Fri Aug 26 14:29:07 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
-0.121082	107.619922	0.000000
-0.355986	103.999271	0.005005
-0.473938	95.301714	0.010010
-0.253631	84.137622	0.015014
-0.578519	86.725435	0.020019
-0.637418	76.047732	0.025024
-1.068882	77.959296	0.030029
-1.113054	66.754138	0.035034
-1.363260	53.888509	0.040038
-2.036857	54.784273	0.045043
-1.910752	44.976262	0.050048
-2.663532	42.692227	0.055053
-2.655091	39.388031	0.060058
-2.141553	34.170276	0.065062
-2.983342	28.432738	0.070067
-3.207606	10.823952	0.075072
-4.062850	1.798324	0.080077
-4.214042	1.094199	0.085082
-4.327143	-5.731185	0.090086
-4.827893	6.862138	0.095091
-4.798141	-4.142521	0.100096
-5.085021	2.574248	0.105101
-5.240747	-1.916056	0.110106
-5.545915	-3.399774	0.115110
-6.303916	8.857129	0.120115
-6.646746	-5.142438	0.125120
-6.690198	4.282474	0.130125
-6.960160	-9.121015	0.135130
-6.808155	-12.245081	0.140134
-7.350682	-9.069758	0.145139
-7.522715	-9.865547	0.150144
-8.089882	-0.896916	0.155149
-8.567547	-4.675893	0.160154
-8.564187	-4.673279	0.165158
-8.658145	3.139710	0.170163
-8.388184	-10.297225	0.175168
-8.868405	-4.461486	0.180173
-9.249809	-1.295429	0.185178
-9.654519	-7.645154	0.190182
-10.295414	-1.395269	0.195187
-10.113468	-8.276080	0.200192
-10.266705	-1.665539	0.205197
-10.249611	-7.707627	0.210202
-10.286894	-11.476077	0.215206
-11.243715	-1.535649	0.220211
-11.272817	-5.169337	0.225216
-11.461591	-2.684984	0.230221
-11.657721	-1.126434	0.235226
-12.062282	-10.336116	0.240230
-12.828115	-2.500775	0.245235
-12.881518	-2.308996	0.250240
-13.153697	-8.046625	0.255245
-12.843568	1.218834	0.260250
-13.087987	-0.264852	0.265254
-13.278549	-4.053730	0.270259
-13.417354	-2.307958	0.275264
-13.854378	-1.002957	0.280269
-14.697186	7.613139	0.285274
-14.618627	2.042353	0.290278
-14.685005	-2.664336	0.295283
-15.423378	-14.593395	0.300288
-15.527862	-2.004831	0.305293
-15.708339	2.319473	0.310298
-15.876669	-3.722218	0.315302
-16.050309	7.709735	0.320307
-16.341679	0.728614	0.325312
-16.098908	-0.340561	0.330317
-16.838109	-1.389718	0.335322
-17.012352	-11.030715	0.340326
-17.321249	6.547113	0.345331
-17.247000	-0.902208	0.350336
-17.972795	-3.475166	0.355341
-18.565160	2.817783	0.360346
-18.755544	-3.030656	0.365350
-18.562119	7.391888	0.370355
-18.538111	0.159190	0.375360
-18.800218	3.430055	0.380365
-19.262407	-2.322282	0.385370
-19.627794	-2.654548	0.390374
-20.182181	0.532114	0.395379
-20.270528	-5.221484	0.400384
-20.204483	-4.836338	0.405389
-20.430466	-10.609632	0.410394
-20.314471	-4.290939	0.415398
-21.198476	-4.058419	0.420403
-21.905881	-8.462827	0.425408
-21.881283	-1.879975	0.430413
-21.974969	-4.023021	0.435418
-21.804583	-1.730625	0.440422
-21.774120	6.834922	0.445427
-22.462724	1.680965	0.450432
-22.695961	3.779949	0.455437
-23.461781	1.175259	0.460442
-23.469513	-0.848298	0.465446
-23.798262	4.182440	0.470451
-23.764474	-4.187528	0.475456
-23.949808	-7.486853	0.480461
-24.178940	-3.525122	0.485466
-23.988294	-8.335099	0.490470
-25.083398	-1.261548	0.495475
-25.535142	-1.953679	0.500480
-25.811521	-3.967044	0.505485
-25.946395	2.359074	0.510490
-25.753453	-3.191555	0.515494
-26.170365	-0.706481	0.520499
-25.813913	-5.507475	0.525504
-26.023549	-3.472275	0.530509
-26.744769	0.509128	0.535514
-27.027034	-9.652869	0.540518
-27.251908	-1.990337	0.545523
-27.315256	-4.821454	0.550528
-28.204042	-8.887583	0.555533
-28.673457	-2.072796	0.560538
-28.882958	-5.014031	0.565542
-29.056232	2.067849	0.570547
-29.168322	-3.321396	0.575552
-29.329264	0.303864	0.580557
-29.303322	7.838767	0.585562
-29.137059	-6.056571	0.590566
-28.989493	-0.552686	0.595571
-29.714064	-5.913005	0.600576
-30.313090	-2.719393	0.605581
-30.757147	0.304564	0.610586
-31.014992	-4.916460	0.615590
-31.604108	3.100169	0.620595
-31.588010	-8.664797	0.625600
-31.825037	-2.177248	0.630605
-31.848730	5.014217	0.635610
-32.225114	-1.982138	0.640614
-32.059850	5.610162	0.645619
-32.510115	-1.219671	0.650624
-33.553474	3.144072	0.655629
-33.750044	4.342036	0.660634
-33.711554	-1.867894	0.665638
-33.618836	12.857072	0.670643
-33.840247	-1.386019	0.675648
-33.699631	-5.767442	0.680653
-33.934581	2.997609	0.685658
-34.161955	-0.817173	0.690662
-34.856556	-2.028292	0.695667
-34.927624	-6.123665	0.700672
-35.021402	4.137956	0.705677
-35.524244	5.864480	0.710682
-35.850284	-8.406606	0.715686
-36.247301	1.459317	0.720691
-36.367893	3.015598	0.725696
-36.586222	-4.318566	0.730701
-37.563944	-7.367972	0.735706
-37.545427	-5.121531	0.740710
-37.788093	-5.121739	0.745715
-37.726488	-2.935788	0.750720
-37.801412	-8.099872	0.755725
-38.424282	-2.583597	0.760730
-38.026456	-1.063742	0.765734
-38.301006	0.798073	0.770739
-38.669572	-9.385286	0.775744
-39.174820	-11.182688	0.780749
-39.530304	-2.753201	0.785754
-39.228351	-4.214391	0.790758
-39.631760	-2.329349	0.795763
-40.249976	-8.892592	0.800768
-40.725534	-2.371069	0.805773
-40.888048	-1.580191	0.810778
-41.216486	-14.462057	0.815782
-41.319889	-4.436216	0.820787
-41.173511	-0.646842	0.825792
-41.114545	-5.610318	0.830797
-42.118458	-9.997030	0.835802
-42.339340	-5.571528	0.840806
-42.508421	-6.209595	0.845811
-42.267735	-7.885864	0.850816
-42.708924	-8.187346	0.855821
-43.487607	-14.466183	0.860826
-43.480126	-13.069045	0.865830
-43.909470	-9.636108	0.870835
-43.987914	-4.755073	0.875840
-43.914441	-8.531277	0.880845
-44.145606	-6.027670	0.885850
-44.695159	-15.578590	0.890854
-45.406252	-5.578352	0.895859
-45.700072	-5.640195	0.900864
-45.403100	-4.439985	0.905869
-45.943331	-5.640339	0.910874
-45.802187	-12.166793	0.915878
-45.629990	-0.899422	0.920883
-45.729520	0.957289	0.925888
-46.230963	-3.915768	0.930893
-46.734923	4.603276	0.935898
-47.015507	-8.004481	0.940902
-47.538426	-7.189125	0.945907
-48.426650	-2.552155	0.950912
-48.369787	-3.313983	0.955917
-48.315027	6.127273	0.960922
-48.238643	5.093495	0.965926
-48.170846	1.315010	0.970931
-48.504117	-2.306119	0.975936
-49.451919	0.900670	0.980941
-49.556784	6.788696	0.985946
-49.497925	-5.675766	0.990950
-49.994601	0.501045	0.995955
-49.996225	-10.308901	1.000960
-50.460811	-0.622279	1.005965
-50.833948	4.168604	1.010970
-51.109679	-5.494554	1.015974
-51.252572	11.120987	1.020979
-51.295519	6.059485	1.025984
-51.487926	4.108973	1.030989
-52.027884	-5.955956	1.035994
-52.808290	-2.288030	1.040998
-52.942844	5.363605	1.046003
-52.865104	2.899649	1.051008
-52.898246	-3.134616	1.056013
-52.766614	6.354779	1.061018
-52.981080	-1.812025	1.066022
-53.164470	-0.160549	1.071027
-54.027037	-7.587385	1.076032
-53.808682	-1.901541	1.081037
-54.185547	1.146753	1.086042
-54.686218	0.772279	1.091046
-55.117942	3.019222	1.096051
-55.261840	3.658511	1.101056
-55.444112	-0.561912	1.106061
-55.761883	7.681379	1.111066
-55.554852	-2.971240	1.116070
-56.377608	4.246563	1.121075
-57.007669	-5.506954	1.126080
-56.833008	-9.469748	1.131085
-57.408308	1.486916	1.136090
-57.212651	-9.983312	1.141094
-57.081152	5.548663	1.146099
-57.171911	-8.626179	1.151104
-57.536307	-5.013535	1.156109
-58.290639	-2.684726	1.161114
-58.687001	-6.887632	1.166118
-58.888048	-3.967950	1.171123
-58.767536	-6.732783	1.176128
-59.042276	-8.072546	1.181133
-59.691718	-1.536604	1.186138
-60.044049	-6.192440	1.191142
-60.214735	-3.160429	1.196147
-60.159015	-6.142958	1.201152
-60.372411	3.915831	1.206157
-60.505394	-5.915081	1.211162
-60.497819	-0.209073	1.216166
-61.346695	2.745040	1.221171
-61.366799	-4.945840	1.226176
-61.476490	2.467812	1.231181
-62.318127	1.877516	1.236186
-62.459944	-11.488971	1.241190
-62.818341	-3.574706	1.246195
-62.877707	-2.565778	1.251200
-63.103618	2.755819	1.256205
-63.171677	-5.835561	1.261210
-63.177141	-5.967610	1.266214
-63.476845	1.080171	1.271219
-64.449006	-0.179477	1.276224
-64.706991	-1.600940	1.281229
-64.765232	0.799816	1.286234
-64.864855	-4.420531	1.291238
-64.885831	-8.011191	1.296243
-64.890230	-2.774703	1.301248
-64.615677	1.864716	1.306253
-65.730832	-1.473328	1.311258
-66.158479	-2.403319	1.316262
-66.242547	-6.392266	1.321267
-66.374730	1.034378	1.326272
-66.111687	-8.364663	1.331277
-67.076977	-6.847702	1.336282
-67.457508	-2.625125	1.341286
-67.896396	1.369265	1.346291
-67.934957	-7.957508	1.351296
-67.809862	-8.761596	1.356301
-68.102730	7.760237	1.361306
-68.160345	-1.797683	1.366310
-69.110838	0.343377	1.371315
-69.439469	0.154081	1.376320
-69.011777	1.352920	1.381325
-69.761738	4.025887	1.386330
-69.445343	-3.495932	1.391334
-69.752400	-0.784362	1.396339
-70.141730	1.126962	1.401344
-70.328138	-7.215044	1.406349
-70.781673	0.815272	1.411354
-70.571385	-0.321609	1.416358
-70.896635	4.082181	1.421363
-71.455915	-3.638642	1.426368
-71.849783	-5.921604	1.431373
-72.213025	4.435752	1.436378
-72.165622	-2.693020	1.441382
-72.236860	-2.137809	1.446387
-73.151615	-1.394316	1.451392
-73.047050	0.731163	1.456397
-73.646412	0.368891	1.461402
-73.597254	-0.420210	1.466406
-73.499843	-0.691659	1.471411
-73.849416	2.893369	1.476416
-73.771300	-0.551375	1.481421
-74.661920	14.045128	1.486426
-74.841204	1.529159	1.491430
-75.212411	-5.154797	1.496435
-75.293892	4.538615	1.501440
-75.476779	-8.694933	1.506445
-75.693102	5.110064	1.511450
-75.770490	2.762007	1.516454
-76.669640	-4.326950	1.521459
-76.745224	2.138625	1.526464
-76.546080	-7.133412	1.531469
-76.741951	4.748068	1.536474
-76.870658	3.521605	1.541478
-77.296121	-6.868022	1.546483
-77.990402	1.016287	1.551488
-77.932100	-1.140932	1.556493
-78.262008	9.176435	1.561498
-78.194935	3.825731	1.566502
-78.951787	-4.705857	1.571507
-79.437503	5.831913	1.576512
-79.489536	3.106598	1.581517
-79.784860	1.444185	1.586522
-79.472703	-2.559000	1.591526
-79.650338	12.476963	1.596531
-80.229937	2.399222	1.601536
-80.623552	2.428844	1.606541
-81.039256	4.448675	1.611546
-81.283176	6.637905	1.616550
-81.125613	-2.365078	1.621555
-81.182144	0.481485	1.626560
-81.302196	0.155313	1.631565
-82.192185	6.491437	1.636570
-82.227571	15.877130	1.641574
-82.441580	7.934872	1.646579
-82.658093	7.142844	1.651584
-82.606587	-0.701550	1.656589
-83.395643	8.523085	1.661594
-83.472859	4.767179	1.666598
-83.621267	9.757182	1.671603
-84.117261	-2.174815	1.676608
-84.107531	0.718377	1.681613
-85.038945	14.761266	1.686618
-84.941464	4.056102	1.691622
-85.057292	3.425562	1.696627
-85.544133	4.251120	1.701632
-85.350926	4.692393	1.706637
-85.444845	4.147024	1.711642
-85.900870	-2.476271	1.716646
-86.405352	3.008918	1.721651
-86.874742	7.916024	1.726656
-86.803183	-2.772445	1.731661
-87.219016	7.457063	1.736666
-87.147084	9.299732	1.741670
-87.027682	-1.987789	1.746675
-88.002281	1.653429	1.751680
-88.214463	0.136253	1.756685
-88.230100	-5.989317	1.761690
-88.369214	4.190776	1.766694
-88.537237	1.733449	1.771699
-89.159208	8.992755	1.776704
-89.658515	7.786030	1.781709
-89.857924	4.925480	1.786714
-89.977848	-5.495900	1.791718
-90.250890	-0.078385	1.796723
-90.218592	3.934388	1.801728
-89.988668	6.315586	1.806733
-89.893062	6.639183	1.811738
-90.661395	10.026831	1.816742
-91.303436	-1.025078	1.821747
-91.724148	3.776375	1.826752
-92.376214	-8.846299	1.831757
-92.235195	4.298802	1.836762
-92.446520	1.718507	1.841766
-92.904065	2.881178	1.846771
-92.873970	-3.049040	1.851776
-92.975535	-3.286345	1.856781
-93.318600	4.486334	1.861786
-93.182779	-6.879667	1.866790
-93.394052	-2.923881	1.871795
-93.983559	7.968560	1.876800
-94.480215	-2.583983	1.881805
-94.580204	-1.900913	1.886810
-94.610082	-0.102502	1.891814
-95.024312	9.737629	1.896819
-95.891251	-2.914866	1.901824
-95.798687	4.771004	1.906829
-96.299036	2.257856	1.911834
-95.994510	6.180788	1.916838
-96.177325	6.977991	1.921843
-96.294626	4.167929	1.926848
-96.161757	-7.295684	1.931853
-96.872390	1.094189	1.936858
-97.338931	4.422192	1.941862
-97.182110	4.157311	1.946867
-97.721246	0.419546	1.951872
-97.906213	-4.540748	1.956877
-98.518858	7.468897	1.961882
-98.577239	2.460420	1.966886
-98.702159	1.401040	1.971891
-98.927014	-0.231217	1.976896
-99.153331	-4.077797	1.981901
-100.146391	7.269768	1.986906
-100.239138	3.753555	1.991910
-100.283514	-7.850134	1.996915
-100.521744	-1.388430	2.006912
-99.723077	1.005480	2.016909
-99.237110	3.986586	2.026906
-98.902736	-1.827568	2.036902
-98.872340	-1.350865	2.046899
-98.426470	5.494736	2.056896
-97.956800	3.337211	2.066893
-96.731923	-2.913357	2.076890
-96.734260	-3.011246	2.086886
-96.034892	-0.329454	2.096883
-95.473410	0.663252	2.106880
-95.221827	-4.019813	2.116877
-94.793924	5.540132	2.126874
-94.101266	7.719307	2.136870
-93.807031	1.791030	2.146867
-92.582389	3.567436	2.156864
-92.683672	7.520598	2.166861
-92.337458	7.640861	2.176858
-91.410866	5.348838	2.186854
-91.290537	10.157617	2.196851
-90.196125	-0.969896	2.206848
-89.982134	3.928832	2.216845
-90.002773	10.200862	2.226842
-88.953052	4.411538	2.236838
-88.504922	6.137793	2.246835
-88.234728	4.350269	2.256832
-87.424525	7.363252	2.266829
-87.140502	4.296994	2.276826
-86.660044	2.704806	2.286822
-85.635200	7.249212	2.296819
-85.382485	2.901743	2.306816
-85.723891	2.682424	2.316813
-84.886164	1.918397	2.326810
-83.454594	1.461037	2.336806
-83.638289	1.679646	2.346803
-83.155295	-6.682299	2.356800
-82.701886	-0.046940	2.366797
-81.850483	-1.544835	2.376794
-81.553384	-1.154005	2.386790
-81.073870	0.884133	2.396787
-79.979919	-4.487604	2.406784
-79.847498	3.601023	2.416781
-80.010094	6.860502	2.426778
-79.378784	7.037742	2.436774
-78.624523	1.278584	2.446771
-77.573311	-8.442078	2.456768
-77.269463	-2.236414	2.466765
-77.264651	2.454139	2.476762
-76.792060	2.063733	2.486758
-75.834366	1.195499	2.496755
-75.482519	-5.815595	2.506752
-75.298208	-5.213975	2.516749
-74.435126	0.017664	2.526746
-74.180692	-7.738510	2.536742
-73.406565	-1.720104	2.546739
-73.222642	-4.843632	2.556736
-72.770059	-5.943654	2.566733
-71.766957	-4.943683	2.576730
-71.626865	0.682451	2.586726
-70.763694	4.482279	2.596723
-69.990176	1.023037	2.606720
-69.982913	-4.122485	2.616717
-69.933046	0.313973	2.626714
-68.920245	-4.544633	2.636710
-68.481430	-5.537978	2.646707
-68.158111	2.929560	2.656704
-67.284194	-1.220033	2.666701
-66.957025	-1.733511	2.676698
-66.680706	-0.699572	2.686694
-65.722814	5.645008	2.696691
-65.887899	0.133524	2.706688
-64.924452	-0.121072	2.716685
-64.218763	-1.913048	2.726682
-64.151902	3.708651	2.736678
-63.519711	-1.416968	2.746675
-62.930857	1.855386	2.756672
-62.501823	3.936229	2.766669
-61.932302	2.346013	2.776666
-61.568318	-0.577478	2.786662
-61.345535	-4.619353	2.796659
-60.127077	-5.284275	2.806656
-60.166930	2.951549	2.816653
-59.265261	0.631731	2.826650
-58.741230	2.967037	2.836646
-58.570491	2.436735	2.846643
-58.404460	3.171077	2.856640
-57.385692	-0.202809	2.866637
-57.154438	4.560190	2.876634
-56.044384	2.857304	2.886630
-55.721983	-6.743549	2.896627
-55.532767	0.385927	2.906624
-55.587146	-5.865027	2.916621
-54.620718	-1.897549	2.926618
-53.415113	-4.866551	2.936614
-53.297767	-6.053755	2.946611
-52.900318	-2.954332	2.956608
-52.640049	2.767128	2.966605
-51.965854	2.715954	2.976602
-51.154282	0.080723	2.986598
-50.901681	5.702013	2.996595
-50.500590	3.456966	3.006592
-49.631643	-0.885082	3.016589
-49.610600	-4.420393	3.026586
-49.350342	-0.596381	3.036582
-48.501762	0.845787	3.046579
-48.159689	-2.387894	3.056576
-47.081634	-2.188347	3.066573
-46.903500	-0.974400	3.076570
-46.607012	0.316150	3.086566
-45.905684	-0.125708	3.096563
-45.370294	-2.632409	3.106560
-45.088713	2.955859	3.116557
-44.404837	0.752311	3.126554
-43.912439	2.734594	3.136550
-43.601390	0.864685	3.146547
-42.619699	-7.555902	3.156544
-42.509149	-5.004169	3.166541
-42.130928	2.064204	3.176538
-41.065416	0.821235	3.186534
-40.935381	1.941305	3.196531
-40.957879	1.840220	3.206528
-39.909321	0.843803	3.216525
-39.456862	1.650753	3.226522
-38.687214	5.325767	3.236518
-38.201133	2.167861	3.246515
-38.033877	-3.585429	3.256512
-37.723456	3.113378	3.266509
-36.747810	2.980423	3.276506
-36.492640	-1.215378	3.286502
-35.148492	-3.274648	3.296499
-35.656780	-0.442835	3.306496
-35.037756	3.794139	3.316493
-34.714634	1.830486	3.326490
-33.406680	-3.533391	3.336486
-33.426343	2.279171	3.346483
-33.155175	-1.732227	3.356480
-32.055821	-0.417799	3.366477
-31.768972	-2.752759	3.376474
-31.791117	-5.492590	3.386470
-31.020002	-8.979965	3.396467
-30.545279	-7.184993	3.406464
-29.301592	1.284962	3.416461
-29.108873	-4.114343	3.426458
-28.953072	-6.463744	3.436454
-28.773461	-4.521456	3.446451
-27.885012	-5.201516	3.456448
-27.435267	-6.845939	3.466445
-27.095137	-0.972192	3.476442
-26.136784	-0.944069	3.486438
-26.092900	-0.605677	3.496435
-25.559858	-0.451147	3.506432
-25.081417	0.798403	3.516429
-23.942764	-1.532970	3.526426
-23.654174	-6.038073	3.536422
-23.502437	3.824628	3.546419
-23.347722	6.017873	3.556416
-22.480401	1.311792	3.566413
-21.696012	3.527371	3.576410
-21.222586	4.315219	3.586406
-20.722773	3.169831	3.596403
-20.554152	3.295573	3.606400
-20.063149	0.681745	3.616397
-19.157991	3.774979	3.626394
-18.595914	2.100394	3.636390
-18.387895	6.448878	3.646387
-18.002812	10.829980	3.656384
-17.554306	6.132087	3.666381
-16.687368	3.101778	3.676378
-16.144895	4.610614	3.686374
-15.910718	-2.163593	3.696371
-15.523246	-2.981055	3.706368
-14.931446	0.702644	3.716365
-14.765077	1.481281	3.726362
-13.659421	1.340756	3.736358
-12.935101	4.924630	3.746355
-13.032220	-2.966875	3.756352
-12.522760	3.666099	3.766349
-11.409644	-2.142597	3.776346
-11.451723	-5.132740	3.786342
-11.189362	2.527027	3.796339
-10.284911	-3.607130	3.806336
-10.018309	-2.068013	3.816333
-9.232481	4.236840	3.826330
-8.923702	-2.846746	3.836326
-8.499815	-0.955161	3.846323
-7.322174	-4.049684	3.856320
-7.495234	2.211234	3.866317
-6.996639	-5.864884	3.876314
-6.184674	0.318693	3.886310
-5.558619	0.766008	3.896307
-5.682677	2.552844	3.906304
-4.981821	10.004964	3.916301
-4.823982	9.197913	3.926298
-4.134797	17.687692	3.936294
-3.844868	25.365351	3.946291
-3.269558	34.854855	3.956288
-2.417372	52.233191	3.966285
-2.233742	62.920901	3.976282
-1.750920	76.333780	3.986278
-1.202229	83.727263	3.996275
-0.517032	96.785542	4.006272
-0.242932	112.964684	4.016269
0.000000	116.899390	4.021274
0.306728	133.011626	4.026278
0.836735	131.081495	4.031283
0.559944	143.099058	4.036288
1.076914	130.392330	4.041293
0.902749	143.700510	4.046298
0.768709	148.109366	4.051302
0.898895	146.424977	4.056307
0.178951	152.579658	4.061312
0.601106	139.027168	4.066317
0.699100	149.875933	4.071322
0.937729	146.421986	4.076326
1.191737	150.349656	4.081331
1.253488	161.909571	4.086336
1.299269	158.058551	4.091341
1.062349	151.825010	4.096346
0.477943	141.010793	4.101350
0.817472	149.585237	4.106355
0.976205	158.943952	4.111360
1.080704	164.068627	4.116365
1.285837	170.613944	4.121370
0.740072	170.578671	4.126374
0.800089	164.608933	4.131379
1.175267	165.521741	4.136384
1.384762	166.343288	4.141389
1.369623	167.775600	4.146394
1.139012	171.848329	4.151398
1.361619	171.301128	4.156403
1.010863	175.481147	4.161408
1.233541	163.649100	4.166413
1.402913	168.440980	4.171418
0.896188	165.742141	4.176422
1.271886	168.616347	4.181427
1.173482	172.241396	4.186432
1.327070	165.535771	4.191437
1.347092	161.780507	4.196442
0.967213	166.142224	4.201446
1.259340	159.823146	4.206451
1.213513	167.780570	4.211456
1.389226	165.032424	4.216461
1.443029	163.135305	4.221466
1.191916	168.789900	4.226470
1.304614	160.945393	4.231475
1.020836	170.224319	4.236480
1.430342	172.757912	4.241485
1.191244	179.663456	4.246490
1.462473	186.644566	4.251494
1.679453	182.782704	4.256499
1.357857	192.061202	4.261504
1.725884	187.995492	4.266509
1.397431	192.561175	4.271514
1.567849	194.619480	4.276518
2.117050	182.163956	4.281523
1.761714	177.502209	4.286528
1.489646	173.643727	4.291533
1.385166	169.708534	4.296538
1.217923	173.031098	4.301542
1.646610	170.199272	4.306547
1.324082	180.271992	4.311552
1.287946	185.345805	4.316557
1.871710	190.965330	4.321562
1.820745	194.630452	4.326566
1.784781	185.432879	4.331571
1.442277	190.462647	4.336576
1.720903	190.362292	4.341581
1.643468	195.116679	4.346586
1.713038	189.752872	4.351590
1.628127	191.246668	4.356595
1.775678	191.473598	4.361600
1.661778	186.881823	4.366605
1.821647	187.540259	4.371610
1.718908	195.335719	4.376614
1.874968	187.544558	4.381619
1.856366	200.616593	4.386624
1.809796	189.063726	4.391629
1.757357	193.532653	4.396634
1.718328	197.107335	4.401638
2.175877	193.976789	4.406643
1.653711	206.086380	4.411648
1.934270	194.836909	4.416653
1.628754	188.667817	4.421658
1.651702	198.772178	4.426662
1.721947	191.203179	4.431667
2.187505	202.478792	4.436672
1.926706	194.720895	4.441677
1.721723	194.673690	4.446682
1.559349	193.398671	4.451686
1.777984	198.654279	4.456691
1.975866	203.204454	4.461696
2.060665	203.808142	4.466701
1.786668	203.591353	4.471706
1.646945	194.296037	4.476710
1.856771	197.028398	4.481715
1.533131	198.825113	4.486720
1.906498	215.790734	4.491725
2.091022	215.347534	4.496730
1.901170	221.033735	4.501734
2.179157	228.428253	4.506739
2.297869	233.196402	4.511744
2.184630	218.926797	4.516749
2.330544	218.998962	4.521754
2.141204	220.233779	4.526758
2.105793	198.574359	4.531763
1.912782	214.862551	4.536768
2.257301	214.748773	4.541773
2.312674	212.927334	4.546778
2.282918	212.096727	4.551782
1.939902	210.862486	4.556787
2.343036	208.790754	4.561792
2.394045	204.340973	4.566797
2.487273	214.225597	4.571802
1.911291	208.196683	4.576806
2.320852	204.839495	4.581811
2.426025	215.260085	4.586816
2.369956	203.420793	4.591821
2.254124	204.622018	4.596826
2.271114	208.216453	4.601830
1.953715	213.811781	4.606835
2.014947	214.627942	4.611840
2.020999	222.314728	4.616845
2.578113	219.102239	4.621850
2.553126	225.661259	4.626854
2.693422	219.830861	4.631859
2.890282	224.713388	4.636864
2.657482	221.377117	4.641869
2.284601	204.452489	4.646874
2.262269	203.345486	4.651878
2.608614	208.793179	4.656883
2.349844	215.831511	4.661888
2.358035	224.381651	4.666893
2.502803	217.535013	4.671898
2.297283	223.274274	4.676902
2.773178	228.448708	4.681907
2.600318	233.360328	4.686912
2.375594	222.442605	4.691917
2.889415	219.259002	4.696922
2.693787	223.854632	4.701926
2.894043	215.088490	4.706931
2.524286	203.914956	4.711936
2.076112	208.806161	4.716941
2.587059	222.937853	4.721946
2.282246	228.429989	4.726950
2.632270	221.807651	4.731955
2.388533	228.989177	4.736960
2.798966	228.390584	4.741965
2.503191	221.163293	4.746970
2.148644	221.993570	4.751974
2.367151	214.006018	4.756979
2.171195	218.829483	4.761984
2.904646	231.474407	4.766989
2.462306	226.838848	4.771994
2.717205	237.558836	4.776998
2.857769	238.261408	4.782003
2.759424	246.910402	4.787008
2.812667	252.777059	4.792013
2.794162	249.799716	4.797018
2.629180	260.379451	4.802022
2.652428	253.602340	4.807027
2.526790	255.342922	4.812032
2.893100	256.431118	4.817037
2.919695	243.386217	4.822042
2.816146	247.230377	4.827046
3.200062	245.459019	4.832051
2.659569	255.436006	4.837056
2.619011	256.283836	4.842061
2.892577	245.310663	4.847066
2.847296	250.461846	4.852070
3.222344	252.716084	4.857075
3.288297	259.086955	4.862080
3.029016	249.360981	4.867085
3.080676	254.107938	4.872090
3.103020	255.350926	4.877094
3.195565	248.177057	4.882099
2.967677	252.369601	4.887104
2.663779	255.602727	4.892109
2.859391	250.554629	4.897114
2.932948	249.217563	4.902118
3.127740	247.953368	4.907123
2.857782	252.297992	4.912128
3.041728	251.513203	4.917133
2.999520	247.947941	4.922138
3.217336	253.985123	4.927142
3.430383	251.993600	4.932147
2.931582	252.504660	4.937152
3.077789	255.636070	4.942157
3.149445	250.816075	4.947162
3.075156	246.920457	4.952166
3.170601	248.942986	4.957171
3.164662	244.831086	4.962176
3.163266	251.987544	4.967181
2.903816	251.170552	4.972186
3.486112	267.021710	4.977190
3.902619	257.063966	4.982195
3.376412	266.747676	4.987200
3.469742	253.075456	4.992205
3.354444	264.561766	4.997210
2.979860	262.611115	5.002214
3.210084	255.403151	5.007219
3.048169	258.778684	5.012224
3.013885	259.720448	5.017229
3.268494	262.664141	5.022234
3.152469	276.248100	5.027238
3.873964	275.316341	5.032243
3.739844	281.164724	5.037248
3.344350	265.110412	5.042253
3.209799	262.394739	5.047258
3.427726	276.996031	5.052262
3.627775	275.288099	5.057267
3.553279	280.377402	5.062272
3.416472	270.173612	5.067277
3.248705	259.541222	5.072282
3.190823	275.539516	5.077286
3.513115	277.675423	5.082291
3.700507	275.570835	5.087296
3.854740	280.219573	5.092301
3.644071	279.328547	5.097306
3.436334	279.642433	5.102310
3.824895	270.726725	5.107315
3.910178	279.147831	5.112320
3.348348	267.516952	5.117325
3.565741	275.901669	5.122330
3.431284	283.496465	5.127334
3.694861	276.220027	5.132339
3.517117	275.684536	5.137344
3.517389	274.792305	5.142349
3.528562	281.880380	5.147354
3.549423	277.090433	5.152358
3.980993	270.860334	5.157363
3.614876	279.826276	5.162368
3.892412	272.487555	5.167373
3.845063	271.061747	5.172378
3.539029	276.848311	5.177382
3.474579	279.414585	5.182387
3.540565	281.862476	5.187392
3.731883	280.263467	5.192397
3.694839	275.153512	5.197402
3.417290	286.750517	5.202406
3.730786	279.266992	5.207411
3.486126	272.221544	5.212416
3.693908	279.475156	5.217421
4.190474	290.024674	5.222426
4.000000	279.168022	5.227430
3.822761	272.479064	5.232435
3.783479	276.987091	5.237440
3.810601	279.602382	5.242445
4.035647	285.752343	5.247450
4.034356	288.201219	5.252454
3.922883	280.252358	5.257459
3.962589	288.123754	5.262464
4.021931	282.005389	5.267469
4.213037	273.332390	5.272474
3.839065	277.009856	5.277478
3.927984	274.088549	5.282483
4.005763	296.662046	5.287488
4.108268	293.994879	5.292493
4.128380	302.486254	5.297498
4.172046	289.153928	5.302502
3.957924	288.526026	5.307507
4.016135	294.955061	5.312512
3.854115	303.253335	5.317517
4.309987	291.916396	5.322522
4.170537	308.639253	5.327526
3.884600	305.513716	5.332531
4.111863	306.158501	5.337536
4.074621	298.875107	5.342541
4.147079	304.235761	5.347546
3.753609	302.556960	5.352550
4.296068	301.453763	5.357555
4.571870	307.225676	5.362560
4.441138	299.014055	5.367565
4.477685	301.203945	5.372570
4.399226	297.505114	5.377574
4.293554	290.381071	5.382579
4.208690	297.563199	5.387584
4.336844	291.592301	5.392589
4.497799	299.084162	5.397594
4.106986	304.732078	5.402598
4.451733	300.527600	5.407603
4.405792	312.139180	5.412608
4.250661	302.159684	5.417613
4.266938	299.467978	5.422618
4.357864	302.816807	5.427622
4.404912	294.719874	5.432627
4.128829	301.238925	5.437632
4.154805	291.576080	5.442637
4.662112	299.501225	5.447642
4.400214	302.933461	5.452646
4.442606	297.077153	5.457651
4.137454	309.668709	5.462656
4.280419	306.644070	5.467661
4.226958	302.871744	5.472666
4.362485	308.295345	5.477670
4.545967	302.657509	5.482675
4.363332	309.759953	5.487680
4.288956	312.894079	5.492685
4.557271	308.356656	5.497690
4.803855	319.425995	5.502694
5.025740	307.261787	5.507699
4.466686	315.783232	5.512704
4.649369	317.741567	5.517709
4.622272	305.809112	5.522714
4.524175	307.744724	5.527718
4.789133	301.780997	5.532723
4.784775	299.649314	5.537728
4.355141	298.517137	5.542733
4.614821	296.252598	5.547738
4.514933	305.414380	5.552742
4.950862	306.969458	5.557747
4.566132	306.020112	5.562752
4.960983	304.670982	5.567757
4.574053	304.051002	5.572762
4.461523	315.141451	5.577766
4.516538	313.392822	5.582771
4.938194	323.140951	5.587776
4.808380	325.518095	5.592781
4.825796	315.834424	5.597786
5.074327	324.511704	5.602790
5.066929	321.817353	5.607795
4.847027	318.605604	5.612800
5.088101	316.271194	5.617805
4.820943	311.794996	5.622810
4.669809	312.675863	5.627814
4.878263	319.015077	5.632819
5.206934	321.896630	5.637824
4.635791	322.884020	5.642829
4.554198	320.739050	5.647834
4.636273	327.863561	5.652838
4.806548	318.001067	5.657843
4.929279	328.447464	5.662848
4.994814	328.370795	5.667853
5.021216	315.715006	5.672858
4.763671	328.008102	5.677862
4.914922	322.125345	5.682867
5.186424	321.500925	5.687872
4.810771	327.466021	5.692877
5.091495	322.537527	5.697882
4.784592	325.344033	5.702886
5.085169	321.206538	5.707891
4.755143	317.980298	5.712896
4.798909	322.874033	5.717901
5.150617	331.747221	5.722906
5.301722	356.368950	5.727910
4.957776	340.271743	5.732915
5.186363	354.127968	5.737920
5.373118	354.370943	5.742925
5.579546	344.411058	5.747930
5.151460	343.607662	5.752934
5.000740	333.374365	5.757939
5.076949	335.304988	5.762944
5.137391	350.772407	5.767949
5.807801	353.249586	5.772954
5.495544	347.049851	5.777958
5.149020	332.465305	5.782963
5.160898	328.287337	5.787968
5.204940	333.915012	5.792973
5.026644	330.196918	5.797978
5.122370	348.158168	5.802982
5.397392	353.351259	5.807987
5.446114	351.546659	5.812992
5.353733	357.907417	5.817997
5.400194	351.841652	5.823002
5.364796	357.579778	5.828006
5.510487	357.462156	5.833011
5.604784	356.855833	5.838016
5.281118	350.550308	5.843021
5.514139	350.824043	5.848026
5.503315	353.910318	5.853030
5.359093	348.035592	5.858035
5.342632	353.612583	5.863040
5.556145	350.905978	5.868045
5.593151	352.608592	5.873050
5.200503	351.423197	5.878054
5.479422	358.463289	5.883059
5.644583	348.759760	5.888064
5.700756	353.907833	5.893069
5.628269	349.619611	5.898074
5.475754	351.117618	5.903078
5.762867	355.483099	5.908083
5.411828	354.427266	5.913088
5.412282	356.812605	5.918093
5.884948	359.462940	5.923098
5.809915	357.908558	5.928102
5.843083	351.218449	5.933107
5.921391	360.308222	5.938112
5.593374	352.203222	5.943117
5.627664	354.409289	5.948122
5.717056	362.541897	5.953126
5.483193	359.610721	5.958131
5.820010	356.486290	5.963136
5.535372	355.258769	5.968141
5.664229	357.953142	5.973146
5.628447	367.247342	5.978150
5.555648	362.725051	5.983155
5.526534	350.754915	5.988160
5.101105	352.779461	5.993165
5.537860	355.043086	5.998170
5.200536	360.625744	6.003174
5.725679	375.308998	6.008179
5.670612	372.391110	6.013184
5.675500	378.550071	6.018189
5.852518	379.414650	6.023194
6.039476	385.254205	6.028198
5.714236	380.594045	6.033203
5.805004	373.977216	6.038208
5.586047	387.941113	6.043213
6.030314	384.398156	6.048218
5.757793	383.788834	6.053222
6.052319	382.971004	6.058227
5.821076	380.153310	6.063232
5.757642	375.971238	6.068237
6.228395	378.593401	6.073242
5.793010	386.814054	6.078246
5.859766	387.082040	6.083251
6.036367	381.495870	6.088256
5.707926	386.238768	6.093261
6.084093	376.837725	6.098266
5.814685	380.714065	6.103270
6.036310	383.213667	6.108275
6.092401	388.314306	6.113280
5.933576	388.288388	6.118285
6.219491	384.982055	6.123290
5.786640	386.207340	6.128294
6.138262	377.686467	6.133299
5.781115	364.419654	6.138304
5.651194	374.079685	6.143309
5.740418	375.264814	6.148314
5.570924	385.222074	6.153318
5.894796	383.349322	6.158323
5.810005	382.457674	6.163328
5.911070	390.170867	6.168333
5.801200	380.513306	6.173338
5.752743	385.801063	6.178342
5.894326	379.116209	6.183347
5.982965	380.399504	6.188352
6.090648	383.233218	6.193357
6.074862	382.745273	6.198362
6.055475	394.172441	6.203366
5.914648	378.078375	6.208371
6.010196	384.185258	6.213376
5.740078	379.412114	6.218381
6.320429	369.602802	6.223386
5.995476	367.796270	6.228390
5.549527	349.794563	6.233395
5.734342	353.277477	6.238400
5.864252	371.435906	6.243405
5.854376	366.628574	6.248410
5.852322	381.741924	6.253414
6.048740	371.233096	6.258419
6.042642	370.651896	6.263424
5.831854	365.708169	6.268429
5.837601	347.436822	6.273434
5.591209	356.921993	6.278438
5.984221	376.608663	6.283443
6.217457	374.955664	6.288448
5.918784	363.657068	6.293453
5.553316	358.889284	6.298458
6.094252	353.129340	6.303462
5.644362	345.796281	6.308467
6.014114	354.581250	6.313472
5.808413	369.245412	6.318477
5.693459	357.971998	6.323482
5.745319	365.961758	6.328486
6.066604	367.120245	6.333491
6.045218	369.047085	6.338496
6.120080	362.745943	6.343501
5.957371	349.062895	6.348506
6.059787	342.719506	6.353510
5.746711	344.157091	6.358515
6.030652	348.867909	6.363520
5.918508	355.541786	6.368525
6.100652	345.297784	6.373530
5.714391	357.262933	6.378534
5.567466	356.365142	6.383539
5.804103	357.122362	6.388544
5.293796	359.419549	6.393549
5.852662	360.009542	6.398554
5.780931	372.849534	6.403558
6.116519	362.328535	6.408563
6.540318	368.868353	6.413568
5.847869	371.412196	6.418573
5.388789	364.675338	6.423578
5.583131	367.315225	6.428582
6.091833	375.243351	6.433587
5.932067	365.960557	6.438592
5.743869	370.045710	6.443597
5.924269	366.502711	6.448602
5.603466	368.824177	6.453606
5.862803	373.890004	6.458611
6.049371	385.009857	6.463616
6.004964	383.697475	6.468621
6.145106	367.679894	6.473626
5.522775	359.405581	6.478630
5.370497	367.930155	6.483635
5.957253	375.090001	6.488640
6.054351	378.738436	6.493645
6.007531	373.253493	6.498650
6.058129	376.054965	6.503654
6.018865	371.742583	6.508659
5.965161	358.384237	6.513664
5.261203	356.310853	6.518669
5.903226	367.568587	6.523674
5.910890	383.816198	6.528678
6.181418	384.713674	6.533683
5.923142	374.041524	6.538688
5.986317	375.471150	6.543693
6.015034	361.827889	6.548698
5.792644	364.232107	6.553702
5.756973	355.945548	6.558707
5.930016	351.261599	6.563712
5.360285	352.634743	6.568717
5.683832	367.051988	6.573722
5.893238	369.132717	6.578726
5.682249	371.876841	6.583731
5.830169	364.944237	6.588736
5.828755	379.848680	6.593741
6.077118	378.367330	6.598746
6.043638	377.056411	6.603750
5.947746	388.723274	6.608755
6.110559	372.787579	6.613760
6.152487	384.145084	6.618765
6.255337	369.006493	6.623770
5.892890	359.052915	6.628774
5.856052	350.317294	6.633779
5.861538	346.494653	6.638784
5.376738	349.844546	6.643789
5.672377	358.584110	6.648794
5.973894	375.709765	6.653798
5.705055	375.663011	6.658803
5.958412	373.405774	6.663808
5.825441	383.382657	6.668813
5.920690	371.874029	6.673818
6.011769	374.492030	6.678822
5.854021	378.313019	6.683827
6.006995	377.555193	6.688832
6.122909	380.425589	6.693837
6.227781	372.170924	6.698842
5.893388	362.674879	6.703846
5.640630	356.823376	6.708851
5.494206	343.568061	6.713856
5.695285	364.872783	6.718861
5.960790	368.744929	6.723866
6.216828	377.196443	6.728870
5.697962	365.758124	6.733875
6.059344	348.216006	6.738880
5.748409	348.799057	6.743885
5.573429	344.659670	6.748890
5.802010	375.884677	6.753894
5.988719	365.510241	6.758899
5.942017	374.144928	6.763904
5.807611	378.632991	6.768909
5.988578	378.671226	6.773914
6.221430	375.857204	6.778918
5.621963	370.920208	6.783923
5.964088	364.681857	6.788928
5.867238	362.836646	6.793933
5.945641	357.594799	6.798938
5.856476	363.521629	6.803942
5.731366	363.775196	6.808947
6.019451	374.126273	6.813952
5.923437	363.324463	6.818957
5.868763	358.549418	6.823962
5.699648	354.250930	6.828966
5.709411	362.873657	6.833971
6.311535	372.511459	6.838976
5.591768	369.269962	6.843981
5.933387	360.184350	6.848986
5.904190	368.949185	6.853990
5.718333	360.423420	6.858995
6.004062	373.770897	6.864000
5.847171	379.306486	6.869005
6.213893	367.369620	6.874010
5.663930	364.557260	6.879014
5.739874	356.307107	6.884019
6.099268	361.809762	6.889024
5.775506	360.192868	6.894029
5.545115	354.388503	6.899034
6.013181	366.239625	6.904038
5.870651	371.763484	6.909043
5.973354	375.986842	6.914048
5.916592	373.673487	6.919053
5.928754	364.000099	6.924058
5.837907	354.434501	6.929062
5.734383	364.653558	6.934067
5.996106	378.874798	6.939072
5.988336	373.924769	6.944077
6.127934	368.638590	6.949082
5.907143	366.344447	6.954086
5.833522	360.253084	6.959091
5.491261	356.424473	6.964096
5.376726	371.096588	6.969101
5.927074	371.153241	6.974106
5.704713	385.497312	6.979110
5.889561	389.771157	6.984115
5.936919	380.411815	6.989120
5.983361	375.883610	6.994125
6.162779	379.876729	6.999130
5.987606	379.764772	7.004134
5.938930	384.634952	7.009139
5.985152	378.189570	7.014144
5.595229	376.051471	7.019149
6.028962	368.292928	7.024154
5.802366	370.751585	7.029158
5.699643	373.798388	7.034163
5.981746	375.114835	7.039168
5.943854	383.270434	7.044173
6.050699	375.138846	7.049178
5.650963	371.629224	7.054182
5.859425	372.169372	7.059187
6.237301	373.277921	7.064192
5.815957	373.773760	7.069197
5.441668	359.010020	7.074202
5.804522	365.948462	7.079206
5.406016	366.836210	7.084211
6.107799	365.920171	7.089216
5.759548	379.641604	7.094221
5.828365	372.145517	7.099226
5.892682	379.649295	7.104230
6.107220	381.109138	7.109235
5.948405	381.279369	7.114240
5.648254	373.793272	7.119245
6.109090	382.320468	7.124250
6.073857	385.157451	7.129254
6.010755	382.025680	7.134259
6.238787	373.425976	7.139264
5.715941	370.160147	7.144269
5.725491	358.851528	7.149274
5.936040	364.004041	7.154278
5.872398	366.238012	7.159283
5.989379	370.617331	7.164288
5.053607	364.647545	7.169293
5.764135	373.452232	7.174298
5.631848	377.775451	7.179302
5.782018	380.055227	7.184307
5.797800	366.138734	7.189312
5.604562	371.948895	7.194317
5.885120	377.210733	7.199322
5.833665	374.567525	7.204326
5.986646	379.583475	7.209331
6.157507	378.405253	7.214336
5.945105	378.403496	7.219341
6.289406	380.668864	7.224346
5.726172	379.329696	7.229350
5.901625	375.610297	7.234355
6.271444	371.835328	7.239360
5.886163	375.625305	7.244365
6.192999	375.469939	7.249370
6.023249	386.154894	7.254374
5.982137	374.395415	7.259379
5.908875	358.800205	7.264384
5.755405	352.781387	7.269389
5.668750	354.117282	7.274394
6.035489	368.499331	7.279398
5.586590	370.752157	7.284403
6.074290	370.976749	7.289408
5.787936	380.676959	7.294413
6.190421	369.636182	7.299418
5.884553	365.441240	7.304422
5.727879	362.399970	7.309427
5.904639	357.566746	7.314432
5.971021	358.584589	7.319437
5.915003	353.281415	7.324442
5.753652	356.381635	7.329446
6.206944	361.357150	7.334451
6.192651	354.668101	7.339456
5.563055	355.996783	7.344461
5.299309	359.907037	7.349466
5.810899	367.844202	7.354470
5.894497	379.423002	7.359475
6.017675	374.193161	7.364480
5.943669	383.869802	7.369485
6.413648	364.042377	7.374490
5.701102	369.499964	7.379494
5.632342	359.257054	7.384499
5.949563	355.686427	7.389504
5.684223	364.927783	7.394509
6.145394	373.641581	7.399514
6.179017	371.184442	7.404518
5.787268	363.054559	7.409523
5.791022	348.127565	7.414528
5.632732	359.674413	7.419533
5.654775	356.807796	7.424538
5.989679	366.294213	7.429542
5.775479	374.815776	7.434547
5.664399	361.580255	7.439552
6.015780	371.538666	7.444557
6.011443	376.863843	7.449562
5.980734	373.439132	7.454566
5.622002	366.341805	7.459571
5.859342	372.334860	7.464576
5.784402	377.667866	7.469581
5.670179	378.429096	7.474586
5.549943	382.218936	7.479590
5.932546	375.158040	7.484595
5.945271	373.571012	7.489600
5.914013	378.957328	7.494605
6.077803	386.565842	7.499610
5.839555	382.119926	7.504614
6.054110	385.259699	7.509619
6.187688	375.728749	7.514624
5.838471	379.168267	7.519629
6.141148	372.762051	7.524634
5.928958	362.908461	7.529638
5.722912	355.550087	7.534643
5.758236	356.974557	7.539648
6.217416	367.957043	7.544653
5.943405	358.758479	7.549658
5.763613	362.529114	7.554662
5.707391	363.420516	7.559667
5.953910	349.983795	7.564672
5.844746	359.055301	7.569677
6.036851	358.886160	7.574682
5.749258	358.424717	7.579686
5.986817	354.980387	7.584691
6.241260	341.767062	7.589696
5.944302	357.464137	7.594701
6.017802	355.813864	7.599706
6.121923	347.559328	7.604710
5.792867	355.459695	7.609715
5.939955	357.262228	7.614720
5.856217	358.977314	7.619725
5.849833	356.611826	7.624730
6.170980	355.046380	7.629734
5.808210	355.596374	7.634739
5.956631	348.518167	7.639744
5.862922	359.675314	7.644749
6.008215	352.211620	7.649754
6.012697	356.826747	7.654758
5.777160	348.884518	7.659763
5.924074	346.321159	7.664768
5.794153	353.839349	7.669773
5.795494	350.166047	7.674778
6.167119	347.706905	7.679782
5.664420	349.142377	7.684787
5.829090	349.420427	7.689792
5.471109	356.034505	7.694797
5.718290	351.557309	7.699802
5.852275	354.282520	7.704806
5.615459	357.470419	7.709811
5.655183	355.879189	7.714816
5.901727	350.750367	7.719821
5.561617	348.405203	7.724826
5.899880	358.887661	7.729830
5.747447	364.935073	7.734835
5.984140	364.293925	7.739840
5.973017	372.049887	7.744845
5.812319	361.201203	7.749850
6.130184	357.630476	7.754854
5.776805	358.039804	7.759859
5.755417	355.898112	7.764864
6.013628	363.431805	7.769869
5.953319	364.997713	7.774874
5.918321	358.795935	7.779878
5.631212	358.223686	7.784883
5.841550	359.083076	7.789888
5.563857	361.533868	7.794893
5.809880	375.229210	7.799898
5.999031	380.967182	7.804902
5.974704	383.849923	7.809907
6.122215	377.306514	7.814912
5.728080	376.735110	7.819917
5.899110	374.149010	7.824922
5.677859	361.848118	7.829926
5.887217	376.881092	7.834931
6.018421	373.168583	7.839936
6.071582	380.914541	7.844941
5.649066	372.827408	7.849946
5.712946	370.276974	7.854950
5.884230	377.466708	7.859955
5.942109	375.989706	7.864960
6.143822	380.175503	7.869965
5.996118	370.549148	7.874970
5.803886	362.347073	7.879974
5.610536	359.165983	7.884979
6.181009	371.469393	7.889984
5.760861	362.072120	7.894989
5.752228	357.134885	7.899994
5.720079	357.231611	7.904998
5.567404	376.620434	7.910003
6.206050	373.635665	7.915008
6.216082	376.149228	7.920013
6.156553	374.655706	7.925018
5.870605	356.761955	7.930022
5.827347	355.294374	7.935027
5.917492	355.707413	7.940032
5.856508	355.410001	7.945037
