Tue Jun 08 15:49:29 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.007189	92.826773	0.000000
-0.163817	96.965046	0.005005
-1.042769	68.199337	0.010010
-2.110046	25.293358	0.015014
-6.130964	2.990776	0.020019
-11.298234	-3.364177	0.025024
-16.452348	-0.910190	0.030029
-21.104688	6.002496	0.035034
-24.858537	4.556212	0.040038
-28.853596	0.726962	0.045043
-32.335503	-4.175874	0.050048
-36.295749	-0.442457	0.055053
-39.929000	-4.457281	0.060058
-43.396483	-0.292068	0.065062
-47.317004	7.041044	0.070067
-50.921860	-7.622085	0.075072
-54.596143	-4.075444	0.080077
-58.608953	1.627151	0.085082
-62.176602	-7.893311	0.090086
-66.072969	3.835146	0.095091
-69.906384	5.963253	0.100096
-73.425579	4.548215	0.105101
-77.472651	1.035015	0.110106
-80.916571	2.821225	0.115110
-85.284966	6.197200	0.120115
-88.860808	5.450665	0.125120
-92.425992	5.153856	0.130125
-96.377176	8.616971	0.135130
-99.582006	9.023328	0.140134
-104.061661	-3.814576	0.145139
-107.544536	-1.577614	0.150144
-111.185752	2.998734	0.155149
-114.903122	6.560312	0.160154
-117.915762	-0.264266	0.165158
-122.343342	-1.491908	0.170163
-126.388020	-2.242481	0.175168
-130.329688	-1.930386	0.180173
-134.308682	4.343939	0.185178
-137.797137	-3.078720	0.190182
-142.251738	2.687868	0.195187
-145.429839	-0.580763	0.200192
-149.231622	8.311707	0.205197
-152.993285	4.547143	0.210202
-156.330617	4.424059	0.215206
-160.371609	6.825458	0.220211
-163.837818	4.104772	0.225216
-167.506126	5.459426	0.230221
-171.629014	7.068875	0.235226
-175.087664	2.039805	0.240230
-179.264658	11.028621	0.245235
-182.808579	-0.555025	0.250240
-186.456164	-3.104461	0.255245
-190.414192	9.053850	0.260250
-193.968333	0.667562	0.265254
-197.786537	9.836816	0.270259
-201.745054	2.334970	0.275264
-205.673385	2.985480	0.280269
-209.358259	8.568015	0.285274
-212.709879	3.447597	0.290278
-216.934078	3.614025	0.295283
-220.130512	-4.961474	0.300288
-224.110776	10.077341	0.305293
-228.304819	7.365889	0.310298
-231.766720	6.923984	0.315302
-235.434399	9.216028	0.320307
-238.885963	5.326119	0.325312
-242.869044	4.023936	0.330317
-246.975196	8.617767	0.335322
-250.336873	3.544102	0.340326
-254.272823	11.676555	0.345331
-258.177994	-2.222414	0.350336
-261.695911	1.093107	0.355341
-265.736380	1.359508	0.360346
-269.096840	-0.358899	0.365350
-273.150550	5.524563	0.370355
-277.006745	-3.412565	0.375360
-280.283417	0.167098	0.380365
-284.377682	6.343692	0.385370
-287.997740	0.234050	0.390374
-292.594489	10.505541	0.395379
-295.907936	-3.125829	0.400384
-299.057995	10.771620	0.405389
-303.407717	15.078092	0.410394
-306.758657	1.181201	0.415398
-311.063989	16.382416	0.420403
-314.114760	-2.233429	0.425408
-317.824366	5.204234	0.430413
-321.842242	7.627860	0.435418
-325.437924	-0.956436	0.440422
-329.658441	7.617233	0.445427
-333.476729	0.892331	0.450432
-337.032266	-0.690725	0.455437
-341.068377	-6.073727	0.460442
-344.342681	-10.925867	0.465446
-348.509428	0.001729	0.470451
-351.983092	-0.489771	0.475456
-355.998674	-0.317947	0.480461
-359.764547	-5.970301	0.485466
-363.448958	-5.791338	0.490470
-367.074411	3.622458	0.495475
-370.812197	-5.218452	0.500480
-374.717034	4.896525	0.505485
-378.305944	3.731701	0.510490
-382.189460	1.300266	0.515494
-386.041373	6.088615	0.520499
-389.856989	-1.800697	0.525504
-393.606683	-0.786351	0.530509
-397.130288	7.403757	0.535514
-400.678107	-2.893441	0.540518
-404.785369	4.680791	0.545523
-408.473605	-1.921490	0.550528
-412.299396	0.939757	0.555533
-416.588632	3.790520	0.560538
-419.806384	-3.374013	0.565542
-423.880080	2.611287	0.570547
-427.398237	-2.570773	0.575552
-431.168846	-6.628404	0.580557
-434.806360	4.082952	0.585562
-438.405337	7.002409	0.590566
-442.484600	6.127408	0.595571
-446.431705	-6.987771	0.600576
-450.183337	2.696004	0.605581
-453.464272	5.659586	0.610586
-456.998809	2.269587	0.615590
-461.059512	8.133490	0.620595
-465.124087	4.359595	0.625600
-468.678519	3.374445	0.630605
-472.836041	6.868147	0.635610
-476.051569	3.068981	0.640614
-479.787864	6.160441	0.645619
-483.698146	2.459560	0.650624
-487.472714	3.750603	0.655629
-491.649835	0.592060	0.660634
-494.815878	-9.930802	0.665638
-498.790235	2.217907	0.670643
-502.821804	1.871192	0.675648
-506.690832	7.370294	0.680653
-510.132756	7.460409	0.685658
-513.641711	3.515050	0.690662
-517.635497	17.032820	0.695667
-521.680986	7.164514	0.700672
-525.132384	0.040153	0.705677
-529.004416	7.355461	0.710682
-532.375717	-2.435886	0.715686
-536.525378	1.743321	0.720691
-540.232462	0.603250	0.725696
-543.934435	5.891756	0.730701
-548.018017	5.210214	0.735706
-551.038170	-4.768069	0.740710
-555.409574	0.850033	0.745715
-559.014355	6.881693	0.750720
-562.970859	-1.258788	0.755725
-566.818713	11.285088	0.760730
-569.865319	-0.879686	0.765734
-573.932683	1.636331	0.770739
-577.950364	0.529852	0.775744
-581.804743	-3.016723	0.780749
-585.378829	3.332168	0.785754
-588.670110	-7.880397	0.790758
-592.805963	9.401292	0.795763
-596.656617	5.195710	0.800768
-600.422670	-4.173387	0.805773
-604.015370	7.039973	0.810778
-607.920852	0.120700	0.815782
-611.898275	4.358440	0.820787
-615.189176	1.021103	0.825792
-619.246467	-0.170114	0.830797
-623.334827	5.332776	0.835802
-626.711738	-10.958408	0.840806
-630.895264	-0.446883	0.845811
-634.269171	-0.313873	0.850816
-637.851896	-5.991480	0.855821
-641.588680	2.326164	0.860826
-645.166689	-8.983188	0.865830
-649.141657	-3.616177	0.870835
-653.295004	-7.991190	0.875840
-657.112026	-2.975729	0.880845
-660.508929	-5.169913	0.885850
-664.034483	-3.770280	0.890854
-667.951640	-1.407448	0.895859
-671.784779	0.456265	0.900864
-675.838714	-1.188996	0.905869
-679.816265	0.898441	0.910874
-683.183893	1.305130	0.915878
-687.411892	3.810925	0.920883
-690.974486	-5.120927	0.925888
-693.957095	-0.447570	0.930893
-698.198871	2.291900	0.935898
-701.479198	-7.479778	0.940902
-705.522099	3.317920	0.945907
-709.926610	2.356105	0.950912
-713.427524	0.533473	0.955917
-717.445761	0.234403	0.960922
-720.607555	6.642892	0.965926
-724.291017	4.582801	0.970931
-728.294761	4.408349	0.975936
-732.135933	-2.424345	0.980941
-735.822997	4.547956	0.985946
-739.457594	0.397000	0.990950
-743.192786	3.677157	0.995955
-746.888269	3.046028	1.000960
-750.788539	5.405640	1.005965
-754.926885	12.425810	1.010970
-758.214417	0.596207	1.015974
-762.091704	8.394151	1.020979
-766.131946	4.308893	1.025984
-769.717555	3.141855	1.030989
-773.402433	4.871663	1.035994
-776.639142	-0.190653	1.040998
-780.940462	5.079340	1.046003
-784.881576	4.851957	1.051008
-788.508878	-10.643777	1.056013
-792.498842	-1.303288	1.061018
-795.981343	1.570408	1.066022
-799.724200	9.776727	1.071027
-803.440049	5.560041	1.076032
-806.844878	3.947558	1.081037
-811.094739	16.271300	1.086042
-814.788304	-4.427954	1.091046
-818.600420	10.855972	1.096051
-822.692435	3.460538	1.101056
-826.052124	3.221413	1.106061
-830.053073	9.849010	1.111066
-833.411329	3.838588	1.116070
-837.491369	7.219067	1.121075
-841.071734	0.437229	1.126080
-845.004425	-2.743185	1.131085
-848.756063	7.049439	1.136090
-852.402411	-2.967551	1.141094
-856.637496	2.115891	1.146099
-859.959707	7.001193	1.151104
-863.496864	6.872292	1.156109
-867.280123	-3.624831	1.161114
-871.057934	1.017391	1.166118
-875.094566	3.441570	1.171123
-878.703855	1.883584	1.176128
-882.393039	-0.543650	1.181133
-886.110699	-1.761338	1.186138
-889.932807	-5.504600	1.191142
-893.629884	-0.055223	1.196147
-897.645832	-4.559359	1.201152
-901.596217	-6.618074	1.206157
-905.498234	2.929635	1.211162
-908.697109	4.021953	1.216166
-912.635570	7.872373	1.221171
-916.442806	8.326290	1.226176
-920.211830	-1.834959	1.231181
-923.682366	0.665359	1.236186
-927.143171	-3.821953	1.241190
-931.334842	-0.145929	1.246195
-935.225270	-0.408715	1.251200
-939.293899	-2.560771	1.256205
-943.032390	7.105729	1.261210
-946.572957	-0.777770	1.266214
-950.297675	-4.405864	1.271219
-953.915204	0.405475	1.276224
-957.570402	-3.838452	1.281229
-961.585907	-1.565443	1.286234
-965.140362	-6.592394	1.291238
-968.958535	-3.658963	1.296243
-972.588690	-3.623002	1.301248
-976.544811	-6.060371	1.306253
-980.372967	-1.933589	1.311258
-983.773741	1.231331	1.316262
-987.456642	-1.432924	1.321267
-991.534975	-0.624129	1.326272
-995.310513	2.001238	1.331277
-999.155839	7.329718	1.336282
-1003.073405	1.569405	1.341286
-1007.282533	8.501693	1.346291
-1010.882787	8.450847	1.351296
-1014.343514	-1.027503	1.356301
-1018.059247	-3.216784	1.361306
-1021.164923	-3.768559	1.366310
-1025.348987	1.227338	1.371315
-1029.082959	10.494474	1.376320
-1032.877260	2.101235	1.381325
-1037.005358	1.700546	1.386330
-1040.480453	-9.050218	1.391334
-1044.044307	0.831090	1.396339
-1048.246534	-1.426597	1.401344
-1051.586361	2.553642	1.406349
-1055.436369	5.503272	1.411354
-1059.417905	0.023586	1.416358
-1063.250329	-1.747357	1.421363
-1067.147500	-1.085246	1.426368
-1070.420607	1.050917	1.431373
-1074.626841	-0.797137	1.436378
-1078.176420	7.987617	1.441382
-1081.740787	-0.488866	1.446387
-1085.448508	1.492214	1.451392
-1089.086760	-2.045607	1.456397
-1093.210560	6.861833	1.461402
-1096.607726	-1.778731	1.466406
-1100.799159	3.285209	1.471411
-1104.736953	7.656304	1.476416
-1108.064498	-4.598711	1.481421
-1112.046007	-0.231946	1.486426
-1115.713808	-6.152656	1.491430
-1119.470597	-4.392841	1.496435
-1123.372830	-0.087439	1.501440
-1126.909553	-2.824035	1.506445
-1130.625699	4.876281	1.511450
-1134.303595	-8.345577	1.516454
-1138.173270	-6.384006	1.521459
-1141.895445	-2.208185	1.526464
-1145.750322	-8.399087	1.531469
-1149.979128	-1.437243	1.536474
-1153.529075	2.098794	1.541478
-1157.440794	8.007584	1.546483
-1161.076919	-2.058229	1.551488
-1164.513985	-4.732569	1.556493
-1168.599458	-2.042778	1.561498
-1171.425080	-1.143038	1.566502
-1176.092100	3.456367	1.571507
-1179.857365	-0.838716	1.576512
-1183.343171	-9.218861	1.581517
-1187.488323	1.594030	1.586522
-1191.067034	6.051551	1.591526
-1194.591729	5.434109	1.596531
-1198.146462	7.508610	1.601536
-1202.178750	0.535522	1.606541
-1206.004996	4.953071	1.611546
-1209.662717	-3.509231	1.616550
-1213.678367	1.945383	1.621555
-1217.436763	4.455111	1.626560
-1220.675725	-2.441454	1.631565
-1224.881828	1.988061	1.636570
-1228.512002	-3.373389	1.641574
-1232.108649	-9.807094	1.646579
-1236.166485	0.625738	1.651584
-1239.816809	-4.666719	1.656589
-1243.819580	4.017186	1.661594
-1247.313802	-4.801952	1.666598
-1250.848679	-1.189089	1.671603
-1254.993361	3.235827	1.676608
-1258.619005	-6.066744	1.681613
-1262.304164	-4.866567	1.686618
-1266.307424	-7.641720	1.691622
-1270.464489	2.471105	1.696627
-1274.057305	-6.139640	1.701632
-1277.014527	-10.342903	1.706637
-1281.000095	0.040057	1.711642
-1284.847817	0.060763	1.716646
-1288.925949	-2.542441	1.721651
-1292.735905	-3.199613	1.726656
-1296.494469	-8.484872	1.731661
-1300.242477	3.740059	1.736666
-1303.787782	0.101210	1.741670
-1307.225629	-2.241716	1.746675
-1311.090779	-1.889595	1.751680
-1314.688096	0.222313	1.756685
-1319.010270	6.856564	1.761690
-1322.577858	-3.713852	1.766694
-1326.646715	3.306730	1.771699
-1330.530120	6.595078	1.776704
-1333.813505	-1.718656	1.781709
-1337.688353	1.889914	1.786714
-1341.019196	6.282876	1.791718
-1345.061205	5.096838	1.796723
-1348.940436	1.455391	1.801728
-1352.680522	0.644967	1.806733
-1356.618147	0.286869	1.811738
-1360.275376	-6.017109	1.816742
-1363.833607	-7.148870	1.821747
-1367.787718	1.042871	1.826752
-1371.271034	-8.826365	1.831757
-1375.046454	1.156656	1.836762
-1378.626082	-5.189055	1.841766
-1382.492512	-0.960622	1.846771
-1386.838694	1.260646	1.851776
-1390.293633	3.019369	1.856781
-1394.270326	11.460130	1.861786
-1397.787273	-4.718629	1.866790
-1401.255637	3.757566	1.871795
-1405.234159	5.212721	1.876800
-1408.858907	-4.810200	1.881805
-1413.011348	4.760814	1.886810
-1416.770429	0.032294	1.891814
-1420.588627	0.525254	1.896819
-1424.370574	3.395628	1.901824
-1427.795606	1.068365	1.906829
-1432.105457	-4.505320	1.911834
-1435.399337	-5.865971	1.916838
-1438.778084	-2.706062	1.921843
-1442.671828	-3.505400	1.926848
-1446.302781	-5.396643	1.931853
-1450.806168	-2.137458	1.936858
-1454.278484	-1.830983	1.941862
-1458.141398	-4.324949	1.946867
-1461.909905	5.864967	1.951872
-1465.358065	2.952016	1.956877
-1469.388350	11.879645	1.961882
-1472.951944	2.818045	1.966886
-1476.487956	2.565919	1.971891
-1480.538471	4.466902	1.976896
-1484.126699	1.990501	1.981901
-1488.272831	10.004960	1.986906
-1492.152424	4.173878	1.991910
-1495.667117	3.049750	1.996915
-1499.855767	6.199366	2.006912
-1500.367031	3.092023	2.016909
-1497.917946	3.624222	2.026906
-1494.925590	2.423349	2.036902
-1493.258483	-2.504727	2.046899
-1491.073809	4.020454	2.056896
-1489.453679	1.668540	2.066893
-1487.219663	3.763215	2.076890
-1485.630925	0.398233	2.086886
-1483.516984	-0.503117	2.096883
-1481.417495	2.413002	2.106880
-1479.735294	-1.968318	2.116877
-1477.946762	4.866405	2.126874
-1475.940394	-9.326818	2.136870
-1473.529594	-6.494216	2.146867
-1472.192374	-3.060616	2.156864
-1470.353860	-3.161367	2.166861
-1468.460206	6.054241	2.176858
-1466.447961	-1.606339	2.186854
-1464.526815	-3.454289	2.196851
-1462.710068	1.897498	2.206848
-1460.710315	-2.622945	2.216845
-1458.717413	1.046989	2.226842
-1457.124368	-3.333234	2.236838
-1454.984679	-4.847620	2.246835
-1453.294193	-8.013888	2.256832
-1451.306626	-2.798150	2.266829
-1449.646495	-4.426173	2.276826
-1447.879973	-1.574560	2.286822
-1445.951558	-2.338102	2.296819
-1443.827939	-4.718004	2.306816
-1441.944283	-2.456012	2.316813
-1440.086762	-1.900009	2.326810
-1438.051171	-6.879511	2.336806
-1436.357965	-1.497003	2.346803
-1434.225400	-4.521448	2.356800
-1432.281703	1.059900	2.366797
-1430.632880	0.325426	2.376794
-1428.939850	1.956611	2.386790
-1427.173534	5.145387	2.396787
-1425.117424	-0.467211	2.406784
-1423.057170	3.579270	2.416781
-1421.297050	-0.281482	2.426778
-1419.407553	4.338148	2.436774
-1417.038036	-2.463731	2.446771
-1415.348072	0.848035	2.456768
-1413.915203	-1.255106	2.466765
-1411.875648	-2.838426	2.476762
-1410.083355	0.708700	2.486758
-1408.265703	-4.240465	2.496755
-1406.132465	-3.591511	2.506752
-1404.311353	-0.995868	2.516749
-1402.628391	1.042151	2.526746
-1400.796969	1.752046	2.536742
-1398.299247	-4.561232	2.546739
-1396.877748	-2.248679	2.556736
-1395.053703	-3.621866	2.566733
-1392.958592	-1.236904	2.576730
-1391.126615	-2.474709	2.586726
-1389.281702	-1.653701	2.596723
-1387.415051	-1.610252	2.606720
-1385.506569	6.333826	2.616717
-1383.684487	2.403557	2.626714
-1381.677191	0.333358	2.636710
-1379.744557	-3.402880	2.646707
-1378.058933	2.303453	2.656704
-1376.444803	5.663833	2.666701
-1374.305184	5.231592	2.676698
-1372.379305	4.546376	2.686694
-1370.422369	4.873104	2.696691
-1368.679409	-2.027821	2.706688
-1366.822368	0.528471	2.716685
-1364.896420	7.189466	2.726682
-1362.960109	2.636883	2.736678
-1360.735459	3.752715	2.746675
-1359.238262	4.486051	2.756672
-1357.645680	1.648853	2.766669
-1355.705735	6.991389	2.776666
-1353.707524	2.667677	2.786662
-1351.770020	5.098309	2.796659
-1349.630735	-1.651343	2.806656
-1347.929681	1.829280	2.816653
-1346.097571	1.159393	2.826650
-1344.202677	-2.341914	2.836646
-1342.249508	-8.201189	2.846643
-1340.422427	-4.337513	2.856640
-1338.705824	-0.087706	2.866637
-1336.592167	-6.247639	2.876634
-1334.665379	-8.588540	2.886630
-1332.880243	-1.812841	2.896627
-1331.166303	1.500377	2.906624
-1329.190914	4.211834	2.916621
-1327.558206	1.796559	2.926618
-1325.390963	-1.332199	2.936614
-1323.493487	-6.152766	2.946611
-1321.589097	-8.369274	2.956608
-1319.796839	-7.394148	2.966605
-1318.141485	1.525356	2.976602
-1315.862752	-1.367635	2.986598
-1314.274321	-5.228497	2.996595
-1312.197431	-0.705421	3.006592
-1310.587686	6.471919	3.016589
-1308.472170	1.866841	3.026586
-1306.621411	-1.882572	3.036582
-1304.799817	-1.189126	3.046579
-1302.945331	-5.113862	3.056576
-1301.234619	-2.158930	3.066573
-1298.977480	0.337367	3.076570
-1297.571609	-7.679811	3.086566
-1295.344769	2.610554	3.096563
-1293.427318	-3.939724	3.106560
-1291.791278	-0.357802	3.116557
-1289.206248	0.112836	3.126554
-1287.723890	3.957890	3.136550
-1286.116487	-5.634837	3.146547
-1284.371992	0.824979	3.156544
-1282.365653	-4.304357	3.166541
-1280.445373	-2.177813	3.176538
-1278.814629	-5.970839	3.186534
-1276.610830	-7.804810	3.196531
-1274.460024	-3.782103	3.206528
-1272.886200	-3.998156	3.216525
-1271.081781	-0.584654	3.226522
-1268.747460	-1.718193	3.236518
-1267.062505	-5.666361	3.246515
-1265.457524	-4.279245	3.256512
-1263.676811	-0.792110	3.266509
-1261.881816	1.775678	3.276506
-1259.447146	-3.501514	3.286502
-1257.656578	-4.023138	3.296499
-1256.241803	-7.805543	3.306496
-1254.296195	3.842492	3.316493
-1252.233743	2.432370	3.326490
-1250.235963	1.954204	3.336486
-1248.496560	1.752009	3.346483
-1246.887941	3.632525	3.356480
-1245.155487	0.003839	3.366477
-1242.877141	7.519296	3.376474
-1240.858952	2.080860	3.386470
-1239.000041	-1.716957	3.396467
-1237.212917	2.681637	3.406464
-1235.263704	4.436081	3.416461
-1233.195962	6.836105	3.426458
-1231.655669	0.083460	3.436454
-1230.077862	3.689639	3.446451
-1228.055918	9.993943	3.456448
-1225.780283	5.103328	3.466445
-1223.851642	6.714687	3.476442
-1222.162195	4.301563	3.486438
-1220.116717	-5.163638	3.496435
-1218.385623	-1.843436	3.506432
-1216.912510	8.387912	3.516429
-1214.720764	3.791916	3.526426
-1212.814407	0.200167	3.536422
-1210.386296	7.240961	3.546419
-1209.015953	0.072893	3.556416
-1207.317869	1.365001	3.566413
-1205.558451	4.007297	3.576410
-1203.846151	-0.264878	3.586406
-1201.543567	3.562654	3.596403
-1199.542659	-0.397068	3.606400
-1197.740818	-0.128199	3.616397
-1196.020256	1.039118	3.626394
-1194.142070	2.882451	3.636390
-1192.241515	1.755074	3.646387
-1190.269201	-0.107077	3.656384
-1188.287170	0.540688	3.666381
-1186.642286	0.282032	3.676378
-1184.463726	3.221882	3.686374
-1182.716037	0.759644	3.696371
-1181.052917	-1.884095	3.706368
-1179.068975	0.176235	3.716365
-1177.252720	4.744541	3.726362
-1175.249786	9.312802	3.736358
-1173.418854	3.809329	3.746355
-1171.645426	8.071983	3.756352
-1169.614227	6.226603	3.766349
-1167.755408	6.977347	3.776346
-1165.918068	3.677675	3.786342
-1164.219998	6.941526	3.796339
-1162.103290	1.807118	3.806336
-1160.153679	6.225272	3.816333
-1158.545913	7.530539	3.826330
-1156.025093	7.831674	3.836326
-1154.694539	-0.475669	3.846323
-1153.194879	0.347033	3.856320
-1151.108009	2.094082	3.866317
-1149.004279	5.729337	3.876314
-1146.887704	5.233981	3.886310
-1145.074360	0.100693	3.896307
-1143.270801	3.453541	3.906304
-1141.662203	-1.347385	3.916301
-1139.817897	1.168122	3.926298
-1137.755226	3.839787	3.936294
-1135.499693	1.362290	3.946291
-1134.095223	7.782953	3.956288
-1132.148442	-0.525076	3.966285
-1130.306905	-3.527857	3.976282
-1128.637398	0.882686	3.986278
-1126.167282	-3.808493	3.996275
-1124.737325	2.985225	4.006272
-1122.935646	3.790460	4.016269
-1120.705801	5.814917	4.026266
-1118.855720	-0.062534	4.036262
-1117.019117	-0.461187	4.046259
-1115.454906	2.162895	4.056256
-1113.718680	6.074691	4.066253
-1110.996901	0.836406	4.076250
-1109.296754	-0.414212	4.086246
-1107.569401	2.065272	4.096243
-1105.956473	-1.757835	4.106240
-1103.970634	0.717181	4.116237
-1102.556282	3.091143	4.126234
-1100.626109	-0.519668	4.136230
-1098.001666	4.079446	4.146227
-1096.188261	6.042633	4.156224
-1094.741907	5.595596	4.166221
-1093.100163	5.143070	4.176218
-1090.847570	3.586553	4.186214
-1088.636953	-1.558413	4.196211
-1087.242739	5.395988	4.206208
-1084.976556	-0.695967	4.216205
-1083.126490	0.748733	4.226202
-1081.800174	0.711203	4.236198
-1079.425505	2.123131	4.246195
-1077.770060	3.450279	4.256192
-1075.756749	0.510900	4.266189
-1074.301624	5.211216	4.276186
-1071.868079	-5.297532	4.286182
-1070.142945	-2.045403	4.296179
-1068.472770	-2.818183	4.306176
-1066.422091	-3.244878	4.316173
-1064.572508	-4.895405	4.326170
-1062.844917	-2.382746	4.336166
-1060.987025	-0.943332	4.346163
-1058.516958	-6.253767	4.356160
-1057.334085	-5.061652	4.366157
-1055.189446	-4.856324	4.376154
-1053.134906	-3.232909	4.386150
-1051.561132	-10.669435	4.396147
-1049.629897	0.316041	4.406144
-1047.526232	-4.498323	4.416141
-1045.690455	-11.363693	4.426138
-1043.981068	-7.423549	4.436134
-1042.179933	-2.540761	4.446131
-1039.981964	-3.153191	4.456128
-1038.108284	-8.351335	4.466125
-1036.563388	-3.054233	4.476122
-1034.570408	-2.159686	4.486118
-1032.569405	-8.602087	4.496115
-1030.861518	-13.021644	4.506112
-1028.745411	-6.996618	4.516109
-1027.213945	1.249513	4.526106
-1025.483643	-4.214889	4.536102
-1023.444173	0.081987	4.546099
-1021.172378	-2.984347	4.556096
-1019.456245	-11.111242	4.566093
-1017.938037	0.456968	4.576090
-1015.524866	-8.208531	4.586086
-1013.788320	-7.645004	4.596083
-1012.035330	-9.333069	4.606080
-1010.186074	-1.593224	4.616077
-1008.123880	-2.109606	4.626074
-1006.406116	-3.894377	4.636070
-1004.568112	-4.834272	4.646067
-1002.537837	-1.516729	4.656064
-1000.597607	-3.925401	4.666061
-999.232199	-6.392282	4.676058
-997.263990	-6.179160	4.686054
-995.184559	-5.146884	4.696051
-993.108460	-4.766138	4.706048
-991.372306	-1.019477	4.716045
-989.331887	-1.664508	4.726042
-987.620883	-4.072551	4.736038
-985.777985	-6.688987	4.746035
-983.810661	-3.297788	4.756032
-982.162960	-4.405770	4.766029
-980.248916	-5.676462	4.776026
-977.902463	-3.300446	4.786022
-976.337665	-0.515952	4.796019
-974.538048	-3.054211	4.806016
-972.654974	-1.272873	4.816013
-971.113273	-0.727650	4.826010
-968.970054	-3.687704	4.836006
-967.040485	0.449433	4.846003
-964.879983	-1.510926	4.856000
-962.970318	-2.859507	4.865997
-961.415865	0.504178	4.875994
-959.576244	0.743345	4.885990
-957.584040	-4.705924	4.895987
-955.700616	-1.886410	4.905984
-953.954912	2.019087	4.915981
-952.239298	1.474494	4.925978
-949.733007	0.190667	4.935974
-948.185232	5.252557	4.945971
-946.348178	9.603197	4.955968
-944.804465	6.832626	4.965965
-942.593936	6.697091	4.975962
-940.639169	7.567812	4.985958
-938.979571	6.308412	4.995955
-936.563453	6.403960	5.005952
-934.815246	0.444077	5.015949
-933.341152	3.488007	5.025946
-931.499148	0.907314	5.035942
-929.436062	6.588577	5.045939
-927.518213	1.751230	5.055936
-925.641882	3.397398	5.065933
-923.996374	-1.803823	5.075930
-922.068332	2.573100	5.085926
-920.592868	1.160751	5.095923
-918.296057	-1.622110	5.105920
-916.286301	5.045286	5.115917
-914.376005	2.951637	5.125914
-912.405085	0.268197	5.135910
-910.548058	-1.434923	5.145907
-908.758046	-4.286097	5.155904
-907.099024	-1.956440	5.165901
-905.030218	-0.653153	5.175898
-903.166439	-2.571240	5.185894
-901.356205	-4.040655	5.195891
-899.322504	3.344301	5.205888
-897.548337	4.904079	5.215885
-895.727932	5.344971	5.225882
-894.131820	2.059547	5.235878
-891.918989	0.417082	5.245875
-889.888355	0.821887	5.255872
-888.108767	-4.403128	5.265869
-886.292721	-2.944597	5.275866
-884.338458	-2.217226	5.285862
-882.650345	-2.755885	5.295859
-880.810715	0.070788	5.305856
-878.831204	2.524474	5.315853
-876.823696	3.433598	5.325850
-875.118686	0.063091	5.335846
-873.310034	1.455316	5.345843
-870.825658	3.597465	5.355840
-869.386525	3.679355	5.365837
-867.943268	1.042248	5.375834
-865.829263	3.205688	5.385830
-863.397139	-2.105247	5.395827
-861.696319	-5.299553	5.405824
-860.225053	-2.090701	5.415821
-858.280117	4.616703	5.425818
-856.008857	-0.268239	5.435814
-854.516506	-4.039341	5.445811
-852.664707	-5.455008	5.455808
-850.761081	-0.801162	5.465805
-848.521757	2.328023	5.475802
-846.762668	4.580062	5.485798
-845.080857	1.723375	5.495795
-842.965276	-5.719544	5.505792
-841.189508	-4.076232	5.515789
-839.526494	-1.665028	5.525786
-837.599638	-1.023435	5.535782
-835.652017	-0.533216	5.545779
-833.850491	-0.779104	5.555776
-831.863339	-2.991827	5.565773
-829.885186	-0.788056	5.575770
-828.129780	-4.146249	5.585766
-826.525049	-6.104414	5.595763
-824.579324	1.922890	5.605760
-822.398427	5.384615	5.615757
-820.358473	-0.978629	5.625754
-818.644300	-4.269668	5.635750
-816.647688	-3.304897	5.645747
-815.145508	-1.325711	5.655744
-813.471496	2.373995	5.665741
-811.577243	-3.945265	5.675738
-809.240356	0.587599	5.685734
-807.371576	3.890280	5.695731
-805.605736	3.595594	5.705728
-803.615068	-1.517812	5.715725
-801.858846	5.797843	5.725722
-800.223120	2.590623	5.735718
-798.143549	0.773074	5.745715
-796.133655	-0.137745	5.755712
-794.149626	-0.127620	5.765709
-792.585442	4.939818	5.775706
-790.627371	5.397041	5.785702
-788.992688	1.382578	5.795699
-786.840274	-0.455372	5.805696
-784.957559	5.420547	5.815693
-782.665771	1.275121	5.825690
-780.952714	1.539645	5.835686
-779.426588	2.204200	5.845683
-777.652499	3.588172	5.855680
-775.549769	4.141510	5.865677
-773.777913	2.266918	5.875674
-771.834699	2.902176	5.885670
-769.762956	-3.438838	5.895667
-768.122882	0.331528	5.905664
-766.460443	1.529154	5.915661
-763.966753	5.707105	5.925658
-762.442083	4.024335	5.935654
-760.867342	-1.024780	5.945651
-758.911282	1.767737	5.955648
-756.900441	0.459976	5.965645
-755.112323	12.560592	5.975642
-752.836956	-3.442821	5.985638
-750.899060	4.662935	5.995635
-749.732090	4.543777	6.005632
-747.295484	2.672483	6.015629
-745.462514	4.768816	6.025626
-743.711182	-0.330758	6.035622
-741.708920	-0.498819	6.045619
-739.754892	-5.463632	6.055616
-738.165269	-5.275524	6.065613
-736.632184	0.128463	6.075610
-734.471558	-0.673825	6.085606
-732.211881	1.772160	6.095603
-730.609532	-0.286739	6.105600
-728.661411	-6.962213	6.115597
-726.310617	-5.451530	6.125594
-724.808909	1.351378	6.135590
-723.175406	2.335434	6.145587
-721.346443	-4.425900	6.155584
-719.539759	3.437202	6.165581
-717.393493	0.136460	6.175578
-715.224038	1.664835	6.185574
-713.297555	2.494671	6.195571
-711.910574	0.619760	6.205568
-710.160023	4.899199	6.215565
-708.272147	1.394612	6.225562
-706.473806	2.311258	6.235558
-704.110496	-4.127589	6.245555
-702.510473	-4.171269	6.255552
-700.574869	-5.121464	6.265549
-698.639642	-2.592509	6.275546
-696.655742	-3.824481	6.285542
-694.819940	-2.302465	6.295539
-693.126267	-1.646477	6.305536
-691.113779	-2.016644	6.315533
-689.268189	-2.136056	6.325530
-687.372519	4.627319	6.335526
-685.565980	7.198918	6.345523
-683.440217	0.805588	6.355520
-682.028338	0.870876	6.365517
-680.137272	5.790968	6.375514
-677.954559	4.574287	6.385510
-676.043385	-0.139300	6.395507
-674.101487	-2.495161	6.405504
-672.440234	-1.915807	6.415501
-670.349075	-1.628784	6.425498
-668.883575	0.100256	6.435494
-666.713017	1.229693	6.445491
-664.655335	0.592916	6.455488
-663.191713	1.090787	6.465485
-660.931470	0.305428	6.475482
-659.505860	2.217978	6.485478
-657.229792	0.215011	6.495475
-655.567920	5.860937	6.505472
-653.628970	0.344255	6.515469
-651.676802	6.143111	6.525466
-649.842467	1.051457	6.535462
-647.951975	1.321153	6.545459
-646.276550	1.268902	6.555456
-644.265672	5.150374	6.565453
-642.115366	1.343887	6.575450
-640.626515	3.853434	6.585446
-638.613698	3.940104	6.595443
-636.754054	4.811481	6.605440
-634.644311	-0.976374	6.615437
-633.040659	4.391440	6.625434
-631.076056	2.579074	6.635430
-629.103205	4.281533	6.645427
-627.525439	-2.813700	6.655424
-625.867808	-1.479238	6.665421
-623.816088	1.285467	6.675418
-621.711481	7.679065	6.685414
-619.559629	0.689250	6.695411
-617.677620	1.227187	6.705408
-616.129376	0.997583	6.715405
-614.237222	0.602651	6.725402
-612.453580	8.704917	6.735398
-610.445219	5.829032	6.745395
-608.556109	2.155515	6.755392
-606.619766	4.286340	6.765389
-604.840411	5.903449	6.775386
-603.093605	5.092006	6.785382
-601.379659	7.435683	6.795379
-599.260516	3.418774	6.805376
-597.178360	5.305238	6.815373
-595.380013	10.577612	6.825370
-593.577303	8.948362	6.835366
-591.702373	7.229653	6.845363
-589.730051	1.166613	6.855360
-588.096617	3.292513	6.865357
-585.882562	5.304555	6.875354
-584.529135	0.570516	6.885350
-582.060443	2.947519	6.895347
-579.977319	0.494743	6.905344
-578.615328	1.715148	6.915341
-576.758406	4.201478	6.925338
-574.960281	1.190555	6.935334
-573.091037	2.649185	6.945331
-571.135439	4.034901	6.955328
-569.179331	2.763885	6.965325
-567.341869	9.000212	6.975322
-565.387764	2.840712	6.985318
-563.198110	-1.196579	6.995315
-561.749063	5.141966	7.005312
-560.110787	4.819470	7.015309
-558.154322	4.162170	7.025306
-555.719058	6.945675	7.035302
-554.118035	2.735899	7.045299
-552.212609	6.628397	7.055296
-550.423895	4.528097	7.065293
-548.552130	1.619951	7.075290
-546.842818	2.236953	7.085286
-544.946865	7.819447	7.095283
-543.062076	3.174067	7.105280
-540.885305	3.109738	7.115277
-539.141351	12.421497	7.125274
-537.267492	8.128551	7.135270
-535.055363	13.433899	7.145267
-533.525889	6.667100	7.155264
-531.870553	9.686803	7.165261
-530.067722	7.307040	7.175258
-527.559988	1.619303	7.185254
-526.110039	6.098214	7.195251
-524.210694	6.894455	7.205248
-522.205690	0.789473	7.215245
-520.729382	6.327787	7.225242
-518.672342	5.536657	7.235238
-516.306715	8.220683	7.245235
-514.782117	0.144585	7.255232
-513.069037	1.968341	7.265229
-510.974557	-0.411262	7.275226
-509.020206	-0.518827	7.285222
-507.298555	-5.518770	7.295219
-505.335164	-0.392845	7.305216
-503.364089	5.596894	7.315213
-501.959655	3.247557	7.325210
-499.633707	1.809569	7.335206
-497.602477	0.220588	7.345203
-496.110600	4.563475	7.355200
-494.295244	10.326999	7.365197
-492.291417	3.344848	7.375194
-490.384062	9.851801	7.385190
-488.494405	-0.607639	7.395187
-486.701623	4.945157	7.405184
-484.622916	3.293891	7.415181
-482.933618	2.917615	7.425178
-480.849475	-0.503968	7.435174
-479.193669	5.786885	7.445171
-477.117728	3.350010	7.455168
-475.152738	-2.049739	7.465165
-473.712568	4.818374	7.475162
-471.593925	4.308367	7.485158
-469.696068	2.532815	7.495155
-467.783843	0.128776	7.505152
-466.255864	-3.451505	7.515149
-463.952658	3.766121	7.525146
-462.116145	1.986869	7.535142
-460.391837	-1.516828	7.545139
-458.439185	-2.001907	7.555136
-456.480705	5.990209	7.565133
-454.807983	6.524206	7.575130
-453.075391	6.255918	7.585126
-450.649276	0.572737	7.595123
-449.035033	4.391538	7.605120
-447.037645	0.938613	7.615117
-445.359516	4.938134	7.625114
-443.418373	3.600577	7.635110
-441.540845	4.634171	7.645107
-439.981445	4.029629	7.655104
-438.000022	6.054389	7.665101
-435.862855	11.746528	7.675098
-434.329604	5.094512	7.685094
-432.193549	-1.854969	7.695091
-430.114685	-6.566402	7.705088
-428.158939	-3.531801	7.715085
-426.484568	2.285976	7.725082
-424.874334	-1.227780	7.735078
-423.031259	-6.227184	7.745075
-420.828901	-8.161663	7.755072
-418.585855	-4.514753	7.765069
-417.404903	5.514140	7.775066
-415.476649	0.195806	7.785062
-413.389061	3.051291	7.795059
-412.032827	8.314230	7.805056
-409.743433	4.945993	7.815053
-407.735851	3.067067	7.825050
-405.758127	-0.889136	7.835046
-404.175499	-2.272671	7.845043
-402.107277	-2.499714	7.855040
-400.008858	2.754863	7.865037
-398.360692	5.824857	7.875034
-396.810877	0.825972	7.885030
-394.569638	4.493759	7.895027
-392.829858	0.347573	7.905024
-390.831049	-5.214845	7.915021
-389.131459	3.912518	7.925018
-386.874934	1.534023	7.935014
-385.142227	4.384006	7.945011
-383.582317	0.592758	7.955008
-381.878019	1.416989	7.965005
-379.732153	8.603957	7.975002
-377.678141	6.678347	7.984998
-376.037275	4.176245	7.994995
-374.216841	6.442861	8.004992
-372.025534	1.092855	8.014989
-369.681523	0.275487	8.024986
-368.394578	3.522466	8.034982
-366.796538	4.277983	8.044979
-364.181356	2.034396	8.054976
-362.792762	9.110988	8.064973
-361.116855	7.822521	8.074970
-359.099463	3.474195	8.084966
-357.341167	6.709484	8.094963
-355.444743	1.362249	8.104960
-353.403857	4.087845	8.114957
-351.687492	-1.069623	8.124954
-349.616521	7.990893	8.134950
-347.646885	5.472320	8.144947
-345.458542	8.651234	8.154944
-344.145797	3.174111	8.164941
-342.138677	7.972888	8.174938
-340.332596	8.370625	8.184934
-338.566570	-1.731625	8.194931
-336.270590	3.065424	8.204928
-334.516429	-0.199106	8.214925
-332.690219	3.273530	8.224922
-331.158122	2.180478	8.234918
-329.116933	4.088328	8.244915
-326.807095	4.727293	8.254912
-325.248734	5.213770	8.264909
-323.399180	11.402296	8.274906
-321.300652	1.802641	8.284902
-319.483038	4.269744	8.294899
-317.775876	7.332022	8.304896
-316.337509	5.038572	8.314893
-314.029966	12.940460	8.324890
-312.011362	2.958904	8.334886
-309.880487	-1.174899	8.344883
-308.305271	-0.539149	8.354880
-306.293529	6.221899	8.364877
-304.908505	4.221369	8.374874
-303.155966	5.983902	8.384870
-301.012985	4.324855	8.394867
-298.776190	1.116667	8.404864
-297.138711	4.418946	8.414861
-295.379390	2.911473	8.424858
-293.296104	3.160900	8.434854
-291.363960	5.125809	8.444851
-289.489108	4.281062	8.454848
-287.703405	9.185428	8.464845
-286.043683	8.246371	8.474842
-283.957574	6.312530	8.484838
-282.113860	5.060520	8.494835
-280.088888	9.536535	8.504832
-278.484811	4.644571	8.514829
-276.602336	-3.533557	8.524826
-274.713841	2.733281	8.534822
-272.679545	1.862774	8.544819
-270.491245	0.805789	8.554816
-269.074335	1.366345	8.564813
-267.149077	0.251722	8.574810
-265.259204	8.594016	8.584807
-263.200878	12.633927	8.594803
-261.632319	7.357584	8.604800
-259.616922	12.461278	8.614797
-257.315626	9.698917	8.624794
-255.687832	10.827991	8.634791
-254.083701	6.520946	8.644787
-252.041433	4.193098	8.654784
-250.063977	6.106384	8.664781
-248.660112	2.830827	8.674778
-246.633105	11.713192	8.684775
-244.318086	3.156168	8.694771
-242.627445	3.569398	8.704768
-240.736342	-0.269916	8.714765
-238.924582	-2.200945	8.724762
-237.072587	9.558590	8.734759
-234.933828	9.469708	8.744755
-233.163049	1.503221	8.754752
-232.152879	-1.590984	8.764749
-229.484862	4.764686	8.774746
-227.350903	2.964942	8.784743
-225.744329	-1.118027	8.794739
-223.915683	2.035695	8.804736
-221.973794	-2.524900	8.814733
-219.817598	-4.404336	8.824730
-218.292646	-1.623780	8.834727
-216.529615	1.287863	8.844723
-214.556852	-2.997419	8.854720
-212.516833	-9.370709	8.864717
-210.864427	-12.852500	8.874714
-208.999592	-4.548970	8.884711
-207.037150	-10.362761	8.894707
-204.914258	-4.580317	8.904704
-203.223881	-6.861624	8.914701
-201.614904	-2.547800	8.924698
-199.673268	-5.221176	8.934695
-197.571574	-8.988299	8.944691
-195.681563	-9.456989	8.954688
-194.016312	-7.967556	8.964685
-192.353315	-3.999324	8.974682
-190.300396	-3.568769	8.984679
-188.109542	-7.055558	8.994675
-186.464356	-4.686877	9.004672
-184.231738	-10.667142	9.014669
-182.648694	-4.115092	9.024666
-180.677453	-4.222249	9.034663
-178.927225	-5.192598	9.044659
-177.131899	-1.256539	9.054656
-174.998574	-3.989655	9.064653
-173.124355	-5.144887	9.074650
-171.542995	-1.651530	9.084647
-169.741480	2.796861	9.094643
-167.357365	-3.461531	9.104640
-165.914171	-6.823642	9.114637
-164.419520	3.025074	9.124634
-161.883403	-6.250394	9.134631
-159.861638	-11.733268	9.144627
-158.162504	-8.824081	9.154624
-156.445557	-5.802544	9.164621
-154.803792	-1.795481	9.174618
-152.345281	-9.589793	9.184615
-150.614251	-4.746342	9.194611
-148.952016	-10.840610	9.204608
-146.776506	-9.024874	9.214605
-145.040185	-7.624678	9.224602
-143.212573	-2.238157	9.234599
-141.315385	-0.654105	9.244595
-139.398232	-4.613646	9.254592
-137.872664	-10.011417	9.264589
-136.009064	-5.515959	9.274586
-134.012943	0.916662	9.284583
-132.106769	-8.075284	9.294579
-130.237458	-5.409873	9.304576
-127.725091	-9.182974	9.314573
-126.543387	-4.751977	9.324570
-124.590502	-2.028570	9.334567
-122.756540	-1.444240	9.344563
-120.603915	-1.307405	9.354560
-118.666328	-5.268071	9.364557
-117.041062	-1.032097	9.374554
-115.096670	-0.501086	9.384551
-113.286733	4.427262	9.394547
-111.168340	6.452003	9.404544
-109.366705	0.783991	9.414541
-107.809144	0.682201	9.424538
-105.773256	-0.073497	9.434535
-103.845484	1.153187	9.444531
-102.060293	-2.560807	9.454528
-100.039227	-0.308325	9.464525
-98.032349	6.007859	9.474522
-96.382940	2.808407	9.484519
-94.206894	7.227385	9.494515
-92.605218	4.123463	9.504512
-90.804528	0.501271	9.514509
-88.626222	-0.158695	9.524506
-87.220465	-2.214887	9.534503
-85.495602	1.109642	9.544499
-83.494558	-1.588104	9.554496
-81.014398	-5.054502	9.564493
-79.616619	1.064587	9.574490
-77.613608	2.542782	9.584487
-75.563062	0.477200	9.594483
-73.867433	2.109283	9.604480
-71.933616	2.895066	9.614477
-69.962258	5.020923	9.624474
-68.218268	5.434555	9.634471
-66.378517	12.267117	9.644467
-64.432567	8.742542	9.654464
-62.750432	-0.593540	9.664461
-60.717996	7.896331	9.674458
-58.749542	1.632196	9.684455
-56.829287	-6.753899	9.694451
-55.206827	-0.584800	9.704448
-53.300596	2.718522	9.714445
-51.173472	1.292721	9.724442
-49.503661	2.649030	9.734439
-47.339948	-0.439405	9.744435
-45.664416	1.123414	9.754432
-43.747648	1.769459	9.764429
-42.078275	4.378690	9.774426
-40.230042	2.630791	9.784423
-38.126916	3.179672	9.794419
-36.090825	2.084477	9.804416
-34.362425	4.836539	9.814413
-32.667825	7.841410	9.824410
-30.624731	8.097456	9.834407
-28.876719	1.739523	9.844403
-27.029299	2.400232	9.854400
-25.214593	3.755814	9.864397
-23.146076	1.382065	9.874394
-21.085240	-1.502966	9.884391
-19.488600	-3.162661	9.894387
-17.525326	2.661483	9.904384
-15.634920	0.109601	9.914381
-13.752225	6.706385	9.924378
-11.990570	4.630292	9.934375
-10.158815	10.058852	9.944371
-7.890885	3.273469	9.954368
-6.163744	2.748207	9.964365
-4.557079	11.283846	9.974362
-3.377033	33.785400	9.984359
-2.312445	77.289838	9.994355
-0.933351	135.143160	10.004352
0.000000	200.351185	10.009357
0.978718	228.528590	10.014362
1.655065	261.768075	10.019367
1.956420	292.059023	10.024371
2.616733	322.531630	10.029376
2.700435	341.465172	10.034381
3.024859	362.111609	10.039386
3.414954	371.984688	10.044391
3.426565	376.185763	10.049395
3.222548	384.854975	10.054400
3.551165	408.598149	10.059405
3.895703	413.185424	10.064410
3.915265	422.477090	10.069415
4.005981	424.858751	10.074419
4.060144	426.407892	10.079424
3.769770	426.100905	10.084429
4.032952	425.187046	10.089434
4.036276	442.584015	10.094439
4.474553	457.936747	10.099443
4.743935	467.009556	10.104448
4.610037	468.574762	10.109453
4.655067	447.766661	10.114458
4.149707	450.633810	10.119463
4.473684	459.788830	10.124467
4.447559	469.432557	10.129472
4.450126	474.684390	10.134477
4.757947	469.880354	10.139482
4.453297	476.788239	10.144487
4.650208	476.026658	10.149491
4.637995	485.092104	10.154496
4.621791	476.341896	10.159501
4.911388	479.611544	10.164506
4.582285	495.381277	10.169511
4.845757	484.099493	10.174515
5.382308	494.060035	10.179520
5.091998	493.813034	10.184525
4.855014	486.603003	10.189530
4.951220	512.059033	10.194535
5.190539	521.519124	10.199539
5.512300	524.746162	10.204544
5.521304	525.208873	10.209549
5.591318	527.245951	10.214554
5.301452	533.373319	10.219559
5.412353	521.349135	10.224563
5.687313	537.028756	10.229568
5.618594	533.529892	10.234573
5.810645	525.079861	10.239578
5.387967	515.898417	10.244583
5.708172	522.924966	10.249587
5.725310	535.567950	10.254592
5.668522	534.653686	10.259597
5.771424	538.753497	10.264602
5.541795	551.950372	10.269607
5.820483	543.084038	10.274611
5.911861	551.350990	10.279616
5.748026	550.226139	10.284621
5.945668	551.241886	10.289626
5.821640	558.831320	10.294631
6.112116	551.803576	10.299635
5.894893	558.214938	10.304640
6.116759	556.803694	10.309645
6.268692	556.444944	10.314650
6.103112	553.958186	10.319655
6.290725	556.236808	10.324659
6.235923	558.879488	10.329664
6.152914	569.025256	10.334669
6.718905	580.513140	10.339674
6.441830	591.921381	10.344679
6.587837	594.935417	10.349683
6.724703	598.026809	10.354688
6.484143	601.036866	10.359693
6.647175	597.636406	10.364698
6.554330	607.469286	10.369703
6.546126	604.695804	10.374707
6.844495	605.730205	10.379712
6.845264	606.017491	10.384717
7.236880	601.748116	10.389722
6.903023	609.018296	10.394727
7.251951	610.808224	10.399731
6.711549	610.539761	10.404736
6.716840	615.186844	10.409741
6.933576	608.415660	10.414746
6.893161	615.527374	10.419751
7.092360	610.342060	10.424755
6.851338	605.242492	10.429760
7.396528	623.103715	10.434765
7.281033	614.080723	10.439770
7.193130	623.471853	10.444775
7.287456	630.636653	10.449779
7.412849	641.021860	10.454784
7.479632	656.925977	10.459789
7.585126	655.819673	10.464794
7.525638	656.753203	10.469799
7.901778	649.347575	10.474803
7.479568	657.548305	10.479808
7.535919	662.830452	10.484813
7.894139	658.871915	10.489818
7.670321	663.900922	10.494823
7.625747	662.578774	10.499827
7.334698	659.922463	10.504832
7.541321	660.946151	10.509837
7.690793	662.557525	10.514842
7.497685	674.871150	10.519847
8.145030	681.622209	10.524851
8.088359	686.455593	10.529856
8.370560	692.452172	10.534861
8.373235	692.254008	10.539866
8.443116	692.572867	10.544871
8.491724	695.654938	10.549875
8.754275	698.110203	10.554880
8.426820	689.107721	10.559885
8.572643	686.318473	10.564890
8.228688	686.301321	10.569895
8.531858	686.953199	10.574899
8.593456	690.372905	10.579904
8.611147	703.941180	10.584909
8.739380	697.371052	10.589914
8.118402	708.187827	10.594919
8.029404	708.505901	10.599923
8.141292	703.317764	10.604928
8.050662	704.668736	10.609933
8.758001	728.152858	10.614938
8.432871	737.891044	10.619943
8.556039	743.960700	10.624947
8.949302	741.046122	10.629952
8.688127	744.855521	10.634957
9.010998	744.808506	10.639962
8.806186	746.825631	10.644967
8.898380	746.651986	10.649971
9.235762	752.328472	10.654976
9.039541	771.117901	10.659981
9.167170	774.112229	10.664986
9.342533	786.307501	10.669991
9.523156	782.685697	10.674995
9.476849	779.663719	10.680000
8.881141	783.419173	10.685005
9.234234	785.472089	10.690010
9.086991	784.027404	10.695015
9.015657	781.286031	10.700019
9.281106	802.417239	10.705024
9.103775	817.891274	10.710029
9.720107	809.017423	10.715034
9.872896	819.218053	10.720039
9.918579	818.563306	10.725043
9.819982	821.892878	10.730048
9.907089	826.385075	10.735053
10.477568	818.277366	10.740058
10.159627	826.729120	10.745063
10.062892	828.197990	10.750067
9.881390	822.121046	10.755072
10.264127	828.593463	10.760077
10.585622	829.035365	10.765082
9.903690	837.057696	10.770087
9.782410	825.264536	10.775091
9.732420	826.541050	10.780096
9.434916	836.381534	10.785101
9.846448	844.870457	10.790106
10.005554	856.070680	10.795111
10.115558	862.548033	10.800115
10.195363	858.082975	10.805120
10.049220	878.194994	10.810125
10.624590	886.543743	10.815130
10.886504	896.696502	10.820135
10.716323	900.053364	10.825139
10.768333	893.015829	10.830144
10.575326	899.886598	10.835149
10.885206	893.902610	10.840154
10.523438	895.559823	10.845159
10.737255	900.426631	10.850163
10.518724	897.598766	10.855168
10.681682	903.606399	10.860173
10.763842	891.889622	10.865178
10.741802	920.808691	10.870183
11.127666	929.432719	10.875187
11.037503	926.709944	10.880192
10.992481	937.917990	10.885197
11.511118	933.406878	10.890202
11.234540	930.596854	10.895207
11.375077	937.742030	10.900211
11.340253	939.102005	10.905216
11.249027	940.873494	10.910221
11.706682	938.426656	10.915226
11.383584	943.155405	10.920231
11.385545	939.233014	10.925235
11.620028	939.857998	10.930240
11.279588	943.313930	10.935245
11.555732	938.315447	10.940250
11.429279	946.209432	10.945255
11.584235	962.581505	10.950259
12.010138	978.133847	10.955264
11.696558	974.205550	10.960269
12.254625	973.382811	10.965274
11.894773	980.301565	10.970279
11.799650	980.447800	10.975283
12.029446	978.885554	10.980288
11.731633	975.092712	10.985293
12.513956	975.644684	10.990298
12.304443	978.050277	10.995303
12.316932	973.713571	11.000307
12.200876	980.429470	11.005312
11.650428	983.986946	11.010317
11.652506	979.247812	11.015322
11.885219	991.524201	11.020327
12.255416	1011.877465	11.025331
12.510805	1003.250921	11.030336
12.545217	1010.224456	11.035341
12.568370	1017.118609	11.040346
12.429621	1016.574820	11.045351
12.535538	1014.831309	11.050355
12.538044	1016.651078	11.055360
12.639766	1016.940404	11.060365
12.650749	1010.400117	11.065370
12.896163	1023.776465	11.070375
12.747644	1021.536972	11.075379
13.155943	1018.760292	11.080384
12.725359	1020.728530	11.085389
12.550442	1022.930039	11.090394
12.824223	1038.812868	11.095399
12.985296	1053.605029	11.100403
13.000903	1052.873323	11.105408
13.178288	1056.404705	11.110413
13.415046	1051.023726	11.115418
13.259023	1049.582495	11.120423
13.127184	1048.659359	11.125427
13.739965	1052.875172	11.130432
13.404138	1060.226029	11.135437
13.442849	1053.318598	11.140442
13.445334	1058.854854	11.145447
13.404936	1050.721109	11.150451
13.738297	1060.262115	11.155456
13.332766	1056.462459	11.160461
13.635450	1054.182308	11.165466
13.587284	1067.429029	11.170471
13.590428	1058.192410	11.175475
13.571867	1061.980418	11.180480
13.778139	1076.842615	11.185485
14.734820	1074.307035	11.190490
14.301850	1066.749808	11.195495
14.310891	1062.192614	11.200499
13.822803	1057.263945	11.205504
13.679751	1060.676585	11.210509
13.855085	1053.061643	11.215514
13.759569	1068.536898	11.220519
13.940551	1082.636851	11.225523
14.468941	1080.019966	11.230528
14.182165	1092.174320	11.235533
14.492557	1085.425163	11.240538
14.979330	1088.845477	11.245543
14.799703	1084.726420	11.250547
14.841990	1074.643070	11.255552
14.513948	1077.723086	11.260557
14.402755	1054.806995	11.265562
14.236456	1067.333045	11.270567
14.108778	1085.569120	11.275571
14.301828	1079.302721	11.280576
14.137607	1087.880628	11.285581
14.368937	1087.520490	11.290586
14.405482	1093.024865	11.295591
14.795711	1110.425318	11.300595
15.151312	1118.947271	11.305600
14.959905	1128.991986	11.310605
15.115088	1124.361162	11.315610
15.000829	1126.109779	11.320615
14.906036	1118.385989	11.325619
15.073058	1122.887859	11.330624
14.864269	1124.830712	11.335629
15.055345	1120.756638	11.340634
15.177950	1122.560563	11.345639
15.059603	1127.781241	11.350643
15.235678	1135.543317	11.355648
15.000963	1129.678669	11.360653
15.259432	1123.759857	11.365658
15.367248	1138.682416	11.370663
15.341005	1151.386626	11.375667
15.723208	1158.687838	11.380672
15.672880	1164.317661	11.385677
15.978231	1151.754777	11.390682
15.867095	1155.979083	11.395687
16.051001	1160.687677	11.400691
15.683480	1137.088299	11.405696
15.931550	1146.126869	11.410701
15.607917	1141.883275	11.415706
15.687049	1145.809292	11.420711
15.763866	1159.169664	11.425715
15.912733	1161.546994	11.430720
16.055375	1169.993383	11.435725
16.162288	1166.103862	11.440730
16.166892	1166.986957	11.445735
15.885308	1161.499024	11.450739
15.991839	1170.200686	11.455744
15.706419	1167.162000	11.460749
16.063578	1168.042279	11.465754
16.049248	1176.149658	11.470759
15.908028	1187.033713	11.475763
16.622738	1196.039277	11.480768
16.532953	1203.470385	11.485773
16.804480	1192.185528	11.490778
16.521989	1205.207276	11.495783
16.485004	1200.551352	11.500787
16.554648	1203.156619	11.505792
16.561942	1202.847918	11.510797
16.974514	1196.652783	11.515802
16.807631	1199.009257	11.520807
16.785560	1196.422393	11.525811
16.876891	1198.523405	11.530816
16.925259	1202.611820	11.535821
16.973200	1203.183929	11.540826
16.813875	1206.261489	11.545831
17.027539	1196.795662	11.550835
17.400296	1192.465020	11.555840
16.809168	1199.811163	11.560845
17.484225	1201.308791	11.565850
16.954412	1200.322433	11.570855
17.067812	1197.816948	11.575859
17.140408	1197.231388	11.580864
17.395724	1215.956957	11.585869
17.728183	1215.824613	11.590874
17.378993	1214.579121	11.595879
17.421474	1209.169424	11.600883
17.796465	1215.870310	11.605888
17.881386	1214.711441	11.610893
17.274000	1202.318831	11.615898
17.468457	1212.506653	11.620903
17.696607	1221.938295	11.625907
18.041193	1220.410424	11.630912
17.817109	1232.870328	11.635917
17.763409	1226.790260	11.640922
17.736409	1231.030555	11.645927
17.889921	1228.935432	11.650931
18.321755	1236.808841	11.655936
18.555232	1237.370061	11.660941
18.433819	1221.924445	11.665946
18.133722	1215.168589	11.670951
18.042376	1200.296929	11.675955
18.288350	1204.026194	11.680960
18.065860	1212.949297	11.685965
18.374132	1219.833733	11.690970
18.321564	1232.380283	11.695975
17.743318	1229.652718	11.700979
18.012095	1236.312612	11.705984
17.941240	1240.848592	11.710989
18.245532	1238.385372	11.715994
17.854717	1244.947965	11.720999
18.124555	1262.014354	11.726003
18.387026	1264.133006	11.731008
18.203719	1269.748167	11.736013
18.644588	1269.538813	11.741018
18.671012	1271.959260	11.746023
18.938958	1265.944820	11.751027
18.918138	1259.539753	11.756032
18.919087	1276.212515	11.761037
18.797794	1267.632254	11.766042
18.956318	1269.318325	11.771047
18.844673	1265.180063	11.776051
19.085937	1266.437859	11.781056
19.271884	1278.630122	11.786061
19.353683	1263.621344	11.791066
19.001386	1278.291341	11.796071
19.235411	1290.997619	11.801075
19.627236	1289.179004	11.806080
19.603022	1287.436065	11.811085
19.257275	1274.881691	11.816090
19.198429	1281.083425	11.821095
19.177195	1287.478454	11.826099
19.361536	1288.009416	11.831104
19.851994	1295.480030	11.836109
19.853206	1296.217264	11.841114
19.882247	1298.196335	11.846119
19.928414	1296.971867	11.851123
20.149270	1298.239086	11.856128
19.986311	1292.081803	11.861133
19.931365	1283.404892	11.866138
19.768548	1281.996778	11.871143
19.713509	1277.785648	11.876147
19.788094	1277.551463	11.881152
19.653796	1288.514140	11.886157
19.943619	1298.369475	11.891162
20.231701	1299.649247	11.896167
19.661716	1299.772691	11.901171
19.756198	1307.672793	11.906176
19.712986	1303.321466	11.911181
19.868699	1298.214437	11.916186
19.934388	1304.893392	11.921191
19.955235	1322.331363	11.926195
20.848779	1322.127684	11.931200
20.353398	1330.303413	11.936205
20.585215	1329.058164	11.941210
20.383140	1329.309189	11.946215
20.299246	1329.414026	11.951219
20.645201	1335.750853	11.956224
20.507802	1327.705045	11.961229
20.866273	1333.979329	11.966234
20.534280	1335.821356	11.971239
20.544005	1341.440157	11.976243
20.861057	1335.668725	11.981248
20.453051	1343.923429	11.986253
20.537544	1341.491959	11.991258
20.811189	1340.942977	11.996263
20.949433	1357.980322	12.001267
21.531013	1350.410454	12.006272
21.343819	1358.065185	12.011277
21.800966	1341.371930	12.016282
21.927830	1333.849245	12.021287
21.183495	1322.786237	12.026291
21.611272	1318.879165	12.031296
21.466794	1326.684455	12.036301
21.662488	1306.973223	12.041306
21.242305	1298.435508	12.046311
21.172677	1287.175523	12.051315
21.158270	1284.829310	12.056320
21.387788	1292.515589	12.061325
21.304580	1288.536659	12.066330
21.068672	1287.349898	12.071335
20.994769	1286.410497	12.076339
21.278061	1286.463430	12.081344
20.947908	1289.680825	12.086349
20.986275	1290.023258	12.091354
21.268213	1285.079332	12.096359
20.825266	1290.692043	12.101363
21.180500	1283.932350	12.106368
20.792424	1286.334262	12.111373
20.594144	1283.398641	12.116378
20.668878	1289.666292	12.121383
20.780809	1304.446196	12.126387
21.127628	1309.316381	12.131392
21.214245	1328.974191	12.136397
21.013717	1315.347226	12.141402
21.557291	1315.225659	12.146407
21.133485	1312.177907	12.151411
21.329370	1305.472764	12.156416
20.899081	1302.797977	12.161421
21.101525	1290.959222	12.166426
21.227319	1297.388653	12.171431
20.846598	1294.254173	12.176435
21.487484	1297.575872	12.181440
21.091583	1304.625294	12.186445
21.296608	1298.005431	12.191450
21.283058	1301.408155	12.196455
21.254150	1303.413348	12.201459
21.461508	1292.938388	12.206464
21.262336	1306.089227	12.211469
21.620550	1300.261012	12.216474
21.641884	1291.493252	12.221479
21.364348	1299.721221	12.226483
21.364179	1275.320471	12.231488
21.043402	1278.587179	12.236493
21.150340	1269.378034	12.241498
21.278646	1277.608645	12.246503
20.978625	1286.268367	12.251507
21.246825	1277.791058	12.256512
20.997275	1279.015771	12.261517
21.126114	1278.108320	12.266522
21.174472	1274.526846	12.271527
20.921907	1275.193115	12.276531
21.127661	1280.282088	12.281536
21.137948	1281.845942	12.286541
21.228965	1273.053218	12.291546
21.011527	1281.043894	12.296551
21.181632	1283.764979	12.301555
21.355139	1276.207481	12.306560
21.088282	1289.558599	12.311565
21.094803	1278.566624	12.316570
21.225611	1284.607944	12.321575
21.209865	1278.043311	12.326579
21.109335	1274.201963	12.331584
21.069055	1284.147047	12.336589
21.338220	1282.378281	12.341594
21.485679	1282.090547	12.346599
21.177946	1284.334996	12.351603
21.333850	1281.343778	12.356608
21.202410	1278.363144	12.361613
21.138805	1270.471295	12.366618
20.860465	1266.462669	12.371623
20.703888	1280.266592	12.376627
21.141456	1283.306168	12.381632
21.062218	1280.039076	12.386637
21.051996	1285.606802	12.391642
21.194324	1287.167754	12.396647
21.095705	1286.036798	12.401651
21.184848	1279.443522	12.406656
20.826584	1289.533923	12.411661
21.052809	1290.196259	12.416666
21.437761	1277.814236	12.421671
21.012463	1285.997268	12.426675
21.170007	1285.966364	12.431680
20.753930	1282.582153	12.436685
21.057642	1280.045209	12.441690
21.302806	1282.605789	12.446695
21.032047	1291.618136	12.451699
21.675038	1282.620237	12.456704
21.188389	1291.337225	12.461709
21.376627	1279.399465	12.466714
21.066187	1263.320282	12.471719
20.867995	1264.413816	12.476723
21.414854	1252.906440	12.481728
21.094015	1257.227914	12.486733
21.180130	1257.304785	12.491738
21.416684	1255.933595	12.496743
21.267528	1268.102779	12.501747
21.315273	1253.117218	12.506752
21.561965	1264.574698	12.511757
21.227752	1250.717284	12.516762
21.551004	1260.382123	12.521767
21.438864	1260.035083	12.526771
21.624259	1250.322617	12.531776
21.278427	1235.168104	12.536781
20.962860	1222.052797	12.541786
21.240281	1230.198209	12.546791
20.756936	1228.625185	12.551795
21.280838	1224.191249	12.556800
20.751694	1235.148956	12.561805
20.562468	1227.143271	12.566810
21.058793	1237.741597	12.571815
20.901597	1244.314266	12.576819
21.266968	1255.512964	12.581824
20.917847	1263.443313	12.586829
21.076704	1260.942656	12.591834
21.113218	1257.365980	12.596839
21.157836	1258.648807	12.601843
21.356466	1252.589809	12.606848
21.619295	1256.577123	12.611853
21.513385	1241.184094	12.616858
21.278652	1227.485305	12.621863
20.997348	1232.292240	12.626867
20.793004	1228.932923	12.631872
20.997625	1235.098544	12.636877
20.758081	1219.399627	12.641882
20.949106	1233.831159	12.646887
21.150046	1241.731133	12.651891
21.352392	1234.845698	12.656896
20.969666	1238.912509	12.661901
20.708045	1238.404384	12.666906
21.213612	1246.052783	12.671911
20.978607	1251.026262	12.676915
21.211170	1249.294170	12.681920
20.929299	1262.648234	12.686925
20.884978	1257.573542	12.691930
21.347070	1264.299779	12.696935
21.148947	1267.371371	12.701939
21.589340	1253.798782	12.706944
21.266115	1239.630014	12.711949
21.175688	1246.109129	12.716954
20.897661	1232.815267	12.721959
20.941729	1237.655628	12.726963
20.900354	1231.800818	12.731968
20.861982	1246.703545	12.736973
21.246751	1249.653876	12.741978
21.336132	1250.869816	12.746983
20.906470	1257.976323	12.751987
20.816604	1244.224260	12.756992
21.319530	1258.438123	12.761997
21.235089	1262.093393	12.767002
21.336833	1252.265398	12.772007
20.734510	1244.036448	12.777011
21.126242	1235.474823	12.782016
20.535017	1248.715335	12.787021
21.181399	1257.001582	12.792026
21.236310	1259.027530	12.797031
21.302612	1266.218348	12.802035
21.458503	1266.130095	12.807040
21.201989	1252.437783	12.812045
21.170675	1245.753462	12.817050
20.905862	1240.150121	12.822055
20.869645	1241.057195	12.827059
20.968341	1239.530429	12.832064
20.894092	1255.293938	12.837069
21.260780	1261.613365	12.842074
21.671150	1264.218249	12.847079
21.141891	1259.329337	12.852083
21.218440	1244.268186	12.857088
20.910199	1244.879262	12.862093
20.797360	1249.916664	12.867098
21.184418	1248.757306	12.872103
20.697528	1255.439009	12.877107
21.081959	1258.740723	12.882112
21.259466	1265.304171	12.887117
21.277463	1260.471825	12.892122
20.959910	1249.884390	12.897127
21.001643	1247.369475	12.902131
20.991696	1240.508594	12.907136
21.351013	1262.801067	12.912141
21.471890	1257.140275	12.917146
21.530089	1248.898729	12.922151
21.120077	1252.181916	12.927155
21.608202	1246.534740	12.932160
21.251420	1245.890955	12.937165
21.564186	1240.367798	12.942170
21.485428	1233.971491	12.947175
21.037933	1238.945478	12.952179
21.471074	1233.477474	12.957184
21.003281	1217.789667	12.962189
20.752347	1221.591109	12.967194
20.688477	1226.914982	12.972199
20.832226	1242.659654	12.977203
21.057913	1245.739499	12.982208
20.928836	1251.672994	12.987213
20.780832	1251.687768	12.992218
20.919079	1243.413158	12.997223
20.873264	1247.168779	13.002227
20.982873	1246.726874	13.007232
21.117459	1242.079416	13.012237
21.047105	1244.732378	13.017242
21.298581	1249.903504	13.022247
21.203584	1250.971843	13.027251
21.271090	1255.377918	13.032256
21.353532	1248.045657	13.037261
21.250396	1254.399451	13.042266
21.299414	1253.180419	13.047271
21.201160	1256.140936	13.052275
21.041100	1256.000669	13.057280
21.070414	1260.450005	13.062285
20.878007	1256.783497	13.067290
21.002182	1249.168943	13.072295
20.862505	1255.786771	13.077299
20.968455	1257.685149	13.082304
21.067004	1254.940223	13.087309
20.786587	1261.125859	13.092314
21.502532	1250.029635	13.097319
21.175647	1262.710877	13.102323
21.394005	1257.353904	13.107328
21.251515	1262.307972	13.112333
21.232264	1260.733136	13.117338
21.282996	1258.839189	13.122343
21.098203	1262.377058	13.127347
21.120655	1260.725202	13.132352
21.197534	1259.579551	13.137357
21.187888	1257.065548	13.142362
21.169549	1260.516849	13.147367
21.016619	1262.867782	13.152371
21.121951	1261.538828	13.157376
21.258984	1261.671707	13.162381
20.983810	1261.996845	13.167386
21.348063	1252.623193	13.172391
20.777918	1247.217469	13.177395
20.796453	1248.296737	13.182400
20.835648	1261.321403	13.187405
21.158755	1261.432641	13.192410
21.297633	1264.697510	13.197415
21.098965	1259.463356	13.202419
21.090916	1257.735018	13.207424
21.095312	1264.540125	13.212429
21.222118	1264.472254	13.217434
21.711183	1264.769384	13.222439
21.467226	1254.634732	13.227443
21.191641	1238.602099	13.232448
21.075261	1239.073698	13.237453
20.925421	1237.385068	13.242458
21.064618	1236.001361	13.247463
20.729997	1233.014124	13.252467
20.948579	1237.728245	13.257472
20.897739	1242.050395	13.262477
20.848638	1245.819605	13.267482
21.340277	1264.959854	13.272487
20.990148	1269.452540	13.277491
21.179003	1264.427473	13.282496
21.394695	1269.516712	13.287501
21.015095	1256.834338	13.292506
21.275686	1242.588757	13.297511
21.237220	1240.814714	13.302515
21.421984	1245.193180	13.307520
21.475050	1238.001359	13.312525
21.196920	1232.872419	13.317530
21.380759	1224.715926	13.322535
20.992647	1235.182864	13.327539
21.033033	1237.911971	13.332544
20.920694	1231.460632	13.337549
21.180752	1238.683744	13.342554
21.246422	1242.507882	13.347559
21.342996	1241.794654	13.352563
21.290504	1238.687988	13.357568
20.939831	1236.316542	13.362573
20.866821	1245.397196	13.367578
21.260169	1238.072028	13.372583
21.085254	1237.854569	13.377587
21.141828	1237.200306	13.382592
20.809517	1249.614831	13.387597
21.026150	1245.269101	13.392602
21.252554	1237.010564	13.397607
20.873229	1247.618506	13.402611
20.746190	1241.014944	13.407616
20.738470	1244.072834	13.412621
20.897981	1244.585551	13.417626
21.031225	1242.290608	13.422631
20.749299	1250.123375	13.427635
20.762838	1245.477328	13.432640
21.036544	1270.784948	13.437645
21.047165	1283.053856	13.442650
21.190891	1275.128430	13.447655
21.290024	1278.866310	13.452659
21.230276	1277.463420	13.457664
21.320735	1267.275369	13.462669
20.758802	1253.591606	13.467674
21.494653	1251.416765	13.472679
20.850525	1255.113523	13.477683
21.044866	1246.740871	13.482688
21.259185	1246.062324	13.487693
21.162239	1245.599387	13.492698
21.402384	1254.802804	13.497703
21.213779	1249.700747	13.502707
21.607482	1244.240291	13.507712
21.427851	1259.177119	13.512717
21.368345	1242.991378	13.517722
21.056108	1237.644465	13.522727
20.748819	1244.020627	13.527731
20.787418	1246.575565	13.532736
20.915329	1238.105357	13.537741
20.655844	1241.729451	13.542746
21.090216	1235.673855	13.547751
20.714855	1249.726452	13.552755
20.908875	1246.646599	13.557760
20.964973	1256.964754	13.562765
21.210234	1275.556326	13.567770
21.570034	1275.174157	13.572775
20.818245	1258.110761	13.577779
20.803510	1249.213022	13.582784
20.665914	1265.652154	13.587789
20.996127	1275.339099	13.592794
21.307918	1280.904112	13.597799
21.279832	1285.828703	13.602803
21.278780	1286.312503	13.607808
21.005647	1275.854806	13.612813
20.915421	1288.435885	13.617818
20.994838	1285.526466	13.622823
21.038782	1298.242446	13.627827
21.714902	1290.466524	13.632832
21.515201	1276.386283	13.637837
21.156581	1263.309508	13.642842
21.246715	1256.977393	13.647847
21.124425	1260.155985	13.652851
20.906114	1250.407737	13.657856
20.769244	1255.016226	13.662861
20.598526	1264.136933	13.667866
21.034000	1269.868635	13.672871
20.896243	1280.143463	13.677875
21.235731	1280.103074	13.682880
21.517578	1289.712266	13.687885
21.141973	1274.500449	13.692890
21.061841	1263.778742	13.697895
20.767243	1261.659788	13.702899
20.976366	1276.060230	13.707904
21.180170	1284.745278	13.712909
21.132994	1293.446522	13.717914
21.556493	1279.681013	13.722919
21.551154	1278.171686	13.727923
21.251297	1269.121898	13.732928
21.017734	1267.265642	13.737933
20.879163	1267.402354	13.742938
21.265403	1258.834157	13.747943
21.245884	1265.834028	13.752947
21.112004	1265.109785	13.757952
20.886516	1267.357104	13.762957
20.781734	1267.876453	13.767962
20.978275	1266.261459	13.772967
20.801290	1261.172801	13.777971
21.127216	1252.688766	13.782976
20.916862	1259.555167	13.787981
21.074774	1279.951102	13.792986
21.366074	1283.886172	13.797991
20.686109	1278.452686	13.802995
21.286886	1284.398819	13.808000
21.321380	1283.402148	13.813005
