805.632173	19.640947
52.272180	1813.330599	19.645965
52.758600	1814.428827	19.650983
52.264801	1812.078792	19.656000
52.359635	1816.523276	19.661018
52.573459	1819.630070	19.666035
52.491547	1823.139525	19.671053
52.853989	1830.849729	19.676071
52.982678	1837.059407	19.681088
52.568620	1819.734839	19.686106
53.031278	1817.052846	19.691123
52.743421	1823.728172	19.696141
52.701911	1819.114368	19.701159
52.770226	1825.507016	19.706176
52.988106	1823.494313	19.711194
52.897868	1826.342327	19.716211
52.895017	1821.795089	19.721229
53.225393	1819.247304	19.726247
53.026287	1816.655721	19.731264
53.188529	1815.828831	19.736282
53.204595	1827.742967	19.741299
53.388454	1831.567661	19.746317
53.223614	1821.153582	19.751335
52.816310	1828.797431	19.756352
53.246466	1831.053168	19.761370
53.340318	1841.951626	19.766387
53.172354	1852.748839	19.771405
53.814423	1857.436346	19.776423
53.783472	1850.087877	19.781440
53.400434	1853.019353	19.786458
53.732632	1850.250367	19.791475
53.365813	1841.054343	19.796493
53.812327	1858.692560	19.801511
53.926690	1862.559640	19.806528
53.983050	1869.134051	19.811546
54.363852	1869.844771	19.816563
54.250217	1872.668032	19.821581
54.357114	1874.579615	19.826599
54.158088	1870.757208	19.831616
54.019005	1868.468707	19.836634
54.212783	1868.274398	19.841651
54.147084	1868.644367	19.846669
54.143612	1870.254388	19.851687
54.536219	1869.161247	19.856704
54.294649	1864.916262	19.861722
54.371176	1866.217172	19.866739
54.411575	1876.710550	19.871757
54.559043	1883.201351	19.876775
54.403509	1893.507487	19.881792
54.617315	1889.813311	19.886810
54.998636	1894.831768	19.891827
54.805593	1894.217986	19.896845
54.789395	1887.933903	19.901863
55.014580	1898.464798	19.906880
54.694856	1888.917422	19.911898
55.029795	1895.849270	19.916915
55.364457	1902.266751	19.921933
55.338929	1906.089347	19.926951
55.310341	1910.903377	19.931968
55.277558	1909.144293	19.936986
55.578172	1917.817247	19.942003
55.732523	1921.018528	19.947021
55.817478	1912.089810	19.952039
55.877033	1906.504007	19.957056
55.726787	1892.764438	19.962074
55.758657	1889.960151	19.967091
55.834485	1882.825426	19.972109
55.847570	1877.190061	19.977127
55.794733	1885.608750	19.982144
55.534532	1900.453605	19.987162
55.788694	1901.344995	19.992179
55.842626	1916.412362	19.997197
56.078584	1911.171490	20.002215
56.138922	1910.859096	20.007232
56.016778	1906.756458	20.012250
56.192027	1909.635736	20.017267
55.940403	1916.302299	20.022285
56.059207	1904.878299	20.027303
56.248387	1908.967278	20.032320
56.036191	1917.798971	20.037338
56.397701	1924.606769	20.042355
56.211296	1933.803697	20.047373
56.768701	1926.559260	20.052391
56.649858	1929.320222	20.057408
56.495081	1927.848384	20.062426
56.715559	1930.695376	20.067443
56.251462	1935.618246	20.072461
56.772253	1937.683153	20.077479
56.612350	1945.821884	20.082496
56.880480	1954.051772	20.087514
57.331425	1954.723172	20.092531
57.042191	1956.229363	20.097549
57.090464	1947.341054	20.102567
56.945132	1947.073305	20.107584
56.918732	1952.641270	20.112602
57.295713	1954.378263	20.117619
57.089943	1955.271834	20.122637
57.685315	1967.869069	20.127655
57.784080	1966.809049	20.132672
57.329657	1971.831412	20.137690
57.460597	1969.485077	20.142707
57.789679	1978.519715	20.147725
57.481246	1964.552245	20.152743
57.968967	1969.487884	20.157760
57.836495	1974.280234	20.162778
57.863563	1969.964994	20.167795
57.739754	1968.762896	20.172813
57.737151	1972.269500	20.177831
57.816828	1977.533769	20.182848
57.808814	1982.029022	20.187866
58.507458	1984.975151	20.192883
58.468158	1995.178039	20.197901
58.502865	1985.632234	20.202919
58.641495	1989.069514	20.207936
58.607200	1990.974689	20.212954
58.573423	1980.085657	20.217971
58.538945	1981.713139	20.222989
58.875104	1987.287785	20.228007
59.041448	1981.259282	20.233024
58.369441	1986.198756	20.238042
58.934719	1983.317719	20.243059
58.594082	1985.441009	20.248077
58.805199	1978.581839	20.253095
59.080047	1978.513767	20.258112
58.878561	1977.462623	20.263130
59.057582	1983.490939	20.268147
58.864653	1984.350953	20.273165
59.068185	1975.135489	20.278183
59.046693	1979.437173	20.283200
58.697998	1992.758946	20.288218
59.312291	1995.743457	20.293235
59.391906	2010.538651	20.298253
59.126292	2011.615118	20.303271
59.606535	2003.297025	20.308288
59.555635	2012.116275	20.313306
59.586107	1998.001336	20.318323
59.558266	2003.670531	20.323341
59.583252	2007.368514	20.328359
59.457271	2005.163166	20.333376
59.736037	2010.942423	20.338394
60.174521	2021.156147	20.343411
60.055527	2032.340335	20.348429
60.168316	2032.521566	20.353447
60.188730	2034.888463	20.358464
60.093190	2032.940314	20.363482
60.163452	2044.208657	20.368499
60.160315	2027.406913	20.373517
60.187151	2021.419053	20.378535
60.337877	2026.533412	20.383552
60.174110	2021.443110	20.388570
60.438254	2025.043899	20.393587
60.589084	2020.330666	20.398605
60.374753	2029.787621	20.403623
60.551707	2031.189677	20.408640
60.219170	2043.827290	20.413658
60.442395	2042.899372	20.418675
60.186572	2054.534085	20.423693
60.767980	2052.537344	20.428711
61.149013	2058.799333	20.433728
60.950691	2069.800227	20.438746
61.699418	2069.443770	20.443763
61.171010	2074.698596	20.448781
61.516434	2082.061249	20.453799
61.483236	2067.659509	20.458816
61.586092	2056.925891	20.463834
61.454697	2057.208259	20.468851
61.430008	2066.834531	20.473869
61.544664	2068.628158	20.478887
61.819849	2069.390046	20.483904
61.687456	2073.806853	20.488922
61.805097	2068.988317	20.493939
61.825072	2070.736722	20.498957
61.759882	2076.923018	20.503975
62.122583	2067.262985	20.508992
62.037677	2073.547027	20.514010
62.130815	2066.643074	20.519027
62.122296	2065.735457	20.524045
62.026848	2065.952265	20.529063
62.337929	2066.326696	20.534080
62.392669	2061.609478	20.539098
61.833115	2055.611913	20.544115
62.191123	2066.668205	20.549133
62.373894	2085.726857	20.554151
62.626408	2083.304772	20.559168
62.898487	2087.289363	20.564186
62.714702	2082.893311	20.569203
62.647112	2088.963215	20.574221
62.284226	2090.676553	20.579239
62.663454	2078.962576	20.584256
62.798696	2086.190690	20.589274
62.745701	2078.889743	20.594291
62.879547	2076.937435	20.599309
62.760442	2090.261405	20.604327
62.954524	2098.029497	20.609344
62.850756	2101.630776	20.614362
62.823549	2098.337016	20.619379
63.133269	2101.435241	20.624397
63.176422	2095.735162	20.629415
63.696891	2110.670093	20.634432
63.711007	2128.199166	20.639450
63.895792	2115.653864	20.644467
63.892035	2101.159146	20.649485
63.775016	2099.410003	20.654503
63.712785	2088.774655	20.659520
63.693286	2102.130465	20.664538
63.635589	2110.218642	20.669555
64.306550	2113.844477	20.674573
64.190757	2117.122569	20.679591
64.208273	2125.072804	20.684608
63.743817	2124.264574	20.689626
63.877750	2122.353275	20.694643
64.397897	2119.977883	20.699661
64.423952	2112.986522	20.704679
64.628978	2098.654969	20.709696
64.334426	2107.783613	20.714714
64.135954	2115.016356	20.719731
64.496810	2110.765884	20.724749
64.217321	2117.985995	20.729767
64.550755	2129.456426	20.734784
64.568686	2137.431850	20.739802
64.589415	2125.701072	20.744819
64.663461	2130.047880	20.749837
64.665304	2130.221138	20.754855
65.162511	2126.482790	20.759872
64.699825	2141.157388	20.764890
65.225315	2150.546560	20.769907
65.733533	2152.367286	20.774925
65.317802	2159.709617	20.779943
65.872201	2158.745912	20.784960
65.601502	2158.857457	20.789978
65.599860	2161.511840	20.794995
65.721829	2152.959111	20.800013
65.551504	2156.700158	20.805031
65.841865	2152.347037	20.810048
65.728833	2152.882180	20.815066
65.574326	2160.903398	20.820083
65.941409	2160.451718	20.825101
65.761643	2151.005493	20.830119
65.974630	2142.561680	20.835136
65.599481	2153.183038	20.840154
65.734205	2155.462722	20.845171
66.124385	2160.341013	20.850189
66.331634	2174.917646	20.855207
66.668426	2176.260112	20.860224
66.575901	2180.673894	20.865242
66.511937	2185.259964	20.870259
66.414437	2173.329801	20.875277
66.663967	2185.438211	20.880295
66.759619	2174.364799	20.885312
66.441225	2186.489045	20.890330
66.290591	2179.493608	20.895347
66.689414	2182.906194	20.900365
66.600952	2192.876996	20.905383
66.987843	2199.845058	20.910400
67.173283	2196.259382	20.915418
66.947209	2194.341007	20.920435
66.981275	2193.347854	20.925453
66.776285	2197.791774	20.930471
67.073962	2198.480735	20.935488
67.684236	2214.045587	20.940506
67.725002	2231.722099	20.945523
67.686066	2224.090683	20.950541
67.405379	2229.423756	20.955559
67.837249	2224.682494	20.960576
67.862929	2222.933213	20.965594
68.045528	2220.966986	20.970611
68.177564	2226.062222	20.975629
67.675140	2218.862751	20.980647
67.668464	2222.821342	20.985664
67.929077	2218.539112	20.990682
67.801361	2227.061143	20.995699
68.280767	2210.840540	21.000717
68.142169	2229.794738	21.005735
68.086767	2218.325073	21.010752
68.449431	2226.294204	21.015770
68.492329	2231.794659	21.020787
68.453179	2237.847562	21.025805
68.705956	2246.247242	21.030823
68.848545	2247.768280	21.035840
68.683899	2252.758228	21.040858
68.595531	2249.925266	21.045875
68.736069	2242.720359	21.050893
68.723111	2246.629438	21.055911
68.829724	2247.629030	21.060928
68.858703	2246.762905	21.065946
68.810534	2260.164325	21.070963
68.993999	2268.013043	21.075981
69.236724	2267.015803	21.080999
68.991049	2262.818701	21.086016
69.124556	2265.401563	21.091034
69.093474	2269.427083	21.096051
69.361047	2273.036857	21.101069
69.640791	2291.853400	21.106087
69.889700	2287.468829	21.111104
69.895774	2279.394857	21.116122
69.698268	2288.745181	21.121139
70.039342	2281.108228	21.126157
70.212106	2288.554656	21.131175
70.273858	2281.150550	21.136192
70.288028	2281.255614	21.141210
70.407462	2285.690073	21.146227
70.424608	2286.684661	21.151245
70.213065	2286.269415	21.156263
70.195975	2294.165150	21.161280
70.497277	2279.061028	21.166298
70.580192	2277.646833	21.171315
70.236450	2284.441489	21.176333
70.506447	2291.970615	21.181351
70.300602	2298.756431	21.186368
70.835552	2302.939999	21.191386
70.651794	2309.166927	21.196403
71.273002	2310.155835	21.201421
71.065927	2302.298085	21.206439
70.774055	2301.557656	21.211456
70.893755	2300.115639	21.216474
71.010040	2320.040163	21.221491
71.184778	2321.190107	21.226509
71.411630	2323.723728	21.231527
71.504524	2327.578472	21.236544
71.437484	2323.776446	21.241562
71.147970	2332.853923	21.246579
71.452780	2319.718558	21.251597
71.365155	2332.286683	21.256615
71.477058	2345.369737	21.261632
71.844692	2348.114986	21.266650
71.732309	2351.834428	21.271667
71.932344	2347.287028	21.276685
71.868417	2355.644545	21.281703
71.809323	2359.466152	21.286720
72.201527	2356.258532	21.291738
72.067136	2373.208171	21.296755
71.852661	2369.031435	21.301773
72.209647	2371.907741	21.306791
72.385250	2371.116617	21.311808
72.285200	2368.982930	21.316826
72.737688	2376.688819	21.321843
72.868230	2385.420040	21.326861
73.032990	2390.709055	21.331879
73.018145	2393.687440	21.336896
73.402727	2385.844841	21.341914
72.995400	2368.862694	21.346931
73.115757	2357.558092	21.351949
73.264909	2372.898214	21.356967
73.396852	2385.883498	21.361984
73.205819	2391.474076	21.367002
73.109803	2393.243727	21.372019
73.599429	2390.816245	21.377037
73.147351	2390.006075	21.382055
73.437075	2398.068694	21.387072
73.626714	2385.882232	21.392090
73.530603	2392.543694	21.397107
73.759854	2390.071538	21.402125
73.692655	2397.703705	21.407143
73.930014	2412.152759	21.412160
74.334737	2412.563114	21.417178
73.922539	2409.594341	21.422195
74.433708	2413.257741	21.427213
74.612266	2420.027937	21.432231
74.184742	2419.062455	21.437248
74.648835	2414.899987	21.442266
74.241130	2416.626645	21.447283
74.608850	2407.880888	21.452301
74.839535	2409.170460	21.457319
74.830334	2413.899550	21.462336
74.510775	2400.962328	21.467354
74.786951	2406.192973	21.472371
74.832715	2403.828283	21.477389
74.855226	2396.446019	21.482407
74.557253	2414.948670	21.487424
75.041824	2416.012510	21.492442
74.958921	2422.981216	21.497459
74.987378	2406.912702	21.502477
75.257276	2420.640285	21.507495
75.084131	2425.300223	21.512512
75.280173	2428.959037	21.517530
75.442697	2440.434186	21.522547
75.719453	2440.873933	21.527565
75.980227	2443.774699	21.532583
75.661735	2447.299018	21.537600
75.776503	2439.479467	21.542618
75.430674	2449.572537	21.547635
75.974662	2452.814243	21.552653
76.296237	2462.175364	21.557671
76.112497	2464.078609	21.562688
76.671183	2473.844661	21.567706
76.893270	2462.618835	21.572723
76.813621	2459.229024	21.577741
76.911233	2458.143907	21.582759
76.772419	2459.560443	21.587776
76.737047	2448.431518	21.592794
76.670549	2449.742114	21.597811
76.281378	2451.806739	21.602829
76.499504	2452.990965	21.607847
76.665503	2452.813599	21.612864
76.618226	2455.661336	21.617882
76.925952	2465.999822	21.622899
77.196397	2470.941026	21.627917
77.219494	2472.862565	21.632935
77.255585	2483.003496	21.637952
77.563799	2473.768322	21.642970
77.295403	2480.358804	21.647987
76.922264	2475.585011	21.653005
77.394719	2470.531233	21.658023
77.558167	2503.893234	21.663040
77.894188	2492.280396	21.668058
77.988236	2502.598520	21.673075
78.139650	2499.096982	21.678093
78.249989	2493.938620	21.683111
78.271215	2500.029551	21.688128
78.502915	2493.526766	21.693146
78.689421	2501.940041	21.698163
78.466798	2496.940822	21.703181
78.369153	2488.280105	21.708199
78.141516	2493.952158	21.713216
78.359215	2490.433990	21.718234
78.387585	2491.859216	21.723251
78.414671	2496.065092	21.728269
78.476030	2486.458062	21.733287
78.548106	2502.665576	21.738304
78.655823	2510.021231	21.743322
78.874710	2509.687298	21.748339
79.012212	2515.839031	21.753357
78.951395	2515.192016	21.758375
78.962665	2513.829984	21.763392
79.365081	2530.636231	21.768410
79.481136	2541.411730	21.773427
79.417205	2544.214733	21.778445
79.791850	2540.451198	21.783463
79.710399	2542.373242	21.788480
79.626335	2540.117116	21.793498
79.674099	2535.463980	21.798515
79.518234	2543.826431	21.803533
79.996569	2534.296477	21.808551
79.720860	2539.256455	21.813568
79.830762	2551.648803	21.818586
79.896130	2559.894760	21.823603
80.166602	2568.424390	21.828621
80.592313	2566.439212	21.833639
80.251794	2571.027410	21.838656
80.295768	2561.770211	21.843674
80.497961	2562.972705	21.848691
80.856722	2575.373664	21.853709
81.004708	2583.436343	21.858727
81.187214	2590.663614	21.863744
80.825131	2581.507497	21.868762
81.026337	2590.028986	21.873779
80.805418	2589.526824	21.878797
81.401052	2576.096665	21.883815
80.958071	2579.075462	21.888832
81.306133	2576.531131	21.893850
81.475760	2585.568811	21.898867
80.920723	2580.472990	21.903885
81.451036	2588.646571	21.908903
81.472870	2602.930505	21.913920
81.606327	2600.713094	21.918938
81.906829	2603.494083	21.923955
81.807165	2601.432897	21.928973
81.647236	2596.326052	21.933991
82.194762	2616.470963	21.939008
82.115697	2616.827249	21.944026
82.644140	2626.181497	21.949043
82.393598	2621.849358	21.954061
82.810236	2620.701937	21.959079
82.631086	2622.393029	21.964096
82.659092	2615.779893	21.969114
82.459607	2616.663049	21.974131
83.072946	2618.076110	21.979149
82.941854	2617.509465	21.984167
82.774693	2621.303768	21.989184
82.676361	2619.359145	21.994202
82.958444	2611.516626	21.999219
82.759200	2612.131481	22.004237
82.898945	2617.222472	22.009255
83.142586	2633.242434	22.014272
83.395023	2642.361931	22.019290
83.635395	2646.534635	22.024307
83.440830	2649.761967	22.029325
83.851339	2640.993655	22.034343
83.525668	2649.013336	22.039360
83.433466	2644.000082	22.044378
83.595248	2637.517600	22.049395
83.933800	2639.036566	22.054413
84.243903	2654.907333	22.059431
84.082780	2652.183472	22.064448
84.001088	2655.869794	22.069466
83.948514	2659.898749	22.074483
84.293795	2658.437362	22.079501
84.422705	2656.125971	22.084519
84.125688	2660.713731	22.089536
83.978532	2663.624392	22.094554
84.375149	2677.723792	22.099571
84.669425	2687.193432	22.104589
84.610319	2683.547896	22.109607
84.852117	2692.997305	22.114624
84.461612	2688.074667	22.119642
84.970985	2703.510479	22.124659
85.305195	2706.450351	22.129677
85.873761	2699.503694	22.134695
85.838613	2695.406266	22.139712
85.757936	2700.481102	22.144730
86.023436	2692.461234	22.149747
86.087689	2690.967854	22.154765
86.104269	2685.827190	22.159783
85.979525	2681.112506	22.164800
85.891604	2675.445275	22.169818
86.120259	2668.422153	22.174835
85.945811	2692.772951	22.179853
86.357778	2687.084696	22.184871
86.032103	2695.319008	22.189888
86.371176	2691.955487	22.194906
86.532554	2688.638568	22.199923
86.091703	2682.202555	22.204941
86.409244	2682.134147	22.209959
86.311805	2683.957702	22.214976
86.822609	2698.039341	22.219994
86.693098	2700.290801	22.225011
86.821903	2711.875523	22.230029
87.008689	2707.986555	22.235047
87.122065	2700.826723	22.240064
87.192449	2708.879448	22.245082
87.273452	2702.535761	22.250099
87.230162	2712.799643	22.255117
87.556914	2718.688434	22.260135
87.513208	2728.927142	22.265152
87.427145	2728.094685	22.270170
87.683983	2725.002758	22.275187
87.417595	2721.133846	22.280205
87.530952	2722.564795	22.285223
87.892743	2732.996013	22.290240
88.093857	2748.132690	22.295258
88.113203	2756.490053	22.300275
88.159967	2748.923972	22.305293
88.514232	2741.268990	22.310311
88.222882	2746.057877	22.315328
88.177377	2752.411768	22.320346
88.395644	2755.050937	22.325363
88.448782	2761.035995	22.330381
88.577554	2768.625183	22.335399
88.850244	2769.538983	22.340416
88.864186	2768.820353	22.345434
88.795287	2773.426278	22.350451
88.683695	2771.269091	22.355469
88.687165	2780.802993	22.360487
88.744950	2784.549683	22.365504
88.864163	2799.285711	22.370522
89.547910	2803.604034	22.375539
89.501482	2804.747416	22.380557
89.286571	2800.333940	22.385575
89.592368	2800.459881	22.390592
89.543440	2809.383367	22.395610
89.573939	2820.024019	22.400627
89.587572	2820.779321	22.405645
89.969744	2825.305563	22.410663
90.068971	2828.701798	22.415680
90.175354	2829.543655	22.420698
90.316963	2830.705104	22.425715
90.134736	2846.018322	22.430733
90.398856	2845.260738	22.435751
90.644292	2845.736934	22.440768
90.921733	2843.781123	22.445786
91.152542	2837.593961	22.450803
90.894963	2838.975364	22.455821
90.779705	2841.152034	22.460839
91.273823	2830.473811	22.465856
90.936112	2839.884123	22.470874
90.933259	2828.497413	22.475891
91.166432	2859.488477	22.480909
91.101969	2858.643183	22.485927
91.415930	2860.620473	22.490944
91.229869	2861.577296	22.495962
91.648471	2857.181948	22.500979
91.528120	2874.035192	22.505997
91.963540	2876.201875	22.511015
92.327593	2886.402436	22.516032
91.827243	2892.887159	22.521050
92.262262	2884.310590	22.526067
92.189375	2889.620973	22.531085
92.193165	2887.183853	22.536103
92.062929	2885.319914	22.541120
92.154150	2898.100452	22.546138
92.852423	2895.198567	22.551155
92.652728	2906.316962	22.556173
92.639889	2913.404348	22.561191
92.914468	2904.777004	22.566208
92.662268	2906.728827	22.571226
93.075547	2909.350281	22.576243
93.371327	2907.287458	22.581261
93.031230	2926.381069	22.586279
93.627072	2936.555039	22.591296
93.390801	2935.297794	22.596314
93.583858	2917.596744	22.601331
93.863982	2923.969432	22.606349
93.996575	2920.076232	22.611367
94.123590	2914.296559	22.616384
93.802117	2920.087506	22.621402
93.763775	2918.954095	22.626419
94.421672	2923.263848	22.631437
94.320450	2920.243415	22.636455
94.165453	2920.217017	22.641472
94.274493	2926.013529	22.646490
94.673664	2936.331738	22.651507
94.536318	2932.862450	22.656525
94.660599	2932.552708	22.661543
94.559797	2936.601857	22.666560
94.234497	2938.498787	22.671578
94.812727	2939.005230	22.676595
94.877331	2953.705701	22.681613
94.669428	2960.495242	22.686631
94.982746	2955.005316	22.691648
95.310528	2969.980436	22.696666
95.482784	2954.756970	22.701683
95.457644	2963.780980	22.706701
95.346050	2953.708277	22.711719
95.826407	2958.171925	22.716736
95.400485	2970.799479	22.721754
95.737978	2969.560208	22.726771
95.835316	2977.167003	22.731789
95.928373	2982.003410	22.736807
96.609123	2976.115412	22.741824
96.133392	2983.372735	22.746842
96.197884	2970.075476	22.751859
96.168872	2979.147438	22.756877
96.608734	2994.474392	22.761895
97.222309	2986.737904	22.766912
96.932666	3002.626610	22.771930
97.051230	3001.137373	22.776947
97.045339	3003.309658	22.781965
96.855132	3005.917778	22.786983
97.181717	3002.552988	22.792000
96.770151	3010.194844	22.797018
97.059000	3005.327309	22.802035
97.130204	3000.203300	22.807053
97.157086	3021.928879	22.812071
97.486735	3026.333949	22.817088
97.187812	3031.487043	22.822106
97.389309	3041.387922	22.827123
97.362381	3033.034698	22.832141
97.614044	3059.563645	22.837159
97.832411	3053.043798	22.842176
97.868170	3057.229519	22.847194
98.121297	3075.486085	22.852211
98.182634	3074.700098	22.857229
98.317761	3073.230369	22.862247
98.302360	3068.763672	22.867264
98.394481	3083.598834	22.872282
98.391660	3084.334617	22.877299
98.583375	3085.791268	22.882317
98.551803	3091.644443	22.887335
98.537291	3097.586491	22.892352
98.745811	3105.633668	22.897370
98.991264	3113.154338	22.902387
99.207729	3114.291526	22.907405
99.143371	3121.996149	22.912423
99.860133	3125.359417	22.917440
99.757964	3135.345500	22.922458
99.974152	3146.661252	22.927475
100.189513	3140.599480	22.932493
99.930893	3138.266304	22.937511
100.426996	3135.209646	22.942528
100.521803	3147.456417	22.947546
100.193134	3142.599773	22.952563
100.434225	3142.811539	22.957581
100.224844	3140.783153	22.962599
100.425527	3133.076170	22.967616
100.452517	3128.713323	22.972634
100.432196	3152.475799	22.977651
100.856414	3164.257841	22.982669
100.567263	3163.542199	22.987687
101.136090	3160.654115	22.992704
101.050016	3171.805481	22.997722
100.987723	3176.022276	23.002739
101.032602	3175.011605	23.007757
101.160880	3178.690592	23.012775
101.518834	3183.804581	23.017792
101.922681	3178.814943	23.022810
101.254124	3185.745724	23.027827
101.870110	3180.704121	23.032845
101.589214	3183.572564	23.037863
102.312715	3194.219164	23.042880
102.311752	3204.281055	23.047898
102.140893	3210.522067	23.052915
102.536041	3203.902051	23.057933
102.307939	3218.998643	23.062951
102.480580	3197.885550	23.067968
102.539493	3201.950922	23.072986
102.552656	3201.724754	23.078003
102.813772	3207.223095	23.083021
103.173330	3218.330358	23.088039
103.352452	3218.895793	23.093056
103.601337	3230.042387	23.098074
103.597415	3224.854263	23.103091
103.815645	3228.673907	23.108109
103.625303	3233.462976	23.113127
103.690010	3217.817329	23.118144
103.833931	3224.211330	23.123162
103.922214	3223.206523	23.128179
103.845366	3219.967627	23.133197
103.797485	3226.789165	23.138215
103.771302	3224.640718	23.143232
103.954729	3227.077077	23.148250
103.680949	3239.015184	23.153267
104.078717	3245.978807	23.158285
104.388896	3259.413552	23.163303
104.147686	3247.479799	23.168320
104.115555	3267.276987	23.173338
104.300124	3273.415341	23.178355
104.329690	3279.940787	23.183373
104.481675	3297.575782	23.188391
104.795235	3296.125598	23.193408
105.250776	3293.820082	23.198426
105.346087	3305.918544	23.203443
105.708880	3315.911239	23.208461
105.774690	3324.574092	23.213479
105.580454	3318.759089	23.218496
105.693109	3317.766264	23.223514
106.389120	3326.331000	23.228531
106.192490	3321.668368	23.233549
105.823621	3320.854665	23.238567
106.124184	3316.963634	23.243584
106.355805	3307.689460	23.248602
106.274559	3315.595632	23.253619
106.670397	3323.436999	23.258637
106.755874	3327.406735	23.263655
106.730302	3337.081168	23.268672
106.910815	3334.442884	23.273690
106.714442	3340.384921	23.278707
107.161251	3341.868157	23.283725
106.850447	3343.810213	23.288743
106.921267	3343.950651	23.293760
107.512388	3358.310672	23.298778
106.634763	3360.385166	23.303795
107.416713	3363.438496	23.308813
107.494366	3378.566522	23.313831
108.140149	3381.754677	23.318848
108.157756	3391.457135	23.323866
107.693830	3397.712277	23.328883
108.305698	3388.757602	23.333901
108.585794	3394.802220	23.338919
108.190938	3392.281913	23.343936
108.328909	3389.413531	23.348954
108.468370	3394.043986	23.353971
108.405708	3387.659302	23.358989
108.680740	3409.820140	23.364007
108.567281	3407.950378	23.369024
108.865288	3414.951692	23.374042
108.794216	3414.053746	23.379059
108.952759	3416.658126	23.384077
109.048993	3422.636694	23.389095
109.143649	3429.420335	23.394112
109.439312	3427.641528	23.399130
109.348640	3431.515621	23.404147
109.414803	3422.582767	23.409165
109.429416	3436.991579	23.414183
109.342348	3447.556221	23.419200
109.557842	3454.081188	23.424218
109.914500	3471.015377	23.429235
110.029586	3472.862733	23.434253
110.240009	3482.901338	23.439271
110.409139	3467.327590	23.444288
110.743413	3479.209061	23.449306
110.298759	3475.989509	23.454323
110.393414	3476.574415	23.459341
110.981740	3493.766082	23.464359
111.145334	3506.800905	23.469376
111.116240	3499.139009	23.474394
111.051880	3501.923290	23.479411
111.315400	3498.574540	23.484429
111.480274	3509.475580	23.489447
111.508408	3512.665236	23.494464
111.913725	3514.615752	23.499482
111.652981	3519.062364	23.504499
112.145364	3518.376526	23.509517
112.195769	3510.809558	23.514535
112.181461	3515.274613	23.519552
112.537005	3503.011066	23.524570
112.149166	3520.869199	23.529587
112.772053	3523.691670	23.534605
112.728561	3534.135955	23.539623
112.994393	3536.004035	23.544640
112.916561	3534.936701	23.549658
113.006849	3538.485960	23.554675
113.121346	3531.893739	23.559693
113.340158	3535.211522	23.564711
113.379215	3537.297969	23.569728
113.411833	3527.458144	23.574746
112.912262	3538.046032	23.579763
113.268993	3541.803149	23.584781
113.635612	3545.457728	23.589799
113.644129	3545.970831	23.594816
113.990639	3548.145127	23.599834
114.158697	3553.112041	23.604851
114.215546	3568.584335	23.609869
114.527385	3568.895559	23.614887
114.691805	3573.440113	23.619904
114.753126	3564.785688	23.624922
114.368971	3561.581951	23.629939
114.742451	3562.637911	23.634957
115.020477	3565.996980	23.639975
114.806638	3574.564619	23.644992
115.033080	3579.948537	23.650010
114.959661	3601.488434	23.655027
115.216150	3589.331781	23.660045
115.596289	3586.697098	23.665063
115.797331	3586.214428	23.670080
116.255145	3582.409324	23.675098
115.611625	3585.141759	23.680115
115.550298	3589.554185	23.685133
116.088231	3607.059959	23.690151
115.877233	3613.364170	23.695168
116.079699	3621.368335	23.700186
116.031779	3613.507323	23.705203
116.087682	3604.998909	23.710221
116.324429	3619.284909	23.715239
116.575747	3639.499182	23.720256
117.055695	3632.701684	23.725274
116.639979	3634.871572	23.730291
116.696650	3636.800633	23.735309
116.763682	3634.262035	23.740327
116.714719	3659.494123	23.745344
116.983297	3653.528050	23.750362
116.868318	3664.526411	23.755379
117.364356	3673.450695	23.760397
117.356920	3682.560682	23.765415
117.544656	3688.805997	23.770432
118.038799	3689.120402	23.775450
