Fri Aug 26 14:32:03 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.180565	106.156467	0.000000
0.914253	96.874575	0.005005
0.806130	91.528964	0.010010
0.800934	87.730177	0.015014
0.782258	97.606839	0.020019
0.729823	86.943932	0.025024
0.479447	77.286257	0.030029
0.205079	76.405149	0.035034
-0.232672	56.051856	0.040038
-0.531423	52.517075	0.045043
-1.393997	41.720911	0.050048
-1.298085	40.962482	0.055053
-1.471262	38.673613	0.060058
-1.550698	38.306306	0.065062
-2.127511	24.624700	0.070067
-2.218190	19.105558	0.075072
-2.139128	28.476598	0.080077
-2.963779	24.122062	0.085082
-3.016584	18.271167	0.090086
-3.390127	22.707781	0.095091
-3.431581	15.153075	0.100096
-3.937195	9.919995	0.105101
-4.662568	4.135857	0.110106
-4.649502	4.734879	0.115110
-4.773486	1.337407	0.120115
-4.565387	-2.048495	0.125120
-4.938641	8.243979	0.130125
-5.419492	7.910698	0.135130
-5.385398	9.733941	0.140134
-6.368245	6.210771	0.145139
-6.960482	12.481547	0.150144
-6.492619	6.758390	0.155149
-6.856490	8.362030	0.160154
-6.708472	0.227357	0.165158
-7.497758	11.524210	0.170163
-7.355116	6.639438	0.175168
-7.237261	4.197697	0.180173
-8.065899	10.002259	0.185178
-8.143990	4.807017	0.190182
-8.756509	9.018252	0.195187
-8.724484	-3.021283	0.200192
-9.406050	0.457244	0.205197
-10.149551	-0.524817	0.210202
-9.422003	-4.586361	0.215206
-10.185283	13.422864	0.220211
-10.060038	5.623917	0.225216
-10.031453	2.607638	0.230221
-9.864655	2.970759	0.235226
-10.502155	4.234201	0.240230
-11.422833	3.257579	0.245235
-11.566147	7.892453	0.250240
-11.609506	11.005869	0.255245
-11.598087	4.828614	0.260250
-11.573492	0.152042	0.265254
-12.338047	8.088414	0.270259
-12.591705	-1.182741	0.275264
-12.853969	-3.312205	0.280269
-13.352497	-4.886046	0.285274
-13.292881	2.877712	0.290278
-13.625683	3.856440	0.295283
-14.279402	3.948694	0.300288
-14.462193	4.843956	0.305293
-14.696727	13.890503	0.310298
-14.644517	3.901029	0.315302
-14.808085	7.912654	0.320307
-14.745019	7.061267	0.325312
-14.807461	-2.217513	0.330317
-15.250219	3.580748	0.335322
-15.528707	-5.082282	0.340326
-16.231883	2.028311	0.345331
-16.107679	-0.484017	0.350336
-16.770783	2.112142	0.355341
-17.489345	11.297322	0.360346
-17.234479	3.686995	0.365350
-17.613381	2.828495	0.370355
-17.505490	2.947696	0.375360
-17.145858	7.327098	0.380365
-17.786956	0.409910	0.385370
-18.348109	-6.143249	0.390374
-19.028514	9.005788	0.395379
-18.965561	4.307424	0.400384
-18.846446	0.400720	0.405389
-18.907444	4.731721	0.410394
-19.006312	0.609028	0.415398
-20.096352	14.730390	0.420403
-20.417495	3.767698	0.425408
-20.150377	5.067457	0.430413
-20.357022	4.837011	0.435418
-20.813216	-0.599905	0.440422
-21.323107	7.097506	0.445427
-21.504763	10.235618	0.450432
-21.767633	4.202306	0.455437
-22.077509	12.058397	0.460442
-21.912964	9.406913	0.465446
-21.919701	5.693803	0.470451
-22.930012	3.067060	0.475456
-23.135619	-2.661964	0.480461
-23.686251	6.623614	0.485466
-23.079707	-1.256594	0.490470
-23.418875	1.561203	0.495475
-23.472916	-1.375774	0.500480
-23.925805	-1.839954	0.505485
-24.654999	1.883262	0.510490
-24.930521	1.024484	0.515494
-25.110414	13.283114	0.520499
-24.762199	0.833692	0.525504
-24.818326	-0.287027	0.530509
-25.526109	6.678757	0.535514
-26.013602	-1.689150	0.540518
-26.447932	4.658273	0.545523
-26.332443	8.423976	0.550528
-26.186395	0.985613	0.555533
-26.380928	4.606602	0.560538
-26.796847	-1.659133	0.565542
-27.279500	4.509160	0.570547
-27.362508	-3.690777	0.575552
-27.927528	-0.097523	0.580557
-28.524013	1.520188	0.585562
-28.885780	-7.642384	0.590566
-29.050782	2.475296	0.595571
-29.047384	-1.584227	0.600576
-28.979049	-1.414576	0.605581
-29.191993	4.544050	0.610586
-28.987696	4.211658	0.615590
-29.507044	4.301973	0.620595
-30.120825	1.531237	0.625600
-30.240226	11.066039	0.630605
-30.506656	1.037597	0.635610
-30.974722	1.398328	0.640614
-31.544748	4.100215	0.645619
-31.900845	-5.249896	0.650624
-31.927391	2.590548	0.655629
-32.296196	-3.192156	0.660634
-32.255195	-1.699009	0.665638
-32.267704	-2.222264	0.670643
-32.296487	2.382121	0.675648
-32.755939	0.947724	0.680653
-32.959009	5.376772	0.685658
-33.370266	2.239157	0.690662
-33.849505	5.894983	0.695667
-33.936424	2.738506	0.700672
-33.806488	1.807108	0.705677
-34.574662	-1.265444	0.710682
-34.859821	-4.027236	0.715686
-35.111725	1.674872	0.720691
-35.066618	-15.112156	0.725696
-34.917493	-6.865648	0.730701
-35.388806	-4.274042	0.735706
-35.597154	-5.348915	0.740710
-36.241502	1.426662	0.745715
-36.584369	-0.519415	0.750720
-36.557923	-5.262710	0.755725
-36.689992	1.338197	0.760730
-36.744368	-1.136836	0.765734
-37.863929	-1.892671	0.770739
-37.919473	2.896208	0.775744
-38.265311	0.042627	0.780749
-38.380004	6.811667	0.785754
-37.845340	2.289789	0.790758
-37.963508	2.083531	0.795763
-38.685854	-7.355082	0.800768
-39.173017	-3.891006	0.805773
-39.251133	2.344009	0.810778
-39.319322	-9.562860	0.815782
-40.470924	-3.186016	0.820787
-40.257787	-6.227864	0.825792
-40.577340	-13.233072	0.830797
-40.753506	1.239518	0.835802
-40.672745	-12.098363	0.840806
-40.951567	-11.023640	0.845811
-41.177659	-6.802975	0.850816
-42.221228	0.309997	0.855821
-42.130352	0.371738	0.860826
-42.118756	-7.447471	0.865830
-42.358863	-6.682486	0.870835
-42.367007	-4.795723	0.875840
-42.306475	-3.381545	0.880845
-43.275413	-4.356978	0.885850
-43.529638	-10.268246	0.890854
-43.740244	-1.241253	0.895859
-43.778408	-3.149353	0.900864
-43.803142	-4.926671	0.905869
-44.238741	-2.815172	0.910874
-44.753505	-8.597293	0.915878
-45.004268	-6.220354	0.920883
-45.343940	2.181353	0.925888
-44.999487	-1.102397	0.930893
-45.849638	0.285900	0.935898
-46.439500	-2.662559	0.940902
-46.921427	-4.919167	0.945907
-46.440385	-10.416587	0.950912
-46.537591	-10.338216	0.955917
-46.989531	1.760288	0.960922
-46.887556	-11.169622	0.965926
-46.849161	-7.467847	0.970931
-47.566408	-10.757126	0.975936
-47.987790	-4.933724	0.980941
-48.220856	-5.811766	0.985946
-48.157088	-11.731418	0.990950
-48.304668	-12.005860	0.995955
-48.997914	3.543788	1.000960
-49.468309	-2.912773	1.005965
-49.925618	4.086775	1.010970
-49.618058	-5.537502	1.015974
-50.243824	-4.557451	1.020979
-50.168911	-4.493225	1.025984
-49.976518	3.085348	1.030989
-50.527204	2.563632	1.035994
-50.760266	-1.101583	1.040998
-51.128093	-1.487260	1.046003
-51.498659	-1.745965	1.051008
-51.246953	-0.342571	1.056013
-52.030751	2.269217	1.061018
-52.250168	-4.906603	1.066022
-52.616448	2.331862	1.071027
-52.789756	5.968528	1.076032
-52.117466	2.643225	1.081037
-53.093824	6.113870	1.086042
-53.272250	-3.789068	1.091046
-53.581235	3.671423	1.096051
-53.740217	-8.920475	1.101056
-54.711886	-1.961063	1.106061
-54.849172	0.749373	1.111066
-55.210763	-4.167614	1.116070
-54.882271	-10.691611	1.121075
-55.341282	-12.255784	1.126080
-55.520946	0.670327	1.131085
-55.737957	1.969536	1.136090
-55.731212	-5.143424	1.141094
-56.001095	1.229012	1.146099
-56.219688	-8.227923	1.151104
-56.594619	-0.380693	1.156109
-56.998041	0.621685	1.161114
-57.388674	-4.249653	1.166118
-57.518320	4.388264	1.171123
-57.487355	2.168854	1.176128
-58.196225	0.839729	1.181133
-58.322890	1.802179	1.186138
-58.476638	-11.394787	1.191142
-58.756826	-4.109620	1.196147
-58.674403	4.488950	1.201152
-59.031346	2.073682	1.206157
-59.552319	5.147568	1.211162
-59.784042	-0.529933	1.216166
-60.394308	5.927138	1.221171
-60.252219	1.431583	1.226176
-60.356641	-6.534070	1.231181
-60.491743	5.094340	1.236186
-60.308938	-0.941922	1.241190
-61.429470	3.519245	1.246195
-62.029233	-4.378775	1.251200
-61.614997	-0.140753	1.256205
-62.261633	1.962478	1.261210
-61.974863	-1.891237	1.266214
-61.886723	7.693501	1.271219
-62.768077	2.455656	1.276224
-63.018795	-1.421936	1.281229
-63.026216	0.518496	1.286234
-62.971485	-4.469639	1.291238
-63.503412	-7.952281	1.296243
-64.430196	0.578801	1.301248
-64.457436	-1.536637	1.306253
-64.883193	4.758832	1.311258
-64.381293	-0.137582	1.316262
-64.979383	3.416531	1.321267
-64.995615	0.704614	1.326272
-65.262049	-0.864235	1.331277
-66.020970	5.011725	1.336282
-65.667721	-4.157773	1.341286
-66.061233	3.619588	1.346291
-66.307806	3.025213	1.351296
-66.640708	0.318310	1.356301
-67.393633	11.562044	1.361306
-67.298834	2.040491	1.366310
-67.529423	3.965053	1.371315
-67.832562	12.841950	1.376320
-67.693288	3.683618	1.381325
-67.956640	9.023691	1.386330
-68.468502	-0.934895	1.391334
-69.110755	10.225169	1.396339
-69.197760	7.701435	1.401344
-68.923285	1.859700	1.406349
-69.257728	1.386571	1.411354
-70.022355	-5.710686	1.416358
-70.583564	0.362270	1.421363
-70.711657	7.838888	1.426368
-70.766402	-0.517302	1.431373
-71.091548	5.908030	1.436378
-71.313017	0.953407	1.441382
-71.027787	-4.772945	1.446387
-70.962634	2.373037	1.451392
-71.097864	-9.501245	1.456397
-71.643413	6.594861	1.461402
-71.942841	-2.643852	1.466406
-72.178176	0.860106	1.471411
-72.702025	0.976432	1.476416
-73.010083	-2.993469	1.481421
-73.758418	3.402843	1.486426
-73.423180	-10.895277	1.491430
-73.389104	-1.779837	1.496435
-73.927986	-7.355728	1.501440
-73.779597	-0.485291	1.506445
-74.641439	3.764762	1.511450
-74.543798	-3.950788	1.516454
-74.836594	-5.670550	1.521459
-75.139966	-2.086399	1.526464
-75.929438	-4.421666	1.531469
-76.354946	6.992540	1.536474
-76.334447	-0.002344	1.541478
-76.474103	3.622755	1.546483
-76.570547	13.774054	1.551488
-76.306898	3.862393	1.556493
-76.924770	4.648232	1.561498
-76.725186	-1.994897	1.566502
-77.246105	-5.570999	1.571507
-77.885042	-3.769514	1.576512
-77.641248	-7.812682	1.581517
-77.915722	-8.687440	1.586522
-78.336198	-11.823615	1.591526
-79.008353	-5.258840	1.596531
-79.331892	-4.161336	1.601536
-79.156210	-8.193899	1.606541
-79.121589	-2.526914	1.611546
-79.415938	-0.484862	1.616550
-80.444991	-1.001696	1.621555
-81.187366	2.742554	1.626560
-80.970249	-5.137125	1.631565
-80.986070	0.325750	1.636570
-80.635410	-10.785817	1.641574
-80.658548	-6.536644	1.646579
-80.937973	0.786369	1.651584
-81.590017	-0.086547	1.656589
-82.303552	-1.971746	1.661594
-82.093803	-1.542549	1.666598
-82.236891	-8.179777	1.671603
-82.757549	-0.040948	1.676608
-83.459861	0.906730	1.681613
-83.977891	9.149554	1.686618
-83.933623	-5.122248	1.691622
-84.100706	-10.667445	1.696627
-83.952398	-1.294554	1.701632
-83.816379	1.389146	1.706637
-83.952012	-3.022038	1.711642
-84.112988	-4.290942	1.716646
-84.573555	-0.675988	1.721651
-85.239522	0.623523	1.726656
-85.550630	-3.845757	1.731661
-86.129281	-2.202350	1.736666
-86.432909	-4.923300	1.741670
-86.616589	-9.393438	1.746675
-86.874883	-4.481249	1.751680
-86.519766	-3.543194	1.756685
-86.860419	-1.813461	1.761690
-86.800703	-3.293890	1.766694
-87.230901	-4.723348	1.771699
-87.836458	-4.939137	1.776704
-88.117990	-18.223763	1.781709
-88.073762	-5.433755	1.786714
-88.345429	-8.251427	1.791718
-88.349329	-8.209730	1.796723
-89.528653	-2.337916	1.801728
-89.809552	-10.459579	1.806733
-90.145192	1.171576	1.811738
-89.819358	-3.153276	1.816742
-89.793261	-6.570947	1.821747
-89.995129	-14.277821	1.826752
-90.027690	-9.596927	1.831757
-90.842383	-4.841707	1.836762
-91.244967	-8.800051	1.841766
-91.406823	-10.650927	1.846771
-91.305564	-14.912337	1.851776
-91.330904	-14.180792	1.856781
-92.395421	-9.813767	1.861786
-92.663861	-10.721101	1.866790
-92.740443	-16.508169	1.871795
-93.017284	-7.679669	1.876800
-93.140008	-14.123918	1.881805
-93.085667	-9.355318	1.886810
-93.304333	-8.729707	1.891814
-93.319825	-10.774209	1.896819
-94.202523	-6.609493	1.901824
-94.464982	-11.121146	1.906829
-94.645635	-6.853775	1.911834
-94.365427	-3.676853	1.916838
-94.414448	-7.190392	1.921843
-95.567525	0.439485	1.926848
-96.191037	-11.782696	1.931853
-96.013017	-8.529754	1.936858
-96.256636	-2.961812	1.941862
-96.113798	-8.153482	1.946867
-96.135239	-11.791532	1.951872
-96.633142	-8.398549	1.956877
-97.469481	-5.481199	1.961882
-97.643827	-3.758378	1.966886
-97.053903	-11.411371	1.971891
-97.639864	-3.002959	1.976896
-97.618203	-6.758449	1.981901
-98.806274	-1.480038	1.986906
-98.817151	-5.689190	1.991910
-98.818587	-7.362571	1.996915
-99.191588	-7.751391	2.006912
-98.798262	-5.221534	2.016909
-97.978963	0.045409	2.026906
-97.685019	-11.147545	2.036902
-97.585756	-1.995771	2.046899
-96.680034	-5.960273	2.056896
-96.198968	-2.430414	2.066893
-96.321040	-2.611047	2.076890
-95.260298	2.887559	2.086886
-94.770116	0.200982	2.096883
-93.985013	3.563131	2.106880
-93.844203	-2.189227	2.116877
-93.841191	-1.876168	2.126874
-92.918470	-6.568719	2.136870
-92.349988	-1.376760	2.146867
-91.343326	-4.108907	2.156864
-91.031117	-3.349831	2.166861
-91.178698	0.306419	2.176858
-90.477563	0.304879	2.186854
-89.524759	7.100041	2.196851
-89.127238	4.066774	2.206848
-89.198171	3.453708	2.216845
-88.215905	-6.633195	2.226842
-87.790849	-11.121550	2.236838
-86.918810	-9.169891	2.246835
-86.870953	-5.699290	2.256832
-86.782854	-3.372155	2.266829
-85.858934	-2.030435	2.276826
-85.375799	-8.586835	2.286822
-84.538393	1.967338	2.296819
-84.004353	-1.318425	2.306816
-84.048088	-5.296649	2.316813
-83.466755	-1.522650	2.326810
-82.408124	-5.596488	2.336806
-82.421629	-0.342423	2.346803
-81.799595	-2.263939	2.356800
-81.303801	-5.597598	2.366797
-81.102881	-3.316539	2.376794
-79.991847	2.126721	2.386790
-79.648918	-3.834498	2.396787
-79.541201	-0.420730	2.406784
-78.582092	-3.981745	2.416781
-78.186119	-2.158694	2.426778
-77.965249	-3.742160	2.436774
-77.007818	-6.504653	2.446771
-76.502750	-0.485555	2.456768
-76.411100	-6.965164	2.466765
-76.216044	0.622697	2.476762
-75.494761	-6.540969	2.486758
-74.612175	-1.768535	2.496755
-74.197254	-4.798175	2.506752
-73.730811	-5.146463	2.516749
-72.711501	1.761883	2.526746
-72.845555	1.925227	2.536742
-72.668942	-8.707786	2.546739
-72.073134	-3.361697	2.556736
-71.345293	-0.234544	2.566733
-70.247401	0.509904	2.576730
-69.861775	-3.528837	2.586726
-69.919662	-0.225496	2.596723
-69.716065	1.659186	2.606720
-68.788041	0.320398	2.616717
-68.462515	0.681440	2.626714
-67.490703	-2.225840	2.636710
-66.895799	-6.620269	2.646707
-66.788352	-6.941172	2.656704
-66.426119	-5.141377	2.666701
-65.484091	-6.577375	2.676698
-65.293410	-5.659998	2.686694
-64.465036	-5.386752	2.696691
-64.007346	-3.839397	2.706688
-64.164735	-1.838324	2.716685
-63.380335	2.537598	2.726682
-62.468195	1.286811	2.736678
-62.285289	4.036328	2.746675
-61.686861	7.208974	2.756672
-61.161846	6.230697	2.766669
-61.058200	3.224180	2.776666
-60.102273	4.282161	2.786662
-59.292157	-0.706461	2.796659
-59.513351	-7.289410	2.806656
-58.756276	-2.696998	2.816653
-58.130850	-3.313952	2.826650
-57.935412	0.757709	2.836646
-57.133993	-2.471487	2.846643
-56.624810	-5.005804	2.856640
-56.344233	1.653279	2.866637
-55.402405	-0.140638	2.876634
-55.164230	-2.825989	2.886630
-55.022902	1.380805	2.896627
-53.693705	3.387996	2.906624
-53.830132	-3.524922	2.916621
-53.520713	0.791912	2.926618
-52.651177	-1.589445	2.936614
-52.360434	-3.025405	2.946611
-51.627728	-7.761227	2.956608
-50.933389	-0.102222	2.966605
-50.869463	5.567430	2.976602
-50.409505	0.284881	2.986598
-49.558643	-3.753440	2.996595
-49.314450	-4.947743	3.006592
-48.344053	3.105424	3.016589
-48.128508	7.091597	3.026586
-47.829675	5.575184	3.036582
-47.094691	2.536890	3.046579
-46.801239	7.065279	3.056576
-46.411688	8.353991	3.066573
-45.481251	3.486013	3.076570
-45.192961	-1.171112	3.086566
-44.827484	-3.847775	3.096563
-44.005522	-1.942167	3.106560
-43.753260	-0.600403	3.116557
-43.446640	2.269231	3.126554
-42.123864	-3.740016	3.136550
-42.057434	4.862532	3.146547
-41.940494	2.956303	3.156544
-41.149145	-2.092750	3.166541
-40.673578	2.207719	3.176538
-40.243671	-0.833758	3.186534
-39.652298	-3.789505	3.196531
-39.141049	-3.498559	3.206528
-38.541984	0.047776	3.216525
-37.810229	-1.608899	3.226522
-37.922676	1.835981	3.236518
-37.667891	0.076178	3.246515
-36.503566	-0.390272	3.256512
-36.145725	-0.414384	3.266509
-35.175656	5.424618	3.276506
-34.846952	3.406225	3.286502
-34.739805	5.223565	3.296499
-34.603158	-2.412927	3.306496
-33.628069	2.411630	3.316493
-33.263387	2.871110	3.326490
-32.578064	-3.903668	3.336486
-31.864499	-4.955648	3.346483
-32.019017	0.472424	3.356480
-31.001167	2.382379	3.366477
-30.359788	2.858964	3.376474
-29.965215	2.965343	3.386470
-29.905848	4.467017	3.396467
-29.311505	0.139195	3.406464
-29.009356	-2.587794	3.416461
-28.038029	6.814671	3.426458
-27.757079	5.304209	3.436454
-26.922617	2.307446	3.446451
-26.763676	8.652864	3.456448
-26.200358	10.624086	3.466445
-25.495580	4.885280	3.476442
-25.203516	9.255503	3.486438
-24.782678	2.540908	3.496435
-23.808092	6.326541	3.506432
-23.381521	-4.123659	3.516429
-23.364400	2.937564	3.526426
-22.540303	4.617935	3.536422
-21.978836	0.450448	3.546419
-21.751613	-1.054815	3.556416
-21.173910	3.923478	3.566413
-20.274151	9.602374	3.576410
-20.262060	0.125835	3.586406
-19.710834	-0.280001	3.596403
-18.731305	2.681260	3.606400
-18.540850	0.285263	3.616397
-18.483858	6.329785	3.626394
-17.404359	6.712815	3.636390
-17.384583	-6.122678	3.646387
-16.408256	-8.102523	3.656384
-16.106242	-3.870064	3.666381
-15.939401	1.067665	3.676378
-15.116529	2.688041	3.686374
-14.786441	-2.887890	3.696371
-13.718580	-3.640251	3.706368
-13.260117	-2.108852	3.716365
-13.220765	-0.037045	3.726362
-13.039070	-7.211731	3.736358
-12.049768	2.872158	3.746355
-11.552800	3.985762	3.756352
-11.256519	-3.254282	3.766349
-10.360224	-1.920928	3.776346
-9.995396	-0.593522	3.786342
-9.567733	-2.440427	3.796339
-8.785319	1.850281	3.806336
-8.494723	-0.874910	3.816333
-8.430682	-5.918425	3.826330
-7.563600	0.022141	3.836326
-7.071217	1.104781	3.846323
-6.810828	-0.196579	3.856320
-5.971974	-1.499307	3.866317
-5.717737	6.503818	3.876314
-5.363434	7.234169	3.886310
-4.720714	14.426068	3.896307
-4.190895	23.672380	3.906304
-3.845106	24.058777	3.916301
-3.442455	40.512413	3.926298
-2.990972	45.542049	3.936294
-2.607397	54.456364	3.946291
-1.900511	68.917686	3.956288
-1.492836	77.261240	3.966285
-1.002301	96.444483	3.976282
-0.772788	105.639395	3.986278
0.000000	114.238745	3.991283
0.099274	133.967704	3.996288
0.630815	130.765530	4.001293
0.631655	141.034636	4.006298
0.700520	135.237523	4.011302
0.678753	134.155736	4.016307
0.808614	140.706424	4.021312
0.376433	137.920044	4.026317
0.628345	133.695249	4.031322
0.363957	145.846909	4.036326
0.812529	130.749595	4.041331
0.396106	139.299356	4.046336
0.887540	141.965708	4.051341
0.623731	137.960409	4.056346
0.657656	148.907721	4.061350
0.967916	140.472484	4.066355
0.629413	138.661748	4.071360
0.753812	148.851511	4.076365
1.057765	148.744040	4.081370
1.103651	162.337492	4.086374
1.012658	137.943886	4.091379
0.776536	140.913335	4.096384
0.833961	137.427482	4.101389
0.806821	130.594980	4.106394
0.517653	137.672804	4.111398
1.184881	143.345745	4.116403
1.375204	149.814258	4.121408
1.020935	145.253581	4.126413
0.851663	137.721888	4.131418
0.877946	146.813314	4.136422
1.230839	139.029483	4.141427
1.069154	143.961474	4.146432
1.094629	140.312921	4.151437
1.383794	133.573535	4.156442
0.806663	141.294128	4.161446
1.189464	139.684291	4.166451
1.327730	141.209762	4.171456
1.159573	135.519153	4.176461
0.959612	141.371403	4.181466
0.890126	143.596755	4.186470
1.209194	143.686241	4.191475
0.779887	140.291989	4.196480
1.019333	142.785608	4.201485
1.401380	147.829091	4.206490
1.087953	143.214600	4.211494
1.021855	138.450874	4.216499
1.535662	161.079683	4.221504
1.345360	154.468723	4.226509
1.437001	152.401193	4.231514
0.977547	147.379178	4.236518
1.106928	138.820247	4.241523
0.986792	143.359801	4.246528
1.034474	160.860107	4.251533
1.524748	159.420192	4.256538
1.564146	162.849772	4.261542
1.412963	161.348382	4.266547
0.991743	156.779144	4.271552
1.459655	162.995640	4.276557
1.538955	164.612549	4.281562
1.378278	168.171354	4.286566
1.098542	165.168251	4.291571
1.508148	165.227823	4.296576
1.484963	162.055066	4.301581
1.946304	159.778118	4.306586
1.338188	151.473208	4.311590
1.134312	147.373157	4.316595
1.445633	151.598770	4.321600
1.394211	155.621441	4.326605
1.719054	157.873981	4.331610
1.417011	164.343231	4.336614
1.512475	166.413193	4.341619
1.425033	165.983855	4.346624
1.404407	167.334755	4.351629
1.803571	162.783314	4.356634
1.151599	165.703621	4.361638
1.423728	169.682247	4.366643
1.656203	157.408918	4.371648
1.261618	160.630827	4.376653
1.626351	167.521434	4.381658
1.536399	166.969103	4.386662
2.047873	155.057288	4.391667
1.679326	166.408951	4.396672
1.631449	166.125310	4.401677
1.674595	165.058724	4.406682
1.668746	164.708429	4.411686
1.891134	163.183676	4.416691
1.532253	150.274779	4.421696
1.573753	163.641130	4.426701
1.658166	161.245703	4.431706
1.401707	162.465646	4.436710
1.469045	166.150298	4.441715
1.550499	170.313631	4.446720
1.361914	160.912039	4.451725
1.457572	161.523516	4.456730
1.803530	166.968082	4.461734
1.888601	170.969505	4.466739
1.746452	166.609908	4.471744
1.984110	173.969544	4.476749
1.803807	161.931318	4.481754
1.893438	178.665829	4.486758
1.999760	173.160258	4.491763
1.797842	166.427718	4.496768
1.616156	178.152082	4.501773
1.988823	179.672697	4.506778
2.016371	178.092859	4.511782
1.945819	173.450037	4.516787
1.933016	191.080011	4.521792
1.879665	182.676057	4.526797
2.373330	184.529002	4.531802
1.942433	178.309824	4.536806
2.158693	168.044785	4.541811
1.985026	171.444266	4.546816
1.959281	174.890318	4.551821
2.158599	166.155973	4.556826
1.671813	171.872562	4.561830
2.161080	173.308585	4.566835
2.375650	182.278967	4.571840
1.769460	184.473994	4.576845
1.882322	182.602469	4.581850
2.108052	182.535650	4.586854
2.302068	182.261801	4.591859
2.182423	172.748231	4.596864
2.199893	186.181615	4.601869
2.443385	184.229641	4.606874
2.129129	197.341368	4.611878
2.226256	188.800089	4.616883
2.517326	184.895045	4.621888
1.815996	180.682617	4.626893
2.060771	173.807761	4.631898
2.055025	184.821382	4.636902
2.510427	191.210674	4.641907
2.239843	182.539993	4.646912
1.908794	188.741691	4.651917
2.158626	186.108539	4.656922
2.006942	193.965390	4.661926
2.419941	181.458299	4.666931
2.042751	188.882033	4.671936
2.207158	183.978005	4.676941
2.244606	184.022756	4.681946
2.157169	184.226153	4.686950
2.253689	178.614541	4.691955
2.205523	185.977556	4.696960
2.550200	183.060724	4.701965
2.599610	173.109555	4.706970
1.937515	180.413133	4.711974
2.171248	181.053732	4.716979
2.900033	195.825339	4.721984
2.567122	198.676992	4.726989
2.894600	183.880055	4.731994
2.360269	189.980529	4.736998
2.255100	183.865655	4.742003
1.871539	188.177322	4.747008
2.154847	198.082950	4.752013
2.789818	204.861895	4.757018
2.174440	207.434834	4.762022
2.293044	201.791303	4.767027
2.657745	205.534066	4.772032
2.943777	205.707788	4.777037
2.795205	213.766639	4.782042
2.610604	208.606902	4.787046
2.566924	209.999359	4.792051
2.840779	211.601799	4.797056
3.229753	216.081087	4.802061
3.245601	213.047773	4.807066
3.006012	204.090687	4.812070
2.789162	190.153596	4.817075
2.536786	182.346928	4.822080
2.443929	177.963836	4.827085
2.670148	180.991018	4.832090
2.600909	187.221553	4.837094
2.598695	190.743037	4.842099
2.429942	199.526342	4.847104
3.043383	207.371637	4.852109
2.715389	204.676591	4.857114
2.742563	207.699967	4.862118
2.710344	199.026966	4.867123
2.937658	208.435129	4.872128
2.602861	202.846372	4.877133
3.015597	213.367757	4.882138
2.772337	215.395552	4.887142
2.596145	204.989119	4.892147
2.775413	216.644654	4.897152
2.844144	213.258264	4.902157
3.136021	208.600132	4.907162
2.768956	213.554628	4.912166
2.808416	208.932632	4.917171
2.697927	216.030123	4.922176
2.683818	211.631598	4.927181
2.834593	212.351551	4.932186
2.598006	220.961935	4.937190
2.909317	210.001880	4.942195
3.223648	211.215212	4.947200
3.187888	223.549623	4.952205
3.005481	208.645394	4.957210
2.593407	207.200438	4.962214
3.198228	211.076655	4.967219
3.237359	225.326091	4.972224
3.281859	227.979785	4.977229
3.434966	217.395526	4.982234
3.263334	209.437073	4.987238
2.968006	204.829239	4.992243
2.953226	208.843053	4.997248
2.896911	210.863887	5.002253
3.109704	219.318884	5.007258
2.889870	234.703281	5.012262
3.727442	228.596632	5.017267
3.430276	220.379314	5.022272
3.175527	220.744800	5.027277
3.423084	211.310076	5.032282
2.861534	223.422636	5.037286
3.219104	223.218233	5.042291
3.141098	232.626491	5.047296
3.448750	231.556682	5.052301
3.802252	232.634206	5.057306
3.302347	222.800172	5.062310
3.377688	207.909596	5.067315
3.563189	203.242718	5.072320
3.179910	219.411834	5.077325
3.192403	214.945892	5.082330
2.947930	219.185292	5.087334
3.092335	218.934986	5.092339
3.362549	221.392189	5.097344
3.335365	238.429676	5.102349
3.525532	231.715157	5.107354
3.387652	231.673314	5.112358
3.683507	231.057749	5.117363
3.341429	235.530644	5.122368
3.474382	235.471942	5.127373
3.702627	229.523436	5.132378
3.511232	237.092266	5.137382
3.791334	232.201848	5.142387
3.665290	224.986084	5.147392
2.950715	223.256038	5.152397
3.785087	220.550852	5.157402
3.677752	231.624610	5.162406
3.772097	227.791314	5.167411
3.519120	218.826814	5.172416
3.221795	228.712133	5.177421
3.625062	219.819460	5.182426
3.438102	230.946744	5.187430
3.776209	224.462289	5.192435
3.864026	229.399749	5.197440
3.368590	224.554153	5.202445
3.578007	225.834440	5.207450
3.371825	227.840645	5.212454
3.716313	231.304992	5.217459
3.832268	232.460629	5.222464
3.634554	240.242412	5.227469
3.822839	227.438088	5.232474
3.806262	238.687541	5.237478
4.024422	240.909247	5.242483
4.031959	230.499503	5.247488
3.674689	237.714517	5.252493
3.857133	228.236139	5.257498
3.640064	234.445416	5.262502
3.473606	232.851487	5.267507
3.364330	230.024309	5.272512
3.494152	236.227033	5.277517
3.474049	221.104539	5.282522
3.546840	230.812013	5.287526
3.462626	243.422894	5.292531
3.831508	248.022375	5.297536
3.837898	261.119026	5.302541
4.442284	260.730665	5.307546
3.973459	259.009808	5.312550
4.001353	255.664569	5.317555
4.013787	252.173044	5.322560
4.171136	262.031882	5.327565
3.763016	244.533738	5.332570
4.205220	255.044232	5.337574
4.136641	250.739598	5.342579
3.824055	248.292077	5.347584
4.309601	246.466922	5.352589
4.038619	239.444557	5.357594
3.914155	245.136393	5.362598
4.083144	241.785007	5.367603
4.327514	238.940730	5.372608
3.740952	243.220743	5.377613
4.396552	246.462651	5.382618
4.201329	245.831798	5.387622
3.998774	237.583924	5.392627
3.750599	244.297910	5.397632
3.981689	252.585563	5.402637
4.199824	249.501765	5.407642
4.390513	258.672053	5.412646
4.467943	262.102057	5.417651
4.166486	260.320341	5.422656
4.280223	249.843431	5.427661
4.384048	251.048414	5.432666
4.102581	260.067593	5.437670
4.170699	258.123934	5.442675
4.201746	260.472850	5.447680
4.356488	261.619286	5.452685
4.514193	267.551930	5.457690
4.564517	258.128907	5.462694
4.279556	256.996344	5.467699
4.125919	248.184038	5.472704
4.270089	253.546155	5.477709
4.657696	246.196626	5.482714
4.115108	250.801981	5.487718
4.008809	249.518218	5.492723
4.485696	255.372688	5.497728
4.390851	262.676565	5.502733
4.714379	256.855581	5.507738
4.494043	256.741155	5.512742
4.604975	257.660299	5.517747
4.842431	256.430579	5.522752
4.172644	246.749529	5.527757
4.569256	253.315673	5.532762
4.204055	257.535914	5.537766
4.475608	254.105283	5.542771
4.680101	250.666112	5.547776
4.268702	252.150625	5.552781
4.621709	253.149135	5.557786
4.591784	265.384592	5.562790
4.838758	257.332468	5.567795
4.767515	253.642004	5.572800
4.569672	259.750222	5.577805
4.567246	250.411345	5.582810
4.674125	255.364826	5.587814
4.613425	258.015923	5.592819
4.605992	257.618417	5.597824
4.413179	263.523378	5.602829
4.474109	257.958410	5.607834
4.719492	252.874079	5.612838
4.656140	253.114855	5.617843
4.017146	251.483768	5.622848
4.226728	252.007909	5.627853
4.435813	256.739837	5.632858
4.421241	256.909745	5.637862
4.533994	266.183918	5.642867
4.859237	276.003968	5.647872
4.985920	280.558911	5.652877
5.276646	273.923631	5.657882
4.508719	264.684950	5.662886
4.357608	259.178305	5.667891
4.474921	270.903632	5.672896
4.866083	267.156989	5.677901
4.832557	271.809638	5.682906
5.144065	274.175000	5.687910
4.922513	276.278514	5.692915
5.170951	276.012010	5.697920
4.978237	272.504966	5.702925
4.946128	271.965773	5.707930
4.637386	280.040101	5.712934
5.007683	277.742513	5.717939
5.115228	276.865206	5.722944
4.871761	283.803097	5.727949
4.837265	276.253525	5.732954
5.253543	286.983206	5.737958
5.115291	276.969449	5.742963
5.143811	275.588764	5.747968
5.203950	284.674990	5.752973
5.437396	278.184666	5.757978
4.839765	270.741756	5.762982
4.727242	266.478760	5.767987
5.153336	269.360944	5.772992
4.711176	280.727305	5.777997
5.066519	277.270969	5.783002
5.048973	280.817003	5.788006
5.264117	277.290748	5.793011
5.339648	280.876074	5.798016
5.168285	271.734328	5.803021
4.975709	272.020533	5.808026
5.089311	281.098433	5.813030
5.317735	285.507825	5.818035
5.436359	286.685196	5.823040
5.057168	283.314750	5.828045
5.173426	283.008715	5.833050
5.128151	271.306890	5.838054
5.188927	275.691762	5.843059
5.122563	275.955153	5.848064
5.231606	282.366768	5.853069
5.180385	282.127938	5.858074
5.318166	282.701224	5.863078
5.388412	281.215967	5.868083
5.279053	273.194006	5.873088
5.309161	278.921897	5.878093
5.222994	280.653163	5.883098
5.306444	277.400508	5.888102
5.269475	279.082985	5.893107
5.596601	277.424858	5.898112
5.281904	284.335875	5.903117
5.469703	274.862966	5.908122
5.388375	277.416039	5.913126
5.299388	276.003030	5.918131
5.634536	277.798409	5.923136
5.242674	290.770430	5.928141
5.167282	268.380000	5.933146
5.513278	283.619396	5.938150
5.389077	294.569272	5.943155
5.721479	298.215845	5.948160
5.408278	290.779261	5.953165
5.794270	294.806625	5.958170
5.463891	287.442318	5.963174
5.447657	282.579042	5.968179
5.360733	294.181163	5.973184
5.424143	303.583259	5.978189
5.837965	298.229085	5.983194
5.571519	304.841537	5.988198
5.505424	301.998133	5.993203
5.332663	302.078777	5.998208
5.520922	305.826887	6.003213
5.447725	303.902061	6.008218
5.509548	311.121455	6.013222
5.495420	305.688379	6.018227
5.263960	292.895578	6.023232
5.421638	301.884370	6.028237
5.775239	295.701193	6.033242
5.853633	299.131054	6.038246
5.802526	304.662794	6.043251
5.772163	301.060866	6.048256
5.450782	298.627363	6.053261
5.534118	299.674190	6.058266
5.738733	305.207243	6.063270
5.759939	303.027278	6.068275
5.833732	296.163179	6.073280
5.575488	313.154456	6.078285
5.839099	298.829267	6.083290
6.034436	304.920576	6.088294
5.965948	309.860248	6.093299
5.507165	303.474528	6.098304
5.695741	309.161938	6.103309
5.908366	308.530856	6.108314
5.995165	308.223081	6.113318
5.713978	285.608410	6.118323
5.629118	287.725444	6.123328
5.329464	284.048391	6.128333
5.471141	289.255886	6.133338
5.720531	290.944399	6.138342
5.640032	298.910434	6.143347
5.502449	303.411616	6.148352
5.545611	303.816140	6.153357
5.815968	308.351884	6.158362
5.575584	307.835626	6.163366
5.729361	308.555116	6.168371
6.128580	304.557279	6.173376
5.741903	291.943666	6.178381
5.667565	280.515274	6.183386
5.519025	278.434506	6.188390
5.397779	283.259001	6.193395
5.821320	278.181725	6.198400
5.912882	282.489041	6.203405
5.890427	280.853705	6.208410
5.634348	280.659425	6.213414
5.641266	280.272340	6.218419
5.901439	271.322829	6.223424
5.678865	286.609623	6.228429
5.840858	289.754389	6.233434
5.606093	288.712083	6.238438
5.450179	286.382530	6.243443
5.290496	265.878136	6.248448
5.840619	292.389638	6.253453
5.574061	279.513727	6.258458
5.486526	286.123626	6.263462
5.736276	286.878792	6.268467
5.672018	276.075246	6.273472
5.614468	277.564778	6.278477
5.627297	287.212018	6.283482
5.636317	287.976191	6.288486
5.308512	294.107819	6.293491
5.493571	278.330085	6.298496
5.522768	285.665277	6.303501
5.497363	277.503695	6.308506
5.461057	290.714581	6.313510
5.406189	290.912909	6.318515
5.828794	296.491111	6.323520
5.267676	305.155228	6.328525
5.645863	305.077326	6.333530
6.036404	306.221854	6.338534
5.699614	313.392581	6.343539
5.700039	308.637434	6.348544
5.526425	303.567706	6.353549
5.711608	302.327140	6.358554
5.721484	299.452926	6.363558
5.332857	290.098229	6.368563
5.726901	294.304669	6.373568
5.561701	302.831213	6.378573
5.721031	303.160703	6.383578
5.846799	308.047984	6.388582
5.389091	303.797595	6.393587
6.006086	302.198737	6.398592
5.839007	294.128807	6.403597
5.800044	288.443343	6.408602
5.622080	281.359023	6.413606
5.348613	284.229909	6.418611
5.744295	277.233443	6.423616
5.458594	283.788775	6.428621
5.487180	284.632158	6.433626
5.504676	281.301188	6.438630
5.732200	298.011178	6.443635
5.866748	291.767197	6.448640
5.534392	294.356193	6.453645
5.390635	283.568183	6.458650
5.665957	289.099714	6.463654
5.833508	293.341418	6.468659
5.811683	283.591099	6.473664
5.771289	288.051837	6.478669
5.479982	283.319972	6.483674
5.621176	283.282133	6.488678
5.653423	286.659067	6.493683
5.761665	275.604041	6.498688
5.661016	282.516532	6.503693
5.366663	277.022692	6.508698
5.597779	276.477316	6.513702
5.618812	276.999178	6.518707
5.615453	274.240921	6.523712
5.552379	276.708896	6.528717
5.804428	287.435674	6.533722
5.909534	282.651581	6.538726
5.402876	282.455187	6.543731
5.646389	271.043751	6.548736
5.771702	277.696435	6.553741
5.716022	269.878086	6.558746
5.516342	278.372022	6.563750
5.509945	274.832806	6.568755
5.836849	277.262208	6.573760
5.550915	290.711273	6.578765
5.526879	278.098155	6.583770
5.509572	275.595166	6.588774
5.822620	280.026181	6.593779
5.657777	280.981936	6.598784
5.582896	280.496857	6.603789
5.662171	276.166033	6.608794
5.472132	276.521444	6.613798
5.659740	280.500600	6.618803
5.693959	278.435669	6.623808
5.757277	286.091410	6.628813
5.336634	284.631963	6.633818
5.693022	287.445911	6.638822
5.775169	297.082363	6.643827
5.916309	281.725908	6.648832
5.767397	282.530489	6.653837
5.837104	276.767999	6.658842
5.517059	288.589907	6.663846
5.467435	290.941896	6.668851
5.762683	276.333394	6.673856
5.350191	273.142138	6.678861
5.270171	280.149490	6.683866
5.696663	289.738653	6.688870
5.645466	295.877834	6.693875
5.533480	294.395639	6.698880
5.703345	301.936723	6.703885
5.746596	307.947310	6.708890
5.721041	303.085481	6.713894
5.429518	284.860473	6.718899
5.815023	292.004154	6.723904
5.610913	297.787500	6.728909
5.654964	295.983623	6.733914
5.827760	286.949634	6.738918
5.355538	281.088025	6.743923
5.408987	289.843106	6.748928
5.498864	303.518401	6.753933
5.794127	300.666191	6.758938
5.805008	302.638608	6.763942
5.941057	301.105140	6.768947
5.764521	276.594950	6.773952
4.919118	291.175142	6.778957
5.401698	292.931750	6.783962
6.010823	301.717378	6.788966
5.985045	298.801259	6.793971
5.883634	282.596732	6.798976
5.684883	284.519530	6.803981
5.802661	274.747481	6.808986
5.714040	278.386836	6.813990
5.638272	276.889513	6.818995
6.055259	278.491820	6.824000
5.795910	286.121870	6.829005
5.851585	272.427016	6.834010
5.866289	273.395944	6.839014
5.577475	281.675974	6.844019
5.880199	273.115299	6.849024
5.579062	282.045805	6.854029
5.687158	266.998222	6.859034
5.795118	282.217731	6.864038
5.581459	280.745041	6.869043
5.884406	273.452973	6.874048
5.959375	280.948713	6.879053
5.792385	273.343842	6.884058
5.760171	279.442097	6.889062
5.397376	274.348050	6.894067
5.490525	267.980811	6.899072
5.946562	274.401672	6.904077
5.917781	263.137037	6.909082
5.482314	257.041928	6.914086
5.560212	256.966488	6.919091
5.508281	247.647975	6.924096
5.509326	270.147955	6.929101
5.284521	274.684856	6.934106
5.632887	275.756855	6.939110
5.559096	277.163497	6.944115
5.716237	276.512582	6.949120
5.646883	278.899278	6.954125
5.988847	267.064399	6.959130
6.022441	266.464357	6.964134
5.648308	261.973180	6.969139
5.355370	249.579116	6.974144
5.341855	266.060855	6.979149
5.539665	271.275424	6.984154
5.418073	277.435051	6.989158
5.400814	277.836326	6.994163
5.667389	277.937151	6.999168
5.991801	278.066934	7.004173
5.763217	281.804011	7.009178
5.525361	281.587911	7.014182
5.441054	277.029460	7.019187
5.746876	278.769295	7.024192
5.315559	284.945510	7.029197
5.567754	280.809220	7.034202
5.437831	281.563389	7.039206
5.548781	279.018284	7.044211
5.672705	266.809236	7.049216
5.527989	285.791757	7.054221
5.209120	272.550680	7.059226
5.374970	276.979304	7.064230
5.490481	278.596913	7.069235
5.713840	279.210657	7.074240
5.642660	277.108353	7.079245
5.850272	275.576400	7.084250
5.534014	280.681189	7.089254
5.400065	282.628698	7.094259
5.546543	279.306120	7.099264
5.697227	280.427879	7.104269
5.700891	279.908426	7.109274
5.647857	274.509890	7.114278
5.033062	278.038183	7.119283
5.712709	281.406066	7.124288
5.841729	293.287770	7.129293
5.843214	291.126696	7.134298
5.642965	276.117623	7.139302
5.498000	282.742789	7.144307
5.618690	277.215966	7.149312
5.564155	283.605595	7.154317
5.653970	279.836266	7.159322
5.806572	273.051653	7.164326
5.252339	286.583615	7.169331
5.733745	284.477532	7.174336
5.346979	305.253611	7.179341
5.427034	309.648145	7.184346
5.570447	306.028651	7.189350
5.488679	304.747391	7.194355
5.964518	298.561000	7.199360
5.946002	305.976394	7.204365
6.140704	297.268014	7.209370
6.159794	289.036225	7.214374
5.744222	275.076225	7.219379
5.587125	276.609729	7.224384
5.387217	284.062848	7.229389
5.639787	287.104928	7.234394
5.650777	283.929991	7.239398
5.715596	283.442144	7.244403
5.877435	282.610166	7.249408
5.595387	284.859139	7.254413
5.476267	286.288658	7.259418
5.649438	284.645009	7.264422
5.563935	283.978090	7.269427
5.633524	287.235317	7.274432
5.387800	286.685090	7.279437
5.164872	285.112604	7.284442
5.450219	288.592498	7.289446
5.665821	312.647302	7.294451
5.907697	293.367981	7.299456
5.776878	297.412537	7.304461
5.732139	285.495487	7.309466
5.544704	283.854201	7.314470
5.581013	288.321978	7.319475
5.452249	283.757792	7.324480
5.792947	280.025331	7.329485
5.767152	282.285025	7.334490
5.889033	281.661745	7.339494
5.508957	285.631214	7.344499
5.729850	280.892367	7.349504
5.452010	284.580167	7.354509
5.511429	283.751481	7.359514
5.763304	287.113202	7.364518
5.500125	280.763474	7.369523
5.531618	274.079972	7.374528
5.646150	283.654428	7.379533
5.653103	282.340374	7.384538
5.881527	279.251805	7.389542
5.503894	285.191876	7.394547
6.077752	285.662466	7.399552
5.847404	279.642977	7.404557
5.875772	280.065622	7.409562
5.940151	274.458984	7.414566
6.241199	285.750762	7.419571
5.823078	276.672742	7.424576
5.628087	288.430887	7.429581
6.065441	284.439771	7.434586
5.656027	276.591074	7.439590
5.105425	271.292155	7.444595
5.704934	281.952177	7.449600
5.908845	279.680495	7.454605
5.635653	280.501262	7.459610
5.633424	282.124548	7.464614
5.440886	290.047912	7.469619
5.885800	277.364945	7.474624
5.758716	287.866021	7.479629
5.625985	274.735164	7.484634
5.714004	267.916315	7.489638
5.404991	271.814606	7.494643
5.582010	274.261017	7.499648
5.248377	276.834390	7.504653
5.627753	269.881595	7.509658
5.538853	278.149479	7.514662
5.987289	278.775635	7.519667
5.907591	275.067501	7.524672
5.513401	279.624449	7.529677
6.016681	275.765436	7.534682
5.765502	260.628267	7.539686
5.547581	265.110312	7.544691
5.482835	256.138632	7.549696
5.265483	260.339018	7.554701
5.961373	269.145921	7.559706
5.719060	272.059409	7.564710
5.686453	263.731279	7.569715
5.839606	253.273540	7.574720
5.232879	250.950908	7.579725
5.407104	266.697914	7.584730
5.853983	271.509879	7.589734
5.716008	279.794896	7.594739
5.669412	271.377194	7.599744
5.565274	274.553901	7.604749
5.679565	268.755999	7.609754
5.687587	267.017845	7.614758
5.597121	269.205351	7.619763
5.645216	264.670580	7.624768
5.568710	274.717692	7.629773
5.521080	269.011438	7.634778
5.738102	274.798810	7.639782
5.625111	272.756800	7.644787
6.030415	267.299559	7.649792
5.683493	263.667834	7.654797
5.550883	253.510845	7.659802
5.456710	252.826295	7.664806
5.290870	265.848526	7.669811
5.752574	266.507417	7.674816
5.648740	276.574604	7.679821
5.914008	267.292113	7.684826
5.544786	254.694792	7.689830
5.350920	264.845591	7.694835
5.763251	270.830338	7.699840
5.465737	276.371961	7.704845
5.621576	273.611064	7.709850
5.789380	280.560849	7.714854
5.884408	279.435559	7.719859
5.934968	271.898055	7.724864
5.563168	260.386278	7.729869
5.359466	258.712726	7.734874
5.699544	254.720943	7.739878
5.555514	258.833985	7.744883
5.590357	255.304170	7.749888
5.694491	266.607612	7.754893
5.442775	269.471945	7.759898
5.741511	279.599839	7.764902
5.844682	278.258149	7.769907
5.397824	264.091061	7.774912
5.527259	265.500861	7.779917
5.449887	269.141627	7.784922
5.796610	276.500143	7.789926
5.771653	284.368940	7.794931
5.899814	280.185524	7.799936
5.439039	265.998455	7.804941
5.284780	266.784886	7.809946
5.529118	275.364710	7.814950
5.537930	278.473213	7.819955
5.880203	276.521668	7.824960
5.665137	280.648938	7.829965
5.568288	274.817470	7.834970
5.700419	276.192051	7.839974
5.557775	274.961399	7.844979
5.587677	268.458478	7.849984
5.616360	273.607633	7.854989
5.718834	274.088341	7.859994
5.593785	278.805861	7.864998
5.448568	282.292681	7.870003
5.886109	275.998367	7.875008
5.623162	277.969124	7.880013
5.570448	268.502028	7.885018
5.814997	271.732011	7.890022
5.518333	276.428795	7.895027
5.782624	271.670540	7.900032
5.474460	276.657010	7.905037
5.484375	281.847054	7.910042
5.571287	282.811067	7.915046
5.620231	274.008336	7.920051
6.269470	279.272842	7.925056