21.017165	1282.718558	13.818010
21.214944	1265.614712	13.823015
21.166532	1266.417296	13.828019
21.193137	1264.720911	13.833024
21.138517	1266.760903	13.838029
21.110316	1264.169947	13.843034
21.382044	1262.681802	13.848039
21.187986	1268.404598	13.853043
21.456646	1265.317864	13.858048
21.422414	1266.419603	13.863053
20.864553	1271.392391	13.868058
21.161438	1264.303229	13.873063
21.176740	1269.320245	13.878067
21.189427	1268.368368	13.883072
21.335815	1262.977153	13.888077
21.245826	1266.708772	13.893082
21.163901	1261.267492	13.898087
20.999324	1275.339236	13.903091
21.135670	1269.786316	13.908096
21.215997	1272.705164	13.913101
20.849135	1275.001988	13.918106
21.194045	1269.467782	13.923111
21.119120	1271.999557	13.928115
20.874195	1272.944390	13.933120
21.086231	1272.840589	13.938125
21.127372	1270.422484	13.943130
20.971422	1266.458006	13.948135
20.945974	1276.674890	13.953139
21.177456	1274.336651	13.958144
21.196811	1268.888266	13.963149
21.337736	1274.177436	13.968154
21.469506	1270.911668	13.973159
21.378882	1270.641071	13.978163
21.181257	1261.905344	13.983168
20.951024	1246.034668	13.988173
20.661566	1253.425824	13.993178
20.961840	1263.946465	13.998183
21.042450	1274.927155	14.003187
20.621577	1270.159791	14.008192
20.935749	1273.583958	14.013210
20.816201	1274.195120	14.018227
21.158670	1273.918718	14.023245
21.074620	1274.106037	14.028263
21.028136	1270.098715	14.033280
20.938475	1266.325985	14.038298
21.227019	1270.268289	14.043315
21.546871	1264.960243	14.048333
21.118143	1279.486381	14.053351
21.579024	1279.377884	14.058368
21.376512	1277.876687	14.063386
21.194433	1282.163492	14.068403
21.426183	1273.740718	14.073421
21.284136	1277.125296	14.078439
21.157892	1265.194273	14.083456
21.016985	1277.556684	14.088474
21.230504	1271.354181	14.093491
21.463884	1270.527531	14.098509
21.067935	1264.305896	14.103527
20.866762	1265.411020	14.108544
21.296655	1280.779012	14.113562
21.263266	1302.463678	14.118579
21.541661	1294.623505	14.123597
21.388758	1305.509897	14.128615
21.574867	1312.238945	14.133632
21.693321	1307.882043	14.138650
21.591154	1311.713772	14.143667
21.788877	1302.605017	14.148685
21.949459	1311.584725	14.153703
21.711154	1312.071354	14.158720
22.175366	1305.480151	14.163738
21.340987	1290.923797	14.168755
21.911081	1284.472338	14.173773
21.711705	1280.774720	14.178791
21.556680	1280.177281	14.183808
21.536572	1279.981552	14.188826
21.687492	1298.648102	14.193843
21.728154	1293.609985	14.198861
21.520707	1306.936284	14.203879
21.281079	1308.468124	14.208896
21.388292	1311.077221	14.213914
21.350385	1313.725770	14.218931
21.468392	1311.004144	14.223949
21.627750	1312.413239	14.228967
21.896517	1316.605033	14.233984
21.946264	1333.430914	14.239002
21.783130	1344.639986	14.244019
21.961646	1341.146092	14.249037
21.695037	1350.165995	14.254055
21.654956	1351.315559	14.259072
21.906060	1342.967784	14.264090
21.863046	1356.867960	14.269107
22.069272	1344.302647	14.274125
22.185584	1352.457209	14.279143
21.958017	1346.099967	14.284160
21.866773	1348.239897	14.289178
21.659388	1347.091533	14.294195
22.347538	1340.228431	14.299213
21.811489	1341.614228	14.304231
21.618522	1344.662635	14.309248
21.996113	1347.253335	14.314266
22.011951	1366.886136	14.319283
22.865841	1372.043478	14.324301
22.242411	1355.001825	14.329319
22.372987	1350.972393	14.334336
22.360840	1345.903153	14.339354
21.987468	1347.491002	14.344371
22.193876	1346.793002	14.349389
22.217587	1346.349184	14.354407
22.479379	1361.589763	14.359424
22.642385	1358.751347	14.364442
22.392407	1352.636158	14.369459
21.983551	1340.406649	14.374477
22.150570	1352.254857	14.379495
22.213401	1361.079684	14.384512
22.772940	1369.025175	14.389530
22.537250	1383.282853	14.394547
22.717923	1377.640722	14.399565
22.745109	1384.074182	14.404583
22.681511	1366.532943	14.409600
22.575917	1354.785732	14.414618
22.274704	1354.724036	14.419635
22.440923	1370.663363	14.424653
22.356352	1374.993717	14.429671
22.494085	1379.931692	14.434688
22.520680	1370.323838	14.439706
22.640522	1386.073474	14.444723
22.744870	1377.686270	14.449741
22.754821	1381.475562	14.454759
22.636317	1380.662386	14.459776
23.012070	1373.578395	14.464794
23.055042	1381.336843	14.469811
23.234428	1380.362343	14.474829
23.302185	1373.255957	14.479847
23.470601	1363.019398	14.484864
23.593685	1350.211616	14.489882
22.966669	1346.108518	14.494899
23.115019	1340.711730	14.499917
23.433961	1337.265814	14.504935
23.050723	1345.969851	14.509952
22.962170	1337.160973	14.514970
23.022011	1343.806163	14.519987
22.895879	1340.329855	14.525005
22.603543	1338.641277	14.530023
22.300849	1348.173322	14.535040
22.572627	1346.207293	14.540058
22.415768	1341.996021	14.545075
22.566890	1345.499262	14.550093
23.268358	1363.198964	14.555111
22.952585	1380.563206	14.560128
23.473771	1371.531641	14.565146
23.364379	1382.954383	14.570163
23.436683	1364.644492	14.575181
23.313390	1352.233320	14.580199
22.506479	1352.928084	14.585216
23.189229	1354.731349	14.590234
23.230060	1372.444718	14.595251
23.179999	1373.695610	14.600269
23.215951	1382.345512	14.605287
22.870282	1381.578766	14.610304
23.250029	1380.426591	14.615322
23.128573	1382.647698	14.620339
23.394944	1381.047197	14.625357
23.044096	1376.143512	14.630375
22.967680	1380.421282	14.635392
23.056214	1374.107084	14.640410
23.017072	1378.626127	14.645427
23.802808	1393.268975	14.650445
23.731683	1399.913807	14.655463
23.669105	1382.424743	14.660480
23.491376	1382.353293	14.665498
23.504519	1382.264472	14.670515
23.265961	1387.603617	14.675533
23.715041	1379.502222	14.680551
23.551960	1399.256302	14.685568
23.834538	1400.261167	14.690586
23.744294	1403.280553	14.695603
23.927393	1391.729116	14.700621
23.818454	1382.172843	14.705639
23.486946	1389.665154	14.710656
23.494036	1371.746791	14.715674
23.794212	1385.071560	14.720691
23.338981	1393.573378	14.725709
23.837344	1393.560827	14.730727
23.746749	1406.539581	14.735744
23.983616	1393.724461	14.740762
23.407372	1406.955006	14.745779
23.815317	1400.947093	14.750797
23.975269	1397.623710	14.755815
23.883193	1406.614113	14.760832
23.851982	1404.069647	14.765850
23.761747	1403.879247	14.770867
24.129900	1407.996540	14.775885
24.050896	1398.937932	14.780903
23.758404	1409.304572	14.785920
23.870590	1405.020379	14.790938
23.848921	1398.242338	14.795955
24.266687	1401.640418	14.800973
24.344438	1395.049291	14.805991
24.007438	1399.518612	14.811008
24.077335	1402.589683	14.816026
23.888742	1398.209015	14.821043
24.006331	1405.549521	14.826061
24.263674	1397.019527	14.831079
24.055073	1402.023585	14.836096
24.247020	1407.421219	14.841114
24.072286	1414.314161	14.846131
24.279197	1426.596972	14.851149
24.466912	1421.792683	14.856167
24.399631	1432.197897	14.861184
24.153976	1412.819513	14.866202
24.365845	1416.951791	14.871219
24.746745	1418.372129	14.876237
24.813271	1402.426426	14.881255
24.250334	1401.402806	14.886272
24.220372	1391.532561	14.891290
24.585130	1387.693305	14.896307
24.305064	1392.651339	14.901325
24.630434	1399.921568	14.906343
24.328446	1404.384494	14.911360
24.457554	1413.125537	14.916378
24.823872	1422.580325	14.921395
24.942140	1412.116481	14.926413
24.811503	1402.203641	14.931431
24.590691	1396.630341	14.936448
24.845670	1389.446172	14.941466
24.785681	1396.632851	14.946483
24.506957	1397.320526	14.951501
24.740582	1384.627242	14.956519
24.761399	1396.876970	14.961536
24.597234	1394.465155	14.966554
24.772598	1390.001218	14.971571
24.956237	1394.088325	14.976589
25.034729	1392.444832	14.981607
24.749496	1402.675564	14.986624
24.832637	1390.953451	14.991642
24.810149	1388.452772	14.996659
24.571335	1405.041956	15.001677
24.859790	1416.157901	15.006695
24.887036	1425.216842	15.011712
24.584999	1427.677208	15.016730
24.701920	1425.326654	15.021747
24.829022	1425.923881	15.026765
25.261784	1422.899423	15.031783
24.799022	1430.184312	15.036800
24.922575	1424.175934	15.041818
25.146656	1425.782625	15.046835
25.166387	1439.357910	15.051853
25.693870	1427.826147	15.056871
25.459472	1429.254335	15.061888
24.904253	1428.996795	15.066906
25.297092	1421.435787	15.071923
24.970946	1428.627953	15.076941
24.769947	1424.988460	15.081959
25.053900	1437.494709	15.086976
24.934321	1428.082373	15.091994
25.040849	1441.478586	15.097011
25.490696	1459.223115	15.102029
25.671405	1449.696280	15.107047
25.646473	1455.850487	15.112064
25.827986	1447.183057	15.117082
25.303557	1434.941395	15.122099
25.633809	1434.817103	15.127117
25.253347	1425.247115	15.132135
25.206837	1430.543896	15.137152
25.591232	1436.098328	15.142170
25.471127	1434.831044	15.147187
25.868961	1455.333600	15.152205
25.308289	1441.286140	15.157223
25.402860	1442.284263	15.162240
25.340740	1453.337495	15.167258
25.766681	1456.177433	15.172275
25.415885	1462.212692	15.177293
25.620292	1458.159942	15.182311
25.647433	1461.148188	15.187328
25.845164	1459.863025	15.192346
25.605072	1459.372693	15.197363
25.233292	1463.170756	15.202381
25.625777	1459.343661	15.207399
25.620960	1463.939135	15.212416
25.711460	1464.395378	15.217434
26.061037	1456.240919	15.222451
25.671216	1458.293067	15.227469
25.830563	1453.334166	15.232487
25.946292	1462.855175	15.237504
25.787097	1475.919378	15.242522
26.219976	1470.806081	15.247539
26.402815	1483.137163	15.252557
25.937638	1462.121762	15.257575
26.229599	1465.531977	15.262592
26.072264	1459.162646	15.267610
26.435397	1452.357979	15.272627
25.910375	1456.668982	15.277645
26.035641	1458.771412	15.282663
25.982874	1456.453098	15.287680
26.026311	1482.361126	15.292698
26.279337	1478.300429	15.297715
26.068824	1484.599471	15.302733
26.399059	1480.987397	15.307751
26.334722	1481.659186	15.312768
26.190740	1491.166074	15.317786
26.547447	1490.103284	15.322803
26.579972	1486.850949	15.327821
26.552208	1474.769007	15.332839
26.176076	1476.529408	15.337856
26.425328	1484.577772	15.342874
26.637124	1483.392174	15.347891
26.728620	1491.606582	15.352909
26.645642	1469.554273	15.357927
26.363606	1458.640079	15.362944
26.214669	1456.320930	15.367962
26.552807	1468.536387	15.372979
26.616178	1483.414213	15.377997
26.931393	1475.720409	15.383015
26.996729	1483.627453	15.388032
26.107112	1468.529949	15.393050
26.457707	1472.413628	15.398067
26.817510	1488.232080	15.403085
26.944353	1481.394284	15.408103
26.934875	1485.542877	15.413120
26.820442	1477.758548	15.418138
26.971319	1457.673859	15.423155
26.916448	1451.670863	15.428173
26.832894	1448.387646	15.433191
26.905939	1454.359680	15.438208
26.448700	1460.778977	15.443226
27.055531	1466.433091	15.448243
27.039736	1485.744265	15.453261
26.968954	1482.440739	15.458279
26.743227	1480.953739	15.463296
26.528527	1493.915651	15.468314
26.870339	1488.580928	15.473331
27.103299	1493.036419	15.478349
26.851325	1494.091206	15.483367
27.002683	1502.515853	15.488384
26.330007	1494.398836	15.493402
26.775450	1486.228318	15.498419
26.644260	1491.210075	15.503437
26.929934	1507.984274	15.508455
27.210911	1513.341087	15.513472
27.161689	1511.882096	15.518490
27.254969	1508.285443	15.523507
27.458927	1517.538968	15.528525
27.368424	1512.640212	15.533543
27.810350	1514.755686	15.538560
27.428250	1519.323728	15.543578
27.291469	1511.526676	15.548595
27.479421	1509.882122	15.553613
27.487179	1507.406950	15.558631
27.582988	1518.353613	15.563648
27.492047	1516.355650	15.568666
27.572833	1513.476574	15.573683
27.543884	1514.691965	15.578701
27.442124	1505.279283	15.583719
27.567330	1507.155326	15.588736
27.580368	1505.948288	15.593754
27.756750	1511.129706	15.598771
27.449538	1511.195429	15.603789
27.601955	1505.554159	15.608807
27.689731	1502.948326	15.613824
27.582855	1515.188147	15.618842
27.628530	1499.840475	15.623859
27.467606	1500.024045	15.628877
27.498990	1506.809238	15.633895
27.636720	1505.047690	15.638912
27.609596	1498.384728	15.643930
27.706547	1497.216852	15.648947
27.829781	1501.441130	15.653965
27.817546	1504.174296	15.658983
27.777934	1513.556991	15.664000
27.814143	1536.518775	15.669018
28.310893	1537.213275	15.674035
28.026089	1545.826126	15.679053
28.007390	1535.507352	15.684071
28.234417	1525.146845	15.689088
27.853917	1531.124618	15.694106
27.911978	1542.226212	15.699123
28.184700	1538.204647	15.704141
28.264361	1541.024830	15.709159
28.286097	1538.301560	15.714176
28.136677	1542.783252	15.719194
28.361327	1536.504318	15.724211
28.384356	1536.616187	15.729229
28.200030	1546.212712	15.734247
28.355503	1528.592780	15.739264
28.393883	1540.436413	15.744282
28.475988	1533.641309	15.749299
28.214242	1535.118689	15.754317
28.421333	1542.502975	15.759335
28.173229	1538.809320	15.764352
28.071998	1544.572660	15.769370
28.518169	1543.294505	15.774387
28.360649	1546.148268	15.779405
28.180015	1544.878754	15.784423
28.353797	1539.460212	15.789440
28.298814	1537.621454	15.794458
28.368958	1536.168375	15.799475
28.222265	1536.837750	15.804493
28.573393	1540.719781	15.809511
28.609152	1557.333316	15.814528
28.665097	1574.358417	15.819546
29.088805	1567.492521	15.824563
29.173356	1567.857257	15.829581
28.967909	1555.769494	15.834599
28.664928	1543.352360	15.839616
28.765017	1548.134226	15.844634
28.936391	1538.856997	15.849651
28.908631	1544.981405	15.854669
28.574352	1552.502618	15.859687
28.896702	1556.851057	15.864704
28.978058	1573.559559	15.869722
29.025836	1573.241151	15.874739
29.170124	1567.935543	15.879757
29.374808	1566.505856	15.884775
29.148085	1551.344618	15.889792
28.881829	1551.505693	15.894810
28.979605	1555.319737	15.899827
29.459495	1562.870276	15.904845
29.063457	1566.342170	15.909863
29.307715	1558.476613	15.914880
29.082199	1565.293279	15.919898
29.394351	1564.802755	15.924915
29.101697	1555.429861	15.929933
29.255428	1567.452185	15.934951
29.477810	1558.380791	15.939968
29.194371	1568.598329	15.944986
29.328803	1561.770616	15.950003
29.515293	1564.420107	15.955021
29.241092	1566.233522	15.960039
29.459834	1564.114731	15.965056
29.349943	1562.866553	15.970074
29.151032	1568.996691	15.975091
29.396994	1567.816648	15.980109
29.031957	1569.693675	15.985127
29.568878	1562.253975	15.990144
29.150935	1569.676930	15.995162
29.273301	1570.584459	16.000179
29.844934	1569.828948	16.005197
29.540064	1569.537142	16.010215
29.760304	1577.292856	16.015232
29.317386	1585.168183	16.020250
29.786585	1586.070976	16.025267
30.361576	1589.657127	16.030285
29.998344	1584.321589	16.035303
29.613241	1565.951683	16.040320
29.741261	1568.998646	16.045338
30.122543	1581.202070	16.050355
29.948315	1563.353162	16.055373
29.851373	1577.156075	16.060391
30.276127	1573.822690	16.065408
29.999017	1569.814672	16.070426
30.010727	1557.838904	16.075443
30.014087	1559.950436	16.080461
29.693821	1573.399859	16.085479
30.202578	1580.834028	16.090496
30.128684	1586.238325	16.095514
30.159472	1589.613023	16.100531
30.583908	1587.720802	16.105549
30.246638	1587.147903	16.110567
30.384054	1579.314042	16.115584
30.371464	1572.678481	16.120602
30.403864	1574.410977	16.125619
30.302383	1562.975144	16.130637
30.283493	1563.489128	16.135655
30.622144	1561.037931	16.140672
30.225328	1561.691524	16.145690
30.152741	1564.474816	16.150707
30.384263	1581.341065	16.155725
30.622544	1582.694522	16.160743
30.740910	1580.396854	16.165760
30.843418	1589.665059	16.170778
30.670914	1570.641695	16.175795
30.684222	1554.006063	16.180813
30.405910	1558.049570	16.185831
30.684840	1556.452018	16.190848
30.547162	1567.905338	16.195866
30.466273	1579.433586	16.200883
30.657803	1587.232027	16.205901
30.423462	1590.640765	16.210919
30.992304	1585.810454	16.215936
30.637416	1589.880486	16.220954
30.588342	1586.598021	16.225971
30.934108	1592.220557	16.230989
30.888411	1587.974409	16.236007
31.170898	1580.030231	16.241024
31.131586	1586.880735	16.246042
30.580938	1590.214164	16.251059
30.725784	1584.863568	16.256077
30.415813	1591.179704	16.261095
30.651474	1589.152508	16.266112
30.908330	1595.595502	16.271130
30.814358	1606.974814	16.276147
30.923997	1616.941895	16.281165
31.156802	1622.917315	16.286183
31.173175	1616.179120	16.291200
30.930067	1617.052452	16.296218
31.060583	1615.359066	16.301235
31.431549	1605.012022	16.306253
31.297138	1617.744496	16.311271
31.557144	1612.067417	16.316288
31.351655	1615.218427	16.321306
31.025158	1614.776767	16.326323
31.425991	1604.551388	16.331341
31.411231	1613.028201	16.336359
31.556957	1618.648033	16.341376
31.394655	1618.358162	16.346394
31.142474	1623.870609	16.351411
31.376622	1616.308367	16.356429
31.194092	1616.468868	16.361447
31.585863	1622.852122	16.366464
31.533382	1626.488379	16.371482
31.479315	1638.278638	16.376499
31.911589	1643.050827	16.381517
31.562696	1639.951663	16.386535
31.935081	1642.474401	16.391552
32.237341	1646.913723	16.396570
32.331273	1630.031087	16.401587
32.289639	1613.237470	16.406605
32.139333	1610.588965	16.411623
31.771286	1615.099895	16.416640
32.036057	1607.317420	16.421658
31.999790	1608.276169	16.426675
31.828072	1605.154508	16.431693
31.583777	1608.624019	16.436711
31.730581	1606.540394	16.441728
32.067310	1607.005612	16.446746
31.615186	1615.240449	16.451763
32.126730	1626.768347	16.456781
32.458381	1627.579752	16.461799
32.470911	1633.055084	16.466816
32.357818	1624.990891	16.471834
32.216163	1623.134302	16.476851
32.317419	1616.086243	16.481869
32.073941	1619.914319	16.486887
32.081321	1630.795506	16.491904
32.589959	1628.674645	16.496922
32.266681	1635.974694	16.501939
32.623212	1646.703102	16.506957
32.265255	1638.482043	16.511975
32.230253	1642.956352	16.516992
32.455532	1634.134447	16.522010
32.208808	1631.536333	16.527027
32.831107	1640.787503	16.532045
32.465627	1638.052250	16.537063
32.263639	1642.608739	16.542080
32.218637	1634.273780	16.547098
32.363276	1638.665313	16.552115
32.250252	1635.929299	16.557133
32.333350	1638.817817	16.562151
32.461994	1656.738919	16.567168
32.663676	1666.255158	16.572186
33.028440	1668.345690	16.577203
33.113537	1657.180985	16.582221
32.800152	1659.556313	16.587239
32.825644	1661.689265	16.592256
33.240229	1669.619996	16.597274
33.056545	1661.779724	16.602291
33.313887	1653.271641	16.607309
33.159708	1637.474971	16.612327
32.941366	1636.770248	16.617344
33.033213	1632.633591	16.622362
32.731449	1653.191784	16.627379
32.610007	1654.103714	16.632397
33.027830	1656.967919	16.637415
33.059546	1663.570817	16.642432
33.198612	1654.517984	16.647450
33.075501	1659.075917	16.652467
33.534237	1660.988111	16.657485
33.752787	1666.519875	16.662503
33.190780	1658.450340	16.667520
33.464531	1650.005595	16.672538
33.580153	1661.136386	16.677555
33.084226	1651.849080	16.682573
33.304993	1650.344571	16.687591
33.140493	1657.376039	16.692608
33.380459	1654.584618	16.697626
33.343709	1658.830858	16.702643
33.594208	1662.130495	16.707661
33.599250	1672.558906	16.712679
33.509847	1677.811544	16.717696
34.353694	1672.867118	16.722714
34.098755	1665.456828	16.727731
33.964699	1658.795594	16.732749
34.069512	1647.316848	16.737767
33.960981	1653.270872	16.742784
33.936879	1653.212848	16.747802
33.672793	1656.944849	16.752819
33.911626	1657.149261	16.757837
33.605232	1646.852570	16.762855
33.443536	1646.440927	16.767872
33.434121	1653.529277	16.772890
33.785495	1668.718179	16.777907
34.116564	1682.240687	16.782925
34.189105	1681.792032	16.787943
33.989311	1695.003947	16.792960
34.114022	1686.132319	16.797978
33.865156	1689.652243	16.802995
34.085301	1682.540063	16.808013
33.974482	1682.374451	16.813031
33.708618	1690.397448	16.818048
34.085938	1677.141429	16.823066
33.915545	1692.462339	16.828083
34.237430	1685.227190	16.833101
34.127663	1696.727399	16.838119
34.209893	1710.039810	16.843136
34.741972	1709.640725	16.848154
34.480932	1715.146847	16.853171
34.552676	1715.587414	16.858189
34.541827	1710.947414	16.863207
34.490717	1717.777554	16.868224
34.904444	1715.670593	16.873242
34.922698	1716.468013	16.878259
34.682633	1710.485645	16.883277
34.786464	1713.437559	16.888295
34.772307	1706.620297	16.893312
34.844945	1698.515558	16.898330
34.719321	1699.369539	16.903347
34.720869	1708.062926	16.908365
35.349630	1712.650248	16.913383
34.984715	1708.252080	16.918400
35.189073	1687.354285	16.923418
34.812279	1694.244981	16.928435
35.011873	1689.832717	16.933453
34.687208	1689.480515	16.938471
35.082250	1699.387690	16.943488
35.120722	1702.625251	16.948506
35.095392	1709.701000	16.953523
35.071074	1721.632695	16.958541
34.974711	1718.256330	16.963559
34.734840	1722.206663	16.968576
34.986552	1719.037186	16.973594
34.911835	1729.199354	16.978611
34.772065	1720.489998	16.983629
35.070144	1725.838834	16.988647
34.637068	1729.488001	16.993664
34.914354	1747.167552	16.998682
34.906280	1753.502079	17.003699
35.309609	1750.373538	17.008717
35.127995	1745.624599	17.013735
35.430399	1754.648760	17.018752
35.640323	1749.445238	17.023770
35.328662	1747.444139	17.028787
35.390842	1758.220730	17.033805
35.662912	1771.821944	17.038823
35.830704	1778.846499	17.043840
36.037951	1772.746856	17.048858
35.752821	1759.786262	17.053875
36.062221	1755.494541	17.058893
35.809142	1748.935576	17.063911
35.785322	1747.971089	17.068928
36.002276	1746.018350	17.073946
35.753590	1744.786867	17.078963
35.609214	1751.843277	17.083981
35.923125	1748.864336	17.088999
35.837393	1771.721767	17.094016
35.915173	1774.361977	17.099034
35.704541	1780.183930	17.104051
35.912429	1777.746852	17.109069
36.249531	1770.310603	17.114087
36.135707	1777.730337	17.119104
36.460694	1768.357335	17.124122
36.361056	1770.102254	17.129139
36.067353	1773.324334	17.134157
36.274983	1771.917748	17.139175
36.028907	1775.360825	17.144192
36.290847	1775.230919	17.149210
36.318904	1776.034536	17.154227
36.302478	1772.654297	17.159245
36.647671	1771.813965	17.164263
36.456421	1784.060193	17.169280
36.498773	1778.384147	17.174298
36.323126	1777.214952	17.179315
36.454406	1790.668646	17.184333
36.735843	1772.184215	17.189351
36.609037	1778.661566	17.194368
36.553668	1773.089295	17.199386
36.513495	1777.408997	17.204403
36.836261	1789.617893	17.209421
36.585294	1783.053432	17.214439
36.820153	1798.712102	17.219456
37.015405	1801.041586	17.224474
37.261816	1794.883639	17.229491
37.290515	1781.612098	17.234509
37.295071	1763.219250	17.239527
37.008070	1766.351191	17.244544
37.287351	1758.965025	17.249562
37.167991	1756.556890	17.254579
37.112373	1761.267080	17.259597
37.315897	1753.142235	17.264615
37.199471	1762.426424	17.269632
37.524778	1759.123439	17.274650
37.467309	1758.330097	17.279667
37.031718	1757.471254	17.284685
37.207642	1753.294556	17.289703
36.970484	1762.076938	17.294720
37.078578	1763.367289	17.299738
37.296575	1756.320807	17.304755
36.782669	1762.114426	17.309773
37.440234	1772.124687	17.314791
37.307398	1796.046270	17.319808
37.574967	1794.900701	17.324826
37.418184	1797.903614	17.329843
37.741912	1802.746046	17.334861
37.613461	1797.973014	17.339879
37.686236	1795.733925	17.344896
37.542215	1792.663391	17.349914
37.768446	1789.599857	17.354931
37.575861	1790.603530	17.359949
38.019745	1782.762304	17.364967
37.802976	1792.765774	17.369984
37.972873	1791.810596	17.375002
37.935647	1784.634610	17.380019
37.551285	1792.915015	17.385037
38.031062	1787.891619	17.390055
37.913032	1786.342811	17.395072
37.913493	1782.782486	17.400090
38.288680	1784.436152	17.405107
37.995538	1782.969344	17.410125
38.230684	1789.567735	17.415143
38.104089	1793.806184	17.420160
38.182737	1797.529854	17.425178
38.274371	1793.880263	17.430195
37.887979	1795.489288	17.435213
38.502156	1784.641704	17.440231
38.270639	1789.348987	17.445248
38.044176	1793.588021	17.450266
38.545748	1780.310218	17.455283
38.260456	1786.602120	17.460301
38.404429	1789.613710	17.465319
38.531834	1802.071493	17.470336
38.476984	1807.695071	17.475354
38.817172	1795.590744	17.480371
38.554730	1807.845260	17.485389
38.601619	1797.052801	17.490407
38.644722	1803.501424	17.495424
38.468222	1802.982852	17.500442
38.807378	1795.956529	17.505459
38.859309	1794.461267	17.510477
38.991939	1786.539923	17.515495
39.089694	1791.671128	17.520512
39.108014	1797.002592	17.525530
39.287997	1797.224972	17.530547
39.336029	1797.963346	17.535565
39.106698	1788.011269	17.540583
39.616324	1793.853455	17.545600
38.890951	1784.655808	17.550618
39.011349	1773.055778	17.555635
38.941533	1772.435439	17.560653
39.055097	1778.381751	17.565671
39.098371	1790.162916	17.570688
39.497266	1792.809104	17.575706
39.391537	1790.197813	17.580723
39.089778	1796.352760	17.585741
39.590854	1791.819083	17.590759
39.495913	1785.485383	17.595776
39.519643	1789.650807	17.600794
39.449968	1784.821238	17.605811
39.228072	1792.205171	17.610829
39.983653	1786.021352	17.615847
39.801854	1788.576526	17.620864
39.796970	1788.959358	17.625882
39.964764	1772.018230	17.630899
39.441611	1773.275850	17.635917
39.755347	1775.847254	17.640935
40.221055	1788.953808	17.645952
39.460434	1783.145714	17.650970
39.883964	1781.861973	17.655987
39.919902	1782.548870	17.661005
39.835763	1789.089785	17.666023
39.830435	1786.469549	17.671040
39.681768	1801.300164	17.676058
39.531676	1791.925521	17.681075
39.744421	1783.893185	17.686093
39.536851	1788.425079	17.691111
39.731609	1791.029880	17.696128
39.614823	1816.674557	17.701146
39.797652	1809.071803	17.706163
39.731064	1818.419931	17.711181
40.028370	1814.887059	17.716199
40.195118	1817.108426	17.721216
40.180717	1825.200203	17.726234
40.378633	1823.977979	17.731251
40.074187	1846.982877	17.736269
40.499170	1848.454367	17.741287
40.520923	1845.708202	17.746304
40.425236	1859.678888	17.751322
40.950816	1856.212788	17.756339
40.517259	1856.093846	17.761357
40.522998	1851.245814	17.766375
40.848393	1846.701293	17.771392
40.517956	1842.774010	17.776410
40.874867	1838.731635	17.781427
40.920404	1848.683473	17.786445
40.945620	1848.999721	17.791463
41.439723	1850.886583	17.796480
41.014970	1842.857599	17.801498
40.855225	1837.561897	17.806515
40.818916	1840.657564	17.811533
41.025848	1844.152530	17.816551
41.238823	1838.331839	17.821568
40.983822	1841.703616	17.826586
41.211470	1839.056814	17.831603
41.409175	1845.826631	17.836621
41.072640	1839.792634	17.841639
41.368166	1837.522829	17.846656
41.073434	1844.369595	17.851674
41.480429	1836.827618	17.856691
41.228266	1843.249314	17.861709
41.061936	1842.496288	17.866727
41.495839	1838.286361	17.871744
41.466101	1844.049366	17.876762
41.170113	1832.186781	17.881779
41.040675	1845.043801	17.886797
41.100376	1849.673608	17.891815
41.466334	1860.687595	17.896832
41.613725	1871.147645	17.901850
41.937594	1871.793841	17.906867
41.667766	1880.692142	17.911885
41.537377	1882.845944	17.916903
42.016254	1873.930418	17.921920
41.691331	1875.866752	17.926938
41.947722	1874.250982	17.931955
41.699554	1874.619616	17.936973
41.712797	1873.102630	17.941991
41.645780	1861.208246	17.947008
41.854576	1880.735765	17.952026
41.670689	1866.316584	17.957043
42.110877	1877.671840	17.962061
42.163824	1900.844704	17.967079
42.546514	1902.489222	17.972096
42.096196	1904.430521	17.977114
42.319272	1894.971359	17.982131
42.411286	1896.181790	17.987149
41.971070	1899.595179	17.992167
42.484535	1894.360435	17.997184
41.924266	1896.715127	18.002202
42.233991	1891.628323	18.007219
42.451609	1891.557992	18.012237
42.227076	1899.575977	18.017255
42.361326	1903.105075	18.022272
41.783836	1907.425981	18.027290
42.386345	1918.592391	18.032307
42.440760	1936.505278	18.037325
42.427017	1936.249387	18.042343
42.814135	1931.983668	18.047360
42.723368	1936.580630	18.052378
42.754556	1928.806152	18.057395
42.598264	1930.579309	18.062413
42.663941	1929.030884	18.067431
42.982351	1939.549860	18.072448
42.897042	1953.292833	18.077466
43.381862	1950.237695	18.082483
43.455630	1950.173915	18.087501
43.493243	1945.927561	18.092519
43.655779	1920.501348	18.097536
43.422518	1920.968622	18.102554
43.258742	1916.822168	18.107571
43.475703	1917.909589	18.112589
43.304368	1918.984834	18.117607
43.514950	1908.803297	18.122624
43.214902	1917.786732	18.127642
43.444482	1916.531510	18.132659
43.381758	1919.864037	18.137677
43.444997	1916.896150	18.142695
43.601837	1923.749790	18.147712
43.478812	1938.711589	18.152730
43.839151	1936.195979	18.157747
43.704550	1941.053643	18.162765
43.594771	1946.652825	18.167783
44.002346	1940.318349	18.172800
43.859931	1936.083963	18.177818
43.794387	1946.723506	18.182835
43.950948	1940.896699	18.187853
44.092826	1948.688478	18.192871
44.274599	1939.815586	18.197888
43.973114	1939.948840	18.202906
44.053102	1938.609407	18.207923
44.240861	1939.840832	18.212941
43.984513	1943.809795	18.217959
44.187338	1940.589593	18.222976
44.368595	1947.039001	18.227994
44.216760	1947.170616	18.233011
44.065655	1947.951803	18.238029
44.137057	1948.915737	18.243047
44.599804	1948.471835	18.248064
44.196431	1947.664944	18.253082
44.670279	1945.421644	18.258099
44.506365	1942.120994	18.263117
44.396712	1952.321979	18.268135
44.518581	1943.292402	18.273152
44.074827	1946.146488	18.278170
44.375983	1941.265890	18.283187
44.831261	1948.783433	18.288205
44.588148	1950.273799	18.293223
44.839154	1959.061975	18.298240
44.779092	1977.053600	18.303258
44.893066	1973.596227	18.308275
45.119801	1974.576844	18.313293
44.581508	1982.612048	18.318311
44.891872	1976.083958	18.323328
45.115994	1985.179164	18.328346
44.813101	1974.980095	18.333363
45.388973	1967.080709	18.338381
44.973141	1970.608847	18.343399
45.165399	1973.973269	18.348416
45.064470	1971.433970	18.353434
45.239062	1977.117496	18.358451
45.319851	1971.210348	18.363469
45.115286	1978.050769	18.368487
45.539567	1972.454859	18.373504
45.411455	1977.066111	18.378522
45.333229	1971.926883	18.383539
45.778409	1977.810507	18.388557
45.858254	1996.183342	18.393575
45.939003	1978.832052	18.398592
45.662012	1976.841909	18.403610
45.864961	1973.277930	18.408627
46.074826	1971.859131	18.413645
45.604794	1974.253882	18.418663
45.734111	1974.554252	18.423680
45.810954	1969.033269	18.428698
45.671552	1969.019032	18.433715
46.458848	1988.649103	18.438733
45.939680	1991.828376	18.443751
46.120255	1982.056324	18.448768
45.941987	1982.607491	18.453786
46.189832	1992.032932	18.458803
46.408466	1991.868713	18.463821
46.285388	2006.747897	18.468839
46.081697	2002.515337	18.473856
46.778749	2003.883495	18.478874
45.858595	1992.712139	18.483891
46.100715	1987.321890	18.488909
46.158619	2008.738697	18.493927
46.290456	2001.067810	18.498944
46.581395	2005.121720	18.503962
46.149861	1996.641786	18.508979
46.090043	1992.692479	18.513997
46.079966	2011.809593	18.519015
46.143980	2019.973077	18.524032
46.605161	2020.311444	18.529050
46.236685	2028.782977	18.534067
46.767596	2033.725806	18.539085
46.632433	2033.999466	18.544103
47.074087	2027.811890	18.549120
46.696238	2028.751659	18.554138
46.646665	2046.990421	18.559155
47.135601	2052.735844	18.564173
46.907009	2055.708592	18.569191
47.130024	2051.784804	18.574208
47.471881	2049.319596	18.579226
47.453957	2056.356824	18.584243
47.663630	2051.236723	18.589261
47.425460	2050.505847	18.594279
47.838203	2050.415449	18.599296
47.893331	2030.019625	18.604314
47.148337	2025.569585	18.609331
47.437283	2017.785127	18.614349
46.990767	2026.089697	18.619367
47.278669	2045.132925	18.624384
47.799890	2050.701133	18.629402
47.345461	2051.340602	18.634419
47.634005	2048.319886	18.639437
47.535928	2055.838641	18.644455
47.575077	2052.781144	18.649472
47.660954	2056.423704	18.654490
47.586185	2057.869072	18.659507
47.889252	2064.643364	18.664525
47.723668	2074.255898	18.669543
47.914728	2080.239045	18.674560
48.090765	2082.461221	18.679578
47.968650	2078.782454	18.684595
48.124793	2074.233023	18.689613
48.007345	2080.740788	18.694631
47.977740	2080.389174	18.699648
47.992019	2088.329691	18.704666
48.452269	2083.694254	18.709683
48.293406	2081.044773	18.714701
47.959888	2078.729220	18.719719
48.222378	2091.216049	18.724736
48.703464	2097.837769	18.729754
48.589423	2112.284731	18.734771
48.748019	2105.458939	18.739789
48.681217	2105.219229	18.744807
48.847186	2106.556388	18.749824
49.050643	2103.826669	18.754842
48.341676	2109.497929	18.759859
48.873237	2106.114228	18.764877
48.883502	2108.790877	18.769895
49.116430	2102.474467	18.774912
48.882058	2103.655822	18.779930
48.980038	2104.940061	18.784947
48.898320	2106.687458	18.789965
48.712884	2107.707644	18.794983
48.748225	2104.189304	18.800000
49.247474	2100.070089	18.805018
49.066878	2105.420800	18.810035
49.477622	2096.700323	18.815053
49.018589	2112.458590	18.820071
48.965675	2112.267688	18.825088
49.071019	2113.262433	18.830106
49.008321	2131.092457	18.835123
49.247473	2139.314965	18.840141
49.554159	2139.331741	18.845159
49.584929	2137.305742	18.850176
49.576031	2135.620453	18.855194
49.616696	2141.773526	18.860211
49.777237	2136.156233	18.865229
49.888484	2135.396945	18.870247
49.721372	2133.099316	18.875264
50.027262	2129.210914	18.880282
49.935402	2125.230053	18.885299
50.268929	2126.606999	18.890317
49.952796	2134.855408	18.895335
50.094418	2137.451265	18.900352
50.256908	2140.705848	18.905370
50.332111	2142.305854	18.910387
50.529841	2123.007677	18.915405
50.405287	2130.852315	18.920423
49.944700	2134.419269	18.925440
50.087658	2136.588060	18.930458
50.351589	2155.047253	18.935475
50.600898	2155.552679	18.940493
50.520017	2160.024764	18.945511
50.538222	2157.542579	18.950528
50.956085	2155.618740	18.955546
50.492138	2159.800543	18.960563
50.556508	2162.954613	18.965581
51.014386	2156.330281	18.970599
50.918661	2165.237086	18.975616
51.008858	2154.506653	18.980634
51.022539	2159.038126	18.985651
51.003732	2150.474744	18.990669
50.988551	2157.031159	18.995687
50.661172	2154.672015	19.000704
51.059156	2144.040022	19.005722
50.938640	2152.955795	19.010739
50.960352	2158.103309	19.015757
50.972751	2155.469341	19.020775
50.751566	2158.397525	19.025792
50.973255	2155.851314	19.030810
51.275055	2163.116492	19.035827
51.635129	2178.923393	19.040845
51.627007	2169.031980	19.045863
51.527185	2165.129652	19.050880
51.964710	2153.552146	19.055898
51.234119	2149.943823	19.060915
51.465878	2162.501343	19.065933
51.560843	2168.675043	19.070951
51.716471	2182.489130	19.075968
52.047872	2183.257690	19.080986
51.911589	2186.660375	19.086003
51.998478	2183.179643	19.091021
52.030548	2179.025528	19.096039
51.986006	2185.005009	19.101056
52.268784	2179.067483	19.106074
52.065732	2187.597366	19.111091
52.095004	2180.651961	19.116109
52.286763	2176.794139	19.121127
52.080335	2184.047237	19.126144
52.280067	2181.374058	19.131162
52.371916	2181.404830	19.136179
52.007146	2178.009413	19.141197
52.233951	2180.977345	19.146215
52.083422	2183.752453	19.151232
52.663977	2179.339707	19.156250
52.045815	2182.753345	19.161267
52.192029	2181.268264	19.166285
52.332174	2188.022505	19.171303
52.418985	2199.041672	19.176320
52.986775	2193.199392	19.181338
52.914544	2206.296544	19.186355
52.585978	2198.220171	19.191373
52.965803	2195.772845	19.196391
52.754363	2201.510039	19.201408
53.176788	2195.398147	19.206426
52.962478	2200.531015	19.211443
52.977007	2195.787685	19.216461
52.745361	2198.423136	19.221479
52.882441	2212.378246	19.226496
53.039360	2223.438962	19.231514
52.969634	2229.544844	19.236531
52.980268	2231.343360	19.241549
53.185668	2230.469484	19.246567
52.868350	2231.717834	19.251584
53.205506	2230.161422	19.256602
53.596324	2250.529199	19.261619
53.586009	2265.211313	19.266637
53.724006	2255.566490	19.271655
53.523120	2258.894426	19.276672
53.739534	2252.839885	19.281690
53.828538	2259.098907	19.286707
53.771486	2251.114559	19.291725
54.053752	2246.117403	19.296743
53.766386	2254.075071	19.301760
53.945319	2252.715103	19.306778
54.242063	2256.623966	19.311795
54.096160	2248.870636	19.316813
54.100982	2251.007212	19.321831
53.937068	2269.105180	19.326848
54.302005	2254.863240	19.331866
54.073356	2250.558500	19.336883
53.715548	2261.216865	19.341901
54.502558	2253.692620	19.346919
54.578168	2282.803267	19.351936
54.875795	2282.499498	19.356954
54.780786	2278.012757	19.361971
54.604823	2274.257336	19.366989
55.014683	2261.943430	19.372007
54.729024	2254.528282	19.377024
54.883089	2246.106101	19.382042
54.549706	2260.185230	19.387059
54.565269	2272.092394	19.392077
54.924314	2275.888202	19.397095
55.558424	2283.669782	19.402112
55.539752	2270.266951	19.407130
55.390709	2254.964918	19.412147
55.101002	2246.172296	19.417165
55.261632	2237.711981	19.422183
55.006034	2246.271380	19.427200
55.376748	2267.543556	19.432218
55.174289	2267.657864	19.437235
55.053295	2276.815561	19.442253
55.366755	2273.775568	19.447271
55.178680	2283.096762	19.452288
55.346097	2276.496980	19.457306
55.394745	2274.552164	19.462323
54.995598	2274.974254	19.467341
55.403698	2281.786548	19.472359
55.857776	2304.111581	19.477376
55.662485	2303.113456	19.482394
55.672650	2298.271615	19.487411
55.844071	2303.183238	19.492429
55.998453	2300.194928	19.497447
55.982254	2307.334351	19.502464
56.069979	2295.878142	19.507482
56.278232	2289.410746	19.512499
55.813765	2295.795390	19.517517
56.230134	2291.041413	19.522535
55.929907	2297.865691	19.527552
56.049404	2311.460066	19.532570
56.678058	2323.678757	19.537587
56.448610	2330.327895	19.542605
56.641959	2322.311605	19.547623
56.340378	2333.742395	19.552640
56.649267	2326.606441	19.557658
56.890081	2322.899255	19.562675
56.977469	2322.980407	19.567693
56.811790	2326.651196	19.572711
56.691624	2319.210793	19.577728
56.773351	2322.917129	19.582746
57.073620	2319.413171	19.587763
57.000355	2325.125932	19.592781
57.553816	2315.448429	19.597799
56.989384	2327.392862	19.602816
56.823019	2322.196178	19.607834
57.289373	2325.606610	19.612851
56.977451	2323.300705	19.617869
57.110654	2328.274016	19.622887
57.281176	2325.921620	19.627904
57.189610	2318.772425	19.632922
57.392389	2319.002324	19.637939
57.195717	2321.051389	19.642957
57.631812	2315.178880	19.647975
57.061984	2320.437318	19.652992
57.288793	2334.275561	19.658010
57.661794	2337.548434	19.663027
57.157404	2347.368066	19.668045
57.344634	2345.747570	19.673063
57.598735	2349.236926	19.678080
57.731218	2360.893365	19.683098
57.976222	2371.614620	19.688115
57.886527	2378.569794	19.693133
58.026368	2373.645056	19.698151
57.933277	2375.997683	19.703168
58.018970	2380.565701	19.708186
58.322772	2372.672204	19.713203
58.072810	2379.077594	19.718221
58.372240	2368.220575	19.723239
58.507076	2369.281158	19.728256
57.937190	2377.978779	19.733274
58.653606	2381.243184	19.738291
58.697652	2393.302276	19.743309
58.716887	2390.059908	19.748327
58.824903	2396.761470	19.753344
59.326825	2395.829659	19.758362
59.126129	2390.868010	19.763379
58.902517	2380.359757	19.768397
58.641564	2381.843377	19.773415
59.050249	2389.542380	19.778432
59.051308	2391.307117	19.783450
59.697273	2387.542266	19.788467
59.138196	2392.481508	19.793485
59.450933	2390.227575	19.798503
59.551714	2392.551689	19.803520
59.319715	2380.686378	19.808538
59.210525	2363.166014	19.813555
59.146648	2382.298317	19.818573
59.619544	2377.884287	19.823591
59.907789	2378.542915	19.828608
59.636257	2393.817271	19.833626
59.708856	2391.219407	19.838643
59.516197	2399.969707	19.843661
59.519195	2384.254801	19.848679
59.591486	2393.628287	19.853696
59.338294	2392.780265	19.858714
59.320028	2388.989115	19.863731
59.325113	2401.911730	19.868749
59.790219	2406.904551	19.873767
60.221167	2413.794102	19.878784
59.850418	2416.716475	19.883802
59.886162	2422.497998	19.888819
59.952652	2426.759820	19.893837
60.259335	2424.094253	19.898855
60.258792	2422.053110	19.903872
60.361353	2447.249330	19.908890
60.280851	2442.351323	19.913907
60.616396	2449.170617	19.918925
60.523504	2446.584579	19.923943
60.599076	2449.231188	19.928960
60.508707	2450.015374	19.933978
60.845344	2437.921008	19.938995
60.741505	2447.287710	19.944013
60.785532	2443.716615	19.949031
60.916616	2443.275227	19.954048
60.657071	2451.250274	19.959066
60.608027	2455.898118	19.964083
60.914279	2476.259424	19.969101
61.007357	2477.791034	19.974119
61.206604	2471.393623	19.979136
60.849347	2477.361464	19.984154
61.020391	2482.052698	19.989171
61.046855	2489.271518	19.994189
61.207078	2494.059903	19.999207
61.454647	2497.866216	20.004224
61.391411	2508.355323	20.009242
61.915305	2503.866362	20.014259
61.847526	2501.903677	20.019277
62.042766	2496.943414	20.024295
62.306900	2498.823717	20.029312
61.973623	2497.059336	20.034330
62.256739	2494.150510	20.039347
62.017126	2497.333140	20.044365
62.073443	2490.641273	20.049383
62.074040	2497.740102	20.054400
61.958647	2496.645574	20.059418
62.513681	2491.002258	20.064435
62.257783	2490.092478	20.069453
62.179998	2488.587496	20.074471
62.658123	2490.964272	20.079488
62.320120	2497.157994	20.084506
62.379241	2496.446216	20.089523
62.225412	2499.095151	20.094541
62.407738	2498.841073	20.099559
63.060857	2521.011010	20.104576
62.598128	2525.853445	20.109594
62.648469	2518.149814	20.114611
62.746523	2526.047050	20.119629
62.832714	2527.946839	20.124647
62.951674	2525.581204	20.129664
62.903470	2526.078587	20.134682
63.037962	2518.239247	20.139699
63.349720	2524.032550	20.144717
63.336527	2517.987347	20.149735
63.361103	2518.158023	20.154752
63.186782	2517.016106	20.159770
63.175931	2501.988617	20.164787
63.463223	2518.483262	20.169805
63.029178	2519.976094	20.174823
63.713059	2526.863282	20.179840
63.924316	2541.425762	20.184858
63.834791	2544.602358	20.189875
63.978797	2542.484439	20.194893
63.669973	2543.296632	20.199911
64.154334	2532.077027	20.204928
64.134716	2546.953948	20.209946
64.324070	2541.646586	20.214963
64.410733	2538.998246	20.219981
64.470548	2547.943179	20.224999
64.489724	2532.964064	20.230016
63.890504	2524.870921	20.235034
64.319849	2526.535468	20.240051
64.500808	2540.021061	20.245069
64.642284	2541.258502	20.250087
64.419268	2535.746991	20.255104
64.331488	2541.074062	20.260122
64.813981	2533.007303	20.265139
64.269031	2536.332859	20.270157
64.596776	2534.527594	20.275175
64.457618	2535.398902	20.280192
64.501178	2546.917943	20.285210
64.626242	2557.519707	20.290227
64.896073	2573.948101	20.295245
64.768617	2568.595030	20.300263
65.321484	2563.211161	20.305280
64.848432	2572.339610	20.310298
64.892906	2571.767373	20.315315
65.079797	2571.792089	20.320333
65.011464	2580.095113	20.325351
65.281220	2591.203684	20.330368
65.040495	2591.269426	20.335386
65.331327	2580.512178	20.340403
65.638470	2590.427511	20.345421
65.086292	2585.523699	20.350439
65.226600	2600.196841	20.355456
65.113478	2612.757150	20.360474
65.883672	2614.649146	20.365491
65.907767	2618.267778	20.370509
65.781247	2623.640107	20.375527
66.118074	2614.631177	20.380544
66.198678	2620.524000	20.385562
66.106940	2623.377310	20.390579
66.416751	2617.425535	20.395597
66.087674	2625.425980	20.400615
66.857470	2619.619003	20.405632
66.698869	2629.970971	20.410650
66.676059	2617.080458	20.415667
66.771787	2607.889205	20.420685
66.619224	2607.016041	20.425703
66.805484	2602.566039	20.430720
66.778970	2598.644733	20.435738
66.493617	2604.159269	20.440755
67.314374	2614.310240	20.445773
66.841477	2627.510301	20.450791
67.223012	2635.143990	20.455808
67.456490	2633.304474	20.460826
66.886880	2630.192152	20.465843
67.220677	2629.293093	20.470861
67.258642	2630.274222	20.475879
67.920839	2621.938769	20.480896
67.609034	2636.685523	20.485914
67.864304	2631.234523	20.490931
67.589906	2612.636490	20.495949
67.325683	2614.101002	20.500967
68.066831	2617.348619	20.505984
67.739412	2622.992443	20.511002
67.953377	2627.067589	20.516019
67.814124	2629.357289	20.521037
67.875318	2636.373336	20.526055
67.924851	2635.330064	20.531072
68.126656	2632.579275	20.536090
68.017032	2622.897927	20.541107
67.755233	2628.198946	20.546125
67.841772	2632.133707	20.551143
67.741236	2620.507927	20.556160
67.925991	2642.312587	20.561178
67.693414	2655.117073	20.566195
68.119770	2654.772327	20.571213
67.993434	2660.024143	20.576231
68.240483	2678.056847	20.581248
68.255253	2685.256499	20.586266
68.271135	2690.769822	20.591283
68.734835	2688.661652	20.596301
68.563524	2691.739680	20.601319
68.955404	2696.010367	20.606336
68.983448	2705.151423	20.611354
69.181839	2713.968736	20.616371
69.440592	2711.393243	20.621389
69.455387	2716.957952	20.626407
69.655902	2707.375377	20.631424
69.582200	2705.112051	20.636442
69.522584	2689.975397	20.641459
69.685324	2674.662814	20.646477
69.395054	2679.789171	20.651495
69.517842	2675.465799	20.656512
69.883405	2702.195584	20.661530
69.494057	2706.256843	20.666547
70.371909	2699.121617	20.671565
70.429955	2695.247218	20.676583
70.448606	2680.425562	20.681600
70.358465	2678.617899	20.686618
70.171885	2669.190706	20.691635
70.004206	2666.123660	20.696653
69.879153	2667.832083	20.701671
69.973995	2659.666338	20.706688
70.154912	2670.509043	20.711706
70.048455	2698.217553	20.716723
70.442308	2698.545432	20.721741
70.679911	2703.247373	20.726759
70.798882	2707.427032	20.731776
70.641293	2704.732335	20.736794
70.161350	2703.664067	20.741811
70.787650	2693.161097	20.746829
70.761857	2708.442454	20.751847
70.822354	2698.458613	20.756864
71.014771	2704.663069	20.761882
70.793239	2720.863991	20.766899
71.573259	2725.966736	20.771917
71.345798	2726.377513	20.776935
71.469556	2723.944084	20.781952
71.526710	2712.792082	20.786970
71.725598	2714.468597	20.791987
71.961765	2704.887785	20.797005
71.470283	2706.593669	20.802023
71.533788	2712.987979	20.807040
71.808407	2714.667261	20.812058
71.471546	2722.460388	20.817075
71.840996	2717.255975	20.822093
71.537624	2728.963788	20.827111
71.857592	2713.232798	20.832128
71.647566	2719.190451	20.837146
71.932235	2715.869430	20.842163
71.939488	2726.788414	20.847181
72.286203	2748.042521	20.852199
72.270499	2750.593786	20.857216
72.472341	2743.480723	20.862234
72.113829	2750.994058	20.867251
72.327531	2753.878504	20.872269
72.364520	2751.544215	20.877287
72.535473	2748.881388	20.882304
72.354815	2753.011624	20.887322
72.106343	2773.589708	20.892339
72.456591	2775.586802	20.897357
72.721157	2778.116797	20.902375
72.582323	2776.249741	20.907392
73.438799	2774.836570	20.912410
73.444766	2777.154946	20.917427
73.503745	2772.349480	20.922445
73.295490	2772.903451	20.927463
73.537740	2768.813952	20.932480
73.483420	2778.573226	20.937498
73.059632	2774.874348	20.942515
73.278790	2779.561360	20.947533
73.458989	2798.689338	20.952551
73.631997	2797.068873	20.957568
73.675125	2800.138508	20.962586
73.483089	2797.852929	20.967603
73.558209	2805.668395	20.972621
73.589116	2802.801179	20.977639
74.033388	2811.132998	20.982656
74.190440	2813.393186	20.987674
74.497218	2823.407175	20.992691
75.060549	2822.992476	20.997709
74.775884	2813.700146	21.002727
74.401117	2797.091139	21.007744
74.895743	2789.381296	21.012762
74.590119	2792.667446	21.017779
74.848029	2791.223801	21.022797
74.733982	2786.158176	21.027815
74.879826	2784.305315	21.032832
74.991603	2782.448058	21.037850
74.876600	2786.342593	21.042867
74.642504	2778.261534	21.047885
74.911498	2793.584578	21.052903
74.737565	2796.950533	21.057920
75.178907	2799.817224	21.062938
75.064728	2815.088637	21.067955
75.397732	2808.861108	21.072973
75.150639	2810.723566	21.077991
75.242603	2813.954156	21.083008
75.427818	2803.910275	21.088026
75.404431	2816.824725	21.093043
75.756448	2826.220604	21.098061
75.718686	2834.064101	21.103079
75.478410	2848.131728	21.108096
75.833948	2839.566794	21.113114
75.922430	2846.316789	21.118131
76.127609	2843.901671	21.123149
76.115479	2838.960316	21.128167
75.940184	2841.990227	21.133184
76.251200	2842.231506	21.138202
76.126380	2861.798547	21.143219
76.574785	2864.037143	21.148237
76.728312	2869.244197	21.153255
76.461072	2859.277853	21.158272
76.669733	2857.821381	21.163290
76.579727	2855.643522	21.168307
76.700987	2857.319973	21.173325
76.593389	2863.099458	21.178343
76.474185	2869.201469	21.183360
76.586685	2872.643554	21.188378
76.832127	2887.857319	21.193395
77.023088	2888.286932	21.198413
77.307983	2890.392116	21.203431
77.030541	2888.848870	21.208448
77.675304	2883.491668	21.213466
77.435968	2886.860192	21.218483
77.397241	2886.258105	21.223501
77.622944	2889.987145	21.228519
77.747215	2894.453405	21.233536
78.077374	2882.955204	21.238554
77.869898	2889.832351	21.243571
77.709872	2884.588714	21.248589
78.049213	2885.389817	21.253607
78.042946	2893.139737	21.258624
78.234553	2883.644425	21.263642
78.059906	2888.565162	21.268659
78.060988	2897.328200	21.273677
77.751113	2915.197554	21.278695
78.070241	2913.381124	21.283712
77.851711	2912.394031	21.288730
78.030325	2929.296797	21.293747
78.518627	2930.706350	21.298765
78.828226	2939.493697	21.303783
78.615406	2942.959282	21.308800
78.757419	2939.723315	21.313818
78.749331	2948.636015	21.318835
78.992326	2943.268919	21.323853
78.756631	2945.752400	21.328871
79.173123	2953.362138	21.333888
79.505714	2957.361904	21.338906
79.410181	2962.758176	21.343923
79.501748	2963.078822	21.348941
79.763970	2958.787385	21.353959
79.615595	2968.650321	21.358976
79.870893	2959.827649	21.363994
79.762449	2966.086153	21.369011
79.584253	2959.761920	21.374029
79.556816	2961.230757	21.379047
79.395627	2963.820389	21.384064
80.062440	2955.273693	21.389082
79.654874	2969.003106	21.394099
79.768788	2977.657849	21.399117
79.924959	2987.334697	21.404135
80.100976	2992.672610	21.409152
80.167010	2989.166136	21.414170
79.898547	2998.304644	21.419187
80.049990	3013.546461	21.424205
80.082719	3015.433424	21.429223
80.296905	3023.352741	21.434240
80.614247	3021.212917	21.439258
80.690458	3047.358908	21.444275
81.169643	3049.486721	21.449293
81.458439	3047.768410	21.454311
81.499535	3053.761104	21.459328
81.537479	3049.183616	21.464346
81.479414	3040.001940	21.469363
81.387473	3021.254005	21.474381
81.832010	3018.667088	21.479399
80.783409	3027.774764	21.484416
81.412653	3024.856904	21.489434
81.478383	3043.867770	21.494451
81.855137	3052.723213	21.499469
81.466528	3054.184675	21.504487
81.756749	3053.824672	21.509504
82.425874	3047.223609	21.514522
82.101652	3045.904160	21.519539
81.937452	3053.691475	21.524557
82.356600	3052.973864	21.529575
82.185356	3051.454135	21.534592
82.782369	3043.198159	21.539610
82.503793	3048.793594	21.544627
82.130431	3042.335035	21.549645
82.686098	3038.708377	21.554663
82.175700	3049.848646	21.559680
82.038957	3068.776120	21.564698
82.246852	3075.682944	21.569715
82.569801	3078.478627	21.574733
82.778145	3083.267606	21.579751
82.413982	3110.657955	21.584768
83.144609	3100.698367	21.589786
83.266294	3104.933585	21.594803
83.095947	3103.492454	21.599821
83.687544	3099.930504	21.604839
83.177804	3106.075148	21.609856
82.974818	3102.143806	21.614874
83.344767	3123.231411	21.619891
83.524210	3129.937580	21.624909
83.748572	3122.605479	21.629927
83.745071	3128.402654	21.634944
83.728151	3125.762524	21.639962
83.665348	3135.106060	21.644979
84.017882	3149.498396	21.649997
84.534895	3150.744746	21.655015
84.747149	3151.692089	21.660032
84.807993	3157.490056	21.665050
84.904955	3137.014742	21.670067
84.424653	3132.911991	21.675085
84.199078	3127.243984	21.680103
84.348630	3157.823421	21.685120
84.271472	3157.909949	21.690138
84.614236	3154.823025	21.695155
84.405718	3163.586705	21.700173
84.775064	3175.683560	21.705191
84.892390	3185.726324	21.710208
84.890886	3184.342084	21.715226
85.245297	3179.273986	21.720243
85.558972	3185.421616	21.725261
85.414234	3181.935485	21.730279
85.241925	3186.979562	21.735296
85.329573	3183.492967	21.740314
85.278212	3194.678286	21.745331
85.408526	3207.897486	21.750349
85.558112	3209.818780	21.755367
85.632390	3220.995967	21.760384
86.091594	3205.152408	21.765402
86.169055	3207.831113	21.770419
85.763575	3203.035052	21.775437
86.019843	3215.612056	21.780455
86.065994	3239.038510	21.785472
86.022788	3241.223621	21.790490
86.572597	3228.751084	21.795507
86.198232	3243.936782	21.800525
86.543675	3239.513653	21.805543
86.528057	3244.331628	21.810560
87.028757	3244.094626	21.815578
86.735781	3239.850258	21.820595
86.601131	3258.957956	21.825613
87.238758	3260.471891	21.830631
87.054752	3265.495946	21.835648
86.945744	3266.688969	21.840666
87.595309	3260.665316	21.845683
87.274439	3258.727026	21.850701
87.582623	3252.263369	21.855719
87.574333	3262.279675	21.860736
87.382282	3259.193064	21.865754
87.676233	3260.708427	21.870771
87.835495	3276.261826	21.875789
87.944081	3283.247985	21.880807
87.985771	3288.182161	21.885824
88.272493	3283.710807	21.890842
88.082210	3276.504854	21.895859
88.576874	3284.781820	21.900877
88.397814	3272.560222	21.905895
88.354545	3279.154998	21.910912
88.434415	3277.226759	21.915930
88.441895	3283.007931	21.920947
88.122011	3284.368634	21.925965
88.520075	3292.444007	21.930983
88.597718	3311.790238	21.936000
88.945421	3311.462117	21.941018
89.361975	3308.787806	21.946035
88.932101	3306.736671	21.951053
89.231513	3295.826252	21.956071
89.505047	3300.151263	21.961088
89.266563	3295.491934	21.966106
89.083930	3302.266554	21.971123
89.449850	3314.776008	21.976141
89.787551	3316.978521	21.981159
89.975138	3327.337751	21.986176
89.860216	3327.099183	21.991194
89.681284	3319.476997	21.996211
90.175297	3333.221483	22.001229
90.346807	3319.032225	22.006247
90.168537	3330.064555	22.011264
90.007397	3327.288450	22.016282
89.930193	3322.167505	22.021299
89.801628	3324.857925	22.026317
90.295227	3330.759756	22.031335
90.413048	3347.252039	22.036352
90.117519	3354.859608	22.041370
90.689784	3355.052170	22.046387
90.758066	3356.297500	22.051405
90.619569	3355.655793	22.056423
90.896087	3355.462739	22.061440
90.789501	3359.536328	22.066458
91.558084	3364.683779	22.071475
91.199475	3381.874456	22.076493
91.344081	3373.447784	22.081511
91.444219	3373.099099	22.086528
91.354688	3379.140302	22.091546
91.975367	3361.446436	22.096563
92.149312	3358.595551	22.101581
92.369037	3355.749418	22.106599
92.328679	3360.329095	22.111616
92.367099	3362.707363	22.116634
92.627336	3354.101785	22.121651
92.402629	3348.219325	22.126669
92.252029	3334.906724	22.131687
92.433023	3337.677175	22.136704
92.279901	3353.279482	22.141722
92.672300	3353.330400	22.146739
92.716631	3361.138033	22.151757
92.651030	3364.166563	22.156775
92.211380	3356.935594	22.161792
92.282745	3362.782239	22.166810
92.505902	3364.644472	22.171827
92.764221	3386.436766	22.176845
92.662615	3385.199621	22.181863
92.957040	3383.133774	22.186880
92.814381	3392.471463	22.191898
93.286970	3403.846695	22.196915
93.245213	3423.334034	22.201933
93.518417	3422.414607	22.206951
93.250768	3424.214502	22.211968
93.223119	3419.287438	22.216986
93.692954	3435.317007	22.222003
93.338941	3450.333233	22.227021
93.733824	3450.301030	22.232039
93.771038	3446.674170	22.237056
93.624876	3459.240029	22.242074
94.196089	3471.434819	22.247091
94.292660	3476.013106	22.252109
94.151808	3481.652026	22.257127
94.335323	3479.329525	22.262144
94.528130	3488.820044	22.267162
95.082825	3496.956092	22.272179
95.003128	3508.394582	22.277197
95.087131	3500.048328	22.282215
95.282564	3498.529485	22.287232
95.307153	3506.840693	22.292250
96.038866	3502.829335	22.297267
95.669021	3490.997841	22.302285
95.739569	3476.665870	22.307303
94.983341	3463.663338	22.312320
95.278021	3477.361004	22.317338
95.779894	3486.893833	22.322355
95.950579	3500.017360	22.327373
95.778454	3501.409455	22.332391
96.289033	3496.795701	22.337408
95.710362	3505.028400	22.342426
95.995612	3496.731129	22.347443
95.938889	3504.528592	22.352461
96.002576	3509.062908	22.357479
96.198483	3516.577638	22.362496
95.604340	3533.229194	22.367514
95.954708	3533.199109	22.372531
96.070976	3548.853873	22.377549
96.286096	3561.942267	22.382567
96.496535	3562.783623	22.387584
96.356909	3568.480645	22.392602
97.142771	3579.614849	22.397619
96.925725	3580.978423	22.402637
97.163195	3591.853024	22.407655
97.568090	3595.525522	22.412672
97.271632	3588.537678	22.417690
97.674022	3585.776752	22.422707
97.556954	3589.741147	22.427725
97.980481	3588.840043	22.432743
98.088323	3570.590404	22.437760
98.053142	3576.915349	22.442778
98.437123	3571.359263	22.447795
98.460112	3575.062578	22.452813
98.513439	3567.003505	22.457831
98.542631	3562.266701	22.462848
98.210201	3576.694165	22.467866
98.636712	3576.709309	22.472883
98.822550	3576.147454	22.477901
98.400816	3575.473963	22.482919
98.723394	3590.387714	22.487936
98.650579	3602.424451	22.492954
99.121661	3595.170336	22.497971
99.046587	3608.232125	22.502989
98.862517	3605.021211	22.508007
98.487752	3602.072969	22.513024
98.588822	3623.654698	22.518042
99.433706	3632.171093	22.523059
99.509063	3626.698616	22.528077
99.707446	3640.058516	22.533095
99.780539	3635.459081	22.538112
99.532885	3643.551615	22.543130
99.869797	3652.893088	22.548147
99.988301	3667.721397	22.553165
99.901642	3659.654773	22.558183
100.174367	3661.395918	22.563200
100.280317	3663.917023	22.568218
100.228993	3661.133845	22.573235
100.459201	3669.592610	22.578253
100.771467	3671.204112	22.583271
100.829466	3673.171882	22.588288
100.703062	3681.687066	22.593306
100.661287	3679.459868	22.598323
100.944354	3688.230921	22.603341
101.050865	3690.381763	22.608359
100.888430	3680.921468	22.613376
101.050466	3682.701282	22.618394
101.390632	3676.088627	22.623411
101.603607	3684.926039	22.628429
101.497289	3702.008439	22.633447
101.502422	3710.068695	22.638464
101.542585	3715.244272	22.643482
101.422830	3714.484347	22.648499
101.641667	3713.000852	22.653517
101.817217	3716.522887	22.658535
102.376034	3732.197260	22.663552
102.339875	3745.756555	22.668570
102.610609	3744.765074	22.673587
102.550637	3742.616596	22.678605
102.254088	3742.147676	22.683623
102.530523	3742.109791	22.688640
102.605270	3739.640503	22.693658
102.402097	3740.113298	22.698675
102.624458	3757.108691	22.703693
102.671351	3768.550870	22.708711
102.942724	3768.031840	22.713728
103.218607	3771.548499	22.718746
103.583566	3766.059404	22.723763
103.750359	3774.381816	22.728781
103.439948	3773.493904	22.733799
103.794145	3780.316098	22.738816
103.707074	3788.535546	22.743834
103.880882	3792.782492	22.748851
103.700238	3793.004905	22.753869
103.628802	3790.003048	22.758887
103.797481	3791.472208	22.763904
103.689509	3804.505144	22.768922
103.671775	3820.198902	22.773939
103.949700	3820.624661	22.778957
104.173240	3841.430377	22.783975
104.721538	3846.680341	22.788992
105.070210	3849.888400	22.794010
105.098913	3854.686361	22.799027
105.264699	3852.547208	22.804045
105.232187	3854.347793	22.809063
105.215883	3850.771759	22.814080
105.194788	3848.858397	22.819098
104.928259	3850.372245	22.824115
105.328442	3859.133554	22.829133
104.960512	3879.216098	22.834151
105.503743	3875.522078	22.839168
105.395959	3877.558464	22.844186
105.380389	3885.018263	22.849203
106.039359	3899.218558	22.854221
106.224090	3904.982960	22.859239
106.037296	3906.847020	22.864256
106.021194	3908.239179	22.869274
106.189197	3908.817679	22.874291
106.623745	3909.953004	22.879309
106.638972	3912.950455	22.884327
106.515579	3906.347868	22.889344
106.586074	3912.402795	22.894362
106.674117	3931.671606	22.899379
106.996801	3934.779385	22.904397
106.927490	3934.949633	22.909415
107.495869	3936.001370	22.914432
107.517989	3939.264644	22.919450
107.373079	3934.570966	22.924467
107.755263	3936.724987	22.929485
107.296159	3939.728940	22.934503
107.932198	3951.599522	22.939520
107.940952	3962.487600	22.944538
108.096828	3963.220191	22.949555
108.252622	3966.954386	22.954573
108.358109	3972.582752	22.959591
108.455568	3962.720156	22.964608
108.455706	3969.238468	22.969626
108.154284	3963.668222	22.974643
108.563547	3950.372533	22.979661
108.056721	3969.891446	22.984679
108.039884	3981.988973	22.989696
108.020423	3994.224790	22.994714
108.297765	3996.981991	22.999731
108.759376	4010.510521	23.004749
108.666194	4016.476981	23.009767
108.873629	4029.725393	23.014784
109.311450	4036.462478	23.019802
109.384205	4049.165337	23.024819
109.493333	4033.931514	23.029837
109.344682	4040.978651	23.034855
109.970995	4057.527059	23.039872
109.995044	4068.578776	23.044890
110.264831	4070.799343	23.049907
110.263274	4071.572318	23.054925
110.296576	4075.956846	23.059943
110.484936	4067.597915	23.064960
110.338111	4067.401822	23.069978
110.428063	4071.152056	23.074995
110.536167	4076.813878	23.080013
110.816026	4099.421801	23.085031
110.978018	4098.725397	23.090048
111.280295	4090.244533	23.095066
111.389943	4101.879400	23.100083
111.430792	4092.272166	23.105101
111.284536	4093.449582	23.110119
111.707968	4094.503339	23.115136
111.713536	4094.233075	23.120154
111.679037	4099.679917	23.125171
111.849829	4097.001142	23.130189
111.976090	4093.215521	23.135207
112.010201	4091.259584	23.140224
112.037135	4102.415583	23.145242
112.042866	4123.637858	23.150259
112.359730	4123.111806	23.155277
112.447493	4127.144397	23.160295
112.508327	4122.584728	23.165312
112.617284	4123.758562	23.170330
112.550582	4128.603679	23.175347
112.951296	4129.874779	23.180365
112.393504	4140.595468	23.185383
112.457611	4142.106217	23.190400
113.201899	4144.250172	23.195418
112.872409	4153.540791	23.200435
113.145206	4169.590712	23.205453
113.416618	4183.584403	23.210471
113.444137	4181.546098	23.215488
113.538857	4178.555850	23.220506
113.507951	4192.465120	23.225523
114.075062	4194.193662	23.230541
114.114655	4208.550044	23.235559
114.173946	4219.915600	23.240576
114.610503	4211.004449	23.245594
114.217541	4214.633513	23.250611
114.469113	4215.208725	23.255629
114.738508	4215.636746	23.260647
114.677248	4208.399582	23.265664
114.570455	4211.165181	23.270682
114.636219	4230.787093	23.275699
114.938860	4229.757821	23.280717
114.883367	4232.164923	23.285735
114.850097	4253.173523	23.290752
115.852296	4245.178268	23.295770
115.901652	4252.575915	23.300787
116.075067	4241.772299	23.305805
116.400358	4236.161460	23.310823
116.179052	4239.465742	23.315840
116.384377	4231.147136	23.320858
116.172708	4232.478336	23.325875
116.390642	4236.228722	23.330893
116.590299	4228.665635	23.335911
116.747004	4227.355783	23.340928
116.487382	4227.967439	23.345946