117.503930	3702.279893	23.780467
117.884161	3711.231695	23.785485
118.277036	3716.280432	23.790503
118.257016	3721.690140	23.795520
118.600036	3713.326347	23.800538
118.180380	3730.855080	23.805555
118.929381	3729.974626	23.810573
119.075045	3735.472168	23.815591
118.907606	3739.547653	23.820608
119.220814	3732.646672	23.825626
119.609512	3737.929627	23.830643
119.093399	3730.889486	23.835661
119.654139	3739.368169	23.840679
119.823005	3758.553856	23.845696
119.564176	3752.732988	23.850714
119.932264	3765.022851	23.855731
119.343768	3758.615747	23.860749
120.029374	3753.875615	23.865767
120.059347	3765.580560	23.870784
120.160368	3772.903057	23.875802
120.442745	3769.074729	23.880819
120.416080	3768.955755	23.885837
120.867409	3774.721342	23.890855
120.693972	3785.230191	23.895872
121.353044	3779.891341	23.900890
121.265645	3794.104853	23.905907
121.301559	3785.372216	23.910925
121.519136	3781.983223	23.915943
121.584517	3785.315472	23.920960
121.316953	3778.356552	23.925978
121.729870	3801.929340	23.930995
121.654267	3805.166761	23.936013
121.939583	3802.947654	23.941031
121.809993	3807.449667	23.946048
121.910389	3805.331944	23.951066
122.212264	3823.673212	23.956083
122.206222	3835.554246	23.961101
122.477393	3829.123743	23.966119
122.184238	3832.928447	23.971136
122.722876	3837.301180	23.976154
122.707466	3855.515128	23.981171
123.159127	3850.363207	23.986189
123.125565	3858.050723	23.991207
122.910941	3873.300419	23.996224
122.926138	3865.587284	24.001242
122.703056	3877.653638	24.006259
123.048115	3886.399535	24.011277
123.613350	3893.397306	24.016295
123.327834	3911.858521	24.021312
124.030892	3918.433998	24.026330
123.767934	3920.861043	24.031347
123.558222	3924.362398	24.036365
124.543978	3927.753380	24.041383
124.360273	3935.268617	24.046400
124.669541	3935.835906	24.051418
124.659565	3941.045272	24.056435
125.064521	3943.986960	24.061453
125.124866	3926.169864	24.066471
124.879690	3934.089205	24.071488
124.883534	3945.659458	24.076506
125.378646	3956.692417	24.081523
125.418535	3966.101338	24.086541
125.647555	3956.088669	24.091559
125.565671	3963.117780	24.096576
125.857097	3967.510097	24.101594
126.054020	3977.424828	24.106611
125.795273	3985.753464	24.111629
126.328267	3976.627716	24.116647
126.201325	3987.161006	24.121664
126.436596	3991.593634	24.126682
126.375063	3981.228497	24.131699
126.328022	3995.555822	24.136717
126.812782	4002.278943	24.141735
126.667729	4007.761861	24.146752
126.538273	4010.063975	24.151770
126.803896	4029.496857	24.156787
127.348370	4037.406927	24.161805
127.507104	4033.458917	24.166823
127.345020	4046.055611	24.171840
127.623243	4058.040880	24.176858
127.785106	4055.960902	24.181875
127.602937	4059.113959	24.186893
128.168475	4051.419219	24.191911
128.760790	4052.832518	24.196928
128.736270	4058.899536	24.201946
129.156463	4059.399059	24.206963
129.421788	4056.125677	24.211981
129.218399	4032.213711	24.216999
129.371338	4030.662225	24.222016
129.555222	4033.300625	24.227034
129.364362	4019.616251	24.232051
129.649817	4032.755577	24.237069
129.928187	4027.987245	24.242087
129.590934	4037.202418	24.247104
129.741286	4037.617701	24.252122
130.129038	4048.897841	24.257139
129.950342	4061.566570	24.262157
130.075330	4055.398625	24.267175
129.858922	4057.521749	24.272192
129.624804	4067.693018	24.277210
130.522908	4080.711744	24.282227
130.109775	4087.495785	24.287245
130.329317	4087.467884	24.292263
130.352412	4100.313539	24.297280
130.438684	4110.416012	24.302298
130.931572	4113.520791	24.307315
130.987629	4127.806919	24.312333
131.088176	4137.373769	24.317351
131.148936	4142.897279	24.322368
131.497832	4141.005957	24.327386
131.541029	4153.640204	24.332403
131.580634	4156.777688	24.337421
131.895069	4164.142868	24.342439
131.568167	4163.985415	24.347456
132.059983	4183.995571	24.352474
132.136269	4180.922039	24.357491
131.976656	4193.275415	24.362509
132.261802	4196.775529	24.367527
132.562887	4205.395861	24.372544
132.585427	4214.861270	24.377562
132.973029	4223.032570	24.382579
132.948577	4230.245378	24.387597
133.247720	4229.921016	24.392615
133.360095	4238.715936	24.397632
133.480203	4233.542931	24.402650
133.627946	4231.484070	24.407667
133.653479	4244.588266	24.412685
133.945230	4243.008837	24.417703
134.076543	4249.430416	24.422720
134.225843	4259.655725	24.427738
134.277393	4248.313306	24.432755
134.271836	4253.238004	24.437773
134.673209	4255.687915	24.442791
135.345576	4261.283525	24.447808
135.156152	4266.741865	24.452826
135.121961	4269.906639	24.457843
134.982465	4272.175630	24.462861
135.087314	4258.814326	24.467879
135.267749	4267.292500	24.472896
135.476469	4288.066489	24.477914
135.689035	4296.015724	24.482931
135.480900	4306.602873	24.487949
135.423515	4301.195507	24.492967
135.724806	4309.626478	24.497984
135.546261	4325.618988	24.503002
136.060479	4328.651045	24.508019
136.344438	4347.368082	24.513037
136.644892	4348.280799	24.518055
136.880887	4356.639893	24.523072
136.384504	4360.088117	24.528090
137.061834	4366.677235	24.533107
136.666600	4378.909604	24.538125
137.140196	4376.790525	24.543143
137.286960	4394.231712	24.548160
137.368722	4402.024603	24.553178
137.544856	4396.012709	24.558195
137.622096	4411.993879	24.563213
138.163529	4418.137034	24.568231
138.308772	4422.154521	24.573248
137.989360	4425.811931	24.578266
138.291012	4418.132871	24.583283
138.078733	4443.416730	24.588301
138.755056	4439.842564	24.593319
138.928574	4452.538795	24.598336
138.848511	4460.618883	24.603354
138.865303	4467.254063	24.608371
139.165164	4481.979123	24.613389
139.255909	4478.436148	24.618407
139.233835	4475.119058	24.623424
139.622625	4492.917205	24.628442
139.792313	4506.860835	24.633459
139.733077	4512.422078	24.638477
139.965345	4511.132805	24.643495
140.690103	4519.346439	24.648512
140.281219	4511.812683	24.653530
140.606688	4505.695438	24.658547
140.706251	4511.680161	24.663565
141.218637	4498.299420	24.668583
141.205413	4507.009865	24.673600
140.975346	4506.483818	24.678618
141.630494	4518.117167	24.683635
141.606491	4522.934337	24.688653
141.813217	4521.617476	24.693671
141.944815	4517.642023	24.698688
141.989415	4527.476612	24.703706
142.057004	4524.480129	24.708723
142.111265	4530.389846	24.713741
142.164966	4524.374877	24.718759
142.184303	4537.041514	24.723776
142.067240	4552.819488	24.728794
142.327474	4550.566320	24.733811
142.384379	4556.535605	24.738829
142.382808	4574.018999	24.743847
142.871588	4576.635261	24.748864
142.795470	4589.225260	24.753882
142.964894	4598.570153	24.758899
143.289652	4602.865901	24.763917
143.594782	4608.351507	24.768935
143.079314	4614.432019	24.773952
143.639784	4635.571442	24.778970
143.642458	4640.715912	24.783987
143.803634	4637.897379	24.789005
143.889060	4648.634719	24.794023
144.403506	4652.537960	24.799040
144.358802	4651.490653	24.804058
144.805475	4659.839181	24.809075
145.102871	4678.229360	24.814093
144.809416	4687.270753	24.819111
145.273036	4686.750331	24.824128
145.362664	4695.927783	24.829146
145.219320	4695.823811	24.834163
145.612450	4700.263601	24.839181
145.795549	4714.344185	24.844199
145.909943	4703.717670	24.849216
145.805093	4723.938107	24.854234
146.081521	4735.718939	24.859251
145.995712	4736.464553	24.864269
146.222486	4742.543178	24.869287
146.554626	4744.063327	24.874304
146.750468	4767.519663	24.879322
146.985016	4773.451894	24.884339
146.811332	4763.447819	24.889357
146.956021	4777.569152	24.894375
147.101220	4793.022426	24.899392
147.233442	4804.917290	24.904410
147.302256	4809.742181	24.909427
147.773718	4817.717622	24.914445
147.592996	4820.719076	24.919463
147.862630	4820.642344	24.924480
147.796503	4839.982552	24.929498
148.135825	4845.964778	24.934515
148.057875	4849.811942	24.939533
148.696046	4870.639682	24.944551
148.858450	4864.733934	24.949568
148.853250	4871.723050	24.954586
148.874906	4886.169797	24.959603
149.255661	4895.911216	24.964621
149.114166	4898.092216	24.969639
150.150871	4895.241495	24.974656
150.222905	4903.680028	24.979674
150.338775	4901.872256	24.984691
150.489262	4898.629229	24.989709
150.659700	4890.345425	24.994727
150.816993	4899.370405	24.999744
150.710364	4903.465091	25.004762
150.906496	4904.965395	25.009779
150.946995	4905.252606	25.014797
150.804260	4898.576836	25.019815
150.962081	4899.271900	25.024832
151.449008	4916.546999	25.029850
151.337283	4920.781365	25.034867
151.404405	4919.369423	25.039885
151.721826	4939.224494	25.044903
151.960902	4937.609018	25.049920
151.857766	4945.197352	25.054938
151.793055	4946.091199	25.059955
152.035559	4952.805048	25.064973
152.219772	4969.802213	25.069991
152.371108	4969.355655	25.075008
152.162075	4978.920645	25.080026
152.406971	4992.830845	25.085043
152.852156	5003.124140	25.090061
152.979396	5004.458417	25.095079
153.180227	5008.325339	25.100096
153.419521	5021.892380	25.105114
153.286501	5021.019780	25.110131
153.517570	5025.582732	25.115149
154.048269	5042.163028	25.120167
154.430614	5048.959304	25.125184
154.537762	5054.119189	25.130202
154.310842	5049.192526	25.135219
154.502399	5048.297799	25.140237
154.592306	5076.818213	25.145255
154.821719	5072.934730	25.150272
155.004552	5071.949823	25.155290
155.284062	5067.970160	25.160307
155.337449	5080.341480	25.165325
155.154034	5101.761401	25.170343
155.544432	5107.000304	25.175360
155.350980	5109.353555	25.180378
155.675795	5122.134020	25.185395
155.934294	5129.164248	25.190413
155.938350	5132.828254	25.195431
156.742532	5146.152773	25.200448
156.568552	5151.479557	25.205466
156.910737	5156.902745	25.210483
156.936415	5154.752307	25.215501
156.784546	5154.141467	25.220519
157.392344	5162.840764	25.225536
157.536831	5173.319857	25.230554
157.255517	5174.080144	25.235571
157.682410	5185.048722	25.240589
158.028786	5199.631395	25.245607
157.954426	5202.493250	25.250624
158.110306	5205.372919	25.255642
158.256470	5208.219380	25.260659
158.799687	5210.271718	25.265677
158.705853	5221.280355	25.270695
158.773270	5213.078730	25.275712
158.789091	5231.712168	25.280730
158.984709	5230.406456	25.285747
159.263803	5244.380968	25.290765
158.899945	5250.450712	25.295783
159.473095	5263.009536	25.300800
160.074770	5274.986288	25.305818
159.921205	5273.700216	25.310835
160.338254	5273.568967	25.315853
160.234109	5277.821175	25.320871
159.981368	5284.953154	25.325888
160.017198	5304.634667	25.330906
160.283740	5313.557619	25.335923
160.347129	5312.345088	25.340941
160.682061	5333.785589	25.345959
160.845702	5342.535185	25.350976
161.027100	5348.927260	25.355994
160.901876	5364.962887	25.361011
161.305861	5373.637201	25.366029
160.872304	5390.977149	25.371047
161.845859	5396.914476	25.376064
161.600266	5412.419649	25.381082
161.849414	5432.607855	25.386099
162.258158	5427.490583	25.391117
162.911429	5438.323060	25.396135
162.972245	5443.540774	25.401152
163.372306	5456.650666	25.406170
163.248860	5459.715908	25.411187
163.632473	5449.255374	25.416205
163.843992	5466.422362	25.421223
163.582398	5457.028176	25.426240
163.474189	5451.865120	25.431258
163.611089	5461.698471	25.436275
163.802483	5473.341508	25.441293
163.905762	5477.694043	25.446311
164.176858	5488.216737	25.451328
164.401259	5501.009946	25.456346
164.455128	5507.074713	25.461363
164.873540	5515.787884	25.466381
164.917728	5533.943733	25.471399
164.785529	5529.059009	25.476416
164.857453	5548.851959	25.481434
165.147131	5568.200677	25.486451
165.266794	5558.822837	25.491469
165.494319	5577.777203	25.496487
165.586240	5583.457284	25.501504
165.981333	5590.472739	25.506522
166.281437	5611.003587	25.511539
166.417399	5610.098550	25.516557
166.454032	5616.200759	25.521575
166.689452	5629.847771	25.526592
166.813608	5634.373861	25.531610
167.163174	5643.893266	25.536627
167.686758	5645.049091	25.541645
167.958121	5663.176013	25.546663
168.061603	5649.160491	25.551680
168.121149	5646.654344	25.556698
168.287580	5649.197845	25.561715
168.241545	5646.521898	25.566733
168.618263	5671.475863	25.571751
168.587482	5670.805117	25.576768
168.715209	5671.186083	25.581786
168.949027	5677.775291	25.586803
169.508624	5683.919209	25.591821
169.303643	5695.826120	25.596839
169.756655	5693.754290	25.601856
169.757957	5694.798882	25.606874
169.809096	5703.547228	25.611891
169.888690	5717.202783	25.616909
169.788824	5725.292829	25.621927
170.242145	5725.171714	25.626944
170.103915	5732.557505	25.631962
170.140130	5751.901687	25.636979
170.594041	5751.032370	25.641997
170.720049	5772.821574	25.647015
170.481821	5772.931232	25.652032
170.984894	5784.753218	25.657050
171.186376	5809.390586	25.662067
171.172021	5804.102337	25.667085
171.476215	5824.383419	25.672103
171.767330	5832.965045	25.677120
171.923584	5836.829615	25.682138
171.947772	5854.562756	25.687156
172.149636	5851.699824	25.692173
172.364518	5870.501789	25.697191
172.606709	5879.820230	25.702208
172.745163	5883.779123	25.707226
172.877604	5908.749348	25.712244
173.059377	5910.349827	25.717261
173.156929	5925.738880	25.722279
173.553075	5932.391292	25.727296
173.607111	5935.561559	25.732314
173.840527	5956.658744	25.737332
174.384223	5964.686579	25.742349
174.375898	5973.646336	25.747367
174.210349	5971.279358	25.752384
174.411817	5979.480433	25.757402
174.806660	5991.524584	25.762420
174.833294	5980.409085	25.767437
175.019678	5994.395451	25.772455
175.071833	6019.081604	25.777472
175.621679	6013.105694	25.782490
175.184888	6026.794528	25.787508
175.505076	6026.867754	25.792525
175.650489	6039.159108	25.797543
175.881125	6065.392697	25.802560
176.177041	6065.453919	25.807578
176.217624	6077.777403	25.812596
176.871082	6095.390711	25.817613
176.893791	6092.981781	25.822631
177.080386	6099.275456	25.827648
177.326233	6104.717083	25.832666
177.330123	6110.212166	25.837684
177.209807	6120.262691	25.842701
177.865603	6139.409808	25.847719
177.560896	6137.269656	25.852736
177.999790	6136.093308	25.857754
178.163933	6161.627141	25.862772
178.433278	6164.568214	25.867789
178.712775	6175.443543	25.872807
178.912309	6186.239784	25.877824
178.962012	6188.239649	25.882842
179.290731	6200.139557	25.887860
179.597240	6202.983307	25.892877
179.704682	6208.225548	25.897895
179.469418	6213.723172	25.902912
180.188884	6223.627225	25.907930
180.324090	6233.451787	25.912948
180.802177	6233.478335	25.917965
180.742725	6240.517459	25.922983
180.469067	6243.009607	25.928000
181.254511	6259.579765	25.933018
181.170903	6262.736795	25.938036
181.503817	6252.779295	25.943053
182.036646	6265.686013	25.948071
181.499128	6274.374760	25.953088
182.367177	6277.835035	25.958106
182.338639	6282.514483	25.963124
182.632075	6283.920837	25.968141
182.803942	6275.617243	25.973159
182.337026	6291.766857	25.978176
182.575893	6298.560688	25.983194
182.948667	6307.502312	25.988212
182.770519	6323.900568	25.993229
183.321581	6326.873568	25.998247
183.462535	6335.046344	26.003264
183.438116	6349.457231	26.008282
183.711702	6359.332920	26.013300
183.944147	6368.921447	26.018317
184.117582	6380.586800	26.023335
183.828726	6399.347783	26.028352
184.422934	6405.666490	26.033370
184.478345	6409.944626	26.038388
184.620359	6418.994837	26.043405
184.765221	6429.193648	26.048423
184.876185	6446.651847	26.053440
184.903911	6462.872966	26.058458
185.165673	6476.936354	26.063476
185.630619	6484.443196	26.068493
186.172095	6494.627646	26.073511
186.370503	6498.065952	26.078528
186.654047	6497.661909	26.083546
186.857143	6513.757913	26.088564
186.888379	6518.254495	26.093581
187.249154	6526.610946	26.098599
187.136785	6530.381747	26.103616
187.195957	6516.871220	26.108634
187.545895	6528.717532	26.113652
187.661795	6544.650361	26.118669
187.887703	6539.725397	26.123687
187.722797	6545.246890	26.128704
188.057222	6563.308068	26.133722
187.945489	6563.451700	26.138740
188.404002	6575.710453	26.143757
188.690321	6594.792462	26.148775
188.831057	6603.195833	26.153792
189.228417	6613.475391	26.158810
189.297556	6623.458815	26.163828
189.423025	6625.816270	26.168845
189.766218	6636.401008	26.173863
189.849622	6647.161938	26.178880
190.028959	6654.735414	26.183898
190.320311	6657.338527	26.188916
190.495605	6676.422122	26.193933
190.792285	6678.209968	26.198951
190.759002	6690.450663	26.203968
191.096355	6703.309207	26.208986
191.215696	6698.031452	26.214004
191.619764	6698.969200	26.219021
191.936460	6710.145261	26.224039
191.891480	6729.522059	26.229056
192.147547	6722.051164	26.234074
191.953703	6722.330695	26.239092
192.263389	6741.323986	26.244109
192.975392	6748.495739	26.249127
192.791357	6755.898543	26.254144
193.271437	6771.683326	26.259162
193.268140	6774.010340	26.264180
193.603437	6774.516852	26.269197
193.685453	6778.216402	26.274215
194.153041	6795.884581	26.279232
194.017759	6807.822401	26.284250
194.082481	6806.104481	26.289268
194.296253	6823.329217	26.294285
194.850716	6819.353722	26.299303
194.753760	6822.667608	26.304320
194.886401	6831.653190	26.309338
195.095564	6840.768918	26.314356
195.232023	6841.050691	26.319373
195.449064	6858.584315	26.324391
195.701890	6878.568358	26.329408
195.703450	6871.610544	26.334426
196.157709	6884.713026	26.339444
195.933868	6897.273951	26.344461
196.743532	6902.757466	26.349479
196.702402	6922.133868	26.354496
196.933802	6907.103080	26.359514
197.033310	6921.817115	26.364532
197.226091	6933.321970	26.369549
197.603804	6939.504104	26.374567
197.361555	6957.001998	26.379584
198.121369	6964.216901	26.384602
197.792686	6969.745079	26.389620
198.161978	6993.840204	26.394637
198.267836	6994.571852	26.399655
198.778534	7007.551991	26.404672
198.944348	7018.442365	26.409690
198.929665	7021.721381	26.414708
198.895613	7037.636947	26.419725
199.648401	7040.089354	26.424743
199.629256	7050.153049	26.429760
199.583612	7050.958795	26.434778
199.643903	7074.366597	26.439796
200.140525	7081.063768	26.444813
200.435294	7082.211119	26.449831
200.520401	7102.410927	26.454848
200.377213	7107.474626	26.459866
200.763263	7117.105925	26.464884
201.149894	7126.430927	26.469901
201.164727	7128.439480	26.474919
201.496535	7156.275175	26.479936
201.751097	7160.610873	26.484954
201.984169	7163.428326	26.489972
201.924793	7180.143479	26.494989
202.745627	7169.115119	26.500007
202.508598	7180.011484	26.505024
202.954405	7192.509392	26.510042
202.954733	7201.064328	26.515060
203.256002	7213.610009	26.520077
203.540705	7227.411542	26.525095
203.793941	7226.488169	26.530112
203.441778	7237.664510	26.535130
204.111515	7238.529358	26.540148
204.177051	7250.594042	26.545165
204.565094	7267.593183	26.550183
204.746977	7267.107091	26.555200
204.594129	7286.564408	26.560218
204.866678	7293.871090	26.565236
205.040333	7309.202105	26.570253
205.033796	7327.635964	26.575271
205.190697	7326.626565	26.580288
205.450354	7349.877405	26.585306
205.789423	7355.933108	26.590324
206.072966	7377.197756	26.595341
206.181603	7384.359521	26.600359
206.582154	7399.671071	26.605376
206.572879	7413.098649	26.610394
207.123988	7437.083972	26.615412
207.051678	7442.225119	26.620429
207.436638	7450.212031	26.625447
207.926404	7472.587472	26.630464
207.802144	7471.662879	26.635482
208.294665	7478.259814	26.640500
207.973833	7507.416206	26.645517
208.615983	7500.800385	26.650535
209.068854	7515.671393	26.655552
209.291117	7525.363133	26.660570
209.943977	7517.874337	26.665588
209.408925	7534.310297	26.670605
209.899518	7540.494002	26.675623
210.141446	7541.450726	26.680640
209.834075	7550.524106	26.685658
210.469082	7556.066582	26.690676
210.527878	7567.283319	26.695693
210.769166	7588.349591	26.700711
210.889137	7595.099278	26.705728
211.262391	7601.481215	26.710746
211.319379	7611.820642	26.715764
211.396606	7612.919817	26.720781
211.608026	7622.906888	26.725799
212.368860	7636.539895	26.730816
212.296843	7637.668620	26.735834
212.711705	7641.073443	26.740852
212.823072	7664.177295	26.745869
213.215182	7665.590494	26.750887
213.145382	7669.986283	26.755904
213.239921	7674.545903	26.760922
213.835765	7684.410019	26.765940
213.550152	7701.732270	26.770957
214.014294	7698.152639	26.775975
214.330679	7707.886646	26.780992
214.302229	7720.723933	26.786010
214.544780	7722.586606	26.791028
214.361959	7727.947082	26.796045
214.736777	7742.555774	26.801063
215.305400	7745.895637	26.806080
215.274116	7753.704403	26.811098
215.213850	7766.417241	26.816116
215.378286	7784.158826	26.821133
215.677694	7792.550668	26.826151
216.352767	7796.521139	26.831168
216.287149	7813.518806	26.836186
216.682021	7810.278260	26.841204
216.888329	7827.719773	26.846221
217.114409	7834.074194	26.851239
217.585816	7848.289099	26.856256
217.695457	7849.178041	26.861274
217.712570	7859.893177	26.866292
218.224364	7868.435091	26.871309
217.916344	7875.785037	26.876327
218.274515	7885.831486	26.881344
218.166008	7895.322362	26.886362
218.345639	7909.210219	26.891380
218.705288	7926.785801	26.896397
218.567375	7948.659722	26.901415
218.827252	7959.526539	26.906432
218.936071	7982.599618	26.911450
219.680000	7999.079955	26.916468
219.778986	8013.150923	26.921485
220.149246	8020.423740	26.926503
220.597083	8032.154761	26.931520
220.801200	8036.871045	26.936538
221.217793	8039.416975	26.941556
221.461675	8058.532369	26.946573
221.432884	8069.055885	26.951591
221.643586	8086.064452	26.956608
221.650984	8091.821611	26.961626
222.191291	8104.122325	26.966644
222.447313	8119.286499	26.971661
222.443918	8131.652937	26.976679
222.865418	8137.443507	26.981696
222.674875	8143.897625	26.986714
223.227802	8157.067740	26.991732
223.615137	8176.205121	26.996749
223.431039	8190.733865	27.001767
223.803177	8195.120957	27.006784
223.941219	8217.953005	27.011802
224.370607	8223.808672	27.016820
224.364606	8245.021534	27.021837
224.619796	8253.297347	27.026855
225.203905	8260.388586	27.031872
225.226783	8281.186582	27.036890
225.474688	8282.211869	27.041908
225.809292	8304.757704	27.046925
225.782797	8314.753779	27.051943
226.132411	8318.623499	27.056960
226.267181	8335.378928	27.061978
226.080048	8343.351116	27.066996
226.330038	8371.018280	27.072013
226.264296	8382.052852	27.077031
227.014393	8390.747330	27.082048
227.224882	8422.745865	27.087066
227.170715	8436.733661	27.092084
227.732963	8452.683894	27.097101
227.878399	8461.163154	27.102119
228.475259	8477.647876	27.107136
228.467675	8494.539266	27.112154
228.945174	8511.819237	27.117172
229.295230	8508.610804	27.122189
229.255248	8510.274452	27.127207
229.452984	8524.349378	27.132224
229.834497	8535.683786	27.137242
230.193284	8534.273515	27.142260
230.356132	8551.154208	27.147277
230.469730	8569.820014	27.152295
231.064457	8566.623992	27.157312
230.846496	8578.897851	27.162330
231.118822	8592.932803	27.167348
231.186075	8593.452688	27.172365
231.282642	8612.162230	27.177383
231.462616	8606.773464	27.182400
231.747505	8632.913877	27.187418
231.893034	8650.842351	27.192436
232.099541	8669.632704	27.197453
232.289736	8691.519564	27.202471
232.762780	8699.755346	27.207488
232.756594	8707.645849	27.212506
233.199877	8723.409627	27.217524
233.422161	8741.247312	27.222541
233.453923	8761.826625	27.227559
234.333856	8773.667646	27.232576
234.106153	8784.020481	27.237594
234.154665	8793.780982	27.242612
234.598433	8812.433515	27.247629
234.800624	8831.518316	27.252647
235.137480	8836.757162	27.257664
235.602906	8854.680229	27.262682
236.188469	8856.148648	27.267700
236.586850	8862.448186	27.272717
236.835799	8885.165922	27.277735
237.041586	8889.787450	27.282752
236.703171	8892.391060	27.287770
237.026161	8898.408736	27.292788
237.552643	8910.418529	27.297805
237.478558	8918.231293	27.302823
238.098180	8933.333215	27.307840
238.056616	8939.868601	27.312858
238.140015	8955.177152	27.317876
238.592591	8962.011314	27.322893
238.523631	8977.975031	27.327911
239.048184	8988.075107	27.332928
239.165293	8993.525010	27.337946
239.200300	9013.608427	27.342964
239.609905	9022.293074	27.347981
240.087617	9035.781772	27.352999
239.996124	9046.953349	27.358016
240.247301	9059.874318	27.363034
240.592015	9071.457885	27.368052
241.220895	9076.622921	27.373069
241.388492	9091.299674	27.378087
241.657908	9082.297686	27.383104
241.736404	9098.642666	27.388122
241.488056	9113.036905	27.393140
242.403095	9113.585832	27.398157
242.408813	9128.054186	27.403175
242.580357	9144.466807	27.408192
242.868795	9161.618964	27.413210
242.720224	9169.468687	27.418228
243.032353	9185.887872	27.423245
243.233201	9205.109026	27.428263
243.689423	9217.300446	27.433280
243.812085	9234.759468	27.438298
244.007257	9248.857446	27.443316
244.655313	9254.853044	27.448333
244.470882	9273.007136	27.453351
244.635036	9281.095524	27.458368
245.068325	9301.496108	27.463386
245.147781	9311.002646	27.468404
245.482437	9320.466301	27.473421
245.592254	9332.162375	27.478439
246.316338	9335.048951	27.483456
246.473026	9343.735240	27.488474
246.466107	9360.579957	27.493492
246.880911	9361.468821	27.498509
246.902578	9380.203429	27.503527
247.600873	9385.458777	27.508544
247.642150	9392.363447	27.513562
247.957631	9407.658340	27.518580
248.460322	9412.745245	27.523597
248.382699	9439.394717	27.528615
248.644940	9447.758371	27.533632
248.995071	9453.888820	27.538650
249.094786	9463.966896	27.543668
249.286829	9469.780983	27.548685
249.676407	9487.965894	27.553703
250.175217	9495.471860	27.558720
249.712272	9507.206700	27.563738
249.826657	9532.026792	27.568756
250.306597	9545.603919	27.573773
250.546735	9557.949180	27.578791
250.901104	9579.363202	27.583808
250.994783	9596.593441	27.588826
251.206552	9613.675865	27.593844
251.754612	9619.845014	27.598861
252.377173	9639.862892	27.603879
252.421870	9648.061598	27.608896
252.443692	9655.146202	27.613914
252.620467	9677.809843	27.618932
253.418342	9685.316685	27.623949
253.252906	9700.771939	27.628967
253.899059	9705.716614	27.633984
254.092387	9711.754742	27.639002
253.720283	9730.102676	27.644020
254.332745	9740.798830	27.649037
254.941155	9760.032883	27.654055
254.715725	9767.932711	27.659072
255.068853	9786.922381	27.664090
254.916200	9805.485648	27.669108
255.703586	9817.726939	27.674125
255.786437	9841.425205	27.679143
256.294867	9862.679805	27.684160
256.578205	9866.749609	27.689178
256.422924	9889.923013	27.694196
256.856332	9897.088865	27.699213
257.262052	9918.331104	27.704231
257.538481	9937.077127	27.709248
257.526844	9941.960095	27.714266
257.798143	9951.705465	27.719284
258.291440	9962.578166	27.724301
258.536634	9987.728963	27.729319
258.658141	10004.096459	27.734336
259.028847	10014.053712	27.739354
258.919170	10021.559906	27.744372
259.443780	10045.353836	27.749389
259.344602	10067.385248	27.754407
260.010074	10082.310477	27.759424
260.210989	10090.949184	27.764442
260.329410	10119.482450	27.769460
260.782967	10134.090249	27.774477
260.781850	10148.535202	27.779495
260.894515	10165.254682	27.784512
261.434860	10177.493628	27.789530
261.581759	10203.215711	27.794548
261.915567	10207.369295	27.799565
262.206453	10217.547469	27.804583
262.557283	10234.100480	27.809600