5.924915	269.620234	7.930061
5.419655	265.339294	7.935066
5.476002	264.441486	7.940070
5.708863	274.547997	7.945075
5.882829	264.245195	7.950080
5.664882	270.707717	7.955085
5.472980	257.003966	7.960090
5.790100	256.717277	7.965094
5.420451	262.972467	7.970099
5.576664	267.393097	7.975104
5.708880	270.311546	7.980109
5.557211	279.845191	7.985114
6.004414	283.151190	7.990118
5.841016	274.921566	7.995136
5.365259	260.385067	8.000154
5.270966	263.842495	8.005171
5.032505	272.033715	8.010189
5.664073	280.670114	8.015206
5.504078	280.246889	8.020224
5.622371	280.834314	8.025242
5.485698	283.563083	8.030259
5.387511	278.138035	8.035277
5.719682	282.889141	8.040294
5.480885	280.638455	8.045312
5.650283	277.538464	8.050330
5.632717	283.981794	8.055347
5.287746	282.072668	8.060365
5.498377	276.435446	8.065382
5.367605	286.597950	8.070400
6.115930	295.957750	8.075418
5.993671	293.367044	8.080435
6.062891	294.003133	8.085453
5.802155	279.209091	8.090470
5.687376	280.252502	8.095488
5.593018	280.418626	8.100506
5.941806	279.720536	8.105523
5.747254	286.860415	8.110541
5.634093	285.735660	8.115558
5.963058	291.986191	8.120576
5.844406	278.334454	8.125594
5.736953	281.396326	8.130611
5.399475	273.903733	8.135629
5.893888	276.455353	8.140646
5.814138	280.532177	8.145664
5.805755	286.775274	8.150682
6.047799	274.092960	8.155699
5.877589	272.727793	8.160717
6.138322	270.970501	8.165734
5.858596	280.048569	8.170752
5.985774	277.614678	8.175770
5.937461	283.359090	8.180787
5.726909	290.226922	8.185805
5.811464	275.369655	8.190822
5.869492	285.354449	8.195840
6.046498	281.145648	8.200858
5.758067	278.782776	8.205875
5.599843	281.016312	8.210893
5.775257	278.707446	8.215910
5.920141	285.526247	8.220928
5.964037	281.032076	8.225946
6.022316	286.027787	8.230963
5.867441	278.995884	8.235981
5.917874	282.159398	8.240998
5.842178	274.493510	8.246016
5.904500	284.439768	8.251034
6.003087	289.602764	8.256051
5.850843	284.792011	8.261069
5.661098	279.753581	8.266086
6.008226	281.520293	8.271104
5.912041	285.981508	8.276122
6.097558	279.496176	8.281139
6.013455	276.249473	8.286157
5.586445	275.138871	8.291174
5.477247	286.178436	8.296192
5.370885	275.301739	8.301210
5.718412	283.322838	8.306227
5.681458	310.375445	8.311245
5.993318	305.741722	8.316262
5.901818	315.150243	8.321280
5.975384	306.883622	8.326298
6.262448	310.594090	8.331315
6.182651	310.275135	8.336333
6.281736	305.254841	8.341350
6.326505	298.800883	8.346368
5.756129	287.567259	8.351386
5.940001	288.431636	8.356403
6.160094	297.214154	8.361421
6.187307	299.371486	8.366438
5.876520	296.197940	8.371456
6.015602	278.716165	8.376474
5.986339	288.250675	8.381491
5.577780	290.201314	8.386509
6.048817	305.312822	8.391526
6.110945	305.814324	8.396544
6.022544	304.111388	8.401562
6.225040	308.762778	8.406579
6.114925	309.240607	8.411597
5.921578	312.688221	8.416614
5.864448	315.549770	8.421632
6.033719	310.354453	8.426650
6.479831	305.431599	8.431667
5.948049	311.472188	8.436685
6.220556	304.758720	8.441702
6.120715	308.624096	8.446720
6.475975	303.746944	8.451738
6.629125	299.592343	8.456755
5.752036	288.201356	8.461773
6.024888	282.507110	8.466790
5.511403	282.517597	8.471808
5.992193	292.868893	8.476826
5.957211	291.612051	8.481843
6.000302	310.741040	8.486861
6.253151	306.157527	8.491878
6.096653	312.417382	8.496896
6.379640	305.689659	8.501914
6.559972	306.582989	8.506931
6.276779	304.216142	8.511949
6.464811	312.792234	8.516966
6.410652	312.488221	8.521984
6.395699	307.293188	8.527002
6.062288	287.818032	8.532019
6.082483	288.837274	8.537037
6.210318	297.056677	8.542054
6.360848	301.346947	8.547072
6.131716	293.013858	8.552090
6.303373	293.091230	8.557107
6.171748	303.676731	8.562125
6.270357	303.238487	8.567143
6.406245	303.046888	8.572160
6.149267	292.061095	8.577178
6.277714	293.713542	8.582195
5.821968	300.275590	8.587213
5.948996	301.559050	8.592231
6.193242	302.000640	8.597248
6.342602	304.142110	8.602266
6.238578	303.763815	8.607283
5.966224	309.426359	8.612301
6.213037	303.663581	8.617319
6.297858	308.576276	8.622336
5.963695	306.848491	8.627354
6.293670	297.828779	8.632371
5.995791	303.675167	8.637389
6.262746	297.808274	8.642407
6.190009	305.383605	8.647424
6.321456	302.743930	8.652442
6.277579	296.196483	8.657459
6.187728	299.530156	8.662477
6.242485	309.433426	8.667495
6.561871	320.097031	8.672512
6.439278	315.180672	8.677530
6.465772	300.824703	8.682547
6.185787	300.801990	8.687565
6.256302	298.424252	8.692583
6.554310	318.930438	8.697600
6.200460	321.951788	8.702618
6.683925	315.416898	8.707635
6.245475	308.757320	8.712653
6.483158	322.964798	8.717671
6.745157	318.461904	8.722688
6.272581	313.375987	8.727706
6.572066	308.914593	8.732723
6.099656	310.335563	8.737741
6.486509	310.234271	8.742759
6.456344	309.816075	8.747776
6.381160	315.018757	8.752794
6.372331	313.603216	8.757811
6.566563	328.798865	8.762829
6.738797	311.908311	8.767847
6.602383	309.203048	8.772864
6.325099	306.557586	8.777882
6.348418	307.099842	8.782899
6.281356	314.223038	8.787917
6.379466	312.434260	8.792935
6.424929	320.407738	8.797952
6.066440	325.013938	8.802970
6.580410	315.384934	8.807987
6.540828	318.628738	8.813005
6.210709	319.068242	8.818023
6.306719	322.120531	8.823040
6.255872	329.941759	8.828058
6.424229	319.735436	8.833075
6.297546	328.130173	8.838093
6.566361	322.603791	8.843111
6.779509	321.339871	8.848128
5.910774	330.213041	8.853146
6.531582	331.738343	8.858163
6.642032	343.311758	8.863181
6.931529	350.278473	8.868199
6.673830	329.620742	8.873216
6.566170	320.486130	8.878234
6.663838	321.076768	8.883251
6.264646	324.594301	8.888269
6.484100	325.036597	8.893287
6.899265	334.139037	8.898304
6.835713	341.507837	8.903322
6.714395	336.607052	8.908339
6.525538	333.853149	8.913357
6.850957	330.526896	8.918375
6.732211	318.131086	8.923392
6.595779	324.009145	8.928410
6.849809	326.042807	8.933427
6.822533	327.754214	8.938445
6.801662	323.068155	8.943463
6.479664	321.370031	8.948480
6.724722	324.891393	8.953498
6.711676	316.950660	8.958515
6.440068	324.323445	8.963533
6.481486	320.511266	8.968551
6.814731	316.921880	8.973568
6.700774	319.098038	8.978586
6.785703	315.032946	8.983603
6.703336	324.982820	8.988621
6.720703	330.590795	8.993639
6.777414	326.754144	8.998656
6.519357	322.840277	9.003674
6.984738	328.324852	9.008691
6.652006	321.380581	9.013709
6.738527	326.741116	9.018727
6.675964	327.217853	9.023744
6.964914	345.538625	9.028762
7.212749	334.957021	9.033779
6.669664	335.174077	9.038797
6.574058	334.630377	9.043815
7.127354	320.511090	9.048832
6.903093	331.928340	9.053850
6.790267	320.942175	9.058867
6.549559	325.930803	9.063885
6.400344	325.531143	9.068903
7.170077	329.056018	9.073920
6.793408	337.963027	9.078938
6.792572	342.788088	9.083955
6.851014	345.533822	9.088973
6.774835	350.588354	9.093991
6.846915	341.873847	9.099008
6.969593	347.370762	9.104026
7.168825	347.011519	9.109043
6.934576	334.378074	9.114061
6.403283	334.094704	9.119079
6.958432	339.565306	9.124096
6.982085	346.491364	9.129114
7.161823	340.881021	9.134131
7.186442	336.471883	9.139149
6.489259	341.834528	9.144167
7.020360	337.911391	9.149184
7.044424	349.144829	9.154202
7.039849	347.769646	9.159219
7.024521	334.347919	9.164237
6.608866	332.534995	9.169255
7.040051	337.807158	9.174272
6.925007	347.285631	9.179290
7.120022	345.317670	9.184307
6.704601	358.421409	9.189325
7.040218	355.431217	9.194343
7.584400	353.774945	9.199360
7.330970	348.512894	9.204378
6.987651	336.240394	9.209395
6.703185	330.860110	9.214413
6.753046	332.389104	9.219431
7.041574	334.669847	9.224448
7.152095	340.973340	9.229466
7.441524	349.360101	9.234483
7.006276	338.430437	9.239501
6.839756	335.240733	9.244519
6.688150	331.502784	9.249536
6.942501	344.006797	9.254554
6.959541	348.343107	9.259571
6.956656	357.053081	9.264589
6.818526	348.589038	9.269607
7.191957	342.850713	9.274624
7.100924	362.224690	9.279642
6.955533	358.665638	9.284659
7.159601	354.190689	9.289677
7.348554	349.172168	9.294695
7.414073	353.365240	9.299712
7.132729	356.700338	9.304730
7.300792	350.075694	9.309747
7.264317	353.729253	9.314765
7.345535	363.284469	9.319783
7.446825	348.512894	9.324800
7.054059	345.585620	9.329818
6.903015	339.225247	9.334835
7.037377	343.795741	9.339853
7.189611	352.800280	9.344871
7.350740	348.076411	9.349888
6.780238	356.322524	9.354906
7.001851	354.372509	9.359923
7.418843	352.982180	9.364941
7.040329	357.029803	9.369959
7.093240	353.099069	9.374976
7.426746	358.392758	9.379994
7.019665	354.817650	9.385011
7.020634	354.751193	9.390029
6.878855	359.355218	9.395047
6.908092	348.914932	9.400064
7.089195	351.259737	9.405082
6.957789	354.353751	9.410099
7.210084	359.429723	9.415117
7.237009	368.573695	9.420135
7.573663	357.741575	9.425152
7.155766	359.340244	9.430170
7.309286	353.591975	9.435187
7.186111	353.686851	9.440205
7.270831	368.419928	9.445223
7.558031	368.230015	9.450240
7.339654	364.884287	9.455258
7.517266	354.550277	9.460275
7.176198	355.086155	9.465293
7.094573	355.004158	9.470311
7.404230	362.901808	9.475328
7.200782	366.032286	9.480346
7.377839	369.845096	9.485363
7.786722	368.859950	9.490381
7.426899	368.007111	9.495399
7.338088	352.163813	9.500416
7.473006	359.467007	9.505434
7.270104	360.009774	9.510451
7.420805	365.669581	9.515469
7.585633	376.628669	9.520487
7.503719	363.233065	9.525504
7.357092	353.596445	9.530522
7.357804	347.632142	9.535539
7.676620	358.157010	9.540557
7.497325	358.715035	9.545575
7.539967	349.891505	9.550592
7.081936	349.262229	9.555610
7.102995	363.727518	9.560627
7.467315	369.158417	9.565645
7.507446	380.316793	9.570663
7.398128	370.649110	9.575680
7.440763	385.562314	9.580698
7.620737	376.061014	9.585715
7.858343	377.175792	9.590733
7.610933	376.971291	9.595751
7.621338	375.985073	9.600768
7.288786	376.159883	9.605786
7.299260	375.034806	9.610803
7.267736	374.342280	9.615821
7.409232	374.263411	9.620839
8.034799	371.622528	9.625856
7.582368	374.965333	9.630874
7.439377	377.931773	9.635891
7.527003	372.534567	9.640909
7.165728	381.000567	9.645927
7.678602	374.423208	9.650944
7.694097	371.593303	9.655962
7.572164	382.025871	9.660979
7.562313	380.944982	9.665997
7.564203	373.266972	9.671015
7.753359	373.613005	9.676032
7.561944	372.980085	9.681050
7.619028	385.921919	9.686067
7.625363	364.651867	9.691085
7.414060	370.667824	9.696103
7.314188	376.303534	9.701120
7.591665	377.393171	9.706138
7.338576	373.800394	9.711155
7.432815	378.686397	9.716173
7.900930	400.292756	9.721191
7.992918	389.164212	9.726208
8.025134	383.879766	9.731226
7.746519	379.404226	9.736243
7.443286	376.507186	9.741261
7.412862	383.659418	9.746279
7.439670	384.062285	9.751296
7.904359	397.773755	9.756314
7.906166	397.741879	9.761331
8.056385	391.542855	9.766349
7.688322	387.507252	9.771367
7.659516	377.959567	9.776384
7.668706	379.403383	9.781402
7.890614	393.749066	9.786419
7.814200	372.558157	9.791437
7.342524	386.822484	9.796455
7.944985	400.260054	9.801472
8.148980	409.613152	9.806490
7.898369	404.694610	9.811507
8.143151	392.529312	9.816525
8.023257	379.862252	9.821543
7.954742	381.128828	9.826560
7.870824	380.501261	9.831578
7.759123	378.805101	9.836595
7.738345	375.428606	9.841613
7.402620	382.161335	9.846631
7.580735	389.202209	9.851648
8.093519	396.699038	9.856666
8.004312	392.758866	9.861683
8.175536	397.339412	9.866701
7.670503	387.913203	9.871719
7.370798	386.508232	9.876736
8.034026	389.759383	9.881754
7.598829	397.318607	9.886771
8.135998	401.996805	9.891789
8.227833	401.644815	9.896807
8.394768	404.332643	9.901824
8.311149	393.275617	9.906842
7.898238	388.533821	9.911859
7.917277	375.195070	9.916877
7.693232	376.773025	9.921895
7.780353	394.184890	9.926912
8.558499	402.268379	9.931930
8.194071	399.295661	9.936947
7.853276	382.399714	9.941965
7.775650	380.944389	9.946983
7.603870	395.966720	9.952000
7.768676	400.557734	9.957018
7.640453	406.901578	9.962035
8.396617	401.027908	9.967053
8.005248	395.089921	9.972071
7.968058	400.813705	9.977088
8.145436	399.498547	9.982106
7.895421	401.509715	9.987123
8.106816	400.763589	9.992141
8.130811	397.389585	9.997159
7.882646	399.548780	10.002176
8.150935	402.347054	10.007194
7.826298	409.983738	10.012211
7.999947	394.112161	10.017229
7.998899	404.491208	10.022247
8.227036	408.516969	10.027264
7.913624	407.167777	10.032282
8.104249	413.338909	10.037299
8.210253	401.321439	10.042317
8.321026	408.830374	10.047335
7.668659	406.833401	10.052352
8.034598	408.600353	10.057370
8.176343	423.624384	10.062387
8.637450	421.422490	10.067405
8.412165	422.060258	10.072423
8.371134	413.240256	10.077440
8.173012	404.006083	10.082458
7.844584	405.546646	10.087475
8.068023	409.137660	10.092493
8.303319	424.491091	10.097511
8.309989	430.974879	10.102528
8.229630	429.643046	10.107546
8.200406	438.454985	10.112563
8.385669	424.361361	10.117581
8.428657	432.369986	10.122599
8.164805	421.877465	10.127616
8.469434	431.713498	10.132634
8.196735	425.662355	10.137651
8.288167	422.912133	10.142669
8.381678	411.944276	10.147687
8.624719	422.708188	10.152704
8.695483	411.283148	10.157722
8.013478	418.764048	10.162739
8.383089	410.410262	10.167757
8.497039	410.496620	10.172775
8.272314	415.571142	10.177792
8.448276	404.050837	10.182810
7.838965	416.174999	10.187827
8.422455	418.403517	10.192845
8.486984	431.416805	10.197863
8.341838	432.707939	10.202880
8.281085	433.623033	10.207898
8.774985	439.355654	10.212915
8.684038	431.628961	10.217933
8.232463	417.012832	10.222951
8.137321	422.805603	10.227968
8.512571	424.975031	10.232986
8.245760	431.725450	10.238003
8.633769	442.144926	10.243021
8.686830	429.794868	10.248039
8.494342	431.945399	10.253056
8.764983	433.247532	10.258074
8.577299	429.638249	10.263091
8.679698	421.196680	10.268109
8.594996	410.382797	10.273127
7.995987	413.656917	10.278144
8.047618	414.636559	10.283162
8.105336	417.549667	10.288179
8.414890	420.742286	10.293197
8.687448	431.672012	10.298215
8.436628	426.744030	10.303232
8.730954	424.060043	10.308250
8.654812	432.459583	10.313267
8.892446	417.493161	10.318285
8.728712	419.841175	10.323303
8.607856	421.065413	10.328320
9.113833	419.743271	10.333338
8.792967	427.742276	10.338355
8.541007	417.828545	10.343373
8.955161	428.960275	10.348391
8.527797	424.908652	10.353408
8.733416	425.457240	10.358426
8.724959	424.581248	10.363443
8.594639	413.316897	10.368461
8.636014	421.988455	10.373479
8.333100	428.066029	10.378496
8.753718	423.065065	10.383514
8.595785	421.290896	10.388531
8.578308	424.133665	10.393549
8.970179	425.334876	10.398567
8.770747	433.251863	10.403584
8.425253	426.820753	10.408602
8.317626	430.441227	10.413619
8.434284	428.103623	10.418637
8.717052	426.308173	10.423655
8.297271	429.532301	10.428672
8.621395	429.017918	10.433690
8.442034	422.441029	10.438707
8.330357	441.427005	10.443725
8.934123	444.993523	10.448743
8.289234	448.341061	10.453760
9.333136	441.905051	10.458778
8.980675	452.824811	10.463795
8.821043	454.875559	10.468813
8.947995	453.751276	10.473831
8.658653	453.843623	10.478848
9.351436	444.584321	10.483866
8.973416	443.787958	10.488883
8.737918	430.441461	10.493901
9.080773	426.020621	10.498919
8.726835	429.849850	10.503936
8.772818	438.066284	10.508954
9.293951	447.467849	10.513971
8.875602	435.216430	10.518989
8.649844	429.104331	10.524007
8.841742	444.701211	10.529024
9.129602	446.401432	10.534042
8.987174	439.048806	10.539059
8.960745	437.784311	10.544077
9.040546	440.558291	10.549095
9.087723	448.310663	10.554112
8.718709	437.197064	10.559130
8.813648	437.478876	10.564147
9.024704	450.661859	10.569165
9.180872	453.512310	10.574183
9.078546	452.726667	10.579200
9.345499	452.429459	10.584218
8.974290	443.140166	10.589235
8.859048	435.060665	10.594253
9.010528	436.387662	10.599271
8.887911	444.766043	10.604288
8.830386	450.552966	10.609306
8.714189	451.224241	10.614323
8.768758	450.818095	10.619341
9.084664	443.444597	10.624359
8.766029	448.476949	10.629376
8.858523	451.510874	10.634394
8.454123	447.910084	10.639411
8.855187	455.941860	10.644429
9.294110	464.557853	10.649447
9.321604	469.359603	10.654464
9.542576	464.850438	10.659482
9.227134	454.520557	10.664499
9.040184	447.944839	10.669517
9.211827	444.850781	10.674535
8.939154	462.896217	10.679552
9.124247	461.967999	10.684570
9.417630	476.987399	10.689587
9.166884	462.078045	10.694605
9.321744	448.737026	10.699623
8.923999	445.715841	10.704640
9.260831	462.530343	10.709658
9.347474	471.923834	10.714675
9.411139	470.424413	10.719693
9.765412	462.404335	10.724711
9.167651	455.693770	10.729728
9.282258	453.612090	10.734746
9.106250	453.579499	10.739763
9.255430	449.674778	10.744781
9.174267	447.809762	10.749799
9.494368	454.916914	10.754816
9.322195	456.830766	10.759834
9.149517	454.197396	10.764851
9.497120	464.004666	10.769869
9.404194	458.951111	10.774887
9.106112	456.646520	10.779904
9.430730	462.411817	10.784922
9.461021	465.253467	10.789939
9.191982	467.908203	10.794957
9.427205	470.803150	10.799975
9.489783	479.812246	10.804992
9.420707	472.154709	10.810010
9.638412	478.454186	10.815027
9.493452	473.601223	10.820045
9.459914	449.793815	10.825063
9.348949	452.821550	10.830080
9.480718	457.023265	10.835098
9.638933	458.986658	10.840115
9.374173	466.547776	10.845133
9.416368	453.060201	10.850151
9.460110	471.103715	10.855168
9.382275	474.552310	10.860186
9.890720	472.144233	10.865203
9.100592	468.890660	10.870221
9.923132	471.334419	10.875239
9.637102	471.423094	10.880256
9.389944	459.810848	10.885274
9.652799	463.222174	10.890291
9.621647	467.127381	10.895309
9.464174	449.899884	10.900327
9.518928	482.464028	10.905344
9.447769	475.766135	10.910362
9.524663	476.233786	10.915379
9.632750	486.766296	10.920397
9.959526	471.334690	10.925415
9.842136	478.661439	10.930432
9.550769	467.627245	10.935450
9.640154	463.201681	10.940467
9.571417	469.612021	10.945485
9.607183	464.068234	10.950503
9.815448	465.525241	10.955520
9.594189	473.710720	10.960538
9.766131	467.880655	10.965555
9.776699	463.577810	10.970573
9.765100	463.213522	10.975591
9.832360	471.622310	10.980608
9.502388	458.719671	10.985626
9.812958	465.440165	10.990643
9.459372	475.615379	10.995661
9.785747	477.442144	11.000679
9.566886	483.181617	11.005696
9.702739	478.789838	11.010714
10.137713	470.728790	11.015731
9.650415	484.380274	11.020749
9.685270	468.262009	11.025767
9.634144	478.563694	11.030784
9.446363	478.993662	11.035802
10.103109	482.826481	11.040819
9.283990	483.480973	11.045837
9.546131	472.076588	11.050855
9.525881	476.406113	11.055872
9.365051	477.220032	11.060890
9.557383	473.781936	11.065907
9.266850	495.916766	11.070925
9.804587	493.270606	11.075943
10.168204	501.614333	11.080960
9.928440	503.421953	11.085978
10.135775	494.556931	11.090995
10.030271	495.639934	11.096013
10.171921	487.987450	11.101031
10.100142	501.552163	11.106048
9.861442	508.285612	11.111066
10.059227	499.926980	11.116083
9.916422	501.022103	11.121101
9.986632	494.980660	11.126119
10.150131	493.427825	11.131136
9.817483	498.913633	11.136154
9.984441	494.718969	11.141171
10.015743	502.164581	11.146189
10.045549	500.417976	11.151207
10.094197	499.245925	11.156224
10.349753	504.861049	11.161242
10.363717	499.749817	11.166259
9.985012	498.180419	11.171277
10.403413	489.071108	11.176295
9.688073	474.514933	11.181312
9.733421	482.933449	11.186330
9.913271	495.483880	11.191347
9.903489	505.378374	11.196365
10.448954	502.241882	11.201383
10.133898	497.118764	11.206400
10.461776	498.506660	11.211418
10.134687	498.002152	11.216435
9.904985	494.434111	11.221453
10.016476	496.234377	11.226471
10.034367	498.229089	11.231488
10.037907	504.561920	11.236506
10.353832	492.025731	11.241523
10.034967	490.462796	11.246541
9.832982	493.653026	11.251559
9.802856	494.651713	11.256576
9.768230	502.514671	11.261594
10.551406	498.416559	11.266611
10.268353	500.672712	11.271629
10.235516	497.263359	11.276647
10.439775	489.421253	11.281664
10.116587	495.006567	11.286682
10.398010	495.265657	11.291699
10.512290	498.971511	11.296717
10.370278	494.632457	11.301735
10.367909	500.385563	11.306752
10.384266	505.236392	11.311770
10.376190	498.254126	11.316787
10.302616	494.888984	11.321805
10.198940	489.963320	11.326823
10.481535	497.925202	11.331840
10.030118	497.518943	11.336858
10.273039	505.534340	11.341875
10.720693	510.586250	11.346893
10.354056	512.451494	11.351911
10.781497	507.064453	11.356928
10.234571	509.598366	11.361946
10.125634	504.294838	11.366963
10.476271	521.075689	11.371981
10.663417	528.866261	11.376999
10.978712	521.439180	11.382016
10.571953	512.073339	11.387034
10.291530	502.870862	11.392051
10.505107	501.613174	11.397069
10.103030	506.182028	11.402087
10.496393	523.641009	11.407104
10.313282	528.620726	11.412122
10.691409	520.341299	11.417139
10.619195	523.233630	11.422157
10.413544	528.412508	11.427175
10.359740	528.679613	11.432192
10.575518	526.866182	11.437210
10.308404	522.249966	11.442227
10.271789	528.532255	11.447245
10.413997	517.629332	11.452263
10.620371	519.449540	11.457280
10.860114	520.147446	11.462298
10.638947	519.168874	11.467315
10.795684	517.677048	11.472333
10.610133	526.254606	11.477351
10.957726	530.530028	11.482368
10.841222	531.810398	11.487386
10.845082	525.321703	11.492403
10.699996	526.915778	11.497421
10.777644	524.593702	11.502439
10.874901	524.515409	11.507456
10.350839	522.141855	11.512474
10.907831	520.530909	11.517491
10.812346	520.381644	11.522509
10.240893	518.753896	11.527527
10.735468	507.543663	11.532544
10.511218	524.701191	11.537562
11.059778	515.590535	11.542579
10.962455	520.399109	11.547597
10.645981	515.547594	11.552615
10.671051	514.297165	11.557632
10.470140	522.605725	11.562650
10.680998	514.175626	11.567667
10.476953	519.133355	11.572685
10.465988	537.807121	11.577703
11.105526	532.251355	11.582720
10.620426	542.570154	11.587738
10.986658	542.696125	11.592755
11.155778	547.428510	11.597773
11.178237	549.905335	11.602791
11.191377	551.998619	11.607808
10.624784	535.519520	11.612826
11.155787	535.234844	11.617843
10.655036	540.951956	11.622861
10.695584	551.277278	11.627879
11.211665	544.932878	11.632896
11.064537	543.343199	11.637914
10.895263	535.609721	11.642931
11.391671	551.727305	11.647949
11.270165	542.067737	11.652967
11.087350	537.476260	11.657984
10.902983	536.419378	11.663002
10.820473	535.965147	11.668019
10.885161	543.960977	11.673037
11.458463	544.143067	11.678055
11.398615	543.887271	11.683072
11.156851	545.846680	11.688090
10.994044	526.887475	11.693107
10.968048	526.680056	11.698125
11.111336	543.751977	11.703143
10.948294	537.443891	11.708160
10.854817	551.018332	11.713178
11.131976	537.153298	11.718195
11.405007	546.505185	11.723213
10.969329	546.033361	11.728231
11.144718	548.486375	11.733248
10.566571	552.978518	11.738266
11.026365	553.200370	11.743283
11.218366	544.871019	11.748301
10.901544	549.691687	11.753319
11.128762	540.173477	11.758336
11.046387	545.648733	11.763354
11.095803	536.956594	11.768371
11.422061	555.265462	11.773389
11.086374	555.923579	11.778407
11.179780	563.334302	11.783424
11.276010	568.516681	11.788442
11.233320	573.698601	11.793459
11.261596	570.525861	11.798477
11.100893	570.440396	11.803495
11.436197	562.962847	11.808512
11.772343	569.190268	11.813530
11.818002	565.661387	11.818547
11.674680	562.231355	11.823565
11.153548	545.016208	11.828583
11.194050	541.756366	11.833600
11.199859	560.863028	11.838618
11.734343	561.527668	11.843635
11.802468	562.864498	11.848653
11.595225	553.057334	11.853671
11.232404	545.148867	11.858688
11.494320	546.168356	11.863706
11.436914	546.802080	11.868723
11.597940	533.100292	11.873741
10.982807	545.092909	11.878759
11.417489	564.763935	11.883776
11.440560	563.879872	11.888794
11.515458	564.492997	11.893811
11.624124	561.045822	11.898829
11.445488	571.821831	11.903847
12.028095	564.296310	11.908864
11.400181	572.781824	11.913882
11.653014	566.535206	11.918899
11.679290	570.141172	11.923917
11.658894	567.282111	11.928935
12.054815	558.258312	11.933952
11.316102	557.732687	11.938970
11.522145	552.951280	11.943987
12.169599	557.432476	11.949005
11.918510	557.522023	11.954023
12.017829	548.190973	11.959040
11.615694	540.045643	11.964058
11.688832	545.032803	11.969075
11.716171	534.545368	11.974093
11.243040	544.433134	11.979111
11.695654	543.415925	11.984128
11.625048	566.172979	11.989146
11.984903	558.110966	11.994163
12.255615	562.701311	11.999181
11.649351	558.232560	12.004199
11.627701	546.768175	12.009216
11.339307	557.138404	12.014234
11.838824	562.551468	12.019251
11.955836	566.136994	12.024269
12.087078	578.022893	12.029287
12.170365	568.056882	12.034304
12.078025	559.478317	12.039322
11.536080	551.402084	12.044339
11.643793	547.724696	12.049357
11.791887	571.214535	12.054375
11.821096	562.115291	12.059392
11.983830	565.302394	12.064410
11.728269	577.327408	12.069427
12.141715	569.159220	12.074445
11.618323	573.775380	12.079463
11.933619	571.264824	12.084480
12.246650	568.369629	12.089498
12.046600	570.679137	12.094515
12.031417	566.582240	12.099533
11.310811	573.444391	12.104551
11.984134	568.501867	12.109568
12.059425	570.894733	12.114586
11.744921	566.159657	12.119603
12.160244	560.222243	12.124621
11.964179	569.520953	12.129639
11.844151	563.957212	12.134656
11.842961	567.782039	12.139674
11.761086	565.415370	12.144691
11.767915	566.026470	12.149709
12.066514	584.513238	12.154727
12.026618	593.083928	12.159744
12.208646	603.421964	12.164762
12.104350	602.724981	12.169779
12.385936	585.993860	12.174797
12.605807	590.961343	12.179815
12.480651	594.369993	12.184832
12.241357	576.852167	12.189850
12.336927	573.523789	12.194867
12.244749	566.971139	12.199885
12.118780	570.938467	12.204903
12.188777	570.454179	12.209920
12.432712	560.418981	12.214938
12.637486	571.643358	12.219955
12.338368	568.193402	12.224973
12.239024	569.988634	12.229991
12.249659	567.260436	12.235008
12.046705	567.683302	12.240026
12.209695	575.487122	12.245043
12.336349	565.773126	12.250061
11.845977	577.654826	12.255079
12.498326	579.828464	12.260096
12.597464	593.729540	12.265114
12.648124	598.363622	12.270131
12.634762	580.794837	12.275149
12.317808	575.615190	12.280167
12.601555	564.608153	12.285184
12.473370	566.594059	12.290202
12.646100	573.086757	12.295219
12.254139	565.107082	12.300237
12.511933	566.253442	12.305255
12.524720	559.649740	12.310272
12.018937	558.324176	12.315290
12.143961	576.235226	12.320307
12.386404	586.068404	12.325325
12.482226	587.366211	12.330343
12.199686	589.871594	12.335360
12.621799	586.385079	12.340378
12.492192	595.490425	12.345395
12.588067	594.329948	12.350413
12.221133	604.261170	12.355431
12.511965	586.992142	12.360448
12.558146	600.585900	12.365466
12.547547	597.154131	12.370483
12.450597	594.802427	12.375501
12.232198	591.917389	12.380519
12.631083	594.707982	12.385536
13.038365	592.886819	12.390554
12.649250	593.319735	12.395571
12.769133	588.173052	12.400589
12.314654	589.603873	12.405607
12.552378	593.915351	12.410624
12.362223	602.935458	12.415642
12.494955	608.206835	12.420659
13.192571	605.128684	12.425677
12.958752	613.846337	12.430695
12.761065	614.205270	12.435712
13.200951	602.959313	12.440730
12.561958	604.529313	12.445747
12.747698	601.458278	12.450765
12.591264	622.325891	12.455783
12.896075	614.288201	12.460800
12.984139	612.507269	12.465818
13.058334	619.015325	12.470835
13.225394	603.722077	12.475853
12.640599	609.742619	12.480871
12.870142	609.684753	12.485888
12.882161	607.180387	12.490906
12.474261	611.415672	12.495923
12.726244	608.583622	12.500941
12.913383	613.401579	12.505959
12.862895	616.653446	12.510976
13.267338	616.877606	12.515994
13.164682	615.893200	12.521011
13.336306	606.860119	12.526029
13.067573	621.288688	12.531047
13.171989	606.039904	12.536064
13.088911	612.919570	12.541082
13.165950	610.960481	12.546099
13.196735	606.831172	12.551117
13.039429	616.619313	12.556135
13.135311	621.003373	12.561152
12.938862	609.695546	12.566170
12.967077	615.620647	12.571187
13.349872	618.107648	12.576205
12.976265	611.248519	12.581223
12.738592	616.132618	12.586240
12.814634	619.588839	12.591258
12.886310	615.106036	12.596275
13.115382	606.587855	12.601293
13.097145	607.531050	12.606311
12.887144	610.290220	12.611328
13.179118	605.485953	12.616346
12.896672	624.258880	12.621363
12.897569	620.916832	12.626381
13.404912	633.769808	12.631399
13.204856	637.796021	12.636416
13.404547	636.534174	12.641434
13.646714	632.176295	12.646451
13.409092	632.468865	12.651469
13.439404	625.010375	12.656487
13.364499	620.032860	12.661504
13.483950	609.979147	12.666522
13.262853	617.615578	12.671539
13.484082	619.868968	12.676557
13.487299	618.726072	12.681575
13.355852	620.182337	12.686592
13.850356	607.848629	12.691610
13.448188	616.005537	12.696627
13.523287	607.883699	12.701645
13.320266	613.137928	12.706663
13.194062	615.221358	12.711680
13.444851	608.365996	12.716698
13.852350	636.678442	12.721715
13.391212	623.852908	12.726733
13.396625	618.316954	12.731751
13.458525	617.572005	12.736768
13.665415	631.831860	12.741786
13.463883	634.536068	12.746803
13.469818	629.239863	12.751821
14.002297	632.432524	12.756839
14.022143	627.525459	12.761856
13.608785	614.888144	12.766874
13.561991	617.375760	12.771891
13.210020	609.560246	12.776909
13.707664	627.921398	12.781927
13.452431	641.423266	12.786944
13.828558	639.509122	12.791962
13.548766	641.215695	12.796979
13.888272	629.404703	12.801997
14.159684	628.538774	12.807015
13.744063	620.212477	12.812032
13.782724	615.078431	12.817050
13.515275	610.266592	12.822067
13.391760	614.880462	12.827085
13.897628	624.275031	12.832103
13.663964	630.543856	12.837120
13.817473	627.178046	12.842138
13.709104	634.841112	12.847155
13.677569	627.329137	12.852173
14.045420	635.770093	12.857191
13.980076	631.545297	12.862208
13.861448	641.343208	12.867226
13.650677	633.672951	12.872243
13.846772	636.823316	12.877261
14.172726	648.697880	12.882279
13.851587	637.775510	12.887296
13.831456	632.249841	12.892314
13.522393	634.579486	12.897331
13.679277	633.011891	12.902349
13.566166	637.977584	12.907367
13.822085	639.029569	12.912384
13.663702	634.298569	12.917402
13.878087	644.256064	12.922419
14.323557	660.318563	12.927437
14.502970	654.304244	12.932455
14.295497	639.608902	12.937472
14.185395	629.789727	12.942490
13.775908	637.193575	12.947507
13.905940	632.480784	12.952525
14.214163	634.935218	12.957543
14.213278	630.454242	12.962560
14.072648	626.124408	12.967578
14.117180	636.392356	12.972595
13.977891	644.126510	12.977613
14.185144	652.106503	12.982631
14.046606	653.636456	12.987648
14.546821	652.113230	12.992666
14.324376	662.444851	12.997683
14.150237	653.746437	13.002701
14.431186	650.906714	13.007719
14.225902	663.463581	13.012736
14.247865	655.605605	13.017754
13.996079	658.150390	13.022771
14.421298	658.292423	13.027789
14.395539	659.318841	13.032807
14.100260	663.145297	13.037824
14.387759	658.745642	13.042842
14.532243	661.676837	13.047859
14.111627	657.996481	13.052877
14.571812	660.446193	13.057895
14.138007	661.129057	13.062912
14.374398	657.851319	13.067930
14.164980	664.570800	13.072947
14.131066	660.322169	13.077965
14.484121	658.174938	13.082983
14.116690	673.581403	13.088000
14.271833	647.926673	13.093018
14.388372	669.345110	13.098035
14.098955	654.182849	13.103053
14.518589	666.348942	13.108071
14.469446	683.154322	13.113088
14.891363	682.848761	13.118106
15.170036	682.638084	13.123123
14.949403	667.543994	13.128141
14.852685	652.970247	13.133159
14.199773	654.154268	13.138176
14.604796	656.432694	13.143194
14.336661	658.547694	13.148211
14.428529	662.197112	13.153229
14.915018	656.923905	13.158247
14.524106	667.354339	13.163264
14.781524	658.572952	13.168282
14.904681	655.000430	13.173299
14.467110	658.940555	13.178317
14.619766	660.273698	13.183335
14.753256	673.011347	13.188352
15.082790	683.285440	13.193370
14.707839	676.540100	13.198387
14.731360	681.809569	13.203405
14.928999	673.113219	13.208423
14.770641	682.223086	13.213440
15.159488	674.109171	13.218458
14.839948	662.552241	13.223475
15.063576	655.735802	13.228493
15.229337	648.385597	13.233511
14.783303	654.930484	13.238528
14.729347	654.430781	13.243546
14.570390	658.542114	13.248563
14.686172	674.848454	13.253581
15.256328	673.651997	13.258599
15.185160	682.997589	13.263616
15.403662	671.688231	13.268634
15.274756	664.639509	13.273651
14.848169	664.775314	13.278669
14.644035	659.215172	13.283687
14.655874	666.263110	13.288704
15.133928	678.713595	13.293722
15.111439	677.047696	13.298739
15.147936	686.928774	13.303757
15.248230	684.628396	13.308775
15.190111	682.835505	13.313792
15.086906	675.467207	13.318810
15.170273	678.168088	13.323827
15.056070	681.679188	13.328845
15.225134	676.060934	13.333863
15.023858	677.180950	13.338880
15.173812	681.995248	13.343898
15.115704	682.319827	13.348915
14.887170	690.080519	13.353933
15.001222	681.637012	13.358951
14.965173	688.282175	13.363968
15.089679	683.936291	13.368986
15.021228	687.206747	13.374003
15.005881	686.644229	13.379021
15.369453	683.558116	13.384039
15.314018	681.742717	13.389056
15.282494	692.161389	13.394074
15.546656	690.839010	13.399091
15.024269	685.303164	13.404109
15.640047	690.537226	13.409127
15.717631	704.590061	13.414144
15.425667	689.387143	13.419162
15.418561	690.508484	13.424179
15.301043	688.469229	13.429197
15.505364	691.201771	13.434215
15.500481	692.152359	13.439232
15.952254	701.388140	13.444250
15.709477	698.734090	13.449267
15.427182	693.687862	13.454285
15.472619	683.550961	13.459303
15.476933	685.557275	13.464320
15.426956	679.878453	13.469338
15.649454	690.071389	13.474355
15.420400	684.764418	13.479373
16.096640	692.185432	13.484391
15.640005	699.836480	13.489408
15.204556	681.575945	13.494426
15.414400	690.360255	13.499443
15.510056	701.396583	13.504461
15.734741	703.794608	13.509479
15.628233	698.544290	13.514496
15.841305	707.283925	13.519514
16.022597	699.865011	13.524531
15.803373	699.905417	13.529549
16.012372	703.539763	13.534567
15.978467	710.386565	13.539584
15.691903	702.548203	13.544602
15.573891	694.443769	13.549619
15.479710	705.572770	13.554637
15.604171	694.906023	13.559655
15.431552	702.187815	13.564672
16.016649	697.615587	13.569690
16.137760	703.482074	13.574707
15.679150	711.234417	13.579725
15.791500	699.783783	13.584743
15.896582	701.159049	13.589760
15.529293	702.598393	13.594778
16.150492	703.618756	13.599795
15.691728	707.407562	13.604813
16.035445	695.087803	13.609831
16.289762	703.199342	13.614848
16.286666	705.064806	13.619866
16.148489	700.100276	13.624883
15.777596	697.844857	13.629901
16.246653	707.778515	13.634919
16.154086	697.940794	13.639936
15.912669	699.619308	13.644954
16.017917	700.022592	13.649971
16.116530	702.153077	13.654989
16.150526	695.022177	13.660007
16.187990	700.617673	13.665024
16.198976	699.965851	13.670042
16.067856	698.200103	13.675059
16.089379	705.114009	13.680077
16.420784	711.010870	13.685095
16.393419	719.522868	13.690112
15.967944	700.973591	13.695130
16.414326	709.878867	13.700147
16.110897	719.740307	13.705165
16.526307	714.288807	13.710183
16.434499	713.192257	13.715200
16.571204	713.303475	13.720218
16.782672	703.027106	13.725235
16.410352	702.554880	13.730253
16.497051	697.309193	13.735271
16.277522	700.950301	13.740288
16.135032	703.970364	13.745306
16.220434	691.700293	13.750323
16.214099	712.225916	13.755341
16.316983	707.312211	13.760359
16.395454	721.301808	13.765376
16.535880	730.213706	13.770394
16.603067	730.436730	13.775411
16.699836	731.769113	13.780429
16.785612	719.820846	13.785447
16.457186	730.304702	13.790464
16.304130	725.601249	13.795482
16.362810	720.397787	13.800499
16.498288	725.741353	13.805517
16.555677	724.829849	13.810535
16.589234	729.050075	13.815552
16.501478	727.113476	13.820570
16.712802	723.536680	13.825587
16.369111	722.233201	13.830605
16.468447	714.369464	13.835623
16.763958	720.240360	13.840640
16.615757	724.637203	13.845658
16.785567	726.504149	13.850675
16.746131	717.267196	13.855693
16.632479	724.593463	13.860711
16.626802	714.521304	13.865728
16.648903	733.104923	13.870746
17.043733	731.841089	13.875763
16.598664	730.247290	13.880781
17.123049	743.233388	13.885799
17.045881	738.716926	13.890816
16.791448	739.924114	13.895834
16.719767	729.562432	13.900851
17.094815	735.162181	13.905869
16.875239	744.237431	13.910887
17.669926	746.887532	13.915904
16.987221	734.326780	13.920922
17.085998	724.377205	13.925939
16.845093	729.517449	13.930957
16.859998	714.402426	13.935975
17.113891	708.616326	13.940992
17.019577	716.589653	13.946010
17.207789	712.858673	13.951027
17.201127	725.917973	13.956045
17.076412	714.545264	13.961063
17.164562	726.062443	13.966080
16.946461	730.050461	13.971098
17.333014	727.389938	13.976115
17.407422	731.979334	13.981133
17.198982	725.836035	13.986151
17.092013	722.573876	13.991168
17.145733	739.899765	13.996186
17.470182	742.399023	14.001203
17.239095	734.315332	14.006221
17.191843	740.709802	14.011239
17.394879	743.452019	14.016256
17.470615	746.453891	14.021274
17.383487	743.690396	14.026291
17.245349	744.630177	14.031309
17.578438	748.658610	14.036327
17.391352	740.628024	14.041344
17.290090	744.118186	14.046362
17.355941	742.526887	14.051379
17.810718	748.754836	14.056397
17.253034	741.346821	14.061415
17.635265	741.773251	14.066432
17.227620	749.110589	14.071450
17.507263	745.043485	14.076467
17.106202	750.114000	14.081485
17.477033	740.854182	14.086503
17.589644	743.629412	14.091520
17.431573	743.612962	14.096538
17.351473	749.662265	14.101555
17.711590	749.647183	14.106573
17.447285	745.803620	14.111591
17.852663	751.445988	14.116608
17.463588	755.839317	14.121626
17.310956	748.365079	14.126643
17.414904	748.803280	14.131661
16.991535	740.569648	14.136679
17.678909	752.236536	14.141696
17.580550	765.095554	14.146714
18.018142	762.947771	14.151731
18.177740	760.877985	14.156749
17.674100	751.388250	14.161767
17.776676	750.510733	14.166784
18.082548	762.808210	14.171802
17.968385	750.209420	14.176819
18.221447	747.796889	14.181837
18.119371	745.004164	14.186855
17.792198	735.878270	14.191872
17.706999	743.149624	14.196890
18.101436	739.042558	14.201907
18.131458	748.195710	14.206925
17.891282	746.532140	14.211943
18.158572	734.684986	14.216960
18.006296	751.077313	14.221978
18.065228	736.394059	14.226995
17.945886	751.676761	14.232013
17.728927	744.831059	14.237031
18.035582	735.044765	14.242048
17.860166	750.266771	14.247066
18.234333	752.076657	14.252083
18.326775	736.201640	14.257101
17.920647	739.862340	14.262119
18.065323	745.191857	14.267136
17.807618	752.941340	14.272154
18.094260	760.953201	14.277171
18.181067	761.050098	14.282189
18.412619	758.057108	14.287207
18.420478	773.705021	14.292224
17.994104	770.621967	14.297242
18.003050	763.580144	14.302259
18.480260	772.606880	14.307277
18.349958	769.629204	14.312295
18.232257	765.813302	14.317312
18.326386	771.144385	14.322330
17.967347	766.760162	14.327347
18.142160	777.219340	14.332365
18.239213	767.509843	14.337383
18.448842	762.197662	14.342400
18.231028	761.975925	14.347418
18.375452	756.484555	14.352435
18.405430	757.817872	14.357453
18.258418	769.235996	14.362471
18.418412	772.571882	14.367488
18.220388	783.852796	14.372506
18.504681	782.883871	14.377523
18.833981	791.715902	14.382541
18.579259	778.321645	14.387559
18.830398	795.572671	14.392576
18.672549	800.453859	14.397594
18.696405	795.650261	14.402611
18.893460	788.983072	14.407629
18.969688	791.003447	14.412647
19.221895	775.343355	14.417664
18.909756	772.479193	14.422682
19.061486	753.230941	14.427699
18.893847	748.409835	14.432717
18.737775	761.277836	14.437735
18.889320	750.947655	14.442752
18.446424	759.533835	14.447770
18.802566	761.062515	14.452787
18.983983	750.405801	14.457805
18.708561	752.976369	14.462823
18.699242	756.174516	14.467840
18.859838	755.953821	14.472858
18.812735	756.494432	14.477875
19.142142	748.869405	14.482893
18.708439	752.534402	14.487911
18.623675	757.435756	14.492928
18.788234	766.817272	14.497946
18.797980	772.707432	14.502963
19.321753	779.237065	14.507981
19.480407	776.703534	14.512999
19.533136	776.777335	14.518016
19.261486	767.955195	14.523034
19.157530	755.244362	14.528051
19.207431	756.271628	14.533069
18.654378	766.096222	14.538087
19.029656	761.196895	14.543104
19.081928	767.528543	14.548122
19.417681	763.670442	14.553139
19.138696	768.235976	14.558157
18.998661	775.746248	14.563175
19.108626	780.610979	14.568192
19.541269	776.826150	14.573210
19.560061	769.113780	14.578227
19.313150	762.963835	14.583245
19.151645	774.728193	14.588263
19.386395	777.096259	14.593280
19.162187	783.890670	14.598298
19.331066	784.845766	14.603315
19.436353	775.769281	14.608333
19.128059	788.512683	14.613351
19.585114	788.271076	14.618368
19.507203	790.580530	14.623386
19.258289	786.299073	14.628403
19.449141	776.650703	14.633421
19.450647	781.709041	14.638439
19.144745	774.706767	14.643456
18.939758	777.042316	14.648474
19.345682	775.401221	14.653491
19.700172	781.518567	14.658509
19.544831	777.746392	14.663527