116.712972	4223.794574	23.350963
117.053578	4236.224828	23.355981
116.772397	4230.017765	23.360999
116.787597	4238.332544	23.366016
117.268761	4240.174280	23.371034
117.196930	4249.431808	23.376051
117.397031	4255.426053	23.381069
117.507483	4259.134224	23.386087
117.251963	4258.804751	23.391104
117.751400	4254.065096	23.396122
117.529337	4258.992810	23.401139
117.830324	4275.983160	23.406157
117.712305	4284.884743	23.411175
117.470796	4293.698809	23.416192
117.907668	4292.475606	23.421210
117.807103	4301.787711	23.426227
117.895249	4316.434379	23.431245
118.126409	4311.817888	23.436263
117.874489	4325.055510	23.441280
118.147427	4342.023960	23.446298
118.541689	4352.451613	23.451315
119.140689	4357.522931	23.456333
118.760147	4377.326294	23.461351
118.775411	4386.982478	23.466368
119.176932	4389.451453	23.471386
119.107435	4403.483305	23.476403
119.312988	4408.893825	23.481421
119.244357	4408.665418	23.486439
119.411731	4412.455232	23.491456
119.684772	4423.674808	23.496474
119.858228	4437.274372	23.501491
120.262207	4440.178496	23.506509
120.250245	4438.493487	23.511527
120.454918	4436.766612	23.516544
120.652228	4447.474623	23.521562
120.471142	4468.960953	23.526579
120.935064	4473.604150	23.531597
121.176357	4475.861166	23.536615
120.622162	4484.769113	23.541632
121.217963	4481.588148	23.546650
121.294725	4483.113302	23.551667
121.286349	4491.661457	23.556685
121.833584	4500.683828	23.561703
121.584133	4499.781482	23.566720
121.637988	4499.245375	23.571738
121.872304	4508.717578	23.576755
121.651650	4505.267795	23.581773
122.133352	4512.072388	23.586791
121.882044	4528.849727	23.591808
122.056922	4527.507594	23.596826
121.922589	4533.307234	23.601843
122.335862	4530.930228	23.606861
122.606173	4545.176474	23.611879
122.510720	4561.445091	23.616896
122.914886	4551.447633	23.621914
122.712401	4558.993354	23.626931
123.542098	4577.913690	23.631949
123.677031	4580.347272	23.636967
123.543498	4588.608968	23.641984
123.906201	4574.933220	23.647002
123.629299	4591.000620	23.652019
123.767975	4588.081525	23.657037
124.019203	4583.285084	23.662055
123.807686	4589.806856	23.667072
123.992213	4579.283870	23.672090
124.101630	4603.430858	23.677107
124.452011	4610.345436	23.682125
124.896788	4610.442523	23.687143
124.800789	4618.585166	23.692160
124.704857	4608.400883	23.697178
124.985074	4622.350921	23.702195
124.910334	4612.351249	23.707213
125.283353	4612.465363	23.712231
125.268104	4623.592729	23.717248
125.463645	4616.527168	23.722266
125.515327	4628.878090	23.727283
125.456724	4644.785248	23.732301
125.535183	4653.334357	23.737319
125.551997	4647.215455	23.742336
125.801338	4653.595234	23.747354
125.682142	4650.681741	23.752371
126.235861	4664.929918	23.757389
126.408128	4668.349548	23.762407
126.646018	4674.815577	23.767424
126.509415	4663.585933	23.772442
126.820429	4669.566048	23.777459
126.657235	4676.883760	23.782477
126.757650	4679.982535	23.787495
126.931535	4698.379028	23.792512
126.865554	4704.680560	23.797530
127.248606	4705.586118	23.802547
127.343113	4695.577069	23.807565
127.467787	4711.639546	23.812583
127.264284	4722.636999	23.817600
127.552692	4719.388178	23.822618
127.904623	4728.281906	23.827635
127.977584	4749.317847	23.832653
128.074625	4742.343156	23.837671
128.095674	4752.189182	23.842688
128.107161	4742.631484	23.847706
128.273981	4757.506093	23.852723
128.694862	4760.570424	23.857741
128.974478	4768.407729	23.862759
128.902277	4776.139157	23.867776
129.391896	4760.267572	23.872794
129.131113	4768.525184	23.877811
129.201074	4774.124482	23.882829
129.724445	4782.732863	23.887847
129.679251	4784.237208	23.892864
130.242261	4789.863045	23.897882
130.044159	4792.993328	23.902899
130.201329	4786.519496	23.907917
130.294132	4780.693125	23.912935
130.303808	4793.701979	23.917952
130.552891	4784.817136	23.922970
130.674643	4788.363601	23.927987
130.704212	4789.299046	23.933005
130.648129	4785.718592	23.938023
131.035039	4803.811673	23.943040
131.347892	4823.484903	23.948058
131.304600	4821.786320	23.953075
131.320348	4820.960576	23.958093
131.158995	4814.291653	23.963111
130.567619	4826.726980	23.968128
130.823746	4826.354674	23.973146
131.469871	4842.742983	23.978163
131.454906	4842.568382	23.983181
131.516938	4846.754435	23.988199
131.494889	4863.388853	23.993216
131.824443	4871.506718	23.998234
131.840259	4883.048762	24.003251
132.271012	4902.983861	24.008269
132.269073	4911.530351	24.013287
132.482238	4908.308569	24.018304
132.586048	4914.582651	24.023322
133.204463	4928.202451	24.028339
133.356701	4935.281892	24.033357
133.724448	4927.425004	24.038375
133.638880	4927.269594	24.043392
133.435627	4929.565867	24.048410
133.935253	4933.882504	24.053427
133.933540	4927.539036	24.058445
134.177665	4927.292449	24.063463
133.818527	4936.997400	24.068480
133.989709	4947.829167	24.073498
134.118886	4960.593974	24.078515
134.313309	4963.712135	24.083533
134.575292	4950.157304	24.088551
134.664176	4966.897263	24.093568
135.055833	4981.651622	24.098586
135.242373	4992.237398	24.103603
134.834362	4999.729555	24.108621
135.381300	4988.005995	24.113639
135.345473	4996.578032	24.118656
135.224270	5007.567874	24.123674
135.259035	5015.178685	24.128691
134.979608	5015.380239	24.133709
135.510868	5034.764236	24.138727
136.094976	5046.183769	24.143744
135.895780	5052.879267	24.148762
136.347063	5048.439074	24.153779
136.128792	5062.773485	24.158797
136.916192	5074.577225	24.163815
136.895013	5070.867060	24.168832
136.775877	5077.125078	24.173850
137.205834	5070.787105	24.178867
137.105122	5075.350055	24.183885
137.595442	5065.005899	24.188903
137.871967	5071.952246	24.193920
137.856589	5079.758361	24.198938
138.012453	5078.632112	24.203955
138.099879	5090.550351	24.208973
138.108036	5093.872181	24.213991
137.785295	5098.939501	24.219008
137.884227	5100.779132	24.224026
138.086052	5087.091142	24.229043
138.191167	5107.061845	24.234061
138.631862	5113.557088	24.239079
138.456311	5120.076061	24.244096
139.143601	5124.339312	24.249114
139.069107	5120.671357	24.254131
138.594860	5124.587092	24.259149
139.242027	5126.812431	24.264167
139.221585	5135.415776	24.269184
139.461310	5144.565277	24.274202
139.648440	5140.994247	24.279219
139.126303	5147.282785	24.284237
139.735069	5162.288380	24.289255
140.187615	5181.210299	24.294272
140.253201	5167.866179	24.299290
140.275628	5174.507981	24.304307
140.226851	5180.316820	24.309325
140.360806	5183.131897	24.314343
140.328871	5199.075996	24.319360
140.480456	5207.475026	24.324378
140.699810	5212.638490	24.329395
141.003094	5234.209016	24.334413
141.267615	5234.411054	24.339431
140.752221	5238.947469	24.344448
140.978589	5260.345326	24.349466
141.288779	5260.739605	24.354483
141.887242	5281.935070	24.359501
142.002240	5288.212896	24.364519
142.253285	5291.249736	24.369536
142.422919	5302.041839	24.374554
142.546338	5293.962784	24.379571
142.573334	5304.394954	24.384589
142.664503	5299.134227	24.389607
142.379240	5309.598665	24.394624
142.880274	5328.131210	24.399642
142.919605	5324.030950	24.404659
143.123097	5336.284719	24.409677
143.883902	5350.542126	24.414695
143.604221	5360.058059	24.419712
143.708921	5358.599496	24.424730
144.031850	5341.458599	24.429747
144.031175	5356.564131	24.434765
144.008096	5353.173237	24.439783
144.097116	5374.352975	24.444800
144.361908	5379.908059	24.449818
144.545153	5373.757983	24.454835
144.763624	5377.230499	24.459853
145.080796	5379.846425	24.464871
145.104184	5391.589974	24.469888
145.041521	5405.645171	24.474906
145.559254	5404.324533	24.479923
145.645594	5401.905776	24.484941
145.849323	5398.778460	24.489959
145.507600	5396.450417	24.494976
145.884409	5406.239799	24.499994
146.036823	5398.200619	24.505011
146.064605	5428.387063	24.510029
145.916479	5425.158586	24.515047
146.111183	5424.352545	24.520064
146.168778	5439.907387	24.525082
146.550437	5443.628419	24.530099
146.474481	5454.322519	24.535117
146.416701	5457.621071	24.540135
147.257444	5464.780427	24.545152
147.503722	5485.123612	24.550170
147.761714	5484.361068	24.555187
147.917269	5489.793134	24.560205
147.524788	5484.102475	24.565223
147.763308	5494.616661	24.570240
147.308172	5490.805137	24.575258
147.948468	5489.420946	24.580275
148.056264	5514.773188	24.585293
148.181931	5523.599029	24.590311
148.164859	5517.183129	24.595328
148.196270	5537.394650	24.600346
148.351911	5542.697538	24.605363
148.578066	5548.283724	24.610381
148.954352	5569.909146	24.615399
149.105991	5578.077568	24.620416
148.960313	5583.606993	24.625434
149.325023	5580.241731	24.630451
149.622496	5602.006739	24.635469
149.996500	5607.425815	24.640487
150.009170	5603.111863	24.645504
150.100025	5606.966282	24.650522
150.224952	5611.320562	24.655539
150.496342	5623.202149	24.660557
150.547770	5628.595399	24.665575
150.914953	5626.925611	24.670592
150.449077	5631.218913	24.675610
151.107075	5640.605773	24.680627
151.026493	5645.514383	24.685645
150.978203	5654.897876	24.690663
151.548996	5663.388334	24.695680
151.642381	5686.595271	24.700698
151.934446	5684.422412	24.705715
151.810781	5689.053276	24.710733
152.077070	5688.520884	24.715751
152.530060	5685.876176	24.720768
152.374793	5710.246668	24.725786
152.329040	5713.388034	24.730803
152.550333	5717.395776	24.735821
152.421418	5721.185498	24.740839
152.622850	5735.780185	24.745856
152.743071	5750.625117	24.750874
153.025180	5746.750947	24.755891
153.323107	5764.960419	24.760909
153.518619	5777.972879	24.765927
153.799991	5780.973107	24.770944
153.762954	5782.100413	24.775962
153.718003	5789.303051	24.780979
154.203708	5804.411487	24.785997
154.283238	5814.716042	24.791015
154.266452	5819.216767	24.796032
154.039970	5813.339990	24.801050
154.400176	5820.173859	24.806067
154.779616	5830.482937	24.811085
154.532293	5844.510311	24.816103
155.530845	5850.068956	24.821120
155.110130	5865.704636	24.826138
155.375891	5869.817436	24.831155
155.371694	5869.953697	24.836173
155.794363	5876.807602	24.841191
156.058830	5878.565383	24.846208
156.271047	5886.580216	24.851226
156.543033	5895.814420	24.856243
156.383740	5889.822907	24.861261
156.521644	5903.943410	24.866279
156.791152	5905.260000	24.871296
157.015964	5918.176177	24.876314
156.796110	5917.281275	24.881331
157.156422	5922.204975	24.886349
157.077261	5928.313898	24.891367
157.493125	5938.608926	24.896384
157.533626	5952.247549	24.901402
157.510730	5954.813166	24.906419
157.908851	5960.813500	24.911437
157.656015	5982.867933	24.916455
158.165121	5983.644045	24.921472
158.206077	5991.318066	24.926490
158.268402	6003.709194	24.931507
158.965128	6001.793036	24.936525
159.179353	5998.295155	24.941543
159.093842	5998.513888	24.946560
159.225298	6025.125590	24.951578
159.360174	6024.969400	24.956595
159.636733	6028.242262	24.961613
159.685938	6031.571430	24.966631
159.505471	6033.834808	24.971648
159.994073	6052.093844	24.976666
159.891469	6055.504969	24.981683
160.301594	6062.034992	24.986701
160.548495	6070.272410	24.991719
161.088719	6079.077907	24.996736
161.011932	6075.350258	25.001754
161.270360	6075.558081	25.006771
161.916967	6073.006155	25.011789
161.842560	6075.107204	25.016807
161.807342	6074.754098	25.021824
161.877964	6072.978349	25.026842
162.021881	6073.677645	25.031859
162.135518	6072.926431	25.036877
161.974520	6081.184155	25.041895
162.623894	6080.359217	25.046912
162.404283	6103.070591	25.051930
162.595591	6095.766424	25.056947
162.716019	6104.234287	25.061965
162.257824	6108.992726	25.066983
162.838204	6114.369509	25.072000
162.743922	6124.195982	25.077018
163.147599	6124.356851	25.082035
163.146059	6134.857474	25.087053
163.532023	6153.702169	25.092071
163.350169	6157.739748	25.097088
163.722048	6170.103146	25.102106
163.805122	6190.876162	25.107123
164.251736	6188.345112	25.112141
164.379339	6202.092690	25.117159
164.470642	6211.517172	25.122176
164.763503	6224.641708	25.127194
164.820913	6227.693807	25.132211
164.954574	6227.626837	25.137229
164.800365	6238.706683	25.142247
165.330369	6246.547487	25.147264
165.440817	6254.468096	25.152282
165.644120	6256.978442	25.157299
165.437414	6273.402581	25.162317
165.772644	6292.690962	25.167335
165.982879	6289.174797	25.172352
166.346043	6305.157040	25.177370
166.174328	6317.494792	25.182387
166.686671	6315.963899	25.187405
166.539334	6337.095634	25.192423
166.882031	6337.558419	25.197440
167.566516	6342.251015	25.202458
167.330403	6338.786148	25.207475
167.506023	6343.105944	25.212493
167.899104	6365.414107	25.217511
167.822897	6374.076519	25.222528
168.024506	6375.959353	25.227546
168.061642	6385.905250	25.232563
168.562830	6388.972681	25.237581
168.968012	6391.350763	25.242599
169.143673	6385.057445	25.247616
169.383015	6388.457286	25.252634
169.284530	6394.893458	25.257651
169.467544	6388.493322	25.262669
169.436788	6415.117728	25.267687
169.550159	6424.371553	25.272704
169.792438	6424.760966	25.277722
169.523370	6425.969056	25.282739
169.940572	6435.884491	25.287757
169.779051	6451.158850	25.292775
170.114966	6454.872211	25.297792
170.291775	6464.431855	25.302810
170.264762	6490.981698	25.307827
171.269535	6482.138884	25.312845
171.443100	6488.140103	25.317863
171.592193	6495.241262	25.322880
171.496358	6501.337507	25.327898
171.532603	6510.877162	25.332915
172.171609	6510.787368	25.337933
172.090963	6507.782635	25.342951
172.412258	6501.991303	25.347968
172.773921	6507.316702	25.352986
172.274788	6516.336065	25.358003
172.119191	6509.678832	25.363021
171.921164	6529.412610	25.368039
172.531539	6534.487419	25.373056
172.803291	6555.629524	25.378074
172.816339	6574.890766	25.383091
172.836518	6569.435404	25.388109
172.846688	6586.181106	25.393127
173.146392	6597.594589	25.398144
173.603276	6607.685298	25.403162
173.593478	6627.980888	25.408179
174.389246	6627.692494	25.413197
174.365862	6642.666857	25.418215
174.498455	6649.186406	25.423232
174.849979	6655.488821	25.428250
174.800725	6663.445676	25.433267
175.057721	6674.969730	25.438285
175.168603	6689.598144	25.443303
175.390126	6693.783339	25.448320
175.791664	6685.556650	25.453338
175.730629	6702.888161	25.458355
176.199972	6696.670417	25.463373
176.603746	6710.324613	25.468391
176.752766	6701.232142	25.473408
176.912111	6698.564351	25.478426
176.986813	6703.248154	25.483443
177.492542	6701.552934	25.488461
177.245174	6701.208611	25.493479
177.212529	6717.740434	25.498496
177.852225	6730.549913	25.503514
177.492597	6738.302417	25.508531
178.183006	6729.605527	25.513549
177.530563	6741.090956	25.518567
177.491669	6751.100530	25.523584
178.045303	6759.501568	25.528602
178.125558	6766.007293	25.533619
178.239981	6784.389609	25.538637
178.567883	6799.149500	25.543655
178.748112	6818.892840	25.548672
178.785951	6822.981941	25.553690
178.993336	6837.400160	25.558707
179.238006	6849.539327	25.563725
179.532823	6861.499751	25.568743
179.346258	6862.573990	25.573760
179.874985	6887.772753	25.578778
180.063475	6897.559892	25.583795
180.308043	6888.427303	25.588813
181.125860	6905.312180	25.593831
180.879175	6903.604914	25.598848
181.500468	6908.496789	25.603866
181.355493	6907.962389	25.608883
181.327698	6903.073657	25.613901
181.616831	6895.185172	25.618919
181.543261	6902.561010	25.623936
181.576715	6897.302563	25.628954
181.715826	6916.183388	25.633971
182.490420	6921.488557	25.638989
182.233239	6927.523606	25.644007
182.243677	6930.751684	25.649024
182.486692	6939.969406	25.654042
182.547103	6954.796565	25.659059
182.816110	6959.654315	25.664077
182.894891	6973.033589	25.669095
182.935780	6988.335207	25.674112
183.374864	6995.371123	25.679130
183.487430	7013.215191	25.684148
183.303412	7019.540233	25.689165
183.963611	7030.744918	25.694183
184.383717	7041.910416	25.699200
184.663752	7040.777715	25.704218
184.384846	7048.702442	25.709236
184.787830	7048.230081	25.714253
184.770526	7075.262129	25.719271
184.929814	7081.646510	25.724288
185.383322	7088.264841	25.729306
185.339454	7101.490363	25.734324
185.515380	7097.701035	25.739341
185.544897	7115.999816	25.744359
186.074824	7140.370041	25.749376
186.361989	7136.274099	25.754394
186.162328	7145.026626	25.759412
186.368172	7165.794043	25.764429
186.904518	7171.805806	25.769447
186.762851	7185.122212	25.774464
187.146328	7194.865079	25.779482
187.663569	7199.922984	25.784500
187.490122	7211.174594	25.789517
187.539058	7216.043364	25.794535
187.765148	7232.204439	25.799552
188.019123	7234.263526	25.804570
188.086865	7248.222361	25.809588
188.309570	7253.359921	25.814605
188.890003	7262.150521	25.819623
188.729130	7280.576660	25.824640
189.065561	7289.002610	25.829658
188.876209	7301.480427	25.834676
189.087856	7305.464230	25.839693
189.529799	7324.985294	25.844711
189.468973	7339.754026	25.849728
190.062159	7342.981552	25.854746
190.601155	7355.871822	25.859764
191.000820	7348.776369	25.864781
191.628296	7337.480818	25.869799
191.523224	7335.807524	25.874816
191.979311	7326.390278	25.879834
191.891635	7333.382720	25.884852
191.760231	7329.383690	25.889869
192.097713	7331.589183	25.894887
191.822974	7339.737855	25.899904
192.164512	7332.598017	25.904922
192.022347	7335.948446	25.909940
192.429031	7327.659102	25.914957
192.601689	7340.666515	25.919975
192.549027	7360.337007	25.924992
192.944341	7362.080404	25.930010
192.734467	7364.226113	25.935028
192.872129	7383.557560	25.940045
192.927318	7396.227503	25.945063
192.821535	7409.063698	25.950080
193.089981	7425.351631	25.955098
193.242416	7440.053962	25.960116
193.367744	7463.040576	25.965133
193.984909	7472.339420	25.970151
193.504162	7494.827317	25.975168
194.094963	7505.528233	25.980186
194.272213	7527.253456	25.985204
194.396590	7539.848628	25.990221
195.046096	7558.204707	25.995239
195.244305	7573.764307	26.000256
195.543338	7583.057879	26.005274
195.481350	7596.226255	26.010292
195.705395	7616.463316	26.015309
195.836501	7621.743532	26.020327
196.218157	7640.193675	26.025344
196.472697	7646.854225	26.030362
196.968013	7662.303897	26.035380
196.925614	7667.382259	26.040397
197.088810	7676.339935	26.045415
197.243152	7689.277506	26.050432
197.767574	7681.902125	26.055450
198.223736	7705.183731	26.060468
198.054974	7713.159228	26.065485
198.342605	7708.868476	26.070503
198.407911	7715.169959	26.075520
198.693405	7731.871238	26.080538
198.893212	7735.420738	26.085556
199.056583	7740.277929	26.090573
199.022186	7747.625381	26.095591
199.049353	7777.806912	26.100608
199.476020	7770.454551	26.105626
199.276289	7788.726434	26.110644
199.481454	7806.548422	26.115661
200.185814	7826.430045	26.120679
200.220958	7839.567001	26.125696
200.198151	7845.027296	26.130714
200.175955	7851.961470	26.135732
200.532353	7864.555726	26.140749
200.747122	7888.940939	26.145767
200.900131	7907.742557	26.150784
201.560975	7892.325397	26.155802
202.178269	7905.951107	26.160820
202.223148	7909.298740	26.165837
202.537850	7909.424470	26.170855
202.743058	7905.117071	26.175872
202.704806	7911.746778	26.180890
203.162942	7912.865768	26.185908
203.159952	7919.008871	26.190925
203.320658	7927.110768	26.195943
203.242428	7948.251684	26.200960
203.427410	7953.159594	26.205978
203.864379	7954.363360	26.210996
203.710973	7969.772486	26.216013
203.779641	7977.380472	26.221031
204.160752	7989.648376	26.226048
204.090592	8001.599740	26.231066
204.388836	8020.590091	26.236084
204.435329	8034.127045	26.241101
205.138010	8043.948067	26.246119
204.696697	8064.540820	26.251136
205.326827	8072.970410	26.256154
205.488728	8082.783315	26.261172
205.404447	8105.253732	26.266189
206.006220	8104.993069	26.271207
206.264405	8133.341807	26.276224
205.961009	8136.093724	26.281242
206.574202	8149.241351	26.286260
207.081214	8168.607332	26.291277
207.331867	8170.146364	26.296295
207.391316	8175.409896	26.301312
207.665373	8190.430042	26.306330
207.972368	8196.650892	26.311348
208.108157	8197.409190	26.316365
208.686820	8199.868108	26.321383
208.635494	8214.791216	26.326400
208.892656	8222.624625	26.331418
208.994767	8219.389710	26.336436
209.211202	8209.919283	26.341453
210.176712	8232.283979	26.346471
210.104270	8240.492965	26.351488
210.241626	8238.239148	26.356506
210.398227	8238.496763	26.361524
210.444154	8240.259185	26.366541
210.789191	8227.554747	26.371559
210.834691	8239.080733	26.376576
211.000846	8232.059588	26.381594
211.189209	8243.374374	26.386612
211.131634	8264.404233	26.391629
211.290993	8260.804188	26.396647
211.562253	8267.915131	26.401664
211.556061	8285.307488	26.406682
211.967287	8293.879502	26.411700
211.706691	8310.460704	26.416717
212.188856	8313.596382	26.421735
212.129034	8322.036443	26.426752
212.480155	8348.102263	26.431770
212.974496	8351.666803	26.436788
213.108234	8362.896497	26.441805
213.626073	8363.010258	26.446823
213.511273	8378.292618	26.451840
213.552229	8383.269468	26.456858
213.658538	8386.156031	26.461876
214.227017	8402.473885	26.466893
214.626873	8412.768535	26.471911
214.948789	8422.632214	26.476928
214.803845	8422.966734	26.481946
215.167736	8439.449688	26.486964
215.378046	8446.468740	26.491981
215.610715	8439.925348	26.496999
215.748169	8457.364173	26.502016
215.535798	8475.566520	26.507034
215.638791	8480.918804	26.512052
215.417788	8504.361767	26.517069
215.763840	8515.726134	26.522087
216.144443	8537.922081	26.527104
216.458601	8563.064937	26.532122
216.540378	8571.612425	26.537140
216.608874	8594.364592	26.542157
217.064286	8604.306344	26.547175
217.814514	8624.541929	26.552192
217.559743	8641.081504	26.557210
218.271559	8660.338916	26.562228
218.622470	8671.868008	26.567245
218.785485	8664.658131	26.572263
219.066341	8676.284322	26.577280
218.826252	8695.369326	26.582298
219.423892	8700.802341	26.587316
219.746502	8726.423014	26.592333
219.912516	8717.391098	26.597351
219.964705	8733.662279	26.602368
220.012023	8759.393222	26.607386
220.604711	8765.137520	26.612404
220.694998	8764.153045	26.617421
220.864371	8776.904558	26.622439
221.139009	8784.841607	26.627456
221.236169	8788.959645	26.632474
221.706638	8794.661876	26.637492
221.707641	8808.510601	26.642509
221.974402	8815.747828	26.647527
222.329461	8831.401514	26.652544
222.338389	8844.439000	26.657562
222.449813	8855.259239	26.662580
222.766594	8876.765405	26.667597
222.931499	8877.734617	26.672615
223.377594	8893.501967	26.677632
223.589142	8906.019451	26.682650
223.962696	8898.773382	26.687668
223.994180	8917.465439	26.692685
224.678491	8924.372723	26.697703
224.704622	8924.142973	26.702720
224.621068	8932.863170	26.707738
225.382131	8944.892561	26.712756
225.257771	8954.174417	26.717773
225.142441	8960.972976	26.722791
225.450440	8963.800648	26.727808
225.483766	8965.625974	26.732826
225.506348	8986.769879	26.737844
225.775003	9002.663871	26.742861
225.937542	9011.220597	26.747879
226.525918	9027.690098	26.752896
226.448939	9053.479057	26.757914
226.487098	9060.300194	26.762932
226.634866	9081.321917	26.767949
226.990253	9093.934647	26.772967
227.781792	9110.030625	26.777984
228.000059	9119.575294	26.783002
228.399038	9118.131345	26.788020
228.364871	9135.840621	26.793037
228.716591	9148.896804	26.798055
228.964001	9145.159351	26.803072
228.941017	9152.162763	26.808090
229.442782	9170.145781	26.813108
229.405342	9180.975999	26.818125
229.818194	9193.069993	26.823143
230.270254	9211.983386	26.828160
230.126935	9221.993486	26.833178
230.716489	9218.622819	26.838196
230.564775	9248.710919	26.843213
230.694209	9252.086095	26.848231
231.258559	9260.353473	26.853248
231.080847	9276.562187	26.858266
231.009882	9287.158709	26.863284
231.435173	9303.927477	26.868301
231.729441	9310.301427	26.873319
232.003120	9323.237190	26.878336
232.360633	9334.724657	26.883354
232.620136	9341.786881	26.888372
233.102456	9355.975873	26.893389
233.160978	9380.254612	26.898407
233.885700	9378.138683	26.903424
233.856491	9389.774418	26.908442
233.838448	9399.208487	26.913460
234.225132	9399.298260	26.918477
234.412363	9415.567466	26.923495
234.687495	9423.908141	26.928512
235.004443	9446.798558	26.933530
235.268189	9445.198125	26.938548
235.480993	9456.795575	26.943565
235.436942	9474.760615	26.948583
235.902381	9474.707677	26.953600
235.854385	9498.650305	26.958618
236.136981	9505.924523	26.963636
236.447979	9510.478822	26.968653
236.410737	9534.604025	26.973671
236.853368	9536.318287	26.978688
236.933803	9550.114637	26.983706
237.921612	9547.255524	26.988724
238.449793	9559.809060	26.993741
238.097221	9569.634635	26.998759
238.735922	9561.269719	27.003776
238.660357	9564.114396	27.008794
238.704856	9567.091344	27.013812
239.143762	9581.976592	27.018829
238.829994	9588.837793	27.023847
239.388033	9592.629639	27.028864
239.393226	9606.850214	27.033882
239.643896	9609.714616	27.038900
239.699709	9622.106501	27.043917
239.707605	9644.070037	27.048935
240.190715	9651.174433	27.053952
239.949074	9683.765343	27.058970
240.360424	9688.896564	27.063988
240.699250	9714.487663	27.069005
240.984477	9731.545618	27.074023
241.261444	9747.041820	27.079040
241.055751	9770.595871	27.084058
241.633631	9775.533116	27.089076
242.386994	9806.384224	27.094093
242.325115	9813.446591	27.099111
242.455105	9825.433542	27.104128
242.357309	9851.080789	27.109146
242.766903	9870.079448	27.114164
242.897448	9886.664551	27.119181
243.164290	9906.787636	27.124199
243.840138	9923.276153	27.129216
244.094530	9940.828116	27.134234
244.350024	9956.712698	27.139252
245.117451	9964.193968	27.144269
245.018320	9966.744926	27.149287
245.946866	9960.641846	27.154304
246.131215	9979.378263	27.159322
246.363045	9992.406830	27.164340
246.457190	9988.957043	27.169357
246.817188	9997.207829	27.174375
246.612079	9999.070991	27.179392
246.803171	10008.872976	27.184410
247.723853	10019.657709	27.189428
247.487630	10014.267980	27.194445
247.492102	10034.062728	27.199463
247.862429	10040.423931	27.204480
247.890512	10051.159981	27.209498
248.039522	10068.890880	27.214516
248.192878	10082.437235	27.219533
248.278364	10100.908666	27.224551
248.769901	10121.998882	27.229568
248.736483	10146.407989	27.234586
248.930339	10154.104276	27.239604
249.552687	10170.417845	27.244621
249.648220	10199.105381	27.249639
249.718041	10200.196555	27.254656
250.106509	10236.033948	27.259674
250.148184	10236.735989	27.264692
250.629849	10255.993793	27.269709
250.853291	10263.662999	27.274727
250.970084	10277.096020	27.279744
251.432637	10297.638312	27.284762
251.561103	10307.626131	27.289780
251.799305	10310.530617	27.294797
251.977614	10332.670735	27.299815
252.557648	10343.198906	27.304832
252.700975	10361.068198	27.309850
252.904721	10381.785755	27.314868
253.063776	10373.743749	27.319885
253.131475	10402.530967	27.324903
253.428963	10407.763881	27.329920
254.024654	10430.095757	27.334938
253.972637	10452.286548	27.339956
254.488219	10460.168941	27.344973
254.758386	10477.364212	27.349991
255.211019	10490.714630	27.355008
255.568627	10507.253568	27.360026
255.540364	10518.251722	27.365044
255.840364	10530.884526	27.370061
255.736252	10547.854067	27.375079
256.374703	10555.326205	27.380096
256.633760	10572.879629	27.385114
256.659163	10585.119875	27.390132
256.937282	10592.031324	27.395149
257.299868	10612.873233	27.400167
257.746151	10629.936046	27.405184
258.011028	10640.274172	27.410202
258.062111	10655.523152	27.415220
258.556951	10663.013654	27.420237
258.594488	10680.548433	27.425255
258.991810	10693.883285	27.430272
259.280934	10698.206865	27.435290
258.979523	10724.686213	27.440308
259.930384	10726.165360	27.445325
260.010525	10755.464809	27.450343
260.026451	10769.585280	27.455360
260.503139	10773.229039	27.460378
260.794938	10790.301167	27.465396
261.151804	10796.144932	27.470413
260.911024	10819.870408	27.475431
261.221280	10827.857515	27.480448
261.423057	10847.734474	27.485466
261.415337	10866.164442	27.490484
261.851129	10878.819942	27.495501
262.312405	10909.663337	27.500519
262.863526	10924.536892	27.505536
263.127144	10936.474969	27.510554
263.365200	10949.706531	27.515572
263.703348	10957.359557	27.520589
264.228798	10989.693947	27.525607
264.200024	10982.106182	27.530624
264.384404	10994.267480	27.535642
264.590749	11015.708744	27.540660
264.964624	11012.913653	27.545677
265.051963	11037.071736	27.550695
265.291143	11047.323123	27.555712
265.541569	11048.856174	27.560730
265.576963	11066.921245	27.565748
266.149145	11079.498367	27.570765
266.208208	11103.461254	27.575783
266.474629	11105.401309	27.580800
266.981894	11125.144297	27.585818
266.924085	11136.426872	27.590836
267.447770	11147.612936	27.595853
267.282756	11175.087684	27.600871
267.843528	11189.442923	27.605888
268.599827	11203.227267	27.610906
268.213040	11216.800962	27.615924
268.960993	11230.273148	27.620941
268.903679	11248.325944	27.625959
270.217726	11258.333341	27.630976
271.035852	11262.139321	27.635994
270.718876	11261.771355	27.641012
270.962485	11257.964734	27.646029
270.987600	11264.406081	27.651047
271.013343	11253.734186	27.656064
271.349247	11257.451042	27.661082
271.203394	11270.769157	27.666100
271.485412	11271.170016	27.671117
271.376135	11301.870832	27.676135
271.787547	11311.185121	27.681152
272.280113	11335.622474	27.686170
272.375472	11353.395490	27.691188
272.539002	11368.042761	27.696205
272.919537	11387.502056	27.701223
272.815033	11410.491124	27.706240
273.286454	11417.850460	27.711258
273.363784	11453.181252	27.716276
274.029779	11470.703718	27.721293
273.893636	11492.826819	27.726311
274.513260	11511.170474	27.731328
274.966950	11535.321660	27.736346
274.966240	11550.329776	27.741364
274.711281	11569.430151	27.746381
275.223655	11596.830477	27.751399
275.580972	11612.757537	27.756416
276.250254	11632.353597	27.761434
276.425706	11663.025199	27.766452
276.678067	11676.371523	27.771469
276.692908	11700.620238	27.776487
277.316603	11719.371610	27.781504
277.800963	11736.107560	27.786522
277.756252	11758.421802	27.791540
278.657224	11767.006285	27.796557
278.873544	11790.003936	27.801575
278.930554	11796.284002	27.806592
279.699284	11804.750909	27.811610
279.281334	11810.939032	27.816628
279.745577	11815.760855	27.821645
279.843227	11838.391220	27.826663
279.982436	11843.016603	27.831680
280.372959	11860.329820	27.836698
280.686092	11879.055808	27.841716
281.050912	11888.112070	27.846733
281.064965	11912.436883	27.851751
280.864028	11920.717030	27.856768
281.575413	11937.838220	27.861786
281.757075	11961.669455	27.866804
282.212228	11968.592125	27.871821
282.695083	11982.349931	27.876839
283.160711	11991.968944	27.881856
283.529960	12005.684778	27.886874
284.024183	12027.825060	27.891892
283.880247	12028.142925	27.896909
284.197779	12043.092218	27.901927
284.113006	12065.139517	27.906944
284.501408	12067.120248	27.911962
285.008961	12086.030640	27.916980
285.054023	12108.016343	27.921997
285.585883	12119.543675	27.927015
285.990400	12138.717648	27.932032
286.402104	12148.604465	27.937050
286.533478	12161.108261	27.942068
286.961592	12176.536747	27.947085
287.460913	12184.247833	27.952103
287.207077	12205.459059	27.957120
287.836711	12215.270739	27.962138
287.835518	12232.293733	27.967156
287.927542	12251.773566	27.972173
288.555578	12269.292369	27.977191
288.462205	12293.005745	27.982208
289.119058	12295.347109	27.987226
289.019439	12308.361846	27.992244
289.653229	12316.046795	27.997261
289.826361	12331.374136	28.002279
289.818862	12344.349472	28.007296
290.625925	12361.861330	28.012314
290.631051	12381.950382	28.017332
291.152955	12399.148665	28.022349
291.215511	12415.754302	28.027367
291.451021	12432.744812	28.032384
291.803333	12443.827181	28.037402
291.805194	12464.542587	28.042420
292.413927	12482.526713	28.047437
293.130565	12499.444284	28.052455
292.933447	12516.799029	28.057472
293.458427	12527.267141	28.062490
293.620483	12534.418386	28.067508
293.674803	12550.863236	28.072525
294.262520	12558.611360	28.077543
294.291470	12585.492573	28.082560
294.940584	12592.393298	28.087578
295.413794	12610.098188	28.092596
295.480230	12624.668664	28.097613
296.241954	12621.143303	28.102631
295.761619	12640.338715	28.107648
296.465776	12656.346043	28.112666
296.397861	12668.525040	28.117684
296.835418	12684.247114	28.122701
297.040282	12690.554192	28.127719
297.102235	12719.278707	28.132736
297.579190	12725.398891	28.137754
297.862522	12745.158585	28.142772
297.867332	12759.326810	28.147789
298.252608	12783.374940	28.152807
298.318428	12793.920348	28.157824
298.882253	12806.848559	28.162842
299.342210	12833.449836	28.167860
299.855341	12851.978747	28.172877
299.847376	12855.258442	28.177895
300.107052	12879.340850	28.182912
300.608457	12894.516310	28.187930
300.124257	12919.230627	28.192948
300.365691	12940.547044	28.197965
301.073822	12961.124686	28.202983
301.536595	12989.070149	28.208000
301.893076	13009.711277	28.213018
302.317170	13027.609443	28.218036
303.147092	13038.424374	28.223053
303.678805	13049.621408	28.228071
303.717435	13070.159480	28.233088
304.121337	13065.207506	28.238106
304.114958	13087.528018	28.243124
304.502902	13097.154697	28.248141
304.974611	13105.173570	28.253159
305.365749	13120.045036	28.258176
305.523127	13130.300722	28.263194
305.878731	13153.884798	28.268212
305.804706	13171.476043	28.273229
305.967281	13181.379395	28.278247
305.861726	13203.852610	28.283264
306.001511	13225.402749	28.288282
306.353587	13243.291428	28.293300
306.612749	13283.851398	28.298317
307.140547	13310.440245	28.303335
307.372972	13335.981192	28.308352
307.838015	13354.432226	28.313370
308.030485	13372.176603	28.318388
308.204024	13400.679859	28.323405
309.047547	13426.779765	28.328423
308.799536	13450.961059	28.333440
309.531439	13470.465062	28.338458
309.848534	13495.433787	28.343476
310.240705	13514.520072	28.348493
310.569814	13533.133308	28.353511
310.409959	13556.894575	28.358528
311.166365	13576.731804	28.363546
311.284922	13596.203956	28.368564
311.276874	13614.172101	28.373581
311.796180	13628.683185	28.378599
311.953413	13657.252727	28.383616
312.345733	13673.081227	28.388634
312.544787	13698.622152	28.393652
312.801538	13727.808382	28.398669
313.427190	13744.600984	28.403687
313.346512	13766.025694	28.408704
313.837466	13784.133891	28.413722
314.381849	13806.914219	28.418740
314.705473	13836.730688	28.423757
315.000321	13851.411263	28.428775
315.097051	13872.430572	28.433792
315.367995	13895.962447	28.438810
315.917412	13917.846788	28.443828
315.723935	13947.250854	28.448845
316.228227	13968.528280	28.453863
316.484276	14001.348256	28.458880
316.954204	14022.519731	28.463898
317.550349	14050.753077	28.468916
317.615263	14074.527003	28.473933
318.123021	14090.400744	28.478951
318.518239	14110.983025	28.483968
319.664959	14120.628422	28.488986
320.350882	14132.406611	28.494004
320.335935	14145.302678	28.499021
320.969519	14144.517945	28.504039
320.789654	14157.292547	28.509056
321.145567	14161.574084	28.514074
321.451450	14179.077645	28.519092
321.130455	14196.819494	28.524109
321.542890	14208.291538	28.529127
321.561605	14233.884692	28.534144
322.000150	14253.652698	28.539162
322.864400	14283.025815	28.544180
322.579341	14299.131793	28.549197
322.783318	14311.791863	28.554215
323.300507	14339.489133	28.559232
323.490849	14366.247862	28.564250
324.088756	14395.048943	28.569268
324.284344	14415.941663	28.574285
324.815158	14432.926188	28.579303
324.826037	14459.829317	28.584320
325.035316	14484.788071	28.589338
325.503076	14495.677079	28.594356
325.518632	14530.539588	28.599373
326.573983	14539.127466	28.604391
326.713457	14556.535425	28.609408
326.951160	14583.566963	28.614426
327.457915	14601.963385	28.619444
327.885344	14621.951263	28.624461
328.309439	14634.670007	28.629479
329.007041	14642.250548	28.634496
329.527743	14639.205865	28.639514
330.026276	14646.383903	28.644532
330.219188	14665.738963	28.649549
330.638074	14670.832652	28.654567
330.777417	14663.315253	28.659584
330.846822	14660.445642	28.664602
331.126802	14671.608121	28.669620
331.216816	14686.813192	28.674637
331.545750	14697.751348	28.679655
331.376110	14709.262031	28.684672
331.182998	14737.929744	28.689690
332.086726	14757.500407	28.694708
332.037766	14787.997199	28.699725
332.131306	14805.063359	28.704743
332.237526	14831.887701	28.709760
332.913894	14869.905301	28.714778
333.316412	14896.928019	28.719796
333.632246	14927.721940	28.724813
333.832747	14945.349987	28.729831
334.297863	14984.130727	28.734848
334.502248	15006.920548	28.739866
335.055990	15032.111129	28.744884
335.331605	15071.186218	28.749901
335.670419	15088.456536	28.754919
335.783689	15120.128856	28.759936
336.303985	15143.020774	28.764954
336.626788	15175.429681	28.769972
336.763367	15204.120507	28.774989
337.213935	15238.066617	28.780007
337.858575	15256.801116	28.785024
338.331721	15279.113335	28.790042
338.976124	15300.614375	28.795060
339.888929	15321.862942	28.800077
340.241007	15334.736439	28.805095
340.334301	15334.414697	28.810112
340.807378	15365.805133	28.815130
341.184413	15369.840612	28.820148
341.253714	15394.028680	28.825165
341.686247	15407.298292	28.830183
341.787722	15420.033527	28.835200
341.888742	15444.022342	28.840218
342.214690	15452.314835	28.845236
342.459610	15487.335511	28.850253
343.027544	15513.314142	28.855271
343.146057	15534.809462	28.860288
343.005099	15561.592224	28.865306
343.690128	15582.394649	28.870324
343.577090	15623.698831	28.875341
344.227068	15650.710318	28.880359
344.532058	15675.236726	28.885376
344.541529	15711.802078	28.890394
345.018074	15744.199933	28.895412
345.325080	15779.440733	28.900429
345.744700	15802.848952	28.905447
346.512944	15835.088222	28.910464
346.695128	15865.607278	28.915482
347.307409	15881.242562	28.920500
347.538986	15907.839075	28.925517
347.614618	15921.157657	28.930535
348.411204	15942.964490	28.935552
348.491907	15968.770390	28.940570
349.232642	15986.202912	28.945588
349.098071	16014.186517	28.950605
349.324586	16027.165622	28.955623
349.845275	16049.686697	28.960640
350.239436	16071.827507	28.965658
350.465985	16094.202004	28.970676
350.925812	16126.504157	28.975693
351.388404	16140.532186	28.980711
352.208576	16158.644895	28.985728
352.196814	16189.445281	28.990746
352.338157	16208.379043	28.995764
352.887209	16234.683629	29.000781
353.093539	16248.799809	29.005799
353.693125	16263.375126	29.010816
354.165760	16286.210583	29.015834
355.130945	16295.776464	29.020852
355.623135	16309.000318	29.025869
356.124430	16313.232280	29.030887
356.664509	16310.409410	29.035904
356.003730	16333.650425	29.040922
356.628061	16343.566391	29.045940
356.792899	16351.399832	29.050957
356.826180	16382.949541	29.055975
357.365910	16384.821326	29.060992
357.316423	16425.396174	29.066010
357.703846	16444.165067	29.071028
358.011506	16475.571764	29.076045
358.034250	16495.391643	29.081063
359.082179	16526.742504	29.086080
358.833483	16559.860565	29.091098
359.303140	16580.827273	29.096116
359.901221	16607.803496	29.101133
360.167089	16635.459399	29.106151
360.501228	16663.573430	29.111168
360.678019	16689.321413	29.116186
361.029540	16715.433604	29.121204
361.665958	16751.569035	29.126221
362.046978	16775.253239	29.131239
362.566008	16794.586418	29.136256
363.035889	16823.074724	29.141274
363.715127	16839.008427	29.146292
363.998947	16862.528119	29.151309
364.577568	16879.792309	29.156327
364.772259	16885.790597	29.161344
365.093145	16919.590531	29.166362
365.729479	16931.223157	29.171380
365.695653	16936.861778	29.176397
365.596935	16959.493396	29.181415
366.437080	16981.710325	29.186432
366.067559	17016.817451	29.191450
366.583499	17030.446121	29.196468
367.086266	17046.106004	29.201485
367.751092	17079.259285	29.206503
368.147128	17093.660544	29.211520
367.755981	17118.623686	29.216538
368.414640	17133.107666	29.221556
368.596901	17166.591334	29.226573
368.898750	17192.906696	29.231591
369.167271	17219.607749	29.236608
369.547200	17254.577470	29.241626
369.607884	17286.559304	29.246644
370.271577	17314.400393	29.251661
370.361125	17346.995391	29.256679
371.055154	17376.746857	29.261696
371.482816	17413.206426	29.266714
372.026358	17439.952135	29.271732
372.429816	17465.058655	29.276749
372.592513	17490.088234	29.281767
373.260568	17516.301930	29.286784
373.991800	17541.417028	29.291802
374.648961	17568.294819	29.296820
374.968510	17585.739724	29.301837
375.203008	17599.645693	29.306855
375.462416	17621.759631	29.311872
375.486753	17655.023823	29.316890
375.814375	17677.688972	29.321908
376.268275	17693.145005	29.326925
376.852760	17728.646643	29.331943
377.116584	17748.076692	29.336960
376.825314	17782.263909	29.341978
377.069107	17813.792849	29.346996
377.721682	17853.241833	29.352013
378.144729	17892.077547	29.357031
378.640460	17913.807677	29.362048
379.112776	17943.639141	29.367066
379.646892	17979.263455	29.372084
380.171413	18011.335872	29.377101
380.697339	18032.315257	29.382119
381.319743	18051.215959	29.387136
381.768249	18079.350609	29.392154
381.711141	18093.521380	29.397172
382.299557	18113.490599	29.402189
382.546510	18143.605414	29.407207
383.141574	18162.793139	29.412224
383.274326	18191.902824	29.417242
383.786452	18217.316628	29.422260
384.070678	18238.514274	29.427277
384.004082	18270.422046	29.432295
384.871896	18288.804823	29.437312
385.632119	18305.776074	29.442330
386.690326	18302.285471	29.447348
387.445924	18324.034663	29.452365
387.606240	18341.329488	29.457383
388.494578	18338.410345	29.462400
388.590468	18337.397547	29.467418
388.517955	18335.357280	29.472436
389.248282	18332.965004	29.477453
389.182795	18341.895183	29.482471
389.645202	18352.041912	29.487488
389.722151	18367.399202	29.492506
389.610817	18374.864698	29.497524
390.083388	18389.627618	29.502541
390.382636	18408.574647	29.507559
390.846535	18422.230719	29.512576
390.956663	18447.521419	29.517594
391.230980	18466.939468	29.522612
391.606708	18488.019268	29.527629
391.875883	18519.231435	29.532647
391.975565	18548.183436	29.537664
392.079884	18571.870306	29.542682
392.496895	18614.464273	29.547700
393.312917	18645.417409	29.552717
393.792633	18689.400878	29.557735
394.215539	18718.266245	29.562752
394.485659	18742.129904	29.567770
394.774138	18764.437448	29.572788
395.335355	18784.856747	29.577805
395.227675	18823.285771	29.582823
396.018671	18857.592411	29.587840
396.576861	18883.885415	29.592858
396.584531	18925.115555	29.597876
397.196421	18954.432977	29.602893
397.827339	18991.911207	29.607911
397.911938	19018.902065	29.612928
398.436131	19045.316245	29.617946
399.042278	19072.616708	29.622964
400.054547	19090.817946	29.627981
400.453645	19125.997982	29.632999
400.968768	19139.105056	29.638016
401.652686	19158.431634	29.643034
401.744672	19174.074041	29.648052
401.739139	19198.162176	29.653069
402.047218	19224.258919	29.658087
402.478891	19250.602560	29.663104
403.000143	19274.447587	29.668122
402.692505	19299.426445	29.673140
403.234351	19330.500360	29.678157
403.155701	19371.697505	29.683175
403.759165	19399.727398	29.688192
403.931000	19438.023198	29.693210
404.351420	19480.625076	29.698228
405.096334	19514.680795	29.703245
405.091191	19562.358754	29.708263
405.141001	19606.678450	29.713280
406.071476	19642.219442	29.718298
406.295575	19680.598285	29.723316
406.799046	19723.557076	29.728333
407.188019	19758.571453	29.733351
407.908726	19792.013796	29.738368
408.673411	19828.327819	29.743386
409.069303	19853.024519	29.748404
409.516395	19874.770253	29.753421
409.810171	19905.747408	29.758439
410.567133	19926.552390	29.763456
410.936440	19948.940677	29.768474
410.989848	19987.172870	29.773492
411.781516	20000.239530	29.778509
411.737372	20035.749704	29.783527
412.255144	20057.548208	29.788544
412.900416	20085.376556	29.793562
412.997934	20114.106132	29.798580
413.364367	20138.295844	29.803597
413.442088	20169.638480	29.808615
413.952823	20197.141599	29.813632
414.752632	20233.445743	29.818650
414.983589	20264.655072	29.823668
416.288509	20275.175770	29.828685
416.655635	20299.926933	29.833703
417.170541	20318.083867	29.838720
417.896610	20336.903154	29.843738
417.900698	20361.629899	29.848756
418.499775	20376.850657	29.853773
418.754491	20386.963255	29.858791
419.284332	20419.974395	29.863808
419.645381	20435.847800	29.868826
419.632205	20463.031165	29.873844
420.090822	20481.931139	29.878861
420.120519	20515.578483	29.883879
420.653402	20536.780557	29.888896
421.252902	20562.266500	29.893914
421.636239	20598.346358	29.898932
422.310977	20620.982790	29.903949
422.504654	20648.638741	29.908967
422.714139	20674.123886	29.913984
423.271040	20709.073608	29.919002
423.434518	20745.814306	29.924020
424.163424	20771.907547	29.929037
424.575725	20805.431554	29.934055
424.656707	20837.766698	29.939072
425.330971	20864.984277	29.944090
425.685013	20893.735861	29.949108
426.090001	20918.968688	29.954125
426.639080	20950.093223	29.959143
426.913471	20980.541111	29.964160
427.300031	21021.206823	29.969178
427.875204	21057.644267	29.974196
428.391526	21086.521324	29.979213
428.625103	21105.622976	29.984231
429.179244	21140.462101	29.989248
430.198585	21163.281466	29.994266
430.309619	21193.811344	29.999284
430.924713	21225.030722	30.004301
431.314139	21244.072708	30.009319
431.178057	21275.220642	30.014336
431.746673	21301.914578	30.019354
431.898359	21341.320371	30.024372
432.433146	21358.735452	30.029389
432.714692	21395.334321	30.034407
433.237400	21423.848172	30.039424
434.041706	21447.234609	30.044442
434.281129	21473.668271	30.049460
434.518406	21504.954486	30.054477
435.033053	21528.713940	30.059495
435.383577	21551.457637	30.064512
435.960053	21584.522973	30.069530
436.006438	21618.838249	30.074548
436.579600	21643.475641	30.079565
437.392268	21671.514448	30.084583
437.656186	21714.334832	30.089600
438.213160	21744.126966	30.094618
438.193769	21776.403822	30.099636
438.856561	21811.635705	30.104653
439.297277	21840.443422	30.109671
439.744848	21876.964412	30.114688
440.341277	21907.208960	30.119706
440.426166	21945.653044	30.124724
440.989492	21967.917707	30.129741
441.690728	22004.020185	30.134759
441.937468	22041.487422	30.139776
442.459089	22073.293656	30.144794
442.765311	22108.410638	30.149812
443.096258	22138.738939	30.154829
443.161265	22177.839815	30.159847
443.257149	22225.252449	30.164864
444.307870	22260.399858	30.169882
444.480843	22308.897090	30.174900
445.114234	22336.019948	30.179917
445.425234	22378.800812	30.184935
445.823043	22424.276179	30.189952
446.630254	22467.379095	30.194970
446.953524	22506.789712	30.199988
447.749107	22544.135610	30.205005
448.242369	22578.896643	30.210023
448.608298	22618.707075	30.215040
449.545414	22646.961137	30.220058
449.835258	22684.170072	30.225076
450.179687	22714.755715	30.230093
450.791497	22738.252613	30.235111
450.897889	22772.796471	30.240128
451.644210	22804.243848	30.245146
452.091871	22833.152979	30.250164
452.694907	22863.707187	30.255181
453.332390	22895.570795	30.260199
453.307240	22927.601634	30.265216
453.906265	22944.698231	30.270234
454.692769	22978.551914	30.275252
455.412079	22995.208456	30.280269
455.866798	23015.521793	30.285287
456.291806	23038.887104	30.290304
456.432561	23058.213441	30.295322
457.064324	23099.086525	30.300340
457.293203	23102.784978	30.305357
457.801515	23126.640791	30.310375
458.030149	23159.864986	30.315392
458.500336	23183.982896	30.320410
458.439848	23215.736456	30.325428
458.958488	23247.494920	30.330445
459.551265	23267.841672	30.335463
460.067705	23305.662879	30.340480
460.708738	23323.380333	30.345498
461.005653	23364.163184	30.350516
461.177301	23385.705123	30.355533
462.116707	23418.927878	30.360551
462.450154	23457.222360	30.365568
463.056206	23476.857397	30.370586
463.916861	23517.925666	30.375604
464.356608	23530.044452	30.380621
464.797168	23552.625560	30.385639
465.024242	23580.860905	30.390656
465.350031	23609.303329	30.395674
465.513942	23636.969217	30.400692
466.036554	23670.913651	30.405709
466.432203	23699.555585	30.410727
466.550538	23751.103766	30.415744
467.256696	23782.477813	30.420762
467.282150	23822.737353	30.425780
467.443026	23863.655099	30.430797
468.414781	23895.333961	30.435815
468.406051	23940.611745	30.440832
469.224720	23986.227313	30.445850
469.635927	24036.483378	30.450868
470.398240	24070.100484	30.455885
470.802091	24119.651491	30.460903
471.535659	24162.869074	30.465920
472.023712	24193.457973	30.470938
472.346355	24231.655091	30.475956
472.868685	24273.268905	30.480973
473.340717	24310.677252	30.485991
473.703383	24353.917866	30.491008
474.198980	24399.839085	30.496026
474.916622	24437.092062	30.501044
475.036920	24479.270498	30.506061
475.762225	24512.929509	30.511079
476.155907	24560.127211	30.516096
476.705935	24592.794395	30.521114
477.327299	24632.083097	30.526132
477.400148	24672.304950	30.531149
478.118845	24706.539572	30.536167
478.647785	24749.380464	30.541184
478.664285	24791.517514	30.546202
479.348526	24834.391938	30.551220
479.438189	24880.059087	30.556237
480.360968	24919.728951	30.561255
480.536319	24963.567833	30.566272
481.341746	25008.033845	30.571290
482.052722	25040.857256	30.576308
481.912814	25087.201491	30.581325
482.744307	25113.651283	30.586343
482.891334	25161.000142	30.591360
483.440391	25189.085154	30.596378
484.112584	25230.861709	30.601396
484.531498	25269.820630	30.606413
485.150686	25304.761171	30.611431
485.421335	25354.171351	30.616448
486.119031	25390.000805	30.621466
486.738201	25423.216062	30.626484
486.970609	25466.488086	30.631501
487.852997	25504.939098	30.636519
487.735070	25540.561625	30.641536
488.313580	25574.512842	30.646554
489.330662	25617.007252	30.651572
489.395076	25661.368483	30.656589
490.222004	25691.267895	30.661607
491.022297	25728.686151	30.666624
491.591967	25746.569754	30.671642
492.509743	25774.538906	30.676660
492.792043	25805.033422	30.681677
493.041449	25833.300165	30.686695
493.432899	25876.255733	30.691712
493.834562	25905.982328	30.696730
494.538972	25946.594189	30.701748
494.424273	25980.844801	30.706765
495.430154	26010.647853	30.711783
495.933652	26054.953777	30.716800
496.123571	26082.357281	30.721818
497.319743	26110.244571	30.726836
497.948082	26149.497665	30.731853
498.330907	26168.691361	30.736871
499.122732	26187.915944	30.741888
499.705539	26217.820242	30.746906
500.502002	26232.431942	30.751924
500.453617	26262.655838	30.756941
501.061049	26282.173961	30.761959
501.449939	26318.783830	30.766976
501.870473	26344.782248	30.771994
502.611269	26373.255900	30.777012
502.402735	26401.949055	30.782029
502.916877	26434.647947	30.787047
503.742586	26470.501866	30.792064
503.731331	26508.556159	30.797082
504.332287	26539.987945	30.802100
504.359401	26587.042606	30.807117
504.963930	26616.909167	30.812135
505.750180	26664.016930	30.817152
506.008902	26715.691829	30.822170
506.433662	26745.400128	30.827188
506.776134	26793.877742	30.832205
507.846796	26832.592832	30.837223
507.878523	26868.813922	30.842240
508.544338	26902.140745	30.847258
508.952518	26934.707302	30.852276
509.180073	26986.987758	30.857293
509.951666	27025.249752	30.862311
510.442647	27071.286095	30.867328
510.122890	27111.940512	30.872346
510.677196	27151.599752	30.877364
510.896526	27205.450227	30.882381
512.145963	27245.889703	30.887399
512.647184	27294.048100	30.892416
513.419432	27333.746126	30.897434
513.906604	27369.546329	30.902452
514.168983	27420.348781	30.907469
515.225525	27463.386744	30.912487
515.587444	27499.574644	30.917504
516.181604	27548.900909	30.922522
516.789340	27583.589290	30.927540
517.582641	27618.018789	30.932557
518.050720	27638.862145	30.937575
518.870135	27682.606972	30.942592
519.349476	27720.362145	30.947610
520.195403	27751.347151	30.952628
520.786295	27779.050586	30.957645
521.139648	27809.489107	30.962663
521.706239	27833.316186	30.967680
522.010149	27866.722639	30.972698
522.657887	27898.521145	30.977716
522.782955	27933.696764	30.982733
523.110040	27971.412312	30.987751
523.859776	28002.508896	30.992768
523.995108	28046.810396	30.997786
524.407108	28091.597798	31.002804
524.597657	28136.366470	31.007821
525.165220	28180.212486	31.012839
525.658815	28224.121767	31.017856
525.994200	28285.966319	31.022874
526.595764	28334.709843	31.027892
527.112111	28385.017241	31.032909
527.783426	28436.730635	31.037927
528.308326	28494.435538	31.042944
529.000125	28541.081815	31.047962
529.808062	28570.891623	31.052980
530.217628	28628.843896	31.057997
531.309446	28658.652537	31.063015
531.988868	28705.159391	31.068032
532.316505	28751.202893	31.073050
532.718203	28779.419908	31.078068
533.246337	28817.828505	31.083085
533.422768	28861.090124	31.088103
534.038970	28905.163097	31.093120
534.638780	28954.687965	31.098138
535.357040	28994.774472	31.103156
535.466720	29041.581769	31.108173
536.163473	29080.287030	31.113191
537.356395	29114.338633	31.118208
537.995557	29151.533114	31.123226
538.657188	29173.916423	31.128244
539.119808	29205.206321	31.133261
539.817755	29224.336758	31.138279
539.801309	29245.741485	31.143296
540.775974	29274.940205	31.148314
541.210742	29297.476133	31.153332
541.634030	29340.292761	31.158349
542.442343	29363.376885	31.163367
542.428461	29390.511268	31.168384
542.534678	29429.914826	31.173402
543.296263	29463.867476	31.178420
543.784851	29503.909304	31.183437
544.142446	29549.473313	31.188455
544.710204	29583.352125	31.193472
545.243023	29631.066620	31.198490
545.790649	29669.170825	31.203508
546.092624	29712.151129	31.208525
546.538837	29755.990310	31.213543
547.390276	29796.466014	31.218560
547.785953	29852.294845	31.223578
548.463913	29888.300984	31.228596
548.996231	29944.968102	31.233613
549.607375	29984.295844	31.238631
550.128066	30029.094789	31.243648
550.583887	30081.954311	31.248666
551.124146	30120.991587	31.253684
551.894885	30157.162234	31.258701
552.482692	30207.023988	31.263719
553.153269	30250.239047	31.268736
553.834985	30295.654779	31.273754
554.438606	30335.028765	31.278772
555.206722	30370.389356	31.283789
555.832584	30398.990224	31.288807
556.326041	30432.034585	31.293824
556.865663	30472.546332	31.298842
557.460967	30509.312583	31.303860
557.875016	30554.494006	31.308877
558.560232	30598.802351	31.313895
559.177137	30626.250222	31.318912
559.349402	30654.074091	31.323930
559.933863	30704.717220	31.328948
560.570925	30752.921754	31.333965
560.585260	30794.843235	31.338983
561.726012	30837.363845	31.344000
561.874557	30890.871661	31.349018
562.584944	30930.247610	31.354036
563.014070	30980.653077	31.359053
563.652701	31028.100762	31.364071
563.968808	31070.719049	31.369088
564.226913	31124.764172	31.374106
565.078784	31184.838986	31.379124
565.197771	31230.486062	31.384141
565.612190	31292.848251	31.389159
566.417757	31346.156503	31.394176
566.437816	31408.340529	31.399194
567.387235	31460.002494	31.404212
568.098309	31513.519930	31.409229
568.361938	31555.280571	31.414247
569.362297	31606.874277	31.419264
569.584782	31664.013353	31.424282
570.549434	31704.082716	31.429300
570.970399	31763.441242	31.434317
571.063730	31811.584022	31.439335
571.805488	31865.520118	31.444352
572.527559	31927.412105	31.449370
573.038516	31984.029423	31.454388
573.585892	32031.072550	31.459405
573.920420	32096.862563	31.464423
575.007560	32138.925271	31.469440
575.353581	32190.992534	31.474458
575.879706	32237.626443	31.479476
576.716774	32295.059859	31.484493
577.232720	32351.030553	31.489511
578.105597	32391.887195	31.494528
578.706035	32455.136744	31.499546
579.852498	32485.829267	31.504564
580.757776	32521.776550	31.509581
581.255296	32564.569291	31.514599
582.022185	32607.751484	31.519616
582.353915	32646.391370	31.524634
582.739453	32682.131379	31.529652
583.709530	32731.170992	31.534669
584.108398	32773.889616	31.539687
584.591776	32810.313715	31.544704
585.142761	32855.474348	31.549722
585.598650	32897.886847	31.554740
586.227870	32940.493816	31.559757
586.348300	32982.859848	31.564775
587.475432	33026.811327	31.569792
587.658007	33077.214456	31.574810
588.009753	33130.750962	31.579828
589.285854	33182.333535	31.584845
589.368385	33227.783658	31.589863
589.803641	33273.741529	31.594880
590.532446	33332.367672	31.599898
591.221112	33379.194463	31.604916
591.490492	33423.843014	31.609933
592.293200	33485.928552	31.614951
592.954161	33527.212280	31.619968
593.379183	33587.570284	31.624986
593.788417	33633.618745	31.630004
594.902407	33682.409071	31.635021
595.678014	33729.392303	31.640039
596.217420	33771.155040	31.645056
596.888278	33821.514465	31.650074
597.677276	33870.266304	31.655092
598.263852	33907.820589	31.660109
598.865961	33962.642213	31.665127
599.957664	33986.258201	31.670144
600.545485	34028.189978	31.675162
600.645767	34049.160701	31.680180
601.160079	34097.385813	31.685197
601.767266	34131.866172	31.690215
602.353455	34159.848650	31.695232
602.827481	34189.923942	31.700250
603.632598	34236.821385	31.705268
604.449460	34272.582184	31.710285
604.196068	34317.524507	31.715303
605.228732	34358.661244	31.720320
605.783705	34403.417940	31.725338
605.965042	34447.796904	31.730356
606.822357	34486.170791	31.735373
607.463437	34535.782996	31.740391
607.924010	34581.294848	31.745408
608.357221	34621.692194	31.750426
608.767483	34667.443282	31.755444
609.448815	34727.584440	31.760461
609.599319	34785.099258	31.765479
610.384004	34833.264231	31.770496
610.993868	34891.316144	31.775514
611.559710	34950.417340	31.780532
612.222439	35004.935056	31.785549
612.796025	35076.199473	31.790567
613.599745	35138.915464	31.795584
614.313554	35195.735385	31.800602
614.806440	35253.805345	31.805620
615.712970	35301.695030	31.810637
615.723226	35364.008018	31.815655
616.384486	35419.335244	31.820672
617.530187	35484.525199	31.825690
617.756372	35551.883511	31.830708
618.407387	35613.285864	31.835725
619.006893	35671.847065	31.840743
619.591792	35733.463159	31.845760
620.638888	35801.944296	31.850778
620.701594	35854.215865	31.855796
621.594287	35912.699203	31.860813
622.101157	35979.919473	31.865831
622.416788	36040.354897	31.870848
623.513348	36098.775498	31.875866
624.055673	36170.169504	31.880884
624.641685	36226.200181	31.885901
625.454545	36287.987421	31.890919
626.175660	36344.721301	31.895936
626.846003	36398.377022	31.900954
627.169768	36458.929229	31.905972
628.914929	36513.644801	31.910989
629.027903	36577.787733	31.916007
629.531195	36624.089666	31.921024
630.402694	36669.943538	31.926042
630.632962	36730.746248	31.931060
631.208940	36785.262068	31.936077
631.455874	36848.312929	31.941095
632.032977	36907.061861	31.946112
633.110287	36958.910238	31.951130
634.175200	37016.082887	31.956148
634.921929	37056.757058	31.961165
635.205647	37087.816735	31.966183
636.119268	37136.521283	31.971200
637.253515	37174.859728	31.976218
638.240227	37215.622560	31.981236
638.820585	37247.187251	31.986253
639.385134	37274.966752	31.991271
639.561424	37315.669784	31.996288
640.252808	37354.447493	32.001306
640.461524	37406.957331	32.006324
641.115377	37442.553439	32.011341
641.649828	37496.384030	32.016359
642.030695	37545.834373	32.021376
642.504842	37595.145757	32.026394
643.242790	37653.992641	32.031412
643.602047	37706.123994	32.036429
644.096300	37775.733184	32.041447
644.910027	37831.142619	32.046464
645.439312	37894.104510	32.051482
646.102737	37956.920522	32.056500
647.010719	38024.764603	32.061517
647.413111	38089.248361	32.066535
648.149645	38147.626712	32.071552
648.840972	38205.148033	32.076570
649.183041	38272.597522	32.081588
650.199285	38345.699253	32.086605
650.650740	38401.687034	32.091623
651.319797	38465.305651	32.096640
652.031111	38516.940187	32.101658
652.569378	38589.982718	32.106676
653.556182	38653.118215	32.111693
654.615621	38711.891310	32.116711
655.471899	38770.105905	32.121728
656.326125	38814.276016	32.126746
656.894034	38868.490033	32.131764
658.436995	38897.433426	32.136781
659.177552	38937.203638	32.141799
660.174095	38973.694238	32.146816
661.152298	39000.695178	32.151834
661.733505	39023.319217	32.156852
662.628907	39046.767083	32.161869
662.981765	39078.591730	32.166887
663.692014	39107.460287	32.171904
664.428053	39122.755916	32.176922
664.265730	39156.613635	32.181940
665.024156	39194.206203	32.186957
665.430975	39238.422413	32.191975
665.694530	39284.317527	32.196992
666.573643	39331.035450	32.202010
666.875721	39383.118205	32.207028
667.493811	39426.790396	32.212045
668.275365	39485.256827	32.217063
667.954631	39541.247762	32.222080
668.820793	39589.884867	32.227098
669.308357	39654.113256	32.232116
669.603889	39696.316495	32.237133
670.693723	39750.412116	32.242151
671.084043	39810.105236	32.247168
671.885799	39862.447855	32.252186
672.270612	39933.697200	32.257204
672.444219	39996.490417	32.262221
673.202150	40071.218628	32.267239
673.531417	40149.408166	32.272256
674.311519	40211.804595	32.277274
674.780685	40293.509916	32.282292
675.462792	40367.099949	32.287309
676.329878	40448.160019	32.292327
677.025372	40531.630355	32.297344
678.089000	40602.974348	32.302362
678.454087	40685.450632	32.307380
679.267325	40757.744232	32.312397
679.955974	40831.155018	32.317415
680.632072	40896.482535	32.322432
681.667262	40970.049193	32.327450
682.163450	41048.059202	32.332468
683.283239	41119.051409	32.337485
683.441508	41185.775766	32.342503
684.128117	41259.340138	32.347520
685.503236	41324.511514	32.352538
685.920985	41400.367355	32.357556
686.809121	41462.613705	32.362573
687.836568	41522.951458	32.367591
688.543347	41590.764143	32.372608
689.284820	41651.249180	32.377626
689.812626	41724.618416	32.382644
690.867655	41784.737587	32.387661
691.427783	41846.757244	32.392679
691.882847	41910.370656	32.397696
692.636018	41973.124913	32.402714
693.088789	42057.783487	32.407732
693.934708	42123.982918	32.412749
694.335370	42179.886593	32.417767
695.261887	42257.035399	32.422784
696.146509	42315.862489	32.427802
696.948126	42379.673881	32.432820
697.536386	42437.680654	32.437837
698.554862	42495.351832	32.442855
699.441334	42565.278059	32.447872
700.425977	42612.229275	32.452890