262.735029	10244.141573	27.814618
262.848601	10263.970993	27.819636
263.341365	10275.507006	27.824653
263.654791	10288.974835	27.829671
263.888592	10303.755904	27.834688
263.995218	10315.222607	27.839706
263.836259	10342.103892	27.844724
264.576521	10353.648782	27.849741
264.972889	10367.946774	27.854759
264.944750	10374.373223	27.859776
265.431710	10399.670064	27.864794
265.540507	10412.361552	27.869812
266.018175	10424.998777	27.874829
265.928029	10433.667171	27.879847
266.205123	10461.169050	27.884864
266.751992	10468.522691	27.889882
266.983588	10489.432748	27.894900
266.987964	10509.370994	27.899917
267.247478	10525.379622	27.904935
267.632622	10546.515273	27.909952
268.420728	10546.509368	27.914970
268.641216	10563.531316	27.919988
268.995630	10574.438628	27.925005
269.205644	10594.859608	27.930023
269.298521	10601.302027	27.935040
269.804891	10600.212787	27.940058
269.842726	10616.581219	27.945076
270.906727	10631.299604	27.950093
270.739684	10645.445561	27.955111
271.036485	10657.302803	27.960128
271.139432	10660.513630	27.965146
271.242901	10675.305813	27.970164
271.666165	10683.139767	27.975181
272.217164	10698.102259	27.980199
272.329907	10711.469025	27.985216
272.684902	10720.586069	27.990234
272.644965	10740.976660	27.995252
272.916825	10745.793599	28.000269
272.920587	10763.964048	28.005287
273.393157	10786.620877	28.010304
273.733661	10797.972528	28.015322
273.902770	10815.678400	28.020340
274.263807	10816.354687	28.025357
274.646887	10831.375003	28.030375
274.726750	10846.300452	28.035392
275.255362	10854.904284	28.040410
275.221700	10875.369823	28.045428
275.868002	10886.159254	28.050445
275.838757	10898.004261	28.055463
276.133766	10909.824054	28.060480
276.615767	10925.192153	28.065498
276.673743	10948.579952	28.070516
276.789814	10955.511447	28.075533
276.877324	10974.193202	28.080551
276.953158	10990.972833	28.085568
277.890141	11011.540004	28.090586
278.004188	11032.153222	28.095604
278.398273	11043.585092	28.100621
278.735693	11069.253447	28.105639
278.570962	11085.398069	28.110656
279.482871	11088.498814	28.115674
279.275937	11107.933822	28.120692
279.385300	11117.155609	28.125709
279.778525	11138.445391	28.130727
280.167703	11156.486751	28.135744
280.555729	11172.340154	28.140762
280.627658	11187.301843	28.145780
280.904058	11207.675268	28.150797
281.439754	11213.060655	28.155815
281.170506	11238.119565	28.160832
281.506954	11242.415060	28.165850
282.013260	11260.141479	28.170868
282.232638	11265.718215	28.175885
282.267937	11285.665105	28.180903
282.749480	11310.329362	28.185920
282.983897	11317.078375	28.190938
283.289134	11342.066931	28.195956
283.525756	11348.045172	28.200973
284.013335	11371.129800	28.205991
284.438990	11395.641837	28.211008
284.520122	11404.400843	28.216026
285.312277	11425.973018	28.221044
285.667029	11426.849234	28.226061
286.406884	11442.591256	28.231079
286.193305	11472.946508	28.236096
286.418600	11473.119800	28.241114
286.736234	11482.956642	28.246132
287.077067	11478.501906	28.251149
287.783050	11492.651517	28.256167
288.102631	11504.805720	28.261184
288.310462	11508.448740	28.266202
288.130606	11514.375044	28.271220
288.238450	11524.077218	28.276237
288.881330	11540.942728	28.281255
289.144855	11557.339998	28.286272
289.230950	11563.025986	28.291290
289.631902	11581.103815	28.296308
289.930560	11583.314955	28.301325
290.246210	11594.563604	28.306343
290.522213	11602.916613	28.311360
290.641935	11623.539072	28.316378
290.971186	11636.269693	28.321396
291.176453	11654.037039	28.326413
291.602813	11665.827388	28.331431
291.481417	11689.670312	28.336448
292.391301	11686.885716	28.341466
292.613127	11707.924963	28.346484
292.904437	11710.285669	28.351501
293.136220	11728.535228	28.356519
293.611885	11735.474181	28.361536
294.235047	11753.498637	28.366554
294.421995	11762.105560	28.371572
294.450442	11764.728230	28.376589
294.763548	11774.016507	28.381607
294.654357	11786.502886	28.386624
294.819079	11808.741557	28.391642
295.180027	11824.230287	28.396660
295.397524	11843.874693	28.401677
295.495988	11857.790770	28.406695
295.377577	11880.581983	28.411712
295.786738	11911.807227	28.416730
296.525142	11931.386414	28.421748
296.604739	11959.063338	28.426765
297.169702	11972.786884	28.431783
297.271372	11996.560735	28.436800
297.570004	11999.273996	28.441818
298.516321	12017.434697	28.446836
298.533608	12031.461429	28.451853
298.975607	12051.819464	28.456871
299.547744	12073.897133	28.461888
299.514095	12081.701766	28.466906
299.403520	12091.172995	28.471924
299.711864	12112.783393	28.476941
300.121431	12123.310421	28.481959
300.389745	12146.856428	28.486976
300.521234	12152.949183	28.491994
301.085724	12177.273271	28.497012
301.333564	12183.764736	28.502029
301.326852	12196.557516	28.507047
301.729423	12217.872333	28.512064
301.777033	12237.180464	28.517082
302.537443	12248.113964	28.522100
303.809058	12260.022553	28.527117
303.833069	12270.448646	28.532135
303.982545	12291.730322	28.537152
303.950676	12299.398987	28.542170
304.439579	12304.959336	28.547188
304.456722	12318.206351	28.552205
304.971953	12342.822517	28.557223
304.842574	12356.288148	28.562240
305.186171	12370.128549	28.567258
305.673817	12392.125016	28.572276
305.830408	12412.878383	28.577293
306.241249	12429.446101	28.582311
306.336768	12443.483065	28.587328
306.331566	12463.746968	28.592346
307.018742	12485.687218	28.597364
307.019453	12518.098054	28.602381
307.610447	12535.904071	28.607399
307.727003	12563.525607	28.612416
308.201344	12574.898552	28.617434
308.309966	12594.841732	28.622452
308.728854	12624.007793	28.627469
309.193017	12633.266664	28.632487
309.493674	12657.869281	28.637504
309.674472	12673.456230	28.642522
310.028567	12692.221344	28.647540
310.313596	12717.259086	28.652557
310.612117	12744.640987	28.657575
310.805812	12763.333253	28.662592
311.267174	12789.764638	28.667610
311.764125	12813.089575	28.672628
311.746125	12836.043146	28.677645
312.116822	12847.085035	28.682663
312.283656	12875.621275	28.687680
312.924192	12898.412400	28.692698
313.440404	12920.041890	28.697716
313.608305	12942.594027	28.702733
313.940195	12954.409369	28.707751
314.183430	12982.772828	28.712768
314.643504	12999.380751	28.717786
315.058296	13017.931482	28.722804
315.292388	13038.897678	28.727821
315.488622	13047.813212	28.732839
315.952129	13075.327798	28.737856
316.412704	13106.569126	28.742874
316.918479	13113.557588	28.747892
317.022005	13137.923106	28.752909
317.795819	13142.937252	28.757927
318.020458	13162.907180	28.762944
318.071946	13179.392559	28.767962
318.420294	13182.925609	28.772980
318.385326	13201.284440	28.777997
318.760214	13220.668940	28.783015
318.988126	13242.015266	28.788032
318.954499	13266.039148	28.793050
319.179583	13290.689092	28.798068
319.839351	13320.658722	28.803085
320.256587	13341.410427	28.808103
320.571014	13364.199202	28.813120
320.939668	13383.430104	28.818138
321.163312	13397.905723	28.823156
321.077852	13408.497907	28.828173
321.451484	13437.255431	28.833191
321.824736	13461.850952	28.838208
322.014494	13479.451909	28.843226
323.041932	13493.174041	28.848244
323.137745	13519.486517	28.853261
323.316463	13533.268180	28.858279
323.405351	13550.310167	28.863296
324.030183	13573.758241	28.868314
324.131369	13591.467828	28.873332
324.103691	13623.929190	28.878349
324.616012	13640.346384	28.883367
325.137664	13670.859130	28.888384
325.304607	13694.918646	28.893402
326.105936	13713.902522	28.898420
325.793131	13741.823152	28.903437
326.576994	13755.068653	28.908455
326.511943	13784.138161	28.913472
326.962982	13806.246190	28.918490
328.113081	13815.326222	28.923508
328.846290	13826.069086	28.928525
329.522954	13832.592257	28.933543
329.751555	13858.584526	28.938560
329.834741	13869.055973	28.943578
330.405228	13872.358777	28.948596
330.394644	13896.323027	28.953613
330.775084	13905.507136	28.958631
330.755180	13909.789250	28.963648
330.997580	13917.390608	28.968666
331.660207	13938.944786	28.973684
331.981093	13949.710860	28.978701
332.232439	13961.261470	28.983719
332.966073	13963.692553	28.988736
333.169573	13976.096959	28.993754
332.885001	13990.560571	28.998772
333.272573	14009.896537	29.003789
333.484331	14035.544292	29.008807
333.999293	14053.366740	29.013824
333.649073	14073.240803	29.018842
334.357247	14085.500394	29.023860
334.585544	14112.112025	29.028877
334.903569	14138.457083	29.033895
335.494699	14158.737334	29.038912
335.542564	14187.834093	29.043930
336.166790	14200.372102	29.048948
335.987666	14222.941895	29.053965
336.746079	14240.072908	29.058983
337.094692	14261.341589	29.064000
337.292346	14293.153200	29.069018
337.818646	14314.012156	29.074036
337.820413	14336.181273	29.079053
338.039718	14365.156872	29.084071
338.820155	14388.569101	29.089088
339.132143	14415.442877	29.094106
339.669418	14430.419960	29.099124
339.931487	14449.659065	29.104141
340.546484	14462.059729	29.109159
340.599516	14490.243467	29.114176
340.858308	14513.901281	29.119194
341.365620	14508.740936	29.124212
341.517788	14546.111936	29.129229
341.964896	14558.813554	29.134247
341.999316	14585.686571	29.139264
342.155440	14611.078485	29.144282
342.810678	14634.428398	29.149300
342.914828	14663.788718	29.154317
343.469773	14683.481443	29.159335
343.977868	14695.611516	29.164352
344.453324	14701.727339	29.169370
345.374117	14709.532895	29.174388
346.069207	14714.862901	29.179405
346.193986	14719.454273	29.184423
346.752763	14729.362648	29.189440
346.760881	14747.608890	29.194458
346.969960	14752.310312	29.199476
346.960129	14761.495592	29.204493
347.341883	14773.686441	29.209511
347.872790	14786.886780	29.214528
347.752892	14804.243469	29.219546
347.872178	14822.390365	29.224564
348.576564	14839.334529	29.229581
348.542432	14861.794078	29.234599
348.901683	14883.456567	29.239616
349.089043	14901.198173	29.244634
349.589547	14929.824516	29.249652
349.982096	14947.199458	29.254669
350.028842	14977.687181	29.259687
350.544222	14999.047578	29.264704
350.660525	15022.308173	29.269722
351.221290	15045.824892	29.274740
351.375410	15063.893957	29.279757
351.565567	15107.734374	29.284775
352.475948	15127.441704	29.289792
352.472619	15155.736262	29.294810
353.034341	15186.769464	29.299828
353.502419	15209.185977	29.304845
354.101140	15243.734888	29.309863
354.138073	15258.522073	29.314880
354.194002	15282.420865	29.319898
354.949988	15307.123420	29.324916
355.124907	15336.271633	29.329933
354.903569	15365.942679	29.334951
355.549528	15386.957887	29.339968
356.086079	15423.604382	29.344986
356.812029	15451.438438	29.350004
357.444717	15471.603084	29.355021
357.419847	15495.018879	29.360039
358.094501	15517.330954	29.365056
358.119517	15537.324982	29.370074
358.915070	15553.153365	29.375092
359.274556	15580.381431	29.380109
359.766864	15600.833362	29.385127
360.265291	15611.831715	29.390144
360.419569	15635.810385	29.395162
360.850982	15657.509893	29.400180
361.254681	15674.043666	29.405197
361.237736	15687.819452	29.410215
361.776898	15715.635600	29.415232
362.037955	15731.395746	29.420250
362.507567	15760.426087	29.425268
362.890525	15771.556207	29.430285
362.804882	15800.253002	29.435303
363.426186	15813.676852	29.440320
363.950999	15839.799416	29.445338
364.048535	15858.430742	29.450356
364.399010	15885.287967	29.455373
364.321026	15909.369462	29.460391
364.907329	15932.210581	29.465408
364.753597	15969.467758	29.470426
365.384053	15991.793586	29.475444
366.010153	16022.837076	29.480461
366.250856	16051.698206	29.485479
366.971893	16079.587634	29.490496
367.108132	16104.968839	29.495514
367.865048	16122.774511	29.500532
368.209875	16148.094874	29.505549
368.231925	16156.682093	29.510567
368.514749	16186.099052	29.515584
369.059719	16205.981247	29.520602
369.542083	16230.099085	29.525620
370.271978	16258.072671	29.530637
369.734656	16286.290955	29.535655
370.659446	16289.990677	29.540672
370.807594	16319.182454	29.545690
370.981197	16344.356023	29.550708
371.667052	16374.983352	29.555725
371.646739	16396.349751	29.560743
372.413489	16420.221418	29.565760
372.930592	16446.611315	29.570778
372.934088	16472.392677	29.575796
373.327935	16501.189583	29.580813
373.555496	16530.015577	29.585831
374.019059	16551.287868	29.590848
374.277004	16581.015671	29.595866
374.996470	16606.758394	29.600884
375.429462	16635.003000	29.605901
375.718886	16662.164551	29.610919
375.935520	16673.662200	29.615936
376.230152	16707.111429	29.620954
376.876523	16735.588273	29.625972
377.624090	16756.112245	29.630989
377.940053	16785.449161	29.636007
378.460778	16797.774433	29.641024
378.888736	16827.965709	29.646042
379.066923	16841.418209	29.651060
379.547876	16861.986960	29.656077
379.274456	16881.204492	29.661095
380.252003	16898.543830	29.666112
380.723965	16930.247637	29.671130
380.818355	16953.905638	29.676148
381.353182	16972.946897	29.681165
381.681399	16992.778374	29.686183
382.416407	17018.114945	29.691200
382.710120	17036.934809	29.696218
382.834959	17059.656447	29.701236
383.208950	17079.382974	29.706253
383.378994	17100.136199	29.711271
383.858495	17115.064376	29.716288
384.357009	17147.860407	29.721306
384.663537	17177.673165	29.726324
385.441355	17197.074789	29.731341
385.580310	17227.760195	29.736359
386.118692	17249.997593	29.741376
386.528372	17263.888127	29.746394
386.905110	17292.698358	29.751412
387.423944	17313.564914	29.756429
387.712101	17343.298668	29.761447
388.250710	17356.528014	29.766464
388.265749	17376.572887	29.771482
388.681121	17402.859911	29.776500
389.005866	17422.594457	29.781517
389.327539	17454.041414	29.786535
390.122580	17468.374312	29.791552
390.675650	17495.312798	29.796570
391.349156	17492.747396	29.801588
392.504050	17498.590943	29.806605
392.731998	17503.776525	29.811623
393.503549	17491.878105	29.816640
393.837170	17498.373829	29.821658
393.759722	17514.725094	29.826676
394.058234	17519.271141	29.831693
394.296068	17533.384454	29.836711
394.790444	17549.242431	29.841728
394.903630	17559.736497	29.846746
394.489539	17564.721985	29.851764
394.800717	17586.341320	29.856781
395.327172	17616.208959	29.861799
395.383634	17640.571754	29.866816
395.751804	17658.714173	29.871834
396.177596	17685.609569	29.876852
396.601744	17704.229739	29.881869
396.605336	17728.967273	29.886887
396.887314	17752.884483	29.891904
397.244443	17775.766635	29.896922
397.311666	17820.368337	29.901940
398.012793	17842.919057	29.906957
397.891750	17879.211458	29.911975
398.708239	17911.542348	29.916992
399.240836	17942.641402	29.922010
399.535079	17995.148970	29.927028
400.290945	18019.599194	29.932045
400.445781	18064.162549	29.937063
401.156262	18079.592487	29.942080
401.838722	18111.022250	29.947098
403.078526	18126.211888	29.952116
404.030490	18138.426664	29.957133
404.385086	18142.844098	29.962151
404.807091	18157.649372	29.967168
405.192586	18174.374496	29.972186
405.365578	18184.133097	29.977204
405.974605	18186.628363	29.982221
406.317443	18193.795685	29.987239
406.200192	18214.143143	29.992256
406.643610	18231.535256	29.997274
406.697791	18251.470706	30.002292
407.062068	18276.373896	30.007309
407.698603	18300.963085	30.012327
407.596802	18324.890210	30.017344
408.071833	18349.953140	30.022362
408.263242	18380.708018	30.027380
408.618032	18407.027953	30.032397
409.010191	18440.853526	30.037415
409.240794	18478.463187	30.042432
409.731765	18504.850497	30.047450
409.956107	18547.489957	30.052468
410.617580	18567.628109	30.057485
411.280265	18596.699007	30.062503
411.625964	18633.716160	30.067520
412.331519	18658.225566	30.072538
412.527418	18684.722233	30.077556
413.064734	18703.679529	30.082573
413.572756	18737.108531	30.087591
413.948514	18755.351879	30.092608
414.863783	18766.959969	30.097626
415.120027	18802.134014	30.102644
415.744036	18814.779331	30.107661
416.253893	18831.915256	30.112679
416.040697	18850.951631	30.117696
416.585086	18880.414107	30.122714
416.952289	18901.002743	30.127732
417.530175	18927.301288	30.132749
418.345551	18944.895157	30.137767
418.412127	18971.961980	30.142784
418.795262	18987.039279	30.147802
419.021655	19018.743681	30.152820
419.332029	19049.335793	30.157837
419.799127	19067.192475	30.162855
420.130787	19093.125248	30.167872
420.652460	19115.996003	30.172890
420.949206	19144.720363	30.177908
421.158266	19166.761692	30.182925
421.515352	19192.823310	30.187943
421.842198	19219.180285	30.192960
422.606226	19240.768874	30.197978
422.279479	19267.354019	30.202996
422.996684	19297.131380	30.208013
423.420129	19327.990624	30.213031
423.480148	19352.967833	30.218048
424.198819	19394.173882	30.223066
424.212841	19424.187263	30.228084
425.015311	19462.297350	30.233101
425.474567	19495.008705	30.238119
425.578673	19522.847537	30.243136
426.267978	19558.757889	30.248154
426.534044	19598.739684	30.253172
426.941818	19632.255328	30.258189
427.533784	19661.086118	30.263207
427.873958	19708.360007	30.268224
428.255872	19735.340891	30.273242
428.885588	19767.931400	30.278260
429.620686	19806.741296	30.283277
430.078058	19827.822305	30.288295
430.399132	19856.758735	30.293312
430.910889	19901.447636	30.298330
430.823838	19940.404743	30.303348
431.224366	19974.294860	30.308365
431.793468	20001.543913	30.313383
432.339324	20045.513908	30.318400
432.838792	20070.025590	30.323418
432.669142	20113.532194	30.328436
433.413506	20156.542793	30.333453
434.079086	20184.699508	30.338471
433.939783	20231.126880	30.343488
434.666071	20260.392540	30.348506
435.126306	20304.477536	30.353524
435.813216	20343.750899	30.358541
436.664128	20378.468763	30.363559
436.979259	20412.031758	30.368576
437.698504	20440.199441	30.373594
438.154151	20463.486415	30.378612
438.844403	20495.455860	30.383629
439.461366	20506.928212	30.388647
439.906672	20543.409082	30.393664
440.308594	20567.266855	30.398682
440.879511	20598.225193	30.403700
441.269361	20612.601394	30.408717
441.785271	20631.481767	30.413735
442.146084	20663.237412	30.418752
442.655074	20686.320484	30.423770
442.890060	20713.755227	30.428788
443.358499	20731.189909	30.433805
444.038942	20753.254415	30.438823
444.011188	20786.283841	30.443840
444.525572	20799.661474	30.448858
444.949259	20832.064696	30.453876
445.245651	20860.077677	30.458893
445.780249	20888.300024	30.463911
445.673694	20927.268446	30.468928
446.248446	20948.660940	30.473946
446.666068	20992.987893	30.478964
447.262292	21020.069869	30.483981
447.987687	21055.724625	30.488999
448.074817	21093.121563	30.494016
448.793186	21119.483332	30.499034
448.984198	21145.124810	30.504052
449.572929	21182.494376	30.509069
450.246280	21211.933979	30.514087
450.976300	21235.147564	30.519104
451.455791	21260.725328	30.524122
451.497168	21279.951890	30.529140
452.412675	21300.874709	30.534157
452.798455	21322.796180	30.539175
453.435044	21340.950794	30.544192
453.669139	21352.843396	30.549210
454.328307	21378.115333	30.554228
454.749074	21392.411474	30.559245
455.120857	21406.133959	30.564263
455.410058	21421.783782	30.569280
456.206578	21445.713880	30.574298
456.505664	21461.734982	30.579316
456.601029	21482.027465	30.584333
457.051464	21509.619332	30.589351
457.258220	21545.349400	30.594368
457.618546	21568.071229	30.599386
458.267289	21609.937314	30.604404
458.300630	21642.882845	30.609421
458.663337	21661.061437	30.614439
458.818659	21702.619107	30.619456
459.216900	21738.420810	30.624474
459.834413	21779.988831	30.629492
460.451418	21824.078107	30.634509
460.915432	21855.806976	30.639527
461.057126	21902.131360	30.644544
461.746639	21940.889395	30.649562
462.056343	21978.967362	30.654580
462.633490	22028.876387	30.659597
463.217571	22054.211431	30.664615
463.536132	22099.857929	30.669632
463.659836	22135.677818	30.674650
463.913788	22185.005689	30.679668
464.809574	22233.279647	30.684685
465.369856	22268.305166	30.689703
465.951028	22315.971164	30.694720
466.533849	22352.844697	30.699738
467.219728	22386.700872	30.704756
467.600890	22432.275204	30.709773
468.421133	22472.707348	30.714791
468.662061	22502.462631	30.719808
469.135316	22533.963677	30.724826
469.552046	22579.324292	30.729844
470.145162	22611.268071	30.734861
470.763600	22653.204274	30.739879
470.776892	22690.476720	30.744896
471.476779	22724.628277	30.749914
471.960211	22760.639728	30.754932
472.084151	22789.358411	30.759949
472.849289	22830.349603	30.764967
473.717025	22864.538459	30.769984
474.091577	22905.363134	30.775002
474.312848	22940.170908	30.780020
474.853582	22979.428058	30.785037
475.692607	23004.857329	30.790055
475.870575	23047.001954	30.795072
476.642339	23078.413162	30.800090
477.276619	23107.135003	30.805108
477.562733	23130.742196	30.810125
478.385823	23155.927705	30.815143
478.773607	23186.590037	30.820160
479.706648	23220.061618	30.825178
480.195878	23241.735314	30.830196
480.754857	23264.036393	30.835213
481.410494	23286.278216	30.840231
481.397666	23309.376090	30.845248
482.186428	23335.546615	30.850266
482.432821	23363.836331	30.855284
482.724291	23393.888396	30.860301
482.950953	23413.435732	30.865319
483.242396	23440.758052	30.870336
483.366094	23467.834805	30.875354
483.804873	23510.085147	30.880372
484.458419	23539.531307	30.885389
485.070729	23562.323625	30.890407
485.265563	23610.608960	30.895424
485.476953	23649.564838	30.900442
486.067621	23674.723998	30.905460
486.459916	23716.109978	30.910477
486.675383	23749.485632	30.915495
487.339139	23792.598867	30.920512
487.610018	23834.067185	30.925530
488.492696	23874.934811	30.930548
488.951344	23918.611061	30.935565
489.301428	23956.155726	30.940583
489.801765	23994.877720	30.945600
490.153106	24036.769959	30.950618
491.049012	24076.915549	30.955636
491.314057	24125.564036	30.960653
492.279472	24158.690921	30.965671
492.991460	24198.372486	30.970688
493.463095	24221.452869	30.975706
494.445188	24250.387627	30.980724
494.466285	24284.912951	30.985741
495.147797	24314.855130	30.990759
495.650469	24339.725503	30.995776
496.230866	24370.062666	31.000794
497.194355	24394.450613	31.005812
497.625107	24426.896540	31.010829
497.920418	24454.030067	31.015847
498.318171	24478.980141	31.020864
498.915681	24501.251333	31.025882
499.523619	24533.309645	31.030900
499.955132	24566.172759	31.035917
500.656953	24590.462655	31.040935
500.736946	24625.478631	31.045952
500.757531	24650.102151	31.050970
501.922460	24687.780436	31.055988
502.200422	24720.269584	31.061005
502.436538	24749.883629	31.066023
502.949486	24778.026425	31.071040
503.346268	24825.512284	31.076058
503.901874	24861.124494	31.081076
504.433911	24888.594608	31.086093
505.007925	24938.182814	31.091111
505.323264	24970.925649	31.096128
505.617203	25017.113513	31.101146
506.559353	25049.133263	31.106164
506.941186	25096.318753	31.111181
507.598742	25126.051014	31.116199
508.154286	25170.384789	31.121216
508.484360	25199.169646	31.126234
508.936077	25242.236866	31.131252
509.588091	25279.850766	31.136269
509.778517	25310.009920	31.141287
510.568727	25350.452590	31.146304
510.398907	25393.534739	31.151322
511.418918	25434.453696	31.156340
511.542751	25484.656826	31.161357
511.995853	25518.541930	31.166375
512.601012	25567.387438	31.171392
513.031258	25617.416804	31.176410
513.633678	25651.177771	31.181428
514.056882	25699.009169	31.186445
514.789071	25748.600032	31.191463
515.575465	25781.719561	31.196480
515.657361	25826.659382	31.201498
516.550374	25860.836807	31.206516
516.895019	25895.226054	31.211533
517.207742	25935.384007	31.216551
518.077120	25969.919207	31.221568
518.209324	26016.463177	31.226586
518.490155	26047.765894	31.231604
518.477400	26094.503247	31.236621
519.578334	26127.315264	31.241639
520.344969	26182.204215	31.246656
521.003578	26218.497987	31.251674
522.244066	26245.676392	31.256692
522.648438	26276.138643	31.261709
523.124116	26298.354960	31.266727
523.993200	26329.888856	31.271744
524.367673	26359.938771	31.276762
524.930478	26394.996424	31.281780
525.231580	26424.994659	31.286797
525.808755	26456.176037	31.291815
526.108770	26489.637889	31.296832
526.263613	26527.135600	31.301850
527.422015	26552.039357	31.306868
528.278117	26581.932465	31.311885
528.829443	26616.183327	31.316903
529.385601	26646.774189	31.321920
529.661269	26681.794881	31.326938
530.012488	26715.084814	31.331956
530.650053	26752.172831	31.336973
531.021353	26777.022438	31.341991
531.709451	26816.776104	31.347008
531.898192	26850.780444	31.352026
532.686292	26870.344872	31.357044
533.544799	26898.044994	31.362061
534.113662	26932.830874	31.367079
534.718727	26964.223581	31.372096
534.964947	26999.432691	31.377114
535.568039	27028.348303	31.382132
536.225423	27067.626912	31.387149
536.352574	27094.303527	31.392167
537.207463	27132.489724	31.397184
537.338753	27175.750003	31.402202
537.977674	27209.962955	31.407220
538.552074	27247.630534	31.412237
539.026649	27286.710499	31.417255
539.450658	27327.264709	31.422272
540.000592	27371.654763	31.427290
540.462608	27401.995972	31.432308
540.561788	27450.330700	31.437325
541.187459	27493.274522	31.442343
541.943580	27548.156180	31.447360
542.342518	27586.572222	31.452378
542.625282	27639.587473	31.457396
543.258036	27683.813627	31.462413
543.879046	27737.813019	31.467431
544.663618	27776.535968	31.472448
544.900125	27813.840055	31.477466
545.505328	27860.030208	31.482484
545.982642	27906.954586	31.487501
546.735180	27963.253701	31.492519
547.410347	27999.623937	31.497536
547.314179	28047.516460	31.502554
548.179171	28101.605244	31.507572
548.500381	28142.903943	31.512589
548.841713	28192.827109	31.517607
549.923783	28241.219281	31.522624
550.332689	28294.456780	31.527642
551.083258	28334.797829	31.532660
552.028065	28378.894749	31.537677
552.431321	28417.292725	31.542695
553.101860	28458.032033	31.547712
553.795039	28490.791277	31.552730
554.404365	28520.434916	31.557748
555.189811	28552.781697	31.562765
555.425134	28589.695508	31.567783
555.977291	28616.232107	31.572800
556.404122	28661.939875	31.577818
556.840377	28689.872520	31.582836
557.613478	28731.070458	31.587853
558.147684	28766.086097	31.592871
558.670529	28804.750617	31.597888
559.228046	28844.806693	31.602906
559.436406	28882.072870	31.607924
560.142504	28914.976162	31.612941
560.770028	28955.419764	31.617959
561.878072	28987.154466	31.622976
561.992879	29021.837624	31.627994
562.474557	29069.124281	31.633012
563.609351	29104.394648	31.638029
563.487974	29141.820083	31.643047
564.270290	29181.361441	31.648064
564.638400	29230.088336	31.653082
565.191354	29275.234248	31.658100
565.674340	29314.993126	31.663117
566.121484	29363.847094	31.668135
566.978377	29407.087640	31.673152
567.544370	29447.175181	31.678170
567.903664	29493.186081	31.683188
568.917001	29528.577224	31.688205
569.026745	29576.611934	31.693223
569.417315	29614.736011	31.698240
569.957920	29665.959154	31.703258
570.568385	29715.724041	31.708276
571.492074	29766.887799	31.713293
571.789251	29815.823078	31.718311
572.489884	29859.107867	31.723328