5.778561	357.541795	7.950042
5.841596	353.681719	7.955046
5.704024	348.862637	7.960051
5.859153	350.866394	7.965056
5.685009	352.554427	7.970061
5.804887	365.709425	7.975066
6.132850	371.080938	7.980070
5.924274	366.212795	7.985075
5.881683	355.269797	7.990080
5.681544	366.095511	7.995085
5.871687	366.420215	8.000090
6.376967	363.196789	8.005094
6.216008	359.725922	8.010099
6.197258	341.382467	8.015104
5.708447	353.610349	8.020109
5.729534	345.292110	8.025126
5.696725	355.205895	8.030144
5.424574	353.111873	8.035162
5.811610	349.138594	8.040179
5.860447	362.248955	8.045197
5.932935	360.113896	8.050214
5.996203	365.304513	8.055232
5.808810	365.949012	8.060250
5.964412	357.445553	8.065267
6.050750	363.942168	8.070285
6.105718	349.187281	8.075302
6.122647	346.824201	8.080320
5.667879	344.291579	8.085338
5.710647	347.311149	8.090355
6.009661	345.633102	8.095373
5.963039	348.338403	8.100390
5.776237	349.724385	8.105408
5.923160	367.126923	8.110426
6.300872	367.273204	8.115443
5.633897	364.925090	8.120461
5.802423	371.607717	8.125478
6.154657	367.355845	8.130496
6.282879	377.493866	8.135514
6.307905	364.921021	8.140531
6.029651	359.000157	8.145549
5.973892	355.401915	8.150566
6.154638	345.553401	8.155584
5.829765	354.651169	8.160602
6.054948	350.605265	8.165619
5.944467	354.507030	8.170637
5.930500	355.802990	8.175654
5.942357	361.446556	8.180672
5.530843	357.894236	8.185690
6.035901	365.789876	8.190707
6.160624	373.523841	8.195725
6.374494	369.877305	8.200742
6.339147	369.482015	8.205760
6.001231	374.529981	8.210778
5.795121	362.384425	8.215795
6.155926	370.696981	8.220813
6.129432	378.454492	8.225830
6.416525	372.407733	8.230848
6.173683	366.191034	8.235866
5.970772	351.066063	8.240883
5.912064	359.137834	8.245901
5.931341	365.755338	8.250918
6.465337	373.482383	8.255936
6.138779	373.126121	8.260954
6.162923	361.673669	8.265971
6.063454	364.923660	8.270989
6.051289	359.838635	8.276006
6.128898	365.626591	8.281024
6.132169	366.856755	8.286042
6.212418	364.587950	8.291059
6.109360	361.978475	8.296077
5.829640	360.273775	8.301094
6.385819	368.729472	8.306112
6.202934	381.513026	8.311130
6.423059	377.111316	8.316147
5.958485	367.688294	8.321165
5.886258	367.106252	8.326182
6.015635	375.789341	8.331200
6.195379	382.265109	8.336218
6.328995	385.463035	8.341235
6.365444	390.222356	8.346253
6.301104	386.688558	8.351270
6.266085	380.720349	8.356288
6.105238	388.539806	8.361306
6.064010	385.371619	8.366323
6.224574	379.126819	8.371341
6.483425	385.325197	8.376358
6.239613	379.124423	8.381376
6.315639	386.370539	8.386394
6.279037	378.225183	8.391411
6.245462	371.720293	8.396429
6.230458	378.081221	8.401446
6.536735	374.915733	8.406464
6.291360	373.549649	8.411482
6.077324	366.571111	8.416499
6.246886	372.464667	8.421517
6.016548	385.050495	8.426534
6.194436	383.268233	8.431552
6.195744	387.569145	8.436570
6.235841	379.904127	8.441587
5.942314	379.952956	8.446605
6.162604	381.202978	8.451622
6.248657	385.279267	8.456640
5.948696	388.364828	8.461658
5.961261	381.691813	8.466675
6.119427	376.823247	8.471693
5.898611	382.121213	8.476710
6.372722	389.936479	8.481728
6.202215	397.413479	8.486746
6.670982	398.179868	8.491763
6.619296	400.753429	8.496781
6.670633	394.329980	8.501798
6.289519	383.404491	8.506816
5.970398	394.035027	8.511834
6.345751	392.487094	8.516851
6.786459	396.369318	8.521869
6.317632	393.526469	8.526886
6.358942	388.562491	8.531904
6.426810	393.316921	8.536922
6.599506	391.661693	8.541939
6.321620	386.286689	8.546957
6.231904	390.333544	8.551974
6.589196	393.919503	8.556992
6.349200	392.909168	8.562010
6.217666	397.883984	8.567027
6.467432	401.521398	8.572045
6.525400	397.223821	8.577063
6.586897	394.203733	8.582080
6.791712	403.752360	8.587098
6.601940	395.047049	8.592115
6.620334	384.624218	8.597133
6.448541	383.133074	8.602151
6.743457	381.957409	8.607168
6.505907	382.253130	8.612186
6.320484	383.017237	8.617203
6.631259	381.113305	8.622221
6.499220	389.234374	8.627239
6.636348	377.287819	8.632256
6.401987	385.311214	8.637274
6.305465	384.590950	8.642291
6.373929	373.832142	8.647309
6.489189	381.898927	8.652327
6.638870	389.300826	8.657344
6.752553	389.194741	8.662362
6.215122	389.773826	8.667379
6.268313	387.335670	8.672397
6.258428	402.266543	8.677415
6.677795	393.905027	8.682432
6.634795	399.197402	8.687450
6.700796	392.298324	8.692467
6.685644	396.819540	8.697485
6.238804	410.057601	8.702503
6.716091	398.698666	8.707520
6.598210	398.808506	8.712538
6.521925	406.554848	8.717555
6.775408	397.843636	8.722573
6.469938	392.709598	8.727591
6.553614	393.204602	8.732608
6.558718	398.675670	8.737626
6.634728	402.747216	8.742643
6.649858	403.126666	8.747661
6.196310	406.485440	8.752679
6.590205	398.203623	8.757696
6.564673	403.180871	8.762714
6.582523	410.944115	8.767731
6.310097	399.992226	8.772749
5.914098	406.226301	8.777767
6.519788	413.330004	8.782784
6.984474	412.427691	8.787802
6.685368	420.641055	8.792819
7.103168	417.978878	8.797837
7.210012	418.943623	8.802855
6.569576	407.749240	8.807872
6.798974	403.822583	8.812890
6.981573	404.589349	8.817907
6.720839	398.463782	8.822925
6.850064	408.093605	8.827943
6.744152	404.780859	8.832960
6.716698	409.114656	8.837978
6.573734	409.591301	8.842995
7.012806	396.231325	8.848013
6.519607	399.814010	8.853031
6.703939	406.730863	8.858048
6.602524	398.270557	8.863066
6.598519	401.442579	8.868083
6.942478	411.821571	8.873101
6.335303	415.961621	8.878119
6.720377	422.755711	8.883136
6.575506	425.337473	8.888154
6.542253	430.369576	8.893171
7.429941	417.397307	8.898189
7.238145	433.041304	8.903207
7.131897	417.790778	8.908224
7.144941	406.740792	8.913242
6.650087	400.168863	8.918259
6.939737	403.115291	8.923277
7.012510	399.342402	8.928295
6.880065	400.581076	8.933312
6.885212	407.248131	8.938330
6.850088	411.535787	8.943347
6.994657	399.666949	8.948365
6.907743	398.323526	8.953383
6.763691	396.275823	8.958400
7.364877	397.431829	8.963418
6.679201	405.121579	8.968435
6.847957	395.315927	8.973453
7.193927	399.108767	8.978471
7.032593	400.206779	8.983488
6.952059	405.552334	8.988506
6.819147	408.365750	8.993523
6.877999	400.590510	8.998541
6.941454	406.049341	9.003559
6.943636	399.198063	9.008576
6.834455	402.850340	9.013594
6.826840	398.067538	9.018611
6.993041	398.502358	9.023629
6.883974	400.217050	9.028647
6.788046	402.368332	9.033664
6.719162	408.349515	9.038682
7.202764	429.458073	9.043699
7.292308	418.645466	9.048717
6.922680	412.953394	9.053735
6.811327	411.332923	9.058752
7.058556	418.978409	9.063770
7.237592	426.442022	9.068787
7.375921	421.497642	9.073805
7.164876	405.114786	9.078823
7.150618	404.855060	9.083840
6.683211	404.729001	9.088858
6.929172	411.061932	9.093875
7.352818	408.891127	9.098893
7.283317	402.641115	9.103911
6.929630	410.591587	9.108928
6.730451	407.236561	9.113946
6.901443	414.332210	9.118963
7.048342	420.245088	9.123981
7.108420	425.404663	9.128999
6.719893	420.539157	9.134016
7.087771	421.122450	9.139034
7.231195	423.940178	9.144051
7.147017	423.107542	9.149069
7.335231	426.536805	9.154087
7.005592	424.218207	9.159104
7.105353	422.249299	9.164122
7.105790	425.086134	9.169139
7.317379	416.813760	9.174157
7.232440	421.778172	9.179175
7.123113	422.303227	9.184192
7.440169	430.707826	9.189210
7.139226	438.744767	9.194227
7.603739	425.156757	9.199245
7.179276	430.609515	9.204263
7.109715	434.953029	9.209280
7.055774	422.588089	9.214298
7.144582	425.641528	9.219315
7.406801	423.398030	9.224333
7.354835	421.828268	9.229351
7.047959	423.567449	9.234368
7.385657	425.951006	9.239386
7.098489	423.537437	9.244403
7.280848	426.494264	9.249421
7.449347	439.216839	9.254439
7.375844	427.508161	9.259456
7.413769	424.185639	9.264474
7.394708	425.838985	9.269491
7.306593	415.782996	9.274509
7.301386	408.749838	9.279527
7.115210	411.230737	9.284544
7.341766	417.478334	9.289562
7.323621	425.635333	9.294579
7.197062	424.291769	9.299597
7.167733	430.023816	9.304615
7.228454	425.350281	9.309632
7.424910	416.354463	9.314650
7.370587	417.792403	9.319667
7.255983	424.168856	9.324685
7.648540	420.917346	9.329703
7.314275	424.642540	9.334720
7.628525	426.906678	9.339738
7.368566	430.342606	9.344755
7.518349	424.717977	9.349773
7.368830	423.983873	9.354791
7.206088	425.119973	9.359808
7.605069	426.973306	9.364826
7.658187	422.973110	9.369843
7.360868	419.273617	9.374861
7.500298	417.898107	9.379879
7.176552	418.753176	9.384896
7.183972	418.524787	9.389914
7.312020	424.311220	9.394931
7.328835	424.311731	9.399949
7.472459	421.815311	9.404967
7.616687	422.386091	9.409984
7.425959	417.515034	9.415002
7.588856	421.781329	9.420019
7.290469	416.797653	9.425037
7.279692	425.606724	9.430055
7.274612	428.150943	9.435072
7.643385	428.440621	9.440090
7.282013	427.395536	9.445107
7.259431	421.557914	9.450125
7.611720	416.132120	9.455143
7.476238	432.846582	9.460160
7.552032	422.818715	9.465178
7.220763	418.843655	9.470195
7.504059	423.173251	9.475213
7.439955	423.012799	9.480231
7.217677	426.531219	9.485248
7.452187	415.374167	9.490266
7.579527	434.972998	9.495283
7.561068	442.262249	9.500301
7.703175	446.219377	9.505319
7.706236	448.509878	9.510336
7.629565	434.801004	9.515354
7.920649	431.249726	9.520371
7.506693	424.876620	9.525389
7.237026	426.357556	9.530407
7.292036	437.807138	9.535424
7.672247	447.707159	9.540442
7.553792	455.800899	9.545459
7.835260	455.880119	9.550477
7.819189	450.057252	9.555495
7.833182	447.366428	9.560512
8.215146	443.718950	9.565530
7.662475	442.495375	9.570547
7.367118	425.683836	9.575565
7.696282	425.474777	9.580583
7.401998	449.686563	9.585600
7.996064	445.210837	9.590618
7.997323	452.175145	9.595635
7.612612	437.535976	9.600653
7.595468	439.416232	9.605671
7.703590	451.501307	9.610688
7.625572	446.685274	9.615706
7.644013	452.409890	9.620723
7.964151	458.286342	9.625741
8.300950	447.084943	9.630759
7.639559	438.254234	9.635776
7.640625	432.567554	9.640794
7.630889	440.148922	9.645811
7.410938	447.772490	9.650829
7.790782	440.455316	9.655847
7.366700	445.358935	9.660864
7.756577	444.903749	9.665882
7.852433	449.464497	9.670899
7.841370	455.424071	9.675917
7.899640	449.668522	9.680935
7.781011	458.323996	9.685952
7.905489	459.712011	9.690970
7.583703	448.095623	9.695987
7.583685	449.704983	9.701005
7.639674	446.587918	9.706023
7.275485	454.596846	9.711040
7.355311	459.371522	9.716058
8.010516	470.039744	9.721075
8.231035	481.738128	9.726093
8.228153	474.755072	9.731111
7.705239	464.457497	9.736128
7.600129	463.814303	9.741146
7.894428	471.357814	9.746163
7.936899	483.093387	9.751181
8.502499	470.796047	9.756199
7.991302	473.822998	9.761216
7.971800	467.808164	9.766234
8.028832	454.270953	9.771251
7.453967	452.769979	9.776269
8.201181	469.205038	9.781287
8.070217	474.318636	9.786304
7.748457	470.985838	9.791322
8.099986	480.760961	9.796339
8.115923	477.388206	9.801357
8.208624	466.672904	9.806375
7.837019	463.650812	9.811392
8.242672	468.406317	9.816410
8.174691	472.579188	9.821427
8.130476	455.722208	9.826445
7.978490	453.511639	9.831463
7.905665	461.175419	9.836480
7.923171	458.512447	9.841498
8.199026	462.978905	9.846515
7.679327	463.135528	9.851533
8.206234	468.380215	9.856551
8.238723	474.007982	9.861568
8.302257	466.273009	9.866586
8.429204	454.173359	9.871603
8.145423	453.958752	9.876621
8.191560	451.524841	9.881639
7.997826	457.579126	9.886656
7.723930	454.693294	9.891674
7.710005	460.820565	9.896691
7.880108	465.208819	9.901709
8.636291	465.845259	9.906727
8.285540	476.038976	9.911744
8.277546	469.877190	9.916762
8.412809	476.410409	9.921779
7.900028	469.140688	9.926797
7.964024	466.252736	9.931815
8.228872	473.712475	9.936832
8.278357	478.687531	9.941850
8.436746	466.538798	9.946867
8.316053	480.603405	9.951885
8.080521	477.285581	9.956903
8.298207	482.467969	9.961920
8.244120	477.875409	9.966938
8.506193	476.780587	9.971955
8.296055	472.685674	9.976973
8.466287	477.670331	9.981991
8.221981	460.910767	9.987008
8.164921	460.768153	9.992026
8.352069	460.988284	9.997043
8.095809	464.931705	10.002061
8.367093	465.716222	10.007079
8.342484	472.482604	10.012096
8.339743	475.263140	10.017114
8.245821	469.767954	10.022131
8.177213	482.890377	10.027149
8.556733	470.666189	10.032167
8.257982	473.461256	10.037184
8.250064	475.696669	10.042202
8.292468	474.317327	10.047219
8.169682	482.951371	10.052237
8.450983	475.671616	10.057255
8.047661	477.735073	10.062272
8.339697	476.556695	10.067290
8.368516	471.357964	10.072307
8.583470	473.669125	10.077325
8.796034	472.427384	10.082343
8.589820	477.581100	10.087360
8.661793	484.171510	10.092378
8.690532	481.910711	10.097395
8.568114	472.923488	10.102413
8.427398	461.850073	10.107431
8.579977	457.900652	10.112448
8.458700	460.096911	10.117466
8.094774	454.539632	10.122483
8.215515	470.453722	10.127501
8.200415	474.656229	10.132519
8.568389	481.891642	10.137536
8.330764	479.766984	10.142554
8.276809	471.277164	10.147571
8.496259	478.488365	10.152589
8.662895	467.584834	10.157607
8.490052	472.035952	10.162624
8.486747	478.937868	10.167642
8.599922	476.430404	10.172659
8.241830	482.926834	10.177677
8.460444	484.117166	10.182695
8.713161	477.798026	10.187712
8.199997	478.344934	10.192730
8.837692	491.338462	10.197747
8.608831	479.808566	10.202765
8.658084	476.484271	10.207783
8.381974	488.282072	10.212800
8.552545	486.179061	10.217818
8.748308	473.229278	10.222835
8.480875	477.291201	10.227853
8.710988	472.581813	10.232871
9.024355	469.348935	10.237888
8.681023	480.731183	10.242906
8.476399	477.575798	10.247923
8.288677	489.558645	10.252941
8.421768	481.200637	10.257959
8.678623	481.138528	10.262976
8.628856	496.116713	10.267994
8.675519	506.737700	10.273011
8.645383	499.765189	10.278029
8.683246	504.473830	10.283047
8.603376	499.512910	10.288064
8.830935	503.759690	10.293082
8.834911	501.013615	10.298099
9.048994	505.496013	10.303117
8.822431	501.337382	10.308135
8.811414	503.358695	10.313152
8.815743	500.334867	10.318170
9.298305	488.697355	10.323187
8.744318	479.414422	10.328205
8.555038	475.918992	10.333223
8.663019	482.090403	10.338240
8.606779	493.771928	10.343258
8.967952	504.779427	10.348275
8.861825	512.151781	10.353293
8.785072	503.949505	10.358311
9.014056	506.627698	10.363328
8.677729	504.000876	10.368346
9.145804	496.332286	10.373363
8.773273	507.766433	10.378381
8.734102	503.263058	10.383399
8.906612	512.883043	10.388416
8.945497	516.831012	10.393434
8.956127	503.771182	10.398451
8.971879	509.745534	10.403469
9.097560	508.514163	10.408487
8.844532	509.197287	10.413504
8.769466	513.648970	10.418522
8.773403	506.279849	10.423539
9.225475	506.894215	10.428557
8.729531	510.613043	10.433575
9.016599	502.275231	10.438592
8.760450	511.337134	10.443610
8.972316	507.002947	10.448627
8.824249	514.691087	10.453645
8.780459	509.806594	10.458663
9.090639	500.338611	10.463680
8.802536	507.698273	10.468698
9.236497	504.781113	10.473715
8.950664	502.256878	10.478733
8.825708	508.818000	10.483751
8.899614	502.993730	10.488768
8.430351	506.569554	10.493786
8.724315	501.320066	10.498803
9.270571	515.533311	10.503821
8.947584	510.162136	10.508839
9.096674	509.346824	10.513856
9.168518	521.538577	10.518874
9.442580	505.016986	10.523891
8.750462	505.273035	10.528909
9.053043	512.285122	10.533927
9.745596	513.026142	10.538944
9.170337	519.569020	10.543962
9.412649	501.149509	10.548979
8.973284	508.614769	10.553997
8.680428	512.655412	10.559015
9.434909	498.324797	10.564032
9.045225	503.242010	10.569050
9.008129	508.479852	10.574067
8.986002	510.922600	10.579085
9.219849	531.445343	10.584103
9.272351	522.692782	10.589120
9.457275	527.148168	10.594138
9.493590	527.903003	10.599155
9.222238	514.580969	10.604173
8.925854	515.845175	10.609191
9.290068	519.704625	10.614208
9.243312	522.249034	10.619226
9.113776	528.138720	10.624243
9.647642	519.901323	10.629261
9.192113	522.291636	10.634279
9.521917	518.245184	10.639296
9.177552	534.471578	10.644314
9.665816	533.445673	10.649331
9.532098	511.152733	10.654349
8.859190	513.166653	10.659367
9.271321	510.312850	10.664384
9.041153	526.612971	10.669402
9.100746	524.836490	10.674419
9.302009	524.612631	10.679437
9.294795	529.713289	10.684455
9.605036	525.467918	10.689472
9.398300	528.030926	10.694490
9.496318	528.268091	10.699507
9.485461	534.672609	10.704525
9.121484	531.134943	10.709543
9.460702	530.700265	10.714560
9.441099	530.873696	10.719578
9.416408	531.817902	10.724595
9.275393	528.179253	10.729613
9.267979	523.636217	10.734631
9.299792	519.715052	10.739648
9.071967	527.055869	10.744666
9.086337	535.580225	10.749683
9.720000	535.487851	10.754701
9.323387	535.454904	10.759719
9.613368	546.511382	10.764736
9.561832	559.470264	10.769754
9.711135	554.382133	10.774771
9.407877	538.190230	10.779789
9.248809	543.301912	10.784807
9.758078	556.261836	10.789824
9.512545	552.424869	10.794842
9.988903	555.765115	10.799859
9.775931	546.006191	10.804877
9.481808	541.892781	10.809895
9.493565	530.852386	10.814912
9.534832	546.065737	10.819930
9.447912	539.603804	10.824947
9.918763	546.476101	10.829965
9.384148	545.464293	10.834983
9.765798	541.381362	10.840000
9.648944	554.606021	10.845018
9.283478	558.534908	10.850035
9.543241	553.085610	10.855053
9.712028	556.902915	10.860071
9.664102	556.443310	10.865088
9.666416	558.090184	10.870106
9.931132	554.492497	10.875123
9.821384	553.291467	10.880141
9.625548	562.265113	10.885159
9.795074	553.917176	10.890176
9.599934	560.858459	10.895194
9.794985	560.020210	10.900211
9.553946	555.103303	10.905229
9.447525	559.645082	10.910247
9.936714	551.001234	10.915264
10.114753	553.838839	10.920282
9.740866	558.150874	10.925299
9.680047	556.976938	10.930317
9.529357	552.812792	10.935335
10.236887	544.762932	10.940352
9.950277	557.464935	10.945370
10.059799	554.358451	10.950387
10.249719	557.800096	10.955405
9.989075	562.170236	10.960423
9.932386	557.224625	10.965440
10.072948	554.230067	10.970458
9.992555	558.221863	10.975475
9.943392	546.345222	10.980493
9.984202	552.855307	10.985511
10.080920	538.169499	10.990528
9.565044	537.934224	10.995546
9.726121	543.065485	11.000563
10.546300	550.798541	11.005581
9.787243	545.148125	11.010599
9.905047	537.445695	11.015616
10.161835	538.377634	11.020634
9.939953	541.949661	11.025651
10.048749	529.180628	11.030669
9.826254	528.852341	11.035687
9.922099	543.053688	11.040704
9.907292	547.953570	11.045722
10.235844	557.953210	11.050739
10.144243	556.790378	11.055757
10.195721	552.010957	11.060775
9.856603	546.626504	11.065792
9.887117	547.227615	11.070810
10.093467	550.508917	11.075827
10.257394	555.712318	11.080845
10.104918	554.476917	11.085863
10.322543	550.810826	11.090880
10.265245	552.851973	11.095898
10.010985	543.386646	11.100915
9.892807	541.947098	11.105933
9.784460	552.690073	11.110951
10.396704	554.191492	11.115968
9.921385	549.781258	11.120986
10.156079	554.932617	11.126003
10.281570	552.161304	11.131021
9.981376	558.904357	11.136039
10.175129	554.894857	11.141056
10.219996	552.650472	11.146074
10.283661	559.614573	11.151091
10.220956	551.526848	11.156109
9.760447	555.325371	11.161127
10.038162	553.940943	11.166144
10.082112	547.332404	11.171162
9.835251	550.640089	11.176179
10.318541	554.862844	11.181197
10.153410	564.191457	11.186215
10.339212	561.978773	11.191232
10.250805	558.060539	11.196250
9.687443	555.980277	11.201267
10.103324	561.232811	11.206285
10.479011	584.892363	11.211303
10.387905	571.412840	11.216320
10.780743	581.932638	11.221338
10.574256	565.826624	11.226355
10.694156	563.977637	11.231373
10.255763	557.526240	11.236391
10.203879	554.937171	11.241408
10.280913	544.353644	11.246426
10.243634	548.887812	11.251443
10.745939	563.600224	11.256461
10.455832	557.649582	11.261479
10.372568	559.047860	11.266496
10.571844	554.677754	11.271514
9.764161	563.995961	11.276531
10.296908	571.893694	11.281549
10.277949	582.960426	11.286567
10.347984	580.390239	11.291584
10.841710	581.698684	11.296602
10.219707	581.060227	11.301619
10.531714	580.124875	11.306637
10.644286	581.177096	11.311655
10.313207	571.468104	11.316672
10.436867	576.845033	11.321690
10.554316	587.379310	11.326707
10.831093	585.307087	11.331725
10.650160	584.562089	11.336743
10.484963	583.123547	11.341760
10.567226	578.538133	11.346778
10.528051	577.247222	11.351795
11.052041	581.290083	11.356813
10.878587	582.042868	11.361831
10.617400	585.788274	11.366848
10.854298	583.116371	11.371866
10.709158	580.885786	11.376883
11.224320	576.725258	11.381901
10.490504	561.837395	11.386919
10.492664	559.517610	11.391936
10.748523	574.703886	11.396954
10.506519	580.263975	11.401971
10.815743	581.048902	11.406989
10.904398	578.213894	11.412007
10.625205	572.662319	11.417024
11.041563	574.613945	11.422042
10.354876	572.969431	11.427059
10.676910	576.346330	11.432077
10.803152	577.415357	11.437095
10.868181	571.608224	11.442112
11.115874	573.848032	11.447130
10.610904	581.929426	11.452147
10.484671	580.570022	11.457165
10.592639	584.633477	11.462183
10.671171	590.503411	11.467200
10.642481	578.500490	11.472218
10.663435	589.886047	11.477235
10.844501	583.682163	11.482253
10.612964	580.915942	11.487271
10.775719	593.806773	11.492288
10.603981	583.435518	11.497306
10.296552	582.208462	11.502323
10.485899	585.299921	11.507341
10.820067	592.834121	11.512359
11.002010	598.766848	11.517376
10.819379	591.373093	11.522394
10.679126	613.778161	11.527411
10.555482	604.888888	11.532429
10.726899	608.364981	11.537447
10.815378	600.111689	11.542464
10.733317	609.361123	11.547482
10.691337	606.839929	11.552499
10.687370	609.936245	11.557517
10.814942	610.269792	11.562535
11.094133	616.193696	11.567552
11.367227	621.490569	11.572570
10.824330	617.371695	11.577587
11.213936	613.839754	11.582605
11.325511	615.176144	11.587623
11.269164	621.941213	11.592640
10.956472	609.865728	11.597658
10.868793	609.406000	11.602675
10.981870	607.526513	11.607693
11.242132	614.548386	11.612711
10.920337	619.609689	11.617728
11.219234	615.618518	11.622746
11.208918	622.221791	11.627763
11.352239	631.877942	11.632781
11.571351	619.041178	11.637799
11.440604	607.688420	11.642816
11.152909	603.321540	11.647834
11.327516	605.332899	11.652851
11.231584	597.657410	11.657869
11.359379	600.537557	11.662887
11.164517	599.438135	11.667904
11.021949	595.695576	11.672922
11.190962	605.903112	11.677939
11.231076	599.273061	11.682957
11.245981	597.112227	11.687975
11.221543	604.815870	11.692992
11.440436	604.387302	11.698010
11.056042	605.983941	11.703027
11.364428	600.110508	11.708045
11.154196	601.967198	11.713063
11.295247	625.568666	11.718080
11.383715	629.092390	11.723098
11.520132	630.970847	11.728115
11.437338	624.375701	11.733133
11.322244	610.994553	11.738151
11.136224	627.477234	11.743168
11.381635	626.372375	11.748186
11.274580	631.965115	11.753203
11.185262	626.021057	11.758221
11.454943	636.007817	11.763239
11.518342	633.246158	11.768256
11.175198	632.703132	11.773274
11.244248	638.517755	11.778291
11.439012	637.616434	11.783309
11.671335	633.837588	11.788327
11.293326	630.144302	11.793344
11.546418	630.777031	11.798362
11.423443	633.800366	11.803379
11.347862	635.004956	11.808397
11.481412	632.358603	11.813415
11.243854	629.451306	11.818432
11.621028	625.138688	11.823450
11.451116	632.912328	11.828467
11.210538	627.496730	11.833485
11.320096	630.303985	11.838503
11.787486	641.544331	11.843520
11.593562	645.834678	11.848538
11.430194	641.375851	11.853555
11.498449	648.351895	11.858573
11.788239	654.239449	11.863591
11.798311	654.263099	11.868608
11.876762	657.731585	11.873626
11.777735	645.771127	11.878643
11.461695	642.740352	11.883661
11.670442	638.024781	11.888679
11.706344	650.291643	11.893696
11.681537	650.399616	11.898714
11.794767	653.556585	11.903731
11.656752	662.508656	11.908749
11.939535	658.901823	11.913767
11.796051	656.778265	11.918784
11.919463	652.609288	11.923802
11.872719	651.707699	11.928819
11.410882	648.750114	11.933837
11.748097	647.842392	11.938855
11.840689	654.660020	11.943872
11.921606	652.129153	11.948890
12.019125	646.313782	11.953907
11.729537	653.213003	11.958925
11.996848	651.697649	11.963943
11.747522	647.747647	11.968960
11.968295	648.688355	11.973978
12.140564	645.546840	11.978995
12.024779	642.951928	11.984013
11.958716	629.821899	11.989031
11.787612	640.407445	11.994048
11.876663	644.047842	11.999066
11.820767	660.810084	12.004083
11.965692	648.451893	12.009101
12.027229	648.773632	12.014119
11.655877	653.564960	12.019136
12.053293	645.957799	12.024154
12.152673	648.176528	12.029171
11.663155	656.766772	12.034189
12.074520	649.687594	12.039207
11.864523	653.851063	12.044224
12.220357	644.344339	12.049242
11.978559	644.145282	12.054259
11.528078	651.817452	12.059277
11.836754	644.511276	12.064295
11.290846	655.388709	12.069312
11.708964	658.952628	12.074330
12.448874	666.092339	12.079347
11.982528	658.471340	12.084365
12.528256	671.835912	12.089383
12.506369	674.224998	12.094400
12.261137	649.689769	12.099418
11.998328	646.417185	12.104435
11.929795	651.050915	12.109453
12.390391	659.638394	12.114471
12.305255	664.565036	12.119488
12.425894	652.690288	12.124506
11.842209	649.354058	12.129523
12.121944	664.880663	12.134541
12.159811	663.173822	12.139559
12.409538	672.889164	12.144576
12.636406	671.686207	12.149594
12.365594	662.832442	12.154611
11.881441	658.126921	12.159629
12.286813	657.262233	12.164647
12.263703	674.707324	12.169664
12.091167	683.667937	12.174682
12.470508	678.442972	12.179699
12.404484	675.067163	12.184717
12.538126	670.101354	12.189735
12.436525	669.915181	12.194752
12.566315	670.302030	12.199770
12.549160	669.424235	12.204787
12.380753	676.538120	12.209805
12.568991	669.455806	12.214823
12.638347	667.819797	12.219840
12.270597	654.717787	12.224858
12.562725	654.435600	12.229875
12.220134	664.110620	12.234893
12.752414	665.476182	12.239911
12.729995	664.226835	12.244928
12.625884	660.509832	12.249946
12.498421	649.424770	12.254963
11.965147	649.990592	12.259981
12.597930	647.616790	12.264999
12.955065	661.373622	12.270016
12.578788	659.125368	12.275034
12.226866	647.923781	12.280051
12.579810	664.076437	12.285069
13.035472	662.872571	12.290087
13.028687	658.140061	12.295104
12.257251	656.710698	12.300122
12.449293	645.225611	12.305139
12.332771	664.622830	12.310157
12.861371	666.080481	12.315175
12.492865	664.749323	12.320192
12.099199	666.505196	12.325210
12.545383	673.141551	12.330227
12.401949	670.490982	12.335245
12.413500	664.562762	12.340263
12.759150	672.650611	12.345280
12.488105	662.124364	12.350298
12.984450	671.242750	12.355315
12.568607	668.621972	12.360333
13.023117	667.156362	12.365351
12.954668	667.561454	12.370368
13.020351	675.408881	12.375386
12.858941	666.604350	12.380403
12.887323	675.530520	12.385421
12.638615	660.724830	12.390439
12.877578	669.315264	12.395456
12.690893	662.758369	12.400474
12.706940	672.844598	12.405491
12.655533	670.583630	12.410509
13.225397	673.511722	12.415527
12.836686	671.337983	12.420544
12.379376	676.849576	12.425562
13.167188	684.366831	12.430579
12.837608	686.611328	12.435597
13.277501	678.262262	12.440615
13.375403	682.156900	12.445632
13.309782	677.332563	12.450650
13.014628	671.209105	12.455667
12.739902	673.814276	12.460685
13.236993	662.205947	12.465703
13.264901	665.455094	12.470720
13.009424	666.110204	12.475738
12.887704	668.331803	12.480755
12.954679	670.173741	12.485773
12.778763	670.078031	12.490791
12.994217	662.638044	12.495808
13.125559	685.568941	12.500826
13.158372	678.580247	12.505843
13.363636	682.972548	12.510861
13.153455	672.540957	12.515879
12.998245	665.013518	12.520896
13.122871	686.629537	12.525914
13.238649	689.180222	12.530931
13.398271	691.459002	12.535949
12.961601	679.194497	12.540967
13.104195	681.545352	12.545984
13.101034	690.081979	12.551002
13.653397	694.672696	12.556019
13.200545	693.828023	12.561037
13.538486	692.541502	12.566055
13.386549	681.889405	12.571072
13.152260	679.278226	12.576090
13.435788	662.429980	12.581107
12.898564	679.226156	12.586125
13.231000	694.507905	12.591143
13.344692	693.963174	12.596160
13.492265	695.761009	12.601178
13.334860	684.929887	12.606195
13.506308	691.126202	12.611213
13.610949	686.458384	12.616231
13.647857	692.438970	12.621248
13.010276	688.741906	12.626266
13.439792	684.903946	12.631283
13.523236	688.860795	12.636301
13.213600	686.908264	12.641319
13.377868	685.023955	12.646336
13.274539	691.925749	12.651354
13.543507	689.876820	12.656371
13.449018	699.617369	12.661389
13.598537	692.392756	12.666407
13.636559	690.802649	12.671424
13.201418	693.432798	12.676442
13.416624	685.421659	12.681459
13.461931	693.199685	12.686477
13.404072	694.010214	12.691495
13.748268	689.620667	12.696512
13.578293	693.882052	12.701530
13.824574	692.754963	12.706547
13.555381	694.551417	12.711565
13.470627	696.148747	12.716583
13.833527	699.232138	12.721600
13.537471	696.835694	12.726618
13.437365	692.587904	12.731635
13.634655	690.701608	12.736653
13.604173	690.829399	12.741671
13.733098	686.751071	12.746688
13.410320	698.900248	12.751706
13.871358	706.184377	12.756723
13.607151	708.693244	12.761741
13.861523	713.611220	12.766759
14.403425	710.917055	12.771776
13.893598	708.178364	12.776794
13.544310	698.326976	12.781811
13.612813	697.543136	12.786829
13.645184	705.118061	12.791847
13.837879	717.123879	12.796864
13.993178	720.353203	12.801882
14.042052	715.653035	12.806899
14.005786	717.305932	12.811917
14.018237	713.854783	12.816935
14.000427	687.785133	12.821952
13.536036	699.542963	12.826970
13.526083	700.077799	12.831987
13.560509	712.303909	12.837005
13.569657	719.304962	12.842023
13.797891	711.099285	12.847040
13.859974	716.315435	12.852058
14.478553	709.876136	12.857075
14.559574	716.970136	12.862093
14.314673	722.114167	12.867111
14.491045	717.397304	12.872128
13.902053	720.385916	12.877146
14.153482	716.017118	12.882163
14.470304	717.646596	12.887181
14.237404	710.333200	12.892199
14.217352	695.371962	12.897216
14.039470	693.862805	12.902234
13.997703	699.890355	12.907251
13.901185	701.290708	12.912269
14.421710	709.291387	12.917287
14.572416	703.754886	12.922304
14.178476	706.050430	12.927322
14.106341	696.515640	12.932339
14.073774	687.776242	12.937357
14.127816	706.938676	12.942375
14.281998	705.564003	12.947392
14.053782	708.543778	12.952410
14.318442	703.573339	12.957427
14.458680	708.073597	12.962445
14.581915	713.239200	12.967463
14.418394	705.233372	12.972480
14.102033	714.377333	12.977498
14.345841	710.075993	12.982515
14.339070	712.794079	12.987533
14.464515	710.761182	12.992551
14.027585	715.897241	12.997568
14.073094	711.301737	13.002586
14.541646	712.964395	13.007603
14.653234	712.997485	13.012621
14.473892	716.758577	13.017639
14.594358	712.927705	13.022656
14.678457	718.781035	13.027674
14.466083	710.167448	13.032691
14.482605	704.771755	13.037709
14.688415	717.905273	13.042727
14.768334	707.112924	13.047744
14.370947	721.432232	13.052762
14.453682	716.546917	13.057779
14.644889	714.645788	13.062797
14.456996	725.035190	13.067815
14.630318	716.585604	13.072832
14.625437	721.509234	13.077850
14.358121	717.199112	13.082867
14.551843	709.412206	13.087885
14.269153	714.047739	13.092903
14.388043	711.659269	13.097920
14.288351	726.888410	13.102938
14.542918	723.510012	13.107955
14.746425	722.869248	13.112973
14.482808	718.426010	13.117991
14.633807	725.341866	13.123008
14.634862	736.989384	13.128026
15.002669	729.623476	13.133043
15.021865	734.909422	13.138061
14.638530	723.472845	13.143079
14.592876	721.886295	13.148096
14.515159	738.260700	13.153114
14.928450	737.814485	13.158131
14.958578	735.982613	13.163149
14.792181	741.638274	13.168167
15.153835	742.945204	13.173184
14.835661	744.812403	13.178202
15.154927	732.152463	13.183219
15.277219	721.893133	13.188237
14.797642	715.072562	13.193255
14.869346	710.450890	13.198272
14.660208	718.448418	13.203290
14.573256	718.881637	13.208307
15.253293	728.239688	13.213325
15.165551	732.605040	13.218343
15.351554	729.786409	13.223360
14.685462	724.108838	13.228378
14.844063	727.148306	13.233395
15.223112	734.489392	13.238413
15.069822	736.797963	13.243431
15.147805	737.571565	13.248448
14.871534	742.619504	13.253466
15.100441	739.055756	13.258483
15.387749	735.385089	13.263501
15.027680	743.456619	13.268519
15.045258	734.239190	13.273536
14.921041	738.887925	13.278554
15.149371	741.607280	13.283571
14.961874	731.752772	13.288589
15.212645	740.243575	13.293607
15.453602	742.503387	13.298624
15.019932	740.901511	13.303642
15.234881	743.452542	13.308659
15.526438	742.826470	13.313677
15.143058	743.018673	13.318695
15.003997	734.822836	13.323712
15.105778	740.578750	13.328730
14.952692	737.563612	13.333747
15.293757	738.371990	13.338765
15.158474	741.854836	13.343783
15.305869	738.881274	13.348800
15.089434	740.098335	13.353818
15.346499	760.365271	13.358835
15.623259	753.426926	13.363853
15.412979	757.934436	13.368871
15.447309	754.325242	13.373888
15.753794	759.323477	13.378906
15.592789	757.183701	13.383923
15.619468	741.091716	13.388941
15.543503	745.199625	13.393959
15.391079	734.446590	13.398976
15.403971	740.800149	13.403994
15.515333	766.078950	13.409011
15.699331	765.131963	13.414029
15.204740	768.247892	13.419047
15.799919	763.734046	13.424064
15.687811	756.345020	13.429082
15.758384	767.451575	13.434099
15.861488	758.378604	13.439117
15.667185	747.389091	13.444135
15.832280	748.556217	13.449152
15.763769	739.465796	13.454170
15.272474	740.050330	13.459187
15.812778	739.275080	13.464205
15.933702	753.980760	13.469223
15.751239	749.660574	13.474240
15.518026	748.096913	13.479258
15.542389	757.156290	13.484275
15.629484	758.726869	13.489293
15.537621	764.923182	13.494311
15.733436	762.784652	13.499328
15.846358	762.927984	13.504346
15.642942	765.891284	13.509363
15.857818	757.476233	13.514381
15.715590	763.093426	13.519399
15.580405	762.959816	13.524416
15.791118	765.861793	13.529434
15.813584	766.319002	13.534451
15.709677	761.762527	13.539469
16.023579	770.521218	13.544487
15.724485	760.728250	13.549504
15.932934	756.618590	13.554522
15.965838	757.784208	13.559539
16.298232	763.116071	13.564557
16.025289	763.855952	13.569575
15.880172	758.150904	13.574592
16.051311	762.406530	13.579610
16.098630	771.077343	13.584627
16.293168	757.385952	13.589645
15.976258	761.424085	13.594663
16.033594	757.113897	13.599680
16.299187	756.908421	13.604698
16.111433	772.574177	13.609715
16.494354	755.716679	13.614733
16.377106	761.386784	13.619751
16.266288	763.385797	13.624768
16.103953	758.134696	13.629786
15.911687	755.466472	13.634803
16.281645	751.069743	13.639821
16.020112	759.340527	13.644839
16.270637	772.814252	13.649856
16.499635	772.062223	13.654874
16.114602	782.397148	13.659891
16.523979	775.466549	13.664909
16.485276	785.624480	13.669927
16.062776	775.569859	13.674944
16.621368	777.338421	13.679962
16.323008	774.409009	13.684979
16.553173	765.126909	13.689997
16.457258	771.516354	13.695015
16.383217	768.356363	13.700032
16.597184	769.026746	13.705050
16.440089	776.378743	13.710067
16.388278	770.435108	13.715085
16.723962	777.950216	13.720103
16.373747	774.217860	13.725120
16.458326	777.189969	13.730138
16.469903	772.066417	13.735155
16.818274	777.932268	13.740173
16.399988	787.019554	13.745191
16.495791	784.640980	13.750208
16.795799	780.154152	13.755226
16.546462	783.692633	13.760243
16.770112	774.831252	13.765261
16.804317	779.594183	13.770279
16.544103	780.736014	13.775296
16.525378	771.669381	13.780314
16.556545	773.532684	13.785331
16.636888	771.509958	13.790349
16.750111	783.023281	13.795367
16.525958	775.307719	13.800384
16.736629	779.579285	13.805402
16.502033	768.170012	13.810419
16.690964	772.747909	13.815437
16.505636	778.002598	13.820455
16.452090	778.522133	13.825472
16.607386	769.579882	13.830490
16.156139	771.707636	13.835507
16.741756	781.194022	13.840525
16.603491	794.914483	13.845543
16.933777	795.699297	13.850560
17.552449	788.881269	13.855578
17.079811	799.804184	13.860595
16.923468	787.483335	13.865613
16.986879	794.532772	13.870631
16.976654	792.618817	13.875648
17.110576	787.100681	13.880666
17.230773	788.940656	13.885683
17.142250	771.354993	13.890701
16.786156	770.189148	13.895719
16.590847	781.939849	13.900736
17.148460	781.821447	13.905754
17.167259	797.947357	13.910771
17.047902	790.521577	13.915789
17.145532	796.246598	13.920807
17.036642	790.113033	13.925824
16.862401	792.216595	13.930842
17.133502	791.685223	13.935859
16.968895	790.120343	13.940877
17.438069	795.257356	13.945895
17.522917	794.912767	13.950912
17.352539	793.137353	13.955930
17.101067	789.616831	13.960947
17.478840	796.096631	13.965965
17.691396	798.524969	13.970983
17.337912	788.929796	13.976000
17.342066	780.913606	13.981018
17.301359	789.096374	13.986035
17.231207	788.627601	13.991053
17.663451	791.750704	13.996071
17.178379	787.786884	14.001088
17.673488	786.150847	14.006106
17.538654	794.932080	14.011123
17.566229	790.512912	14.016141
17.757052	787.248566	14.021159
17.389953	793.342579	14.026176
17.371495	786.948790	14.031194
17.442353	796.632091	14.036211
17.432633	805.034098	14.041229
17.315126	791.129341	14.046247
17.504339	802.198511	14.051264
17.770203	792.907682	14.056282
17.400874	793.842447	14.061299
17.356032	786.998342	14.066317
17.532808	787.889105	14.071335
17.224747	791.323125	14.076352
17.437861	788.358256	14.081370
17.653298	792.932032	14.086387
17.560663	785.921804	14.091405
17.474087	791.157966	14.096423
17.363966	791.121437	14.101440
17.731945	810.566453	14.106458
17.745251	818.441032	14.111475
17.668771	814.599778	14.116493
18.002992	823.550986	14.121511
17.628721	814.706942	14.126528
18.166786	807.951949	14.131546
17.897481	812.310876	14.136563
17.838557	808.195497	14.141581
17.853373	812.623793	14.146599
17.650909	815.173554	14.151616
17.974562	815.123135	14.156634
18.080191	814.680639	14.161651
18.191948	816.304187	14.166669
18.378922	808.556157	14.171687
17.578627	805.168417	14.176704
17.999474	804.370739	14.181722
18.035360	809.619397	14.186739
17.937663	816.580321	14.191757
18.021009	808.554944	14.196775
18.153615	819.774946	14.201792
18.334981	812.983971	14.206810
18.062138	818.646763	14.211827
17.968632	817.010852	14.216845
18.205071	807.153412	14.221863
18.087769	811.646458	14.226880
18.205827	805.581692	14.231898
17.944568	813.511640	14.236915
18.139322	813.285636	14.241933
18.133224	806.965652	14.246951
17.871945	805.958606	14.251968
17.939464	807.358672	14.256986
18.062581	811.694369	14.262003
17.844220	810.131546	14.267021
18.225277	814.748966	14.272039
18.116690	815.917684	14.277056
18.382332	827.375747	14.282074
18.505498	837.600022	14.287091
18.317891	832.876684	14.292109
18.612393	836.841729	14.297127
18.549567	828.561397	14.302144
18.334264	812.759482	14.307162
18.426469	828.264936	14.312179
18.371528	838.198214	14.317197
18.896370	826.689596	14.322215
18.587059	824.067986	14.327232
18.554943	816.776932	14.332250
18.417457	815.258319	14.337267
18.312715	820.491006	14.342285
18.788252	817.182326	14.347303
18.386137	835.383999	14.352320
18.953460	834.023885	14.357338
18.518354	835.704177	14.362355
18.574456	831.940103	14.367373
18.364211	832.310473	14.372391
18.561334	837.821206	14.377408
18.639045	834.653355	14.382426
18.713800	833.978987	14.387443
18.640991	841.816492	14.392461
19.027891	831.118280	14.397479
18.596532	844.969618	14.402496
18.829778	837.223839	14.407514
18.841550	835.344323	14.412531
18.657435	838.383523	14.417549
19.035714	842.149338	14.422567
18.747577	843.346012	14.427584
18.742339	843.425693	14.432602
18.979207	835.063985	14.437619
18.934867	830.419324	14.442637
19.093802	832.799213	14.447655
18.779621	840.772126	14.452672
18.897251	826.802329	14.457690
19.118380	827.903934	14.462707
18.635174	836.871968	14.467725
18.964719	832.948559	14.472743
18.668531	845.118941	14.477760
18.848336	832.900354	14.482778
19.029470	842.178357	14.487795
19.274566	850.701654	14.492813
19.273001	845.999838	14.497831
18.965743	842.052501	14.502848
19.059012	845.386177	14.507866
19.316425	858.770534	14.512883
19.354563	849.470952	14.517901
19.376579	844.629769	14.522919
19.387542	840.093257	14.527936
19.191834	840.669641	14.532954
19.378900	844.493629	14.537971
19.153643	837.270506	14.542989
19.080815	836.382436	14.548007
19.289083	839.054439	14.553024
18.865992	834.658091	14.558042
19.434133	842.777646	14.563059
19.434533	849.322532	14.568077
19.283733	858.185176	14.573095
19.526468	860.744520	14.578112
19.494683	856.426094	14.583130
19.517095	858.271834	14.588147
19.509230	866.386410	14.593165
19.713183	848.619437	14.598183
19.610757	853.280587	14.603200
19.624959	846.755462	14.608218
19.507251	853.555418	14.613235
19.520966	859.331393	14.618253
19.652022	850.569595	14.623271
19.767705	851.182702	14.628288
19.562184	845.521743	14.633306
19.855061	842.055310	14.638323
19.712349	849.916325	14.643341
19.672507	827.084522	14.648359
19.305130	835.223501	14.653376
19.676420	843.351616	14.658394
19.657647	848.274288	14.663411
19.734814	851.967070	14.668429
19.701248	852.063785	14.673447
19.592028	857.275090	14.678464
19.644381	859.513790	14.683482