19.357952	780.413628	14.668544
19.572416	788.944810	14.673562
19.775404	790.718237	14.678579
19.895880	801.706583	14.683597
19.454362	797.057491	14.688615
19.546697	792.726057	14.693632
19.845322	791.953710	14.698650
20.176617	793.378967	14.703667
20.107104	794.282820	14.708685
19.786816	792.111026	14.713703
19.766405	776.455510	14.718720
19.668513	784.744996	14.723738
19.982373	791.332562	14.728755
19.721822	790.659899	14.733773
19.789657	795.575374	14.738791
20.047024	801.868790	14.743808
19.887674	805.260715	14.748826
19.771617	800.507301	14.753843
19.918253	799.143253	14.758861
19.906016	807.536176	14.763879
20.133084	793.637717	14.768896
20.043587	805.867397	14.773914
20.283458	799.707920	14.778931
20.290323	793.834024	14.783949
20.191045	793.780018	14.788967
19.884330	806.567367	14.793984
20.120879	800.638774	14.799002
19.895970	801.352233	14.804019
20.181479	799.666770	14.809037
20.092639	793.056715	14.814055
19.975576	799.932277	14.819072
19.989415	803.193097	14.824090
19.937419	803.046525	14.829107
20.228754	792.700867	14.834125
20.019846	799.884211	14.839143
20.027791	796.979677	14.844160
20.618856	795.461229	14.849178
20.230381	800.141646	14.854195
20.197973	799.502888	14.859213
20.504726	800.856229	14.864231
20.459986	797.309819	14.869248
20.494079	805.802822	14.874266
20.430518	808.479264	14.879283
20.371821	805.490432	14.884301
20.508618	802.644728	14.889319
20.430250	805.654825	14.894336
20.435530	814.919158	14.899354
20.735458	819.236785	14.904371
20.869342	809.821323	14.909389
20.264724	806.494623	14.914407
20.416776	803.488758	14.919424
21.104726	819.160208	14.924442
20.860568	812.842564	14.929459
20.368211	803.000759	14.934477
20.474320	808.099621	14.939495
20.493086	818.390621	14.944512
20.872939	829.572123	14.949530
20.832002	835.091509	14.954547
20.940853	824.231460	14.959565
20.772330	832.503564	14.964583
21.061310	812.337653	14.969600
20.716977	809.093500	14.974618
20.570648	818.715946	14.979635
20.541666	825.760836	14.984653
20.726769	823.765964	14.989671
20.892076	829.089138	14.994688
21.039196	824.193760	14.999706
20.823306	825.675812	15.004723
20.917982	826.068122	15.009741
20.853494	824.828459	15.014759
20.919820	828.059022	15.019776
20.860999	827.881955	15.024794
20.610937	825.891722	15.029811
20.977130	816.945003	15.034829
20.853238	832.774422	15.039847
20.528329	821.890394	15.044864
21.116953	840.644689	15.049882
20.963061	844.660604	15.054899
21.311484	849.668104	15.059917
21.061682	848.652947	15.064935
21.250546	853.243488	15.069952
21.415592	849.686495	15.074970
21.600004	844.160471	15.079987
22.044603	844.261621	15.085005
21.351407	839.402400	15.090023
21.433964	830.903768	15.095040
21.110388	813.717558	15.100058
21.113512	818.318075	15.105075
21.510571	835.483306	15.110093
21.239627	836.358565	15.115111
21.085491	843.426103	15.120128
21.826194	848.707033	15.125146
21.526507	839.952337	15.130163
21.982393	837.571330	15.135181
21.648181	825.625268	15.140199
21.258389	818.613948	15.145216
21.406115	820.414917	15.150234
21.232935	837.145083	15.155251
21.591240	837.562618	15.160269
21.480576	843.821835	15.165287
21.455845	836.378137	15.170304
21.731556	828.218653	15.175322
21.375480	837.772782	15.180339
21.611134	838.553387	15.185357
21.598484	842.427394	15.190375
20.882623	849.557147	15.195392
21.359687	840.296516	15.200410
21.841968	854.589410	15.205427
21.515302	846.359607	15.210445
21.905945	856.267689	15.215463
21.959174	856.625428	15.220480
22.015689	862.808131	15.225498
21.659720	868.086248	15.230515
22.202932	858.837399	15.235533
22.172635	851.410340	15.240551
21.957447	847.638001	15.245568
21.963089	839.722526	15.250586
21.705012	843.928227	15.255603
22.264710	854.712524	15.260621
22.292220	857.564137	15.265639
22.137078	859.588987	15.270656
22.197816	835.097370	15.275674
21.956218	835.412652	15.280691
21.940072	832.600223	15.285709
22.488117	843.610385	15.290727
22.292059	838.979867	15.295744
22.274096	836.167720	15.300762
21.918447	832.256311	15.305779
21.592917	837.356116	15.310797
22.122952	853.819024	15.315815
22.312950	864.692446	15.320832
22.325555	858.240137	15.325850
22.213822	861.293306	15.330867
22.240919	862.617612	15.335885
22.084766	858.116573	15.340903
22.212461	863.432990	15.345920
22.332404	863.092394	15.350938
22.134828	865.133318	15.355955
22.212750	861.201733	15.360973
22.183897	859.438980	15.365991
22.509490	877.407467	15.371008
22.737112	879.719854	15.376026
22.774447	881.301337	15.381043
22.783689	871.529717	15.386061
22.745765	862.686919	15.391079
22.282860	863.181821	15.396096
22.472710	852.552135	15.401114
22.301835	873.431758	15.406131
22.633697	885.703184	15.411149
22.473454	888.098051	15.416167
22.770296	893.463880	15.421184
23.025991	880.883149	15.426202
23.133489	883.633952	15.431219
23.043981	891.180585	15.436237
23.031035	864.870075	15.441255
22.960938	856.250034	15.446272
22.818400	855.937682	15.451290
22.692347	856.850342	15.456307
22.747588	847.200958	15.461325
23.074987	863.054812	15.466343
22.775432	870.277543	15.471360
23.421454	880.051205	15.476378
22.857626	869.936476	15.481395
22.676906	857.714036	15.486413
22.810906	869.441914	15.491431
22.966848	878.752249	15.496448
23.135256	874.244853	15.501466
22.945889	876.322368	15.506483
22.978067	877.532278	15.511501
23.029772	882.434509	15.516519
23.013791	880.575078	15.521536
23.071148	873.317395	15.526554
23.071986	885.697163	15.531571
22.732827	882.572109	15.536589
23.128600	874.958786	15.541607
22.970297	875.611386	15.546624
22.978703	882.470600	15.551642
23.118362	895.065441	15.556659
23.181141	915.223939	15.561677
23.435880	910.968175	15.566695
23.424542	917.562239	15.571712
23.700647	912.896058	15.576730
23.406505	902.878172	15.581747
23.287581	907.059067	15.586765
23.850297	900.274946	15.591783
23.413693	904.375916	15.596800
23.515733	905.218352	15.601818
23.555053	905.609815	15.606835
23.810461	895.099282	15.611853
23.844059	901.591672	15.616871
23.442463	906.851659	15.621888
23.553437	903.075861	15.626906
23.385162	907.213948	15.631923
23.352563	903.536242	15.636941
23.870230	900.287248	15.641959
23.414197	896.224200	15.646976
23.548791	899.926974	15.651994
23.896500	898.462186	15.657011
23.562695	897.876662	15.662029
23.800803	899.098691	15.667047
23.630281	900.248645	15.672064
24.076129	902.350337	15.677082
23.698528	897.022251	15.682099
23.710698	896.569048	15.687117
23.960577	890.493187	15.692135
23.799853	900.259926	15.697152
24.283016	909.380477	15.702170
24.410468	907.918425	15.707187
24.022024	899.054445	15.712205
24.000021	896.413328	15.717223
23.814177	908.544472	15.722240
24.119932	900.575932	15.727258
24.158962	903.684529	15.732275
24.427496	906.041042	15.737293
24.566659	893.980207	15.742311
24.164340	897.690839	15.747328
23.978758	891.341956	15.752346
24.275669	900.422076	15.757363
23.974282	895.700647	15.762381
24.371321	900.949895	15.767399
24.380133	921.533361	15.772416
24.658134	913.506022	15.777434
24.269621	902.641313	15.782451
24.071393	893.157598	15.787469
24.596778	905.468333	15.792487
24.629611	920.329864	15.797504
24.575916	914.386464	15.802522
24.534041	912.161840	15.807539
24.282040	899.720100	15.812557
24.524322	908.625697	15.817575
24.183905	923.614770	15.822592
24.328870	923.674211	15.827610
24.489584	919.168002	15.832627
24.351000	920.562288	15.837645
24.310414	918.324840	15.842663
24.511914	923.298432	15.847680
24.446529	919.789925	15.852698
24.546914	925.653401	15.857715
24.476801	917.279481	15.862733
24.703959	921.166660	15.867751
25.109353	945.402712	15.872768
24.557317	933.922828	15.877786
24.820726	929.429029	15.882803
24.865677	945.061850	15.887821
24.844078	937.765943	15.892839
25.252559	939.371694	15.897856
24.928117	939.292786	15.902874
25.378372	936.006945	15.907891
25.160851	924.282485	15.912909
25.192554	907.634148	15.917927
25.115115	920.322767	15.922944
25.018473	914.777365	15.927962
25.142575	916.383210	15.932979
24.826075	917.306590	15.937997
24.842847	918.976483	15.943015
24.790315	927.593482	15.948032
25.145454	936.279554	15.953050
25.019720	937.195324	15.958067
25.215343	943.451068	15.963085
25.609461	932.533915	15.968103
25.419147	932.011254	15.973120
25.419035	946.290968	15.978138
25.564872	933.067754	15.983155
25.311261	935.600239	15.988173
25.364867	934.563083	15.993191
25.731790	941.701010	15.998208
25.393926	938.326440	16.003226
25.825307	936.668745	16.008243
25.576040	949.535613	16.013261
25.628215	926.780863	16.018279
25.061525	925.796105	16.023296
25.490320	943.202647	16.028314
25.303344	941.562333	16.033331
25.220364	941.395338	16.038349
25.539614	938.290836	16.043367
25.486257	943.853213	16.048384
25.713182	941.368988	16.053402
25.790056	946.592360	16.058419
25.628280	940.293401	16.063437
25.872992	938.570097	16.068455
25.733635	947.279517	16.073472
25.648880	949.378623	16.078490
25.804786	946.368978	16.083507
25.812641	944.714108	16.088525
25.739919	938.565383	16.093543
25.416159	952.295902	16.098560
25.424596	960.591005	16.103578
26.000981	953.413423	16.108595
25.821822	960.933020	16.113613
25.666387	964.393791	16.118631
25.646308	960.256541	16.123648
25.776193	963.975840	16.128666
26.051170	957.937072	16.133683
25.938661	956.979427	16.138701
26.220408	949.800384	16.143719
26.266702	962.106857	16.148736
26.053862	964.314267	16.153754
26.337048	972.639181	16.158771
26.293180	977.177629	16.163789
26.629013	971.902540	16.168807
26.278956	964.269605	16.173824
26.040847	968.071446	16.178842
26.499734	977.022246	16.183859
26.553556	968.288185	16.188877
26.486802	960.248231	16.193895
26.428981	956.571285	16.198912
26.363260	956.512054	16.203930
26.629679	951.774788	16.208947
26.285668	955.776149	16.213965
26.591724	958.328794	16.218983
26.702466	971.480446	16.224000
26.649400	968.339235	16.229018
26.736853	949.198606	16.234035
26.674238	961.522036	16.239053
26.673633	946.863657	16.244071
26.496725	949.450472	16.249088
26.296457	947.676530	16.254106
27.094707	963.157369	16.259123
26.749936	967.821557	16.264141
26.919129	975.428932	16.269159
27.149079	975.875922	16.274176
26.915297	959.051125	16.279194
26.823490	956.231522	16.284211
26.562331	954.192510	16.289229
27.094346	957.530468	16.294247
27.005869	977.548489	16.299264
26.740507	972.799341	16.304282
27.086884	970.804589	16.309299
26.797824	974.336659	16.314317
27.196272	979.345874	16.319335
27.318049	974.059931	16.324352
26.987653	969.210458	16.329370
27.315845	973.877167	16.334387
27.378572	972.554572	16.339405
27.224987	970.388358	16.344423
27.337090	974.407068	16.349440
27.162409	971.685571	16.354458
27.184488	971.079349	16.359475
26.893253	974.472904	16.364493
27.145860	968.718477	16.369511
27.060573	968.889506	16.374528
27.047793	969.390067	16.379546
27.326680	963.445361	16.384563
27.046916	966.338521	16.389581
27.195321	968.713746	16.394599
27.496264	970.809606	16.399616
27.382425	993.671766	16.404634
27.745966	984.068980	16.409651
27.272577	999.094598	16.414669
27.497746	999.059503	16.419687
27.717956	993.764541	16.424704
27.500021	994.618931	16.429722
27.472430	993.534455	16.434739
27.855613	1001.717584	16.439757
27.800050	991.813979	16.444775
27.890965	989.903180	16.449792
27.488264	994.361803	16.454810
28.022080	989.403017	16.459827
27.774394	995.039847	16.464845
27.505490	991.174856	16.469863
27.583715	992.200881	16.474880
27.785610	991.904327	16.479898
27.806206	983.361621	16.484915
27.707136	990.793023	16.489933
27.735109	986.307464	16.494951
27.945769	997.976155	16.499968
28.037764	1003.096205	16.504986
28.502328	1003.910604	16.510003
27.906458	1016.594803	16.515021
28.056314	1009.231147	16.520039
28.575145	1002.182425	16.525056
28.137963	1005.494569	16.530074
28.376243	1007.451870	16.535091
27.938475	1004.881780	16.540109
28.403212	995.089666	16.545127
28.438127	994.888536	16.550144
28.124263	1005.490204	16.555162
28.360944	995.257078	16.560179
28.123283	1004.994829	16.565197
28.119291	1005.232095	16.570215
28.414975	1000.108413	16.575232
28.194179	1011.598140	16.580250
28.256569	1002.187397	16.585267
28.442316	1004.263327	16.590285
28.347290	1002.110083	16.595303
28.414607	1004.005640	16.600320
28.437662	997.813581	16.605338
28.630694	1000.923463	16.610355
28.507044	996.382615	16.615373
28.522832	1007.930177	16.620391
28.895196	1011.892596	16.625408
28.991170	1024.658429	16.630426
29.256229	1010.252121	16.635443
28.758098	997.166992	16.640461
29.071117	988.367319	16.645479
28.997303	992.093094	16.650496
28.642360	988.882117	16.655514
28.842394	986.323178	16.660531
28.740652	991.829989	16.665549
29.022258	1005.886011	16.670567
29.436189	1004.732791	16.675584
29.066566	1002.022707	16.680602
29.412313	993.388346	16.685619
28.965844	996.673534	16.690637
28.953122	994.920879	16.695655
29.321143	989.615527	16.700672
29.017437	994.860299	16.705690
28.756381	990.044205	16.710707
29.188558	1000.488690	16.715725
29.202133	1015.179732	16.720743
29.392322	1004.527813	16.725760
29.047716	1021.890747	16.730778
29.579617	1010.724881	16.735795
29.263580	1018.616102	16.740813
29.174290	1013.965759	16.745831
28.919573	1016.561542	16.750848
29.128229	1026.258217	16.755866
29.216724	1014.653307	16.760883
29.338110	1017.635494	16.765901
29.502332	1028.137494	16.770919
29.748071	1031.210774	16.775936
29.757996	1030.546482	16.780954
30.031307	1020.796781	16.785971
29.799286	1007.711236	16.790989
29.932341	1003.386034	16.796007
29.786232	1004.645801	16.801024
29.673218	1008.327190	16.806042
29.876525	1010.340428	16.811059
29.595388	1003.362609	16.816077
29.476531	1006.334863	16.821095
29.936916	1012.947035	16.826112
30.016116	1033.614344	16.831130
29.902905	1030.422526	16.836147
29.958561	1030.205543	16.841165
30.504437	1028.713047	16.846183
30.182723	1008.626217	16.851200
29.916328	1017.689961	16.856218
30.034399	999.942511	16.861235
30.283107	1004.776235	16.866253
30.038311	1008.045803	16.871271
30.285159	1009.118159	16.876288
30.267414	1007.363129	16.881306
30.048000	1010.956945	16.886323
30.094690	1006.443220	16.891341
30.177539	1018.314858	16.896359
30.450300	1025.697850	16.901376
30.462477	1035.705983	16.906394
30.239118	1028.804363	16.911411
30.804196	1022.682537	16.916429
30.476349	1025.759916	16.921447
30.592793	1016.397552	16.926464
30.205329	1018.158794	16.931482
30.538524	1014.966903	16.936499
30.707903	1026.272816	16.941517
30.719993	1031.963885	16.946535
30.863725	1018.043513	16.951552
30.494310	1024.103241	16.956570
30.216416	1017.689792	16.961587
30.480207	1023.991755	16.966605
30.891397	1031.103891	16.971623
30.629127	1025.290757	16.976640
30.512045	1034.542698	16.981658
30.504974	1033.028997	16.986675
30.993697	1029.569895	16.991693
30.635437	1030.632323	16.996711
30.656950	1029.019500	17.001728
30.666024	1043.095893	17.006746
30.394899	1028.274441	17.011763
30.695456	1037.991527	17.016781
31.011936	1047.927043	17.021799
31.426213	1049.295220	17.026816
31.206537	1054.264998	17.031834
30.986830	1046.898906	17.036851
30.652109	1054.960307	17.041869
30.551370	1056.534901	17.046887
30.832994	1062.865659	17.051904
31.149245	1065.350462	17.056922
31.340072	1081.424588	17.061939
31.460698	1074.387344	17.066957
31.466841	1071.240052	17.071975
31.234061	1061.591215	17.076992
31.166795	1060.557093	17.082010
31.679590	1076.499036	17.087027
31.906487	1078.789472	17.092045
31.375721	1067.262009	17.097063
31.660110	1069.562427	17.102080
31.525415	1058.465603	17.107098
31.442780	1067.649083	17.112115
31.707904	1068.936344	17.117133
31.562484	1076.296104	17.122151
31.780428	1077.896821	17.127168
31.709262	1073.332002	17.132186
31.963052	1071.638830	17.137203
31.909674	1072.111001	17.142221
31.857905	1078.556787	17.147239
31.720825	1070.092237	17.152256
31.991790	1077.437660	17.157274
32.016615	1071.554565	17.162291
31.726213	1081.818115	17.167309
31.710171	1077.512953	17.172327
32.054789	1080.977941	17.177344
31.816003	1076.284586	17.182362
32.093170	1078.923797	17.187379
31.771980	1069.752619	17.192397
31.869441	1076.768454	17.197415
31.872248	1082.217990	17.202432
31.789678	1084.430378	17.207450
31.654017	1093.647373	17.212467
32.063660	1094.883734	17.217485
32.273538	1092.522061	17.222503
32.343813	1091.283488	17.227520
32.625558	1092.890052	17.232538
32.424952	1093.060102	17.237555
32.945590	1092.682362	17.242573
32.792018	1099.674175	17.247591
32.745706	1077.676172	17.252608
32.250524	1075.133946	17.257626
32.309028	1072.641212	17.262643
32.611586	1073.020096	17.267661
32.370926	1088.533412	17.272679
32.496870	1083.470848	17.277696
32.402324	1087.834180	17.282714
32.806167	1088.487626	17.287731
32.808696	1079.316533	17.292749
32.229100	1088.924532	17.297767
32.727063	1079.603720	17.302784
32.801893	1080.371506	17.307802
33.050795	1085.249402	17.312819
32.916421	1078.425426	17.317837
32.720274	1077.584937	17.322855
32.897280	1078.983747	17.327872
33.031402	1083.857423	17.332890
32.743879	1086.436234	17.337907
32.685941	1088.972988	17.342925
33.028499	1098.058725	17.347943
32.996809	1110.942326	17.352960
33.427833	1111.743017	17.357978
33.057979	1107.341458	17.362995
33.312504	1103.969297	17.368013
33.105836	1103.221962	17.373031
33.127427	1106.800364	17.378048
33.450502	1103.338636	17.383066
33.552326	1110.180238	17.388083
33.607587	1110.755414	17.393101
33.333968	1113.739159	17.398119
33.777488	1106.007852	17.403136
33.905498	1107.076625	17.408154
34.012969	1091.937402	17.413171
33.733106	1079.619793	17.418189
33.303578	1077.859442	17.423207
33.202445	1078.509460	17.428224
33.755355	1088.831060	17.433242
33.679417	1097.230881	17.438259
34.262202	1099.106152	17.443277
33.640393	1091.386085	17.448295
33.543609	1075.641211	17.453312
33.565900	1092.568399	17.458330
33.322147	1096.951808	17.463347
33.501658	1099.965985	17.468365
33.259764	1103.197250	17.473383
33.821216	1101.992654	17.478400
33.683099	1100.729722	17.483418
33.958674	1114.679473	17.488435
34.286792	1116.310377	17.493453
34.212623	1126.515039	17.498471
34.190732	1118.518521	17.503488
34.084978	1117.935352	17.508506
34.291792	1114.226638	17.513523
34.098176	1117.298912	17.518541
34.312829	1125.700840	17.523559
34.258881	1117.904971	17.528576
34.442693	1120.871145	17.533594
34.081240	1115.695111	17.538611
34.332307	1117.530513	17.543629
34.373027	1121.538281	17.548647
34.458670	1116.497761	17.553664
34.509031	1113.621285	17.558682
34.212217	1113.187782	17.563699
34.404599	1111.624086	17.568717
34.816894	1118.897030	17.573735
34.740542	1119.786186	17.578752
34.884661	1118.135331	17.583770
34.458943	1118.154239	17.588787
34.926342	1120.811175	17.593805
34.652811	1124.255650	17.598823
34.605711	1119.437766	17.603840
34.821944	1116.983584	17.608858
34.661828	1110.554919	17.613875
34.452948	1115.939595	17.618893
34.509283	1120.352026	17.623911
34.912540	1130.952569	17.628928
35.128553	1129.580850	17.633946
34.510504	1134.641077	17.638963
34.763949	1140.698541	17.643981
34.587363	1153.743587	17.648999
34.683123	1151.554308	17.654016
35.162821	1142.652869	17.659034
35.178462	1147.229432	17.664051
34.924804	1145.126114	17.669069
35.479919	1153.399308	17.674087
35.872365	1148.004901	17.679104
35.549587	1140.074154	17.684122
35.182761	1142.220355	17.689139
35.266491	1140.149714	17.694157
35.226161	1139.960298	17.699175
35.385192	1137.770637	17.704192
35.472286	1142.225621	17.709210
35.268734	1161.961966	17.714227
35.949189	1160.028788	17.719245
35.315316	1168.089480	17.724263
35.510885	1160.794383	17.729280
35.813727	1159.333404	17.734298
35.947743	1165.491522	17.739315
35.994573	1168.182388	17.744333
36.168447	1166.659439	17.749351
35.914614	1160.201166	17.754368
36.135808	1156.379753	17.759386
36.066920	1160.508736	17.764403
36.126334	1147.863703	17.769421
35.967679	1134.877094	17.774439
35.683514	1143.981538	17.779456
35.872111	1140.158891	17.784474
35.863302	1152.167965	17.789491
36.013719	1151.816307	17.794509
35.956856	1151.134007	17.799527
35.965832	1157.497782	17.804544
36.462793	1156.612490	17.809562
36.029267	1148.941978	17.814579
35.776610	1156.163833	17.819597
35.888485	1157.228811	17.824615
36.207356	1172.658239	17.829632
36.654771	1171.685987	17.834650
36.265058	1180.699587	17.839667
36.640729	1174.872285	17.844685
36.878070	1174.453445	17.849703
36.856201	1165.983534	17.854720
36.918678	1162.817987	17.859738
36.659379	1153.608727	17.864755
37.146330	1154.151407	17.869773
36.983921	1143.967709	17.874791
36.633523	1148.522368	17.879808
37.198206	1141.516945	17.884826
36.512093	1142.043450	17.889843
36.799456	1132.212606	17.894861
36.812819	1145.619388	17.899879
36.626737	1138.964384	17.904896
37.128725	1137.860562	17.909914
36.559377	1142.335701	17.914931
36.733620	1138.581561	17.919949
36.667221	1151.625228	17.924967
37.073348	1169.960166	17.929984
37.060289	1165.888046	17.935002
37.355355	1166.302813	17.940019
37.335376	1171.367762	17.945037
37.275433	1172.140758	17.950055
37.114757	1169.606396	17.955072
37.442936	1175.828961	17.960090
37.521950	1168.659305	17.965107
37.494645	1168.925449	17.970125
37.193169	1172.462646	17.975143
37.183142	1176.860177	17.980160
37.375219	1167.362883	17.985178
37.391613	1172.144461	17.990195
37.032606	1172.537988	17.995213
37.190383	1169.225059	18.000231
37.228926	1176.732942	18.005248
37.647791	1183.061310	18.010266
37.793056	1193.657878	18.015283
37.872124	1195.144529	18.020301
37.749583	1190.937971	18.025319
37.524056	1191.989211	18.030336
38.045868	1183.734443	18.035354
38.114745	1186.150482	18.040371
37.922183	1184.542572	18.045389
37.853121	1184.531197	18.050407
37.702338	1187.858744	18.055424
38.156513	1179.788077	18.060442
37.791166	1173.407122	18.065459
38.053387	1183.082920	18.070477
38.049514	1182.228268	18.075495
37.940012	1187.853111	18.080512
38.090995	1170.128769	18.085530
38.096025	1198.277558	18.090547
38.508426	1204.499643	18.095565
38.471613	1201.122331	18.100583
38.419432	1202.402201	18.105600
39.129949	1191.239970	18.110618
38.749200	1193.643964	18.115635
38.210349	1185.210354	18.120653
38.510245	1174.045794	18.125671
38.414667	1186.024219	18.130688
38.615931	1186.156947	18.135706
38.945788	1202.067526	18.140723
38.568606	1200.759758	18.145741
38.757537	1204.823363	18.150759
38.615456	1207.846603	18.155776
38.911942	1203.502219	18.160794
38.850412	1196.761530	18.165811
38.655316	1205.564961	18.170829
39.289649	1197.999565	18.175847
38.994123	1201.602113	18.180864
39.073459	1201.911614	18.185882
38.958472	1204.397306	18.190899
39.102586	1192.502756	18.195917
39.283012	1194.128260	18.200935
38.891859	1194.466832	18.205952
39.243353	1199.597029	18.210970
39.168732	1200.227144	18.215987
38.890645	1196.098451	18.221005
39.222497	1201.181214	18.226023
39.297743	1204.969032	18.231040
39.383686	1199.331997	18.236058
39.513784	1200.933780	18.241075
39.489795	1211.452569	18.246093
39.012433	1194.182637	18.251111
39.186762	1209.495748	18.256128
39.904919	1218.971191	18.261146
39.608746	1223.009343	18.266163
39.511841	1226.312730	18.271181
39.745380	1221.321737	18.276199
39.441744	1228.103437	18.281216
39.724504	1220.861011	18.286234
39.457913	1221.098140	18.291251
39.699167	1224.831713	18.296269
39.658252	1216.620363	18.301287
39.629029	1221.361719	18.306304
39.785492	1215.549599	18.311322
39.988848	1222.403838	18.316339
39.599012	1236.779177	18.321357
39.805324	1238.148191	18.326375
39.789319	1244.241332	18.331392
39.832753	1239.403009	18.336410
39.731891	1243.779985	18.341427
39.879923	1245.211722	18.346445
40.510193	1245.138801	18.351463
40.568857	1246.180511	18.356480
40.553202	1237.252008	18.361498
40.380862	1241.580153	18.366515
40.281309	1239.061511	18.371533
40.292411	1242.669976	18.376551
40.422487	1261.205777	18.381568
40.937666	1258.323180	18.386586
40.780238	1261.897927	18.391603
40.756225	1266.051506	18.396621
41.136878	1250.705513	18.401639
40.973190	1251.409457	18.406656
40.924290	1236.935083	18.411674
40.731898	1231.988312	18.416691
40.881478	1235.669889	18.421709
41.274120	1238.455247	18.426727
40.778074	1239.946237	18.431744
40.765148	1228.126606	18.436762
40.913650	1243.368028	18.441779
41.026225	1258.002831	18.446797
41.279902	1250.787013	18.451815
41.302507	1270.507202	18.456832
41.192638	1257.411922	18.461850
41.347356	1257.018567	18.466867
41.466251	1258.584230	18.471885
41.339842	1257.193232	18.476903
41.140884	1258.751578	18.481920
41.463850	1253.184920	18.486938
41.265376	1258.691095	18.491955
41.303724	1260.177780	18.496973
41.546590	1260.051567	18.501991
41.606038	1266.151903	18.507008
41.241561	1263.362081	18.512026
41.433864	1261.116732	18.517043
40.840153	1270.471406	18.522061
41.216742	1257.909456	18.527079
41.503326	1278.721486	18.532096
41.584358	1277.777871	18.537114
41.926808	1272.148214	18.542131
41.546898	1287.184766	18.547149
41.874860	1276.116758	18.552167
41.329685	1287.366833	18.557184
41.571461	1277.022300	18.562202
42.054711	1294.610057	18.567219
41.979168	1297.083309	18.572237
42.242615	1298.332979	18.577255
41.602548	1307.410867	18.582272
42.421128	1299.248697	18.587290
42.653793	1290.884265	18.592307
42.258322	1307.968219	18.597325
42.136860	1290.696430	18.602343
42.415945	1288.674252	18.607360
42.355150	1299.486001	18.612378
42.666669	1305.272549	18.617395
42.604902	1310.546015	18.622413
42.823385	1300.192472	18.627431
42.143279	1300.847434	18.632448
42.365177	1291.784088	18.637466
42.694497	1291.256251	18.642483
42.489175	1300.408459	18.647501
42.519298	1292.908693	18.652519
42.430607	1296.239216	18.657536
42.729573	1296.138983	18.662554
42.751695	1305.284184	18.667571
42.935638	1315.698077	18.672589
43.098833	1305.406787	18.677607
42.899616	1323.511084	18.682624
42.851618	1322.622270	18.687642
43.211913	1318.075419	18.692659
43.159309	1314.855179	18.697677
43.059283	1312.424963	18.702695
43.216492	1314.104586	18.707712
43.071866	1312.593343	18.712730
43.284541	1315.564524	18.717747
43.127586	1322.250838	18.722765
43.010560	1319.832735	18.727783
43.326128	1317.097972	18.732800
43.382913	1321.043323	18.737818
43.260401	1319.765322	18.742835
43.639776	1334.560621	18.747853
44.062384	1330.224972	18.752871
43.794330	1326.321905	18.757888
43.611904	1302.934169	18.762906
43.828586	1316.063270	18.767923
44.209445	1322.975119	18.772941
44.200510	1307.232142	18.777959
44.327879	1306.177169	18.782976
44.006896	1305.741113	18.787994
44.152498	1292.161063	18.793011
44.001120	1303.296187	18.798029
44.097999	1292.892152	18.803047
44.071395	1295.600782	18.808064
44.182808	1283.704950	18.813082
44.282796	1289.101549	18.818099
44.121188	1308.938825	18.823117
43.995509	1295.823887	18.828135
43.951609	1295.502481	18.833152
44.342302	1309.039986	18.838170
44.674478	1320.333364	18.843187
44.185891	1316.934851	18.848205
44.303650	1319.494776	18.853223
44.480934	1312.022582	18.858240
44.469372	1328.895305	18.863258
44.851641	1321.447998	18.868275
44.598637	1325.066041	18.873293
44.838583	1316.037743	18.878311
44.727600	1322.265618	18.883328
44.692654	1321.138086	18.888346
44.852128	1317.222106	18.893363
44.520732	1327.990797	18.898381
44.785561	1319.217400	18.903399
44.656499	1321.844156	18.908416
44.507630	1329.030987	18.913434
45.010967	1336.173081	18.918451
45.018542	1345.768694	18.923469
45.379816	1348.461122	18.928487
45.059049	1339.681059	18.933504
45.014569	1343.083602	18.938522
45.324780	1336.319696	18.943539
44.964097	1348.159624	18.948557
45.353497	1343.766026	18.953575
45.356720	1339.618747	18.958592
45.154537	1340.565375	18.963610
45.258320	1335.165362	18.968627
45.342132	1343.843386	18.973645
45.543224	1340.274372	18.978663
45.509226	1350.289871	18.983680
45.698807	1363.543149	18.988698
45.867828	1352.932187	18.993715
45.854990	1365.090354	18.998733
46.061199	1358.554072	19.003751
45.850738	1354.465306	19.008768
45.665820	1354.440411	19.013786
45.914733	1356.553886	19.018803
45.936970	1361.192593	19.023821
45.708777	1355.585483	19.028839
46.047749	1359.493220	19.033856
45.964920	1361.784578	19.038874
46.157543	1349.715112	19.043891
45.860762	1362.861075	19.048909
45.687707	1361.556227	19.053927
46.217283	1361.757761	19.058944
46.188610	1379.507357	19.063962
46.329414	1375.310247	19.068979
45.992718	1390.690455	19.073997
46.473410	1379.216750	19.079015
46.433988	1383.618908	19.084032
46.273672	1379.279331	19.089050
46.753004	1382.070150	19.094067
46.888836	1388.887629	19.099085
46.444773	1378.728714	19.104103
46.986872	1384.457296	19.109120
46.782951	1386.953705	19.114138
47.050382	1377.469814	19.119155
46.979339	1373.289909	19.124173
46.999009	1380.071822	19.129191
47.086149	1378.032181	19.134208
47.020579	1384.069970	19.139226
46.999278	1389.851559	19.144243
47.210293	1395.726368	19.149261
47.239914	1400.133560	19.154279
47.440087	1400.970209	19.159296
47.225716	1405.980283	19.164314
47.756549	1393.630910	19.169331
47.818358	1399.289109	19.174349
47.531729	1383.147484	19.179367
47.282168	1383.505040	19.184384
47.583256	1394.566619	19.189402
47.633693	1395.606462	19.194419
47.820819	1398.597413	19.199437
48.073936	1401.713791	19.204455
47.894959	1377.189323	19.209472
47.422302	1373.125596	19.214490
47.479625	1384.761611	19.219507
47.453274	1386.321496	19.224525
47.652803	1392.936555	19.229543
47.944991	1386.528888	19.234560
48.003404	1390.000628	19.239578
48.112051	1392.404191	19.244595
48.030461	1394.995164	19.249613
48.095416	1394.148720	19.254631
48.307653	1386.891961	19.259648
47.879171	1394.302235	19.264666
47.922522	1388.993666	19.269683
47.932654	1398.390092	19.274701
48.212253	1411.174951	19.279719
48.540945	1414.487849	19.284736
48.174768	1416.567709	19.289754
48.363779	1410.873535	19.294771
48.443463	1413.060702	19.299789
48.231305	1415.564709	19.304807
48.416998	1411.590977	19.309824
47.965667	1411.897896	19.314842
48.929815	1423.897681	19.319859
48.851642	1440.604155	19.324877
48.821871	1446.437574	19.329895
49.041779	1430.040315	19.334912
48.836018	1439.416727	19.339930
49.280730	1434.291810	19.344947
49.263668	1438.223438	19.349965
49.342157	1427.408775	19.354983
49.652850	1423.756408	19.360000
49.313563	1423.143316	19.365018
49.632836	1412.376380	19.370035
49.169688	1405.530883	19.375053
49.159915	1397.450301	19.380071
49.308145	1405.768029	19.385088
49.317718	1425.689236	19.390106
49.384161	1418.660293	19.395123
49.647883	1424.511126	19.400141
49.770994	1429.841051	19.405159
49.946065	1428.728151	19.410176
49.694846	1423.847290	19.415194
49.761989	1421.829692	19.420211
49.748449	1425.558796	19.425229
49.481421	1430.062676	19.430247
49.391771	1426.753508	19.435264
49.489065	1430.061411	19.440282
49.402327	1435.894229	19.445299
49.879217	1440.591558	19.450317
49.815434	1451.602683	19.455335
50.091333	1453.409008	19.460352
50.377115	1455.759754	19.465370
50.123833	1453.504860	19.470387
50.330179	1456.751607	19.475405
50.130599	1458.893896	19.480423
50.724923	1448.267154	19.485440
50.593222	1448.041467	19.490458
50.610501	1447.634792	19.495475
50.544937	1445.107674	19.500493
50.498407	1452.180791	19.505511
51.027435	1448.803697	19.510528
50.543878	1451.772845	19.515546
50.676037	1447.343533	19.520563
50.666138	1444.217607	19.525581
50.646213	1444.255387	19.530599
51.025167	1436.833794	19.535616
50.740586	1442.451262	19.540634
51.141327	1462.642970	19.545651
51.379178	1457.821655	19.550669
50.859948	1456.460243	19.555687
50.790713	1456.357375	19.560704
50.919594	1462.333358	19.565722
50.654432	1463.315043	19.570739
50.796774	1461.181591	19.575757
50.826984	1478.521327	19.580775
51.223168	1474.265498	19.585792
51.235041	1482.746504	19.590810
51.406519	1487.112697	19.595827
51.754983	1486.591341	19.600845
51.720543	1495.991602	19.605863
51.802893	1486.435483	19.610880
51.704940	1498.234604	19.615898
51.767769	1488.602627	19.620915
51.979605	1484.293446	19.625933
51.928565	1496.110508	19.630951
51.799027	1491.772424	19.635968
52.014755	1493.786939	19.640986
51.837169	1488.279207	19.646003
52.442182	1484.502108	19.651021
51.955054	1486.484041	19.656039
52.416849	1484.401835	19.661056
52.121118	1482.601676	19.666074
52.041755	1482.658176	19.671091
52.257133	1477.894005	19.676109
52.117195	1482.595863	19.681127
52.239622	1485.022540	19.686144
52.301086	1480.042487	19.691162
52.155157	1486.253770	19.696179
52.346723	1489.136746	19.701197
52.034428	1506.570862	19.706215
52.514486	1503.876733	19.711232
52.381591	1516.725891	19.716250
52.542034	1502.332318	19.721267
52.527179	1510.400928	19.726285
52.549368	1526.040960	19.731303
52.790186	1526.618819	19.736320
52.739174	1531.966416	19.741338
52.906839	1539.258686	19.746355
53.500005	1539.087400	19.751373
53.003136	1542.374221	19.756391
53.246579	1531.076214	19.761408
53.185485	1536.920852	19.766426
53.222591	1526.147286	19.771443
53.295626	1529.238075	19.776461
53.320911	1532.699221	19.781479
53.352446	1526.653983	19.786496
53.480890	1537.142919	19.791514
53.783573	1544.392079	19.796531
53.990265	1548.879038	19.801549
53.682446	1545.597504	19.806567
53.964434	1538.658033	19.811584
53.739875	1528.329154	19.816602
53.752353	1539.022342	19.821619
54.231772	1547.875560	19.826637
53.892946	1550.812723	19.831655
54.029868	1550.330614	19.836672
54.094711	1552.062510	19.841690
53.823961	1560.152049	19.846707
54.389976	1549.302433	19.851725
54.267232	1550.823691	19.856743
54.366534	1542.426256	19.861760
54.509884	1550.678538	19.866778
54.208538	1556.895108	19.871795
54.328994	1542.744418	19.876813
53.969075	1553.662854	19.881831
54.252795	1544.971613	19.886848
54.190883	1554.161584	19.891866
54.252654	1557.762224	19.896883
54.471855	1569.726611	19.901901
54.300115	1569.835365	19.906919
54.761501	1571.363511	19.911936
54.736350	1570.736219	19.916954
54.759141	1561.015760	19.921971
54.921801	1565.922996	19.926989
54.489582	1571.585582	19.932007
54.665209	1578.775641	19.937024
54.996969	1585.594249	19.942042
54.714711	1593.180657	19.947059
54.761157	1584.463222	19.952077
55.067303	1594.624719	19.957095
55.351169	1586.927530	19.962112
55.568501	1604.983038	19.967130
55.568429	1596.096111	19.972147
55.719501	1591.045271	19.977165
55.669411	1589.203699	19.982183
55.653223	1583.689744	19.987200
55.637148	1583.723769	19.992218
55.691471	1582.339320	19.997235
56.136592	1590.964366	20.002253
55.918867	1595.179740	20.007271
55.915593	1596.546699	20.012288
56.395151	1594.231338	20.017306
56.106808	1585.979444	20.022323
56.007989	1577.701202	20.027341
55.977185	1586.668592	20.032359
55.920494	1589.050586	20.037376
56.356119	1593.580810	20.042394
56.040253	1603.820220	20.047411
56.512182	1605.861133	20.052429
56.310313	1607.009700	20.057447
56.207079	1603.500639	20.062464
56.371371	1620.109569	20.067482
56.192936	1618.856032	20.072499
56.414510	1601.495819	20.077517
56.556630	1611.998450	20.082535
56.537371	1622.245341	20.087552
56.868904	1628.884117	20.092570
56.666741	1625.062245	20.097587
56.873653	1630.398118	20.102605
56.528655	1628.567744	20.107623
56.645025	1627.508153	20.112640
56.801379	1627.288109	20.117658
56.962195	1625.625140	20.122675
57.240906	1628.668144	20.127693
57.156534	1636.387866	20.132711
57.324896	1648.921966	20.137728
57.802992	1638.420507	20.142746
57.499119	1636.855134	20.147763
57.625387	1632.887449	20.152781
57.192699	1643.965596	20.157799
57.424230	1640.682124	20.162816
57.569790	1635.114567	20.167834
57.364358	1642.960439	20.172851
57.712103	1640.905440	20.177869
58.089058	1637.510963	20.182887
58.022861	1633.251346	20.187904
58.022315	1633.008392	20.192922
57.991984	1637.181975	20.197939
58.292502	1638.728861	20.202957
58.261788	1632.765864	20.207975
57.964331	1632.689060	20.212992
57.951149	1631.425573	20.218010
58.003281	1650.030721	20.223027
58.530036	1651.668619	20.228045
58.417674	1657.432914	20.233063
58.651933	1660.028399	20.238080
58.807967	1659.808404	20.243098
58.826640	1657.470116	20.248115
58.913939	1653.413818	20.253133
58.881162	1654.356177	20.258151
58.912855	1655.907049	20.263168
59.092468	1653.849823	20.268186
58.735254	1646.514358	20.273203
59.115419	1649.317504	20.278221
58.920350	1655.886798	20.283239
58.870798	1655.960748	20.288256
58.994852	1648.086440	20.293274
58.622584	1652.903412	20.298291
58.961550	1651.736578	20.303309
59.008505	1657.182572	20.308327
58.734644	1648.603339	20.313344
58.915302	1654.719651	20.318362
59.114034	1680.055566	20.323379
59.320723	1676.009078	20.328397
59.257435	1672.982945	20.333415
59.161276	1682.683253	20.338432
59.536400	1676.543443	20.343450
59.508306	1679.021985	20.348467
59.762817	1691.993992	20.353485
60.012352	1702.947022	20.358503
59.800057	1708.480734	20.363520
60.107560	1701.407836	20.368538
59.767325	1698.377479	20.373555
59.927722	1703.114688	20.378573
59.907551	1698.298766	20.383591
59.950340	1708.655970	20.388608
60.091900	1703.395134	20.393626
59.929673	1707.557711	20.398643
60.093172	1720.629118	20.403661
60.480253	1727.776848	20.408679
60.309805	1729.567486	20.413696
60.584704	1732.336540	20.418714
60.441856	1723.392883	20.423731
60.557519	1725.675475	20.428749
60.705703	1715.720810	20.433767
60.368195	1715.356744	20.438784
60.704992	1724.734041	20.443802
60.832509	1736.659165	20.448819
61.151040	1732.759357	20.453837
61.696345	1736.865432	20.458855
61.925879	1725.402207	20.463872
61.422736	1716.820769	20.468890
61.139493	1704.339147	20.473907
61.384279	1713.251070	20.478925
61.352540	1706.130000	20.483943
61.347021	1708.778603	20.488960
61.574538	1716.740142	20.493978
61.461622	1731.946942	20.498995
61.486949	1728.487270	20.504013
61.681617	1728.179207	20.509031
61.254941	1731.489847	20.514048
61.851225	1724.065858	20.519066
61.690212	1732.210974	20.524083
61.642018	1729.782099	20.529101
61.796377	1727.359559	20.534119
62.214294	1747.451084	20.539136
62.098386	1748.759850	20.544154
62.092150	1756.262325	20.549171
62.182197	1753.127096	20.554189
62.569729	1760.877543	20.559207
62.252994	1760.434501	20.564224
62.604198	1745.708067	20.569242
62.357043	1749.981709	20.574259
62.482926	1752.777123	20.579277
62.404617	1753.496196	20.584295
62.252933	1749.609632	20.589312
62.530741	1742.718071	20.594330
62.354908	1755.488877	20.599347
62.670248	1773.797546	20.604365
62.706831	1778.396258	20.609383
62.591973	1771.190270	20.614400
62.951184	1770.380048	20.619418
62.817078	1774.093282	20.624435
62.723920	1770.519502	20.629453
63.083757	1786.416469	20.634471
63.003530	1792.895347	20.639488
63.310364	1786.958641	20.644506
63.550363	1795.186522	20.649523
63.711139	1794.470312	20.654541
63.915593	1798.752550	20.659559
63.818417	1796.157717	20.664576
63.701554	1793.389221	20.669594
63.795634	1793.519707	20.674611
63.576471	1790.120180	20.679629
63.613508	1791.673387	20.684647
63.522538	1793.985004	20.689664
63.974607	1785.756599	20.694682
63.740126	1792.041737	20.699699
63.689690	1790.888183	20.704717
63.861261	1793.809038	20.709735
64.037792	1804.552584	20.714752
64.437318	1807.349585	20.719770
64.230864	1811.878844	20.724787
64.323124	1810.305429	20.729805
64.754923	1812.908052	20.734823
64.215970	1814.576187	20.739840
64.773185	1809.629313	20.744858
64.481765	1820.120669	20.749875
64.535056	1822.087927	20.754893
64.869822	1815.660854	20.759911
64.829970	1822.840378	20.764928
65.063628	1815.750529	20.769946
64.766194	1830.143517	20.774963
65.145046	1828.967306	20.779981
64.919659	1834.591460	20.784999
65.018626	1843.762844	20.790016
64.965572	1835.016595	20.795034
65.158551	1834.674078	20.800051
65.105790	1838.810174	20.805069
65.396203	1827.454173	20.810087
65.633399	1841.293702	20.815104
66.123948	1835.858569	20.820122
65.984823	1825.020740	20.825139
65.932742	1821.809794	20.830157
66.193130	1813.425022	20.835175
65.750899	1819.606811	20.840192
66.205129	1819.681224	20.845210
66.208756	1814.940464	20.850227
65.876500	1815.172043	20.855245
66.147772	1816.016577	20.860263
65.866540	1823.871174	20.865280
65.713316	1837.809357	20.870298
66.326058	1836.621978	20.875315
66.241510	1841.264812	20.880333
66.667669	1847.671181	20.885351
66.682208	1837.996039	20.890368
67.049483	1842.025712	20.895386
66.502234	1842.316012	20.900403
66.410047	1844.277519	20.905421
66.456962	1841.682338	20.910439
66.631524	1842.901704	20.915456
67.033835	1843.347129	20.920474
67.138852	1856.882192	20.925491
67.081744	1856.455531	20.930509
67.355575	1849.621354	20.935527
67.374728	1861.077425	20.940544
67.473153	1848.671982	20.945562
67.479332	1844.173821	20.950579
67.271049	1847.652458	20.955597
67.565429	1852.526641	20.960615
67.737887	1849.403812	20.965632
67.753645	1843.490315	20.970650
67.667339	1833.903462	20.975667
67.774067	1842.306753	20.980685
67.611701	1847.375127	20.985703
67.849636	1857.392756	20.990720
67.977860	1847.602076	20.995738
67.864120	1853.546534	21.000755
67.540547	1859.921308	21.005773
68.138477	1850.956929	21.010791
67.974906	1854.801003	21.015808
67.874265	1845.664514	21.020826
67.949868	1858.380467	21.025843
67.898328	1875.253619	21.030861
68.519374	1873.077145	21.035879
68.290540	1873.188478	21.040896
68.540397	1878.602949	21.045914
68.309376	1876.887351	21.050931
68.034882	1877.671689	21.055949
68.590896	1879.213533	21.060967
68.714047	1905.438879	21.065984
68.449099	1906.158613	21.071002
68.970451	1903.054040	21.076019
68.886394	1897.092947	21.081037
69.059886	1890.621527	21.086055
69.040666	1901.644927	21.091072