572.962939	29922.409033	31.728346
573.303166	29962.204031	31.733364
574.302723	30002.490647	31.738381
574.674860	30049.208754	31.743399
575.303529	30095.823821	31.748416
576.187059	30153.613000	31.753434
576.837584	30194.896178	31.758452
577.503723	30231.107442	31.763469
577.776231	30287.386544	31.768487
578.341584	30328.607394	31.773504
579.027641	30376.225552	31.778522
580.035191	30425.026409	31.783540
580.551578	30456.368763	31.788557
580.901414	30503.767744	31.793575
581.836574	30544.311977	31.798592
582.161285	30592.878184	31.803610
582.847691	30637.898853	31.808628
583.240798	30674.437858	31.813645
583.556613	30726.223300	31.818663
584.633091	30769.912952	31.823680
584.903633	30813.639660	31.828698
585.780009	30862.461974	31.833716
586.404235	30906.677455	31.838733
587.030976	30950.582893	31.843751
587.534721	30993.527757	31.848768
588.005041	31034.297029	31.853786
588.696117	31073.236736	31.858804
589.344019	31111.064345	31.863821
589.779344	31164.166101	31.868839
590.207928	31196.022641	31.873856
591.114450	31240.985073	31.878874
591.580501	31286.882216	31.883892
592.612502	31313.284390	31.888909
592.973686	31356.688383	31.893927
593.604860	31390.271061	31.898944
593.940194	31422.136145	31.903962
594.616759	31466.344676	31.908980
595.038686	31503.607637	31.913997
595.846141	31538.800394	31.919015
595.889964	31577.437230	31.924032
596.479753	31628.638626	31.929050
596.866951	31668.050304	31.934068
597.173504	31715.256508	31.939085
597.980831	31766.803676	31.944103
598.236417	31815.187542	31.949120
598.546495	31870.997301	31.954138
599.300567	31930.663850	31.959156
600.191400	31986.939820	31.964173
600.546774	32045.638331	31.969191
601.242494	32096.609451	31.974208
602.002419	32146.091415	31.979226
602.085241	32204.282811	31.984244
603.341433	32255.792925	31.989261
603.897245	32315.181675	31.994279
604.358000	32374.522174	31.999296
605.001768	32432.519413	32.004314
605.333105	32489.787863	32.009332
606.364109	32543.205011	32.014349
606.759257	32602.992581	32.019367
607.362248	32656.160555	32.024384
608.003636	32707.362896	32.029402
608.867796	32767.330801	32.034420
609.502342	32817.434462	32.039437
610.184048	32889.423847	32.044455
610.792918	32938.362233	32.049472
611.716342	32992.815119	32.054490
612.352032	33043.867444	32.059508
612.726385	33080.950974	32.064525
613.479055	33147.183485	32.069543
614.077444	33193.304469	32.074560
615.158441	33246.747247	32.079578
615.462315	33291.441253	32.084596
616.356885	33341.689034	32.089613
616.573141	33396.531231	32.094631
617.363377	33449.197916	32.099648
617.943614	33489.626139	32.104666
618.440788	33537.521194	32.109684
619.282609	33591.880868	32.114701
620.004174	33646.834723	32.119719
620.625575	33697.789714	32.124736
621.666976	33737.874771	32.129754
622.509807	33780.165664	32.134772
623.145975	33817.468954	32.139789
623.655122	33862.246022	32.144807
624.047627	33913.888363	32.149824
624.628042	33952.073044	32.154842
625.169138	33998.141497	32.159860
626.018710	34043.491864	32.164877
626.155811	34093.928912	32.169895
626.699716	34146.395447	32.174912
627.869533	34191.949176	32.179930
627.939517	34240.038784	32.184948
628.679127	34280.842031	32.189965
629.105112	34341.236711	32.194983
629.648824	34388.532158	32.200000
630.260205	34443.726536	32.205018
630.721133	34492.780095	32.210036
632.443594	34518.073587	32.215053
633.766366	34559.911992	32.220071
634.413782	34593.023114	32.225088
634.958242	34639.927016	32.230106
635.318292	34664.756269	32.235124
635.355451	34694.662207	32.240141
636.453063	34737.206202	32.245159
637.040885	34763.441647	32.250176
637.660810	34802.026364	32.255194
637.812304	34844.496572	32.260212
638.302490	34881.388219	32.265229
638.926602	34916.539343	32.270247
639.657386	34944.845531	32.275264
640.877126	34980.346620	32.280282
641.019863	35019.537118	32.285300
641.924458	35057.483663	32.290317
642.210621	35099.952387	32.295335
642.946034	35146.473623	32.300352
643.650536	35191.994472	32.305370
644.068825	35247.910184	32.310388
644.724696	35289.702115	32.315405
645.395934	35328.855172	32.320423
645.523932	35374.801263	32.325440
646.249331	35432.800409	32.330458
646.990023	35487.237629	32.335476
647.567713	35531.874798	32.340493
648.181012	35589.784338	32.345511
648.244910	35661.645448	32.350528
649.100530	35712.695307	32.355546
649.383994	35770.877986	32.360564
650.281393	35832.948645	32.365581
651.053423	35894.223352	32.370599
651.286101	35949.980126	32.375616
652.087744	36011.010291	32.380634
652.917013	36078.555260	32.385652
653.566419	36136.770495	32.390669
654.210673	36196.289221	32.395687
654.714403	36271.801821	32.400704
656.008296	36324.106427	32.405722
656.271215	36393.163234	32.410740
657.180301	36445.009554	32.415757
657.803312	36507.795141	32.420775
658.413142	36575.287326	32.425792
659.242024	36626.292960	32.430810
659.710630	36691.234002	32.435828
660.331117	36753.508535	32.440845
661.415852	36818.885195	32.445863
661.932811	36879.133837	32.450880
662.634395	36931.494205	32.455898
663.358844	36989.813908	32.460916
664.330113	37043.251773	32.465933
664.627901	37096.212876	32.470951
665.449071	37157.123147	32.475968
666.411759	37212.516652	32.480986
666.891610	37273.663763	32.486004
667.348061	37324.994623	32.491021
668.261332	37384.879480	32.496039
669.003947	37442.084688	32.501056
669.535883	37490.008569	32.506074
670.059662	37549.530856	32.511092
670.623677	37606.650487	32.516109
671.273631	37661.967373	32.521127
672.190446	37712.443397	32.526144
673.051589	37769.182067	32.531162
673.779359	37830.165705	32.536180
674.394028	37880.366665	32.541197
675.103011	37937.540492	32.546215
675.756979	37991.510705	32.551232
676.825483	38035.912304	32.556250
677.747064	38094.925211	32.561268
678.287459	38130.916739	32.566285
679.231161	38172.941434	32.571303
679.846413	38233.165939	32.576320
680.332424	38252.465633	32.581338
680.674768	38300.016130	32.586356
681.274889	38350.403838	32.591373
682.068207	38384.807140	32.596391
682.470734	38428.674542	32.601408
683.653361	38481.691033	32.606426
684.117641	38528.173331	32.611444
684.612442	38571.527092	32.616461
685.127475	38623.104884	32.621479
685.891077	38680.082475	32.626496
686.555475	38708.119441	32.631514
687.069625	38767.267181	32.636532
687.830845	38820.014950	32.641549
688.547321	38871.745367	32.646567
688.967415	38931.553221	32.651584
689.568983	38979.532823	32.656602
690.336163	39039.900353	32.661620
690.889606	39090.834582	32.666637
691.678537	39149.965891	32.671655
692.343982	39218.418958	32.676672
692.769114	39280.611083	32.681690
693.378813	39342.167563	32.686708
694.246280	39404.044553	32.691725
695.219763	39463.457862	32.696743
695.341666	39533.470012	32.701760
696.751360	39582.956730	32.706778
697.857698	39640.945928	32.711796
698.283843	39697.061760	32.716813
699.440381	39751.837182	32.721831
700.016127	39815.278521	32.726848
700.352615	39856.382860	32.731866
701.180914	39915.579698	32.736884
701.804571	39971.798300	32.741901
702.544599	40034.019458	32.746919
703.417140	40093.127680	32.751936
703.933376	40147.554767	32.756954
704.862863	40201.753233	32.761972
704.993466	40272.398824	32.766989
706.052260	40327.760092	32.772007
706.786097	40389.312869	32.777024
707.129060	40446.879178	32.782042
707.838209	40516.417304	32.787060
708.717752	40578.732139	32.792077
709.567061	40635.669916	32.797095
710.159361	40701.033839	32.802112
711.139559	40750.830408	32.807130
711.856757	40808.162336	32.812148
712.393858	40877.753694	32.817165
713.309988	40939.874138	32.822183
714.059976	41005.650808	32.827200
714.784267	41064.051121	32.832218
715.148975	41124.493428	32.837236
715.905640	41185.083592	32.842253
717.196488	41230.810573	32.847271
717.908716	41297.055681	32.852288
718.995244	41345.148430	32.857306
719.687240	41395.883087	32.862324
720.087594	41456.491524	32.867341
720.750005	41500.546040	32.872359
721.603023	41558.756877	32.877376
722.643468	41622.687700	32.882394
722.793571	41670.882666	32.887412
723.856022	41729.858250	32.892429
724.422629	41772.903647	32.897447
725.025460	41834.676958	32.902464
725.982423	41889.697543	32.907482
726.501781	41941.870731	32.912500
726.740374	41993.297168	32.917517
727.590249	42043.262441	32.922535
727.814997	42100.927404	32.927552
728.728562	42159.320152	32.932570
729.351942	42212.420170	32.937588
729.831488	42278.805665	32.942605
730.519528	42336.032290	32.947623
730.691279	42402.301628	32.952640
731.937686	42460.738236	32.957658
732.738296	42530.761860	32.962676
733.506578	42602.802034	32.967693
734.167551	42659.053366	32.972711
734.931915	42733.365195	32.977728
735.496968	42800.396737	32.982746
736.619501	42872.369998	32.987764
736.966194	42936.324093	32.992781
737.497735	43008.174748	32.997799
738.360415	43069.101484	33.002816
739.375298	43140.149958	33.007834
740.424231	43212.192710	33.012852
740.710523	43272.526632	33.017869
741.652345	43340.829418	33.022887
742.170393	43425.105903	33.027904
742.949726	43491.429404	33.032922
744.080770	43560.203094	33.037940
744.625573	43638.612861	33.042957
745.586226	43701.904336	33.047975
746.082839	43771.574411	33.052992
746.824017	43832.711920	33.058010
748.268303	43906.264033	33.063028
748.988509	43978.037867	33.068045
749.808727	44034.312188	33.073063
750.473375	44116.373624	33.078080
751.262895	44170.546759	33.083098
751.848967	44244.562505	33.088116
752.848420	44312.290040	33.093133
753.735042	44362.381351	33.098151
754.634953	44433.103979	33.103168
755.382669	44488.530490	33.108186
756.209401	44551.573247	33.113204
756.861773	44615.750269	33.118221
757.729431	44669.476005	33.123239
758.140151	44737.631729	33.128256
759.182063	44803.760142	33.133274
759.846461	44863.647351	33.138292
760.428697	44932.517051	33.143309
761.521708	44996.892249	33.148327
761.984025	45059.714849	33.153344
762.850817	45123.803026	33.158362
763.707509	45182.351769	33.163380
764.139048	45255.673817	33.168397
764.839776	45323.615394	33.173415
765.341754	45393.821061	33.178432
766.419228	45461.432408	33.183450
767.482581	45522.967204	33.188468
767.891328	45585.673108	33.193485
768.539236	45659.291731	33.198503
769.832675	45725.883452	33.203520
770.171480	45792.870680	33.208538
771.046408	45851.064094	33.213556
771.809268	45922.255578	33.218573
772.644182	46002.127704	33.223591
773.429402	46075.391052	33.228608
774.322085	46141.881924	33.233626
774.912227	46199.753677	33.238644
775.678636	46272.463922	33.243661
776.559859	46334.427827	33.248679
777.196477	46397.214393	33.253696
777.846698	46457.690055	33.258714
778.784724	46512.503649	33.263732
779.416916	46582.869891	33.268749
780.230225	46633.920276	33.273767
781.134426	46701.043605	33.278784
781.770960	46761.882797	33.283802
782.812641	46818.439630	33.288820
783.264131	46887.576076	33.293837
784.117887	46942.745442	33.298855
784.618384	47016.878565	33.303872
785.300926	47083.582061	33.308890
786.052121	47150.325676	33.313908
786.886231	47223.351083	33.318925
787.452883	47287.511139	33.323943
788.409069	47368.767315	33.328960
789.254682	47432.542743	33.333978
790.113457	47506.912705	33.338996
791.048875	47578.228064	33.344013
792.396965	47647.423376	33.349031
793.370887	47706.561441	33.354048
793.991908	47776.623155	33.359066
795.028825	47835.119121	33.364084
795.667128	47900.244010	33.369101
796.589469	47951.413254	33.374119
797.468882	48017.196844	33.379136
798.129024	48088.449112	33.384154
798.801659	48148.027465	33.389172
799.604971	48219.238877	33.394189
800.488818	48281.764442	33.399207
801.095527	48331.996755	33.404224
801.822354	48407.687132	33.409242
802.670444	48472.641824	33.414260
803.793465	48554.755661	33.419277
804.130953	48612.919654	33.424295
805.227732	48680.575610	33.429312
805.874936	48756.298521	33.434330
807.114250	48811.899567	33.439348
807.455150	48892.440848	33.444365
808.103757	48954.214055	33.449383
809.344778	49023.601049	33.454400
810.347227	49099.693684	33.459418
811.351964	49153.193670	33.464436
811.908201	49225.889172	33.469453
812.792990	49292.656247	33.474471
813.542188	49362.759830	33.479488
814.189940	49432.297359	33.484506
815.035130	49500.589625	33.489524
815.723552	49567.350110	33.494541
816.624063	49634.046140	33.499559
817.819469	49701.196279	33.504576
818.387824	49771.158439	33.509594
819.392576	49824.286710	33.514612
819.935333	49901.668328	33.519629
820.765157	49975.848399	33.524647
821.877071	50048.630837	33.529664
822.272221	50122.898027	33.534682
823.127332	50192.456198	33.539700
824.061016	50266.715945	33.544717
824.417450	50332.568635	33.549735
825.259196	50405.267720	33.554752
825.797394	50481.930720	33.559770
826.961153	50559.692412	33.564788
827.491084	50637.445470	33.569805
828.238557	50719.277542	33.574823
829.963524	50785.652438	33.579840
830.894151	50845.918948	33.584858
831.875902	50915.991071	33.589876
832.674013	50979.435808	33.594893
833.430252	51037.338293	33.599911
834.564163	51086.026672	33.604928
834.897311	51148.266157	33.609946
835.610728	51213.698814	33.614964
836.483247	51271.748294	33.619981
837.030464	51337.738663	33.624999
837.946522	51407.892105	33.630016
838.365886	51475.876883	33.635034
839.793057	51534.846727	33.640052
839.753693	51607.579192	33.645069
840.470629	51686.616429	33.650087
842.046574	51756.320201	33.655104
842.819233	51834.267286	33.660122
843.807082	51897.849519	33.665140
844.534255	51969.755124	33.670157
845.158445	52044.562305	33.675175
846.479509	52114.496655	33.680192
846.925003	52197.665440	33.685210
847.834590	52258.963961	33.690228
848.858518	52344.466669	33.695245
849.798810	52407.057948	33.700263
850.416600	52484.398564	33.705280
851.227789	52569.504940	33.710298
852.283145	52635.983055	33.715316
852.474103	52710.467501	33.720333
853.285402	52793.227121	33.725351
854.411555	52877.848984	33.730368
855.388732	52966.335265	33.735386
856.000087	53038.122987	33.740404
856.886605	53121.606078	33.745421
857.766349	53195.889936	33.750439
859.284425	53271.707236	33.755456
859.728884	53359.588201	33.760474
860.873585	53437.678896	33.765492
861.552342	53519.392313	33.770509
862.470059	53599.353961	33.775527
864.002877	53671.525402	33.780544
864.824235	53741.998028	33.785562
866.200586	53802.107901	33.790580
867.074464	53869.320175	33.795597
867.749003	53942.771415	33.800615
868.839753	54015.506312	33.805632
869.512583	54082.940333	33.810650
869.963123	54150.124389	33.815668
871.094525	54223.593981	33.820685
871.688920	54292.907589	33.825703
872.831707	54362.091739	33.830720
873.520544	54438.763299	33.835738
874.244138	54518.492512	33.840756
875.466564	54587.734539	33.845773
875.715812	54666.354726	33.850791
876.817947	54742.178244	33.855808
877.908573	54826.002656	33.860826
878.382377	54907.246539	33.865844
879.386423	54977.029961	33.870861
879.913939	55062.929941	33.875879
880.698379	55140.822912	33.880896
881.186191	55230.134302	33.885914
882.052546	55310.818527	33.890932
883.406148	55406.374780	33.895949
883.788807	55495.595957	33.900967
885.262986	55575.895363	33.905984
885.981611	55661.362744	33.911002
886.968417	55745.098988	33.916020
887.962974	55825.366315	33.921037
888.803882	55924.371213	33.926055
890.002525	55997.570057	33.931072
890.419502	56077.016833	33.936090
891.622929	56153.550556	33.941108
892.626950	56215.800307	33.946125
892.796107	56294.476327	33.951143
893.808342	56361.781736	33.956160
894.871841	56441.230345	33.961178
895.975016	56510.907918	33.966196
896.651495	56584.987261	33.971213
897.628142	56661.671834	33.976231
898.957335	56725.536749	33.981248
900.066043	56796.650915	33.986266
901.083995	56872.785466	33.991284
902.341263	56943.123820	33.996301
902.895715	57008.787217	34.001319
903.540612	57077.797313	34.006336
904.587849	57147.365204	34.011354
905.457394	57218.024204	34.016372
906.410768	57296.682709	34.021389
906.768838	57374.630370	34.026407
907.840958	57447.720452	34.031424
908.639086	57533.264437	34.036442
909.763353	57609.878440	34.041460
910.954416	57689.488551	34.046477
911.594957	57764.691037	34.051495
912.860012	57842.790167	34.056512
914.094737	57903.400833	34.061530
914.902042	57974.938827	34.066548
915.481365	58057.506111	34.071565
916.240363	58133.330546	34.076583
917.380988	58212.969230	34.081600
918.002593	58284.429454	34.086618
918.819784	58387.340643	34.091636
919.944783	58462.185083	34.096653
920.943111	58535.695025	34.101671
921.764266	58613.523978	34.106688
922.844157	58693.578772	34.111706
923.630864	58767.736299	34.116724
924.422247	58851.444201	34.121741
925.062869	58948.055986	34.126759
926.223353	59037.049006	34.131776
927.032741	59119.989185	34.136794
927.860874	59207.110443	34.141812
928.864377	59299.135313	34.146829
929.571718	59385.181028	34.151847
930.511641	59488.413250	34.156864
931.634770	59572.723935	34.161882
932.566307	59662.254915	34.166900
933.322835	59759.915242	34.171917
934.078223	59855.993753	34.176935
935.434970	59932.705524	34.181952
936.507390	60022.279194	34.186970
937.719422	60113.983526	34.191988
938.900891	60183.501294	34.197005
940.013739	60270.006044	34.202023
940.918515	60354.296458	34.207040
941.823981	60432.061147	34.212058
942.485982	60520.833367	34.217076
943.766311	60603.597690	34.222093
944.360360	60685.677901	34.227111
945.406315	60768.150116	34.232128
946.408024	60847.629174	34.237146
947.051629	60939.292161	34.242164
948.309103	61013.706070	34.247181
949.047491	61103.531924	34.252199
950.237175	61171.797913	34.257216
951.435862	61262.451541	34.262234
952.565935	61330.119578	34.267252
953.807218	61407.778123	34.272269
954.265157	61479.918857	34.277287
955.044538	61545.800060	34.282304
956.187015	61614.049307	34.287322
957.147707	61686.758048	34.292340
958.112994	61762.314801	34.297357
958.512622	61845.853410	34.302375
959.127541	61921.515830	34.307392
960.361388	61997.810100	34.312410
960.987358	62079.307628	34.317428
961.834537	62169.025485	34.322445
962.637551	62252.141860	34.327463
963.338347	62335.647905	34.332480
964.184288	62425.715046	34.337498
965.395992	62520.156737	34.342516
966.197683	62614.972793	34.347533
967.058709	62713.989607	34.352551
968.229488	62800.962687	34.357568
969.251792	62890.193787	34.362586
970.126038	62992.013985	34.367604
971.369058	63076.742176	34.372621
971.854649	63176.154784	34.377639
973.193444	63264.401066	34.382656
974.232034	63366.222536	34.387674
975.235387	63462.061289	34.392692
976.053631	63548.775341	34.397709
977.276677	63649.474084	34.402727
978.722242	63749.378932	34.407744
979.760094	63837.275267	34.412762
980.586091	63927.857402	34.417780
981.992150	64020.900807	34.422797
982.634899	64114.101360	34.427815
983.802142	64206.195052	34.432832
984.753525	64290.934786	34.437850
985.674487	64385.827649	34.442868
987.010906	64466.564019	34.447885
987.801511	64564.839463	34.452903
988.686420	64647.229384	34.457920
990.027165	64745.996003	34.462938
990.758149	64836.792471	34.467956
991.861511	64918.402242	34.472973
992.398113	65015.585769	34.477991
993.575000	65102.262039	34.483008
995.286059	65192.609684	34.488026
996.095747	65291.461111	34.493044
997.538860	65373.361344	34.498061
998.265058	65463.477077	34.503079
999.522560	65535.087251	34.508096
1000.428153	65623.915766	34.513114
1001.098876	65705.126938	34.518132
1002.252868	65793.018377	34.523149
1003.066143	65888.623757	34.528167
1004.067616	65978.223647	34.533184
1005.531088	66068.081158	34.538202
1006.320814	66151.946974	34.543220
1007.157190	66236.622526	34.548237
1008.140106	66325.568094	34.553255
1008.926613	66416.323615	34.558272
1010.570779	66502.805335	34.563290
1011.183180	66594.171067	34.568308
1012.165269	66681.376917	34.573325
1013.111323	66764.175763	34.578343
1014.273935	66864.624536	34.583360
1015.090513	66947.716381	34.588378
1015.854803	67046.442437	34.593396
1017.189567	67132.638901	34.598413
1018.300054	67206.328056	34.603431
1018.954463	67303.970549	34.608448
1020.008694	67388.780645	34.613466
1020.751381	67489.499853	34.618484
1021.955579	67575.629499	34.623501
1022.617963	67653.479841	34.628519
1023.422495	67737.962737	34.633536
1024.776047	67831.382920	34.638554
1025.693911	67927.289928	34.643572
1026.403699	68005.330241	34.648589
1027.979567	68107.099866	34.653607
1028.392138	68202.890277	34.658624
1029.530432	68290.286253	34.663642
1030.097629	68402.142119	34.668660
1031.396608	68494.363860	34.673677
1032.452425	68598.489473	34.678695
1033.296450	68698.615135	34.683712
1034.359284	68790.450467	34.688730
1035.411747	68896.591318	34.693748
1037.135892	69006.224543	34.698765
1038.030046	69103.690932	34.703783
1038.745154	69195.683144	34.708800
1040.074098	69290.410502	34.713818
1040.983074	69398.228382	34.718836
1041.810469	69493.446130	34.723853
1043.030049	69609.251807	34.728871
1044.018711	69711.157168	34.733888
1045.315781	69815.554074	34.738906
1046.356794	69910.341185	34.743924
1047.523908	70017.247634	34.748941
1048.417585	70126.514642	34.753959
1049.684914	70228.138037	34.758976
1050.984144	70329.585895	34.763994
1051.870374	70434.011245	34.769012
1052.876329	70521.625334	34.774029
1054.092563	70630.945568	34.779047
1054.966068	70734.633232	34.784064
1056.062643	70834.449215	34.789082
1057.213412	70936.777407	34.794100
1058.196068	71037.093153	34.799117
1059.167413	71145.427822	34.804135
1060.276008	71253.918882	34.809152
1061.331334	71355.491016	34.814170
1062.131849	71467.260449	34.819188
1063.279507	71575.455468	34.824205
1064.657744	71681.120038	34.829223
1065.703729	71786.811421	34.834240
1066.663972	71891.212071	34.839258
1067.991354	72002.357172	34.844276
1069.462502	72098.497434	34.849293
1070.490654	72191.338051	34.854311
1071.412842	72294.099742	34.859328
1072.722175	72387.251909	34.864346
1073.696036	72493.717279	34.869364
1074.794064	72588.270909	34.874381
1076.016169	72694.736444	34.879399
1077.048868	72790.592847	34.884416
1078.295748	72890.950534	34.889434
1079.409952	72995.331591	34.894452
1080.274479	73089.277412	34.899469
1081.275340	73190.827107	34.904487
1082.294302	73289.714562	34.909504
1083.747810	73384.393026	34.914522
1084.672525	73489.970780	34.919540
1085.637921	73581.686119	34.924557
1087.003267	73676.923984	34.929575
1087.919950	73776.247147	34.934592
1088.976106	73870.887868	34.939610
1090.045994	73979.345491	34.944628
1090.991805	74077.613959	34.949645
1092.452118	74172.572826	34.954663
1092.921500	74276.704634	34.959680
1094.461280	74364.508060	34.964698
1095.383657	74449.507292	34.969716
1096.145000	74544.487617	34.974733
1097.402876	74628.700547	34.979751
1098.331064	74728.760116	34.984768
1099.481993	74824.415447	34.989786
1100.558065	74913.749504	34.994804
1101.772769	74996.234995	34.999821
1102.932078	75091.509978	35.004839
1103.704963	75181.525451	35.009856
1105.233797	75282.798259	35.014874
1106.322164	75382.860668	35.019892
1107.544772	75470.248421	35.024909
1108.784713	75571.567285	35.029927
1109.515343	75667.037703	35.034944
1110.485073	75761.951898	35.039962
1111.085974	75861.952627	35.044980
1112.604428	75978.088040	35.049997
1113.648947	76073.498370	35.055015
1114.682438	76184.098639	35.060032
1115.957431	76283.337311	35.065050
1117.150136	76385.515284	35.070068
1118.481440	76498.996614	35.075085
1119.803613	76601.091912	35.080103
1120.760413	76711.655605	35.085120
1121.722965	76800.405547	35.090138
1123.105893	76912.601163	35.095156
1124.131211	77012.996107	35.100173
1125.241195	77123.360285	35.105191
1126.155049	77233.451417	35.110208
1127.278403	77340.748831	35.115226
1128.535466	77445.923013	35.120244
1129.464703	77554.948960	35.125261
1130.523205	77659.990194	35.130279
1131.351288	77785.171609	35.135296
1132.711471	77896.133362	35.140314
1133.893472	78016.066895	35.145332
1135.349366	78129.991675	35.150349
1136.776402	78232.000753	35.155367
1137.902382	78350.082259	35.160384
1138.802373	78466.527249	35.165402
1140.117517	78568.783023	35.170420
1140.994800	78681.216625	35.175437
1142.549988	78789.301274	35.180455
1143.564672	78905.160193	35.185472
1144.889018	79022.618296	35.190490
1145.955310	79118.707310	35.195508
1146.794498	79233.429423	35.200525
1147.984919	79347.881976	35.205543
1149.128155	79459.111842	35.210560
1150.200492	79575.838736	35.215578
1151.236949	79689.949277	35.220596
1152.298319	79816.167788	35.225613
1153.696374	79922.216314	35.230631
1154.991708	80042.799805	35.235648
1156.361685	80139.681242	35.240666
1157.845511	80258.297979	35.245684
1158.490596	80370.014445	35.250701
1160.167600	80472.132250	35.255719
1161.547124	80578.806954	35.260736
1162.534963	80677.612112	35.265754
1163.995333	80775.723277	35.270772
1164.901925	80892.126759	35.275789
1166.377327	80990.312354	35.280807
1167.344971	81096.875778	35.285824
1168.207508	81206.382609	35.290842
1169.733418	81306.385852	35.295860
1170.271055	81403.439246	35.300877
1171.717629	81506.040135	35.305895
1172.624656	81600.148049	35.310912
1174.035247	81693.468396	35.315930
1174.870131	81787.385453	35.320948
1175.792986	81888.143462	35.325965
1177.348883	81984.204163	35.330983
1178.247871	82094.443632	35.336000
1179.623797	82198.261680	35.341018
1180.657916	82304.477252	35.346036
1181.580487	82407.150323	35.351053
1182.826312	82515.322923	35.356071
1183.722183	82632.280093	35.361088
1185.019120	82729.435258	35.366106
1185.957163	82849.807697	35.371124
1186.967508	82955.902715	35.376141
1188.363265	83065.346444	35.381159
1189.945770	83189.687171	35.386176
1191.092938	83308.622600	35.391194
1192.269594	83415.048219	35.396212
1193.813482	83524.648047	35.401229
1195.088954	83630.463579	35.406247
1195.917125	83753.479747	35.411264
1197.538273	83870.341796	35.416282
1199.023658	83980.471981	35.421300
1199.860883	84084.127371	35.426317
1201.489102	84187.774054	35.431335
1202.318349	84297.944239	35.436352
1203.680734	84416.293273	35.441370
1205.021598	84523.077592	35.446388
1206.416352	84634.795599	35.451405
1207.708868	84741.106760	35.456423
1208.765439	84854.348099	35.461440
1210.188377	84959.220607	35.466458
1211.729424	85058.449120	35.471476
1212.812706	85174.665286	35.476493
1214.237347	85274.470196	35.481511
1215.568735	85377.989986	35.486528
1216.454113	85480.553192	35.491546
1217.884333	85584.742593	35.496564
1218.726087	85689.834939	35.501581
1220.298431	85796.727342	35.506599
1221.196606	85920.198067	35.511616
1222.518437	86026.154603	35.516634
1223.555606	86121.587700	35.521652
1224.494247	86256.217259	35.526669
1225.926323	86360.687943	35.531687
1227.435589	86479.858920	35.536704
1228.366093	86583.483436	35.541722
1229.589398	86689.140933	35.546740
1230.667714	86804.312647	35.551757
1232.095743	86924.283749	35.556775
1233.008478	87044.994495	35.561792
1234.360072	87164.725042	35.566810
1235.895787	87277.166292	35.571828
1237.032472	87392.255209	35.576845
1238.346809	87513.855795	35.581863
1239.198236	87631.625876	35.586880
1240.362467	87750.602302	35.591898
1241.648189	87864.947555	35.596916
1242.632137	87986.157991	35.601933
1243.945739	88099.409987	35.606951
1245.594658	88215.765687	35.611968