19.925205	857.923733	14.688499
19.569060	854.712977	14.693517
19.725921	849.484734	14.698535
19.859146	847.501102	14.703552
19.489141	850.635516	14.708570
19.747099	850.749957	14.713587
19.535191	853.373775	14.718605
20.050421	849.553992	14.723623
20.143376	861.423962	14.728640
19.962522	865.633434	14.733658
20.080343	852.566126	14.738675
19.865835	856.970180	14.743693
19.960715	870.761695	14.748711
19.980861	869.874926	14.753728
20.156411	871.299203	14.758746
20.277697	871.605332	14.763763
20.018433	876.180456	14.768781
20.400076	867.240783	14.773799
20.134767	868.730543	14.778816
20.234783	871.394159	14.783834
20.196550	872.703401	14.788851
20.138875	878.698776	14.793869
20.499658	873.006440	14.798887
20.232382	868.813037	14.803904
20.357694	873.463980	14.808922
20.489437	871.666764	14.813939
20.464690	878.490125	14.818957
20.474880	873.363604	14.823975
20.454157	854.826894	14.828992
19.992814	851.695633	14.834010
20.405298	862.291432	14.839027
20.647814	865.504047	14.844045
20.685919	865.248785	14.849063
20.330173	852.472955	14.854080
20.139610	857.289836	14.859098
20.331072	860.232695	14.864115
20.415396	870.557708	14.869133
20.404228	870.742452	14.874151
20.450931	875.090062	14.879168
20.472681	873.988454	14.884186
20.631115	868.393895	14.889203
19.997649	866.892540	14.894221
20.266729	868.273853	14.899239
20.307907	863.581156	14.904256
20.225050	870.353602	14.909274
21.119329	878.952559	14.914291
20.822948	877.610155	14.919309
20.589848	870.463977	14.924327
21.068544	874.955761	14.929344
20.682897	877.524584	14.934362
20.882971	882.694052	14.939379
20.861459	887.964292	14.944397
20.957011	880.321982	14.949415
21.173089	862.247001	14.954432
20.887081	865.166374	14.959450
21.270459	857.460325	14.964467
20.824441	861.076780	14.969485
20.350925	856.000329	14.974503
20.870089	868.466648	14.979520
21.030611	875.583046	14.984538
20.592364	884.392629	14.989555
20.671775	883.597617	14.994573
20.999439	885.582021	14.999591
21.019825	888.273816	15.004608
21.075882	896.785543	15.009626
20.821729	887.288458	15.014643
20.783147	894.852421	15.019661
20.997267	889.457464	15.024679
21.055884	884.938767	15.029696
20.651989	898.568125	15.034714
21.284554	894.764777	15.039731
21.593594	906.212979	15.044749
21.582279	897.927751	15.049767
21.379389	885.932810	15.054784
21.216434	887.684340	15.059802
20.985461	888.253593	15.064819
21.215765	896.230118	15.069837
21.477595	907.414277	15.074855
21.422727	889.413012	15.079872
21.319955	898.397583	15.084890
21.672695	905.162181	15.089907
21.723833	899.571695	15.094925
21.297825	895.655457	15.099943
21.371983	885.488732	15.104960
21.329487	895.751457	15.109978
21.414822	896.359823	15.114995
21.721338	918.200263	15.120013
21.498401	920.437652	15.125031
21.693544	907.897896	15.130048
21.730781	912.370062	15.135066
21.622661	914.737894	15.140083
21.967092	907.129404	15.145101
21.358284	890.713359	15.150119
21.882126	897.678527	15.155136
21.307563	911.732090	15.160154
21.729813	905.152879	15.165171
21.721169	905.419279	15.170189
21.440410	913.440669	15.175207
21.853250	912.429643	15.180224
21.929236	911.859219	15.185242
21.877756	910.806879	15.190259
21.586328	921.357679	15.195277
21.469086	914.610002	15.200295
21.624930	912.490301	15.205312
21.450680	908.831502	15.210330
21.657001	909.843900	15.215347
21.736997	910.232197	15.220365
21.925198	925.470331	15.225383
21.946304	924.160542	15.230400
22.142987	932.053956	15.235418
22.110388	924.018178	15.240435
22.373716	924.084446	15.245453
21.854384	918.084167	15.250471
22.023762	918.818302	15.255488
21.766866	932.118692	15.260506
22.063014	928.314068	15.265523
22.156786	927.011899	15.270541
22.020892	927.859834	15.275559
22.318254	930.391749	15.280576
22.464564	938.577025	15.285594
22.452044	936.549805	15.290611
22.571476	932.018473	15.295629
22.317577	930.988180	15.300647
22.692917	923.974462	15.305664
22.434756	924.626843	15.310682
22.160414	920.453462	15.315699
22.375893	919.823451	15.320717
22.250821	925.744129	15.325735
22.325089	924.763727	15.330752
22.200471	933.196307	15.335770
22.166872	934.855119	15.340787
22.379630	927.270278	15.345805
22.411648	933.630395	15.350823
22.627804	926.518387	15.355840
22.697885	931.348354	15.360858
22.616252	923.487465	15.365875
22.540981	919.147392	15.370893
22.492887	929.704491	15.375911
22.485036	923.469944	15.380928
22.319781	926.398927	15.385946
22.700165	922.335041	15.390963
22.617729	925.273220	15.395981
22.599942	933.780683	15.400999
22.897249	928.514771	15.406016
22.698208	927.627413	15.411034
22.817613	932.342406	15.416051
22.540184	926.004666	15.421069
22.507456	935.966097	15.426087
22.905532	946.961814	15.431104
22.804230	954.500854	15.436122
22.851983	952.262280	15.441139
23.059055	946.432910	15.446157
22.909479	956.049635	15.451175
23.042888	944.295779	15.456192
23.162265	948.212378	15.461210
22.935668	949.857060	15.466227
23.119303	948.796513	15.471245
23.167670	945.756286	15.476263
23.336426	944.530801	15.481280
22.983566	954.185487	15.486298
23.091985	949.879922	15.491315
23.275207	944.729596	15.496333
22.977023	949.121454	15.501351
23.169303	942.527543	15.506368
22.979971	940.174407	15.511386
23.334064	931.415714	15.516403
23.687572	941.351726	15.521421
22.944880	948.820215	15.526439
23.304268	942.080368	15.531456
22.946950	947.185163	15.536474
23.323946	947.334718	15.541491
23.632835	943.916264	15.546509
23.130630	941.059586	15.551527
23.052368	943.129289	15.556544
23.277142	949.560384	15.561562
23.253825	943.050532	15.566579
23.272932	941.463347	15.571597
23.257073	955.732908	15.576615
23.786608	952.175959	15.581632
23.882453	961.476770	15.586650
23.916913	951.199426	15.591667
23.585012	939.880930	15.596685
23.254018	941.283095	15.601703
23.269273	945.048650	15.606720
23.452152	952.552911	15.611738
23.590288	960.202994	15.616755
24.045024	957.484495	15.621773
23.695435	970.641559	15.626791
23.946997	969.450516	15.631808
24.134040	969.269891	15.636826
23.886960	959.512895	15.641843
24.393225	955.050714	15.646861
23.971999	947.542482	15.651879
23.875672	938.292191	15.656896
23.963716	936.050502	15.661914
23.777907	941.611420	15.666931
24.154965	932.451527	15.671949
24.235641	930.624387	15.676967
24.281558	927.783356	15.681984
23.591787	933.066138	15.687002
23.987567	937.116421	15.692019
24.086038	933.471959	15.697037
23.585252	937.179005	15.702055
24.385203	947.443135	15.707072
24.315300	938.993444	15.712090
23.923363	936.173247	15.717107
23.986737	944.371439	15.722125
24.120878	953.600013	15.727143
24.415951	959.433198	15.732160
24.002671	959.330262	15.737178
24.424481	969.246189	15.742195
24.344593	961.527019	15.747213
24.220272	962.524630	15.752231
24.107957	963.662380	15.757248
24.101745	962.483070	15.762266
24.497227	958.154899	15.767283
24.379970	953.786642	15.772301
23.961833	957.840579	15.777319
24.135463	959.905778	15.782336
24.430983	957.366701	15.787354
24.550871	957.269114	15.792371
24.622892	955.654754	15.797389
24.083675	967.396008	15.802407
24.392427	961.475064	15.807424
24.760004	975.126375	15.812442
24.562555	985.798278	15.817459
25.076989	973.764176	15.822477
25.068364	987.032263	15.827495
24.825595	958.816618	15.832512
24.966212	958.087810	15.837530
24.662832	954.272386	15.842547
24.711385	947.868104	15.847565
24.851431	951.699437	15.852583
24.914843	951.913594	15.857600
24.881455	954.004713	15.862618
24.388150	964.331354	15.867635
24.593815	958.969250	15.872653
24.722293	969.265356	15.877671
24.983537	982.270520	15.882688
24.837346	978.702011	15.887706
24.794782	982.258829	15.892723
25.118900	981.943255	15.897741
25.095968	985.992471	15.902759
25.393372	977.122662	15.907776
25.124707	985.524046	15.912794
25.049891	984.759353	15.917811
25.302696	980.232488	15.922829
25.321231	990.476297	15.927847
25.465314	979.396087	15.932864
25.142465	983.097529	15.937882
24.823422	987.309610	15.942899
25.027254	974.285625	15.947917
25.028963	985.478776	15.952935
24.952513	983.067035	15.957952
25.131275	976.153330	15.962970
25.378030	983.300526	15.967987
25.557050	976.724445	15.973005
25.362782	987.660937	15.978023
25.295499	980.807628	15.983040
25.351210	978.899166	15.988058
25.026957	979.637577	15.993075
25.166209	965.392910	15.998093
25.387502	991.828855	16.003111
25.604800	992.697541	16.008128
25.808994	997.333079	16.013146
25.691713	990.446526	16.018163
25.461018	988.740443	16.023181
25.624228	991.769772	16.028199
25.710855	989.159073	16.033216
25.802021	987.942511	16.038234
25.473823	999.133387	16.043251
25.938073	995.564504	16.048269
26.192573	993.634557	16.053287
25.965853	996.159718	16.058304
26.105516	994.345478	16.063322
25.677953	981.978361	16.068339
25.690948	974.661283	16.073357
25.744956	984.492475	16.078375
25.804196	992.410471	16.083392
25.697041	986.005173	16.088410
25.645490	991.718771	16.093427
26.035440	991.834752	16.098445
25.574175	989.372473	16.103463
25.479310	993.868383	16.108480
25.967482	992.684681	16.113498
25.490101	1003.220301	16.118515
25.990154	1006.702108	16.123533
26.242183	1015.271741	16.128551
26.182458	1017.455329	16.133568
26.192847	1012.997757	16.138586
26.039479	1009.247325	16.143603
26.458002	1011.637313	16.148621
26.439855	1013.596680	16.153639
26.123810	1019.932126	16.158656
26.559859	1008.430904	16.163674
26.484390	1007.691558	16.168691
26.538517	1010.232953	16.173709
26.568106	1018.887713	16.178727
26.512710	1016.261254	16.183744
27.001241	1009.662218	16.188762
26.605540	1020.342918	16.193779
26.734663	1007.336852	16.198797
26.541190	998.937929	16.203815
26.153535	986.476234	16.208832
26.199432	992.654334	16.213850
26.414388	1010.605479	16.218867
26.585307	999.502143	16.223885
26.743987	1005.823631	16.228903
26.779569	1006.341919	16.233920
26.759284	1010.867246	16.238938
26.800607	1010.374799	16.243955
26.757037	1010.599303	16.248973
26.714359	1013.742741	16.253991
26.654531	1012.925221	16.259008
26.824102	1012.640020	16.264026
26.498725	1022.034847	16.269043
27.135790	1008.201782	16.274061
26.856511	1010.040862	16.279079
26.802308	1008.446150	16.284096
26.684064	1005.621198	16.289114
26.671527	1013.673454	16.294131
26.881993	1015.600382	16.299149
27.637538	1024.079002	16.304167
27.183965	1024.181151	16.309184
27.071747	1014.220093	16.314202
26.860606	1011.447473	16.319219
27.264673	1007.913204	16.324237
26.980412	1007.960590	16.329255
26.943190	1027.336391	16.334272
27.532942	1028.620453	16.339290
27.419855	1034.075405	16.344307
27.439757	1023.844466	16.349325
27.130314	1018.897054	16.354343
27.490441	1031.000091	16.359360
27.907897	1024.203836	16.364378
27.190584	1024.482746	16.369395
27.409740	1018.433724	16.374413
27.388266	1013.794923	16.379431
27.222054	1017.560345	16.384448
27.728086	1031.537276	16.389466
27.142157	1041.998302	16.394483
27.620186	1036.527497	16.399501
27.980893	1035.931675	16.404519
27.641619	1049.175551	16.409536
27.712032	1042.016762	16.414554
27.841718	1037.717332	16.419571
27.385408	1033.458648	16.424589
27.769853	1033.692250	16.429607
27.725638	1038.199220	16.434624
27.757065	1030.781421	16.439642
27.797763	1037.096043	16.444659
27.690950	1041.761081	16.449677
27.613450	1036.957430	16.454695
27.477681	1044.173675	16.459712
27.523623	1031.451938	16.464730
27.710892	1039.163832	16.469747
27.777771	1044.628637	16.474765
27.993214	1037.671327	16.479783
28.014031	1047.413048	16.484800
27.960214	1048.254521	16.489818
27.883706	1050.873065	16.494835
27.979094	1056.816267	16.499853
28.376391	1057.637996	16.504871
28.492562	1051.728072	16.509888
28.715992	1046.965926	16.514906
28.672183	1033.775330	16.519923
28.709029	1027.275014	16.524941
28.508046	1022.137148	16.529959
28.593731	1025.901222	16.534976
28.790895	1019.167668	16.539994
28.542155	1017.634802	16.545011
28.505902	1020.322812	16.550029
28.524469	1029.007695	16.555047
28.284827	1028.088784	16.560064
28.538480	1018.881789	16.565082
28.491118	1012.154752	16.570099
28.495779	1017.017019	16.575117
28.564986	1015.690267	16.580135
28.581815	1027.849907	16.585152
28.403506	1016.908230	16.590170
28.680181	1025.565548	16.595187
28.215885	1019.963757	16.600205
28.305434	1014.502952	16.605223
28.284524	1018.567639	16.610240
28.471105	1017.396178	16.615258
28.532228	1023.259498	16.620275
28.527125	1029.268828	16.625293
28.787681	1035.539752	16.630311
28.711872	1041.033083	16.635328
28.695005	1049.196480	16.640346
28.809055	1044.962598	16.645363
28.874510	1040.452265	16.650381
28.984870	1036.973186	16.655399
28.894065	1044.460138	16.660416
28.788951	1046.792805	16.665434
28.827719	1055.685992	16.670451
28.799883	1043.679468	16.675469
29.131937	1043.110197	16.680487
28.670208	1050.967323	16.685504
28.856598	1044.620440	16.690522
29.113972	1052.340360	16.695539
29.206014	1059.420157	16.700557
29.504937	1055.861225	16.705575
29.119567	1069.383689	16.710592
29.282337	1062.185265	16.715610
29.105723	1063.026923	16.720627
28.833164	1067.664125	16.725645
29.333349	1058.715368	16.730663
29.095728	1060.592147	16.735680
28.755521	1066.934527	16.740698
29.383113	1069.926282	16.745715
29.555785	1076.696891	16.750733
29.595705	1081.149747	16.755751
29.589597	1071.853782	16.760768
29.699113	1070.918375	16.765786
30.124146	1070.138970	16.770803
29.693654	1065.320843	16.775821
29.722365	1056.922013	16.780839
29.583501	1059.212600	16.785856
29.795023	1064.162592	16.790874
29.988495	1049.852613	16.795891
29.844125	1057.168031	16.800909
29.979150	1051.169966	16.805927
30.101318	1060.413083	16.810944
30.328889	1058.916505	16.815962
30.339785	1054.301055	16.820979
29.729845	1067.239953	16.825997
30.067120	1054.949360	16.831015
29.844678	1060.664340	16.836032
29.989521	1053.841091	16.841050
29.927800	1048.258663	16.846067
29.380568	1055.267580	16.851085
29.609603	1054.474510	16.856103
29.957475	1069.082001	16.861120
30.099795	1075.424996	16.866138
30.309021	1071.930517	16.871155
30.460853	1077.634567	16.876173
30.337739	1075.993774	16.881191
30.364147	1086.738180	16.886208
30.452260	1075.174325	16.891226
30.579113	1080.604557	16.896243
30.321701	1082.945162	16.901261
30.752574	1070.914538	16.906279
30.563956	1077.593077	16.911296
30.576240	1076.401413	16.916314
30.461322	1058.797485	16.921331
30.147945	1066.407460	16.926349
30.432715	1076.407899	16.931367
30.230405	1086.531515	16.936384
30.313924	1087.790260	16.941402
30.389442	1076.193651	16.946419
29.891515	1084.835902	16.951437
30.338368	1077.179836	16.956455
30.617265	1090.377989	16.961472
30.884200	1092.659048	16.966490
30.633906	1092.732703	16.971507
30.354946	1099.908150	16.976525
30.765281	1095.823784	16.981543
30.591860	1097.756843	16.986560
30.645990	1100.080502	16.991578
30.832984	1098.943685	16.996595
30.916882	1101.366851	17.001613
30.964961	1097.411468	17.006631
30.798228	1100.716247	17.011648
31.101585	1095.133766	17.016666
31.233687	1095.198377	17.021683
31.102321	1099.160360	17.026701
31.115169	1093.421142	17.031719
31.273065	1091.913320	17.036736
30.806143	1096.678620	17.041754
31.224010	1107.671356	17.046771
31.036095	1120.210072	17.051789
31.205648	1122.534698	17.056807
31.044328	1128.480023	17.061824
30.975855	1121.652091	17.066842
31.449899	1107.500352	17.071859
31.250065	1114.379465	17.076877
31.225392	1119.129563	17.081895
31.224441	1119.397925	17.086912
31.039853	1115.450361	17.091930
31.658198	1130.965680	17.096947
31.317747	1135.436747	17.101965
31.858657	1143.803677	17.106983
31.658533	1148.268677	17.112000
31.536783	1146.892751	17.117018
31.918437	1146.953222	17.122035
31.612322	1145.378785	17.127053
31.941444	1134.866111	17.132071
31.936994	1145.766834	17.137088
31.688110	1141.520009	17.142106
32.295285	1134.277611	17.147123
32.080828	1142.828418	17.152141
32.261865	1133.515906	17.157159
32.166257	1147.611847	17.162176
31.958679	1130.006496	17.167194
31.936657	1116.844004	17.172211
31.741465	1131.110069	17.177229
31.966888	1132.845335	17.182247
32.177399	1133.838160	17.187264
32.199395	1141.222383	17.192282
32.464002	1140.256515	17.197299
31.951801	1132.547776	17.202317
32.565831	1141.951038	17.207335
32.296053	1140.374100	17.212352
32.188153	1140.154189	17.217370
32.184560	1133.095246	17.222387
32.430365	1134.679018	17.227405
32.450502	1138.942467	17.232423
32.468451	1145.443704	17.237440
32.218186	1144.813617	17.242458
32.503347	1133.944873	17.247475
32.378280	1137.277884	17.252493
32.115558	1137.836309	17.257511
32.274338	1135.630918	17.262528
32.246096	1134.694867	17.267546
32.685854	1136.324179	17.272563
32.472166	1137.992115	17.277581
32.615093	1154.455625	17.282599
32.698899	1164.758800	17.287616
32.798531	1164.143662	17.292634
33.330982	1155.877793	17.297651
32.827415	1147.142074	17.302669
32.852856	1146.140860	17.307687
33.202818	1152.947011	17.312704
32.656495	1141.447177	17.317722
32.944686	1143.330460	17.322739
33.179837	1153.398628	17.327757
33.065243	1150.961245	17.332775
33.109123	1149.206084	17.337792
33.075654	1151.669620	17.342810
33.429760	1152.753697	17.347827
33.204347	1148.370673	17.352845
32.967774	1147.287178	17.357863
32.776099	1141.478802	17.362880
32.696298	1154.953755	17.367898
32.806235	1150.401755	17.372915
32.698923	1160.974523	17.377933
32.806332	1164.470158	17.382951
33.279446	1180.828636	17.387968
33.127828	1188.101055	17.392986
33.550211	1182.802971	17.398003
33.632767	1175.516006	17.403021
33.310317	1183.307324	17.408039
33.592198	1178.577068	17.413056
33.623062	1180.408902	17.418074
33.676907	1177.535039	17.423091
33.858992	1170.402991	17.428109
33.802618	1171.651964	17.433127
33.741182	1174.473306	17.438144
34.050242	1177.372662	17.443162
34.095014	1171.909313	17.448179
33.882484	1176.814906	17.453197
33.898418	1180.507823	17.458215
33.977202	1175.847058	17.463232
33.899721	1175.704461	17.468250
33.958887	1167.531209	17.473267
34.013836	1164.799186	17.478285
33.934489	1169.886012	17.483303
33.988356	1172.096114	17.488320
34.105767	1168.628535	17.493338
34.360393	1173.521353	17.498355
34.238636	1171.514270	17.503373
33.918264	1170.446975	17.508391
33.882118	1175.697489	17.513408
34.064008	1177.720402	17.518426
34.058078	1167.001100	17.523443
34.308142	1166.056430	17.528461
34.027314	1168.192410	17.533479
34.436033	1180.180687	17.538496
34.529685	1198.154064	17.543514
34.497741	1188.376068	17.548531
34.422581	1189.362881	17.553549
34.404040	1203.437400	17.558567
34.903655	1196.726117	17.563584
34.816493	1206.112354	17.568602
34.658895	1194.561431	17.573619
34.739974	1185.526385	17.578637
34.719867	1188.839908	17.583655
34.805845	1174.922103	17.588672
34.348147	1179.392501	17.593690
34.549455	1184.047473	17.598707
34.677635	1192.816355	17.603725
34.436838	1189.060562	17.608743
34.669736	1195.730322	17.613760
34.620013	1194.362113	17.618778
34.734286	1188.622852	17.623795
34.866109	1190.959673	17.628813
34.643453	1194.740232	17.633831
35.220292	1201.163941	17.638848
35.174640	1212.815886	17.643866
34.963422	1209.538320	17.648883
35.213193	1214.952612	17.653901
35.168344	1214.312630	17.658919
35.605571	1210.757380	17.663936
35.175187	1210.827517	17.668954
35.505801	1206.320039	17.673971
35.420506	1202.139247	17.678989
35.072951	1199.643455	17.684007
35.376495	1204.601249	17.689024
35.859593	1212.333431	17.694042
35.867056	1204.326002	17.699059
35.575323	1190.646873	17.704077
35.370909	1186.800210	17.709095
35.166968	1192.051607	17.714112
35.360248	1202.290422	17.719130
35.644809	1208.879560	17.724147
35.984899	1201.880689	17.729165
35.710931	1217.651777	17.734183
35.891405	1218.661906	17.739200
35.873170	1216.521936	17.744218
35.992462	1209.080915	17.749235
35.582015	1210.741622	17.754253
36.030831	1213.508772	17.759271
35.930535	1203.204926	17.764288
35.861025	1213.197486	17.769306
35.482775	1208.178683	17.774323
35.568082	1212.062775	17.779341
35.645120	1212.606173	17.784359
36.110758	1213.792809	17.789376
36.077603	1220.971059	17.794394
36.325927	1225.006497	17.799411
36.660470	1223.546899	17.804429
36.189593	1225.936537	17.809447
36.456830	1209.033507	17.814464
36.288441	1201.321701	17.819482
36.295787	1201.241635	17.824499
36.467658	1205.992713	17.829517
36.461626	1224.975711	17.834535
36.973758	1217.609223	17.839552
36.641937	1218.481364	17.844570
36.447694	1209.252488	17.849587
36.316386	1210.740347	17.854605
36.315997	1235.535445	17.859623
36.212534	1232.420978	17.864640
36.359272	1237.848162	17.869658
36.576295	1228.605737	17.874675
36.763999	1227.768602	17.879693
36.256083	1240.111073	17.884711
36.414431	1230.227688	17.889728
36.711973	1247.834856	17.894746
36.723932	1252.210058	17.899763
36.941339	1257.376938	17.904781
36.560763	1251.020426	17.909799
36.901673	1253.927460	17.914816
37.454381	1252.623240	17.919834
37.362113	1254.477409	17.924851
37.442171	1251.334366	17.929869
37.174153	1254.560268	17.934887
37.331715	1250.524689	17.939904
37.314802	1256.640077	17.944922
37.482337	1241.636550	17.949939
37.421022	1233.100176	17.954957
37.045708	1234.386187	17.959975
37.390228	1238.838995	17.964992
37.583404	1249.077854	17.970010
37.517003	1238.099681	17.975027
37.722797	1240.844713	17.980045
37.266001	1223.830335	17.985063
37.535601	1235.979165	17.990080
37.355899	1239.560542	17.995098
37.138475	1237.789252	18.000115
37.437650	1238.452698	18.005133
37.375112	1244.758221	18.010151
37.631897	1241.281552	18.015168
37.320785	1246.691661	18.020186
37.270612	1247.933362	18.025203
37.461032	1251.498141	18.030221
37.800383	1265.008903	18.035239
38.239033	1262.681027	18.040256
37.916674	1270.917337	18.045274
38.024544	1267.085151	18.050291
38.220910	1260.042363	18.055309
38.020716	1266.773268	18.060327
38.150669	1258.961338	18.065344
37.910286	1259.926542	18.070362
37.855226	1257.688159	18.075379
38.348453	1263.986053	18.080397
37.981459	1261.455409	18.085415
38.031607	1263.625076	18.090432
38.115399	1258.998224	18.095450
38.223282	1269.676407	18.100467
38.544434	1272.132084	18.105485
38.062774	1293.515033	18.110503
38.218285	1293.796907	18.115520
38.626196	1285.616640	18.120538
38.411928	1293.346981	18.125555
38.329679	1284.782283	18.130573
38.429199	1285.678788	18.135591
38.411526	1289.894511	18.140608
38.733774	1284.602521	18.145626
38.585228	1282.728983	18.150643
39.085034	1279.078770	18.155661
38.871893	1288.828647	18.160679
39.119757	1286.098127	18.165696
39.057499	1286.499113	18.170714
38.934847	1286.489780	18.175731
39.317272	1283.328056	18.180749
39.017261	1289.402325	18.185767
39.164011	1282.837467	18.190784
38.865916	1291.278291	18.195802
39.050272	1281.753746	18.200819
38.920035	1285.797646	18.205837
39.110900	1285.057846	18.210855
39.023530	1294.642977	18.215872
39.446881	1302.611719	18.220890
39.011926	1302.187106	18.225907
39.391630	1307.672714	18.230925
39.227103	1311.469494	18.235943
39.009230	1301.398492	18.240960
39.178404	1312.404829	18.245978
38.861990	1304.043838	18.250995
39.423068	1304.180516	18.256013
39.517633	1322.898647	18.261031
39.911764	1332.023822	18.266048
39.955425	1315.319603	18.271066
39.309865	1304.743987	18.276083
39.801765	1316.908754	18.281101
39.727133	1328.164499	18.286119
39.960513	1326.187312	18.291136
39.781288	1337.146922	18.296154
39.930175	1336.145412	18.301171
39.934552	1333.452795	18.306189
40.154309	1333.926638	18.311207
39.883307	1334.991288	18.316224
40.445347	1329.362148	18.321242
40.118732	1322.590109	18.326259
40.052050	1328.845814	18.331277
40.047239	1324.437868	18.336295
39.985296	1322.926384	18.341312
40.274297	1324.067946	18.346330
40.274298	1325.639512	18.351347
40.297283	1323.139660	18.356365
40.090278	1322.111510	18.361383
40.140548	1324.893392	18.366400
40.692173	1322.781449	18.371418
40.596900	1333.636468	18.376435
40.311139	1318.258484	18.381453
40.373800	1328.536643	18.386471
40.647479	1329.541735	18.391488
40.735228	1318.501643	18.396506
40.624712	1324.997701	18.401523
40.528869	1320.105311	18.406541
40.148973	1324.345880	18.411559
40.531669	1345.013646	18.416576
41.172742	1346.557987	18.421594
41.088877	1352.551287	18.426611
40.957831	1342.820194	18.431629
40.983393	1347.565688	18.436647
40.995330	1351.770504	18.441664
40.696144	1353.196150	18.446682
41.039214	1346.881571	18.451699
41.020649	1348.178318	18.456717
41.041033	1348.528569	18.461735
41.241798	1346.588015	18.466752
41.241207	1342.504456	18.471770
41.066568	1346.640490	18.476787
41.348929	1346.104193	18.481805
41.043512	1352.081494	18.486823
41.523115	1355.288844	18.491840
41.796134	1364.887330	18.496858
41.280092	1367.160942	18.501875
41.413110	1363.697207	18.506893
41.473406	1364.170632	18.511911
41.566208	1371.667004	18.516928
41.581469	1364.308388	18.521946
41.250639	1370.236003	18.526963
41.465476	1357.039611	18.531981
41.798023	1364.078929	18.536999
41.893620	1366.415102	18.542016
41.748973	1365.929509	18.547034
41.198887	1376.867989	18.552051
42.110884	1373.743719	18.557069
42.083607	1387.974378	18.562087
41.958549	1388.498754	18.567104
42.260248	1390.970100	18.572122
42.211066	1389.586012	18.577139
42.236873	1384.220225	18.582157
42.278666	1380.871677	18.587175
42.419206	1379.252923	18.592192
42.798984	1379.260038	18.597210
42.627593	1368.989257	18.602227
42.501753	1350.127569	18.607245
42.278759	1352.216696	18.612263
42.165527	1353.455600	18.617280
42.347738	1345.875337	18.622298
42.672579	1363.626693	18.627315
42.372181	1365.118801	18.632333
42.588912	1368.657416	18.637351
42.444168	1377.557244	18.642368
42.521659	1368.222862	18.647386
42.606276	1378.623864	18.652403
42.358717	1366.354685	18.657421
42.899844	1369.861729	18.662439
42.513592	1368.848861	18.667456
42.624723	1376.882026	18.672474
42.945731	1367.244641	18.677491
42.636101	1366.680593	18.682509
42.668106	1381.410104	18.687527
42.882223	1390.178326	18.692544
43.100226	1394.168031	18.697562
43.037467	1398.561214	18.702579
42.950476	1404.605511	18.707597
43.398367	1396.646189	18.712615
42.945872	1396.868093	18.717632
43.516602	1388.413119	18.722650
43.134128	1393.092765	18.727667
43.176890	1398.280566	18.732685
43.464292	1395.149396	18.737703
43.379255	1404.125149	18.742720
43.693532	1409.662001	18.747738
43.362345	1422.923830	18.752755
43.791673	1418.104282	18.757773
43.943753	1413.286876	18.762791
43.649491	1421.313751	18.767808
44.121847	1415.089472	18.772826
43.987564	1421.447254	18.777843
43.746196	1401.495803	18.782861
43.871545	1406.961083	18.787879
43.613205	1425.655372	18.792896
44.428260	1417.212838	18.797914
44.172989	1420.149605	18.802931
44.061548	1421.438727	18.807949
44.168564	1417.183762	18.812967
44.054755	1423.850783	18.817984
44.254757	1413.825111	18.823002
43.982185	1423.574847	18.828019
43.971770	1422.036397	18.833037
44.219232	1420.337876	18.838055
44.177626	1417.693431	18.843072
44.429427	1415.653405	18.848090
44.263854	1418.967529	18.853107
44.140480	1408.424159	18.858125
44.550265	1416.401376	18.863143
44.725220	1429.963106	18.868160
45.109388	1427.826730	18.873178
44.937445	1428.061758	18.878195
44.668304	1421.542667	18.883213
44.728570	1409.250778	18.888231
44.412390	1420.070815	18.893248
44.798493	1428.386243	18.898266
44.879110	1439.094019	18.903283
45.142805	1439.772465	18.908301
44.971060	1443.030749	18.913319
45.034093	1443.803554	18.918336
44.983048	1440.371618	18.923354
44.977793	1449.890398	18.928371
44.766579	1439.101908	18.933389
45.131567	1434.923539	18.938407
44.844393	1443.949719	18.943424
45.366321	1446.749705	18.948442
45.179751	1440.539646	18.953459
44.651815	1450.124026	18.958477
45.066195	1451.265010	18.963495
45.398925	1470.350162	18.968512
45.702534	1464.735969	18.973530
45.613342	1466.630707	18.978547
45.479414	1463.940669	18.983565
45.512861	1466.810400	18.988583
45.667385	1469.077451	18.993600
45.679525	1455.991441	18.998618
45.576630	1463.701359	19.003635
45.488493	1461.559619	19.008653
45.875847	1459.040888	19.013671
45.668968	1462.879007	19.018688
45.817998	1453.476637	19.023706
45.859841	1466.702510	19.028723
46.299868	1473.630463	19.033741
46.406655	1471.758177	19.038759
46.067845	1465.840058	19.043776
46.314881	1478.465943	19.048794
46.287152	1473.506100	19.053811
46.041940	1486.887135	19.058829
46.508864	1474.651809	19.063847
46.578531	1483.104893	19.068864
46.644076	1479.923043	19.073882
46.644107	1479.083558	19.078899
46.530583	1477.267664	19.083917
46.756604	1467.367300	19.088935
46.613300	1476.374252	19.093952
46.550282	1469.526403	19.098970
46.581703	1482.220574	19.103987
46.076093	1484.126498	19.109005
46.836314	1479.132338	19.114023
47.076532	1485.943080	19.119040
46.292285	1482.707343	19.124058
46.810766	1474.882164	19.129075
46.594174	1482.966402	19.134093
46.791274	1472.123787	19.139111
46.650897	1495.369435	19.144128
47.050856	1504.197142	19.149146
47.139654	1500.898058	19.154163
47.138823	1504.773534	19.159181
47.110914	1503.809009	19.164199
47.033059	1506.326842	19.169216
47.465165	1500.029906	19.174234
47.574730	1502.865701	19.179251
47.152914	1506.693113	19.184269
47.142993	1500.105231	19.189287
47.232983	1507.460085	19.194304
47.537780	1521.923175	19.199322
47.814882	1529.570802	19.204339
47.729510	1520.189113	19.209357
47.963333	1518.628407	19.214375
47.590027	1510.512865	19.219392
48.037983	1515.271535	19.224410
48.162786	1510.717128	19.229427
48.305552	1521.115472	19.234445
48.330269	1500.617547	19.239463
47.951939	1499.126905	19.244480
47.530584	1493.909603	19.249498
47.905900	1506.282002	19.254515
47.959983	1506.358762	19.259533
48.098679	1507.365945	19.264551
47.859164	1515.763040	19.269568
48.278439	1518.670540	19.274586
48.045308	1505.534317	19.279603
48.059190	1519.105413	19.284621
48.251599	1515.294727	19.289639
48.414501	1515.559674	19.294656
48.173833	1527.545150	19.299674
48.620392	1526.121737	19.304691
48.469441	1543.578117	19.309709
48.664714	1532.757840	19.314727
48.751053	1544.209569	19.319744
48.829827	1535.521848	19.324762
48.894887	1537.585084	19.329779
48.738698	1543.286746	19.334797
48.775502	1531.320323	19.339815
48.703590	1534.137041	19.344832
48.502824	1539.851955	19.349850
48.922427	1540.610274	19.354867
48.689046	1544.004407	19.359885
49.317004	1547.463253	19.364903
49.645274	1548.977418	19.369920
49.533258	1544.781771	19.374938
49.352928	1538.267744	19.379955
49.177934	1539.680380	19.384973
49.360016	1540.065420	19.389991
49.277075	1553.395994	19.395008
49.015065	1556.971314	19.400026
49.455677	1555.476241	19.405043
49.492717	1560.567148	19.410061
49.734490	1554.227241	19.415079
49.977683	1556.376356	19.420096
49.443774	1552.871252	19.425114
49.746941	1553.499375	19.430131
49.787753	1555.108790	19.435149
49.970843	1555.402153	19.440167
49.867868	1553.007088	19.445184
49.626367	1557.888894	19.450202
49.580549	1545.925857	19.455219
50.075463	1565.156275	19.460237
50.073262	1572.629653	19.465255
50.355557	1579.945128	19.470272
50.220555	1584.100292	19.475290
50.002272	1568.197181	19.480307
50.511500	1581.034784	19.485325
50.613936	1570.127952	19.490343
50.772714	1565.606112	19.495360
50.789992	1573.025964	19.500378
51.076208	1560.531531	19.505395
50.830318	1552.383508	19.510413
50.639735	1540.720729	19.515431
50.292140	1549.365043	19.520448
50.741105	1560.028166	19.525466
50.879861	1557.500789	19.530483
50.775012	1561.629161	19.535501
51.082442	1566.775803	19.540519
51.153800	1564.583971	19.545536
50.876506	1571.573152	19.550554
51.208093	1566.030312	19.555571
50.638933	1563.117684	19.560589
50.932406	1562.188325	19.565607
51.116162	1561.367569	19.570624
51.099450	1566.649886	19.575642
51.211635	1562.539251	19.580659
51.351974	1568.390417	19.585677
51.036035	1564.169710	19.590695
51.182452	1565.772151	19.595712
51.378066	1574.369773	19.600730
51.435279	1578.236228	19.605747
51.683262	1584.704967	19.610765
51.488346	1589.828841	19.615783
51.643446	1580.053068	19.620800
51.703241	1586.024079	19.625818
51.484899	1580.708869	19.630835
51.479472	1586.510151	19.635853
51.590488	1575.333732	19.640871
51.575363	1577.655613	19.645888
51.726843	1598.848832	19.650906
51.894098	1601.745090	19.655923
52.417158	1608.732752	19.660941
52.070700	1610.822197	19.665959
52.263338	1604.209051	19.670976
52.268647	1609.702551	19.675994
52.382783	1594.423015	19.681011
52.422524	1602.237020	19.686029
52.145529	1597.723058	19.691047
52.312835	1600.944361	19.696064
51.929452	1602.919632	19.701082
52.366510	1601.917422	19.706099
52.167368	1605.230495	19.711117
52.604499	1607.718656	19.716135
52.868546	1613.702058	19.721152
52.704293	1631.034359	19.726170
52.719592	1629.801163	19.731187
52.852496	1637.483911	19.736205
52.670178	1620.830369	19.741223
53.200573	1618.283033	19.746240
52.742260	1629.453535	19.751258
52.787531	1626.634584	19.756275
53.036818	1621.306517	19.761293
52.882619	1626.869038	19.766311
53.009604	1624.797928	19.771328
53.240732	1628.855072	19.776346
53.362686	1641.336441	19.781363
53.571582	1642.613575	19.786381
53.536627	1645.263607	19.791399
53.786689	1639.029679	19.796416
53.324204	1641.651599	19.801434
53.629485	1632.079637	19.806451
53.821455	1644.764707	19.811469
53.654465	1645.336644	19.816487
54.375303	1635.797812	19.821504
54.097944	1642.480912	19.826522
54.005626	1622.187265	19.831539
53.870551	1619.642551	19.836557
53.993743	1615.965698	19.841575
54.329799	1628.858701	19.846592
53.785799	1637.599911	19.851610
53.736525	1637.676984	19.856627
54.006821	1646.556510	19.861645
53.956605	1636.118381	19.866663
53.918031	1635.957099	19.871680
53.502764	1653.808195	19.876698
53.992048	1658.241727	19.881715
54.256529	1657.373684	19.886733
54.371666	1661.900183	19.891751
54.404614	1652.944980	19.896768
54.433076	1659.375339	19.901786
54.906829	1654.684514	19.906803
54.828742	1657.019364	19.911821
54.605311	1656.959448	19.916839
54.775682	1651.492176	19.921856
54.642287	1658.197049	19.926874
54.924339	1669.646789	19.931891
54.948781	1683.263705	19.936909
55.066027	1680.578710	19.941927
55.247835	1669.337560	19.946944
55.228006	1674.229066	19.951962
54.941769	1683.059556	19.956979
55.543578	1679.431252	19.961997
55.397503	1679.428720	19.967015
55.506624	1670.335413	19.972032
55.457177	1677.598436	19.977050
55.433582	1675.269892	19.982067
55.589994	1676.343756	19.987085
55.421191	1672.415702	19.992103
55.921762	1673.309747	19.997120
55.439231	1676.038937	20.002138
55.743036	1683.748746	20.007155
55.667338	1681.945877	20.012173
55.121828	1680.231934	20.017191
55.673515	1677.870628	20.022208
55.535424	1700.166268	20.027226
55.517034	1701.109556	20.032243
55.871286	1704.121887	20.037261
55.536901	1701.078005	20.042279
55.962313	1700.083916	20.047296
55.700421	1721.575174	20.052314
56.049005	1723.313415	20.057331
56.586618	1727.086172	20.062349
56.372934	1729.760887	20.067367
56.551633	1711.700334	20.072384
56.572993	1714.805523	20.077402
56.973327	1712.666597	20.082419
57.121452	1708.938505	20.087437
56.838863	1712.820025	20.092455
56.710812	1718.668845	20.097472
56.540919	1720.554082	20.102490
56.866067	1715.722273	20.107507
56.837023	1707.830757	20.112525
57.146588	1716.637930	20.117543
57.187514	1713.317857	20.122560
57.245941	1714.545838	20.127578
57.078915	1714.543413	20.132595
56.980281	1707.091932	20.137613
56.865456	1707.867193	20.142631
57.054668	1711.536397	20.147648
57.202632	1726.301789	20.152666
57.300343	1734.258308	20.157683
57.382359	1734.270759	20.162701
57.216655	1736.754964	20.167719
57.716021	1736.434185	20.172736
57.380665	1736.394850	20.177754
57.669527	1740.859607	20.182771
58.137791	1728.352494	20.187789
57.729414	1741.168973	20.192807
57.682051	1731.222663	20.197824
57.880852	1739.873519	20.202842
58.349178	1750.328609	20.207859
58.425229	1743.459002	20.212877
57.813571	1734.215945	20.217895
58.392352	1739.677005	20.222912
58.353814	1746.070489	20.227930
58.385588	1749.085697	20.232947
58.538839	1745.369423	20.237965
58.352132	1741.756574	20.242983
58.545634	1740.697601	20.248000
58.496774	1736.952835	20.253018
58.484077	1741.259411	20.258035
58.828410	1737.614377	20.263053
58.557702	1738.249803	20.268071
58.750060	1736.487247	20.273088
58.744741	1741.644762	20.278106
58.742566	1744.362290	20.283123
58.830470	1742.858999	20.288141
58.704300	1741.095541	20.293159
58.896328	1741.488505	20.298176
58.843875	1752.409696	20.303194
59.215384	1760.897970	20.308211
59.143810	1759.823461	20.313229
59.290384	1773.525575	20.318247
59.403291	1756.863811	20.323264
59.504336	1759.650480	20.328282
59.433374	1765.689248	20.333299
59.774728	1765.225808	20.338317
59.422136	1767.369876	20.343335
59.461458	1759.136325	20.348352
59.381030	1770.424810	20.353370
59.405153	1771.853801	20.358387
59.549523	1767.943240	20.363405
59.357060	1774.344920	20.368423
59.745594	1771.873300	20.373440
59.319192	1780.331175	20.378458
59.443083	1790.656873	20.383475
59.811812	1785.894001	20.388493
59.579203	1796.483497	20.393511
59.945612	1806.837720	20.398528
59.900272	1819.992220	20.403546
60.303461	1822.845469	20.408563
60.335123	1815.395748	20.413581
60.311961	1821.821580	20.418599
60.772360	1815.434919	20.423616
60.549918	1821.506758	20.428634
60.064098	1816.040613	20.433651
60.863192	1820.419638	20.438669
60.945989	1837.685272	20.443687
60.764792	1833.310974	20.448704
60.769394	1836.582900	20.453722
60.880012	1838.610674	20.458739
61.277669	1830.084608	20.463757
61.204968	1829.338484	20.468775
61.299336	1822.608010	20.473792
61.701970	1819.947990	20.478810
61.331160	1822.180110	20.483827
61.771074	1820.426341	20.488845
61.240435	1808.816331	20.493863
61.167889	1815.243537	20.498880
61.508920	1816.500111	20.503898
61.579155	1827.891411	20.508915
61.641388	1821.509934	20.513933
61.315696	1820.942059	20.518951
61.219352	1820.448932	20.523968
61.721266	1820.825209	20.528986
61.502061	1827.477231	20.534003
61.649359	1833.961737	20.539021
61.846255	1841.940733	20.544039
62.050739	1852.061409	20.549056
62.285703	1850.178596	20.554074
62.107514	1850.474563	20.559091
62.434235	1844.010872	20.564109
62.133481	1846.582393	20.569127
62.171808	1853.806574	20.574144
62.443993	1845.038095	20.579162
62.364624	1850.358655	20.584179
62.595581	1851.787008	20.589197
62.627724	1848.506148	20.594215
62.367602	1847.628253	20.599232
62.554948	1846.062132	20.604250
62.781586	1872.375472	20.609267
62.754765	1859.181620	20.614285
62.710997	1867.267527	20.619303
63.101134	1862.245673	20.624320
63.300937	1866.124705	20.629338
63.133493	1866.093942	20.634355
63.377098	1854.199249	20.639373
63.356322	1860.126091	20.644391
63.120594	1866.682867	20.649408
63.338478	1860.267674	20.654426
63.558784	1860.981296	20.659443
63.754050	1854.481262	20.664461
63.460526	1851.566696	20.669479
63.787985	1851.755534	20.674496
63.890596	1851.203028	20.679514
63.348550	1853.843676	20.684531
63.666500	1850.177480	20.689549
63.751140	1844.518363	20.694567
63.585254	1852.913620	20.699584
63.877996	1851.990673	20.704602
63.778234	1850.636516	20.709619
63.724834	1866.014061	20.714637
64.226496	1880.803410	20.719655
64.006936	1881.746469	20.724672
64.432472	1879.471052	20.729690
64.059875	1885.266479	20.734707
64.080787	1877.083079	20.739725
64.561803	1870.955129	20.744743
64.325547	1876.640961	20.749760
64.285101	1863.547060	20.754778
64.268931	1885.274821	20.759795
64.650945	1897.359262	20.764813
64.521088	1903.602913	20.769831
64.809398	1903.422293	20.774848
64.894945	1908.351108	20.779866
64.489352	1899.965849	20.784883
64.814750	1902.143233	20.789901
65.056142	1908.789848	20.794919
65.138794	1921.217570	20.799936
65.166514	1922.081104	20.804954
65.329932	1929.468883	20.809971
65.503570	1921.760319	20.814989
65.411961	1925.476445	20.820007
65.714887	1924.286812	20.825024
65.499511	1920.703637	20.830042
65.622381	1918.970817	20.835059
65.718564	1922.509377	20.840077
65.501708	1925.522298	20.845095
65.511665	1929.415123	20.850112
65.619529	1919.640207	20.855130
65.893503	1927.184347	20.860147
65.792789	1940.559004	20.865165
65.934970	1952.794436	20.870183
65.898260	1956.811302	20.875200
66.164092	1950.495913	20.880218
66.151563	1949.977109	20.885235
65.970364	1947.521584	20.890253
66.535666	1945.356947	20.895271
66.475874	1957.911017	20.900288
66.644210	1951.617120	20.905306
66.491193	1968.474610	20.910323
66.415521	1965.971093	20.915341
66.590395	1966.694949	20.920359
67.022866	1962.748958	20.925376
67.110067	1966.509839	20.930394
67.032497	1969.295947	20.935411
67.078479	1963.567070	20.940429
67.308154	1961.798681	20.945447
67.235441	1964.277907	20.950464
67.333353	1961.580101	20.955482
67.392710	1968.223520	20.960499
67.428560	1967.791861	20.965517
67.205738	1965.844605	20.970535
67.113752	1961.973957	20.975552
67.381630	1964.826205	20.980570
67.608660	1960.864862	20.985587
67.536019	1971.110807	20.990605
67.934147	1982.836178	20.995623
67.652521	1990.103917	21.000640
67.739215	1980.341731	21.005658
67.736725	1990.314823	21.010675
67.622910	1978.794445	21.015693
68.079188	1975.128778	21.020711
67.861166	1977.046784	21.025728
67.736376	1973.793490	21.030746
67.467981	1992.439441	21.035763
68.051214	2003.807790	21.040781
68.425291	2001.423600	21.045799
68.278840	2007.284847	21.050816
68.558960	2006.821468	21.055834
68.300623	2005.990625	21.060851
68.529041	2001.609318	21.065869
68.379692	2011.128741	21.070887
68.519568	2021.136491	21.075904
68.979743	2026.142716	21.080922
68.745506	2029.275130	21.085939
69.022866	2017.655952	21.090957
69.137328	2012.433971	21.095975
