Tue Jun 08 16:14:27 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.954785	88.082346	0.000000
-0.690542	82.574246	0.005005
-2.114778	52.319078	0.010010
-4.227041	0.708893	0.015014
-8.526666	-7.735585	0.020019
-13.900953	3.805251	0.025024
-18.555358	-6.109465	0.030029
-22.738050	13.766621	0.035034
-26.406486	-1.080127	0.040038
-30.627932	4.272136	0.045043
-34.213499	5.113951	0.050048
-37.755297	-0.782336	0.055053
-41.636905	1.591596	0.060058
-45.475414	-14.209576	0.065062
-49.527774	-3.477188	0.070067
-53.779891	-7.683078	0.075072
-56.914448	-6.658075	0.080077
-60.600496	4.384118	0.085082
-63.955422	-3.169213	0.090086
-67.733407	-9.219957	0.095091
-71.652592	-5.767525	0.100096
-75.504451	-11.814671	0.105101
-79.865496	-5.324954	0.110106
-82.853942	-4.740223	0.115110
-86.938530	-10.304191	0.120115
-90.859269	-2.866486	0.125120
-94.066020	-4.233255	0.130125
-98.305103	-5.083540	0.135130
-102.044423	-4.641591	0.140134
-105.367852	-0.511744	0.145139
-108.895448	-6.819718	0.150144
-112.785784	-15.278222	0.155149
-116.951065	-12.841373	0.160154
-120.890683	-15.690093	0.165158
-124.499050	-10.324478	0.170163
-128.826157	-8.932292	0.175168
-132.404035	-14.358127	0.180173
-136.052398	3.095632	0.185178
-139.621722	-4.834919	0.190182
-143.557869	-6.073406	0.195187
-147.079860	-7.204507	0.200192
-150.897867	-6.672055	0.205197
-154.849456	-2.324321	0.210202
-158.177200	-3.184801	0.215206
-162.084609	7.957792	0.220211
-166.016995	8.202788	0.225216
-169.374473	0.020023	0.230221
-173.918674	0.184835	0.235226
-177.232063	-9.397621	0.240230
-181.028794	-1.737182	0.245235
-184.471397	6.115143	0.250240
-188.336082	-3.754836	0.255245
-192.300078	11.454707	0.260250
-195.483659	4.086026	0.265254
-199.763690	-2.412539	0.270259
-204.032289	1.079801	0.275264
-207.470901	-13.011230	0.280269
-211.476109	-3.661971	0.285274
-214.627643	-5.064963	0.290278
-218.347694	-5.969420	0.295283
-222.199138	-3.747343	0.300288
-225.884758	-5.790120	0.305293
-229.917023	-3.323092	0.310298
-233.382707	-9.442644	0.315302
-237.514986	-3.967349	0.320307
-241.146240	-0.705072	0.325312
-244.696057	-4.804668	0.330317
-248.831663	-0.575283	0.335322
-252.474270	-9.433754	0.340326
-256.287667	-5.568291	0.345331
-259.909521	-5.716321	0.350336
-263.688585	-7.001380	0.355341
-267.512680	4.201599	0.360346
-270.850531	-5.751952	0.365350
-274.850526	3.406217	0.370355
-278.740275	-6.843030	0.375360
-282.315284	-7.324317	0.380365
-286.300523	-0.638760	0.385370
-289.991137	-6.395234	0.390374
-293.627750	-2.553749	0.395379
-297.714791	-7.202157	0.400384
-301.306666	-6.734024	0.405389
-305.119462	-0.185392	0.410394
-309.004650	-7.344819	0.415398
-312.956166	-6.112009	0.420403
-316.382227	-0.410836	0.425408
-320.402937	-8.014735	0.430413
-324.396331	-12.499192	0.435418
-327.453817	-7.341993	0.440422
-331.329801	-8.513269	0.445427
-335.142405	-2.181343	0.450432
-338.977304	-10.124575	0.455437
-342.986937	3.006466	0.460442
-346.472229	-5.287633	0.465446
-350.216092	-9.407928	0.470451
-353.933873	-2.823062	0.475456
-357.467479	-10.002887	0.480461
-361.513177	-3.140332	0.485466
-365.295021	-9.190933	0.490470
-369.093900	-5.892303	0.495475
-373.209050	-5.364344	0.500480
-376.353608	-13.060070	0.505485
-380.385735	-3.416342	0.510490
-384.275366	-12.682282	0.515494
-388.411531	-9.099607	0.520499
-391.958953	-12.106541	0.525504
-395.158305	-10.575225	0.530509
-399.045358	-6.638989	0.535514
-402.607315	-10.567827	0.540518
-406.824808	3.363867	0.545523
-410.434837	-4.674321	0.550528