700.960252	42672.566811	32.457908
701.600485	42729.327825	32.462925
701.973901	42788.045045	32.467943
702.414748	42852.554519	32.472960
703.416134	42913.226449	32.477978
704.096469	42980.786613	32.482996
704.536397	43042.366646	32.488013
705.113130	43111.463837	32.493031
705.700187	43183.931861	32.498048
706.115208	43251.573181	32.503066
706.948578	43328.710770	32.508084
707.551738	43386.976846	32.513101
708.175841	43457.390251	32.518119
708.572542	43529.699596	32.523136
709.494266	43588.969549	32.528154
709.943727	43666.126919	32.533172
710.554787	43735.302614	32.538189
710.942765	43802.549510	32.543207
711.538749	43881.899389	32.548224
712.662514	43955.358382	32.553242
713.528347	44038.306746	32.558260
714.154587	44109.369558	32.563277
715.075247	44175.594980	32.568295
715.973161	44245.809685	32.573312
717.110195	44310.681708	32.578330
718.270354	44373.175306	32.583348
718.811828	44444.114951	32.588365
719.795972	44499.060300	32.593383
720.598763	44572.582993	32.598400
721.361078	44616.394168	32.603418
721.982865	44686.629390	32.608436
722.715232	44743.418571	32.613453
723.550058	44802.438796	32.618471
723.982128	44867.585072	32.623488
724.715778	44928.059870	32.628506
724.894591	44997.023691	32.633524
725.489846	45067.372235	32.638541
726.415621	45132.523267	32.643559
726.975156	45226.920051	32.648576
727.619072	45298.394825	32.653594
728.245903	45374.101350	32.658612
728.895813	45450.382138	32.663629
729.531952	45524.988681	32.668647
730.660203	45607.324190	32.673664
731.353209	45675.438137	32.678682
731.847349	45754.150097	32.683700
732.533471	45833.505322	32.688717
733.570789	45909.652105	32.693735
734.276406	45998.870534	32.698752
734.597031	46067.340216	32.703770
735.748098	46140.430333	32.708788
736.397626	46216.935318	32.713805
737.532968	46285.471497	32.718823
738.216245	46368.372870	32.723840
739.150413	46439.691663	32.728858
740.174300	46505.847515	32.733876
740.441833	46585.707080	32.738893
741.285699	46652.589080	32.743911
742.261700	46726.658891	32.748928
743.038458	46799.686162	32.753946
743.912663	46858.488090	32.758964
744.827085	46917.655983	32.763981
745.891881	46975.234962	32.768999
746.974599	47032.384677	32.774016
747.930718	47077.902206	32.779034
748.687744	47126.713298	32.784052
749.015188	47166.846475	32.789069
749.564940	47209.521983	32.794087
749.833771	47274.764437	32.799104
750.578401	47322.633816	32.804122
750.771409	47387.712775	32.809140
751.504547	47454.123840	32.814157
752.180535	47512.058443	32.819175
752.827385	47584.059222	32.824192
753.546990	47658.634515	32.829210
754.113085	47727.197563	32.834228
754.821715	47803.566100	32.839245
755.614388	47862.843039	32.844263
756.350714	47964.493676	32.849280
757.275796	48032.408850	32.854298
758.155633	48098.762267	32.859316
758.667082	48183.311712	32.864333
759.796955	48258.845548	32.869351
760.594086	48330.179043	32.874368
761.262867	48406.392551	32.879386
762.539215	48473.367888	32.884404
763.052627	48538.117893	32.889421
763.999429	48612.256823	32.894439
764.593333	48682.230361	32.899456
765.242353	48757.760078	32.904474
765.940098	48819.567266	32.909492
766.348238	48906.629674	32.914509
767.328913	48981.149561	32.919527
768.068901	49057.277629	32.924544
768.917432	49136.811339	32.929562
769.783649	49211.219055	32.934580
770.490669	49285.641693	32.939597
771.310494	49349.312206	32.944615
772.278061	49433.867946	32.949632
773.087108	49514.603942	32.954650
773.977012	49579.716197	32.959668
774.497143	49645.896476	32.964685
775.810841	49718.706997	32.969703
776.314138	49802.699493	32.974720
777.229124	49865.142448	32.979738
778.156155	49933.736770	32.984756
778.490318	50015.541718	32.989773
779.537873	50075.745196	32.994791
780.267100	50160.079584	32.999808
781.022733	50228.483189	33.004826
782.289959	50279.261747	33.009844
782.814702	50364.977697	33.014861
783.987415	50423.524548	33.019879
784.453920	50504.563395	33.024896
785.284330	50567.629588	33.029914
786.043506	50630.379665	33.034932
786.633215	50704.909953	33.039949
787.428793	50770.295057	33.044967
787.980520	50848.534603	33.049984
788.383789	50929.428098	33.055002
789.334071	51002.615242	33.060020
790.097721	51077.875296	33.065037
790.472642	51151.414265	33.070055
791.287083	51224.840317	33.075072
792.133247	51292.259182	33.080090
792.901424	51355.464934	33.085108
793.517126	51434.788866	33.090125
794.468554	51497.458250	33.095143
795.248039	51587.444785	33.100160
796.124200	51651.978734	33.105178
797.620544	51725.668941	33.110196
798.018253	51801.221903	33.115213
798.798126	51858.064960	33.120231
799.633953	51947.626499	33.125248
800.448383	52033.097943	33.130266
801.356842	52105.076962	33.135284
802.060300	52182.221744	33.140301
802.916723	52254.728316	33.145319
803.237315	52335.351123	33.150336
803.635644	52428.768107	33.155354
804.681332	52502.639515	33.160372
805.112850	52591.041162	33.165389
805.888433	52683.409071	33.170407
806.955202	52768.701479	33.175424
807.620379	52856.293445	33.180442
808.970890	52938.580963	33.185460
809.629689	53039.702642	33.190477
810.754554	53124.089409	33.195495
811.436791	53209.936112	33.200512
812.436637	53286.004517	33.205530
813.460662	53365.095676	33.210548
813.951366	53451.905067	33.215565
814.892651	53536.223938	33.220583
815.321110	53620.877436	33.225600
815.605323	53713.081569	33.230618
816.729308	53804.402997	33.235636
817.971959	53884.248621	33.240653
818.963867	53961.489948	33.245671
820.129778	54046.549723	33.250688
820.922329	54128.091038	33.255706
822.118468	54196.186548	33.260724
822.816036	54275.495226	33.265741
823.689512	54352.511923	33.270759
824.674498	54420.871852	33.275776
825.408317	54494.153260	33.280794
826.453530	54567.514301	33.285812
826.732000	54644.052695	33.290829
827.560449	54728.964665	33.295847
828.603138	54805.688733	33.300864
829.314613	54879.461952	33.305882
830.274411	54951.600499	33.310900
831.097160	55040.280947	33.315917
831.782622	55122.419713	33.320935
832.931237	55194.735331	33.325952
833.513049	55271.546449	33.330970
834.584639	55326.776016	33.335988
835.491245	55397.440272	33.341005
836.014526	55449.446499	33.346023
837.145656	55513.462778	33.351040
837.797682	55573.093588	33.356058
838.642386	55632.982262	33.361076
839.606946	55711.637943	33.366093
840.273218	55779.159770	33.371111
840.827921	55848.040641	33.376128
841.347201	55921.067019	33.381146
842.415433	55984.109752	33.386164
843.151628	56073.100293	33.391181
843.540250	56152.090167	33.396199
844.720841	56231.311233	33.401216
845.080651	56318.319812	33.406234
845.874818	56398.644126	33.411252
846.581117	56497.234736	33.416269
847.253582	56587.849962	33.421287
847.826191	56681.497164	33.426304
848.755291	56786.749842	33.431322
849.741829	56873.862023	33.436340
850.373818	56978.060641	33.441357
851.365885	57068.932955	33.446375
852.809929	57167.482639	33.451392
853.065595	57276.562929	33.456410
854.100311	57369.312596	33.461428
854.994812	57470.447904	33.466445
855.775156	57571.312553	33.471463
856.802818	57656.070057	33.476480
857.839822	57763.211642	33.481498
858.706817	57857.003466	33.486516
859.790346	57958.058273	33.491533
860.356169	58059.891141	33.496551
861.645398	58147.064405	33.501568
862.493902	58234.383050	33.506586
863.904926	58311.581979	33.511604
864.805132	58400.143870	33.516621
865.536817	58480.714684	33.521639
866.501619	58564.387038	33.526656
867.100214	58663.411139	33.531674
868.201546	58740.949155	33.536692
868.759257	58826.297660	33.541709
869.795065	58924.774126	33.546727
870.814134	59005.506366	33.551744
871.525770	59107.022443	33.556762
872.376448	59195.703725	33.561780
873.134539	59291.075639	33.566797
873.492886	59382.174297	33.571815
874.364804	59479.076108	33.576832
874.933290	59574.146829	33.581850
875.966010	59669.574600	33.586868
876.988346	59767.899426	33.591885
878.234600	59876.470028	33.596903
879.343265	59963.328037	33.601920
880.321164	60062.451970	33.606938
880.454086	60143.934623	33.611956
881.498415	60222.790095	33.616973
882.294486	60306.852449	33.621991
883.061631	60392.835298	33.627008
884.296694	60489.527994	33.632026
885.349766	60578.540886	33.637044
885.903198	60664.687893	33.642061
887.023443	60746.446296	33.647079
888.260138	60817.667075	33.652096
889.301846	60893.263981	33.657114
890.451557	60964.297897	33.662132
891.787640	61041.709614	33.667149
892.512066	61119.175813	33.672167
893.706848	61174.387583	33.677184
894.309815	61254.422466	33.682202
895.193232	61322.753572	33.687220
896.040127	61402.582904	33.692237
896.454389	61484.288160	33.697255
897.917538	61561.970844	33.702272
898.176540	61637.622359	33.707290
898.766783	61724.355357	33.712308
899.937596	61808.486083	33.717325
900.776855	61897.996424	33.722343
901.423993	61975.870991	33.727360
902.298614	62082.481433	33.732378
903.149741	62178.843246	33.737396
904.263339	62271.576344	33.742413
904.744325	62370.265486	33.747431
905.714234	62458.605379	33.752448
906.754248	62553.482657	33.757466
907.433615	62654.996469	33.762484
908.539431	62752.499441	33.767501
909.169661	62850.899801	33.772519
910.426833	62947.644469	33.777536
910.949997	63042.365956	33.782554
911.678209	63138.803844	33.787572
912.742536	63242.757953	33.792589
913.464070	63351.815994	33.797607
914.712361	63449.620237	33.802624
916.016777	63552.908924	33.807642
916.277293	63657.799305	33.812660
917.416726	63759.473607	33.817677
918.025731	63867.200743	33.822695
919.136309	63969.728136	33.827712
919.945946	64079.059366	33.832730
920.803678	64188.047867	33.837748
921.856677	64285.326815	33.842765
922.964577	64404.319205	33.847783
923.746030	64512.614392	33.852800
924.703976	64621.265557	33.857818
925.782622	64722.771605	33.862836
926.880668	64826.057663	33.867853
927.802355	64929.519841	33.872871
929.158770	65026.067465	33.877888
930.353336	65119.039587	33.882906
931.176691	65201.410066	33.887924
932.325954	65274.456611	33.892941
933.192580	65364.128856	33.897959
934.166411	65435.947870	33.902976
934.923266	65516.219317	33.907994
935.594443	65597.321328	33.913012
936.714584	65678.074898	33.918029
937.352781	65771.006087	33.923047
938.437496	65853.245840	33.928064
939.211485	65950.719365	33.933082
939.755477	66043.351761	33.938100
940.763713	66127.116753	33.943117
941.213026	66237.026696	33.948135
942.016545	66335.160801	33.953152
943.113341	66441.635241	33.958170
943.654789	66553.162277	33.963188
945.096083	66653.920016	33.968205
945.247467	66759.988921	33.973223
946.013543	66879.705045	33.978240
947.071085	67002.482735	33.983258
948.290839	67127.136522	33.988276
949.161992	67245.104254	33.993293
950.146441	67358.576634	33.998311
951.060613	67481.103429	34.003328
952.131321	67597.559373	34.008346
953.036928	67722.479098	34.013364
954.331788	67837.026356	34.018381
955.227611	67960.241929	34.023399
955.928760	68071.332234	34.028416
957.642533	68177.842478	34.033434
958.932825	68272.538241	34.038452
960.457101	68374.693650	34.043469
961.581892	68479.592681	34.048487
962.714384	68567.614166	34.053504
963.626777	68666.518113	34.058522
964.630396	68768.593837	34.063540
965.414608	68858.649031	34.068557
966.337488	68957.192091	34.073575
967.557894	69044.852694	34.078592
968.045490	69158.900281	34.083610
969.144806	69256.447015	34.088628
970.385219	69345.717897	34.093645
971.060410	69452.380717	34.098663
971.675709	69550.498581	34.103680
972.502452	69648.549063	34.108698
973.541364	69758.452005	34.113716
974.395679	69868.968893	34.118733
975.381576	69978.799828	34.123751
976.538211	70078.269178	34.128768
977.921764	70174.089287	34.133786
978.226784	70290.222996	34.138804
979.996923	70378.528435	34.143821
981.053049	70481.305213	34.148839
982.426238	70581.074953	34.153856
983.331726	70666.190656	34.158874
984.050401	70750.118175	34.163892
984.821022	70830.261752	34.168909
985.371777	70930.249826	34.173927
986.508693	71005.714852	34.178944
988.060899	71092.941188	34.183962
988.543654	71197.836898	34.188980
989.553775	71280.217765	34.193997
990.254778	71378.790882	34.199015
990.816900	71482.194539	34.204032
991.873189	71588.246082	34.209050
992.388373	71700.107840	34.214068
993.516908	71801.885568	34.219085
994.310287	71914.466010	34.224103
995.038572	72032.598222	34.229120
996.140886	72150.350807	34.234138
996.838794	72281.017977	34.239156
997.639579	72395.098487	34.244173
998.658110	72515.966320	34.249191
999.514624	72638.386751	34.254208
1000.895432	72779.520714	34.259226
1002.013289	72905.926569	34.264244
1003.271215	73013.923735	34.269261
1003.855806	73147.436208	34.274279
1005.107294	73264.486173	34.279296
1006.369470	73379.700785	34.284314
1007.588245	73502.955768	34.289332
1008.977771	73612.868689	34.294349
1010.308278	73731.507756	34.299367
1011.058605	73846.211608	34.304384
1011.662720	73959.752029	34.309402
1012.721743	74077.743717	34.314420
1013.738783	74197.684960	34.319437
1014.772657	74315.675899	34.324455
1015.731980	74435.217194	34.329472
1017.135248	74546.435345	34.334490
1017.672926	74674.652098	34.339508
1018.900974	74789.734431	34.344525
1020.128622	74914.077340	34.349543
1021.190655	75030.890797	34.354560
1022.539684	75136.567748	34.359578
1023.586557	75255.320474	34.364596
1024.792123	75363.913677	34.369613
1025.630967	75476.561432	34.374631
1026.675509	75593.051923	34.379648
1027.900511	75704.375974	34.384666
1028.764831	75826.907584	34.389684
1029.580815	75936.253423	34.394701
1030.367626	76051.152167	34.399719
1031.194517	76178.822014	34.404736
1032.497872	76293.355230	34.409754
1033.471259	76413.493000	34.414772
1034.705617	76530.170937	34.419789
1035.851239	76653.006803	34.424807
1036.396907	76773.080579	34.429824
1037.775451	76882.853405	34.434842
1038.793500	76999.222911	34.439860
1039.493092	77104.735723	34.444877
1040.803541	77211.637300	34.449895
1041.308570	77317.646204	34.454912
1042.435906	77433.341362	34.459930
1043.963363	77533.843568	34.464948
1045.609866	77629.885095	34.469965
1046.674813	77736.274528	34.474983
1047.716789	77842.839195	34.480000
1048.639179	77944.946082	34.485018
1049.448990	78056.327590	34.490036
1050.436722	78165.338562	34.495053
1051.285924	78268.610774	34.500071
1052.119765	78383.791717	34.505088
1053.047726	78491.441739	34.510106
1053.874668	78612.508284	34.515124
1054.954716	78726.162169	34.520141
1056.175789	78854.058017	34.525159
1056.856365	78979.099117	34.530176
1058.330151	79101.847828	34.535194
1058.834080	79230.672027	34.540212
1059.796170	79358.450573	34.545229
1061.288751	79483.026430	34.550247
1062.240993	79615.540220	34.555264
1063.280204	79738.948806	34.560282
1064.256268	79865.329657	34.565300
1065.453919	79992.691830	34.570317
1066.550956	80130.441135	34.575335
1067.531899	80267.103997	34.580352
1069.129551	80388.250448	34.585370
1069.824987	80520.244056	34.590388
1071.325530	80643.388725	34.595405
1072.434734	80765.297762	34.600423
1073.915698	80887.479106	34.605440
1074.847455	81016.461530	34.610458
1076.211244	81143.826955	34.615476
1076.814671	81266.805911	34.620493
1077.757169	81389.993192	34.625511
1078.736952	81524.942817	34.630528
1079.737421	81647.893780	34.635546
1080.862856	81787.584198	34.640564
1081.698254	81922.554541	34.645581
1082.909878	82053.304368	34.650599
1083.732975	82181.647564	34.655616
1085.191409	82305.244894	34.660634
1086.316977	82435.790166	34.665652
1087.144338	82580.490579	34.670669
1088.715612	82709.784215	34.675687
1090.121725	82838.562705	34.680704
1091.290964	82958.182554	34.685722
1092.373298	83088.498459	34.690740
1093.167699	83218.472097	34.695757
1094.282205	83328.764007	34.700775
1095.045437	83463.489907	34.705792
1096.473180	83587.036033	34.710810
1097.504680	83707.600798	34.715828
1098.446640	83828.978787	34.720845
1099.535884	83948.376965	34.725863
1100.514186	84068.978011	34.730880
1101.392326	84187.628931	34.735898
1102.169006	84311.923129	34.740916
1103.363560	84431.109577	34.745933
1104.198893	84568.335260	34.750951
1105.138081	84710.296127	34.755968
1106.581645	84833.605664	34.760986
1107.608076	84965.409642	34.766004
1109.019123	85102.362684	34.771021
1109.870881	85224.598613	34.776039
1111.084260	85370.547399	34.781056
1113.037746	85480.610858	34.786074
1114.592390	85588.610579	34.791092
1115.800099	85711.686664	34.796109
1117.634573	85810.951075	34.801127
1118.807029	85910.727926	34.806144
1120.280909	86014.098593	34.811162
1121.570120	86128.892025	34.816180
1122.389823	86224.598307	34.821197
1123.550325	86322.796894	34.826215
1124.182046	86433.711272	34.831232
1125.409631	86541.897911	34.836250
1126.024203	86652.835233	34.841268
1126.731599	86771.730879	34.846285
1127.941972	86885.560576	34.851303
1128.841703	87022.068031	34.856320
1129.845983	87144.635806	34.861338
1130.950175	87276.129230	34.866356
1131.697417	87400.824397	34.871373
1133.228036	87532.872744	34.876391
1134.034687	87670.981979	34.881408
1134.911845	87800.454043	34.886426
1136.027213	87946.511370	34.891444
1137.363442	88091.019215	34.896461
1139.024895	88223.340091	34.901479
1139.808794	88363.843137	34.906496
1140.997963	88496.562818	34.911514
1142.155370	88625.712884	34.916532
1143.432786	88766.045178	34.921549
1144.830170	88897.199835	34.926567
1145.863645	89038.132422	34.931584
1146.968281	89167.395689	34.936602
1148.313980	89300.991714	34.941620
1148.954834	89441.088827	34.946637
1150.179395	89574.934952	34.951655
1151.315222	89714.607131	34.956672
1152.698573	89848.471885	34.961690
1153.860174	89988.407053	34.966708
1154.983207	90125.026793	34.971725
1156.005740	90265.430413	34.976743
1156.998466	90398.529618	34.981760
1158.369668	90527.874757	34.986778
1159.759100	90657.242780	34.991796
1160.598599	90789.990598	34.996813
1161.776494	90905.085410	35.001831
1162.578631	91031.606462	35.006848
1163.890793	91165.547616	35.011866
1164.809666	91292.594368	35.016884
1165.504056	91427.288335	35.021901
1167.208811	91552.752419	35.026919
1168.010857	91692.201919	35.031936
1169.495851	91819.629200	35.036954
1171.129321	91960.267104	35.041972
1172.296455	92090.617564	35.046989
1173.299988	92221.414489	35.052007
1174.382626	92355.426760	35.057024
1175.448457	92503.172036	35.062042
1176.723945	92635.614664	35.067060
1177.459066	92782.152258	35.072077
1178.897188	92920.043935	35.077095
1179.996937	93078.661682	35.082112
1181.097412	93209.004146	35.087130
1182.657904	93359.005624	35.092148
1183.531391	93512.436267	35.097165
1185.031698	93650.542920	35.102183
1186.063966	93801.593360	35.107200
1186.754853	93954.975705	35.112218
1188.238140	94104.317574	35.117236
1188.914498	94254.672068	35.122253
1190.379093	94404.835545	35.127271
1191.360511	94574.143349	35.132288
1192.553130	94737.782085	35.137306
1193.548000	94890.010314	35.142324
1194.832848	95058.326212	35.147341
1196.368832	95210.172544	35.152359
1198.029500	95380.065866	35.157376
1199.229741	95526.723560	35.162394
1200.892730	95682.868479	35.167412
1201.566800	95837.018582	35.172429
1202.614722	95981.413301	35.177447
1203.942631	96146.342185	35.182464
1205.393628	96296.987798	35.187482
1207.111556	96441.688279	35.192500
1208.503084	96594.289411	35.197517
1209.783021	96725.182915	35.202535
1211.172813	96874.455983	35.207552
1212.443500	97022.192902	35.212570
1213.681164	97144.757923	35.217588
1214.745378	97278.046349	35.222605
1216.258246	97413.094675	35.227623
1217.605404	97550.761510	35.232640
1218.452289	97692.269103	35.237658
1220.067780	97828.764561	35.242676
1220.925792	97967.232812	35.247693
1222.497584	98094.550596	35.252711
1223.747007	98219.993166	35.257728
1225.016203	98346.787866	35.262746
1226.478343	98465.895583	35.267764
1227.043598	98590.830299	35.272781
1228.357685	98709.249052	35.277799
1229.329341	98836.654279	35.282816
1230.390926	98967.830953	35.287834
1231.517291	99083.358439	35.292852
1232.547861	99226.831157	35.297869
1233.629309	99358.379984	35.302887
1234.570977	99501.742822	35.307904
1235.462985	99646.634549	35.312922
1236.697553	99792.164927	35.317940
1237.511637	99939.357365	35.322957
1239.298220	100092.981816	35.327975
1240.431140	100254.937721	35.332992
1241.379852	100397.949747	35.338010
1242.711296	100556.289748	35.343028
1243.543085	100720.338965	35.348045
1244.880765	100884.707855	35.353063
1246.875962	101046.293133	35.358080
1247.874958	101208.309571	35.363098
1249.350522	101355.694403	35.368116
1250.236897	101521.202021	35.373133
1251.867364	101683.290604	35.378151
1253.033517	101836.113418	35.383168
1254.566365	102003.299085	35.388186
1255.955743	102153.071411	35.393204
1257.131001	102313.228175	35.398221
1258.106350	102473.293491	35.403239
1259.648443	102634.111296	35.408256
1260.807285	102796.046870	35.413274
1262.430654	102950.988910	35.418292
1263.519563	103109.911487	35.423309
1264.446239	103264.417379	35.428327
1265.946163	103422.688887	35.433344
1267.195611	103589.654519	35.438362
1268.736945	103747.350950	35.443380
1269.898922	103907.355020	35.448397
1271.082337	104075.170925	35.453415
1272.347656	104230.587050	35.458432
1273.778818	104396.057458	35.463450
1275.593252	104545.238637	35.468468
1276.739594	104703.451660	35.473485
1277.882614	104867.441775	35.478503
1279.323927	105014.890920	35.483520
1280.240561	105182.987458	35.488538
1281.819369	105335.544528	35.493556
1283.140531	105497.367461	35.498573
1284.420898	105651.459348	35.503591
1285.654968	105815.009034	35.508608
1286.932414	105981.807525	35.513626
1288.127705	106129.773572	35.518644
1289.596755	106293.450605	35.523661
1291.246856	106444.532467	35.528679
1292.078172	106600.188639	35.533696
1293.186692	106758.610251	35.538714
1294.517690	106896.056621	35.543732
1295.873261	107045.950928	35.548749
1296.860637	107188.308983	35.553767
1298.086521	107332.134320	35.558784
1298.905129	107490.077825	35.563802
1300.457737	107639.308333	35.568820
1300.952282	107810.292911	35.573837
1302.349097	107967.266175	35.578855
1303.995515	108135.699513	35.583872
1304.712627	108306.408421	35.588890
1306.793168	108473.654803	35.593908
1308.127567	108646.692318	35.598925
1308.845401	108815.250796	35.603943
1310.627911	108991.849386	35.608960
1311.452659	109164.382027	35.613978
1312.933456	109334.839933	35.618996
1313.994109	109503.407287	35.624013
1315.056436	109683.528602	35.629031
1316.892036	109863.696078	35.634048
1317.917743	110049.843393	35.639066
1319.444678	110232.207030	35.644084
1320.756985	110408.451796	35.649101
1321.595313	110604.034815	35.654119
1323.452412	110785.978194	35.659136
1324.281228	110968.554852	35.664154
1325.633185	111153.285513	35.669172
1327.306132	111349.719062	35.674189
1328.502594	111550.923032	35.679207
1329.711027	111732.020792	35.684224
1331.190747	111922.296333	35.689242
1332.827813	112117.474516	35.694260
1333.837841	112304.095660	35.699277
1335.394002	112495.388208	35.704295
1336.956642	112674.302980	35.709312
1338.563383	112865.893453	35.714330
1340.567588	113046.584745	35.719348
1341.528334	113225.086590	35.724365
1343.260836	113402.976009	35.729383
1344.840813	113577.205753	35.734400
1346.247134	113750.655424	35.739418
1347.525712	113913.117864	35.744436
1349.150360	114081.755629	35.749453
1350.637683	114255.143836	35.754471
1352.161266	114413.005970	35.759488
1353.619531	114584.614667	35.764506
1355.169437	114748.707899	35.769524
1356.307980	114914.950426	35.774541
1357.409994	115082.606590	35.779559
1358.529440	115243.824133	35.784576
1359.857720	115417.968837	35.789594
1361.183098	115587.350928	35.794612
1363.094512	115750.741817	35.799629
1364.410293	115916.212233	35.804647
1365.907669	116077.952621	35.809664
1367.214124	116235.595869	35.814682
1368.452734	116391.097519	35.819700
1369.660384	116540.687912	35.824717
1371.040690	116685.067030	35.829735
1372.365846	116828.581995	35.834752
1373.338277	116985.551572	35.839770
1374.460971	117146.880560	35.844788
1375.763342	117305.911505	35.849805
1376.260685	117475.230967	35.854823
1377.333759	117649.635532	35.859840
1378.580951	117834.845582	35.864858
1379.857584	118019.392837	35.869876
1381.258932	118214.830327	35.874893
1382.237545	118418.426142	35.879911
1383.896660	118601.707766	35.884928
1385.000189	118805.424272	35.889946
1386.325983	119009.649044	35.894964
1387.818362	119210.932105	35.899981
1389.520193	119410.127773	35.904999
1390.835410	119597.580284	35.910016
1392.541639	119805.965352	35.915034
1393.816338	119992.793674	35.920052
1395.568659	120197.232434	35.925069
1396.506348	120409.529732	35.930087
1398.215511	120608.047860	35.935104
1399.839289	120814.984064	35.940122
1400.930190	121017.805473	35.945140
1402.476370	121221.830312	35.950157
1404.076689	121419.396630	35.955175
1405.362867	121618.133264	35.960192
1406.932550	121828.545524	35.965210
1407.894604	122034.804984	35.970228
1409.508580	122242.259643	35.975245
1410.796526	122461.583329	35.980263
1412.592762	122658.148370	35.985280
1413.863746	122871.065040	35.990298
1415.317065	123083.875951	35.995316
1417.169746	123290.536503	36.000333
1418.665702	123492.075833	36.005351
1419.805492	123692.980379	36.010368
1421.071946	123904.878450	36.015386
1422.588483	124111.640119	36.020404
1424.356617	124322.745457	36.025421
1425.610619	124526.449637	36.030439
1427.151607	124727.457067	36.035456
1428.722777	124937.079392	36.040474
1429.814716	125146.138755	36.045492
1431.349368	125342.258839	36.050509
1433.686656	125545.277351	36.055527
1435.798445	125722.592951	36.060544
1437.521195	125904.032161	36.065562
1438.988256	126076.440822	36.070580
1440.551661	126246.590446	36.075597
1441.844350	126438.119762	36.080615
1443.683794	126607.172067	36.085632
1445.180149	126776.588217	36.090650
1446.600672	126921.351849	36.095668
1448.018331	127067.713754	36.100685
1449.301692	127223.339812	36.105703
1450.829103	127393.273684	36.110720
1451.697503	127544.168290	36.115738
1452.661463	127708.027236	36.120756
1454.138357	127871.710516	36.125773
1455.264756	128044.543247	36.130791
1456.790197	128216.624125	36.135808
1457.857517	128408.343468	36.140826
1458.632221	128597.249250	36.145844
1460.465015	128779.408801	36.150861
1461.623547	128974.183589	36.155879
1462.735048	129173.822658	36.160896
1464.430989	129372.031927	36.165914
1465.700359	129570.290081	36.170932
1467.328200	129770.250159	36.175949
1468.600216	129979.944675	36.180967
1470.087090	130184.228851	36.185984
1471.728640	130387.638507	36.191002
1473.287877	130596.159653	36.196020
1474.967207	130799.121752	36.201037
1476.365960	130998.444122	36.206055
1478.300654	131205.700629	36.211072
1479.146222	131414.995735	36.216090
1480.484123	131625.374243	36.221108
1482.194668	131834.562049	36.226125
1483.443209	132052.958049	36.231143
1485.093197	132266.659498	36.236160
1486.759323	132485.329219	36.241178
1488.239317	132706.263536	36.246196
1489.664455	132922.923630	36.251213
1490.937020	133135.313459	36.256231
1492.275096	133356.783555	36.261248
1493.909064	133581.221879	36.266266
1495.217699	133814.199090	36.271284
1497.060258	134034.281543	36.276301
1498.311555	134253.262207	36.281319
1500.169888	134468.096017	36.286336
1501.970012	134688.291497	36.291354
1503.327008	134913.014448	36.296372
1505.050635	135122.182852	36.301389
1506.812212	135344.798206	36.306407
1508.392956	135562.526606	36.311424
1510.128685	135781.307601	36.316442
1511.158807	136005.941676	36.321460
1513.092003	136212.507180	36.326477
1514.483863	136428.942209	36.331495
1515.608629	136637.360348	36.336512
1517.118113	136852.839696	36.341530
1518.684037	137078.213353	36.346548
1520.090515	137294.943035	36.351565
1521.442108	137518.403648	36.356583
1523.001108	137750.122711	36.361600
1524.195325	137962.962274	36.366618
1525.635077	138183.939606	36.371636
1527.084987	138385.275501	36.376653
1529.219465	138581.841884	36.381671
1530.804037	138791.880915	36.386688
1532.565180	138979.041484	36.391706
1534.150336	139185.646509	36.396724
1535.506837	139393.496521	36.401741
1536.744975	139603.777294	36.406759
1538.110175	139809.041521	36.411776
1540.104885	140007.922402	36.416794
1541.803246	140224.404997	36.421812
1543.575298	140422.527473	36.426829
1544.967275	140635.958301	36.431847
1546.235264	140846.063924	36.436864
1548.093730	141052.582524	36.441882
1549.392740	141268.607318	36.446900
1550.721865	141483.436269	36.451917
1552.119010	141697.760324	36.456935
1553.701437	141924.037659	36.461952
1555.404707	142139.795698	36.466970
1556.724533	142366.133473	36.471988
1558.584664	142582.006849	36.477005
1559.650558	142815.124748	36.482023
1561.705547	143041.467818	36.487040
1563.233639	143260.572506	36.492058
1564.906843	143488.505531	36.497076
1566.621666	143713.427296	36.502093
1568.289851	143930.115235	36.507111
1569.576967	144154.263259	36.512128
1571.119459	144372.104052	36.517146
1572.771654	144606.439474	36.522164
1574.615063	144824.878282	36.527181
1576.243267	145052.689369	36.532199
1577.516965	145281.868824	36.537216
1579.017697	145508.842174	36.542234
1580.778859	145748.404130	36.547252
1582.600372	145967.145217	36.552269
1584.380964	146190.511094	36.557287
1585.840098	146410.344124	36.562304
1587.988028	146630.225473	36.567322
1589.426473	146864.244118	36.572340
1591.019316	147084.223152	36.577357
1592.802914	147299.389346	36.582375
1594.396830	147516.022435	36.587392
1596.085106	147725.132197	36.592410
1597.324551	147952.317461	36.597428
1598.904978	148167.929296	36.602445
1600.821375	148393.847217	36.607463
1602.534510	148613.535643	36.612480
1604.398108	148821.746363	36.617498
1605.537071	149047.826609	36.622516
1607.247828	149266.479188	36.627533
1609.104363	149484.144118	36.632551
1610.000596	149708.240437	36.637568
1611.671505	149927.144633	36.642586
1613.329341	150127.901546	36.647604
1614.985581	150337.272256	36.652621
1616.403069	150539.353546	36.657639
1617.766741	150749.207831	36.662656
1619.578887	150949.359174	36.667674
1620.893786	151171.096567	36.672692
1622.431869	151374.049511	36.677709
1624.115305	151592.682010	36.682727
1625.733126	151809.627244	36.687744
1627.610978	152016.774738	36.692762
1628.757563	152238.065025	36.697780
1630.428617	152460.116703	36.702797
1631.906909	152684.282937	36.707815
1633.449374	152909.631854	36.712832
1635.389215	153132.237543	36.717850
1637.145521	153366.165580	36.722868
1638.595286	153594.413789	36.727885
1640.482602	153831.328539	36.732903
1642.002796	154062.764067	36.737920
1643.568699	154292.797738	36.742938
1645.214147	154520.332789	36.747956
1647.022744	154749.845529	36.752973
1648.699263	154986.092846	36.757991
1650.080252	155223.736800	36.763008
1651.684074	155450.079131	36.768026
1653.168656	155702.690007	36.773044
1654.749800	155939.365193	36.778061
1656.937825	156169.874052	36.783079
1658.429452	156421.244993	36.788096
1660.038031	156665.556703	36.793114
1661.514966	156910.919983	36.798132
1662.816558	157162.683229	36.803149
1664.482596	157418.254990	36.808167
1666.219061	157689.839209	36.813184
1668.544825	157935.583529	36.818202
1669.848839	158192.439946	36.823220
1671.129393	158450.494515	36.828237
1673.240918	158706.543562	36.833255
1674.652488	158961.838562	36.838272
1676.136185	159217.744442	36.843290
1677.876610	159488.933789	36.848308
1679.402451	159746.294688	36.853325
1681.349770	160010.017408	36.858343
1682.966461	160274.711827	36.863360
1685.248414	160532.671328	36.868378
1686.522637	160804.431026	36.873396
1688.194987	161071.239685	36.878413
1690.188535	161334.467933	36.883431
1691.511094	161601.631569	36.888448
1693.729154	161854.408104	36.893466
1695.552076	162118.977196	36.898484
1697.078522	162371.938546	36.903501
1699.218472	162624.377707	36.908519
1701.187616	162879.892675	36.913536
1703.122167	163110.039017	36.918554
1705.302173	163341.362637	36.923572
1706.654489	163561.866535	36.928589
1708.554494	163777.849650	36.933607
1710.211030	164002.249750	36.938624
1711.808445	164214.911706	36.943642
1713.262618	164435.326434	36.948660
1715.098117	164659.559691	36.953677
1716.886595	164882.368325	36.958695
1718.425399	165113.493761	36.963712
1720.197758	165330.965504	36.968730
1721.312337	165573.611080	36.973748
1722.026881	165809.284134	36.978765
1724.444197	166046.012113	36.983783
1725.582910	166302.615253	36.988800
1727.391974	166547.228252	36.993818
1729.176804	166813.177056	36.998836
1730.518833	167063.544769	37.003853
1732.404270	167328.261218	37.008871
1733.911661	167597.815059	37.013888
1735.646612	167854.921352	37.018906
1737.612154	168130.909590	37.023924
1739.340136	168396.902720	37.028941
1741.293580	168653.887270	37.033959
1742.786634	168931.699607	37.038976
1744.654199	169201.848379	37.043994
1746.613306	169480.535987	37.049012
1748.411875	169744.646667	37.054029
1750.071541	170013.934721	37.059047
1751.537158	170288.092417	37.064064
1753.896810	170548.139638	37.069082
1755.547718	170827.154449	37.074100
1757.333125	171109.104716	37.079117
1759.486031	171372.364388	37.084135
1761.096307	171642.088923	37.089152
1762.910607	171914.419685	37.094170
1764.395063	172188.470881	37.099188
1766.470133	172460.201733	37.104205
1768.417848	172728.960900	37.109223
1769.985185	173011.340349	37.114240
1771.717545	173278.997231	37.119258
1773.443541	173556.327126	37.124276
1775.292452	173834.069053	37.129293
1777.312367	174097.163224	37.134311
1778.685323	174381.753983	37.139328
1780.165427	174655.045591	37.144346
1782.030891	174947.220802	37.149364
1783.517075	175241.620135	37.154381
1785.594611	175509.191959	37.159399
1787.450624	175818.773770	37.164416
1789.562552	176093.729253	37.169434
1791.252716	176372.616634	37.174452
1792.714178	176670.302972	37.179469
1794.579741	176951.016501	37.184487
1796.255181	177241.156044	37.189504
1797.734075	177518.156669	37.194522
1799.863790	177793.092880	37.199540
1801.169762	178063.158129	37.204557
1803.090171	178341.737596	37.209575
1804.666937	178619.095436	37.214592
1806.662123	178897.385852	37.219610
1808.735380	179175.055159	37.224628
1810.145514	179465.595199	37.229645
1811.959194	179742.969212	37.234663
1813.662474	180025.288250	37.239680
1815.381161	180299.229060	37.244698
1817.503028	180595.542870	37.249716
1819.049760	180885.851519	37.254733
1821.239364	181163.498610	37.259751
1823.158633	181460.410324	37.264768
1825.055886	181746.144983	37.269786
1827.387010	182028.951002	37.274804
1828.766297	182328.384183	37.279821
1830.673767	182604.233708	37.284839
1832.913767	182893.698267	37.289856
1834.534889	183181.023513	37.294874
1835.923883	183470.776295	37.299892
1837.764983	183757.851102	37.304909
1839.680165	184107.696441	37.309927
1841.475316	184408.986405	37.314944
1843.486874	184716.803537	37.319962
1845.168910	185002.769478	37.324980
1847.192998	185305.725993	37.329997
1849.063003	185613.165988	37.335015
1851.072650	185904.970313	37.340032
1852.730359	186203.373683	37.345050
1854.808334	186512.128450	37.350068
1856.708485	186807.548450	37.355085
1859.052040	187106.308809	37.360103
1860.602233	187413.013321	37.365120
1862.645462	187713.034085	37.370138
1864.512038	188008.834001	37.375156
1866.797315	188306.506001	37.380173
1868.876763	188599.987454	37.385191
1870.399647	188899.036875	37.390208
1872.009603	189192.982372	37.395226
1873.942779	189488.676641	37.400244
1876.121204	189797.583637	37.405261
1877.711591	190084.440471	37.410279
1879.576073	190386.675937	37.415296
1881.891319	190666.492833	37.420314
1884.276326	190965.366822	37.425332
1885.733146	191272.348081	37.430349
1887.534501	191571.109004	37.435367
1889.479204	191860.858700	37.440384
1891.315571	192149.206404	37.445402
1893.256982	192448.214128	37.450420
1895.010939	192751.559024	37.455437
1896.742758	193040.982365	37.460455
1898.866148	193354.677098	37.465472
1900.160678	193637.487453	37.470490
1902.744124	193913.832378	37.475508
1904.118744	194203.944111	37.480525
1905.768537	194477.086808	37.485543
1907.843524	194761.634793	37.490560
1909.435071	195055.636144	37.495578
1911.349985	195329.701898	37.500596
1913.047577	195619.561480	37.505613
1914.949464	195911.977333	37.510631
1916.926717	196210.285182	37.515648
1918.633002	196505.161994	37.520666
1920.752852	196789.774417	37.525684
1922.660377	197093.100319	37.530701
1925.104996	197380.871768	37.535719
1927.132976	197674.416287	37.540736
1929.033874	197982.406752	37.545754
1931.616144	198258.490437	37.550772
1933.721488	198548.698979	37.555789
1935.873688	198823.220623	37.560807
1938.090671	199107.406966	37.565824
1939.789334	199389.461215	37.570842
1942.604507	199664.063164	37.575860
1944.051898	199945.946748	37.580877
1945.926596	200226.882275	37.585895
1948.008512	200497.448320	37.590912
1949.759124	200792.259385	37.595930
1951.649199	201072.865435	37.600948
1953.478004	201366.751266	37.605965
1955.119271	201645.040437	37.610983
1957.193886	201940.587889	37.616000
1958.537372	202242.343439	37.621018
1960.741349	202529.021267	37.626036
1962.333084	202837.224942	37.631053
1964.231803	203136.400462	37.636071
1966.449613	203444.017017	37.641088
1968.482149	203746.739955	37.646106
1970.204209	204061.566941	37.651124
1972.135516	204378.505270	37.656141
1974.066624	204696.346436	37.661159
1976.316479	204999.583064	37.666176
1977.932950	205325.911706	37.671194
1980.219585	205631.125272	37.676212
1982.275478	205953.927584	37.681229
1983.815844	206265.226389	37.686247
1986.338266	206580.954995	37.691264
1987.669125	206908.380110	37.696282
1989.938714	207226.059116	37.701300
1991.537852	207557.212177	37.706317
1993.129013	207884.393470	37.711335
1995.607303	208215.893995	37.716352
1996.987539	208556.650019	37.721370
1999.025924	208893.790174	37.726388
2000.885866	209231.063763	37.731405
2002.921608	209583.038487	37.736423
2005.134958	209920.228922	37.741440
2006.757512	210268.848566	37.746458
2008.902612	210581.824914	37.751476
2011.207457	210902.648031	37.756493
2013.121563	211219.348656	37.761511
2014.973712	211537.813379	37.766528
2016.888842	211862.490716	37.771546
2019.311994	212180.860033	37.776564
2021.596411	212497.298601	37.781581
2023.496579	212815.023038	37.786599
2025.749305	213129.208824	37.791616
2027.139535	213461.880122	37.796634
2029.599736	213771.156257	37.801652
2031.138665	214101.290008	37.806669
2033.110576	214438.055832	37.811687
2034.950733	214765.676763	37.816704
2036.573200	215116.371891	37.821722
2038.795504	215461.174944	37.826740
2040.693459	215813.374705	37.831757
2042.274814	216164.207557	37.836775
2044.749910	216521.771693	37.841792
2046.873682	216882.648155	37.846810
2048.874322	217239.737182	37.851828
2050.825604	217607.782631	37.856845
2053.001835	217967.968138	37.861863
2055.645399	218315.350216	37.866880
2057.677738	218685.061867	37.871898
2060.086177	219033.223050	37.876916
2062.930786	219391.013140	37.881933
2064.354683	219738.938571	37.886951
2066.695825	220087.343201	37.891968
2068.871743	220439.688645	37.896986
2070.945985	220777.143227	37.902004
2072.905716	221131.762926	37.907021
2075.596764	221482.093147	37.912039
2078.046389	221830.611552	37.917056
2079.914210	222175.191966	37.922074
2082.180664	222511.450335	37.927092
2084.273079	222852.285954	37.932109
2086.492159	223199.933405	37.937127
2088.647614	223538.499590	37.942144
2090.304851	223896.100226	37.947162
2092.612250	224230.552930	37.952180
2095.116425	224575.183681	37.957197
2096.984013	224909.433991	37.962215
2099.583108	225250.418113	37.967232
2101.900551	225585.304439	37.972250
2104.097898	225928.086247	37.977268
2106.152428	226256.084953	37.982285
2107.561118	226584.169506	37.987303
2109.928207	226910.897128	37.992320
2112.062048	227254.556774	37.997338
2114.469270	227579.780481	38.002356
2116.385485	227916.087395	38.007373
2118.358147	228261.047095	38.012391
2120.900349	228579.493413	38.017408
2123.049982	228911.825614	38.022426
2124.840998	229215.237478	38.027444
2127.095708	229508.638896	38.032461
2128.979434	229820.316835	38.037479
2130.877938	230115.380604	38.042496
2132.865624	230439.717142	38.047514
2135.026407	230755.566172	38.052532
2137.047629	231070.423653	38.057549
2138.900731	231395.115382	38.062567
2141.497772	231703.118900	38.067584
2143.494179	232023.748571	38.072602
2145.501569	232353.013453	38.077620
2147.618135	232671.566305	38.082637
2149.342331	232997.858097	38.087655
2151.398419	233332.730269	38.092672
2153.306784	233680.811763	38.097690
2155.368163	234026.353009	38.102708
2157.280504	234375.121013	38.107725
2159.394637	234728.021054	38.112743
2161.827952	235075.634415	38.117760
2163.861850	235445.187684	38.122778
2165.800735	235798.068878	38.127796
2168.020404	236155.475036	38.132813
2170.362698	236522.920041	38.137831
2172.937635	236871.096609	38.142848
2175.712867	237231.229279	38.147866
2178.149324	237572.521340	38.152884
2180.773926	237915.864745	38.157901
2182.610104	238263.509465	38.162919
2185.077585	238607.795293	38.167936
2187.345042	238958.745834	38.172954
2189.448943	239311.096597	38.177972
2191.801122	239658.706001	38.182989
2193.691108	240010.306902	38.188007
2195.877264	240358.885581	38.193024
2198.114317	240729.759374	38.198042
2200.140606	241089.391044	38.203060
2202.267066	241450.225397	38.208077
2203.946035	241824.447679	38.213095
2206.064443	242194.810341	38.218112
2207.728687	242568.426471	38.223130
2209.761565	242944.164672	38.228148
2211.863868	243339.375317	38.233165
2214.264659	243715.483406	38.238183
2216.432928	244110.378913	38.243200
2218.450323	244511.854606	38.248218
2220.447839	244895.907862	38.253236
2222.921979	245284.579561	38.258253
2225.034185	245701.155080	38.263271
2227.302731	246092.936531	38.268288
2229.581959	246499.983689	38.273306
2231.846588	246891.487165	38.278324
2234.347885	247280.562660	38.283341
2236.217614	247690.526115	38.288359
2238.816113	248091.067832	38.293376
2240.952694	248487.395756	38.298394
2243.458963	248854.752137	38.303412
2246.044572	249208.148937	38.308429
2248.545132	249575.049528	38.313447
2250.986451	249927.353713	38.318464
2252.897548	250285.794695	38.323482
2254.997706	250656.498648	38.328500
2257.137738	251009.083563	38.333517
2259.020891	251389.097138	38.338535
2261.203618	251753.004892	38.343552
2263.564905	252130.701583	38.348570
2265.476194	252508.678597	38.353588
2268.398212	252885.720841	38.358605
2269.878351	253276.727463	38.363623
2272.525021	253656.611384	38.368640
2274.600744	254049.523253	38.373658
2277.068497	254436.703275	38.378676
2279.151179	254828.877436	38.383693
2281.453615	255221.674571	38.388711
2283.969050	255614.816388	38.393728
2286.249196	256026.110957	38.398746
2288.078464	256423.383857	38.403764
2290.739684	256827.347981	38.408781
2293.018130	257239.913018	38.413799
2295.415942	257631.169733	38.418816
2297.829851	258029.180906	38.423834
2300.278907	258449.617038	38.428852
2302.846786	258843.588049	38.433869
2304.879792	259252.130239	38.438887
2307.381969	259651.192927	38.443904
2309.578982	260059.097167	38.448922
2312.186733	260471.427398	38.453940
2314.538547	260872.903274	38.458957
2316.495218	261285.598515	38.463975
2318.924999	261695.037281	38.468992
2321.584449	262106.036965	38.474010
2323.945688	262522.599878	38.479028
2326.052315	262928.206533	38.484045
2328.828291	263341.471832	38.489063
2331.524322	263747.993305	38.494080
2334.030024	264146.570477	38.499098
2335.893564	264554.986496	38.504116
2338.717200	264957.039713	38.509133
2341.489127	265356.205501	38.514151
2343.469316	265756.954274	38.519168
2346.540049	266151.851388	38.524186
2348.969938	266550.007657	38.529204
2351.065227	266940.752300	38.534221
2353.079336	267337.429296	38.539239
2355.661760	267722.653654	38.544256
2358.311587	268119.043313	38.549274
2360.405732	268525.968063	38.554292
2362.838138	268911.242175	38.559309
2365.348972	269314.462140	38.564327
2367.700827	269704.778819	38.569344
2369.839311	270072.904177	38.574362
2372.053647	270449.424381	38.579380
2374.599859	270806.556007	38.584397
2376.351017	271171.672495	38.589415
2378.405826	271540.394555	38.594432
2380.875066	271916.615203	38.599450
2382.525820	272304.203122	38.604468
2384.691920	272690.737068	38.609485
2386.906595	273091.690658	38.614503
2389.063380	273484.169121	38.619520
2391.770818	273878.203954	38.624538
2394.010992	274287.660957	38.629556
2396.786870	274681.657329	38.634573
2399.148049	275085.783155	38.639591
2401.716984	275496.959905	38.644608
2404.258794	275902.958491	38.649626
2406.109308	276310.217566	38.654644
2409.041477	276714.826937	38.659661
2411.049897	277130.186006	38.664679
2413.299374	277552.056669	38.669696
2415.908089	277973.636389	38.674714
2418.053679	278408.477841	38.679732
2420.738701	278827.019804	38.684749
2423.143178	279259.427243	38.689767
2425.489662	279689.176394	38.694784
2427.907598	280111.190234	38.699802
2429.992709	280567.755065	38.704820
2432.649961	281004.534819	38.709837
2434.966528	281446.934551	38.714855
2436.919114	281895.389996	38.719872
2439.290816	282348.344750	38.724890
2441.898564	282815.482452	38.729908
2444.483265	283266.391459	38.734925
2447.441482	283720.613606	38.739943
2449.921892	284168.743656	38.744960
2453.131523	284618.195534	38.749978
2455.319833	285065.763157	38.754996
2458.763260	285504.910432	38.760013
2461.254547	285943.152280	38.765031
2463.719661	286374.107293	38.770048
2466.519601	286805.943526	38.775066
2469.044559	287240.848016	38.780084
2471.638215	287664.766456	38.785101
2474.128658	288092.765188	38.790119
2476.324022	288517.129940	38.795136
2479.161397	288945.752327	38.800154
2481.330188	289388.279664	38.805172
2484.025124	289821.800170	38.810189
2486.584289	290251.989595	38.815207
2488.711199	290683.724557	38.820224
2491.247388	291104.263021	38.825242
2493.647415	291549.282885	38.830260
2496.353395	291987.949725	38.835277
2498.496728	292423.053585	38.840295
2500.154708	292857.578369	38.845312
2502.602578	293293.058610	38.850330
2504.935709	293724.111949	38.855348
2507.359795	294142.728029	38.860365
2509.536077	294569.487042	38.865383
2511.744060	295001.115472	38.870400
2513.852085	295430.219383	38.875418
2516.550939	295866.433693	38.880436
2519.850268	296287.888714	38.885453
2523.345269	296698.819106	38.890471
2526.294816	297111.009383	38.895488
2529.297957	297525.906394	38.900506
2531.627212	297948.841000	38.905524
2533.931548	298352.831316	38.910541
2536.630271	298772.245122	38.915559
2538.633272	299189.591837	38.920576
2541.058851	299600.083385	38.925594
2543.272538	300036.717825	38.930612
2545.796464	300462.249420	38.935629
2548.024655	300903.118663	38.940647
2550.801923	301345.618935	38.945664
2553.035419	301789.911590	38.950682
2555.331794	302240.337313	38.955700
2557.713946	302695.774626	38.960717
2560.315618	303150.791126	38.965735
2562.550907	303616.254977	38.970752
2565.353421	304071.816451	38.975770
2568.259271	304550.417452	38.980788
2570.547810	305016.626488	38.985805
2573.430249	305485.271008	38.990823
2575.708822	305958.587316	38.995840
2579.077691	306425.238713	39.000858
2581.394338	306900.193795	39.005876
2584.328768	307352.159450	39.010893
2587.207901	307814.188445	39.015911
2589.955333	308286.395219	39.020928
2592.701728	308744.835399	39.025946
2595.520786	309215.068950	39.030964
2597.896613	309674.049487	39.035981
2600.498439	310138.600789	39.040999
2602.977904	310608.071232	39.046016
2606.051973	311066.593907	39.051034
2608.781908	311539.367724	39.056052
2611.173248	311999.321823	39.061069
2613.757476	312463.455397	39.066087
2616.074008	312939.211122	39.071104
2618.643283	313406.820106	39.076122
2621.340265	313885.729486	39.081140
2624.015402	314360.982809	39.086157
2626.648480	314827.835156	39.091175
2629.618508	315305.977233	39.096192
2631.784697	315776.102473	39.101210
2634.633315	316244.305031	39.106228
2637.135667	316715.940687	39.111245
2640.064228	317171.706538	39.116263
2642.371171	317660.483045	39.121280
2645.541647	318123.843939	39.126298
2647.751820	318555.575882	39.131316
2650.494101	318998.411514	39.136333
2653.122092	319428.212750	39.141351
2655.058490	319873.973152	39.146368
2657.761784	320319.929480	39.151386
2660.369698	320779.685971	39.156404
2662.843040	321229.534567	39.161421
2665.290403	321676.616881	39.166439
2667.376357	322159.379687	39.171456
2669.726710	322626.656668	39.176474
2672.327304	323111.761500	39.181492
2674.915791	323596.940726	39.186509
2677.513775	324083.536243	39.191527
2680.469254	324581.923315	39.196544
2683.146752	325069.411263	39.201562
2685.683166	325563.164871	39.206580
2688.542297	326071.279682	39.211597
2691.561782	326564.536121	39.216615
2694.517590	327061.201220	39.221632
2697.374571	327549.120246	39.226650
2700.309356	328044.206435	39.231668
2703.291929	328543.088220	39.236685
2706.329883	329032.156817	39.241703
2708.878530	329531.967166	39.246720
2712.350628	329999.019076	39.251738
2714.999848	330496.087234	39.256756
2717.613535	330980.997104	39.261773
2720.669695	331453.768834	39.266791
2723.533079	331946.497035	39.271808
2726.644955	332428.846467	39.276826
2729.471107	332909.158817	39.281844
2732.029989	333397.280277	39.286861
2735.217053	333868.713749	39.291879
2737.902797	334357.616969	39.296896
2740.506791	334829.217615	39.301914
2743.158429	335308.243330	39.306932
2745.725077	335795.325756	39.311949
2748.273095	336280.502995	39.316967
2751.082748	336771.139069	39.321984
2753.886884	337249.917513	39.327002
2756.361058	337749.282401	39.332020
2758.630868	338239.158829	39.337037
2761.781033	338747.332856	39.342055
2763.981003	339263.430912	39.347072
2767.049195	339752.927510	39.352090
2770.008529	340253.199531	39.357108
2772.313654	340764.238281	39.362125
2775.334645	341264.768528	39.367143
2778.624742	341775.272919	39.372160
2781.614839	342274.401968	39.377178
2784.678778	342772.802514	39.382196
2787.323551	343270.178096	39.387213
2790.214182	343771.516365	39.392231
2792.615345	344272.120755	39.397248
2795.690115	344746.312007	39.402266
2797.876914	345219.609595	39.407284
2800.746120	345692.481157	39.412301
2803.402624	346158.202134	39.417319
2806.148131	346631.237359	39.422336
2808.827625	347103.999759	39.427354
2811.522159	347579.216229	39.432372
2814.016693	348046.848680	39.437389
2816.943605	348534.881476	39.442407
2819.617275	349015.770588	39.447424
2821.974263	349515.943806	39.452442
2824.847549	350011.227024	39.457460
2827.521643	350519.937030	39.462477
2830.338785	351014.355631	39.467495
2832.908159	351527.410870	39.472512
2835.431589	352047.445897	39.477530
2838.428850	352574.701476	39.482548
2840.693442	353107.125152	39.487565
2843.722134	353641.162342	39.492583
2846.546186	354181.266599	39.497600
2849.533189	354710.577774	39.502618
2852.820941	355248.229231	39.507636
2855.323647	355801.941776	39.512653
2858.195053	356337.544210	39.517671
2861.142343	356894.058439	39.522688
2864.438927	357438.022562	39.527706
2867.435496	357982.106724	39.532724
2870.344996	358538.630093	39.537741
2873.545607	359082.080905	39.542759
2876.245730	359639.208180	39.547776
2879.111535	360179.326905	39.552794
2882.101115	360731.010880	39.557812
2884.912036	361290.759581	39.562829
2887.890829	361836.696333	39.567847
2891.065670	362393.246577	39.572864
2894.100456	362952.983688	39.577882
2897.458937	363501.038940	39.582900
2900.137064	364055.239940	39.587917
2903.363524	364608.857168	39.592935
2906.227685	365146.039936	39.597952
2909.548679	365692.294121	39.602970
2912.985424	366222.844483	39.607988
2916.104632	366774.418686	39.613005
2918.817002	367304.519258	39.618023
2921.902876	367846.647302	39.623040
2924.613385	368389.795278	39.628058
2927.881958	368917.570732	39.633076
2930.420985	369457.586898	39.638093
2933.394228	370003.481119	39.643111
2936.080604	370538.966584	39.648128
2939.490969	371069.552192	39.653146
2943.102118	371586.298636	39.658164
2946.052317	372119.356527	39.663181
2949.015018	372633.231104	39.668199
2952.039953	373161.467125	39.673216
2955.008385	373673.651605	39.678234
2957.923174	374161.872367	39.683252
2960.852090	374651.199651	39.688269
2963.706653	375129.729565	39.693287
2966.473219	375603.500328	39.698304
2969.047491	376089.114532	39.703322
2971.706579	376574.047994	39.708340
2974.210279	377064.960186	39.713357
2977.283225	377564.414927	39.718375
2980.298936	378067.447387	39.723392
2983.063738	378571.960486	39.728410
2986.122531	379070.355523	39.733428
2989.064568	379592.927356	39.738445
2992.481235	380101.996686	39.743463
2995.635922	380617.289578	39.748480
2998.522587	381136.879770	39.753498
3001.783281	381644.557247	39.758516
3004.504002	382159.519593	39.763533
3007.907647	382670.275131	39.768551
3010.432725	383197.297338	39.773568
3012.934361	383727.382587	39.778586
3015.700703	384251.557412	39.783604
3018.999484	384795.381845	39.788621
3021.998592	385336.459465	39.793639
3024.808639	385882.782432	39.798656
3027.031007	386440.578743	39.803674
3030.299544	387001.963569	39.808692
3033.032959	387574.862425	39.813709
3035.955404	388142.090863	39.818727
3039.267679	388718.139713	39.823744
3042.051000	389307.702736	39.828762
3045.539211	389885.043065	39.833780
3048.269788	390477.608896	39.838797
3051.087350	391064.648023	39.843815
3054.360072	391649.063345	39.848832
3056.985780	392244.958123	39.853850
3060.242057	392846.993620	39.858868
3063.463287	393446.285694	39.863885
3066.657045	394051.196789	39.868903
3070.016875	394644.637066	39.873920
3073.585259	395245.531351	39.878938
3077.060426	395832.617408	39.883956
3080.382832	396424.862212	39.888973
3083.641763	397010.263498	39.893991
3086.877064	397597.734941	39.899008
3089.913717	398180.489609	39.904026
3093.066645	398760.881264	39.909044
3096.294125	399349.433099	39.914061
3099.663523	399934.198305	39.919079
3102.893997	400506.052449	39.924096
3105.855200	401093.295892	39.929114
3108.929628	401674.350675	39.934132
3111.966356	402259.909819	39.939149
3115.088306	402833.888630	39.944167
3118.516546	403412.743765	39.949184
3120.857626	403976.900540	39.954202
3124.802339	404529.269744	39.959220
3127.546941	405067.544161	39.964237
3130.773735	405589.207838	39.969255
3133.844807	406130.521582	39.974272
3136.556702	406671.404543	39.979290
3139.818430	407205.165656	39.984308
3143.013601	407742.246043	39.989325
3145.716959	408286.213847	39.994343
3148.841217	408832.961082	39.999360
3151.696007	409392.686965	40.004378
3154.745096	409950.341460	40.009396
3157.297861	410518.732619	40.014413
3160.256952	411099.655844	40.019431
3163.444339	411672.903413	40.024448
3166.361215	412263.610044	40.029466
3169.839010	412856.258957	40.034484
3172.597208	413462.668213	40.039501
3175.906388	414060.383647	40.044519
3179.403052	414647.213937	40.049536
3182.485184	415255.855536	40.054554
3186.046370	415866.224139	40.059572
3188.985799	416464.731596	40.064589
3192.247608	417076.793579	40.069607
3195.488168	417687.299688	40.074624
3198.919713	418307.684447	40.079642
3202.298766	418916.567051	40.084660
3205.692320	419528.977178	40.089677
3208.807067	420143.014981	40.094695
3212.413905	420748.902012	40.099712
3215.019527	421381.225811	40.104730
3218.341064	421997.359527	40.109748
3221.465896	422626.119320	40.114765
3224.280001	423258.915995	40.119783
3227.654081	423889.170217	40.124800
3230.913603	424540.084837	40.129818
3234.380052	425175.808425	40.134836
3237.804787	425822.103515	40.139853
3240.884366	426468.895729	40.144871
3244.356057	427107.098406	40.149888
3247.252596	427750.748265	40.154906
3250.448362	428399.239862	40.159924
3254.103903	429043.787890	40.164941
3257.595419	429689.510473	40.169959
3261.404898	430330.959606	40.174976
3264.857652	430977.361814	40.179994
3268.605164	431597.679386	40.185012
3272.223602	432220.583666	40.190029
3274.996006	432846.956023	40.195047
3278.897003	433464.666457	40.200064
3282.309085	434088.263836	40.205082
3285.602347	434703.109170	40.210100
3288.770236	435319.123229	40.215117
3291.985468	435933.847286	40.220135
3295.098065	436543.612883	40.225152
3298.247524	437164.387088	40.230170
3301.546435	437750.001036	40.235188
3304.901138	438333.262469	40.240205
3308.120734	438904.084321	40.245223
3311.387194	439476.957978	40.250240
3314.433481	440065.944038	40.255258
3317.469644	440639.737568	40.260276
3320.115057	441231.391824	40.265293
3323.495846	441824.574048	40.270311
3326.723624	442414.831998	40.275328
3329.670506	443035.323851	40.280346
3332.457569	443648.844081	40.285364
3336.188366	444271.443071	40.290381
3339.350393	444891.996605	40.295399
3342.740932	445517.602118	40.300416
3345.700491	446160.713775	40.305434
3349.286522	446793.633491	40.310452
3352.542538	447436.048996	40.315469
3355.576828	448092.948047	40.320487
3358.796854	448751.969686	40.325504
3361.912038	449420.395395	40.330522
3365.375284	450083.834775	40.335540
3368.625339	450761.196526	40.340557
3371.592811	451449.102914	40.345575
3375.429412	452131.073320	40.350592
3378.582634	452837.510736	40.355610
3382.169823	453524.534215	40.360628
3385.791365	454221.540196	40.365645
3389.171140	454921.647887	40.370663
3392.838871	455618.648766	40.375680
3396.313599	456313.939689	40.380698
3399.787551	457007.589032	40.385716
3403.596759	457706.010402	40.390733
3407.402724	458405.570703	40.395751
3411.093080	459082.934627	40.400768
3414.348345	459781.529715	40.405786
3417.814984	460476.424748	40.410804
3421.402569	461168.090373	40.415821
3424.699758	461868.019880	40.420839
3428.452065	462562.287163	40.425856
3431.819058	463259.021524	40.430874
3435.581416	463952.327985	40.435892
3439.553725	464631.120525	40.440909
3443.340607	465317.854842	40.445927
3446.679419	465993.220877	40.450944
3449.997399	466664.726425	40.455962
3453.603785	467343.991228	40.460980
3457.992513	468029.161577	40.465997
3461.109366	468690.524866	40.471015
3464.413986	469368.707988	40.476032
3467.976424	470028.331779	40.481050
3471.372698	470708.371020	40.486068
3474.698408	471378.395105	40.491085
3477.854887	472056.506784	40.496103
3481.479248	472727.088319	40.501120
3484.658159	473389.923289	40.506125
3488.065444	474010.861040	40.511130
3491.072700	474581.308824	40.516135
3494.032546	475106.325431	40.521140
3496.969947	475576.188316	40.526144
3500.061907	475993.048752	40.531149
3502.378048	476352.410868	40.536154
3504.711354	476644.623613	40.541159
3506.918895	476902.524426	40.546164
3508.736550	477101.957845	40.551168
3510.884755	477265.131233	40.556173
3512.977992	477383.149689	40.561178
3514.165484	477453.729076	40.566183
3515.495630	477480.792032	40.571188
3516.588492	477474.428528	40.576192
3517.831111	477451.381903	40.581197
3518.213567	477396.128921	40.586202
3519.262960	477311.800838	40.591207
3519.504146	477212.977858	40.596212
3519.926130	477073.972406	40.601216
3520.321447	476936.793214	40.606221
3520.773263	476786.590746	40.611226
3521.093703	476618.687874	40.616231
3521.490565	476440.593052	40.621236
3521.615410	476243.099419	40.626240
3521.592538	476048.413794	40.631245
3521.698461	475832.184106	40.636250
3521.712160	475615.106811	40.641255
3521.475436	475409.665479	40.646260
3521.433006	475168.438872	40.651264
3521.206088	474942.583868	40.656269
3521.318059	474711.958864	40.661274
3521.340317	474483.878254	40.666279
3520.969021	474250.544864	40.671284
3520.772324	474013.228776	40.676288
3520.709339	473783.533607	40.681293
3520.376093	473558.591409	40.686298
3520.313486	473316.229999	40.691303
3519.666395	473084.600234	40.696308
3519.536889	472858.601925	40.701312
3519.174407	472633.501606	40.706317
3518.923417	472406.860193	40.711322
3519.383834	472197.516543	40.716327
3518.733222	471973.521019	40.721332
3518.598940	471745.281639	40.726336
3518.403889	471528.040277	40.731341
3517.838221	471319.520429	40.736346
3517.917634	471100.961069	40.741351
3517.572837	470896.805212	40.746356
3517.017916	470688.681720	40.751360
3517.003076	470482.489706	40.756365
3516.183823	470288.133039	40.761370
3515.954797	470102.436200	40.766375
3515.508317	469922.245017	40.771380
3515.413478	469730.038226	40.776384
3514.964448	469567.116389	40.781389
3514.697016	469389.270217	40.786394
3514.856136	469209.475371	40.791399
3514.070003	469057.801090	40.796404
3513.957509	468894.309470	40.801408
3513.801961	468737.206271	40.806413
3513.263960	468587.815978	40.811418
3513.424372	468430.909574	40.816423
3513.381198	468288.574849	40.821428
3513.209024	468138.358728	40.826432
3513.176778	467998.755405	40.831437
3512.815545	467866.603141	40.836442
3512.532581	467712.299375	40.841447
3512.174558	467593.264904	40.846452
3511.895577	467450.254984	40.851456
3511.640918	467316.814270	40.856461
3511.794815	467194.295799	40.861466
3511.509423	467059.693391	40.866471
3511.336521	466945.891821	40.871476
3511.233665	466818.146216	40.876480
3511.155048	466703.364576	40.881485
3510.531234	466593.133442	40.886490
3511.166063	466479.748454	40.891495
3510.716961	466370.246118	40.896500
3510.395427	466262.950466	40.901504
3510.025856	466159.462021	40.906509
3509.901234	466054.563331	40.911514
3510.536543	465951.560790	40.916519
3509.793610	465848.235748	40.921524
3509.754636	465753.807870	40.926528
3509.415041	465651.324827	40.931533
3509.199080	465567.464102	40.936538
3509.317080	465479.391609	40.941543
3509.274424	465401.985459	40.946548
3508.946996	465317.028085	40.951552
3509.179560	465238.763671	40.956557
3509.192124	465155.166119	40.961562
3508.992801	465070.287115	40.966567
3508.742236	464989.824296	40.971572
3508.827053	464902.666805	40.976576
3508.478047	464832.099751	40.981581
3508.210367	464762.531854	40.986586
3508.323359	464684.336282	40.991591
3508.280156	464617.566790	40.996596
3508.026364	464542.321203	41.001600
3508.131180	464479.781875	41.006605
3507.906446	464416.082634	41.011610
3508.630329	464348.522581	41.016615
3508.204349	464273.305351	41.021620
3508.269072	464192.076059	41.026624
3508.048546	464126.905821	41.031629
3507.756661	464062.304885	41.036634
3507.898451	464001.277711	41.041639
3507.909610	463944.326027	41.046644
3507.568464	463876.236847	41.051648
3507.758103	463809.070149	41.056653
3507.500102	463746.742418	41.061658
3507.257371	463681.219804	41.066663
3506.828956	463629.966390	41.071668
3506.822693	463575.550002	41.076672