69.166840	2021.900304	21.100992
69.246637	2016.951973	21.106010
69.417547	2020.693521	21.111027
69.500141	2011.436906	21.116045
69.579416	2005.822757	21.121063
69.594217	2002.380461	21.126080
69.404064	2006.923021	21.131098
69.868469	2019.720582	21.136115
69.518496	2022.574356	21.141133
69.964223	2022.059946	21.146151
69.549651	2033.321722	21.151168
70.028922	2029.002342	21.156186
69.831548	2033.874250	21.161203
70.094665	2026.372626	21.166221
70.357657	2031.308562	21.171239
70.138130	2039.223087	21.176256
69.860026	2033.241676	21.181274
69.920440	2034.993255	21.186291
69.963868	2040.357871	21.191309
70.602250	2051.973295	21.196327
70.306722	2062.664266	21.201344
70.806216	2061.302003	21.206362
70.652368	2063.140595	21.211379
70.244129	2058.097816	21.216397
70.532102	2060.533522	21.221415
70.417560	2066.282518	21.226432
70.753355	2071.418579	21.231450
70.957315	2088.807609	21.236467
70.868917	2082.032907	21.241485
71.411957	2075.892075	21.246503
71.162546	2083.284229	21.251520
70.943470	2075.545220	21.256538
71.418399	2079.274162	21.261555
71.253202	2084.141074	21.266573
71.532760	2097.636531	21.271591
71.696606	2101.401287	21.276608
71.691449	2101.102247	21.281626
72.014250	2105.078952	21.286643
72.164835	2098.592098	21.291661
72.073306	2089.100610	21.296679
71.997206	2099.205149	21.301696
71.955874	2097.712481	21.306714
72.178764	2096.058751	21.311731
72.072105	2100.578867	21.316749
72.083366	2095.877880	21.321767
72.332003	2093.611043	21.326784
72.011240	2099.609917	21.331802
71.907680	2095.794694	21.336819
72.115001	2107.104865	21.341837
72.415740	2110.523247	21.346855
72.351484	2115.541717	21.351872
72.508128	2118.316630	21.356890
72.495350	2122.998868	21.361907
72.940716	2123.219848	21.366925
72.836429	2119.575154	21.371943
72.892294	2127.860271	21.376960
73.004162	2144.077054	21.381978
72.863656	2145.740000	21.386995
73.222653	2140.183249	21.392013
73.300927	2145.981149	21.397031
73.060476	2149.559541	21.402048
73.212266	2140.664490	21.407066
73.606234	2145.554818	21.412083
73.118202	2145.084794	21.417101
73.704729	2157.383735	21.422119
73.750066	2160.213856	21.427136
73.519262	2170.367769	21.432154
73.903026	2167.230931	21.437171
73.966120	2171.749883	21.442189
73.540976	2166.936934	21.447207
73.667403	2176.486095	21.452224
73.854150	2181.699045	21.457242
74.063909	2178.731315	21.462259
74.075123	2192.511632	21.467277
74.344573	2184.756478	21.472295
74.325856	2186.564576	21.477312
74.634040	2196.906000	21.482330
74.704762	2189.162849	21.487347
74.669605	2192.422094	21.492365
75.110799	2199.501636	21.497383
74.973623	2211.604006	21.502400
75.350778	2205.656224	21.507418
75.146318	2183.214407	21.512435
74.957676	2192.632741	21.517453
75.273179	2202.878350	21.522471
75.125250	2208.051891	21.527488
75.416712	2205.020941	21.532506
75.380598	2197.152402	21.537523
75.393988	2205.939655	21.542541
75.688204	2202.318110	21.547559
75.544674	2202.327806	21.552576
75.504334	2198.420662	21.557594
75.533149	2195.386422	21.562611
75.312734	2203.143359	21.567629
75.885675	2205.853471	21.572647
76.159469	2220.202029	21.577664
76.263238	2215.205727	21.582682
76.287053	2220.033780	21.587699
75.927358	2216.226849	21.592717
76.149185	2220.983045	21.597735
76.583168	2221.751781	21.602752
76.121632	2228.138708	21.607770
76.847726	2218.305246	21.612787
76.467022	2224.231439	21.617805
76.615675	2221.828667	21.622823
76.453911	2232.861849	21.627840
76.818549	2245.327949	21.632858
77.134364	2240.418553	21.637875
77.346063	2245.548737	21.642893
77.141860	2247.174270	21.647911
77.352483	2260.443884	21.652928
77.405369	2253.524037	21.657946
77.746469	2240.805980	21.662963
77.492427	2246.112824	21.667981
77.664073	2234.926554	21.672999
77.501316	2248.159613	21.678016
77.068092	2242.173879	21.683034
77.673705	2240.697245	21.688051
77.384108	2237.580022	21.693069
77.548740	2237.216674	21.698087
77.730523	2243.812730	21.703104
77.637998	2238.446175	21.708122
77.878958	2251.976162	21.713139
77.843915	2256.930160	21.718157
77.837977	2259.048717	21.723175
77.956154	2266.503643	21.728192
77.989238	2270.326665	21.733210
78.226767	2268.910494	21.738227
78.373848	2279.277049	21.743245
78.296398	2281.602413	21.748263
78.396294	2288.416374	21.753280
77.969797	2280.731662	21.758298
78.079691	2289.573362	21.763315
78.332249	2309.198943	21.768333
78.506443	2308.739425	21.773351
78.878770	2315.242722	21.778368
78.835874	2316.019434	21.783386
79.012215	2324.096525	21.788403
78.985014	2330.684124	21.793421
79.261990	2334.828971	21.798439
79.245360	2331.820719	21.803456
79.225376	2334.023527	21.808474
79.887375	2328.186000	21.813491
79.582120	2332.434120	21.818509
79.874668	2328.099556	21.823527
79.718487	2351.052113	21.828544
79.556086	2361.858243	21.833562
79.916084	2348.764760	21.838579
79.937227	2353.807872	21.843597
80.359604	2356.213226	21.848615
80.308965	2355.798180	21.853632
80.255170	2356.778574	21.858650
80.321704	2350.572975	21.863667
80.374590	2361.828452	21.868685
80.608071	2368.514342	21.873703
80.707407	2371.749524	21.878720
80.798142	2379.145650	21.883738
81.012700	2369.158205	21.888755
80.583826	2377.976528	21.893773
80.936957	2374.345776	21.898791
80.850126	2379.607691	21.903808
81.121417	2378.665966	21.908826
81.070869	2371.869481	21.913843
81.085070	2376.042625	21.918861
80.993001	2381.946023	21.923879
81.577654	2390.344604	21.928896
80.979472	2405.311939	21.933914
81.493455	2401.110151	21.938931
81.701460	2402.949247	21.943949
81.639776	2397.044479	21.948967
81.947070	2399.142688	21.953984
82.016849	2401.842801	21.959002
82.747793	2393.898934	21.964019
82.566291	2392.658454	21.969037
82.331464	2382.400120	21.974055
82.367849	2374.703264	21.979072
82.176317	2373.852534	21.984090
82.450940	2376.299831	21.989107
82.040009	2388.776321	21.994125
82.576046	2402.049028	21.999143
82.534067	2401.632633	22.004160
82.638886	2399.889953	22.009178
82.928834	2398.841175	22.014195
82.365996	2406.610485	22.019213
82.911305	2404.761352	22.024231
82.883137	2411.573207	22.029248
82.943853	2427.908672	22.034266
83.244350	2430.563400	22.039283
83.247716	2431.178270	22.044301
83.312076	2433.812956	22.049319
83.564409	2435.086541	22.054336
83.095601	2432.038213	22.059354
83.429498	2420.703482	22.064371
83.286858	2438.162595	22.069389
83.611192	2445.740143	22.074407
84.162704	2455.226426	22.079424
83.938896	2452.430303	22.084442
83.994652	2449.609590	22.089459
84.052971	2450.427357	22.094477
83.856107	2458.527899	22.099495
83.997663	2449.593260	22.104512
84.160952	2465.395204	22.109530
84.305935	2468.421312	22.114547
84.430755	2477.137696	22.119565
84.668692	2473.638476	22.124583
84.750521	2478.965685	22.129600
84.524486	2476.561251	22.134618
84.713978	2473.312587	22.139635
84.698519	2483.354248	22.144653
84.991351	2492.151786	22.149671
85.517278	2490.810625	22.154688
85.146619	2501.197952	22.159706
85.582965	2498.352693	22.164723
85.499282	2500.950474	22.169741
85.311470	2502.062202	22.174759
85.313739	2492.896745	22.179776
85.328910	2495.987253	22.184794
85.579321	2497.475751	22.189811
85.702698	2512.286649	22.194829
86.041875	2512.637785	22.199847
86.146692	2507.694891	22.204864
86.119571	2516.046760	22.209882
86.230697	2513.024900	22.214899
86.066233	2515.117672	22.219917
86.517464	2512.866581	22.224935
86.408887	2511.371724	22.229952
86.169088	2512.330590	22.234970
86.130473	2530.840332	22.239987
86.549589	2533.167318	22.245005
86.507963	2541.878088	22.250023
87.028707	2539.792909	22.255040
86.811470	2546.085103	22.260058
86.746314	2533.651012	22.265075
87.309022	2551.764176	22.270093
86.970297	2565.413057	22.275111
87.012081	2562.528225	22.280128
87.288613	2569.081247	22.285146
87.219849	2563.862384	22.290163
87.316926	2557.939156	22.295181
87.442275	2575.435579	22.300199
88.036887	2590.681295	22.305216
87.943731	2596.187272	22.310234
88.255759	2583.280981	22.315251
88.397918	2581.911195	22.320269
88.325378	2587.877896	22.325287
88.431645	2574.479746	22.330304
88.315159	2580.888819	22.335322
88.695696	2571.866415	22.340339
89.050282	2572.625438	22.345357
88.773940	2581.237061	22.350375
88.753947	2571.696307	22.355392
88.741003	2564.736092	22.360410
88.801829	2565.888013	22.365427
88.543203	2569.002226	22.370445
88.550886	2579.157111	22.375463
88.578074	2574.248377	22.380480
88.337446	2580.708339	22.385498
88.889858	2587.780189	22.390515
88.823435	2596.479066	22.395533
88.872229	2592.832534	22.400551
89.592279	2601.812938	22.405568
89.105551	2608.702574	22.410586
89.178728	2614.018546	22.415603
89.462304	2610.338612	22.420621
89.299543	2620.564242	22.425639
89.531791	2618.836418	22.430656
90.023092	2631.822750	22.435674
89.825038	2636.729643	22.440691
89.656267	2646.148277	22.445709
89.762966	2645.784472	22.450727
90.063115	2647.659745	22.455744
90.704452	2667.613382	22.460762
90.939767	2664.458543	22.465779
90.827553	2664.886273	22.470797
90.750947	2663.803024	22.475815
91.013806	2664.999242	22.480832
90.895819	2663.717293	22.485850
91.007841	2666.180478	22.490867
91.286985	2660.036352	22.495885
91.074576	2662.221819	22.500903
91.389662	2654.112193	22.505920
91.229824	2664.905482	22.510938
91.505946	2652.190939	22.515955
91.685228	2667.239432	22.520973
91.127295	2674.342167	22.525991
91.473011	2684.725371	22.531008
91.359263	2686.939665	22.536026
91.409485	2690.059465	22.541043
91.894186	2698.293859	22.546061
91.672904	2717.368763	22.551079
92.016642	2715.888681	22.556096
92.045130	2720.141739	22.561114
92.132538	2716.454452	22.566131
92.496780	2718.013616	22.571149
92.631378	2735.407762	22.576167
92.891373	2731.860873	22.581184
92.577264	2734.958504	22.586202
92.974155	2727.028629	22.591219
93.002826	2729.845654	22.596237
92.772640	2730.591578	22.601255
92.965678	2728.178672	22.606272
92.926682	2735.260601	22.611290
93.388357	2753.635872	22.616307
93.330000	2756.248683	22.621325
92.881361	2761.989952	22.626343
93.349648	2758.161300	22.631360
93.452653	2755.140663	22.636378
93.530474	2758.442386	22.641395
93.986051	2768.060547	22.646413
93.820942	2774.423606	22.651431
94.098579	2770.662507	22.656448
94.446442	2766.499123	22.661466
94.480881	2773.389737	22.666483
94.729232	2772.609368	22.671501
94.513481	2769.496334	22.676519
94.836384	2759.021551	22.681536
94.918885	2770.496755	22.686554
94.838698	2768.019077	22.691571
94.953786	2770.983613	22.696589
94.696985	2770.430228	22.701607
95.162833	2762.934606	22.706624
95.043492	2771.411414	22.711642
94.864522	2773.421261	22.716659
94.881684	2773.172388	22.721677
95.289084	2787.210242	22.726695
95.467933	2793.295675	22.731712
95.655517	2797.946895	22.736730
95.580378	2797.131676	22.741747
95.482663	2792.078213	22.746765
95.393501	2797.072347	22.751783
95.753928	2791.947555	22.756800
96.041985	2808.405775	22.761818
95.915908	2821.586204	22.766835
96.055544	2816.293792	22.771853
95.836743	2820.989353	22.776871
95.995535	2821.005632	22.781888
96.192308	2835.076316	22.786906
96.045530	2848.392543	22.791923
96.436151	2841.470383	22.796941
96.332730	2844.831901	22.801959
96.590220	2851.223874	22.806976
96.971253	2860.058359	22.811994
96.620076	2864.578863	22.817011
97.056484	2867.007352	22.822029
97.299627	2859.757821	22.827047
97.225040	2865.535569	22.832064
97.247454	2875.094984	22.837082
97.405388	2886.665825	22.842099
97.849405	2885.211146	22.847117
97.854095	2899.857789	22.852135
97.682799	2890.577129	22.857152
98.053793	2888.060749	22.862170
97.792125	2892.958679	22.867187
97.998041	2894.305803	22.872205
97.979189	2912.203736	22.877223
98.292084	2917.264705	22.882240
98.276700	2921.382617	22.887258
98.385210	2915.268126	22.892275
98.404492	2920.188600	22.897293
98.198168	2927.508114	22.902311
98.516742	2933.186797	22.907328
98.849306	2937.613491	22.912346
98.945372	2940.994465	22.917363
98.964972	2939.290251	22.922381
99.060906	2952.341527	22.927399
99.575523	2954.454866	22.932416
99.762705	2956.499253	22.937434
100.207845	2958.796995	22.942451
100.100737	2944.084136	22.947469
99.996526	2938.760219	22.952487
100.110096	2945.408185	22.957504
100.477659	2937.148238	22.962522
99.974305	2928.695656	22.967539
100.224117	2927.574195	22.972557
100.156504	2936.721587	22.977575
100.025915	2951.010603	22.982592
100.151258	2942.450663	22.987610
100.060194	2945.257959	22.992627
100.059703	2956.152856	22.997645
100.380774	2968.604151	23.002663
100.851477	2968.319380	23.007680
100.618334	2967.260484	23.012698
100.534590	2980.232448	23.017715
100.820666	2995.962089	23.022733
101.048822	3002.658514	23.027751
100.966386	2998.044470	23.032768
101.522694	2994.618670	23.037786
101.019507	2998.014052	23.042803
101.399270	2996.790295	23.047821
101.008766	3014.733570	23.052839
101.797910	3016.267636	23.057856
101.767005	3017.642172	23.062874
101.914273	3024.035587	23.067891
101.615618	3025.278224	23.072909
101.989202	3036.200144	23.077927
102.023786	3041.093020	23.082944
102.583516	3035.747763	23.087962
102.026845	3051.166806	23.092979
102.602359	3045.686532	23.097997
102.778395	3053.562008	23.103015
103.278042	3045.436097	23.108032
103.880524	3039.484521	23.113050
103.220475	3034.780499	23.118067
103.427336	3016.076715	23.123085
103.529982	3016.991758	23.128103
103.210397	3023.524138	23.133120
103.307576	3023.398516	23.138138
103.748826	3041.619458	23.143155
103.944514	3044.833449	23.148173
104.110037	3049.361924	23.153191
103.972864	3045.595916	23.158208
104.001018	3042.394362	23.163226
103.921407	3044.530794	23.168243
103.835269	3041.331254	23.173261
104.043383	3048.346428	23.178279
103.828832	3059.492488	23.183296
104.455813	3054.793227	23.188314
104.351544	3069.466441	23.193331
104.660274	3061.925724	23.198349
105.091821	3062.780094	23.203367
105.086194	3060.211864	23.208384
105.214237	3047.542190	23.213402
105.340826	3060.232131	23.218419
105.452380	3052.955669	23.223437
105.448594	3062.102656	23.228455
105.485665	3070.577346	23.233472
105.858496	3075.108269	23.238490
105.968387	3088.908628	23.243507
106.228850	3082.962946	23.248525
106.068058	3079.816052	23.253543
105.868774	3078.171152	23.258560
106.265690	3071.954895	23.263578
106.284975	3072.807173	23.268595
106.264535	3076.985874	23.273613
106.685948	3080.155259	23.278631
106.371822	3078.537708	23.283648
106.415373	3077.044367	23.288666
106.270126	3090.704552	23.293683
106.593184	3097.493545	23.298701
106.771014	3109.272892	23.303719
106.620890	3106.386291	23.308736
106.512736	3108.299934	23.313754
106.420475	3129.318296	23.318771
106.887967	3132.704601	23.323789
106.828647	3149.636984	23.328807
106.978544	3161.259751	23.333824
106.931380	3160.724212	23.338842
106.977179	3179.754866	23.343859
107.487627	3185.331166	23.348877
107.903104	3188.829733	23.353895
108.147270	3186.831728	23.358912
108.027623	3193.339352	23.363930
108.075041	3198.867813	23.368947
108.078195	3203.970775	23.373965
108.512191	3210.420612	23.378983
108.084997	3207.201551	23.384000
108.538702	3209.087694	23.389018
108.892509	3226.233568	23.394035
108.943735	3230.136031	23.399053
108.790717	3235.812486	23.404071
109.154292	3232.568145	23.409088
109.453082	3234.229074	23.414106
109.205964	3236.937622	23.419123
109.463279	3228.745205	23.424141
109.376216	3233.805411	23.429159
109.284891	3247.176422	23.434176
109.996252	3252.093389	23.439194
109.600950	3258.855415	23.444211
109.818641	3253.787434	23.449229
109.857191	3249.896184	23.454247
109.967416	3266.881183	23.459264
110.119322	3271.497051	23.464282
110.673215	3277.445354	23.469299
110.533430	3284.025581	23.474317
110.749334	3278.897904	23.479335
110.891376	3274.375086	23.484352
110.482562	3276.509145	23.489370
111.055458	3285.509650	23.494387
110.825790	3294.799232	23.499405
110.867481	3293.179918	23.504423
110.764793	3304.255057	23.509440
111.335058	3300.558755	23.514458
111.690486	3318.323072	23.519475
111.935206	3319.073984	23.524493
112.206795	3319.334664	23.529511
112.164163	3325.984997	23.534528
112.555397	3320.896290	23.539546
112.466445	3321.819087	23.544563
112.294910	3323.468034	23.549581
112.182313	3322.926896	23.554599
112.106968	3319.517319	23.559616
112.403407	3318.618975	23.564634
112.418483	3333.665188	23.569651
112.318841	3340.144500	23.574669
112.912032	3335.510396	23.579687
112.940203	3337.623769	23.584704
112.986404	3335.539792	23.589722
112.975037	3364.979110	23.594739
113.056891	3359.162142	23.599757
113.393593	3353.441215	23.604775
113.420108	3372.765443	23.609792
113.627468	3372.758381	23.614810
113.386616	3389.012269	23.619827
113.790434	3385.275584	23.624845
114.118558	3387.304389	23.629863
113.875986	3393.525074	23.634880
114.042721	3398.640498	23.639898
114.260682	3407.582702	23.644915
114.312338	3405.709332	23.649933
114.671630	3406.773809	23.654951
114.473512	3418.817042	23.659968
114.795191	3408.291575	23.664986
115.138257	3428.125222	23.670003
114.712737	3434.784708	23.675021
115.080896	3426.887407	23.680039
115.235993	3433.254500	23.685056
115.097548	3421.964274	23.690074
115.190624	3436.045262	23.695091
115.418810	3449.773825	23.700109
115.822793	3445.289086	23.705127
115.860031	3453.006446	23.710144
116.102608	3439.665334	23.715162
116.267532	3441.990986	23.720179
116.053995	3448.942561	23.725197
116.637286	3459.213478	23.730215
116.655354	3473.621791	23.735232
116.482173	3474.276809	23.740250
116.599005	3481.050712	23.745267
116.716383	3480.956661	23.750285
116.623272	3473.516211	23.755303
116.670347	3467.546814	23.760320
116.865821	3483.404611	23.765338
117.004998	3493.602664	23.770355
117.407934	3495.067500	23.775373
117.537609	3492.834792	23.780391
117.196718	3495.955658	23.785408
117.560886	3491.985254	23.790426
117.798761	3509.222041	23.795443
118.076489	3517.324916	23.800461
117.983912	3515.442428	23.805479
118.026034	3521.732456	23.810496
118.418353	3510.646753	23.815514
118.336673	3518.404748	23.820531
118.420644	3511.779416	23.825549
118.741113	3522.719372	23.830567
118.773420	3534.739432	23.835584
118.922837	3536.436271	23.840602
118.825115	3547.835875	23.845619
118.651069	3541.023457	23.850637
118.754945	3549.974026	23.855655
119.023267	3558.498159	23.860672
119.195989	3565.335985	23.865690
118.975728	3566.055147	23.870707
119.340496	3580.993466	23.875725
119.554632	3579.208405	23.880743
119.844237	3590.077458	23.885760
119.923200	3602.450107	23.890778
120.123171	3611.461494	23.895795
120.013243	3609.849976	23.900813
120.457431	3611.794456	23.905831
120.274648	3617.961723	23.910848
120.505504	3623.155601	23.915866
120.852892	3628.807927	23.920883
120.788901	3645.025040	23.925901
120.939886	3637.600174	23.930919
121.074546	3635.666513	23.935936
121.416792	3644.333832	23.940954
121.638977	3641.638520	23.945971
122.017233	3651.423850	23.950989
122.161880	3649.406571	23.956007
122.550218	3647.370290	23.961024
122.261722	3640.843931	23.966042
122.639935	3640.668239	23.971059
122.204797	3636.591845	23.976077
122.754215	3636.376873	23.981095
122.361598	3645.628881	23.986112
122.593217	3645.880008	23.991130
122.826556	3634.351861	23.996147
122.570436	3647.758295	24.001165
122.625565	3641.935929	24.006183
122.824319	3642.908635	24.011200
123.093118	3647.711555	24.016218
123.112535	3658.354436	24.021235
123.216861	3660.421273	24.026253
123.501856	3654.004463	24.031271
123.578118	3660.450192	24.036288
123.377470	3664.915896	24.041306
123.669603	3669.885624	24.046323
123.118372	3686.494257	24.051341
124.114596	3695.978244	24.056359
123.738562	3709.911546	24.061376
123.820499	3711.849312	24.066394
123.818815	3717.432920	24.071411
124.124262	3723.363241	24.076429
124.332359	3718.268218	24.081447
124.212429	3729.813426	24.086464
124.641998	3744.978510	24.091482
124.450983	3744.932473	24.096499
125.180588	3764.800997	24.101517
125.095561	3760.641659	24.106535
125.114780	3765.694936	24.111552
125.460286	3782.397603	24.116570
125.647359	3783.855041	24.121587
125.490603	3794.414962	24.126605
125.248752	3791.466782	24.131623
125.725025	3816.304859	24.136640
125.650089	3814.419593	24.141658
126.129028	3812.113532	24.146675
126.331913	3835.412920	24.151693
126.540289	3844.306334	24.156711
126.609483	3842.221875	24.161728
126.579256	3843.728931	24.166746
126.854720	3838.206760	24.171763
127.025585	3846.847203	24.176781
127.272136	3858.092403	24.181799
126.976705	3860.505565	24.186816
126.992384	3868.573647	24.191834
127.788912	3864.750473	24.196851
127.606076	3874.430749	24.201869
127.762201	3882.401221	24.206887
128.092756	3876.406492	24.211904
128.196907	3884.176743	24.216922
128.390271	3884.178173	24.221939
128.447821	3888.486952	24.226957
128.452847	3897.118520	24.231975
128.817294	3907.389047	24.236992
128.790569	3915.365908	24.242010
128.912178	3910.461047	24.247027
128.830652	3909.990804	24.252045
129.045463	3902.600080	24.257063
128.839757	3916.958368	24.262080
128.882333	3935.390631	24.267098
129.434024	3937.084846	24.272115
129.412193	3945.322929	24.277133
129.425522	3951.462932	24.282151
129.866444	3959.771006	24.287168
130.160938	3964.102882	24.292186
130.162939	3954.617940	24.297203
129.815980	3968.332286	24.302221
130.303937	3974.745592	24.307239
130.518945	3982.789004	24.312256
130.671660	3986.675830	24.317274
130.726702	3979.107947	24.322291
130.748567	4002.391545	24.327309
131.239571	3997.369181	24.332327
131.225280	4005.713430	24.337344
131.073828	4010.146309	24.342362
131.391382	4007.069967	24.347379
131.549821	4020.468946	24.352397
131.586386	4024.834680	24.357415
131.979762	4030.511536	24.362432
132.029559	4029.796747	24.367450
132.207269	4031.388227	24.372467
132.092870	4034.426578	24.377485
132.281612	4031.275597	24.382503
132.502858	4039.466409	24.387520
132.361709	4048.742596	24.392538
132.403766	4050.677139	24.397555
132.619177	4057.063469	24.402573
132.982705	4057.426630	24.407591
133.364576	4066.444645	24.412608
133.231830	4077.518626	24.417626
133.391774	4068.877014	24.422643
133.520913	4072.657059	24.427661
133.708697	4076.557381	24.432679
133.535071	4087.268446	24.437696
133.788515	4103.351329	24.442714
133.956432	4103.785978	24.447731
134.156244	4098.174506	24.452749
133.962550	4100.900114	24.457767
134.239478	4115.783114	24.462784
134.168586	4121.200869	24.467802
134.215373	4123.728068	24.472819
134.474171	4136.802191	24.477837
134.574584	4139.011726	24.482855
134.964926	4150.553508	24.487872
134.956530	4171.272801	24.492890
135.170750	4162.082966	24.497907
135.123513	4166.597504	24.502925
135.267295	4178.521729	24.507943
135.799413	4191.382897	24.512960
135.532877	4200.135797	24.517978
135.890718	4192.637465	24.522995
136.207698	4215.319880	24.528013
136.121864	4215.759319	24.533031
136.041434	4227.633264	24.538048
136.392185	4233.888115	24.543066
136.987080	4237.115918	24.548083
137.156251	4241.893476	24.553101
137.023121	4246.030022	24.558119
137.363277	4240.115743	24.563136
137.484204	4238.297785	24.568154
137.667514	4244.310420	24.573171
137.739922	4257.618811	24.578189
137.738682	4264.881684	24.583207
137.962423	4259.541037	24.588224
137.747194	4267.474806	24.593242
138.209751	4259.713950	24.598259
137.998326	4267.953290	24.603277
138.235195	4281.267656	24.608295
138.905158	4275.526117	24.613312
138.767458	4281.958034	24.618330
138.975878	4270.259765	24.623347
138.978040	4286.331432	24.628365
139.122024	4298.498742	24.633383
139.581394	4298.187314	24.638400
139.485606	4303.132393	24.643418
139.891363	4294.345088	24.648435
139.614801	4292.986708	24.653453
139.723058	4296.407072	24.658471
140.281333	4312.799347	24.663488
140.210239	4317.118788	24.668506
140.652635	4318.037817	24.673523
140.293251	4325.766798	24.678541
140.522572	4322.959803	24.683559
140.739941	4319.460275	24.688576
140.476746	4331.356430	24.693594
140.887290	4341.231799	24.698611
140.774169	4343.629265	24.703629
141.210497	4349.201688	24.708647
141.635339	4359.141124	24.713664
141.851929	4367.683163	24.718682
141.646071	4362.428309	24.723699
141.904086	4371.743518	24.728717
141.919570	4371.008808	24.733735
142.187932	4376.099218	24.738752
142.261219	4378.243566	24.743770
142.199005	4381.056061	24.748787
142.488625	4393.677370	24.753805
142.533286	4405.165819	24.758823
142.689380	4402.528030	24.763840
142.212612	4392.435627	24.768858
142.503873	4406.265571	24.773875
142.635875	4412.674482	24.778893
142.784337	4429.364238	24.783911
143.039186	4432.395668	24.788928
143.244882	4446.046426	24.793946
142.989043	4452.206412	24.798963
143.681106	4457.477075	24.803981
143.714337	4471.722849	24.808999
144.405071	4471.956168	24.814016
144.122454	4495.953800	24.819034
144.612176	4488.002392	24.824051
144.770943	4493.924241	24.829069
144.704908	4494.966627	24.834087
145.286587	4492.385664	24.839104
144.912902	4492.768922	24.844122
145.310955	4501.765697	24.849139
145.495352	4500.057773	24.854157
145.681519	4506.360437	24.859175
145.673893	4509.072919	24.864192
145.613116	4511.361253	24.869210
146.018026	4514.347239	24.874227
146.013426	4525.976002	24.879245
146.266055	4541.156679	24.884263
146.440720	4527.904250	24.889280
146.446750	4531.321636	24.894298
146.497332	4546.155009	24.899315
146.356330	4554.904317	24.904333
146.468078	4561.401657	24.909351
146.817370	4568.474353	24.914368
146.827284	4577.812514	24.919386
146.958508	4589.631649	24.924403
147.375827	4592.827194	24.929421
147.255130	4608.659451	24.934439
147.717971	4613.208315	24.939456
147.565767	4627.890256	24.944474
147.802154	4637.060620	24.949491
148.391615	4635.829361	24.954509
148.028365	4655.326117	24.959527
148.454036	4653.157658	24.964544
148.618800	4659.069158	24.969562
148.758409	4665.243401	24.974579
149.182998	4664.602806	24.979597
149.006677	4675.541897	24.984615
149.626213	4677.692770	24.989632
149.554727	4674.875739	24.994650
150.021728	4665.554759	24.999667
150.295223	4665.108132	25.004685
150.178539	4663.497570	25.009703
150.508957	4664.273076	25.014720
150.506181	4675.892182	25.019738
150.771824	4680.455983	25.024755
151.167277	4681.202426	25.029773
150.992114	4689.395278	25.034791
151.309579	4684.210361	25.039808
151.210729	4680.939911	25.044826
150.936396	4688.134998	25.049843
151.465609	4678.662287	25.054861
151.088121	4693.044777	25.059879
151.342141	4704.387190	25.064896
151.457980	4707.200423	25.069914
151.195128	4705.334851	25.074931
151.939915	4719.002889	25.079949
151.974726	4740.145378	25.084967
152.438641	4737.008249	25.089984
152.225682	4730.318227	25.095002
152.225729	4752.974906	25.100019
152.523591	4753.206269	25.105037
152.463069	4764.392524	25.110055
153.111857	4772.652830	25.115072
153.108160	4779.909980	25.120090
153.028086	4786.566678	25.125107
153.275499	4785.890535	25.130125
153.053227	4796.328670	25.135143
153.520983	4800.059304	25.140160
154.071860	4803.309847	25.145178
153.912509	4812.813365	25.150195
153.850087	4825.445595	25.155213
154.153971	4832.459180	25.160231
154.426381	4846.813206	25.165248
154.559803	4855.103285	25.170266
154.472134	4861.549713	25.175283
154.849898	4870.953854	25.180301
155.298399	4877.913377	25.185319
155.410804	4888.242643	25.190336
155.134141	4891.315868	25.195354
155.030740	4894.147481	25.200371
155.489643	4898.056275	25.205389
155.347515	4916.957038	25.210407
155.588224	4921.995092	25.215424
155.715129	4936.690644	25.220442
156.079436	4946.706114	25.225459
156.401758	4958.988143	25.230477
156.292096	4962.789771	25.235495
157.040005	4973.462047	25.240512
157.044832	4988.697462	25.245530
157.000689	5000.275869	25.250547
157.183618	4990.620175	25.255565
157.537999	5008.086456	25.260583
157.704054	5012.501711	25.265600
157.804219	5020.364609	25.270618
157.683005	5018.180245	25.275635
158.343097	5033.600917	25.280653
158.408109	5039.474413	25.285671
158.700927	5029.280774	25.290688
158.957298	5033.161156	25.295706
159.226465	5043.320907	25.300723
159.790158	5054.340715	25.305741
159.879918	5053.496562	25.310759
159.673186	5046.956963	25.315776
159.894119	5054.980992	25.320794
159.826226	5055.237739	25.325811
159.837741	5046.830255	25.330829
160.086681	5053.811446	25.335847
160.078815	5046.735851	25.340864
160.580463	5052.232038	25.345882
160.341910	5070.188408	25.350899
160.474293	5070.300342	25.355917
160.556346	5079.952646	25.360935
160.563434	5081.681260	25.365952
160.964448	5099.152995	25.370970
161.298395	5088.630959	25.375987
161.309843	5101.532806	25.381005
161.569632	5113.556376	25.386023
161.841076	5122.592112	25.391040
161.957665	5122.422422	25.396058
161.797773	5130.426863	25.401075
162.417797	5141.949303	25.406093
162.445523	5149.675180	25.411111
162.198285	5156.976710	25.416128
162.818334	5145.352677	25.421146
162.642272	5155.963743	25.426163
163.239330	5158.026638	25.431181
163.131557	5165.745209	25.436199
163.168706	5164.034897	25.441216
163.246439	5159.228069	25.446234
162.787651	5179.377869	25.451251
163.653484	5173.068954	25.456269
163.636197	5190.182934	25.461287
163.891111	5202.551379	25.466304
164.102086	5209.541697	25.471322
163.777497	5224.380375	25.476339
164.112281	5233.583068	25.481357
164.267533	5240.793560	25.486375
164.434033	5245.612834	25.491392
164.962765	5258.140702	25.496410
165.197459	5271.809664	25.501427
165.269037	5273.967010	25.506445
165.335387	5288.508136	25.511463
165.619167	5298.548965	25.516480
165.704803	5292.484582	25.521498
165.908415	5301.584628	25.526515
165.988739	5311.063716	25.531533
166.094583	5320.624062	25.536551
166.475207	5333.979951	25.541568
167.041979	5338.459159	25.546586
166.930610	5339.887432	25.551603
167.258134	5341.802922	25.556621
167.289559	5340.421762	25.561639
167.220838	5355.804665	25.566656
167.217513	5357.184553	25.571674
167.388684	5375.127938	25.576691
167.745902	5389.955295	25.581709
167.773539	5391.655487	25.586727
167.931094	5409.238025	25.591744
168.220061	5419.609549	25.596762
168.379696	5427.258189	25.601779
168.676560	5437.237083	25.606797
168.429513	5452.912981	25.611815
168.827256	5455.142673	25.616832
169.173764	5474.924369	25.621850
169.214511	5488.267001	25.626867
169.272766	5473.437955	25.631885
169.798187	5496.035860	25.636903
169.525362	5500.162874	25.641920
169.848569	5511.577091	25.646938
170.170208	5533.187205	25.651955
170.382266	5534.603018	25.656973
170.416179	5537.656406	25.661991
170.520949	5556.642499	25.667008
170.911310	5549.047009	25.672026
171.173647	5565.413895	25.677044
171.575722	5567.548231	25.682061
171.447543	5580.560539	25.687079
171.573800	5574.543400	25.692096
172.140822	5580.263155	25.697114
172.129399	5594.630398	25.702132
172.587369	5592.358948	25.707149
172.494362	5601.764164	25.712167
172.554434	5592.073618	25.717184
172.639665	5601.583659	25.722202
172.883273	5622.899842	25.727220
172.966286	5627.650146	25.732237
172.941420	5627.833914	25.737255
173.105203	5649.440334	25.742272
173.556407	5647.870689	25.747290
173.566044	5651.776993	25.752308
173.874589	5664.506721	25.757325
174.256720	5664.399852	25.762343
174.369180	5668.653156	25.767360
174.554855	5660.597062	25.772378
174.951866	5666.456951	25.777396
175.080415	5671.260151	25.782413
174.997629	5675.622768	25.787431
175.429782	5687.136927	25.792448
175.773297	5686.834049	25.797466
175.724426	5694.382688	25.802484
175.803020	5685.083782	25.807501
175.952393	5689.097757	25.812519
176.129873	5686.311252	25.817536
176.602551	5690.366434	25.822554
176.530009	5708.894179	25.827572
176.121619	5707.117448	25.832589
176.456521	5712.276791	25.837607
176.257922	5724.728825	25.842624
176.719539	5735.076806	25.847642
176.709137	5740.343579	25.852660
176.785226	5759.372228	25.857677
177.095986	5766.612379	25.862695
177.206427	5786.244929	25.867712
177.421851	5796.773321	25.872730
177.667133	5812.401286	25.877748
177.963436	5819.466939	25.882765
178.012426	5831.302842	25.887783
178.037479	5846.731535	25.892800
178.433215	5848.952119	25.897818
178.812981	5867.712640	25.902836
178.880591	5865.836532	25.907853
179.119265	5877.999630	25.912871
179.141826	5889.643975	25.917888
179.568931	5901.219031	25.922906
180.038718	5916.635362	25.927924
180.244642	5927.559886	25.932941
180.249561	5921.435258	25.937959
180.407729	5930.113396	25.942976
180.906246	5943.905932	25.947994
180.915894	5949.930389	25.953012
181.142652	5952.773896	25.958029
181.474851	5958.650283	25.963047
181.149749	5960.553807	25.968064
181.805021	5972.516373	25.973082
181.677638	5973.868274	25.978100
181.936501	5976.893026	25.983117
181.864045	5988.826854	25.988135
181.735867	5999.257340	25.993152
182.002220	6005.911055	25.998170
181.984402	6015.955043	26.003188
182.198515	6025.694614	26.008205
182.502164	6045.679315	26.013223
182.613723	6060.513899	26.018240
183.021926	6076.539715	26.023258
183.290959	6083.612874	26.028276
183.633046	6092.398190	26.033293
183.915297	6106.196111	26.038311
183.916251	6111.637995	26.043328
184.287679	6121.640380	26.048346
184.316003	6133.738541	26.053364
184.461161	6136.569527	26.058381
185.008974	6146.986396	26.063399
185.093882	6156.512560	26.068416
185.332777	6158.195717	26.073434
185.521380	6169.119925	26.078452
185.641888	6169.697745	26.083469
185.821238	6178.375859	26.088487
186.067715	6184.792827	26.093504
185.716123	6183.183979	26.098522
185.889484	6199.991438	26.103540
185.844854	6202.690992	26.108557
187.031334	6226.159138	26.113575
186.499164	6234.657642	26.118592
186.981249	6230.005390	26.123610
187.099712	6246.013331	26.128628
187.356531	6245.225189	26.133645
187.486349	6246.009901	26.138663
187.613519	6255.943061	26.143680
188.008729	6253.693930	26.148698
188.247457	6263.846477	26.153716
188.422535	6275.300019	26.158733
188.633109	6277.798862	26.163751
188.290939	6293.275635	26.168768
188.765303	6301.506979	26.173786
188.985738	6303.325604	26.178804
188.634261	6313.456426	26.183821
189.468555	6323.610983	26.188839
188.939400	6337.832134	26.193856
189.646441	6353.915839	26.198874
189.684630	6358.051444	26.203892
190.436908	6369.235250	26.208909
191.169159	6369.780968	26.213927
191.153207	6376.090497	26.218944
191.051848	6373.943915	26.223962
191.470473	6375.580171	26.228980
191.487652	6371.890451	26.233997
191.762392	6369.072917	26.239015
191.425839	6383.788129	26.244032
191.799727	6387.404285	26.249050
192.092767	6390.344869	26.254068
192.254052	6398.157809	26.259085
192.779923	6407.362915	26.264103
192.484463	6422.037036	26.269120
192.947075	6427.909055	26.274138
192.954186	6422.964525	26.279156
192.841054	6440.296628	26.284173
193.434211	6441.580576	26.289191
193.247401	6452.241418	26.294208
193.644050	6455.693051	26.299226
193.877040	6479.047965	26.304244
193.798740	6482.980764	26.309261
193.853278	6498.061335	26.314279
194.120673	6502.881019	26.319296
194.583827	6514.949615	26.324314
194.859244	6523.837064	26.329332
195.006897	6537.097527	26.334349
195.280499	6543.838698	26.339367
195.341342	6561.715196	26.344384
195.171564	6564.620535	26.349402
195.432343	6575.615825	26.354420
195.796375	6589.758089	26.359437
195.814050	6597.915460	26.364455
196.229075	6617.681417	26.369472
196.332364	6617.198112	26.374490
196.767107	6629.621605	26.379508
196.079575	6648.002979	26.384525
196.608786	6663.814754	26.389543
197.023860	6670.865405	26.394560
197.389060	6694.231578	26.399578
197.545373	6701.941249	26.404596
197.474613	6715.393683	26.409613
197.928160	6722.091121	26.414631
198.412417	6737.540619	26.419648
198.481321	6753.843985	26.424666
198.696847	6753.093819	26.429684
198.938648	6766.112503	26.434701
198.997698	6775.810324	26.439719
199.507463	6781.539376	26.444736
199.687211	6778.326190	26.449754
199.715166	6795.017936	26.454772
199.928338	6798.337206	26.459789
200.110412	6803.520654	26.464807
200.129796	6806.548105	26.469824
200.191932	6820.557614	26.474842
200.609343	6814.393723	26.479860
200.859576	6833.873050	26.484877
200.888545	6841.050171	26.489895
201.096459	6851.463540	26.494912
201.328491	6861.352293	26.499930
201.175369	6866.449047	26.504948
201.467585	6888.608314	26.509965
201.958580	6897.875921	26.514983
202.082231	6906.522015	26.520000
202.158364	6916.286700	26.525018
202.318061	6927.506286	26.530036
202.828596	6946.904170	26.535053
202.877846	6953.525739	26.540071
203.533210	6952.833359	26.545088
203.529070	6970.603571	26.550106
204.032415	6975.932771	26.555124
204.073002	6984.692852	26.560141
204.316831	6982.760784	26.565159
204.073221	6998.102847	26.570176
204.157245	7003.639395	26.575194
204.619681	7011.203676	26.580212
204.745763	7022.908389	26.585229
205.460455	7033.435528	26.590247
205.243685	7049.221721	26.595264
205.556777	7052.964278	26.600282
205.824845	7059.251920	26.605300
206.083580	7070.301492	26.610317
206.558090	7077.901803	26.615335
206.379891	7087.788253	26.620352
206.371437	7103.062224	26.625370
207.211411	7103.941605	26.630388
206.905177	7111.022648	26.635405
207.388952	7119.994751	26.640423
207.239979	7127.695309	26.645440
207.552166	7140.955848	26.650458
207.844670	7154.645633	26.655476
207.692780	7165.825485	26.660493
208.147969	7172.497579	26.665511
208.786490	7181.350915	26.670528
208.611730	7195.053498	26.675546
209.227674	7193.650646	26.680564
209.142507	7202.960757	26.685581
209.258851	7209.543561	26.690599
209.486318	7227.511570	26.695616
209.580895	7239.546481	26.700634
210.570658	7235.695698	26.705652
210.165307	7254.437819	26.710669
210.472340	7260.473231	26.715687
210.410183	7265.909499	26.720704
210.716695	7268.920736	26.725722
211.213425	7267.621675	26.730740
211.574553	7297.261907	26.735757
211.841103	7299.114492	26.740775
212.266784	7295.288381	26.745792
212.266994	7292.166195	26.750810
212.299447	7293.875286	26.755828
212.002774	7309.847769	26.760845
212.608866	7317.475048	26.765863
212.651739	7323.804156	26.770880
212.504192	7343.835268	26.775898
213.199552	7339.597809	26.780916
213.313623	7354.369914	26.785933
213.228253	7370.713631	26.790951
213.568953	7374.679250	26.795968
213.831195	7384.513072	26.800986
213.896353	7393.556798	26.806004
213.765989	7414.522901	26.811021
214.517693	7423.623912	26.816039
214.578947	7428.068697	26.821056
214.824696	7446.286624	26.826074
214.872383	7451.548002	26.831092
215.200109	7473.550918	26.836109
215.179748	7479.905709	26.841127
215.553794	7488.004836	26.846144
215.823471	7515.494036	26.851162
215.846380	7519.818538	26.856180
216.113577	7539.431720	26.861197
216.590513	7548.436668	26.866215
216.572236	7567.311415	26.871232
216.555549	7572.519712	26.876250
216.976919	7584.825975	26.881268
217.421738	7598.160902	26.886285
217.505189	7612.344484	26.891303
217.824586	7619.350417	26.896320
217.987190	7632.486225	26.901338
218.609835	7630.795021	26.906356
218.798620	7646.985809	26.911373
219.221066	7649.660212	26.916391
219.285462	7662.157850	26.921408
219.565469	7663.436977	26.926426
219.670092	7673.147118	26.931444
219.618706	7686.562521	26.936461
220.188571	7694.375542	26.941479
220.636725	7710.683852	26.946496
220.355644	7711.706231	26.951514
220.463717	7720.295153	26.956532
220.594755	7740.725294	26.961549
220.759039	7755.212093	26.966567
221.003445	7768.429971	26.971584
221.182584	7782.093677	26.976602
221.418500	7797.314395	26.981620
221.753800	7818.741982	26.986637
221.971511	7833.574103	26.991655
222.380031	7837.797605	26.996672
222.376881	7865.358216	27.001690
222.392052	7861.624313	27.006708
222.953862	7878.716942	27.011725
223.176656	7885.097156	27.016743
223.774518	7900.697268	27.021760
223.500760	7915.735406	27.026778
223.817213	7928.863259	27.031796
224.399853	7941.747633	27.036813
224.234376	7952.901665	27.041831
224.897332	7961.565316	27.046848
224.968371	7971.909080	27.051866
225.587231	7992.168842	27.056884
225.311235	8001.193369	27.061901
225.425134	7997.283063	27.066919
225.767097	8012.032844	27.071936
225.720679	8025.349852	27.076954
226.078793	8035.828906	27.081972
226.211195	8048.189940	27.086989
226.135436	8073.116616	27.092007
226.778777	8082.509485	27.097024
227.143314	8100.902142	27.102042
227.207163	8102.303349	27.107060
227.851621	8133.220440	27.112077
228.368645	8136.356898	27.117095
228.873915	8118.498015	27.122112
228.659467	8123.383673	27.127130
229.133140	8123.571931	27.132148
228.886665	8135.168034	27.137165
229.287913	8133.852210	27.142183
229.309410	8145.927505	27.147200
229.353465	8144.553639	27.152218
230.020340	8169.806807	27.157236
229.609830	8172.254227	27.162253
230.038469	8173.503936	27.167271
230.309141	8187.706168	27.172288
230.606123	8191.868192	27.177306
230.773182	8192.479871	27.182324
231.283996	8216.182054	27.187341
231.361150	8223.929946	27.192359
231.412248	8224.303961	27.197376
231.696057	8242.835610	27.202394
231.846696	8245.261973	27.207412
232.113910	8262.533420	27.212429
232.234684	8273.766203	27.217447
232.430395	8292.608377	27.222464
232.537707	8313.219640	27.227482
232.770737	8310.490390	27.232500
232.867607	8333.155367	27.237517
233.540684	8347.743371	27.242535
233.747688	8352.989674	27.247552
233.775070	8370.626892	27.252570
234.309483	8379.244457	27.257588
234.553679	8394.628545	27.262605
234.714870	8409.122655	27.267623
235.140629	8409.094227	27.272640
235.007974	8422.633313	27.277658
235.116315	8437.337724	27.282676
235.619350	8448.590027	27.287693
235.884107	8468.005685	27.292711
235.851864	8478.646790	27.297728
236.014919	8499.259053	27.302746
236.501320	8500.989137	27.307764
236.762024	8516.531767	27.312781
236.851861	8534.651919	27.317799
237.239837	8545.789598	27.322816
237.611492	8561.756982	27.327834