1246.780524	88342.750183	35.616986
1248.140693	88454.995165	35.622004
1249.416390	88575.300876	35.627021
1250.414155	88692.621555	35.632039
1251.812468	88810.805466	35.637056
1253.167419	88926.246595	35.642074
1254.690570	89015.936051	35.647092
1255.791534	89116.222683	35.652109
1256.920344	89209.446484	35.657127
1258.106854	89313.775816	35.662144
1259.500068	89420.760027	35.667162
1260.624686	89513.377130	35.672180
1261.487696	89625.399781	35.677197
1262.854330	89736.115165	35.682215
1264.138081	89843.954367	35.687232
1264.884441	89964.715631	35.692250
1266.567621	90063.685531	35.697268
1267.670459	90195.215258	35.702285
1268.987369	90304.787217	35.707303
1270.080416	90421.504238	35.712320
1271.116503	90542.007289	35.717338
1272.456040	90668.331457	35.722356
1274.154524	90787.173542	35.727373
1275.312506	90899.294465	35.732391
1276.566427	91034.695179	35.737408
1277.979876	91155.268693	35.742426
1279.633396	91263.879252	35.747444
1280.560960	91392.843377	35.752461
1281.965811	91507.868483	35.757479
1283.376006	91633.311206	35.762496
1284.218628	91753.621093	35.767514
1285.626264	91869.585022	35.772532
1287.202396	92002.721966	35.777549
1288.706957	92120.243362	35.782567
1289.962083	92242.658271	35.787584
1290.983728	92380.648694	35.792602
1292.448223	92501.764630	35.797620
1293.764063	92628.024643	35.802637
1295.392568	92728.418673	35.807655
1296.508319	92850.819702	35.812672
1297.743020	92984.495724	35.817690
1299.391310	93103.912409	35.822708
1300.850296	93230.152636	35.827725
1302.063213	93349.790144	35.832743
1303.433251	93459.884933	35.837760
1304.676759	93588.948623	35.842778
1305.762227	93705.324586	35.847796
1306.961508	93827.767223	35.852813
1308.113385	93958.532490	35.857831
1309.643174	94085.322917	35.862848
1310.671050	94216.235331	35.867866
1312.228788	94347.420731	35.872884
1313.519613	94480.093202	35.877901
1314.755299	94611.596031	35.882919
1316.173440	94734.553242	35.887936
1317.225727	94875.680917	35.892954
1318.412631	94996.773864	35.897972
1319.825334	95133.245454	35.902989
1321.013224	95270.906106	35.908007
1322.474736	95397.167497	35.913024
1323.324088	95538.811445	35.918042
1325.218314	95665.627679	35.923060
1326.364861	95811.587031	35.928077
1327.700417	95948.822075	35.933095
1329.182549	96070.101412	35.938112
1330.665532	96206.059735	35.943130
1332.131643	96333.604466	35.948148
1333.121564	96476.118099	35.953165
1334.302771	96603.213910	35.958183
1336.143405	96743.175224	35.963200
1337.646121	96870.336159	35.968218
1338.766653	97001.334597	35.973236
1340.127763	97127.238317	35.978253
1341.127081	97253.629847	35.983271
1342.653966	97373.424131	35.988288
1343.984315	97496.773495	35.993306
1345.055934	97602.568729	35.998324
1346.471859	97731.711494	36.003341
1347.719507	97855.227247	36.008359
1348.942502	97973.397803	36.013376
1350.712551	98094.259833	36.018394
1352.326170	98197.855698	36.023412
1353.800930	98324.367651	36.028429
1354.829024	98459.214882	36.033447
1356.102169	98574.464213	36.038464
1357.565120	98689.785833	36.043482
1358.769866	98814.452909	36.048500
1359.779564	98938.364859	36.053517
1361.397484	99058.480935	36.058535
1363.162844	99196.271683	36.063552
1364.667572	99328.880622	36.068570
1365.619740	99442.218091	36.073588
1367.438171	99573.384726	36.078605
1368.579270	99695.466311	36.083623
1369.688372	99826.883838	36.088640
1371.064389	99965.613225	36.093658
1372.525462	100087.507043	36.098676
1374.090173	100216.966311	36.103693
1375.254882	100350.456420	36.108711
1376.768794	100478.669571	36.113728
1377.928442	100621.885281	36.118746
1379.793487	100745.734446	36.123764
1381.215601	100874.217005	36.128781
1382.163192	101017.543535	36.133799
1384.175799	101142.550281	36.138816
1385.011931	101292.272315	36.143834
1386.379175	101410.458418	36.148852
1388.309260	101554.217572	36.153869
1389.401384	101690.120623	36.158887
1391.128022	101825.367643	36.163904
1392.129917	101965.241445	36.168922
1393.390324	102099.585949	36.173940
1395.236149	102233.763816	36.178957
1396.000892	102382.563761	36.183975
1397.519065	102519.380166	36.188992
1398.715768	102674.428019	36.194010
1400.390006	102814.758640	36.199028
1401.567027	102960.124551	36.204045
1402.642039	103111.034841	36.209063
1404.345176	103257.359815	36.214080
1405.622578	103422.465459	36.219098
1406.865231	103564.514669	36.224116
1408.890973	103706.404565	36.229133
1410.119292	103858.219948	36.234151
1411.888493	103995.700727	36.239168
1412.963142	104153.056704	36.244186
1414.504471	104296.368486	36.249204
1415.931403	104435.552627	36.254221
1417.225356	104585.801579	36.259239
1419.031703	104731.368903	36.264256
1420.786500	104873.711674	36.269274
1421.995925	105009.217034	36.274292
1423.815318	105133.089791	36.279309
1425.296829	105279.521533	36.284327
1426.697205	105415.138282	36.289344
1428.152028	105556.858626	36.294362
1429.626008	105685.694150	36.299380
1430.978989	105816.260746	36.304397
1432.288917	105953.288493	36.309415
1433.313358	106085.555620	36.314432
1434.515631	106230.792338	36.319450
1435.484130	106371.615448	36.324468
1437.503900	106506.683694	36.329485
1439.072227	106643.775450	36.334503
1440.519008	106770.336945	36.339520
1441.576326	106902.830375	36.344538
1442.938503	107038.865326	36.349556
1444.125333	107169.462982	36.354573
1445.269127	107311.213697	36.359591
1446.318180	107444.788327	36.364608
1447.739685	107597.896516	36.369626
1449.211279	107755.067977	36.374644
1450.619177	107903.132876	36.379661
1451.985104	108053.335257	36.384679
1453.343488	108207.445058	36.389696
1455.178352	108357.398249	36.394714
1456.839911	108512.463988	36.399732
1458.259922	108668.290816	36.404749
1459.611886	108829.302669	36.409767
1461.335670	108978.007767	36.414784
1463.008204	109131.476790	36.419802
1464.101375	109283.831981	36.424820
1466.084405	109437.431559	36.429837
1467.092012	109597.283194	36.434855
1468.825028	109749.198442	36.439872
1470.627645	109909.244791	36.444890
1471.835679	110061.965932	36.449908
1473.477121	110212.768822	36.454925
1475.135356	110367.057097	36.459943
1476.209519	110527.422547	36.464960
1477.879141	110682.243049	36.469978
1479.692745	110844.181476	36.474996
1481.397086	110988.637176	36.480013
1482.802200	111148.789080	36.485031
1484.062290	111299.212119	36.490048
1486.007410	111448.501961	36.495066
1487.463276	111608.445136	36.500084
1488.813004	111751.094925	36.505101
1490.396854	111911.412678	36.510119
1491.966734	112062.221912	36.515136
1493.651131	112210.173206	36.520154
1494.904446	112370.417648	36.525172
1496.840106	112513.004650	36.530189
1497.979789	112679.571139	36.535207
1499.609631	112831.629812	36.540224
1501.334570	112986.083948	36.545242
1502.376667	113141.532786	36.550260
1504.194542	113280.755005	36.555277
1505.394553	113447.379069	36.560295
1507.169132	113601.739341	36.565312
1508.713089	113754.703046	36.570330
1509.955114	113911.024533	36.575348
1511.564241	114072.413322	36.580365
1512.613448	114237.453801	36.585383
1514.108013	114397.961398	36.590400
1516.025474	114562.690654	36.595418
1517.307825	114716.865939	36.600436
1519.128049	114877.527884	36.605453
1520.699565	115040.195099	36.610471
1522.301647	115188.285532	36.615488
1523.646403	115338.369802	36.620506
1524.720716	115508.916545	36.625524
1526.809680	115674.232895	36.630541
1528.156309	115830.115076	36.635559
1530.041268	115988.184430	36.640576
1532.049716	116135.847612	36.645594
1533.411803	116295.356775	36.650612
1535.012211	116428.486090	36.655629
1536.651106	116594.967381	36.660647
1537.975175	116725.020639	36.665664
1539.498164	116865.710258	36.670682
1540.701676	117010.280580	36.675700
1542.473414	117145.998619	36.680717
1543.495199	117289.114319	36.685735
1544.883951	117434.240900	36.690752
1546.446066	117562.712609	36.695770
1547.717464	117727.150638	36.700788
1549.192275	117863.957569	36.705805
1550.472539	118038.707585	36.710823
1552.055186	118189.121479	36.715840
1553.578515	118342.716218	36.720858
1554.924506	118502.846129	36.725876
1556.124013	118669.417701	36.730893
1557.767659	118832.800560	36.735911
1559.535782	118987.273077	36.740928
1561.577381	119158.028379	36.745946
1562.670967	119322.792758	36.750964
1564.866391	119481.145615	36.755981
1566.391018	119654.330223	36.760999
1567.946400	119816.018631	36.766016
1569.330855	119989.492947	36.771034
1570.992740	120153.259160	36.776052
1572.469273	120329.650836	36.781069
1573.958008	120497.606050	36.786087
1575.334851	120672.606802	36.791104
1577.072625	120857.078518	36.796122
1577.969272	121040.553068	36.801140
1579.818629	121217.385481	36.806157
1581.263174	121404.455126	36.811175
1582.586880	121596.199918	36.816192
1584.342851	121789.235689	36.821210
1585.799337	121983.955424	36.826228
1587.544235	122173.341464	36.831245
1588.989723	122368.128247	36.836263
1590.183145	122566.710118	36.841280
1591.861671	122765.661481	36.846298
1593.522148	122961.952687	36.851316
1595.329835	123169.854681	36.856333
1596.874963	123359.861057	36.861351
1598.345534	123558.074946	36.866368
1600.609295	123753.844864	36.871386
1603.147501	123932.637383	36.876404
1605.328596	124111.537030	36.881421
1607.056297	124297.751747	36.886439
1608.679253	124476.689154	36.891456
1610.293689	124639.073322	36.896474
1611.925604	124818.251894	36.901492
1613.523411	124990.674822	36.906509
1614.949893	125175.177107	36.911527
1616.167342	125347.165994	36.916544
1617.781486	125529.230285	36.921562
1619.289717	125721.854310	36.926580
1621.047177	125902.692761	36.931597
1622.442950	126087.089798	36.936615
1623.635394	126274.272310	36.941632
1625.716483	126467.445032	36.946650
1627.197565	126666.649444	36.951668
1628.742496	126854.566327	36.956685
1629.920237	127052.272033	36.961703
1631.586527	127236.327657	36.966720
1633.465944	127432.555793	36.971738
1634.496157	127647.338603	36.976756
1636.063574	127846.877833	36.981773
1637.616185	128051.913866	36.986791
1639.100122	128258.966180	36.991808
1641.121682	128449.112511	36.996826
1642.040898	128661.380376	37.001844
1643.729862	128872.298835	37.006861
1645.454751	129066.579492	37.011879
1646.861571	129270.210509	37.016896
1648.378011	129454.223129	37.021914
1650.023726	129648.290417	37.026932
1651.340247	129857.558947	37.031949
1653.021691	130052.650233	37.036967
1654.199946	130266.890529	37.041984
1655.913316	130474.488980	37.047002
1657.739698	130698.387558	37.052020
1659.717965	130888.437421	37.057037
1662.293460	131084.777273	37.062055
1663.785540	131294.050905	37.067072
1665.543515	131499.706101	37.072090
1667.715661	131702.696725	37.077108
1669.648857	131892.555031	37.082125
1671.178898	132091.130381	37.087143
1672.820526	132296.794789	37.092160
1674.676077	132485.969914	37.097178
1675.933475	132690.097234	37.102196
1677.549741	132898.280759	37.107213
1679.351358	133098.404507	37.112231
1681.187732	133313.559887	37.117248
1683.119590	133513.271906	37.122266
1684.571679	133724.390631	37.127284
1686.010622	133933.799410	37.132301
1688.012160	134128.783099	37.137319
1689.651605	134338.682833	37.142336
1691.254432	134535.608339	37.147354
1692.819411	134759.530381	37.152372
1695.049955	134966.663669	37.157389
1697.247684	135179.538565	37.162407
1698.385010	135381.780910	37.167424
1700.461432	135571.721593	37.172442
1701.769531	135789.940480	37.177460
1703.274445	136005.236585	37.182477
1704.997960	136206.820366	37.187495
1706.490658	136428.059086	37.192512
1708.886954	136642.965691	37.197530
1711.104423	136843.853624	37.202548
1712.569292	137050.557282	37.207565
1714.443160	137255.637368	37.212583
1715.850936	137459.712271	37.217600
1717.350990	137669.433432	37.222618
1718.932177	137883.812840	37.227636
1719.918016	138109.415086	37.232653
1722.168286	138332.512032	37.237671
1723.339594	138565.435210	37.242688
1724.939900	138791.275073	37.247706
1726.060385	139037.038358	37.252724
1727.421299	139262.562424	37.257741
1729.762679	139508.912274	37.262759
1731.339549	139748.961002	37.267776
1733.169587	139989.466478	37.272794
1735.062572	140229.620730	37.277812
1736.781264	140480.691946	37.282829
1738.838714	140714.604604	37.287847
1740.403715	140957.415178	37.292864
1742.392043	141192.927286	37.297882
1744.155985	141445.938228	37.302900
1745.608101	141679.112196	37.307917
1747.577876	141924.669364	37.312935
1748.739884	142159.705622	37.317952
1750.866169	142401.141601	37.322970
1753.322978	142627.716622	37.327988
1754.644811	142874.445491	37.333005
1756.370600	143106.949134	37.338023
1759.150047	143316.432587	37.343040
1761.670257	143527.277195	37.348058
1763.597354	143715.750968	37.353076
1765.142615	143920.390526	37.358093
1767.411529	144106.858080	37.363111
1768.393823	144308.172799	37.368128
1769.896231	144501.538495	37.373146
1771.159155	144709.309328	37.378164
1772.617216	144922.825444	37.383181
1773.984844	145139.504135	37.388199
1775.386906	145358.082192	37.393216
1776.990279	145583.445476	37.398234
1778.623578	145818.869923	37.403252
1780.211971	146060.013910	37.408269
1782.185443	146292.443025	37.413287
1783.552209	146536.872959	37.418304
1785.684999	146772.135213	37.423322
1786.921400	147023.682755	37.428340
1788.313649	147276.755744	37.433357
1789.664000	147533.834626	37.438375
1791.348753	147797.729413	37.443392
1793.476836	148066.747822	37.448410
1795.525934	148332.429035	37.453428
1797.144286	148611.023707	37.458445
1798.744805	148880.877267	37.463463
1800.425349	149152.496753	37.468480
1802.242228	149440.114925	37.473498
1804.051753	149706.233805	37.478516
1805.893953	149990.741212	37.483533
1807.714039	150275.507431	37.488551
1809.358422	150569.136987	37.493568
1810.871246	150861.430429	37.498586
1812.668400	151158.504670	37.503604
1814.073933	151454.448297	37.508621
1816.496164	151743.215782	37.513639
1818.557463	152056.209516	37.518656
1820.438153	152345.153296	37.523674
1822.323568	152653.163796	37.528692
1824.190188	152955.657133	37.533709
1826.404956	153249.263005	37.538727
1827.960386	153545.956100	37.543744
1830.141247	153835.838304	37.548762
1832.380970	154124.126078	37.553780
1834.328294	154415.151974	37.558797
1836.166006	154701.486878	37.563815
1838.059317	154997.055963	37.568832
1840.138841	155284.879453	37.573850
1841.801104	155561.039729	37.578868
1843.675317	155859.535906	37.583885
1845.546854	156140.985334	37.588903
1847.221057	156433.930006	37.593920
1849.294614	156730.876262	37.598938
1851.072013	157017.739757	37.603956
1852.574976	157314.066849	37.608973
1854.763713	157608.638362	37.613991
1856.220100	157910.142452	37.619008
1857.853105	158207.570886	37.624026
1859.970777	158503.275009	37.629044
1861.778883	158807.915294	37.634061
1863.591881	159100.216693	37.639079
1865.688729	159410.515160	37.644096
1867.326908	159702.948208	37.649114
1869.396821	159993.830101	37.654132
1871.671350	160296.767499	37.659149
1873.909642	160591.091822	37.664167
1875.868099	160881.893656	37.669184
1877.550275	161174.567995	37.674202
1879.997016	161449.655561	37.679220
1881.221062	161750.973400	37.684237
1883.459798	162022.198257	37.689255
1885.018055	162293.949135	37.694272
1886.864207	162564.437559	37.699290
1888.674383	162832.241195	37.704308
1890.305972	163107.627808	37.709325
1891.808848	163381.055049	37.714343
1893.610584	163665.837956	37.719360
1895.239163	163951.220375	37.724378
1897.124965	164236.284683	37.729396
1898.418780	164529.098159	37.734413
1900.223373	164830.746200	37.739431
1901.805463	165132.392143	37.744448
1903.991986	165433.869193	37.749466
1906.180877	165746.634345	37.754484
1907.747977	166052.463860	37.759501
1910.476994	166346.141076	37.764519
1912.409664	166645.707745	37.769536
1913.747642	166957.912562	37.774554
1916.091142	167258.700315	37.779572
1917.714045	167577.427772	37.784589
1919.772998	167881.449384	37.789607
1921.610178	168198.648091	37.794624
1923.536882	168514.704262	37.799642
1925.616577	168823.132531	37.804660
1927.720399	169158.907811	37.809677
1929.554947	169466.856425	37.814695
1931.724789	169781.636026	37.819712
1933.414183	170104.960805	37.824730
1935.517590	170411.093966	37.829748
1937.310892	170747.724840	37.834765
1939.211782	171069.548054	37.839783
1941.355334	171384.897296	37.844800
1943.194025	171712.903917	37.849818
1945.786847	172032.185666	37.854836
1947.546104	172350.760451	37.859853
1949.676634	172678.103651	37.864871
1952.079124	172998.269815	37.869888
1953.359175	173316.402587	37.874906
1955.552936	173639.181533	37.879924
1957.681042	173967.673371	37.884941
1959.440686	174292.617720	37.889959
1960.927553	174622.113634	37.894976
1962.776147	174947.554741	37.899994
1965.328013	175284.531846	37.905012
1967.034800	175630.708343	37.910029
1968.945762	175958.061239	37.915047
1971.284867	176290.212234	37.920064
1972.977520	176626.769895	37.925082
1974.893129	176955.319675	37.930100
1976.764970	177307.534642	37.935117
1978.430754	177662.526017	37.940135
1980.177262	178009.404683	37.945152
1981.719548	178361.421356	37.950170
1983.929963	178708.154466	37.955188
1985.567298	179077.429354	37.960205
1987.219318	179440.684339	37.965223
1989.026643	179797.389498	37.970240
1990.535969	180184.822775	37.975258
1992.673135	180560.375482	37.980276
1994.318526	180926.228131	37.985293
1996.848988	181301.290944	37.990311
1999.238221	181663.043313	37.995328
2001.607048	182051.417509	38.000346
2003.590993	182405.006859	38.005364
2005.755114	182772.309990	38.010381
2007.943117	183137.680550	38.015399
2009.897964	183499.075831	38.020416
2011.509771	183878.863653	38.025434
2013.188744	184234.488334	38.030452
2015.611156	184598.989778	38.035469
2017.839686	184939.698582	38.040487
2019.653398	185283.825774	38.045504
2021.433424	185640.074740	38.050522
2023.440273	185984.148863	38.055540
2025.110513	186338.893410	38.060557
2027.206331	186710.717489	38.065575
2028.928783	187044.908272	38.070592
2030.568180	187498.592310	38.075610
2032.881035	187877.498598	38.080628
2034.502057	188257.860078	38.085645
2036.470456	188637.229037	38.090663
2038.470274	189017.305616	38.095680
2039.917391	189409.077299	38.100698
2042.385304	189793.452472	38.105716
2044.351406	190197.896958	38.110733
2046.260524	190584.165179	38.115751
2048.381623	190977.208983	38.120768
2050.185488	191386.153328	38.125786
2052.420147	191801.001155	38.130804
2054.553289	192200.778279	38.135821
2057.058356	192601.540265	38.140839
2059.569997	192989.652972	38.145856
2061.363301	193401.374443	38.150874
2063.475075	193814.292344	38.155892
2065.452245	194211.331518	38.160909
2067.219885	194614.449976	38.165927
2069.283048	195043.509053	38.170944
2071.453272	195463.713232	38.175962
2073.263867	195880.850337	38.180980
2075.342055	196302.468520	38.185997
2077.637086	196724.232054	38.191015
2079.844087	197138.923532	38.196032
2081.645226	197569.961814	38.201050
2083.765819	197989.927339	38.206068
2085.606053	198421.927329	38.211085
2087.760402	198858.299606	38.216103
2090.157170	199300.300039	38.221120
2092.687021	199724.220232	38.226138
2094.756819	200154.868508	38.231156
2096.948811	200594.389675	38.236173
2099.000634	201017.016003	38.241191
2101.355171	201443.965493	38.246208
2103.022249	201884.740309	38.251226
2105.444167	202314.882210	38.256244
2107.812224	202743.052171	38.261261
2109.720586	203183.640327	38.266279
2112.005365	203604.763427	38.271296
2114.204543	204036.823941	38.276314
2116.598494	204469.185377	38.281332
2118.497655	204899.846606	38.286349
2120.306171	205342.436802	38.291367
2122.619776	205767.548430	38.296384
2125.114184	206196.290828	38.301402
2127.391635	206623.391282	38.306420
2129.540928	207050.588751	38.311437
2131.697089	207485.711744	38.316455
2134.135505	207902.222001	38.321472
2136.017506	208344.248160	38.326490
2138.231634	208769.050915	38.331508
2139.938191	209203.764470	38.336525
2142.000289	209639.693628	38.341543
2144.083284	210069.752123	38.346560
2145.876515	210510.170196	38.351578
2147.985264	210946.729384	38.356596
2150.197589	211385.813495	38.361613
2152.326500	211816.731350	38.366631
2154.666701	212255.187212	38.371648
2157.529062	212668.590757	38.376666
2159.962719	213059.884241	38.381684
2162.266051	213454.272327	38.386701
2164.821469	213839.908203	38.391719
2166.867905	214234.692843	38.396736
2168.985910	214630.330516	38.401754
2171.457001	215026.167707	38.406772
2173.561593	215418.912287	38.411789
2175.303821	215809.351104	38.416807
2177.761383	216211.237704	38.421824
2179.600128	216612.763723	38.426842
2181.450388	217017.235164	38.431860
2183.568201	217422.249609	38.436877
2185.362331	217837.044462	38.441895
2187.356156	218255.822394	38.446912
2189.347780	218676.887352	38.451930
2191.416415	219109.982112	38.456948
2193.757996	219535.464321	38.461965
2195.842551	219966.651902	38.466983
2197.825820	220398.998695	38.472000
2199.933163	220858.203883	38.477018
2202.083564	221293.599050	38.482036
2204.615204	221729.646413	38.487053
2206.922525	222186.814246	38.492071
2208.957174	222626.470494	38.497088
2211.136259	223081.677115	38.502106
2213.412807	223528.790213	38.507124
2215.928946	223976.704474	38.512141
2217.469794	224439.123923	38.517159
2219.758004	224896.371723	38.522176
2221.707683	225363.147987	38.527194
2223.943624	225839.431669	38.532212
2226.273082	226309.044927	38.537229
2228.466539	226787.824802	38.542247
2230.555865	227253.537724	38.547264
2232.663581	227738.732647	38.552282
2234.361841	228226.074320	38.557300
2236.451845	228725.599655	38.562317
2238.786174	229210.885921	38.567335
2241.232907	229714.445421	38.572352
2243.409433	230211.035219	38.577370
2245.587410	230705.211148	38.582388
2248.126510	231212.337441	38.587405
2250.515031	231720.579206	38.592423
2252.993039	232199.973164	38.597440
2255.115490	232701.218694	38.602458
2257.298722	233203.775350	38.607476
2259.505117	233703.304884	38.612493
2261.848131	234215.946486	38.617511
2264.203130	234720.685089	38.622528
2266.300619	235234.938843	38.627546
2268.514327	235746.455698	38.632564
2270.876313	236254.265301	38.637581
2272.950653	236782.111749	38.642599
2275.229070	237289.805970	38.647616
2277.507755	237809.566166	38.652634
2279.946445	238327.700245	38.657652
2282.513302	238840.428002	38.662669
2284.797175	239363.411185	38.667687
2287.291138	239872.414255	38.672704
2289.485323	240385.019572	38.677722
2291.734074	240893.220677	38.682740
2294.578379	241398.559185	38.687757
2296.683966	241911.632676	38.692775
2299.197994	242414.581884	38.697792
2300.971117	242926.993748	38.702810
2302.934229	243435.361253	38.707828
2305.878360	243932.600844	38.712845
2308.111850	244434.547884	38.717863
2310.526833	244917.032261	38.722880
2312.774862	245402.996332	38.727898
2314.836782	245875.804156	38.732916
2317.238731	246363.342396	38.737933
2319.384190	246851.732248	38.742951
2321.655728	247342.819340	38.747968
2324.233414	247832.943026	38.752986
2326.475667	248332.110120	38.758004
2328.919218	248814.631307	38.763021
2330.992309	249323.017670	38.768039
2333.306588	249809.392010	38.773056
2335.365421	250321.308572	38.778074
2337.796711	250825.138518	38.783092
2340.400656	251324.215257	38.788109
2342.845118	251833.857096	38.793127
2344.966504	252335.977789	38.798144
2347.217928	252850.218693	38.803162
2349.219270	253363.658511	38.808180
2351.927102	253882.016138	38.813197
2354.385393	254413.213148	38.818215
2356.526589	254929.216649	38.823232
2359.115026	255456.833291	38.828250
2361.238105	255981.497586	38.833268
2363.966254	256506.319699	38.838285
2366.258468	257045.482998	38.843303
2368.545717	257564.349470	38.848320
2371.036154	258093.164776	38.853338
2373.467967	258635.881219	38.858356
2375.930619	259179.733529	38.863373
2378.212296	259710.428712	38.868391
2380.888516	260235.345064	38.873408
2383.913298	260759.061838	38.878426
2386.004936	261297.450405	38.883444
2388.533798	261832.999807	38.888461
2390.659801	262373.308370	38.893479
2393.227162	262907.729077	38.898496
2395.791583	263442.909643	38.903514
2397.507157	263987.185729	38.908532
2399.940113	264526.191320	38.913549
2402.560896	265077.382006	38.918567
2404.743072	265632.498710	38.923584
2407.279008	266184.306283	38.928602
2409.579865	266736.325227	38.933620
2412.577126	267277.971641	38.938637
2414.930596	267840.897726	38.943655
2417.628779	268385.759386	38.948672
2419.827668	268930.340080	38.953690
2421.984000	269494.734858	38.958708
2424.395843	270041.155457	38.963725
2426.540469	270603.107122	38.968743
2429.135157	271161.835971	38.973760
2431.506666	271716.405489	38.978778
2434.104521	272272.841136	38.983796
2436.454342	272837.159614	38.988813
2438.875889	273399.202927	38.993831
2441.381075	273962.854949	38.998848
2444.096110	274519.842022	39.003866
2446.580377	275092.581790	39.008884
2448.923314	275641.568568	39.013901
2451.294893	276206.927783	39.018919
2453.777980	276777.040162	39.023936
2456.273767	277342.600651	39.028954
2458.276689	277898.278700	39.033972
2461.007800	278463.464389	39.038989
2463.083261	279036.087244	39.044007
2465.200640	279614.971902	39.049024
2467.967973	280184.126322	39.054042
2470.302993	280742.601734	39.059060
2472.662819	281286.162490	39.064077
2475.001876	281842.749778	39.069095
2476.891217	282392.241647	39.074112
2479.873366	282952.097772	39.079130
2481.674970	283510.914331	39.084148
2484.009904	284075.128495	39.089165
2486.214813	284653.527853	39.094183
2488.469491	285235.495083	39.099200
2490.989573	285815.816330	39.104218
2493.192059	286402.707984	39.109236
2496.320841	286982.467442	39.114253
2499.330064	287571.965712	39.119271
2501.401845	288156.348460	39.124288
2503.927712	288741.924923	39.129306
2506.329292	289325.001679	39.134324
2508.701257	289931.869454	39.139341
2511.384366	290543.532727	39.144359
2513.257057	291157.449023	39.149376
2515.819283	291772.851592	39.154394
2518.226414	292391.928391	39.159412
2520.413793	293018.396267	39.164429
2523.087509	293645.746816	39.169447
2525.903037	294277.105698	39.174464
2529.077410	294885.500911	39.179482
2532.133971	295500.103120	39.184500
2535.212350	296117.945248	39.189517
2537.716354	296742.166533	39.194535
2539.771506	297352.081170	39.199552
2542.789311	297975.269704	39.204570
2545.185322	298601.746983	39.209588
2547.652530	299219.295217	39.214605
2550.134942	299847.217549	39.219623
2552.888205	300483.569772	39.224640
2555.063823	301119.725231	39.229658
2557.161324	301761.444961	39.234676
2559.764239	302398.991249	39.239693
2562.341769	303044.936492	39.244711
2564.429431	303704.785049	39.249728
2567.335189	304357.136351	39.254746
2569.556972	305012.225905	39.259764
2572.015505	305680.749357	39.264781
2575.080535	306330.157085	39.269799
2578.598962	306973.013102	39.274816
2581.469426	307625.378947	39.279834
2583.636221	308275.586679	39.284852
2586.254555	308929.878357	39.289869
2588.972351	309586.328716	39.294887
2590.998296	310253.309884	39.299904
2593.883776	310908.980175	39.304922
2596.393248	311570.766138	39.309940
2599.058379	312228.026250	39.314957
2601.738654	312883.675880	39.319975
2604.628621	313549.791108	39.324992