69.108557	1897.717832	21.096090
68.971664	1902.933740	21.101107
68.908500	1917.826829	21.106125
69.329472	1919.654798	21.111143
69.719243	1910.129487	21.116160
70.023535	1909.725455	21.121178
70.277013	1907.473657	21.126195
70.388273	1912.161765	21.131213
70.574453	1904.476494	21.136231
70.452460	1897.419893	21.141248
70.111464	1881.336776	21.146266
69.851657	1877.328158	21.151283
70.244517	1881.508496	21.156301
70.373301	1872.099580	21.161319
70.324819	1879.861158	21.166336
70.290675	1889.520365	21.171354
70.227823	1890.959741	21.176371
70.235539	1910.752387	21.181389
70.405816	1904.085796	21.186407
70.394869	1907.969236	21.191424
70.374183	1901.401808	21.196442
70.727651	1894.362705	21.201459
70.319927	1908.258513	21.206477
70.830325	1920.660654	21.211495
70.742818	1930.788955	21.216512
71.282814	1936.376029	21.221530
70.893877	1933.006063	21.226547
70.948528	1935.465445	21.231565
70.961016	1933.954935	21.236583
70.812950	1930.727355	21.241600
70.893629	1942.915539	21.246618
71.255222	1946.567410	21.251635
71.231564	1955.347674	21.256653
71.467700	1956.358638	21.261671
71.402702	1956.103623	21.266688
71.610512	1957.753338	21.271706
71.692888	1958.851360	21.276723
71.376440	1961.867159	21.281741
71.944374	1972.723444	21.286759
71.805431	1980.110970	21.291776
71.964283	1970.003018	21.296794
72.054121	1967.508437	21.301811
72.150586	1981.262684	21.306829
72.298949	1971.181612	21.311847
72.287509	1961.084398	21.316864
71.832058	1970.588329	21.321882
72.519698	1977.850317	21.326899
72.936206	1988.193680	21.331917
72.818372	1985.217013	21.336935
72.948558	1995.242027	21.341952
72.630858	1992.204954	21.346970
73.254752	1987.143506	21.351987
73.121150	1991.544698	21.357005
73.197633	1994.382556	21.362023
73.071961	1983.990678	21.367040
73.451191	1989.362949	21.372058
73.403537	1996.963496	21.377075
73.118278	1995.960103	21.382093
73.080679	1986.444483	21.387111
73.306037	1994.905119	21.392128
73.015022	2001.994426	21.397146
73.280263	1983.494064	21.402163
73.286066	1992.146678	21.407181
73.521386	1995.436352	21.412199
73.502805	2009.669299	21.417216
73.681809	2013.990267	21.422234
73.965078	2004.333158	21.427251
73.763216	2009.707541	21.432269
74.050073	2009.978435	21.437287
73.945809	2012.143821	21.442304
74.458370	2037.128413	21.447322
74.339620	2028.925651	21.452339
74.426402	2042.381639	21.457357
74.558711	2037.043248	21.462375
74.908723	2031.588909	21.467392
74.492453	2038.401074	21.472410
74.397752	2028.708122	21.477427
74.388443	2036.157543	21.482445
74.328609	2033.910327	21.487463
74.219065	2033.166764	21.492480
74.768008	2052.733284	21.497498
74.977772	2059.460611	21.502515
75.245285	2057.588479	21.507533
75.160358	2062.341887	21.512551
75.234280	2051.701134	21.517568
75.358985	2062.001605	21.522586
75.220720	2060.331510	21.527603
75.435789	2074.837413	21.532621
75.608242	2084.354101	21.537639
75.964889	2082.092531	21.542656
75.915677	2085.325531	21.547674
76.536271	2073.416173	21.552691
75.975553	2085.410813	21.557709
75.891239	2077.818076	21.562727
76.287550	2073.199154	21.567744
76.521404	2074.936347	21.572762
76.294149	2065.456525	21.577779
76.239212	2077.145185	21.582797
76.443258	2071.581011	21.587815
76.212981	2067.290029	21.592832
76.227810	2079.270799	21.597850
76.189876	2071.705559	21.602867
76.374404	2077.811946	21.607885
76.775588	2086.324148	21.612903
76.862460	2091.902922	21.617920
77.077152	2093.056094	21.622938
76.909466	2093.997389	21.627955
76.855227	2096.808277	21.632973
76.944704	2091.833161	21.637991
77.238354	2092.210301	21.643008
76.952932	2097.935406	21.648026
77.138554	2094.586413	21.653043
77.305282	2099.092357	21.658061
77.299742	2100.500735	21.663079
77.056248	2111.095257	21.668096
77.015473	2121.184830	21.673114
77.384679	2112.413730	21.678131
77.794937	2111.333602	21.683149
77.998762	2117.758905	21.688167
78.449979	2113.869916	21.693184
77.788602	2118.930849	21.698202
78.098900	2111.885759	21.703219
78.177550	2126.214118	21.708237
78.523789	2137.938192	21.713255
78.255403	2129.897543	21.718272
78.723852	2140.507476	21.723290
78.730464	2137.492472	21.728307
78.609972	2144.315433	21.733325
78.447510	2138.013001	21.738343
79.025215	2142.839996	21.743360
78.675027	2138.908510	21.748378
78.695468	2134.963503	21.753395
78.681448	2127.246187	21.758413
79.018519	2132.293690	21.763431
78.612148	2141.954179	21.768448
78.606659	2151.811047	21.773466
79.191900	2153.326274	21.778483
79.089266	2164.198712	21.783501
78.784570	2163.996793	21.788519
78.980312	2166.920258	21.793536
79.417287	2175.272289	21.798554
79.511955	2175.311163	21.803571
79.836957	2180.553073	21.808589
79.662235	2184.657742	21.813607
79.518225	2178.008422	21.818624
79.778173	2181.445783	21.823642
80.094602	2201.054978	21.828659
79.943084	2199.374310	21.833677
80.352137	2201.355651	21.838695
80.375684	2196.330808	21.843712
79.889262	2199.534064	21.848730
80.252855	2198.792573	21.853747
80.387197	2201.798191	21.858765
80.583269	2217.964050	21.863783
80.951370	2225.525211	21.868800
80.694865	2223.434831	21.873818
80.957425	2225.284340	21.878835
80.976620	2221.907583	21.883853
80.812550	2223.305937	21.888871
80.780145	2220.931344	21.893888
80.642467	2234.542350	21.898906
81.076927	2229.971100	21.903923
81.682819	2244.719265	21.908941
81.554642	2241.037228	21.913959
81.812850	2233.848713	21.918976
81.914674	2246.945888	21.923994
81.878450	2240.020974	21.929011
81.848484	2244.526020	21.934029
81.932829	2242.123779	21.939047
82.235649	2238.500878	21.944064
81.661087	2242.443738	21.949082
81.632824	2235.205145	21.954099
82.031800	2248.584278	21.959117
82.259049	2255.207966	21.964135
82.210021	2249.730478	21.969152
82.255096	2256.597136	21.974170
82.309495	2260.634590	21.979187
82.830049	2258.347479	21.984205
82.846630	2265.114429	21.989223
82.812815	2261.496595	21.994240
82.320370	2260.058360	21.999258
82.790491	2252.805284	22.004275
82.747356	2263.122535	22.009293
82.666485	2276.860436	22.014311
83.035345	2285.693364	22.019328
83.063286	2290.905813	22.024346
83.450710	2285.489757	22.029363
83.138744	2281.640655	22.034381
83.007329	2290.204317	22.039399
83.246378	2291.404207	22.044416
83.118667	2304.534005	22.049434
83.331965	2308.915980	22.054451
83.733279	2309.074380	22.059469
83.999768	2305.425562	22.064487
83.930224	2303.350247	22.069504
83.785040	2314.437696	22.074522
83.834653	2326.766686	22.079539
84.280952	2331.671000	22.084557
84.465566	2331.421301	22.089575
85.029468	2312.792045	22.094592
84.533471	2319.941795	22.099610
85.032650	2319.794608	22.104627
84.849332	2319.700028	22.109645
84.549642	2320.371536	22.114663
85.146436	2325.331317	22.119680
84.998557	2322.775862	22.124698
85.385237	2320.992452	22.129715
85.267754	2319.224418	22.134733
84.904641	2321.449078	22.139751
84.900139	2315.434431	22.144768
85.015709	2312.374031	22.149786
85.303652	2334.881847	22.154803
85.545352	2338.268427	22.159821
85.140218	2345.211526	22.164839
85.728590	2340.720432	22.169856
85.602831	2341.819323	22.174874
85.585038	2348.702116	22.179891
85.943683	2351.249934	22.184909
85.869536	2367.786223	22.189927
85.694906	2368.917972	22.194944
86.005284	2369.219927	22.199962
85.913471	2364.430760	22.204979
86.620073	2362.092578	22.209997
86.210840	2368.035873	22.215015
86.303911	2376.621434	22.220032
86.522487	2384.565727	22.225050
86.586819	2386.061084	22.230067
86.943778	2378.513133	22.235085
87.066759	2389.498913	22.240103
87.151010	2383.438866	22.245120
87.185739	2383.417641	22.250138
87.014596	2376.930272	22.255155
87.444827	2383.197337	22.260173
87.341080	2386.451506	22.265191
87.158926	2376.970808	22.270208
87.422832	2392.608681	22.275226
87.539546	2400.092284	22.280243
87.461354	2404.620658	22.285261
87.759419	2409.456549	22.290279
87.588165	2406.825821	22.295296
87.727554	2404.664313	22.300314
88.055609	2404.256571	22.305331
88.224019	2419.530615	22.310349
88.323468	2422.418618	22.315367
88.478992	2429.896191	22.320384
88.845579	2428.115900	22.325402
88.857465	2431.446754	22.330419
88.777072	2405.523194	22.335437
88.787270	2401.753303	22.340455
88.813812	2388.601238	22.345472
88.396837	2399.756303	22.350490
89.050838	2413.906947	22.355507
88.975099	2413.741966	22.360525
88.988443	2414.371052	22.365543
88.984487	2410.256202	22.370560
89.117951	2419.094287	22.375578
88.939412	2419.055771	22.380595
89.287453	2415.242746	22.385613
89.061849	2433.216565	22.390631
89.408023	2436.558494	22.395648
89.625015	2442.760944	22.400666
89.611642	2444.012768	22.405683
89.644035	2448.022130	22.410701
89.563284	2445.478298	22.415719
89.839185	2464.074702	22.420736
89.817360	2476.885163	22.425754
89.626059	2470.296750	22.430771
90.472731	2473.715407	22.435789
90.028084	2473.071339	22.440807
90.085314	2488.129206	22.445824
90.633196	2499.007871	22.450842
90.688490	2491.424783	22.455859
90.933148	2483.992108	22.460877
90.760309	2487.730455	22.465895
90.848106	2489.550394	22.470912
90.864001	2494.913111	22.475930
91.024496	2492.451640	22.480947
91.373888	2505.829218	22.485965
90.929638	2517.856508	22.490983
91.058291	2509.163696	22.496000
91.216473	2505.556949	22.501018
91.237484	2504.748855	22.506035
91.600495	2513.125185	22.511053
91.530904	2520.760930	22.516071
91.765808	2533.051745	22.521088
92.023370	2528.678387	22.526106
91.864731	2534.377579	22.531123
92.378261	2526.091928	22.536141
91.863506	2542.924211	22.541159
91.909103	2547.468064	22.546176
91.997587	2557.749212	22.551194
92.402878	2548.492566	22.556211
92.517461	2552.760574	22.561229
92.245968	2549.612062	22.566247
92.285311	2560.462635	22.571264
92.715158	2559.183759	22.576282
92.976234	2575.368225	22.581299
93.373146	2563.843688	22.586317
93.091544	2575.138743	22.591335
93.186156	2568.461594	22.596352
93.289420	2565.005407	22.601370
93.557675	2583.082379	22.606387
93.949379	2578.770181	22.611405
94.275267	2589.560379	22.616423
94.634313	2570.385197	22.621440
94.356606	2558.918357	22.626458
94.310004	2552.219015	22.631475
94.072579	2543.791480	22.636493
94.134223	2554.300883	22.641511
94.456302	2548.333149	22.646528
94.852077	2550.209293	22.651546
94.648898	2555.820746	22.656563
94.835293	2546.468784	22.661581
95.046314	2546.237062	22.666599
94.898335	2546.433646	22.671616
94.562570	2549.733436	22.676634
94.956907	2549.353245	22.681651
94.777188	2540.973534	22.686669
94.350350	2551.729414	22.691687
94.540605	2550.692983	22.696704
95.091681	2564.616757	22.701722
94.760945	2568.761584	22.706739
95.069270	2562.723398	22.711757
94.771515	2569.113339	22.716775
95.136717	2585.095396	22.721792
95.403012	2590.848377	22.726810
95.419776	2598.322376	22.731827
95.519285	2609.435030	22.736845
95.317873	2622.844799	22.741863
95.763039	2626.862525	22.746880
95.875660	2619.664963	22.751898
95.734605	2633.380946	22.756915
96.008596	2638.069158	22.761933
96.241611	2644.527979	22.766951
96.365052	2641.346367	22.771968
96.533406	2650.548391	22.776986
96.299820	2658.383309	22.782003
96.701812	2665.579592	22.787021
96.697944	2669.200143	22.792039
96.597277	2670.989478	22.797056
97.210050	2667.371887	22.802074
97.242158	2671.100456	22.807091
97.878279	2679.806756	22.812109
97.189650	2677.868813	22.817127
97.394956	2684.795902	22.822144
97.994553	2682.947748	22.827162
97.911935	2695.250238	22.832179
98.350007	2680.326463	22.837197
98.454444	2690.567331	22.842215
97.895526	2686.646127	22.847232
98.126141	2677.381894	22.852250
97.956314	2687.270955	22.857267
97.966175	2679.259326	22.862285
98.535148	2685.419684	22.867303
98.951808	2690.656942	22.872320
98.492791	2686.852739	22.877338
98.489238	2693.266352	22.882355
98.602897	2695.754524	22.887373
98.948065	2708.413331	22.892391
98.904361	2707.889881	22.897408
98.931106	2703.312557	22.902426
98.946681	2708.460776	22.907443
99.079531	2714.477589	22.912461
99.128524	2726.986846	22.917479
98.918185	2735.149564	22.922496
99.596955	2725.922838	22.927514
99.620714	2734.588795	22.932531
99.904819	2727.399207	22.937549
100.097237	2744.285692	22.942567
100.259420	2743.168407	22.947584
100.265461	2744.934824	22.952602
100.156388	2743.004478	22.957619
100.696328	2735.825553	22.962637
100.818361	2742.951837	22.967655
100.474330	2745.441841	22.972672
100.484043	2740.078144	22.977690
100.684209	2744.462272	22.982707
100.624354	2743.524735	22.987725
100.890971	2745.013877	22.992743
100.530380	2742.990137	22.997760
100.931103	2750.388640	23.002778
100.592511	2769.371390	23.007795
100.641869	2769.603529	23.012813
101.126538	2769.480692	23.017831
101.158499	2771.792231	23.022848
101.478760	2785.950946	23.027866
101.524957	2800.202839	23.032883
101.265253	2792.908529	23.037901
101.825672	2790.965469	23.042919
101.815496	2794.587028	23.047936
101.738815	2794.157080	23.052954
102.035572	2810.636030	23.057971
102.499665	2805.271003	23.062989
102.631196	2816.924802	23.068007
102.352664	2823.548545	23.073024
102.518228	2815.032891	23.078042
102.405958	2814.362309	23.083059
102.545544	2816.534010	23.088077
102.758461	2820.439604	23.093095
102.955544	2825.007284	23.098112
103.081745	2827.436713	23.103130
103.218829	2831.619226	23.108147
102.978503	2828.756171	23.113165
103.118344	2829.564410	23.118183
103.020610	2845.151676	23.123200
103.413972	2852.529274	23.128218
103.571644	2860.013005	23.133235
103.631558	2859.877396	23.138253
103.887694	2863.946699	23.143271
103.619792	2868.337454	23.148288
104.062911	2873.709514	23.153306
103.912877	2872.656612	23.158323
104.032825	2882.033563	23.163341
104.592333	2884.922604	23.168359
104.280292	2897.188361	23.173376
104.795669	2895.754122	23.178394
104.680470	2896.662037	23.183411
104.910901	2904.033463	23.188429
105.240975	2901.785398	23.193447
105.019373	2899.531698	23.198464
105.370869	2898.703694	23.203482
105.199673	2905.332849	23.208499
105.119010	2911.367190	23.213517
105.430867	2920.749000	23.218535
105.227385	2933.360831	23.223552
105.736105	2922.364663	23.228570
105.456079	2932.823331	23.233587
105.763923	2935.265524	23.238605
106.084255	2942.026467	23.243623
106.237732	2953.200366	23.248640
106.335634	2946.585687	23.253658
106.503745	2940.894283	23.258675
106.413417	2940.169783	23.263693
106.863637	2936.056692	23.268711
106.782075	2938.969805	23.273728
106.940218	2935.681744	23.278746
106.970701	2931.542476	23.283763
106.900497	2941.889581	23.288781
107.219382	2959.460387	23.293799
107.253339	2968.260582	23.298816
107.099018	2965.084285	23.303834
107.142833	2972.986614	23.308851
107.335484	2960.982338	23.313869
107.812761	2958.143250	23.318887
107.977559	2960.150083	23.323904
108.226937	2965.773262	23.328922
108.476034	2962.549938	23.333939
108.302634	2955.832314	23.338957
108.310111	2949.165434	23.343975
108.325839	2958.927915	23.348992
108.390815	2961.928680	23.354010
108.600598	2972.330049	23.359027
108.568483	2976.848237	23.364045
108.537996	2981.104217	23.369063
108.376514	2980.488632	23.374080
108.626620	2972.467873	23.379098
108.514078	2981.956820	23.384115
108.503770	3003.804946	23.389133
108.992155	2999.496532	23.394151
108.649040	2999.483637	23.399168
109.179270	3008.566381	23.404186
109.495182	3024.180928	23.409203
109.083324	3023.301336	23.414221
109.667518	3016.835003	23.419239
109.551990	3036.357717	23.424256
109.985756	3037.154921	23.429274
110.193743	3041.528436	23.434291
109.968148	3048.532221	23.439309
110.450810	3044.344621	23.444327
110.047741	3041.065014	23.449344
110.259769	3044.841394	23.454362
110.693211	3057.410959	23.459379
110.597277	3069.390698	23.464397
110.634190	3058.808764	23.469415
110.448782	3069.473709	23.474432
110.720213	3071.628070	23.479450
111.125648	3080.979615	23.484467
111.478518	3082.344893	23.489485
111.691446	3079.404917	23.494503
111.719511	3089.512722	23.499520
111.631975	3089.400068	23.504538
111.794855	3089.690284	23.509555
111.431303	3101.244604	23.514573
112.069067	3108.899870	23.519591
111.698421	3114.114649	23.524608
111.960963	3113.947491	23.529626
111.870144	3114.627536	23.534643
112.039223	3137.801873	23.539661
112.428836	3136.251483	23.544679
112.317591	3135.015782	23.549696
112.615751	3133.754214	23.554714
112.829463	3164.104988	23.559731
112.834765	3167.989327	23.564749
112.952220	3163.972180	23.569767
113.715077	3158.813026	23.574784
114.537551	3141.771222	23.579802
114.294294	3132.340667	23.584819
114.300369	3135.107610	23.589837
114.817395	3126.152041	23.594855
114.532866	3115.010987	23.599872
114.530214	3101.657797	23.604890
114.757725	3108.051364	23.609907
114.843726	3111.345556	23.614925
115.005853	3097.322865	23.619943
114.588004	3100.704970	23.624960
114.668214	3104.890089	23.629978
114.688403	3101.667662	23.634995
114.473973	3100.230256	23.640013
114.378980	3108.615050	23.645031
114.689528	3118.293844	23.650048
114.670362	3122.147266	23.655066
114.838920	3132.896008	23.660083
114.789771	3132.562761	23.665101
115.114313	3147.188203	23.670119
115.320248	3154.178498	23.675136
115.319959	3159.837454	23.680154
116.106491	3148.617996	23.685171
115.741524	3155.716113	23.690189
115.870726	3144.674745	23.695207
115.941041	3161.167180	23.700224
116.147176	3172.465575	23.705242
116.138812	3173.530458	23.710259
116.325774	3170.143183	23.715277
116.291350	3175.428722	23.720295
116.716815	3175.965265	23.725312
116.337971	3174.035845	23.730330
116.565459	3186.037899	23.735347
116.775534	3201.432367	23.740365
117.047448	3193.657450	23.745383
117.194223	3198.150999	23.750400
117.064090	3195.980860	23.755418
117.055779	3217.469134	23.760435
116.896144	3224.693117	23.765453
116.980155	3229.616213	23.770471
117.398990	3242.775224	23.775488
117.466912	3243.525244	23.780506
117.801501	3249.185744	23.785523
118.195228	3261.455489	23.790541
118.203682	3271.225584	23.795559
118.147928	3276.615470	23.800576
118.277786	3275.386408	23.805594
118.701149	3276.286240	23.810611
118.553181	3289.041172	23.815629
119.031366	3296.844455	23.820647
119.194351	3299.501776	23.825664
119.064896	3295.545135	23.830682
119.108805	3300.483961	23.835699
118.720739	3300.736868	23.840717
119.290702	3309.961920	23.845735
119.138888	3320.356665	23.850752
119.675618	3322.485533	23.855770
119.643902	3325.775999	23.860787
119.528236	3345.990270	23.865805
119.987473	3341.869372	23.870823
120.250905	3350.637182	23.875840
120.411084	3343.084748	23.880858
120.461144	3341.284215	23.885875
120.352156	3359.903598	23.890893
120.732564	3362.467111	23.895911
120.426065	3355.899462	23.900928
120.443834	3365.860685	23.905946
120.665870	3376.588623	23.910963
121.183431	3391.831228	23.915981
121.523248	3387.476418	23.920999
121.586403	3389.849460	23.926016
121.337772	3386.015506	23.931034
121.765024	3385.567053	23.936051
121.583045	3398.336826	23.941069
121.905993	3397.996140	23.946087
121.983200	3398.782595	23.951104
122.476748	3404.961258	23.956122
122.407128	3396.166328	23.961139
122.006492	3400.801965	23.966157
122.718816	3404.610997	23.971175
122.909713	3421.807661	23.976192
122.806373	3425.920435	23.981210
123.100309	3426.297563	23.986227
123.015100	3429.861496	23.991245
123.369946	3425.393871	23.996263
123.291222	3431.169277	24.001280
123.218651	3434.478748	24.006298
123.610717	3412.668431	24.011315
123.389546	3430.254345	24.016333
123.789850	3435.380747	24.021351
124.159298	3440.631890	24.026368
124.184823	3434.012519	24.031386
125.096313	3430.212556	24.036403
124.772379	3438.184970	24.041421
124.501913	3432.889937	24.046439
124.580772	3433.369987	24.051456
124.711973	3433.097028	24.056474
124.562021	3427.142529	24.061491
124.417322	3437.842384	24.066509
124.566107	3430.844019	24.071527
124.769400	3437.153101	24.076544
124.927448	3454.184476	24.081562
125.036418	3452.611474	24.086579
124.952632	3456.749616	24.091597
125.283473	3459.453421	24.096615
125.282457	3477.686841	24.101632
125.321207	3477.762832	24.106650
125.503422	3483.885840	24.111667
125.228672	3505.548500	24.116685
125.462673	3505.616185	24.121703
125.904098	3522.606663	24.126720
126.035980	3534.873174	24.131738
126.566504	3524.435050	24.136755
126.950486	3528.001702	24.141773
126.554470	3543.907445	24.146791
126.918900	3541.029026	24.151808
127.173611	3544.805180	24.156826
127.422179	3538.198388	24.161843
127.311124	3542.126174	24.166861
127.654709	3541.163658	24.171879
127.881745	3549.820452	24.176896
127.641517	3556.110255	24.181914
127.905235	3560.692998	24.186931
127.848040	3558.479897	24.191949
127.914747	3558.674628	24.196967
128.405911	3568.795819	24.201984
128.550492	3587.748391	24.207002
128.462547	3586.726809	24.212019
128.397759	3585.799464	24.217037
128.459206	3595.444706	24.222055
128.396808	3600.217105	24.227072
128.403808	3616.318975	24.232090
129.076785	3606.483556	24.237107
129.032632	3617.107895	24.242125
129.331942	3635.411496	24.247143
129.601429	3645.785023	24.252160
129.462168	3644.102309	24.257178
129.786328	3638.585232	24.262195
129.740357	3646.643866	24.267213
129.547903	3656.394951	24.272231
130.030177	3668.051505	24.277248
129.940691	3684.654517	24.282266
130.474379	3686.086377	24.287283
130.444903	3695.799484	24.292301
130.420175	3698.583934	24.297319
130.973248	3696.749237	24.302336
130.638387	3705.597745	24.307354
131.286970	3694.096431	24.312371
131.176846	3702.572231	24.317389
131.311056	3702.279863	24.322407
131.590829	3696.147902	24.327424
131.516675	3693.849052	24.332442
131.799456	3703.516703	24.337459
132.255629	3720.123167	24.342477
132.619474	3724.210616	24.347495
132.621229	3725.996733	24.352512
132.577784	3736.059222	24.357530
132.483122	3735.423738	24.362547
132.277231	3729.058069	24.367565
132.407986	3739.525843	24.372583
132.556259	3720.947221	24.377600
132.633838	3738.748890	24.382618
132.840570	3751.884485	24.387635
133.461175	3754.224441	24.392653
133.152096	3763.681273	24.397671
133.442086	3755.300460	24.402688
132.939088	3759.948968	24.407706
133.575252	3763.463780	24.412723
133.500792	3787.222900	24.417741
133.279918	3786.013691	24.422759
133.710708	3787.524705	24.427776
133.915066	3802.844829	24.432794
134.062172	3805.848729	24.437811
134.061620	3820.803083	24.442829
134.036661	3824.048401	24.447847
134.609914	3831.489928	24.452864
134.159158	3840.930983	24.457882
134.971796	3851.223221	24.462899
134.872125	3854.401269	24.467917
135.088541	3853.947756	24.472935
135.167241	3863.309547	24.477952
135.547928	3873.931018	24.482970
136.320131	3856.460808	24.487987
136.596907	3867.672892	24.493005
136.395821	3865.163375	24.498023
136.283259	3859.048255	24.503040
136.371961	3861.237474	24.508058
136.552281	3855.988915	24.513075
136.559195	3860.930499	24.518093
136.284474	3878.439967	24.523111
136.922852	3876.692972	24.528128
136.680938	3888.042637	24.533146
137.022871	3888.920461	24.538163
137.049681	3900.477640	24.543181
137.095192	3908.850399	24.548199
137.525064	3909.436782	24.553216
137.006830	3913.311260	24.558234
137.611516	3924.844766	24.563251
137.521388	3922.835593	24.568269
137.658071	3930.010568	24.573287
137.953652	3943.609067	24.578304
137.904132	3963.681167	24.583322
138.474545	3951.162916	24.588339
138.760079	3968.178085	24.593357
138.732589	3984.396123	24.598375
139.123015	3983.467323	24.603392
139.015427	3996.914005	24.608410
139.363974	3989.919043	24.613427
139.218168	3990.620306	24.618445
139.221775	4003.670927	24.623463
139.656322	4008.817414	24.628480
139.546004	4015.961439	24.633498
139.633813	4007.536236	24.638515
139.661509	4023.524777	24.643533
139.838023	4035.304925	24.648551
140.252814	4035.694814	24.653568
140.362000	4041.406440	24.658586
140.340409	4053.526759	24.663603
140.541432	4052.431755	24.668621
140.468170	4068.230895	24.673639
140.882914	4065.723315	24.678656
141.442034	4083.295694	24.683674
141.092837	4082.068567	24.688691
141.532806	4080.229349	24.693709
141.644532	4082.572826	24.698727
141.527115	4089.796893	24.703744
141.898430	4105.286970	24.708762
141.554645	4099.008922	24.713779
142.084223	4098.247830	24.718797
142.193406	4115.729320	24.723815
142.458782	4106.556789	24.728832
142.595573	4112.668146	24.733850
142.546519	4124.319343	24.738867
142.714457	4126.736138	24.743885
142.932962	4127.257591	24.748903
142.919582	4130.867292	24.753920
143.068835	4135.793102	24.758938
143.225893	4151.202950	24.763955
143.117456	4155.221993	24.768973
143.117028	4157.311499	24.773991
143.521476	4164.927793	24.779008
143.673925	4177.365137	24.784026
143.716587	4181.174439	24.789043
143.923131	4191.715895	24.794061
144.073248	4204.327218	24.799079
144.249658	4204.132431	24.804096
144.155953	4213.120393	24.809114
144.710296	4226.363187	24.814131
145.003750	4237.181520	24.819149
144.418707	4246.309122	24.824167
144.783264	4244.955077	24.829184
144.763960	4251.217037	24.834202
145.366525	4255.709327	24.839219
145.830626	4260.377835	24.844237
146.381779	4257.981558	24.849255
146.665759	4261.873247	24.854272
146.748318	4259.890808	24.859290
146.890489	4260.809221	24.864307
147.180664	4254.236724	24.869325
147.192482	4258.353852	24.874343
147.270516	4264.565942	24.879360
147.275161	4254.370247	24.884378
147.246602	4251.764375	24.889395
147.104557	4251.133094	24.894413
147.242006	4259.141349	24.899431
147.554116	4259.818675	24.904448
147.274780	4272.626316	24.909466
147.564647	4278.006879	24.914483
147.904628	4284.111910	24.919501
147.855846	4286.448840	24.924519
148.156529	4305.062228	24.929536
148.131628	4306.476949	24.934554
147.897952	4307.523320	24.939571
148.324861	4319.002693	24.944589
148.572419	4336.715361	24.949607
148.535279	4339.508154	24.954624
148.918589	4360.337111	24.959642
148.954871	4370.706331	24.964659
149.193250	4368.279827	24.969677
149.175360	4378.771113	24.974695
149.489628	4378.131911	24.979712
149.588218	4385.369811	24.984730
149.709949	4391.452043	24.989747
149.976549	4403.808644	24.994765
149.811016	4416.570261	24.999783
150.803048	4406.353321	25.004800
151.526111	4410.290310	25.009818
151.300944	4404.577612	25.014835
151.494389	4397.060592	25.019853
151.089831	4402.359927	25.024871
151.243047	4411.565209	25.029888
151.638762	4420.641207	25.034906
151.327536	4424.070080	25.039923
151.712164	4421.740741	25.044941
151.528150	4431.465677	25.049959
152.003929	4434.623675	25.054976
152.205271	4444.253902	25.059994
152.190204	4438.830430	25.065011
152.394095	4438.871245	25.070029
152.430005	4437.580980	25.075047
153.007611	4434.505101	25.080064
152.964076	4437.895457	25.085082
152.937161	4449.751736	25.090099
153.423401	4454.880834	25.095117
153.653443	4457.161750	25.100135
153.386453	4455.312620	25.105152
153.447884	4462.224919	25.110170
153.581854	4474.422304	25.115187
153.890455	4481.924245	25.120205
153.652294	4486.793682	25.125223
153.397601	4492.003427	25.130240
154.000368	4498.070774	25.135258
154.116625	4509.548132	25.140275
154.715242	4496.542191	25.145293
154.805480	4517.921978	25.150311
155.093833	4526.995806	25.155328
155.028995	4529.145885	25.160346
155.165465	4529.285575	25.165363
155.525824	4535.513774	25.170381
156.234817	4544.954546	25.175399
156.323414	4540.528101	25.180416
156.687096	4537.334006	25.185434
156.169446	4548.493440	25.190451
156.983644	4538.957484	25.195469
156.686944	4535.986145	25.200487
156.782740	4547.536154	25.205504
156.703192	4544.881363	25.210522
156.606151	4533.795463	25.215539
157.064560	4539.850579	25.220557
157.166289	4559.852447	25.225575
157.594200	4551.831715	25.230592
157.810901	4558.773535	25.235610
157.853825	4556.932959	25.240627
158.146455	4549.548784	25.245645
158.279974	4566.076852	25.250663
158.229642	4575.998843	25.255680
158.534249	4573.536749	25.260698
158.422173	4579.043109	25.265715
158.956161	4566.987781	25.270733
158.979290	4571.371512	25.275751
158.891024	4572.246909	25.280768
159.304323	4581.907337	25.285786
159.174756	4598.438518	25.290803
159.281939	4595.773586	25.295821
159.019684	4611.173355	25.300839
159.515269	4622.241369	25.305856
159.745540	4623.651107	25.310874
159.556138	4633.869387	25.315891
159.857617	4640.662315	25.320909
159.808330	4655.340871	25.325927
159.659903	4666.597557	25.330944
160.403763	4668.792191	25.335962
160.323068	4682.759157	25.340979
160.601954	4702.228577	25.345997
160.643656	4713.954402	25.351015
160.848323	4730.856624	25.356032
160.837425	4727.360983	25.361050
160.877783	4752.255582	25.366067
161.439529	4749.936503	25.371085
161.531548	4760.275173	25.376103
161.873787	4772.396144	25.381120
162.126614	4779.392397	25.386138
161.900961	4801.790719	25.391155
162.576834	4800.517580	25.396173
162.366226	4805.657421	25.401191
162.915861	4808.532535	25.406208
163.206081	4819.459039	25.411226
163.138916	4828.181191	25.416243
162.987173	4832.162937	25.421261
163.205430	4834.508864	25.426279
163.211361	4843.557381	25.431296
163.711624	4848.072061	25.436314
163.961080	4856.896441	25.441331
164.384982	4866.549058	25.446349
164.249496	4876.730672	25.451367
164.149606	4880.745389	25.456384
164.359952	4887.151731	25.461402
164.801014	4906.119498	25.466419
165.032256	4910.306775	25.471437
165.109040	4899.357723	25.476455
165.043887	4911.112938	25.481472
165.479474	4923.067967	25.486490
165.604360	4925.643082	25.491507
165.786007	4931.056472	25.496525
166.074877	4942.125301	25.501543
166.236262	4951.702046	25.506560
166.709493	4953.399099	25.511578
166.419040	4958.652420	25.516595
166.970064	4958.345643	25.521613
166.705216	4966.290588	25.526631
166.535510	4971.970174	25.531648
166.874047	4977.608511	25.536666
166.931913	4996.367734	25.541683
167.121297	4998.074262	25.546701
167.857732	5004.480806	25.551719
167.826728	5027.294162	25.556736
168.201607	5024.423354	25.561754
168.375612	5028.228168	25.566771
168.292191	5027.748711	25.571789
168.229469	5033.358000	25.576807
168.637407	5052.283731	25.581824
168.711428	5056.700689	25.586842
168.829269	5070.589696	25.591859
168.895631	5069.149447	25.596877
169.202581	5077.437853	25.601895
169.342158	5097.052487	25.606912
169.818365	5101.583603	25.611930
169.685702	5107.181708	25.616947
169.908694	5116.969903	25.621965
170.554285	5124.126093	25.626983
170.532074	5129.779608	25.632000
170.652782	5128.097314	25.637018
170.727116	5146.222833	25.642035
170.569399	5145.669714	25.647053
170.870392	5152.829062	25.652071
170.820992	5171.791399	25.657088
171.441630	5178.806297	25.662106
171.306422	5181.361969	25.667123
171.481717	5192.647492	25.672141
171.508802	5202.169523	25.677159
171.866668	5222.858237	25.682176
172.270828	5223.473922	25.687194
172.503955	5230.325061	25.692212
172.491897	5229.149528	25.697229
173.142042	5242.829533	25.702247
173.059137	5255.645161	25.707264
173.372813	5251.136154	25.712282
173.110805	5257.234231	25.717300
173.521866	5259.881629	25.722317
173.711466	5276.357421	25.727335
173.712107	5280.586999	25.732352
174.129988	5279.865350	25.737370
174.255435	5292.452862	25.742388
174.170493	5306.559854	25.747405
174.612156	5308.545942	25.752423
173.977826	5309.326469	25.757440
174.832619	5323.353454	25.762458
174.551868	5333.564253	25.767476
174.822725	5332.985439	25.772493
175.358616	5350.158634	25.777511
175.320437	5369.349855	25.782528
175.397689	5363.034223	25.787546
175.954616	5368.512420	25.792564
175.768052	5383.291849	25.797581
176.131558	5375.391263	25.802599
176.202683	5385.607281	25.807616
176.432025	5393.835315	25.812634
176.766521	5398.180238	25.817652
176.674950	5396.452056	25.822669
177.037792	5426.246800	25.827687
177.711471	5430.324280	25.832704
177.715479	5418.407723	25.837722
177.768442	5425.375367	25.842740
178.010346	5431.158309	25.847757
178.499140	5433.234925	25.852775
178.691384	5436.516158	25.857792
178.801655	5434.541904	25.862810
178.841062	5444.450397	25.867828
178.739720	5440.870847	25.872845
179.280452	5455.871696	25.877863
179.106628	5459.923303	25.882880
179.425708	5462.594522	25.887898
179.469378	5468.897601	25.892916
179.249575	5470.999316	25.897933
179.597823	5484.644436	25.902951
179.609297	5490.523246	25.907968
179.893948	5509.645415	25.912986
179.766080	5523.393099	25.918004
179.804845	5530.520822	25.923021
180.542733	5549.095830	25.928039
180.202417	5566.115243	25.933056
180.731929	5571.263176	25.938074
180.950308	5575.544150	25.943092
181.209615	5584.392603	25.948109
181.538101	5595.641900	25.953127
181.726546	5611.234339	25.958144
181.925715	5610.941299	25.963162
182.363884	5616.955738	25.968180
182.522789	5625.103302	25.973197
182.553027	5636.452720	25.978215
183.136324	5644.638387	25.983232
183.153176	5638.262618	25.988250
183.414701	5637.975652	25.993268
183.751986	5651.313261	25.998285
183.839825	5651.211164	26.003303
184.008928	5663.564864	26.008320
183.995671	5662.219036	26.013338
183.963754	5657.975224	26.018356
184.027860	5674.319400	26.023373
184.428938	5682.435600	26.028391
184.325445	5692.565340	26.033408
184.846737	5701.767633	26.038426
185.213223	5712.970052	26.043444
184.933272	5725.614667	26.048461
185.577903	5715.539475	26.053479
185.719560	5732.089432	26.058496
185.786231	5743.947768	26.063514
186.076166	5734.767438	26.068532
185.433359	5740.230513	26.073549
185.874880	5756.029889	26.078567
186.198594	5773.201796	26.083584
186.442064	5771.595029	26.088602
186.507448	5780.038159	26.093620
186.249850	5793.111794	26.098637
187.067048	5794.303984	26.103655
187.340898	5811.947710	26.108672
187.206577	5814.206612	26.113690
187.180842	5820.915193	26.118708
187.445664	5836.079263	26.123725
187.936458	5837.199166	26.128743
187.958027	5844.067691	26.133760
188.074329	5865.552330	26.138778
188.255773	5871.628919	26.143796
188.213614	5888.081372	26.148813
188.481035	5888.424806	26.153831
189.023225	5921.314326	26.158848
189.118246	5924.822278	26.163866
189.279810	5938.787212	26.168884
189.260474	5961.363174	26.173901
189.532351	5956.434358	26.178919
190.043675	5975.332329	26.183936
190.172004	5966.776802	26.188954
190.484837	5982.621663	26.193972
190.498409	5995.643754	26.198989
190.765226	6000.195070	26.204007
190.876820	6013.984758	26.209024
191.150046	6029.251849	26.214042
191.574379	6029.823388	26.219060
191.663145	6050.122479	26.224077
192.253659	6045.213478	26.229095
192.128237	6057.048261	26.234112
192.280583	6064.852970	26.239130
192.690380	6072.895385	26.244148
192.173469	6078.743009	26.249165
192.497463	6084.466029	26.254183
193.033289	6103.581283	26.259200
193.184260	6094.242480	26.264218
193.548836	6118.495020	26.269236
193.484536	6133.448576	26.274253
193.820831	6125.270962	26.279271
193.909751	6137.561707	26.284288
194.200194	6148.567895	26.289306
194.496993	6150.712367	26.294324
194.597596	6166.593586	26.299341
194.963512	6169.989964	26.304359
194.977679	6170.697969	26.309376
194.985743	6172.489658	26.314394
195.555728	6194.327042	26.319412
195.684737	6205.168997	26.324429
195.680226	6192.745037	26.329447
195.920298	6219.782332	26.334464
195.945064	6230.741545	26.339482
196.091090	6234.718272	26.344500
196.308895	6245.533800	26.349517
196.220957	6257.485987	26.354535
196.515973	6276.253799	26.359552
196.968857	6282.215663	26.364570
197.054147	6294.923760	26.369588
197.260550	6315.065938	26.374605
197.879246	6323.786194	26.379623
197.679964	6340.427664	26.384640
198.195761	6344.649888	26.389658
198.726068	6351.089007	26.394676
198.529919	6365.741298	26.399693
198.959077	6366.321567	26.404711
198.846905	6367.907870	26.409728
199.168503	6374.808801	26.414746
199.489153	6384.677175	26.419764
199.461533	6384.457312	26.424781
199.796314	6385.532093	26.429799
199.986684	6392.393485	26.434816
200.081971	6407.574954	26.439834
200.507331	6408.698769	26.444852
200.663393	6411.010392	26.449869
200.586557	6411.666284	26.454887
200.903880	6435.680380	26.459904
201.004832	6437.820654	26.464922
201.320943	6436.663399	26.469940
201.468983	6461.865552	26.474957
201.327526	6469.605692	26.479975
201.274294	6472.900077	26.484992
201.631434	6483.817165	26.490010
202.080305	6485.420301	26.495028
202.530426	6514.691850	26.500045
202.723287	6517.859541	26.505063
202.477630	6521.341729	26.510080
202.336863	6544.600227	26.515098
202.981626	6552.135921	26.520116
203.019708	6571.123972	26.525133
203.654699	6582.162011	26.530151
203.941820	6589.788125	26.535168
203.867292	6597.590503	26.540186
204.093627	6596.497723	26.545204
204.436174	6617.572371	26.550221
204.749984	6619.101845	26.555239
204.908212	6628.856742	26.560256
204.983050	6645.575767	26.565274
205.264167	6637.400203	26.570292
205.370350	6667.164329	26.575309
205.831105	6661.063179	26.580327
206.278151	6668.263521	26.585344
207.063437	6671.408455	26.590362
207.598633	6664.055113	26.595380
208.011833	6666.213093	26.600397
207.566181	6663.176203	26.605415
207.676222	6650.996106	26.610432
207.461716	6652.923510	26.615450
207.890350	6649.671588	26.620468
207.634506	6669.235834	26.625485
207.724676	6667.274047	26.630503
208.017562	6678.144434	26.635520
208.116042	6694.862980	26.640538
208.345799	6701.914074	26.645556
208.477608	6721.935730	26.650573
208.672200	6730.640136	26.655591
209.201681	6742.427066	26.660608
209.148811	6749.058136	26.665626
209.186854	6763.421743	26.670644
209.243584	6784.054940	26.675661
209.593383	6790.856936	26.680679
209.681115	6800.834403	26.685696
209.809744	6822.940131	26.690714
210.008961	6834.162968	26.695732
210.002469	6850.519187	26.700749
210.187885	6858.751565	26.705767
210.691075	6869.428328	26.710784
210.943613	6893.396290	26.715802
211.918619	6898.399483	26.720820
211.817831	6919.350937	26.725837
212.200955	6936.962954	26.730855
212.843047	6933.860844	26.735872
212.450584	6937.602725	26.740890
212.800100	6950.333277	26.745908
212.849610	6964.228051	26.750925
212.764910	6960.490929	26.755943
213.508535	6979.618945	26.760960
213.398928	6998.949269	26.765978
213.454793	6987.298257	26.770996
213.408754	7014.498072	26.776013
213.887339	7021.128576	26.781031
213.901586	7030.451524	26.786048
214.086108	7048.182959	26.791066
214.294490	7054.135790	26.796084
214.428179	7069.337084	26.801101
214.841091	7089.432180	26.806119
215.258228	7092.732366	26.811136
215.357378	7108.762999	26.816154
215.477212	7123.006822	26.821172
215.843155	7130.279954	26.826189
215.904579	7147.093073	26.831207
216.461917	7153.272566	26.836224
216.332009	7166.775568	26.841242
216.674060	7174.765881	26.846260
216.813205	7186.121403	26.851277
216.996567	7202.966098	26.856295
217.981151	7219.900733	26.861312
217.754766	7230.372453	26.866330
217.776256	7232.057980	26.871348
218.085855	7243.765821	26.876365
218.978560	7257.254896	26.881383
218.900142	7255.069903	26.886400
218.894764	7268.556749	26.891418
219.273402	7273.132014	26.896436
219.593165	7276.712569	26.901453
219.669091	7288.488388	26.906471
220.035011	7291.758702	26.911488
220.090686	7310.015546	26.916506
220.451280	7304.469600	26.921524
220.467186	7325.453859	26.926541
220.655293	7326.400004	26.931559
221.361351	7320.591917	26.936576
221.382943	7347.320794	26.941594
221.685902	7346.860041	26.946612
221.805146	7342.608090	26.951629
221.825522	7358.932166	26.956647
221.929234	7375.259067	26.961664
222.253820	7378.188577	26.966682
222.681165	7390.421162	26.971700
222.773723	7393.967662	26.976717
222.715008	7402.010998	26.981735
223.019541	7411.885594	26.986752
223.187859	7424.171156	26.991770
223.644401	7438.564842	26.996788
223.822205	7450.921553	27.001805
223.665984	7457.985677	27.006823
224.202731	7475.867886	27.011840
224.596375	7482.975845	27.016858
225.167048	7493.348878	27.021876
225.265558	7502.324316	27.026893
225.153663	7517.447411	27.031911
225.703378	7516.676745	27.036928
225.162235	7535.932758	27.041946
225.681942	7542.115086	27.046964
225.918932	7558.490852	27.051981
225.899666	7571.509704	27.056999
226.664968	7579.055472	27.062016
226.252899	7594.136970	27.067034
227.030080	7607.025537	27.072052
227.375427	7614.027418	27.077069
227.147973	7620.408175	27.082087
227.626309	7633.384327	27.087104
228.046545	7637.176609	27.092122
227.972245	7644.935199	27.097140
228.314903	7656.461370	27.102157
228.442738	7672.052375	27.107175
228.545978	7681.200795	27.112192
228.589234	7687.927730	27.117210
228.784242	7688.995941	27.122228
229.426485	7707.742732	27.127245
229.576597	7719.434667	27.132263
230.224712	7731.794112	27.137280
229.933828	7744.350266	27.142298
230.401796	7742.771517	27.147316
230.464403	7757.656127	27.152333
230.958943	7774.402389	27.157351
230.992060	7772.951321	27.162368
230.915912	7797.454646	27.167386
231.024635	7803.985172	27.172404
231.529918	7814.867364	27.177421
231.823194	7822.679295	27.182439
232.272045	7845.434083	27.187456
232.364843	7856.213200	27.192474
232.486290	7861.690502	27.197492
232.580395	7874.136295	27.202509
232.771409	7888.334903	27.207527
233.534453	7900.452425	27.212544
233.054773	7923.411852	27.217562
233.716299	7934.007762	27.222580
233.834712	7941.060884	27.227597
234.194461	7961.007363	27.232615
234.142416	7966.619044	27.237632
234.715547	7994.172200	27.242650
234.419317	8003.925971	27.247668
234.691228	8010.825786	27.252685
234.714557	8036.011633	27.257703
235.205938	8044.762008	27.262720
235.660697	8060.425567	27.267738
235.930176	8085.459507	27.272756
236.376608	8101.089669	27.277773
236.309043	8119.123414	27.282791
236.850779	8127.528192	27.287808
236.904829	8143.055315	27.292826
237.204363	8149.707793	27.297844
237.890256	8155.037323	27.302861
238.085823	8171.268548	27.307879
238.202508	8173.223470	27.312896
238.271498	8182.197522	27.317914