3506.891842	463536.321066	41.081677
3506.821754	463486.424801	41.086682
3506.850192	463429.772673	41.091687
3506.777522	463385.095447	41.096692
3506.754713	463337.116136	41.101696
3506.477993	463288.116015	41.106701
3506.653363	463243.548119	41.111706
3506.970762	463192.014200	41.116711
3506.505613	463151.963678	41.121716
3506.566576	463099.966609	41.126720
3506.535321	463065.111437	41.131725
3506.599224	463029.581250	41.136730
3506.591584	462988.692231	41.141735
3506.313230	462941.515627	41.146740
3506.131878	462900.352065	41.151744
3506.084322	462855.872021	41.156749
3506.003014	462829.841556	41.161754
3506.205231	462783.494575	41.166759
3505.986881	462746.086600	41.171764
3506.163923	462719.251821	41.176768
3506.123579	462679.533158	41.181773
3506.117810	462636.464253	41.186778
3506.391431	462603.532354	41.191783
3506.106300	462577.739039	41.196788
3506.394826	462534.974356	41.201792
3506.461616	462493.108847	41.206797
3506.217552	462460.011747	41.211802
3506.478599	462405.597132	41.216807
3505.925459	462377.265085	41.221812
3505.740304	462326.828125	41.226816
3506.123018	462294.991852	41.231821
3505.558069	462268.536508	41.236826
3505.451799	462242.408181	41.241831
3505.479422	462220.006661	41.246836
3505.794432	462178.300784	41.251840
3506.040251	462155.456559	41.256845
3505.794840	462119.825523	41.261850
3505.905103	462080.738667	41.266855
3505.368048	462052.555419	41.271860
3505.901814	462024.594666	41.276864
3506.291070	461995.594433	41.281869
3505.752830	461965.283028	41.286874
3505.987319	461921.360773	41.291879
3505.778870	461889.219404	41.296884
3506.202494	461851.294726	41.301888
3506.044520	461828.975123	41.306893
3505.607808	461785.724572	41.311898
3505.597611	461751.978271	41.316903
3505.495076	461735.881858	41.321908
3505.439384	461699.153533	41.326912
3505.648905	461676.061585	41.331917
3505.376936	461650.923554	41.336922
3505.413677	461627.455666	41.341927
3505.044031	461602.232904	41.346932
3505.100465	461577.038703	41.351936
3505.569272	461554.662440	41.356941
3504.947051	461534.246014	41.361946
3505.211331	461497.158637	41.366951
3505.288780	461481.639365	41.371956
3505.180821	461458.398678	41.376960
3505.161889	461435.598825	41.381965
3504.921881	461421.856617	41.386970
3504.954799	461389.470523	41.391975
3505.095546	461378.399656	41.396980
3505.059885	461355.450545	41.401984
3505.319314	461335.846175	41.406989
3504.993434	461317.861946	41.411994
3505.315103	461288.618844	41.416999
3505.403260	461275.833981	41.422004
3505.664295	461247.259934	41.427008
3505.356226	461215.691891	41.432013
3505.471756	461192.159358	41.437018
3505.497367	461163.980108	41.442023
3505.726895	461146.204933	41.447028
3505.968680	461113.782724	41.452032
3505.647398	461085.561245	41.457037
3505.437246	461062.540239	41.462042
3505.599111	461020.452665	41.467047
3505.209090	460994.067084	41.472052
3505.351492	460960.546746	41.477056
3505.426634	460938.389030	41.482061
3505.408411	460923.341730	41.487066
3505.553635	460886.526911	41.492071
3505.436826	460863.945810	41.497076
3505.124152	460837.394787	41.502080
3505.239599	460810.719951	41.507085
3505.016672	460793.325767	41.512090
3505.729079	460758.491552	41.517095
3505.561553	460734.956131	41.522100
3505.461141	460709.432876	41.527104
3505.406402	460684.661924	41.532109
3505.629142	460656.904373	41.537114
3505.743077	460627.290359	41.542119
3505.733209	460604.487999	41.547124
3505.537797	460564.690196	41.552128
3505.319958	460532.396190	41.557133
3504.802232	460523.312290	41.562138
3504.740529	460490.788852	41.567143
3504.621835	460480.217867	41.572148
3504.744347	460454.605544	41.577152
3504.767600	460449.939418	41.582157
3504.874244	460434.312988	41.587162
3505.014383	460415.336190	41.592167
3505.082245	460395.054131	41.597172
3505.102146	460383.699284	41.602176
3505.589468	460356.149517	41.607181
3504.905701	460336.806561	41.612186
3505.438475	460307.728671	41.617191
3505.260903	460288.299235	41.622196
3504.832757	460262.476628	41.627200
3505.170223	460240.678753	41.632205
3505.212103	460218.576587	41.637210
3505.441294	460198.368134	41.642215
3505.079924	460165.185854	41.647220
3504.908729	460145.248420	41.652224
3505.073782	460126.115061	41.657229
3505.001935	460113.863539	41.662234
3505.094199	460083.086840	41.667239
3505.194600	460071.363329	41.672244
3505.050373	460045.542637	41.677248
3505.122751	460028.553453	41.682253
3504.846283	460014.157685	41.687258
3504.956526	459982.617600	41.692263
3504.799948	459973.877199	41.697268
3505.184993	459949.942430	41.702272
3505.061553	459929.236462	41.707277
3504.578915	459920.602390	41.712282
3504.806676	459897.657287	41.717287
3504.655356	459886.179358	41.722292
3504.871840	459867.898489	41.727296
3505.284631	459845.073765	41.732301
3504.924154	459835.709308	41.737306
3505.016866	459801.638041	41.742311
3505.069821	459791.848225	41.747316
3504.995885	459762.822456	41.752320
3505.510799	459740.537633	41.757325
3504.919264	459721.685106	41.762330
3505.445089	459688.097149	41.767335
3505.310134	459670.129497	41.772340
3504.861883	459652.215324	41.777344
3504.990668	459626.904932	41.782349
3505.031513	459609.312634	41.787354
3505.080388	459582.495479	41.792359
3505.085323	459566.683019	41.797364
3504.956656	459549.322326	41.802368
3504.932702	459528.903025	41.807373
3504.970707	459501.884904	41.812378
3504.646420	459484.760270	41.817383
3504.972763	459466.409596	41.822388
3504.700042	459449.934951	41.827392
3505.174819	459431.254827	41.832397
3505.032127	459413.896410	41.837402
3504.929954	459389.081261	41.842407
3504.841439	459377.896388	41.847412
3504.783444	459347.600318	41.852416
3504.814092	459331.073774	41.857421
3504.581086	459318.494526	41.862426
3504.988075	459307.072969	41.867431
3504.721490	459294.702156	41.872436
3504.777474	459273.458077	41.877440
3504.575060	459263.559568	41.882445
3504.470648	459245.079524	41.887450
3504.460380	459235.959061	41.892455
3504.523742	459216.284720	41.897460
3504.789707	459210.309877	41.902464
3505.116661	459192.668358	41.907469
3504.948278	459175.010043	41.912474
3504.778287	459156.845192	41.917479
3504.896107	459127.228280	41.922484
3504.841643	459117.405795	41.927488
3504.891125	459091.956225	41.932493
3504.697839	459085.552966	41.937498
3505.011840	459056.155849	41.942503
3505.121007	459053.704635	41.947508
3504.440034	459031.116420	41.952512
3505.243592	459015.724637	41.957517
3504.727427	458997.416030	41.962522
3504.861511	458974.536540	41.967527
3505.088228	458947.941565	41.972532
3505.233609	458922.982206	41.977536
3505.381232	458894.626863	41.982541
3504.746043	458886.677228	41.987546
3505.063421	458862.296587	41.992551
3505.053464	458844.205486	41.997556
3504.580372	458819.148880	42.002560
3504.758064	458791.649821	42.007565
3504.828458	458786.164370	42.012570
3505.199765	458764.409784	42.017575
3504.900996	458742.617548	42.022580
3504.419888	458724.150662	42.027584
3505.013878	458703.320918	42.032589
3504.897146	458705.469493	42.037594
3504.811572	458677.407062	42.042599
3505.027743	458665.156150	42.047604
3505.000916	458635.360484	42.052608
3504.988932	458617.725651	42.057613
3504.715701	458600.388815	42.062618
3505.052080	458586.444859	42.067623
3504.560177	458562.759528	42.072628
3504.768262	458547.722469	42.077632
3504.980759	458523.714092	42.082637
3504.672463	458521.587501	42.087642
3505.041323	458488.176374	42.092647
3504.935595	458470.709462	42.097652
3504.881269	458453.487164	42.102656
3504.756806	458428.775989	42.107661
3504.682370	458413.584345	42.112666
3504.785922	458402.315448	42.117671
3504.684460	458375.116890	42.122676
3504.725902	458360.868367	42.127680
3504.826355	458348.738384	42.132685
3504.898475	458330.176669	42.137690
3504.839928	458307.582716	42.142695
3505.027835	458291.738004	42.147700
3504.854687	458280.972421	42.152704
3504.644537	458252.069075	42.157709
3504.763043	458247.234125	42.162714
3504.668070	458220.338339	42.167719
3504.791340	458212.208245	42.172724
3504.554535	458189.695279	42.177728
3505.028478	458171.622307	42.182733
3504.580710	458153.960112	42.187738
3504.550661	458134.604748	42.192743
3504.856218	458120.615050	42.197748
3504.702140	458103.510848	42.202752
3504.814159	458098.372876	42.207757
3504.353131	458083.804495	42.212762
3504.975618	458056.735302	42.217767
3504.609923	458058.875774	42.222772
3504.779201	458037.915131	42.227776
3504.750754	458016.785499	42.232781
3504.838254	457999.437229	42.237786
3504.750061	457990.380186	42.242791
3505.223656	457968.911367	42.247796
3504.901109	457952.748087	42.252800
3504.544288	457920.524259	42.257805
3504.339177	457915.693803	42.262810
3504.342914	457897.447460	42.267815
3504.771494	457879.787434	42.272820
3504.624719	457875.808615	42.277824
3504.940944	457846.307978	42.282829
3504.728122	457843.354086	42.287834
3505.103920	457822.966150	42.292839
3504.814243	457805.378018	42.297844
3504.483386	457788.405098	42.302848
3504.730042	457767.228229	42.307853
3504.458847	457754.654515	42.312858
3504.613624	457735.723355	42.317863
3504.645615	457729.585292	42.322868
3504.631972	457711.848579	42.327872
3504.694203	457689.638773	42.332877
3504.455048	457675.589725	42.337882
3504.647218	457666.687396	42.342887
3504.651864	457649.352971	42.347892
3504.510484	457632.296882	42.352896
3504.684403	457602.668137	42.357901
3504.721334	457604.081022	42.362906
3504.973547	457586.907006	42.367911
3505.043756	457568.953115	42.372916
3504.523804	457558.347726	42.377920
3505.015771	457533.884978	42.382925
3504.490260	457526.473589	42.387930
3504.592677	457500.252704	42.392935
3504.987499	457488.629459	42.397940
3504.514450	457468.740891	42.402944
3504.754927	457454.964578	42.407949
3504.863695	457436.446463	42.412954
3504.577227	457421.188903	42.417959
3504.691168	457406.927324	42.422964
3504.474148	457384.511443	42.427968
3504.305113	457374.707666	42.432973
3504.545227	457363.769657	42.437978
3504.684330	457342.762758	42.442983
3504.654536	457341.652851	42.447988
3504.306929	457312.467517	42.452992
3504.743317	457302.915118	42.457997
3504.487488	457300.728752	42.463002
3504.296153	457273.391993	42.468007
3504.452364	457263.076468	42.473012
3504.326423	457261.526814	42.478016
3504.714317	457241.440331	42.483021
3504.607181	457230.358805	42.488026
3504.471705	457220.701275	42.493031
3504.804278	457201.080357	42.498036
3504.592116	457192.550966	42.503040
3504.460336	457171.083297	42.508045
3504.190453	457155.214488	42.513050
3504.514635	457146.998974	42.518055
3504.700775	457139.060449	42.523060
3504.188426	457122.168639	42.528064
3504.712979	457109.458647	42.533069
3504.661287	457099.685383	42.538074
3504.627468	457077.541987	42.543079
3504.568919	457071.621922	42.548084
3504.461293	457055.725330	42.553088
3504.270886	457038.423684	42.558093
3503.979627	457035.331010	42.563098
3504.296626	457029.498863	42.568103
3504.409273	457002.160516	42.573108
3504.181532	457002.199458	42.578112
3504.439623	456994.096536	42.583117
3504.172249	456980.964150	42.588122
3504.087501	456963.745769	42.593127
3504.052520	456961.014804	42.598132
3504.197335	456955.870942	42.603136
3504.673518	456950.417072	42.608141
3504.195452	456938.131594	42.613146
3504.611606	456928.835900	42.618151
3504.670852	456918.992921	42.623156
3504.245284	456913.135478	42.628160
3504.532633	456896.005559	42.633165
3504.800697	456894.692712	42.638170
3504.607719	456877.036570	42.643175
3504.654314	456861.518974	42.648180
3504.532528	456836.349214	42.653184
3504.426523	456818.323372	42.658189
3504.214927	456816.129399	42.663194
3504.767417	456796.065054	42.668199
3504.691267	456781.835491	42.673204
3504.116153	456786.495442	42.678208
3504.292965	456752.810114	42.683213
3503.946730	456747.699360	42.688218
3504.110620	456741.437103	42.693223
3504.270051	456743.893530	42.698228
3503.958228	456734.367249	42.703232
3504.122089	456704.941644	42.708237
3503.935909	456711.309201	42.713242
3504.103680	456705.705184	42.718247
3504.195728	456701.077124	42.723252
3504.049623	456702.622697	42.728256
3504.355838	456683.056463	42.733261
3504.166721	456686.028583	42.738266
3504.149802	456676.198491	42.743271
3504.347074	456672.312744	42.748276
3504.197700	456654.294161	42.753280
3504.132043	456642.799743	42.758285
3504.237728	456642.680381	42.763290
3504.374288	456638.602250	42.768295
3504.577658	456627.112573	42.773300
3504.476385	456608.781620	42.778304
3504.288052	456601.413686	42.783309
3504.355520	456593.495211	42.788314
3504.350192	456566.429848	42.793319
3504.395625	456563.786471	42.798324
3504.283631	456561.372719	42.803329
3504.383414	456534.238680	42.808333
3503.966192	456529.139991	42.813338
3503.964478	456515.556450	42.818343
3504.381744	456522.226517	42.823348
3504.380649	456510.974430	42.828353
3504.256411	456491.481510	42.833357
3504.255501	456492.698190	42.838362
3504.397211	456474.933862	42.843367
3504.639967	456459.990698	42.848372
3504.478067	456463.566439	42.853377
3504.741124	456441.726457	42.858381
3504.682398	456431.497894	42.863386
3504.467235	456422.613884	42.868391
3504.578866	456392.892625	42.873396
3504.347621	456393.337657	42.878401
3504.584405	456381.233897	42.883405
3504.656364	456358.666158	42.888410
3504.365878	456337.731566	42.893415
3504.563623	456335.416959	42.898420
3504.141603	456324.185955	42.903425
3504.266057	456302.166742	42.908429
3504.311524	456308.951051	42.913434
3504.206296	456304.457959	42.918439
3504.392633	456280.856869	42.923444
3503.766380	456270.167574	42.928449
3504.063510	456264.693409	42.933453
3504.166145	456266.906158	42.938458
3504.243562	456260.911952	42.943463
3504.522849	456236.382577	42.948468
3504.195945	456235.323340	42.953473
3504.434862	456227.831629	42.958477
3504.290534	456219.492990	42.963482
3504.328352	456200.276239	42.968487
3504.578079	456191.768930	42.973492
3504.328276	456186.337445	42.978497
3504.682079	456166.255716	42.983501
3504.591484	456159.529862	42.988506
3504.520782	456138.354788	42.993511
3504.468425	456119.457481	42.998516
3504.396021	456119.165776	43.003521
3504.390737	456090.072282	43.008525
3504.397509	456085.205206	43.013530
3504.530672	456080.063111	43.018535
3504.588109	456057.598891	43.023540
3504.247884	456042.400152	43.028545
3504.358768	456028.847746	43.033549
3503.910639	456030.698377	43.038554
3504.141886	456001.158869	43.043559
3504.324367	455997.782393	43.048564
3504.103544	455992.244532	43.053569
3504.358773	455991.744820	43.058573
3504.275131	455985.271159	43.063578
3504.349774	455963.868334	43.068583
3504.732163	455955.388961	43.073588
3504.385889	455938.569175	43.078593
3504.594523	455920.083306	43.083597
3504.322963	455917.544659	43.088602
3504.243169	455911.779945	43.093607
3503.982584	455876.596527	43.098612
3504.312851	455878.770451	43.103617
3504.487758	455866.930388	43.108621
3504.648753	455865.382320	43.113626
3504.477910	455845.896736	43.118631
3504.824328	455841.579861	43.123636
3504.961397	455825.944646	43.128641
3504.756569	455802.054976	43.133645
3504.713756	455779.810317	43.138650
3504.932031	455774.501548	43.143655
3505.093521	455748.014864	43.148660
3504.805494	455736.101707	43.153665
3505.000846	455712.244976	43.158669
3504.697860	455698.154759	43.163674
3504.279549	455685.554184	43.168679
3504.839636	455659.861024	43.173684
3504.968924	455649.802716	43.178689
3504.796752	455627.427913	43.183693
3504.691522	455617.054814	43.188698
3504.546885	455591.532588	43.193703
3504.582538	455564.154758	43.198708
3504.103654	455553.439918	43.203713
3504.146066	455534.779327	43.208717
3504.069517	455530.635986	43.213722
3504.308731	455523.346720	43.218727
3504.434833	455525.961053	43.223732
3504.115847	455508.984184	43.228737
3504.585705	455497.093544	43.233741
3504.256258	455480.929456	43.238746
3504.440659	455478.566342	43.243751
3504.302222	455457.706255	43.248756
3504.246841	455455.485459	43.253761
3504.610454	455444.728084	43.258765
3504.409267	455426.108987	43.263770
3504.293640	455417.106161	43.268775
3504.297295	455411.732567	43.273780
3504.303867	455407.169496	43.278785
3504.274976	455385.733051	43.283789
3504.212202	455365.620284	43.288794
3504.371180	455372.030702	43.293799
3504.343123	455362.404630	43.298804
3504.113258	455349.974424	43.303809
3504.107020	455332.132980	43.308813
3504.055911	455331.939006	43.313818
3504.470900	455328.978921	43.318823
3504.316805	455306.347232	43.323828
3504.104980	455303.848997	43.328833
3504.432219	455297.862539	43.333837
3504.308804	455286.275835	43.338842
3504.497048	455275.801761	43.343847
3504.486777	455257.859561	43.348852
3504.189920	455252.790684	43.353857
3504.249015	455227.486659	43.358861
3504.021352	455231.986254	43.363866
3503.806620	455217.221671	43.368871
3504.169146	455217.261204	43.373876
3504.090008	455222.597160	43.378881
3504.418018	455202.366816	43.383885
3504.612609	455193.716437	43.388890
3504.494239	455182.331569	43.393895
3504.470183	455156.838898	43.398900
3504.220973	455152.471513	43.403905
3504.589207	455146.478011	43.408909
3504.658627	455117.623816	43.413914
3504.409860	455104.740480	43.418919
3504.333365	455096.592555	43.423924
3503.926574	455084.192396	43.428929
3504.278144	455075.008265	43.433933
3504.614626	455066.130844	43.438938
3504.089528	455069.870225	43.443943
3504.630153	455052.087227	43.448948
3504.400592	455045.080593	43.453953
3504.060349	455043.313910	43.458957
3504.034889	455032.369303	43.463962
3504.058697	455013.457961	43.468967
3504.474001	455004.465676	43.473972
3504.041015	454999.065149	43.478977
3504.374271	454997.690362	43.483981
3504.304706	454978.389411	43.488986
3504.161729	454962.446521	43.493991
3504.346006	454958.309217	43.498996
3504.015270	454960.444037	43.504001
3504.085825	454949.482991	43.509005
3503.965760	454938.706558	43.514010
3504.194390	454923.916748	43.519015
3504.102019	454917.596306	43.524020
3503.810422	454928.747294	43.529025
3504.574994	454914.220796	43.534029
3504.483441	454890.969684	43.539034
3504.363316	454881.916698	43.544039
3504.908417	454871.736315	43.549044
3504.603723	454851.410897	43.554049
3504.516204	454840.679545	43.559053
3504.580580	454821.102123	43.564058
3504.461383	454806.067477	43.569063
3504.251597	454797.536667	43.574068
3504.198041	454792.223369	43.579073
3504.085469	454767.150847	43.584077
3503.931996	454762.209435	43.589082
3503.896044	454764.547394	43.594087
3504.006460	454764.123071	43.599092
3504.039128	454768.071411	43.604097
3503.975412	454750.695486	43.609101
3504.270788	454737.414861	43.614106
3504.032365	454727.165431	43.619111
3504.387202	454728.068020	43.624116
3503.953536	454722.718226	43.629121
3504.311627	454720.325368	43.634125
3504.173280	454698.349292	43.639130
3503.742202	454696.598088	43.644135
3504.061440	454687.368613	43.649140
3503.865195	454685.780074	43.654145
3503.843957	454683.147837	43.659149
3503.852330	454689.584186	43.664154
3503.692636	454680.994084	43.669159
3504.000314	454657.573155	43.674164
3503.726957	454649.914882	43.679169
3503.863129	454643.808786	43.684173
3504.227451	454652.566838	43.689178
3503.313588	454655.004022	43.694183
3504.001000	454652.453542	43.699188
3503.960895	454652.257682	43.704193
3504.199554	454662.152385	43.709197
3504.236626	454646.026431	43.714202
3504.019099	454629.284956	43.719207
3504.440318	454622.116364	43.724212
3503.868967	454631.541100	43.729217
3504.263513	454618.040702	43.734221
3504.476079	454599.806419	43.739226
3504.128465	454592.211494	43.744231
3504.402735	454581.164775	43.749236
3504.333751	454580.923154	43.754241
3504.427209	454557.487998	43.759245
3504.248431	454541.855038	43.764250
3504.344473	454541.635929	43.769255
3504.245631	454522.238164	43.774260
3504.032194	454516.952093	43.779265
3504.095668	454501.683267	43.784269
3504.140224	454501.675714	43.789274
3504.013914	454504.282587	43.794279
3504.141797	454496.352980	43.799284
3504.052635	454488.764577	43.804289
3504.210965	454476.216862	43.809293
3504.263975	454471.899108	43.814298
3504.151120	454472.425346	43.819303
3504.308807	454446.140384	43.824308
3504.006063	454440.514703	43.829313
3504.516499	454431.860762	43.834317
3504.499893	454432.015727	43.839322
3504.409785	454411.805303	43.844327
3504.503810	454400.586498	43.849332
3503.933221	454397.743877	43.854337
3503.879493	454371.444226	43.859341
3503.718692	454365.185989	43.864346
3503.948371	454368.745926	43.869351
3504.098426	454354.678802	43.874356
3504.170335	454360.952332	43.879361
3504.268187	454357.336579	43.884365
3503.947170	454345.073397	43.889370
3504.330671	454330.003256	43.894375
3504.137595	454319.036195	43.899380
3504.028060	454322.704751	43.904385
3504.289877	454325.296067	43.909389
3504.028426	454313.326844	43.914394
3504.101603	454292.834964	43.919399
3504.461866	454281.266482	43.924404
3503.673804	454291.184603	43.929409
3504.309381	454279.569111	43.934413
3504.183329	454264.788695	43.939418
3504.031673	454264.611878	43.944423
3504.155371	454247.659750	43.949428
3503.849047	454250.398777	43.954433
3503.919787	454245.368263	43.959437
3504.202889	454246.435199	43.964442
3503.899343	454235.486955	43.969447
3504.430217	454219.073580	43.974452
3503.829373	454215.982640	43.979457
3504.012274	454214.582784	43.984461
3504.252153	454206.938093	43.989466
3504.507836	454201.825297	43.994471
3504.534035	454176.677663	43.999476
3504.059805	454177.873917	44.004481
3504.244379	454164.459765	44.009485
3504.149390	454141.512537	44.014490
3503.933896	454136.074642	44.019495
3504.290490	454124.506699	44.024500
3504.191111	454128.477709	44.029505
3504.056992	454120.035079	44.034509
3503.991048	454093.939926	44.039514
3504.276730	454090.444131	44.044519
3503.845414	454086.766610	44.049524
3503.845299	454094.623978	44.054529
3503.650516	454083.302235	44.059533
3503.921798	454091.163956	44.064538
3503.608052	454097.959647	44.069543
3503.959667	454083.148230	44.074548
3503.844575	454070.393491	44.079553
3504.149832	454049.658970	44.084557
3504.070013	454052.105885	44.089562
3503.894611	454057.509274	44.094567
3503.967840	454055.570519	44.099572
3504.017061	454055.359400	44.104577
3504.336542	454047.396904	44.109581
3504.462854	454028.771302	44.114586
3503.736883	454026.005852	44.119591
3504.389971	454017.276687	44.124596
3504.175374	454021.267391	44.129601
3503.963978	453993.929636	44.134605
3504.142767	453979.147655	44.139610
3504.009514	453976.585146	44.144615
3504.447154	453974.280005	44.149620
3504.316656	453968.523396	44.154625
3504.485693	453949.231424	44.159629
3504.674242	453940.581547	44.164634
3504.525199	453932.851085	44.169639
3504.705280	453902.708963	44.174644
3504.658914	453903.173169	44.179649
3504.654472	453881.629584	44.184653
3504.441160	453871.578207	44.189658
3504.486463	453868.478269	44.194663
3504.341275	453834.640321	44.199668
3504.026501	453822.071602	44.204673
3504.429833	453826.311682	44.209677
3504.105683	453810.297441	44.214682
3504.571325	453791.715069	44.219687
3504.615883	453778.628730	44.224692
3504.186243	453771.757206	44.229697
3504.267959	453753.037582	44.234701
3504.345611	453749.627944	44.239706
3504.620136	453743.751422	44.244711
3504.652908	453718.450024	44.249716
3504.417013	453710.582228	44.254721
3504.141622	453704.698206	44.259725
3504.411809	453677.936811	44.264730
3503.885007	453677.722658	44.269735
3504.035831	453659.548774	44.274740
3504.258288	453660.321937	44.279745
3504.164510	453659.729686	44.284749
3503.746121	453634.505220	44.289754
3503.299901	453634.125227	44.294759
3503.476563	453622.891886	44.299764
3504.056719	453627.253895	44.304769
3503.827465	453622.071679	44.309773
3503.790336	453620.962820	44.314778
3503.968247	453627.776102	44.319783
3504.128444	453626.126616	44.324788
3503.833573	453632.108143	44.329793
3503.751120	453627.103635	44.334797
3503.863769	453628.199710	44.339802
3503.700562	453634.412221	44.344807
3504.332180	453624.216450	44.349812
3504.176839	453605.435783	44.354817
3503.635337	453595.136147	44.359821
3503.955741	453591.330179	44.364826
3503.967646	453592.088603	44.369831
3504.324618	453587.465295	44.374836
3504.118644	453580.352742	44.379841
3504.018100	453562.880709	44.384845
3504.065914	453561.858729	44.389850
3503.698183	453561.211865	44.394855
3504.313206	453550.664037	44.399860
3503.951992	453560.408235	44.404865
3504.092366	453550.549776	44.409869
3504.185188	453515.656791	44.414874
3503.946165	453518.739277	44.419879
3504.106359	453511.209321	44.424884
3504.177627	453516.165184	44.429889
3503.973244	453506.314877	44.434893
3503.916264	453483.309728	44.439898
3504.233193	453477.577971	44.444903
3504.253416	453468.348313	44.449908
3504.167573	453470.441469	44.454913
3504.268657	453464.543789	44.459917
3504.210358	453446.151956	44.464922
3504.012382	453439.342150	44.469927
3503.867560	453427.504576	44.474932
3504.312393	453433.258468	44.479937
3504.330043	453417.793883	44.484941
3504.109442	453402.116499	44.489946
3503.780773	453406.025411	44.494951
3503.952568	453389.419219	44.499956
3504.116420	453402.825188	44.504961
3504.083333	453399.839952	44.509965
3504.328443	453385.248994	44.514970
3503.754972	453369.124897	44.519975
3504.315299	453357.116184	44.524980
3504.236751	453360.576845	44.529985
3504.070397	453356.194926	44.534989
3504.347035	453333.386113	44.539994
3503.833943	453333.321697	44.544999
3504.026065	453320.564728	44.550004
3504.195971	453315.973301	44.555009
3504.443694	453315.728281	44.560013
3503.883352	453293.113033	44.565018
3503.894232	453286.926539	44.570023
3504.151943	453274.817368	44.575028
3503.874468	453283.533513	44.580033
3503.687110	453277.634337	44.585037
3504.032969	453281.022544	44.590042
3503.816653	453283.695634	44.595047
3504.292787	453273.729016	44.600052
3504.003154	453259.026500	44.605057
3504.288766	453259.231258	44.610061
3504.552834	453256.448734	44.615066
3503.984553	453250.766675	44.620071
3504.150809	453226.861318	44.625076
3504.015447	453224.552546	44.630081
3504.016903	453214.666952	44.635085
3503.947654	453214.171888	44.640090
3503.913197	453225.685448	44.645095
3504.072694	453202.541632	44.650100
3503.907961	453186.550376	44.655105
3503.720715	453181.462264	44.660109
3504.028115	453182.322331	44.665114
3504.156156	453181.996357	44.670119
3504.208798	453178.236033	44.675124
3504.108630	453180.787916	44.680129
3504.265433	453155.515340	44.685133
3504.460068	453138.296710	44.690138
3504.245612	453140.766723	44.695143
3504.275285	453121.142908	44.700148
3504.301557	453113.534285	44.705153
3503.989152	453105.223068	44.710157
3504.589096	453099.544271	44.715162
3504.187228	453085.570519	44.720167
3504.044467	453070.285148	44.725172
3503.692459	453065.427918	44.730177
3503.640427	453064.017405	44.735181
3503.654543	453067.310209	44.740186
3503.966856	453064.975673	44.745191
3504.111610	453061.554464	44.750196
3504.568102	453059.448783	44.755201
3504.034077	453047.626751	44.760205
3504.139666	453030.980879	44.765210
3504.064163	453026.887545	44.770215
3504.338928	453019.337847	44.775220
3504.441403	453004.466805	44.780225
3504.307958	452981.930405	44.785229
3504.598306	452984.111462	44.790234
3504.145193	452975.215879	44.795239
3504.008227	452949.841126	44.800244
3504.077694	452943.796611	44.805249
3503.976596	452946.450071	44.810253
3504.419169	452939.936286	44.815258
3504.089545	452923.719506	44.820263
3504.095866	452900.905677	44.825268
3504.088339	452907.243910	44.830273
3504.041599	452900.103931	44.835277
3504.442163	452887.615274	44.840282
3503.951323	452882.274755	44.845287
3503.855408	452865.308290	44.850292
3503.924752	452860.429761	44.855297
3503.800270	452862.884444	44.860301
3503.934059	452855.155976	44.865306
3503.807838	452863.187434	44.870311
3504.213093	452861.242568	44.875316
3504.145799	452855.170683	44.880321
3503.985168	452832.638761	44.885325
3504.177196	452818.715506	44.890330
3503.638420	452823.572920	44.895335
3503.861600	452809.847121	44.900340
3504.013165	452814.738747	44.905345
3503.904963	452820.637939	44.910349
3504.039704	452811.793995	44.915354
3503.896395	452802.896133	44.920359
3504.277297	452786.203054	44.925364
3504.068819	452788.114438	44.930369
3504.053000	452783.808083	44.935373
3504.507087	452787.634151	44.940378
3504.019043	452765.310148	44.945383
3504.311050	452748.632218	44.950388
3504.045367	452743.405303	44.955393
3503.828154	452752.669034	44.960397
3504.378433	452744.768018	44.965402
3504.204237	452719.906295	44.970407
3504.292332	452718.978787	44.975412
3504.026788	452709.290627	44.980417
3503.937107	452712.297037	44.985421
3504.227287	452702.311201	44.990426
3503.994708	452685.824184	44.995431
3504.098938	452665.680247	45.000436
3504.102853	452667.758159	45.005441
3504.065355	452667.206964	45.010445
3504.104594	452665.121795	45.015450
3503.725503	452653.577254	45.020455
3503.956719	452639.444404	45.025460
3504.285577	452643.748144	45.030465
3504.076755	452638.663581	45.035469
3504.477566	452642.143904	45.040474
3504.334047	452631.927913	45.045479
3503.972336	452610.393303	45.050484
3503.920749	452603.406137	45.055489
3503.763764	452603.787868	45.060493
3503.894595	452603.157234	45.065498
3503.847803	452608.843217	45.070503
3503.546203	452603.774487	45.075508
3503.726385	452604.859086	45.080513
3503.670387	452612.726563	45.085517
3504.030856	452602.475198	45.090522
3503.644583	452583.834419	45.095527
3503.757628	452569.620306	45.100532
3503.675403	452565.578724	45.105537
3503.796881	452563.428806	45.110541
3504.008596	452561.516960	45.115546
3503.835779	452564.638978	45.120551
3504.111899	452561.245951	45.125556
3504.109236	452570.675913	45.130561
3504.231405	452554.077521	45.135565
3504.141669	452539.188268	45.140570
3504.185580	452535.581407	45.145575
3504.453661	452530.313994	45.150580
3504.491053	452522.855342	45.155585
3504.267998	452497.494732	45.160589
3504.435017	452483.220648	45.165594
3504.233266	452487.361542	45.170599
3504.239188	452461.556221	45.175604
3504.171831	452454.926570	45.180609
3504.265850	452447.965184	45.185613
3504.008425	452441.013110	45.190618
3503.641689	452440.822304	45.195623
3504.045829	452423.567305	45.200628
3503.932595	452411.267485	45.205633
3504.030685	452409.577811	45.210637
3504.439134	452403.120382	45.215642
3504.181678	452414.520383	45.220647
3504.403770	452383.811203	45.225652
3504.306540	452373.739270	45.230657
3503.933031	452367.466045	45.235661
3504.265364	452361.275082	45.240666
3504.252654	452352.912387	45.245671
3504.294857	452336.530261	45.250676
3504.064725	452328.103288	45.255681
3504.009274	452323.702211	45.260685
3504.237014	452320.063922	45.265690
3503.999389	452306.974134	45.270695
3503.983821	452283.656394	45.275700
3503.782322	452284.147125	45.280705
3504.121282	452283.278156	45.285709
3504.441700	452279.776126	45.290714
3503.930210	452269.115820	45.295719
3503.950850	452247.160667	45.300724
3504.032070	452246.842674	45.305729
3504.031064	452241.012773	45.310733
3504.236190	452236.009518	45.315738
3504.132169	452242.110949	45.320743
3504.266936	452228.653344	45.325748
3504.350210	452207.245119	45.330753
3504.138721	452213.719786	45.335757
3504.202783	452197.232423	45.340762
3503.772515	452193.605074	45.345767
3504.519538	452172.641143	45.350772
3504.356063	452166.838963	45.355777
3503.909983	452159.057157	45.360781
3503.946653	452159.557921	45.365786
3504.187687	452162.254456	45.370791
3503.848766	452128.091902	45.375796
3504.245184	452124.171293	45.380801
3503.946938	452125.134820	45.385805
3504.071707	452118.979227	45.390810
3504.045268	452114.421060	45.395815
3504.466534	452103.905582	45.400820
3504.434985	452089.766526	45.405825
3504.088160	452084.249115	45.410829
3504.354357	452077.258206	45.415834
3503.900742	452060.301459	45.420839
3504.423043	452045.104555	45.425844
3504.424720	452040.440176	45.430849
3504.045858	452045.219767	45.435853
3504.544136	452021.966084	45.440858
3504.282982	452020.337720	45.445863
3504.476131	452007.985345	45.450868
3504.128399	451992.075106	45.455873
3504.031474	451980.887586	45.460877
3504.240441	451971.371543	45.465882
3504.049621	451976.930200	45.470887
3504.241017	451963.310662	45.475892
3504.262533	451948.199196	45.480897
3504.002749	451938.611084	45.485901
3503.976978	451927.157899	45.490906
3503.712720	451931.867250	45.495911
3503.864070	451920.738700	45.500916
3503.907337	451928.893673	45.505921
3503.918536	451931.375995	45.510925
3504.220669	451911.451019	45.515930
3503.740409	451901.849839	45.520935
3503.938802	451886.454639	45.525940
3504.045918	451888.413612	45.530945
3503.753610	451890.187299	45.535949
3503.844071	451890.577489	45.540954
3503.752465	451899.769455	45.545959
3503.950649	451892.536609	45.550964
3504.054369	451883.951053	45.555969
3504.022530	451861.750963	45.560973
3504.082533	451856.316118	45.565978
3503.853284	451859.954856	45.570983
3503.705739	451864.340107	45.575988
3503.832942	451862.341232	45.580993
3503.724930	451857.492751	45.585997
3504.002603	451852.071435	45.591002
3503.960907	451854.613496	45.596007
3503.672887	451839.757596	45.601012
3503.943686	451822.524866	45.606017
3503.599736	451822.786442	45.611021
3504.069897	451812.059677	45.616026
3503.799845	451810.838398	45.621031
3503.766514	451822.606037	45.626036
3503.889564	451815.132504	45.631041
3503.853941	451824.162852	45.636045
3503.886662	451821.166150	45.641050
3504.047099	451814.902980	45.646055
3503.852848	451807.027343	45.651060
3503.906034	451794.597343	45.656065
3503.643579	451784.806824	45.661069
3504.278698	451774.203967	45.666074
3503.990529	451784.088620	45.671079
3503.842893	451783.708301	45.676084
3504.186021	451779.137655	45.681089
3504.077694	451767.901269	45.686093
3504.176621	451740.101947	45.691098
3503.996442	451741.957896	45.696103
3504.151991	451737.216477	45.701108
3504.047718	451734.547343	45.706113
3503.978311	451735.928096	45.711117
3504.247274	451723.765398	45.716122
3503.847373	451705.835924	45.721127
3503.934848	451699.635876	45.726132
3504.090588	451699.507942	45.731137
3504.144248	451704.010966	45.736141
3503.969601	451692.583071	45.741146
3504.279746	451673.264876	45.746151
3504.156929	451659.141110	45.751156
3504.316763	451653.790562	45.756161
3504.265089	451666.220499	45.761165
3504.482149	451636.271543	45.766170
3504.130133	451623.910629	45.771175
3504.403708	451621.430453	45.776180
3504.416213	451612.454774	45.781185
3504.395382	451589.593435	45.786189
3504.556757	451572.429880	45.791194
3504.441689	451571.080726	45.796199
3504.613405	451541.190074	45.801204
3504.528518	451541.508815	45.806209
3504.159924	451522.559867	45.811213
3504.444835	451498.328060	45.816218
3504.454214	451499.644677	45.821223
3504.684948	451491.797750	45.826228
3504.436691	451465.071314	45.831233
3504.190014	451456.545412	45.836237
3504.351644	451447.493499	45.841242
3503.934699	451435.447752	45.846247
3503.809825	451421.172078	45.851252
3503.861315	451409.350522	45.856257
3503.709198	451415.105517	45.861261
3504.038649	451404.453267	45.866266
3504.183333	451417.154018	45.871271
3504.096389	451404.899808	45.876276
3504.128382	451379.798470	45.881281
3504.141314	451380.962391	45.886285
3504.552140	451379.726224	45.891290
3504.464451	451388.867049	45.896295
3504.140849	451361.240764	45.901300
3504.241966	451342.870534	45.906305
3504.146272	451340.605475	45.911309
3504.275946	451329.632407	45.916314
3504.363124	451310.808238	45.921319
3504.284681	451301.036769	45.926324
3504.484981	451292.231681	45.931329
3504.011208	451277.052200	45.936333
3504.301528	451253.123378	45.941338
3503.609484	451263.685631	45.946343
3503.520599	451254.372215	45.951348
3503.424457	451255.402671	45.956353
3503.266647	451258.015330	45.961357
3503.779623	451254.328153	45.966362
3503.572444	451265.061110	45.971367
3503.667178	451263.878909	45.976372
3503.740282	451254.284337	45.981377
3503.852862	451252.541397	45.986381
3504.307512	451259.105414	45.991386
3503.682697	451261.290823	45.996391
3503.798851	451258.381192	46.001396
3504.053624	451255.295794	46.006401
3503.699357	451248.309153	46.011405
3503.912722	451229.514063	46.016410
3503.763244	451216.560630	46.021415
3503.698685	451217.788491	46.026420
3503.886859	451216.894528	46.031425
3503.671620	451220.226789	46.036429
3503.897034	451213.901644	46.041434
3503.871117	451226.530243	46.046439
3504.091872	451216.149954	46.051444
3504.067707	451214.683856	46.056449
3503.827517	451203.520379	46.061453
3504.024504	451187.313712	46.066458
3503.895925	451186.169637	46.071463
3504.001687	451177.431343	46.076468
3504.258507	451173.534394	46.081473
3503.876228	451181.204630	46.086477
3504.087641	451176.808440	46.091482
3503.938824	451158.277926	46.096487
3504.008074	451149.292357	46.101492
3504.209801	451137.343595	46.106497
3504.212866	451133.844863	46.111501
3504.261936	451140.072575	46.116506
3504.274686	451119.283662	46.121511
3503.820692	451111.401411	46.126516
3504.191729	451098.866022	46.131521
3504.216607	451103.830387	46.136525
3503.963779	451087.953946	46.141530
3503.626339	451072.142641	46.146535
3503.685233	451066.099383	46.151540
3503.969715	451053.629445	46.156545
3503.858155	451060.695804	46.161549
3503.914347	451050.901228	46.166554
3503.640520	451048.210256	46.171559
3503.572430	451048.576836	46.176564
3503.756737	451053.868887	46.181569
3503.692554	451059.101968	46.186573
3503.798498	451050.414289	46.191578
3503.698392	451060.064375	46.196583
3503.577676	451065.966203	46.201588
3503.881585	451055.115338	46.206593
3503.614810	451062.005400	46.211597
3503.771984	451057.415649	46.216602
3503.767892	451054.627921	46.221607
3503.903301	451054.249957	46.226612
3503.724985	451024.519729	46.231617
3503.620769	451023.726383	46.236621
3503.816084	451015.936026	46.241626
3503.482270	451020.454659	46.246631
3503.447193	451029.637358	46.251636
3503.694956	451021.483148	46.256641
3503.624796	451017.794101	46.261645
3503.995472	451019.860254	46.266650
3504.118809	451029.928499	46.271655
3503.784965	451033.838738	46.276660
3503.933443	451022.811597	46.281665
3504.174746	451030.983808	46.286669
3504.059140	451018.683565	46.291674
3503.865887	451001.123793	46.296679
3503.803511	450988.256745	46.301684
3504.061191	450978.478430	46.306689
3504.017916	450987.662547	46.311693
3504.171465	450975.164220	46.316698
3503.981513	450985.945079	46.321703
3503.825009	450989.520847	46.326708
3504.400464	450959.813919	46.331713
3503.793098	450954.847691	46.336717
3504.153562	450942.314014	46.341722
3503.990822	450938.995660	46.346727
3503.946675	450946.557546	46.351732
3503.969307	450940.216243	46.356737
3504.021915	450924.084724	46.361741
3504.214655	450913.658368	46.366746
3503.894769	450908.186741	46.371751
3503.609421	450905.954018	46.376756
3504.211271	450896.725299	46.381761
3504.075790	450901.463593	46.386765
3504.459791	450891.511568	46.391770
3504.453166	450875.238025	46.396775
3504.256878	450860.315058	46.401780
3504.381487	450853.094415	46.406785
3504.319297	450842.559452	46.411789
3504.511120	450826.657587	46.416794
3504.547453	450821.784216	46.421799
3504.232578	450804.143645	46.426804
3504.209178	450783.867572	46.431809
3504.172176	450786.814564	46.436813
3504.529732	450775.092488	46.441818
3504.655714	450759.252515	46.446823
3503.980064	450755.109104	46.451828
3504.135788	450751.736343	46.456833
3503.988259	450737.464068	46.461837
3504.075216	450713.417249	46.466842
3503.633146	450704.468096	46.471847
3503.269954	450703.161252	46.476852
3503.924661	450709.944787	46.481857
3503.774512	450716.967150	46.486861
3503.797332	450703.476973	46.491866
3504.205201	450708.680239	46.496871
3503.771000	450705.458900	46.501876
3503.879581	450706.505126	46.506881
3503.968859	450710.647380	46.511885
3504.098506	450695.465839	46.516890
3503.825816	450675.688532	46.521895
3503.944037	450668.012609	46.526900
3504.188840	450664.016216	46.531905
3503.946382	450667.403912	46.536909
3504.031743	450668.656908	46.541914
3504.269273	450662.278827	46.546919
3504.056814	450642.440503	46.551924
3504.186579	450626.751885	46.556929
3504.073398	450626.467062	46.561933
3504.312464	450618.415582	46.566938
3504.190657	450605.051437	46.571943
3504.106938	450591.832883	46.576948
3504.164045	450591.113376	46.581953
3504.048917	450585.606701	46.586957
3504.041457	450579.422529	46.591962
3504.426430	450558.518798	46.596967
3504.200828	450550.749438	46.601972
3504.033545	450546.468480	46.606977
3504.087740	450547.219795	46.611981
3503.837074	450533.624102	46.616986
3503.763406	450512.697236	46.621991
3503.342874	450510.994563	46.626996
3503.881053	450499.190790	46.632001
3503.672674	450504.550033	46.637005
3503.860512	450498.281789	46.642010
3503.708391	450501.755489	46.647015
3503.746041	450511.230205	46.652020
3504.170299	450499.445884	46.657025
3503.614647	450507.652980	46.662029
3504.268140	450496.336525	46.667034
3504.183447	450497.669269	46.672039
3503.819420	450491.089646	46.677044
3504.197473	450469.882801	46.682049
3503.882070	450461.216121	46.687053
3504.052212	450458.550666	46.692058
3503.943958	450461.915480	46.697063
3503.889476	450465.524617	46.702068
3503.782536	450459.053190	46.707073
3504.061675	450458.599973	46.712077
3504.224060	450435.655380	46.717082
3504.071936	450427.366415	46.722087
3504.118220	450423.758782	46.727092
3504.409053	450412.453505	46.732097
3504.114291	450401.603123	46.737101
3503.977993	450385.351339	46.742106
3504.157662	450379.692870	46.747111
3503.978246	450378.760236	46.752116
3504.019205	450380.933454	46.757121
3503.959571	450373.389194	46.762125
3503.958521	450351.283636	46.767130
3503.746268	450348.784864	46.772135
3503.849369	450347.347676	46.777140
3504.287228	450340.124069	46.782145
3503.976724	450343.320630	46.787149
3504.177957	450336.695141	46.792154
3503.982427	450326.182685	46.797159
3503.867614	450302.220546	46.802164
3503.950456	450299.772784	46.807169
3503.720789	450294.894008	46.812173
3504.012316	450296.263927	46.817178
3504.376581	450295.948277	46.822183
3504.357583	450305.939773	46.827188
3504.405340	450272.316555	46.832193
3504.289131	450273.350484	46.837197
3504.145904	450261.713630	46.842202
3504.100840	450260.859453	46.847207
3504.261468	450231.425129	46.852212
3504.078423	450226.183464	46.857217
3504.264379	450221.132299	46.862221
3504.243034	450204.607237	46.867226
3504.308924	450193.847270	46.872231
3503.899538	450184.081082	46.877236
3504.231215	450166.785887	46.882241
3503.953223	450182.500271	46.887245
3503.831481	450175.574966	46.892250
3503.968816	450171.951743	46.897255
3503.717469	450152.525207	46.902260
3503.640000	450134.742126	46.907265
3503.709974	450136.099185	46.912269
3503.846698	450128.825520	46.917274
3503.819416	450126.852859	46.922279
3503.639512	450136.466296	46.927284
3503.849628	450129.129398	46.932289
3503.753821	450132.593543	46.937293
3504.156733	450133.538840	46.942298
3504.250356	450135.348178	46.947303
3503.679910	450129.361407	46.952308
3503.669352	450109.893716	46.957313
3503.691307	450105.884567	46.962317
3503.721799	450100.707812	46.967322
3503.514387	450099.374330	46.972327
3503.283905	450104.230429	46.977332
3503.608126	450102.806170	46.982337
3503.799258	450122.598058	46.987341
3503.472095	450106.581455	46.992346
3503.927617	450101.687041	46.997351
3503.484895	450096.996704	47.002356
3503.834495	450098.306019	47.007361
3503.520497	450112.353437	47.012365
3503.672402	450105.939106	47.017370
3504.216811	450102.347766	47.022375
3504.035141	450100.908484	47.027380
3504.240459	450093.978009	47.032385
3503.824709	450101.045930	47.037389
3504.113633	450092.630821	47.042394
3504.417513	450068.749028	47.047399
3503.635371	450059.908366	47.052404
3503.676290	450053.969288	47.057409
3503.785879	450055.775907	47.062413
3504.085820	450054.203684	47.067418
3504.301279	450062.634200	47.072423
3504.043935	450056.543244	47.077428
3504.008754	450035.812136	47.082433
3503.403589	450026.535623	47.087437
3503.787024	450022.667543	47.092442
3503.673263	450019.340679	47.097447
3503.951470	450025.529599	47.102452
3503.971781	450021.723523	47.107457
3503.809815	450034.883096	47.112461
3503.661627	450026.187682	47.117466
3503.637184	450024.163824	47.122471
3503.556960	450027.878837	47.127476
3503.695014	450014.013622	47.132481
3503.564840	450028.688837	47.137485
3503.412626	450030.996480	47.142490
3503.748944	450026.933638	47.147495
3503.790579	450026.774478	47.152500
3503.952793	450020.104849	47.157505
3503.633442	450004.999473	47.162509
3503.940440	449987.505535	47.167514
3504.173809	449989.392429	47.172519
3503.589370	449992.838626	47.177524
3503.877896	449981.432107	47.182529
3503.725204	449992.308521	47.187533
3503.852174	449984.123831	47.192538
3503.640332	449985.579722	47.197543
3503.718212	449989.014234	47.202548
3504.082260	449973.335824	47.207553
3504.037525	449991.596340	47.212557
3503.995301	449968.787575	47.217562
3503.745316	449946.318476	47.222567
3503.651549	449959.111535	47.227572
3503.893044	449952.935371	47.232577
3504.140300	449943.259758	47.237581
3503.893574	449938.079597	47.242586
3504.019674	449949.516857	47.247591
3504.046493	449951.540428	47.252596
3504.020159	449918.385612	47.257601
3503.693039	449912.762849	47.262605
3503.847622	449899.351058	47.267610
3503.975890	449890.506978	47.272615
3503.477958	449896.574950	47.277620
3503.763166	449903.269736	47.282625
3503.841054	449911.267481	47.287629
3503.722175	449912.099075	47.292634
3503.772193	449902.507824	47.297639
3503.705780	449915.042727	47.302644
3503.724423	449906.572289	47.307649
3503.780348	449912.545685	47.312653
3503.926553	449913.788337	47.317658
3504.275611	449904.805158	47.322663
3504.284525	449887.869060	47.327668
3504.325685	449877.315962	47.332673
3504.377772	449871.780546	47.337677
3504.395502	449857.175234	47.342682
3504.388002	449836.996932	47.347687
3504.090469	449838.518167	47.352692
3503.861843	449828.467435	47.357697
3504.011345	449821.444995	47.362701
3503.833169	449809.154721	47.367706
3504.128391	449796.428688	47.372711
3503.862022	449789.629355	47.377716
3503.709547	449788.083661	47.382721
3503.718736	449803.090157	47.387725
3503.626761	449794.537156	47.392730
3504.210669	449794.183995	47.397735
3503.574620	449796.726387	47.402740
3503.868870	449785.470893	47.407745
3503.625819	449794.334727	47.412749
3503.780152	449778.032845	47.417754
3503.959031	449755.591717	47.422759
3503.881925	449747.391078	47.427764
3503.706253	449750.919626	47.432769
3503.555286	449755.914337	47.437773
3503.859466	449749.879519	47.442778
3503.934303	449751.387881	47.447783
3503.674585	449757.719435	47.452788
3503.982934	449745.041832	47.457793
3504.276205	449740.175039	47.462797
3504.523486	449738.307568	47.467802
3504.709170	449718.958114	47.472807
3504.208196	449719.500037	47.477812
3504.657551	449698.128128	47.482817
3504.022750	449684.394660	47.487821
3504.411969	449670.131410	47.492826
3504.587323	449667.414262	47.497831
3504.248337	449649.371205	47.502836
3504.326655	449633.183596	47.507841
3504.201191	449636.145855	47.512845
3504.032923	449614.727211	47.517850
3503.893666	449587.269907	47.522855
3503.951251	449593.344518	47.527860
3503.925135	449587.315348	47.532865
3503.849870	449591.688733	47.537869
3503.721090	449582.026459	47.542874
3503.692411	449589.687601	47.547879
3503.553157	449589.356511	47.552884
3504.066849	449584.908375	47.557889
3503.838706	449589.814897	47.562893
3503.618294	449577.126072	47.567898
3503.928281	449556.082035	47.572903
3503.918359	449548.072659	47.577908
3504.045946	449539.279251	47.582913
3503.498556	449557.524566	47.587917
3503.713126	449555.206335	47.592922
3503.729642	449547.344554	47.597927
3503.340424	449552.785622	47.602932
3504.143234	449548.288111	47.607937
3503.824654	449553.260787	47.612941
3503.775733	449553.674822	47.617946
3503.883015	449552.439679	47.622951
3503.374471	449556.937757	47.627956
3503.761439	449550.331009	47.632961
3503.630749	449550.099864	47.637965
3503.790673	449552.455668	47.642970
3504.210141	449536.159029	47.647975
3503.582703	449517.810188	47.652980
3504.041306	449504.650453	47.657985
3503.762401	449511.289578	47.662989
3503.940061	449508.673423	47.667994
3503.860130	449507.368837	47.672999
3503.601890	449516.691713	47.678004
3503.644168	449511.309988	47.683009
3503.923984	449514.405876	47.688013
3503.871766	449507.721996	47.693018
3504.106402	449508.341132	47.698023
3503.577115	449499.811978	47.703028
3503.896579	449487.943578	47.708033
3503.791680	449487.860138	47.713037
3503.597622	449484.597602	47.718042
3503.912718	449485.557924	47.723047
3503.689612	449486.103110	47.728052
3503.842046	449480.195532	47.733057
3503.543845	449485.671779	47.738061
3503.782762	449480.459283	47.743066
3504.387261	449484.209586	47.748071
3504.231104	449488.241880	47.753076
3504.048669	449462.465000	47.758081
3503.553952	449451.242636	47.763085
3503.638816	449446.056436	47.768090
3503.756491	449431.687280	47.773095
3503.671425	449453.200182	47.778100
3503.763809	449444.463448	47.783105
3503.698306	449451.370375	47.788109
3503.691135	449437.884501	47.793114
3504.130904	449436.592579	47.798119
3503.703294	449439.403644	47.803124
3503.813484	449434.415931	47.808129
3503.746780	449442.489248	47.813133
3503.969991	449441.132897	47.818138
3503.912847	449415.435972	47.823143
3503.536725	449414.435474	47.828148
3503.862123	449404.036419	47.833153
3503.803115	449409.928176	47.838157
3503.659311	449407.011973	47.843162
3503.823012	449398.415154	47.848167
3503.826997	449396.792010	47.853172
3504.009939	449408.726898	47.858177
3503.991953	449406.397655	47.863181
3503.750815	449405.171293	47.868186
3504.077658	449400.755023	47.873191
3503.643915	449389.978548	47.878196
3503.777165	449368.356056	47.883201
3503.548516	449368.800784	47.888205
3503.639923	449359.912070	47.893210
3503.642479	449361.432802	47.898215
3503.418041	449359.747252	47.903220
3503.704482	449359.343471	47.908225
3503.915987	449359.053893	47.913229
3503.531114	449365.102712	47.918234
3503.552950	449361.600478	47.923239
3503.566898	449365.147416	47.928244
3503.634638	449356.161335	47.933249
3503.340388	449358.594712	47.938253
3503.316927	449361.945223	47.943258
3504.071771	449360.498090	47.948263
3503.673157	449369.388666	47.953268
3503.927540	449358.393269	47.958273
3504.020859	449367.199849	47.963277
3503.434405	449363.243739	47.968282
3503.858385	449362.664362	47.973287
3503.774883	449364.808234	47.978292
3503.938087	449362.194529	47.983297
3503.798034	449365.362133	47.988301
3503.800287	449373.880037	47.993306
3503.999395	449364.263082	47.998311
3503.702719	449348.798433	48.003316
3503.730210	449333.785459	48.008321
3503.708494	449333.839927	48.013325
3504.034416	449337.029377	48.018330
3504.088080	449331.392142	48.023335
3503.755249	449332.463105	48.028340
3504.158029	449332.952128	48.033345
3504.376539	449332.509242	48.038349
3504.413198	449319.624255	48.043354
3504.516362	449303.381445	48.048359
3504.281747	449295.866675	48.053364
3504.270661	449272.950428	48.058369
3504.210815	449261.805819	48.063373
3504.388483	449257.871327	48.068378
3504.461944	449246.754652	48.073383
3504.280478	449226.047721	48.078388
3504.366425	449207.779613	48.083393
3504.206034	449209.074659	48.088397
3503.730392	449212.096771	48.093402
3504.018025	449184.718160	48.098407
3503.801347	449168.986197	48.103412
3503.919203	449179.512610	48.108417
3503.936384	449168.354799	48.113421
3503.647844	449173.575956	48.118426
3504.145375	449168.116408	48.123431
3503.641381	449175.199706	48.128436
3503.783212	449168.685401	48.133441
3503.787302	449169.191800	48.138445
3503.323374	449166.887972	48.143450
3503.978729	449163.531052	48.148455
3503.590375	449168.972071	48.153460
3503.598109	449167.551086	48.158465
3503.845203	449169.232895	48.163469
3503.635800	449143.460227	48.168474
3504.013394	449123.925343	48.173479
3503.404563	449130.012470	48.178484
3503.767939	449121.888486	48.183489
3503.683463	449126.162132	48.188493
3503.520927	449128.420932	48.193498
3503.663595	449123.579713	48.198503
3503.393151	449134.071043	48.203508
3503.442902	449127.825969	48.208513
3503.598210	449133.579800	48.213517
3503.373192	449134.733773	48.218522
3504.147381	449137.643895	48.223527
3503.799294	449139.275221	48.228532
3503.743008	449126.659507	48.233537
3503.876296	449125.572012	48.238541
3503.979908	449133.819184	48.243546
3504.398635	449128.778716	48.248551
3504.056942	449141.969537	48.253556
3504.048464	449124.579453	48.258561
3503.990489	449108.313302	48.263565
3503.925279	449094.837118	48.268570
3504.055663	449084.420500	48.273575
3503.898413	449088.148831	48.278580
3504.078844	449082.641997	48.283585
3504.147638	449081.210580	48.288589
3503.911973	449065.481782	48.293594
3504.156595	449054.893529	48.298599
3503.859770	449054.690745	48.303604
3504.051634	449043.300223	48.308609
3503.991248	449043.107771	48.313613
3503.985741	449050.308812	48.318618
3504.312083	449018.867012	48.323623
3503.701208	449016.284030	48.328628
3504.173802	449006.113168	48.333633
3504.058973	449003.749712	48.338637
3503.916929	449016.145953	48.343642
3504.746825	448999.373181	48.348647
3504.349100	448978.804342	48.353652
3504.655738	448978.853448	48.358657
3504.318735	448959.440429	48.363661
3504.504473	448945.566367	48.368666
3504.509556	448934.106269	48.373671
3504.303754	448914.315872	48.378676
3504.163972	448895.173348	48.383681
3504.156268	448891.321145	48.388685
3504.103388	448887.273836	48.393690
3504.320914	448881.456385	48.398695
3503.862962	448869.771086	48.403700
3503.629210	448853.433342	48.408705
3503.653587	448852.617955	48.413709
3503.376458	448859.510506	48.418714
3503.584649	448845.936774	48.423719
3503.815016	448856.292023	48.428724
3503.754118	448846.414998	48.433729
3503.736296	448844.491306	48.438733
3503.515197	448854.416593	48.443738
3503.613540	448854.957611	48.448743
3503.573649	448861.302603	48.453748
3503.914215	448844.917493	48.458753
3503.512458	448849.093256	48.463757
3503.475033	448856.604043	48.468762
3503.892434	448848.014385	48.473767
3503.700156	448850.227588	48.478772
3503.632315	448850.543457	48.483777
3503.721731	448856.764961	48.488781
3503.531466	448858.217244	48.493786
3503.726352	448852.707882	48.498791
3503.689297	448865.542629	48.503796
3503.922858	448850.139188	48.508801
3503.696019	448859.609108	48.513805
3503.468631	448857.163445	48.518810
3504.313010	448853.419267	48.523815
3503.532195	448833.422748	48.528820
3503.831346	448815.067188	48.533825
3503.855430	448816.330759	48.538829
3503.785514	448816.849803	48.543834
3503.945020	448813.628201	48.548839
3503.944720	448818.495998	48.553844
3504.342771	448812.749114	48.558849
3503.836744	448815.066599	48.563853
3503.851446	448795.897605	48.568858
3504.190691	448775.304138	48.573863
3503.722201	448781.874453	48.578868
3503.829615	448777.495521	48.583873
3503.945457	448777.019450	48.588877
3504.175953	448781.949257	48.593882
3504.125900	448773.946438	48.598887
3503.904132	448754.158617	48.603892
3504.056576	448740.391515	48.608897
3504.063175	448737.094599	48.613901
3503.656864	448739.344360	48.618906
3503.777565	448733.137760	48.623911
3503.885994	448737.682778	48.628916
3504.671857	448727.154059	48.633921
3503.948099	448713.536551	48.638925
3504.098724	448704.485333	48.643930
3504.372007	448700.483706	48.648935
3503.956312	448700.605447	48.653940
3504.178052	448689.057516	48.658945
3503.972909	448667.289263	48.663949
3504.017584	448651.410875	48.668954
3503.659921	448646.959212	48.673959
3504.063082	448656.676588	48.678964
3503.696034	448650.756069	48.683969
3503.965998	448652.434015	48.688973
3503.940427	448665.520451	48.693978
3503.907050	448639.767813	48.698983
3503.734073	448630.061941	48.703988
3504.088218	448619.251947	48.708993
3504.033701	448611.148417	48.713997
3503.961035	448607.662194	48.719002
3504.130723	448606.010696	48.724007
3504.166359	448613.306272	48.729012
3503.922914	448587.792263	48.734017
3503.953128	448569.634528	48.739021
3503.701344	448561.006900	48.744026
3504.376512	448561.297316	48.749031
3504.144423	448565.646986	48.754036
3504.089338	448564.287393	48.759041
3504.079109	448548.570420	48.764045
3503.752191	448536.761149	48.769050
3503.803305	448523.873205	48.774055
3503.730979	448528.043486	48.779060
3503.983590	448531.499108	48.784065
3504.191997	448517.925128	48.789069
3503.773624	448528.644840	48.794074
3504.022479	448517.852772	48.799079
3504.136688	448506.120279	48.804084
3503.907638	448488.868743	48.809089
3503.715937	448488.901532	48.814093
3503.557157	448487.103287	48.819098
3503.797747	448482.295907	48.824103
3503.756571	448480.781816	48.829108
3503.690270	448481.705898	48.834113
3503.545939	448481.223539	48.839117
3503.381385	448491.443577	48.844122
3503.928611	448475.732776	48.849127
3503.724093	448488.647053	48.854132
3503.779907	448484.327577	48.859137
3504.262979	448482.470441	48.864141
3503.793634	448475.299691	48.869146
3503.939620	448449.414783	48.874151
3504.046953	448444.832972	48.879156
3503.771863	448439.809399	48.884161
3503.718330	448440.021419	48.889165
3503.557676	448444.003975	48.894170
3504.162753	448432.491860	48.899175
3503.956302	448449.970033	48.904180
3503.900290	448448.052825	48.909185
3503.805709	448442.795606	48.914189
3503.728300	448423.287060	48.919194
3503.907809	448404.140275	48.924199
3503.671523	448402.101727	48.929204
3503.576914	448402.117937	48.934209
3503.813185	448397.970454	48.939213
3503.400439	448402.452417	48.944218
3503.693493	448403.467262	48.949223
3503.706722	448404.834123	48.954228
3503.689898	448405.648348	48.959233
3503.875280	448405.058983	48.964237
3503.810785	448409.785717	48.969242
3503.896635	448406.373805	48.974247
3504.030237	448414.616139	48.979252
3503.994863	448411.174221	48.984257
3503.869225	448409.826666	48.989261
3503.801972	448390.620591	48.994266
3504.051888	448364.819245	48.999271
3503.922200	448372.548784	49.004276
3503.697434	448367.110952	49.009281
3503.939513	448369.199331	49.014285
3503.735767	448371.465248	49.019290
3504.219851	448372.650300	49.024295
3504.254214	448375.991095	49.029300
3504.278592	448359.811716	49.034305
3504.421174	448331.239816	49.039309
3503.812254	448332.560795	49.044314
3504.152156	448325.353227	49.049319
3504.099307	448309.491234	49.054324
3503.887620	448297.966391	49.059329
3503.849436	448286.361209	49.064333
3503.759163	448282.421580	49.069338
3503.982304	448284.766734	49.074343
3503.698212	448296.325644	49.079348
3503.812700	448282.209780	49.084353
3503.774101	448279.731813	49.089357
3503.341480	448280.008564	49.094362
3503.683849	448279.848747	49.099367
3503.818134	448284.440154	49.104372
3503.625526	448286.501353	49.109377
3503.751417	448278.316184	49.114381
3503.606329	448288.786528	49.119386
3503.884037	448285.595370	49.124391
3503.563569	448287.222043	49.129396
3503.694261	448272.089277	49.134401
3503.617228	448250.704370	49.139405
3503.488301	448249.763017	49.144410
3503.579452	448248.124901	49.149415
3504.026235	448268.889016	49.154420
3504.294439	448249.372002	49.159425
3504.274854	448245.217471	49.164429
3504.245842	448246.845087	49.169434
3504.247668	448236.399295	49.174439
3503.630543	448226.616956	49.179444
3503.465084	448214.019336	49.184449
3504.052284	448211.941571	49.189453
3503.364475	448217.079018	49.194458
3503.855047	448209.085086	49.199463
3503.891414	448207.101376	49.204468
3503.645071	448214.090293	49.209473
3503.988404	448210.837211	49.214477
3503.874818	448208.879106	49.219482
3503.988176	448201.050993	49.224487
3504.121563	448212.234424	49.229492
3503.482427	448197.233053	49.234497
3503.754033	448186.943998	49.239501
3503.481234	448175.835176	49.244506
3503.494759	448168.581870	49.249511
3503.644184	448187.824933	49.254516
3503.551799	448190.680334	49.259521
3503.793692	448190.436259	49.264525
3503.615295	448176.522454	49.269530
3504.102460	448172.382794	49.274535
3503.790087	448174.819400	49.279540
3503.878355	448172.319758	49.284545
3503.849201	448166.645646	49.289549
3503.586081	448176.172773	49.294554
3503.550236	448174.099977	49.299559
3503.793483	448175.072630	49.304564
3503.643809	448171.244537	49.309569
3503.751006	448173.406675	49.314573
3503.786834	448175.834532	49.319578
3504.225941	448170.638238	49.324583
3503.699531	448173.770577	49.329588
3503.920538	448165.619830	49.334593
3504.333998	448133.908303	49.339597
3503.990562	448135.031842	49.344602
3503.708424	448132.189788	49.349607
3503.734963	448133.655807	49.354612
3503.803479	448134.607592	49.359617
3503.893199	448136.772717	49.364621
3503.933848	448140.720957	49.369626
3504.075405	448117.625268	49.374631
3503.839843	448104.684606	49.379636
3503.707872	448098.875911	49.384641
3504.276835	448087.166949	49.389645
3503.571790	448100.116221	49.394650
3503.860988	448092.917233	49.399655
3503.686592	448093.859789	49.404660
3503.678834	448096.954286	49.409665
3503.944779	448092.953798	49.414669
3503.718290	448102.221170	49.419674
3503.854691	448096.417357	49.424679
3503.873044	448104.730197	49.429684
3503.731949	448083.001110	49.434689
3503.981361	448070.383272	49.439693
3503.839389	448072.537259	49.444698
3504.063463	448055.816480	49.449703
3504.241778	448054.822656	49.454708
3503.959736	448052.487644	49.459713
3504.009401	448046.698628	49.464717
3503.712782	448027.227145	49.469722
3504.221611	448016.086189	49.474727
3503.781013	448015.045922	49.479732
3503.535134	448013.161094	49.484737
3503.797500	448008.045647	49.489741
3503.824149	448016.864176	49.494746
3503.880866	448008.234351	49.499751
3503.874312	448006.562193	49.504756
3503.956871	448010.097644	49.509761
3504.083963	447997.804891	49.514765
3503.743442	447985.034198	49.519770
3504.009619	447971.855660	49.524775
3503.863490	447963.311160	49.529780
3503.968254	447967.197778	49.534785
3503.885034	447960.417285	49.539789
3503.747245	447971.596440	49.544794
3503.841327	447968.132345	49.549799