2607.328849	314207.297175	39.330010
2609.554335	314869.029988	39.335028
2611.685685	315532.798221	39.340045
2614.691172	316206.496090	39.345063
2616.857965	316877.497420	39.350080
2620.008782	317544.072067	39.355098
2622.480622	318213.432407	39.360116
2625.154424	318881.888342	39.365133
2627.917592	319540.676982	39.370151
2630.732284	320210.029602	39.375168
2633.674575	320866.054949	39.380186
2636.208129	321533.705167	39.385204
2638.975620	322197.197725	39.390221
2642.155163	322838.311253	39.395239
2644.436572	323474.048503	39.400256
2647.227255	324099.217318	39.405274
2649.531827	324730.364434	39.410292
2651.834268	325356.300686	39.415309
2654.234264	325985.662910	39.420327
2656.745793	326620.833729	39.425344
2659.394616	327270.105485	39.430362
2661.525620	327915.895289	39.435380
2663.971413	328569.211683	39.440397
2667.061841	329214.374428	39.445415
2669.283118	329874.833408	39.450432
2672.428910	330535.137380	39.455450
2675.265271	331195.529038	39.460468
2677.681786	331858.384825	39.465485
2680.282643	332517.547394	39.470503
2682.664851	333208.417597	39.475520
2685.728845	333867.231037	39.480538
2688.423676	334543.264130	39.485556
2690.653525	335227.880670	39.490573
2693.664308	335916.244162	39.495591
2696.138706	336611.222736	39.500608
2698.679942	337301.764181	39.505626
2701.272425	338002.582790	39.510644
2703.894809	338700.897499	39.515661
2706.598409	339405.907518	39.520679
2709.396940	340123.139477	39.525696
2711.575841	340822.648599	39.530714
2714.486378	341544.907019	39.535732
2717.210259	342279.049057	39.540749
2719.809047	343005.104855	39.545767
2722.231914	343747.555993	39.550784
2725.034360	344480.878458	39.555802
2727.941359	345224.541136	39.560820
2730.524964	345963.952208	39.565837
2733.426119	346708.217315	39.570855
2735.999460	347457.918264	39.575872
2738.851998	348205.961446	39.580890
2741.598414	348961.712838	39.585908
2744.516819	349711.740354	39.590925
2747.793339	350462.734604	39.595943
2750.881545	351214.146566	39.600960
2753.865286	351955.212691	39.605978
2756.630243	352713.384473	39.610996
2759.046339	353460.031443	39.616013
2761.655140	354204.628064	39.621031
2764.140843	354970.902528	39.626048
2767.157164	355740.929228	39.631066
2770.157837	356507.669147	39.636084
2772.766915	357262.460385	39.641101
2775.856870	358016.473938	39.646119
2778.475593	358774.699602	39.651136
2781.165116	359540.576056	39.656154
2784.320518	360311.430299	39.661172
2786.744484	361063.951280	39.666189
2790.284041	361836.861254	39.671207
2792.592202	362605.203178	39.676224
2795.591565	363366.777222	39.681242
2798.362768	364130.293339	39.686260
2801.376087	364886.706325	39.691277
2804.655239	365652.790196	39.696295
2806.992444	366410.282593	39.701312
2809.775324	367169.028916	39.706330
2812.541959	367932.597934	39.711348
2815.128388	368698.429924	39.716365
2818.450330	369467.066269	39.721383
2820.877116	370234.883476	39.726400
2823.546021	370994.761766	39.731418
2826.696684	371750.617086	39.736436
2829.743025	372487.085168	39.741453
2832.616620	373205.672956	39.746471
2835.227333	373930.490207	39.751488
2837.915167	374651.222669	39.756506
2840.866926	375378.583342	39.761524
2843.599106	376100.157250	39.766541
2846.376824	376832.243404	39.771559
2849.150227	377573.050001	39.776576
2852.175180	378308.831918	39.781594
2854.959910	379048.861171	39.786612
2857.138302	379793.092961	39.791629
2860.024259	380537.320289	39.796647
2862.373710	381308.306659	39.801664
2865.375847	382059.817990	39.806682
2868.169396	382833.830784	39.811700
2870.804049	383602.957087	39.816717
2873.811291	384384.462747	39.821735
2876.491922	385167.666826	39.826752
2879.734050	385950.759440	39.831770
2882.480091	386738.691198	39.836788
2884.771976	387542.141197	39.841805
2887.721822	388325.256188	39.846823
2890.581968	389135.150317	39.851840
2893.585808	389940.640590	39.856858
2896.321480	390766.249982	39.861876
2899.229899	391582.284983	39.866893
2902.381557	392403.115923	39.871911
2905.179343	393223.670449	39.876928
2908.282856	394054.225381	39.881946
2911.361713	394868.250047	39.886964
2914.072412	395713.137173	39.891981
2917.355111	396539.730367	39.896999
2920.487956	397371.076853	39.902016
2923.507174	398209.347147	39.907034
2926.738665	399038.037696	39.912052
2929.622881	399884.419171	39.917069
2932.477590	400717.006440	39.922087
2935.418457	401563.115451	39.927104
2938.522639	402393.427019	39.932122
2942.122006	403217.760457	39.937140
2945.054361	404048.241178	39.942157
2948.042518	404879.188954	39.947175
2951.110564	405711.915614	39.952192
2954.314583	406554.913693	39.957210
2956.993030	407384.956892	39.962228
2959.678931	408224.481034	39.967245
2963.091576	409048.124008	39.972263
2966.477852	409889.044628	39.977280
2969.644334	410707.857149	39.982298
2972.728153	411531.508875	39.987316
2975.085906	412361.111070	39.992333
2978.279760	413201.023472	39.997351
2981.540594	414025.160048	40.002368
2984.434800	414853.419518	40.007386
2987.646253	415685.391343	40.012404
2990.318779	416523.990163	40.017421
2993.012325	417351.020394	40.022439
2996.034006	418192.128932	40.027456
2998.734324	419030.977923	40.032474
3001.900250	419876.396560	40.037492
3004.614315	420727.009509	40.042509
3007.344675	421575.511700	40.047527
3010.300333	422434.563122	40.052544
3012.987938	423282.799401	40.057562
3015.919983	424132.833332	40.062580
3018.720271	425005.958706	40.067597
3021.471198	425878.043013	40.072615
3024.527912	426733.459503	40.077632
3027.786890	427579.556651	40.082650
3030.693073	428404.542026	40.087668
3033.645445	429237.978543	40.092685
3036.594787	430069.763006	40.097703
3039.397573	430915.132183	40.102720
3042.496296	431750.562956	40.107738
3045.556477	432591.978599	40.112756
3048.116058	433438.590920	40.117773
3051.494516	434289.789467	40.122791
3054.252343	435148.273691	40.127808
3056.759881	436028.892015	40.132826
3059.987280	436902.890037	40.137844
3062.980251	437778.602539	40.142861
3066.094168	438647.030745	40.147879
3069.333301	439535.255418	40.152896
3072.070118	440427.659192	40.157914
3075.300161	441311.709303	40.162932
3078.566706	442202.784258	40.167949
3081.862142	443091.791559	40.172967
3085.250452	443993.218145	40.177984
3088.175290	444906.188920	40.183002
3091.185781	445803.444081	40.188020
3094.398425	446717.795196	40.193037
3097.562851	447626.199331	40.198055
3100.685452	448534.110069	40.203072
3103.979648	449448.159597	40.208090
3107.164206	450357.483893	40.213108
3110.243802	451288.338172	40.218125
3113.641186	452207.482140	40.223143
3116.562615	453137.810075	40.228160
3119.589182	454065.599120	40.233178
3122.759473	454985.795401	40.238196
3126.118312	455913.889665	40.243213
3129.356845	456841.196287	40.248231
3132.443940	457771.757841	40.253248
3135.687175	458712.490574	40.258266
3139.033296	459650.885062	40.263284
3141.684219	460594.837170	40.268301
3144.749980	461531.153968	40.273319
3147.751301	462488.723019	40.278336
3150.305434	463445.803152	40.283354
3153.991818	464406.336052	40.288372
3156.693836	465375.443003	40.293389
3160.176969	466333.475862	40.298407
3163.369915	467306.329585	40.303424
3166.556065	468281.599133	40.308442
3169.619918	469256.527704	40.313460
3172.389417	470234.571497	40.318477
3175.525800	471213.256505	40.323495
3178.822223	472204.818436	40.328512
3181.831512	473194.599825	40.333530
3184.728375	474175.564747	40.338548
3188.248914	475187.683962	40.343565
3191.295580	476176.924038	40.348583
3194.548812	477177.262805	40.353600
3197.438973	478177.292946	40.358618
3201.404946	479173.413061	40.363636
3204.818231	480174.748159	40.368653
3207.921838	481172.388606	40.373671
3211.883244	482165.951587	40.378688
3215.010470	483153.987467	40.383706
3218.478735	484140.647855	40.388724
3221.816444	485133.010102	40.393741
3225.151616	486111.453168	40.398759
3228.546595	487087.759106	40.403776
3231.391696	488071.292621	40.408794
3234.680710	489058.975668	40.413812
3237.662152	490030.825648	40.418829
3240.914802	490976.731874	40.423847
3244.335829	491933.733878	40.428864
3247.068107	492877.436114	40.433882
3250.480522	493814.527116	40.438900
3253.811958	494756.355785	40.443917
3256.940616	495696.998295	40.448935
3260.333329	496645.193242	40.453952
3263.341077	497598.371566	40.458970
3266.614872	498551.648160	40.463988
3271.264598	499472.783379	40.469005
3274.936270	500408.761463	40.474023
3278.436908	501339.169295	40.479040
3281.197442	502274.414050	40.484058
3284.702340	503224.379362	40.489076
3287.749399	504173.699086	40.494093
3290.506002	505126.674654	40.499111
3293.221934	506081.958000	40.504128
3296.272788	507048.345207	40.509146
3299.219887	508024.090857	40.514164
3302.545170	509009.671154	40.519181
3305.496698	509988.952829	40.524199
3308.704232	510992.873904	40.529216
3311.646653	512001.894454	40.534234
3315.086027	513011.971715	40.539252
3318.369138	514025.117784	40.544269
3321.640081	515045.332097	40.549287
3325.338514	516072.544390	40.554304
3328.325051	517104.365940	40.559322
3331.724442	518124.633370	40.564340
3335.442863	519158.398019	40.569357
3339.051666	520199.339419	40.574375
3342.545302	521236.800893	40.579392
3345.483448	522276.430144	40.584410
3349.040935	523317.792297	40.589428
3352.175466	524366.727127	40.594445
3355.774325	525420.431416	40.599463
3359.204234	526471.214652	40.604480
3362.189498	527532.885488	40.609498
3365.514350	528585.275401	40.614516
3369.141178	529659.283877	40.619533
3372.043011	530713.327035	40.624551
3376.590267	531765.723254	40.629568
3380.309014	532818.163205	40.634586
3384.187185	533874.660630	40.639604
3387.658506	534935.101490	40.644621
3390.884400	535983.694738	40.649639
3394.404450	537040.038112	40.654656
3397.594335	538086.958537	40.659674
3401.102161	539147.145028	40.664692
3404.433416	540209.127361	40.669709
3407.360625	541282.374940	40.674727
3410.895918	542332.403460	40.679744
3413.925744	543419.904603	40.684762
3416.937412	544493.366136	40.689780
3420.511135	545569.607606	40.694797
3423.967354	546648.683512	40.699815
3427.115448	547726.358921	40.704832
3430.584075	548814.823925	40.709850
3433.729206	549903.894739	40.714868
3437.435547	551002.760280	40.719885
3440.658271	552100.498925	40.724903
3444.109315	553180.304357	40.729920
3447.367770	554275.584404	40.734938
3450.847058	555380.104492	40.739956
3454.458564	556483.149191	40.744973
3457.645016	557598.387299	40.749991
3460.981187	558702.372691	40.755008
3464.836077	559799.029039	40.760013
3468.124059	560838.078656	40.765018
3471.508788	561842.565159	40.770023
3474.888572	562800.358633	40.775028
3478.125367	563678.647510	40.780032
3481.392344	564515.888792	40.785037
3484.244345	565294.886930	40.790042
3486.999512	566012.842385	40.795047
3489.444997	566683.556376	40.800052
3491.992038	567282.121551	40.805056
3494.027335	567835.251894	40.810061
3496.116717	568335.235367	40.815066
3498.237621	568784.441678	40.820071
3500.361453	569194.677420	40.825076
3502.380047	569559.739377	40.830080
3503.835590	569871.069757	40.835085
3505.081452	570134.892015	40.840090
3506.872676	570369.211108	40.845095
3507.907029	570566.502109	40.850100
3509.071561	570727.733080	40.855104
3509.966249	570865.766096	40.860109
3510.777629	570960.095879	40.865114
3511.817182	571039.684113	40.870119
3512.222072	571095.229958	40.875124
3513.311842	571116.290018	40.880128
3513.857369	571132.315531	40.885133
3514.917519	571110.519376	40.890138
3515.265228	571081.456344	40.895143
3515.514317	571030.576529	40.900148
3516.134536	570944.355882	40.905152
3516.075452	570873.598252	40.910157
3516.907041	570775.699506	40.915162
3517.191094	570666.240991	40.920167
3517.298451	570549.732028	40.925172
3517.604288	570416.778431	40.930176
3517.576371	570285.431180	40.935181
3517.909783	570139.219396	40.940186
3517.726798	569979.383352	40.945191
3518.343253	569821.277857	40.950196
3518.240039	569655.502004	40.955200
3518.821982	569482.639977	40.960205
3518.455160	569292.504898	40.965210
3518.904835	569093.555518	40.970215
3518.175174	568911.702940	40.975220
3518.545646	568714.064479	40.980224
3518.500504	568518.545493	40.985229
3518.496441	568314.181511	40.990234
3518.478953	568105.247669	40.995239
3518.314253	567906.222817	41.000244
3518.198248	567683.993069	41.005248
3518.451136	567486.753537	41.010253
3518.611844	567267.033134	41.015258
3518.638338	567055.663649	41.020263
3518.090054	566847.944442	41.025268
3518.148541	566616.228155	41.030272
3518.214547	566406.999640	41.035277
3517.831967	566191.661365	41.040282
3518.194389	565965.608712	41.045287
3517.712509	565751.633427	41.050292
3517.813781	565525.110739	41.055296
3517.372062	565316.343312	41.060301
3517.423239	565097.502770	41.065306
3517.567275	564870.107051	41.070311
3516.837590	564654.292201	41.075316
3517.184582	564440.766462	41.080320
3516.952727	564226.824718	41.085325
3516.712541	564013.834518	41.090330
3516.413763	563806.323539	41.095335
3516.397133	563592.186038	41.100340
3516.274123	563382.229589	41.105344
3516.135596	563177.997184	41.110349
3516.180421	562977.097671	41.115354
3516.399054	562752.361277	41.120359
3515.905763	562563.843432	41.125364
3515.806761	562351.253092	41.130368
3514.914751	562138.079131	41.135373
3515.310796	561943.385689	41.140378
3515.346800	561747.037278	41.145383
3515.100600	561549.574229	41.150388
3514.839999	561349.498129	41.155392
3514.827154	561164.449477	41.160397
3514.502405	560954.782487	41.165402
3514.600636	560771.870385	41.170407
3514.331455	560584.592057	41.175412
3514.220505	560392.413389	41.180416
3514.153037	560209.267200	41.185421
3513.549517	560017.812159	41.190426
3513.586582	559832.433486	41.195431
3513.171740	559650.236976	41.200436
3513.454727	559455.620640	41.205440
3513.023600	559305.121840	41.210445
3512.807252	559123.891145	41.215450
3513.070782	558952.480426	41.220455
3512.721111	558792.667932	41.225460
3512.548911	558620.013952	41.230464
3512.436406	558448.403277	41.235469
3512.386116	558280.649199	41.240474
3512.364432	558125.499597	41.245479
3511.892148	557968.307813	41.250484
3512.346041	557798.408454	41.255488
3512.256336	557636.178452	41.260493
3511.801908	557472.947815	41.265498
3511.732761	557321.965646	41.270503
3511.334927	557162.490524	41.275508
3510.803056	557008.410761	41.280512
3511.095280	556868.622373	41.285517
3510.836061	556727.762413	41.290522
3511.085074	556577.525340	41.295527
3510.576326	556429.565106	41.300532
3510.512376	556290.880679	41.305536
3510.550031	556147.957631	41.310541
3510.368599	556012.102401	41.315546
3510.600833	555871.859450	41.320551
3510.296785	555731.648061	41.325556
3510.382743	555602.078610	41.330560
3510.227124	555472.193569	41.335565
3510.173418	555333.094445	41.340570
3510.099305	555196.409197	41.345575
3509.730121	555061.678080	41.350580
3509.709865	554929.856353	41.355584
3509.668128	554807.836853	41.360589
3509.449080	554677.400266	41.365594
3509.539853	554548.673126	41.370599
3509.445631	554432.136236	41.375604
3509.111274	554310.659836	41.380608
3509.322826	554184.724585	41.385613
3509.276836	554060.738024	41.390618
3508.737875	553932.202825	41.395623
3508.719017	553817.658745	41.400628
3508.696337	553698.540271	41.405632
3508.814814	553586.837606	41.410637
3508.740682	553473.756501	41.415642
3508.335043	553361.329095	41.420647
3508.047494	553259.689141	41.425652
3508.019761	553145.441664	41.430656
3508.049518	553049.732103	41.435661
3508.090612	552931.350137	41.440666
3508.250410	552826.017789	41.445671
3507.678243	552726.378036	41.450676
3507.898141	552629.127566	41.455680
3507.970924	552521.544095	41.460685
3508.005570	552416.931418	41.465690
3507.856122	552317.473867	41.470695
3507.803938	552211.113535	41.475700
3507.823156	552111.175628	41.480704
3507.754100	552008.887962	41.485709
3507.835576	551907.480872	41.490714
3507.780153	551810.216423	41.495719
3507.350153	551715.975468	41.500724
3507.374465	551614.574833	41.505728
3507.673955	551518.710694	41.510733
3507.389085	551416.954353	41.515738
3507.688719	551322.546540	41.520743
3507.101108	551227.622515	41.525748
3507.364642	551134.727053	41.530752
3507.100663	551047.040886	41.535757
3506.935226	550956.875326	41.540762
3507.080565	550864.750312	41.545767
3506.896422	550772.726149	41.550772
3506.734745	550681.150273	41.555776
3506.658099	550598.408970	41.560781
3506.576992	550508.880560	41.565786
3506.648091	550416.009576	41.570791
3506.572706	550335.981217	41.575796
3506.639581	550248.941705	41.580800
3506.669280	550173.420853	41.585805
3506.566556	550093.093496	41.590810
3506.435792	550006.887457	41.595815
3506.311404	549931.489647	41.600820
3506.204388	549843.167073	41.605824
3506.060040	549771.039489	41.610829
3505.775863	549685.357848	41.615834
3505.821140	549611.842279	41.620839
3505.707785	549543.177819	41.625844
3505.886392	549475.272023	41.630848
3505.769824	549393.836071	41.635853
3505.918812	549331.062691	41.640858
3505.856788	549259.220969	41.645863
3505.681703	549185.737136	41.650868
3505.779125	549108.288493	41.655872
3505.603688	549035.507758	41.660877
3505.728023	548974.043720	41.665882
3505.728841	548895.200864	41.670887
3505.471448	548827.510181	41.675892
3505.443289	548761.241661	41.680896
3505.412846	548692.559540	41.685901
3505.529846	548629.184151	41.690906
3505.528820	548553.155269	41.695911
3505.162604	548493.675952	41.700916
3505.297117	548428.436292	41.705920
3505.552391	548359.908990	41.710925
3505.002731	548306.038909	41.715930
3505.326993	548239.159602	41.720935
3505.051074	548171.870472	41.725940
3505.333689	548103.639203	41.730944
3505.511774	548042.011287	41.735949
3505.106788	547978.914923	41.740954
3505.139732	547916.102093	41.745959
3504.891425	547865.150090	41.750964
3505.068389	547794.419215	41.755968
3505.486245	547730.590091	41.760973
3504.859289	547670.745072	41.765978
3505.157348	547609.146611	41.770983
3504.790636	547541.063561	41.775988
3504.419461	547475.796973	41.780992
3505.055098	547420.581940	41.785997
3504.652627	547376.893452	41.791002
3504.824279	547318.531689	41.796007
3504.547932	547259.082712	41.801012
3504.657065	547211.441760	41.806016
3504.695559	547151.490668	41.811021
3504.769728	547093.495039	41.816026
3504.811810	547040.331977	41.821031
3504.799656	546984.813483	41.826036
3504.272397	546927.162114	41.831040
3504.399769	546870.967620	41.836045
3504.225765	546824.123596	41.841050
3504.397339	546760.679825	41.846055
3504.512950	546726.262574	41.851060
3504.453360	546670.498595	41.856064
3504.896142	546626.625629	41.861069
3504.371718	546565.049372	41.866074
3504.416181	546506.250940	41.871079
3504.498665	546460.421764	41.876084
3504.772358	546400.430433	41.881088
3504.585892	546349.714017	41.886093
3504.222149	546302.746666	41.891098
3504.167160	546249.997660	41.896103
3504.297225	546205.870109	41.901108
3504.241498	546153.724329	41.906112
3504.438843	546105.059519	41.911117
3504.176635	546052.241329	41.916122
3504.554648	546000.027407	41.921127
3504.183199	545944.912221	41.926132
3503.960258	545896.462879	41.931136
3503.872919	545857.799747	41.936141
3503.795641	545816.469293	41.941146
3504.330589	545761.916378	41.946151
3504.425435	545717.541095	41.951156
3504.208595	545668.234889	41.956160
3504.247987	545617.832402	41.961165
3504.336733	545574.312586	41.966170
3504.440822	545520.177729	41.971175
3503.815313	545477.523164	41.976180
3503.980304	545435.097516	41.981184
3504.090317	545395.295710	41.986189
3504.072996	545336.149270	41.991194
3504.232637	545282.608298	41.996199
3504.154637	545238.358795	42.001204
3503.792830	545194.505382	42.006208
3504.141046	545145.159467	42.011213
3503.676655	545104.892840	42.016218
3503.792707	545060.863998	42.021223
3503.739463	545017.716416	42.026228
3503.398643	544972.903287	42.031232
3503.599562	544937.160042	42.036237
3503.170319	544902.520730	42.041242
3503.975666	544851.694153	42.046247
3503.399944	544822.912088	42.051252
3503.390842	544786.597505	42.056256
3503.507421	544756.349477	42.061261
3503.299802	544717.399719	42.066266
3503.797701	544679.346044	42.071271
3503.128055	544649.924299	42.076276
3503.103577	544605.966017	42.081280
3503.542829	544570.888833	42.086285
3503.429636	544543.794648	42.091290
3503.382273	544495.865825	42.096295
3503.525191	544460.935046	42.101300
3503.330011	544425.905880	42.106304
3503.735677	544382.081076	42.111309
3503.298501	544357.199837	42.116314
3503.204316	544313.905284	42.121319
3503.441831	544280.015602	42.126324
3503.538864	544240.866042	42.131328
3503.542814	544210.734821	42.136333
3503.492503	544175.682408	42.141338
3503.481720	544130.513079	42.146343
3503.298779	544105.038453	42.151348
3503.859311	544064.759875	42.156352
3503.161434	544028.097544	42.161357
3503.148187	543987.857703	42.166362
3503.004260	543947.185344	42.171367
3503.059037	543917.498228	42.176372
3503.127870	543886.752495	42.181376
3503.465233	543847.765517	42.186381
3503.358194	543827.560325	42.191386
3503.534630	543777.078761	42.196391
3503.262160	543746.536704	42.201396
3503.507104	543698.659939	42.206400
3503.675300	543668.149725	42.211405
3502.980773	543630.026894	42.216410
3503.217254	543590.350558	42.221415
3502.868251	543570.635339	42.226420
3503.087616	543539.010157	42.231424
3503.635160	543503.762217	42.236429
3503.151142	543471.340840	42.241434
3503.408468	543431.861976	42.246439
3503.097367	543408.770191	42.251444
3503.138785	543375.260705	42.256448
3503.495233	543345.223458	42.261453
3503.142466	543313.837653	42.266458
3503.657832	543264.407992	42.271463
3503.221806	543236.355100	42.276468
3503.472547	543203.064107	42.281472
3503.398235	543157.549009	42.286477
3503.274329	543134.427588	42.291482
3503.292481	543087.237752	42.296487
3503.055649	543052.613663	42.301492
3503.325842	543021.432021	42.306496
3502.984158	542984.459663	42.311501
3503.262646	542963.740324	42.316506
3503.149289	542917.777672	42.321511
3503.503857	542884.519984	42.326516
3503.360579	542846.912663	42.331520
3503.494425	542825.762842	42.336525
3503.412943	542791.969078	42.341530
3503.141833	542738.635152	42.346535
3502.587216	542712.159068	42.351540
3502.881168	542690.179183	42.356544
3503.112105	542655.481205	42.361549
3502.750950	542629.528226	42.366554
3503.157142	542596.865438	42.371559
3503.200092	542575.125643	42.376564
3503.038985	542543.506848	42.381568
3503.503187	542510.885117	42.386573
3503.141844	542476.580661	42.391578
3503.221426	542440.044226	42.396583
3503.148547	542409.115684	42.401588
3502.818629	542370.429184	42.406592
3503.148511	542342.909119	42.411597
3503.031321	542321.193804	42.416602
3503.147535	542272.476370	42.421607
3503.120318	542254.067352	42.426612
3502.954683	542231.504161	42.431616
3503.099815	542184.291169	42.436621
3502.823072	542164.914656	42.441626
3502.782003	542127.088032	42.446631
3502.634645	542104.622389	42.451636
3502.517996	542067.863857	42.456640
3503.170569	542045.072388	42.461645
3502.987338	542021.052560	42.466650
3503.530622	541993.448213	42.471655
3502.975616	541959.021546	42.476660
3502.855335	541928.652613	42.481664
3502.786476	541896.665659	42.486669
3503.101412	541865.876673	42.491674
3503.011851	541832.534382	42.496679
3503.199747	541815.852135	42.501684
3503.044294	541772.055216	42.506688
3503.137674	541741.954451	42.511693
3503.207912	541717.995224	42.516698
3502.943095	541674.768411	42.521703
3503.172400	541651.186798	42.526708
3503.077090	541615.379547	42.531712
3503.075169	541583.029195	42.536717
3503.067957	541563.006066	42.541722
3503.103194	541534.876028	42.546727
3503.133411	541500.206098	42.551732
3503.073069	541465.147664	42.556736
3503.417888	541437.422047	42.561741
3502.992491	541411.677795	42.566746
3502.749770	541370.509321	42.571751
3503.041965	541337.206937	42.576756
3503.101882	541310.330383	42.581760
3503.208258	541270.817907	42.586765
3503.107639	541240.393939	42.591770
3503.229860	541209.331459	42.596775
3502.872631	541170.293318	42.601780
3503.263144	541150.660466	42.606784
3502.767226	541121.102744	42.611789
3502.509475	541103.885137	42.616794
3502.962582	541068.141932	42.621799
3503.262228	541030.409935	42.626804
3503.069236	540997.987186	42.631808
3503.224890	540970.742809	42.636813
3502.898236	540947.347024	42.641818
3503.196288	540909.313026	42.646823
3503.169315	540892.159846	42.651828
3502.713833	540853.286957	42.656832
3502.979433	540806.855095	42.661837
3502.621549	540791.816195	42.666842
3502.778446	540768.193884	42.671847
3502.742179	540732.978721	42.676852
3502.723069	540711.446627	42.681856
3502.612256	540685.702252	42.686861
3502.639464	540657.923717	42.691866
3502.998330	540628.282139	42.696871
3502.738706	540603.466439	42.701876
3502.924812	540577.273110	42.706880
3503.057873	540536.747862	42.711885
3502.914579	540512.266094	42.716890
3503.031674	540484.473189	42.721895
3503.015020	540454.537424	42.726900
3502.998265	540424.802871	42.731904
3502.899191	540392.162683	42.736909
3502.680458	540364.975260	42.741914
3502.962921	540336.300909	42.746919
3502.903977	540315.025922	42.751924
3502.451857	540288.629410	42.756928
3502.907962	540262.594684	42.761933
3503.145525	540238.204070	42.766938
3502.882981	540211.375356	42.771943
3503.070444	540174.614296	42.776948
3502.880310	540150.441021	42.781952
3503.024293	540126.467297	42.786957
3503.000143	540088.833196	42.791962
3502.932671	540056.690403	42.796967
3502.898496	540025.146167	42.801972
3502.682842	539995.290600	42.806977
3503.228246	539959.077035	42.811981
3502.859015	539930.956045	42.816986
3502.872403	539902.020671	42.821991
3502.804866	539878.733537	42.826996
3503.031259	539851.375104	42.832001
3502.944362	539819.687603	42.837005
3502.762988	539793.700795	42.842010
3502.929749	539752.966515	42.847015
3502.854173	539726.560552	42.852020
3502.924060	539698.068794	42.857025
3502.868849	539670.200276	42.862029
3502.465124	539649.984217	42.867034
3502.647692	539634.356637	42.872039
3502.570788	539598.389840	42.877044
3502.480260	539575.709566	42.882049
3502.723035	539559.217083	42.887053
3502.360118	539538.541615	42.892058
3502.704098	539509.000376	42.897063
3502.705813	539478.103356	42.902068
3502.029642	539464.370412	42.907073
3502.661301	539437.149304	42.912077
3502.439079	539412.577047	42.917082
3502.421822	539381.229858	42.922087
3502.376172	539362.165318	42.927092
3502.451415	539345.648306	42.932097
3502.585043	539320.567608	42.937101
3502.840228	539297.581434	42.942106
3502.890841	539271.859382	42.947111
3502.838929	539245.247448	42.952116
3502.440315	539225.281521	42.957121
3502.959689	539191.384605	42.962125
3502.549721	539167.948164	42.967130
3502.783491	539141.543165	42.972135
3502.706899	539111.060011	42.977140
3502.210981	539091.109015	42.982145
3502.228850	539061.063939	42.987149
3502.485986	539061.225182	42.992154
3502.700914	539019.273321	42.997159
3502.922520	539008.469833	43.002164
3502.291434	538988.338418	43.007169
3502.587652	538961.822684	43.012173
3502.412936	538944.337597	43.017178