239.093928	8194.132359	27.322932
239.442802	8199.899526	27.327949
239.302194	8204.173868	27.332967
239.869829	8193.323222	27.337984
240.179522	8198.711334	27.343002
240.884398	8211.245372	27.348020
240.921045	8212.366682	27.353037
241.299553	8216.863280	27.358055
241.118499	8208.301209	27.363072
241.519065	8202.063702	27.368090
241.477085	8218.354051	27.373108
241.580682	8215.035653	27.378125
241.260013	8236.840503	27.383143
241.947677	8241.866710	27.388160
241.943873	8254.558465	27.393178
242.009888	8263.065782	27.398196
242.322488	8280.835292	27.403213
242.132443	8293.464516	27.408231
242.620162	8303.371056	27.413248
242.559394	8322.998240	27.418266
243.038639	8338.516157	27.423284
243.414524	8350.192285	27.428301
243.185532	8383.364141	27.433319
243.950309	8388.889823	27.438336
244.027433	8396.577798	27.443354
244.229108	8411.734891	27.448372
244.595876	8423.033639	27.453389
244.751003	8449.970634	27.458407
245.393017	8461.797980	27.463424
245.064574	8466.398389	27.468442
245.499997	8477.557043	27.473460
245.433363	8498.643885	27.478477
245.775044	8519.465131	27.483495
245.798612	8525.346187	27.488512
246.488304	8549.674453	27.493530
246.303908	8570.470318	27.498548
246.833053	8581.431335	27.503565
246.861325	8600.801856	27.508583
247.377835	8607.076598	27.513600
247.594493	8626.512530	27.518618
247.687955	8651.814580	27.523636
248.058002	8665.771232	27.528653
248.319540	8690.889315	27.533671
248.428225	8699.014495	27.538688
248.824226	8715.205522	27.543706
249.162829	8740.482157	27.548724
249.346203	8738.111003	27.553741
249.361154	8766.790901	27.558759
249.942805	8792.165523	27.563776
250.241824	8804.169617	27.568794
250.626855	8818.982786	27.573812
250.980646	8824.376845	27.578829
251.059174	8853.230092	27.583847
251.640450	8860.533530	27.588864
251.791461	8871.534647	27.593882
251.909303	8883.819569	27.598900
252.511241	8889.607540	27.603917
252.450041	8911.805315	27.608935
252.824395	8912.886719	27.613952
253.342122	8924.680043	27.618970
253.614473	8941.452488	27.623988
253.934466	8950.255236	27.629005
253.694630	8962.719025	27.634023
253.835706	8964.704963	27.639040
254.221619	8979.480238	27.644058
254.601425	8996.201276	27.649076
254.979253	9007.034561	27.654093
254.931232	9019.566396	27.659111
255.492174	9042.952427	27.664128
256.012611	9045.059271	27.669146
255.840921	9057.973458	27.674164
256.234343	9063.089902	27.679181
256.661620	9080.106712	27.684199
256.777339	9094.289556	27.689216
256.822732	9102.105894	27.694234
256.769740	9120.940265	27.699252
256.935525	9131.292018	27.704269
257.394406	9146.949544	27.709287
257.671567	9162.461732	27.714304
258.056297	9173.628700	27.719322
258.040356	9194.118051	27.724340
258.426135	9208.966145	27.729357
258.696178	9224.378463	27.734375
259.100521	9238.481753	27.739392
259.234132	9256.902034	27.744410
259.480571	9279.506989	27.749428
260.456694	9270.366463	27.754445
261.812814	9235.281017	27.759463
262.452473	9234.171095	27.764480
262.326298	9237.152140	27.769498
262.087841	9236.352573	27.774516
262.486093	9233.976318	27.779533
262.464143	9242.513566	27.784551
262.737390	9243.610732	27.789568
262.887204	9242.043507	27.794586
263.028682	9240.455481	27.799604
263.290989	9244.604190	27.804621
263.090601	9237.001278	27.809639
262.917040	9253.003618	27.814656
263.264593	9268.350234	27.819674
263.308730	9278.468433	27.824692
263.625668	9285.494318	27.829709
263.617710	9305.212194	27.834727
263.851442	9323.923203	27.839744
264.044057	9343.332059	27.844762
264.348449	9365.394529	27.849780
264.742396	9379.982599	27.854797
265.220387	9396.196189	27.859815
265.213749	9406.423393	27.864832
265.457024	9425.527671	27.869850
265.784855	9452.934920	27.874868
266.455618	9461.553857	27.879885
266.811372	9479.557751	27.884903
266.844336	9490.410281	27.889920
267.305923	9500.062643	27.894938
267.456144	9513.738437	27.899956
267.935845	9531.682042	27.904973
268.032470	9544.046479	27.909991
268.083799	9562.041018	27.915008
268.890823	9572.517350	27.920026
268.894089	9598.036798	27.925044
269.238397	9599.779630	27.930061
269.447386	9621.336312	27.935079
269.733165	9636.127702	27.940096
270.349691	9649.450004	27.945114
270.342820	9656.933730	27.950132
270.338196	9669.768658	27.955149
270.910785	9679.369102	27.960167
271.208806	9700.498414	27.965184
271.263692	9697.897720	27.970202
271.360940	9731.065396	27.975220
271.426211	9742.579227	27.980237
272.153346	9767.758889	27.985255
272.061047	9779.594058	27.990272
272.699066	9795.745196	27.995290
273.032821	9816.253408	28.000308
273.357140	9816.468090	28.005325
273.216862	9844.431860	28.010343
273.666251	9864.385383	28.015360
274.109850	9877.516919	28.020378
274.676369	9902.276591	28.025396
274.558367	9906.446771	28.030413
274.577492	9928.071256	28.035431
275.021296	9942.721468	28.040448
275.199746	9957.311969	28.045466
275.199658	9968.138351	28.050484
275.798023	9982.931869	28.055501
276.339903	10010.537101	28.060519
276.420824	10023.071640	28.065536
276.637751	10037.971946	28.070554
276.765108	10059.939668	28.075572
277.109718	10075.445276	28.080589
277.645086	10091.470574	28.085607
277.878609	10106.355723	28.090624
277.970343	10119.737965	28.095642
278.402382	10139.745003	28.100660
278.711911	10147.299645	28.105677
278.658347	10174.331624	28.110695
279.275231	10189.779152	28.115712
279.635924	10209.727911	28.120730
279.740620	10223.941750	28.125748
280.314371	10243.690036	28.130765
280.576351	10248.325255	28.135783
280.594336	10267.951706	28.140800
280.830862	10277.907888	28.145818
281.255343	10290.998490	28.150836
281.555710	10301.263639	28.155853
281.678985	10321.555744	28.160871
281.711766	10331.922559	28.165888
282.139360	10352.274671	28.170906
282.489084	10367.419786	28.175924
282.912500	10376.440758	28.180941
283.453794	10362.239823	28.185959
284.223686	10374.342126	28.190976
284.908038	10384.165497	28.195994
284.985428	10384.507038	28.201012
285.582024	10371.011053	28.206029
286.330079	10369.656864	28.211047
286.225014	10372.123307	28.216064
286.175091	10365.971002	28.221082
286.337102	10375.149493	28.226100
286.504398	10393.660379	28.231117
286.542392	10396.814964	28.236135
286.790618	10403.504661	28.241152
286.839707	10415.289806	28.246170
286.920654	10436.343241	28.251188
287.428825	10449.670360	28.256205
287.530957	10457.251103	28.261223
287.484275	10481.642878	28.266240
288.423841	10483.403631	28.271258
288.676052	10502.248718	28.276276
288.712081	10525.386816	28.281293
289.106982	10530.250847	28.286311
288.735223	10553.698743	28.291328
289.351382	10567.451172	28.296346
289.827101	10587.691855	28.301364
289.375907	10609.693464	28.306381
290.061620	10623.251975	28.311399
290.656214	10651.462491	28.316416
291.014489	10673.508654	28.321434
290.928265	10680.882005	28.326452
291.637033	10703.350408	28.331469
291.824556	10722.300512	28.336487
292.350755	10740.266463	28.341504
292.929076	10750.308613	28.346522
293.061496	10772.232183	28.351540
293.188312	10774.757302	28.356557
293.478269	10785.974730	28.361575
293.576872	10805.541834	28.366592
294.247924	10808.642136	28.371610
294.625822	10820.780500	28.376628
294.563540	10834.417727	28.381645
295.243254	10852.950332	28.386663
294.968931	10863.011618	28.391680
295.441239	10890.101691	28.396698
295.824838	10905.185137	28.401716
296.107138	10924.019651	28.406733
296.271945	10939.822357	28.411751
296.384237	10959.198042	28.416768
296.762979	10966.445440	28.421786
296.876941	10996.610005	28.426804
297.011196	11014.441477	28.431821
297.453348	11032.076629	28.436839
297.863380	11055.090849	28.441856
298.128992	11076.911945	28.446874
298.339565	11100.718230	28.451892
298.555217	11111.158047	28.456909
298.896287	11131.685514	28.461927
299.374686	11159.242341	28.466944
299.863659	11160.732303	28.471962
300.186165	11185.001210	28.476980
300.531207	11204.438796	28.481997
300.891824	11208.784196	28.487015
301.126107	11223.919562	28.492032
301.520089	11233.671763	28.497050
301.852399	11252.893514	28.502068
301.844913	11267.599241	28.507085
302.317320	11273.123955	28.512103
302.273990	11298.940319	28.517120
303.216125	11308.768255	28.522138
303.104357	11325.905777	28.527156
302.759868	11345.918175	28.532173
303.215269	11355.705084	28.537191
303.302094	11387.709036	28.542208
303.698630	11407.773484	28.547226
303.911935	11431.908150	28.552244
304.598488	11458.021584	28.557261
305.001703	11471.798361	28.562279
305.214304	11502.696726	28.567296
305.824975	11526.033937	28.572314
305.798854	11539.053478	28.577332
305.793176	11565.770571	28.582349
306.227927	11586.261849	28.587367
306.662796	11613.368272	28.592384
307.134457	11632.609766	28.597402
307.485367	11661.743872	28.602420
307.999974	11680.293532	28.607437
308.444441	11689.924438	28.612455
308.478201	11718.037581	28.617472
309.212328	11732.735575	28.622490
309.406371	11732.260106	28.627508
309.380289	11760.183699	28.632525
309.905402	11769.075841	28.637543
310.250045	11782.713558	28.642560
310.569098	11810.927675	28.647578
310.854029	11831.609900	28.652596
310.737368	11848.464475	28.657613
311.415846	11869.372817	28.662631
311.406733	11894.609984	28.667648
311.834658	11912.083985	28.672666
312.740226	11921.715851	28.677684
312.906345	11940.919974	28.682701
313.107514	11957.453608	28.687719
313.842959	11975.972337	28.692736
314.520335	11979.412881	28.697754
314.653576	11996.730749	28.702772
314.789177	12010.827460	28.707789
315.253838	12011.784477	28.712807
315.065711	12038.846412	28.717824
315.297991	12053.101774	28.722842
315.581286	12063.155831	28.727860
315.974113	12095.185975	28.732877
315.892990	12106.676689	28.737895
316.250736	12129.024628	28.742912
316.852764	12149.171555	28.747930
317.092082	12164.553197	28.752948
317.455912	12182.015324	28.757965
317.422701	12191.657703	28.762983
317.792854	12224.945199	28.768000
318.042399	12250.060474	28.773018
318.692637	12267.133903	28.778036
318.404277	12298.781001	28.783053
318.911336	12317.499825	28.788071
319.686242	12348.978317	28.793088
319.945729	12354.643863	28.798106
320.202409	12380.692884	28.803124
320.013699	12405.485039	28.808141
320.797456	12421.198949	28.813159
321.060175	12444.165182	28.818176
321.198965	12466.449721	28.823194
321.465210	12486.646129	28.828212
321.795654	12510.527114	28.833229
322.398444	12519.767503	28.838247
322.692954	12538.453325	28.843264
323.461223	12554.125550	28.848282
323.767574	12562.619517	28.853300
324.121890	12568.308258	28.858317
324.892222	12590.140955	28.863335
324.942386	12597.869596	28.868352
325.117998	12621.016967	28.873370
325.764659	12628.381189	28.878388
325.707884	12632.270873	28.883405
325.864661	12648.988862	28.888423
326.002641	12674.829411	28.893440
326.374547	12682.166958	28.898458
326.569590	12701.563136	28.903476
326.542245	12721.521304	28.908493
327.238663	12740.274225	28.913511
327.260187	12766.751954	28.918528
327.739975	12795.318300	28.923546
328.005647	12818.821354	28.928564
328.153072	12847.824773	28.933581
328.751940	12871.585483	28.938599
328.858540	12891.684025	28.943616
328.973575	12924.453544	28.948634
329.693432	12947.513428	28.953652
330.090698	12975.009765	28.958669
330.503632	12995.575451	28.963687
330.633188	13018.361014	28.968704
331.642122	13041.094963	28.973722
331.934791	13043.796670	28.978740
332.353712	13077.018081	28.983757
332.557228	13077.340037	28.988775
332.788724	13103.482397	28.993792
333.078321	13118.970673	28.998810
333.951337	13125.403026	29.003828
334.280579	13136.748376	29.008845
334.938743	13148.573043	29.013863
335.375288	13165.184777	29.018880
335.470642	13168.176164	29.023898
335.638769	13182.335003	29.028916
335.626958	13203.765977	29.033933
336.046011	13214.686871	29.038951
336.488007	13242.239791	29.043968
336.509151	13254.280539	29.048986
337.221091	13266.899005	29.054004
336.818848	13294.611856	29.059021
337.145069	13315.219811	29.064039
337.710842	13333.722087	29.069056
337.838024	13361.052615	29.074074
338.409784	13382.569781	29.079092
338.444826	13411.774719	29.084109
338.722690	13427.621916	29.089127
338.762666	13459.804050	29.094144
338.938206	13483.123015	29.099162
339.980466	13503.092331	29.104180
340.457777	13534.110714	29.109197
340.609438	13553.593469	29.114215
341.351619	13581.336993	29.119232
341.525513	13601.741605	29.124250
342.012155	13613.678532	29.129268
342.083472	13633.278089	29.134285
342.382919	13659.925381	29.139303
342.695867	13682.692668	29.144320
342.864054	13705.523572	29.149338
343.398768	13724.732129	29.154356
344.152434	13733.595940	29.159373
344.912592	13750.034648	29.164391
345.146470	13762.238392	29.169408
344.965250	13776.287849	29.174426
345.302649	13786.773359	29.179444
345.576888	13802.611961	29.184461
345.957787	13816.236035	29.189479
346.214311	13839.460725	29.194496
346.272011	13861.462686	29.199514
346.656428	13875.976800	29.204532
347.280338	13904.582389	29.209549
347.761611	13922.362591	29.214567
347.802268	13947.620016	29.219584
347.929982	13972.188114	29.224602
348.569571	13991.497459	29.229620
348.889413	14010.989240	29.234637
349.402572	14022.814926	29.239655
350.436016	14040.193477	29.244672
350.821227	14045.855750	29.249690
351.184763	14061.039594	29.254708
351.182129	14079.103707	29.259725
351.406331	14095.474572	29.264743
352.010939	14106.619736	29.269760
352.017413	14127.022556	29.274778
352.316437	14144.698704	29.279796
352.680253	14164.253272	29.284813
353.045803	14167.066958	29.289831
353.544772	14190.380654	29.294848
353.758513	14221.254873	29.299866
354.178366	14240.080767	29.304884
354.189095	14265.033787	29.309901
354.742147	14292.593054	29.314919
354.907633	14303.291938	29.319936
355.454711	14332.099617	29.324954
355.953400	14363.479205	29.329972
356.279480	14379.512334	29.334989
356.747157	14411.256847	29.340007
357.170644	14418.972324	29.345024
357.419077	14442.994842	29.350042
357.736531	14445.238134	29.355060
358.506010	14472.050247	29.360077
358.763266	14487.209924	29.365095
358.996076	14495.804638	29.370112
359.568944	14515.023848	29.375130
359.608466	14533.779763	29.380148
359.769041	14554.522230	29.385165
360.434969	14573.265932	29.390183
360.906582	14592.017797	29.395200
360.775540	14616.595431	29.400218
360.931338	14639.400965	29.405236
361.266108	14662.267090	29.410253
361.650851	14692.676478	29.415271
362.407189	14715.398084	29.420288
362.415812	14746.920920	29.425306
362.899270	14768.544995	29.430324
363.383774	14787.651914	29.435341
363.553216	14802.017035	29.440359
364.017060	14833.327030	29.445376
364.179122	14857.527740	29.450394
364.670246	14884.813276	29.455412
365.152801	14911.894907	29.460429
365.320098	14941.687969	29.465447
365.864873	14956.320063	29.470464
365.721960	14990.286031	29.475482
366.524524	15009.021525	29.480500
367.064610	15034.537405	29.485517
367.007102	15049.506513	29.490535
367.173042	15083.516150	29.495552
367.526454	15112.588866	29.500570
368.205735	15125.665281	29.505588
368.702178	15160.106802	29.510605
368.804204	15184.478340	29.515623
369.317452	15205.226616	29.520640
369.451124	15235.897031	29.525658
369.498846	15261.170889	29.530676
371.099123	15254.292671	29.535693
371.700365	15267.586615	29.540711
372.492017	15285.499792	29.545728
372.645747	15294.688287	29.550746
372.663424	15304.036929	29.555764
373.502469	15328.884496	29.560781
373.896791	15331.194882	29.565799
374.819785	15324.987398	29.570816
374.909176	15347.440925	29.575834
375.062761	15350.284630	29.580852
375.139583	15358.904019	29.585869
375.254218	15377.121649	29.590887
375.565366	15380.259809	29.595904
375.928974	15399.894637	29.600922
376.156174	15409.687602	29.605940
376.332109	15433.359461	29.610957
376.453397	15457.974692	29.615975
377.026820	15484.755593	29.620992
376.840812	15518.384961	29.626010
377.445345	15533.699851	29.631028
378.233840	15562.686571	29.636045
378.168076	15590.306158	29.641063
378.445420	15616.950160	29.646080
378.675715	15655.037576	29.651098
379.033265	15688.513139	29.656116
379.413646	15717.014090	29.661133
379.993375	15753.686088	29.666151
380.160572	15789.917055	29.671168
380.737596	15821.511089	29.676186
381.110207	15844.574871	29.681204
382.028767	15863.580554	29.686221
382.573766	15890.710704	29.691239
382.779185	15909.606375	29.696256
383.211431	15935.468713	29.701274
383.470822	15963.985709	29.706292
383.791294	15991.760511	29.711309
384.009001	16012.208260	29.716327
384.868901	16036.993497	29.721344
384.802306	16061.774561	29.726362
385.423349	16096.157314	29.731380
385.990495	16122.485287	29.736397
386.177387	16141.608313	29.741415
387.040098	16162.290592	29.746432
387.322365	16181.686219	29.751450
387.706187	16207.622789	29.756468
388.275944	16229.813065	29.761485
388.541930	16249.438697	29.766503
388.996541	16255.867785	29.771520
389.066154	16287.481574	29.776538
389.359464	16305.356434	29.781556
390.008551	16336.362118	29.786573
390.147232	16355.549714	29.791591
390.237003	16383.683153	29.796608
390.400627	16412.515772	29.801626
390.811993	16439.272706	29.806644
391.765932	16459.142032	29.811661
392.016917	16496.144570	29.816679
392.704560	16514.732043	29.821696
393.027436	16529.166170	29.826714
393.644786	16539.723319	29.831732
394.303778	16557.374090	29.836749
394.337873	16584.003613	29.841767
394.572282	16597.841991	29.846784
394.849417	16623.669396	29.851802
395.068546	16644.297629	29.856820
395.344577	16670.194754	29.861837
395.429127	16701.064667	29.866855
395.982993	16722.105160	29.871872
395.996421	16751.950262	29.876890
396.838142	16781.934927	29.881908
397.126097	16811.828978	29.886925
397.514948	16836.530661	29.891943
397.869032	16866.733506	29.896960
398.360843	16901.390499	29.901978
398.643339	16928.288198	29.906996
399.257704	16957.272556	29.912013
399.492663	16989.512403	29.917031
399.664634	17012.807811	29.922048
400.224261	17044.409728	29.927066
400.565150	17076.598486	29.932084
401.515193	17096.434338	29.937101
401.785428	17134.370022	29.942119
402.865094	17150.044954	29.947136
403.263166	17176.031150	29.952154
403.581162	17193.621887	29.957172
404.521059	17202.726810	29.962189
404.456273	17235.872849	29.967207
404.850924	17254.787762	29.972224
404.932056	17270.659307	29.977242
404.931254	17301.767726	29.982260
405.932608	17320.114472	29.987277
405.753248	17350.034731	29.992295
405.905644	17376.511116	29.997312
406.559208	17410.458440	30.002330
407.266021	17437.287634	30.007348
407.679578	17468.518169	30.012365
407.502870	17498.700406	30.017383
407.999931	17530.834024	30.022400
408.239177	17565.446251	30.027418
408.817720	17599.102364	30.032436
409.412023	17625.447122	30.037453
409.860234	17669.193211	30.042471
410.501865	17698.765097	30.047488
410.746919	17733.117715	30.052506
410.973953	17760.890667	30.057524
411.644312	17788.057678	30.062541
411.960051	17818.116369	30.067559
412.306057	17848.467306	30.072576
412.509679	17873.167569	30.077594
412.966690	17915.819963	30.082612
413.613738	17949.143842	30.087629
413.842398	17983.095151	30.092647
414.604779	18004.436243	30.097664
414.948185	18036.998931	30.102682
415.328400	18071.122637	30.107700
416.330626	18091.478890	30.112717
416.611128	18117.064555	30.117735
416.674867	18141.603735	30.122752
417.162312	18161.320027	30.127770
417.771809	18193.740477	30.132788
418.618021	18218.581203	30.137805
418.737209	18237.817927	30.142823
418.913561	18271.234592	30.147840
419.484139	18290.047323	30.152858
419.692922	18316.219298	30.157876
420.939798	18319.600791	30.162893
421.711248	18347.277195	30.167911
422.098784	18359.504174	30.172928
422.264391	18371.367713	30.177946
422.528424	18383.860313	30.182964
422.598476	18391.493440	30.187981
423.000824	18422.935737	30.192999
423.495633	18439.738834	30.198016
423.436655	18450.121202	30.203034
424.124765	18478.714162	30.208052
424.269396	18507.259106	30.213069
424.418007	18532.556298	30.218087
424.552930	18555.884604	30.223104
425.344683	18584.752189	30.228122
425.539225	18619.714404	30.233140
426.337248	18646.332079	30.238157
426.450347	18682.039916	30.243175
426.919614	18707.748594	30.248192
427.377887	18747.521836	30.253210
427.603828	18774.310876	30.258228
428.001042	18801.907206	30.263245
428.753805	18836.814496	30.268263
428.717877	18863.423313	30.273280
429.224712	18896.473726	30.278298
429.608729	18924.552420	30.283316
430.747251	18966.772516	30.288333
430.926963	18994.137641	30.293351
431.344157	19032.768057	30.298368
431.914475	19061.601332	30.303386
431.979328	19090.563881	30.308404
432.671960	19129.884456	30.313421
433.019663	19161.633386	30.318439
433.727339	19195.935528	30.323456
434.228046	19221.134579	30.328474
434.275120	19252.456633	30.333492
435.016623	19272.020786	30.338509
435.556150	19306.766269	30.343527
436.201396	19334.855430	30.348544
436.925340	19357.208518	30.353562
437.459627	19382.737390	30.358580
437.683398	19404.252327	30.363597
438.066380	19432.938421	30.368615
438.369561	19450.719890	30.373632
438.877960	19471.268198	30.378650
439.066529	19505.784374	30.383668
439.595287	19531.459610	30.388685
439.844165	19557.816549	30.393703
440.229080	19592.283358	30.398720
441.185671	19617.847880	30.403738
441.091937	19652.964232	30.408756
441.598618	19679.963527	30.413773
442.105679	19715.201266	30.418791
442.329851	19749.206903	30.423808
442.778432	19776.739759	30.428826
442.862337	19812.593205	30.433844
443.809811	19845.064883	30.438861
444.535811	19880.502599	30.443879
444.727225	19905.270526	30.448896
445.391905	19931.613781	30.453914
445.525180	19968.123208	30.458932
446.035435	19989.069802	30.463949
446.325420	20040.553745	30.468967
446.792818	20066.030746	30.473984
447.191104	20095.423043	30.479002
447.405031	20140.291542	30.484020
447.971157	20164.540250	30.489037
448.689509	20199.025719	30.494055
449.009017	20237.528415	30.499072
449.595559	20264.655083	30.504090
449.877204	20295.556892	30.509108
450.204756	20328.258563	30.514125
450.705367	20358.235539	30.519143
451.333002	20386.948128	30.524160
451.999364	20418.971718	30.529178
452.102293	20452.991135	30.534196
452.443756	20480.156255	30.539213
452.524524	20507.513632	30.544231
453.693550	20534.208816	30.549248
454.246364	20552.344150	30.554266
454.794025	20584.430717	30.559284
455.354557	20614.556710	30.564301
455.749823	20642.099086	30.569319
456.559413	20666.620104	30.574336
456.912364	20681.324326	30.579354
457.278421	20719.732270	30.584372
457.139012	20730.715960	30.589389
458.085784	20767.308732	30.594407
458.067304	20800.362016	30.599424
458.492965	20831.393887	30.604442
458.994142	20860.284813	30.609460
459.517618	20900.279748	30.614477
459.834623	20932.257473	30.619495
460.143815	20971.938411	30.624512
460.888848	20997.714590	30.629530
461.227285	21038.465213	30.634548
461.575366	21069.996045	30.639565
462.048422	21107.800491	30.644583
462.858462	21132.119838	30.649600
463.944937	21142.161036	30.654618
464.684823	21173.548903	30.659636
465.208832	21203.940539	30.664653
465.614027	21230.092164	30.669671
465.780824	21252.079241	30.674688
466.270324	21263.230691	30.679706
466.399511	21293.810299	30.684724
466.860323	21317.994693	30.689741
466.832149	21347.297299	30.694759
467.627991	21395.982832	30.699776
468.007987	21422.410326	30.704794
468.064284	21458.018341	30.709812
468.734316	21497.606255	30.714829
469.144822	21534.144938	30.719847
469.368773	21578.516008	30.724864
469.823515	21606.928742	30.729882
470.317514	21653.665271	30.734900
470.942139	21700.741729	30.739917
471.624594	21736.069532	30.744935
471.724004	21791.934858	30.749952
472.282736	21806.696348	30.754970
472.605449	21856.227533	30.759988
473.259692	21893.145961	30.765005
473.802198	21930.941176	30.770023
474.167644	21982.209947	30.775040
474.744263	22016.916554	30.780058
475.355188	22054.360151	30.785076
475.953749	22094.680711	30.790093
476.153699	22136.510373	30.795111
476.806421	22163.212334	30.800128
477.592862	22197.576981	30.805146
477.905681	22237.563198	30.810164
478.638262	22266.748736	30.815181
479.426632	22297.486345	30.820199
479.573784	22336.936191	30.825216
480.144895	22356.125566	30.830234
480.571159	22383.697147	30.835252
481.182299	22422.676855	30.840269
481.519879	22443.791965	30.845287
481.932295	22486.853036	30.850304
482.681205	22515.764695	30.855322
482.947336	22542.015534	30.860340
483.043740	22567.698868	30.865357
483.728764	22597.549450	30.870375
483.679593	22638.635428	30.875392
484.536988	22666.133968	30.880410
485.022709	22692.654124	30.885428
485.241147	22736.523148	30.890445
485.761748	22768.276273	30.895463
486.280794	22800.573110	30.900480
486.713815	22829.016260	30.905498
487.118138	22867.504576	30.910516
487.829769	22905.452255	30.915533
488.453106	22943.653870	30.920551
488.514564	22982.454860	30.925568
489.168500	23012.601577	30.930586
489.477042	23055.825390	30.935604
490.014388	23094.609384	30.940621
491.270619	23119.202948	30.945639
491.866360	23148.771272	30.950656
492.266577	23174.281715	30.955674
492.718531	23207.310021	30.960692
493.583358	23238.669088	30.965709
494.066234	23265.999284	30.970727
494.485507	23291.974516	30.975744
495.287468	23316.234630	30.980762
495.620836	23336.612026	30.985780
496.092836	23365.561717	30.990797
496.391547	23395.688490	30.995815
496.802577	23428.306479	31.000832
497.477695	23454.501176	31.005850
497.859056	23487.964315	31.010868
498.242216	23518.046531	31.015885
499.810171	23519.698118	31.020903
500.924897	23534.943063	31.025920
501.491237	23550.304986	31.030938
501.585045	23566.201775	31.035956
501.882316	23593.011556	31.040973
502.286515	23607.602560	31.045991
502.525054	23625.025042	31.051008
502.873542	23643.258226	31.056026
503.431277	23671.556788	31.061044
503.661427	23705.119662	31.066061
503.751367	23722.325236	31.071079
504.439763	23778.369872	31.076096
504.747467	23795.465779	31.081114
505.080427	23836.621127	31.086132
505.325365	23879.610186	31.091149
506.115149	23907.316871	31.096167
506.056882	23947.086259	31.101184
506.757731	23991.742364	31.106202
507.074529	24026.657240	31.111220
507.566007	24074.139221	31.116237
508.630293	24113.001153	31.121255
509.108662	24152.851709	31.126272
509.475236	24189.579069	31.131290
510.606780	24230.661465	31.136308
511.556503	24242.823554	31.141325
512.276727	24265.056423	31.146343
512.360150	24297.663645	31.151360
513.028227	24315.765541	31.156378
513.146102	24354.042237	31.161396
513.641426	24381.435221	31.166413
513.949647	24407.599822	31.171431
514.846032	24451.253338	31.176448
515.628818	24479.322113	31.181466
515.657907	24515.167345	31.186484
515.736010	24545.772556	31.191501
516.252088	24578.173855	31.196519
516.219063	24620.386259	31.201536
516.897851	24655.239562	31.206554
517.316659	24690.607355	31.211572
518.006401	24725.206298	31.216589
518.308103	24757.135704	31.221607
518.798919	24796.359981	31.226624
519.705685	24831.727894	31.231642
519.895987	24869.381311	31.236660
520.560910	24914.847650	31.241677
521.164518	24949.011704	31.246695
521.543892	24996.405897	31.251712
522.088923	25032.866882	31.256730
522.616101	25071.390888	31.261748
522.936008	25121.360372	31.266765
523.602252	25159.919775	31.271783
523.839893	25210.913422	31.276800
524.502957	25252.197243	31.281818
524.960404	25289.399086	31.286836
525.542733	25335.504880	31.291853
525.757659	25371.284792	31.296871
526.595870	25425.964640	31.301888
527.503532	25465.833137	31.306906
527.760685	25506.529746	31.311924
528.097998	25568.637761	31.316941
528.200821	25606.179783	31.321959
529.054303	25656.269764	31.326976
529.518514	25712.329439	31.331994
530.345255	25758.265440	31.337012
530.609639	25810.438240	31.342029
531.507440	25847.351371	31.347047
532.139438	25891.245099	31.352064
533.361018	25930.838137	31.357082
534.183299	25965.582903	31.362100
534.590704	25993.832317	31.367117
535.214098	26028.165764	31.372135
535.800259	26067.529359	31.377152
535.961391	26102.693280	31.382170
536.570409	26135.569256	31.387188
537.076466	26178.269798	31.392205
538.082054	26219.988919	31.397223
537.981936	26238.433343	31.402240
538.263608	26295.060250	31.407258
539.194518	26327.981230	31.412276
539.489622	26368.035356	31.417293
540.574899	26406.001041	31.422311
540.988986	26447.275516	31.427328
541.030897	26489.853054	31.432346
541.620512	26519.989800	31.437364
541.875231	26573.095119	31.442381
542.709438	26613.211168	31.447399
542.999432	26658.569177	31.452416
543.520223	26701.843657	31.457434
544.058240	26750.961621	31.462452
544.344630	26803.316845	31.467469
545.363946	26853.023741	31.472487
545.718641	26898.226852	31.477504
545.690203	26941.549426	31.482522
546.968628	26983.796465	31.487540
546.782579	27042.280559	31.492557
547.723938	27088.682081	31.497575
548.191820	27142.210762	31.502592
548.849840	27196.759140	31.507610
549.342721	27240.803864	31.512628
550.026907	27289.325238	31.517645
550.733259	27339.815200	31.522663
551.391289	27378.500213	31.527680
551.677525	27427.330358	31.532698
552.437631	27451.127983	31.537716
552.931974	27503.629610	31.542733
553.632754	27536.992887	31.547751
554.137605	27568.269409	31.552768
554.362816	27603.697735	31.557786
555.404724	27646.267395	31.562804
555.866975	27695.664898	31.567821
556.421950	27717.371124	31.572839
557.113024	27761.601018	31.577856
557.640916	27803.827561	31.582874
558.291172	27827.674332	31.587892
558.746114	27872.845047	31.592909
559.371365	27914.342455	31.597927
560.221921	27952.783697	31.602944
560.434266	27989.952824	31.607962
561.070068	28029.224021	31.612980
561.114387	28072.999074	31.617997
561.625037	28108.794677	31.623015
562.843594	28152.677846	31.628032
563.723076	28189.029262	31.633050
564.263976	28210.422180	31.638068
564.785412	28256.815901	31.643085
565.462090	28288.743081	31.648103
566.319915	28322.133766	31.653120
566.734364	28359.158334	31.658138
566.992176	28392.863762	31.663156
566.995607	28444.255968	31.668173
567.818591	28482.607695	31.673191
568.308612	28516.827072	31.678208
568.606634	28562.074310	31.683226
569.211667	28606.136136	31.688244
569.667345	28655.890948	31.693261
570.104336	28710.224969	31.698279
571.125355	28754.449902	31.703296
571.648242	28799.909167	31.708314
572.020332	28845.581632	31.713332
572.538678	28893.696519	31.718349
573.162582	28940.341313	31.723367
574.047416	29000.598468	31.728384
574.490839	29035.660311	31.733402
575.269893	29081.124570	31.738420
575.993375	29129.701101	31.743437
576.595968	29160.471829	31.748455
577.076167	29201.735284	31.753472
577.741167	29251.534810	31.758490
578.485541	29301.435877	31.763508
578.720367	29357.351700	31.768525
579.378101	29389.112888	31.773543
579.851690	29438.038777	31.778560
580.293901	29481.982457	31.783578
580.922974	29532.489881	31.788596
581.460928	29576.810757	31.793613
581.545964	29620.412116	31.798631
582.344828	29668.548364	31.803648
583.089658	29715.643852	31.808666
584.341233	29746.718975	31.813684
585.315878	29795.314875	31.818701
585.899777	29835.021133	31.823719
586.268530	29866.632096	31.828736
587.086993	29898.760957	31.833754
587.514458	29936.860933	31.838772
587.883034	29983.408786	31.843789
588.235039	30023.872111	31.848807
589.039449	30056.471168	31.853824
589.259524	30099.685897	31.858842
589.757049	30141.523767	31.863860
590.476693	30189.743102	31.868877
590.802745	30237.530773	31.873895
591.585717	30282.801130	31.878912
592.539703	30321.768029	31.883930
593.471030	30345.605593	31.888948
593.878594	30385.378292	31.893965
594.315919	30414.292910	31.898983
594.797178	30451.386713	31.904000
595.178322	30486.764149	31.909018
596.222147	30520.382318	31.914036
596.880935	30562.379256	31.919053
597.399500	30589.404060	31.924071
597.750154	30616.739497	31.929088
598.219841	30658.557466	31.934106
599.324167	30691.477476	31.939124
599.857444	30726.395472	31.944141
600.388808	30773.931179	31.949159
601.177590	30801.445187	31.954176
601.239088	30855.697947	31.959194
601.839071	30886.920485	31.964212
602.428664	30937.424862	31.969229
602.835320	30975.194965	31.974247
603.341515	31020.560601	31.979264
603.673336	31066.718374	31.984282
604.557168	31109.977282	31.989300
605.462170	31163.644396	31.994317
605.699033	31212.345852	31.999335
606.486109	31257.251066	32.004352
606.768888	31306.527171	32.009370
607.624505	31357.149198	32.014388
607.845876	31405.752376	32.019405
608.751367	31464.907271	32.024423
609.372113	31508.037286	32.029440
610.191059	31567.275483	32.034458
610.790813	31615.093268	32.039476
611.467363	31659.618302	32.044493
611.270714	31713.041111	32.049511
612.583394	31770.218042	32.054528
612.819001	31827.240398	32.059546
613.794605	31876.574366	32.064564
614.205091	31929.675638	32.069581
614.768481	31978.207948	32.074599
615.894904	32019.445982	32.079616
616.851870	32065.565555	32.084634
617.174058	32100.594590	32.089652
618.064301	32156.460212	32.094669
618.819605	32198.546594	32.099687
619.689403	32229.280309	32.104704
620.269734	32261.759689	32.109722
621.374570	32297.564912	32.114740
621.714430	32331.143895	32.119757
622.115069	32374.170896	32.124775
622.875884	32407.842517	32.129792
623.596895	32454.018651	32.134810
623.941843	32488.791923	32.139828
624.810735	32531.246928	32.144845
624.957074	32568.289188	32.149863
625.946109	32624.336667	32.154880
626.200456	32668.145674	32.159898
626.835328	32705.655810	32.164916
627.027117	32742.071757	32.169933
627.653237	32795.590526	32.174951
628.290390	32845.915129	32.179968
628.808622	32898.439445	32.184986
629.405593	32947.657882	32.190004
630.109352	33004.585294	32.195021
630.253063	33053.969371	32.200039
630.861930	33103.205289	32.205056
631.528591	33168.085714	32.210074
632.256892	33215.615317	32.215092
632.868520	33268.562246	32.220109
633.565871	33323.967904	32.225127
634.351111	33374.283371	32.230144
634.612241	33427.493894	32.235162
635.263464	33472.671605	32.240180
635.995843	33511.432438	32.245197
636.561676	33567.649484	32.250215
637.346960	33623.908384	32.255232
637.690567	33677.498678	32.260250
638.613693	33730.195973	32.265268
639.079519	33786.593551	32.270285
639.899701	33840.622174	32.275303
640.548321	33881.609519	32.280320
640.912354	33948.398217	32.285338
641.462883	33993.011074	32.290356
642.087237	34052.090631	32.295373
642.653411	34105.305964	32.300391
644.136516	34147.592771	32.305408
644.599832	34207.323746	32.310426
645.370347	34264.667787	32.315444
646.199703	34318.418027	32.320461
646.261545	34368.165672	32.325479
647.439963	34406.365576	32.330496
647.748579	34456.637710	32.335514
648.428085	34511.176785	32.340532
649.686485	34562.496262	32.345549
650.096906	34614.605408	32.350567
650.970710	34656.273651	32.355584
651.302601	34704.829358	32.360602
652.140526	34758.863902	32.365620
652.772277	34807.297294	32.370637
653.139039	34859.888034	32.375655
654.151135	34904.854584	32.380672
655.006945	34957.887888	32.385690
655.521962	35012.061864	32.390708
656.756347	35043.097029	32.395725
657.559929	35085.662219	32.400743
658.520317	35118.074221	32.405760
659.138705	35160.466068	32.410778
659.569346	35200.699585	32.415796
660.226265	35241.953841	32.420813
660.517548	35290.479280	32.425831
661.080960	35339.468283	32.430848
661.885921	35375.881857	32.435866
662.252093	35424.971313	32.440884
662.988185	35465.524503	32.445901
663.524926	35518.975605	32.450919
664.302094	35560.597451	32.455936
664.952596	35616.648717	32.460954
665.856867	35677.301562	32.465972
666.344160	35708.921896	32.470989
666.842335	35764.674802	32.476007
667.681999	35804.434811	32.481024
668.255603	35862.250123	32.486042
668.834038	35904.833043	32.491060
669.170671	35957.696761	32.496077
669.771284	36011.689254	32.501095
670.786699	36061.779301	32.506112
671.538867	36107.996553	32.511130
671.889921	36167.200447	32.516148
672.901295	36217.032249	32.521165
673.128898	36266.853396	32.526183
673.910799	36316.461911	32.531200
674.851540	36369.675222	32.536218
675.210578	36428.796402	32.541236
675.981372	36481.549576	32.546253
676.628557	36533.165003	32.551271
677.178345	36575.614620	32.556288
678.116214	36633.318417	32.561306
678.443145	36680.956252	32.566324
679.560690	36723.773045	32.571341
679.726217	36779.586719	32.576359
680.648683	36824.153973	32.581376
681.153303	36879.750721	32.586394
681.783247	36919.558112	32.591412
682.689857	36969.907518	32.596429
683.043110	37033.122376	32.601447
683.883386	37080.598989	32.606464
684.601703	37133.924713	32.611482
684.807115	37179.255627	32.616500
685.759015	37228.922007	32.621517
686.487493	37296.258908	32.626535
687.076544	37347.537576	32.631552
687.939038	37400.373598	32.636570
688.499335	37466.915187	32.641588
689.380022	37514.911312	32.646605
689.826010	37578.644506	32.651623
690.334453	37636.942706	32.656640
691.251325	37702.885709	32.661658
692.169685	37762.644378	32.666676
692.697543	37821.591370	32.671693
693.151305	37889.099369	32.676711
693.886026	37943.151755	32.681728
694.688603	38003.061912	32.686746
695.024622	38068.192201	32.691764
695.898641	38134.946289	32.696781
696.318781	38198.716967	32.701799
697.209370	38266.664036	32.706816
698.033353	38326.906913	32.711834
698.792518	38387.235933	32.716852
699.885058	38444.914217	32.721869
700.627351	38514.763271	32.726887
701.332007	38575.164540	32.731904
702.155812	38627.434156	32.736922
702.646873	38689.462561	32.741940
703.261646	38749.890959	32.746957
704.353739	38810.017568	32.751975
705.241609	38866.748668	32.756992
705.707948	38926.327991	32.762010
706.073175	38998.937558	32.767028
706.818184	39051.606220	32.772045
707.525874	39122.506056	32.777063
708.137335	39182.727496	32.782080
709.104997	39246.156763	32.787098
709.659124	39307.152662	32.792116
710.371870	39368.604656	32.797133
711.071573	39438.128163	32.802151
711.673798	39493.248511	32.807168
712.627949	39569.151616	32.812186
713.317245	39634.838739	32.817204
714.199712	39694.311132	32.822221
715.103422	39749.062676	32.827239
715.718505	39816.033026	32.832256
716.936622	39864.519407	32.837274
717.884671	39908.918335	32.842292
718.601826	39957.754844	32.847309
719.317024	40009.652621	32.852327
719.787791	40068.386973	32.857344
720.499787	40118.546383	32.862362
721.166963	40173.399061	32.867380
721.909305	40221.656748	32.872397
722.637780	40278.561820	32.877415
723.585724	40323.657272	32.882432
724.299883	40377.244643	32.887450
725.047285	40445.012155	32.892468
725.778430	40484.158993	32.897485
726.085028	40534.882085	32.902503
727.024292	40584.286230	32.907520
727.573197	40627.300512	32.912538
728.043023	40682.381248	32.917556
728.483793	40725.210180	32.922573
729.111569	40776.111510	32.927591
729.763325	40844.704666	32.932608
730.602290	40895.655617	32.937626
731.210293	40958.228852	32.942644
732.120459	41011.173809	32.947661
732.836546	41069.980189	32.952679
733.240226	41125.654185	32.957696
734.484955	41169.630044	32.962714
736.054084	41223.674577	32.967732
737.006374	41276.518755	32.972749
737.665160	41311.371399	32.977767
738.156656	41366.716117	32.982784
738.690821	41409.670992	32.987802
739.355176	41463.003158	32.992820
740.104543	41512.375724	32.997837
740.518799	41578.895771	33.002855
741.418161	41632.944388	33.007872
742.821541	41665.885517	33.012890
743.943128	41719.621474	33.017908
744.477186	41748.662977	33.022925
745.210463	41804.508755	33.027943
745.504433	41855.451916	33.032960
746.416914	41897.899811	33.037978
746.717206	41963.237087	33.042996
747.530436	42015.390014	33.048013
747.950578	42079.184735	33.053031
748.847587	42123.849113	33.058048
750.650540	42169.207417	33.063066
751.152956	42219.948209	33.068084
751.900136	42273.788083	33.073101
753.123807	42322.576340	33.078119
753.659097	42373.666555	33.083136
753.902107	42428.717424	33.088154
754.636564	42475.842863	33.093172
755.432699	42525.349577	33.098189
755.712222	42585.910385	33.103207
756.387285	42658.287838	33.108224
757.212619	42712.066021	33.113242
757.756404	42775.799242	33.118260
758.156199	42832.705202	33.123277
759.452748	42896.315266	33.128295
759.572823	42970.241191	33.133312
760.621075	43036.957905	33.138330
761.032803	43103.052860	33.143348
761.887945	43169.781062	33.148365
762.718894	43232.117351	33.153383
763.557157	43302.150234	33.158400
764.201038	43371.720245	33.163418
765.116459	43432.930743	33.168436
766.174044	43500.785918	33.173453
767.414888	43565.197219	33.178471
767.728201	43635.464677	33.183488
768.405755	43693.936198	33.188506
769.354268	43767.969857	33.193524
769.894793	43827.139853	33.198541
771.151329	43892.403563	33.203559
771.316891	43957.343927	33.208576
772.326005	44024.790789	33.213594
772.847583	44093.547174	33.218612
773.199471	44154.063058	33.223629
774.587229	44222.153684	33.228647
775.236361	44291.599259	33.233664
776.040389	44351.678430	33.238682
776.853708	44420.219628	33.243700
778.103578	44468.009148	33.248717
779.554192	44518.183814	33.253735
779.942174	44567.910448	33.258752
780.685459	44611.319738	33.263770
781.392843	44672.888640	33.268788
781.628138	44725.422578	33.273805
782.336885	44784.701771	33.278823
783.029485	44847.525896	33.283840
783.822476	44909.145380	33.288858
784.631510	44981.174314	33.293876
785.048564	45030.720341	33.298893
785.964794	45099.532258	33.303911
786.278775	45170.677386	33.308928
787.429383	45234.278928	33.313946
787.994812	45306.410089	33.318964
789.135591	45377.243727	33.323981
789.521581	45445.588923	33.328999