-414.056475	-6.485958	0.555533
-417.828736	-1.650912	0.560538
-421.702800	-9.579058	0.565542
-425.795530	-8.844911	0.570547
-429.455046	-8.897532	0.575552
-432.929760	-13.262071	0.580557
-436.858988	-5.647780	0.585562
-440.635342	-10.415268	0.590566
-444.219420	-3.084380	0.595571
-448.103242	-7.417401	0.600576
-451.419515	-10.478546	0.605581
-455.705865	-5.478698	0.610586
-459.186752	-5.402479	0.615590
-463.292239	-2.760457	0.620595
-467.147846	-7.077383	0.625600
-470.695542	-16.062452	0.630605
-474.458394	-7.282685	0.635610
-478.048962	-12.933004	0.640614
-482.053487	-6.005181	0.645619
-485.694474	-1.654018	0.650624
-489.257944	-8.777292	0.655629
-493.239482	-1.197792	0.660634
-496.786434	-5.048607	0.665638
-500.828330	-4.259960	0.670643
-504.560079	-1.406520	0.675648
-508.383910	-5.556372	0.680653
-512.240163	-0.617635	0.685658
-515.821250	-5.051480	0.690662
-519.446846	-4.412003	0.695667
-523.264292	-3.055181	0.700672
-526.815720	-7.758560	0.705677
-530.807692	-3.092947	0.710682
-534.348729	-0.983864	0.715686
-538.337872	-8.619013	0.720691
-542.596386	-6.707714	0.725696
-545.950392	-7.754037	0.730701
-549.895953	1.867476	0.735706
-553.476370	-3.308504	0.740710
-557.177953	-1.982980	0.745715
-560.571688	-8.040791	0.750720
-564.407492	-15.680513	0.755725
-568.613537	-4.298498	0.760730
-572.385561	-2.810096	0.765734
-576.026119	-4.398893	0.770739
-579.610408	-1.896724	0.775744
-583.114376	-7.853106	0.780749
-587.580491	2.846505	0.785754
-591.314037	-0.416858	0.790758
-594.849554	-4.079302	0.795763
-598.953245	-14.063373	0.800768
-602.000361	-3.624223	0.805773
-605.762915	-4.181609	0.810778
-610.286436	-5.621624	0.815782
-613.574402	-5.889812	0.820787
-617.110091	-5.068329	0.825792
-621.014728	-9.015540	0.830797
-625.099819	-2.552946	0.835802
-628.691413	-12.223843	0.840806
-632.473421	-0.864016	0.845811
-636.311741	-4.396310	0.850816
-639.768530	-10.892015	0.855821
-643.748183	-5.168236	0.860826
-647.303320	-8.304675	0.865830
-651.377762	-2.979853	0.870835
-654.652572	0.352227	0.875840
-658.511220	0.369493	0.880845
-662.583221	1.140166	0.885850
-666.252956	-7.699849	0.890854
-669.846509	-3.492856	0.895859
-673.529105	-3.430794	0.900864
-677.378472	-12.029590	0.905869
-681.457068	-5.339132	0.910874
-685.227224	-7.246228	0.915878
-688.767798	-12.306565	0.920883
-692.508530	1.007918	0.925888
-696.120354	-3.812441	0.930893
-700.653638	-0.726945	0.935898
-704.296858	-4.514485	0.940902
-707.454612	2.636072	0.945907
-711.401336	-7.542970	0.950912
-714.579548	-6.442128	0.955917
-718.672821	-4.141420	0.960922
-722.664407	-4.205089	0.965926
-726.469317	-5.833835	0.970931
-730.819897	-4.189954	0.975936
-733.975439	-6.945330	0.980941
-737.670029	-4.369635	0.985946
-741.524392	-7.585681	0.990950
-745.379441	-4.851397	0.995955
-749.192502	-2.884916	1.000960
-752.782818	-3.074661	1.005965
-756.468219	-0.414086	1.010970
-760.039875	-6.353961	1.015974
-763.684960	-1.825442	1.020979
-767.872989	1.702142	1.025984
-771.665412	-6.123239	1.030989
-775.607978	1.375996	1.035994
-778.799894	0.608720	1.040998
-782.618831	0.237994	1.046003
-786.836416	-5.146550	1.051008
-790.372194	-9.070867	1.056013
-794.308303	5.555682	1.061018
-797.887549	-2.595980	1.066022
-801.673565	-2.849192	1.071027
-805.875066	5.690361	1.076032
-809.268759	-3.821329	1.081037
-812.973556	-3.586404	1.086042
-816.554726	4.204491	1.091046
-820.384182	2.325849	1.096051
-824.553593	4.969305	1.101056
-827.925833	-8.142222	1.106061
-831.612722	-0.358433	1.111066
-835.861584	-0.034835	1.116070