3502.619834	538907.972422	43.022183
3502.500351	538897.825791	43.027188
3502.337346	538863.027731	43.032193
3502.562551	538850.260956	43.037197
3502.314199	538822.974183	43.042202
3502.285022	538811.102446	43.047207
3502.385975	538785.925130	43.052212
3502.210916	538769.999876	43.057217
3502.765717	538734.183945	43.062221
3502.226937	538717.057138	43.067226
3502.222830	538689.077865	43.072231
3502.733481	538673.498697	43.077236
3502.542989	538654.405309	43.082241
3502.915683	538616.302494	43.087245
3502.397899	538606.922144	43.092250
3502.667902	538579.604510	43.097255
3502.709990	538553.479739	43.102260
3502.738620	538531.584242	43.107265
3502.795701	538498.160012	43.112269
3502.633689	538477.954792	43.117274
3502.790266	538442.753579	43.122279
3502.562147	538418.633235	43.127284
3502.822250	538397.154409	43.132289
3502.922574	538373.234493	43.137293
3502.514570	538343.253992	43.142298
3502.688243	538323.600189	43.147303
3502.486237	538295.248245	43.152308
3502.474588	538272.754669	43.157313
3502.453322	538243.317654	43.162317
3502.563071	538227.599026	43.167322
3502.737824	538197.930102	43.172327
3502.399872	538173.574757	43.177332
3502.225217	538164.694265	43.182337
3502.529659	538139.182051	43.187341
3502.388835	538120.231109	43.192346
3502.040217	538084.050676	43.197351
3502.525652	538077.885660	43.202356
3502.308325	538052.253162	43.207361
3502.675844	538027.989063	43.212365
3503.016663	538008.258438	43.217370
3502.547948	537977.531627	43.222375
3502.851123	537951.063033	43.227380
3502.758934	537923.850682	43.232385
3502.779951	537890.128509	43.237389
3502.612669	537866.500918	43.242394
3502.667865	537836.849758	43.247399
3502.800058	537806.783931	43.252404
3502.423358	537793.606492	43.257409
3502.699898	537768.047551	43.262413
3502.911249	537753.319073	43.267418
3502.561791	537717.942967	43.272423
3502.694667	537704.837122	43.277428
3502.435906	537688.772556	43.282433
3502.414463	537654.452436	43.287437
3502.399821	537640.564238	43.292442
3502.396027	537618.068283	43.297447
3502.643835	537588.889852	43.302452
3502.471670	537564.557871	43.307457
3502.835591	537547.490325	43.312461
3502.493914	537525.348754	43.317466
3502.364746	537496.178445	43.322471
3502.583480	537480.643251	43.327476
3502.150489	537449.154680	43.332481
3502.400179	537428.430771	43.337485
3502.655415	537410.574698	43.342490
3502.494152	537390.619278	43.347495
3502.610964	537359.900519	43.352500
3502.755419	537339.343828	43.357505
3502.932607	537306.552060	43.362509
3502.614594	537289.439299	43.367514
3502.609532	537258.135311	43.372519
3502.627924	537228.790441	43.377524
3502.368853	537212.473675	43.382529
3502.431820	537187.349443	43.387533
3502.379651	537170.849439	43.392538
3502.133485	537146.175867	43.397543
3502.454716	537113.260529	43.402548
3502.514371	537103.487228	43.407553
3502.765621	537079.642061	43.412557
3502.160443	537057.440021	43.417562
3502.165141	537029.304744	43.422567
3502.575272	537013.185568	43.427572
3502.421913	536995.744810	43.432577
3502.752938	536964.186482	43.437581
3502.491382	536940.622176	43.442586
3502.695222	536921.716479	43.447591
3502.885938	536896.773119	43.452596
3502.787416	536875.246880	43.457601
3502.702947	536839.575448	43.462605
3502.406140	536820.193868	43.467610
3502.224460	536788.714890	43.472615
3502.308575	536776.269986	43.477620
3502.349155	536755.778853	43.482625
3502.617649	536731.477374	43.487629
3502.841593	536702.904611	43.492634
3502.622631	536675.306674	43.497639
3502.508838	536659.016924	43.502644
3502.337840	536630.606121	43.507649
3502.912740	536597.347993	43.512653
3502.779622	536581.312811	43.517658
3502.799969	536552.419072	43.522663
3502.693836	536526.917201	43.527668
3502.339230	536500.094975	43.532673
3502.658449	536468.587596	43.537677
3502.919611	536455.460509	43.542682
3502.888420	536431.909750	43.547687
3502.516771	536402.523015	43.552692
3502.474076	536378.420289	43.557697
3502.458569	536352.299976	43.562701
3502.207874	536341.920062	43.567706
3502.491908	536318.823370	43.572711
3502.773174	536293.411749	43.577716
3502.280416	536270.637182	43.582721
3502.580116	536243.259601	43.587725
3502.653423	536222.762523	43.592730
3502.666941	536196.184375	43.597735
3502.351388	536173.281391	43.602740
3502.325225	536157.128367	43.607745
3502.147096	536126.402210	43.612749
3502.147660	536121.368721	43.617754
3502.114380	536096.760663	43.622759
3502.062868	536081.567831	43.627764
3502.158671	536064.942706	43.632769
3502.113409	536040.739077	43.637773
3502.289491	536023.245727	43.642778
3502.270276	536003.668710	43.647783
3502.008243	535978.441678	43.652788
3502.207133	535959.837339	43.657793
3502.489826	535949.021764	43.662797
3502.650786	535920.759067	43.667802
3502.416529	535903.681750	43.672807
3502.604711	535876.824087	43.677812
3502.320937	535856.683998	43.682817
3502.599031	535832.379323	43.687821
3502.251089	535807.064652	43.692826
3502.193593	535781.151049	43.697831
3502.281710	535765.936115	43.702836
3502.158074	535743.153502	43.707841
3502.517926	535740.329037	43.712845
3502.235403	535722.050944	43.717850
3502.321757	535694.655059	43.722855
3502.568275	535672.418745	43.727860
3502.003916	535653.228037	43.732865
3502.389828	535620.097460	43.737869
3502.319688	535621.215727	43.742874
3502.224095	535584.233804	43.747879
3502.330296	535575.609819	43.752884
3502.142056	535550.269790	43.757889
3502.100336	535525.963966	43.762893
3502.425941	535506.986902	43.767898
3502.620300	535492.208136	43.772903
3502.529784	535459.906328	43.777908
3502.514504	535441.183557	43.782913
3502.173931	535415.967640	43.787917
3502.554365	535397.283901	43.792922
3502.206717	535373.126068	43.797927
3502.141007	535352.296876	43.802932
3502.431117	535333.627100	43.807937
3502.328527	535315.874133	43.812941
3502.479160	535302.159027	43.817946
3502.154035	535276.588074	43.822951
3502.403313	535242.722733	43.827956
3502.265992	535237.710354	43.832961
3502.185119	535212.302612	43.837965
3502.259114	535204.388112	43.842970
3502.251420	535173.985514	43.847975
3502.427939	535151.255819	43.852980
3502.163290	535133.880181	43.857985
3502.482995	535099.651142	43.862989
3502.676155	535095.996736	43.867994
3502.316375	535080.397649	43.872999
3502.555491	535049.402635	43.878004
3502.528071	535035.765291	43.883009
3502.409059	535000.245132	43.888013
3502.350725	534985.605783	43.893018
3502.368733	534958.772686	43.898023
3502.244872	534944.294501	43.903028
3502.545337	534921.494775	43.908033
3502.436143	534889.899179	43.913037
3502.120561	534876.658877	43.918042
3502.235245	534858.921807	43.923047
3502.517341	534834.463610	43.928052
3501.778439	534817.060665	43.933057
3501.986509	534794.929497	43.938061
3502.105054	534796.521863	43.943066
3502.158020	534772.199880	43.948071
3502.188289	534754.878515	43.953076
3502.436914	534745.879439	43.958081
3502.687300	534720.268161	43.963085
3502.724449	534687.441154	43.968090
3502.338204	534671.543653	43.973095
3502.623322	534651.514504	43.978100
3502.505847	534633.863590	43.983105
3502.524048	534597.918253	43.988109
3502.609473	534585.471024	43.993114
3502.844604	534551.102670	43.998119
3502.708886	534528.923865	44.003124
3502.204702	534505.443177	44.008129
3502.526858	534467.184875	44.013133
3502.676501	534462.429579	44.018138
3502.388508	534435.894711	44.023143
3502.706176	534413.594814	44.028148
3502.328657	534395.077912	44.033153
3502.382103	534367.180919	44.038157
3502.260843	534350.990083	44.043162
3502.188966	534313.698774	44.048167
3502.388451	534285.174788	44.053172
3502.157578	534283.146705	44.058177
3502.256277	534255.494133	44.063181
3502.114913	534243.736298	44.068186
3501.755353	534218.974056	44.073191
3502.346833	534217.120042	44.078196
3501.862563	534195.699678	44.083201
3502.226079	534176.815442	44.088205
3502.276588	534153.046429	44.093210
3502.196756	534136.899219	44.098215
3501.908177	534126.372380	44.103220
3502.004233	534104.005752	44.108225
3502.294302	534086.290670	44.113229
3502.341504	534065.643193	44.118234
3502.216587	534050.660751	44.123239
3502.647603	534028.543919	44.128244
3502.198819	534011.195418	44.133249
3502.466365	533987.039932	44.138253
3502.289817	533967.987722	44.143258
3502.602341	533949.866222	44.148263
3502.371980	533929.362404	44.153268
3502.210267	533912.925602	44.158273
3502.213852	533883.525052	44.163277
3502.385756	533856.061603	44.168282
3502.099929	533840.902586	44.173287
3502.079885	533815.130226	44.178292
3502.117228	533801.984925	44.183297
3502.813808	533781.034573	44.188301
3502.629272	533756.143520	44.193306
3502.413184	533741.124563	44.198311
3502.332505	533717.073105	44.203316
3501.911724	533696.950951	44.208321
3502.222493	533680.591359	44.213325
3502.261674	533676.859829	44.218330
3501.898456	533645.451742	44.223335
3501.933559	533628.933608	44.228340
3501.739507	533620.455727	44.233345
3502.038797	533593.022240	44.238349
3502.057327	533590.451801	44.243354
3502.089518	533570.158275	44.248359
3502.404492	533545.390461	44.253364
3502.251230	533532.123516	44.258369
3502.341337	533512.928451	44.263373
3502.034063	533496.161362	44.268378
3502.025154	533475.169267	44.273383
3502.368322	533462.076719	44.278388
3502.015308	533439.929855	44.283393
3502.019070	533425.883203	44.288397
3502.168217	533409.900829	44.293402
3502.284765	533383.200156	44.298407
3502.431126	533365.808517	44.303412
3502.120252	533358.858978	44.308417
3502.218591	533344.143041	44.313421
3501.964610	533312.415079	44.318426
3502.067245	533301.323242	44.323431
3502.189130	533274.420134	44.328436
3501.759513	533266.733850	44.333441
3501.860562	533237.870459	44.338445
3501.763244	533234.009008	44.343450
3501.448176	533223.233828	44.348455
3502.190854	533215.667161	44.353460
3501.597695	533200.857287	44.358465
3501.955564	533166.214428	44.363469
3501.998756	533157.951052	44.368474
3502.148767	533154.202125	44.373479
3502.041128	533131.714477	44.378484
3501.829556	533132.099786	44.383489
3501.963582	533105.345474	44.388493
3502.102425	533096.009919	44.393498
3501.979094	533085.708243	44.398503
3501.999429	533062.948834	44.403508
3501.751356	533055.183827	44.408513
3502.222379	533035.072903	44.413517
3502.114413	533021.093544	44.418522
3501.830669	533006.134605	44.423527
3502.047290	532979.115451	44.428532
3501.773237	532968.333676	44.433537
3502.018908	532956.514442	44.438541
3502.047835	532930.531315	44.443546
3501.893399	532915.250073	44.448551
3502.053161	532905.961471	44.453556
3502.247042	532884.282361	44.458561
3501.522779	532872.513290	44.463565
3501.905888	532870.288747	44.468570
3501.865664	532849.099124	44.473575
3501.657088	532830.402646	44.478580
3501.580160	532830.263545	44.483585
3502.005452	532805.628192	44.488589
3501.871239	532792.659603	44.493594
3501.911057	532791.142974	44.498599
3502.019541	532774.461291	44.503604
3501.929415	532752.725462	44.508609
3502.391854	532749.783697	44.513613
3502.180820	532721.169108	44.518618
3501.989538	532715.006162	44.523623
3502.577350	532687.324475	44.528628
3502.437724	532672.090988	44.533633
3502.151925	532649.026061	44.538637
3502.034863	532634.040755	44.543642
3501.949570	532618.345624	44.548647
3502.323844	532589.287231	44.553652
3502.205389	532586.687562	44.558657
3502.035295	532563.453434	44.563661
3502.121944	532560.771496	44.568666
3501.998976	532527.057666	44.573671
3502.326234	532509.133253	44.578676
3501.873811	532505.175799	44.583681
3502.194819	532472.701782	44.588685
3502.206779	532459.710114	44.593690
3502.028445	532444.230643	44.598695
3501.991594	532424.147458	44.603700
3501.676384	532419.765841	44.608705
3502.032155	532391.062321	44.613709
3501.862263	532380.515588	44.618714
3502.171093	532381.122026	44.623719
3501.977798	532358.042186	44.628724
3501.689162	532354.613030	44.633729
3502.059735	532335.573973	44.638733
3502.130568	532319.149307	44.643738
3501.943105	532307.094792	44.648743
3502.185756	532277.754094	44.653748
3501.700088	532265.242458	44.658753
3502.073790	532253.906150	44.663757
3502.026392	532231.357218	44.668762
3502.091468	532224.701006	44.673767
3502.146719	532210.645025	44.678772
3501.783881	532194.186988	44.683777
3502.017393	532180.506027	44.688781
3502.077746	532160.608705	44.693786
3501.750596	532134.729745	44.698791
3501.890361	532133.147136	44.703796
3501.874405	532115.779083	44.708801
3502.011360	532102.364812	44.713805
3501.962081	532092.302570	44.718810
3502.162541	532079.281189	44.723815
3502.188909	532061.906477	44.728820
3501.775153	532056.533080	44.733825
3501.882102	532029.831116	44.738829
3502.181057	532012.665669	44.743834
3501.563709	531983.407783	44.748839
3501.843254	531968.410341	44.753844
3501.899503	531967.193158	44.758849
3501.799088	531969.524847	44.763853
3501.764530	531939.622325	44.768858
3501.840666	531924.807535	44.773863
3501.794996	531918.873301	44.778868
3501.670751	531920.000305	44.783873
3501.949013	531891.861597	44.788877
3501.863695	531886.688771	44.793882
3501.756116	531864.954171	44.798887
3502.082409	531845.468136	44.803892
3502.057264	531843.860805	44.808897
3501.856745	531822.140596	44.813901
3501.793554	531814.597826	44.818906
3501.644262	531802.990058	44.823911
3502.140098	531792.591004	44.828916
3501.907146	531777.270288	44.833921
3502.016075	531761.443197	44.838925
3502.139983	531736.600968	44.843930
3501.575868	531725.661892	44.848935
3502.126169	531715.405354	44.853940
3502.144357	531701.304240	44.858945
3501.774647	531680.264684	44.863949
3501.843055	531667.817302	44.868954
3501.814579	531651.054789	44.873959
3501.924447	531644.693417	44.878964
3501.850827	531638.813756	44.883969
3501.659933	531617.041356	44.888973
3501.862666	531602.961769	44.893978
3501.607419	531593.837515	44.898983
3501.687885	531580.834309	44.903988
3501.566377	531565.143541	44.908993
3501.350662	531553.747292	44.913997
3501.799841	531552.015763	44.919002
3502.000283	531545.136733	44.924007
3501.984184	531523.689437	44.929012
3501.687696	531512.406424	44.934017
3501.797648	531498.895031	44.939021
3501.830956	531485.093440	44.944026
3501.633810	531477.571320	44.949031
3501.421594	531459.175543	44.954036
3501.538979	531465.702984	44.959041
3501.681606	531457.523757	44.964045
3501.946754	531429.436444	44.969050
3501.887482	531421.036853	44.974055
3502.091507	531415.718110	44.979060
3501.887313	531390.875926	44.984065
3501.643017	531386.029752	44.989069
3501.939605	531373.596934	44.994074
3501.933651	531358.038991	44.999079
3501.910739	531340.620634	45.004084
3501.988485	531340.910617	45.009089
3501.925162	531311.816766	45.014093
3502.129338	531311.432494	45.019098
3501.934987	531293.084055	45.024103
3501.980152	531268.656007	45.029108
3501.975305	531263.973937	45.034113
3501.942207	531244.240815	45.039117
3501.868176	531227.837315	45.044122
3501.679739	531226.456728	45.049127
3501.772096	531203.632504	45.054132
3501.579483	531181.809290	45.059137
3501.868946	531167.917149	45.064141
3501.990620	531164.121709	45.069146
3501.741961	531154.039413	45.074151
3501.995319	531130.334005	45.079156
3501.763912	531123.270189	45.084161
3501.755634	531106.252066	45.089165
3502.199688	531092.084023	45.094170
3501.975530	531086.227538	45.099175
3502.014578	531071.417550	45.104180
3501.742944	531068.891766	45.109185
3501.865785	531053.162357	45.114189
3501.811549	531034.691043	45.119194
3501.812459	531025.476175	45.124199
3501.990338	531007.875067	45.129204
3501.872698	530996.664482	45.134209
3501.556282	530978.989192	45.139213
3501.918001	530970.674860	45.144218
3501.752052	530977.548759	45.149223
3501.558190	530940.770272	45.154228
3502.003491	530946.793762	45.159233
3501.804256	530935.595822	45.164237
3501.569209	530915.742566	45.169242
3501.669411	530899.915788	45.174247
3501.588198	530881.297393	45.179252
3501.666304	530894.830450	45.184257
3501.403783	530887.167099	45.189261
3501.763691	530856.294333	45.194266
3501.578201	530846.403386	45.199271
3501.738709	530839.983389	45.204276
3502.021619	530833.091152	45.209281
3501.661880	530815.674153	45.214285
3501.740247	530808.612316	45.219290
3501.552113	530806.627385	45.224295
3502.051179	530788.019266	45.229300
3501.892985	530776.764449	45.234305
3501.942202	530765.175219	45.239309
3501.641722	530744.425503	45.244314
3501.964935	530730.225519	45.249319
3501.942811	530717.338126	45.254324
3501.828116	530708.090669	45.259329
3501.696121	530685.451515	45.264333
3501.833084	530680.747168	45.269338
3501.644848	530681.582105	45.274343
3501.939029	530656.509904	45.279348
3501.594502	530646.190359	45.284353
3501.704378	530645.921453	45.289357
3501.498129	530631.300203	45.294362
3501.478036	530621.332992	45.299367
3501.717061	530604.477152	45.304372
3501.449052	530597.318035	45.309377
3501.580871	530588.938527	45.314381
3501.951570	530572.263576	45.319386
3501.871329	530563.917050	45.324391
3501.697611	530555.786487	45.329396
3501.738059	530555.629094	45.334401
3501.877490	530535.515566	45.339405
3502.062779	530519.675087	45.344410
3501.531541	530516.283193	45.349415
3501.928948	530498.546527	45.354420
3501.708687	530476.172523	45.359425
3501.690339	530468.823418	45.364429
3501.700034	530462.980617	45.369434
3501.574490	530454.490004	45.374439
3501.808875	530430.333078	45.379444
3501.896323	530419.946132	45.384449
3501.747510	530409.998791	45.389453
3501.817347	530385.968101	45.394458
3501.909046	530390.636906	45.399463
3501.929986	530379.756718	45.404468
3502.000879	530364.084921	45.409473
3501.710568	530346.555779	45.414477
3501.962733	530334.833874	45.419482
3501.796879	530314.465374	45.424487
3501.996263	530314.937878	45.429492
3501.739567	530299.115555	45.434497
3502.275034	530273.149015	45.439501
3502.163167	530266.972548	45.444506
3501.996297	530252.999379	45.449511
3501.911099	530233.625333	45.454516
3501.814160	530226.389035	45.459521
3502.078133	530204.140639	45.464525
3501.860784	530182.923883	45.469530
3501.871047	530193.396461	45.474535
3501.926971	530169.266824	45.479540
3501.833758	530159.814208	45.484545
3501.915206	530144.845502	45.489549
3501.677023	530116.430838	45.494554
3501.783191	530106.997515	45.499559
3501.939572	530095.743515	45.504564
3502.158207	530077.782314	45.509569
3501.739251	530070.596040	45.514573
3502.066659	530060.221826	45.519578
3502.099582	530043.699480	45.524583
3502.011379	530026.843460	45.529588
3501.835723	530022.590384	45.534593
3502.062643	529982.822992	45.539597
3501.918345	529975.191064	45.544602
3501.832457	529966.794678	45.549607
3501.698659	529946.017755	45.554612
3501.709126	529935.138827	45.559617
3501.939734	529929.009622	45.564621
3502.028491	529916.003470	45.569626
3501.620226	529907.506138	45.574631
3502.039096	529898.326152	45.579636
3501.901471	529874.729670	45.584641
3501.898070	529854.939470	45.589645
3502.084281	529844.234552	45.594650
3501.871991	529825.987556	45.599655
3502.123461	529808.675534	45.604660
3501.744428	529813.266723	45.609665
3501.793581	529786.972032	45.614669
3501.880711	529767.620838	45.619674
3501.802853	529766.726470	45.624679
3501.482536	529754.237040	45.629684
3501.589016	529734.580635	45.634689
3501.601361	529737.398758	45.639693
3501.552937	529743.952864	45.644698
3501.519132	529743.958092	45.649703
3501.479222	529717.777839	45.654708
3501.605294	529704.312443	45.659713
3501.717178	529688.683818	45.664717
3501.892747	529687.044987	45.669722
3501.457975	529676.587640	45.674727
3501.300773	529661.605160	45.679732
3501.444089	529647.683793	45.684737
3501.373020	529640.191351	45.689741
3501.695634	529643.766954	45.694746
3501.701476	529648.247950	45.699751
3501.520117	529624.859258	45.704756
3501.703140	529610.931674	45.709761
3501.797729	529598.478248	45.714765
3501.698279	529604.990005	45.719770
3501.774610	529586.294890	45.724775
3501.989494	529565.362386	45.729780
3501.675068	529551.562507	45.734785
3501.507912	529547.761185	45.739789
3501.781963	529527.171928	45.744794
3501.625690	529523.419265	45.749799
3501.995590	529517.066756	45.754804
3501.801426	529493.981979	45.759809
3501.940554	529487.564648	45.764813
3501.933916	529454.177287	45.769818
3502.049004	529392.871589	45.774823
3501.795263	529278.644116	45.779828
3501.359443	529127.177013	45.784833
3501.089502	528918.824185	45.789837
3500.507183	528663.326976	45.794842
3500.729549	528376.121571	45.799847
3500.191310	528029.849475	45.804852
3499.925249	527646.204401	45.809857
3499.160181	527208.228313	45.814861
3498.619184	526723.509916	45.819866
3498.109650	526204.667085	45.824871
3497.749118	525628.656582	45.829876
3496.820295	525011.249748	45.834881
3495.675304	524352.386078	45.839885
3495.339680	523641.067857	45.844890
3494.042500	522895.700834	45.849895
3493.233687	522100.282524	45.854900
3492.251286	521269.873204	45.859905
3490.884744	520390.187478	45.864909
3489.952931	519476.963611	45.869914
3488.833509	518531.501510	45.874919
3487.725107	517520.396047	45.879924
3486.222478	516473.235291	45.884929
3485.355629	515397.009536	45.889933
3483.840118	514269.224841	45.894938
3482.438086	513116.069903	45.899943
3480.855539	511906.926226	45.904948
3479.470151	510655.992470	45.909953
3477.591569	509382.025989	45.914957
3476.222555	508060.906631	45.919962
3474.341904	506721.382210	45.924967
3472.910261	505338.024025	45.929972
3471.188521	503912.852299	45.934977
3469.237254	502451.244961	45.939981
3467.522470	500969.519939	45.944986
3465.730148	499443.142451	45.949991
3464.047012	497885.143213	45.954996
3461.629570	496304.024054	45.960001
3460.023603	494675.557537	45.965005
3458.075779	493012.026561	45.970010
3455.920913	491317.742341	45.975015
3453.672992	489604.647067	45.980020
3451.199099	487858.563606	45.985025
3449.127115	486089.487089	45.990029
3447.102924	484281.602955	45.995034
3444.630285	482448.668848	46.000039
3441.948820	480598.219986	46.005044
3440.153616	478707.693227	46.010049
3437.654168	476805.678589	46.015053
3435.366727	474872.266175	46.020058
3433.065938	472908.947744	46.025063
3430.344884	470912.288936	46.030068
3427.512907	468895.126366	46.035073
3425.262783	466863.061754	46.040077
3422.633622	464804.203171	46.045082
3419.543149	462736.615330	46.050087
3417.305406	460630.394671	46.055092
3414.720537	458511.218180	46.060097
3411.793778	456369.518255	46.065101
3409.101196	454208.742284	46.070106
3406.317598	452026.051224	46.075111
3403.501939	449813.431853	46.080116
3400.909506	447587.037929	46.085121
3397.591607	445354.509096	46.090125
3394.908977	443082.918861	46.095130
3392.007547	440813.921096	46.100135
3389.261542	438514.130356	46.105140
3386.159002	436198.563316	46.110145
3383.095545	433871.259911	46.115149
3379.983910	431522.756743	46.120154
3376.741128	429169.026494	46.125159
3373.703810	426782.952088	46.130164
3370.887509	424393.569379	46.135169
3367.523366	421990.100342	46.140173
3364.903109	419562.911662	46.145178
3361.562470	417140.674565	46.150183
3358.254663	414687.827191	46.155188
3354.908008	412225.676726	46.160193
3351.869553	409738.393734	46.165197
3348.606247	407254.618930	46.170202
3345.038531	404768.737819	46.175207
3342.089436	402245.343081	46.180212
3338.600485	399727.845035	46.185217
3335.082926	397200.639123	46.190221
3331.888872	394657.732560	46.195226
3328.219225	392115.189195	46.200231
3325.259724	389548.966506	46.205236
3321.741559	386988.886602	46.210241
3318.077646	384399.750794	46.215245
3314.697151	381813.152995	46.220250
3311.266758	379220.210940	46.225255
3307.855258	376616.700336	46.230260
3304.116874	374005.648189	46.235265
3300.382693	371392.517686	46.240269
3297.168822	368764.758395	46.245274
3293.478285	366146.688579	46.250279
3290.340953	363510.026342	46.255284
3286.620749	360872.406199	46.260289
3282.982718	358231.009627	46.265293
3279.349249	355566.764500	46.270298
3275.559405	352920.084975	46.275303
3271.562653	350257.864700	46.280308
3267.963561	347599.611432	46.285313
3264.231746	344936.031595	46.290317
3260.800507	342271.866851	46.295322
3256.842639	339600.791612	46.300327
3253.162838	336939.289951	46.305332
3249.611378	334269.640167	46.310337
3245.510008	331594.417878	46.315341
3242.112770	328914.728718	46.320346
3238.280499	326245.431322	46.325351
3234.891433	323567.240031	46.330356
3231.077488	320883.523947	46.335361
3226.866481	318194.460547	46.340365
3223.490294	315509.454313	46.345370
3219.448859	312822.357395	46.350375
3215.530414	310143.891910	46.355380
3211.759348	307460.979846	46.360385
3207.579071	304772.719314	46.365389
3204.301004	302101.612386	46.370394
3200.041547	299427.623226	46.375399
3196.262877	296747.805046	46.380404
3192.611093	294079.220459	46.385409
3188.782888	291391.808843	46.390413
3184.885123	288722.697213	46.395418
3180.470226	286063.917547	46.400423
3176.629761	283383.482429	46.405428
3172.927037	280733.476136	46.410433
3168.940360	278072.496972	46.415437
3165.053399	275418.719057	46.420442
3161.067368	272766.526019	46.425447
3157.155800	270120.657144	46.430452
3153.137154	267474.983581	46.435457
3148.677340	264846.393783	46.440461
3144.865416	262196.170146	46.445466
3140.619326	259577.783353	46.450471
3136.841586	256958.070049	46.455476
3132.835907	254336.506248	46.460481
3128.700110	251739.490276	46.465485
3124.774254	249144.232420	46.470490
3120.636378	246552.763719	46.475495
3116.367595	243975.263179	46.480500
3112.465161	241393.117197	46.485505
3108.190715	238832.702799	46.490509
3104.607604	236259.196266	46.495514
3100.153130	233718.128315	46.500519
3095.908773	231172.328796	46.505524
3092.043754	228631.504525	46.510529
3087.506479	226115.001407	46.515533
3083.564821	223585.212066	46.520538
3079.231476	221098.351398	46.525543
3075.468097	218605.041841	46.530548
3071.540182	216108.559684	46.535553
3066.760738	213647.855322	46.540557
3062.803789	211179.502237	46.545562
3058.458000	208737.157966	46.550567
3054.077914	206296.677537	46.555572
3049.837118	203868.555542	46.560577
3045.449235	201455.539121	46.565581
3041.207345	199052.772251	46.570586
3036.944910	196673.959257	46.575591
3033.066142	194303.377782	46.580596
3028.820386	191942.191550	46.585601
3024.088336	189604.580361	46.590605
3019.467755	187275.785383	46.595610
3015.308695	184963.037345	46.600615
3010.888008	182663.089571	46.605620
3006.340384	180391.964657	46.610625
3001.331415	178141.643934	46.615629
2996.990819	175905.969385	46.620634
2992.105691	173707.867667	46.625639
2987.204447	171510.135516	46.630644
2982.615800	169344.306438	46.635649
2977.860667	167222.942013	46.640653
2973.443335	165096.065193	46.645658
2968.386108	163006.267484	46.650663
2963.485239	160946.792431	46.655668
2958.250812	158923.290173	46.660673
2953.232269	156917.168442	46.665677
2948.231188	154944.290409	46.670682
2942.641164	152941.601129	46.675687
2936.738978	151051.388338	46.680692
2931.138907	149210.479422	46.685697
2924.912989	147405.043252	46.690701
2918.379533	145667.297552	46.695706
2912.185339	143993.267986	46.700711
2904.821098	142372.025549	46.705716
2897.855544	140821.783497	46.710721