790.225454	45524.549900	33.334016
791.198893	45595.309067	33.339034
791.879307	45664.545300	33.344052
792.890697	45740.543023	33.349069
793.625112	45807.803993	33.354087
794.136614	45897.695480	33.359104
795.187063	45965.559282	33.364122
795.852806	46040.131593	33.369140
796.558242	46111.294680	33.374157
797.722268	46185.100392	33.379175
798.309724	46266.466947	33.384192
799.618210	46335.518918	33.389210
799.906108	46415.528297	33.394228
800.752894	46491.604794	33.399245
802.319091	46566.354978	33.404263
802.858792	46637.672049	33.409280
803.953829	46706.170071	33.414298
804.663366	46777.777448	33.419316
805.452202	46848.752757	33.424333
806.596524	46912.284127	33.429351
807.104071	46985.264728	33.434368
808.097431	47045.979571	33.439386
808.883324	47116.861291	33.444404
809.808763	47177.365646	33.449421
811.107977	47251.387879	33.454439
811.527086	47302.526458	33.459456
813.079338	47365.426251	33.464474
813.810259	47423.525970	33.469492
814.279463	47479.654843	33.474509
815.408463	47546.467361	33.479527
816.040141	47607.758766	33.484544
816.647792	47663.449012	33.489562
817.808463	47728.333955	33.494580
818.167972	47802.118368	33.499597
819.398544	47857.288262	33.504615
820.051922	47911.694085	33.509632
820.529361	47980.146606	33.514650
821.404688	48049.555940	33.519668
822.256961	48110.991505	33.524685
823.316567	48172.451900	33.529703
823.997481	48248.224832	33.534720
824.644593	48314.766675	33.539738
825.512751	48384.386921	33.544756
826.039249	48447.904902	33.549773
826.918522	48517.201175	33.554791
827.558011	48592.140276	33.559808
828.691435	48658.423954	33.564826
829.343955	48724.485336	33.569844
829.967621	48802.755361	33.574861
830.733036	48875.284346	33.579879
831.376838	48953.216443	33.584896
832.317264	49017.886289	33.589914
833.118340	49077.497709	33.594932
833.634331	49150.053741	33.599949
834.836476	49209.046326	33.604967
835.742830	49283.079399	33.609984
836.525852	49344.054568	33.615002
837.230451	49416.778215	33.620020
837.752399	49487.746378	33.625037
839.154064	49553.022905	33.630055
839.731449	49632.909979	33.635072
840.741103	49683.278687	33.640090
841.804783	49751.828744	33.645108
842.643548	49822.008386	33.650125
843.706854	49886.174392	33.655143
844.101202	49961.655966	33.660160
845.300096	50025.567162	33.665178
846.156704	50103.027163	33.670196
846.718792	50173.194005	33.675213
847.512311	50238.168553	33.680231
848.493780	50314.939173	33.685248
848.888666	50381.640179	33.690266
850.077354	50455.721669	33.695284
850.591263	50546.706761	33.700301
851.453247	50619.903231	33.705319
852.220017	50706.218173	33.710336
853.392568	50773.115612	33.715354
854.250525	50845.377012	33.720372
855.054752	50929.788818	33.725389
856.315615	50995.705102	33.730407
856.801700	51078.401693	33.735424
857.458705	51155.016821	33.740442
858.708706	51242.258247	33.745460
859.724827	51319.830379	33.750477
860.866577	51396.472087	33.755495
861.417062	51472.332918	33.760512
862.279039	51542.210476	33.765530
863.037943	51620.304532	33.770548
863.843968	51702.915586	33.775565
865.178345	51769.195948	33.780583
866.399919	51848.560158	33.785600
867.082832	51919.371547	33.790618
867.970530	51982.944310	33.795636
868.673532	52057.384948	33.800653
869.684528	52129.000113	33.805671
870.469507	52198.372780	33.810688
871.696078	52272.106182	33.815706
873.154195	52320.740377	33.820724
874.226528	52391.676086	33.825741
875.169360	52444.668183	33.830759
875.974253	52517.626436	33.835776
876.349732	52576.458932	33.840794
877.344150	52641.807598	33.845812
877.288404	52715.033319	33.850829
878.012842	52788.327654	33.855847
879.201054	52869.744380	33.860864
879.735635	52947.466512	33.865882
880.935785	53019.200509	33.870900
881.559242	53105.546682	33.875917
882.482837	53165.738068	33.880935
883.589882	53243.365744	33.885952
884.833693	53317.144063	33.890970
885.686832	53397.614995	33.895988
886.212943	53464.835967	33.901005
887.248484	53534.357110	33.906023
888.002871	53615.679441	33.911040
888.428235	53689.877420	33.916058
889.622208	53769.353714	33.921076
890.245345	53844.375666	33.926093
891.388244	53918.665169	33.931111
892.019233	53993.882543	33.936128
892.621659	54059.669541	33.941146
893.987016	54130.533273	33.946164
894.309496	54206.546058	33.951181
895.586046	54277.259528	33.956199
896.450026	54346.455410	33.961216
897.696919	54410.377534	33.966234
898.678756	54474.062653	33.971252
899.449174	54542.742115	33.976269
900.321718	54620.183035	33.981287
901.258684	54693.760320	33.986304
901.910095	54764.705456	33.991322
902.910697	54840.722307	33.996340
903.468497	54927.977673	34.001357
904.299619	54994.250596	34.006375
905.654294	55073.763234	34.011392
906.329656	55159.969647	34.016410
906.987610	55231.180954	34.021428
908.009374	55317.751689	34.026445
909.021416	55391.996594	34.031463
909.695015	55482.184996	34.036480
910.930052	55560.116810	34.041498
912.072702	55642.461521	34.046516
912.685843	55734.622108	34.051533
913.859327	55810.292409	34.056551
914.927038	55903.825786	34.061568
915.556866	55981.100098	34.066586
916.527109	56058.283701	34.071604
917.546630	56140.427807	34.076621
918.693793	56215.116239	34.081639
919.762334	56295.019257	34.086656
920.865872	56366.360794	34.091674
921.909051	56444.186143	34.096692
922.230162	56535.496620	34.101709
923.676013	56599.994910	34.106727
924.731316	56681.951781	34.111744
925.848072	56749.248362	34.116762
927.612199	56815.501380	34.121780
928.795400	56860.757587	34.126797
930.066373	56917.752741	34.131815
930.575379	56986.796405	34.136832
930.973157	57043.351862	34.141850
931.874433	57121.612882	34.146868
932.815911	57184.336919	34.151885
933.556614	57253.459204	34.156903
934.337297	57328.100577	34.161920
934.704232	57403.407831	34.166938
935.828992	57471.996297	34.171956
936.300128	57560.116541	34.176973
937.080791	57638.258785	34.181991
938.238221	57717.994500	34.187008
938.832202	57813.862213	34.192026
939.796272	57897.191852	34.197044
940.711798	57984.839420	34.202061
941.566092	58081.560075	34.207079
942.510264	58161.330455	34.212096
943.332795	58259.740310	34.217114
944.315844	58342.530560	34.222132
944.894955	58436.820779	34.227149
946.120607	58530.555023	34.232167
947.101204	58622.144196	34.237184
947.684571	58714.814557	34.242202
948.851143	58812.052832	34.247220
949.779542	58910.986848	34.252237
951.075298	59006.332324	34.257255
952.094975	59092.841082	34.262272
953.037295	59175.134176	34.267290
954.118368	59246.266237	34.272308
955.277328	59333.893464	34.277325
956.140095	59409.509557	34.282343
957.053031	59480.592525	34.287360
957.619470	59558.641409	34.292378
958.582747	59633.014637	34.297396
959.398486	59723.247477	34.302413
960.109037	59803.914119	34.307431
961.292608	59897.381702	34.312448
962.480446	59980.183647	34.317466
963.231739	60069.604957	34.322484
963.493074	60159.052225	34.327501
964.809663	60250.728164	34.332519
965.895356	60339.819907	34.337536
967.065225	60446.159939	34.342554
968.241070	60527.243933	34.347572
969.366339	60619.280182	34.352589
970.302181	60707.833247	34.357607
971.443418	60783.422916	34.362624
972.062952	60890.698736	34.367642
973.958479	60966.532357	34.372660
974.887875	61050.840352	34.377677
976.060598	61130.103833	34.382695
976.947499	61214.786139	34.387712
977.732628	61301.959575	34.392730
978.898216	61381.351576	34.397748
979.729985	61469.778004	34.402765
980.379997	61556.112499	34.407783
981.618532	61637.867717	34.412800
982.212833	61723.932953	34.417818
983.258786	61810.219367	34.422836
984.101454	61907.393792	34.427853
985.169426	61995.633419	34.432871
986.196897	62089.703373	34.437888
987.139210	62184.818753	34.442906
988.461692	62268.481029	34.447924
989.516901	62352.223173	34.452941
990.618024	62431.369056	34.457959
991.721435	62526.144164	34.462976
992.524081	62623.523873	34.467994
993.583505	62710.482342	34.473012
994.707953	62796.734663	34.478029
995.753045	62873.282599	34.483047
996.905840	62966.456465	34.488064
997.903363	63054.812122	34.493082
998.948206	63133.614510	34.498100
999.874359	63220.791755	34.503117
1000.617037	63309.707081	34.508135
1001.478781	63395.958064	34.513152
1002.639154	63487.366508	34.518170
1003.624345	63580.682714	34.523188
1004.587724	63670.799422	34.528205
1005.073897	63771.322183	34.533223
1006.323343	63858.653916	34.538240
1007.192543	63963.561887	34.543258
1008.453298	64051.506602	34.548276
1009.287396	64143.708921	34.553293
1010.066955	64237.572373	34.558311
1011.157562	64333.267973	34.563328
1012.321588	64437.688893	34.568346
1013.195243	64521.283009	34.573364
1014.502019	64620.826800	34.578381
1015.202098	64714.704410	34.583399
1016.373648	64811.003321	34.588416
1017.649018	64909.375616	34.593434
1018.456007	65001.306753	34.598452
1020.255796	65087.347914	34.603469
1020.912177	65172.408797	34.608487
1022.092572	65254.526824	34.613504
1023.001370	65328.089983	34.618522
1023.915473	65406.521036	34.623540
1025.027134	65483.047613	34.628557
1025.687528	65568.710651	34.633575
1026.642163	65652.910032	34.638592
1027.247056	65736.999526	34.643610
1028.300723	65830.712300	34.648628
1029.778384	65911.861862	34.653645
1030.779989	66000.575484	34.658663
1031.609155	66080.497000	34.663680
1032.946581	66183.891523	34.668698
1033.772775	66269.347524	34.673716
1034.379467	66367.506702	34.678733
1035.307384	66463.545948	34.683751
1036.687806	66551.480774	34.688768
1037.524727	66653.764848	34.693786
1038.555792	66745.528163	34.698804
1040.050306	66830.951670	34.703821
1041.449846	66922.835546	34.708839
1043.013787	66996.662463	34.713856
1044.167270	67086.040026	34.718874
1045.392182	67165.802056	34.723892
1046.373787	67262.450109	34.728909
1047.212878	67343.722647	34.733927
1048.200651	67423.756660	34.738944
1048.756701	67516.711031	34.743962
1049.994194	67609.622983	34.748980
1051.166762	67696.587411	34.753997
1051.974498	67792.048880	34.759015
1053.041286	67880.860218	34.764032
1054.095928	67970.769122	34.769050
1055.148177	68068.055048	34.774068
1055.854908	68158.398661	34.779085
1056.949852	68273.894858	34.784103
1057.807059	68362.873455	34.789120
1058.762990	68471.458978	34.794138
1059.819476	68564.193620	34.799156
1060.750826	68668.668172	34.804173
1061.636130	68787.878066	34.809191
1062.830372	68890.527030	34.814208
1063.707641	69000.469374	34.819226
1064.879706	69102.369144	34.824244
1066.326554	69212.622641	34.829261
1067.224446	69326.913181	34.834279
1068.857478	69423.740244	34.839296
1070.182211	69517.810595	34.844314
1071.649685	69613.543381	34.849332
1072.765766	69699.421607	34.854349
1073.932689	69795.385477	34.859367
1075.293032	69892.668325	34.864384
1075.723630	69980.940060	34.869402
1076.704955	70074.603645	34.874420
1078.119473	70168.890341	34.879437
1079.122527	70256.947264	34.884455
1080.219511	70359.617195	34.889472
1081.182243	70453.975248	34.894490
1082.011354	70546.068510	34.899508
1083.358920	70649.682075	34.904525
1083.844851	70743.817779	34.909543
1085.471364	70837.636974	34.914560
1086.819419	70936.882321	34.919578
1088.065849	71022.314030	34.924596
1089.228568	71108.822886	34.929613
1089.574806	71197.802099	34.934631
1090.982684	71290.517125	34.939648
1092.295175	71385.311699	34.944666
1093.202874	71472.076754	34.949684
1093.917743	71564.064736	34.954701
1094.459727	71647.607078	34.959719
1095.826647	71732.465091	34.964736
1096.884362	71833.481475	34.969754
1097.674730	71931.411577	34.974772
1098.922713	72020.329208	34.979789
1099.684573	72128.434607	34.984807
1100.749667	72207.857100	34.989824
1102.146648	72312.647422	34.994842
1102.778056	72419.013842	34.999860
1104.802716	72509.180088	35.004877
1106.074545	72613.269158	35.009895
1107.040026	72696.381609	35.014912
1108.136354	72795.964474	35.019930
1108.997252	72881.905536	35.024948
1110.114938	72979.636594	35.029965
1110.727070	73085.489406	35.034983
1112.457438	73192.181838	35.040000
1113.607461	73290.630956	35.045018
1114.955604	73392.254053	35.050036
1116.236469	73470.240851	35.055053
1116.966276	73572.948824	35.060071
1118.471412	73668.468909	35.065088
1119.325590	73771.816921	35.070106
1120.566748	73874.243808	35.075124
1121.640974	73970.465353	35.080141
1123.070127	74077.005570	35.085159
1123.829729	74172.630845	35.090176
1124.887645	74287.754035	35.095194
1125.698041	74393.593855	35.100212
1127.005506	74492.048244	35.105229
1128.131961	74613.305343	35.110247
1129.329278	74725.280118	35.115264
1130.303896	74820.886909	35.120282
1130.996618	74933.384424	35.125300
1132.459653	75047.548498	35.130317
1133.244503	75168.430615	35.135335
1134.637036	75273.144630	35.140352
1135.258795	75395.598493	35.145370
1136.316674	75509.637593	35.150388
1137.697244	75632.734431	35.155405
1138.778753	75766.189268	35.160423
1140.052090	75887.935933	35.165440
1141.226448	76002.554336	35.170458
1142.658887	76121.313198	35.175476
1144.136636	76238.051451	35.180493
1145.254953	76358.595652	35.185511
1146.266865	76468.795124	35.190528
1147.854975	76581.160139	35.195546
1149.061769	76693.356961	35.200564
1150.309484	76793.817844	35.205581
1151.371189	76901.667851	35.210599
1152.559480	77007.915142	35.215616
1153.750867	77127.767339	35.220634
1154.805720	77239.470695	35.225652
1156.174558	77347.173321	35.230669
1157.172246	77452.400598	35.235687
1158.541627	77559.052555	35.240704
1159.702291	77667.751600	35.245722
1160.711086	77777.462812	35.250740
1162.407810	77877.110396	35.255757
1163.131531	77991.934010	35.260775
1164.300488	78086.255280	35.265792
1165.780657	78186.026373	35.270810
1166.476902	78294.762194	35.275828
1167.800559	78401.399216	35.280845
1169.190904	78511.434021	35.285863
1170.103214	78605.645007	35.290880
1171.317724	78704.851261	35.295898
1172.614249	78794.860556	35.300916
1173.556204	78877.983060	35.305933
1174.451591	78979.418939	35.310951
1175.688483	79075.202568	35.315968
1177.059997	79170.978244	35.320986
1178.021627	79276.724870	35.326004
1179.430983	79354.911331	35.331021
1180.225412	79470.806940	35.336039
1180.983299	79571.202228	35.341056
1182.490789	79678.525025	35.346074
1182.969716	79798.398426	35.351092
1184.506475	79914.307032	35.356109
1185.903606	80020.052054	35.361127
1187.226646	80133.790454	35.366144
1188.455776	80238.814991	35.371162
1189.744234	80343.475956	35.376180
1191.622213	80440.266728	35.381197
1192.398010	80547.085989	35.386215
1193.802569	80649.702971	35.391232
1195.145840	80757.498921	35.396250
1196.276336	80862.047061	35.401268
1197.232037	80972.539380	35.406285
1198.374044	81077.745340	35.411303
1199.682437	81192.136478	35.416320
1201.141033	81296.470470	35.421338
1202.203992	81409.279004	35.426356
1203.304208	81506.942040	35.431373
1204.638158	81623.624155	35.436391
1205.831996	81742.685126	35.441408
1207.197173	81854.156098	35.446426
1208.250173	81955.122174	35.451444
1209.516343	82062.048260	35.456461
1210.522665	82177.250620	35.461479
1211.762350	82292.442466	35.466496
1212.953755	82400.977887	35.471514
1214.243489	82508.586178	35.476532
1215.933940	82610.557673	35.481549
1217.766605	82700.850891	35.486567
1219.000420	82818.415109	35.491584
1220.192137	82915.232553	35.496602
1221.823675	83021.142465	35.501620
1222.734020	83127.114347	35.506637
1223.598906	83217.331786	35.511655
1224.876465	83315.024158	35.516672
1226.405269	83418.708887	35.521690
1227.371013	83532.656034	35.526708
1229.011595	83630.495714	35.531725
1229.636891	83741.379738	35.536743
1230.865688	83843.756960	35.541760
1232.557710	83943.312913	35.546778
1232.861090	84062.661617	35.551796
1233.939800	84169.713525	35.556813
1235.317299	84291.366795	35.561831
1236.156014	84404.792351	35.566848
1237.262235	84517.948641	35.571866
1238.521826	84644.449385	35.576884
1240.054267	84759.580314	35.581901
1240.977390	84885.779705	35.586919
1242.204264	85018.825471	35.591936
1243.604244	85124.893274	35.596954
1244.278896	85253.755889	35.601972
1245.880066	85367.902870	35.606989
1247.226415	85486.208156	35.612007
1248.967548	85606.150445	35.617024
1250.619048	85700.168730	35.622042
1252.189426	85820.936791	35.627060
1253.524802	85924.280547	35.632077
1254.655404	86016.416851	35.637095
1255.661942	86110.600219	35.642112
1256.884526	86205.954072	35.647130
1257.768616	86310.142419	35.652148
1259.078135	86416.659883	35.657165
1259.955882	86512.043073	35.662183
1261.079856	86628.271447	35.667200
1262.220887	86739.226122	35.672218
1263.514619	86851.133190	35.677236
1264.354392	86959.689910	35.682253
1265.849480	87071.211667	35.687271
1266.860977	87197.762189	35.692288
1267.997349	87315.524696	35.697306
1269.093286	87441.024011	35.702324
1270.394707	87566.479208	35.707341
1271.594919	87692.140780	35.712359
1273.118373	87825.786857	35.717376
1274.417671	87949.520581	35.722394
1275.347462	88082.094365	35.727412
1276.633740	88213.396695	35.732429
1278.194618	88343.275558	35.737447
1279.317319	88478.190872	35.742464
1280.922069	88597.824531	35.747482
1282.106993	88735.696748	35.752500
1283.832325	88870.672129	35.757517
1285.243521	88992.365163	35.762535
1286.360168	89121.404145	35.767552
1288.034112	89256.389284	35.772570
1288.916081	89380.612171	35.777588
1290.613812	89505.507009	35.782605
1292.072784	89625.560376	35.787623
1293.014885	89756.074022	35.792640
1294.715364	89866.509840	35.797658
1296.012598	90012.316628	35.802676
1297.124125	90139.244382	35.807693
1298.577940	90266.271480	35.812711
1300.023863	90381.133825	35.817728
1302.241341	90482.772117	35.822746
1304.065749	90584.357875	35.827764
1305.528306	90691.424595	35.832781
1306.858685	90806.382599	35.837799
1308.482136	90919.635174	35.842816
1309.745772	91017.925813	35.847834
1310.410665	91128.933042	35.852852
1311.563785	91235.251419	35.857869
1312.904104	91349.779044	35.862887
1313.546931	91462.768061	35.867904
1315.676565	91572.991288	35.872922
1316.321908	91694.738488	35.877940
1317.907010	91812.981279	35.882957
1319.479556	91917.627171	35.887975
1320.230716	92054.580950	35.892992
1321.513620	92162.263873	35.898010
1322.853982	92288.898919	35.903028
1324.220052	92407.178123	35.908045
1325.593042	92527.560653	35.913063
1326.612590	92647.707162	35.918080
1328.091044	92772.827151	35.923098
1329.169150	92893.383772	35.928116
1330.369095	93013.883882	35.933133
1331.814950	93133.243500	35.938151
1332.990569	93259.819505	35.943168
1334.680989	93389.370511	35.948186
1335.959177	93510.988452	35.953204
1337.236555	93635.534885	35.958221
1338.453689	93762.651523	35.963239
1339.387276	93895.605262	35.968256
1341.037458	94016.647635	35.973274
1342.146178	94132.083678	35.978292
1343.375155	94249.351996	35.983309
1344.590337	94362.376744	35.988327
1345.586882	94489.568745	35.993344
1347.453112	94603.469030	35.998362
1348.400556	94737.641064	36.003380
1349.468201	94863.860219	36.008397
1350.988495	94986.587084	36.013415
1351.973485	95118.448006	36.018432
1353.540625	95255.567931	36.023450
1355.083510	95373.640910	36.028468
1356.811900	95502.979407	36.033485
1359.055827	95615.024692	36.038503
1360.143669	95744.020245	36.043520
1361.152429	95864.599279	36.048538
1362.878323	95992.152919	36.053556
1363.868405	96118.693460	36.058573
1365.365806	96240.085196	36.063591
1366.427524	96380.508414	36.068608
1367.837702	96499.886584	36.073626
1368.757066	96636.188057	36.078644
1370.066399	96775.623800	36.083661
1371.623837	96907.048244	36.088679
1373.361340	97048.598852	36.093696
1374.910621	97187.352587	36.098714
1375.955066	97323.257280	36.103732
1377.541251	97457.126075	36.108749
1378.750162	97587.872378	36.113767
1379.760571	97732.049155	36.118784
1381.485106	97870.841997	36.123802
1382.968856	98010.775788	36.128820
1384.844213	98143.753148	36.133837
1388.291632	98220.835722	36.138855
1389.697036	98341.907605	36.143872
1391.026325	98446.461288	36.148890
1391.999278	98565.801232	36.153908
1393.522830	98681.836001	36.158925
1394.602624	98786.860648	36.163943
1395.897536	98907.711018	36.168960
1397.141383	99037.278891	36.173978
1398.256389	99159.755518	36.178996
1399.385237	99282.116364	36.184013
1401.065941	99415.065942	36.189031
1402.114780	99546.352287	36.194048
1403.639722	99676.132535	36.199066
1404.895112	99807.261025	36.204084
1406.066360	99947.809744	36.209101
1407.449751	100079.160288	36.214119
1408.584546	100219.449639	36.219136
1410.192577	100350.221191	36.224154
1411.137533	100487.004224	36.229172
1412.796967	100632.994684	36.234189
1414.106443	100771.040654	36.239207
1415.703366	100919.818549	36.244224
1416.711847	101057.925266	36.249242
1418.334442	101201.908250	36.254260
1419.561784	101346.701389	36.259277
1421.491481	101486.263955	36.264295
1422.394727	101636.395533	36.269312
1423.763415	101784.046522	36.274330
1425.188194	101925.895541	36.279348
1426.623641	102071.407510	36.284365
1428.446437	102208.745762	36.289383
1429.698325	102359.270127	36.294400
1430.774970	102507.616423	36.299418
1432.920254	102653.324769	36.304436
1434.239016	102799.352582	36.309453
1436.259960	102925.100226	36.314471
1437.541957	103053.841399	36.319488
1439.368441	103164.634164	36.324506
1440.665530	103283.902966	36.329524
1442.135837	103406.010623	36.334541
1443.840615	103525.597202	36.339559
1444.677340	103646.206837	36.344576
1446.012757	103768.996123	36.349594
1446.809259	103887.812500	36.354612
1448.479067	104031.344083	36.359629
1449.492319	104159.408676	36.364647
1451.270707	104285.224592	36.369664
1452.748801	104426.809788	36.374682
1454.010256	104561.544530	36.379700
1455.576768	104702.914267	36.384717
1456.676561	104846.183055	36.389735
1458.237663	104993.678937	36.394752
1459.580158	105136.961908	36.399770
1461.129866	105279.300320	36.404788
1462.426807	105433.622732	36.409805
1463.979399	105579.715087	36.414823
1465.362186	105741.988289	36.419840
1466.426221	105884.962752	36.424858
1468.234503	106043.481401	36.429876
1469.446535	106210.944065	36.434893
1471.179343	106360.245080	36.439911
1473.082666	106512.259063	36.444928
1474.630393	106669.122086	36.449946
1476.339803	106804.582215	36.454964
1478.093916	106959.639256	36.459981
1479.612103	107109.332003	36.464999
1480.983278	107255.003320	36.470016
1482.163865	107414.450260	36.475034
1484.073639	107565.846604	36.480052
1485.557516	107719.643082	36.485069
1487.332890	107865.520368	36.490087
1488.692722	108014.607696	36.495104
1490.249874	108157.616368	36.500122
1492.369500	108291.801202	36.505140
1493.698430	108430.826801	36.510157
1495.502938	108577.602888	36.515175
1497.349881	108717.943885	36.520192
1498.483897	108863.481390	36.525210
1499.788335	108996.007852	36.530228
1501.450036	109139.029670	36.535245
1502.867008	109271.831329	36.540263
1504.304353	109418.617396	36.545280
1505.345495	109569.485623	36.550298
1507.049832	109715.216903	36.555316
1508.393550	109870.972265	36.560333
1510.143071	110009.101758	36.565351
1511.586456	110160.290360	36.570368
1512.620420	110314.827784	36.575386
1514.313606	110462.745087	36.580404
1515.760510	110620.313823	36.585421
1517.153513	110778.868124	36.590439
1518.598456	110936.527348	36.595456
1520.249112	111091.631631	36.600474
1521.669046	111243.779648	36.605492
1523.314572	111397.998360	36.610509
1524.796587	111547.956776	36.615527
1526.375226	111707.183835	36.620544
1528.078635	111863.767050	36.625562
1529.429738	112015.827632	36.630580
1530.940364	112168.548858	36.635597
1532.747557	112319.284235	36.640615
1534.504280	112478.791388	36.645632
1535.504007	112630.541496	36.650650
1537.384285	112766.606889	36.655668
1538.788869	112911.370724	36.660685
1540.146255	113035.939687	36.665703
1541.731467	113188.311228	36.670720
1542.994494	113327.569293	36.675738
1544.701188	113463.664340	36.680756
1546.058970	113625.445407	36.685773
1547.316399	113763.031940	36.690791
1548.840175	113916.456077	36.695808
1550.035206	114059.519622	36.700826
1551.560266	114209.558547	36.705844
1552.969452	114375.063653	36.710861
1554.225288	114536.610991	36.715879
1556.081439	114706.651875	36.720896
1557.506107	114873.146089	36.725914
1559.152057	115033.607594	36.730932
1560.295857	115197.826022	36.735949
1561.746414	115381.554697	36.740967
1563.406892	115547.939172	36.745984
1565.053825	115725.500376	36.751002
1566.931628	115893.818480	36.756020
1568.332829	116070.354198	36.761037
1569.842891	116245.947931	36.766055
1571.815546	116420.734859	36.771072
1573.390470	116598.958317	36.776090
1575.596906	116763.056361	36.781108
1577.051581	116939.220066	36.786125
1578.723440	117109.833417	36.791143
1580.395956	117271.835216	36.796160
1581.659288	117450.225391	36.801178
1583.723797	117619.536946	36.806196
1585.318900	117793.805614	36.811213
1586.829056	117956.989875	36.816231
1588.760648	118128.924617	36.821248
1589.851246	118307.256955	36.826266
1591.456198	118464.949153	36.831284
1593.135074	118648.074914	36.836301
1595.103289	118823.609418	36.841319
1596.710043	118992.871540	36.846336
1598.095897	119163.487967	36.851354
1600.203967	119324.048194	36.856372
1602.012526	119494.067567	36.861389
1603.363568	119664.133536	36.866407
1604.937897	119837.184432	36.871424
1606.579890	120003.807166	36.876442
1608.289057	120171.447625	36.881460
1609.815399	120335.387965	36.886477
1611.758098	120492.477848	36.891495
1613.653143	120657.846292	36.896512
1615.259459	120819.251962	36.901530
1616.822784	120975.286588	36.906548
1618.782507	121145.023349	36.911565
1619.989778	121313.216226	36.916583
1621.651091	121468.616018	36.921600
1623.078946	121642.674553	36.926618
1624.803090	121801.351345	36.931636
1625.979226	121977.581665	36.936653
1627.568237	122158.721158	36.941671
1629.169984	122320.450896	36.946688
1630.375815	122501.575499	36.951706
1631.804395	122670.006160	36.956724
1633.373550	122865.524649	36.961741
1634.776937	123046.887407	36.966759
1636.373101	123231.544634	36.971776
1637.808699	123431.298346	36.976794
1639.581178	123614.712087	36.981812
1640.849608	123810.446959	36.986829
1642.077169	123998.704471	36.991847
1644.002563	124195.810549	36.996864
1645.207355	124391.279081	37.001882
1646.816621	124563.711118	37.006900
1648.545509	124757.742456	37.011917
1649.821892	124933.818069	37.016935
1651.339330	125133.060095	37.021952
1652.594485	125336.974432	37.026970
1654.441201	125522.656198	37.031988
1655.704869	125737.177041	37.037005
1657.249039	125948.153881	37.042023
1659.047386	126148.321350	37.047040
1660.336069	126355.128119	37.052058
1662.368446	126564.129165	37.057076
1664.106842	126778.239054	37.062093
1665.742674	126986.682321	37.067111
1667.822905	127195.806005	37.072128
1669.674002	127413.986845	37.077146
1671.506454	127613.445684	37.082164
1673.582685	127817.764758	37.087181
1674.800864	128029.970237	37.092199
1676.914155	128240.438894	37.097216
1678.422795	128452.981938	37.102234
1680.374721	128663.312910	37.107252
1681.968606	128867.547271	37.112269
1683.649981	129080.942052	37.117287
1685.235628	129293.084062	37.122304
1687.165421	129509.449299	37.127322
1688.797574	129723.070683	37.132340
1690.369723	129944.188246	37.137357
1692.175494	130157.315353	37.142375
1694.050324	130368.618415	37.147392
1695.578055	130587.246729	37.152410
1697.737769	130798.050816	37.157428
1699.553046	131011.713609	37.162445
1701.447390	131209.149756	37.167463
1703.503320	131415.062734	37.172480
1705.395504	131629.833189	37.177498
1707.152178	131836.657557	37.182516
1708.705112	132044.339366	37.187533
1709.983097	132252.115715	37.192551
1712.106320	132463.783753	37.197568
1713.524208	132678.151059	37.202586
1715.172305	132883.639634	37.207604
1716.697129	133104.120978	37.212621
1718.440098	133313.124249	37.217639
1719.960215	133542.211479	37.222656
1721.775765	133769.997721	37.227674
1723.592913	133983.408348	37.232692
1725.382697	134198.105849	37.237709
1727.203451	134409.119748	37.242727
1729.524104	134610.159351	37.247744
1730.844174	134824.628443	37.252762
1732.918414	135032.090944	37.257780
1734.711343	135245.422565	37.262797
1735.912630	135466.359366	37.267815
1737.871505	135674.781803	37.272832
1739.674976	135899.903333	37.277850
1741.206937	136111.693489	37.282868
1742.793531	136336.305293	37.287885
1743.597351	136569.453269	37.292903
1746.078537	136779.360318	37.297920
1747.493407	137024.445354	37.302938
1749.158580	137246.854079	37.307956
1751.038242	137474.230317	37.312973
1752.793088	137698.949523	37.317991
1754.733279	137925.684070	37.323008
1756.460422	138164.038930	37.328026
1758.237567	138376.182084	37.333044
1759.913455	138589.864788	37.338061
1761.544161	138817.159462	37.343079
1763.799498	139026.312389	37.348096
1764.834202	139233.130843	37.353114
1766.677639	139437.514679	37.358132
1768.321627	139644.836565	37.363149
1769.648268	139863.985575	37.368167
1771.442587	140092.936100	37.373184
1772.826575	140320.809432	37.378202
1774.615620	140549.585308	37.383220
1776.642266	140784.188446	37.388237
1778.212343	141012.251861	37.393255
1779.719007	141236.455502	37.398272
1781.418752	141479.603136	37.403290
1782.965461	141730.758475	37.408308
1784.509418	141967.168486	37.413325
1786.220010	142227.540014	37.418343
1787.817719	142485.925288	37.423360
1789.327800	142748.323326	37.428378
1791.271088	143016.658365	37.433396
1792.794864	143276.747268	37.438413
1794.538459	143560.143013	37.443431
1796.447055	143825.492656	37.448448
1798.355563	144090.196458	37.453466
1800.128137	144370.965152	37.458484
1802.823192	144631.805356	37.463501
1804.912694	144891.459288	37.468519
1806.810704	145147.565245	37.473536
1808.621685	145415.971884	37.478554
1810.570819	145675.613623	37.483572
1812.933405	145934.646581	37.488589
1814.465465	146204.852310	37.493607
1816.265987	146452.044727	37.498624
1818.195343	146718.612123	37.503642
1819.809364	146985.496516	37.508660
1821.535113	147239.088614	37.513677
1823.383345	147520.015224	37.518695
1825.378238	147784.674039	37.523712
1827.247253	148062.516047	37.528730
1828.786906	148342.809711	37.533748
1830.266162	148618.786035	37.538765
1831.681130	148901.678711	37.543783
1833.935057	149182.665320	37.548800
1835.611077	149459.173890	37.553818
1837.548988	149745.289840	37.558836
1839.634265	150023.248107	37.563853
1841.245499	150319.394743	37.568871
1842.689650	150596.744935	37.573888
1845.006621	150886.120891	37.578906
1847.127108	151172.799893	37.583924
1849.127247	151464.601896	37.588941
1850.993177	151758.165351	37.593959
1852.978689	152040.896839	37.598976
1854.710707	152314.948701	37.603994
1856.457465	152597.961375	37.609012
1858.569532	152882.759230	37.614029
1860.213192	153170.500244	37.619047
1862.405897	153449.043070	37.624064
1863.811994	153732.063725	37.629082
1865.229509	154017.737071	37.634100
1867.884645	154305.491479	37.639117
1869.290137	154606.643747	37.644135
1871.197558	154881.950226	37.649152
1873.184724	155166.563211	37.654170
1874.997841	155465.688931	37.659188
1876.883262	155750.587211	37.664205
1878.450726	156052.077262	37.669223
1880.282099	156343.714923	37.674240
1882.549478	156621.436377	37.679258
1884.157439	156890.375514	37.684276
1886.460571	157146.322557	37.689293
1888.341664	157427.598965	37.694311
1890.168981	157692.584920	37.699328
1892.101448	157958.812477	37.704346
1893.500850	158222.889870	37.709364
1895.097878	158505.256534	37.714381
1896.934606	158778.751455	37.719399
1898.709926	159065.028443	37.724416
1900.846005	159360.619662	37.729434
1902.519957	159642.941544	37.734452
1904.498375	159924.150931	37.739469
1906.285504	160217.604291	37.744487
1908.380536	160494.024667	37.749504
1910.635751	160790.721382	37.754522
1912.747267	161067.078251	37.759540
1914.993614	161350.969217	37.764557
1916.932399	161646.957484	37.769575
1918.684829	161939.256296	37.774592
1920.602999	162230.362645	37.779610
1922.266836	162519.034216	37.784628
1924.311589	162819.962789	37.789645
1926.122850	163111.305591	37.794663
1927.932758	163407.118896	37.799680
1929.586642	163710.651624	37.804698
1931.261704	164019.781441	37.809716
1933.317438	164326.149181	37.814733
1935.021025	164643.923563	37.819751
1936.879944	164954.578066	37.824768
1938.164646	165284.266316	37.829786
1940.270913	165613.637872	37.834804
1942.136612	165950.133100	37.839821
1943.618793	166294.244115	37.844839
1945.482849	166622.439382	37.849856
1947.714301	166967.148168	37.854874
1948.973712	167309.584879	37.859892
1950.973626	167657.621577	37.864909
1953.292084	168012.390542	37.869927
1955.691479	168351.290262	37.874944
1958.349613	168677.962248	37.879962
1959.914997	169041.182775	37.884980
1962.271666	169362.940271	37.889997
1964.106051	169715.025082	37.895015
1966.025799	170063.530400	37.900032
1967.763703	170403.114107	37.905050
1969.380633	170759.707232	37.910068
1971.678203	171103.613034	37.915085
1973.642816	171454.530443	37.920103
1975.707279	171800.977132	37.925120
1977.854663	172140.543127	37.930138
1980.077582	172502.687949	37.935156
1982.186999	172850.922797	37.940173
1984.120336	173200.710355	37.945191
1985.973065	173547.223309	37.950208
1988.054476	173893.740306	37.955226
1989.871647	174255.740612	37.960244
1991.859254	174596.916786	37.965261
1993.605167	174954.245823	37.970279
1995.465748	175312.891905	37.975296
1997.580824	175674.357053	37.980314
1999.638320	176026.651981	37.985332
2001.370563	176389.449698	37.990349
2003.248952	176755.400842	37.995367
2004.995494	177107.812275	38.000384
2007.407403	177472.718460	38.005402
2009.576445	177840.991021	38.010420
2011.734926	178192.428589	38.015437
2013.953753	178551.070996	38.020455
2015.601390	178892.025724	38.025472
2017.868102	179217.621646	38.030490
2019.747849	179558.314281	38.035508
2021.914067	179885.020409	38.040525
2024.377924	180218.183208	38.045543
2026.578866	180540.340164	38.050560
2029.073704	180853.995068	38.055578
2030.702619	181186.021505	38.060596
2032.694960	181505.674570	38.065613
2034.607802	181842.687998	38.070631
2036.198243	182174.444613	38.075648
2038.570679	182511.998496	38.080666
2040.218983	182861.578111	38.085684
2041.913223	183215.215616	38.090701
2043.484609	183563.184277	38.095719
2045.471708	183915.204072	38.100736
2047.621552	184284.775727	38.105754
2049.551953	184653.519366	38.110772
2052.029026	185004.628654	38.115789
2053.576236	185382.121058	38.120807
2055.333022	185754.781830	38.125824
2057.237877	186135.040679	38.130842
2058.936493	186530.369409	38.135860
2060.812339	186919.042825	38.140877
2063.037105	187322.318878	38.145895
2064.654225	187788.301003	38.150912
2066.306861	188194.082358	38.155930
2068.434066	188618.511014	38.160948
2070.898304	189015.253794	38.165965
2072.697527	189434.732865	38.170983
2074.675050	189849.334344	38.176000
2077.505247	190245.364128	38.181018
2079.397815	190661.912198	38.186036
2081.686928	191078.679454	38.191053
2084.205627	191490.002171	38.196071
2085.960002	191896.187360	38.201088
2088.232154	192314.206219	38.206106
2089.851068	192735.173056	38.211124
2091.766941	193168.033478	38.216141
2094.286688	193597.423105	38.221159
2095.683252	194023.331256	38.226176
2098.053152	194444.440953	38.231194
2099.968862	194885.587975	38.236212
2102.376913	195317.794834	38.241229
2104.315394	195757.137725	38.246247
2106.580335	196191.782785	38.251264
2108.869075	196632.902881	38.256282
2110.778391	197068.495088	38.261300
2113.314010	197496.497690	38.266317
2115.430713	197927.081528	38.271335
2117.545220	198368.157898	38.276352
2119.766615	198812.013144	38.281370
2121.683385	199253.249906	38.286388
2124.018391	199680.883599	38.291405
2126.419825	200123.088896	38.296423
2128.183412	200561.838400	38.301440
2130.648370	200996.822030	38.306458
2132.602834	201439.837163	38.311476
2134.984827	201871.457505	38.316493
2137.449214	202301.287953	38.321511
2139.522373	202743.475134	38.326528
2142.126407	203174.200484	38.331546
2144.005405	203612.381041	38.336564
2146.186488	204032.073333	38.341581
2148.380910	204458.851837	38.346599
2150.460471	204887.198738	38.351616
2152.593236	205315.944747	38.356634
2154.344520	205745.259109	38.361652
2157.008203	206148.750061	38.366669
2159.524091	206555.719601	38.371687
2161.247447	206957.605653	38.376704
2163.566435	207354.776405	38.381722
2165.492855	207763.414949	38.386740
2167.694241	208167.667507	38.391757
2169.767750	208579.612433	38.396775
2171.300760	208992.378887	38.401792
2173.885417	209401.400521	38.406810
2175.674622	209824.899487	38.411828
2177.468119	210251.523101	38.416845
2179.353069	210676.837607	38.421863
2181.739446	211115.640176	38.426880
2183.585411	211552.012603	38.431898
2185.850804	211988.650667	38.436916
2187.822082	212439.484923	38.441933
2190.290535	212871.291408	38.446951
2192.261514	213314.175670	38.451968
2194.862337	213764.964661	38.456986
2196.929103	214221.731022	38.462004
2198.792847	214671.721380	38.467021
2201.156131	215124.810019	38.472039
2202.600736	215590.439210	38.477056
2204.880229	216065.516247	38.482074
2207.069144	216541.522461	38.487092
2208.846512	217021.378416	38.492109
2211.962310	217498.511589	38.497127
2213.915848	217972.879256	38.502144
2216.606836	218446.751532	38.507162
2218.911077	218917.229468	38.512180
2221.348484	219395.994155	38.517197
2224.371048	219859.400344	38.522215
2225.966494	220337.229786	38.527232
2228.982929	220801.806131	38.532250
2230.786936	221275.970924	38.537268
2233.219935	221747.878737	38.542285
2235.729666	222205.624775	38.547303
2237.808080	222681.144760	38.552320
2240.476228	223157.741731	38.557338
2242.812527	223628.293518	38.562356
2244.654224	224099.151038	38.567373
2247.463810	224568.537012	38.572391
2249.396847	225041.031750	38.577408
2251.632889	225506.061381	38.582426
2254.271714	225973.390930	38.587444
2256.542645	226438.821612	38.592461
2259.535951	226896.188362	38.597479
2261.685064	227366.236060	38.602496
2264.103548	227831.262555	38.607514
2266.182953	228295.528786	38.612532
2267.963684	228763.397941	38.617549
2270.167100	229224.519892	38.622567
2272.856933	229693.314205	38.627584
2275.571145	230148.462549	38.632602
2277.931632	230597.949819	38.637620
2279.932760	231064.691299	38.642637
2282.226247	231529.354683	38.647655
2284.388076	231991.396244	38.652672
2286.523727	232457.836446	38.657690
2288.439009	232931.245868	38.662708
2290.205078	233402.950658	38.667725
2292.533085	233878.860846	38.672743
2294.681040	234362.419772	38.677760
2296.601844	234848.757179	38.682778
2298.687180	235336.973748	38.687796
2300.774556	235830.244802	38.692813
2303.018698	236327.530064	38.697831
2305.005112	236815.633249	38.702848
2307.225734	237297.780287	38.707866
2309.652409	237768.869421	38.712884
2311.547279	238260.261954	38.717901
2313.869530	238736.141865	38.722919
2315.694009	239230.414485	38.727936
2317.913091	239715.047775	38.732954
2320.214836	240216.535303	38.737972
2322.207327	240715.809171	38.742989
2324.870992	241215.155506	38.748007
2326.974763	241725.587675	38.753024
2329.272701	242231.466835	38.758042
2331.665040	242738.092374	38.763060
2334.136831	243259.362113	38.768077
2336.625488	243775.090194	38.773095
2338.890416	244293.163605	38.778112
2340.826631	244813.268394	38.783130
2343.148417	245336.715916	38.788148
2345.716142	245877.143772	38.793165
2348.608337	246392.167718	38.798183
2351.701022	246909.546987	38.803200
2354.196463	247428.211748	38.808218
2355.911441	247967.979081	38.813236
2358.447084	248498.523027	38.818253
2360.903447	249027.604409	38.823271
2362.693019	249557.651654	38.828288
2365.023031	250094.649595	38.833306
2368.017940	250610.839563	38.838324
2370.637234	251158.330972	38.843341
2373.330134	251680.711867	38.848359
2375.923144	252223.809167	38.853376
2378.207674	252753.464187	38.858394
2380.421176	253286.760866	38.863412
2382.758020	253831.340185	38.868429
2384.962334	254369.714714	38.873447
2386.952431	254923.310641	38.878464
2389.243408	255472.818745	38.883482
2391.361477	256031.521430	38.888500
2393.383534	256603.140544	38.893517
2395.663754	257162.219705	38.898535
2398.288952	257735.518115	38.903552
2400.272059	258299.515579	38.908570
2403.023233	258877.640789	38.913588
2405.385875	259450.438836	38.918605
2407.749931	260027.831452	38.923623
2410.190906	260610.721186	38.928640
2412.759910	261183.885220	38.933658
2415.163743	261762.863340	38.938676
2417.382203	262356.015142	38.943693
2420.190615	262933.603495	38.948711
2422.778939	263522.525936	38.953728
2425.293711	264095.886697	38.958746
2428.174723	264675.257847	38.963764
2430.213483	265264.561002	38.968781
2433.020034	265844.115050	38.973799
2435.130741	266433.781300	38.978816
2437.488508	267026.301117	38.983834
2440.114154	267615.550074	38.988852
2442.445921	268191.811769	38.993869
2445.076983	268772.976130	38.998887
2447.652992	269355.237632	39.003904
2450.583189	269932.208403	39.008922
2453.235986	270513.434803	39.013940
2455.457802	271083.981334	39.018957
2457.775108	271661.874699	39.023975
2460.246767	272250.610392	39.028992
2462.576089	272830.576853	39.034010
2465.244407	273400.175475	39.039028
2467.594460	273975.178598	39.044045
2470.469324	274530.134317	39.049063
2472.765529	275082.230414	39.054080
2474.554732	275629.246268	39.059098
2477.532939	276181.228876	39.064116
2479.586626	276730.177096	39.069133
2481.782906	277286.667345	39.074151
2484.231391	277837.578182	39.079168
2486.611602	278399.542834	39.084186
2489.500392	278962.770229	39.089204
2491.668438	279532.683004	39.094221
2493.926610	280104.253552	39.099239