3503.646150	447963.297841	49.554804
3503.688994	447963.594824	49.559809
3503.730754	447958.669154	49.564813
3503.576573	447975.073944	49.569818
3503.977750	447949.550506	49.574823
3503.997241	447934.892852	49.579828
3503.713040	447920.794115	49.584833
3504.052731	447921.750313	49.589837
3503.563210	447932.076817	49.594842
3504.028820	447921.044605	49.599847
3503.645264	447920.197422	49.604852
3503.676283	447922.068350	49.609857
3503.833784	447924.171216	49.614861
3503.881051	447925.937954	49.619866
3504.384638	447926.663338	49.624871
3503.846171	447906.878089	49.629876
3503.954978	447890.582520	49.634881
3503.935176	447883.486929	49.639885
3503.931812	447896.265806	49.644890
3504.148065	447886.493130	49.649895
3504.380294	447887.163435	49.654900
3504.083647	447863.483096	49.659905
3504.387606	447852.224914	49.664909
3503.912238	447854.182313	49.669914
3503.982113	447846.209372	49.674919
3504.282186	447841.493105	49.679924
3503.556097	447817.683213	49.684929
3503.655590	447802.099071	49.689933
3503.838005	447812.868682	49.694938
3503.694346	447801.889734	49.699943
3503.808949	447809.172105	49.704948
3503.771700	447799.746920	49.709953
3503.993526	447790.683154	49.714957
3503.920021	447800.887978	49.719962
3504.295756	447784.496042	49.724967
3504.606503	447788.448935	49.729972
3504.344740	447771.405228	49.734977
3504.125316	447763.430946	49.739981
3503.533357	447765.205431	49.744986
3503.932806	447749.164371	49.749991
3503.587948	447737.408422	49.754996
3503.653301	447739.881995	49.760001
3503.662385	447731.513729	49.765005
3503.840833	447733.258084	49.770010
3503.874044	447722.654556	49.775015
3503.645907	447726.902307	49.780020
3503.444047	447727.291784	49.785025
3503.829465	447715.512543	49.790029
3503.798420	447724.797415	49.795034
3503.878782	447714.337954	49.800039
3503.725826	447722.020996	49.805044
3503.722348	447722.224476	49.810049
3503.879605	447726.659960	49.815053
3503.756677	447739.510054	49.820058
3504.004057	447722.125833	49.825063
3504.096558	447716.481534	49.830068
3504.303203	447691.193833	49.835073
3504.335165	447684.444292	49.840077
3503.814402	447686.865828	49.845082
3503.840772	447679.762285	49.850087
3504.028989	447679.780910	49.855092
3504.243895	447667.472971	49.860097
3504.000894	447639.980132	49.865101
3503.606021	447648.110171	49.870106
3504.092418	447638.595501	49.875111
3503.973506	447639.477895	49.880116
3503.941728	447643.337179	49.885121
3504.159536	447634.476864	49.890125
3504.198634	447615.606881	49.895130
3504.034807	447598.901268	49.900135
3504.240657	447597.699889	49.905140
3504.060243	447600.570400	49.910145
3504.713896	447592.599099	49.915149
3504.223752	447577.064764	49.920154
3503.954264	447567.476298	49.925159
3503.925681	447569.763098	49.930164
3503.983763	447554.490094	49.935169
3504.110628	447522.928005	49.940173
3503.852147	447525.101941	49.945178
3504.109264	447520.747895	49.950183
3503.520467	447518.059537	49.955188
3503.527993	447518.261140	49.960193
3504.004510	447509.660847	49.965197
3503.696643	447516.711207	49.970202
3504.014760	447508.188668	49.975207
3503.942597	447512.764787	49.980212
3503.463307	447519.033085	49.985217
3503.829174	447516.283133	49.990221
3503.930349	447508.608969	49.995226
3503.622074	447478.033862	50.000231
3503.629101	447475.395885	50.005236
3503.595398	447470.077321	50.010241
3503.934039	447465.760053	50.015245
3503.837921	447477.540853	50.020250
3503.777208	447476.537109	50.025255
3503.751420	447468.377526	50.030260
3503.838681	447473.940598	50.035265
3503.863970	447470.437461	50.040269
3503.698113	447479.035543	50.045274
3503.873699	447470.080952	50.050279
3503.729299	447476.241372	50.055284
3503.785047	447477.905282	50.060289
3503.897668	447465.310442	50.065293
3503.655992	447453.790257	50.070298
3503.669895	447441.060133	50.075303
3503.632420	447433.612451	50.080308
3503.573980	447435.701530	50.085313
3503.674120	447417.175906	50.090317
3503.580245	447428.499974	50.095322
3503.979120	447429.344673	50.100327
3503.564961	447425.510897	50.105332
3503.513221	447431.503382	50.110337
3503.922938	447419.516995	50.115341
3503.612441	447424.995872	50.120346
3503.710343	447442.220074	50.125351
3503.772274	447442.361680	50.130356
3504.085138	447432.318756	50.135361
3503.963281	447422.299348	50.140365
3503.554175	447426.172392	50.145370
3503.639287	447417.993854	50.150375
3503.503622	447426.282551	50.155380
3503.433134	447431.264069	50.160385
3503.724164	447413.770725	50.165389
3503.458018	447430.499304	50.170394
3503.735152	447422.947190	50.175399
3503.785039	447431.204203	50.180404
3503.715788	447428.427119	50.185409
3503.780300	447426.945614	50.190413
3503.659965	447436.195151	50.195418
3503.645817	447427.070105	50.200423
3504.035687	447429.792554	50.205428
3504.133811	447418.569288	50.210433
3504.098096	447395.705915	50.215437
3504.192692	447395.385567	50.220442
3503.959807	447393.752007	50.225447
3504.016273	447391.714080	50.230452
3503.948635	447379.302093	50.235457
3504.246114	447351.057380	50.240461
3503.995985	447355.613212	50.245466
3504.147626	447354.826745	50.250471
3504.458925	447348.790029	50.255476
3503.994373	447336.648625	50.260481
3504.129021	447311.271347	50.265485
3504.136690	447318.774981	50.270490
3504.106366	447317.816749	50.275495
3504.109407	447303.567136	50.280500
3503.863987	447284.644023	50.285505
3503.674635	447270.985035	50.290509
3503.721173	447272.549118	50.295514
3503.445489	447267.119694	50.300519
3503.790990	447270.711790	50.305524
3503.452404	447277.564639	50.310529
3503.956499	447260.846128	50.315533
3503.924930	447268.964986	50.320538
3503.951979	447274.234139	50.325543
3503.822472	447270.250312	50.330548
3503.698401	447270.778641	50.335553
3504.049664	447267.929733	50.340557
3503.892856	447269.680663	50.345562
3503.779842	447257.377770	50.350567
3504.030325	447240.195460	50.355572
3503.747666	447235.527852	50.360577
3503.834129	447229.225240	50.365581
3503.810673	447237.799105	50.370586
3503.729154	447235.632597	50.375591
3503.971116	447228.745635	50.380596
3503.840820	447226.283202	50.385601
3503.814843	447219.391279	50.390605
3503.758008	447228.528645	50.395610
3503.868991	447230.183144	50.400615
3503.900836	447217.399113	50.405620
3503.842832	447197.581869	50.410625
3503.781361	447180.402067	50.415629
3504.001813	447191.723299	50.420634
3503.944671	447187.270719	50.425639
3503.863918	447187.538108	50.430644
3503.805579	447192.416189	50.435649
3503.740524	447181.322079	50.440653
3503.837100	447189.114833	50.445658
3503.870141	447185.306071	50.450663
3504.085823	447167.571844	50.455668
3503.791680	447159.711510	50.460673
3503.951597	447148.021169	50.465677
3503.940852	447154.006732	50.470682
3503.947555	447146.957079	50.475687
3504.022820	447139.642170	50.480692
3503.399095	447147.710058	50.485697
3504.124537	447140.791222	50.490701
3503.738167	447144.863271	50.495706
3503.848254	447128.262642	50.500711
3503.688064	447114.547866	50.505716
3503.671751	447103.800357	50.510721
3503.862633	447095.857180	50.515725
3503.839169	447102.808406	50.520730
3503.892331	447094.990163	50.525735
3504.189130	447069.737037	50.530740
3503.865704	447041.851480	50.535745
3504.098128	446988.617665	50.540749
3503.524733	446940.693691	50.545754
3503.460443	446877.774017	50.550759
3503.667099	446802.130414	50.555764
3503.253264	446712.495076	50.560769
3503.183675	446626.553146	50.565773
3502.947066	446526.947533	50.570778
3502.933799	446424.311380	50.575783
3502.429242	446311.971380	50.580788
3502.076177	446191.389678	50.585793
3502.054497	446058.681328	50.590797
3501.888456	445927.011043	50.595802
3501.730660	445777.944203	50.600807
3501.894586	445632.371280	50.605812
3500.965525	445476.486390	50.610817
3501.088182	445309.111679	50.615821
3500.494518	445136.330161	50.620826
3499.973625	444958.869109	50.625831
3499.804579	444781.092937	50.630836
3499.204075	444595.477403	50.635841
3499.069365	444406.534931	50.640845
3498.737584	444216.457984	50.645850
3498.223875	444012.108366	50.650855
3497.691662	443805.071969	50.655860
3496.986126	443597.860313	50.660865
3496.777015	443387.315952	50.665869
3496.535756	443174.492701	50.670874
3495.972920	442952.745006	50.675879
3495.503611	442727.225829	50.680884
3494.873024	442490.471990	50.685889
3494.551207	442259.495725	50.690893
3493.826947	442028.382845	50.695898
3493.576016	441785.774304	50.700903
3493.441983	441543.853220	50.705908
3492.663275	441299.807735	50.710913
3492.253619	441047.986550	50.715917
3491.376184	440800.249546	50.720922
3490.784900	440534.047850	50.725927
3490.374785	440277.703416	50.730932
3489.342751	440026.940581	50.735937
3488.923606	439766.635131	50.740941
3488.514919	439520.883470	50.745946
3488.069114	439251.952925	50.750951
3487.341000	438988.495236	50.755956
3486.455130	438726.786133	50.760961
3486.458520	438450.870057	50.765965
3485.491852	438182.167677	50.770970
3485.012102	437915.661790	50.775975
3484.284848	437637.526796	50.780980
3483.856485	437370.954902	50.785985
3483.322558	437097.650440	50.790989
3482.197309	436821.196698	50.795994
3481.707107	436547.015597	50.800999
3481.348184	436270.677894	50.806004
3480.646050	435990.793223	50.811009
3480.113580	435716.609230	50.816013
3479.295221	435441.253057	50.821018
3478.965156	435162.055628	50.826023
3478.347636	434874.582899	50.831028
3477.560827	434601.443583	50.836033
3477.199691	434303.315582	50.841037
3476.702234	434020.225821	50.846042
3475.787497	433728.831696	50.851047
3475.109536	433425.114174	50.856052
3474.234790	433141.773508	50.861057
3474.022994	432848.117000	50.866061
3473.073862	432563.767059	50.871066
3472.239080	432274.471980	50.876071
3472.131746	431981.699954	50.881076
3471.520498	431696.215986	50.886081
3470.856078	431393.585706	50.891085
3470.101548	431101.674230	50.896090
3469.134568	430804.213246	50.901095
3468.647696	430504.484345	50.906100
3468.242800	430209.964607	50.911105
3467.746922	429911.143072	50.916109
3466.987625	429614.392658	50.921114
3466.264294	429317.074092	50.926119
3465.581114	429005.331795	50.931124
3464.838423	428704.354743	50.936129
3464.311172	428406.686661	50.941133
3463.462258	428115.363034	50.946138
3462.682588	427811.284999	50.951143
3462.347926	427502.863762	50.956148
3461.615628	427208.717604	50.961153
3460.886245	426900.355934	50.966157
3460.331912	426598.000285	50.971162
3459.453422	426301.533112	50.976167
3459.115881	426000.757067	50.981172
3458.178733	425696.780395	50.986177
3457.711881	425380.842157	50.991181
3456.882580	425076.534654	50.996186
3455.995240	424776.192443	51.001191
3455.549842	424462.725686	51.006196
3454.299892	424165.128064	51.011201
3453.681184	423868.535732	51.016205
3452.511414	423577.566917	51.021210
3451.641514	423283.193078	51.026215
3451.304604	422987.709394	51.031220
3450.402730	422706.177104	51.036225
3449.846770	422414.531157	51.041229
3449.011738	422127.802818	51.046234
3448.654509	421836.979051	51.051239
3447.882869	421557.797279	51.056244
3447.026034	421264.259902	51.061249
3446.571765	420985.855089	51.066253
3445.821286	420695.541878	51.071258
3445.373019	420403.802897	51.076263
3444.750283	420123.513313	51.081268
3443.945414	419831.650793	51.086273
3443.010380	419538.030109	51.091277
3442.739345	419252.238210	51.096282
3442.180456	418969.005374	51.101287
3441.941013	418670.965505	51.106292
3441.026340	418382.785733	51.111297
3439.872745	418079.563800	51.116301
3439.185669	417791.592232	51.121306
3438.274874	417500.177523	51.126311
3437.986000	417204.515078	51.131316
3436.842644	416921.105060	51.136321
3436.488842	416633.647273	51.141325
3435.586948	416360.141858	51.146330
3434.800024	416066.988453	51.151335
3434.395090	415779.580500	51.156340
3433.356757	415502.737819	51.161345
3433.004491	415214.603603	51.166349
3432.380347	414936.541526	51.171354
3431.335809	414655.729924	51.176359
3431.092717	414361.956272	51.181364
3430.239468	414080.470952	51.186369
3429.788527	413791.245804	51.191373
3428.707564	413516.318664	51.196378
3428.242650	413231.939348	51.201383
3427.318048	412945.223194	51.206388
3426.648232	412669.429703	51.211393
3426.195787	412385.445246	51.216397
3425.522951	412103.780657	51.221402
3424.708040	411822.416607	51.226407
3424.119169	411536.059273	51.231412
3423.309029	411259.893938	51.236417
3422.812707	410977.069760	51.241421
3422.078835	410693.495891	51.246426
3421.670607	410412.783687	51.251431
3421.024838	410125.430319	51.256436
3419.779431	409846.251748	51.261441
3419.361204	409569.595447	51.266445
3418.501255	409294.129084	51.271450
3417.887707	409011.557830	51.276455
3417.514806	408728.307586	51.281460
3416.636459	408455.908577	51.286465
3416.161775	408169.419088	51.291469
3415.259140	407887.444017	51.296474
3414.337115	407613.621682	51.301479
3413.669725	407333.276806	51.306484
3413.071601	407068.206400	51.311489
3412.612177	406780.505814	51.316493
3411.636144	406503.278128	51.321498
3410.851296	406233.989972	51.326503
3410.301530	405949.572341	51.331508
3409.488081	405687.369801	51.336513
3409.181328	405406.841785	51.341517
3408.635348	405135.647836	51.346522
3407.689212	404855.959921	51.351527
3407.320708	404576.881696	51.356532
3406.329505	404306.365152	51.361537
3405.788063	404022.434031	51.366541
3405.373070	403749.451388	51.371546
3404.272642	403475.236857	51.376551
3403.760175	403188.904539	51.381556
3403.005018	402922.068043	51.386561
3402.491666	402642.639361	51.391565
3401.634777	402366.949785	51.396570
3401.176463	402085.804194	51.401575
3400.555388	401812.482050	51.406580
3399.935907	401544.262858	51.411585
3399.746600	401259.938516	51.416589
3399.111187	400975.687476	51.421594
3397.919491	400694.475336	51.426599
3397.079082	400414.114922	51.431604
3396.399960	400140.252941	51.436609
3395.863158	399853.280946	51.441613
3395.127653	399579.931251	51.446618
3394.286579	399305.504559	51.451623
3393.768033	399023.551147	51.456628
3392.973212	398755.818107	51.461633
3392.364403	398471.486585	51.466637
3391.620213	398196.626194	51.471642
3390.720653	397929.843312	51.476647
3390.585016	397658.303610	51.481652
3389.385691	397380.921731	51.486657
3388.985484	397107.186271	51.491661
3387.956538	396835.918412	51.496666
3387.201346	396571.232463	51.501671
3386.888527	396294.120680	51.506676
3386.070525	396031.523922	51.511681
3385.641519	395745.915286	51.516685
3384.797148	395489.314345	51.521690
3384.065826	395218.539544	51.526695
3383.566555	394938.804290	51.531700
3382.751591	394670.655770	51.536705
3382.433468	394389.842602	51.541709
3381.592932	394120.931177	51.546714
3381.185584	393845.972147	51.551719
3380.606318	393575.105441	51.556724
3379.542865	393303.632885	51.561729
3379.176991	393023.983757	51.566733
3378.402023	392750.474905	51.571738
3377.637060	392474.878180	51.576743
3376.951355	392208.209934	51.581748
3376.110540	391927.361109	51.586753
3375.646947	391654.043166	51.591757
3374.750103	391398.330565	51.596762
3374.383200	391122.551792	51.601767
3373.374415	390838.214690	51.606772
3372.608409	390574.366392	51.611777
3372.118313	390306.606012	51.616781
3371.334209	390033.938047	51.621786
3370.595998	389769.798474	51.626791
3370.563875	389498.572884	51.631796
3369.540437	389233.867475	51.636801
3368.625946	388950.741877	51.641805
3368.356992	388688.901691	51.646810
3367.268646	388414.466881	51.651815
3366.566758	388142.682931	51.656820
3365.880658	387888.785546	51.661825
3365.489505	387618.443361	51.666829
3364.708787	387350.503503	51.671834
3364.264174	387076.582254	51.676839
3363.834067	386805.833013	51.681844
3363.016421	386537.689144	51.686849
3362.400541	386257.766511	51.691853
3361.440570	385980.594218	51.696858
3360.667284	385714.494409	51.701863
3360.387794	385439.259829	51.706868
3359.379638	385175.355958	51.711873
3358.845152	384897.211888	51.716877
3358.482728	384620.281421	51.721882
3357.597204	384359.349001	51.726887
3356.880843	384075.611605	51.731892
3355.921316	383812.196436	51.736897
3355.488173	383548.053753	51.741901
3354.848036	383268.693446	51.746906
3354.219820	383009.154875	51.751911
3353.530548	382731.755488	51.756916
3352.823880	382463.736162	51.761921
3352.070321	382188.071544	51.766925
3351.732791	381919.501704	51.771930
3350.607128	381642.701297	51.776935
3350.036996	381380.419862	51.781940
3348.962865	381107.851155	51.786945
3349.003763	380844.240909	51.791949
3348.107382	380574.382744	51.796954
3347.493978	380309.761454	51.801959
3347.171581	380036.572459	51.806964
3346.259305	379770.243854	51.811969
3345.714603	379493.300632	51.816973
3344.664659	379226.914894	51.821978
3343.668422	378952.637220	51.826983
3342.958607	378685.223031	51.831988
3342.349642	378431.873126	51.836993
3341.367469	378161.781122	51.841997
3340.870773	377900.298403	51.847002
3340.574884	377646.406057	51.852007
3339.963588	377373.422476	51.857012
3338.946923	377115.454494	51.862017
3338.189861	376858.279159	51.867021
3337.480009	376590.314391	51.872026
3336.949136	376341.130210	51.877031
3336.579369	376075.111732	51.882036
3335.831355	375804.248993	51.887041
3335.402982	375538.871930	51.892045
3334.738845	375277.092451	51.897050
3334.052696	375015.365578	51.902055
3333.021150	374744.746268	51.907060
3332.472444	374488.000536	51.912065
3331.745522	374222.765987	51.917069
3331.130636	373954.306704	51.922074
3330.597265	373699.154274	51.927079
3330.509870	373424.575008	51.932084
3329.659967	373161.539938	51.937089
3328.694290	372895.980068	51.942093
3327.833250	372619.797635	51.947098
3327.239495	372355.594005	51.952103
3326.891230	372075.658330	51.957108
3325.970957	371823.940013	51.962113
3325.285450	371558.373030	51.967117
3324.473174	371292.901985	51.972122
3323.696371	371030.830141	51.977127
3322.911308	370761.688953	51.982132
3322.180503	370503.724610	51.987137
3321.429784	370246.880626	51.992141
3321.380359	369987.601080	51.997146
3320.097391	369724.563544	52.002151
3319.358291	369467.762850	52.007156
3318.986479	369216.034158	52.012161
3318.450730	368954.770520	52.017165
3317.677329	368691.841851	52.022170
3316.706703	368432.276166	52.027175
3316.487699	368170.062764	52.032180
3315.760144	367919.962448	52.037185
3315.051000	367658.947978	52.042189
3314.495360	367394.548699	52.047194
3313.670991	367140.645127	52.052199
3313.156119	366874.556767	52.057204
3312.321178	366619.379899	52.062209
3311.717884	366350.480097	52.067213
3310.884090	366088.356843	52.072218
3310.423497	365833.415795	52.077223
3309.867421	365567.096205	52.082228
3308.801982	365311.542821	52.087233
3308.552921	365049.846451	52.092237
3307.990955	364781.691216	52.097242
3307.196901	364534.478603	52.102247
3306.400635	364264.833797	52.107252
3305.822724	364010.078414	52.112257
3305.104706	363750.513116	52.117261
3304.541154	363488.376418	52.122266
3303.710676	363233.048577	52.127271
3303.057092	362964.997855	52.132276
3302.139909	362714.717049	52.137281
3301.702205	362446.040864	52.142285
3301.831925	362185.023049	52.147290
3300.481331	361927.435478	52.152295
3300.109794	361658.411865	52.157300
3299.278053	361397.858146	52.162305
3298.323648	361125.013572	52.167309
3298.359347	360859.551932	52.172314
3297.288768	360601.475352	52.177319
3296.858545	360339.447089	52.182324
3296.085653	360073.329747	52.187329
3295.171641	359809.829061	52.192333
3294.643453	359542.165676	52.197338
3293.990826	359272.410611	52.202343
3293.336037	359011.810813	52.207348
3292.535513	358747.113638	52.212353
3291.792225	358482.532107	52.217357
3290.976442	358224.320172	52.222362
3290.120227	357969.598215	52.227367
3289.851809	357707.601239	52.232372
3288.671708	357454.635559	52.237377
3288.122340	357195.277746	52.242381
3287.214180	356935.394505	52.247386
3286.496671	356690.230406	52.252391
3286.412646	356435.137950	52.257396
3285.659181	356187.662198	52.262401
3284.801299	355919.522244	52.267405
3284.590801	355664.777267	52.272410
3283.977900	355416.840412	52.277415
3283.389645	355149.844950	52.282420
3282.339699	354896.586798	52.287425
3281.958829	354638.532209	52.292429
3281.171803	354379.273472	52.297434
3279.995226	354117.815633	52.302439
3279.360328	353858.196970	52.307444
3278.793322	353605.713387	52.312449
3278.132333	353353.320653	52.317453
3277.370962	353095.372398	52.322458
3276.738595	352842.055905	52.327463
3276.282455	352578.939082	52.332468
3275.348445	352324.399044	52.337473
3274.662306	352079.456776	52.342477
3274.330372	351824.327559	52.347482
3273.397752	351569.986295	52.352487
3272.803971	351313.397798	52.357492
3272.337435	351068.666637	52.362497
3271.553101	350816.839612	52.367501
3271.277859	350550.244963	52.372506
3270.257127	350296.598124	52.377511
3270.098837	350038.197702	52.382516
3269.359955	349781.497697	52.387521
3268.487969	349515.303921	52.392525
3267.975613	349259.732456	52.397530
3267.025234	348999.400440	52.402535
3266.406750	348750.586130	52.407540
3265.721244	348489.417172	52.412545
3265.108867	348219.609376	52.417549
3264.270860	347967.902344	52.422554
3263.364703	347729.053838	52.427559
3263.285169	347457.420346	52.432564
3262.216870	347212.617824	52.437569
3261.343098	346961.928937	52.442573
3260.941575	346691.541613	52.447578
3260.312614	346443.632180	52.452583
3259.626720	346187.996423	52.457588
3258.537774	345937.313165	52.462593
3258.081911	345676.495717	52.467597
3257.353789	345424.806609	52.472602
3256.845134	345181.322368	52.477607
3256.116703	344920.648947	52.482612
3255.346494	344683.465912	52.487617
3254.951839	344430.772985	52.492621
3254.336894	344162.977018	52.497626
3253.476116	343917.154507	52.502631
3252.650892	343667.075402	52.507636
3251.823470	343420.659355	52.512641
3251.511033	343157.309642	52.517645
3250.768487	342915.456498	52.522650
3249.946758	342664.022874	52.527655
3249.544833	342411.930972	52.532660
3248.730389	342162.198263	52.537665
3248.108273	341911.515359	52.542669
3247.609053	341656.077276	52.547674
3246.511724	341412.037868	52.552679
3245.793361	341154.471660	52.557684
3245.357959	340910.698332	52.562689
3244.792428	340662.416601	52.567693
3244.177904	340412.335286	52.572698
3243.608274	340167.334280	52.577703
3243.173941	339907.270077	52.582708
3242.105675	339658.407483	52.587713
3241.477116	339406.440361	52.592717
3241.259735	339152.162393	52.597722
3240.275904	338898.090369	52.602727
3239.714512	338640.636761	52.607732
3238.983406	338401.456475	52.612737
3238.187159	338141.546565	52.617741
3237.436863	337889.032676	52.622746
3236.796306	337644.183950	52.627751
3236.345112	337381.640949	52.632756
3235.422551	337137.906733	52.637761
3234.705611	336887.087124	52.642765
3234.242915	336639.047589	52.647770
3233.582153	336380.785031	52.652775
3233.224952	336127.584439	52.657780
3232.278915	335884.535331	52.662785
3231.508245	335634.227710	52.667789
3230.921327	335372.435548	52.672794
3230.487179	335126.521514	52.677799
3229.522951	334872.884014	52.682804
3229.245695	334617.677336	52.687809
3228.621121	334366.295224	52.692813
3228.099818	334102.347724	52.697818
3226.792055	333850.748992	52.702823
3226.470711	333584.041641	52.707828
3225.754579	333347.736476	52.712833
3225.116942	333090.395269	52.717837
3224.262513	332828.381599	52.722842
3223.486226	332582.412315	52.727847
3222.826530	332334.691371	52.732852
3222.068370	332080.521718	52.737857
3221.949493	331825.529059	52.742861
3221.162710	331573.296143	52.747866
3220.335315	331322.239725	52.752871
3219.659320	331060.085183	52.757876
3219.002541	330814.825525	52.762881
3218.371218	330563.630327	52.767885
3217.974778	330302.417005	52.772890
3216.848993	330056.165128	52.777895
3216.496096	329802.399233	52.782900
3215.616032	329542.766572	52.787905
3214.995077	329290.571224	52.792909
3214.746958	329043.808633	52.797914
3213.538099	328789.039018	52.802919
3213.042019	328534.935511	52.807924
3212.167111	328286.775004	52.812929
3211.502544	328037.712109	52.817933
3211.212491	327778.479587	52.822938
3210.709911	327529.997664	52.827943
3209.845285	327268.239377	52.832948
3209.052906	327017.743085	52.837953
3208.728679	326752.224970	52.842957
3207.757313	326499.848054	52.847962
3207.129451	326252.629231	52.852967
3206.266988	325990.890265	52.857972
3205.812624	325751.275619	52.862977
3205.017011	325488.097615	52.867981
3204.655719	325228.840440	52.872986
3203.741310	324979.603490	52.877991
3202.800759	324727.570061	52.882996
3202.422584	324471.392363	52.888001
3201.832295	324227.314929	52.893005
3201.226065	323977.053917	52.898010
3200.181575	323724.626772	52.903015
3199.831754	323464.978203	52.908020
3198.832694	323212.897530	52.913025
3198.411940	322973.622405	52.918029
3197.802207	322708.465964	52.923034
3197.086760	322466.464663	52.928039
3196.444212	322209.278966	52.933044
3195.684418	321952.595873	52.938049
3194.961835	321710.007380	52.943053
3194.454068	321460.024758	52.948058
3193.641114	321217.678890	52.953063
3192.861242	320957.838717	52.958068
3192.564303	320704.227901	52.963073
3191.559979	320454.657036	52.968077
3191.195680	320199.044736	52.973082
3190.138517	319950.600969	52.978087
3189.843366	319694.618469	52.983092
3188.807724	319450.445654	52.988097
3188.253286	319196.185553	52.993101
3187.923889	318947.079041	52.998106
3186.816230	318699.173675	53.003111
3186.389341	318448.707290	53.008116
3185.814144	318199.818119	53.013121
3185.097804	317951.766724	53.018125
3184.743948	317694.717260	53.023130
3183.424455	317448.447143	53.028135
3182.788353	317185.512548	53.033140
3182.439847	316943.529634	53.038145
3181.575710	316692.724029	53.043149
3181.473645	316439.445282	53.048154
3180.090794	316181.242047	53.053159
3179.896634	315944.524274	53.058164
3179.055707	315689.892443	53.063169
3177.989594	315440.796920	53.068173
3177.562489	315203.429044	53.073178
3176.954673	314955.093584	53.078183
3176.297852	314696.200709	53.083188
3175.255746	314455.778600	53.088193
3174.537923	314210.386925	53.093197
3174.286018	313963.972870	53.098202
3173.118863	313725.478976	53.103207
3172.713802	313483.442726	53.108212
3172.273361	313236.625575	53.113217
3171.678583	312991.081392	53.118221
3171.142343	312740.027383	53.123226
3170.475565	312495.613982	53.128231
3169.739007	312243.421390	53.133236
3169.110482	311995.206467	53.138241
3168.480638	311739.862511	53.143245
3168.314821	311490.573961	53.148250
3167.331093	311245.294028	53.153255
3167.031127	310982.355305	53.158260
3166.063277	310721.184580	53.163265
3164.988407	310465.937736	53.168269
3164.548656	310214.858678	53.173274
3163.596827	309962.058657	53.178279
3163.004547	309713.117116	53.183284
3162.570958	309468.042948	53.188289
3161.514814	309216.429419	53.193293
3161.297939	308969.178050	53.198298
3160.163777	308721.955289	53.203303
3159.882720	308472.472858	53.208308
3159.377572	308225.268378	53.213313
3158.511150	307978.150296	53.218317
3158.016601	307716.201131	53.223322
3156.825807	307464.477683	53.228327
3156.539501	307221.331765	53.233332
3155.692538	306965.958139	53.238337
3155.252754	306719.221572	53.243341
3154.409397	306466.875531	53.248346
3153.549052	306233.754253	53.253351
3152.935821	305971.947009	53.258356
3151.945015	305720.922347	53.263361
3151.216290	305486.045148	53.268365
3151.232733	305247.017196	53.273370
3150.196678	305010.103376	53.278375
3149.734963	304749.335757	53.283380
3148.756973	304507.954948	53.288385
3148.187634	304265.128748	53.293389
3147.799770	304012.824782	53.298394
3147.111295	303771.137821	53.303399
3146.336362	303524.780080	53.308404
3145.466935	303279.405312	53.313409
3144.707447	303039.663505	53.318413
3144.170637	302793.237557	53.323418
3143.635812	302555.874892	53.328423
3143.105387	302298.803546	53.333428
3142.382582	302067.098705	53.338433
3141.551889	301817.537540	53.343437
3141.145725	301573.428380	53.348442
3140.370827	301327.395522	53.353447
3139.912365	301079.041828	53.358452
3138.951918	300836.298474	53.363457
3138.259187	300579.606438	53.368461
3137.781049	300332.705430	53.373466
3136.828981	300096.527942	53.378471
3136.355456	299852.756731	53.383476
3135.626628	299606.100329	53.388481
3135.038729	299368.331060	53.393485
3134.382469	299113.156526	53.398490
3133.745229	298877.431463	53.403495
3132.761581	298619.357885	53.408500
3132.418795	298381.340598	53.413505
3131.511923	298143.266313	53.418509
3131.107457	297895.658919	53.423514
3130.487982	297662.066755	53.428519
3129.874275	297401.151316	53.433524
3129.336916	297157.613388	53.438529
3128.205752	296913.412415	53.443533
3127.787436	296656.153804	53.448538
3127.118971	296417.245314	53.453543
3126.357996	296170.458458	53.458548
3125.915603	295931.102802	53.463553
3125.072165	295690.898420	53.468557
3124.783749	295437.714172	53.473562
3123.883645	295205.768507	53.478567
3122.928133	294946.585796	53.483572
3122.278409	294702.144574	53.488577
3121.744865	294454.831014	53.493581
3121.444269	294202.180634	53.498586
3120.670608	293956.078280	53.503591
3119.869872	293707.637321	53.508596
3119.533974	293457.614020	53.513601
3119.140776	293207.345301	53.518605
3118.453558	292956.158613	53.523610
3117.783150	292708.202427	53.528615
3117.436368	292449.571866	53.533620
3116.579157	292198.361599	53.538625
3115.672745	291938.883304	53.543629
3114.578842	291685.675207	53.548634
3113.710430	291428.964883	53.553639
3112.740131	291186.098578	53.558644
3112.433096	290936.395844	53.563649
3111.501091	290694.540563	53.568653
3111.347963	290443.486347	53.573658
3110.355313	290202.557156	53.578663
3109.854956	289956.883350	53.583668
3109.075639	289710.976592	53.588673
3108.330176	289474.103554	53.593677
3108.086810	289229.683093	53.598682
3107.202835	288985.855422	53.603687
3106.782143	288741.769879	53.608692
3105.538599	288494.004689	53.613697
3105.359906	288251.379295	53.618701
3104.654962	287990.966862	53.623706
3103.750587	287753.302865	53.628711
3103.305048	287511.994927	53.633716
3102.593424	287260.418590	53.638721
3101.804077	287013.795313	53.643725
3101.198923	286765.892315	53.648730
3100.253529	286525.202750	53.653735
3100.052228	286280.005593	53.658740
3099.402647	286044.001208	53.663745
3098.579913	285799.087612	53.668749
3097.855206	285552.374251	53.673754
3096.719965	285309.193909	53.678759
3096.371678	285059.792425	53.683764
3095.857698	284825.392624	53.688769
3094.866022	284576.634991	53.693773
3094.452296	284334.450225	53.698778
3093.786766	284098.852784	53.703783
3093.219177	283849.843207	53.708788
3092.436104	283607.491153	53.713793
3091.516545	283368.829118	53.718797
3091.133303	283117.316640	53.723802
3090.152889	282883.171714	53.728807
3089.915908	282637.949032	53.733812
3089.148189	282390.295492	53.738817
3088.122594	282149.968927	53.743821
3088.004002	281912.186461	53.748826
3087.068230	281675.638292	53.753831
3086.627586	281428.640436	53.758836
3085.809543	281194.669011	53.763841
3085.301170	280939.125323	53.768845
3084.719974	280686.012988	53.773850
3083.749080	280456.421384	53.778855
3082.889057	280202.948497	53.783860
3082.357768	279970.734497	53.788865
3081.875023	279726.262514	53.793869
3081.248847	279483.622817	53.798874
3080.260641	279246.392612	53.803879
3080.033732	278996.706205	53.808884
3079.191310	278758.329922	53.813889
3078.597409	278518.968605	53.818893
3077.999291	278266.441418	53.823898
3077.288128	278039.476329	53.828903
3076.709625	277784.296605	53.833908
3076.212747	277543.669600	53.838913
3075.349915	277298.113318	53.843917
3074.739807	277049.432063	53.848922
3073.713983	276809.938662	53.853927
3073.660415	276569.514867	53.858932
3072.982774	276320.156638	53.863937
3072.071182	276073.206503	53.868941
3071.422891	275817.857915	53.873946
3070.707223	275583.428965	53.878951
3069.725961	275326.990653	53.883956
3069.299438	275091.620421	53.888961
3068.509743	274846.150598	53.893965
3067.971570	274603.922797	53.898970
3067.298798	274363.856972	53.903975
3066.513647	274130.100491	53.908980
3066.021933	273887.252777	53.913985
3065.236155	273634.573754	53.918989
3064.893047	273388.236591	53.923994
3064.095321	273149.107690	53.928999
3063.375207	272900.287708	53.934004
3062.792109	272654.449218	53.939009
3062.213677	272409.042635	53.944013
3061.639128	272172.752486	53.949018
3060.389278	271932.859246	53.954023
3060.091383	271675.408882	53.959028
3059.400644	271442.092152	53.964033
3058.997624	271187.791783	53.969037
3058.304686	270940.213202	53.974042
3057.692759	270693.435524	53.979047
3057.060220	270449.207911	53.984052
3056.506415	270201.732259	53.989057
3055.551145	269956.591606	53.994061
3054.905553	269704.776262	53.999066
3054.276892	269456.650630	54.004071
3053.552216	269206.350985	54.009076
3053.070818	268965.228885	54.014081
3052.118631	268717.081548	54.019085
3050.926991	268468.974934	54.024090
3049.728646	268231.693076	54.029095
3049.585822	267991.938628	54.034100
3049.386758	267752.652044	54.039105
3048.644870	267516.412305	54.044109
3048.303968	267274.959410	54.049114
3047.351629	267040.130585	54.054119
3046.766127	266799.024790	54.059124
3046.161156	266554.178399	54.064129
3045.005327	266311.208722	54.069133
3044.699700	266060.325942	54.074138
3043.567151	265818.931011	54.079143
3043.021334	265574.761573	54.084148
3042.300580	265351.531062	54.089153
3041.386208	265107.475274	54.094157
3040.885614	264875.955306	54.099162
3040.569076	264647.816490	54.104167
3039.871224	264400.336114	54.109172
3039.576797	264172.269709	54.114177
3038.578125	263935.053170	54.119181
3037.833032	263693.005217	54.124186
3037.111880	263469.442857	54.129191
3036.401991	263230.775941	54.134196
3035.979042	262980.395542	54.139201
3035.523878	262737.762836	54.144205
3034.827180	262493.464943	54.149210
3033.726599	262240.907904	54.154215
3033.886182	262001.888243	54.159220
3033.085661	261763.363621	54.164225
3031.912832	261520.241870	54.169229
3031.343761	261271.948742	54.174234
3030.734708	261036.982195	54.179239
3030.523173	260788.627843	54.184244
3029.777044	260545.611193	54.189249
3028.852486	260304.407738	54.194253
3028.146738	260061.817033	54.199258
3027.236693	259824.711362	54.204263
3026.620621	259573.522469	54.209268
3026.074313	259327.440708	54.214273
3025.277993	259100.706481	54.219277
3024.701139	258851.217125	54.224282
3024.123428	258612.806530	54.229287
3023.400638	258370.167507	54.234292
3023.069399	258131.791149	54.239297
3021.925598	257896.304155	54.244301
3021.535481	257640.415707	54.249306
3020.486152	257412.527521	54.254311
3019.772270	257176.788747	54.259316
3019.416455	256931.998521	54.264321
3018.572855	256693.047433	54.269325
3017.767540	256446.933242	54.274330
3017.012791	256221.974470	54.279335
3016.449422	255983.230185	54.284340
3015.606187	255755.485039	54.289345
3015.007959	255530.626882	54.294349
3014.760844	255285.563420	54.299354
3013.728919	255053.215339	54.304359
3013.246425	254816.112729	54.309364
3012.318494	254579.697481	54.314369
3011.445115	254361.329869	54.319373
3011.208049	254123.701506	54.324378
3010.700980	253887.188967	54.329383
3010.017468	253658.958292	54.334388
3009.135827	253422.662630	54.339393
3008.262514	253197.546104	54.344397
3008.351139	252939.767917	54.349402
3007.466969	252713.838354	54.354407
3006.595222	252477.566653	54.359412
3006.363701	252249.641040	54.364417
3005.322428	252003.363973	54.369421
3005.083352	251764.080985	54.374426
3004.250187	251519.067369	54.379431
3003.530594	251276.148272	54.384436
3002.742239	251045.694894	54.389441
3002.321126	250800.050800	54.394445
3001.534190	250569.902944	54.399450
3000.990702	250328.023728	54.404455
3000.415164	250085.997266	54.409460
2999.776833	249838.429590	54.414465
2998.903097	249596.938157	54.419469
2998.277794	249355.709992	54.424474
2997.708688	249119.107504	54.429479
2996.940070	248887.963889	54.434484
2995.818129	248645.089058	54.439489
2994.894196	248399.047948	54.444493
2994.259609	248159.044365	54.449498
2993.569971	247930.612756	54.454503
2993.109605	247697.736129	54.459508
2992.619806	247468.404688	54.464513
2991.652680	247237.499502	54.469517
2991.246539	247005.887359	54.474522
2990.379130	246775.907691	54.479527
2990.008807	246535.808874	54.484532
2989.315151	246308.448435	54.489537
2988.828785	246075.729927	54.494541
2988.426763	245833.981533	54.499546
2988.100057	245598.510972	54.504551
2987.011229	245354.282510	54.509556
2986.786533	245119.507920	54.514561
2985.655522	244878.444988	54.519565
2985.034978	244622.447307	54.524570
2984.452482	244396.775379	54.529575
2983.289614	244153.018816	54.534580
2982.794867	243910.880080	54.539585
2981.759571	243676.830731	54.544589
2981.480003	243432.847383	54.549594
2980.489691	243212.594160	54.554599
2979.731073	242975.569281	54.559604
2979.284357	242744.246974	54.564609
2978.269622	242512.639882	54.569613
2977.911607	242286.370825	54.574618
2977.471247	242055.200778	54.579623
2977.074565	241814.218463	54.584628
2976.210033	241574.640601	54.589633
2975.392094	241352.602076	54.594637
2974.971109	241103.169334	54.599642
2974.037317	240874.886005	54.604647
2973.246094	240641.383165	54.609652
2972.858275	240410.613022	54.614657
2971.926458	240170.564047	54.619661
2971.460639	239933.695499	54.624666
2970.500467	239707.302305	54.629671
2970.006204	239478.843268	54.634676
2969.600180	239242.117977	54.639681
2968.379539	239016.202880	54.644685
2968.149547	238783.166188	54.649690
2967.388606	238544.719537	54.654695
2966.477577	238314.601073	54.659700
2966.223751	238087.222872	54.664705
2965.574855	237851.686529	54.669709
2965.378791	237609.604428	54.674714
2964.580941	237377.099162	54.679719
2963.787567	237145.637532	54.684724
2963.461326	236901.592044	54.689729
2962.145084	236662.936722	54.694733
2961.655656	236415.150576	54.699738
2961.132494	236168.312769	54.704743
2960.510848	235937.459822	54.709748
2959.986499	235703.177960	54.714753
2959.079816	235456.941367	54.719757
2958.491860	235220.175203	54.724762
2957.539338	234984.770425	54.729767
2957.389913	234747.624314	54.734772
2956.821061	234505.380429	54.739777
2955.539695	234258.929270	54.744781
2955.179519	234018.127432	54.749786
2954.209002	233795.689739	54.754791
2953.591185	233554.525073	54.759796
2952.807667	233312.625048	54.764801
2951.722368	233088.221460	54.769805
2951.268945	232852.886952	54.774810
2950.913125	232627.493456	54.779815
2949.861888	232392.872915	54.784820
2949.514898	232158.667160	54.789825
2948.769287	231933.799579	54.794829
2947.921452	231697.209813	54.799834
2947.277621	231469.447781	54.804839
2946.425694	231236.628381	54.809844
2946.070158	231014.573087	54.814849
2945.045755	230790.162171	54.819853
2944.612667	230546.041641	54.824858
2944.063418	230320.760752	54.829863
2943.256388	230097.306855	54.834868
2943.125067	229865.996165	54.839873
2941.997007	229635.976633	54.844877
2941.510857	229399.634085	54.849882
2940.835802	229165.972634	54.854887
2940.084403	228939.200366	54.859892
2939.683801	228704.677836	54.864897
2938.881427	228469.485822	54.869901
2938.328299	228235.626746	54.874906
2937.736269	228022.605611	54.879911
2937.108607	227784.914685	54.884916
2936.341084	227535.050037	54.889921
2936.031813	227314.112781	54.894925
2935.206573	227072.560582	54.899930
2934.549477	226832.584396	54.904935
2933.767072	226597.799517	54.909940
2933.136110	226358.787377	54.914945
2932.182282	226138.980750	54.919949
2931.798393	225898.883127	54.924954
2931.130994	225664.283938	54.929959
2930.136171	225430.072157	54.934964
2929.804721	225182.836614	54.939969
2928.925966	224964.776197	54.944973
2928.191782	224735.308564	54.949978
2927.747461	224503.092520	54.954983
2926.720476	224276.120378	54.959988
2926.332713	224043.386207	54.964993
2925.397957	223804.685290	54.969997
2925.052241	223575.993714	54.975002
2924.193672	223345.633119	54.980007
2923.534616	223116.690353	54.985012
2922.875275	222886.067393	54.990017
2922.127833	222650.519786	54.995021
2921.736262	222415.599374	55.000026
2920.858778	222197.645433	55.005031
2920.441994	221965.760491	55.010036
2919.582993	221733.493203	55.015041
2918.736785	221505.298490	55.020045
2918.038908	221258.846414	55.025050
2917.268142	221044.186737	55.030055
2916.786391	220824.614405	55.035060
2916.404544	220581.012698	55.040065
2915.533118	220363.213937	55.045069
2915.004552	220128.117826	55.050074
2914.361875	219899.993384	55.055079
2913.543435	219677.323268	55.060084
2913.006873	219443.121202	55.065089
2911.968926	219210.125716	55.070093
2911.782920	218970.568270	55.075098
2910.864764	218752.296838	55.080103
2910.307812	218521.486909	55.085108
2909.694157	218296.645658	55.090113
2908.923978	218073.028413	55.095117
2908.360793	217836.695422	55.100122
2907.928635	217613.352413	55.105127
2907.106883	217377.522975	55.110132
2906.725873	217134.820036	55.115137
2905.954414	216904.050287	55.120141
2905.425741	216672.271962	55.125146
2904.636721	216439.952994	55.130151
2903.780981	216203.546388	55.135156
2903.309986	215968.245892	55.140161
2902.433360	215738.260639	55.145165
2902.039565	215499.485074	55.150170
2901.543896	215265.921921	55.155175
2900.461442	215031.619311	55.160180
2900.011347	214791.862017	55.165185
2899.177086	214571.802715	55.170189
2898.443980	214333.622667	55.175194
2897.921291	214094.617908	55.180199
2897.055094	213871.026350	55.185204
2896.644007	213634.218905	55.190209
2895.767077	213400.852689	55.195213
2894.999663	213165.838741	55.200218
2894.315685	212940.690490	55.205223
2893.533588	212712.631389	55.210228
2893.359394	212483.730565	55.215233
2892.130641	212259.695532	55.220237
2892.105237	212027.434873	55.225242
2891.028917	211800.064843	55.230247
2890.549729	211566.507944	55.235252
2889.983859	211330.623966	55.240257
2888.811648	211099.274563	55.245261
2888.398036	210868.941904	55.250266
2888.010085	210645.480098	55.255271
2887.300816	210421.258986	55.260276
2887.007564	210181.308515	55.265281
2885.908621	209945.621126	55.270285
2885.060763	209709.662312	55.275290
2884.916520	209474.806045	55.280295
2883.576123	209242.420861	55.285300
2883.472121	209016.928697	55.290305
2882.288618	208780.953379	55.295309
2882.285508	208552.211632	55.300314
2881.291196	208319.871648	55.305319
2880.645473	208088.312944	55.310324
2879.738534	207860.033038	55.315329
2879.031112	207633.081809	55.320333
2878.797066	207388.927986	55.325338
2877.846957	207169.097562	55.330343
2877.245018	206942.041078	55.335348
2876.771299	206706.141250	55.340353
2876.132187	206471.925289	55.345357
2875.500378	206236.906750	55.350362
2874.763919	206010.194089	55.355367
2873.996386	205781.730618	55.360372
2873.185691	205539.717657	55.365377
2872.441531	205316.063478	55.370381
2872.118734	205078.614996	55.375386
2871.412078	204852.193302	55.380391
2870.471624	204622.693380	55.385396
2869.891872	204382.910399	55.390401
2869.165124	204161.064148	55.395405
2868.476762	203929.575510	55.400410
2867.755791	203703.872445	55.405415
2867.193643	203471.294305	55.410420
2866.578461	203240.775408	55.415425
2865.707722	203018.995224	55.420429
2865.033772	202786.043645	55.425434
2864.446076	202563.707234	55.430439
2863.397002	202336.396689	55.435444
2863.214557	202102.510342	55.440449
2862.164742	201886.428699	55.445453
2861.851130	201661.807727	55.450458
2861.185221	201442.097528	55.455463
2860.125256	201212.768286	55.460468
2860.232657	200975.653606	55.465473
2859.127674	200753.016369	55.470477
2858.576381	200527.001052	55.475482
2858.245381	200296.022595	55.480487
2857.338294	200069.980389	55.485492
2857.055822	199834.985425	55.490497
2855.679469	199606.199000	55.495501
2855.108377	199370.325650	55.500506
2854.596777	199152.072551	55.505511
2854.095403	198934.607567	55.510516
2853.314150	198695.208261	55.515521
2852.656084	198469.052185	55.520525
2852.063052	198240.887297	55.525530
2851.478669	198011.016016	55.530535
2850.280993	197780.155624	55.535540
2849.780888	197542.074182	55.540545
2848.867991	197333.709125	55.545549
2848.535644	197107.094486	55.550554
2847.832493	196877.667302	55.555559
2847.027355	196662.794292	55.560564
2847.043897	196435.740395	55.565569
2845.970379	196210.833711	55.570573
2845.192986	195984.375219	55.575578
2844.784863	195753.284902	55.580583
2843.862298	195522.996075	55.585588
2843.143898	195297.993567	55.590593
2842.677406	195079.503809	55.595597
2841.906649	194845.462005	55.600602
2841.186851	194616.898148	55.605607
2840.357034	194401.552922	55.610612
2839.897926	194168.147578	55.615617
2838.934602	193946.768104	55.620621
2838.584514	193722.828087	55.625626
2838.164186	193502.451934	55.630631
2837.359288	193280.627631	55.635636
2836.827684	193047.060503	55.640641
2835.709088	192820.098434	55.645645
2834.996477	192591.273177	55.650650
2834.271796	192377.813137	55.655655
2833.814348	192157.715218	55.660660
2833.303188	191925.255999	55.665665
2832.184029	191702.281751	55.670669
2831.993329	191481.326034	55.675674
2830.997259	191257.403219	55.680679
2830.315306	191048.891356	55.685684
2829.937981	190818.411566	55.690689
2829.334707	190601.856772	55.695693
2828.761751	190364.106604	55.700698
2828.080427	190143.430381	55.705703
2827.375899	189929.275243	55.710708
2826.605126	189698.319596	55.715713
2826.006861	189475.175241	55.720717
2825.251353	189248.444088	55.725722
2824.696930	189026.744770	55.730727
2823.847719	188799.598589	55.735732
2823.261596	188574.839146	55.740737
2822.601980	188350.933075	55.745741
2822.456902	188129.561637	55.750746
2821.673898	187903.349317	55.755751
2820.913512	187674.932267	55.760756
2820.441793	187444.799570	55.765761
2819.787233	187225.300298	55.770765
2818.902795	186988.596606	55.775770
2818.408334	186753.876196	55.780775
2817.375396	186537.791231	55.785780
2816.917602	186296.181364	55.790785
2815.920704	186083.438977	55.795789
2815.343987	185848.876257	55.800794
2814.838167	185633.340892	55.805799
2813.801807	185413.366459	55.810804
2813.671468	185174.568720	55.815809
2812.858890	184961.671713	55.820813
2812.434882	184726.667513	55.825818
2811.583367	184502.478114	55.830823
2810.677145	184272.012314	55.835828
2810.266562	184034.578024	55.840833
2809.406285	183817.175759	55.845837
2808.681129	183593.579217	55.850842
2807.970846	183364.216248	55.855847
2807.407682	183151.156187	55.860852
2806.938875	182918.317838	55.865857
2806.279524	182704.550562	55.870861
2805.509551	182470.289391	55.875866
2804.785483	182243.287640	55.880871
2803.840737	182019.836768	55.885876
2803.096272	181795.601781	55.890881
2802.523218	181583.402066	55.895885
2802.011713	181354.916980	55.900890
2801.797568	181131.179460	55.905895
2800.927337	180917.060717	55.910900
2800.733555	180686.882597	55.915905
2799.681875	180462.616543	55.920909
2799.119958	180234.704713	55.925914
2798.477871	179993.700811	55.930919
2797.818262	179764.280682	55.935924
2797.251198	179541.577190	55.940929
2796.362373	179324.108626	55.945933
2795.725160	179089.572205	55.950938
2795.182281	178858.061913	55.955943
2794.347397	178630.967102	55.960948
2793.762434	178398.308084	55.965953
2792.982765	178167.782927	55.970957
2792.326216	177936.372483	55.975962
2791.682921	177720.191959	55.980967
2791.032104	177496.213572	55.985972
2790.447906	177259.653132	55.990977
2789.515089	177038.778763	55.995981
2789.090257	176815.400927	56.000986
2788.386546	176588.279925	56.005991
2787.432585	176368.875337	56.010996
2787.125073	176132.896294	56.016001
2786.180229	175907.499110	56.021005
2785.512613	175692.909070	56.026010
2784.871447	175464.929897	56.031015
2784.414238	175240.521159	56.036020
2783.917652	175007.442544	56.041025
2782.894068	174783.425290	56.046029
2782.105901	174559.037994	56.051034
2781.465483	174339.550489	56.056039
2780.539278	174117.046422	56.061044
2779.941204	173896.052264	56.066049
2779.234376	173684.302165	56.071053
2778.379693	173464.575243	56.076058
2777.949721	173250.184128	56.081063
2777.178472	173029.490646	56.086068
2776.829549	172808.306119	56.091073
2776.223150	172592.955627	56.096077
2775.468993	172367.694610	56.101082
2774.997317	172140.528801	56.106087
2774.094517	171925.091975	56.111092
2773.530436	171706.163037	56.116097
2772.992142	171486.887171	56.121101
2772.077859	171268.694387	56.126106
2771.178603	171050.843544	56.131111
2770.555637	170827.933740	56.136116
2770.276938	170606.289296	56.141121
2769.455979	170399.649399	56.146125
2768.434754	170177.421393	56.151130
2768.133872	169956.534405	56.156135
2767.359954	169749.405858	56.161140
2766.668983	169526.093967	56.166145
2765.882603	169306.463457	56.171149
2765.146704	169089.904126	56.176154
2765.007605	168874.923127	56.181159
2763.938959	168658.384500	56.186164
2763.447964	168428.835301	56.191169
2762.720051	168225.738534	56.196173
2762.154669	168012.271967	56.201178
2761.585803	167785.868858	56.206183
2761.002106	167566.161060	56.211188
2760.724104	167344.150322	56.216193
2759.790450	167126.310927	56.221197
2758.838959	166900.206576	56.226202
2758.105647	166682.551329	56.231207
2757.589936	166469.337898	56.236212
2757.215944	166234.334897	56.241217
2756.038940	166020.854954	56.246221
2755.276977	165804.989814	56.251226
2754.707342	165584.678571	56.256231
2754.193612	165376.456692	56.261236
2753.730142	165153.737841	56.266241
2752.851857	164942.196472	56.271245
2752.130371	164724.892142	56.276250
2751.704060	164502.004825	56.281255
2750.961445	164283.701312	56.286260
2750.344201	164056.498332	56.291265
2749.352795	163847.373030	56.296269
2748.775138	163636.002773	56.301274
2748.429869	163413.806735	56.306279
2747.464777	163191.183493	56.311284
2747.048221	162970.134019	56.316289
2746.108019	162762.353515	56.321293
2745.252974	162545.438952	56.326298
2745.007449	162329.426204	56.331303
2743.856711	162118.428370	56.336308
2743.300369	161896.759518	56.341313
2743.086016	161689.152674	56.346317
2742.095651	161473.322388	56.351322
2741.504349	161256.000347	56.356327
2740.588636	161042.563547	56.361332
2740.367762	160825.002307	56.366337
2739.716699	160611.217157	56.371341
2739.297344	160400.955003	56.376346
2738.504589	160175.608594	56.381351
2737.209655	159961.796843	56.386356
2736.957193	159744.450051	56.391361
2736.206500	159538.509854	56.396365
2735.218107	159322.041469	56.401370
2735.240887	159098.202239	56.406375
2734.251237	158891.619212	56.411380
2733.702760	158673.387332	56.416385
2733.071476	158457.332998	56.421389
2732.229969	158237.271053	56.426394
2731.830784	158024.626169	56.431399
2730.801970	157817.075811	56.436404
2730.383303	157597.848040	56.441409
2729.760227	157381.581694	56.446413
2729.122031	157164.644977	56.451418
2728.451841	156937.311002	56.456423
2727.622780	156728.523724	56.461428
2727.147957	156501.527619	56.466433
2726.492773	156297.011694	56.471437
2726.031346	156068.756582	56.476442
2725.431348	155849.594603	56.481447
2724.532897	155639.603812	56.486452
2724.012982	155412.150927	56.491457
2723.378932	155194.829737	56.496461
2722.467108	154976.170928	56.501466
2721.813748	154755.103590	56.506471
2721.156131	154541.465461	56.511476
2720.534202	154313.769154	56.516481
2719.852651	154090.217613	56.521485
2719.535694	153877.300600	56.526490
2718.944934	153654.435463	56.531495
2718.061867	153437.624228	56.536500
2717.290930	153209.985149	56.541505
2716.804474	152987.665512	56.546509
2715.958313	152770.253917	56.551514
2715.311283	152544.848475	56.556519
2714.584811	152334.591380	56.561524
2714.269743	152103.548887	56.566529
2713.000692	151889.393742	56.571533
2712.323632	151665.600852	56.576538
2711.899588	151448.925631	56.581543
2710.984039	151237.651266	56.586548
2710.691503	151015.907399	56.591553
2710.023440	150805.495986	56.596557
2709.070307	150575.728862	56.601562
2708.217574	150359.400067	56.606567
2707.763382	150152.974101	56.611572
2707.510234	149920.026587	56.616577
2706.419431	149724.380811	56.621581
2705.424120	149506.517093	56.626586
2705.092522	149288.363156	56.631591
2704.255755	149085.772346	56.636596
2703.601894	148854.705523	56.641601
2703.066087	148651.137324	56.646605
2702.570516	148437.021848	56.651610
2702.069282	148223.684221	56.656615
2701.334313	147999.579347	56.661620
2700.621027	147777.913517	56.666625
2699.787057	147570.638277	56.671629
2698.728956	147363.097321	56.676634
2698.427425	147143.323070	56.681639
2697.704847	146940.800593	56.686644
2697.405155	146721.498987	56.691649
2696.406668	146502.038376	56.696653
2695.729279	146282.613191	56.701658
2695.359855	146074.008091	56.706663
2694.528823	145862.329736	56.711668
2693.850658	145644.256274	56.716673
2693.117693	145436.695971	56.721677
2692.403997	145222.547272	56.726682
2692.040853	145005.580811	56.731687
2691.411166	144795.705120	56.736692
2690.294152	144574.102073	56.741697
2689.768795	144364.541613	56.746701
2689.188901	144153.224375	56.751706
2688.571220	143933.472486	56.756711
2687.987126	143726.087197	56.761716
2687.350648	143511.083519	56.766721
2686.558891	143294.442111	56.771725
2685.794149	143079.640929	56.776730
2685.541160	142859.706109	56.781735
2684.837978	142655.869116	56.786740
2684.099464	142437.278553	56.791745
2683.077174	142215.978944	56.796749
2682.381570	142005.393363	56.801754
2682.177610	141786.956981	56.806759
2681.194664	141582.487409	56.811764
2681.104358	141366.157350	56.816769
2680.431819	141154.136258	56.821773
2679.442170	140925.045823	56.826778
2678.796519	140707.581528	56.831783
2677.927262	140484.868129	56.836788
2677.160548	140271.991239	56.841793
2676.606923	140064.533091	56.846797
2675.636609	139845.209973	56.851802
2675.310475	139637.283239	56.856807
2674.412883	139437.375467	56.861812
2674.029512	139216.671994	56.866817
2672.952168	138997.766601	56.871821
2672.313033	138795.352106	56.876826
2671.828395	138578.839710	56.881831
2670.887409	138369.271348	56.886836
2670.511373	138158.120360	56.891841
2669.904474	137947.366068	56.896845
2669.380358	137741.582076	56.901850
2668.529869	137523.689666	56.906855
2667.731914	137317.255865	56.911860
2667.297146	137096.256960	56.916865
2666.382795	136886.375313	56.921869
2665.637887	136683.152373	56.926874
2665.530238	136480.126806	56.931879
2664.808513	136264.546673	56.936884
2664.338800	136045.950346	56.941889
2663.318132	135832.979072	56.946893
2662.526723	135627.240844	56.951898
2662.185987	135412.719626	56.956903
2661.380206	135194.300663	56.961908
2660.639331	134978.668470	56.966913
2660.218679	134761.521163	56.971917
2659.612457	134558.592389	56.976922
2658.632380	134344.161868	56.981927
2658.179433	134129.947686	56.986932
2657.706668	133921.216579	56.991937
2656.899698	133709.353543	56.996941
2656.432216	133493.112252	57.001946
2656.146152	133264.550363	57.006951
2654.525943	133052.919507	57.011956
2653.964679	132837.512001	57.016961
2653.354380	132628.774428	57.021965
2652.878908	132420.269338	57.026970
2652.226156	132204.983295	57.031975
2651.266059	131983.116607	57.036980
2650.789180	131772.366221	57.041985
2650.047960	131570.025418	57.046989
2649.177394	131360.463447	57.051994
2648.888425	131138.284438	57.056999
2647.916542	130939.024587	57.062004
2647.477710	130727.219576	57.067009
2646.663606	130511.463933	57.072013
2645.865464	130314.770941	57.077018
2645.357239	130098.876808	57.082023
2644.642372	129879.410051	57.087028
2644.199557	129669.430070	57.092033
2643.133647	129470.932488	57.097037
2642.614426	129265.213008	57.102042
2642.012054	129047.308619	57.107047
2641.223130	128838.803923	57.112052
2640.880706	128630.351357	57.117057
2640.282004	128416.326784	57.122061
2639.600993	128208.189030	57.127066
2638.682853	127996.356912	57.132071
2638.153658	127784.319937	57.137076
2637.535667	127573.532258	57.142081
2636.798385	127376.224280	57.147085
2636.132968	127162.854995	57.152090
2635.328799	126940.437396	57.157095
2634.834501	126740.080090	57.162100
2633.757009	126529.327119	57.167105
2633.135569	126318.268876	57.172109
2632.516148	126114.721912	57.177114
2631.993078	125911.159806	57.182119
2631.704495	125702.120160	57.187124
2631.002008	125485.464716	57.192129
2630.051400	125280.162667	57.197133
2628.907846	125065.529761	57.202138
2628.628047	124861.399250	57.207143
2628.417147	124660.968759	57.212148
2627.518999	124446.590466	57.217153
2627.046933	124243.640529	57.222157
2626.259998	124031.927259	57.227162
2625.708838	123825.778790	57.232167
2624.774874	123616.444254	57.237172
2624.225187	123395.558789	57.242177
2623.361044	123200.077960	57.247181
2622.692669	122997.792444	57.252186
2622.469137	122777.186068	57.257191
2621.460493	122573.436787	57.262196
2620.368726	122353.096255	57.267201
2620.087850	122151.118613	57.272205
2619.273636	121948.941248	57.277210
2618.659366	121741.750382	57.282215
2617.743824	121534.968196	57.287220
2617.369200	121330.712328	57.292225
2616.561415	121137.509482	57.297229
2615.888394	120936.788617	57.302234
2615.588330	120724.405333	57.307239
2614.895917	120522.356493	57.312244
2613.773170	120312.950034	57.317249
2613.362016	120113.028473	57.322253
2612.755560	119906.230101	57.327258
2612.010423	119700.549496	57.332263
2611.452639	119498.840317	57.337268
2611.078376	119283.341878	57.342273
2610.474234	119085.569205	57.347277
2609.422505	118876.529164	57.352282
2609.169376	118669.933105	57.357287
2608.400535	118465.090925	57.362292
2607.533357	118254.041861	57.367297
2607.179539	118042.690589	57.372301
2606.649138	117830.240352	57.377306
2605.592792	117619.139259	57.382311
2604.764464	117412.472504	57.387316
2604.553423	117213.146158	57.392321
2603.616206	117001.965640	57.397325
2602.541194	116807.477446	57.402330
2602.403638	116589.938415	57.407335
2601.953279	116385.932900	57.412340
2601.237926	116176.168654	57.417345
2600.575034	115967.692699	57.422349
2599.564309	115761.805647	57.427354
2599.166889	115545.373245	57.432359
2598.328645	115336.563429	57.437364
2597.530766	115126.731991	57.442369
2596.938143	114919.725142	57.447373
2596.361507	114715.638690	57.452378
2595.894846	114502.401664	57.457383
2594.743219	114307.727471	57.462388
2594.164483	114088.148694	57.467393
2593.712473	113886.688970	57.472397
2592.699207	113691.550746	57.477402
2592.424495	113474.490594	57.482407
2591.622579	113285.454201	57.487412
2590.785728	113068.264607	57.492417
2590.296395	112863.897044	57.497421
2589.301582	112664.723510	57.502426
2589.095853	112450.898377	57.507431
2588.168951	112244.882650	57.512436
2587.165678	112044.089131	57.517441
2586.900259	111841.570530	57.522445
2586.135470	111651.090764	57.527450
2585.466894	111439.803803	57.532455
2584.483110	111244.283717	57.537460
2583.878159	111047.595242	57.542465
2583.248168	110836.687274	57.547469
2582.428957	110643.708869	57.552474
2581.936752	110437.403511	57.557479
2581.157449	110256.931304	57.562484
2580.782988	110061.378860	57.567489
2579.883673	109857.522427	57.572493
2579.039180	109665.342577	57.577498
2578.678795	109463.098788	57.582503
2577.666827	109270.378794	57.587508
2577.632209	109076.007148	57.592513
2576.745590	108877.642272	57.597517
2575.828997	108687.653280	57.602522
2575.395142	108484.946625	57.607527
2574.672855	108288.501003	57.612532
2573.942835	108094.026576	57.617537
2573.518911	107897.570854	57.622541
2572.786871	107704.217115	57.627546
2572.302128	107498.199172	57.632551
2571.198453	107303.133876	57.637556
2570.895251	107100.402451	57.642561
2570.591875	106908.822479	57.647565
2569.615786	106707.161455	57.652570
2569.096268	106504.293670	57.657575
2568.300953	106307.570039	57.662580
2567.871571	106099.915076	57.667585
2566.965833	105903.314856	57.672589
2565.986549	105708.481056	57.677594
2565.780862	105502.303593	57.682599
2564.764565	105302.958370	57.687604
2564.045412	105109.646351	57.692609
2563.570957	104911.976481	57.697613
2562.757617	104717.426262	57.702618
2562.386338	104514.052903	57.707623
2561.630814	104314.289518	57.712628
2561.183377	104110.792571	57.717633
2560.439126	103913.455560	57.722637
2559.627463	103714.442740	57.727642
2559.031390	103509.185424	57.732647
2558.183772	103315.921059	57.737652
2557.255460	103112.348892	57.742657
2556.775578	102918.389693	57.747661
2555.654690	102725.214449	57.752666
2555.863233	102525.248933	57.757671
2554.967198	102336.647158	57.762676
2554.364343	102123.986678	57.767681
2553.614385	101931.617235	57.772685
2553.086312	101743.109177	57.777690
2552.524424	101542.965408	57.782695
2551.502563	101333.671395	57.787700
2550.853475	101138.446499	57.792705
2550.619749	100940.358854	57.797709
2549.413132	100745.225859	57.802714
2549.164623	100546.147076	57.807719
2548.239790	100364.363239	57.812724
2547.699819	100158.011606	57.817729
2547.159551	99957.311335	57.822733
2546.324798	99762.045978	57.827738
2545.806754	99553.676772	57.832743
2545.086095	99360.197731	57.837748
2544.344953	99151.622341	57.842753
2543.887694	98962.125729	57.847757
2543.108858	98761.608826	57.852762
2542.569954	98562.283905	57.857767
2541.824900	98370.377978	57.862772
2541.167133	98160.431644	57.867777
2540.605166	97959.185707	57.872781
2539.700565	97762.589100	57.877786
2539.368957	97556.076691	57.882791
2538.283978	97368.317737	57.887796
2537.990898	97164.518557	57.892801
2537.071575	96962.637018	57.897805
2536.096372	96773.302273	57.902810
2535.402818	96569.049511	57.907815
2534.527997	96377.415600	57.912820
2534.388645	96184.546680	57.917825
2533.611545	95989.116182	57.922829
2532.897015	95795.383819	57.927834
2532.784280	95606.862391	57.932839
2531.579426	95408.958068	57.937844
2530.983781	95212.664784	57.942849
2530.571957	95008.820745	57.947853
2529.767812	94815.250868	57.952858
2529.328188	94616.657113	57.957863
2528.516526	94426.366378	57.962868
2527.906805	94233.066049	57.967873
2527.463423	94029.781166	57.972877
2526.298730	93838.019417	57.977882
2526.228622	93624.399170	57.982887
2524.782648	93435.354080	57.987892
2523.875271	93240.030742	57.992897
2523.635669	93048.339049	57.997901
2522.632493	92857.667836	58.002906
2522.294268	92658.006192	58.007911
2521.861436	92473.853087	58.012916
2521.644133	92278.920689	58.017921
2520.658759	92078.029002	58.022925
2519.692426	91888.907379	58.027930