2890.668945	139328.128270	46.715725
2884.126189	137901.951197	46.720730
2877.418393	136542.901979	46.725735
2871.021177	135238.701104	46.730740
2865.242840	134009.930557	46.735745
2859.163721	132818.895186	46.740749
2853.962705	131677.620819	46.745754
2848.395915	130595.367144	46.750759
2843.191687	129549.807362	46.755764
2838.311591	128549.937939	46.760769
2833.780444	127596.489741	46.765773
2828.880243	126661.678237	46.770778
2824.319222	125768.451622	46.775783
2820.097450	124907.064820	46.780788
2815.825733	124059.719858	46.785793
2811.319750	123245.674540	46.790797
2807.444603	122452.112585	46.795802
2803.472121	121673.486838	46.800807
2799.340608	120923.693543	46.805812
2795.785342	120184.393012	46.810817
2791.415955	119463.138776	46.815821
2787.605769	118751.679254	46.820826
2783.642279	118056.737421	46.825831
2780.049755	117381.270048	46.830836
2776.568570	116717.890415	46.835841
2772.279491	116064.592036	46.840845
2768.393539	115406.397800	46.845850
2764.645586	114774.756171	46.850855
2760.663734	114157.491765	46.855860
2756.908384	113551.378970	46.860865
2752.931612	112949.481185	46.865869
2749.103409	112355.580456	46.870874
2745.223900	111785.384258	46.875879
2741.387001	111211.795877	46.880884
2737.775479	110639.389508	46.885889
2734.127939	110093.111912	46.890893
2730.102764	109542.934963	46.895898
2726.388711	108998.795198	46.900903
2722.963157	108478.977322	46.905908
2719.595432	107949.610849	46.910913
2715.606085	107417.870252	46.915917
2712.145394	106897.484163	46.920922
2708.399159	106384.536285	46.925927
2705.406428	105870.131387	46.930932
2701.853910	105349.617978	46.935937
2698.287479	104842.296834	46.940941
2695.000117	104322.469886	46.945946
2691.829233	103824.305741	46.950951
2688.345771	103300.826201	46.955956
2684.988356	102804.193563	46.960961
2681.458353	102288.058787	46.965965
2678.195596	101776.936610	46.970970
2674.806782	101265.295471	46.975975
2671.698349	100747.136530	46.980980
2667.997193	100230.743090	46.985985
2664.487984	99723.161305	46.990989
2661.397775	99201.897651	46.995994
2657.692682	98690.308292	47.000999
2654.557127	98166.170805	47.006004
2651.454329	97649.573248	47.011009
2648.102292	97120.924173	47.016013
2644.670412	96598.371044	47.021018
2641.263692	96080.334130	47.026023
2637.787700	95541.182991	47.031028
2634.072052	95003.870275	47.036033
2630.812716	94484.083241	47.041037
2627.583829	93946.929118	47.046042
2624.128897	93424.343890	47.051047
2620.746955	92880.942124	47.056052
2617.473746	92344.216860	47.061057
2613.555811	91805.060078	47.066061
2610.312267	91250.064800	47.071066
2606.936243	90710.957538	47.076071
2603.777179	90166.959830	47.081076
2600.319755	89625.928020	47.086081
2596.686483	89074.680130	47.091085
2593.284782	88518.832571	47.096090
2589.660652	87975.620649	47.101095
2586.437424	87416.424670	47.106100
2583.189249	86867.305146	47.111105
2579.881979	86315.816740	47.116109
2576.351418	85757.005228	47.121114
2572.520440	85201.909906	47.126119
2569.072482	84635.294410	47.131124
2565.984570	84072.686371	47.136129
2562.129754	83511.872813	47.141133
2558.868540	82937.601936	47.146138
2555.223544	82385.377650	47.151143
2551.735686	81808.065507	47.156148
2548.348715	81242.638512	47.161153
2544.862670	80684.529095	47.166157
2541.138723	80118.897772	47.171162
2537.949134	79555.747713	47.176167
2534.360221	78978.103257	47.181172
2531.249295	78416.259613	47.186177
2527.333856	77849.243860	47.191181
2524.059958	77269.465252	47.196186
2520.667937	76692.155701	47.201191
2516.969819	76114.893331	47.206196
2513.710029	75536.774982	47.211201
2509.763288	74969.316131	47.216205
2506.813689	74391.123283	47.221210
2503.089722	73815.780898	47.226215
2499.433147	73235.970647	47.231220
2496.463127	72659.037516	47.236225
2492.692514	72071.537392	47.241229
2489.562921	71488.572444	47.246234
2485.985446	70909.892869	47.251239
2482.397718	70327.126598	47.256244
2479.120584	69733.736087	47.261249
2475.798949	69156.579174	47.266253
2472.421311	68557.930509	47.271258
2468.918592	67973.134451	47.276263
2465.310677	67373.279603	47.281268
2461.944683	66779.494807	47.286273
2458.318082	66195.596516	47.291277
2454.870282	65595.200006	47.296282
2451.823167	64999.972699	47.301287
2447.988335	64396.123239	47.306292
2444.547120	63801.601261	47.311297
2440.534246	63207.994743	47.316301
2437.166602	62597.604323	47.321306
2433.117995	62002.915137	47.326311
2429.534673	61415.573840	47.331316
2426.676818	60814.388120	47.336321
2423.369098	60221.720795	47.341325
2420.245556	59620.802404	47.346330
2416.427201	59022.183481	47.351335
2412.798875	58420.548356	47.356340
2409.802400	57810.466810	47.361345
2406.210572	57209.395509	47.366349
2402.970149	56596.070560	47.371354
2399.058423	55994.965270	47.376359
2395.388082	55384.815527	47.381364
2392.282345	54773.108981	47.386369
2388.717142	54167.611970	47.391373
2385.423622	53554.868608	47.396378
2381.936037	52937.070875	47.401383
2378.321776	52322.557167	47.406388
2375.118484	51703.618584	47.411393
2371.536925	51097.251933	47.416397
2368.148921	50469.012076	47.421402
2364.071940	49861.701932	47.426407
2360.984368	49230.791302	47.431412
2357.401857	48624.286882	47.436417
2353.751350	48016.470858	47.441421
2350.351440	47394.501128	47.446426
2347.068535	46779.272058	47.451431
2343.411345	46155.759113	47.456436
2340.178140	45528.525482	47.461441
2336.672604	44915.861632	47.466445
2333.321366	44283.030749	47.471450
2329.651369	43658.809267	47.476455
2325.806864	43028.272268	47.481460
2322.733461	42404.164474	47.486465
2319.308592	41790.369484	47.491469
2315.939505	41152.704036	47.496474
2312.373613	40522.113017	47.501479
2308.788605	39899.550976	47.506484
2305.268031	39263.130911	47.511489
2301.597376	38633.561959	47.516493
2298.147773	38009.790491	47.521498
2295.210881	37373.246501	47.526503
2291.563271	36730.505315	47.531508
2288.030475	36105.337765	47.536513
2284.427172	35470.925591	47.541517
2280.816567	34837.826620	47.546522
2277.556428	34206.916894	47.551527
2273.651547	33568.894243	47.556532
2270.379215	32931.863675	47.561537
2266.668888	32290.750214	47.566541
2263.609467	31657.192231	47.571546
2260.069912	31024.539470	47.576551
2256.516470	30375.164631	47.581556
2252.847019	29733.040030	47.586561
2249.207437	29098.497235	47.591565
2245.934250	28457.573834	47.596570
2242.421329	27826.516956	47.601575
2238.654374	27194.517973	47.606580
2235.447752	26552.579534	47.611585
2231.595661	25920.424373	47.616589
2228.546689	25281.479671	47.621594
2224.650546	24647.166399	47.626599
2221.273342	24005.474956	47.631604
2217.811187	23365.274425	47.636609
2214.161026	22723.413241	47.641613
2210.533587	22087.815414	47.646618
2206.837482	21453.654957	47.651623
2203.083445	20819.403526	47.656628
2199.807043	20189.209121	47.661633
2196.681008	19562.957655	47.666637
2192.505493	18935.983824	47.671642
2188.870690	18297.792481	47.676647
2184.817855	17671.004974	47.681652
2181.971056	17035.227874	47.686657
2178.053932	16419.761409	47.691661
2174.737611	15793.654815	47.696666
2170.865025	15169.995102	47.701671
2167.407217	14559.003448	47.706676
2164.041738	13936.748838	47.711681
2160.282449	13322.148921	47.716685
2156.472049	12709.875308	47.721690
2152.977604	12093.450483	47.726695
2149.178642	11500.186891	47.731700
2145.665418	10886.954340	47.736705
2141.992320	10285.238437	47.741709
2138.264115	9686.478456	47.746714
2134.228489	9091.197725	47.751719
2129.827955	8525.194833	47.756724
2124.610169	7992.427457	47.761729
2117.631310	7514.650365	47.766733
2111.650155	7052.976003	47.771738
2105.714481	6626.281002	47.776743
2100.486169	6225.418128	47.781748
2095.797849	5840.778320	47.786753
2090.614845	5500.943439	47.791757
2086.074238	5172.065728	47.796762
2081.574608	4862.326801	47.801767
2077.860121	4570.185847	47.806772
2073.884754	4301.181226	47.811777
2070.077005	4040.426283	47.816781
2066.354019	3789.531565	47.821786
2063.195502	3538.495522	47.826791
2059.496238	3313.146171	47.831796
2056.214920	3071.558974	47.836801
2052.481743	2848.929297	47.841805
2049.377974	2611.788488	47.846810
2046.237437	2392.005409	47.851815
2042.575919	2173.182552	47.856820
2039.564790	1962.753445	47.861825
2035.785410	1737.923568	47.866829
2032.562901	1518.027902	47.871834
2029.129430	1308.507500	47.876839
2025.807421	1096.940987	47.881844
2022.612411	884.268849	47.886849
2019.116267	687.468384	47.891853
2015.171352	485.013482	47.896858
2011.557672	288.090191	47.901863
2006.886106	120.465258	47.906868
1996.339026	120.657723	47.911873
1987.900138	125.928885	47.916877
1981.875282	130.390914	47.921882
1978.335296	137.361021	47.926887
1975.811265	135.210180	47.931892
1974.173176	127.707641	47.936897
1971.626440	129.957910	47.941901
1968.975403	124.935195	47.946906
1966.463282	130.780393	47.951911
1963.059923	130.275504	47.956916
1959.681765	135.730311	47.961921
1956.244127	129.143754	47.966925
1952.553052	133.233077	47.971930
1949.702641	124.599949	47.976935
1946.209304	142.768704	47.981940
1943.279689	126.564456	47.986945
1939.949323	125.339535	47.991949
1936.130301	128.025096	47.996954
1932.641144	128.764251	48.001959
1929.032035	124.210186	48.006964
1926.544824	125.752010	48.011969
1923.379787	119.746287	48.016973
1919.434880	125.175405	48.021978
1915.510170	126.267083	48.026983
1911.999975	130.834452	48.031988
1908.747822	120.830691	48.036993
1905.354401	133.902950	48.041997
1902.103944	126.771583	48.047002
1899.354369	120.293082	48.052007
1895.587729	127.839459	48.057012
1891.804432	119.522373	48.062017
1888.469287	135.113374	48.067021
1885.277704	131.443447	48.072026
1882.092595	130.063047	48.077031
1878.362970	132.975143	48.082036
1875.235199	125.264707	48.087041
1871.198519	126.171337	48.092045
1868.140169	121.702403	48.097050
1864.382922	116.342510	48.102055
1860.984831	122.025043	48.107060
1857.589924	115.393889	48.112065
1854.220022	121.575066	48.117069
1850.439702	125.668792	48.122074
1847.095567	116.875245	48.127079
1843.814016	119.252538	48.132084
1840.634842	114.185489	48.137089
1836.798820	112.976003	48.142093
1833.228671	119.435115	48.147098
1829.736974	117.874650	48.152103
1826.161101	122.616756	48.157108
1822.959450	120.663141	48.162113
1819.662525	119.951876	48.167117
1815.882818	122.340264	48.172122
1812.725974	109.787555	48.177127
1809.032522	117.635746	48.182132
1805.617994	116.480884	48.187137
1802.523213	125.396987	48.192141
1798.922684	118.984503	48.197146
1795.141506	119.446418	48.202151
1791.555491	119.716609	48.207156
1788.133718	115.032169	48.212161
1784.525903	123.689602	48.217165
1781.092984	119.911719	48.222170
1777.934418	117.480009	48.227175
1774.237564	117.799090	48.232180
1770.997323	112.045537	48.237185
1767.355194	119.888906	48.242189
1763.825274	111.383716	48.247194
1760.627933	112.669080	48.252199
1756.876013	126.037567	48.257204
1753.241658	124.445529	48.262209
1749.803557	120.823478	48.267213
1746.314102	117.576413	48.272218
1743.235153	115.606872	48.277223
1739.727071	116.548300	48.282228
1736.771085	119.991720	48.287233
1732.794286	118.876920	48.292237
1728.948196	123.189694	48.297242
1725.279587	117.604056	48.302247
1721.601777	124.497540	48.307252
1718.461540	123.088026	48.312257
1714.845262	126.450720	48.317261
1711.458493	116.951994	48.322266
1708.299784	114.760756	48.327271
1704.503239	125.478668	48.332276
1701.651244	117.719011	48.337281
1697.784988	125.053109	48.342285
1694.132967	119.806574	48.347290
1690.341537	118.220008	48.352295
1686.594149	122.033374	48.357300
1683.606338	127.111063	48.362305
1680.393794	119.784006	48.367309
1676.660939	124.708739	48.372314
1673.668667	117.388529	48.377319
1669.901123	125.384299	48.382324
1666.240073	119.300789	48.387329
1662.566074	120.233247	48.392333
1658.960954	122.670403	48.397338
1656.037835	116.256910	48.402343
1652.058266	109.520636	48.407348
1648.766817	106.733141	48.412353
1645.278351	116.140778	48.417357
1641.626991	119.198892	48.422362
1638.345613	106.108788	48.427367
1634.898320	115.174663	48.432372
1631.443367	109.435566	48.437377
1628.006195	110.587427	48.442381
1624.037392	115.798816	48.447386
1620.910264	111.002102	48.452391
1617.147278	107.481256	48.457396
1614.208896	115.063236	48.462401
1610.388236	115.249743	48.467405
1606.620990	124.520444	48.472410
1603.172978	108.868363	48.477415
1599.631697	114.424496	48.482420
1596.175762	106.211536	48.487425
1592.224521	105.598969	48.492429
1588.930874	119.481408	48.497434
1586.097157	109.453709	48.502439
1582.817180	116.490917	48.507444
1579.316166	109.161322	48.512449
1575.511867	109.013098	48.517453
1571.652729	111.572052	48.522458
1568.639718	106.877804	48.527463
1564.898169	116.375453	48.532468
1561.468197	113.979681	48.537473
1557.618670	108.637360	48.542477
1554.305516	105.628631	48.547482
1550.855001	102.780486	48.552487
1547.054452	110.003118	48.557492
1543.728686	108.375729	48.562497
1540.646247	100.844957	48.567501
1536.572179	107.047155	48.572506
1533.318767	103.984838	48.577511
1529.492309	109.262661	48.582516
1526.534372	101.880188	48.587521
1523.225294	101.221463	48.592525
1519.336916	106.353901	48.597530
1516.143957	109.014813	48.602535
1512.535273	109.443580	48.607540
1509.153780	104.234062	48.612545
1505.284737	108.794025	48.617549
1501.541322	101.008637	48.622554
1498.157512	105.546859	48.627559
1494.941118	107.809629	48.632564
1491.432066	107.887538	48.637569
1487.752723	96.371664	48.642573
1484.318135	110.959390	48.647578
1481.280681	108.062779	48.652583
1477.442076	112.371239	48.657588
1474.034548	105.992042	48.662593
1470.452006	111.304670	48.667597
1466.569872	106.808985	48.672602
1463.440760	102.990186	48.677607
1459.881849	111.915250	48.682612
1456.146694	108.260382	48.687617
1452.917249	107.291880	48.692621
1449.591699	112.162718	48.697626
1446.350978	93.811419	48.702631
1442.256713	106.157513	48.707636
1438.763709	101.838545	48.712641
1435.492314	96.836526	48.717645
1432.030451	100.820597	48.722650
1428.598961	108.915919	48.727655
1424.600425	107.469187	48.732660
1421.706365	110.017145	48.737665
1417.903307	107.176431	48.742669
1414.060721	109.302559	48.747674
1410.888190	102.431223	48.752679
1407.322134	100.711539	48.757684
1403.988711	98.639276	48.762689
1400.602550	99.441536	48.767693
1396.552950	95.057351	48.772698
1393.102655	91.892822	48.777703
1389.539213	104.121493	48.782708
1386.539761	100.092701	48.787713
1383.311737	104.951525	48.792717
1379.384193	113.022822	48.797722
1375.811700	95.934878	48.802727
1371.925000	110.630935	48.807732
1368.665371	98.904226	48.812737
1365.482490	102.493707	48.817741
1362.099935	92.181329	48.822746
1358.717279	88.224843	48.827751
1354.824444	99.014679	48.832756
1351.304614	93.086413	48.837761
1347.713795	100.260588	48.842765
1344.054943	99.093184	48.847770
1341.328267	92.721932	48.852775
1337.665696	95.772319	48.857780
1334.121631	95.333683	48.862785
1330.437588	99.741477	48.867789
1326.326952	93.813427	48.872794
1323.203595	97.874527	48.877799
1319.582520	95.369329	48.882804
1316.535845	93.802928	48.887809
1313.091621	96.297321	48.892813
1309.287103	94.814079	48.897818
1306.216353	95.981698	48.902823
1302.279206	103.361640	48.907828
1298.989609	93.844711	48.912833
1295.126275	90.178183	48.917837
1291.532114	106.011925	48.922842
1288.669710	97.320666	48.927847
1284.885961	102.224866	48.932852
1281.377042	94.143597	48.937857
1277.937673	105.799309	48.942861
1274.260287	95.472727	48.947866
1271.048845	102.632147	48.952871
1267.141595	99.447011	48.957876
1263.671868	92.517560	48.962881
1260.173191	97.893070	48.967885
1256.451614	100.259800	48.972890
1253.411541	92.985067	48.977895
1249.768090	96.747481	48.982900
1246.755449	93.024476	48.987905
1243.341569	91.524731	48.992909
1239.394086	98.722788	48.997914
1235.907136	95.709515	49.002919
1231.987524	104.371192	49.007924
1228.758341	94.015984	49.012929
1225.607134	103.734952	49.017933
1222.086671	103.976013	49.022938
1218.476957	94.420342	49.027943
1214.508760	93.997118	49.032948
1211.122556	97.298722	49.037953
1207.773320	94.466493	49.042957
1204.081246	101.830439	49.047962
1200.907374	98.578616	49.052967
1197.392286	98.410726	49.057972
1193.837988	96.597491	49.062977
1190.358739	97.854014	49.067981
1186.464290	99.763612	49.072986
1183.510407	89.039703	49.077991
1179.746822	100.638313	49.082996
1176.350983	97.642502	49.088001
1173.012964	91.198756	49.093005
1169.033565	99.442641	49.098010
1165.672301	85.849403	49.103015
1162.361127	92.448554	49.108020
1159.226830	92.392236	49.113025
1155.378578	91.466304	49.118029
1151.400274	93.901477	49.123034
1148.414677	91.167675	49.128039
1144.794431	101.424714	49.133044
1141.104572	99.325707	49.138049
1137.781175	87.643778	49.143053
1134.288941	94.815270	49.148058
1130.875091	87.133678	49.153063
1127.266643	90.798905	49.158068
1123.485702	94.807352	49.163073
1120.226308	85.418635	49.168077
1116.290185	97.528145	49.173082
1113.030494	96.292310	49.178087
1109.624136	100.201325	49.183092
1106.251896	102.349180	49.188097
1103.026084	96.163219	49.193101
1099.307977	94.774119	49.198106
1096.174969	93.660933	49.203111
1092.217685	93.875092	49.208116
1088.484797	96.161342	49.213121
1085.039660	94.432367	49.218125
1081.508397	105.649976	49.223130
1078.120696	100.020717	49.228135
1074.567671	97.270846	49.233140
1071.490021	96.939969	49.238145
1067.798198	96.277594	49.243149
1064.131081	93.298716	49.248154
1060.870921	94.685661	49.253159
1057.134709	99.610950	49.258164
1053.317392	96.282137	49.263169
1050.222409	98.956304	49.268173
1047.139807	98.072554	49.273178
1043.414327	88.073042	49.278183
1039.569000	101.652194	49.283188
1036.223905	97.085639	49.288193
1032.779304	92.626322	49.293197
1029.000719	93.739634	49.298202
1025.692587	90.549862	49.303207
1022.135535	94.687979	49.308212
1018.276137	88.546875	49.313217
1015.111362	97.062589	49.318221
1011.474548	87.947771	49.323226
1008.912204	89.643705	49.328231
1004.798643	108.649216	49.333236
1001.023849	95.047612	49.338241
997.390302	92.829131	49.343245
994.197725	108.508609	49.348250
990.895851	102.562289	49.353255
987.025453	95.502267	49.358260
983.572196	96.261229	49.363265
980.169913	104.576640	49.368269
976.462694	100.161373	49.373274
973.608540	96.388422	49.378279
969.388239	96.048764	49.383284
966.017587	88.091562	49.388289
962.692516	88.988757	49.393293
959.143816	98.889821	49.398298
955.814155	81.637652	49.403303
952.078338	88.812267	49.408308
948.693737	85.653392	49.413313
945.555664	92.902638	49.418317
941.411740	94.705567	49.423322
938.236633	88.847093	49.428327
934.507571	91.347893	49.433332
930.876052	99.537640	49.438337
927.547113	88.239424	49.443341
923.928299	97.964744	49.448346
920.670653	93.707292	49.453351
917.078343	93.725457	49.458356
913.401198	97.793695	49.463361
909.956909	96.928297	49.468365
906.307335	96.053727	49.473370
903.096208	91.026587	49.478375
899.808709	98.507901	49.483380
896.285377	90.890846	49.488385
892.716655	87.225976	49.493389
888.588436	94.673646	49.498394
885.222760	89.385836	49.503399
882.366548	88.027112	49.508404
878.773660	97.463667	49.513409
875.397001	88.216632	49.518413
871.504590	95.646579	49.523418
867.919846	96.071689	49.528423
864.359446	90.548443	49.533428
860.885080	89.548531	49.538433
857.410688	82.265547	49.543437
853.645631	90.906343	49.548442
850.770487	86.567214	49.553447
847.413680	103.980638	49.558452
843.558533	90.477005	49.563457
840.487239	91.837734	49.568461
836.514741	90.814130	49.573466
833.017363	85.597449	49.578471
829.577203	92.583684	49.583476
825.835310	87.791036	49.588481
822.455773	86.523273	49.593485
818.609689	92.006673	49.598490
815.083824	84.579851	49.603495
812.187489	90.171666	49.608500
808.778756	94.403769	49.613505
805.380540	93.208517	49.618509
801.460180	94.726731	49.623514
798.067579	91.584939	49.628519
794.483681	92.528770	49.633524
790.689217	92.657512	49.638529
787.468994	93.193563	49.643533
783.753096	95.214614	49.648538
780.799271	92.362018	49.653543
776.800018	96.031166	49.658548
773.323052	93.389718	49.663553
769.812523	84.859556	49.668557
766.498285	89.978601	49.673562
763.157499	85.066579	49.678567
759.450157	91.961534	49.683572
755.924104	86.793622	49.688577
752.799754	95.663710	49.693581
748.668275	99.075041	49.698586
745.530202	89.161318	49.703591
741.931152	101.654957	49.708596
738.289678	87.289205	49.713601
735.151827	86.293872	49.718605
731.495265	89.450943	49.723610
728.137935	83.535452	49.728615
724.143358	89.219142	49.733620
720.850402	89.209714	49.738625
717.546775	88.502774	49.743629
713.803268	90.078887	49.748634
710.649996	91.240424	49.753639
706.717034	94.386744	49.758644
703.349780	92.601404	49.763649
699.891596	92.380423	49.768653
696.520177	95.502602	49.773658
692.882862	82.661113	49.778663
689.137721	93.810780	49.783668
685.656370	94.409637	49.788673
682.078286	88.854376	49.793677
678.825929	92.682505	49.798682
675.780067	85.244260	49.803687
671.885828	89.513989	49.808692
668.403285	87.942750	49.813697
664.991304	78.017906	49.818701
661.240571	93.021804	49.823706
657.710582	79.657429	49.828711
654.426023	83.335551	49.833716
650.747728	85.426691	49.838721
647.447192	80.230019	49.843725
643.624879	90.733655	49.848730
640.273578	86.057402	49.853735
636.900247	79.983071	49.858740
633.509577	88.714289	49.863745
630.191477	83.754466	49.868749
626.220637	87.612191	49.873754
622.708501	78.484376	49.878759
619.187761	95.072275	49.883764
615.772167	88.915941	49.888769
612.442590	82.145120	49.893773
608.584107	82.948225	49.898778
605.400174	79.147573	49.903783
601.866842	85.642135	49.908788
598.122412	95.589499	49.913793
594.724222	88.237752	49.918797
591.303903	89.156142	49.923802
587.926760	83.999878	49.928807
584.095020	81.486454	49.933812
580.489145	87.916384	49.938817
577.490648	89.784649	49.943821
573.637877	90.200901	49.948826
570.557098	73.542835	49.953831
566.780533	81.688738	49.958836
563.176173	79.491088	49.963841
559.754926	84.864082	49.968845
556.022231	92.705775	49.973850
552.956613	83.236384	49.978855
549.155850	80.075917	49.983860
545.795303	89.153618	49.988865
542.480204	80.931593	49.993869
538.561444	82.775450	49.998874
535.528196	80.868537	50.003879
531.758223	69.654895	50.008884
528.047445	79.840618	50.013889
524.896853	70.397123	50.018893
520.961863	85.423374	50.023898
517.945777	78.951773	50.028903
514.617652	84.186889	50.033908
510.590490	84.184221	50.038913
507.069067	87.016565	50.043917
503.465141	89.358730	50.048922
500.015903	81.901059	50.053927
496.630165	87.404569	50.058932
493.203214	92.749985	50.063937
489.841881	81.681532	50.068941
486.140127	90.005618	50.073946
483.013745	80.741849	50.078951
479.059396	77.523050	50.083956
475.421445	89.019858	50.088961
472.290561	81.585396	50.093965
468.574663	93.515111	50.098970
465.142715	85.564384	50.103975
462.046516	90.054737	50.108980
458.487772	94.316552	50.113985
454.583565	89.732731	50.118989
451.142889	82.979236	50.123994
447.826791	86.823634	50.128999
444.094793	92.365236	50.134004
440.552703	87.592170	50.139009
437.189990	88.178917	50.144013
433.658615	87.349285	50.149018
430.358459	90.609088	50.154023
426.453039	88.284325	50.159028
423.195040	94.650621	50.164033
419.723264	85.709546	50.169037
415.760119	94.479282	50.174042
412.694108	84.598702	50.179047
409.146576	87.121918	50.184052
405.226621	91.955650	50.189057
402.028623	80.580222	50.194061
398.447069	80.255105	50.199066
395.193553	80.090885	50.204071
391.487749	89.567183	50.209076
388.005797	83.427551	50.214081
384.837076	93.924360	50.219085
381.061442	87.381206	50.224090
377.669219	83.125809	50.229095
373.891904	88.165121	50.234100
370.531786	87.998518	50.239105
367.321354	79.228737	50.244109
363.714868	89.471002	50.249114
359.788059	87.079979	50.254119
356.542231	88.281273	50.259124
352.759060	84.599258	50.264129
349.869365	79.088747	50.269133
346.360152	84.095813	50.274138
342.688268	82.743919	50.279143
338.971854	91.820088	50.284148
335.312986	87.036748	50.289153
332.032167	76.832137	50.294157
328.142175	91.152219	50.299162
324.995646	85.172344	50.304167
321.329351	84.607336	50.309172
318.150867	89.322478	50.314177
314.764379	81.794965	50.319181
310.799235	82.722282	50.324186
307.497281	82.780743	50.329191
304.272059	79.489589	50.334196
301.002417	92.185043	50.339201
297.318341	89.243727	50.344205
293.399371	85.225370	50.349210
289.755444	84.457574	50.354215
286.402940	83.122403	50.359220
282.742906	76.422075	50.364225
279.647614	77.150700	50.369229
275.985228	84.209530	50.374234
272.555003	86.021656	50.379239
269.300786	81.804903	50.384244
265.408052	85.229742	50.389249
262.086089	77.287246	50.394253
258.056007	91.379211	50.399258
254.748562	85.974879	50.404263
251.264381	83.391583	50.409268
248.028774	88.147260	50.414273
244.517879	77.446990	50.419277
240.897460	87.273826	50.424282
237.259760	83.316092	50.429287
234.160445	84.744519	50.434292
230.501345	87.370545	50.439297
227.309774	84.972645	50.444301
223.468652	92.821753	50.449306
219.952708	86.674789	50.454311
216.235053	90.047068	50.459316
212.675927	90.091798	50.464321
209.475903	91.887074	50.469325
205.845094	95.701403	50.474330
202.399325	89.901010	50.479335
199.285942	83.903342	50.484340
195.506948	85.921633	50.489345
192.237599	86.671040	50.494349
188.201491	91.048330	50.499354
184.756955	82.552307	50.504359
181.576408	90.279591	50.509364
177.680491	87.934411	50.514369
174.581311	79.416260	50.519373
170.808511	88.023504	50.524378
167.180903	82.166012	50.529383
164.049315	80.904030	50.534388
160.155183	79.551966	50.539393
157.020842	80.805526	50.544397
153.102675	89.425914	50.549402
149.730920	80.494637	50.554407
146.870144	81.512624	50.559412
143.070518	88.675089	50.564417
139.403635	85.436904	50.569421
135.904514	77.642235	50.574426
132.479180	80.418534	50.579431
128.953719	76.889423	50.584436
124.973408	80.581007	50.589441
121.517347	74.234924	50.594445
117.921160	85.424696	50.599450
114.641936	81.319427	50.604455
111.593427	88.605391	50.609460
108.097305	89.114876	50.614465
104.707413	90.591723	50.619469
101.094771	86.655421	50.624474
97.274490	84.409207	50.629479
94.056602	84.163552	50.634484
90.423870	80.935878	50.639489
86.812817	87.433093	50.644493
82.974405	89.432177	50.649498
79.395745	81.577138	50.654503
76.155674	89.857847	50.659508
72.513454	88.491886	50.664513
69.247329	78.595083	50.669517
65.670503	86.229052	50.674522
62.298358	78.566485	50.679527
59.069250	85.855260	50.684532
55.059688	92.208886	50.689537
51.700332	87.413769	50.694541
48.363292	80.109560	50.699546
44.839483	77.851998	50.704551
41.307716	82.426020	50.709556
37.492719	88.695573	50.714561
34.599653	75.975655	50.719565
30.513045	80.579118	50.724570
27.336159	69.346025	50.729575
24.068845	69.149203	50.734580
20.425554	73.610879	50.739585
16.675118	74.795869	50.744589
13.226491	81.040016	50.749594
9.517844	75.850054	50.754599
5.946587	80.351136	50.759604
2.685839	73.962013	50.764609