237.958655	8565.080970	27.332852
238.065758	8583.548917	27.337869
238.570892	8596.183781	27.342887
238.669587	8605.150267	27.347904
238.593658	8622.705940	27.352922
238.802639	8638.774487	27.357940
239.089770	8649.826902	27.362957
238.522989	8662.423484	27.367975
239.446669	8670.996368	27.372992
239.713277	8697.206031	27.378010
239.811755	8710.030568	27.383028
240.423001	8724.006551	27.388045
240.651621	8742.313668	27.393063
241.324231	8742.054227	27.398080
241.049505	8762.403444	27.403098
241.390470	8767.865792	27.408116
242.022744	8781.308151	27.413133
242.276684	8783.860573	27.418151
242.610452	8780.610434	27.423168
242.891581	8803.465142	27.428186
242.688475	8809.602587	27.433204
243.059118	8807.072838	27.438221
243.185862	8829.916885	27.443239
243.508509	8837.143776	27.448256
243.443380	8850.214880	27.453274
243.596023	8859.353046	27.458292
243.995497	8870.849043	27.463309
244.018451	8888.787371	27.468327
244.247483	8901.572773	27.473344
244.519685	8909.331628	27.478362
244.439333	8923.532249	27.483380
245.291328	8935.159891	27.488397
245.416524	8951.046011	27.493415
245.733659	8953.683332	27.498432
245.705982	8970.811924	27.503450
246.051560	8986.322793	27.508468
246.276809	8999.617151	27.513485
246.535143	9011.795053	27.518503
247.182918	9023.587146	27.523520
247.064450	9032.486620	27.528538
247.210248	9046.118567	27.533556
247.558424	9061.790110	27.538573
247.754285	9090.852784	27.543591
247.677248	9092.001328	27.548608
248.298172	9112.565090	27.553626
248.335998	9124.726882	27.558644
248.611570	9138.812268	27.563661
248.972336	9162.049666	27.568679
249.135954	9164.654089	27.573696
249.789643	9185.607479	27.578714
249.713001	9197.092561	27.583732
250.159446	9221.027058	27.588749
250.043827	9238.134859	27.593767
250.264265	9242.230110	27.598784
251.078224	9256.367525	27.603802
251.434121	9270.093215	27.608820
251.661663	9279.456717	27.613837
252.078842	9297.520339	27.618855
252.589752	9304.456057	27.623872
252.529092	9310.937724	27.628890
252.548541	9319.411743	27.633908
252.540065	9333.232094	27.638925
252.944872	9344.585482	27.643943
253.451189	9358.786658	27.648960
253.406402	9361.556158	27.653978
253.189027	9385.082748	27.658996
253.629941	9404.901345	27.664013
254.190482	9419.798184	27.669031
254.638750	9423.845376	27.674048
255.147880	9431.359189	27.679066
255.291431	9441.793517	27.684084
255.925847	9454.898212	27.689101
255.833461	9459.774689	27.694119
256.473782	9467.706946	27.699136
256.362853	9477.994637	27.704154
257.125286	9477.749621	27.709172
257.332442	9476.110315	27.714189
257.061381	9484.591751	27.719207
257.536929	9498.292668	27.724224
257.815659	9496.459098	27.729242
257.748140	9518.153435	27.734260
258.346871	9523.035992	27.739277
258.426526	9533.934961	27.744295
258.493104	9539.531817	27.749312
258.693597	9555.501450	27.754330
258.788573	9565.078327	27.759348
259.525613	9570.482408	27.764365
259.209532	9581.682967	27.769383
259.321751	9606.424578	27.774400
259.825247	9625.018128	27.779418
259.817975	9639.211075	27.784436
260.032738	9651.254105	27.789453
260.508028	9679.825870	27.794471
260.615748	9693.877823	27.799488
260.912836	9712.048950	27.804506
261.044093	9720.543631	27.809524
261.516458	9741.273299	27.814541
261.637403	9758.407894	27.819559
262.169349	9777.041370	27.824576
262.520773	9791.623765	27.829594
262.688730	9806.332611	27.834612
263.110380	9802.235092	27.839629
263.107618	9816.825290	27.844647
263.629606	9836.334942	27.849664
263.967734	9840.705631	27.854682
264.032723	9862.537604	27.859700
264.704284	9864.971486	27.864717
264.975098	9872.143706	27.869735
264.925571	9887.382170	27.874752
265.261658	9908.253219	27.879770
265.305644	9918.374957	27.884788
265.592532	9922.507373	27.889805
265.963208	9939.473806	27.894823
265.994557	9952.186519	27.899840
266.085419	9973.209481	27.904858
266.044680	9995.484308	27.909876
266.722372	10007.285002	27.914893
266.835750	10034.852800	27.919911
266.582234	10049.949502	27.924928
267.258028	10073.896755	27.929946
267.721152	10090.454268	27.934964
267.879719	10104.050274	27.939981
268.222608	10128.447250	27.944999
268.710783	10143.917944	27.950016
268.999678	10159.025009	27.955034
268.970816	10182.371706	27.960052
269.419398	10202.553056	27.965069
270.009051	10202.123392	27.970087
269.928675	10215.924020	27.975104
270.982290	10229.889105	27.980122
270.918136	10249.127350	27.985140
271.481029	10254.287214	27.990157
271.564346	10255.306671	27.995175
271.973589	10273.066216	28.000192
272.377023	10280.830476	28.005210
272.442132	10288.303259	28.010228
272.728494	10303.354003	28.015245
272.819341	10305.152160	28.020263
273.039663	10328.365524	28.025280
273.527700	10336.432372	28.030298
273.487517	10360.374639	28.035316
273.855639	10363.433629	28.040333
273.984781	10386.023471	28.045351
274.092983	10399.554914	28.050368
274.628098	10410.421378	28.055386
274.650118	10437.299898	28.060404
275.221591	10444.583401	28.065421
275.405451	10455.334077	28.070439
275.462421	10467.743200	28.075456
275.497161	10491.014076	28.080474
275.903172	10513.542023	28.085492
276.461504	10519.507808	28.090509
276.764431	10546.383799	28.095527
276.701248	10563.462551	28.100544
277.341542	10579.295130	28.105562
277.827060	10599.913199	28.110580
278.095198	10604.127622	28.115597
278.337635	10631.493080	28.120615
278.380904	10632.784016	28.125632
278.867752	10651.816911	28.130650
278.782737	10676.814828	28.135668
279.699229	10681.967124	28.140685
279.729266	10696.881276	28.145703
279.692332	10706.191951	28.150720
279.939740	10721.264885	28.155738
280.332631	10737.950734	28.160756
280.981977	10742.980451	28.165773
281.114339	10757.212501	28.170791
281.176151	10765.295375	28.175808
281.623977	10777.416518	28.180826
281.929213	10786.424524	28.185844
281.894866	10801.045668	28.190861
282.201865	10804.174239	28.195879
282.405839	10820.725387	28.200896
282.925977	10840.618434	28.205914
282.838784	10867.400908	28.210932
282.847238	10865.126194	28.215949
283.103922	10891.406805	28.220967
283.424782	10915.186221	28.225984
284.332804	10944.601909	28.231002
284.237683	10963.053184	28.236020
284.725258	10978.736218	28.241037
284.935868	10995.078094	28.246055
285.301554	11013.754482	28.251072
285.485491	11030.792030	28.256090
285.830929	11048.230712	28.261108
286.176032	11066.342009	28.266125
286.454141	11079.746454	28.271143
286.111824	11103.092580	28.276160
286.496987	11113.856501	28.281178
286.756191	11142.385215	28.286196
287.413356	11160.716407	28.291213
287.703552	11177.775437	28.296231
287.766999	11214.054855	28.301248
288.088381	11226.963254	28.306266
288.842489	11251.114541	28.311284
289.271503	11270.719112	28.316301
289.990839	11281.162714	28.321319
290.250268	11293.626119	28.326336
290.658610	11295.078134	28.331354
290.732032	11307.557877	28.336372
290.898385	11316.322529	28.341389
291.534317	11337.764217	28.346407
291.840725	11340.179367	28.351424
292.351636	11346.045447	28.356442
292.446342	11364.331790	28.361460
292.763947	11364.260214	28.366477
293.233931	11361.660982	28.371495
293.093715	11390.883767	28.376512
293.666832	11380.437760	28.381530
293.784260	11408.932117	28.386548
294.305270	11406.811198	28.391565
294.151966	11418.116971	28.396583
294.270464	11432.058041	28.401600
294.757380	11431.988524	28.406618
295.362951	11446.542122	28.411636
295.610749	11459.594755	28.416653
295.914194	11472.228251	28.421671
295.822612	11493.224492	28.426688
295.852816	11499.462270	28.431706
295.977251	11513.730864	28.436724
296.033266	11529.993076	28.441741
296.775129	11553.654081	28.446759
296.923140	11577.710698	28.451776
297.309500	11590.403989	28.456794
297.668150	11612.072300	28.461812
297.933598	11640.774469	28.466829
298.438717	11645.201684	28.471847
298.112657	11676.446287	28.476864
298.751213	11682.415747	28.481882
298.862956	11716.936154	28.486900
299.357993	11723.123743	28.491917
299.776584	11741.574747	28.496935
299.973784	11759.940247	28.501952
300.231641	11770.010746	28.506970
300.385303	11795.613992	28.511988
300.518023	11813.440158	28.517005
301.483764	11826.046566	28.522023
301.084093	11844.820835	28.527040
301.597813	11866.310575	28.532058
301.989021	11895.230377	28.537076
301.960429	11901.546910	28.542093
302.412695	11923.298894	28.547111
302.597162	11948.727040	28.552128
303.315597	11965.142269	28.557146
303.297216	11987.854899	28.562164
303.509393	12011.377911	28.567181
304.308924	12019.513831	28.572199
304.262530	12050.305019	28.577216
304.607291	12065.742799	28.582234
304.746354	12082.876705	28.587252
305.264249	12097.321312	28.592269
305.902001	12121.217124	28.597287
306.246398	12143.169301	28.602304
306.914361	12149.244852	28.607322
307.198120	12162.544991	28.612340
307.744831	12178.235614	28.617357
308.157765	12179.570152	28.622375
308.174982	12182.459881	28.627392
308.320861	12193.886898	28.632410
308.513118	12200.538598	28.637428
308.636788	12219.351756	28.642445
309.021061	12224.281050	28.647463
308.988037	12257.441920	28.652480
309.190559	12275.674473	28.657498
309.723221	12295.500808	28.662516
310.000793	12317.542535	28.667533
310.030217	12346.538302	28.672551
310.139558	12372.177653	28.677568
310.644618	12395.838697	28.682586
310.891730	12417.796868	28.687604
311.249921	12443.861759	28.692621
311.853068	12468.720191	28.697639
312.023321	12489.203120	28.702656
312.309741	12502.976745	28.707674
312.692131	12520.464727	28.712692
312.715284	12551.084862	28.717709
313.171061	12571.646581	28.722727
313.201480	12600.579428	28.727744
314.216115	12624.060380	28.732762
314.236515	12652.694880	28.737780
314.550668	12673.730319	28.742797
315.334937	12690.647493	28.747815
315.373134	12707.879774	28.752832
315.698164	12728.357813	28.757850
316.159488	12742.975929	28.762868
316.418333	12771.879793	28.767885
317.010909	12782.167137	28.772903
317.516403	12807.994870	28.777920
317.621159	12829.113608	28.782938
317.759960	12837.586427	28.787956
318.067501	12868.860674	28.792973
318.403126	12873.080895	28.797991
318.431564	12902.125035	28.803008
318.823378	12906.784923	28.808026
319.427160	12931.280721	28.813044
319.535249	12952.585388	28.818061
319.696612	12964.960963	28.823079
320.039428	12985.417567	28.828096
320.371893	13013.091421	28.833114
320.644967	13031.746344	28.838132
320.911582	13051.545423	28.843149
321.510587	13063.129787	28.848167
321.395188	13083.357840	28.853184
321.713999	13098.740510	28.858202
322.124642	13112.637344	28.863220
322.666274	13144.996637	28.868237
322.970469	13147.014481	28.873255
323.550232	13166.483881	28.878272
324.494465	13165.828439	28.883290
326.233974	13144.040051	28.888308
326.580989	13145.204926	28.893325
327.147853	13129.482176	28.898343
327.334255	13112.129228	28.903360
327.311215	13111.832794	28.908378
327.666408	13104.779703	28.913396
327.562047	13107.420085	28.918413
327.255344	13100.068998	28.923431
327.940144	13106.230662	28.928448
327.683434	13104.650630	28.933466
328.067738	13113.022197	28.938484
328.173314	13123.736066	28.943501
328.400422	13139.079364	28.948519
328.594339	13151.869987	28.953536
328.665786	13168.974357	28.958554
329.081922	13189.040825	28.963572
329.393130	13214.731999	28.968589
329.546205	13227.857450	28.973607
329.475366	13255.079717	28.978624
329.901991	13280.933011	28.983642
330.138663	13302.628577	28.988660
330.363933	13322.510168	28.993677
331.120159	13343.622794	28.998695
331.234197	13378.092203	29.003712
331.511828	13394.302575	29.008730
331.851831	13419.572704	29.013748
331.947739	13449.412443	29.018765
332.560268	13478.764432	29.023783
332.824542	13505.849626	29.028800
333.456239	13519.349187	29.033818
333.944130	13534.873260	29.038836
334.019273	13558.504802	29.043853
335.067474	13578.233281	29.048871
335.218091	13608.917392	29.053888
335.407822	13624.314271	29.058906
336.045456	13636.019292	29.063924
336.222404	13659.000368	29.068941
336.453351	13682.528860	29.073959
336.589587	13688.024531	29.078976
337.282858	13712.851628	29.083994
337.543171	13724.751238	29.089012
337.339275	13754.748661	29.094029
337.973937	13770.057443	29.099047
338.118359	13799.861761	29.104064
338.362794	13822.324097	29.109082
338.580774	13843.315812	29.114100
339.031050	13869.867295	29.119117
339.691404	13891.822848	29.124135
339.807310	13926.422440	29.129152
339.965069	13949.681598	29.134170
340.642845	13966.130173	29.139188
340.596881	13993.693847	29.144205
340.981565	14006.922732	29.149223
341.491045	14039.468568	29.154240
341.561340	14071.305967	29.159258
342.426804	14090.700263	29.164276
342.572746	14117.899493	29.169293
342.736399	14135.584085	29.174311
343.440825	14159.342625	29.179328
343.716236	14176.176141	29.184346
344.217475	14188.392232	29.189364
344.450019	14214.100167	29.194381
344.856850	14224.802498	29.199399
345.275921	14243.783270	29.204416
345.550143	14260.215976	29.209434
345.936343	14269.579382	29.214452
346.723835	14287.378583	29.219469
346.774271	14313.762400	29.224487
346.911514	14323.467763	29.229504
346.997569	14349.053416	29.234522
347.938845	14344.908767	29.239540
348.200770	14368.385917	29.244557
348.318399	14389.703347	29.249575
348.961209	14401.635419	29.254592
349.144316	14417.248721	29.259610
349.607753	14430.162467	29.264628
349.707424	14453.996579	29.269645
349.723429	14483.727220	29.274663
350.434524	14495.913998	29.279680
350.520899	14519.364977	29.284698
350.953461	14525.092669	29.289716
351.335334	14561.328947	29.294733
351.814844	14582.789215	29.299751
352.433894	14596.231513	29.304768
352.255901	14624.066145	29.309786
352.854099	14644.102655	29.314804
352.951887	14664.213933	29.319821
353.382022	14687.011564	29.324839
354.240399	14703.558988	29.329856
354.293826	14727.605918	29.334874
354.655639	14731.822481	29.339892
355.000870	14756.998835	29.344909
355.300384	14781.114897	29.349927
355.937798	14805.601573	29.354944
356.214809	14822.697537	29.359962
356.486178	14848.722414	29.364980
356.583810	14871.290957	29.369997
357.456242	14878.172472	29.375015
358.008688	14901.958763	29.380032
357.859341	14914.886128	29.385050
358.215042	14933.053182	29.390068
358.587097	14962.621763	29.395085
358.925810	14984.363372	29.400103
359.721944	15002.758791	29.405120
359.728598	15032.782294	29.410138
359.818700	15044.503951	29.415156
360.365949	15083.624142	29.420173
360.253205	15098.282923	29.425191
360.721679	15121.946760	29.430208
360.927633	15153.985922	29.435226
361.370488	15172.149110	29.440244
361.873250	15208.607821	29.445261
362.045489	15238.918530	29.450279
362.517777	15255.605499	29.455296
362.822191	15286.862114	29.460314
363.521175	15310.951397	29.465332
363.549210	15337.396966	29.470349
363.976581	15360.416908	29.475367
364.982913	15386.921843	29.480384
364.991224	15418.126866	29.485402
365.504434	15439.920784	29.490420
365.834749	15457.283785	29.495437
365.925229	15486.887540	29.500455
366.767860	15510.632573	29.505472
367.085060	15527.037575	29.510490
367.021195	15540.075226	29.515508
367.643945	15562.278593	29.520525
368.117470	15596.433921	29.525543
368.406082	15601.069488	29.530560
368.799103	15632.859252	29.535578
369.069006	15648.150541	29.540596
369.560167	15659.459572	29.545613
369.409463	15681.938246	29.550631
370.145607	15694.924095	29.555648
370.447606	15723.326729	29.560666
370.970903	15738.894469	29.565684
371.715035	15750.476840	29.570701
371.695043	15768.270494	29.575719
372.099155	15794.591823	29.580736
372.432283	15814.064443	29.585754
372.736393	15825.191088	29.590772
373.473186	15845.043056	29.595789
373.533279	15870.972729	29.600807
373.989243	15882.893764	29.605824
374.220611	15914.026971	29.610842
374.674856	15934.955785	29.615860
375.049870	15957.817208	29.620877
375.362083	15985.722787	29.625895
376.020752	15996.102662	29.630912
376.447055	16019.177257	29.635930
377.022954	16033.214738	29.640948
377.444722	16046.947760	29.645965
377.878363	16067.772545	29.650983
377.761270	16081.902157	29.656000
377.808966	16111.216655	29.661018
378.474699	16126.329846	29.666036
378.453526	16157.190088	29.671053
378.893932	16181.191234	29.676071
379.240754	16204.777445	29.681088
379.682815	16240.034768	29.686106
380.107187	16265.702970	29.691124
380.568848	16291.529636	29.696141
380.534979	16323.797594	29.701159
380.795665	16361.840635	29.706176
381.003114	16393.291022	29.711194
381.741912	16418.834678	29.716212
382.084879	16461.703752	29.721229
382.420617	16488.197757	29.726247
383.052498	16521.152000	29.731264
383.415996	16541.381807	29.736282
383.768460	16578.112883	29.741300
384.610743	16596.291044	29.746317
384.341315	16628.773057	29.751335
385.367267	16653.087914	29.756352
385.670139	16677.227954	29.761370
386.129391	16704.903232	29.766388
386.615119	16738.303832	29.771405
386.792053	16764.627118	29.776423
387.513477	16778.279271	29.781440
387.649283	16805.910296	29.786458
388.108497	16828.747016	29.791476
388.457009	16847.488689	29.796493
388.688226	16883.459086	29.801511
389.237579	16905.479615	29.806528
389.584133	16936.921870	29.811546
389.946236	16956.327970	29.816564
390.271533	16975.250256	29.821581
390.605613	17007.872680	29.826599
390.801266	17033.599625	29.831616
391.668772	17055.147559	29.836634
392.294738	17077.936506	29.841652
392.948512	17100.793796	29.846669
393.134150	17117.002706	29.851687
393.661550	17137.769837	29.856704
394.012936	17142.860308	29.861722
394.011026	17175.026803	29.866740
394.295601	17187.389099	29.871757
394.720819	17211.861359	29.876775
395.049872	17232.924787	29.881792
395.426736	17264.805051	29.886810
395.636015	17278.707853	29.891828
396.456652	17303.235536	29.896845
396.385817	17326.126938	29.901863
396.960091	17350.819377	29.906880
397.254379	17369.892171	29.911898
397.773119	17400.291327	29.916916
398.227002	17417.349439	29.921933
398.303491	17441.345644	29.926951
399.004886	17470.301443	29.931968
399.692443	17484.963795	29.936986
400.180507	17513.336951	29.942004
400.691581	17531.457014	29.947021
401.064526	17551.923306	29.952039
401.113606	17558.567588	29.957056
401.566610	17579.969017	29.962074
402.143480	17593.505280	29.967092
402.049678	17623.134698	29.972109
402.477259	17648.911640	29.977127
402.816097	17677.633603	29.982144
403.348818	17699.591302	29.987162
403.757463	17729.837553	29.992180
404.384149	17752.980951	29.997197
404.485102	17782.453949	30.002215
404.591969	17812.734676	30.007232
404.981520	17847.121867	30.012250
405.645358	17873.285583	30.017268
406.079253	17905.726580	30.022285
406.345871	17935.622546	30.027303
406.700126	17960.937524	30.032320
407.197066	17998.795402	30.037338
407.487767	18029.572184	30.042356
407.641266	18050.761753	30.047373
408.164650	18094.636093	30.052391
408.470238	18134.191797	30.057408
408.684901	18167.128527	30.062426
409.286071	18209.853897	30.067444
410.040156	18241.885521	30.072461
410.037174	18272.986374	30.077479
410.702654	18311.109224	30.082496
410.952103	18348.583049	30.087514
411.435623	18382.034221	30.092532
412.037942	18405.131655	30.097549
412.473496	18442.639864	30.102567
412.929043	18475.716506	30.107584
413.502496	18515.648239	30.112602
413.818527	18539.264212	30.117620
414.261652	18571.919682	30.122637
414.623827	18593.203707	30.127655
415.124611	18621.061634	30.132672
415.575648	18647.322702	30.137690
416.231218	18670.608006	30.142708
416.819176	18704.681543	30.147725
416.799758	18739.310876	30.152743
417.577790	18763.562762	30.157760
418.040233	18802.577372	30.162778
418.409507	18824.031119	30.167796
418.676587	18853.467247	30.172813
418.956417	18879.464674	30.177831
419.689624	18902.782394	30.182848
420.122849	18933.418388	30.187866
420.333493	18971.423818	30.192884
421.228213	18976.085879	30.197901
421.317813	19012.436068	30.202919
421.746395	19023.450421	30.207936
422.602594	19047.551506	30.212954
422.658321	19067.045329	30.217972
423.109506	19081.695154	30.222989
422.972535	19113.254128	30.228007
423.474640	19135.515153	30.233024
423.621215	19157.730469	30.238042
423.888261	19191.962221	30.243060
424.388020	19215.708357	30.248077
425.137490	19257.092550	30.253095
425.239569	19291.407019	30.258112
426.090429	19322.363989	30.263130
426.326229	19345.412203	30.268148
427.213753	19370.949254	30.273165
427.330002	19403.486431	30.278183
427.766762	19426.876203	30.283200
428.596693	19455.587525	30.288218
428.727567	19481.368872	30.293236
429.587010	19503.757903	30.298253
429.796731	19533.778908	30.303271
430.215836	19559.073240	30.308288
430.517760	19587.184635	30.313306
430.888269	19605.574919	30.318324
431.223913	19634.793067	30.323341
431.766898	19668.944793	30.328359
432.021092	19686.064424	30.333376
432.655746	19724.093762	30.338394
432.783998	19767.546920	30.343412
433.412263	19780.874543	30.348429
434.459086	19796.544124	30.353447
435.123847	19818.073006	30.358464
435.698857	19852.030532	30.363482
435.850187	19866.898213	30.368500
436.713725	19881.162235	30.373517
436.732464	19917.019709	30.378535
436.992029	19926.411914	30.383552
437.604375	19953.824766	30.388570
437.619434	19983.763045	30.393588
437.911380	20012.148276	30.398605
438.094237	20045.149999	30.403623
438.627556	20075.968065	30.408640
439.099100	20105.671199	30.413658
439.566301	20150.702478	30.418676
440.160388	20179.521082	30.423693
440.158698	20221.750834	30.428711
440.276473	20254.895720	30.433728
441.101759	20282.086343	30.438746
441.456132	20323.578535	30.443764
441.877705	20349.562176	30.448781
442.201941	20387.925445	30.453799
442.542344	20418.805675	30.458816
443.826389	20452.394821	30.463834
444.302548	20495.599574	30.468852
445.083376	20509.775844	30.473869
445.624140	20533.883652	30.478887
446.124037	20552.115687	30.483904
446.463894	20575.749375	30.488922
446.625076	20609.703142	30.493940
447.524149	20629.256777	30.498957
447.661427	20655.967441	30.503975
448.132113	20680.364338	30.508992
448.386711	20699.721422	30.514010
448.853204	20735.719188	30.519028
449.464435	20754.730170	30.524045
449.609218	20791.283576	30.529063
449.729012	20818.047729	30.534080
450.560344	20854.007869	30.539098
450.480585	20882.073136	30.544116
450.907351	20910.565046	30.549133
451.399393	20946.034808	30.554151
451.854346	20973.423047	30.559168
452.106107	21002.321429	30.564186
452.056195	21037.313402	30.569204
453.183105	21067.181335	30.574221
453.815906	21095.565619	30.579239
453.959043	21124.064084	30.584256
454.810857	21155.731466	30.589274
455.227397	21189.697029	30.594292
455.781985	21217.923071	30.599309
456.215096	21252.600134	30.604327
456.593396	21283.147272	30.609344
457.141449	21309.668510	30.614362
457.195248	21336.683740	30.619380
457.891561	21367.251003	30.624397
458.172763	21404.978485	30.629415
458.194284	21429.711612	30.634432
459.459474	21463.305432	30.639450
459.838045	21493.966587	30.644468
460.359004	21528.207126	30.649485
460.848710	21557.473661	30.654503
461.370797	21589.679594	30.659520
461.921317	21619.221084	30.664538
462.308620	21648.067722	30.669556
462.342897	21671.712391	30.674573
463.297857	21707.970774	30.679591
463.540082	21741.402082	30.684608
464.205203	21777.415064	30.689626
464.495703	21810.491455	30.694644
464.821004	21846.165718	30.699661
465.058688	21880.116086	30.704679
465.272785	21923.105715	30.709696
466.042315	21953.624580	30.714714
466.449347	21998.517818	30.719732
466.995957	22029.697044	30.724749
467.359441	22069.782460	30.729767
467.939910	22114.661598	30.734784
468.040000	22148.937143	30.739802
468.541825	22192.571295	30.744820
469.288788	22233.115472	30.749837
469.714346	22270.108128	30.754855
469.836929	22315.532906	30.759872
470.454941	22346.827890	30.764890
470.869267	22398.791516	30.769908
471.588119	22436.446519	30.774925
472.310032	22465.198030	30.779943
472.941808	22502.620285	30.784960
473.991969	22523.409720	30.789978
475.087067	22552.248593	30.794996
475.351840	22569.969373	30.800013
475.889486	22592.134014	30.805031
476.316729	22624.716573	30.810048
476.928340	22641.005930	30.815066
477.525069	22651.282131	30.820084
478.067093	22667.917238	30.825101
478.847493	22681.728661	30.830119
479.123630	22693.230089	30.835136
479.567081	22715.479040	30.840154
479.546612	22737.427427	30.845172
480.305045	22751.905795	30.850189
480.610639	22782.485530	30.855207
480.682396	22794.385326	30.860224
481.543776	22810.162027	30.865242
481.848040	22849.620041	30.870260
482.042841	22869.538306	30.875277
482.793387	22898.311266	30.880295
482.522675	22924.740980	30.885312
483.207765	22958.446621	30.890330
483.571385	22984.613373	30.895348
483.904225	23011.062983	30.900365
484.467050	23042.911087	30.905383
484.788876	23066.967620	30.910400
485.031581	23102.069347	30.915418
485.239934	23141.170055	30.920436
486.002602	23177.006111	30.925453
486.507060	23212.686542	30.930471
486.936513	23253.541319	30.935488
487.310232	23296.376380	30.940506
487.516490	23331.958112	30.945524
487.865480	23368.332840	30.950541
488.571394	23410.996372	30.955559
488.842240	23465.462190	30.960576
489.208715	23508.223007	30.965594
489.647830	23555.263258	30.970612
490.001277	23600.516017	30.975629
491.104760	23639.554183	30.980647
491.196335	23686.389765	30.985664
491.657172	23738.204318	30.990682
492.148641	23780.396497	30.995700
492.874436	23839.468680	31.000717
493.626388	23874.732620	31.005735
493.972860	23918.950844	31.010752
495.000018	23962.197467	31.015770
495.395186	24004.379835	31.020788
495.653323	24029.218391	31.025805
496.451413	24055.578004	31.030823
497.139265	24112.148167	31.035840
497.856258	24144.296319	31.040858
498.269312	24182.646808	31.045876
498.712779	24210.098193	31.050893
499.424976	24252.705679	31.055911
499.821891	24292.272196	31.060928
500.444506	24331.917403	31.065946
500.958806	24361.279043	31.070964
501.083962	24400.963914	31.075981
502.158131	24419.906361	31.080999
502.330287	24469.303210	31.086016
502.784745	24511.218325	31.091034
503.484981	24543.710976	31.096052
503.860112	24581.221337	31.101069
504.519676	24611.066281	31.106087
504.944990	24631.569725	31.111104
506.344534	24660.225246	31.116122
507.558449	24666.734830	31.121140
507.923643	24693.921012	31.126157
508.335500	24705.781644	31.131175
508.735514	24725.259055	31.136192
508.993454	24741.099641	31.141210
509.764277	24767.894165	31.146228
510.082802	24789.210648	31.151245
510.727703	24809.212450	31.156263
511.008702	24837.442008	31.161280
511.304996	24855.867701	31.166298
511.926066	24880.037825	31.171316
511.870068	24910.253713	31.176333
512.347816	24939.495503	31.181351
512.915200	24965.829042	31.186368
513.623441	24995.243576	31.191386
514.307351	25022.323712	31.196404
514.562497	25052.769437	31.201421
514.908591	25086.253395	31.206439
515.098999	25112.671092	31.211456
515.469784	25145.847967	31.216474
516.198426	25182.697743	31.221492
516.286760	25221.688499	31.226509
516.954066	25250.067046	31.231527
517.120391	25288.653975	31.236544
517.762834	25327.975770	31.241562
518.320335	25366.609386	31.246580
518.658005	25404.310390	31.251597
519.045120	25439.987794	31.256615
519.815088	25474.145814	31.261632
520.372924	25520.477045	31.266650
520.885240	25554.131817	31.271668
520.974935	25602.406748	31.276685
521.463746	25627.356730	31.281703
522.123161	25678.627179	31.286720
522.490939	25712.917734	31.291738
522.806828	25760.766006	31.296756
523.359404	25807.136635	31.301773
524.196122	25841.126893	31.306791
524.825201	25897.369982	31.311808
525.260539	25929.849242	31.316826
526.227900	25983.309745	31.321844
526.320036	26024.993717	31.326861
527.030464	26066.853276	31.331879
527.550761	26118.658412	31.336896
528.431652	26147.491610	31.341914
528.817100	26193.402514	31.346932
529.332516	26230.546524	31.351949
529.974629	26275.545511	31.356967
530.227815	26314.455839	31.361984
530.609309	26361.638051	31.367002
531.262827	26406.123636	31.372020
531.632519	26458.054210	31.377037
532.377003	26495.921446	31.382055
533.214088	26552.405741	31.387072
533.396532	26585.146627	31.392090
534.126899	26623.186941	31.397108
534.913358	26668.208573	31.402125
535.211788	26709.014954	31.407143
536.154480	26745.910114	31.412160
536.513638	26796.212616	31.417178
537.057164	26839.761946	31.422196
537.373295	26876.249276	31.427213
538.089916	26921.882756	31.432231
538.023451	26964.876343	31.437248
538.974429	27005.588056	31.442266
539.907477	27041.663638	31.447284
540.578182	27077.558918	31.452301
541.605746	27105.504789	31.457319
542.193159	27145.540241	31.462336
542.544821	27176.138473	31.467354
543.203245	27204.894053	31.472372
543.548856	27246.313554	31.477389
544.104532	27282.321908	31.482407
544.739596	27315.587617	31.487424
545.025777	27356.492013	31.492442
545.312168	27400.404913	31.497460
545.649303	27437.136474	31.502477
546.425293	27471.688802	31.507495
546.705594	27512.998928	31.512512
546.764607	27560.512230	31.517530
547.342429	27597.901850	31.522548
547.999300	27653.589308	31.527565
549.008741	27693.642307	31.532583
549.512132	27742.521580	31.537600
549.996679	27796.510791	31.542618
550.639169	27821.610213	31.547636
550.992084	27877.598420	31.552653
551.393201	27913.271690	31.557671
551.928395	27961.571379	31.562688
552.570693	27998.856892	31.567706
553.367706	28042.217652	31.572724
554.271801	28076.327595	31.577741
554.976753	28097.846558	31.582759
555.863020	28124.760311	31.587776
556.485598	28164.002234	31.592794
557.075200	28185.608773	31.597812
557.430235	28213.376448	31.602829
557.977221	28238.554459	31.607847
558.204595	28269.154724	31.612864
558.419084	28312.448731	31.617882
558.989467	28342.281484	31.622900
559.076749	28387.283046	31.627917
559.735731	28422.114351	31.632935
560.488815	28465.514455	31.637952
560.903592	28507.134336	31.642970
561.490811	28553.038133	31.647988
562.041580	28604.756388	31.653005
562.743438	28649.884078	31.658023
563.251315	28692.867750	31.663040
563.700294	28723.326747	31.668058
564.719417	28764.119871	31.673076
565.405762	28807.284585	31.678093
565.646025	28848.350823	31.683111
566.171598	28893.253664	31.688128
566.639693	28939.296968	31.693146
567.285587	28974.422008	31.698164
567.612647	29031.814297	31.703181
568.328543	29068.413987	31.708199
569.259840	29119.859400	31.713216
569.501860	29160.850142	31.718234
570.158657	29197.339167	31.723252
570.372763	29245.717164	31.728269
571.167894	29291.065621	31.733287
571.930324	29336.874373	31.738304
572.772952	29386.703474	31.743322
573.132264	29428.485566	31.748340
573.562335	29489.093084	31.753357
574.375957	29527.068985	31.758375
575.072658	29578.103284	31.763392
575.453580	29631.550913	31.768410
576.050908	29665.262481	31.773428
576.445644	29718.095048	31.778445
577.158405	29757.604118	31.783463
577.557535	29811.087304	31.788480
578.391246	29854.793857	31.793498
578.921287	29898.339182	31.798516
579.131782	29950.530997	31.803533
579.768013	30004.211655	31.808551
580.382184	30042.421835	31.813568
580.904525	30086.373307	31.818586
581.565161	30145.063175	31.823604
581.918002	30193.390200	31.828621
582.559854	30247.639521	31.833639
583.492861	30293.664058	31.838656
583.590559	30341.013439	31.843674
584.935020	30382.182661	31.848692
585.537026	30422.892316	31.853709
586.107822	30467.930630	31.858727
586.962332	30511.489954	31.863744
587.301706	30554.832464	31.868762
588.013236	30605.247521	31.873780
588.631023	30648.502638	31.878797
589.516409	30676.424975	31.883815
590.411361	30709.877001	31.888832
591.028828	30744.567006	31.893850
591.970617	30767.967271	31.898868
592.087152	30815.599268	31.903885
592.765591	30839.407249	31.908903
593.149767	30861.124450	31.913920
594.096909	30886.275030	31.918938
594.455843	30913.249263	31.923956
594.953026	30946.068245	31.928973
595.268900	30976.627163	31.933991
596.036230	31003.828722	31.939008
596.460023	31041.514109	31.944026
596.683604	31076.367133	31.949044
596.944075	31123.408504	31.954061
597.209508	31161.814121	31.959079
598.224496	31200.526660	31.964096
598.753769	31249.580945	31.969114
599.400017	31293.224913	31.974132
599.868996	31344.318004	31.979149
600.093629	31400.873116	31.984167
601.470379	31437.298289	31.989184
601.678897	31482.780826	31.994202
602.423360	31521.896409	31.999220
602.735324	31562.444852	32.004237
603.250108	31622.495475	32.009255
604.352865	31671.398267	32.014272
604.818489	31727.727107	32.019290
605.491857	31768.200726	32.024308
606.079074	31828.759044	32.029325
606.260581	31877.034495	32.034343
607.371855	31909.582400	32.039360
607.721363	31963.180030	32.044378
608.408675	32003.658259	32.049396
608.877744	32070.911388	32.054413
609.293201	32122.969307	32.059431
610.122373	32169.393492	32.064448
610.821451	32230.523489	32.069466
611.079539	32283.232162	32.074484
612.120654	32336.305850	32.079501
612.908724	32384.772534	32.084519
613.807152	32422.430795	32.089536
614.276446	32472.540408	32.094554
615.363900	32512.514809	32.099572
615.496890	32569.081043	32.104589
616.047377	32604.751836	32.109607
617.047501	32648.311955	32.114624
617.085213	32705.683628	32.119642
618.037320	32752.235380	32.124660
618.488920	32803.448557	32.129677
619.230514	32859.800719	32.134695
619.982497	32906.959269	32.139712
620.236077	32960.561753	32.144730
620.881810	33006.889923	32.149748
621.604088	33058.794941	32.154765
622.108173	33112.478935	32.159783
622.798196	33147.212240	32.164800
623.376665	33211.872623	32.169818
623.965432	33258.728629	32.174836
624.705452	33312.268932	32.179853
625.184614	33375.288892	32.184871
625.446378	33411.682476	32.189888
626.278828	33473.996557	32.194906
627.455641	33514.218177	32.199924
628.205963	33571.841652	32.204941
628.567426	33618.120597	32.209959
629.581498	33659.006371	32.214976
629.933820	33722.072407	32.219994
631.124762	33762.387139	32.225012
631.287710	33807.736426	32.230029
632.089579	33837.560052	32.235047
632.991796	33876.402609	32.240064
633.235221	33927.840612	32.245082
633.784788	33966.744557	32.250100
634.586868	34016.110611	32.255117
634.982688	34062.960518	32.260135
635.428320	34097.461584	32.265152
635.922998	34136.583026	32.270170
636.390800	34188.505169	32.275188
636.897840	34229.711237	32.280205
637.209534	34291.508189	32.285223
638.101023	34338.989656	32.290240
638.551911	34396.232086	32.295258
639.141308	34438.279268	32.300276
640.032933	34500.947565	32.305293
640.574174	34556.115245	32.310311
641.462034	34603.382910	32.315328
641.916298	34652.387319	32.320346
643.061243	34705.937691	32.325364
643.954752	34753.938227	32.330381
644.288951	34801.842587	32.335399
644.767047	34847.372665	32.340416
645.176656	34908.934894	32.345434
646.039750	34965.463476	32.350452
646.545092	35016.553556	32.355469
647.214682	35072.606739	32.360487
647.860301	35114.633874	32.365504
648.681875	35173.812338	32.370522
648.953944	35238.558264	32.375540
650.094983	35278.346249	32.380557
650.946056	35342.237314	32.385575
651.768457	35382.846468	32.390592
652.757235	35429.752528	32.395610
653.134916	35480.364107	32.400628
653.946035	35522.328353	32.405645
654.629537	35568.624676	32.410663
655.224482	35618.336544	32.415680
655.759260	35663.790007	32.420698
657.244615	35700.205719	32.425716
657.624243	35741.794974	32.430733
658.320025	35783.290835	32.435751
658.707180	35818.195835	32.440768
659.471821	35868.880884	32.445786
659.736147	35921.053940	32.450804
660.747810	35971.169658	32.455821
660.854641	36031.018197	32.460839
661.563024	36075.857488	32.465856
662.369678	36133.687853	32.470874
662.996208	36187.619861	32.475892
663.232398	36239.886601	32.480909
663.964364	36291.836017	32.485927
664.317505	36344.824597	32.490944
665.147512	36401.438040	32.495962
665.808983	36452.203771	32.500980
666.841398	36502.488235	32.505997
667.401413	36564.449179	32.511015
668.775151	36610.886927	32.516032
669.569596	36661.885383	32.521050
669.889865	36712.009309	32.526068
670.671427	36752.108950	32.531085
671.353583	36801.436946	32.536103
672.372613	36836.087175	32.541120
673.369836	36881.977107	32.546138
673.631300	36928.120783	32.551156
674.412236	36958.350438	32.556173
674.969961	37012.497590	32.561191
675.634554	37056.017892	32.566208
675.977082	37100.037368	32.571226
676.502208	37152.476355	32.576244
677.355840	37179.963370	32.581261
678.212430	37235.430384	32.586279
679.313599	37274.241895	32.591296
679.744507	37314.384533	32.596314
679.815223	37351.048595	32.601332
680.556299	37393.274049	32.606349
680.846762	37433.773910	32.611367
681.666885	37486.066621	32.616384
682.237310	37528.584488	32.621402
682.815454	37585.910560	32.626420
683.193827	37631.620212	32.631437
683.864071	37687.490487	32.636455
684.426769	37745.047031	32.641472
685.159568	37803.007243	32.646490
685.379419	37859.700567	32.651508
686.516139	37914.360597	32.656525
687.122457	37978.854142	32.661543
687.875164	38039.916726	32.666560
688.642166	38098.776673	32.671578
688.867651	38165.018442	32.676596
689.550462	38225.396844	32.681613
690.752022	38288.559241	32.686631
691.204374	38353.647002	32.691648
692.115953	38409.513206	32.696666
692.567237	38471.597775	32.701684
693.966082	38525.889729	32.706701
694.821007	38572.829871	32.711719
695.643967	38627.293938	32.716736
695.830278	38687.390478	32.721754
696.568279	38750.265944	32.726772
697.414559	38802.507202	32.731789
697.812891	38868.635695	32.736807
698.612335	38924.255094	32.741824
699.579144	38985.565279	32.746842
699.980240	39047.033264	32.751860
700.765847	39103.534288	32.756877
701.508490	39173.897662	32.761895
702.071534	39228.941236	32.766912
702.922440	39287.639600	32.771930
703.449517	39354.995342	32.776948
704.391537	39412.307578	32.781965
704.896920	39478.870270	32.786983
706.039822	39535.778451	32.792000
706.727087	39595.527604	32.797018
707.055348	39654.257732	32.802036
707.610981	39715.362064	32.807053
708.492954	39781.266283	32.812071
708.940747	39842.906332	32.817088
710.508255	39899.047404	32.822106
711.317181	39957.482187	32.827124
712.094419	40018.375803	32.832141
712.845725	40070.217521	32.837159
713.357527	40130.425501	32.842176
714.010759	40171.847946	32.847194
714.752989	40237.136569	32.852212
715.439820	40283.018842	32.857229
716.152593	40348.027796	32.862247
716.606833	40413.975225	32.867264
717.418249	40468.768261	32.872282
717.889294	40535.004355	32.877300
718.920294	40589.554814	32.882317
719.469352	40659.377638	32.887335
719.969679	40717.046673	32.892352
721.132134	40766.353255	32.897370
721.998135	40822.068355	32.902388
722.670614	40876.757561	32.907405
723.522697	40941.873089	32.912423
724.443672	40985.702928	32.917440
725.063714	41036.732569	32.922458
725.528313	41089.728115	32.927476
726.568577	41133.128597	32.932493
727.198309	41197.615439	32.937511
727.822265	41238.690306	32.942528
728.405900	41279.746228	32.947546
729.049764	41327.566348	32.952564
730.457193	41372.529212	32.957581
731.318868	41411.455025	32.962599
732.374809	41454.885329	32.967616
732.844490	41497.755558	32.972634
733.123975	41551.584254	32.977652
734.188804	41591.421117	32.982669
734.397772	41642.117718	32.987687
734.664923	41682.433096	32.992704
735.554794	41736.660544	32.997722
736.192815	41799.863983	33.002740
737.222193	41846.701835	33.007757
737.824353	41899.254180	33.012775
738.598776	41951.843081	33.017792
739.173413	42004.526456	33.022810
739.895342	42065.567217	33.027828
740.545035	42124.336180	33.032845
741.299064	42195.422238	33.037863
741.388338	42263.683658	33.042880
742.435118	42321.689291	33.047898
743.177976	42400.114457	33.052916
744.105546	42451.972342	33.057933
745.098553	42525.299189	33.062951
745.445911	42600.902527	33.067968
746.446168	42655.450278	33.072986
746.647347	42728.192680	33.078004
747.694990	42799.551228	33.083021
748.538127	42858.975128	33.088039
748.882049	42932.454972	33.093056
749.947952	42995.639516	33.098074
750.693170	43061.682443	33.103092
751.776511	43131.208595	33.108109
752.990184	43204.421126	33.113127
753.447646	43259.390094	33.118144
754.305623	43319.654153	33.123162
755.333733	43388.968339	33.128180
755.933361	43438.551979	33.133197
756.518346	43506.695801	33.138215
757.325623	43552.952004	33.143232
758.875213	43607.973209	33.148250
759.416085	43681.538735	33.153268
760.533154	43727.481424	33.158285
761.425175	43779.803378	33.163303
761.680219	43829.821046	33.168320
762.572202	43886.950394	33.173338
763.296362	43943.713852	33.178356
763.985668	43991.229078	33.183373
765.027265	44046.981952	33.188391
765.610188	44107.290973	33.193408
766.227779	44159.207450	33.198426
766.573958	44227.384337	33.203444
766.963903	44283.561836	33.208461
767.499059	44339.425908	33.213479
768.041191	44422.538607	33.218496
769.345707	44487.657452	33.223514
770.043035	44563.377470	33.228532
770.545890	44633.220089	33.233549
771.377916	44704.776479	33.238567
772.181796	44777.267322	33.243584
773.203814	44847.377695	33.248602
774.008324	44920.773448	33.253620
774.891062	44987.926641	33.258637
775.657319	45050.290770	33.263655
776.008508	45113.206752	33.268672
777.015539	45172.990875	33.273690
777.563739	45234.586117	33.278708
778.401144	45303.600710	33.283725
779.109757	45364.545106	33.288743
779.774556	45430.721458	33.293760
781.000683	45490.978378	33.298778
781.295920	45561.956884	33.303796
781.964039	45628.803826	33.308813
782.765887	45691.290717	33.313831
783.406595	45769.193354	33.318848
784.271313	45821.834320	33.323866
785.122734	45898.502715	33.328884
785.753863	45969.828748	33.333901
786.627606	46038.776693	33.338919