-839.571604	-12.929695	1.121075
-843.411570	4.159143	1.126080
-846.610132	-7.130216	1.131085
-850.737506	-1.633119	1.136090
-854.112469	-18.710157	1.141094
-857.817125	-7.927875	1.146099
-861.883705	4.819030	1.151104
-865.471882	-10.786252	1.156109
-869.157564	-4.507658	1.161114
-873.164531	-6.905210	1.166118
-876.811138	-9.309753	1.171123
-880.812223	-1.886827	1.176128
-884.419808	-12.583738	1.181133
-888.132244	-5.200095	1.186138
-892.026080	-3.370009	1.191142
-895.814954	-5.540524	1.196147
-899.304394	3.081330	1.201152
-902.636851	-7.544386	1.206157
-907.094017	0.147501	1.211162
-911.042363	-10.155783	1.216166
-914.835792	-6.665017	1.221171
-918.482850	-2.845323	1.226176
-921.979410	-7.509229	1.231181
-925.542199	-3.930163	1.236186
-929.135122	-3.863938	1.241190
-933.210540	3.331420	1.246195
-937.090557	3.019471	1.251200
-941.273824	-7.318053	1.256205
-944.721809	1.326714	1.261210
-948.140526	-2.149838	1.266214
-952.196020	-7.892406	1.271219
-956.171052	-1.224224	1.276224
-959.590137	-3.462115	1.281229
-963.571046	-6.057065	1.286234
-967.094905	-9.540019	1.291238
-970.756842	-10.656291	1.296243
-974.769890	-9.284442	1.301248
-978.324566	-0.994333	1.306253
-982.377425	-3.552046	1.311258
-986.121679	-6.577179	1.316262
-989.831334	-4.360239	1.321267
-993.345705	-3.557504	1.326272
-997.240163	-6.203972	1.331277
-1001.082497	-0.912771	1.336282
-1005.142709	-7.998844	1.341286
-1008.369998	-8.143343	1.346291
-1012.391945	-9.364333	1.351296
-1016.128452	-10.050952	1.356301
-1020.056618	2.016708	1.361306
-1023.410281	-3.244364	1.366310
-1026.967085	-6.332432	1.371315
-1030.984757	1.919591	1.376320
-1034.684046	-14.152322	1.381325
-1038.768842	-11.635290	1.386330
-1042.785329	-6.009046	1.391334
-1046.202506	-9.971266	1.396339
-1049.990749	-13.709124	1.401344
-1053.435511	-16.952577	1.406349
-1057.333032	-13.096083	1.411354
-1061.034184	-9.865360	1.416358
-1064.904192	-14.375023	1.421363
-1069.258976	1.219600	1.426368
-1072.827962	-3.176365	1.431373
-1076.386393	-0.888614	1.436378
-1079.659336	-10.731819	1.441382
-1083.381447	-12.461689	1.446387
-1087.874835	-6.578661	1.451392
-1091.549629	-9.510238	1.456397
-1094.908894	-5.634433	1.461402
-1098.754300	-7.759533	1.466406
-1102.582405	-16.899932	1.471411
-1106.236919	-15.430067	1.476416
-1109.961930	-19.148333	1.481421
-1114.142231	1.349392	1.486426
-1118.001450	-6.470891	1.491430
-1121.021278	-8.516307	1.496435
-1125.151454	-15.258685	1.501440
-1128.585054	-16.480733	1.506445
-1132.777022	-14.420830	1.511450
-1136.558665	-17.788716	1.516454
-1140.292108	-10.849260	1.521459
-1144.216945	-0.871250	1.526464
-1147.438235	-8.458051	1.531469
-1151.125337	-1.808755	1.536474
-1155.150619	-5.955380	1.541478
-1158.932895	-5.667775	1.546483
-1163.134052	-3.735727	1.551488
-1166.601110	-13.690769	1.556493
-1170.551201	-2.267333	1.561498
-1174.125861	-13.099871	1.566502
-1177.585036	-3.842410	1.571507
-1181.665975	-6.163017	1.576512
-1185.082914	-10.176077	1.581517
-1189.119208	-2.070316	1.586522
-1192.954913	-8.835172	1.591526
-1196.549374	-13.359664	1.596531
-1200.582332	-11.145044	1.601536
-1203.985625	-15.225556	1.606541
-1208.056833	-6.202016	1.611546
-1211.425957	-11.660779	1.616550
-1215.309397	-11.003278	1.621555
-1219.284372	-3.245100	1.626560
-1223.133088	-15.554872	1.631565
-1226.669239	-6.790564	1.636570
-1230.799546	-16.223511	1.641574
-1234.160442	-9.941202	1.646579
-1238.001829	-12.503799	1.651584
-1241.594155	-15.883972	1.656589
-1245.698395	-3.298041	1.661594
-1249.321841	-7.505298	1.666598