2519.421479	91681.696822	58.032935
2518.492306	91496.385729	58.037940
2517.735799	91286.456658	58.042945
2517.317049	91091.549057	58.047949
2516.379326	90906.865757	58.052954
2515.590404	90703.350000	58.057959
2514.912392	90521.512464	58.062964
2514.435016	90333.905631	58.067969
2513.622232	90131.801074	58.072973
2512.806022	89949.997768	58.077978
2511.988383	89750.714569	58.082983
2512.012958	89556.092426	58.087988
2511.492336	89377.015774	58.092993
2510.847511	89177.898089	58.097997
2509.931942	88970.433672	58.103002
2509.318642	88770.666738	58.108007
2508.585721	88583.224978	58.113012
2507.881100	88386.858748	58.118017
2507.406527	88186.762022	58.123021
2506.287198	87995.374533	58.128026
2505.862906	87797.715234	58.133031
2505.303561	87611.241160	58.138036
2504.139330	87415.310398	58.143041
2503.426083	87221.328098	58.148045
2502.876787	87037.508855	58.153050
2502.052247	86844.709706	58.158055
2501.488500	86657.133507	58.163060
2500.760403	86468.292601	58.168065
2500.485305	86283.036496	58.173069
2499.675458	86095.119780	58.178074
2499.464184	85902.654824	58.183079
2498.274752	85713.632313	58.188084
2497.903193	85519.434149	58.193089
2497.169612	85330.324072	58.198093
2496.186280	85139.424744	58.203098
2495.723891	84954.877156	58.208103
2495.146127	84766.817099	58.213108
2494.352658	84574.595690	58.218113
2494.191819	84375.403547	58.223117
2493.465677	84192.429561	58.228122
2492.722217	83992.826404	58.233127
2492.074134	83803.003445	58.238132
2491.528165	83611.616693	58.243137
2490.805725	83408.601981	58.248141
2490.240502	83216.676190	58.253146
2489.521709	83015.776691	58.258151
2488.637169	82813.803485	58.263156
2487.769375	82627.066175	58.268161
2487.332118	82433.393177	58.273165
2486.376421	82243.762341	58.278170
2485.965939	82061.334652	58.283175
2485.333317	81869.247521	58.288180
2484.619591	81669.805036	58.293185
2483.845692	81476.280032	58.298189
2483.063080	81292.228391	58.303194
2482.561381	81099.268943	58.308199
2481.691865	80926.563766	58.313204
2481.187651	80731.089652	58.318209
2480.544212	80528.467180	58.323213
2479.798763	80352.281876	58.328218
2479.237006	80154.526382	58.333223
2478.393014	79972.734779	58.338228
2477.749016	79788.030841	58.343233
2477.481657	79600.067310	58.348237
2476.498063	79409.119903	58.353242
2476.302343	79211.836395	58.358247
2475.314269	79020.544161	58.363252
2474.076593	78834.275009	58.368257
2473.749444	78646.951095	58.373261
2473.015430	78466.972927	58.378266
2472.341407	78271.288801	58.383271
2471.613325	78092.238556	58.388276
2471.075791	77897.618834	58.393281
2470.475336	77714.871291	58.398285
2469.825374	77544.132874	58.403290
2469.512412	77353.030993	58.408295
2468.653033	77162.163668	58.413300
2467.867653	76970.093027	58.418305
2467.559396	76777.879031	58.423309
2466.856738	76595.582918	58.428314
2466.161938	76403.171849	58.433319
2465.484212	76209.903379	58.438324
2464.640046	76010.475591	58.443329
2464.294078	75825.562721	58.448333
2463.237854	75644.609433	58.453338
2463.281402	75445.320272	58.458343
2462.284585	75252.634612	58.463348
2461.653800	75067.186949	58.468353
2460.962322	74873.843584	58.473357
2460.034042	74683.205711	58.478362
2459.452232	74492.091715	58.483367
2458.778859	74294.552407	58.488372
2458.256543	74101.960446	58.493377
2457.619424	73913.961673	58.498381
2456.840291	73727.295017	58.503386
2456.137572	73528.936874	58.508391
2455.343858	73349.599672	58.513396
2454.599666	73158.398114	58.518401
2454.276920	72961.400445	58.523405
2453.616940	72779.166304	58.528410
2452.523460	72589.995014	58.533415
2451.238747	72399.944998	58.538420
2451.234537	72213.437647	58.543425
2450.613216	72028.178675	58.548429
2449.479734	71850.940729	58.553434
2449.192740	71661.005513	58.558439
2448.558446	71481.130035	58.563444
2447.916332	71307.261627	58.568449
2447.345762	71109.752311	58.573453
2446.419833	70934.033329	58.578458
2445.955792	70750.799822	58.583463
2445.387801	70559.622495	58.588468
2444.753964	70382.653408	58.593473
2444.494412	70189.150534	58.598477
2443.353611	70005.538153	58.603482
2442.787251	69813.206909	58.608487
2442.145852	69627.743524	58.613492
2441.261876	69436.243385	58.618497
2440.790471	69256.726156	58.623501
2439.828308	69069.731135	58.628506
2439.199292	68887.606631	58.633511
2438.760915	68704.005659	58.638516
2437.744125	68521.868130	58.643521
2437.359797	68335.123021	58.648525
2436.816928	68158.378464	58.653530
2436.204691	67971.795924	58.658535
2435.473477	67787.061056	58.663540
2434.797487	67599.186770	58.668545
2434.524699	67425.774529	58.673549
2433.636368	67232.988884	58.678554
2433.054449	67041.566196	58.683559
2431.794754	66859.649140	58.688564
2431.373992	66696.315411	58.693569
2431.118903	66441.712853	58.698573
2429.980712	66263.558076	58.703578
2429.599869	66073.193644	58.708583
2428.715840	65889.521869	58.713588
2428.447642	65695.864453	58.718593
2427.496171	65506.756296	58.723597
2426.829348	65326.481436	58.728602
2426.258676	65147.769953	58.733607
2425.413036	64954.991335	58.738612
2424.921223	64769.633247	58.743617
2424.632114	64582.835026	58.748621
2423.498596	64406.767710	58.753626
2422.649317	64216.931075	58.758631
2421.891165	64035.782838	58.763636
2421.302610	63852.217707	58.768641
2421.139038	63665.647012	58.773645
2420.262407	63485.132235	58.778650
2419.522425	63283.940381	58.783655
2418.529770	63114.140702	58.788660
2418.158158	62934.355576	58.793665
2417.803051	62741.576785	58.798669
2416.753792	62562.107196	58.803674
2415.654053	62382.026695	58.808679
2415.221105	62205.256042	58.813684
2414.407119	62018.348616	58.818689
2414.187703	61850.664171	58.823693
2413.227850	61671.313731	58.828698
2412.891395	61480.976997	58.833703
2411.786977	61305.108306	58.838708
2410.945513	61129.994645	58.843713
2411.104445	60948.767124	58.848717
2410.176654	60771.351843	58.853722
2409.882361	60587.758839	58.858727
2408.911469	60403.262888	58.863732
2408.192241	60215.195865	58.868737
2407.683705	60045.858160	58.873741
2407.210466	59863.138680	58.878746
2406.433339	59672.558105	58.883751
2405.698035	59490.038834	58.888756
2404.921557	59310.500138	58.893761
2404.568581	59116.988016	58.898765
2403.653894	58946.239715	58.903770
2403.280450	58760.857963	58.908775
2402.074988	58574.093060	58.913780
2401.558089	58395.874013	58.918785
2400.718721	58209.886257	58.923789
2400.288364	58038.194660	58.928794
2399.786946	57844.808679	58.933799
2398.914138	57668.437334	58.938804
2398.028968	57486.132677	58.943809
2397.896399	57301.343958	58.948813
2396.559106	57125.132785	58.953818
2396.164003	56944.358554	58.958823
2395.331949	56773.468632	58.963828
2394.390523	56597.226050	58.968833
2394.294920	56426.555276	58.973837
2393.278888	56243.904033	58.978842
2392.943269	56066.181312	58.983847
2392.375902	55896.964187	58.988852
2391.390458	55717.005134	58.993857
2391.306697	55525.312191	58.998861
2390.214332	55352.850591	59.003866
2389.201506	55166.521340	59.008871
2388.444388	54992.681416	59.013876
2388.017774	54826.578901	59.018881
2387.152641	54646.152739	59.023885
2386.337852	54471.579640	59.028890
2386.238954	54305.267037	59.033895
2385.463904	54124.050963	59.038900
2384.544197	53957.520502	59.043905
2384.323287	53780.831027	59.048909
2383.593141	53599.922451	59.053914
2382.817597	53432.947287	59.058919
2382.527046	53254.988409	59.063924
2381.827551	53073.420562	59.068929
2381.227724	52887.726126	59.073933
2380.240133	52712.431501	59.078938
2379.942859	52529.900339	59.083943
2378.686017	52342.232948	59.088948
2378.229608	52175.720563	59.093953
2377.362127	51986.444369	59.098957
2376.454354	51814.406270	59.103962
2376.103829	51651.712472	59.108967
2375.162685	51477.504024	59.113972
2374.756580	51304.250773	59.118977
2374.326362	51124.041975	59.123981
2373.108063	50958.867288	59.128986
2372.735017	50776.593331	59.133991
2372.027006	50608.490373	59.138996
2370.891302	50441.538749	59.144001
2370.656600	50277.025030	59.149005
2369.907344	50110.896886	59.154010
2369.310150	49936.871322	59.159015
2368.317428	49776.450007	59.164020
2368.044494	49604.310067	59.169025
2367.627717	49434.602996	59.174029
2366.594676	49273.945699	59.179034
2366.021164	49099.112867	59.184039
2365.664487	48925.175539	59.189044
2364.734950	48752.306721	59.194049
2364.384865	48573.741733	59.199053
2363.340288	48413.885179	59.204058
2362.970056	48234.693432	59.209063
2361.867700	48062.107309	59.214068
2361.321272	47895.599241	59.219073
2360.861663	47721.044335	59.224077
2360.094964	47556.593913	59.229082
2359.251616	47387.553978	59.234087
2358.871237	47219.212136	59.239092
2357.939957	47052.783471	59.244097
2357.380966	46886.023446	59.249101
2356.653799	46722.719603	59.254106
2356.222383	46539.548623	59.259111
2355.503563	46375.128597	59.264116
2354.978001	46203.980301	59.269121
2354.442493	46037.521249	59.274125
2353.642535	45865.099413	59.279130
2353.075067	45684.923416	59.284135
2352.412357	45516.970876	59.289140
2351.570749	45347.147567	59.294145
2350.940475	45175.494460	59.299149
2350.381649	45008.690578	59.304154
2349.583508	44829.980480	59.309159
2349.085319	44658.771677	59.314164
2348.063434	44485.140179	59.319169
2347.468702	44312.070416	59.324173
2346.683421	44156.900070	59.329178
2345.842125	43994.927574	59.334183
2345.331713	43823.437121	59.339188
2344.956322	43656.851166	59.344193
2344.535248	43494.253904	59.349197
2343.575370	43329.917183	59.354202
2343.151554	43157.040840	59.359207
2341.892470	42974.051968	59.364212
2341.133181	42820.271548	59.369217
2340.721863	42645.669278	59.374221
2339.603284	42489.312829	59.379226
2339.026446	42326.505332	59.384231
2338.889974	42167.887983	59.389236
2337.770471	42009.870579	59.394241
2337.222470	41851.408571	59.399245
2336.940967	41683.276036	59.404250
2336.067642	41523.191544	59.409255
2335.484056	41360.732272	59.414260
2334.744846	41194.914018	59.419265
2334.020379	41029.965195	59.424269
2333.348931	40874.251626	59.429274
2332.820462	40701.311292	59.434279
2332.491041	40540.737036	59.439284
2331.571448	40365.128703	59.444289
2330.826840	40208.493106	59.449293
2330.102885	40042.312139	59.454298
2329.750278	39881.022689	59.459303
2329.049596	39716.742932	59.464308
2328.337657	39542.914156	59.469313
2327.567231	39381.130761	59.474317
2326.742396	39219.858163	59.479322
2325.676294	39048.234178	59.484327
2325.510783	38890.814349	59.489332
2324.649688	38734.527600	59.494337
2324.341335	38567.861488	59.499341
2323.485531	38408.436935	59.504346
2323.109428	38246.596021	59.509351
2322.311650	38081.518154	59.514356
2321.639684	37914.505509	59.519361
2320.946655	37747.937891	59.524365
2320.476908	37588.470233	59.529370
2319.959555	37419.691826	59.534375
2319.138528	37253.527176	59.539380
2318.345842	37088.716847	59.544385
2317.824965	36916.693494	59.549389
2316.943220	36754.774931	59.554394
2316.150667	36585.563889	59.559399
2315.462708	36415.896644	59.564404
2314.663596	36262.800711	59.569409
2313.901769	36097.994013	59.574413
2313.284495	35935.777977	59.579418
2312.967282	35789.556056	59.584423
2312.429171	35624.044505	59.589428
2311.343626	35462.245020	59.594433
2310.927398	35300.417958	59.599437
2309.791306	35144.651812	59.604442
2308.970707	34977.438208	59.609447
2308.486589	34832.182828	59.614452
2307.722979	34682.941915	59.619457
2307.598638	34525.156952	59.624461
2306.802114	34366.906081	59.629466
2305.795317	34210.113283	59.634471
2305.522324	34043.153215	59.639476
2304.745254	33901.027814	59.644481
2303.911607	33738.377935	59.649485
2303.184605	33590.158614	59.654490
2302.590993	33439.044710	59.659495
2301.864328	33284.809747	59.664500
2301.046720	33125.785491	59.669505
2300.497010	32966.239061	59.674509
2299.938929	32826.356428	59.679514
2299.217101	32668.705650	59.684519
2298.366758	32518.747581	59.689524
2297.807997	32363.523635	59.694529
2296.906287	32215.165160	59.699533
2296.231322	32071.856601	59.704538
2295.896190	31914.241232	59.709543
2295.490400	31767.007074	59.714548
2294.950867	31618.354318	59.719553
2294.354227	31460.525063	59.724557
2293.481025	31312.640582	59.729562
2292.714961	31156.206545	59.734567
2292.286554	30998.972678	59.739572
2291.370634	30842.348724	59.744577
2290.687600	30690.381105	59.749581
2289.767664	30535.965559	59.754586
2289.135113	30387.810323	59.759591
2288.652605	30235.030900	59.764596
2287.964021	30092.464992	59.769601
2287.272487	29941.397325	59.774605
2286.723755	29794.725851	59.779610
2285.934379	29641.064467	59.784615
2285.203903	29491.756653	59.789620
2284.511635	29350.579732	59.794625
2284.145003	29192.079595	59.799629
2283.405517	29050.435477	59.804634
2282.751725	28901.742695	59.809639
2282.221911	28743.141625	59.814644
2281.252172	28594.356784	59.819649
2280.514127	28439.846141	59.824653
2279.443950	28304.334738	59.829658
2279.073645	28150.203427	59.834663
2278.660321	28014.218166	59.839668
2277.453802	27877.047421	59.844673
2276.969515	27722.240300	59.849677
2276.116755	27582.623237	59.854682
2275.724491	27439.395440	59.859687
2275.377089	27288.209370	59.864692
2274.312809	27152.006816	59.869697
2273.783058	27007.550353	59.874701
2273.113375	26871.567164	59.879706
2272.401869	26724.104553	59.884711
2272.011079	26582.471271	59.889716
2270.763538	26443.794249	59.894721
2270.161578	26295.396131	59.899725
2269.323480	26163.464020	59.904730
2268.809242	26029.915117	59.909735
2268.049301	25886.617404	59.914740
2267.190342	25760.362705	59.919745
2266.631710	25617.130825	59.924750
2266.193582	25497.700732	59.929754
2265.252568	25350.633700	59.934759
2264.539412	25215.784090	59.939764
2263.752998	25097.709814	59.944769
2263.229067	24965.091047	59.949774
2262.555709	24833.125030	59.954778
2261.614181	24705.845302	59.959783
2261.245446	24571.792512	59.964788
2260.337426	24453.354427	59.969793
2259.605321	24324.789341	59.974798
2259.137007	24204.339179	59.979802
2258.470412	24071.236166	59.984807
2257.664389	23950.159282	59.989812
2256.583792	23832.539232	59.994817
2255.934102	23705.381397	59.999822
2254.937782	23599.148778	60.004826
2254.202136	23480.934540	60.009831
2253.689045	23368.188584	60.014836
2252.750305	23256.063227	60.019841
2252.011265	23147.303859	60.024846
2251.113504	23053.052139	60.029850
2250.496866	22943.476246	60.034855
2249.826865	22837.483444	60.039860
2249.034663	22750.668602	60.044865
2248.638833	22641.015766	60.049870
2247.609110	22550.353112	60.054874
2246.899699	22453.495334	60.059879
2246.413618	22349.728675	60.064884
2245.918458	22251.529451	60.069889
2245.107984	22143.538063	60.074894
2244.849710	22049.754823	60.079898
2243.697280	21952.722671	60.084903
2243.082776	21856.335824	60.089908
2242.556226	21758.849917	60.094913
2242.375441	21654.206818	60.099918
2241.480599	21577.992249	60.104922
2240.999883	21473.907457	60.109927
2240.049730	21361.753745	60.114932
2239.045031	21269.824087	60.119937
2238.589757	21171.875605	60.124942
2237.785506	21075.185709	60.129946
2237.082794	20974.569380	60.134951
2236.710489	20879.103082	60.139956
2235.861004	20782.939537	60.144961
2235.307115	20687.268231	60.149966
2234.928744	20592.161858	60.154970
2233.994096	20496.623135	60.159975
2233.724607	20396.432527	60.164980
2232.642311	20305.302293	60.169985
2231.990943	20209.541263	60.174990
2231.398892	20124.525091	60.179994
2230.799888	20019.239513	60.184999
2230.173039	19923.716186	60.190004
2229.682602	19830.278875	60.195009
2229.025337	19713.473118	60.200014
2228.179525	19629.561961	60.205018
2227.821704	19535.615126	60.210023
2227.133364	19434.368396	60.215028
2226.563436	19340.912597	60.220033
2225.607915	19228.023011	60.225038
2225.065999	19143.693973	60.230042
2224.474813	19050.515302	60.235047
2223.383782	18936.716617	60.240052
2222.907071	18850.484174	60.245057
2222.608230	18757.100632	60.250062
2221.971122	18662.659477	60.255066
2221.288294	18550.911727	60.260071
2220.546761	18458.150885	60.265076
2220.007747	18348.697165	60.270081
2219.438955	18246.262664	60.275086
2218.556845	18159.216328	60.280090
2217.818459	18055.059043	60.285095
2216.941243	17945.288006	60.290100
2216.627123	17862.832661	60.295105
2216.134124	17763.452976	60.300110
2215.168848	17665.275301	60.305114
2214.675671	17556.767255	60.310119
2213.911420	17458.671793	60.315124
2212.995177	17361.451670	60.320129
2212.448662	17256.675378	60.325134
2211.638910	17180.112011	60.330138
2210.913717	17081.063736	60.335143
2210.369010	16979.557458	60.340148
2209.258191	16898.883702	60.345153
2208.821875	16801.611618	60.350158
2208.485926	16710.344723	60.355162
2207.905985	16617.733941	60.360167
2206.982296	16526.578046	60.365172
2206.500051	16435.837105	60.370177
2206.252504	16329.476077	60.375182
2205.120903	16235.909151	60.380186
2204.139178	16143.380774	60.385191
2203.956861	16056.056569	60.390196
2203.021933	15974.263520	60.395201
2202.533631	15879.343179	60.400206
2201.923952	15781.806391	60.405210
2201.179179	15689.307968	60.410215
2200.985843	15587.478215	60.415220
2200.074951	15497.501582	60.420225
2199.736054	15390.386178	60.425230
2198.924285	15302.141569	60.430234
2198.488151	15194.667920	60.435239
2197.896601	15095.545349	60.440244
2196.592377	14995.067616	60.445249
2196.166108	14897.785942	60.450254
2195.625128	14802.060549	60.455258
2195.155517	14705.929998	60.460263
2194.208178	14599.083360	60.465268
2193.745619	14509.134965	60.470273
2193.168863	14397.513752	60.475278
2191.987959	14307.212055	60.480282
2191.403242	14207.663777	60.485287
2191.036795	14104.630606	60.490292
2189.795659	14026.665313	60.495297
2188.982911	13930.006926	60.500302
2188.598217	13845.390093	60.505306
2187.632326	13750.743740	60.510311
2187.465048	13654.447484	60.515316
2186.504959	13576.957726	60.520321
2185.612148	13475.513388	60.525326
2185.153365	13389.933403	60.530330
2184.402100	13291.420976	60.535335
2183.961509	13203.895202	60.540340
2183.108065	13115.367558	60.545345
2182.753643	13024.703981	60.550350
2181.855811	12933.572881	60.555354
2181.275198	12848.855607	60.560359
2180.616065	12754.401113	60.565364
2179.588062	12668.911162	60.570369
2179.517819	12578.147715	60.575374
2179.185340	12482.779323	60.580378
2177.758797	12390.518643	60.585383
2177.362074	12297.505618	60.590388
2176.608046	12215.311508	60.595393
2175.614553	12124.580477	60.600398
2175.502423	12032.771705	60.605402
2174.950203	11953.050395	60.610407
2174.124491	11861.236639	60.615412
2173.467912	11777.465377	60.620417
2172.731021	11674.035159	60.625422
2171.941230	11593.864834	60.630426
2171.173942	11495.492314	60.635431
2170.604517	11399.797852	60.640436
2169.942997	11330.666994	60.645441
2169.011917	11233.042969	60.650446
2168.221133	11161.051437	60.655450
2167.625772	11073.873162	60.660455
2167.096010	10983.669538	60.665460
2166.519811	10912.445030	60.670465
2165.787072	10822.142716	60.675470
2165.299151	10749.516615	60.680474
2164.253237	10666.670806	60.685479
2163.859072	10576.157112	60.690484
2162.971574	10501.052020	60.695489
2162.072942	10408.865494	60.700494
2161.307146	10338.369505	60.705498
2160.608902	10267.072314	60.710503
2160.314629	10181.469877	60.715508
2159.172339	10121.351219	60.720513
2158.612053	10038.943753	60.725518
2157.705307	9971.487881	60.730522
2156.986580	9903.775790	60.735527
2156.430608	9821.326033	60.740532
2155.716863	9773.222908	60.745537
2155.010315	9706.196797	60.750542
2154.128565	9639.633805	60.755546
2153.141423	9576.032353	60.760551
2152.581925	9516.449778	60.765556
2152.264661	9460.033043	60.770561
2151.276417	9396.901691	60.775566
2150.633461	9328.123723	60.780570
2149.805605	9281.071617	60.785575
2149.423936	9212.766048	60.790580
2148.780507	9157.437763	60.795585
2148.279660	9096.612877	60.800590
2147.305919	9032.692150	60.805594
2146.482210	8975.328961	60.810599
2145.841724	8918.800355	60.815604
2145.129651	8871.066134	60.820609
2144.483748	8812.137576	60.825614
2143.798353	8757.053223	60.830618
2142.954196	8711.572685	60.835623
2142.606847	8642.262089	60.840628
2142.064542	8601.494756	60.845633
2141.269176	8543.202524	60.850638
2140.601025	8494.341870	60.855642
2139.942776	8439.964837	60.860647
2139.454538	8377.984138	60.865652
2138.789918	8338.371051	60.870657
2138.192830	8259.240261	60.875662
2137.343240	8208.015086	60.880666
2136.446427	8157.768087	60.885671
2135.840675	8106.120033	60.890676
2135.153495	8058.978714	60.895681
2134.442875	8006.923188	60.900686
2134.090820	7961.138656	60.905690
2133.484603	7902.429369	60.910695
2132.925190	7851.730699	60.915700
2132.093418	7795.507291	60.920705
2131.640708	7747.148352	60.925710
2130.935418	7693.357672	60.930714
2130.052893	7643.875968	60.935719
2129.414920	7573.829843	60.940724
2128.708194	7529.117384	60.945729
2128.196819	7485.308361	60.950734
2127.306927	7441.174819	60.955738
2126.588398	7385.513202	60.960743
2126.028492	7324.900972	60.965748
2125.448052	7280.818408	60.970753
2124.956401	7226.424880	60.975758
2123.827535	7181.403326	60.980762
2123.257553	7135.422267	60.985767
2122.615459	7076.843762	60.990772
2121.859333	7036.530821	60.995777
2121.177191	6984.676715	61.000782
2120.732975	6943.018559	61.005786
2119.976320	6889.744034	61.010791
2119.500452	6843.870132	61.015796
2118.417119	6796.917954	61.020801
2117.837877	6750.573914	61.025806
2117.638594	6700.234289	61.030810
2116.519577	6656.080498	61.035815
2116.132848	6606.903398	61.040820
2115.428627	6565.282798	61.045825
2114.767117	6506.432489	61.050830
2113.927304	6462.120122	61.055834
2113.483722	6418.558304	61.060839
2113.067815	6370.092182	61.065844
2112.045343	6329.914242	61.070849
2111.401332	6277.706041	61.075854
2110.738898	6244.747517	61.080858
2110.043078	6191.566002	61.085863
2109.670056	6141.170188	61.090868
2108.672918	6100.147409	61.095873
2108.396121	6051.171185	61.100878
2107.484404	5994.322550	61.105882
2106.948651	5944.769416	61.110887
2106.539986	5900.991385	61.115892
2105.649012	5853.723197	61.120897
2105.267218	5797.188972	61.125902
2104.219425	5750.561536	61.130906
2103.345337	5705.352102	61.135911
2102.928523	5651.656354	61.140916
2102.367247	5615.923312	61.145921
2101.888370	5559.370997	61.150926
2101.050856	5510.210407	61.155930
2100.366896	5463.423657	61.160935
2099.736265	5412.641439	61.165940
2098.820811	5367.923345	61.170945
2098.416643	5324.086900	61.175950
2098.117547	5278.785858	61.180954
2097.005397	5232.921172	61.185959
2096.616964	5184.288903	61.190964
2095.763624	5131.925990	61.195969
2095.309956	5084.031710	61.200974
2094.966929	5025.909452	61.205978
2093.838510	4979.043789	61.210983
2093.352887	4926.997709	61.215988
2092.319700	4883.217949	61.220993
2091.872416	4839.032487	61.225998
2091.348704	4787.591961	61.231002
2090.837153	4736.523041	61.236007
2090.583365	4684.002198	61.241012
2089.776941	4636.749227	61.246017
2089.118796	4581.537964	61.251022
2088.491721	4526.402915	61.256026
2087.568916	4474.604453	61.261031
2086.995264	4416.303553	61.266036
2085.954511	4366.464249	61.271041
2085.226789	4308.306179	61.276046
2084.446365	4254.100099	61.281050
2083.347367	4210.472436	61.286055
2083.006168	4163.634047	61.291060
2081.795885	4130.266661	61.296065
2081.241329	4083.969589	61.301070
2080.973983	4036.946798	61.306074
2079.962389	4014.510718	61.311079
2079.580301	3960.213032	61.316084
2079.119215	3927.674186	61.321089
2078.393546	3881.678611	61.326094
2077.934606	3837.711134	61.331098
2077.248567	3782.873028	61.336103
2076.690373	3732.794466	61.341108
2075.931439	3696.713426	61.346113
2075.337487	3648.574263	61.351118
2074.818500	3602.364113	61.356122
2073.822716	3569.635566	61.361127
2073.393729	3507.115628	61.366132
2072.349130	3465.252630	61.371137
2071.737646	3423.848652	61.376142
2070.931261	3377.802023	61.381146
2070.435075	3349.151328	61.386151
2070.042906	3301.169795	61.391156
2069.101042	3266.813954	61.396161
2068.298963	3211.183595	61.401166
2067.874090	3174.447298	61.406170
2067.273184	3130.082056	61.411175
2066.973094	3082.891621	61.416180
2065.975574	3037.226893	61.421185
2065.343796	2992.665971	61.426190
2065.118356	2952.820605	61.431194
2063.853591	2904.663432	61.436199
2063.491667	2861.585370	61.441204
2062.419676	2811.904765	61.446209
2062.152828	2764.093720	61.451214
2061.572402	2711.002835	61.456218
2060.618132	2683.523697	61.461223
2060.227366	2634.747265	61.466228
2059.071931	2591.166904	61.471233
2058.462049	2540.927261	61.476238
2058.117634	2497.742975	61.481242
2057.292859	2458.677247	61.486247
2056.610245	2419.589668	61.491252
2055.958513	2381.097763	61.496257
2055.281101	2342.397952	61.501262
2054.553360	2300.582555	61.506266
2053.735938	2258.097272	61.511271
2053.457309	2215.765495	61.516276
2052.858728	2174.999766	61.521281
2051.906466	2132.481040	61.526286
2051.816179	2085.835656	61.531290
2050.784615	2039.965684	61.536295
2050.353176	1990.971605	61.541300
2048.889698	1963.416608	61.546305
2048.901964	1909.200643	61.551310
2048.217584	1864.659022	61.556314
2047.189927	1841.087133	61.561319
2046.705471	1793.065187	61.566324
2045.807234	1755.644167	61.571329
2045.152896	1707.797605	61.576334
2044.839213	1676.161160	61.581338
2044.127187	1634.090229	61.586343
2044.011744	1589.282324	61.591348
2042.762776	1550.463537	61.596353
2042.250650	1504.132445	61.601358
2041.592170	1471.491908	61.606362
2040.671741	1430.642635	61.611367
2040.499890	1386.754085	61.616372
2039.383045	1345.802045	61.621377
2038.569979	1304.516295	61.626382
2038.155299	1260.548447	61.631386
2037.407573	1221.748559	61.636391
2037.232583	1178.167459	61.641396
2036.070428	1136.816729	61.646401
2035.400616	1097.084843	61.651406
2034.675463	1051.393130	61.656410
2034.154224	1012.913846	61.661415
2033.928804	966.382536	61.666420
2033.213243	930.867294	61.671425
2032.368405	884.557449	61.676430
2031.347885	841.888511	61.681434
2030.695174	809.962067	61.686439
2029.944649	756.582416	61.691444
2029.251184	740.415647	61.696449
2028.858296	692.779312	61.701454
2027.971118	661.009728	61.706458
2027.099079	632.225394	61.711463
2026.863656	590.740881	61.716468
2026.128085	556.516759	61.721473
2025.561028	519.067713	61.726478
2024.587092	472.523018	61.731482
2024.123885	450.871016	61.736487
2023.085815	405.872216	61.741492
2022.541721	380.938919	61.746497
2021.889044	348.930916	61.751502
2021.034552	316.034620	61.756506
2020.110716	286.826768	61.761511
2020.095354	256.256093	61.766516
2019.210701	224.291975	61.771521
2018.254138	196.420520	61.776526
2017.655003	156.839990	61.781530
2016.710992	141.625364	61.786535
2016.172330	108.894951	61.791540
2015.464500	81.696791	61.796545
2014.778272	53.028190	61.801550
2014.266632	31.838594	61.806554
2013.141537	14.647903	61.811559
2012.530179	-3.551929	61.816564
2010.692079	5.528150	61.821569
2008.479090	41.009863	61.826574
2007.994243	38.118616	61.831578
2007.949328	49.981873	61.836583
2007.519747	39.634319	61.841588
2007.821951	46.060090	61.846593
2007.377200	42.017286	61.851598
2006.524279	48.789465	61.856602
2005.575197	63.530992	61.861607
2004.983188	52.569788	61.866612
2003.940784	63.051238	61.871617
2002.646345	65.693957	61.876622
2002.416857	61.424463	61.881626
2001.566024	67.739203	61.886631
2001.458137	61.979745	61.891636
2001.604909	72.233701	61.896641
2000.523419	69.576744	61.901646
1999.722780	67.463042	61.906650
1999.119008	76.215969	61.911655
1998.930878	60.381485	61.916660
1997.935055	63.816254	61.921665
1996.947690	63.348915	61.926670
1996.703671	56.248975	61.931674
1995.809058	64.808498	61.936679
1994.976499	61.294251	61.941684
1994.435008	66.550318	61.946689
1993.747326	68.544133	61.951694
1992.892369	66.106971	61.956698
1992.019772	65.382772	61.961703
1991.781938	65.439301	61.966708
1991.603574	65.343951	61.971713
1990.934907	70.443754	61.976718
1989.800387	66.289210	61.981722
1988.954895	71.641887	61.986727
1989.011246	64.480299	61.991732
1988.213546	67.704737	61.996737
1987.364797	66.666995	62.001742
1986.720249	63.502285	62.006746
1985.720924	67.401062	62.011751
1985.125403	58.214349	62.016756
1984.462995	63.905165	62.021761
1983.693623	65.689147	62.026766
1983.069143	62.012995	62.031770
1982.034965	68.795666	62.036775
1981.959005	62.529054	62.041780
1981.983329	63.488864	62.046785
1980.705438	68.572888	62.051790
1980.000371	63.788322	62.056794
1978.928291	73.373703	62.061799
1979.194701	61.420549	62.066804
1978.393236	72.111834	62.071809
1977.204516	66.480035	62.076814
1977.174344	70.668536	62.081818
1976.462522	71.766907	62.086823
1975.425209	64.085458	62.091828
1974.523584	63.830028	62.096833
1973.924083	70.442424	62.101838
1974.213423	71.097170	62.106842
1972.933746	71.760989	62.111847
1972.121422	66.076250	62.116852
1971.294714	66.728500	62.121857
1970.426246	69.858471	62.126862
1970.759407	66.204810	62.131866
1969.917789	69.621889	62.136871
1969.069943	68.798725	62.141876
1968.073893	71.844736	62.146881
1967.075257	72.907307	62.151886
1966.922833	64.712918	62.156890
1966.349977	75.355625	62.161895
1965.296751	72.762917	62.166900
1965.504633	72.390316	62.171905
1964.474584	69.662202	62.176910
1963.578737	67.692683	62.181914
1962.630450	67.712070	62.186919
1962.142381	59.196562	62.191924
1961.927612	70.750213	62.196929
1961.421215	70.579143	62.201934
1960.235600	62.509793	62.206938
1959.743704	68.951813	62.211943
1959.202291	68.009126	62.216948
1958.577814	66.395015	62.221953
1957.998986	73.090320	62.226958
1957.636863	71.775527	62.231962
1956.246261	69.870911	62.236967
1955.948057	66.185129	62.241972
1955.636921	62.746685	62.246977
1954.429768	71.662828	62.251982
1953.766737	69.636510	62.256986
1952.610336	77.929785	62.261991
1952.949635	67.033072	62.266996
1952.078712	68.668647	62.272001
1951.026297	73.387669	62.277006
1950.603559	64.124430	62.282010
1949.921728	68.585061	62.287015
1948.851885	67.592253	62.292020
1948.255738	65.685148	62.297025
1947.582152	69.162298	62.302030
1947.548977	68.354897	62.307034
1946.698144	73.747570	62.312039
1946.058705	59.977739	62.317044
1945.327572	66.798173	62.322049
1944.621552	70.378763	62.327054
1944.379586	66.910328	62.332058
1943.594451	72.833717	62.337063
1943.118919	64.501585	62.342068
1941.861496	67.384294	62.347073
1940.331693	66.838057	62.352078
1940.374510	64.136404	62.357082
1940.380323	73.141482	62.362087
1939.529160	67.915352	62.367092
1938.725170	76.696216	62.372097
1938.050114	69.904482	62.377102
1937.231050	67.376325	62.382106
1936.574854	78.479329	62.387111
1936.128143	63.660507	62.392116
1935.317436	64.186477	62.397121
1934.555298	67.537465	62.402126
1934.450276	69.153328	62.407130
1933.763339	76.582765	62.412135
1933.298075	67.382853	62.417140
1932.141009	67.645192	62.422145
1931.010606	69.528837	62.427150
1930.465154	64.552375	62.432154
1929.936200	69.790907	62.437159
1929.164322	63.974920	62.442164
1929.266729	67.541942	62.447169
1928.456046	67.591477	62.452174
1927.712078	63.284482	62.457178
1927.216537	76.347039	62.462183
1926.489162	64.713104	62.467188
1925.574699	65.892725	62.472193
1924.418900	69.568420	62.477198
1924.049411	69.315907	62.482202
1923.600491	66.306022	62.487207
1922.849010	66.047414	62.492212
1922.315142	65.571189	62.497217
1921.523126	65.951863	62.502222
1921.325215	67.409150	62.507226
1920.693303	69.400932	62.512231
1920.061245	56.157988	62.517236
1919.061356	70.674539	62.522241
1917.870188	70.698776	62.527246
1917.398036	57.669258	62.532250
1916.642257	67.116453	62.537255
1916.152844	65.515950	62.542260
1915.452458	63.639314	62.547265
1914.784066	63.874896	62.552270
1914.627077	61.773460	62.557274
1914.278169	75.123156	62.562279
1913.770735	69.352716	62.567284
1912.740872	68.958583	62.572289
1911.236949	72.049253	62.577294
1910.810527	61.788396	62.582298
1909.973222	66.765086	62.587303
1909.897532	58.598630	62.592308
1909.047268	64.682367	62.597313
1908.450985	64.954559	62.602318
1907.958816	60.278055	62.607322
1907.338821	63.219082	62.612327
1906.906192	57.681763	62.617332
1905.459252	63.933102	62.622337
1904.736595	63.651408	62.627342
1904.322802	58.395463	62.632346
1903.405151	64.487176	62.637351
1903.510086	53.842932	62.642356
1902.677426	56.202599	62.647361
1902.054740	58.147804	62.652366
1901.760996	55.687279	62.657370
1900.200345	57.462173	62.662375
1899.445457	53.603881	62.667380
1899.227404	52.434967	62.672385
1898.092894	61.245924	62.677390
1897.743032	52.050757	62.682394
1896.971572	60.126600	62.687399
1896.494201	55.006661	62.692404
1896.209020	50.914070	62.697409
1895.476026	55.746206	62.702414
1895.291448	52.824125	62.707418
1894.380769	64.846548	62.712423
1893.233288	62.037887	62.717428
1892.563959	69.154846	62.722433
1891.890557	65.370635	62.727438
1891.507664	57.766721	62.732442
1890.565231	71.802539	62.737447
1890.087609	70.970917	62.742452
1888.750088	64.334372	62.747457
1888.129763	66.818763	62.752462
1888.240930	51.900179	62.757466
1887.217707	66.016127	62.762471
1886.491082	65.217237	62.767476
1885.964576	63.049156	62.772481
1885.404300	61.637617	62.777486
1885.403460	55.147381	62.782490
1884.578959	64.848299	62.787495
1883.449978	58.456729	62.792500
1882.892695	58.022802	62.797505
1881.853355	55.981143	62.802510
1881.897858	59.524120	62.807514
1881.025971	61.501305	62.812519
1879.611065	58.036582	62.817524
1878.699806	67.330384	62.822529
1878.394323	68.551480	62.827534
1878.224339	57.297844	62.832538
1877.336597	61.314909	62.837543
1876.819062	65.094564	62.842548
1876.591199	60.460474	62.847553
1876.036925	57.682561	62.852558
1874.971327	57.937554	62.857562
1873.792348	59.014811	62.862567
1873.430467	57.338418	62.867572
1873.044841	64.372498	62.872577
1872.352226	72.408808	62.877582
1872.316577	56.031969	62.882586
1870.545074	64.914018	62.887591
1869.527479	62.313660	62.892596
1869.247622	63.001441	62.897601
1868.521056	66.184513	62.902606
1868.043319	57.036094	62.907610
1867.109380	64.366476	62.912615
1866.862938	56.182662	62.917620
1866.748987	58.438320	62.922625
1866.224374	78.407981	62.927630
1865.601198	64.288423	62.932634
1864.160907	72.277393	62.937639
1863.416191	68.358944	62.942644
1862.789647	65.668789	62.947649
1862.279201	64.188729	62.952654
1862.067652	63.586710	62.957658
1860.557494	71.805126	62.962663
1859.901610	64.390020	62.967668
1859.718930	61.721028	62.972673
1858.803486	63.827243	62.977678
1858.489457	62.591464	62.982682
1858.068532	57.779230	62.987687
1857.541722	67.925386	62.992692
1856.557057	73.712005	62.997697
1855.375059	65.542598	63.002702
1855.009898	59.747041	63.007706
1854.365292	68.688920	63.012711
1853.956268	71.990950	63.017716
1853.695594	63.552209	63.022721
1852.188762	60.281241	63.027726
1851.481936	68.849305	63.032730
1850.458309	60.820564	63.037735
1850.103218	65.024781	63.042740
1849.869505	66.715161	63.047745
1848.958104	74.702855	63.052750
1848.879566	70.042032	63.057754
1847.906909	59.401371	63.062759
1846.925393	68.261160	63.067764
1846.196401	71.933713	63.072769
1845.434237	76.317313	63.077774
1845.349037	69.980055	63.082778
1844.789295	71.301099	63.087783
1844.213887	62.056500	63.092788
1843.196360	62.604843	63.097793
1842.320983	72.408021	63.102798
1841.679496	66.131205	63.107802
1840.981426	74.033060	63.112807
1840.708102	63.511556	63.117812
1840.330975	68.205055	63.122817
1838.870866	72.009801	63.127822
1838.031707	62.564022	63.132826
1837.377130	59.315793	63.137831
1837.314911	65.815742	63.142836
1836.524948	64.603764	63.147841
1836.129363	70.417487	63.152846
1835.548881	57.131401	63.157850
1834.986399	64.993475	63.162855
1833.853103	71.743783	63.167860
1833.255831	58.909369	63.172865
1832.545109	63.458238	63.177870
1832.238165	58.430723	63.182874
1831.771453	65.807087	63.187879
1830.556476	59.871545	63.192884
1830.094387	66.235838	63.197889
1829.401760	65.713367	63.202894
1829.250390	53.509222	63.207898
1828.348094	58.328490	63.212903
1826.785789	57.630353	63.217908
1826.408028	59.606291	63.222913
1826.003962	68.189263	63.227918
1825.764618	50.143665	63.232922
1825.145641	65.625663	63.237927
1823.552772	67.190573	63.242932
1822.634211	61.628646	63.247937
1821.686039	60.288218	63.252942
1822.564080	52.868038	63.257946
1821.757745	60.781306	63.262951
1821.038658	60.394412	63.267956
1820.645310	59.550746	63.272961
1818.951796	56.653955	63.277966
1818.625231	54.208920	63.282970
1817.694532	57.771910	63.287975
1817.082947	57.807134	63.292980
1816.947605	54.944132	63.297985
1816.293666	65.646097	63.302990
1816.194035	58.384506	63.307994
1814.962127	58.721647	63.312999
1814.037540	59.238699	63.318004
1813.573899	66.196132	63.323009
1812.865726	67.925060	63.328014
1812.559613	59.140036	63.333018
1811.628364	58.405377	63.338023
1810.655796	60.586502	63.343028
1810.235337	61.906611	63.348033
1809.511668	69.297337	63.353038
1808.925586	58.071091	63.358042
1807.459514	63.152213	63.363047
1807.291066	67.793034	63.368052
1806.854918	63.290504	63.373057
1806.046669	60.617632	63.378062
1806.193698	64.052279	63.383066
1805.361781	63.473120	63.388071
1804.314910	63.708738	63.393076
1803.301626	61.473170	63.398081
1802.518673	65.751385	63.403086
1802.502728	62.537176	63.408090
1801.590050	64.961073	63.413095
1801.296497	61.238198	63.418100
1800.405787	60.274376	63.423105
1799.363955	58.861165	63.428110
1798.939612	52.961669	63.433114
1798.645608	58.663275	63.438119
1797.770732	51.763667	63.443124
1796.873018	50.275669	63.448129
1796.125043	61.692775	63.453134
1795.763265	59.239951	63.458138
1795.440731	58.028921	63.463143
1794.829198	60.683125	63.468148
1793.438201	58.501529	63.473153
1792.811829	62.134027	63.478158
1792.652604	51.810115	63.483162
1791.703953	64.773742	63.488167
1791.027921	59.702807	63.493172
1789.827555	58.804996	63.498177
1788.842435	62.585321	63.503182
1789.307965	60.328432	63.508186
1788.399264	65.397479	63.513191
1787.718248	56.979358	63.518196
1787.288802	53.473941	63.523201
1786.796174	65.224320	63.528206
1786.096401	49.445463	63.533210
1784.625299	64.765374	63.538215
1783.957723	67.182862	63.543220
1783.737393	62.268027	63.548225
1783.066092	64.308403	63.553230
1782.671434	57.484518	63.558234
1782.200140	58.685831	63.563239
1780.859735	61.797894	63.568244
1780.109813	57.821541	63.573249
1779.679363	63.221638	63.578254
1779.040822	50.465355	63.583258
1778.981981	60.812478	63.588263
1778.401827	59.878415	63.593268
1777.135444	55.367953	63.598273
1776.209292	57.166549	63.603278
1775.790638	60.275630	63.608282
1775.610849	57.556809	63.613287
1774.381299	62.127748	63.618292
1773.525805	52.237566	63.623297
1772.857044	62.859569	63.628302
1772.683304	55.023317	63.633306
1772.212164	60.841281	63.638311
1771.499411	60.041614	63.643316
1770.642802	54.248452	63.648321
1769.402132	64.191892	63.653326
1769.021034	54.416322	63.658330
1768.603834	52.274158	63.663335
1768.136562	62.153947	63.668340
1768.186935	63.837166	63.673345
1766.648323	55.904856	63.678350
1766.202981	49.222672	63.683354
1765.521247	53.782768	63.688359
1764.140228	58.122660	63.693364
1763.500521	60.476567	63.698369
1762.815713	62.229924	63.703374
1762.653796	59.865664	63.708378
1762.033734	67.397342	63.713383
1761.638692	67.853399	63.718388
1761.251705	59.949427	63.723393
1759.978765	64.862124	63.728398
1759.199759	58.946345	63.733402
1758.497764	68.285269	63.738407
1757.963474	71.586633	63.743412
1757.753980	56.648722	63.748417
1756.626891	65.013576	63.753422
1756.024815	60.284060	63.758426
1755.208024	59.484829	63.763431
1754.696977	60.212569	63.768436
1754.628670	61.663077	63.773441
1753.023792	67.214789	63.778446
1752.735473	55.717353	63.783450
1751.882069	62.503853	63.788455
1751.365721	62.705545	63.793460
1751.314510	62.029125	63.798465
1750.201427	60.997182	63.803470
1749.999092	58.353270	63.808474
1749.181313	65.196831	63.813479
1748.482712	64.112913	63.818484
1747.738537	56.884251	63.823489
1746.638198	62.369763	63.828494
1746.189315	65.006799	63.833498
1745.446960	63.080135	63.838503
1744.756730	64.293257	63.843508
1744.368778	56.571421	63.848513
1743.333212	61.705599	63.853518
1742.382503	62.517254	63.858522
1741.964014	63.632170	63.863527
1741.421090	68.118785	63.868532
1741.621627	66.613789	63.873537
1740.228264	67.162515	63.878542
1739.647593	65.053061	63.883546
1738.707008	58.559825	63.888551
1738.454079	63.579823	63.893556
1738.075868	61.817028	63.898561
1736.503886	65.528839	63.903566
1736.051668	56.437655	63.908570
1735.602835	59.644661	63.913575
1735.083596	64.214456	63.918580
1734.727220	53.676795	63.923585
1733.029293	62.006306	63.928590
1732.695929	57.398177	63.933594
1731.898653	64.824789	63.938599
1731.556053	58.650401	63.943604
1731.433523	57.735930	63.948609
1730.682730	61.810103	63.953614
1729.777864	53.294911	63.958618
1728.964000	60.526209	63.963623
1728.014346	63.085518	63.968628
1728.038073	61.584725	63.973633
1726.955392	61.069014	63.978638
1726.007032	62.694188	63.983642
1725.442198	61.436995	63.988647
1724.891112	63.932052	63.993652
1724.802518	57.530657	63.998657
1724.005080	68.609272	64.003662
1722.819564	54.476254	64.008666
1721.971338	62.153943	64.013671
1721.210447	60.240718	64.018676
1721.074691	58.720638	64.023681
1720.493883	64.306328	64.028686
1720.320214	60.037966	64.033690
1719.763305	70.084671	64.038695
1718.451134	65.902967	64.043700
1717.946342	60.500387	64.048705
1717.074106	65.499257	64.053710
1716.163918	69.960300	64.058714
1715.121526	69.585323	64.063719
1714.516551	69.129577	64.068724
1714.697853	55.612121	64.073729
1713.685548	59.021333	64.078734
1713.667864	68.438944	64.083738
1713.075883	64.512546	64.088743
1711.461859	68.656674	64.093748
1710.775614	58.284403	64.098753
1710.485349	64.874681	64.103758
1710.244479	62.758399	64.108762
1709.552456	69.231117	64.113767
1708.416848	66.366392	64.118772
1708.228404	64.573496	64.123777
1707.357329	75.805239	64.128782
1706.414071	63.180447	64.133786
1705.531465	58.669463	64.138791
1704.616177	69.649829	64.143796
1704.744441	63.720516	64.148801
1703.858890	61.379827	64.153806
1703.793097	58.362040	64.158810
1703.140735	66.704876	64.163815
1701.868026	63.057195	64.168820
1701.252662	55.893736	64.173825
1700.786930	68.582899	64.178830
1699.798074	61.233883	64.183834
1698.785503	59.912394	64.188839
1698.265487	66.461858	64.193844
1698.176208	65.322232	64.198849
1697.533574	55.720107	64.203854
1696.948707	57.987270	64.208858
1696.344773	68.938831	64.213863
1695.332762	61.503782	64.218868
1694.993528	56.839033	64.223873
1693.950406	67.168665	64.228878
1693.125024	61.530432	64.233882
1692.336605	67.798206	64.238887
1692.032053	74.334881	64.243892
1691.703574	59.163536	64.248897
1690.768086	58.614356	64.253902
1690.423257	58.559738	64.258906
1689.210550	63.723448	64.263911
1688.428825	64.279231	64.268916
1688.348407	56.349258	64.273921
1687.522833	58.274336	64.278926
1686.376321	48.451348	64.283930
1685.587988	56.773632	64.288935
1684.607970	61.902656	64.293940
1684.411301	56.603666	64.298945
1683.937198	65.225460	64.303950
1684.388608	53.856840	64.308954
1683.754685	63.906851	64.313959
1682.498621	64.099742	64.318964
1682.159665	56.463081	64.323969
1680.639935	68.574737	64.328974
1679.530550	66.219067	64.333978
1679.104284	57.304236	64.338983
1678.752496	64.795534	64.343988
1678.058770	60.082109	64.348993
1677.654917	57.791623	64.353998
1676.806422	63.156684	64.359002
1675.783253	59.007248	64.364007
1675.359746	67.912085	64.369012
1675.196304	63.409089	64.374017
1674.400993	60.591138	64.379022
1673.634801	54.478984	64.384026
1672.483481	68.681598	64.389031
1671.723882	68.352576	64.394036
1671.573989	56.782915	64.399041
1670.730335	57.441663	64.404046
1670.445537	59.076054	64.409050
1670.430950	64.776423	64.414055
1669.025065	73.710825	64.419060
1668.488768	61.569017	64.424065
1667.620453	66.191447	64.429070
1666.733553	62.001720	64.434074
1665.811657	60.083690	64.439079
1665.492656	62.106420	64.444084
1664.963444	50.358527	64.449089
1664.269525	64.888640	64.454094
1663.849597	66.105645	64.459098
1663.270063	60.091018	64.464103
1662.463478	65.017083	64.469108
1662.018814	58.822277	64.474113
1661.323678	63.452570	64.479118
1660.047495	58.270817	64.484122
1659.405996	58.830633	64.489127
1658.572496	66.212135	64.494132
1658.609570	55.912277	64.499137
1657.932884	67.159302	64.504142
1656.833734	59.927853	64.509146
1656.425704	64.359021	64.514151
1655.515865	62.597213	64.519156
1655.433989	62.840218	64.524161
1654.632447	61.671697	64.529166
1653.407878	63.138106	64.534170
1653.149051	65.267377	64.539175
1652.152651	59.874332	64.544180
1652.076180	67.568377	64.549185
1651.030873	65.368321	64.554190
1650.353974	63.522836	64.559194
1649.567143	66.445860	64.564199
1649.019486	60.569853	64.569204
1648.985818	58.289044	64.574209
1647.830173	66.221842	64.579214
1646.819906	61.113792	64.584218
1646.652350	59.366665	64.589223
1646.122284	63.097954	64.594228
1645.859898	58.189146	64.599233
1643.834987	59.972511	64.604238
1643.461842	67.112610	64.609242
1643.375431	56.090623	64.614247
1643.052578	67.200520	64.619252
1642.124690	59.105326	64.624257
1640.972302	61.158967	64.629262
1640.375990	63.378754	64.634266
1640.281000	60.914236	64.639271
1639.125239	68.095504	64.644276
1638.084205	59.289437	64.649281
1637.282276	69.165316	64.654286
1636.917236	52.770291	64.659290
1636.694722	61.575204	64.664295
1635.999788	66.972411	64.669300
1635.825497	60.413193	64.674305
1634.534283	69.909006	64.679310
1633.904599	57.064402	64.684314
1633.311937	60.657987	64.689319
1632.562071	63.444033	64.694324
1632.167434	58.047484	64.699329
1631.064130	62.110942	64.704334
1630.573694	64.491026	64.709338
1630.094115	66.302826	64.714343
1629.215471	67.291635	64.719348
1628.186370	52.368889	64.724353
1627.409090	60.437455	64.729358
1627.148882	61.966591	64.734362
1626.712963	61.034704	64.739367
1626.038404	69.213586	64.744372
1626.368871	59.102327	64.749377
1624.983744	69.150245	64.754382
1624.249632	64.904381	64.759386
1623.870218	57.622402	64.764391
1622.177894	58.529020	64.769396
1621.684460	57.002263	64.774401
1621.121270	63.292679	64.779406
1620.599693	60.594860	64.784410
1620.271429	63.741768	64.789415
1619.377735	59.867019	64.794420
1618.873514	55.201699	64.799425
1618.208652	60.549155	64.804430
1617.487171	59.810212	64.809434
1617.049667	55.518329	64.814439
1615.737106	53.981364	64.819444
1615.046740	47.141408	64.824449
1614.577623	61.828827	64.829454
1614.263329	50.408494	64.834458
1613.902132	53.917470	64.839463
1612.857660	57.202338	64.844468
1612.025506	46.982959	64.849473
1611.431180	61.747856	64.854478
1610.714271	58.223763	64.859482
1610.378478	58.561932	64.864487
1608.898601	55.778650	64.869492
1608.621368	60.518605	64.874497
1607.983929	56.611058	64.879502
1607.882265	54.506881	64.884506
1607.442990	56.305074	64.889511
1605.805181	60.246859	64.894516
1605.482326	49.863349	64.899521
1604.437883	58.044345	64.904526
1604.763340	52.658377	64.909530
1604.180158	51.199874	64.914535
1603.058989	57.819455	64.919540
1602.479109	55.526339	64.924545
1601.787033	64.221750	64.929550
1600.261232	49.014562	64.934554
1599.514225	50.235443	64.939559
1598.938750	59.263778	64.944564
1598.886120	49.670835	64.949569
1598.261443	53.666201	64.954574
1598.477543	51.191471	64.959578
1597.567612	56.666522	64.964583
1596.507108	61.941563	64.969588
1595.957970	58.367840	64.974593
1594.698807	61.289600	64.979598
1594.086187	51.077257	64.984602
1593.754794	54.004443	64.989607
1592.843322	63.547371	64.994612
1592.709899	54.311661	64.999617
1591.648097	54.505273	65.004622
1590.679232	46.718285	65.009626
1590.478413	45.193952	65.014631
1589.816096	52.373270	65.019636
1589.531540	48.739270	65.024641
1588.208992	50.371270	65.029646
1587.415671	51.306406	65.034650
1586.999569	54.384664	65.039655
1586.234210	52.306839	65.044660
1586.065208	55.581615	65.049665
1584.932356	62.435691	65.054670
1584.107356	55.079588	65.059674
1583.684984	53.549753	65.064679
1583.089081	56.279455	65.069684
1582.694902	61.318098	65.074689
1581.586823	59.731937	65.079694
1580.873963	67.314634	65.084698
1580.701952	60.795293	65.089703
1579.947416	56.658721	65.094708
1579.465120	54.565610	65.099713
1578.319868	59.949890	65.104718
1577.550453	61.084218	65.109722
1577.475916	57.510587	65.114727
1576.101869	58.957990	65.119732
1575.631659	56.401381	65.124737
1574.598752	57.132795	65.129742
1574.127716	65.750511	65.134746
1574.017817	56.643008	65.139751
1573.345884	60.243455	65.144756
1573.230292	55.823856	65.149761
1571.879253	64.283900	65.154766
1571.345026	60.768809	65.159770
1571.043543	51.298586	65.164775
1569.493341	63.433235	65.169780
1568.902799	49.545415	65.174785
1568.392673	57.652732	65.179790
1568.143722	62.042467	65.184794
1567.665837	57.372252	65.189799
1566.422133	56.248631	65.194804
1565.900458	56.619799	65.199809
1565.141286	55.540355	65.204814
1564.614627	52.685131	65.209818
1564.367018	57.108975	65.214823
1563.205082	62.225730	65.219828
1562.497981	58.585102	65.224833
1561.699528	65.039333	65.229838
1561.267354	56.487889	65.234842
1560.371188	48.996743	65.239847
1559.242095	53.423033	65.244852
1558.810528	51.633468	65.249857
1558.633606	60.483466	65.254862
1558.235276	57.349315	65.259866
1557.907622	56.688238	65.264871
1557.291380	61.522528	65.269876
1556.200070	59.195373	65.274881
1555.765587	61.855612	65.279886
1554.537876	60.329008	65.284890
1553.652309	56.840895	65.289895
1552.957620	60.500104	65.294900
1552.870403	47.943595	65.299905
1552.114115	55.297282	65.304910
1551.771784	51.122536	65.309914
1550.915790	50.586618	65.314919
1549.767506	53.381257	65.319924
1550.026181	52.631673	65.324929
1548.716304	54.433218	65.329934
1547.860612	58.429049	65.334938
1547.105873	52.178784	65.339943
1546.474661	59.291602	65.344948
1546.446770	52.306304	65.349953
1545.423146	55.091450	65.354958
1544.884420	50.917161	65.359962
1544.360918	51.079836	65.364967
1543.721353	50.265308	65.369972
1542.991241	45.154735	65.374977
1541.811848	48.312316	65.379982
1541.451601	56.025706	65.384986
1541.235378	49.915768	65.389991
1540.007770	59.062820	65.394996
1539.148661	49.233716	65.400001
1538.372831	62.313031	65.405006
1537.963075	49.904484	65.410010
1537.728653	54.272388	65.415015
1537.284699	57.677509	65.420020
1536.519054	55.458036	65.425025
1535.905559	59.971343	65.430030
1534.940797	62.466561	65.435034
1533.906274	50.140865	65.440039
1532.996084	51.744144	65.445044
1532.702125	47.366525	65.450049
1532.316750	57.420967	65.455054
1531.874818	59.135149	65.460058
1531.323805	45.489647	65.465063
1530.036577	61.193362	65.470068
1529.663415	54.931079	65.475073
1529.250790	58.448466	65.480078
1528.468118	60.756604	65.485082
1527.444478	55.257337	65.490087
1526.817533	58.833114	65.495092
1526.500635	60.193542	65.500097
1525.980692	58.596335	65.505102
1524.701600	62.653978	65.510106
1524.019190	51.588760	65.515111
1523.497306	64.007268	65.520116
1523.297685	53.813855	65.525121
1522.677372	60.526930	65.530126
1521.412179	60.723395	65.535130
1520.908473	62.691300	65.540135
1520.190422	67.489337	65.545140
1520.014370	59.043663	65.550145
1519.174752	57.259601	65.555150
1518.472486	61.955860	65.560154
1517.951515	54.721810	65.565159
1516.833022	65.446843	65.570164
1516.221823	57.010123	65.575169
1515.309687	60.402223	65.580174
1514.521340	61.797553	65.585178
1514.448516	54.537326	65.590183
1514.097592	64.146156	65.595188
1513.802321	60.208085	65.600193
1512.168993	54.993166	65.605198
1511.465010	62.199359	65.610202
1511.464820	51.662354	65.615207
1510.524917	59.528243	65.620212
1509.835719	59.796647	65.625217
1508.941643	58.111115	65.630222
1508.501828	54.976966	65.635226
1508.095939	59.806833	65.640231
1506.841410	66.033615	65.645236
1506.081123	59.219458	65.650241
1505.276172	60.080810	65.655246
1504.902901	60.269090	65.660250
1505.404130	63.787956	65.665255
1504.288219	54.553054	65.670260
1503.382041	55.801191	65.675265
1502.960440	58.441465	65.680270
1501.890905	52.791777	65.685274
1501.162707	48.173496	65.690279
1500.130036	61.302297	65.695284
1499.639302	53.526254	65.700289
1498.982464	54.066610	65.705294
1498.284936	60.722641	65.710298
1498.208553	51.698621	65.715303
1497.084000	58.078805	65.720308
1496.659167	61.751830	65.725313
1496.112503	45.413197	65.730318
1495.752804	60.506204	65.735322
1494.557663	50.018207	65.740327
1493.556579	58.514281	65.745332
1493.316488	44.716893	65.750337
1492.914325	53.854505	65.755342
1491.500410	53.829337	65.760346
1490.931663	52.230225	65.765351
1490.557195	59.686718	65.770356
1490.319918	48.907676	65.775361
1489.756119	53.806411	65.780366
1488.760595	58.481026	65.785370
1488.427089	50.048495	65.790375
1487.174451	57.256230	65.795380
1485.860244	50.106249	65.800385
1485.685045	60.658381	65.805390
1485.549052	60.446854	65.810394
1484.655653	49.849980	65.815399
1484.317920	51.123978	65.820404
1483.778854	56.243866	65.825409
1482.443434	59.743154	65.830414
1481.169575	58.792868	65.835418
1481.005957	51.722653	65.840423
1480.451533	58.922589	65.845428
1480.291379	54.567464	65.850433
1479.882443	60.829115	65.855438
1478.924685	58.585299	65.860442
1478.248104	55.480232	65.865447
1477.463668	57.023313	65.870452
1476.830187	53.359838	65.875457
1476.072175	51.673918	65.880462
1475.005061	52.425810	65.885466
1474.691322	53.878063	65.890471
1474.227427	56.055464	65.895476
1474.068465	46.240352	65.900481
1472.768514	59.931196	65.905486
1471.894524	51.732488	65.910490
1471.592291	46.770525	65.915495
1470.338384	43.880721	65.920500
1469.873168	48.429831	65.925505
1469.469916	51.098542	65.930510
1468.943548	57.815274	65.935514
1469.030535	55.954329	65.940519
1467.827827	57.771891	65.945524
1467.177679	48.902133	65.950529
1466.472870	54.066574	65.955534
1465.498516	50.835248	65.960538
1464.853350	54.291390	65.965543
1463.698901	58.690064	65.970548
1463.695551	55.063993	65.975553
1463.618787	57.589984	65.980558
1462.005223	61.830411	65.985562
1461.584178	50.298121	65.990567
1460.926253	66.911329	65.995572
1460.926543	53.348311	66.000577
1459.344875	55.458098	66.005582
1458.409324	51.655680	66.010586
1458.148858	49.898811	66.015591
1457.644430	53.667956	66.020596
1457.117266	53.316550	66.025601
1456.027633	46.982713	66.030606
1455.256469	42.648102	66.035610
1455.127518	39.052612	66.040615
1454.169902	53.734814	66.045620
1453.947061	42.374650	66.050625
1452.639740	51.467068	66.055630
1451.753974	63.053024	66.060634
1451.517339	51.375491	66.065639
1451.272432	43.112929	66.070644
1450.754931	48.019134	66.075649
1449.568096	52.224413	66.080654
1449.063718	57.215213	66.085658
1448.642326	50.922517	66.090663
1447.769180	63.689688	66.095668
1446.948250	49.964094	66.100673
1446.259871	55.775436	66.105678
1445.525624	55.011074	66.110682
1445.232793	46.219104	66.115687
1444.734131	57.954710	66.120692
1443.990881	43.155211	66.125697
1443.108533	48.551349	66.130702
1442.361635	52.821453	66.135706
1442.037088	46.853221	66.140711
1440.664242	49.707239	66.145716
1440.145913	45.866567	66.150721
1439.815690	53.872435	66.155726
1439.731520	57.301631	66.160730
1438.911931	52.316125	66.165735
1437.903875	61.504951	66.170740
1437.058821	50.676008	66.175745
1436.303701	49.303403	66.180750
1435.470180	55.110774	66.185754
1434.911468	50.977816	66.190759
1433.844385	66.230983	66.195764
1433.852743	61.657944	66.200769
1433.729822	61.001698	66.205774
1432.597627	58.723017	66.210778
1431.936157	58.320000	66.215783
1431.063457	64.078032	66.220788
1430.509233	52.932081	66.225793
1430.301472	53.071511	66.230798
1428.694834	54.786912	66.235802
1428.415680	48.535397	66.240807
1427.878516	54.998198	66.245812
1427.676904	53.255728	66.250817
1426.825144	54.201680	66.255822
1425.690360	58.292271	66.260826
1425.583416	51.433800	66.265831
1424.739542	58.740123	66.270836
1423.985094	54.846320	66.275841
1423.071718	53.302261	66.280846
1422.681474	62.045482	66.285850
1422.099913	46.782537	66.290855
1420.979603	57.879318	66.295860
1420.225963	60.684586	66.300865
1419.819628	46.950402	66.305870
1419.343025	53.577698	66.310874
1418.594299	52.036244	66.315879
1418.173003	51.048588	66.320884
1417.675166	49.273539	66.325889
1416.537095	51.243462	66.330894
1415.866449	54.316748	66.335898
1415.582528	41.081465	66.340903
1414.294107	52.042419	66.345908
1413.292306	51.105185	66.350913
1413.259847	52.387719	66.355918
1412.730223	54.908730	66.360922
1412.643522	48.822818	66.365927
1411.864882	50.685034	66.370932
1410.614348	55.321209	66.375937
1410.157452	52.527088	66.380942
1409.294440	56.591291	66.385946
1408.676180	50.370982	66.390951
1407.769623	61.996024	66.395956
1407.472958	49.617093	66.400961
1407.381727	49.461456	66.405966
1406.280625	55.289766	66.410970
1405.743907	51.194494	66.415975
1404.798555	55.852243	66.420980
1404.428635	51.646316	66.425985
1403.127429	57.025742	66.430990
1402.497601	58.416452	66.435994
1402.453845	50.255641	66.440999
1401.813980	55.396734	66.446004
1400.916937	54.919183	66.451009
1399.953352	53.593714	66.456014
1398.731982	54.298214	66.461018
1399.051361	55.902217	66.466023
1398.283867	60.607283	66.471028
1397.520333	51.215787	66.476033
1396.243878	54.294490	66.481038
1395.731152	53.148414	66.486042
1395.535656	51.842251	66.491047
1394.888465	55.329535	66.496052
1394.413143	51.668999	66.501057
1393.489964	50.613710	66.506062
1392.650865	57.534760	66.511066
1392.806628	51.631940	66.516071
1391.863678	60.469377	66.521076
1390.470494	51.095273	66.526081
1390.352870	55.733698	66.531086
1389.510657	53.200530	66.536090
1389.420939	52.693727	66.541095
1388.024549	56.838973	66.546100
1386.864767	51.779875	66.551105
1386.898318	55.185761	66.556110
1386.178586	56.015964	66.561114
1385.817698	51.660474	66.566119
1385.511015	53.850441	66.571124
1384.671955	59.133788	66.576129
1383.950574	46.153778	66.581134
1382.828353	54.697834	66.586138
1381.949110	50.855006	66.591143
1381.246934	57.213430	66.596148
1380.801485	60.166070	66.601153
1380.550589	56.807762	66.606158
1380.380989	52.556496	66.611162
1379.670937	42.007216	66.616167
1378.689223	55.852398	66.621172
1377.826940	53.074388	66.626177
1376.833079	50.195354	66.631182
1376.046256	60.318513	66.636186
1375.880796	49.115107	66.641191
1375.254212	58.392578	66.646196
1373.872146	50.271002	66.651201
1373.206259	59.411918	66.656206
1372.651836	56.225169	66.661210
1372.103935	48.868659	66.666215
1371.333335	68.880752	66.671220
1371.009024	65.758818	66.676225
1371.077685	53.425507	66.681230
1370.319682	58.008956	66.686234
1369.435755	48.542949	66.691239
1368.531957	54.565639	66.696244
1367.218830	54.979944	66.701249
1366.603903	53.136922	66.706254
1366.168023	64.722052	66.711258
1365.962912	47.158192	66.716263
1365.531020	53.167596	66.721268
1364.862836	48.264343	66.726273
1363.885010	44.436817	66.731278
1362.907000	49.710399	66.736282
1362.601571	49.150132	66.741287
1361.959029	57.982327	66.746292
1360.839916	60.284529	66.751297
1360.445281	55.272081	66.756302
1359.844027	56.671325	66.761306
1359.737120	53.017988	66.766311
1358.317909	58.386835	66.771316
1357.469525	58.479228	66.776321
1357.277179	55.257342	66.781326
1356.628503	59.533536	66.786330
1356.486758	52.408671	66.791335
1355.078988	56.334829	66.796340
1354.645527	52.294122	66.801345
1354.585032	53.951703	66.806350
1353.276267	46.799653	66.811354
1352.584656	52.506953	66.816359
1351.607003	49.080831	66.821364
1351.390359	49.904256	66.826369
1350.925019	47.903793	66.831374
1349.751513	48.343148	66.836378
1349.169695	51.391366	66.841383
1348.444094	52.525330	66.846388
1348.169450	54.575609	66.851393
1347.380920	55.130633	66.856398
1346.452648	58.379866	66.861402
1346.250481	46.274498	66.866407
1345.287203	53.817573	66.871412
1344.605229	53.500970	66.876417
1343.734168	51.156294	66.881422
1343.006217	54.187295	66.886426
1342.638218	58.497543	66.891431
1342.403997	64.648370	66.896436
1341.518405	60.351917	66.901441
1340.652019	56.956877	66.906446
1340.132732	57.706986	66.911450
1339.876070	53.690881	66.916455
1338.416300	65.416552	66.921460
1337.724675	66.167349	66.926465
1337.250553	61.409684	66.931470
1336.522718	63.437286	66.936474
1336.472735	55.429511	66.941479
1335.549906	57.231952	66.946484
1334.553321	54.007618	66.951489
1333.844123	51.433927	66.956494
1333.502601	57.385628	66.961498
1333.336610	56.447428	66.966503
1332.666909	57.813000	66.971508
1331.510296	57.744224	66.976513
1331.199855	51.443998	66.981518
1329.531067	54.190028	66.986522
1329.003030	49.387126	66.991527
1328.054023	49.239391	66.996532
1328.205148	52.944870	67.001537
1328.346487	50.157290	67.006542
1327.244123	53.231468	67.011546
1326.552144	44.861517	67.016551
1325.849828	52.398602	67.021556
1324.600814	51.414895	67.026561
1323.983091	48.781733	67.031566
1322.998156	61.986053	67.036570
1322.709723	62.860847	67.041575
1322.279100	57.601942	67.046580
1321.826362	54.451082	67.051585
1320.865326	52.699684	67.056590
1319.760360	59.320481	67.061594
1319.422394	56.918888	67.066599
1319.004457	54.817159	67.071604
1318.411881	55.214304	67.076609
1317.354736	51.114984	67.081614
1316.316952	50.766537	67.086618
1316.181760	46.063353	67.091623
1315.440603	50.535373	67.096628
1315.377527	49.891385	67.101633
1314.685437	47.807776	67.106638
1313.884003	51.268578	67.111642
1313.487517	45.947785	67.116647
1312.316137	57.930388	67.121652
1311.249685	52.719549	67.126657
1310.885150	50.182776	67.131662
1310.388771	56.263615	67.136666
1310.099376	50.883436	67.141671
1308.829562	60.382732	67.146676
1308.328460	46.723612	67.151681
1308.230357	43.553095	67.156686
1307.094038	54.514867	67.161690
1306.153154	43.040821	67.166695
1305.240338	50.655783	67.171700
1305.620757	55.016715	67.176705
1305.012519	49.444026	67.181710
1303.808539	54.454736	67.186714
1303.132273	45.160823	67.191719
1302.362625	52.688516	67.196724
1301.610330	49.738935	67.201729
1300.880920	51.321960	67.206734
1300.086029	54.116540	67.211738
1299.778378	51.172546	67.216743
1299.419267	49.628357	67.221748
1298.383089	62.347655	67.226753
1297.572620	63.433790	67.231758
1296.864083	58.361803	67.236762
1296.980423	57.278564	67.241767