787.238466	46115.457973	33.343936
788.295838	46185.845377	33.348954
788.906978	46253.392568	33.353972
789.763854	46330.352578	33.358989
791.049419	46392.044972	33.364007
791.734289	46464.091688	33.369024
792.482698	46530.530284	33.374042
793.419954	46607.719118	33.379060
793.869533	46676.513639	33.384077
794.991913	46744.008024	33.389095
795.655127	46818.191105	33.394112
796.663052	46886.273076	33.399130
797.615073	46959.298281	33.404148
798.333177	47028.450618	33.409165
799.626130	47094.369611	33.414183
800.426044	47154.868151	33.419200
801.796992	47204.757606	33.424218
803.027051	47278.044217	33.429236
803.366777	47320.212072	33.434253
804.230407	47373.925963	33.439271
804.685610	47441.399769	33.444288
805.745945	47500.479586	33.449306
806.549100	47553.690894	33.454324
807.214872	47624.131099	33.459341
807.549967	47685.449913	33.464359
808.043627	47755.436521	33.469376
808.911646	47818.874285	33.474394
809.801039	47890.223125	33.479412
810.023143	47963.339891	33.484429
810.977623	48033.730100	33.489447
812.017763	48121.681884	33.494464
812.980813	48184.397322	33.499482
813.835100	48266.330558	33.504500
814.413464	48333.496829	33.509517
814.610080	48406.947964	33.514535
815.755120	48486.894509	33.519552
816.684691	48564.236723	33.524570
817.579904	48652.782507	33.529588
818.652541	48726.041366	33.534605
819.809057	48783.515262	33.539623
820.476991	48867.327027	33.544640
821.388773	48934.791133	33.549658
822.497051	49008.070657	33.554676
823.154613	49080.022387	33.559693
823.932862	49142.414940	33.564711
825.052609	49225.841357	33.569728
825.949633	49285.090424	33.574746
826.643379	49352.526438	33.579764
827.560865	49415.511755	33.584781
828.191555	49484.147400	33.589799
828.578019	49555.712608	33.594816
829.591675	49618.272272	33.599834
830.486386	49687.341937	33.604852
831.452087	49752.674253	33.609869
832.233432	49832.985816	33.614887
833.487109	49886.916978	33.619904
833.947011	49945.141250	33.624922
834.564531	50009.680695	33.629940
835.251319	50065.769422	33.634957
836.171394	50123.663110	33.639975
836.942329	50202.939970	33.644992
837.700157	50267.224200	33.650010
838.706747	50334.139879	33.655028
839.658676	50395.762223	33.660045
840.271114	50457.197152	33.665063
840.950743	50524.638809	33.670080
841.913272	50595.136889	33.675098
842.659029	50664.713539	33.680116
843.229394	50733.893784	33.685133
844.357465	50801.336043	33.690151
844.949093	50884.243295	33.695168
845.978907	50957.167960	33.700186
846.561179	51026.170068	33.705204
847.600203	51103.446867	33.710221
848.768886	51184.601315	33.715239
849.037985	51256.569713	33.720256
850.326216	51337.358089	33.725274
850.898745	51418.574521	33.730292
851.731135	51503.869870	33.735309
852.582242	51572.774814	33.740327
853.087383	51658.260874	33.745344
854.350921	51733.537020	33.750362
855.303934	51813.759157	33.755380
855.931922	51886.705012	33.760397
856.487793	51968.640962	33.765415
857.694268	52051.608541	33.770432
858.756435	52136.826157	33.775450
859.881943	52228.045363	33.780468
860.696732	52301.823984	33.785485
861.547896	52370.699650	33.790503
862.565225	52452.464232	33.795520
863.110638	52533.460990	33.800538
863.959898	52609.171464	33.805556
865.201147	52684.517438	33.810573
866.100251	52759.746069	33.815591
867.011789	52842.319444	33.820608
868.310288	52906.685029	33.825626
869.406209	52969.171357	33.830644
870.209128	53047.453192	33.835661
871.751161	53100.556003	33.840679
873.057106	53168.989898	33.845696
873.825508	53211.563756	33.850714
874.717086	53264.141741	33.855732
875.541658	53328.360791	33.860749
876.491096	53384.606501	33.865767
877.641995	53437.283721	33.870784
878.411124	53487.888001	33.875802
879.143296	53535.979652	33.880820
879.677860	53604.851293	33.885837
880.829556	53664.989482	33.890855
881.073819	53725.326031	33.895872
881.794231	53786.651709	33.900890
882.663426	53848.859285	33.905908
883.387058	53920.505704	33.910925
884.304611	53982.630171	33.915943
884.683982	54060.899060	33.920960
885.529874	54140.538380	33.925978
886.492212	54213.597654	33.930996
886.620680	54290.830594	33.936013
887.622019	54364.055122	33.941031
888.833063	54451.599393	33.946048
889.715888	54535.138745	33.951066
890.492579	54604.216091	33.956084
891.225277	54683.558459	33.961101
892.399532	54747.246014	33.966119
893.152462	54819.637335	33.971136
893.886891	54892.531688	33.976154
894.907164	54958.028344	33.981172
895.401028	55034.529715	33.986189
896.563138	55101.947469	33.991207
897.566133	55181.844294	33.996224
898.187550	55258.775845	34.001242
899.244522	55328.223020	34.006260
900.006139	55410.778128	34.011277
900.436124	55487.949058	34.016295
901.585539	55573.519965	34.021312
902.553463	55649.747019	34.026330
903.918845	55733.728092	34.031348
904.706427	55825.804932	34.036365
905.743138	55904.926871	34.041383
906.936785	55965.659278	34.046400
907.403519	56050.964792	34.051418
908.617097	56130.692806	34.056436
909.500911	56208.149829	34.061453
911.048018	56282.668640	34.066471
911.820303	56359.877717	34.071488
912.457961	56441.360848	34.076506
913.703186	56516.699479	34.081524
913.893372	56603.682813	34.086541
914.609000	56678.699358	34.091559
915.630284	56766.452591	34.096576
916.531166	56859.230933	34.101594
917.687799	56937.008594	34.106612
918.308666	57022.907479	34.111629
919.234898	57093.361122	34.116647
920.848570	57188.668905	34.121664
921.785165	57260.754269	34.126682
922.610554	57342.230234	34.131700
923.751927	57429.125463	34.136717
924.918451	57500.093514	34.141735
926.061761	57566.394629	34.146752
926.783490	57647.343477	34.151770
927.684283	57715.068796	34.156788
928.462927	57793.876412	34.161805
929.459282	57888.688145	34.166823
930.387928	57963.871753	34.171840
930.987187	58043.252407	34.176858
932.428430	58124.540225	34.181876
932.757067	58214.286313	34.186893
933.659376	58282.044638	34.191911
934.347485	58377.463240	34.196928
935.174117	58470.309997	34.201946
935.991153	58561.310477	34.206964
937.256813	58649.785727	34.211981
937.860584	58743.383426	34.216999
938.839170	58835.176263	34.222016
939.648660	58919.824677	34.227034
940.856488	59008.038080	34.232052
941.930254	59103.228622	34.237069
943.107313	59193.732385	34.242087
943.820761	59276.776677	34.247104
944.698294	59371.429172	34.252122
946.144976	59446.346872	34.257140
946.651194	59538.804541	34.262157
947.535747	59629.323813	34.267175
948.531101	59713.028287	34.272192
949.312195	59809.020364	34.277210
950.490107	59891.899517	34.282228
951.387799	59992.690956	34.287245
952.479939	60073.166179	34.292263
953.555129	60151.897332	34.297280
954.184938	60234.337609	34.302298
955.532741	60309.558195	34.307316
956.486671	60385.985995	34.312333
957.473336	60469.124749	34.317351
958.515927	60533.639379	34.322368
959.235025	60609.370185	34.327386
960.334663	60693.840351	34.332404
961.220187	60764.937671	34.337421
961.832487	60846.363644	34.342439
963.165977	60907.789348	34.347456
963.791267	60999.335179	34.352474
964.786736	61089.000730	34.357492
965.390203	61169.213817	34.362509
966.776903	61254.438797	34.367527
968.112815	61336.006954	34.372544
968.409093	61436.480181	34.377562
969.420901	61511.990973	34.382580
970.329748	61614.287553	34.387597
971.841753	61699.437602	34.392615
972.412744	61781.499776	34.397632
973.652268	61875.485272	34.402650
974.953545	61948.660863	34.407668
975.847976	62043.757841	34.412685
976.555866	62130.009384	34.417703
977.547704	62218.052772	34.422720
978.285289	62307.224840	34.427738
979.331548	62395.570568	34.432756
980.710542	62488.251658	34.437773
981.685350	62570.443502	34.442791
982.853387	62669.184495	34.447808
983.554941	62765.586656	34.452826
984.559341	62852.212360	34.457844
985.576778	62942.419307	34.462861
986.359944	63030.289164	34.467879
987.616655	63111.141196	34.472896
988.311102	63210.622754	34.477914
989.465069	63304.506718	34.482932
990.407010	63403.114904	34.487949
991.037154	63495.023729	34.492967
992.776013	63578.372403	34.497984
993.917678	63672.854739	34.503002
995.020607	63750.725793	34.508020
996.030631	63843.842880	34.513037
996.892291	63929.494326	34.518055
998.141012	64013.579133	34.523072
999.184023	64110.363831	34.528090
1000.090748	64194.856998	34.533108
1001.117602	64281.439866	34.538125
1001.351311	64374.401221	34.543143
1002.355822	64459.278893	34.548160
1003.164127	64556.741254	34.553178
1004.368192	64653.737220	34.558196
1005.644712	64749.354833	34.563213
1006.437421	64837.647398	34.568231
1008.088211	64935.423246	34.573248
1009.008957	65028.058498	34.578266
1010.310700	65107.238637	34.583284
1011.265315	65198.761342	34.588301
1012.324748	65290.780869	34.593319
1012.862245	65375.633039	34.598336
1013.821991	65467.231891	34.603354
1015.181525	65554.223193	34.608372
1016.182256	65630.482598	34.613389
1017.232575	65722.308858	34.618407
1018.214357	65816.292348	34.623424
1018.915238	65911.307562	34.628442
1019.687593	65992.294941	34.633460
1020.751850	66078.631260	34.638477
1021.806706	66168.312183	34.643495
1023.528557	66239.402591	34.648512
1024.642532	66316.159263	34.653530
1025.687310	66389.083898	34.658548
1026.763401	66459.984210	34.663565
1027.538774	66538.440379	34.668583
1028.586637	66606.515431	34.673600
1029.115980	66697.457640	34.678618
1029.967319	66779.138010	34.683636
1030.872734	66860.968509	34.688653
1031.573381	66948.814262	34.693671
1032.892093	67042.072397	34.698688
1033.747704	67145.754780	34.703706
1034.877654	67242.683582	34.708724
1035.822292	67331.208123	34.713741
1036.915167	67430.973564	34.718759
1037.644394	67527.028765	34.723776
1038.808195	67616.469904	34.728794
1039.877041	67708.889292	34.733812
1041.468182	67798.910367	34.738829
1042.218987	67905.568983	34.743847
1043.322016	67986.390936	34.748864
1044.767561	68086.161021	34.753882
1045.691196	68175.533861	34.758900
1046.642366	68268.727053	34.763917
1048.393694	68349.221298	34.768935
1049.413730	68431.064310	34.773952
1050.893746	68519.148717	34.778970
1052.045591	68606.879277	34.783988
1053.050659	68686.034438	34.789005
1053.607331	68790.371529	34.794023
1054.876519	68861.786655	34.799040
1055.526527	68959.119580	34.804058
1056.320668	69061.742868	34.809076
1057.459853	69145.203225	34.814093
1058.752915	69242.848696	34.819111
1059.837531	69334.473657	34.824128
1060.354030	69439.256526	34.829146
1061.163989	69537.364558	34.834164
1062.116552	69628.789497	34.839181
1063.017432	69743.644969	34.844199
1064.355504	69849.346398	34.849216
1065.301565	69959.396096	34.854234
1066.093492	70067.393321	34.859252
1067.135282	70172.546966	34.864269
1068.281221	70298.080718	34.869287
1069.080125	70397.308181	34.874304
1070.416960	70520.185432	34.879322
1071.488083	70630.338814	34.884340
1073.014067	70729.137753	34.889357
1073.907389	70846.323214	34.894375
1075.058907	70954.337798	34.899392
1076.259071	71061.788011	34.904410
1077.427588	71171.941183	34.909428
1079.166560	71260.095920	34.914445
1080.537731	71353.133509	34.919463
1082.208959	71435.410233	34.924480
1083.408048	71530.058348	34.929498
1084.319583	71609.629593	34.934516
1085.951984	71697.840389	34.939533
1086.542929	71781.983467	34.944551
1087.878363	71861.058881	34.949568
1088.837365	71943.321412	34.954586
1089.391590	72039.452240	34.959604
1090.549872	72124.673300	34.964621
1091.660785	72228.557933	34.969639
1092.554283	72309.463957	34.974656
1093.054520	72398.385277	34.979674
1094.139103	72494.777176	34.984692
1095.276191	72578.166521	34.989709
1095.931253	72672.992088	34.994727
1096.811465	72757.726528	34.999744
1097.383984	72863.749279	35.004762
1098.432333	72958.286671	35.009780
1099.669851	73060.115705	35.014797
1100.710840	73163.812249	35.019815
1102.065930	73264.395195	35.024832
1102.982277	73359.030558	35.029850
1104.024445	73472.442797	35.034868
1105.166126	73570.412957	35.039885
1106.090376	73690.544745	35.044903
1107.173464	73795.668458	35.049920
1108.386362	73896.985228	35.054938
1109.335775	74015.835295	35.059956
1110.920961	74125.821941	35.064973
1112.081123	74236.787167	35.069991
1113.274790	74340.084545	35.075008
1114.477949	74458.377769	35.080026
1115.529521	74570.311257	35.085044
1116.879133	74677.765571	35.090061
1117.937931	74792.042150	35.095079
1119.003028	74896.311676	35.100096
1120.066607	75001.481170	35.105114
1121.348987	75114.052331	35.110132
1123.015802	75220.496784	35.115149
1123.465896	75330.766400	35.120167
1124.634534	75445.573333	35.125184
1125.878360	75557.493680	35.130202
1127.064335	75670.335513	35.135220
1128.336509	75778.046955	35.140237
1128.960187	75889.875207	35.145255
1130.384816	76003.137297	35.150272
1131.690000	76112.808329	35.155290
1132.511097	76226.253967	35.160308
1134.098013	76343.064358	35.165325
1135.082297	76453.926773	35.170343
1136.349775	76570.711865	35.175360
1137.759260	76687.716036	35.180378
1138.284316	76802.502237	35.185396
1139.556927	76909.065377	35.190413
1140.889458	77030.820640	35.195431
1141.732023	77147.421001	35.200448
1143.118894	77258.566059	35.205466
1144.073807	77383.548586	35.210484
1145.514415	77498.195209	35.215501
1146.300311	77616.807901	35.220519
1147.558414	77726.695463	35.225536
1149.311613	77838.862632	35.230554
1150.156105	77957.708373	35.235572
1151.399758	78075.479057	35.240589
1152.922929	78171.316325	35.245607
1154.179803	78283.321879	35.250624
1155.427763	78386.081521	35.255642
1156.949887	78487.519385	35.260660
1158.412560	78574.575749	35.265677
1159.525457	78669.287805	35.270695
1160.465593	78767.662889	35.275712
1162.083243	78870.354131	35.280730
1162.942478	78973.163807	35.285748
1164.245414	79056.826087	35.290765
1165.252399	79155.293497	35.295783
1166.309110	79257.959480	35.300800
1167.430364	79353.686072	35.305818
1168.659546	79461.064021	35.310836
1169.722211	79553.151853	35.315853
1170.964306	79657.956812	35.320871
1171.972359	79739.310673	35.325888
1173.030202	79825.167122	35.330906
1174.000198	79911.696291	35.335924
1174.950191	80007.705180	35.340941
1176.364029	80099.816180	35.345959
1177.279575	80195.501687	35.350976
1178.284636	80287.208184	35.355994
1179.395245	80382.433225	35.361012
1180.722620	80481.096189	35.366029
1181.207139	80596.791361	35.371047
1182.765073	80704.008924	35.376064
1184.124018	80799.792190	35.381082
1185.248916	80914.248768	35.386100
1186.390878	81016.097144	35.391117
1187.788961	81123.974670	35.396135
1188.963053	81224.817922	35.401152
1190.385221	81327.574026	35.406170
1191.557333	81431.978462	35.411188
1193.075734	81531.983715	35.416205
1194.073633	81641.623251	35.421223
1194.823612	81752.061985	35.426240
1196.553703	81857.128663	35.431258
1197.588212	81971.008147	35.436276
1198.791490	82067.364779	35.441293
1200.147718	82175.265532	35.446311
1200.735302	82282.361435	35.451328
1202.129142	82385.607276	35.456346
1202.990371	82507.599343	35.461364
1204.596908	82614.322512	35.466381
1205.713961	82730.523507	35.471399
1206.866270	82845.477814	35.476416
1208.409423	82957.736344	35.481434
1209.468687	83071.274313	35.486452
1210.684961	83180.074936	35.491469
1212.155528	83307.233788	35.496487
1212.882753	83419.025637	35.501504
1214.367305	83536.743866	35.506522
1215.752121	83641.465465	35.511540
1217.179481	83750.590189	35.516557
1218.587971	83863.063316	35.521575
1219.428024	83986.268741	35.526592
1220.865923	84082.545021	35.531610
1221.745133	84215.210375	35.536628
1222.942614	84315.300757	35.541645
1224.036518	84431.993794	35.546663
1225.390514	84556.768894	35.551680
1227.577962	84661.812786	35.556698
1228.812521	84772.567967	35.561716
1230.173355	84876.423523	35.566733
1231.796659	84971.584222	35.571751
1233.043960	85084.442029	35.576768
1234.344169	85178.399257	35.581786
1235.083306	85279.020507	35.586804
1236.396386	85381.250726	35.591821
1237.654317	85481.513163	35.596839
1238.778523	85580.795722	35.601856
1240.332423	85684.129957	35.606874
1241.504801	85790.780516	35.611892
1242.576968	85893.518894	35.616909
1243.661147	85999.347630	35.621927
1244.796021	86103.610253	35.626944
1245.836600	86208.901661	35.631962
1247.098979	86325.348050	35.636980
1247.978843	86440.612612	35.641997
1249.329973	86554.689159	35.647015
1249.896499	86665.935733	35.652032
1251.376705	86786.050246	35.657050
1252.151906	86902.448056	35.662068
1253.369593	87017.586287	35.667085
1254.148663	87132.717212	35.672103
1255.145104	87252.389389	35.677120
1256.191704	87369.418438	35.682138
1258.069329	87497.204043	35.687156
1259.198598	87613.283455	35.692173
1260.096016	87734.430327	35.697191
1261.305374	87869.342041	35.702208
1263.085525	87989.528862	35.707226
1264.157010	88117.974892	35.712244
1265.218913	88247.956351	35.717261
1266.773767	88369.611791	35.722279
1268.162480	88500.012380	35.727296
1269.449655	88616.223244	35.732314
1271.251081	88743.493876	35.737332
1272.571458	88872.512743	35.742349
1273.983404	88987.945280	35.747367
1274.707398	89119.174418	35.752384
1276.160315	89234.449463	35.757402
1277.470173	89360.481272	35.762420
1278.831492	89483.007837	35.767437
1280.522681	89603.734672	35.772455
1281.605163	89739.650501	35.777472
1283.061278	89864.990006	35.782490
1284.320169	89991.070439	35.787508
1286.074032	90105.744396	35.792525
1287.567225	90226.707347	35.797543
1288.652542	90346.707726	35.802560
1289.659489	90470.269363	35.807578
1291.069898	90601.943149	35.812596
1292.569461	90709.815289	35.817613
1293.547629	90830.303206	35.822631
1295.099353	90959.548574	35.827648
1296.266680	91077.853512	35.832666
1297.706431	91213.771122	35.837684
1298.778534	91333.207180	35.842701
1300.404496	91452.202635	35.847719
1301.041294	91586.333144	35.852736
1303.144268	91714.456686	35.857754
1304.383322	91841.321093	35.862772
1305.431756	91958.253842	35.867789
1307.433119	92074.950001	35.872807
1308.623587	92209.098485	35.877824
1309.637759	92335.645087	35.882842
1310.528144	92464.467514	35.887860
1312.335313	92576.734467	35.892877
1313.759987	92704.752311	35.897895
1314.572181	92829.900196	35.902912
1315.796446	92960.244389	35.907930
1317.328799	93096.751735	35.912948
1318.485261	93215.979282	35.917965
1320.070586	93338.689456	35.922983
1321.165077	93487.206262	35.928000
1322.754476	93609.561995	35.933018
1324.110474	93736.073874	35.938036
1325.711323	93857.528900	35.943053
1327.086064	93977.156381	35.948071
1327.966284	94105.391580	35.953088
1329.476051	94236.913567	35.958106
1330.942334	94353.422872	35.963124
1332.382637	94479.303606	35.968141
1334.054666	94603.158777	35.973159
1335.075403	94732.350703	35.978176
1336.375296	94856.759149	35.983194
1337.538587	94978.489503	35.988212
1338.789184	95094.350705	35.993229
1340.065199	95208.890135	35.998247
1341.278656	95339.664380	36.003264
1342.480656	95461.948329	36.008282
1343.733775	95583.591021	36.013300
1344.971687	95710.268794	36.018317
1346.247670	95820.652865	36.023335
1347.153216	95953.518404	36.028352
1348.265579	96077.377838	36.033370
1349.598031	96202.280956	36.038388
1350.891207	96324.832966	36.043405
1352.739379	96467.352452	36.048423
1353.510876	96602.358497	36.053440
1355.057663	96736.014870	36.058458
1356.738546	96866.672049	36.063476
1358.296801	96995.954477	36.068493
1359.823712	97116.064721	36.073511
1361.938886	97226.690738	36.078528
1363.695408	97347.387264	36.083546
1365.538169	97459.653718	36.088564
1366.842769	97575.072028	36.093581
1368.273889	97679.835515	36.098599
1369.544620	97789.847034	36.103616
1371.121103	97900.964910	36.108634
1372.544201	98006.339202	36.113652
1373.636447	98115.631714	36.118669
1375.131644	98223.644922	36.123687
1376.397701	98348.693649	36.128704
1377.694282	98444.999878	36.133722
1379.280006	98567.908045	36.138740
1380.335203	98704.881845	36.143757
1381.517232	98812.933121	36.148775
1382.679533	98941.942845	36.153792
1383.927424	99065.539361	36.158810
1385.334124	99200.026586	36.163828
1386.337387	99330.723327	36.168845
1387.767145	99456.156579	36.173863
1389.129423	99591.717243	36.178880
1390.496884	99725.971914	36.183898
1391.992916	99867.027535	36.188916
1393.201434	100009.649811	36.193933
1394.225033	100138.508449	36.198951
1395.763392	100290.550671	36.203968
1397.292634	100431.147201	36.208986
1398.573181	100587.794867	36.214004
1399.694175	100723.854239	36.219021
1401.265617	100859.336961	36.224039
1402.349692	101017.170954	36.229056
1403.726287	101169.521390	36.234074
1405.170254	101314.166571	36.239092
1406.697197	101474.152479	36.244109
1408.347349	101617.245559	36.249127
1409.622781	101768.346738	36.254144
1411.665960	101922.878994	36.259162
1412.762787	102053.179129	36.264180
1413.975930	102199.740528	36.269197
1415.887911	102350.656569	36.274215
1417.188176	102496.977526	36.279232
1418.407082	102649.727071	36.284250
1420.055553	102794.663920	36.289268
1421.484469	102939.952543	36.294285
1423.252069	103078.786411	36.299303
1424.761672	103225.521768	36.304320
1426.393221	103366.951784	36.309338
1427.621476	103507.151944	36.314356
1428.855260	103651.814770	36.319373
1430.752969	103788.514005	36.324391
1432.073356	103920.637826	36.329408
1433.236242	104063.322892	36.334426
1434.621198	104192.090499	36.339444
1436.227205	104333.959692	36.344461
1437.663664	104455.797538	36.349479
1439.343003	104593.168019	36.354496
1440.322181	104706.303982	36.359514
1441.949908	104826.363680	36.364532
1443.028214	104953.584364	36.369549
1444.615487	105069.327593	36.374567
1445.670492	105210.449425	36.379584
1446.929044	105341.561453	36.384602
1448.363119	105475.220607	36.389620
1449.745334	105614.429319	36.394637
1450.571922	105758.949077	36.399655
1452.487272	105915.497809	36.404672
1453.896230	106049.949285	36.409690
1455.326299	106192.158015	36.414708
1456.891437	106353.670346	36.419725
1458.424183	106501.177231	36.424743
1459.569636	106653.652167	36.429760
1460.986258	106802.167465	36.434778
1462.920939	106953.861545	36.439796
1464.541699	107099.873761	36.444813
1466.109693	107247.644672	36.449831
1467.891846	107388.358060	36.454848
1469.183847	107539.875807	36.459866
1470.864958	107685.893809	36.464884
1471.973341	107820.918942	36.469901
1473.520438	107975.290026	36.474919
1474.860181	108133.485536	36.479936
1476.216162	108279.036761	36.484954
1477.898052	108433.528402	36.489972
1478.885400	108595.344119	36.494989
1480.433568	108759.317786	36.500007
1481.917215	108923.568567	36.505024
1483.343256	109090.631552	36.510042
1484.946123	109246.077494	36.515060
1486.415389	109418.486655	36.520077
1487.867135	109581.160388	36.525095
1489.248533	109747.574058	36.530112
1490.975713	109906.059728	36.535130
1492.581797	110064.679094	36.540148
1494.056405	110237.725521	36.545165
1495.585211	110395.445361	36.550183
1497.551175	110561.962131	36.555200
1498.814483	110722.172259	36.560218
1500.545754	110876.096361	36.565236
1502.212494	111046.682018	36.570253
1504.110581	111200.467436	36.575271
1505.150333	111350.379721	36.580288
1506.881969	111509.721581	36.585306
1508.498961	111658.860514	36.590324
1509.798304	111819.095359	36.595341
1511.938088	111964.387708	36.600359
1513.816482	112119.841496	36.605376
1515.261005	112265.940792	36.610394
1516.802284	112411.556392	36.615412
1518.062444	112557.647530	36.620429
1519.610109	112711.646201	36.625447
1520.809865	112858.813264	36.630464
1522.296159	113016.259660	36.635482
1523.671463	113169.094989	36.640500
1525.368505	113327.740128	36.645517
1526.933713	113477.795141	36.650535
1528.664675	113628.116675	36.655552
1529.947297	113780.284165	36.660570
1531.545728	113926.873550	36.665588
1533.047684	114092.806823	36.670605
1534.200125	114243.005345	36.675623
1535.873443	114397.156517	36.680640
1537.131065	114548.151621	36.685658
1539.097927	114684.007831	36.690676
1540.376026	114832.870213	36.695693
1541.624240	114957.069601	36.700711
1543.026831	115104.734203	36.705728
1544.263212	115261.252640	36.710746
1546.123915	115409.214973	36.715764
1547.649628	115561.047656	36.720781
1548.945034	115707.298170	36.725799
1550.202983	115857.816654	36.730816
1551.424757	116019.515338	36.735834
1553.261591	116173.128506	36.740852
1554.788508	116341.198862	36.745869
1556.074979	116512.313378	36.750887
1557.299146	116680.508492	36.755904
1559.338409	116849.516084	36.760922
1561.060310	117011.661273	36.765940
1562.445042	117183.702167	36.770957
1563.582161	117362.758439	36.775975
1565.447439	117537.288276	36.780992
1567.088731	117710.801030	36.786010
1568.970547	117884.213729	36.791028
1570.455433	118062.052290	36.796045
1571.610595	118235.719230	36.801063
1573.743631	118409.691396	36.806080
1575.195642	118583.542046	36.811098
1576.854168	118757.665771	36.816116
1578.859569	118933.194996	36.821133
1580.474976	119109.584844	36.826151
1582.529578	119272.119245	36.831168
1584.071547	119454.521826	36.836186
1585.692410	119616.643195	36.841204
1586.906636	119790.028986	36.846221
1588.338415	119960.591090	36.851239
1590.674112	120128.273380	36.856256
1592.002397	120308.493472	36.861274
1593.822800	120465.589598	36.866292
1595.733839	120636.688976	36.871309
1596.869335	120808.632857	36.876327
1598.348601	120980.054655	36.881344
1599.973351	121157.923910	36.886362
1602.058007	121327.147310	36.891380
1603.401184	121507.053540	36.896397
1604.780588	121679.610256	36.901415
1606.570267	121857.888336	36.906432
1607.985779	122035.857593	36.911450
1609.606959	122213.275550	36.916468
1610.733464	122393.891906	36.921485
1612.118550	122582.777813	36.926503
1614.350111	122763.629810	36.931520
1615.866317	122939.900317	36.936538
1617.695199	123121.450906	36.941556
1619.345097	123294.619582	36.946573
1620.595303	123475.373862	36.951591
1622.535055	123658.127485	36.956608
1623.926245	123842.743345	36.961626
1625.518376	124010.862480	36.966644
1627.637747	124193.121223	36.971661
1629.185820	124389.500455	36.976679
1630.622936	124560.817534	36.981696
1632.053222	124757.889265	36.986714
1633.707469	124941.581221	36.991732
1635.146746	125125.459707	36.996749
1636.822852	125316.355762	37.001767
1638.269716	125503.216072	37.006784
1639.827718	125709.229149	37.011802
1641.448482	125889.327673	37.016820
1643.270284	126072.605402	37.021837
1644.315386	126273.753412	37.026855
1646.135201	126451.146563	37.031872
1647.775294	126625.460209	37.036890
1649.681447	126800.101104	37.041908
1651.018068	126981.745708	37.046925
1652.801196	127164.095520	37.051943
1654.468908	127341.922176	37.056960
1655.743527	127523.908681	37.061978
1656.922891	127715.349981	37.066996
1659.180086	127896.436659	37.072013
1660.844059	128084.873518	37.077031
1662.438191	128269.021131	37.082048
1663.134917	128469.561642	37.087066
1664.900044	128668.744219	37.092084
1666.523773	128870.081236	37.097101
1668.019756	129085.065447	37.102119
1669.843961	129291.219897	37.107136
1671.563339	129502.695087	37.112154
1673.218242	129699.577875	37.117172
1675.037921	129916.609409	37.122189
1676.775237	130122.058236	37.127207
1678.879137	130324.773867	37.132224
1680.545776	130526.340479	37.137242
1682.534609	130729.025191	37.142260
1684.359611	130939.044666	37.147277
1686.125699	131145.762749	37.152295
1688.016948	131353.578904	37.157312
1689.487360	131565.293401	37.162330
1691.178842	131772.559011	37.167348
1693.135276	131981.624186	37.172365
1694.317374	132190.074960	37.177383
1695.990374	132398.602591	37.182400
1697.641111	132602.960166	37.187418
1699.671544	132816.382688	37.192436
1701.250390	133041.689662	37.197453
1702.140106	133262.346783	37.202471
1704.302780	133485.217757	37.207488
1705.954635	133716.810459	37.212506
1707.221029	133938.820803	37.217524
1709.407157	134163.201528	37.222541
1710.951426	134402.630966	37.227559
1712.847046	134627.224207	37.232576
1714.354311	134863.527674	37.237594
1715.987489	135083.494444	37.242612
1717.927669	135318.692418	37.247629
1719.252277	135552.959591	37.252647
1721.169612	135785.613000	37.257664
1723.094007	136021.007438	37.262682
1724.880105	136257.021034	37.267700
1726.527991	136492.181783	37.272717
1728.144615	136725.204054	37.277735
1729.917581	136951.350717	37.282752
1731.828744	137187.083177	37.287770
1733.694441	137420.628576	37.292788
1735.560543	137650.812262	37.297805
1737.051701	137880.459022	37.302823
1738.943972	138104.524314	37.307840
1740.665172	138353.756464	37.312858
1742.480488	138583.863860	37.317876
1744.171732	138821.478956	37.322893
1745.853101	139055.581576	37.327911
1747.477419	139293.831310	37.332928
1749.153533	139532.467595	37.337946
1750.851199	139764.261544	37.342964
1752.429853	140005.504253	37.347981
1753.977093	140250.940991	37.352999
1756.129174	140484.990128	37.358016
1757.467695	140729.522704	37.363034
1759.604445	140959.807396	37.368052
1761.744716	141174.901648	37.373069
1763.636478	141393.157515	37.378087
1765.548226	141592.615884	37.383104
1767.133014	141809.766530	37.388122
1768.941174	142031.414114	37.393140
1770.252542	142248.050869	37.398157
1771.587240	142468.517707	37.403175
1773.814436	142684.315845	37.408192
1776.145843	142910.023347	37.413210
1778.135706	143127.357954	37.418228
1779.793126	143330.175474	37.423245
1781.714370	143555.835553	37.428263
1783.496650	143773.877968	37.433280
1785.032518	143988.228355	37.438298
1786.410825	144214.877040	37.443316
1788.470587	144442.334500	37.448333
1790.026251	144674.986245	37.453351
1792.023446	144902.112853	37.458368
1793.155282	145136.025730	37.463386
1795.255294	145361.221929	37.468404
1797.219765	145587.468280	37.473421
1798.667783	145846.592366	37.478439
1800.408696	146085.999353	37.483456
1802.368345	146327.175712	37.488474
1803.857965	146578.250178	37.493492
1805.987383	146823.832054	37.498509
1807.594841	147073.139053	37.503527
1809.353747	147329.366456	37.508544
1811.075372	147574.761519	37.513562
1812.714988	147837.940110	37.518580
1814.676400	148092.680108	37.523597
1815.901184	148355.430853	37.528615
1817.708948	148612.481976	37.533632
1819.677474	148886.327331	37.538650
1821.656637	149155.768012	37.543668
1823.197266	149416.469399	37.548685
1824.570638	149700.604026	37.553703
1826.785316	149974.632455	37.558720
1828.831194	150244.563279	37.563738
1830.897338	150523.199850	37.568756
1832.573998	150795.501060	37.573773
1834.017732	151062.902176	37.578791
1835.868575	151352.822821	37.583808
1838.002537	151635.364108	37.588826
1839.488084	151937.466973	37.593844
1841.368327	152229.977158	37.598861
1842.743871	152511.777811	37.603879
1844.512751	152798.799272	37.608896
1847.037488	153097.484430	37.613914
1848.683306	153389.910258	37.618932
1850.276041	153685.824010	37.623949
1852.043056	153979.313020	37.628967
1853.874186	154270.622883	37.633984
1855.918979	154573.541513	37.639002
1857.621745	154870.916833	37.644020
1859.794512	155166.989200	37.649037
1861.301197	155474.223526	37.654055
1863.090113	155768.149900	37.659072
1865.038350	156070.177425	37.664090
1866.908750	156381.612586	37.669108
1868.939861	156667.736737	37.674125
1870.753681	156968.977358	37.679143
1872.763581	157278.186677	37.684160
1874.432884	157574.616174	37.689178
1876.124373	157887.991329	37.694196
1878.308488	158171.737667	37.699213
1880.126620	158482.239854	37.704231
1882.161702	158783.163192	37.709248
1884.428721	159066.126426	37.714266
1886.219298	159342.081222	37.719284
1888.235693	159617.925944	37.724301
1889.842218	159899.053453	37.729319
1892.193221	160175.242147	37.734336
1894.340695	160441.142393	37.739354
1895.978372	160717.482600	37.744372
1897.848040	160984.405947	37.749389
1899.698586	161265.438167	37.754407
1901.605003	161533.614983	37.759424
1903.857932	161811.997104	37.764442
1904.613149	162109.911041	37.769460
1906.329665	162397.545518	37.774477
1908.252874	162687.535932	37.779495
1910.287789	162982.512449	37.784512
1912.054838	163284.451294	37.789530
1913.973484	163587.574067	37.794548
1916.075583	163876.957931	37.799565
1917.849035	164187.355530	37.804583
1919.369437	164493.185252	37.809600
1921.433871	164811.831103	37.814618
1923.214753	165127.335830	37.819636
1925.021126	165454.925020	37.824653
1926.743033	165778.796193	37.829671
1928.050672	166109.665673	37.834688
1930.191149	166436.598171	37.839706
1932.249031	166778.095406	37.844724
1933.927968	167106.448761	37.849741
1935.828694	167453.217515	37.854759
1937.777780	167793.543186	37.859776
1939.886918	168135.026405	37.864794
1941.759164	168491.822549	37.869812
1943.866372	168816.536712	37.874829
1946.110422	169164.669802	37.879847
1948.390851	169507.453433	37.884864
1950.642981	169846.014935	37.889882
1952.429620	170185.564659	37.894900
1954.422246	170533.299043	37.899917
1956.205593	170870.871669	37.904935
1958.434588	171213.582410	37.909952
1961.254498	171550.730154	37.914970
1962.841478	171891.258375	37.919988
1964.820554	172226.165568	37.925005
1966.606277	172569.992672	37.930023
1968.585020	172913.854768	37.935040
1970.792372	173245.315217	37.940058
1972.688066	173597.751561	37.945076
1974.646938	173928.809173	37.950093
1976.764193	174280.401447	37.955111
1978.744461	174627.483429	37.960128
1980.420679	174965.179616	37.965146
1982.167546	175318.802314	37.970164
1984.329008	175662.482891	37.975181
1986.506043	176008.321190	37.980199
1988.110921	176363.608599	37.985216
1990.171657	176715.842495	37.990234
1991.814567	177075.025416	37.995252
1993.916311	177419.611501	38.000269
1995.833237	177778.018280	38.005287
1997.514907	178141.847352	38.010304
1999.649506	178503.778891	38.015322
2001.266614	178873.284670	38.020340
2003.329709	179234.925631	38.025357
2005.114921	179599.125680	38.030375
2006.969959	179975.735767	38.035392
2008.769040	180336.025467	38.040410
2011.062666	180728.291618	38.045428
2013.390944	181072.475922	38.050445
2015.370438	181421.922389	38.055463
2017.943358	181764.140979	38.060480
2020.902039	182084.306011	38.065498
2023.376174	182410.439943	38.070516
2025.360775	182733.476406	38.075533
2027.596005	183043.394793	38.080551
2029.114888	183374.023842	38.085568
2030.889239	183704.741264	38.090586
2032.568062	184037.785961	38.095604
2034.095400	184379.668735	38.100621
2036.164650	184712.477172	38.105639
2037.816222	185070.750649	38.110656
2040.258615	185406.398811	38.115674
2042.050692	185774.025164	38.120692
2044.073657	186119.672014	38.125709
2046.262731	186473.548939	38.130727
2047.642582	186910.634348	38.135744
2050.036813	187278.070746	38.140762
2051.361100	187652.253423	38.145780
2053.345548	188038.856694	38.150797
2055.170618	188413.345082	38.155815
2056.745243	188818.734521	38.160832
2059.061308	189203.207527	38.165850
2061.086976	189593.086458	38.170868
2062.739457	189982.847018	38.175885
2064.960829	190383.620256	38.180903
2066.778072	190797.335724	38.185920
2068.997488	191209.034244	38.190938
2071.100221	191624.740234	38.195956
2073.175500	192027.573875	38.200973
2075.411135	192445.014663	38.205991
2076.668857	192871.931133	38.211008
2078.948649	193294.905291	38.216026
2080.954790	193728.617238	38.221044
2082.893883	194143.087166	38.226061
2085.185069	194581.025007	38.231079
2087.484749	195019.318612	38.236096
2090.804730	195427.125825	38.241114
2093.224946	195840.967410	38.246132
2095.096646	196259.569473	38.251149
2097.964087	196667.044415	38.256167
2100.102224	197085.658307	38.261184
2102.094626	197499.368207	38.266202
2104.154389	197915.812193	38.271220
2106.468418	198320.710807	38.276237
2108.826440	198718.923007	38.281255
2110.302671	199138.865089	38.286272
2112.660109	199543.099790	38.291290
2115.113081	199962.028443	38.296308
2117.537971	200352.486853	38.301325
2119.620660	200758.443972	38.306343
2121.923020	201180.599924	38.311360
2124.164334	201582.292230	38.316378
2126.282437	201984.563522	38.321396
2128.478067	202382.225864	38.326413
2130.428105	202786.658985	38.331431
2131.999639	203200.906497	38.336448
2133.919054	203603.568060	38.341466
2136.253299	204022.398218	38.346484
2138.109381	204441.608563	38.351501
2140.093143	204862.654359	38.356519
2141.927069	205281.742969	38.361536
2144.228862	205703.020503	38.366554
2146.273057	206130.842144	38.371572
2148.582481	206549.503737	38.376589
2150.829793	206972.291111	38.381607
2152.444007	207403.560842	38.386624
2154.506576	207824.219358	38.391642
2157.008087	208223.293892	38.396660
2158.938387	208628.072113	38.401677
2161.284383	209039.187943	38.406695
2163.163671	209445.804517	38.411712
2165.176591	209849.301756	38.416730
2166.918138	210264.781437	38.421748
2168.741220	210688.835432	38.426765
2170.821691	211114.272631	38.431783
2172.725537	211535.520997	38.436800
2175.104045	211967.136953	38.441818
2177.345668	212399.816392	38.446836
2179.093104	212857.799104	38.451853
2181.291420	213293.331737	38.456871
2183.399566	213741.961862	38.461888
2185.291763	214191.540726	38.466906
2187.620195	214643.668859	38.471924
2189.493473	215107.401686	38.476941
2191.952186	215560.628425	38.481959
2193.760557	216025.007546	38.486976
2196.011997	216492.138058	38.491994
2198.350397	216961.795924	38.497012
2200.576769	217432.919727	38.502029
2202.844601	217904.621826	38.507047
2205.298004	218379.648797	38.512064
2207.648723	218852.151769	38.517082
2210.336181	219313.170936	38.522100
2212.641436	219780.321477	38.527117
2215.292472	220246.453179	38.532135
2217.435621	220725.340826	38.537152
2220.198565	221185.714383	38.542170
2222.156225	221654.342802	38.547188
2224.592826	222131.077017	38.552205
2226.547927	222598.004194	38.557223
2229.037155	223074.679799	38.562240
2230.877655	223552.117025	38.567258
2232.997583	224035.887320	38.572276
2234.917279	224518.469486	38.577293
2237.408713	224997.888856	38.582311
2239.553282	225481.401509	38.587328
2241.613791	225965.308328	38.592346
2244.326579	226451.501615	38.597364
2246.226000	226954.994618	38.602381
2248.738449	227425.570066	38.607399
2251.681497	227906.824346	38.612416
2254.336759	228383.830009	38.617434
2256.813820	228856.214319	38.622452
2258.986347	229323.641261	38.627469
2261.300883	229801.614003	38.632487
2263.910575	230268.413623	38.637504
2265.888961	230743.719989	38.642522
2268.201188	231229.084927	38.647540
2269.860542	231709.394150	38.652557
2272.254999	232189.131371	38.657575
2274.451856	232680.508595	38.662592
2276.480084	233161.470644	38.667610
2278.531886	233644.638751	38.672628
2280.695201	234138.382482	38.677645
2282.800331	234634.802179	38.682663
2284.704222	235147.942984	38.687680
2286.998126	235648.396806	38.692698
2289.272181	236155.305676	38.697716
2291.473278	236663.724074	38.702733
2293.710377	237163.346505	38.707751
2296.486575	237665.754963	38.712768
2298.431165	238172.636133	38.717786
2301.265700	238661.900361	38.722804
2303.507592	239174.678144	38.727821
2305.835389	239661.047457	38.732839
2308.525152	240144.641471	38.737856
2310.330043	240618.007779	38.742874
2313.079343	241081.725441	38.747892
2314.806782	241557.820334	38.752909
2317.331825	242038.896290	38.757927
2319.455875	242513.073248	38.762944
2321.725497	242989.462116	38.767962
2324.364780	243470.238053	38.772980
2326.197557	243960.842484	38.777997
2328.306421	244448.303715	38.783015
2330.787795	244942.259859	38.788032
2333.153453	245449.671012	38.793050
2335.237611	245948.640188	38.798068
2337.174173	246454.718487	38.803085
2339.639307	246960.205182	38.808103
2342.002696	247468.068839	38.813120
2343.952559	247988.366544	38.818138
2346.065000	248512.803493	38.823156
2348.168398	249040.669653	38.828173
2350.808519	249577.671760	38.833191
2352.912662	250104.162857	38.838208
2355.214876	250645.608779	38.843226
2358.054257	251183.235216	38.848244
2359.670225	251730.017169	38.853261
2362.198902	252275.639113	38.858279
2364.592366	252824.785629	38.863296
2367.382988	253373.258706	38.868314
2370.005766	253923.025960	38.873332
2372.251303	254473.561090	38.878349
2374.717762	255032.340592	38.883367
2376.929322	255589.074623	38.888384
2379.316798	256151.900723	38.893402
2381.383507	256709.389351	38.898420
2383.872421	257286.267120	38.903437
2386.470745	257845.624069	38.908455
2389.372158	258402.137311	38.913472
2391.840944	258972.761997	38.918490
2394.401312	259529.069267	38.923508
2397.397569	260087.871599	38.928525
2399.904838	260645.807599	38.933543
2402.473947	261192.225024	38.938560
2404.766413	261754.481782	38.943578
2407.227271	262308.073565	38.948596
2409.394873	262863.968838	38.953613
2412.271630	263418.176168	38.958631
2414.758209	263980.264468	38.963648
2417.122191	264543.943663	38.968666
2419.668439	265087.246632	38.973684
2422.410580	265639.634588	38.978701
2425.384337	266182.052499	38.983719
2428.428381	266712.112695	38.988736
2430.510834	267260.505249	38.993754
2433.049215	267797.419816	38.998772
2435.478321	268327.871812	39.003789
2438.217161	268868.305031	39.008807
2440.398434	269401.964427	39.013824
2442.457154	269950.497726	39.018842
2445.135719	270484.429107	39.023860
2447.490200	271018.153830	39.028877
2449.820754	271574.686181	39.033895
2452.238890	272117.156645	39.038912
2454.444342	272662.552167	39.043930
2457.172829	273201.767570	39.048948
2459.267830	273745.675040	39.053965
2461.578471	274292.999449	39.058983
2463.947580	274830.812860	39.064000
2466.250896	275392.912076	39.069018
2468.333977	275941.835656	39.074036
2470.532220	276476.084046	39.079053
2472.571768	277016.931152	39.084071
2474.905307	277548.256209	39.089088
2476.822033	278088.937357	39.094106
2479.090277	278646.194079	39.099124
2481.085803	279219.005729	39.104141
2483.420302	279783.278389	39.109159