2496.069470	280679.621525	39.104256
2498.586326	281269.985827	39.109274
2501.059233	281845.267989	39.114292
2503.564565	282436.310338	39.119309
2506.205694	283018.235680	39.124327
2509.170955	283610.161758	39.129344
2511.276852	284193.151126	39.134362
2514.372558	284778.978014	39.139380
2516.853672	285375.535297	39.144397
2519.616995	285962.902039	39.149415
2521.869083	286563.826759	39.154432
2524.694196	287161.152779	39.159450
2527.286601	287746.753067	39.164468
2528.961658	288362.123340	39.169485
2532.151708	288953.028344	39.174503
2534.588520	289578.933077	39.179520
2536.629029	290186.789415	39.184538
2539.909339	290800.134574	39.189556
2542.151289	291404.545448	39.194573
2545.279014	292009.701278	39.199591
2547.938800	292613.603698	39.204608
2550.254883	293241.471016	39.209626
2552.923285	293851.681914	39.214644
2555.370178	294464.942426	39.219661
2557.531919	295082.049373	39.224679
2560.549245	295707.572786	39.229696
2562.771233	296333.390992	39.234714
2565.697681	296954.599061	39.239732
2568.252440	297580.326556	39.244749
2570.665881	298213.279304	39.249767
2573.090058	298843.887623	39.254784
2575.645844	299477.311721	39.259802
2578.218801	300106.790928	39.264820
2580.710168	300758.311250	39.269837
2583.308571	301391.630484	39.274855
2586.624067	302018.636497	39.279872
2589.072086	302660.925470	39.284890
2591.935778	303287.225304	39.289908
2594.792838	303911.284828	39.294925
2597.775700	304532.499602	39.299943
2600.362262	305159.683205	39.304960
2602.914516	305795.774368	39.309978
2605.821661	306414.465151	39.314996
2607.844238	307049.506159	39.320013
2610.312914	307684.875852	39.325031
2613.073122	308316.943057	39.330048
2615.069527	308955.111351	39.335066
2617.629520	309604.757973	39.340084
2620.312736	310246.330669	39.345101
2622.582719	310890.370409	39.350119
2625.051523	311539.776773	39.355136
2627.379721	312196.632771	39.360154
2630.075975	312848.828472	39.365172
2632.590383	313519.900899	39.370189
2634.870751	314170.366247	39.375207
2638.194840	314834.111139	39.380224
2640.774397	315476.516914	39.385242
2643.308033	316111.180236	39.390260
2645.670562	316746.673378	39.395277
2648.078466	317382.480370	39.400295
2650.965695	318010.438117	39.405312
2653.201237	318651.380051	39.410330
2655.859119	319288.389611	39.415348
2658.615276	319938.671908	39.420365
2660.485114	320590.985587	39.425383
2663.527024	321245.416181	39.430400
2666.288458	321902.722444	39.435418
2669.171185	322550.687012	39.440436
2671.571620	323213.357837	39.445453
2674.420025	323877.267919	39.450471
2677.895340	324528.687410	39.455488
2680.542073	325184.412180	39.460506
2683.546483	325836.518585	39.465524
2685.919901	326499.014028	39.470541
2688.482517	327159.388668	39.475559
2691.117193	327824.815606	39.480576
2693.376164	328510.104948	39.485594
2696.522069	329183.066402	39.490612
2698.967590	329861.224824	39.495629
2701.464857	330546.923720	39.500647
2704.110128	331238.371763	39.505664
2707.104576	331920.747062	39.510682
2710.267519	332597.401431	39.515700
2713.021738	333293.158933	39.520717
2716.001749	333977.833557	39.525735
2719.307869	334664.956347	39.530752
2721.884866	335347.842258	39.535770
2724.664655	336018.837983	39.540788
2727.252733	336710.067978	39.545805
2729.892665	337396.508200	39.550823
2732.756541	338090.332589	39.555840
2735.146612	338785.916858	39.560858
2737.810589	339474.799727	39.565876
2740.232993	340188.233410	39.570893
2743.145011	340898.837409	39.575911
2746.062126	341596.745126	39.580928
2748.650351	342310.871085	39.585946
2751.506846	343014.009941	39.590964
2754.089374	343731.024246	39.595981
2756.626760	344455.156948	39.600999
2759.622705	345169.287321	39.606016
2762.219739	345899.162218	39.611034
2765.243326	346624.973700	39.616052
2767.666822	347347.414218	39.621069
2770.250878	348086.144487	39.626087
2772.944300	348816.955296	39.631104
2775.458767	349564.944168	39.636122
2778.282485	350295.499095	39.641140
2781.412461	351039.783353	39.646157
2784.174959	351780.228468	39.651175
2787.295628	352514.718700	39.656192
2790.053985	353257.564499	39.661210
2792.964375	353987.844960	39.666228
2795.903936	354740.540986	39.671245
2798.429024	355487.047007	39.676263
2801.655498	356222.068770	39.681280
2804.240126	356970.228664	39.686298
2806.809722	357705.165494	39.691316
2809.947281	358458.729637	39.696333
2812.578518	359201.530122	39.701351
2815.739363	359950.364349	39.706368
2818.373035	360686.740433	39.711386
2820.705951	361438.328137	39.716404
2823.744170	362187.227273	39.721421
2825.953227	362930.787315	39.726439
2829.159920	363648.270862	39.731456
2831.957033	364377.408425	39.736474
2834.952019	365088.249557	39.741492
2837.553589	365815.683678	39.746509
2840.231148	366536.093213	39.751527
2843.538962	367260.061275	39.756544
2845.807829	367978.217577	39.761562
2848.957410	368683.117687	39.766580
2852.185004	369414.291085	39.771597
2854.773168	370147.369522	39.776615
2857.527016	370866.694875	39.781632
2860.078581	371606.328973	39.786650
2862.994496	372340.059157	39.791668
2865.564811	373088.341602	39.796685
2868.375642	373836.338297	39.801703
2871.530070	374587.884076	39.806720
2874.173414	375348.279785	39.811738
2877.047008	376109.859735	39.816756
2879.958218	376871.792363	39.821773
2882.899106	377630.000246	39.826791
2886.684857	378375.009339	39.831808
2889.725483	379146.559059	39.836826
2892.541231	379897.654464	39.841844
2895.799090	380661.881662	39.846861
2898.368274	381432.500610	39.851879
2901.100638	382199.652119	39.856896
2903.708176	382973.562757	39.861914
2906.238563	383747.386232	39.866932
2908.908793	384537.525063	39.871949
2911.777719	385342.575587	39.876967
2914.635159	386138.587034	39.881984
2917.900438	386940.005139	39.887002
2920.684604	387740.434380	39.892020
2923.555376	388536.114736	39.897037
2926.452364	389348.021628	39.902055
2929.381422	390152.300938	39.907072
2932.544631	390977.887022	39.912090
2935.625043	391785.178372	39.917108
2938.764625	392592.281936	39.922125
2941.481426	393413.551208	39.927143
2944.918291	394226.073171	39.932160
2946.967916	395047.795711	39.937178
2950.203548	395877.608533	39.942196
2953.341295	396702.800695	39.947213
2956.148084	397539.001195	39.952231
2959.538233	398364.804856	39.957248
2962.550678	399197.016508	39.962266
2965.331016	400035.207717	39.967284
2968.521646	400868.901160	39.972301
2971.505977	401701.230054	39.977319
2974.799328	402524.167850	39.982336
2977.743068	403356.291269	39.987354
2980.887621	404185.367095	39.992372
2984.309502	405000.755870	39.997389
2987.417570	405826.639590	40.002407
2990.691385	406645.837997	40.007424
2993.688428	407464.796489	40.012442
2996.806261	408285.375921	40.017460
2999.900317	409085.031315	40.022477
3002.297528	409922.309284	40.027495
3005.695458	410724.792518	40.032512
3008.181033	411553.949823	40.037530
3010.945407	412379.541388	40.042548
3014.017150	413202.625406	40.047565
3017.375345	414041.619138	40.052583
3020.080558	414851.240924	40.057600
3022.778475	415681.623111	40.062618
3025.693551	416506.729232	40.067636
3028.642893	417311.161391	40.072653
3031.521773	418114.208275	40.077671
3034.280032	418907.633841	40.082688
3037.288113	419712.116752	40.087706
3040.121214	420516.697001	40.092724
3043.017244	421337.064711	40.097741
3045.883645	422149.920414	40.102759
3048.764138	422968.556928	40.107776
3051.143366	423798.919041	40.112794
3054.339961	424644.693254	40.117812
3056.975445	425494.210452	40.122829
3059.788494	426341.288152	40.127847
3062.690162	427195.343669	40.132864
3065.236417	428073.329851	40.137882
3068.539574	428949.693681	40.142900
3071.700683	429828.871724	40.147917
3074.877132	430705.278820	40.152935
3078.276028	431585.959142	40.157952
3081.427200	432473.208950	40.162970
3084.137105	433353.664270	40.167988
3087.619610	434262.058320	40.173005
3090.551715	435148.259991	40.178023
3094.019331	436054.550685	40.183040
3097.111595	436955.955560	40.188058
3099.947762	437871.050836	40.193076
3103.115499	438780.694814	40.198093
3106.347705	439717.011747	40.203111
3109.411856	440629.917366	40.208128
3112.653559	441553.561834	40.213146
3115.416656	442480.670200	40.218164
3118.959165	443401.499033	40.223181
3121.914267	444332.273569	40.228199
3125.085175	445267.664807	40.233216
3128.600992	446192.752666	40.238234
3131.688948	447133.566675	40.243252
3135.337509	448072.325839	40.248269
3138.568291	449000.547418	40.253287
3141.836830	449937.653003	40.258304
3145.182676	450876.666906	40.263322
3147.857952	451801.497813	40.268340
3151.519455	452745.463800	40.273357
3154.094255	453677.684862	40.278375
3157.894088	454618.096566	40.283392
3161.117749	455566.624296	40.288410
3163.793290	456509.684073	40.293428
3167.549603	457454.139858	40.298445
3170.237171	458415.063116	40.303463
3173.546930	459356.103248	40.308480
3176.569573	460320.552480	40.313498
3179.705114	461271.355583	40.318516
3183.400632	462227.720555	40.323533
3185.895891	463182.704841	40.328551
3189.015388	464139.001334	40.333568
3192.296665	465108.184334	40.338586
3195.379123	466077.090130	40.343604
3198.572859	467040.827561	40.348621
3202.018418	468005.125816	40.353639
3205.838255	468967.594859	40.358656
3209.180653	469920.347938	40.363674
3212.803654	470884.803604	40.368692
3216.175559	471832.700433	40.373709
3218.617076	472778.821195	40.378727
3222.214716	473743.111967	40.383744
3225.409799	474696.466506	40.388762
3228.249301	475661.365880	40.393780
3231.935416	476611.656751	40.398797
3234.927113	477572.283401	40.403815
3238.287714	478506.279385	40.408832
3241.674495	479434.117169	40.413850
3244.709777	480353.991461	40.418868
3247.767946	481245.584100	40.423885
3250.990676	482173.286168	40.428903
3253.995925	483092.702321	40.433920
3257.691286	484006.464142	40.438938
3260.354996	484933.685780	40.443956
3263.663787	485850.573535	40.448973
3266.529147	486789.392288	40.453991
3269.636086	487719.853791	40.459008
3272.917777	488670.432551	40.464026
3275.993074	489617.458010	40.469044
3279.038278	490570.876499	40.474061
3282.108145	491537.679091	40.479079
3285.124663	492513.040190	40.484096
3288.572229	493480.263534	40.489114
3291.627809	494462.945018	40.494132
3294.847099	495456.563736	40.499149
3298.149984	496449.196633	40.504167
3301.188554	497448.852628	40.509184
3304.516133	498454.084657	40.514202
3307.581077	499472.528167	40.519220
3310.755712	500483.886861	40.524237
3313.957736	501511.025999	40.529255
3317.462392	502539.152563	40.534272
3320.753024	503572.825454	40.539290
3323.722918	504623.684247	40.544308
3327.228541	505662.457147	40.549325
3330.477399	506714.829785	40.554343
3333.811022	507777.827656	40.559360
3337.156852	508834.807610	40.564378
3340.276386	509900.949176	40.569396
3343.889631	510966.077970	40.574413
3348.004435	512023.251821	40.579431
3352.319708	513087.606694	40.584448
3356.435151	514124.755429	40.589466
3359.643099	515173.080538	40.594484
3363.081991	516202.384458	40.599501
3365.992266	517269.602325	40.604519
3369.371754	518322.285896	40.609536
3372.602451	519382.150092	40.614554
3376.037235	520448.032176	40.619572
3379.371663	521515.554788	40.624589
3382.629048	522582.452018	40.629607
3385.619742	523647.848642	40.634624
3388.900098	524724.722909	40.639642
3392.087854	525815.542939	40.644660
3395.282198	526893.310173	40.649677
3398.880930	527974.995842	40.654695
3402.402772	529074.889356	40.659712
3406.128316	530156.426084	40.664730
3409.346812	531240.363024	40.669748
3413.060221	532325.589153	40.674765
3416.771611	533421.973208	40.679783
3420.086809	534498.241291	40.684800
3423.676704	535584.719452	40.689818
3427.380538	536674.049896	40.694836
3430.780756	537761.678220	40.699853
3433.966356	538852.308964	40.704871
3437.322552	539937.750244	40.709888
3440.783684	541021.425901	40.714906
3443.883320	542131.209234	40.719924
3447.425910	543218.446534	40.724941
3450.813069	544318.206895	40.729959
3454.060870	545418.343414	40.734976
3457.422841	546507.830284	40.739994
3460.771674	547622.854756	40.745012
3464.474386	548702.360611	40.750016
3467.536806	549750.849255	40.755021
3470.691940	550758.863037	40.760026
3473.951309	551716.456256	40.765031
3476.628301	552623.445792	40.770036
3479.571476	553464.983503	40.775040
3482.483010	554263.444805	40.780045
3485.004489	555004.419794	40.785050
3487.916798	555684.581174	40.790055
3490.234014	556315.901755	40.795060
3492.384344	556881.388528	40.800064
3494.514214	557411.930023	40.805069
3496.651970	557887.478642	40.810074
3498.760743	558314.578302	40.815079
3500.281199	558699.249757	40.820084
3502.076808	559040.659382	40.825088
3503.325775	559335.673234	40.830093
3504.658642	559602.533500	40.835098
3506.231025	559816.250094	40.840103
3507.113112	560008.167290	40.845108
3508.177395	560170.815999	40.850112
3509.286721	560285.280185	40.855117
3510.183924	560381.541124	40.860122
3511.200775	560454.072097	40.865127
3511.562003	560508.720867	40.870132
3512.434305	560543.095838	40.875136
3513.216377	560539.759130	40.880141
3513.710351	560524.411101	40.885146
3514.505358	560496.960028	40.890151
3514.954246	560454.844115	40.895156
3515.470814	560378.608270	40.900160
3515.851729	560294.405687	40.905165
3515.962523	560201.503591	40.910170
3516.168506	560090.149418	40.915175
3516.289057	559978.606548	40.920180
3516.858892	559841.221220	40.925184
3516.961531	559711.392383	40.930189
3517.162339	559570.243298	40.935194
3517.749555	559406.826909	40.940199
3517.382742	559240.190691	40.945204
3517.575236	559075.524945	40.950208
3517.866509	558903.556626	40.955213
3518.065960	558736.322818	40.960218
3518.065979	558538.570359	40.965223
3518.052346	558357.648210	40.970228
3517.766644	558158.828558	40.975232
3518.036491	557956.402000	40.980237
3517.878782	557757.304512	40.985242
3517.845173	557551.752835	40.990247
3517.551113	557362.669043	40.995252
3517.339688	557152.314417	41.000256
3517.599637	556938.264803	41.005261
3517.376972	556737.301213	41.010266
3517.733503	556523.832162	41.015271
3517.361860	556311.879672	41.020276
3517.326469	556106.403953	41.025280
3517.247256	555893.443764	41.030285
3517.665148	555687.287293	41.035290
3517.398081	555466.911127	41.040295
3516.656876	555247.911364	41.045300
3516.707585	555036.926031	41.050304
3516.997110	554823.939779	41.055309
3516.381695	554614.307150	41.060314
3516.382935	554400.152059	41.065319
3516.260829	554195.310575	41.070324
3515.884154	553985.579607	41.075328
3516.003597	553775.013859	41.080333
3515.840518	553578.813419	41.085338
3515.628060	553361.808177	41.090343
3515.195321	553165.592734	41.095348
3515.105284	552960.323221	41.100352
3515.291191	552756.465024	41.105357
3515.021660	552561.973741	41.110362
3514.920177	552361.270203	41.115367
3515.071090	552163.691022	41.120372
3514.866957	551970.185466	41.125376
3514.869186	551776.745260	41.130381
3514.432670	551581.108038	41.135386
3514.629347	551377.526668	41.140391
3514.356010	551193.269625	41.145396
3514.198703	550996.875750	41.150400
3513.986291	550805.967224	41.155405
3513.710177	550625.522907	41.160410
3513.764250	550425.266014	41.165415
3513.646440	550249.366640	41.170420
3513.424997	550070.413926	41.175424
3513.215297	549880.194403	41.180429
3512.852727	549708.599009	41.185434
3512.766471	549535.047578	41.190439
3512.374207	549366.116839	41.195444
3512.118567	549185.748666	41.200448
3512.174023	549028.107165	41.205453
3512.016234	548871.955020	41.210458
3512.312564	548701.198367	41.215463
3511.785490	548541.831079	41.220468
3511.779769	548378.257260	41.225472
3511.719214	548223.992567	41.230477
3511.813982	548064.522329	41.235482
3512.022862	547901.109921	41.240487
3511.526572	547749.119695	41.245492
3511.503649	547577.190246	41.250496
3511.329726	547423.637207	41.255501
3511.042082	547276.738115	41.260506
3511.038578	547113.096875	41.265511
3510.795137	546968.550856	41.270516
3511.112766	546823.262056	41.275520
3511.116039	546664.391460	41.280525
3510.363219	546519.315957	41.285530
3510.240026	546368.155935	41.290535
3510.505397	546230.512810	41.295540
3509.980067	546086.000348	41.300544
3510.081750	545948.480152	41.305549
3510.162760	545817.399412	41.310554
3510.268628	545672.381548	41.315559
3510.208758	545542.929291	41.320564
3509.770281	545399.250347	41.325568
3510.087649	545272.804672	41.330573
3509.862741	545141.814705	41.335578
3509.643651	544997.443105	41.340583
3509.622188	544870.593384	41.345588
3509.600538	544738.008272	41.350592
3509.127805	544614.847722	41.355597
3509.066887	544472.658617	41.360602
3508.969257	544349.789179	41.365607
3508.834131	544219.882162	41.370612
3508.801581	544100.370337	41.375616
3508.503812	543977.226562	41.380621
3508.351794	543864.521897	41.385626
3508.690845	543741.830035	41.390631
3508.111241	543631.704977	41.395636
3507.939176	543513.718364	41.400640
3507.980950	543402.639419	41.405645
3508.027146	543309.769270	41.410650
3508.129454	543186.706363	41.415655
3507.824531	543081.363051	41.420660
3507.816160	542973.708914	41.425664
3507.780541	542862.083846	41.430669
3507.193304	542762.868923	41.435674
3507.631259	542655.293520	41.440679
3507.171567	542555.805570	41.445684
3507.352658	542453.198604	41.450688
3507.461004	542355.582707	41.455693
3507.509747	542262.855333	41.460698
3507.518963	542165.404311	41.465703
3507.012542	542066.875641	41.470708
3507.162621	541968.696833	41.475712
3507.388343	541875.435954	41.480717
3506.613566	541767.337311	41.485722
3506.790693	541673.529073	41.490727
3506.499246	541584.874569	41.495732
3506.464564	541496.682609	41.500736
3506.765298	541396.513708	41.505741
3506.087122	541316.873170	41.510746
3506.330939	541228.434741	41.515751
3506.640071	541148.991698	41.520756
3506.037199	541058.369396	41.525760
3506.111234	540976.144256	41.530765
3506.375221	540899.725537	41.535770
3506.182847	540807.528109	41.540775
3505.796937	540735.888837	41.545780
3505.838781	540648.232502	41.550784
3506.081019	540576.041733	41.555789
3506.120649	540492.812477	41.560794
3506.170819	540405.958228	41.565799
3506.083816	540334.270163	41.570804
3506.042714	540255.429487	41.575808
3506.051566	540177.033406	41.580813
3505.691276	540095.172023	41.585818
3505.635849	540013.564579	41.590823
3505.939096	539943.272801	41.595828
3505.573124	539855.322199	41.600832
3505.550376	539779.041963	41.605837
3505.640428	539706.668640	41.610842
3505.745099	539638.217572	41.615847
3505.287622	539563.110721	41.620852
3505.424668	539492.741666	41.625856
3505.474507	539416.146029	41.630861
3504.941168	539352.271239	41.635866
3504.990651	539291.224061	41.640871
3505.003032	539216.243322	41.645876
3505.029681	539153.739713	41.650880
3505.240596	539077.871793	41.655885
3505.119926	539019.416209	41.660890
3505.000949	538947.976884	41.665895
3504.657906	538888.347558	41.670900
3504.326562	538825.394813	41.675904
3504.515478	538767.342799	41.680909
3504.727038	538725.088561	41.685914
3504.355244	538649.661025	41.690919
3504.596038	538594.317629	41.695924
3504.561675	538531.669482	41.700928
3504.391842	538474.678442	41.705933
3504.227170	538417.837317	41.710938
3504.147040	538352.477878	41.715943
3504.728891	538318.367623	41.720948
3504.733355	538254.856545	41.725952
3504.670085	538194.173920	41.730957
3504.417069	538135.130957	41.735962
3504.319293	538073.647914	41.740967
3504.611459	538016.784235	41.745972
3504.404277	537956.827440	41.750976
3504.002071	537896.850384	41.755981
3504.086778	537849.127369	41.760986
3504.393729	537789.744032	41.765991
3504.191685	537740.454763	41.770996
3504.108782	537685.006807	41.776000
3504.225409	537633.654436	41.781005
3504.424197	537579.420380	41.786010
3504.190758	537511.765398	41.791015
3503.949931	537467.614587	41.796020
3503.742643	537414.852217	41.801024
3504.178237	537365.210631	41.806029
3504.434844	537325.360525	41.811034
3504.146695	537261.537730	41.816039
3503.757171	537206.739360	41.821044
3503.602993	537154.219295	41.826048
3503.553029	537112.302386	41.831053
3503.488565	537073.206074	41.836058
3503.758346	537028.823298	41.841063
3503.533152	536971.733491	41.846068
3503.597899	536937.750352	41.851072
3503.738485	536882.113140	41.856077
3503.439694	536855.282978	41.861082
3503.449526	536801.980981	41.866087
3503.582545	536764.966897	41.871092
3503.970049	536721.621692	41.876096
3503.955933	536673.456680	41.881101
3503.392577	536625.125297	41.886106
3503.663893	536572.435966	41.891111
3503.615070	536523.873137	41.896116
3503.638549	536482.546722	41.901120
3503.591046	536450.542714	41.906125
3503.449742	536401.943481	41.911130
3503.696498	536357.360632	41.916135
3503.762336	536319.449725	41.921140
3503.400375	536279.340290	41.926144
3503.437187	536226.182697	41.931149
3503.703528	536186.931533	41.936154
3503.523273	536142.062048	41.941159
3503.710090	536104.786018	41.946164
3503.636254	536054.765625	41.951168
3503.587064	536010.428958	41.956173
3503.280746	535967.239504	41.961178
3503.475577	535925.280616	41.966183
3503.299561	535888.513429	41.971188
3503.523223	535839.502928	41.976192
3503.510821	535795.763812	41.981197
3503.259519	535761.222714	41.986202
3502.744468	535709.658910	41.991207
3503.172746	535683.367508	41.996212
3502.804191	535638.122879	42.001216
3502.975871	535606.686685	42.006221
3503.028545	535582.013931	42.011226
3503.023671	535538.927134	42.016231
3502.864137	535510.210051	42.021236
3502.993793	535475.558566	42.026240
3503.238745	535432.835227	42.031245
3503.076173	535395.359826	42.036250
3503.160961	535363.181510	42.041255
3503.208281	535321.293941	42.046260
3503.280129	535288.815432	42.051264
3503.454963	535236.236305	42.056269
3503.045964	535204.688141	42.061274
3503.273001	535159.399480	42.066279
3502.860965	535129.563077	42.071284
3502.809075	535092.371594	42.076288
3503.088483	535058.400410	42.081293
3503.164939	535032.414118	42.086298
3503.209531	534982.018752	42.091303
3503.175650	534954.186960	42.096308
3503.052653	534918.717541	42.101312
3503.095417	534878.087698	42.106317
3502.902050	534848.971694	42.111322
3503.164601	534823.409070	42.116327
3502.871318	534766.370379	42.121332
3502.996426	534736.449476	42.126336
3503.177177	534695.596229	42.131341
3502.822967	534673.149638	42.136346
3502.915408	534628.282770	42.141351
3503.086568	534588.286447	42.146356
3502.963211	534563.135737	42.151360
3503.252579	534521.459599	42.156365
3502.702155	534495.267734	42.161370
3503.023645	534454.794544	42.166375
3502.913697	534422.895883	42.171380
3502.561484	534379.003467	42.176384
3502.981178	534346.317431	42.181389
3502.865231	534320.309303	42.186394
3503.171801	534286.986291	42.191399
3502.785881	534255.532888	42.196404
3502.868429	534214.743740	42.201408
3502.531330	534193.854226	42.206413
3502.536595	534161.030846	42.211418
3502.613270	534131.116077	42.216423
3502.825900	534095.441140	42.221428
3502.622591	534067.885507	42.226432
3502.738109	534038.820289	42.231437
3502.822336	534006.890383	42.236442
3502.723381	533962.604746	42.241447
3502.328207	533942.680362	42.246452
3502.501214	533918.187066	42.251456
3502.518940	533881.383995	42.256461
3502.459400	533859.494240	42.261466
3502.231405	533829.827553	42.266471
3502.508379	533801.592502	42.271476
3502.629570	533777.761460	42.276480
3502.720804	533743.161641	42.281485
3502.609506	533720.071472	42.286490
3502.570155	533689.217217	42.291495
3502.302201	533654.824085	42.296500
3502.442432	533627.818174	42.301504
3502.646654	533595.868580	42.306509
3502.471927	533572.234239	42.311514
3502.604463	533540.547382	42.316519
3502.688137	533507.106015	42.321524
3502.561089	533482.356524	42.326528
3502.662745	533442.619191	42.331533
3502.383279	533427.760763	42.336538
3502.865790	533393.350843	42.341543
3502.811863	533368.086311	42.346548
3502.482679	533334.859778	42.351552
3502.575247	533310.679918	42.356557
3502.244821	533271.210674	42.361562
3502.573855	533248.806315	42.366567
3502.494328	533225.005490	42.371572
3502.285390	533196.492318	42.376576
3502.437747	533154.833098	42.381581
3502.392161	533147.791814	42.386586
3502.626442	533113.319088	42.391591
3502.648734	533094.436030	42.396596
3502.431263	533056.811339	42.401600
3502.533347	533029.306659	42.406605
3502.418342	532997.052845	42.411610
3502.255162	532959.922882	42.416615
3502.387295	532952.602107	42.421620
3502.498795	532929.828280	42.426624
3502.354319	532894.558027	42.431629
3502.197819	532871.120953	42.436634
3502.554771	532837.383600	42.441639
3502.729449	532818.275041	42.446644
3502.478262	532789.616508	42.451648
3502.473383	532758.754671	42.456653
3502.176112	532734.130931	42.461658
3502.189375	532710.616802	42.466663
3502.631935	532680.188622	42.471668
3502.581307	532650.944754	42.476672
3502.678307	532628.374044	42.481677
3502.594710	532600.494571	42.486682
3502.646557	532567.005384	42.491687
3502.666533	532550.135796	42.496692
3502.357254	532523.348576	42.501696
3502.349154	532483.222600	42.506701
3502.289430	532466.063218	42.511706
3502.365771	532438.561292	42.516711
3502.388013	532414.541749	42.521716
3502.367461	532379.250811	42.526720
3502.266830	532349.661608	42.531725
3502.044510	532330.463064	42.536730
3502.485979	532301.343227	42.541735
3502.090471	532286.451196	42.546740
3502.138928	532257.996603	42.551744
3502.443183	532239.773307	42.556749
3502.418518	532214.451625	42.561754
3502.352770	532187.525117	42.566759
3502.158989	532160.114985	42.571764
3502.464972	532140.179410	42.576768
3502.665663	532114.419671	42.581773
3502.344134	532081.591526	42.586778
3502.116091	532054.639648	42.591783
3502.368329	532029.626963	42.596788
3502.097466	532007.162767	42.601792
3502.146779	531984.850108	42.606797
3502.161804	531978.755404	42.611802
3502.556089	531933.177680	42.616807
3502.267814	531914.995784	42.621812
3502.164348	531894.569698	42.626816
3502.270721	531861.976512	42.631821
3502.100856	531836.475287	42.636826
3502.155304	531814.362938	42.641831
3502.416796	531806.618585	42.646836
3502.273556	531774.114373	42.651840
3502.207204	531748.395464	42.656845
3502.133158	531728.468046	42.661850
3502.144375	531695.083637	42.666855
3502.484368	531677.810662	42.671860
3502.025299	531651.296706	42.676864
3502.201588	531618.490627	42.681869
3502.107293	531606.773421	42.686874
3502.236441	531572.262618	42.691879
3502.305381	531554.326739	42.696884
3502.056269	531527.628804	42.701888
3502.455202	531505.915490	42.706893
3502.154408	531483.102584	42.711898
3502.439355	531461.608341	42.716903
3502.498754	531433.955873	42.721908
3502.213728	531411.895668	42.726912
3502.233916	531371.912917	42.731917
3502.108540	531360.401735	42.736922
3502.251256	531330.168117	42.741927
3502.194395	531319.502227	42.746932
3501.947129	531292.602113	42.751936
3502.054342	531264.438321	42.756941
3502.033001	531248.177705	42.761946
3502.071221	531225.361945	42.766951
3501.895347	531210.132384	42.771956
3501.905658	531186.414548	42.776960
3502.072917	531172.541428	42.781965
3501.675424	531145.916153	42.786970
3501.728036	531122.241971	42.791975
3502.014172	531114.946553	42.796980
3501.821986	531098.309510	42.801985
3502.391647	531070.224395	42.806989
3501.709087	531053.512544	42.811994
3502.141770	531021.017538	42.816999
3501.763559	531010.804229	42.822004
3502.091056	530996.704573	42.827009
3502.215882	530971.709686	42.832013
3502.036452	530949.632265	42.837018
3502.293448	530920.336638	42.842023
3502.203820	530897.540200	42.847028
3501.867323	530871.962307	42.852033
3501.910384	530856.043659	42.857037
3502.039002	530838.298926	42.862042
3502.234374	530803.977202	42.867047
3502.207285	530793.104831	42.872052
3501.984497	530773.098389	42.877057
3502.237742	530746.068907	42.882061
3502.297996	530737.650273	42.887066
3502.153315	530701.920913	42.892071
3502.137923	530690.341669	42.897076
3502.161845	530667.325739	42.902081
3502.320966	530642.677371	42.907085
3501.822216	530623.972517	42.912090
3502.148288	530605.743547	42.917095
3501.954854	530574.150545	42.922100
3501.694457	530550.826166	42.927105
3501.819308	530528.398550	42.932109
3501.892862	530520.430906	42.937114
3501.594959	530483.113415	42.942119
3501.714705	530484.857190	42.947124
3501.705784	530462.953834	42.952129
3501.660386	530445.940628	42.957133
3501.771171	530439.427457	42.962138
3501.779176	530408.104841	42.967143
3501.639712	530402.083797	42.972148
3501.619085	530377.412543	42.977153
3501.673633	530370.807377	42.982157
3501.683506	530362.799190	42.987162
3502.248023	530333.655820	42.992167
3501.839942	530310.756843	42.997172
3501.832287	530295.046830	43.002177
3501.717545	530273.612831	43.007181
3502.208343	530257.523069	43.012186
3501.995139	530233.183650	43.017191
3502.395456	530216.553995	43.022196
3502.125669	530196.302199	43.027201
3502.339434	530174.061567	43.032205
3502.419058	530143.482525	43.037210
3502.209460	530128.508733	43.042215
3502.242052	530096.879405	43.047220
3502.074193	530082.201208	43.052225
3502.372667	530058.083982	43.057229
3502.042834	530031.395545	43.062234
3502.146531	530008.517114	43.067239
3501.743234	529986.523258	43.072244
3501.716548	529972.225829	43.077249
3502.091608	529942.406066	43.082253
3502.050447	529933.499119	43.087258
3501.723107	529901.824613	43.092263
3501.975930	529894.835849	43.097268
3501.780029	529873.413824	43.102273
3501.865744	529851.595434	43.107277
3501.969902	529833.903504	43.112282
3501.804998	529814.188734	43.117287
3501.796899	529795.003475	43.122292
3501.663243	529776.492383	43.127297
3502.110576	529753.962901	43.132301
3502.000565	529744.009013	43.137306
3502.104281	529712.367688	43.142311
3502.130165	529703.752303	43.147316
3501.706192	529682.969760	43.152321
3502.004557	529655.578497	43.157325
3501.933130	529638.266138	43.162330
3502.139929	529622.975176	43.167335
3501.823489	529598.298128	43.172340
3501.745107	529575.699071	43.177345
3502.314019	529555.215052	43.182349
3501.912708	529547.572506	43.187354
3501.915964	529518.766463	43.192359
3502.083645	529492.704538	43.197364
3502.156881	529481.009714	43.202369
3501.959620	529467.544029	43.207373
3501.818606	529444.551616	43.212378
3501.844199	529416.446906	43.217383
3501.653718	529406.001686	43.222388
3501.737200	529386.902297	43.227393
3501.787244	529368.362043	43.232397
3501.711806	529355.582325	43.237402
3501.606680	529338.476254	43.242407
3501.491000	529315.429312	43.247412
3501.628125	529306.846716	43.252417
3501.874455	529291.901739	43.257421
3501.655477	529280.856531	43.262426
3501.285988	529267.165640	43.267431
3501.599588	529254.677806	43.272436
3501.364082	529230.440713	43.277441
3501.833028	529218.784799	43.282445
3501.276273	529210.511558	43.287450
3501.613841	529181.501670	43.292455
3501.223054	529176.375299	43.297460
3501.134702	529163.244879	43.302465
3501.150142	529138.867845	43.307469
3501.459023	529142.798243	43.312474
3501.533434	529133.117356	43.317479
3501.677825	529132.691964	43.322484
3501.783243	529104.624526	43.327489
3501.639838	529086.416142	43.332493
3501.613413	529072.470218	43.337498
3501.709664	529067.973071	43.342503
3501.819058	529055.516825	43.347508
3501.707238	529030.857228	43.352513
3501.943263	529014.704871	43.357517
3501.608415	528989.324482	43.362522
3501.601766	528982.073443	43.367527
3501.532557	528955.090449	43.372532
3501.704589	528949.120985	43.377537
3501.912169	528929.649090	43.382541
3502.030484	528908.075868	43.387546
3501.957641	528884.870419	43.392551
3502.119639	528871.046046	43.397556
3501.881095	528851.139839	43.402561
3501.973222	528823.476765	43.407565
3501.968210	528815.570673	43.412570
3501.536510	528797.154940	43.417575
3501.835140	528789.302307	43.422580
3501.634926	528773.016089	43.427585
3501.899844	528747.944800	43.432589
3501.532504	528733.447220	43.437594
3501.599650	528707.751920	43.442599
3501.589796	528703.422246	43.447604
3501.791971	528687.778380	43.452609
3501.605595	528666.503988	43.457613
3501.759536	528663.558965	43.462618
3501.794586	528641.847176	43.467623
3501.913748	528622.942576	43.472628
3501.743592	528604.133334	43.477633
3501.676538	528585.056206	43.482637
3501.661237	528585.511816	43.487642
3501.685238	528551.865585	43.492647
3501.884692	528549.517811	43.497652
3501.548939	528523.330853	43.502657
3501.635586	528499.646638	43.507661
3501.705599	528494.397929	43.512666
3501.721299	528472.991052	43.517671
3502.096063	528457.722963	43.522676
3501.896589	528435.594057	43.527681
3501.833562	528421.552412	43.532685
3501.396812	528401.021640	43.537690
3501.872514	528381.960486	43.542695
3502.157795	528368.519311	43.547700
3501.802826	528340.622613	43.552705
3501.855153	528319.260149	43.557709
3501.999194	528309.064183	43.562714
3501.675857	528292.947621	43.567719
3502.417847	528262.261128	43.572724
3502.050674	528246.554244	43.577729
3502.180740	528213.696471	43.582733
3501.742528	528201.324632	43.587738
3502.161994	528176.933309	43.592743
3501.938904	528170.622064	43.597748
3501.705404	528149.354168	43.602753
3501.940148	528125.293682	43.607757
3501.818156	528113.124376	43.612762
3501.913008	528099.208912	43.617767
3501.620300	528081.173464	43.622772
3501.685220	528072.148017	43.627777
3502.234820	528031.820871	43.632781
3502.215417	528024.772749	43.637786
3502.271143	528004.466913	43.642791
3502.281179	527983.916329	43.647796
3502.082462	527955.037560	43.652801
3502.322166	527926.291965	43.657805
3502.121744	527906.932416	43.662810
3502.033605	527878.539926	43.667815
3501.996912	527856.334351	43.672820
3501.764286	527832.446791	43.677825
3501.983301	527819.770856	43.682829
3501.471108	527795.674905	43.687834
3501.966714	527775.199533	43.692839
3502.032140	527757.309375	43.697844
3501.823659	527754.067985	43.702849
3501.839461	527727.220344	43.707853
3502.043124	527703.365390	43.712858
3501.947810	527684.089890	43.717863
3502.082569	527677.621990	43.722868
3501.651259	527646.210053	43.727873
3502.086322	527631.636758	43.732877
3501.627808	527603.150211	43.737882
3501.590990	527578.576954	43.742887
3501.636885	527579.677844	43.747892
3501.559964	527562.011039	43.752897
3501.733384	527540.175169	43.757901
3501.430067	527534.631605	43.762906
3501.500410	527518.251365	43.767911
3501.794274	527508.585504	43.772916
3501.764872	527489.249095	43.777921
3501.940593	527463.685577	43.782925
3501.738716	527458.579500	43.787930
3502.075227	527436.919550	43.792935
3502.271412	527417.547933	43.797940
3501.928569	527390.705049	43.802945
3502.131200	527368.914719	43.807949
3501.669276	527354.228864	43.812954
3501.799128	527341.868553	43.817959
3501.863928	527309.522363	43.822964
3501.759691	527304.602504	43.827969
3501.586266	527276.624933	43.832973
3501.591263	527274.004987	43.837978
3501.694436	527244.322165	43.842983
3501.717514	527218.630822	43.847988
3501.692034	527217.627388	43.852993
3502.118457	527190.664390	43.857997
3502.137619	527187.639277	43.863002
3501.961889	527152.056196	43.868007
3502.044768	527134.162478	43.873012
3501.837641	527119.487080	43.878017
3501.784067	527092.648945	43.883021
3501.813271	527063.430545	43.888026
3501.735843	527062.485551	43.893031
3502.019415	527036.753319	43.898036
3501.817400	527017.090499	43.903041
3501.977419	526997.623157	43.908045
3502.030802	526987.238803	43.913050
3501.887618	526962.479477	43.918055
3501.811095	526932.672812	43.923060
3501.948691	526922.275303	43.928065
3501.939311	526903.035659	43.933069
3501.911677	526896.743756	43.938074
3501.718828	526866.602458	43.943079
3501.870547	526851.518335	43.948084
3501.773076	526834.810777	43.953089
3501.644702	526815.337675	43.958093
3501.728151	526800.667075	43.963098
3501.381893	526784.149276	43.968103
3501.482458	526777.132189	43.973108
3501.392692	526752.867856	43.978113
3501.669471	526744.211495	43.983117
3501.424290	526735.837831	43.988122
3501.587406	526715.412564	43.993127
3501.760253	526703.447926	43.998132
3501.664176	526687.445146	44.003137
3501.773447	526664.761523	44.008141
3501.293893	526658.287979	44.013146
3501.977108	526633.449810	44.018151
3501.766430	526625.876632	44.023156
3501.342840	526606.952867	44.028161
3501.705204	526580.703784	44.033165
3501.555671	526579.115159	44.038170
3501.822264	526568.143223	44.043175
3501.843195	526540.637557	44.048180
3501.757310	526533.044907	44.053185
3502.193076	526492.630047	44.058189
3501.642682	526494.327525	44.063194
3501.928806	526466.981923	44.068199
3502.031731	526451.753826	44.073204
3501.611969	526425.172805	44.078209
3501.945390	526410.563617	44.083213
3501.639621	526387.238908	44.088218
3501.638153	526368.752827	44.093223
3501.562200	526371.837261	44.098228
3501.668046	526356.004143	44.103233
3501.918399	526326.900820	44.108237
3501.908967	526312.999706	44.113242
3501.732219	526291.669614	44.118247
3501.974977	526268.158595	44.123252
3501.980020	526251.484719	44.128257
3501.673158	526234.708243	44.133261
3501.451363	526226.683220	44.138266
3501.683838	526215.011096	44.143271
3501.725966	526184.378332	44.148276
3501.427333	526177.322305	44.153281
3501.589291	526159.213477	44.158285
3501.526349	526148.493963	44.163290
3501.948522	526133.518055	44.168295
3501.712958	526121.616448	44.173300
3501.581322	526093.831363	44.178305
3501.896340	526084.614526	44.183309
3501.644240	526061.280892	44.188314
3501.631932	526041.788591	44.193319
3501.979522	526038.107638	44.198324
3501.641624	526015.341372	44.203329
3501.766485	525996.381760	44.208333
3501.593895	525988.550426	44.213338
3501.599626	525973.991752	44.218343
3501.378945	525948.033641	44.223348
3501.545137	525940.653290	44.228353
3501.928443	525922.257830	44.233357
3501.951644	525912.028451	44.238362
3501.437835	525887.677400	44.243367
3501.363120	525877.815844	44.248372
3501.676101	525859.582361	44.253377
3502.142867	525834.826758	44.258381
3501.728524	525819.225069	44.263386
3501.765019	525798.112866	44.268391
3501.950142	525789.520521	44.273396
3501.732118	525770.462823	44.278401
3501.871547	525750.291626	44.283405
3501.884462	525732.709148	44.288410
3501.762078	525716.961158	44.293415
3501.907860	525695.428796	44.298420
3501.524999	525684.053455	44.303425
3501.621474	525662.528712	44.308429
3501.593793	525645.859168	44.313434
3501.713986	525635.362613	44.318439
3501.719463	525602.114754	44.323444
3501.438013	525604.324607	44.328449
3501.628618	525586.512788	44.333453
3501.867522	525570.708404	44.338458
3501.493914	525566.132061	44.343463
3501.938622	525534.881035	44.348468
3501.643842	525527.975185	44.353473
3501.826634	525511.826841	44.358477
3501.873264	525498.369523	44.363482
3501.879347	525485.724496	44.368487
3501.414143	525454.917124	44.373492
3501.787207	525452.642541	44.378497
3501.977355	525421.783487	44.383501
3501.904292	525412.979202	44.388506
3501.642435	525389.091778	44.393511
3501.712873	525366.411982	44.398516
3501.522285	525357.928199	44.403521
3501.432868	525324.241037	44.408525
3501.757273	525319.807866	44.413530
3501.699097	525310.900446	44.418535
3501.774445	525283.635585	44.423540
3501.197463	525282.667449	44.428545
3501.813419	525267.559664	44.433549
3501.942342	525246.583330	44.438554
3501.720391	525230.144998	44.443559
3502.172164	525202.216888	44.448564
3501.896072	525190.219999	44.453569
3502.132454	525162.879457	44.458573
3501.949947	525151.321353	44.463578
3501.920230	525125.634174	44.468583
3501.704075	525116.801584	44.473588
3501.689715	525089.197653	44.478593
3501.467593	525081.826877	44.483597
3501.554561	525059.244737	44.488602
3501.471465	525045.202632	44.493607
3501.851455	525034.312541	44.498612
3501.609373	525019.741009	44.503617
3501.974336	525004.873491	44.508621
3501.649360	524985.932064	44.513626
3502.027172	524961.944333	44.518631
3502.245667	524951.180058	44.523636
3501.809652	524931.802442	44.528641
3501.663230	524914.394807	44.533645
3502.146222	524898.199006	44.538650
3501.778983	524869.541240	44.543655
3501.674715	524858.575231	44.548660
3501.591803	524847.656267	44.553665
3501.705690	524824.465016	44.558669
3501.635551	524807.196502	44.563674
3501.697636	524796.859461	44.568679
3501.511124	524771.498261	44.573684
3500.894951	524762.526173	44.578689
3501.694124	524750.966093	44.583693
3501.545157	524741.266380	44.588698
3501.172547	524719.863487	44.593703
3501.557386	524708.871622	44.598708
3501.214113	524703.836859	44.603713
3501.787788	524685.158184	44.608717
3501.627854	524674.704463	44.613722
3501.339631	524658.174982	44.618727
3501.286996	524640.802773	44.623732
3501.401607	524634.487663	44.628737
3501.552948	524625.396047	44.633741
3501.614204	524608.862499	44.638746
3501.539247	524597.740581	44.643751
3501.882292	524580.457855	44.648756
3501.571538	524567.105588	44.653761
3501.781333	524551.052636	44.658765
3501.787714	524529.086679	44.663770
3501.696271	524509.050286	44.668775
3501.309895	524500.344531	44.673780
3501.542280	524481.869816	44.678785
3501.925050	524463.673946	44.683789
3501.578384	524444.483229	44.688794
3501.613293	524426.542954	44.693799
3501.764829	524410.952308	44.698804
3501.427474	524399.316889	44.703809
3501.730703	524386.624580	44.708813
3501.682505	524374.339597	44.713818
3502.027785	524351.716065	44.718823
3501.989031	524328.396568	44.723828
3501.572316	524311.433239	44.728833
3501.712697	524302.443868	44.733837
3501.530179	524281.312965	44.738842
3501.645258	524259.228890	44.743847