1295.977276	51.369684	67.246772
1294.668640	53.352649	67.251777
1294.370878	49.938034	67.256782
1293.673666	55.818002	67.261786
1293.245797	48.789101	67.266791
1292.594183	52.153207	67.271796
1291.474102	60.275744	67.276801
1291.043732	57.145925	67.281806
1290.108848	55.459922	67.286810
1290.573823	58.438671	67.291815
1289.375166	53.452173	67.296820
1288.248568	50.688249	67.301825
1288.134710	48.498152	67.306830
1287.524602	49.838921	67.311834
1286.397347	50.588911	67.316839
1285.656136	50.203119	67.321844
1285.274262	56.734862	67.326849
1284.952925	53.937285	67.331854
1283.724584	52.140082	67.336858
1283.045784	45.105988	67.341863
1282.177057	48.704230	67.346868
1281.665853	51.694972	67.351873
1281.757014	48.237064	67.356878
1280.636589	52.705731	67.361882
1280.292731	47.364880	67.366887
1279.293126	55.890721	67.371892
1278.564330	48.170477	67.376897
1278.133030	49.096572	67.381902
1276.922552	54.825211	67.386906
1276.622835	51.939069	67.391911
1276.136390	43.874586	67.396916
1275.772905	56.790151	67.401921
1275.202333	51.725734	67.406926
1274.315852	56.874323	67.411930
1273.450136	49.660658	67.416935
1272.360795	46.005397	67.421940
1271.545148	46.723752	67.426945
1271.464736	44.242153	67.431950
1270.518583	48.632435	67.436954
1270.347471	48.241013	67.441959
1269.556278	50.854182	67.446964
1268.488230	57.496295	67.451969
1268.242967	54.106245	67.456974
1267.386963	56.296713	67.461978
1266.648768	40.629995	67.466983
1265.914994	54.402339	67.471988
1264.789145	55.099595	67.476993
1264.684831	46.476291	67.481998
1264.186653	56.881995	67.487002
1263.934826	47.599500	67.492007
1262.594091	49.752171	67.497012
1262.233242	50.811463	67.502017
1261.676517	44.811167	67.507022
1260.715927	57.824616	67.512026
1259.792523	50.110852	67.517031
1259.198373	41.409183	67.522036
1258.757677	51.218883	67.527041
1258.798177	48.795132	67.532046
1257.853383	53.544775	67.537050
1256.984111	51.718078	67.542055
1256.170780	50.926234	67.547060
1255.055228	54.056759	67.552065
1254.881276	55.691530	67.557070
1254.197595	53.252425	67.562074
1253.420890	47.045854	67.567079
1252.994733	48.113959	67.572084
1252.221897	49.822051	67.577089
1251.321022	46.102557	67.582094
1250.557987	52.165104	67.587098
1250.252310	47.467430	67.592103
1249.848400	53.224951	67.597108
1249.046768	55.279802	67.602113
1248.379889	47.233584	67.607118
1247.234838	54.568195	67.612122
1246.826683	55.356915	67.617127
1246.375371	56.499194	67.622132
1245.754166	48.092671	67.627137
1245.143805	50.395026	67.632142
1244.533089	54.770119	67.637146
1243.841467	45.249517	67.642151
1242.678812	55.511230	67.647156
1241.842915	53.083189	67.652161
1242.030546	52.410095	67.657166
1241.296517	56.193695	67.662170
1240.140403	47.900463	67.667175
1239.753753	51.933654	67.672180
1239.314246	46.907198	67.677185
1239.069907	41.069336	67.682190
1237.812744	56.962125	67.687194
1237.115279	46.456117	67.692199
1236.292460	56.062043	67.697204
1235.229566	52.810797	67.702209
1234.509885	44.732573	67.707214
1233.941729	48.097394	67.712218
1233.909668	49.268153	67.717223
1233.269292	48.121847	67.722228
1232.852305	46.253640	67.727233
1231.782823	36.281445	67.732238
1230.290907	47.985389	67.737242
1230.163030	51.085366	67.742247
1229.887625	49.316861	67.747252
1229.171217	53.044947	67.752257
1228.551245	46.932331	67.757262
1227.580907	52.683809	67.762266
1227.255977	50.606427	67.767271
1226.562278	50.219615	67.772276
1225.601166	54.305373	67.777281
1225.340276	50.028304	67.782286
1223.835715	56.981596	67.787290
1223.731653	51.541671	67.792295
1223.618004	54.540138	67.797300
1222.492348	50.139954	67.802305
1222.018617	53.693076	67.807310
1221.227277	63.399798	67.812314
1221.035211	59.188703	67.817319
1219.903079	53.336662	67.822324
1219.364272	56.487655	67.827329
1218.644103	45.496481	67.832334
1217.592943	57.155760	67.837338
1217.573048	45.984693	67.842343
1216.952991	50.503091	67.847348
1215.547980	52.585466	67.852353
1214.765263	47.009906	67.857358
1214.049742	56.781403	67.862362
1213.425799	45.878356	67.867367
1213.248656	48.176012	67.872372
1212.746923	50.736077	67.877377
1212.223239	53.498839	67.882382
1211.517476	61.520057	67.887386
1210.693912	53.402780	67.892391
1210.154308	46.837084	67.897396
1209.402338	48.247148	67.902401
1208.455722	53.363015	67.907406
1207.582915	54.933500	67.912410
1207.464271	55.920144	67.917415
1206.922227	56.048135	67.922420
1205.928793	62.421705	67.927425
1205.461349	51.313448	67.932430
1204.893981	53.945143	67.937434
1204.482305	52.753763	67.942439
1203.212641	48.887035	67.947444
1202.219365	52.430038	67.952449
1201.744467	52.349568	67.957454
1201.478069	61.266572	67.962458
1201.311955	54.892311	67.967463
1200.191355	54.490572	67.972468
1199.800584	56.752178	67.977473
1198.682155	49.608247	67.982478
1197.258445	60.644898	67.987482
1197.100619	58.326153	67.992487
1196.674334	51.444226	67.997492
1195.466362	53.589577	68.002497
1195.692125	45.738284	68.007502
1195.182875	52.868126	68.012506
1193.981173	54.315328	68.017511
1193.471885	57.599816	68.022516
1192.728468	50.347864	68.027521
1192.428074	48.516538	68.032526
1191.253134	56.805578	68.037530
1190.695703	47.550946	68.042535
1190.316022	51.663074	68.047540
1189.194134	64.480342	68.052545
1188.396974	50.329593	68.057550
1187.800984	56.502488	68.062554
1187.595308	53.053959	68.067559
1186.802222	54.909206	68.072564
1186.573859	57.944288	68.077569
1185.493301	56.343640	68.082574
1184.628799	55.452416	68.087578
1184.028625	50.249011	68.092583
1183.411534	55.443455	68.097588
1182.826405	58.688037	68.102593
1182.404830	55.965655	68.107598
1181.481457	55.098327	68.112602
1181.191972	57.967039	68.117607
1180.327432	55.754694	68.122612
1179.392260	60.467177	68.127617
1179.021316	46.419898	68.132622
1178.139545	56.547084	68.137626
1177.630956	44.892879	68.142631
1176.733944	52.729745	68.147636
1175.723692	53.274997	68.152641
1175.577542	42.845920	68.157646
1174.992776	55.251493	68.162650
1174.638348	44.931099	68.167655
1173.714069	42.272690	68.172660
1172.535111	53.125729	68.177665
1172.634924	49.294910	68.182670
1171.785097	54.072908	68.187674
1171.162630	41.801127	68.192679
1170.454635	41.958326	68.197684
1169.664981	51.302006	68.202689
1169.735596	50.478032	68.207694
1168.237765	54.903187	68.212698
1167.590045	47.138694	68.217703
1167.302300	48.977677	68.222708
1166.012782	50.357030	68.227713
1165.335027	45.875830	68.232718
1164.873075	47.323081	68.237722
1164.456933	47.798188	68.242727
1163.601784	52.879058	68.247732
1163.183676	54.644052	68.252737
1162.230620	47.674703	68.257742
1161.685912	48.699959	68.262746
1161.288096	40.118636	68.267751
1160.799737	47.094906	68.272756
1159.061108	56.586867	68.277761
1159.208279	49.623731	68.282766
1158.344923	50.934853	68.287770
1158.007891	46.426892	68.292775
1157.435865	43.080567	68.297780
1156.432965	53.242702	68.302785
1156.155296	52.414813	68.307790
1155.324912	58.115497	68.312794
1154.471097	47.134987	68.317799
1154.068571	48.738240	68.322804
1153.350268	60.140410	68.327809
1152.126939	46.901032	68.332814
1151.024605	49.387499	68.337818
1150.320557	42.191581	68.342823
1150.268183	49.015045	68.347828
1149.506266	54.305733	68.352833
1149.419644	45.922956	68.357838
1149.176118	54.472501	68.362842
1148.446846	49.478699	68.367847
1147.513536	47.689435	68.372852
1146.557300	49.291977	68.377857
1145.527382	42.894325	68.382862
1144.500124	49.037647	68.387866
1144.598963	42.188180	68.392871
1144.262211	48.577200	68.397876
1143.409827	45.623078	68.402881
1142.712027	40.411532	68.407886
1141.819683	50.300932	68.412890
1141.255120	47.047669	68.417895
1140.860369	51.541705	68.422900
1139.935862	45.742556	68.427905
1139.155914	40.821775	68.432910
1138.440434	53.718260	68.437914
1137.946764	49.449875	68.442919
1137.548257	47.839818	68.447924
1136.106811	51.817976	68.452929
1135.786804	43.539503	68.457934
1135.532402	52.719302	68.462938
1135.316132	50.866076	68.467943
1134.272435	50.656043	68.472948
1132.908462	48.666194	68.477953
1132.555211	51.317282	68.482958
1132.143358	51.127738	68.487962
1131.056623	51.761882	68.492967
1130.193016	47.571447	68.497972
1129.550864	51.887197	68.502977
1129.434800	45.818574	68.507982
1129.220952	46.715341	68.512986
1128.417712	45.443786	68.517991
1127.964219	46.950773	68.522996
1126.938844	48.497660	68.528001
1125.690762	51.275524	68.533006
1124.932741	46.548744	68.538010
1124.396639	49.411924	68.543015
1124.379224	49.412988	68.548020
1123.504784	45.205464	68.553025
1123.345526	40.402212	68.558030
1121.896127	49.993462	68.563034
1121.595031	46.180374	68.568039
1120.965623	42.838355	68.573044
1119.793861	49.953357	68.578049
1119.096826	45.411917	68.583054
1118.710804	48.478336	68.588058
1117.914612	49.129044	68.593063
1117.696279	44.110127	68.598068
1117.005879	48.989904	68.603073
1115.962716	44.462735	68.608078
1115.443439	46.289658	68.613082
1115.073908	49.643767	68.618087
1114.536739	45.867946	68.623092
1113.526310	50.712132	68.628097
1112.621519	40.031276	68.633102
1112.126738	53.550336	68.638106
1111.535583	52.250361	68.643111
1110.705069	53.460740	68.648116
1109.670017	53.703555	68.653121
1109.375213	40.911889	68.658126
1109.543087	51.717067	68.663130
1108.407570	53.623855	68.668135
1107.549811	56.853549	68.673140
1107.061830	49.293022	68.678145
1106.849904	47.920612	68.683150
1105.203143	41.600176	68.688154
1104.584214	45.552755	68.693159
1103.895459	43.584656	68.698164
1103.408403	54.619609	68.703169
1103.548641	49.674680	68.708174
1101.776715	45.460586	68.713178
1101.292210	52.599219	68.718183
1100.900831	47.966760	68.723188
1100.235162	47.581087	68.728193
1100.266289	54.211839	68.733198
1099.562741	55.303377	68.738202
1098.614481	48.023764	68.743207
1097.737480	50.221799	68.748212
1096.737708	55.901365	68.753217
1096.152326	47.583078	68.758222
1095.181091	50.043555	68.763226
1095.178277	49.439382	68.768231
1094.813320	44.799243	68.773236
1093.651676	49.811819	68.778241
1092.933189	47.510538	68.783246
1092.549081	51.025032	68.788250
1091.470960	55.283604	68.793255
1090.825959	48.129293	68.798260
1090.097220	49.333694	68.803265
1089.998958	38.207646	68.808270
1089.566135	47.740083	68.813274
1088.439538	50.865821	68.818279
1087.726287	53.835914	68.823284
1086.856642	59.673982	68.828289
1086.675590	47.211769	68.833294
1086.050281	58.832084	68.838298
1085.342499	48.494452	68.843303
1084.654268	43.748626	68.848308
1083.651260	45.335109	68.853313
1082.955123	42.667652	68.858318
1082.123074	53.130522	68.863322
1081.748991	50.231476	68.868327
1081.621745	49.390069	68.873332
1080.560525	51.383215	68.878337
1080.134847	54.273277	68.883342
1079.205122	53.668756	68.888346
1078.819383	58.369664	68.893351
1077.705881	53.558113	68.898356
1077.017981	55.483386	68.903361
1076.506767	42.161571	68.908366
1075.519326	56.807054	68.913370
1075.148700	54.008463	68.918375
1074.432120	48.849484	68.923380
1073.105415	54.482805	68.928385
1073.065563	47.239871	68.933390
1072.829662	52.888102	68.938394
1072.265424	56.359632	68.943399
1071.390948	56.416279	68.948404
1070.685286	58.020135	68.953409
1070.151570	50.461130	68.958414
1069.372103	51.675010	68.963418
1068.467557	44.384369	68.968423
1067.784003	46.627041	68.973428
1066.969286	54.900990	68.978433
1066.515027	43.501181	68.983438
1066.367904	49.310648	68.988442
1065.041779	41.747216	68.993447
1064.828605	40.489097	68.998452
1063.886005	49.240843	69.003457
1063.597130	42.729341	69.008462
1062.766754	52.723789	69.013466
1061.476930	55.252249	69.018471
1061.592629	53.725452	69.023476
1060.707898	53.207173	69.028481
1060.243045	44.631029	69.033486
1059.105197	53.400029	69.038490
1058.086066	41.565662	69.043495
1058.198330	47.093483	69.048500
1057.651240	38.829044	69.053505
1056.930070	40.448976	69.058510
1056.130960	52.862436	69.063514
1055.544002	48.261502	69.068519
1054.784099	43.811758	69.073524
1053.747859	39.733401	69.078529
1053.397571	45.055444	69.083534
1052.567363	51.000833	69.088538
1052.137996	47.094065	69.093543
1051.571221	44.355909	69.098548
1050.437367	49.812530	69.103553
1050.514907	48.938029	69.108558
1049.669895	47.085115	69.113562
1048.734175	50.084625	69.118567
1047.946707	45.315143	69.123572
1047.121165	54.659452	69.128577
1047.108532	41.948945	69.133582
1046.321680	48.341231	69.138586
1045.328808	52.895460	69.143591
1044.638627	52.826610	69.148596
1044.138178	47.138410	69.153601
1043.625930	45.474817	69.158606
1042.404098	45.800155	69.163610
1041.765960	45.067949	69.168615
1041.570226	47.110249	69.173620
1040.901617	52.880341	69.178625
1040.980957	46.694978	69.183630
1039.467656	52.853658	69.188634
1038.757242	47.629686	69.193639
1038.675925	47.526041	69.198644
1037.373004	50.222136	69.203649
1036.450479	47.017953	69.208654
1036.093538	55.504024	69.213658
1035.279981	54.019129	69.218663
1035.440279	50.097433	69.223668
1034.170206	54.166263	69.228673
1033.693465	45.787546	69.233678
1033.105212	54.052714	69.238682
1032.595838	54.526824	69.243687
1031.743078	45.208334	69.248692
1030.542560	56.091531	69.253697
1030.378786	47.060033	69.258702
1030.100689	49.349718	69.263706
1029.204476	50.634910	69.268711
1028.100714	43.814561	69.273716
1027.305634	49.668282	69.278721
1027.051486	41.372628	69.283726
1026.650082	46.133056	69.288730
1025.671539	43.236482	69.293735
1024.964896	48.813754	69.298740
1024.090093	54.263122	69.303745
1023.958099	45.254209	69.308750
1023.075943	56.940218	69.313754
1021.909437	53.828737	69.318759
1021.848397	54.263569	69.323764
1021.232863	57.288776	69.328769
1019.921433	54.625253	69.333774
1019.336585	55.302545	69.338778
1018.627756	48.361276	69.343783
1018.718454	48.753149	69.348788
1018.267613	59.021672	69.353793
1017.567556	50.635410	69.358798
1016.324712	59.104651	69.363802
1015.832356	51.743827	69.368807
1015.330931	47.576653	69.373812
1014.265894	50.990665	69.378817
1013.542950	37.841702	69.383822
1013.113413	44.038988	69.388826
1012.538260	54.302349	69.393831
1011.726474	53.275819	69.398836
1010.816633	52.315422	69.403841
1010.694259	52.825492	69.408846
1009.996957	50.135746	69.413850
1009.538540	53.070890	69.418855
1008.493325	42.851461	69.423860
1007.799396	48.030259	69.428865
1007.031730	42.523613	69.433870
1006.521925	44.727458	69.438874
1005.492159	50.106264	69.443879
1005.109894	38.987024	69.448884
1004.266891	45.608392	69.453889
1004.092183	44.886428	69.458894
1003.458057	51.369005	69.463898
1002.398349	42.305035	69.468903
1002.140643	44.527678	69.473908
1001.447122	44.534403	69.478913
1000.713089	44.885155	69.483918
999.888867	40.394731	69.488922
999.320269	47.956694	69.493927
998.835650	40.863356	69.498932
997.504746	45.163258	69.503937
996.961442	42.357936	69.508942
996.268470	47.280793	69.513946
995.702299	46.753363	69.518951
995.892767	36.646783	69.523956
994.647804	49.679730	69.528961
994.043601	46.870627	69.533966
993.701729	44.568415	69.538970
992.436033	45.632297	69.543975
991.859187	34.079435	69.548980
991.189988	49.396696	69.553985
991.046320	32.344236	69.558990
990.477439	34.902788	69.563994
989.689023	46.049339	69.568999
989.200679	41.499026	69.574004
987.752891	44.637159	69.579009
986.644158	40.501764	69.584014
986.186806	42.234017	69.589018
985.877857	47.002691	69.594023
985.698277	42.335161	69.599028
984.716004	48.005427	69.604033
984.301076	45.296537	69.609038
983.026796	48.031158	69.614042
982.075351	44.136051	69.619047
982.011799	39.377996	69.624052
981.336208	48.410849	69.629057
981.353597	42.122816	69.634062
980.375788	53.625083	69.639066
979.645174	34.591789	69.644071
979.354408	45.728110	69.649076
977.829792	46.622400	69.654081
977.564303	35.809997	69.659086
976.852550	36.770725	69.664090
976.402147	45.968685	69.669095
975.251166	36.219733	69.674100
974.214421	50.349471	69.679105
974.129097	41.303365	69.684110
973.506646	41.125035	69.689114
972.815536	49.080991	69.694119
971.965557	43.228070	69.699124
971.050036	45.460746	69.704129
970.786713	44.748038	69.709134
970.214100	40.817660	69.714138
969.755846	48.409276	69.719143
969.458506	45.373553	69.724148
968.290796	46.303822	69.729153
967.951183	41.458843	69.734158
966.575678	46.529382	69.739162
965.929842	48.167212	69.744167
965.516539	43.707468	69.749172
964.899168	48.035959	69.754177
964.226399	45.078347	69.759182
963.054685	48.504323	69.764186
962.585889	46.894084	69.769191
962.438183	40.265661	69.774196
962.204350	48.915372	69.779201
961.370323	44.815826	69.784206
960.377524	41.997496	69.789210
959.835372	45.989830	69.794215
959.390771	35.268103	69.799220
957.768436	51.310287	69.804225
957.527674	41.483603	69.809230
956.987047	42.130829	69.814234
956.418021	48.049257	69.819239
955.188881	39.612321	69.824244
954.426879	44.061104	69.829249
953.551427	44.168464	69.834254
953.291876	48.487382	69.839258
952.700479	50.398905	69.844263
953.041867	43.912495	69.849268
952.486757	47.605089	69.854273
951.580936	38.592147	69.859278
950.907076	38.733268	69.864282
949.393723	46.758206	69.869287
948.761642	41.415844	69.874292
947.953339	52.536598	69.879297
947.680592	34.513929	69.884302
947.605354	38.464583	69.889306
946.657838	34.053311	69.894311
945.635156	38.072288	69.899316
945.181704	45.486247	69.904321
944.456097	38.005924	69.909326
943.898885	42.346216	69.914330
942.816314	44.950912	69.919335
942.421228	41.067103	69.924340
942.077561	45.577656	69.929345
941.183883	43.363246	69.934350
940.116668	41.805766	69.939354
939.452509	45.508354	69.944359
939.622410	43.531768	69.949364
938.474437	48.985300	69.954369
937.551753	51.783262	69.959374
936.867679	52.989902	69.964378
936.347874	51.326037	69.969383
935.954404	34.467548	69.974388
935.412994	45.739157	69.979393
934.606589	37.652571	69.984398
933.773211	37.111311	69.989402
932.910846	40.566015	69.994407
932.951733	47.856629	69.999412
932.004353	46.818207	70.004417
930.979217	40.191649	70.009422
930.609104	42.944706	70.014426
929.906866	41.041706	70.019431
929.303521	44.026148	70.024436
928.539332	43.661714	70.029441
927.786776	43.306340	70.034446
927.416195	42.512931	70.039450
926.736136	46.871898	70.044455
925.639102	41.519571	70.049460
925.162431	51.345689	70.054465
924.702852	46.304164	70.059470
924.322506	43.733430	70.064474
922.990866	45.797788	70.069479
922.788914	38.579083	70.074484
922.321800	41.502299	70.079489
921.799716	50.196641	70.084494
920.511140	43.871772	70.089498
919.695957	49.910517	70.094503
919.547435	41.514292	70.099508
918.218341	49.836086	70.104513
917.303865	46.230701	70.109518
917.263375	47.056733	70.114522
916.646976	41.548672	70.119527
916.264106	43.874461	70.124532
915.694512	47.869920	70.129537
915.000966	42.947809	70.134542
914.581610	39.224074	70.139546
913.300104	42.951087	70.144551
912.361786	43.794714	70.149556
911.564499	52.718158	70.154561
911.328811	36.427096	70.159566
910.945433	41.712177	70.164570
910.426106	47.889321	70.169575
909.689362	37.536571	70.174580
908.622790	40.600353	70.179585
908.008556	41.437814	70.184590
907.683782	43.661685	70.189594
906.677746	49.035651	70.194599
905.854523	38.696924	70.199604
905.023020	44.452293	70.204609
904.786664	41.742826	70.209614
904.614750	44.258659	70.214618
903.897623	38.588651	70.219623
903.093502	35.145547	70.224628
902.329558	44.720877	70.229633
901.113120	44.968750	70.234638
900.371530	41.291919	70.239642
900.004719	49.601657	70.244647
899.800139	38.355300	70.249652
899.021192	39.295180	70.254657
898.124135	42.848196	70.259662
897.667585	47.971347	70.264666
896.678239	49.229488	70.269671
896.863629	39.903352	70.274676
895.458063	50.539063	70.279681
894.761315	38.031408	70.284686
894.155072	36.248545	70.289690
893.847060	39.352529	70.294695
892.797789	32.604204	70.299700
891.938809	42.334357	70.304705
891.286648	39.716634	70.309710
891.073172	47.519341	70.314714
890.237099	52.415405	70.319719
889.421674	41.322617	70.324724
888.860755	46.226023	70.329729
888.611343	36.529908	70.334734
887.818116	42.117677	70.339738
887.052887	46.494788	70.344743
886.327701	41.713885	70.349748
885.777253	45.092673	70.354753
884.903249	32.326451	70.359758
884.081368	37.332181	70.364762
883.044113	39.906627	70.369767
882.983791	41.175771	70.374772
882.258907	39.583749	70.379777
882.028890	41.479957	70.384782
881.478107	43.133094	70.389786
880.519050	50.138679	70.394791
879.895122	42.309784	70.399796
878.609106	52.843316	70.404801
878.146834	40.477073	70.409806
877.447782	31.885430	70.414810
876.947770	47.089236	70.419815
876.777869	37.984607	70.424820
875.803201	41.562366	70.429825
875.184997	36.674726	70.434830
874.561248	37.131733	70.439834
873.693725	47.465694	70.444839
873.502675	41.117454	70.449844
872.275855	41.457898	70.454849
871.703971	41.085797	70.459854
871.442368	40.000187	70.464858
870.127184	47.580693	70.469863
869.487863	31.665477	70.474868
868.658651	38.951173	70.479873
868.263363	43.991596	70.484878
868.104024	44.003944	70.489882
867.509684	40.981998	70.494887
866.488049	36.855402	70.499892
865.986650	42.939479	70.504897
865.133714	34.855751	70.509902
864.671775	38.856060	70.514906
863.608038	55.974898	70.519911
863.158261	46.382571	70.524916
862.606333	47.282783	70.529921
862.052540	45.700535	70.534926
861.130900	45.018097	70.539930
859.937712	53.270838	70.544935
859.713740	38.729145	70.549940
859.345418	34.001593	70.554945
858.968699	41.998828	70.559950
858.061865	48.920474	70.564954
856.761886	49.947632	70.569959
856.710753	39.478250	70.574964
856.356235	41.125403	70.579969
854.985320	37.156131	70.584974
854.640945	37.923297	70.589978
854.181686	41.284099	70.594983
853.685860	34.550720	70.599988
852.270680	39.665577	70.604993
851.819991	38.660116	70.609998
851.445582	40.122790	70.615002
850.886530	38.595916	70.620007
849.487836	35.583071	70.625012
849.152287	42.303445	70.630017
848.771013	38.164268	70.635022
848.643126	45.908893	70.640026
847.331912	38.795728	70.645031
846.725055	42.775075	70.650036
845.901670	45.495255	70.655041
845.418568	36.254419	70.660046
844.559588	33.131367	70.665050
843.789026	40.558986	70.670055
843.442353	42.507149	70.675060
842.682750	42.829543	70.680065
841.886948	35.890586	70.685070
841.473951	44.517690	70.690074
840.399644	46.719956	70.695079
840.464007	38.520951	70.700084
839.802282	46.896595	70.705089
838.648491	40.247103	70.710094
837.842612	37.659272	70.715098
837.447339	47.204615	70.720103
836.949634	30.194677	70.725108
836.113930	42.797157	70.730113
835.330542	47.666439	70.735118
834.834044	43.481082	70.740122
834.540973	37.215451	70.745127
833.816895	42.985977	70.750132
832.756797	42.235292	70.755137
832.084524	41.615141	70.760142
831.388932	41.894994	70.765146
830.402444	42.192703	70.770151
829.738153	35.606599	70.775156
829.182537	40.319239	70.780161
828.954063	40.946166	70.785166
828.932331	42.183043	70.790170
827.397475	41.945897	70.795175
826.874045	41.267885	70.800180
825.949336	45.750868	70.805185
825.596960	39.417241	70.810190
825.055606	36.700422	70.815194
824.012655	38.045518	70.820199
823.630830	36.674203	70.825204
823.070532	43.602410	70.830209
822.211715	48.279756	70.835214
821.457144	37.737461	70.840218
820.596117	44.327594	70.845223
820.408318	36.359275	70.850228
819.755966	37.484710	70.855233
818.579363	42.425689	70.860238
818.300395	35.991074	70.865242
817.478150	44.583679	70.870247
817.070491	43.678610	70.875252
816.410684	41.555607	70.880257
815.411483	45.313228	70.885262
814.953654	41.590965	70.890266
814.150132	38.651436	70.895271
814.311898	38.043547	70.900276
813.131950	40.143129	70.905281
812.212051	43.720596	70.910286
812.065839	37.033120	70.915290
811.122786	42.154348	70.920295
810.450640	33.017742	70.925300
809.746818	42.274502	70.930305
809.343071	36.433603	70.935310
808.262921	37.967829	70.940314
807.546571	40.959797	70.945319
807.195870	35.924116	70.950324
806.540350	40.152578	70.955329
805.580540	42.391683	70.960334
804.965502	33.557912	70.965338
804.206856	41.770167	70.970343
803.849088	38.764547	70.975348
803.135026	34.053201	70.980353
802.131923	39.892445	70.985358
801.591661	34.825686	70.990362
801.191415	40.924015	70.995367
800.689354	37.266566	71.000372
799.146368	44.809136	71.005377
798.644056	52.802627	71.010382
798.398338	44.623581	71.015386
797.787980	47.641209	71.020391
797.912207	39.535368	71.025396
797.281417	48.416481	71.030401
796.110118	43.856086	71.035406
795.236802	42.946315	71.040410
794.164703	55.657981	71.045415
793.672260	47.192003	71.050420
793.067944	41.320728	71.055425
792.616106	41.719877	71.060430
791.968110	41.144913	71.065434
791.164060	45.838537	71.070439
790.630892	33.291842	71.075444
790.003933	39.462557	71.080449
788.914141	37.766488	71.085454
788.115201	41.334684	71.090458
787.561656	44.794927	71.095463
787.606740	38.190338	71.100468
787.479280	42.454656	71.105473
786.085996	41.731847	71.110478
785.054959	36.308259	71.115482
784.542578	45.381841	71.120487
783.891761	36.738141	71.125492
782.563266	40.847029	71.130497
781.766676	39.530583	71.135502
781.494225	31.112585	71.140506
780.962011	35.744248	71.145511
780.780906	39.416600	71.150516
780.314874	29.838926	71.155521
780.010894	38.148155	71.160526
779.127179	36.062725	71.165530
777.869954	38.331072	71.170535
777.157810	38.432198	71.175540
776.017687	37.265781	71.180545
775.748466	37.561022	71.185550
775.182992	38.723287	71.190554
774.916428	44.242955	71.195559
774.695306	37.696598	71.200564
773.661241	42.190426	71.205569
772.685340	45.752231	71.210574
772.594808	34.779636	71.215578
771.018706	38.092167	71.220583
770.576812	30.828142	71.225588
770.191143	34.408831	71.230593
769.659230	37.348288	71.235598
768.247678	32.986158	71.240602
767.963591	40.461889	71.245607
767.686267	39.137412	71.250612
767.035638	44.538932	71.255617
766.022455	43.841012	71.260622
765.300465	36.492736	71.265626
764.465229	41.169995	71.270631
764.321217	39.975831	71.275636
763.783648	40.332435	71.280641
763.091920	33.633815	71.285646
762.714462	37.423877	71.290650
761.437860	43.008810	71.295655
760.501667	37.576086	71.300660
759.675370	41.369620	71.305665
759.076684	34.945969	71.310670
759.068349	33.509495	71.315674
758.534986	36.282631	71.320679
757.761283	27.313826	71.325684
756.869392	46.148660	71.330689
756.380053	41.258700	71.335694
755.661566	33.489454	71.340698
754.873870	41.639191	71.345703
754.218929	34.664284	71.350708
753.642514	37.388350	71.355713
752.319652	41.105510	71.360718
751.698846	39.040965	71.365722
751.006778	40.086374	71.370727
750.645065	32.846114	71.375732
750.376203	27.909313	71.380737
749.969742	38.129557	71.385742
749.666702	32.464829	71.390746
748.154032	37.684432	71.395751
747.847397	28.787978	71.400756
746.656043	31.867244	71.405761
745.943991	35.797515	71.410766
745.445823	30.258184	71.415770
744.954186	45.465282	71.420775
745.071460	34.491039	71.425780
744.111066	39.401309	71.430785
743.202377	40.042928	71.435790
742.599118	30.981771	71.440794
741.165156	37.660979	71.445799
741.037481	41.015114	71.450804
739.914687	37.666106	71.455809
739.512400	41.516473	71.460814
739.164949	31.198132	71.465818
738.202577	32.319057	71.470823
737.750338	32.088705	71.475828
737.071092	36.465704	71.480833
736.460324	30.450688	71.485838
735.866006	24.685080	71.490842
734.551375	35.188000	71.495847
734.329936	28.152651	71.500852
733.687954	35.674296	71.505857
733.011544	42.289255	71.510862
732.715858	31.960863	71.515866
731.152618	26.210460	71.520871
730.807602	31.365423	71.525876
730.274833	30.070894	71.530881
729.712442	34.099075	71.535886
729.777495	29.944636	71.540890
728.383073	37.981612	71.545895
727.952715	32.378564	71.550900
727.508526	33.660182	71.555905
726.185433	30.382201	71.560910
725.491470	34.206354	71.565914
724.697716	28.499386	71.570919
724.686396	33.758623	71.575924
724.293067	40.009707	71.580929
723.016762	39.207669	71.585934
722.445561	27.912451	71.590938
722.063997	37.491355	71.595943
721.073216	30.657275	71.600948
720.329541	32.402678	71.605953
719.378587	41.143253	71.610958
719.273603	33.296150	71.615962
718.639579	34.711338	71.620967
718.253405	31.909137	71.625972
717.469559	35.519753	71.630977
716.700673	35.687054	71.635982
716.388123	32.217800	71.640986
715.136389	32.061654	71.645991
714.242050	27.345688	71.650996
714.133155	33.872500	71.656001
713.304282	37.954230	71.661006
712.340509	28.383686	71.666010
711.306992	36.133848	71.671015
711.101008	32.017947	71.676020
710.786152	42.510644	71.681025
710.521888	31.825179	71.686030
709.466282	25.220094	71.691034
708.427253	30.974323	71.696039
708.034255	28.093166	71.701044
707.623694	22.879872	71.706049
706.588228	35.472759	71.711054
705.779774	31.020751	71.716058
705.166660	38.854412	71.721063
705.082497	30.991113	71.726068
704.080043	35.716366	71.731073
703.029499	38.945985	71.736078
702.863586	36.039344	71.741082
702.027530	43.848046	71.746087
701.376749	35.610919	71.751092
700.562553	36.196096	71.756097
699.778686	40.921796	71.761102
699.672023	32.502642	71.766106
698.708976	41.642377	71.771111
697.813475	38.572189	71.776116
697.053403	47.782149	71.781121
696.283196	38.265281	71.786126
696.500733	33.148054	71.791130
695.869359	43.614848	71.796135
694.852631	27.516859	71.801140
693.854017	34.710806	71.806145
693.344613	41.515041	71.811150
692.951025	34.997057	71.816154
692.162527	43.655334	71.821159
691.320334	36.317801	71.826164
691.094006	28.654510	71.831169
690.068841	37.361223	71.836174
689.350305	32.887893	71.841178
688.464241	37.135336	71.846183
688.046367	29.967864	71.851188
687.935437	35.340081	71.856193
686.852163	32.513634	71.861198
685.826189	31.389261	71.866202
685.203182	34.942327	71.871207
684.886444	30.266353	71.876212
684.287377	35.334980	71.881217
683.777730	37.805258	71.886222
683.410877	34.302285	71.891226
682.312257	40.219092	71.896231
681.297717	40.860699	71.901236
680.472638	42.159420	71.906241
679.583792	46.106569	71.911246
679.496921	28.297646	71.916250
679.071206	38.831830	71.921255
678.612941	37.590066	71.926260
677.655934	40.805243	71.931265
676.902738	39.484935	71.936270
676.329905	26.872441	71.941274
675.805636	34.088936	71.946279
675.024024	34.919575	71.951284
674.597905	31.853052	71.956289
673.812238	39.157357	71.961294
672.921142	37.882779	71.966298
672.104200	36.717464	71.971303
671.753703	40.381733	71.976308
671.277820	36.443516	71.981313
670.199139	36.216289	71.986318
669.719016	28.660031	71.991322
669.053564	35.598361	71.996327
668.346389	36.306517	72.001332
667.973346	36.685074	72.006337
666.763332	41.276165	72.011342
666.172417	38.426551	72.016346
665.777617	47.260527	72.021351
665.180988	33.460060	72.026356
664.224966	37.541870	72.031361
663.368576	40.503771	72.036366
663.178010	28.306554	72.041370
662.749590	29.171021	72.046375
661.942353	38.291169	72.051380
661.133089	26.934915	72.056385
660.460028	31.465194	72.061390
659.998749	32.854740	72.066394
658.619095	35.819845	72.071399
657.770153	32.360788	72.076404
657.482332	27.349881	72.081409
657.141859	32.428676	72.086414
656.872231	30.718039	72.091418
656.249508	35.924136	72.096423
655.020734	29.675165	72.101428
654.299558	31.749469	72.106433
654.069548	35.284152	72.111438
653.361874	30.167554	72.116442
652.220798	40.169462	72.121447
651.872976	33.571017	72.126452
651.289234	35.118906	72.131457
650.570050	44.325414	72.136462
649.828104	39.156267	72.141466
649.197422	45.446045	72.146471
648.901183	44.049031	72.151476
647.735814	36.649252	72.156481
646.723362	33.785025	72.161486
646.631368	32.608006	72.166490
645.501370	44.456086	72.171495
645.662624	42.543344	72.176500
644.724428	39.868884	72.181505
643.547770	41.901234	72.186510
643.746513	31.728925	72.191514
642.918681	32.479071	72.196519
641.554050	31.690610	72.201524
641.173585	41.310771	72.206529
640.378010	41.185829	72.211534
639.774610	36.570024	72.216538
639.421010	42.300382	72.221543
638.421450	38.781873	72.226548
638.109306	41.819077	72.231553
637.285898	46.997196	72.236558
637.008561	38.931746	72.241562
636.002609	49.055373	72.246567
635.443826	46.620236	72.251572
635.255621	47.850110	72.256577
633.760773	52.212525	72.261582
632.697308	35.545088	72.266586
632.031042	41.675576	72.271591
632.068933	40.209475	72.276596
631.456366	36.748212	72.281601
630.698907	38.489674	72.286606
630.195511	35.579284	72.291610
629.280184	43.865366	72.296615
628.825786	36.318915	72.301620
628.322444	33.415227	72.306625
627.345408	39.580802	72.311630
627.008835	33.292260	72.316634
626.300816	40.998114	72.321639
625.348180	40.589836	72.326644
624.846140	33.558366	72.331649
623.822372	37.751258	72.336654
623.603625	33.442956	72.341658
622.994151	36.671226	72.346663
621.711481	35.045742	72.351668
621.247942	34.466435	72.356673
620.750329	42.041507	72.361678
620.385182	38.160899	72.366682
619.433150	40.501725	72.371687
618.468739	33.801700	72.376692
618.143048	36.524266	72.381697
617.462517	35.019817	72.386702
616.924665	29.487701	72.391706
616.332360	43.782479	72.396711
615.492177	34.834175	72.401716
614.746002	32.679822	72.406721
614.230192	35.388780	72.411726
613.698097	28.380622	72.416730
612.661048	39.134015	72.421735
612.418579	31.412712	72.426740
611.751268	29.036042	72.431745
610.386143	39.244493	72.436750
610.498361	37.250946	72.441754
609.656603	34.909296	72.446759
608.927963	35.875336	72.451764
607.965758	36.848632	72.456769
607.202545	38.138343	72.461774
607.047900	38.063848	72.466778
606.400158	43.673296	72.471783
605.801615	39.590322	72.476788
605.013951	37.683461	72.481793
604.105531	35.782291	72.486798
604.227473	35.200561	72.491802
603.142485	42.899167	72.496807
602.000949	31.185405	72.501812
601.712668	32.312826	72.506817
601.200793	37.152583	72.511822
600.450838	32.861882	72.516826
599.316725	39.657897	72.521831
598.702260	36.995082	72.526836
598.505031	34.440376	72.531841
597.674981	37.586448	72.536846
597.049271	34.374536	72.541850
596.310529	36.261604	72.546855
595.331086	34.369447	72.551860
595.128257	39.502027	72.556865
593.983805	39.999340	72.561870
593.288420	32.377746	72.566874
592.518478	28.531371	72.571879
592.077076	34.058886	72.576884
592.171335	32.021841	72.581889
591.800546	36.619936	72.586894
590.545285	27.314100	72.591898
589.865252	39.437568	72.596903
589.024608	31.458383	72.601908
588.231304	30.900451	72.606913
587.337777	35.810337	72.611918
586.979604	32.315362	72.616922
586.612541	36.506655	72.621927
586.146230	36.089660	72.626932
585.328150	30.668719	72.631937
584.689170	34.210716	72.636942
584.043289	33.107288	72.641946
582.606777	38.274809	72.646951
581.963762	30.269659	72.651956
581.789910	32.896739	72.656961
580.971943	37.378439	72.661966
580.985915	29.071651	72.666970
579.864237	37.381645	72.671975
578.817767	39.247236	72.676980
578.635283	29.088546	72.681985
577.895296	35.629937	72.686990
577.457536	29.829638	72.691994
576.319478	32.299839	72.696999
575.655028	37.686767	72.702004
575.367598	34.216380	72.707009
574.776585	37.281237	72.712014
574.160586	35.948096	72.717018
572.929631	42.145741	72.722023
572.498236	37.324432	72.727028
571.938194	37.342293	72.732033
571.294919	40.074280	72.737038
570.419683	37.082749	72.742042
569.647430	36.006502	72.747047
569.206516	39.353915	72.752052
568.850028	41.396532	72.757057
567.649350	38.569311	72.762062
567.008864	34.528267	72.767066
566.499972	40.462855	72.772071
565.743277	36.084109	72.777076
565.970617	34.192410	72.782081
564.845788	38.100275	72.787086
564.217223	33.204995	72.792090
563.528855	40.033187	72.797095
562.830289	39.182724	72.802100
561.940883	33.945316	72.807105
561.305834	38.084638	72.812110
560.874672	28.777731	72.817114
559.907913	37.769700	72.822119
559.109746	41.803954	72.827124
558.279754	36.868586	72.832129
557.693718	41.155031	72.837134
558.152212	35.567066	72.842138
556.884173	38.515442	72.847143
555.731010	37.724322	72.852148
555.464906	31.392139	72.857153
554.937345	39.796117	72.862158
553.713605	33.336325	72.867162
553.768919	40.792579	72.872167
552.884324	46.007638	72.877172
552.839732	30.036798	72.882177
551.450220	34.584856	72.887182
551.159735	30.019262	72.892186
550.189130	37.367896	72.897191
548.934721	39.350039	72.902196
548.676818	31.372061	72.907201
547.686854	33.693347	72.912206
547.542618	33.429184	72.917210
546.960806	34.581642	72.922215
545.853191	32.352662	72.927220
545.111209	31.199394	72.932225
544.182523	35.490474	72.937230
544.332279	33.510232	72.942234
543.747371	34.228637	72.947239
542.945241	34.579679	72.952244
542.228352	31.089731	72.957249
541.317784	42.330250	72.962254
540.982414	35.595089	72.967258
540.737226	35.198627	72.972263
539.494221	33.016135	72.977268
538.933615	35.655411	72.982273
538.098276	33.342280	72.987278
537.817350	32.961415	72.992282
536.548063	35.130443	72.997287
536.255125	38.496315	73.002292
536.292223	22.136508	73.007297
534.626996	39.807987	73.012302
534.270599	32.180029	73.017306
533.629854	33.856508	73.022311
533.088217	40.071037	73.027316
532.429698	28.042049	73.032321
531.076084	35.950104	73.037326
530.701314	32.073920	73.042330
530.612301	41.492567	73.047335
529.812660	37.841150	73.052340
529.246226	24.778807	73.057345
528.175241	40.950378	73.062350
527.905702	35.067973	73.067354
527.074740	46.763779	73.072359
525.895194	41.586751	73.077364
525.253988	38.223960	73.082369
524.675691	42.676046	73.087374
524.466498	36.608836	73.092378
524.035418	35.026527	73.097383
523.070597	37.851904	73.102388
522.603954	47.107510	73.107393
521.767823	46.914541	73.112398
521.276639	39.546902	73.117402
520.244569	41.162550	73.122407
519.600512	42.956041	73.127412
519.510640	44.044337	73.132417
518.267026	41.727750	73.137422
517.675925	36.541073	73.142426
517.038339	43.642001	73.147431
516.425444	48.191592	73.152436
515.816576	37.486658	73.157441
514.495220	42.168699	73.162446
513.875606	38.600904	73.167450
513.451844	35.124676	73.172455
513.330573	47.331605	73.177460
513.128962	32.366969	73.182465
512.183515	39.338290	73.187470
511.201174	35.478986	73.192474
510.699887	37.842851	73.197479
509.522665	32.843054	73.202484
508.975224	25.476381	73.207489
507.770695	41.631760	73.212494
507.616380	37.576098	73.217498
507.017978	38.365501	73.222503
506.610672	41.301785	73.227508
506.657920	40.555623	73.232513
505.402085	39.386209	73.237518
504.966473	34.781149	73.242522
503.877772	44.448858	73.247527
502.788799	41.366867	73.252532
502.459186	41.118289	73.257537
501.920997	44.502506	73.262542
501.311531	37.671035	73.267546
500.314845	45.118879	73.272551
499.587659	41.432948	73.277556
499.316797	44.690440	73.282561
498.734864	44.660747	73.287566
498.456265	45.026290	73.292570
497.628959	41.754601	73.297575
496.618886	43.177415	73.302580
495.904217	30.828074	73.307585
494.944668	33.768598	73.312590
494.158797	37.606552	73.317594
493.753618	40.737856	73.322599
493.304239	39.048560	73.327604
493.368301	32.736382	73.332609
492.345471	34.091123	73.337614
491.872266	34.137926	73.342618
490.537913	39.672813	73.347623
489.451430	46.273986	73.352628
489.113348	28.221192	73.357633
488.743982	43.756249	73.362638
488.735003	34.885796	73.367642
487.822014	33.508829	73.372647
486.872800	36.435348	73.377652
486.460763	24.606494	73.382657
484.937010	35.323306	73.387662
483.971801	32.475495	73.392666
483.263878	35.679993	73.397671
482.841837	33.884177	73.402676
482.825086	32.133377	73.407681
482.153175	32.653157	73.412686
482.038034	26.127757	73.417690
481.186336	39.215725	73.422695
480.117891	35.113829	73.427700
479.738917	31.671770	73.432705
478.491310	34.064060	73.437710
477.653963	32.659922	73.442714
477.193475	33.572924	73.447719
476.508814	33.530051	73.452724
476.414675	28.752013	73.457729
475.503920	36.130265	73.462734
474.980136	31.944115	73.467738
474.132116	36.780696	73.472743
473.866525	41.583783	73.477748
472.886571	31.140209	73.482753
472.278893	35.725614	73.487758
471.743260	34.090179	73.492762
471.192771	33.127123	73.497767
470.219016	32.583951	73.502772
469.425677	27.830211	73.507777
468.789342	36.349929	73.512782
468.246646	30.819459	73.517786
466.901782	34.244812	73.522791
466.454622	45.998002	73.527796
466.111151	32.646815	73.532801
465.517028	33.911518	73.537806
465.206618	28.921476	73.542810
464.677998	29.218161	73.547815
463.808558	32.701378	73.552820
462.961376	24.787295	73.557825
461.999633	32.287173	73.562830
461.367637	31.061390	73.567834
460.856392	35.238713	73.572839
460.225942	35.529955	73.577844
460.037265	31.735963	73.582849
458.867659	38.675049	73.587854
458.036769	41.115927	73.592858
457.884321	35.262015	73.597863
457.030796	41.658278	73.602868
456.662631	30.906194	73.607873
455.279723	36.548877	73.612878
454.896711	26.460491	73.617882
454.189370	33.135631	73.622887
453.752519	32.047715	73.627892
453.509517	24.027729	73.632897
452.290177	29.955389	73.637902
451.869993	22.408639	73.642906
451.398418	29.944907	73.647911
450.172065	32.071074	73.652916
450.049356	37.206104	73.657921
448.915202	39.984332	73.662926
448.314917	29.639905	73.667930
447.232672	35.993262	73.672935
447.005534	32.853196	73.677940
446.691951	34.646900	73.682945
446.087008	44.699059	73.687950
444.889127	29.911881	73.692954
444.295090	24.733619	73.697959
443.917231	36.416506	73.702964
443.109793	24.305309	73.707969
441.677228	31.651808	73.712974
441.497951	25.688031	73.717978
440.858099	23.792186	73.722983
440.532915	35.955100	73.727988
440.293878	25.167079	73.732993
439.547864	30.637858	73.737998
438.615908	26.113527	73.743002
438.210325	25.875999	73.748007
436.907563	35.376327	73.753012
436.279421	30.857164	73.758017
435.186421	39.489880	73.763022
434.699477	30.562799	73.768026
434.529306	28.312926	73.773031
434.227005	33.438076	73.778036
433.972678	28.971293	73.783041
432.769671	46.803572	73.788046
431.842159	30.142133	73.793050
431.431662	40.422269	73.798055
430.315940	35.845355	73.803060
429.693334	36.299064	73.808065
429.183590	42.194729	73.813070
428.793944	31.969330	73.818074
427.699373	35.990056	73.823079
426.854449	42.097495	73.828084
426.619535	35.526309	73.833089
426.006408	40.422111	73.838094
425.434163	38.444027	73.843098
424.841759	33.940844	73.848103
423.846215	44.003893	73.853108
423.199686	39.159082	73.858113
422.926992	43.442757	73.863118
421.907806	39.896483	73.868122
421.175616	30.960121	73.873127
420.675346	43.568681	73.878132
420.411530	36.012105	73.883137
418.906659	36.481232	73.888142
418.389714	44.183563	73.893146
418.455748	41.588094	73.898151
417.483911	44.200756	73.903156
416.485761	43.345213	73.908161
415.270207	43.124134	73.913166
415.210030	43.769996	73.918170
415.043516	37.292084	73.923175
414.311559	40.568600	73.928180
413.364215	43.670461	73.933185
412.234839	37.963451	73.938190
411.960828	41.858555	73.943194
411.417672	41.627238	73.948199
411.043615	38.667082	73.953204
410.175908	38.320079	73.958209
409.572704	33.885063	73.963214
409.134572	41.167329	73.968218
408.262922	35.570881	73.973223
407.065578	42.197379	73.978228
406.940535	35.182257	73.983233
406.353757	40.710222	73.988238
405.244139	32.103796	73.993242
404.735430	41.833952	73.998247
404.073622	42.749491	74.003252
403.844570	33.283638	74.008257
402.861420	44.170311	74.013262
402.401660	34.806756	74.018266
402.070210	35.540554	74.023271
400.286711	37.045017	74.028276
399.489905	32.887512	74.033281
398.719201	41.035547	74.038286
398.531361	41.051612	74.043290
398.301590	41.676015	74.048295
397.552219	35.487064	74.053300
397.581703	32.880492	74.058305
396.473267	39.100196	74.063310
395.622629	34.991389	74.068314
395.207534	34.386829	74.073319
393.644663	34.940505	74.078324
393.374860	34.911804	74.083329
392.789704	40.298973	74.088334
392.124341	31.740750	74.093338
391.564970	25.833436	74.098343
391.027935	43.711044	74.103348
390.398234	30.247097	74.108353
389.577623	31.891264	74.113358
389.051743	35.444290	74.118362
388.857348	34.973214	74.123367
387.605909	39.655141	74.128372
387.027286	33.887696	74.133377
386.295905	32.617776	74.138382
385.432963	33.582392	74.143386
384.606128	31.370067	74.148391
383.632454	38.013100	74.153396
383.637814	38.568787	74.158401
383.043907	33.348671	74.163406
382.833770	32.985682	74.168410
382.200559	38.848037	74.173415
381.007023	34.035408	74.178420
380.644067	37.304342	74.183425
379.389175	41.208483	74.188430
379.023557	27.008529	74.193434
378.498953	30.281483	74.198439
377.625377	42.923231	74.203444
377.683333	33.125183	74.208449
376.323111	37.276311	74.213454
375.745431	35.272719	74.218458
375.026594	31.598804	74.223463
373.882283	40.549781	74.228468
373.458241	34.000358	74.233473
372.820447	34.659956	74.238478
372.271702	30.401526	74.243482
372.003004	32.120044	74.248487
371.278853	38.607031	74.253492
370.186510	34.336375	74.258497
369.841402	35.152643	74.263502
369.217129	31.556859	74.268506
368.957430	31.683919	74.273511
368.061593	32.385769	74.278516
367.314109	35.893097	74.283521
366.495748	34.932940	74.288526
365.895142	29.198478	74.293530
365.049165	32.537169	74.298535
363.960015	32.955984	74.303540
363.874233	27.969296	74.308545
363.203556	35.654949	74.313550
362.711152	30.172717	74.318554
361.580378	28.684689	74.323559
361.055629	32.096214	74.328564
360.781982	30.424971	74.333569
359.896041	26.306435	74.338574
359.222704	30.503255	74.343578
358.436611	33.828921	74.348583
358.043888	34.929651	74.353588
357.465951	35.494129	74.358593
356.383570	33.913338	74.363598
355.707963	35.953031	74.368602
355.614971	31.303876	74.373607
354.860704	44.207006	74.378612
354.237831	35.199426	74.383617
353.477863	33.961251	74.388622
352.675882	36.364033	74.393626
351.441359	34.903261	74.398631
350.594441	45.390427	74.403636
350.566735	32.816419	74.408641
350.268517	38.552286	74.413646
349.253960	41.150967	74.418650
349.097839	37.478501	74.423655
347.894157	28.642310	74.428660
347.477903	30.288229	74.433665
346.901965	30.283974	74.438670
345.873371	37.652045	74.443674
344.914909	34.409974	74.448679
344.387611	35.982167	74.453684
344.371539	32.421482	74.458689
343.962967	39.289362	74.463694
342.797877	41.677804	74.468698
342.239073	37.077698	74.473703
341.538564	43.874437	74.478708
340.595878	33.613585	74.483713
339.906368	35.307523	74.488718
339.337300	41.621495	74.493722
339.292362	37.508812	74.498727
337.927899	40.995976	74.503732
337.554812	31.990192	74.508737
336.159031	34.488039	74.513742
335.961254	38.749795	74.518746
335.731019	34.104428	74.523751
334.436294	40.922094	74.528756
333.738981	27.357655	74.533761
333.238132	40.573381	74.538766
332.899528	36.621157	74.543770
332.713595	32.569744	74.548775
331.588272	39.323247	74.553780
330.826431	32.086110	74.558785
330.358782	40.099318	74.563790
329.389817	38.620273	74.568794
329.109037	35.957938	74.573799
328.245129	42.183505	74.578804
327.997724	35.489347	74.583809
326.772413	38.465189	74.588814
325.762449	33.349549	74.593818
325.608781	39.150242	74.598823
324.332006	38.458521	74.603828
324.335165	30.954882	74.608833
323.465560	47.292074	74.613838
322.878884	40.251481	74.618842
321.795184	36.823654	74.623847
322.006961	38.622051	74.628852
321.674715	34.053772	74.633857
320.566525	39.664400	74.638862
319.490486	41.176315	74.643866
319.078703	33.101197	74.648871
317.746934	48.578575	74.653876
317.007456	35.788294	74.658881
316.501849	30.294123	74.663886
316.086185	33.403549	74.668890
315.744756	38.274106	74.673895
315.247755	38.036074	74.678900
314.547923	33.541061	74.683905
313.361050	33.452849	74.688910
313.126242	33.374341	74.693914
312.591196	28.699910	74.698919
311.493923	35.184147	74.703924
311.264857	25.286497	74.708929
310.645109	29.591761	74.713934
309.638250	34.673470	74.718938
309.166421	34.186006	74.723943
308.200468	34.416753	74.728948
307.717142	28.411160	74.733953
307.525812	37.552075	74.738958
306.387255	39.894927	74.743962
305.967923	33.358130	74.748967
305.056767	39.791522	74.753972
304.278941	31.923219	74.758977
303.405798	38.529691	74.763982
302.600095	29.112566	74.768986
302.506961	30.499432	74.773991
302.233858	34.240442	74.778996
301.177228	27.210149	74.784001
300.601082	24.383720	74.789006
300.127224	28.611482	74.794010
299.321092	33.022506	74.799015
298.181904	33.192557	74.804020
297.723612	32.775402	74.809025
297.090438	33.111735	74.814030
296.522977	26.772033	74.819034
295.852797	27.355485	74.824039
294.962456	38.586237	74.829044
294.569952	30.747018	74.834049
293.481308	39.566891	74.839054
293.208230	32.221912	74.844058
292.059991	31.569350	74.849063
291.356456	33.788696	74.854068
291.249931	30.608235	74.859073
290.694848	26.879429	74.864078
290.202226	30.701483	74.869082
289.362317	26.361927	74.874087
288.392363	40.361836	74.879092
288.214591	23.376172	74.884097
287.066533	31.323247	74.889102
286.286778	31.631815	74.894106
285.654958	31.262166	74.899111
285.127916	30.470764	74.904116
285.081696	22.870601	74.909121
283.935771	29.700661	74.914126
283.156056	33.340621	74.919130
282.606660	25.364492	74.924135
282.047740	38.077827	74.929140
281.794865	24.532749	74.934145
280.343922	26.266422	74.939150
279.518705	34.547748	74.944154
279.403011	31.796336	74.949159
278.769749	39.584918	74.954164
278.251462	31.655557	74.959169
277.679766	34.232418	74.964174
276.573072	36.072474	74.969178
275.406661	35.048446	74.974183
274.406760	38.876536	74.979188
274.847707	35.987477	74.984193
274.085071	31.936636	74.989198
273.793745	31.595464	74.994202
273.598946	30.968550	74.999207
271.982919	36.393484	75.004212
271.397111	24.613014	75.009217
270.947870	29.356793	75.014222
269.850206	27.044869	75.019226
269.166496	24.063207	75.024231
268.708380	31.193772	75.029236
268.537350	33.700379	75.034241
267.500981	37.185003	75.039246
266.546658	37.146148	75.044250
266.259136	22.880341	75.049255
265.637386	31.742546	75.054260
264.586991	30.040250	75.059265
263.978378	27.989086	75.064270
263.417403	36.366429	75.069274
263.221317	30.811318	75.074279
261.860334	34.736037	75.079284
261.085614	30.956861	75.084289
261.154289	29.565220	75.089294
259.809922	37.048215	75.094298
259.934676	29.761753	75.099303
258.648028	35.134968	75.104308
258.195658	36.488285	75.109313
257.307038	33.851599	75.114318
257.055709	30.530575	75.119322
256.106143	31.551507	75.124327
255.228065	43.112512	75.129332
254.920364	45.977266	75.134337
254.359653	36.516182	75.139342
253.558547	33.951333	75.144346
252.840490	39.002890	75.149351
252.063946	38.689236	75.154356
251.505024	25.408190	75.159361
251.344143	37.583585	75.164366
250.218930	39.349061	75.169370
249.689809	25.830815	75.174375
248.942766	38.417326	75.179380
248.337224	37.250589	75.184385
247.379494	31.467237	75.189390
246.558127	33.508245	75.194394
246.265768	31.272223	75.199399
245.921966	40.906220	75.204404
245.287595	29.868248	75.209409
244.190887	33.890559	75.214414
243.706101	33.256515	75.219418
243.444472	29.533464	75.224423
241.929165	37.217466	75.229428
241.576809	28.549972	75.234433
240.922672	37.221164	75.239438
240.671114	35.887573	75.244442
239.883344	32.778496	75.249447
238.785170	34.102390	75.254452
238.399278	44.825519	75.259457
237.801611	30.497618	75.264462
236.877806	32.898405	75.269466
236.158782	37.272797	75.274471
235.314250	41.938295	75.279476
234.884906	38.645417	75.284481
234.505336	33.226754	75.289486
234.159148	36.726886	75.294490
233.191238	29.006837	75.299495
232.576107	31.545360	75.304500
231.910731	31.638552	75.309505
230.687275	35.070783	75.314510
229.902041	32.197708	75.319514
229.428543	31.999470	75.324519
229.213749	39.294768	75.329524
228.646740	31.484683	75.334529
228.124495	29.299516	75.339534
226.989315	38.696554	75.344538
226.777306	29.105843	75.349543
225.762254	35.627313	75.354548
224.873799	33.152833	75.359553
224.221508	38.319428	75.364558
223.945591	32.878658	75.369562
223.374751	35.869829	75.374567
222.830303	45.059826	75.379572
221.997285	33.821448	75.384577
221.099746	33.754317	75.389582
220.590512	37.386604	75.394586
220.142985	34.117371	75.399591
218.655317	42.563180	75.404596
217.922153	30.952839	75.409601
217.742684	37.020830	75.414606
217.757612	34.938572	75.419610
217.223873	28.409560	75.424615
216.394622	32.991522	75.429620
215.307156	29.860408	75.434625
214.189123	31.200737	75.439630
213.159235	30.166743	75.444634
213.194187	28.851932	75.449639
212.486205	31.876479	75.454644
212.273692	29.331131	75.459649
211.528583	36.662862	75.464654
210.300721	43.139111	75.469658
210.301860	33.247403	75.474663
209.118197	41.557816	75.479668
208.880799	27.337107	75.484673
207.578510	35.332739	75.489678
206.974122	43.377285	75.494682
206.442799	36.927985	75.499687
206.157987	43.883989	75.504692
205.840545	37.587094	75.509697
204.250387	32.507002	75.514702
203.497124	43.745842	75.519706
203.279135	27.708484	75.524711
203.039291	41.258390	75.529716
202.454315	37.392623	75.534721
201.625670	41.963433	75.539726
201.104552	37.071511	75.544730
200.341096	34.754810	75.549735
198.650601	38.436837	75.554740
198.705879	41.112666	75.559745
198.214483	33.049638	75.564750
197.399318	29.571472	75.569754
196.771887	25.766667	75.574759
195.918783	37.937569	75.579764
195.592365	35.487927	75.584769
194.986537	32.310567	75.589774
193.510915	38.703375	75.594778
192.920400	30.291440	75.599783
192.052684	35.448784	75.604788
192.365192	29.483224	75.609793
191.911491	32.153149	75.614798
191.150810	32.747000	75.619802
190.213122	36.836398	75.624807
189.397601	41.011429	75.629812
189.311677	27.556162	75.634817
188.285706	32.514068	75.639822
187.134120	39.103947	75.644826
187.203178	31.477713	75.649831
186.304316	40.741884	75.654836
185.369116	33.566867	75.659841
184.548378	37.022437	75.664846
184.192295	45.564784	75.669850
183.960410	38.114866	75.674855
182.353359	42.742148	75.679860
181.629077	32.978746	75.684865
181.230551	35.619084	75.689870
180.868452	37.093898	75.694874
180.583159	30.573616	75.699879
180.351602	41.712364	75.704884
179.293440	37.969557	75.709889
178.534114	36.113574	75.714894
177.507350	33.711364	75.719898
176.868669	30.228605	75.724903
176.389573	34.563846	75.729908
176.175840	35.217086	75.734913
175.284408	30.424177	75.739918
174.209676	37.566115	75.744922
173.762912	34.285706	75.749927
172.270077	37.373362	75.754932
171.609384	30.880726	75.759937
171.161412	32.806817	75.764942
170.423838	31.710881	75.769946
170.277338	27.334978	75.774951
169.867405	36.716637	75.779956
169.656874	31.889498	75.784961
168.415953	30.225018	75.789966
167.225716	29.370094	75.794970
167.236237	34.600295	75.799975
166.379690	34.731794	75.804980
165.902785	31.141175	75.809985
165.276043	36.885205	75.814990
164.498489	39.014631	75.819994
164.080862	26.411584	75.824999
162.941816	41.815280	75.830004
161.983894	32.069043	75.835009
161.991483	35.008820	75.840014
161.480624	37.195942	75.845018
160.550933	25.083685	75.850023
159.922878	32.366142	75.855028
159.064196	23.444037	75.860033
158.098411	28.049017	75.865038
157.198018	36.012075	75.870042
156.880783	32.584733	75.875047
156.385975	34.680687	75.880052
155.753636	36.453265	75.885057
155.674568	28.187332	75.890062
154.662136	34.411932	75.895066
154.075606	21.285640	75.900071
153.494598	36.505250	75.905076
152.619605	36.636756	75.910081
151.525704	34.724852	75.915086
150.578176	34.011867	75.920090
150.698106	27.187660	75.925095
150.152040	32.919833	75.930100
149.360212	37.223825	75.935105
148.497801	36.916225	75.940110
148.019253	34.607925	75.945114
147.429923	27.042857	75.950119
146.329126	26.813228	75.955124
145.767310	31.265672	75.960129
145.457852	29.711105	75.965134
144.564046	38.211033	75.970138
143.813335	23.533634	75.975143
143.397419	35.341445	75.980148
142.817639	36.090596	75.985153
142.016632	32.875262	75.990158
140.849875	34.865767	75.995162
140.394425	32.693632	76.000167
139.585368	35.442244	76.005172
139.383520	29.056076	76.010177
138.537721	30.901957	76.015182
137.498094	26.069731	76.020186
137.088401	34.883353	76.025191
136.755765	42.344105	76.030196
136.233826	34.666041	76.035201
135.704874	31.686290	76.040206
134.033881	41.072181	76.045210
133.870580	29.021163	76.050215
133.165910	36.492406	76.055220
132.955524	29.431555	76.060225
132.573856	29.295343	76.065230
131.380372	33.733323	76.070234
130.981438	31.394799	76.075239
130.158550	34.169861	76.080244
128.979870	37.517075	76.085249
128.496685	32.540510	76.090254
127.892283	38.457151	76.095258
127.544451	34.831383	76.100263
126.546687	37.189609	76.105268
125.842494	36.610166	76.110273
125.084424	37.052798	76.115278
124.455517	42.453012	76.120282
124.551927	28.928603	76.125287
124.292947	33.647666	76.130292
123.121706	39.407683	76.135297
122.747541	33.706678	76.140302
121.266904	48.305309	76.145306
120.833553	30.197108	76.150311
120.378579	38.443395	76.155316
119.217181	38.303499	76.160321
117.768616	39.291987	76.165326
117.440368	40.480755	76.170330
117.106860	35.697992	76.175335
116.600821	42.482722	76.180340
116.249800	36.511711	76.185345
116.120334	38.608979	76.190350
115.369463	34.778772	76.195354
114.295258	31.266485	76.200359
113.453347	41.830564	76.205364
112.803886	39.333687	76.210369
112.089732	38.387684	76.215374
111.496577	43.854793	76.220378
111.171289	31.282894	76.225383
110.346626	41.377463	76.230388
109.481548	36.270199	76.235393
108.801114	39.380427	76.240398
108.044091	39.792095	76.245402
107.716130	34.163692	76.250407
107.096044	33.986651	76.255412
105.987362	28.465653	76.260417
105.606226	30.658959	76.265422
105.195070	34.749674	76.270426
104.505370	26.926313	76.275431
103.331990	28.436804	76.280436
102.864553	35.123340	76.285441
102.571666	31.814191	76.290446
101.642033	41.410075	76.295450
100.876979	22.628930	76.300455
99.888784	25.463518	76.305460
99.577062	25.220585	76.310465
99.112574	20.884208	76.315470
98.483002	35.125748	76.320474
97.448188	27.852975	76.325479
97.091602	32.458122	76.330484
96.223846	31.509642	76.335489
95.761240	31.066012	76.340494
94.807634	34.575555	76.345498
94.413706	26.223883	76.350503
93.385176	35.585681	76.355508
93.339130	33.095875	76.360513
92.816428	24.691681	76.365518
91.325386	32.207355	76.370522
91.069567	25.961886	76.375527
90.679149	29.608939	76.380532
89.911611	26.523661	76.385537
89.153183	32.074757	76.390542
88.129299	36.527483	76.395546
88.021508	28.248326	76.400551
86.984649	41.474629	76.405556
86.302722	31.278489	76.410561
86.122451	29.470081	76.415566
85.777733	35.515481	76.420570
84.966470	30.615302	76.425575
83.775921	29.659407	76.430580
83.192161	34.017334	76.435585
82.213152	40.390156	76.440590
81.351452	35.187588	76.445594
81.309912	31.322614	76.450599
80.560833	30.775345	76.455604
79.757593	32.181728	76.460609
78.725515	31.349840	76.465614
78.205176	38.819089	76.470618
77.547944	34.680353	76.475623
77.106394	40.702491	76.480628
76.803370	40.801470	76.485633
76.332376	32.316571	76.490638
75.316691	46.572218	76.495642
74.610828	34.419633	76.500647
73.953836	44.355993	76.505652
73.191307	38.921698	76.510657
72.343552	33.807132	76.515662
72.092175	41.702742	76.520666
71.386721	28.950915	76.525671
70.335346	29.394504	76.530676
69.705828	39.064059	76.535681
69.292306	31.969362	76.540686
68.736560	35.131634	76.545690
68.300686	38.675173	76.550695
67.066681	31.319329	76.555700
66.667737	33.867381	76.560705
66.095047	33.716955	76.565710
65.660519	36.993042	76.570714
64.559024	30.438644	76.575719
63.727813	39.573208	76.580724
63.192410	30.844764	76.585729
63.121672	39.344498	76.590734
61.568385	39.183391	76.595738
61.391705	27.167837	76.600743
60.275955	37.448096	76.605748
59.927520	31.099305	76.610753
59.821937	27.191632	76.615758
58.645848	25.736319	76.620762
57.814634	24.024915	76.625767
57.385153	32.663122	76.630772
57.130044	34.710883	76.635777
56.059839	27.129208	76.640782
55.807837	28.478581	76.645786
55.247185	26.322521	76.650791
54.015983	32.484387	76.655796
52.911082	31.043710	76.660801
52.796960	33.833045	76.665806
52.050362	34.040445	76.670810
51.873287	33.691540	76.675815
50.491286	33.842498	76.680820
49.633917	27.924369	76.685825
49.126563	23.699947	76.690830
48.640455	29.260011	76.695834
48.633687	29.433323	76.700839
47.307827	28.182497	76.705844
46.698421	32.176556	76.710849
46.240842	27.680719	76.715854
45.558716	27.963114	76.720858
44.852855	22.882647	76.725863
44.103641	25.824289	76.730868
43.428716	27.222886	76.735873
43.331624	23.603085	76.740878
42.110302	34.145773	76.745882
41.729740	28.634157	76.750887
41.042054	29.038684	76.755892
40.369003	29.699239	76.760897
39.002975	31.257381	76.765902
38.428732	26.229344	76.770906
37.918758	23.303194	76.775911
37.622352	24.371644	76.780916
37.282297	31.506049	76.785921
36.513617	24.264636	76.790926
35.415040	38.241612	76.795930
35.181193	31.349785	76.800935
34.435701	34.321974	76.805940
33.183581	33.156398	76.810945
32.707528	28.194810	76.815950
32.298537	32.310024	76.820954
31.996572	31.885039	76.825959
31.117068	33.535414	76.830964
29.832045	38.691309	76.835969
29.475108	38.431661	76.840974
28.956623	35.465130	76.845978
28.939250	33.127507	76.850983
27.717874	44.866988	76.855988
26.911518	40.474765	76.860993
26.597352	36.287084	76.865998
25.577815	44.163622	76.871002
24.719410	32.956893	76.876007
23.954572	40.321627	76.881012
23.640064	37.139738	76.886017
23.530061	34.679058	76.891022
22.475852	36.013619	76.896026
21.879246	26.832285	76.901031
21.117592	31.153617	76.906036
20.332781	37.730767	76.911041
19.609041	32.347069	76.916046
18.513338	32.041207	76.921050
18.205740	32.659630	76.926055
17.811157	38.701345	76.931060
17.759972	24.969379	76.936065
16.601340	29.213522	76.941070
15.531698	34.615500	76.946074
15.280014	29.805301	76.951079
14.623758	30.317330	76.956084
13.403305	32.322993	76.961089
13.294005	22.400120	76.966094
12.258676	32.060312	76.971098
12.075586	21.347638	76.976103
10.990134	21.118174	76.981108
10.136695	25.719702	76.986113
9.936157	15.662092	76.991118
9.184114	29.845288	76.996122
9.242586	28.709197	77.001127
7.861916	24.797540	77.006132
7.317274	32.574886	77.011137
6.768654	24.119498	77.016142
5.335100	35.503405	77.021147
5.032447	32.988922	77.026151
4.401212	27.039136	77.031156
4.497909	33.329357	77.036161