2485.672355	280378.287467	39.114176
2487.611657	280946.803063	39.119194
2490.558012	281513.735487	39.124212
2493.219867	282092.947846	39.129229
2495.488479	282681.942708	39.134247
2498.163209	283275.389649	39.139264
2500.183194	283875.942174	39.144282
2502.694422	284482.177433	39.149300
2504.804233	285090.247408	39.154317
2507.341758	285703.781126	39.159335
2510.452039	286325.447440	39.164352
2513.365043	286924.336255	39.169370
2516.170685	287531.920573	39.174388
2518.430976	288153.752941	39.179405
2520.989483	288763.827379	39.184423
2523.479464	289390.639784	39.189440
2525.356592	290014.215185	39.194458
2528.611222	290646.634715	39.199476
2531.061580	291288.821560	39.204493
2533.904991	291912.380142	39.209511
2536.431611	292540.780494	39.214528
2538.905273	293173.829009	39.219546
2542.266447	293782.485579	39.224564
2545.039210	294413.443362	39.229581
2547.697892	295039.639036	39.234599
2550.320066	295664.437350	39.239616
2552.561242	296299.418362	39.244634
2555.374212	296923.919573	39.249652
2558.267736	297548.528397	39.254669
2560.833571	298175.440878	39.259687
2563.965195	298799.618037	39.264704
2566.191618	299431.545282	39.269722
2569.795827	300042.890547	39.274740
2571.916395	300663.167539	39.279757
2574.323823	301277.223937	39.284775
2577.804343	301879.834923	39.289792
2580.673936	302502.792119	39.294810
2583.378211	303096.066653	39.299828
2585.970210	303695.647541	39.304845
2588.808706	304307.418767	39.309863
2591.158905	304906.439522	39.314880
2593.683412	305515.605333	39.319898
2596.229338	306116.663043	39.324916
2599.130266	306717.404561	39.329933
2601.561509	307327.908501	39.334951
2604.339377	307932.335244	39.339968
2606.448958	308542.519009	39.344986
2609.240985	309143.045190	39.350004
2611.575009	309752.442912	39.355021
2613.628258	310379.288671	39.360039
2616.361215	310985.537585	39.365056
2618.545823	311614.072750	39.370074
2621.298769	312231.622754	39.375092
2623.960633	312858.112814	39.380109
2626.170633	313490.654553	39.385127
2628.688945	314121.896100	39.390144
2630.554547	314754.423433	39.395162
2633.008261	315413.600176	39.400180
2635.635060	316056.853307	39.405197
2638.218137	316712.234983	39.410215
2640.511402	317345.877798	39.415232
2642.765427	317999.134683	39.420250
2645.401795	318628.746874	39.425268
2647.894653	319259.463586	39.430285
2650.679416	319891.445340	39.435303
2653.311977	320531.511207	39.440320
2655.534846	321187.618102	39.445338
2658.146386	321817.872971	39.450356
2660.894425	322464.692554	39.455373
2663.684491	323135.018014	39.460391
2666.105847	323800.924254	39.465408
2668.163828	324461.243385	39.470426
2670.828399	325124.502387	39.475444
2673.605467	325805.545044	39.480461
2676.004951	326490.339485	39.485479
2678.862739	327168.733350	39.490496
2681.496167	327866.001897	39.495514
2684.558873	328560.349881	39.500532
2687.723501	329255.532457	39.505549
2690.315866	329942.444954	39.510567
2693.640920	330629.053785	39.515584
2696.257715	331312.361190	39.520602
2698.927965	332011.935128	39.525620
2700.913894	332710.537325	39.530637
2703.939503	333411.273427	39.535655
2706.812889	334107.936056	39.540672
2709.120511	334825.677856	39.545690
2711.913639	335534.781745	39.550708
2714.940795	336241.476614	39.555725
2717.787213	336950.824105	39.560743
2720.838324	337660.963065	39.565760
2724.206431	338370.125716	39.570778
2726.858180	339078.092367	39.575796
2729.880970	339783.628511	39.580813
2732.483317	340490.864763	39.585831
2735.279240	341206.401144	39.590848
2737.832414	341928.910036	39.595866
2740.403111	342635.524903	39.600884
2743.376517	343341.454109	39.605901
2746.140676	344056.708852	39.610919
2749.370845	344773.042782	39.615936
2751.898995	345501.795720	39.620954
2754.797162	346210.315027	39.625972
2757.571415	346924.823378	39.630989
2759.997183	347656.538113	39.636007
2762.622541	348372.433455	39.641024
2765.254543	349102.005038	39.646042
2767.798371	349830.230335	39.651060
2770.961525	350560.853313	39.656077
2773.519885	351303.547030	39.661095
2776.735245	352020.158410	39.666112
2779.432031	352762.822421	39.671130
2782.229119	353479.288883	39.676148
2785.454997	354222.014124	39.681165
2787.927322	354954.216624	39.686183
2790.958003	355681.650511	39.691200
2793.613220	356424.640788	39.696218
2796.552706	357154.260109	39.701236
2799.717936	357873.966008	39.706253
2802.423018	358614.639847	39.711271
2805.258895	359336.669501	39.716288
2808.309078	360068.204909	39.721306
2810.947923	360788.963297	39.726324
2814.173265	361510.398924	39.731341
2816.934274	362226.414650	39.736359
2820.298906	362938.390667	39.741376
2823.475542	363655.219737	39.746394
2826.454482	364378.068769	39.751412
2829.191050	365057.473106	39.756429
2831.844603	365740.777404	39.761447
2834.800471	366405.087642	39.766464
2837.301251	367080.071748	39.771482
2839.657458	367758.863733	39.776500
2842.703665	368417.132867	39.781517
2845.303231	369105.585863	39.786535
2848.066162	369779.705170	39.791552
2850.700902	370479.522092	39.796570
2853.017557	371170.984072	39.801588
2855.775052	371878.779209	39.806605
2857.710917	372588.432453	39.811623
2860.837340	373288.178375	39.816640
2864.100762	374010.763425	39.821658
2866.206083	374717.472505	39.826676
2869.764598	375437.465745	39.831693
2872.445911	376168.875255	39.836711
2875.490490	376900.943090	39.841728
2878.207610	377637.272452	39.846746
2881.056413	378366.290851	39.851764
2884.017582	379111.027679	39.856781
2886.466782	379863.700950	39.861799
2889.483804	380617.530843	39.866816
2892.304420	381381.602469	39.871834
2894.689171	382154.077810	39.876852
2897.575470	382915.384088	39.881869
2900.253581	383695.720572	39.886887
2902.884015	384482.980050	39.891904
2905.484505	385275.538205	39.896922
2908.518447	386069.093166	39.901940
2911.771759	386857.929612	39.906957
2914.455927	387664.783644	39.911975
2917.406151	388469.873746	39.916992
2920.279105	389288.142096	39.922010
2922.694096	390096.402647	39.927028
2926.010627	390906.876461	39.932045
2929.248731	391735.463737	39.937063
2932.430034	392552.790759	39.942080
2935.151768	393380.642948	39.947098
2938.079233	394215.472607	39.952116
2941.009439	395043.184704	39.957133
2943.917792	395886.060053	39.962151
2947.151464	396725.918644	39.967168
2949.709357	397575.521944	39.972186
2952.605502	398419.676013	39.977204
2955.446096	399262.188511	39.982221
2958.209984	400129.738998	39.987239
2961.626762	400979.793828	39.992256
2964.612345	401826.037751	39.997274
2967.114854	402674.097207	40.002292
2970.318724	403536.237974	40.007309
2973.372460	404406.213982	40.012327
2976.339217	405264.479780	40.017344
2979.530344	406139.428525	40.022362
2982.200968	407001.570824	40.027380
2985.380860	407873.164360	40.032397
2988.547938	408734.909365	40.037415
2991.617227	409595.269891	40.042432
2994.836173	410463.770054	40.047450
2997.279651	411324.008493	40.052468
3000.655113	412187.912973	40.057485
3003.930038	413057.667145	40.062503
3007.073099	413920.375127	40.067520
3010.337524	414783.586065	40.072538
3013.339587	415648.067619	40.077556
3016.748403	416508.404273	40.082573
3019.549899	417364.400109	40.087591
3022.461391	418221.052216	40.092608
3025.606635	419058.363754	40.097626
3028.639369	419891.562839	40.102644
3032.121893	420698.867114	40.107661
3035.049486	421511.586701	40.112679
3037.869969	422319.790464	40.117696
3041.297775	423136.160730	40.122714
3043.720427	423965.599146	40.127732
3046.988475	424767.366808	40.132749
3049.752290	425582.478447	40.137767
3052.568857	426400.734155	40.142784
3055.760592	427218.241023	40.147802
3058.894697	428046.036424	40.152820
3061.362660	428879.158509	40.157837
3064.528775	429729.121560	40.162855
3067.388071	430574.445564	40.167872
3070.240302	431423.575841	40.172890
3072.759508	432286.569881	40.177908
3075.684353	433155.679175	40.182925
3078.110025	434028.718782	40.187943
3081.137347	434929.319008	40.192960
3084.179202	435815.725633	40.197978
3086.897340	436724.274307	40.202996
3090.050422	437631.651065	40.208013
3092.967333	438550.238148	40.213031
3096.026296	439476.690847	40.218048
3099.144061	440382.072141	40.223066
3101.903395	441319.039797	40.228084
3105.689828	442264.186397	40.233101
3108.876791	443202.660029	40.238119
3112.064040	444140.682049	40.243136
3116.727794	445036.100552	40.248154
3120.211780	445960.396956	40.253172
3123.795453	446886.146288	40.258189
3127.280328	447799.390263	40.263207
3130.203679	448705.504905	40.268224
3133.601262	449612.005297	40.273242
3136.703961	450534.108350	40.278260
3139.757585	451450.213715	40.283277
3142.963767	452359.331463	40.288295
3145.480685	453289.915823	40.293312
3148.803433	454214.621324	40.298330
3152.000989	455148.283268	40.303348
3155.628041	456074.610447	40.308365
3158.747305	456995.667704	40.313383
3161.336464	457930.840446	40.318400
3164.697419	458867.508148	40.323418
3167.656960	459806.811765	40.328436
3171.006153	460747.265039	40.333453
3173.870441	461679.163739	40.338471
3177.091671	462631.593421	40.343488
3180.589330	463567.478199	40.348506
3183.772526	464516.276008	40.353524
3187.092363	465453.496557	40.358541
3190.484555	466409.520661	40.363559
3193.513982	467344.662658	40.368576
3196.418409	468295.257029	40.373594
3199.266565	469252.463503	40.378612
3202.765612	470204.721827	40.383629
3206.061581	471159.125189	40.388647
3208.968320	472108.137529	40.393664
3212.670761	473052.079448	40.398682
3215.917562	474010.458580	40.403700
3219.143697	474951.187341	40.408717
3222.315734	475915.918864	40.413735
3225.430373	476875.610287	40.418752
3229.126977	477828.448797	40.423770
3231.836637	478787.332089	40.428788
3234.939260	479746.197090	40.433805
3238.146129	480693.143090	40.438823
3240.840332	481635.424743	40.443840
3244.141684	482552.709809	40.448858
3246.949521	483480.902822	40.453876
3249.985770	484414.850243	40.458893
3253.201209	485342.616636	40.463911
3256.088149	486288.516832	40.468928
3259.592057	487226.403393	40.473946
3262.613193	488172.771248	40.478964
3265.861329	489130.379543	40.483981
3269.064279	490082.847041	40.488999
3272.115680	491056.836089	40.494016
3275.271914	492016.895509	40.499034
3278.755252	492995.829324	40.504052
3281.962277	493961.497794	40.509069
3285.104663	494943.529812	40.514087
3288.279198	495943.115289	40.519104
3291.541463	496928.219909	40.524122
3294.863492	497932.179391	40.529140
3297.686043	498944.806874	40.534157
3300.981741	499971.234493	40.539175
3304.047274	500998.984763	40.544192
3307.371582	502015.398199	40.549210
3311.364349	503039.437069	40.554228
3314.515519	504071.082807	40.559245
3317.789120	505104.094711	40.564263
3320.883338	506150.746164	40.569280
3324.328223	507190.172042	40.574298
3327.666586	508237.537621	40.579316
3330.986116	509287.042030	40.584333
3334.634359	510343.710904	40.589351
3337.652384	511407.691524	40.594368
3340.874728	512471.056440	40.599386
3344.112308	513544.949082	40.604404
3347.387488	514611.612047	40.609421
3351.366248	515695.078728	40.614439
3354.320817	516781.334531	40.619456
3358.120910	517847.564472	40.624474
3361.276364	518923.714822	40.629492
3364.766215	520004.453094	40.634509
3368.791409	521089.796834	40.639527
3371.748141	522178.436123	40.644544
3375.295649	523266.945618	40.649562
3378.868935	524346.669308	40.654580
3382.341713	525427.476944	40.659597
3385.629139	526516.364818	40.664615
3389.228223	527611.042778	40.669632
3392.570237	528692.809994	40.674650
3396.424204	529776.518167	40.679668
3399.895604	530858.187140	40.684685
3403.424613	531936.141501	40.689703
3406.666837	533027.509348	40.694720
3410.312311	534115.559030	40.699738
3413.830675	535207.402800	40.704756
3416.867751	536297.923382	40.709773
3420.327777	537388.385679	40.714791
3423.358028	538497.143189	40.719808
3427.055357	539579.650706	40.724826
3430.324832	540678.342775	40.729844
3433.587499	541783.815289	40.734861
3437.603644	542860.872970	40.739879
3441.930128	543956.153499	40.744896
3445.367717	545035.070644	40.749914
3448.760797	546117.864167	40.754932
3451.906024	547202.206779	40.759949
3455.656358	548281.745571	40.764967
3458.992623	549368.927348	40.769984
3462.911476	550434.609187	40.775002
3465.759663	551501.034973	40.780007
3469.186210	552534.347415	40.785012
3472.208473	553502.945798	40.790016
3475.466401	554436.600066	40.795021
3478.658622	555305.462710	40.800026
3481.511979	556126.173433	40.805031
3484.193349	556887.811889	40.810036
3486.861265	557604.885757	40.815040
3489.312202	558269.948342	40.820045
3491.653834	558867.467051	40.825050
3493.461061	559409.022824	40.830055
3495.305384	559927.037429	40.835060
3497.277077	560381.462952	40.840064
3498.820332	560807.053857	40.845069
3500.838415	561170.520105	40.850074
3502.158782	561505.251836	40.855079
3504.169269	561785.368729	40.860084
3505.670537	562020.152502	40.865088
3507.067860	562227.222631	40.870093
3508.511406	562390.736016	40.875098
3509.744853	562528.514185	40.880103
3510.638109	562624.958311	40.885108
3511.644972	562706.266341	40.890112
3511.943768	562768.096479	40.895117
3513.391123	562785.299090	40.900122
3513.714031	562784.947469	40.905127
3514.378628	562776.707674	40.910132
3515.157053	562736.306483	40.915136
3515.644908	562690.576322	40.920141
3516.180984	562622.588805	40.925146
3516.666861	562537.180501	40.930151
3516.459619	562425.058839	40.935156
3516.798907	562310.791780	40.940160
3517.056623	562197.339936	40.945165
3517.542716	562066.121193	40.950170
3518.243087	561923.516116	40.955175
3518.227684	561767.207814	40.960180
3518.668797	561600.278229	40.965184
3518.310059	561433.320058	40.970189
3518.605576	561259.978859	40.975194
3518.787306	561075.953487	40.980199
3519.037852	560881.717355	40.985204
3518.991265	560685.665638	40.990208
3519.085832	560490.945026	40.995213
3519.213290	560273.208463	41.000218
3519.063489	560054.054199	41.005223
3518.937667	559841.925314	41.010228
3519.184969	559620.139153	41.015232
3518.746986	559404.835807	41.020237
3518.442062	559185.237479	41.025242
3518.555051	558972.000852	41.030247
3518.468831	558755.726672	41.035252
3518.469865	558529.888927	41.040256
3518.452865	558302.592647	41.045261
3518.273825	558079.085572	41.050266
3518.111442	557852.808225	41.055271
3517.824643	557638.856268	41.060276
3517.667369	557404.982461	41.065280
3518.022473	557198.861784	41.070285
3517.864021	556974.325865	41.075290
3517.661267	556740.647138	41.080295
3517.576830	556523.427734	41.085300
3517.639227	556298.794531	41.090304
3517.038295	556073.406046	41.095309
3517.244090	555853.465948	41.100314
3517.021644	555637.357557	41.105319
3516.621495	555419.715011	41.110324
3516.596078	555204.020468	41.115328
3516.354785	554981.972976	41.120333
3516.243643	554771.912849	41.125338
3516.197718	554560.582435	41.130343
3515.820666	554341.258251	41.135348
3515.670795	554133.605511	41.140352
3515.843230	553932.382804	41.145357
3515.746686	553735.018555	41.150362
3515.614169	553519.712663	41.155367
3515.473656	553324.761205	41.160372
3515.272088	553104.432249	41.165376
3515.093721	552907.519626	41.170381
3514.971670	552714.917981	41.175386
3514.925272	552517.626624	41.180391
3514.418092	552319.448665	41.185396
3514.613874	552120.404044	41.190400
3514.492178	551921.857999	41.195405
3513.936688	551730.414131	41.200410
3513.825749	551546.137182	41.205415
3513.972628	551358.499349	41.210420
3513.721197	551168.959959	41.215424
3513.556311	550985.235926	41.220429
3512.958939	550803.386313	41.225434
3513.297011	550630.437989	41.230439
3512.711657	550443.754714	41.235444
3512.884665	550274.547471	41.240448
3512.534226	550118.089267	41.245453
3512.643364	549936.116803	41.250458
3512.554087	549769.608138	41.255463
3512.326423	549607.593624	41.260468
3512.403955	549429.490078	41.265472
3511.983384	549271.925810	41.270477
3511.751737	549109.151116	41.275482
3511.891396	548953.406279	41.280487
3511.297999	548783.694330	41.285492
3511.713897	548631.371947	41.290496
3511.299966	548479.729936	41.295501
3511.412013	548326.847655	41.300506
3511.020920	548176.656613	41.305511
3510.994331	548031.385330	41.310516
3510.871606	547870.689302	41.315520
3511.112117	547728.792381	41.320525
3511.056366	547578.139561	41.325530
3510.953727	547435.739502	41.330535
3510.671123	547285.872741	41.335540
3510.839826	547140.107971	41.340544
3510.032423	547000.477912	41.345549
3510.371500	546860.416413	41.350554
3510.278705	546708.803229	41.355559
3510.048308	546582.808202	41.360564
3510.203663	546436.685177	41.365568
3509.961965	546312.348808	41.370573
3509.530347	546173.405328	41.375578
3509.609665	546041.472250	41.380583
3509.598651	545901.705861	41.385588
3509.034120	545779.878824	41.390592
3508.943802	545666.074394	41.395597
3509.302513	545542.592492	41.400602
3509.227713	545412.587964	41.405607
3508.903454	545301.532617	41.410612
3509.004915	545170.693377	41.415616
3509.206742	545057.290589	41.420621
3508.712726	544940.172361	41.425626
3508.673807	544816.946325	41.430631
3508.621173	544702.825420	41.435636
3508.575392	544581.107104	41.440640
3508.575857	544473.363933	41.445645
3508.394805	544356.895721	41.450650
3508.525539	544239.070069	41.455655
3507.915555	544136.600021	41.460660
3508.309293	544021.598591	41.465664
3508.153001	543908.844710	41.470669
3508.033426	543802.070173	41.475674
3508.202041	543700.984483	41.480679
3507.880321	543596.201481	41.485684
3507.867168	543484.276662	41.490688
3507.821496	543385.032723	41.495693
3507.453967	543278.493518	41.500698
3507.642002	543178.708522	41.505703
3507.185938	543079.073267	41.510708
3507.140565	542988.830920	41.515712
3507.490264	542886.855267	41.520717
3507.332381	542788.630198	41.525722
3507.050285	542684.889850	41.530727
3507.012310	542605.157880	41.535732
3507.243304	542506.719165	41.540736
3506.580185	542415.411726	41.545741
3507.235670	542323.194104	41.550746
3506.959456	542234.743070	41.555751
3506.826462	542150.444838	41.560756
3506.810088	542044.092043	41.565760
3506.761382	541964.005500	41.570765
3506.939983	541869.997274	41.575770
3506.553112	541786.440459	41.580775
3506.410099	541693.386562	41.585780
3506.388802	541615.205373	41.590784
3506.243896	541532.917330	41.595789
3506.116570	541447.758195	41.600794
3506.051308	541362.387575	41.605799
3506.270441	541293.776742	41.610804
3506.076437	541209.330756	41.615808
3505.832281	541137.923295	41.620813
3505.900002	541054.492134	41.625818
3506.181286	540966.297626	41.630823
3505.688893	540897.443156	41.635828
3505.848397	540828.537182	41.640832
3505.747184	540756.602168	41.645837
3505.637040	540674.605002	41.650842
3505.271671	540604.773170	41.655847
3505.194428	540542.493863	41.660852
3505.330183	540467.853569	41.665856
3505.046099	540407.366860	41.670861
3505.494673	540335.394208	41.675866
3505.571730	540263.831182	41.680871
3505.359536	540202.678181	41.685876
3505.151677	540128.491894	41.690880
3504.967445	540070.755517	41.695885
3504.888206	540006.360519	41.700890
3505.109708	539940.861704	41.705895
3504.686036	539889.904451	41.710900
3505.073957	539815.321704	41.715904
3505.028303	539762.292348	41.720909
3504.964001	539695.075561	41.725914
3505.320439	539629.352861	41.730919
3504.932135	539565.255313	41.735924
3505.222164	539504.071104	41.740928
3505.214555	539436.038996	41.745933
3505.099585	539366.312320	41.750938
3504.804367	539298.424870	41.755943
3504.629002	539251.754025	41.760948
3505.123070	539193.505526	41.765952
3504.564120	539131.243913	41.770957
3504.760173	539066.901946	41.775962
3504.986697	539007.939398	41.780967
3504.385304	538949.407345	41.785972
3504.549999	538888.440963	41.790976
3504.727737	538832.806496	41.795981
3504.788261	538773.365462	41.800986
3504.634941	538723.619527	41.805991
3504.462454	538672.064729	41.810996
3504.314224	538607.774011	41.816000
3504.445113	538556.825747	41.821005
3504.329335	538498.316695	41.826010
3504.345775	538452.871173	41.831015
3504.498928	538410.624994	41.836020
3504.336922	538354.689031	41.841024
3504.408986	538293.985838	41.846029
3504.114289	538249.493859	41.851034
3504.352739	538194.602033	41.856039
3503.968321	538146.298915	41.861044
3504.281243	538082.084757	41.866048
3504.322774	538035.325365	41.871053
3504.217305	537993.721962	41.876058
3504.103626	537937.122402	41.881063
3504.122927	537885.081631	41.886068
3504.016080	537834.016489	41.891072
3504.013885	537796.170890	41.896077
3503.478281	537747.436840	41.901082
3503.894329	537705.600359	41.906087
3503.857259	537660.713939	41.911092
3503.896222	537616.469791	41.916096
3503.906832	537573.085478	41.921101
3503.835030	537530.468763	41.926106
3503.879490	537481.341462	41.931111
3504.012607	537445.134599	41.936116
3503.578564	537393.112038	41.941120
3503.908499	537346.355570	41.946125
3503.889127	537302.723359	41.951130
3503.633201	537259.228467	41.956135
3503.838181	537217.171586	41.961140
3503.524321	537168.249827	41.966144
3504.097926	537121.957916	41.971149
3503.724261	537078.329741	41.976154
3503.883693	537032.252946	41.981159
3503.500337	536989.682907	41.986164
3504.000449	536940.281299	41.991168
3503.775850	536900.454434	41.996173
3503.642272	536860.965596	42.001178
3503.874314	536809.289982	42.006183
3503.685346	536774.993588	42.011188
3503.925661	536724.222302	42.016192
3504.211368	536690.002809	42.021197
3503.689964	536631.195991	42.026202
3503.622863	536591.393986	42.031207
3503.656653	536555.753712	42.036212
3503.569176	536500.854995	42.041216
3503.709116	536461.473358	42.046221
3503.453453	536423.562470	42.051226
3503.609496	536382.517112	42.056231
3503.753539	536342.782143	42.061236
3503.628563	536293.072650	42.066240
3503.474645	536252.377107	42.071245
3503.476934	536213.418793	42.076250
3503.653795	536167.386507	42.081255
3503.084340	536139.237969	42.086260
3503.733919	536092.829853	42.091264
3503.609684	536060.836826	42.096269
3503.700417	536023.877530	42.101274
3503.443816	535981.737419	42.106279
3502.958811	535943.508458	42.111284
3502.930857	535898.715105	42.116288
3503.024998	535874.137142	42.121293
3502.943811	535839.821470	42.126298
3503.776381	535799.172318	42.131303
3503.368878	535759.521370	42.136308
3503.582503	535721.988395	42.141312
3503.392798	535680.440907	42.146317
3503.479168	535640.863745	42.151322
3503.523977	535603.256023	42.156327
3503.059473	535566.784498	42.161332
3503.030522	535530.094084	42.166336
3503.180827	535503.140879	42.171341
3503.240102	535467.141262	42.176346
3503.181529	535435.589484	42.181351
3502.927816	535392.037567	42.186356
3503.193761	535358.069282	42.191360
3503.083013	535337.498773	42.196365
3502.864862	535295.249749	42.201370
3503.066506	535268.590086	42.206375
3503.352380	535233.158596	42.211380
3503.403843	535193.585490	42.216384
3503.232920	535164.215033	42.221389
3503.084771	535130.310586	42.226394
3503.165662	535084.239016	42.231399
3502.804256	535054.495248	42.236404
3502.711926	535025.011567	42.241408
3502.983519	534988.474192	42.246413
3503.045951	534967.976818	42.251418
3503.319247	534929.777850	42.256423
3502.548732	534903.218372	42.261428
3502.433528	534870.616912	42.266432
3502.307332	534855.635617	42.271437
3502.369260	534828.292042	42.276442
3502.547407	534790.157805	42.281447
3502.377929	534774.478406	42.286452
3502.755991	534748.394281	42.291456
3502.348141	534725.150715	42.296461
3502.400285	534699.922634	42.301466
3502.464814	534678.719725	42.306471
3502.742399	534661.611457	42.311476
3502.756128	534629.442378	42.316480
3502.668456	534601.114811	42.321485
3503.037052	534565.165217	42.326490
3502.886127	534533.323559	42.331495
3502.664790	534508.792080	42.336500
3502.410652	534468.710562	42.341504
3502.294861	534449.498601	42.346509
3502.682817	534429.805500	42.351514
3503.043735	534398.739645	42.356519
3502.663165	534372.420430	42.361524
3502.694809	534334.962072	42.366528
3502.834878	534313.646126	42.371533
3502.902605	534283.431071	42.376538
3503.101555	534249.067563	42.381543
3502.477714	534228.474442	42.386548
3502.807601	534194.895872	42.391552
3503.003900	534172.815825	42.396557
3502.966081	534137.280672	42.401562
3503.258409	534105.520006	42.406567
3502.953252	534081.957248	42.411572
3502.957642	534044.905023	42.416576
3503.181993	534009.479747	42.421581
3502.774059	533975.058923	42.426586
3502.765073	533940.324215	42.431591
3503.103915	533914.143825	42.436596
3503.344268	533877.255770	42.441600
3503.018452	533833.055348	42.446605
3503.033297	533804.760421	42.451610
3503.084066	533770.066299	42.456615
3502.878363	533745.681964	42.461620
3502.879808	533709.283694	42.466624
3503.190429	533674.095790	42.471629
3502.881136	533636.990522	42.476634
3503.231348	533613.375268	42.481639
3503.071219	533579.871354	42.486644
3502.940644	533552.706065	42.491648
3502.799663	533524.535461	42.496653
3502.665170	533492.990742	42.501658
3502.679067	533451.756788	42.506663
3502.634444	533442.047287	42.511668
3502.750799	533421.035625	42.516672
3502.746815	533385.895895	42.521677
3502.512021	533349.885785	42.526682
3502.672288	533333.549186	42.531687
3502.623847	533303.551296	42.536692
3502.905871	533275.817773	42.541696
3502.867793	533242.545716	42.546701
3502.707371	533213.118836	42.551706
3503.268011	533177.034812	42.556711
3502.651850	533159.409150	42.561716
3502.854225	533123.431072	42.566720
3503.057732	533087.805136	42.571725
3502.767547	533070.078281	42.576730
3502.724267	533027.140122	42.581735
3502.617734	533006.867313	42.586740
3502.688172	532975.591518	42.591744
3502.657018	532946.798415	42.596749
3502.616935	532926.263409	42.601754
3502.966031	532888.298347	42.606759
3502.750092	532872.170748	42.611764
3502.496502	532848.446676	42.616768
3502.577774	532814.701830	42.621773
3502.531776	532790.290841	42.626778
3502.659644	532762.831944	42.631783
3502.271241	532738.222405	42.636788
3502.395862	532709.404534	42.641792
3502.716133	532692.438066	42.646797
3502.182871	532668.706837	42.651802
3502.347695	532638.019707	42.656807
3502.437316	532618.118544	42.661812
3502.553898	532604.506583	42.666816
3502.483699	532575.265603	42.671821
3502.214385	532539.359306	42.676826
3502.690801	532520.757191	42.681831
3502.596771	532487.693294	42.686836
3502.685453	532460.944727	42.691840
3502.647854	532437.186290	42.696845
3502.461630	532417.478789	42.701850
3502.603353	532384.126202	42.706855
3502.525384	532368.681383	42.711860
3502.657901	532338.904842	42.716864
3502.841337	532318.988623	42.721869
3502.286997	532294.655806	42.726874
3502.216270	532266.471534	42.731879
3502.400443	532261.659718	42.736884
3502.385477	532224.051460	42.741888
3502.442616	532197.559003	42.746893
3502.497598	532165.780172	42.751898
3502.475860	532136.480314	42.756903
3502.279961	532122.161235	42.761908
3502.456759	532098.066720	42.766912
3502.858115	532073.383372	42.771917
3502.421194	532048.075180	42.776922
3502.685588	532028.548715	42.781927
3503.031219	532006.240344	42.786932
3503.090264	531964.591840	42.791937
3502.615205	531937.023621	42.796941
3502.374892	531903.326451	42.801946
3502.944359	531872.272445	42.806951
3502.853644	531850.031707	42.811956
3502.533405	531819.116024	42.816961
3502.972346	531795.181558	42.821965
3502.975873	531766.833596	42.826970
3502.963971	531727.461152	42.831975
3503.098335	531700.099701	42.836980
3502.630468	531670.364707	42.841985
3502.454407	531634.693152	42.846989
3502.303822	531613.518701	42.851994
3502.340637	531590.149947	42.856999
3502.678262	531565.525906	42.862004
3502.206167	531544.250319	42.867009
3502.386657	531514.514779	42.872013
3502.444451	531499.803075	42.877018
3502.543127	531474.007605	42.882023
3502.569941	531448.827490	42.887028
3502.326087	531420.466917	42.892033
3502.616846	531401.438930	42.897037
3502.212946	531385.137323	42.902042
3502.501012	531366.260761	42.907047
3502.679850	531338.085994	42.912052
3502.616031	531302.194652	42.917057
3502.643591	531282.502515	42.922061
3502.451226	531259.370240	42.927066
3502.649767	531224.948438	42.932071
3502.562569	531205.274041	42.937076
3502.576376	531180.800371	42.942081
3502.544989	531151.600504	42.947085
3502.481934	531122.909031	42.952090
3502.462612	531101.864381	42.957095
3502.506041	531077.486614	42.962100
3502.690703	531043.771440	42.967105
3502.245233	531025.965248	42.972109
3502.417249	531003.581474	42.977114
3502.391163	530991.702051	42.982119
3502.382541	530970.202341	42.987124
3502.370002	530931.230420	42.992129
3502.400197	530915.867752	42.997133
3502.297190	530896.396765	43.002138
3502.593380	530860.397832	43.007143
3502.466282	530841.987950	43.012148
3502.620794	530811.852018	43.017153
3502.616309	530788.186128	43.022157
3502.384623	530767.778239	43.027162
3502.203034	530733.565357	43.032167
3502.563432	530717.496462	43.037172
3502.506249	530701.492528	43.042177
3502.700804	530674.169914	43.047181
3502.612852	530648.150079	43.052186
3502.525774	530614.274663	43.057191
3502.580505	530596.087915	43.062196
3502.537941	530568.298427	43.067201
3502.565311	530531.534735	43.072205
3502.523182	530514.218988	43.077210
3502.545751	530490.548349	43.082215
3502.339609	530462.683379	43.087220
3502.580610	530434.094145	43.092225
3502.641770	530409.158458	43.097229
3502.096446	530390.359817	43.102234
3502.205637	530366.222269	43.107239
3501.912083	530347.384387	43.112244
3502.537878	530328.453773	43.117249
3502.683085	530294.239243	43.122253
3501.919952	530273.006866	43.127258
3502.194104	530259.267225	43.132263
3502.215263	530235.797770	43.137268
3502.299725	530215.742673	43.142273
3502.432378	530189.184029	43.147277
3502.491262	530175.779940	43.152282
3502.328277	530148.864365	43.157287
3502.449468	530123.415223	43.162292
3502.279509	530099.975264	43.167297
3502.318852	530075.042336	43.172301
3502.191922	530060.659899	43.177306
3502.400458	530027.190176	43.182311
3502.095182	530009.108991	43.187316
3502.211312	529988.545044	43.192321
3502.272504	529977.507196	43.197325
3502.291808	529956.001472	43.202330
3502.282390	529931.730507	43.207335
3502.423325	529912.169736	43.212340
3501.902086	529886.215809	43.217345
3502.544713	529869.396946	43.222349
3502.155064	529848.156115	43.227354
3502.446077	529818.147729	43.232359
3502.447004	529799.363948	43.237364
3502.454092	529775.241200	43.242369
3502.509932	529746.981430	43.247373
3502.114074	529731.180085	43.252378
3502.120255	529706.251615	43.257383
3502.277091	529688.047717	43.262388
3502.048881	529665.925371	43.267393
3502.204935	529651.901319	43.272397
3502.209119	529627.476598	43.277402
3502.434578	529613.391347	43.282407
3502.470615	529586.342927	43.287412
3502.224078	529569.460610	43.292417
3501.833566	529546.456854	43.297421
3502.026173	529532.628424	43.302426
3502.464393	529497.912986	43.307431
3502.143214	529491.567294	43.312436
3501.911178	529469.243773	43.317441
3501.837870	529449.715650	43.322445
3502.135912	529432.698055	43.327450
3501.881639	529409.471418	43.332455
3502.054559	529400.984044	43.337460
3502.208777	529382.780130	43.342465
3502.403240	529359.131057	43.347469
3502.327817	529338.595900	43.352474
3502.289851	529319.062084	43.357479
3502.009342	529284.609006	43.362484
3502.283060	529257.774723	43.367489
3502.073552	529247.987033	43.372493
3502.208201	529236.634968	43.377498
3502.361045	529203.725775	43.382503
3502.087623	529183.019743	43.387508
3502.064577	529169.425932	43.392513
3502.139768	529143.478441	43.397517
3501.892417	529127.351092	43.402522
3502.009437	529108.497896	43.407527
3502.192983	529083.993892	43.412532
3502.299864	529078.437523	43.417537
3502.311468	529048.773025	43.422541
3502.142129	529038.928566	43.427546
3502.216272	529010.714724	43.432551
3502.131558	529000.907429	43.437556
3502.208099	528981.858905	43.442561
3502.364089	528955.747386	43.447565
3502.255455	528927.461084	43.452570
3502.295990	528903.633699	43.457575
3502.248954	528888.280671	43.462580
3501.769580	528867.606190	43.467585
3502.010219	528849.337728	43.472589
3501.857086	528824.533098	43.477594
3501.905398	528811.330708	43.482599
3501.856843	528798.143379	43.487604
3501.816987	528795.480363	43.492609
3501.952779	528769.623428	43.497613
3501.929297	528756.029257	43.502618
3502.010260	528735.116285	43.507623
3501.894812	528713.478407	43.512628
3501.934916	528708.838797	43.517633
3502.354170	528682.383594	43.522637
3502.435199	528670.938660	43.527642
3502.200331	528634.210457	43.532647
3502.431579	528621.634125	43.537652
3502.069875	528602.099258	43.542657
3502.274086	528591.239440	43.547661
3501.958784	528574.014001	43.552666
3501.833267	528551.571617	43.557671
3502.126719	528537.625724	43.562676
3502.223786	528512.429029	43.567681
3502.434897	528493.006315	43.572685
3502.146631	528476.683080	43.577690
3501.841309	528450.843799	43.582695
3502.244813	528427.966338	43.587700
3501.891867	528417.092350	43.592705
3502.257374	528401.271649	43.597709
3502.387575	528391.833365	43.602714
3502.398491	528362.671063	43.607719
3502.212775	528344.568974	43.612724
3502.024803	528318.761536	43.617729
3502.376325	528292.517547	43.622733
3502.309054	528292.326531	43.627738
3501.990644	528258.632120	43.632743
3501.912922	528239.203614	43.637748
3502.097415	528225.022524	43.642753
3502.245954	528198.104834	43.647757
3502.033007	528185.597209	43.652762
3502.126938	528151.838359	43.657767
3502.059024	528143.337288	43.662772
3502.012443	528116.600888	43.667777
3502.006104	528105.370518	43.672781
3501.767925	528092.715636	43.677786
3502.088079	528071.613295	43.682791
3502.235342	528048.120308	43.687796
3502.030988	528035.006822	43.692801
3502.375435	528015.059006	43.697805
3502.089228	527988.510730	43.702810
3502.155532	527969.865257	43.707815
3502.293876	527945.013612	43.712820
3501.934947	527939.126327	43.717825
3502.190373	527913.097999	43.722829
3502.103571	527899.613528	43.727834
3501.921834	527876.171431	43.732839
3502.205915	527853.915947	43.737844
3502.354159	527836.315214	43.742849
3502.143102	527814.791468	43.747853
3501.992966	527791.847962	43.752858
3502.400808	527769.019051	43.757863
3502.259162	527756.147360	43.762868
3502.080754	527742.626618	43.767873
3501.940571	527716.357267	43.772877
3501.874762	527710.625731	43.777882
3501.718426	527683.502602	43.782887
3501.751449	527676.446147	43.787892
3501.900356	527655.772721	43.792897
3501.847169	527643.995217	43.797901
3502.024571	527629.159828	43.802906
3501.915140	527608.576895	43.807911
3501.911615	527585.610215	43.812916
3502.265328	527584.648545	43.817921
3502.278679	527554.980411	43.822925
3502.165018	527537.621503	43.827930
3501.954609	527516.550472	43.832935
3502.058336	527503.338149	43.837940
3501.870164	527480.551121	43.842945
3501.911851	527450.928711	43.847949
3502.026885	527457.861458	43.852954
3501.912246	527426.752304	43.857959
3502.232860	527410.836670	43.862964
3502.037882	527390.317077	43.867969
3502.178917	527375.789267	43.872973
3502.045328	527357.274770	43.877978
3502.220820	527330.552588	43.882983
3502.085385	527312.239786	43.887988
3501.859953	527301.143560	43.892993
3502.061740	527283.785599	43.897997
3502.011367	527262.890730	43.903002
3501.809589	527253.352190	43.908007
3502.367701	527224.051853	43.913012
3502.140632	527216.229736	43.918017
3502.066103	527184.307879	43.923021
3501.904526	527180.756849	43.928026
3502.148790	527160.470757	43.933031
3501.979146	527137.277307	43.938036
3501.836957	527115.892809	43.943041
3501.896808	527101.427700	43.948045
3501.734822	527089.968844	43.953050
3502.137842	527086.380299	43.958055
3502.155426	527075.296436	43.963060
3501.785862	527052.285051	43.968065
3502.050277	527021.367801	43.973069
3501.555389	527012.529493	43.978074
3501.843755	526998.280556	43.983079
3502.230770	526974.345400	43.988084
3501.914319	526968.148854	43.993089
3502.144127	526941.870756	43.998093
3502.149382	526937.991485	44.003098
3502.003915	526906.583688	44.008103
3501.672873	526893.790998	44.013108
3501.994738	526877.118989	44.018113
3501.973063	526853.801276	44.023117
3501.960682	526844.182597	44.028122
3502.026761	526820.750432	44.033127
3501.810200	526805.874686	44.038132
3502.047455	526796.116387	44.043137
3502.305891	526778.900058	44.048141
3502.095556	526765.534392	44.053146
3501.847540	526738.524329	44.058151
3502.122958	526728.357082	44.063156
3501.664146	526710.194507	44.068161
3502.195155	526678.378680	44.073165
3502.163861	526666.445788	44.078170
3501.757318	526646.713515	44.083175
3501.849618	526632.796918	44.088180
3501.717843	526610.654428	44.093185
3501.688368	526603.808607	44.098189
3501.793678	526605.756640	44.103194
3501.970010	526575.607614	44.108199
3501.949568	526557.678837	44.113204
3501.842561	526546.210953	44.118209
3501.935894	526524.990333	44.123213
3501.899591	526512.604744	44.128218
3501.888806	526495.429942	44.133223
3501.974923	526476.426685	44.138228
3502.124784	526466.933598	44.143233
3502.254435	526445.505715	44.148237
3501.912065	526434.426958	44.153242
3502.126242	526402.760516	44.158247
3502.046849	526396.274955	44.163252
3501.976909	526371.754995	44.168257
3502.083082	526345.797184	44.173261
3502.186105	526333.994205	44.178266
3502.247728	526316.858275	44.183271
3501.871990	526292.234639	44.188276
3501.703434	526280.826475	44.193281
3502.173965	526261.763091	44.198285
3502.101086	526243.993165	44.203290
3502.237567	526225.485429	44.208295
3502.345669	526205.269437	44.213300
3502.116028	526186.012668	44.218305
3502.036269	526165.422873	44.223309
3501.925706	526147.104587	44.228314
3501.932179	526141.663356	44.233319
3502.454461	526112.466888	44.238324
3501.895712	526092.606356	44.243329
3502.490500	526068.486119	44.248333
3502.024361	526059.743441	44.253338
3502.077260	526032.131014	44.258343
3502.209257	526019.970639	44.263348
3501.918958	525999.866703	44.268353
3501.865805	525988.893684	44.273357
3502.249424	525958.660627	44.278362
3501.760689	525943.624774	44.283367
3501.994615	525926.562275	44.288372
3501.788278	525904.329461	44.293377
3502.183208	525900.338875	44.298381
3501.830598	525873.091458	44.303386
3501.978768	525853.019815	44.308391
3502.021609	525842.031736	44.313396
3501.726374	525829.182069	44.318401
3501.883777	525824.674315	44.323405
3501.834110	525804.985999	44.328410
3502.012403	525786.622267	44.333415
3502.181531	525773.498791	44.338420
3501.919410	525750.266928	44.343425
3502.484789	525721.264391	44.348429
3502.267505	525711.324159	44.353434
3501.827191	525686.709446	44.358439
3502.147512	525669.633173	44.363444
3502.243658	525644.531910	44.368449
3501.937172	525625.387033	44.373453
3502.087547	525610.503219	44.378458
3502.032938	525586.735036	44.383463
3501.978929	525577.474536	44.388468
3501.662778	525554.099615	44.393473
3502.065518	525531.872146	44.398477
3502.126270	525536.547495	44.403482
3502.144371	525509.594266	44.408487
3502.158618	525492.968392	44.413492
3502.195036	525467.775341	44.418497
3502.279537	525440.660515	44.423501
3502.311085	525426.953608	44.428506
3501.955736	525413.911393	44.433511
3502.181885	525391.459296	44.438516
3501.627979	525373.259307	44.443521
3501.821353	525348.293481	44.448525
3501.661952	525338.646214	44.453530
3501.735787	525337.224190	44.458535
3501.768455	525314.298318	44.463540
3501.964972	525301.371617	44.468545
3502.388295	525278.989398	44.473549
3501.906528	525259.619392	44.478554
3502.173977	525240.082394	44.483559
3502.199090	525224.411631	44.488564
3502.007734	525217.590287	44.493569
3502.288877	525175.029344	44.498573
3501.914610	525175.389813	44.503578
3501.936430	525145.362339	44.508583
3501.958740	525131.807694	44.513588
3501.612896	525127.680273	44.518593
3501.663504	525102.030937	44.523597
3501.755735	525094.359381	44.528602
3501.746171	525092.194667	44.533607
3501.751174	525067.005746	44.538612
3502.007521	525048.729602	44.543617
3501.775705	525040.806183	44.548621
3501.799525	525026.848186	44.553626
3501.760219	525014.360915	44.558631
3501.960152	524996.345361	44.563636
3502.053849	524972.653756	44.568641
3502.034324	524948.526337	44.573645
3502.014090	524936.287909	44.578650
3502.061042	524931.041390	44.583655
3501.990602	524902.287145	44.588660
3502.078473	524884.137747	44.593665
3501.719633	524873.715146	44.598669
3501.722839	524851.246455	44.603674
3501.364263	524833.317592	44.608679
3501.912258	524817.262720	44.613684
3502.070555	524798.749607	44.618689
3501.993883	524786.822087	44.623693
3502.041240	524775.530162	44.628698
3501.790227	524759.750689	44.633703
3501.722291	524746.058563	44.638708
3501.767142	524724.943371	44.643713
3502.178371	524710.169093	44.648717
3501.578194	524703.360724	44.653722
3501.974967	524682.593723	44.658727
3501.734149	524669.986353	44.663732
3501.213143	524661.906198	44.668737
3501.828329	524634.505640	44.673741
3501.955296	524635.896437	44.678746
3501.684839	524626.719336	44.683751
3501.981439	524606.471584	44.688756
3502.054935	524590.893303	44.693761
3502.009002	524572.462035	44.698765
3501.629392	524547.735009	44.703770
3501.755904	524552.652361	44.708775
3501.859626	524533.341321	44.713780
3501.869550	524520.997062	44.718785
3501.569107	524505.476871	44.723789
3501.510535	524491.379998	44.728794
3501.719238	524472.405183	44.733799
3501.856365	524476.162206	44.738804
3501.714429	524459.508968	44.743809
3501.676674	524429.086124	44.748813
3501.953708	524427.027839	44.753818
3501.818644	524409.718547	44.758823