3502.040081	524253.575306	44.748852
3501.607616	524234.951812	44.753857
3501.362145	524220.178414	44.758861
3501.513739	524207.962947	44.763866
3501.389210	524187.780083	44.768871
3501.445842	524176.133540	44.773876
3501.435628	524169.031560	44.778881
3501.443270	524141.926042	44.783885
3501.687731	524143.802395	44.788890
3501.607809	524123.410973	44.793895
3501.504380	524114.257895	44.798900
3501.836539	524107.404885	44.803905
3501.813334	524083.528362	44.808909
3502.041065	524056.035761	44.813914
3501.771611	524045.598590	44.818919
3501.555276	524025.782428	44.823924
3501.528258	524011.277085	44.828929
3501.361651	523987.120424	44.833933
3501.603698	523978.115014	44.838938
3501.405057	523967.414860	44.843943
3501.501678	523939.488999	44.848948
3501.673509	523931.300573	44.853953
3501.768654	523923.779023	44.858957
3501.686041	523898.299235	44.863962
3501.539207	523886.079533	44.868967
3501.918289	523877.002350	44.873972
3501.374607	523866.154284	44.878977
3501.930818	523851.860297	44.883981
3501.607581	523832.060482	44.888986
3501.509243	523810.109639	44.893991
3501.825075	523794.895757	44.898996
3501.243560	523781.181787	44.904001
3501.743583	523769.314749	44.909005
3501.697150	523750.882413	44.914010
3501.344588	523726.905362	44.919015
3501.609528	523714.873333	44.924020
3501.506829	523706.878634	44.929025
3501.571730	523684.801420	44.934029
3501.691631	523670.524754	44.939034
3501.767162	523651.619868	44.944039
3501.815955	523644.306901	44.949044
3501.542666	523635.431836	44.954049
3501.702955	523617.168674	44.959053
3501.730368	523607.239162	44.964058
3501.569502	523579.453381	44.969063
3501.788618	523566.571858	44.974068
3501.433587	523550.152163	44.979073
3501.813594	523535.734113	44.984077
3501.651970	523536.514958	44.989082
3501.727406	523502.092194	44.994087
3501.770975	523485.156952	44.999092
3501.532677	523476.981688	45.004097
3501.483453	523451.042412	45.009101
3501.844677	523445.393719	45.014106
3501.490084	523426.353918	45.019111
3501.653075	523406.175515	45.024116
3501.448030	523399.556887	45.029121
3501.707091	523379.212346	45.034125
3501.574642	523360.037117	45.039130
3501.520123	523355.158439	45.044135
3501.754836	523327.663258	45.049140
3501.669748	523325.459617	45.054145
3502.181727	523296.661655	45.059149
3501.941825	523289.947631	45.064154
3501.640409	523262.283830	45.069159
3501.491629	523228.651001	45.074164
3501.413959	523223.826260	45.079169
3501.370202	523208.768438	45.084173
3501.733107	523196.267251	45.089178
3501.567333	523187.022473	45.094183
3501.608745	523150.840684	45.099188
3501.649833	523148.466228	45.104193
3501.572297	523144.246041	45.109197
3501.705041	523119.990847	45.114202
3501.712668	523112.986298	45.119207
3501.616338	523083.526785	45.124212
3501.895382	523072.953116	45.129217
3501.701919	523061.495673	45.134221
3501.816859	523032.708546	45.139226
3501.489383	523020.516163	45.144231
3501.510623	523003.734940	45.149236
3501.355161	522999.174145	45.154241
3501.303962	522981.547637	45.159245
3501.232567	522980.752564	45.164250
3501.585781	522966.690763	45.169255
3501.679088	522941.030626	45.174260
3501.831108	522930.577380	45.179265
3501.586195	522909.454018	45.184269
3501.439938	522903.934454	45.189274
3501.040687	522887.823132	45.194279
3501.487630	522870.421269	45.199284
3501.362475	522868.072633	45.204289
3501.616253	522859.165418	45.209293
3501.209620	522838.621341	45.214298
3501.252250	522820.073096	45.219303
3501.260600	522808.130569	45.224308
3501.033779	522805.797742	45.229313
3501.419207	522789.261888	45.234317
3501.260992	522784.096829	45.239322
3501.209159	522778.209825	45.244327
3501.196512	522774.231348	45.249332
3501.124517	522764.165527	45.254337
3501.017528	522742.063124	45.259341
3501.384472	522741.552521	45.264346
3501.333101	522735.615041	45.269351
3501.421338	522733.182790	45.274356
3501.313343	522707.855843	45.279361
3501.141877	522688.181873	45.284365
3501.220618	522680.309483	45.289370
3501.433024	522679.974081	45.294375
3501.266790	522670.779404	45.299380
3501.250500	522647.906953	45.304385
3501.564901	522644.280627	45.309389
3501.715269	522632.769314	45.314394
3501.232800	522626.898870	45.319399
3501.638022	522610.913957	45.324404
3501.289908	522612.076572	45.329409
3501.394417	522584.952832	45.334413
3501.195562	522567.701457	45.339418
3501.586817	522562.198880	45.344423
3501.456654	522534.960399	45.349428
3501.220082	522535.551419	45.354433
3501.180306	522512.531235	45.359437
3501.222106	522512.222377	45.364442
3501.262460	522499.972281	45.369447
3501.473603	522471.622455	45.374452
3501.157066	522487.291343	45.379457
3501.387554	522469.116468	45.384461
3501.398841	522458.281667	45.389466
3501.537798	522445.159613	45.394471
3501.467318	522443.407028	45.399476
3501.312236	522432.850026	45.404481
3501.444268	522406.527822	45.409485
3501.172467	522394.678908	45.414490
3501.300369	522390.577674	45.419495
3501.776661	522379.922381	45.424500
3501.285589	522359.844186	45.429505
3501.236643	522352.545725	45.434509
3501.358336	522348.646990	45.439514
3501.058990	522330.806310	45.444519
3501.325872	522309.652749	45.449524
3501.180343	522307.911825	45.454529
3501.236588	522317.980365	45.459533
3501.300608	522297.664539	45.464538
3501.253586	522284.772816	45.469543
3501.169297	522280.099926	45.474548
3501.379732	522277.598191	45.479553
3501.573708	522266.130165	45.484557
3501.446084	522249.522325	45.489562
3501.543834	522232.425912	45.494567
3501.567343	522211.108520	45.499572
3501.387146	522201.915694	45.504577
3501.587698	522196.493032	45.509581
3501.794365	522177.968763	45.514586
3501.219542	522160.473047	45.519591
3501.384552	522150.218723	45.524596
3501.384198	522143.466846	45.529601
3501.431319	522122.044865	45.534605
3501.512760	522117.497291	45.539610
3501.230018	522104.843626	45.544615
3501.557433	522082.168665	45.549620
3501.637767	522077.218150	45.554625
3501.619735	522068.302323	45.559629
3501.350794	522041.134825	45.564634
3501.291496	522030.109112	45.569639
3501.568313	522025.732655	45.574644
3501.708191	522017.749588	45.579649
3501.709649	521996.032186	45.584653
3501.498554	521990.169619	45.589658
3501.471598	521971.177542	45.594663
3501.469230	521949.259107	45.599668
3501.484748	521951.776055	45.604673
3501.040278	521919.647212	45.609677
3501.514444	521914.988070	45.614682
3501.630026	521897.132634	45.619687
3501.773751	521880.582891	45.624692
3501.499781	521878.307626	45.629697
3501.484127	521860.271010	45.634701
3501.578748	521843.325755	45.639706
3501.471110	521831.249245	45.644711
3501.507989	521820.712279	45.649716
3501.364264	521800.528808	45.654721
3501.364212	521795.792253	45.659725
3501.476467	521787.208685	45.664730
3501.881654	521775.656987	45.669735
3501.374900	521738.952036	45.674740
3501.470429	521734.150197	45.679745
3501.673879	521722.932179	45.684749
3501.632708	521707.066050	45.689754
3501.442104	521702.107170	45.694759
3501.613317	521668.974920	45.699764
3501.582197	521674.018630	45.704769
3501.314329	521651.687525	45.709773
3501.618515	521634.457451	45.714778
3501.730558	521630.660789	45.719783
3501.644894	521605.177123	45.724788
3501.596271	521607.704117	45.729793
3501.381524	521589.950067	45.734797
3501.319084	521586.079766	45.739802
3501.330698	521558.011015	45.744807
3501.195117	521546.845608	45.749812
3501.166612	521540.551316	45.754817
3501.041665	521508.119821	45.759821
3501.354965	521452.591903	45.764826
3501.100578	521348.324027	45.769831
3501.219085	521198.091363	45.774836
3500.598782	521001.057544	45.779841
3500.585249	520752.778162	45.784845
3500.639497	520448.345311	45.789850
3499.900977	520101.193382	45.794855
3499.363673	519702.395450	45.799860
3498.871629	519275.910302	45.804865
3498.074047	518794.725303	45.809869
3497.776460	518261.179011	45.814874
3496.735650	517694.057805	45.819879
3496.085662	517080.881993	45.824884
3495.681822	516422.172053	45.829889
3494.843633	515726.446050	45.834893
3494.021848	514983.091833	45.839898
3492.858432	514185.704191	45.844903
3492.225187	513348.003670	45.849908
3490.949611	512473.947308	45.854913
3489.722951	511557.924392	45.859917
3488.620022	510599.511790	45.864922
3487.652837	509599.102632	45.869927
3486.156745	508547.561689	45.874932
3484.827101	507473.773108	45.879937
3483.774715	506350.676540	45.884941
3482.682236	505184.767538	45.889946
3480.888229	503970.992744	45.894951
3479.684081	502729.221611	45.899956
3478.168540	501452.422082	45.904961
3476.542626	500136.415898	45.909965
3474.979121	498776.775140	45.914970
3473.112959	497385.608889	45.919975
3471.552614	495952.566594	45.924980
3469.589809	494500.920097	45.929985
3467.810841	492989.625423	45.934989
3465.982105	491467.127534	45.939994
3463.905879	489890.932696	45.944999
3462.050516	488310.145716	45.950004
3460.226073	486685.901670	45.955009
3458.227743	485018.674395	45.960013
3456.249594	483330.347897	45.965018
3454.061812	481605.995917	45.970023
3451.929139	479846.526823	45.975028
3449.629336	478073.343173	45.980033
3447.361059	476252.899296	45.985037
3445.198363	474426.368379	45.990042
3442.778498	472562.107186	45.995047
3440.499898	470679.711341	46.000052
3438.164955	468744.365240	46.005057
3435.821703	466794.329736	46.010061
3433.523698	464830.655451	46.015066
3430.951536	462832.749948	46.020071
3428.474621	460801.456334	46.025076
3425.515877	458754.462998	46.030081
3423.228195	456698.165739	46.035085
3420.816775	454615.580831	46.040090
3417.941368	452499.971548	46.045095
3415.550176	450361.457337	46.050100
3412.886312	448209.364753	46.055105
3410.042629	446032.436113	46.060109
3407.600893	443822.674655	46.065114
3404.617981	441609.644021	46.070119
3401.944569	439363.784059	46.075124
3399.432447	437106.791068	46.080129
3396.303071	434816.492586	46.085133
3393.447820	432509.158474	46.090138
3390.566522	430190.407016	46.095143
3387.498809	427849.618888	46.100148
3384.625848	425507.512729	46.105153
3381.475391	423127.613921	46.110157
3378.377924	420736.073499	46.115162
3375.558712	418335.746123	46.120167
3372.257958	415905.552780	46.125172
3369.129290	413485.350980	46.130177
3365.871562	411032.231555	46.135181
3363.056039	408558.882037	46.140186
3359.632479	406086.416522	46.145191
3356.476563	403589.738410	46.150196
3353.237018	401093.104281	46.155201
3350.093584	398583.142414	46.160205
3347.025664	396054.830752	46.165210
3343.397869	393515.779221	46.170215
3340.647342	390956.271291	46.175220
3336.747193	388388.729588	46.180225
3333.456308	385820.651194	46.185229
3330.266658	383237.696804	46.190234
3326.469373	380645.512502	46.195239
3323.471692	378035.499966	46.200244
3319.514138	375440.036813	46.205249
3316.300541	372810.730408	46.210253
3312.932320	370179.699110	46.215258
3309.288269	367551.437368	46.220263
3305.976732	364901.565104	46.225268
3302.324031	362255.291938	46.230273
3298.865683	359598.766156	46.235277
3294.942819	356935.497924	46.240282
3291.453319	354271.984444	46.245287
3287.599605	351597.246083	46.250292
3283.945782	348928.178747	46.255297
3280.980123	346246.763368	46.260301
3277.265763	343559.759822	46.265306
3273.349288	340874.638575	46.270311
3269.593149	338173.191664	46.275316
3265.802588	335474.600563	46.280321
3262.381741	332780.918853	46.285325
3258.696800	330064.094353	46.290330
3254.910796	327363.172857	46.295335
3251.731482	324652.308503	46.300340
3248.000929	321945.473051	46.305345
3244.214061	319217.331394	46.310349
3240.419948	316491.717348	46.315354
3236.810499	313766.392801	46.320359
3232.747457	311032.886685	46.325364
3228.980554	308299.738197	46.330369
3224.754827	305580.252617	46.335373
3221.200770	302847.868963	46.340378
3217.255967	300123.676985	46.345383
3213.654510	297397.692860	46.350388
3209.705771	294682.730471	46.355393
3205.882140	291954.718307	46.360397
3201.989453	289230.923874	46.365402
3197.876775	286505.775503	46.370407
3194.147797	283794.739242	46.375412
3190.416977	281079.779923	46.380417
3186.430033	278367.815904	46.385421
3182.622396	275654.558059	46.390426
3178.313761	272949.869017	46.395431
3174.603764	270242.125023	46.400436
3170.618051	267542.645267	46.405441
3166.522866	264844.661361	46.410445
3162.334098	262153.854441	46.415450
3158.023194	259461.168530	46.420455
3154.249254	256772.821294	46.425460
3150.278014	254096.190007	46.430465
3146.284129	251427.662015	46.435469
3142.280265	248773.250737	46.440474
3138.034761	246112.190292	46.445479
3134.042700	243459.943503	46.450484
3130.137066	240825.760799	46.455489
3125.944043	238182.428536	46.460493
3121.885688	235560.804397	46.465498
3117.347782	232953.118941	46.470503
3113.318960	230343.483040	46.475508
3109.527039	227746.919180	46.480513
3105.008416	225149.395403	46.485517
3100.933150	222570.752579	46.490522
3096.736649	220006.778435	46.495527
3092.550628	217449.968632	46.500532
3088.518997	214886.679009	46.505537
3084.203289	212356.509162	46.510541
3080.073125	209826.305930	46.515546
3075.839853	207318.937531	46.520551
3071.947764	204804.846357	46.525556
3067.604461	202314.415070	46.530561
3062.897657	199829.805956	46.535565
3058.780145	197353.089831	46.540570
3054.430357	194896.494268	46.545575
3050.018780	192444.537662	46.550580
3045.337247	190033.288860	46.555585
3040.958768	187628.842720	46.560589
3036.400319	185244.391308	46.565594
3031.797412	182872.582039	46.570599
3027.414637	180515.005703	46.575604
3022.998134	178197.318730	46.580609
3018.038905	175884.756396	46.585613
3013.551089	173591.090449	46.590618
3008.352634	171331.323799	46.595623
3003.793153	169080.678258	46.600628
2998.830792	166865.298075	46.605633
2994.067543	164685.254405	46.610637
2989.310191	162515.476233	46.615642
2984.288766	160387.012182	46.620647
2979.107290	158286.709558	46.625652
2973.826215	156217.205566	46.630657
2968.163627	154156.958813	46.635661
2962.660082	152099.981440	46.640666
2956.862520	150161.754428	46.645671
2951.143696	148259.546094	46.650676
2944.920744	146398.878442	46.655681
2937.925603	144618.510315	46.660685
2931.291420	142880.341294	46.665690
2923.888083	141221.772790	46.670695
2916.804838	139622.780460	46.675700
2909.331761	138114.461990	46.680705
2902.429160	136645.745912	46.685709
2895.550039	135263.632250	46.690714
2889.095414	133947.722537	46.695719
2883.281960	132679.303279	46.700724
2876.879296	131475.964250	46.705729
2871.185723	130325.019788	46.710733
2865.947009	129234.926274	46.715738
2860.544812	128187.828055	46.720743
2855.842392	127188.039656	46.725748
2850.598018	126214.472080	46.730753
2846.013278	125282.351905	46.735757
2841.411750	124385.778602	46.740762
2836.817334	123534.323110	46.745767
2832.463650	122680.571832	46.750772
2828.521008	121872.406195	46.755777
2823.899961	121091.374683	46.760781
2820.170544	120320.393869	46.765786
2816.169158	119584.188086	46.770791
2812.366113	118846.058061	46.775796
2808.061992	118142.914355	46.780801
2804.113034	117436.218763	46.785805
2800.221771	116754.221989	46.790810
2796.625665	116099.111074	46.795815
2793.066536	115431.888026	46.800820
2788.782156	114799.655383	46.805825
2784.620682	114170.338994	46.810829
2781.087186	113563.542864	46.815834
2777.179769	112952.186920	46.820839
2773.220349	112358.102999	46.825844
2769.235861	111776.085962	46.830849
2765.676990	111192.817058	46.835853
2761.825614	110634.242747	46.840858
2758.075630	110083.315125	46.845863
2754.141786	109532.717157	46.850868
2750.036518	108999.304753	46.855873
2746.571667	108478.081710	46.860877
2742.909112	107944.908997	46.865882
2739.437827	107443.763504	46.870887
2735.994263	106921.187679	46.875892
2732.225987	106402.649326	46.880897
2728.715251	105906.083508	46.885901
2725.412386	105404.827319	46.890906
2721.893983	104903.866345	46.895911
2718.243897	104405.780718	46.900916
2715.041792	103907.518380	46.905921
2711.969308	103417.683549	46.910925
2708.803462	102923.561432	46.915930
2705.270793	102413.526272	46.920935
2702.136763	101904.644478	46.925940
2698.838048	101409.917488	46.930945
2695.018934	100897.243146	46.935949
2692.166467	100406.681723	46.940954
2688.421363	99894.786995	46.945959
2685.491753	99383.256442	46.950964
2681.925269	98872.239836	46.955969
2678.317386	98359.903356	46.960973
2675.297947	97841.611962	46.965978
2671.435740	97330.958377	46.970983
2668.646057	96805.874355	46.975988
2665.213032	96290.862583	46.980993
2661.656453	95774.696627	46.985997
2658.583905	95245.921093	46.991002
2654.905027	94725.356450	46.996007
2651.699255	94192.298938	47.001012
2648.237493	93666.775081	47.006017
2644.650470	93132.244941	47.011021
2641.444108	92597.245563	47.016026
2638.031447	92065.947190	47.021031
2634.657633	91528.286134	47.026036
2631.118623	90997.242158	47.031041
2627.301428	90453.938725	47.036045
2624.290276	89905.971029	47.041050
2620.542344	89368.559268	47.046055
2617.316894	88816.998432	47.051060
2614.081043	88281.140218	47.056065
2610.660867	87731.141820	47.061069
2607.313378	87180.024388	47.066074
2603.598219	86639.392105	47.071079
2600.486622	86082.109746	47.076084
2596.666820	85523.563560	47.081089
2593.277073	84971.516293	47.086093
2589.822402	84415.742200	47.091098
2586.452720	83868.959453	47.096103
2583.095998	83292.904985	47.101108
2579.647983	82745.901876	47.106113
2576.214930	82177.782913	47.111117
2572.698538	81603.718337	47.116122
2568.524844	81043.130119	47.121127
2565.620134	80485.594539	47.126132
2562.212573	79918.228575	47.131137
2558.668189	79348.596572	47.136141
2554.892429	78780.930108	47.141146
2551.443423	78225.671036	47.146151
2548.270498	77653.933291	47.151156
2544.715392	77084.578362	47.156161
2541.090597	76511.525118	47.161165
2538.120807	75939.207489	47.166170
2534.042459	75369.131749	47.171175
2530.956312	74793.249904	47.176180
2527.202706	74219.287487	47.181185
2523.869856	73643.214752	47.186189
2520.510628	73057.965099	47.191194
2516.863348	72487.870946	47.196199
2513.204692	71908.127967	47.201204
2509.956560	71328.448128	47.206209
2506.601685	70751.057769	47.211213
2503.026149	70172.533692	47.216218
2499.259311	69602.736625	47.221223
2496.126947	69005.486660	47.226228
2492.473924	68426.581875	47.231233
2489.212509	67847.305414	47.236237
2485.869265	67257.390673	47.241242
2482.216274	66677.960370	47.246247
2479.036562	66085.755796	47.251252
2475.234811	65499.996370	47.256257
2471.853905	64908.694794	47.261261
2468.761900	64307.594207	47.266266
2465.025241	63726.124678	47.271271
2461.736167	63114.649269	47.276276
2458.408806	62523.909708	47.281281
2454.492869	61931.390941	47.286285
2451.157341	61328.185250	47.291290
2447.911676	60734.937234	47.296295
2444.444283	60125.029407	47.301300
2440.400553	59525.830146	47.306305
2437.132830	58926.765986	47.311309
2434.100638	58318.701225	47.316314
2430.139734	57719.559035	47.321319
2426.455659	57112.996651	47.326324
2423.347255	56511.550135	47.331329
2420.077220	55911.653938	47.336333
2416.694886	55295.763873	47.341338
2412.919102	54698.381562	47.346343
2409.336753	54071.648348	47.351348
2406.155196	53460.970725	47.356353
2402.399664	52849.973250	47.361357
2399.389420	52244.286966	47.366362
2395.433502	51616.288204	47.371367
2392.410795	51013.211372	47.376372
2388.897440	50394.140080	47.381377
2385.224322	49776.004630	47.386381
2382.051115	49143.409571	47.391386
2378.220618	48528.097726	47.396391
2374.894280	47911.055908	47.401396
2371.587863	47298.955767	47.406401
2367.885318	46671.864658	47.411405
2364.409905	46046.804091	47.416410
2360.768918	45425.230283	47.421415
2357.536561	44797.338163	47.426420
2354.254319	44168.310940	47.431425
2350.470405	43549.449604	47.436429
2347.244638	42915.686673	47.441434
2343.684374	42287.269651	47.446439
2340.129592	41657.132310	47.451444
2336.604186	41021.276555	47.456449
2332.998087	40389.573110	47.461453
2329.922112	39757.285557	47.466458
2326.472796	39129.613980	47.471463
2322.798661	38501.304529	47.476468
2319.640527	37868.958070	47.481473
2315.924083	37224.107797	47.486477
2312.295276	36582.730887	47.491482
2308.543485	35949.924838	47.496487
2305.145135	35315.637313	47.501492
2301.713027	34673.139963	47.506497
2298.146897	34033.548016	47.511501
2294.668756	33394.963246	47.516506
2290.898987	32767.636490	47.521511
2287.579409	32131.207832	47.526516
2284.209488	31499.369628	47.531521
2280.744848	30856.861161	47.536525
2277.006821	30218.642203	47.541530
2273.411855	29587.429649	47.546535
2270.075869	28949.795765	47.551540
2266.292291	28306.909418	47.556545
2262.891030	27673.114840	47.561549
2259.631463	27030.814447	47.566554
2255.870057	26403.825710	47.571559
2252.229101	25762.302813	47.576564
2248.817699	25133.290492	47.581569
2245.445402	24497.265545	47.586573
2241.940398	23858.987998	47.591578
2238.184582	23230.659137	47.596583
2234.706638	22585.341674	47.601588
2231.201576	21967.966909	47.606593
2227.291083	21337.466817	47.611597
2223.592165	20703.837412	47.616602
2219.840239	20085.388091	47.621607
2216.292206	19462.245706	47.626612
2213.022434	18842.493797	47.631617
2209.054047	18222.420628	47.636621
2205.507694	17613.239360	47.641626
2201.708790	17001.548435	47.646631
2197.374483	16385.121789	47.651636
2193.755966	15780.797300	47.656641
2189.355856	15212.741034	47.661645
2185.188845	14646.115480	47.666650
2180.322419	14093.166606	47.671655
2176.198629	13550.961889	47.676660
2171.985759	13017.296581	47.681665
2167.551175	12496.686161	47.686669
2164.123759	11986.934407	47.691674
2159.825542	11502.359902	47.696679
2155.659051	11008.343880	47.701684
2151.882112	10531.928057	47.706689
2148.263259	10061.298863	47.711693
2144.733500	9592.364305	47.716698
2140.418344	9135.186730	47.721703
2136.765357	8683.896441	47.726708
2133.538325	8244.844238	47.731713
2129.759276	7804.720453	47.736717
2126.166684	7369.904817	47.741722
2122.235244	6947.305452	47.746727
2118.820237	6512.710299	47.751732
2115.244893	6093.183039	47.756737
2111.417351	5674.562271	47.761741
2108.118060	5263.119035	47.766746
2104.612738	4861.141188	47.771751
2101.082127	4443.619541	47.776756
2097.673573	4036.293718	47.781761
2093.958288	3649.339864	47.786765
2090.953128	3246.047860	47.791770
2086.732433	2852.225150	47.796775
2083.192639	2450.274493	47.801780
2079.524153	2064.676257	47.806785
2075.646110	1696.109596	47.811789
2071.978718	1320.734244	47.816794
2067.193981	966.112154	47.821799
2062.298483	644.484454	47.826804
2055.016387	386.550438	47.831809
2047.857978	173.975138	47.836813
2036.359259	106.482209	47.841818
2025.983142	117.755883	47.846823
2019.054042	127.271896	47.851828
2016.077330	120.430096	47.856833
2013.954108	132.830112	47.861837
2012.802019	123.473912	47.866842
2010.766526	126.255207	47.871847
2008.702367	123.646814	47.876852
2006.431963	119.795539	47.881857
2002.986973	124.517265	47.886861
2000.249890	115.391930	47.891866
1997.006957	125.194785	47.896871
1993.330092	130.022201	47.901876
1990.138526	117.803876	47.906881
1986.870126	127.784699	47.911885
1983.580168	117.799459	47.916890
1980.689391	114.930581	47.921895
1977.157546	118.938168	47.926900
1973.762956	118.590094	47.931905
1970.068331	123.398128	47.936909
1967.359689	124.025291	47.941914
1963.656570	122.681207	47.946919
1960.479078	126.054685	47.951924
1957.229721	125.699828	47.956929
1953.791581	128.284977	47.961933
1950.774945	124.821926	47.966938
1947.100316	124.631332	47.971943
1943.529918	117.739573	47.976948
1940.086108	124.324548	47.981953
1936.526890	122.568933	47.986957
1933.505455	117.518444	47.991962
1930.085574	127.196980	47.996967
1926.410236	124.386936	48.001972
1923.015356	121.068177	48.006977
1919.178174	119.447573	48.011981
1916.435242	118.583636	48.016986
1913.101724	126.113218	48.021991
1909.394910	117.202095	48.026996
1905.897813	115.541219	48.032001
1902.116268	125.266550	48.037005
1899.107086	116.170923	48.042010
1895.397465	119.858173	48.047015
1892.227311	117.978736	48.052020
1888.745323	116.521151	48.057025
1885.285700	122.789053	48.062029
1881.875298	121.136832	48.067034
1878.289118	124.241729	48.072039
1874.474544	120.137255	48.077044
1871.385581	119.577109	48.082049
1867.940482	124.621556	48.087053
1864.560839	117.810850	48.092058
1861.239081	128.989536	48.097063
1857.345974	128.165408	48.102068
1854.066993	118.893480	48.107073
1850.376283	126.576731	48.112077
1847.074515	118.118264	48.117082
1843.430026	129.185829	48.122087
1840.280638	128.866042	48.127092
1837.062401	119.733357	48.132097
1833.112028	119.740712	48.137101
1830.264662	122.423744	48.142106
1826.396523	119.090069	48.147111
1822.568667	123.985284	48.152116
1819.225667	119.304391	48.157121
1815.800364	127.987199	48.162125
1812.186326	116.862868	48.167130
1808.978997	120.076482	48.172135
1805.585955	116.463226	48.177140
1802.082312	109.317495	48.182145
1798.329537	127.086844	48.187149
1795.574323	111.583144	48.192154
1791.774510	109.947247	48.197159
1788.074520	120.232516	48.202164
1784.561234	117.827533	48.207169
1780.767642	121.015337	48.212173
1777.522621	112.380375	48.217178
1773.874258	119.788118	48.222183
1770.462601	119.528138	48.227188
1767.340311	110.883568	48.232193
1763.795646	119.626078	48.237197
1760.149390	114.220445	48.242202
1756.523440	119.773928	48.247207
1753.343290	115.301813	48.252212
1749.819463	116.565222	48.257217
1746.240412	112.974596	48.262221
1743.022760	102.987641	48.267226
1739.270376	117.343270	48.272231
1736.061231	114.764409	48.277236
1732.416045	108.191205	48.282241
1728.406616	120.489301	48.287245
1725.248764	113.776973	48.292250
1721.334475	114.148877	48.297255
1717.970288	109.278311	48.302260
1715.049971	110.599650	48.307265
1711.568113	116.959599	48.312269
1708.071069	115.343026	48.317274
1704.048091	114.618221	48.322279
1700.768923	115.305724	48.327284
1697.440417	104.136982	48.332289
1693.682857	111.039708	48.337293
1690.748259	105.735293	48.342298
1687.215942	108.382570	48.347303
1683.193112	112.925326	48.352308
1679.929638	107.517077	48.357313
1676.355545	114.138152	48.362317
1673.048990	114.298415	48.367322
1669.018067	112.242928	48.372327
1665.393654	110.987865	48.377332
1662.414583	112.033617	48.382337
1658.829050	115.350395	48.387341
1655.810525	107.778011	48.392346
1651.927079	106.120346	48.397351
1648.363589	107.624050	48.402356
1645.262451	100.532758	48.407361
1641.191238	110.144982	48.412365
1637.907424	98.782640	48.417370
1634.645075	102.488872	48.422375
1631.108493	103.912460	48.427380
1627.864514	105.657498	48.432385
1623.559438	117.523887	48.437389
1620.314430	103.415730	48.442394
1616.956288	110.908017	48.447399
1613.456902	102.480352	48.452404
1610.109901	93.959373	48.457409
1606.464951	100.420634	48.462413
1602.832638	96.854138	48.467418
1599.376069	104.785678	48.472423
1595.525432	102.695813	48.477428
1592.848611	100.382125	48.482433
1589.223472	101.522111	48.487437
1585.683355	103.363863	48.492442
1582.324252	106.126554	48.497447
1578.627410	109.799177	48.502452
1575.227352	103.997756	48.507457
1571.232395	105.087738	48.512461
1568.044097	105.327679	48.517466
1564.697889	112.242314	48.522471
1560.550535	105.845372	48.527476
1557.671963	106.287040	48.532481
1553.744639	105.809952	48.537485
1550.399289	104.995515	48.542490
1546.982961	117.119039	48.547495
1543.068132	114.947423	48.552500
1540.087103	110.048880	48.557505
1536.893685	111.558268	48.562509
1533.423721	107.893744	48.567514
1529.903063	106.847170	48.572519
1525.957562	101.896269	48.577524
1522.472441	99.983637	48.582529
1518.833211	111.917228	48.587533
1515.962804	102.376132	48.592538
1512.572917	104.640590	48.597543
1508.250062	108.942157	48.602548
1504.750356	110.461255	48.607553
1501.114919	108.094301	48.612557
1497.693167	105.494774	48.617562
1494.638659	111.573083	48.622567
1491.271690	106.696653	48.627572
1487.649768	101.954818	48.632577
1484.049443	113.290741	48.637581
1480.719321	109.326052	48.642586
1476.732229	106.988525	48.647591
1473.247047	106.002873	48.652596
1470.157969	96.900777	48.657601
1466.664961	108.770479	48.662605
1463.514440	99.719074	48.667610
1459.591651	101.538141	48.672615
1455.973128	103.202285	48.677620
1452.480412	101.154803	48.682625
1448.765951	106.310792	48.687629
1445.842171	97.132352	48.692634
1442.012271	112.404855	48.697639
1438.334372	100.496456	48.702644
1435.146161	109.427092	48.707649
1431.580776	110.560955	48.712653
1428.015058	92.630392	48.717658
1424.201152	107.656795	48.722663
1420.919294	104.057919	48.727668
1417.898900	108.065021	48.732673
1413.941122	111.259423	48.737677
1410.904665	97.103038	48.742682
1407.012372	102.951085	48.747687
1403.148393	106.263763	48.752692
1399.613076	101.888105	48.757697
1396.459758	105.675455	48.762701
1393.492302	99.034785	48.767706
1389.847469	103.436468	48.772711
1386.297730	99.021930	48.777716
1382.643501	105.209405	48.782721
1379.110895	109.498711	48.787725
1375.615677	108.172952	48.792730
1371.862444	104.337408	48.797735
1368.424516	104.318834	48.802740
1365.171415	100.228280	48.807745
1361.280726	108.059722	48.812749
1358.022287	98.474649	48.817754
1354.871086	92.837006	48.822759
1351.046891	105.273937	48.827764
1347.616184	98.847745	48.832769
1343.541289	98.684712	48.837773
1340.519876	99.680131	48.842778
1336.966327	106.323330	48.847783
1333.078584	104.590444	48.852788
1330.384381	99.017710	48.857793
1326.612191	100.250210	48.862797
1322.919034	95.835859	48.867802
1319.634257	96.584377	48.872807
1316.098023	98.659660	48.877812
1312.753142	96.462637	48.882817
1308.744191	99.095546	48.887821
1305.656289	100.809986	48.892826
1301.812644	89.284921	48.897831
1298.541823	104.641232	48.902836
1295.229674	96.219282	48.907841
1291.524977	103.945847	48.912845
1288.215846	92.736211	48.917850
1284.618897	95.270192	48.922855
1280.959493	104.233041	48.927860
1277.600260	100.842378	48.932865
1273.670869	97.549952	48.937869
1270.236567	89.276735	48.942874
1266.635189	98.284333	48.947879
1262.984206	105.714643	48.952884
1260.099023	101.861059	48.957889
1256.607931	104.125471	48.962893
1253.399830	98.559971	48.967898
1249.469745	101.471671	48.972903
1245.694300	110.053960	48.977908
1242.907311	100.904880	48.982913
1238.907286	102.663225	48.987917
1235.639351	106.072963	48.992922
1232.321001	96.579495	48.997927
1228.425389	108.976927	49.002932
1224.704156	91.409140	49.007937
1221.097966	91.818560	49.012941
1217.661445	90.192625	49.017946
1214.637069	100.417019	49.022951
1210.985419	94.664308	49.027956
1207.715183	94.088147	49.032961
1203.863134	95.320435	49.037965
1200.731893	99.376438	49.042970
1197.430040	97.694741	49.047975
1193.479394	99.059435	49.052980
1190.116244	90.876394	49.057985
1185.974222	103.236248	49.062989
1182.728189	91.273343	49.067994
1179.309694	101.884946	49.072999
1175.852070	102.065606	49.078004
1172.898557	90.784822	49.083009
1168.908144	104.532086	49.088013
1165.264041	96.971735	49.093018
1161.777092	98.520515	49.098023
1158.002902	98.801071	49.103028
1154.771537	89.433284	49.108033
1151.268616	99.153211	49.113037
1147.883035	86.373658	49.118042
1144.510339	92.764088	49.123047
1140.889633	91.442073	49.128052
1137.684026	92.307995	49.133057
1133.830984	93.448699	49.138061
1130.272078	93.891897	49.143066
1127.096344	90.083558	49.148071
1123.651179	87.816750	49.153076
1120.319617	82.994979	49.158081
1116.593659	90.924169	49.163085
1112.783673	90.789531	49.168090
1108.960615	82.899555	49.173095
1105.779881	96.226558	49.178100
1102.595460	87.291229	49.183105
1098.691497	86.899144	49.188109
1095.111981	82.400704	49.193114
1091.914892	96.122551	49.198119
1088.218154	84.147570	49.203124
1085.240483	91.001686	49.208129
1081.339382	99.774377	49.213133
1077.589007	91.619993	49.218138
1073.970707	90.038189	49.223143
1070.597338	97.225979	49.228148
1067.849969	95.954689	49.233153
1063.827165	94.609852	49.238157
1060.519048	103.467410	49.243162
1056.800263	97.532187	49.248167
1053.453598	94.535060	49.253172
1049.659990	82.986447	49.258177
1045.831931	87.062339	49.263181
1042.581271	94.031716	49.268186
1039.349841	95.819138	49.273191
1036.096647	89.972797	49.278196
1032.847481	87.808367	49.283201
1028.925627	94.451960	49.288205
1025.589064	98.024252	49.293210
1021.607119	95.907448	49.298215
1017.946384	82.566492	49.303220
1014.808931	85.851531	49.308225
1011.493914	85.997356	49.313229
1007.944889	83.487308	49.318234
1004.191089	92.243397	49.323239
1000.031016	97.497251	49.328244
997.398227	87.789552	49.333249
993.785463	90.939776	49.338253
990.690162	84.752497	49.343258
986.906930	91.428298	49.348263
983.147248	89.476215	49.353268
979.986166	91.148290	49.358273
976.541596	92.725291	49.363277
973.022170	85.651763	49.368282
969.363343	89.647537	49.373287
965.330055	81.774496	49.378292
962.103406	79.065580	49.383297
958.683877	83.277199	49.388301
955.461140	90.182122	49.393306
952.252444	82.025705	49.398311
948.330972	80.285471	49.403316
944.798393	80.702446	49.408321
941.078286	78.684101	49.413325
937.477769	82.617017	49.418330
934.033399	82.669094	49.423335
930.674940	82.378774	49.428340
927.377369	79.256969	49.433345
923.645218	89.056870	49.438349
920.099925	91.661936	49.443354
917.018474	82.868798	49.448359
913.086773	87.897287	49.453364
909.777064	78.203233	49.458369
906.463825	93.328849	49.463373
902.294109	89.634139	49.468378
899.188500	86.226196	49.473383
895.671639	84.492587	49.478388
892.115906	83.141509	49.483393
888.531281	86.322162	49.488397
885.331869	82.837077	49.493402
882.053074	88.425145	49.498407
877.990904	86.308198	49.503412
874.579059	77.591810	49.508417
870.880477	91.088000	49.513421
867.662161	83.366520	49.518426
864.489830	80.620689	49.523431
860.677773	89.022028	49.528436
857.593890	83.484713	49.533441
853.757599	79.500835	49.538445
849.973251	85.398550	49.543450
846.542227	78.558055	49.548455
843.042368	83.405433	49.553460
839.713596	81.882993	49.558465
836.353059	88.916938	49.563469
832.588135	78.575603	49.568474
829.169004	74.365446	49.573479
825.792739	82.227558	49.578484
822.122211	85.314025	49.583489
818.365327	90.413384	49.588493
814.837275	89.380702	49.593498
811.680681	92.985105	49.598503
807.939824	88.799720	49.603508
804.902699	84.318131	49.608513
801.162782	93.135344	49.613517
797.908274	93.357193	49.618522
794.301806	88.103710	49.623527
790.610947	89.124296	49.628532
787.068539	85.948875	49.633537
783.100045	96.108273	49.638541
779.834362	85.711376	49.643546
776.956142	88.237923	49.648551
773.298819	93.388226	49.653556
769.960695	85.365880	49.658561
765.904711	81.466835	49.663565
762.236596	88.817577	49.668570
758.991556	95.466561	49.673575
755.879901	92.483511	49.678580
752.313885	88.293064	49.683585
748.398182	85.878097	49.688589
745.279980	82.127294	49.693594
741.642780	90.779826	49.698599
737.885364	84.278052	49.703604
734.744596	79.103944	49.708609
731.031834	81.409238	49.713613
727.558937	83.920796	49.718618
724.039835	84.123732	49.723623
720.140234	91.478876	49.728628
716.910630	76.587116	49.733633
713.398896	86.732355	49.738637
710.176994	78.805825	49.743642
706.547982	74.087369	49.748647
702.908402	79.241240	49.753652
699.634003	79.886966	49.758657
696.197835	85.081938	49.763661
692.500056	73.486859	49.768666
689.266156	83.354734	49.773671
685.554718	86.004668	49.778676
682.478573	74.508969	49.783681
678.469823	92.811619	49.788685
674.636185	79.684322	49.793690
671.331053	86.399609	49.798695
667.977513	88.781865	49.803700
664.254368	81.458541	49.808705
660.984171	84.223283	49.813709
657.396945	78.998468	49.818714
654.081338	80.583899	49.823719
649.923523	85.590665	49.828724
647.463683	81.905064	49.833729
643.561637	75.881396	49.838733
640.144530	80.367903	49.843738
636.709092	70.044927	49.848743
632.693550	84.004899	49.853748
629.348796	77.432581	49.858753
625.809766	81.858978	49.863757
622.478383	85.961993	49.868762
619.076346	77.373840	49.873767
615.223080	82.380654	49.878772
612.087655	79.224161	49.883777
608.479011	86.587799	49.888781
604.841084	76.565261	49.893786
601.657703	81.534230	49.898791
598.009647	81.491508	49.903796
595.010476	82.110219	49.908801
590.404144	89.600700	49.913805
587.133390	89.904194	49.918810
584.090281	83.958787	49.923815
580.171029	87.776845	49.928820
576.979369	79.583045	49.933825
573.056455	81.335792	49.938829
569.922048	78.346821	49.943834
566.849277	78.749208	49.948839
562.906581	77.708345	49.953844
559.484235	77.845622	49.958849
555.943701	81.554105	49.963853
552.213220	72.289453	49.968858
548.964312	84.959522	49.973863
545.058328	76.528928	49.978868
542.137935	76.974033	49.983873
538.656240	77.930452	49.988877
534.797884	72.839616	49.993882
531.665087	72.574325	49.998887
527.645942	72.658983	50.003892
524.670702	69.667388	50.008897
520.692068	81.179259	50.013901
516.906973	78.288429	50.018906
513.904984	74.124111	50.023911
510.220452	72.302768	50.028916
506.641016	77.178380	50.033921
503.017518	81.159206	50.038925
499.809278	71.898684	50.043930
496.640469	70.879722	50.048935
493.101281	70.933958	50.053940
489.498381	68.587396	50.058945
485.558982	83.171415	50.063949
482.398074	73.036680	50.068954
478.572681	67.592721	50.073959
475.223914	76.646437	50.078964
472.230247	73.436260	50.083969
468.438108	71.897424	50.088973
465.077358	74.334604	50.093978
461.091544	70.187417	50.098983
457.417410	74.894283	50.103988
454.501223	69.748534	50.108993
450.763698	80.789450	50.113997
447.119339	72.935066	50.119002
443.724227	70.094267	50.124007
439.981992	69.705570	50.129012
437.006761	65.489646	50.134017
433.641304	67.250535	50.139021
429.997224	75.796585	50.144026
426.285633	70.689249	50.149031
422.651444	79.050268	50.154036
419.708770	73.804246	50.159041
415.719411	76.016598	50.164045
412.357540	70.908603	50.169050
408.844821	75.821293	50.174055
404.811218	70.346488	50.179060
401.623122	73.183891	50.184065
397.739457	78.799719	50.189069
394.553779	78.748316	50.194074
391.634200	69.594734	50.199079
387.406054	92.167691	50.204084
384.185950	76.075504	50.209089
380.498337	78.636344	50.214093
377.355750	70.463421	50.219098
373.882763	71.228684	50.224103
369.881171	80.887063	50.229108
366.371178	70.708627	50.234113
363.205547	73.874722	50.239117
360.135915	74.903050	50.244122
356.306789	72.474671	50.249127
352.471700	74.394103	50.254132
349.470328	69.100286	50.259137
345.897748	73.218728	50.264141
342.039713	82.161917	50.269146
338.644903	67.985660	50.274151
334.869486	85.185818	50.279156
331.717121	80.010418	50.284161
328.332333	79.202267	50.289165
324.532714	82.751798	50.294170
321.301836	72.688101	50.299175
317.591429	72.136284	50.304180
314.099170	67.004315	50.309185
310.611931	77.924016	50.314189
306.865675	78.443937	50.319194
303.886828	82.295949	50.324199
300.255628	81.288889	50.329204
296.635008	69.985607	50.334209
293.091911	76.728473	50.339213
289.994014	79.842903	50.344218
286.333772	73.066673	50.349223
282.265850	72.848924	50.354228
279.083135	77.080680	50.359233
275.538687	77.505914	50.364237
272.136087	77.156112	50.369242
268.386198	76.126408	50.374247
264.870554	81.555246	50.379252
261.755934	79.322520	50.384257
258.259860	78.462104	50.389261
254.545984	81.245342	50.394266
251.361417	78.716631	50.399271
247.917860	78.531393	50.404276
244.397364	66.943626	50.409281
240.429370	71.139458	50.414285
236.871204	75.527743	50.419290
233.390209	75.221789	50.424295
229.989143	74.352913	50.429300
226.555419	73.065191	50.434305
223.200735	72.983176	50.439309
219.498503	67.118308	50.444314
216.129552	71.360080	50.449319
212.239546	76.027815	50.454324
208.902069	66.692567	50.459329
205.325769	68.824822	50.464333
201.935935	65.350507	50.469338
199.025607	69.644261	50.474343
194.925959	68.548804	50.479348
191.567058	62.766528	50.484353
187.436590	76.228724	50.489357
184.232104	69.204396	50.494362
181.681021	64.546000	50.499367
177.275587	66.484651	50.504372
174.094926	66.188893	50.509377
171.006259	71.367768	50.514381
167.302658	71.093317	50.519386
163.636493	75.216858	50.524391
159.738046	77.215782	50.529396
156.528582	74.630853	50.534401
153.209934	69.873670	50.539405
149.240142	74.319723	50.544410
145.713999	61.106741	50.549415
142.233021	79.694191	50.554420
139.194246	69.942302	50.559425
135.505047	70.383766	50.564429
131.919458	64.431156	50.569434
128.964555	63.495996	50.574439
125.478384	69.704843	50.579444
121.591635	70.211865	50.584449
117.573016	72.204194	50.589453
113.826548	78.886993	50.594458
110.879969	68.934101	50.599463
107.116810	71.528882	50.604468
104.235446	65.333761	50.609473
100.475272	73.151284	50.614477
97.106798	71.363055	50.619482
93.678902	75.139469	50.624487
89.653198	80.030821	50.629492
86.463890	65.613835	50.634497
82.747122	70.694361	50.639501
79.713359	72.726345	50.644506
76.361164	78.117097	50.649511
72.413571	84.619250	50.654516
68.768115	69.786080	50.659521
65.569570	70.894622	50.664525
61.537871	68.159324	50.669530
58.609316	69.409324	50.674535
54.425748	78.371581	50.679540
51.339230	76.431895	50.684545
47.688363	72.577479	50.689549
44.324587	76.312279	50.694554
40.827477	75.094564	50.699559
36.887477	78.795697	50.704564
34.095464	71.941288	50.709569
30.516305	67.401852	50.714573
26.976625	74.039807	50.719578
23.478842	71.154951	50.724583
19.932409	76.129874	50.729588
16.168609	73.485747	50.734593
12.504764	76.568101	50.739597
9.361506	73.106045	50.744602
5.619918	69.733984	50.749607
2.129373	77.364009	50.754612