3502.035388	524386.006753	44.763828
3501.929881	524383.756096	44.768833
3501.770976	524347.810242	44.773837
3501.722579	524345.651449	44.778842
3501.757063	524335.671010	44.783847
3502.105316	524300.250657	44.788852
3501.685901	524314.119783	44.793857
3501.620037	524280.577468	44.798861
3501.722859	524266.556002	44.803866
3501.814170	524251.125691	44.808871
3501.749350	524252.143337	44.813876
3501.661338	524229.738174	44.818881
3501.899210	524206.526569	44.823885
3502.076707	524207.204234	44.828890
3501.685665	524170.437575	44.833895
3501.609670	524167.628112	44.838900
3501.450547	524157.425768	44.843905
3501.682880	524134.819457	44.848909
3501.808088	524126.638416	44.853914
3502.047331	524118.137346	44.858919
3501.705378	524099.247690	44.863924
3501.724279	524091.637350	44.868929
3501.731412	524071.786494	44.873933
3502.051321	524057.277607	44.878938
3502.129177	524049.557308	44.883943
3501.994797	524023.027843	44.888948
3501.920246	524018.202916	44.893953
3501.863521	523982.089037	44.898957
3501.439190	523972.633147	44.903962
3501.680885	523957.481378	44.908967
3501.784686	523951.973726	44.913972
3501.613650	523935.928929	44.918977
3501.998284	523931.586701	44.923981
3501.816946	523930.909564	44.928986
3501.654165	523897.482130	44.933991
3501.832186	523891.005671	44.938996
3501.507393	523873.574066	44.944001
3501.619534	523846.149414	44.949005
3501.251733	523840.563961	44.954010
3500.915356	523838.449899	44.959015
3501.428428	523837.261652	44.964020
3501.325521	523838.537161	44.969025
3501.617076	523822.269100	44.974029
3501.675653	523808.606707	44.979034
3501.696233	523799.383746	44.984039
3501.431165	523789.902943	44.989044
3501.392468	523765.725989	44.994049
3501.502218	523759.663139	44.999053
3501.396744	523760.838293	45.004058
3501.835014	523750.441914	45.009063
3501.899402	523724.283976	45.014068
3501.658184	523729.057330	45.019073
3501.633316	523704.273538	45.024077
3501.663676	523684.216966	45.029082
3501.486944	523665.603275	45.034087
3501.958784	523663.111508	45.039092
3501.614897	523656.816914	45.044097
3501.692073	523631.261383	45.049101
3501.375513	523632.267868	45.054106
3501.648575	523636.407029	45.059111
3501.743114	523606.667070	45.064116
3501.717575	523600.675583	45.069121
3502.051019	523584.400715	45.074125
3501.769014	523561.671947	45.079130
3501.818827	523557.683993	45.084135
3501.615931	523540.787186	45.089140
3501.700470	523525.810531	45.094145
3501.816546	523501.860927	45.099149
3501.914813	523508.294526	45.104154
3502.051055	523478.043970	45.109159
3502.262155	523468.236929	45.114164
3501.901225	523442.799595	45.119169
3502.132500	523424.928196	45.124173
3501.829541	523406.585699	45.129178
3501.951219	523391.502350	45.134183
3502.089940	523373.746051	45.139188
3501.716916	523355.918213	45.144193
3501.813767	523334.641586	45.149197
3501.970545	523320.913031	45.154202
3501.858907	523310.853800	45.159207
3502.352609	523302.161469	45.164212
3501.914253	523280.615360	45.169217
3501.966501	523251.687322	45.174221
3501.756967	523235.849209	45.179226
3501.505009	523220.219211	45.184231
3501.935116	523206.951839	45.189236
3501.699507	523202.252445	45.194241
3501.701391	523175.448179	45.199245
3501.945806	523179.289639	45.204250
3502.022108	523156.353275	45.209255
3501.856414	523148.821508	45.214260
3501.169444	523142.831976	45.219265
3502.042447	523128.588703	45.224269
3501.701704	523109.898993	45.229274
3501.478607	523103.736492	45.234279
3502.060658	523073.667569	45.239284
3501.588004	523064.873543	45.244289
3501.915622	523054.141160	45.249293
3501.791110	523028.817401	45.254298
3501.953913	523014.382220	45.259303
3502.095622	522995.012666	45.264308
3501.664713	522987.370926	45.269313
3502.128010	522966.187844	45.274317
3502.242839	522956.949638	45.279322
3501.754395	522942.212647	45.284327
3501.721999	522922.013548	45.289332
3502.232313	522897.548058	45.294337
3501.661905	522881.816066	45.299341
3501.534209	522869.844391	45.304346
3501.688877	522861.204534	45.309351
3501.745053	522851.471537	45.314356
3501.713338	522846.488366	45.319361
3501.387127	522814.444045	45.324365
3501.595767	522805.191136	45.329370
3501.492202	522796.440268	45.334375
3501.765186	522784.154241	45.339380
3501.588840	522768.260025	45.344385
3501.597478	522763.724009	45.349389
3501.827580	522760.413153	45.354394
3502.061801	522739.265361	45.359399
3501.476216	522722.477457	45.364404
3501.643177	522716.304464	45.369409
3501.775995	522687.664984	45.374413
3501.709226	522675.129416	45.379418
3501.641026	522674.182681	45.384423
3501.461813	522650.932518	45.389428
3501.425400	522645.748463	45.394433
3502.004499	522632.054257	45.399437
3501.772332	522624.834851	45.404442
3501.741714	522605.441167	45.409447
3501.778297	522594.753707	45.414452
3501.731415	522581.711102	45.419457
3501.459910	522556.308554	45.424461
3501.546888	522549.543302	45.429466
3501.157109	522551.266659	45.434471
3501.632116	522536.328911	45.439476
3501.603856	522519.202096	45.444481
3501.500075	522503.900905	45.449485
3501.698083	522496.715262	45.454490
3501.599014	522491.188195	45.459495
3501.889322	522470.434341	45.464500
3501.867287	522474.015152	45.469505
3502.026559	522455.297106	45.474509
3501.646868	522429.860768	45.479514
3501.359194	522423.708002	45.484519
3501.566041	522409.315704	45.489524
3501.394482	522403.044087	45.494529
3501.458380	522387.464739	45.499533
3501.625358	522380.384635	45.504538
3501.509371	522379.898793	45.509543
3501.873246	522349.005635	45.514548
3501.782996	522345.039117	45.519553
3501.585258	522336.151443	45.524557
3501.280663	522304.505633	45.529562
3501.747296	522308.060832	45.534567
3501.998320	522299.556781	45.539572
3501.650526	522287.114969	45.544577
3501.908807	522261.478262	45.549581
3501.983675	522257.989892	45.554586
3501.441741	522240.287627	45.559591
3501.883287	522223.339263	45.564596
3501.521545	522217.852959	45.569601
3501.576986	522198.243747	45.574605
3501.742581	522188.694791	45.579610
3501.256253	522174.964368	45.584615
3501.458043	522171.557000	45.589620
3501.463013	522150.796668	45.594625
3501.510058	522144.490912	45.599629
3501.539779	522130.075492	45.604634
3501.225284	522132.190284	45.609639
3501.749608	522129.438138	45.614644
3501.501964	522113.906953	45.619649
3501.790826	522097.788389	45.624653
3501.817493	522080.753244	45.629658
3501.424206	522064.186527	45.634663
3501.304855	522044.251578	45.639668
3501.226392	522043.759884	45.644673
3501.579532	522039.573117	45.649677
3501.493190	522039.133036	45.654682
3501.460562	522013.289188	45.659687
3501.469320	522002.404036	45.664692
3501.646046	522000.260220	45.669697
3501.565509	521986.466458	45.674701
3501.605459	521970.789578	45.679706
3501.225843	521969.639314	45.684711
3501.914753	521957.086260	45.689716
3501.440652	521960.787942	45.694721
3501.782162	521937.102797	45.699725
3501.678735	521921.095455	45.704730
3501.552391	521924.743032	45.709735
3501.428636	521900.525567	45.714740
3501.291122	521889.864639	45.719745
3501.195265	521870.933541	45.724749
3501.392212	521871.104420	45.729754
3501.538938	521874.860682	45.734759
3501.747315	521853.917076	45.739764
3501.466112	521845.294006	45.744769
3501.817468	521834.204241	45.749773
3501.676773	521823.795698	45.754778
3501.551344	521809.907963	45.759783
3501.618096	521792.110387	45.764788
3501.531079	521799.127913	45.769793
3501.333829	521790.139024	45.774797
3501.588366	521767.626054	45.779802
3501.476641	521767.341080	45.784807
3501.831078	521734.382047	45.789812
3501.673354	521678.626038	45.794817
3501.549868	521564.866348	45.799821
3501.409270	521405.051945	45.804826
3501.235294	521208.153284	45.809831
3501.152333	520953.136055	45.814836
3501.011622	520659.169407	45.819841
3500.117016	520307.562138	45.824845
3499.800474	519902.789285	45.829850
3499.158654	519474.065913	45.834855
3498.660350	518990.422255	45.839860
3498.264782	518457.503744	45.844865
3497.359229	517878.272965	45.849869
3496.635821	517262.848659	45.854874
3495.516746	516605.468617	45.859879
3495.017586	515893.215004	45.864884
3493.754696	515150.039324	45.869889
3493.103742	514366.193973	45.874893
3492.310162	513536.041829	45.879898
3490.894942	512670.036229	45.884903
3490.036304	511731.832208	45.889908
3488.838374	510782.927040	45.894913
3487.733948	509780.535094	45.899917
3486.476081	508732.551688	45.904922
3485.084128	507656.113609	45.909927
3484.271537	506522.955851	45.914932
3482.732405	505359.652951	45.919937
3481.412708	504148.392343	45.924941
3479.809287	502912.198552	45.929946
3477.989012	501624.663972	45.934951
3476.522920	500307.588831	45.939956
3474.909069	498951.050655	45.944961
3473.275862	497549.517311	45.949965
3471.869673	496129.339528	45.954970
3469.541936	494662.621646	45.959975
3467.822566	493174.458753	45.964980
3465.933332	491640.476169	45.969985
3464.181991	490069.804050	45.974989
3462.375081	488470.745086	45.979994
3459.856635	486837.079557	45.984999
3458.287935	485183.087835	45.990004
3456.291027	483500.996521	45.995009
3453.896295	481775.432520	46.000013
3451.871002	480022.029819	46.005018
3449.279383	478251.640464	46.010023
3447.323744	476436.728339	46.015028
3445.378399	474603.916333	46.020033
3443.046740	472739.560864	46.025037
3440.535791	470833.508041	46.030042
3437.822823	468912.044118	46.035047
3435.310969	466966.151186	46.040052
3433.439145	464999.800697	46.045057
3431.026149	463009.023213	46.050061
3428.793822	460984.087302	46.055066
3426.038008	458942.144094	46.060071
3423.625688	456856.133399	46.065076
3420.837925	454766.692398	46.070081
3417.779494	452649.206410	46.075085
3415.452605	450516.521784	46.080090
3412.416745	448362.885638	46.085095
3410.247796	446170.072550	46.090100
3407.418914	443978.618610	46.095105
3404.554669	441757.738009	46.100109
3401.761312	439503.354272	46.105114
3398.529718	437257.026967	46.110119
3396.192284	434972.703058	46.115124
3393.145518	432683.152178	46.120129
3390.147896	430366.973332	46.125133
3387.263326	428027.140610	46.130138
3384.195590	425688.431014	46.135143
3381.192507	423299.050714	46.140148
3378.251263	420921.296490	46.145153
3375.330963	418527.091021	46.150157
3372.364213	416108.227305	46.155162
3368.985036	413674.748803	46.160167
3365.860831	411224.115596	46.165172
3362.473987	408767.972392	46.170177
3359.329903	406299.900614	46.175181
3356.423367	403806.759216	46.180186
3353.037453	401320.523753	46.185191
3350.050615	398805.233296	46.190196
3346.583453	396293.554333	46.195201
3343.095212	393745.775420	46.200205
3340.073402	391191.106135	46.205210
3336.625500	388634.510820	46.210215
3333.196663	386067.875515	46.215220
3329.890196	383492.048634	46.220225
3326.434067	380902.807837	46.225229
3322.957305	378290.533513	46.230234
3319.654223	375699.793649	46.235239
3316.259810	373078.364087	46.240244
3312.777794	370455.403479	46.245249
3309.273005	367823.283979	46.250253
3305.464765	365186.446935	46.255258
3301.979308	362544.848995	46.260263
3298.602644	359890.674187	46.265268
3295.099384	357233.669074	46.270273
3291.144303	354575.057399	46.275277
3287.888753	351904.979435	46.280282
3284.050971	349227.475185	46.285287
3280.826522	346541.776784	46.290292
3277.148833	343856.494363	46.295297
3273.317978	341165.814062	46.300301
3269.573169	338468.837634	46.305306
3265.931911	335770.626638	46.310311
3262.270722	333060.217753	46.315316
3258.308745	330372.197668	46.320321
3254.580451	327669.253385	46.325325
3251.219007	324964.695734	46.330330
3247.273317	322258.753617	46.335335
3243.634038	319547.476795	46.340340
3239.835031	316833.536934	46.345345
3236.345043	314115.974963	46.350349
3232.536278	311401.101762	46.355354
3228.313812	308679.318284	46.360359
3224.640653	305950.707507	46.365364
3221.090497	303235.903571	46.370369
3217.293635	300512.115523	46.375373
3213.514011	297784.574639	46.380378
3209.551978	295071.057938	46.385383
3205.581908	292348.609989	46.390388
3201.512190	289639.319457	46.395393
3197.699254	286920.149426	46.400397
3193.813559	284222.188709	46.405402
3189.835998	281516.602134	46.410407
3186.147484	278794.041407	46.415412
3181.982910	276110.261379	46.420417
3177.919035	273409.979392	46.425421
3174.356965	270712.182411	46.430426
3170.170888	268022.550793	46.435431
3166.240178	265328.399310	46.440436
3161.869261	262649.346693	46.445441
3158.051034	259958.887559	46.450445
3153.943273	257300.907488	46.455450
3150.315177	254639.920536	46.460455
3146.196905	251960.801904	46.465460
3141.827244	249313.688823	46.470465
3137.445618	246660.323092	46.475469
3133.690644	244016.374344	46.480474
3129.420225	241400.591587	46.485479
3125.256492	238777.176405	46.490484
3121.217958	236168.287920	46.495489
3117.303937	233565.704462	46.500493
3112.964483	230972.419493	46.505498
3108.709279	228379.800479	46.510503
3104.637866	225796.801308	46.515508
3100.747685	223240.694633	46.520513
3096.162217	220673.977708	46.525517
3092.459482	218132.575001	46.530522
3087.908114	215597.454342	46.535527
3084.135307	213052.193853	46.540532
3079.700145	210539.375874	46.545537
3075.170650	208040.578034	46.550541
3071.421575	205543.468523	46.555546
3066.825713	203066.564481	46.560551
3062.462782	200585.354274	46.565556
3058.104461	198132.627525	46.570561
3053.712060	195694.386070	46.575565
3049.518221	193263.084100	46.580570
3045.119676	190863.794406	46.585575
3040.917244	188465.007135	46.590580
3036.357397	186080.842531	46.595585
3031.885696	183724.296408	46.600589
3027.471235	181373.629478	46.605594
3022.704653	179047.953971	46.610599
3018.729851	176746.036369	46.615604
3013.581142	174461.334646	46.620609
3008.387722	172197.684547	46.625613
3004.027623	169957.267253	46.630618
2999.186578	167749.020242	46.635623
2994.624311	165550.740339	46.640628
2989.552654	163391.127283	46.645633
2983.899689	161255.782828	46.650637
2979.052479	159158.606053	46.655642
2974.049436	157088.099617	46.660647
2968.726822	155018.618588	46.665652
2962.792981	152972.506883	46.670657
2956.884907	151024.900096	46.675661
2951.909276	149129.748047	46.680666
2945.236583	147279.757473	46.685671
2938.716650	145471.774328	46.690676
2931.898980	143742.320166	46.695681
2924.715464	142085.049680	46.700685
2917.129516	140483.638524	46.705690
2910.176115	138956.890800	46.710695
2903.128720	137489.112008	46.715700
2896.268147	136090.812931	46.720705
2889.813800	134749.181222	46.725709
2883.630359	133471.331948	46.730714
2877.612908	132274.029914	46.735719
2872.109493	131115.796548	46.740724
2866.781929	130011.322740	46.745729
2861.235041	128947.653664	46.750733
2856.337479	127931.380050	46.755738
2851.101473	126947.236592	46.760743
2846.579792	126012.520647	46.765748
2841.913661	125110.497603	46.770753
2837.289096	124242.929829	46.775757
2833.146303	123396.011086	46.780762
2828.695272	122581.652688	46.785767
2824.700481	121782.450450	46.790772
2820.788679	121013.010408	46.795777
2816.596953	120249.936882	46.800781
2812.474219	119515.073890	46.805786
2808.480463	118804.900768	46.810791
2804.643491	118111.591263	46.815796
2801.154476	117412.581589	46.820801
2797.096789	116749.939488	46.825805
2793.484019	116074.511400	46.830810
2789.383881	115434.533432	46.835815
2785.800344	114788.713407	46.840820
2781.753857	114166.906667	46.845825
2777.518479	113558.083711	46.850829
2773.815863	112949.277073	46.855834
2769.703088	112360.633440	46.860839
2765.944542	111775.364484	46.865844
2762.243817	111218.842676	46.870849
2758.238967	110663.355886	46.875853
2754.719802	110098.521252	46.880858
2750.794936	109558.893391	46.885863
2747.609580	109034.834266	46.890868
2743.642160	108502.412369	46.895873
2739.687621	107977.408272	46.900877
2736.609208	107451.830871	46.905882
2732.739177	106924.910042	46.910887
2729.628971	106419.706162	46.915892
2726.175758	105914.296196	46.920897
2722.355021	105399.544103	46.925901
2719.490719	104889.367078	46.930906
2715.781000	104384.795329	46.935911
2712.307255	103880.995277	46.940916
2708.839512	103357.499560	46.945921
2705.504402	102857.265270	46.950925
2702.737827	102348.471967	46.955930
2699.157931	101846.371759	46.960935
2695.848139	101329.721922	46.965940
2692.380432	100819.790396	46.970945
2689.220594	100311.827132	46.975949
2685.738794	99788.632044	46.980954
2682.378329	99273.916565	46.985959
2679.274535	98746.269358	46.990964
2675.701559	98232.086631	46.995969
2672.148696	97713.422801	47.000973
2669.107663	97181.318177	47.005978
2665.642576	96656.710293	47.010983
2662.181774	96115.843817	47.015988
2658.913705	95589.138937	47.020993
2655.122404	95066.857765	47.025997
2652.381369	94522.386795	47.031002
2648.561466	94007.206094	47.036007
2645.036553	93460.588476	47.041012
2641.879528	92918.205602	47.046017
2638.291040	92381.757323	47.051021
2635.103575	91837.962513	47.056026
2631.608032	91295.635798	47.061031
2628.192411	90745.555653	47.066036
2624.910127	90200.712342	47.071041
2621.098430	89654.601822	47.076045
2617.972310	89088.561458	47.081050
2614.337600	88544.756134	47.086055
2610.867887	87993.223226	47.091060
2607.599388	87437.921437	47.096065
2604.014498	86881.701144	47.101069
2600.530728	86321.334122	47.106074
2597.151422	85770.959651	47.111079
2593.933470	85205.338742	47.116084
2590.581094	84647.359209	47.121089
2586.659513	84076.725033	47.126093
2583.007144	83514.761867	47.131098
2579.773442	82953.354343	47.136103
2576.866826	82392.453210	47.141108
2573.180323	81818.410730	47.146113
2569.152361	81240.774911	47.151117
2566.163024	80676.376933	47.156122
2562.565585	80110.395681	47.161127
2559.076753	79535.670607	47.166132
2555.629059	78972.546975	47.171137
2552.202883	78391.688638	47.176141
2548.754399	77815.646772	47.181146
2544.975157	77234.639227	47.186151
2541.237376	76658.527033	47.191156
2537.958183	76080.209439	47.196161
2534.516162	75498.716596	47.201165
2531.178964	74922.083695	47.206170
2527.410519	74344.933425	47.211175
2524.223106	73764.505148	47.216180
2520.880700	73191.719846	47.221185
2517.286187	72605.158056	47.226189
2513.814229	72016.622048	47.231194
2510.363866	71444.907138	47.236199
2507.407353	70856.710457	47.241204
2503.593463	70274.659660	47.246209
2500.364468	69680.602442	47.251213
2496.862767	69085.376058	47.256218
2493.205606	68496.186389	47.261223
2489.796663	67903.150166	47.266228
2486.503978	67308.973307	47.271233
2482.788472	66721.045848	47.276237
2479.161155	66118.716009	47.281242
2476.086940	65525.295718	47.286247
2472.691332	64917.506091	47.291252
2468.943760	64318.785843	47.296257
2465.326108	63711.123391	47.301261
2461.864893	63107.843221	47.306266
2458.166212	62520.664842	47.311271
2455.162098	61917.025097	47.316276
2451.625266	61321.783770	47.321281
2448.382378	60709.643377	47.326285
2444.925276	60088.807002	47.331290
2441.379843	59488.173082	47.336295
2437.782543	58876.901541	47.341300
2434.179934	58268.146297	47.346305
2430.793588	57658.148094	47.351309
2427.347657	57052.939739	47.356314
2423.960730	56446.525583	47.361319
2420.226630	55830.225944	47.366324
2417.318302	55206.733197	47.371329
2413.766008	54593.140097	47.376333
2410.131376	53963.512126	47.381338
2406.465333	53349.144304	47.386343
2402.985941	52724.613270	47.391348
2399.414369	52107.636912	47.396353
2396.032197	51497.961535	47.401357
2392.840323	50872.959587	47.406362
2388.998991	50263.381782	47.411367
2385.361108	49631.270586	47.416372
2382.369671	49000.814122	47.421377
2378.805077	48378.500415	47.426381
2375.376692	47758.389687	47.431386
2371.752817	47136.537750	47.436391
2368.409911	46502.266533	47.441396
2365.110869	45861.042793	47.446401
2361.292178	45242.038480	47.451405
2357.534301	44604.758832	47.456410
2353.955206	43978.173943	47.461415
2351.032139	43346.437913	47.466420
2347.751321	42717.965127	47.471425
2343.876230	42079.824991	47.476429
2340.834151	41441.928795	47.481434
2337.098898	40814.443400	47.486439
2333.252051	40176.195723	47.491444
2330.013364	39540.845647	47.496449
2326.671492	38905.631657	47.501453
2323.326314	38255.043760	47.506458
2319.814699	37620.572337	47.511463
2316.113474	36986.155497	47.516468
2312.716064	36337.694096	47.521473
2308.828444	35700.536138	47.526477
2305.840751	35055.200523	47.531482
2302.008717	34424.201907	47.536487
2298.659955	33773.472286	47.541492
2295.235121	33138.911896	47.546497
2291.390469	32491.988019	47.551501
2287.975801	31847.343255	47.556506
2284.415789	31212.228595	47.561511
2281.116038	30565.121307	47.566516
2277.748669	29921.188079	47.571521
2273.968715	29282.567280	47.576525
2270.827351	28635.014273	47.581530
2266.905913	27996.221062	47.586535
2263.218961	27344.098329	47.591540
2259.953810	26697.050589	47.596545
2255.898643	26063.141797	47.601549
2252.559136	25416.000830	47.606554
2249.243320	24779.673003	47.611559
2245.730748	24143.516329	47.616564
2242.480109	23507.085693	47.621569
2238.865362	22865.385190	47.626573
2235.835767	22215.664028	47.631578
2231.746613	21575.415704	47.636583
2228.113129	20939.557688	47.641588
2224.681727	20293.971962	47.646593
2221.077768	19662.609969	47.651597
2217.268135	19028.101746	47.656602
2213.579983	18388.217974	47.661607
2209.975007	17761.066220	47.666612
2206.478946	17124.620589	47.671617
2202.631896	16493.643122	47.676621
2199.066471	15871.008167	47.681626
2195.063737	15256.260088	47.686631
2191.145852	14633.574507	47.691636
2187.838322	14034.509436	47.696641
2183.558859	13430.482364	47.701645
2179.337663	12846.575347	47.706650
2174.712086	12282.807924	47.711655
2170.643948	11714.161855	47.716660
2166.608307	11157.801068	47.721665
2161.740811	10618.930237	47.726669
2157.936542	10077.962702	47.731674
2153.973179	9574.238108	47.736679
2150.011115	9075.445782	47.741684
2145.971191	8584.848338	47.746689
2142.063941	8096.737342	47.751693
2138.056747	7613.782133	47.756698
2134.122703	7157.065627	47.761703
2130.282995	6687.673616	47.766708
2126.977628	6238.927178	47.771713
2122.489997	5793.334731	47.776717
2119.381966	5362.893281	47.781722
2115.403416	4927.113259	47.786727
2111.423852	4498.293049	47.791732
2108.174318	4078.416417	47.796737
2104.120005	3672.088422	47.801741
2100.840664	3262.282145	47.806746
2097.237441	2867.296593	47.811751
2093.197344	2472.836988	47.816756
2089.477625	2079.915038	47.821761
2085.250415	1712.756555	47.826765
2081.261695	1351.567307	47.831770
2075.821344	1024.126268	47.836775
2070.022976	722.459397	47.841780
2064.756417	458.904877	47.846785
2058.959568	233.199211	47.851789
2050.550413	101.137597	47.856794
2038.788409	114.601131	47.861799
2031.102085	116.740140	47.866804
2026.395295	115.609212	47.871809
2024.199682	130.301549	47.876813
2022.428968	119.820440	47.881818
2021.075481	112.045824	47.886823
2018.845469	120.330642	47.891828
2016.718451	113.989358	47.896833
2013.593361	114.099217	47.901837
2010.763599	104.931373	47.906842
2007.668602	101.730461	47.911847
2004.253518	107.750991	47.916852
2000.981680	106.551763	47.921857
1997.881221	114.130499	47.926861
1994.083137	106.575000	47.931866
1991.115419	110.276501	47.936871
1987.765621	112.635938	47.941876
1984.577654	107.794870	47.946881
1981.001912	119.962209	47.951885
1977.832420	118.190238	47.956890
1974.475730	113.982863	47.961895
1970.798498	113.533258	47.966900
1968.158225	110.812064	47.971905
1964.443436	106.075137	47.976909
1961.094665	110.690148	47.981914
1957.673183	110.248196	47.986919
1954.136628	106.401010	47.991924
1951.173437	100.879566	47.996929
1947.651605	122.324030	48.001933
1943.216655	106.531252	48.006938
1940.144735	101.567728	48.011943
1936.937864	109.590126	48.016948
1933.820730	109.138773	48.021953
1930.308017	109.463988	48.026957
1927.084302	110.804070	48.031962
1923.661910	109.397329	48.036967
1920.171564	113.354177	48.041972
1916.646625	112.630940	48.046977
1912.895734	113.999288	48.051981
1909.931150	100.315671	48.056986
1906.315054	111.802756	48.061991
1902.731008	117.283283	48.066996
1899.294410	111.341980	48.072001
1896.165960	118.637177	48.077005
1892.465531	106.763836	48.082010
1888.847751	108.810650	48.087015
1885.633627	112.142385	48.092020
1882.131866	104.724282	48.097025
1878.607391	110.410669	48.102029
1874.995579	109.220072	48.107034
1871.797896	109.939181	48.112039
1868.483870	104.684318	48.117044
1865.189735	113.818109	48.122049
1861.274068	114.408521	48.127053
1857.787941	102.922612	48.132058
1854.122702	107.665973	48.137063
1850.699312	104.152359	48.142068
1847.376853	113.837881	48.147073
1844.004249	117.096209	48.152077
1840.871679	105.738770	48.157082
1836.989718	103.400665	48.162087
1833.584018	105.721355	48.167092
1830.175301	103.809464	48.172097
1826.468690	118.316170	48.177101
1822.873300	112.462866	48.182106
1819.578254	103.664856	48.187111
1816.319013	112.875472	48.192116
1812.735040	102.265331	48.197121
1808.865121	113.646390	48.202125
1805.844171	109.279215	48.207130
1802.719770	107.810288	48.212135
1798.516206	112.757658	48.217140
1795.395524	110.123905	48.222145
1791.876196	106.710649	48.227149
1788.430469	106.247176	48.232154
1785.097256	105.696589	48.237159
1781.324644	105.075188	48.242164
1777.774904	102.432286	48.247169
1774.167259	104.180141	48.252173
1770.773902	95.970076	48.257178
1767.453105	86.283925	48.262183
1764.038210	101.052093	48.267188
1760.206666	107.089991	48.272193
1756.645103	105.470812	48.277197
1753.836334	97.584210	48.282202
1750.389996	101.331737	48.287207
1746.345092	100.581878	48.292212
1743.289094	103.718168	48.297217
1739.282751	102.633281	48.302221
1736.235296	104.452137	48.307226
1732.581711	107.880750	48.312231
1728.597174	111.576006	48.317236
1725.300561	101.984163	48.322241
1721.908652	98.095511	48.327245
1718.473041	98.734606	48.332250
1715.293612	101.026414	48.337255
1711.591297	105.405398	48.342260
1708.262175	106.050065	48.347265
1704.514323	104.510505	48.352269
1701.161015	94.111257	48.357274
1697.563083	99.834391	48.362279
1693.869408	111.766976	48.367284
1691.146992	104.876165	48.372289
1687.405061	113.718989	48.377293
1683.720451	110.907265	48.382298
1680.254034	103.119865	48.387303
1676.699943	105.286493	48.392308
1672.920204	102.976790	48.397313
1669.586863	101.201878	48.402317
1665.878203	106.505657	48.407322
1662.651717	101.249851	48.412327
1659.109857	100.731750	48.417332
1655.801756	93.425911	48.422337
1651.824362	107.819726	48.427341
1648.983946	99.960210	48.432346
1645.313198	100.604271	48.437351
1641.654735	97.548043	48.442356
1638.226366	89.818008	48.447361
1634.733694	98.043072	48.452365
1631.162527	98.769710	48.457370
1627.540143	103.117276	48.462375
1623.883416	98.513726	48.467380
1620.789071	94.249748	48.472385
1617.392847	95.069379	48.477389
1613.918068	89.811100	48.482394
1610.064502	90.138774	48.487399
1606.805365	94.904358	48.492404
1603.493109	103.199420	48.497409
1599.562996	97.179954	48.502413
1596.208057	95.607726	48.507418
1592.853702	94.272685	48.512423
1588.891705	99.726625	48.517428
1585.912496	93.875532	48.522433
1582.446778	105.247458	48.527437
1579.021427	105.973551	48.532442
1575.212698	96.107110	48.537447
1571.803883	97.691158	48.542452
1568.405297	91.456095	48.547457
1564.305168	96.400033	48.552461
1560.982913	89.776610	48.557466
1557.612461	87.662644	48.562471
1554.580040	96.717729	48.567476
1551.041097	86.727051	48.572481
1546.952872	96.193235	48.577485
1543.703536	93.282147	48.582490
1540.386671	93.817354	48.587495
1536.817032	108.138212	48.592500
1533.857645	95.671890	48.597505
1529.565832	98.440563	48.602509
1526.166863	90.047919	48.607514
1523.002969	95.247929	48.612519
1519.403977	106.264118	48.617524
1516.128887	94.846670	48.622529
1512.126507	96.792023	48.627533
1508.818220	99.755624	48.632538
1505.256042	91.609844	48.637543
1501.617248	99.085711	48.642548
1498.141939	97.497427	48.647553
1494.569487	97.319458	48.652557
1491.425793	91.585727	48.657562
1488.144649	97.487349	48.662567
1484.342096	100.651266	48.667572
1480.941041	95.337237	48.672577
1477.335779	104.820004	48.677581
1474.045080	96.176400	48.682586
1470.446204	99.606005	48.687591
1466.919009	98.804071	48.692596
1463.193353	95.302751	48.697601
1459.277215	104.678884	48.702605
1456.053741	94.256309	48.707610
1452.914039	92.077965	48.712615
1449.141637	92.361385	48.717620
1445.971353	88.969776	48.722625
1442.412428	101.106004	48.727629
1438.581600	102.948734	48.732634
1435.237745	93.952748	48.737639
1431.532735	106.421760	48.742644
1428.408246	98.739367	48.747649
1424.887338	96.307153	48.752653
1421.258557	90.487586	48.757658
1417.996930	99.303107	48.762663
1414.212300	99.863676	48.767668
1410.928507	103.171479	48.772673
1407.270855	102.073486	48.777677
1403.755161	96.413486	48.782682
1400.534476	92.950634	48.787687
1396.765513	100.797937	48.792692
1393.067136	95.780130	48.797697
1389.357842	97.195831	48.802701
1385.989607	88.080267	48.807706
1383.013588	80.441219	48.812711
1379.405566	96.296104	48.817716
1375.985734	84.122948	48.822721
1371.824910	96.020669	48.827725
1368.485044	92.880087	48.832730
1365.773919	81.077508	48.837735
1361.918589	101.137482	48.842740
1358.787957	91.472419	48.847745
1354.901414	87.929720	48.852749
1351.156622	97.870794	48.857754
1347.619198	90.141962	48.862759
1343.877730	91.543692	48.867764
1340.982357	84.331850	48.872769
1337.700972	90.353734	48.877773
1333.767054	92.196701	48.882778
1330.303225	80.675801	48.887783
1326.057633	91.409817	48.892788
1322.901995	92.309084	48.897793
1319.445638	95.548840	48.902797
1316.436031	98.358398	48.907802
1313.391031	93.102867	48.912807
1309.380154	94.511734	48.917812
1305.901215	89.453460	48.922817
1302.140462	96.018189	48.927821
1298.541722	91.415153	48.932826
1295.292491	97.466837	48.937831
1291.865505	84.307738	48.942836
1288.434975	82.234792	48.947841
1284.775565	88.179479	48.952845
1281.091227	94.080593	48.957850
1277.350480	91.306135	48.962855
1273.765272	94.588097	48.967860
1270.669787	93.247597	48.972865
1267.488970	94.036895	48.977869
1264.122221	92.447559	48.982874
1260.833151	91.728805	48.987879
1256.552458	93.616265	48.992884
1252.893216	89.158692	48.997889
1249.705268	86.652529	49.002893
1245.831792	91.754196	49.007898
1243.012658	90.525706	49.012903
1239.222393	98.066288	49.017908
1235.580901	89.347618	49.022913
1231.944107	90.337604	49.027917
1228.683652	89.484688	49.032922
1225.243404	90.437754	49.037927
1221.870510	94.778148	49.042932
1218.487531	87.923789	49.047937
1214.728221	94.399714	49.052941
1211.232026	93.896699	49.057946
1207.834006	92.903848	49.062951
1204.040722	99.169933	49.067956
1200.715798	86.308172	49.072961
1197.182629	89.961682	49.077965
1193.494538	91.022931	49.082970
1190.545811	88.318190	49.087975
1186.558176	90.767472	49.092980
1183.201481	85.117560	49.097985
1179.589468	94.465341	49.102989
1176.316738	84.926834	49.107994
1172.838345	85.923808	49.112999
1168.775757	95.430307	49.118004
1165.520428	88.511795	49.123009
1162.032128	86.846481	49.128013
1158.686047	87.076229	49.133018
1155.522968	78.741848	49.138023
1151.581455	86.875437	49.143028
1148.236480	86.532385	49.148033
1144.644701	89.413590	49.153037
1141.138699	91.977729	49.158042
1137.575542	83.984028	49.163047
1134.115698	86.278395	49.168052
1130.907965	88.289917	49.173057
1127.226889	90.663013	49.178061
1123.634311	92.009953	49.183066
1120.555833	91.403964	49.188071
1116.305434	96.804752	49.193076
1113.362987	88.100679	49.198081
1109.816392	91.487372	49.203085
1106.239016	82.008955	49.208090
1102.328693	76.654039	49.213095
1098.454539	84.862565	49.218100
1095.442439	74.647608	49.223105
1092.019031	92.985715	49.228109
1088.593628	97.331128	49.233114
1085.068590	87.774964	49.238119
1081.494345	85.408043	49.243124
1077.943612	84.834441	49.248129
1074.465070	87.789772	49.253133
1070.958992	87.338931	49.258138
1067.970389	88.686774	49.263143
1064.200186	95.392190	49.268148
1060.704603	87.666387	49.273153
1057.057461	85.045067	49.278157
1053.031120	87.022670	49.283162
1049.779063	81.172999	49.288167
1046.489794	89.537255	49.293172
1043.220962	92.893372	49.298177
1039.909110	86.758785	49.303181
1036.083081	88.993105	49.308186
1032.701450	87.820558	49.313191
1028.974329	93.680891	49.318196
1025.559547	93.573341	49.323201
1021.630682	91.388175	49.328205
1018.319769	89.255514	49.333210
1015.206167	97.934109	49.338215
1011.669483	99.595057	49.343220
1008.600970	90.663856	49.348225
1004.828363	89.754647	49.353229
1000.851781	99.826723	49.358234
997.339731	90.195788	49.363239
993.618098	91.559667	49.368244
990.768366	86.637612	49.373249
986.994773	92.679185	49.378253
983.387325	88.280030	49.383258
980.245112	85.924965	49.388263
976.118805	94.960511	49.393268
973.124097	92.816598	49.398273
969.751944	89.016720	49.403277
965.591113	92.600276	49.408282
962.659384	92.708600	49.413287
959.154482	88.204902	49.418292
955.702792	86.777520	49.423297
952.269384	91.102041	49.428301
948.783777	85.402632	49.433306
944.706856	85.230485	49.438311
941.104572	90.539892	49.443316
937.966075	83.799383	49.448321
934.738478	73.228868	49.453325
931.108630	77.621931	49.458330
927.607932	74.427354	49.463335
923.490464	83.879128	49.468340
920.645748	90.725220	49.473345
916.762903	89.725617	49.478349
913.207749	89.605130	49.483354
909.789702	80.592323	49.488359
906.436603	100.656348	49.493364
903.246625	83.455213	49.498369
899.508827	93.518594	49.503373
896.109808	86.090996	49.508378
892.654560	88.356198	49.513383
888.728562	84.781748	49.518388
885.381859	81.996629	49.523393
881.463018	88.070310	49.528397
878.082718	92.889597	49.533402
875.129101	90.264746	49.538407
871.523263	95.286818	49.543412
868.136223	91.539890	49.548417
864.621876	89.869178	49.553421
860.780025	84.810520	49.558426
857.238708	84.399990	49.563431
853.805427	93.998364	49.568436
850.511383	88.205877	49.573441
847.175047	82.321902	49.578445
843.331970	88.564122	49.583450
839.693863	89.120930	49.588455
836.461635	95.293374	49.593460
833.103015	80.222364	49.598465
829.009919	85.269666	49.603469
825.948481	91.029554	49.608474
822.106514	85.540660	49.613479
818.818032	86.884586	49.618484
815.795826	87.215811	49.623489
811.962277	88.948301	49.628493
808.430187	84.727265	49.633498
804.947541	88.021773	49.638503
801.142868	88.788009	49.643508
797.902512	86.217296	49.648513
794.407557	87.824315	49.653517
790.872981	94.790456	49.658522
787.164856	80.688168	49.663527
783.763472	87.845541	49.668532
780.268794	80.360092	49.673537
776.953752	86.728922	49.678541
773.100289	82.890106	49.683546
769.911427	82.788545	49.688551
766.718065	77.590994	49.693556
763.157963	83.248179	49.698561
759.550782	86.397566	49.703565
755.727981	83.427156	49.708570
752.528419	78.825344	49.713575
748.678468	85.043331	49.718580
745.282901	76.935035	49.723585
741.705830	81.595139	49.728589
737.992459	83.049507	49.733594
735.037794	77.643964	49.738599
730.900630	89.047646	49.743604
727.826202	83.587980	49.748609
724.215612	81.935433	49.753613
720.455247	86.633565	49.758618
717.311568	77.638197	49.763623
713.531145	75.619794	49.768628
710.122816	77.036170	49.773633
706.643544	82.187242	49.778637
703.124406	83.329810	49.783642
699.965173	78.038373	49.788647
696.464304	73.844134	49.793652
692.676898	77.341114	49.798657
689.394885	69.167701	49.803661
685.703029	78.787344	49.808666
682.372638	60.956429	49.813671
678.870787	72.033418	49.818676
675.516147	76.054639	49.823681
671.630782	74.172798	49.828685
668.145466	70.188111	49.833690
664.825691	74.071030	49.838695
660.970203	74.339005	49.843700
657.893913	67.465482	49.848705
654.257661	75.399720	49.853709
650.390693	78.618032	49.858714
647.246374	77.642703	49.863719
643.853963	70.571625	49.868724
640.354104	73.650533	49.873729
636.872790	74.157649	49.878733
632.989472	73.569441	49.883738
629.830627	64.152524	49.888743
626.027578	80.635675	49.893748
622.653345	70.176636	49.898753
619.158479	80.787485	49.903757
615.929361	76.304188	49.908762
612.374815	73.896306	49.913767
608.377785	77.308872	49.918772
604.706545	67.845177	49.923777
601.607219	73.977957	49.928781
598.554318	78.483710	49.933786
595.097777	66.809986	49.938791
591.269897	78.842547	49.943796
587.739564	74.887025	49.948801
584.240490	76.880676	49.953805
580.662175	79.313760	49.958810
577.329081	70.006232	49.963815
573.445463	75.584082	49.968820
570.250275	67.055500	49.973825
566.757017	73.293898	49.978829
562.841466	75.681409	49.983834
559.655089	72.222826	49.988839
555.961098	71.829776	49.993844
552.235885	67.195937	49.998849
549.377024	68.254716	50.003853
545.689286	63.260714	50.008858
542.345189	66.188836	50.013863
538.616019	75.355560	50.018868
534.881277	80.122484	50.023873
531.156632	66.987766	50.028877
527.860508	77.156399	50.033882
524.761554	66.913950	50.038887
521.415109	76.751904	50.043892
517.957092	65.584616	50.048897
514.448266	66.788874	50.053901
510.376471	67.523968	50.058906
506.842901	69.295213	50.063911
502.987266	79.468695	50.068916
500.219598	72.926793	50.073921
496.512616	67.882011	50.078925
493.000068	66.771044	50.083930
489.875833	66.735383	50.088935
486.594053	73.440726	50.093940
482.714557	72.203392	50.098945
478.640578	69.389190	50.103949
475.449096	67.915038	50.108954
472.309338	66.837784	50.113959
468.116029	77.813627	50.118964
464.849610	73.424744	50.123969
461.603411	72.300789	50.128973
458.131021	75.881627	50.133978
454.832958	72.832743	50.138983
451.037762	79.494635	50.143988
447.487420	72.919567	50.148993
444.005772	65.236014	50.153997
439.966370	70.895074	50.159002
437.129994	65.898262	50.164007
433.773518	71.723081	50.169012
429.960484	68.064692	50.174017
426.385491	80.633679	50.179021
422.662884	74.847878	50.184026
419.794932	77.031190	50.189031
416.177179	68.562094	50.194036
412.632100	70.547108	50.199041
409.075601	64.795563	50.204045
405.493913	64.679273	50.209050
401.908097	66.724413	50.214055
398.063330	70.233517	50.219060
394.558919	65.179365	50.224065
391.401676	67.958193	50.229069
387.803796	60.941301	50.234074
384.570561	65.427687	50.239079
380.798222	76.328506	50.244084
377.432127	71.550206	50.249089
374.127744	76.563349	50.254093
370.350986	74.591885	50.259098
367.319353	68.859873	50.264103
363.399762	69.466892	50.269108
359.871027	73.091312	50.274113
356.525145	74.545462	50.279117
352.891478	76.636021	50.284122
349.953444	62.407645	50.289127
345.879538	80.426215	50.294132
342.146643	78.751638	50.299137
338.840099	77.045488	50.304141
335.269682	84.434842	50.309146
331.902237	76.417160	50.314151
328.570293	73.917721	50.319156
324.922998	72.758154	50.324161
321.455608	74.623520	50.329165
317.607967	86.190951	50.334170
314.634723	74.986196	50.339175
310.684702	85.348390	50.344180
307.571953	71.166199	50.349185
304.414491	78.912030	50.354189
300.379333	83.137306	50.359194
296.874302	75.324545	50.364199
293.187674	74.620347	50.369204
289.616391	79.833234	50.374209
286.466215	74.018452	50.379213
282.849931	70.563569	50.384218
279.050445	75.530417	50.389223
275.693844	86.822092	50.394228
272.253720	76.889062	50.399233
268.917926	71.688460	50.404237
265.360648	69.736627	50.409242
262.367477	66.301794	50.414247
258.482809	76.590538	50.419252
254.853931	78.123559	50.424257
251.322387	73.918354	50.429261
247.743597	77.876438	50.434266
244.167985	69.173034	50.439271
240.672445	75.297923	50.444276
237.250765	76.700614	50.449281
234.072151	74.329174	50.454285
230.088315	72.785431	50.459290
227.027873	59.971321	50.464295
223.453501	68.215482	50.469300
219.986363	70.191549	50.474305
216.285702	78.591415	50.479309
212.219853	73.213426	50.484314
209.387804	73.913735	50.489319
205.826217	70.962863	50.494324
202.185739	76.860392	50.499329
198.691035	68.669570	50.504333
194.854056	73.629610	50.509338
191.999868	70.002311	50.514343
188.261724	73.795391	50.519348
184.873245	60.829887	50.524353
181.142142	66.472612	50.529357
177.866701	75.805995	50.534362
174.478911	66.545034	50.539367
170.625905	76.211940	50.544372
167.331760	78.917197	50.549377
163.887149	73.872756	50.554381
159.958994	74.718414	50.559386
157.194697	70.317846	50.564391
152.927587	73.462478	50.569396
149.845398	81.282019	50.574401
146.205149	69.311143	50.579405
142.279457	80.530075	50.584410
138.995914	82.078946	50.589415
135.665184	78.199990	50.594420
132.608750	68.292679	50.599425
129.171111	69.625105	50.604429
125.277097	76.707360	50.609434
121.856812	72.320346	50.614439
117.727645	77.487233	50.619444
114.455701	69.536986	50.624449
111.333747	65.498986	50.629453
107.458859	72.780738	50.634458
104.399675	71.409423	50.639463
100.682554	75.129639	50.644468
96.982257	74.070107	50.649473
93.636595	74.496065	50.654477
90.322216	72.705752	50.659482
86.954320	74.745477	50.664487
83.229446	72.778638	50.669492
79.441120	74.611746	50.674497
76.463993	75.704807	50.679501
72.765245	82.978124	50.684506
68.804721	73.607043	50.689511
65.338088	72.827502	50.694516
62.233301	67.768137	50.699521
58.708721	71.028123	50.704525
55.112424	68.041555	50.709530
51.595724	70.376526	50.714535
48.122005	74.530238	50.719540
44.476246	78.710737	50.724545
40.964388	69.393193	50.729549
37.616671	78.231652	50.734554
33.975960	71.642264	50.739559
30.767753	75.140889	50.744564
26.932145	68.170574	50.749569
23.720442	73.324337	50.754573
19.914997	74.878554	50.759578
16.682066	68.725540	50.764583
13.205605	75.125881	50.769588
9.471403	78.813969	50.774593
6.096752	68.478518	50.779597
2.580717	80.702993	50.784602