-1253.155311	-14.851087	1.671603
-1257.139763	-7.824217	1.676608
-1260.315028	-12.231585	1.681613
-1264.122617	-9.523945	1.686618
-1267.833853	-11.143026	1.691622
-1271.782150	-11.383733	1.696627
-1275.835439	-1.216987	1.701632
-1279.254284	-11.057453	1.706637
-1283.335199	-8.880304	1.711642
-1286.680407	-14.239302	1.716646
-1290.281523	-17.250452	1.721651
-1294.452983	-3.735248	1.726656
-1298.031541	-15.279436	1.731661
-1302.343120	-15.997671	1.736666
-1305.832358	-7.473053	1.741670
-1309.370672	-7.276554	1.746675
-1313.461911	-8.286815	1.751680
-1316.852975	-14.909254	1.756685
-1320.682477	-5.524534	1.761690
-1324.206061	-10.972457	1.766694
-1328.226520	-18.415514	1.771699
-1332.191762	-11.352804	1.776704
-1335.979506	-15.836074	1.781709
-1339.765865	-12.133809	1.786714
-1343.691459	-18.088137	1.791718
-1346.774861	-10.970064	1.796723
-1350.517227	-11.057401	1.801728
-1354.292178	-19.995902	1.806733
-1358.384992	-8.638583	1.811738
-1362.427699	-11.835899	1.816742
-1365.732085	-9.314863	1.821747
-1369.798250	-10.304903	1.826752
-1373.320313	-9.127934	1.831757
-1377.056424	-11.094324	1.836762
-1380.958241	-1.269271	1.841766
-1384.603701	-15.063932	1.846771
-1388.331986	-7.242205	1.851776
-1392.252336	-14.265062	1.856781
-1396.308869	-10.121237	1.861786
-1400.099399	-6.501089	1.866790
-1403.234058	-11.076751	1.871795
-1407.129410	-2.157054	1.876800
-1410.684771	-10.157913	1.881805
-1414.444124	-5.388994	1.886810
-1418.382884	-9.861243	1.891814
-1422.353335	-5.161833	1.896819
-1426.264910	-5.512509	1.901824
-1429.923799	-9.121455	1.906829
-1433.854799	-6.386939	1.911834
-1437.510917	-6.322054	1.916838
-1440.998642	-10.856372	1.921843
-1445.114988	-5.820062	1.926848
-1448.416609	-16.631347	1.931853
-1452.537306	-5.031149	1.936858
-1456.151180	-5.884087	1.941862
-1459.621262	-8.007411	1.946867
-1463.590125	-6.700322	1.951872
-1467.228111	-13.427825	1.956877
-1471.322365	2.261324	1.961882
-1474.843103	0.695748	1.966886
-1478.920042	-3.534038	1.971891
-1482.805584	1.553044	1.976896
-1486.241190	0.042320	1.981901
-1489.969903	0.054991	1.986906
-1493.458014	1.013088	1.991910
-1497.068837	-5.594726	1.996915
-1501.711957	-7.419005	2.006912
-1502.775529	-2.681428	2.016909
-1499.804068	-1.672311	2.026906
-1497.181200	-7.972765	2.036902
-1494.697471	-7.087728	2.046899
-1493.043011	-10.569551	2.056896
-1491.231367	-5.333193	2.066893
-1489.378471	-2.918204	2.076890
-1487.437241	0.542747	2.086886
-1485.178303	-6.463068	2.096883
-1483.734886	-5.752215	2.106880
-1481.946211	1.446753	2.116877
-1479.571115	-1.522193	2.126874
-1477.907055	-4.081266	2.136870
-1475.817768	-4.519193	2.146867
-1474.343572	-4.619456	2.156864
-1472.124652	3.910965	2.166861
-1470.030570	5.208373	2.176858
-1468.293641	-0.349419	2.186854
-1466.724738	-0.720466	2.196851
-1464.831577	-2.394500	2.206848
-1462.648118	0.086226	2.216845
-1460.554481	-0.291577	2.226842
-1458.897109	3.138718	2.236838
-1457.070879	-3.932254	2.246835
-1455.469189	-12.240383	2.256832
-1453.385632	-4.820159	2.266829
-1451.570001	-4.623779	2.276826
-1449.567122	-7.231565	2.286822
-1447.675663	-7.288102	2.296819
-1445.318621	-5.299978	2.306816
-1444.098436	-2.556139	2.316813
-1442.169671	-4.765465	2.326810
-1439.982957	-3.254735	2.336806
-1438.197333	-2.432320	2.346803
-1436.579039	-9.903476	2.356800
-1434.687393	-6.517766	2.366797
-1432.660406	-5.657376	2.376794
-1430.584663	-4.356403	2.386790
-1428.759429	-3.398909	2.396787
-1426.727334	-0.006891	2.406784
-1425.359012	-6.285833	2.416781
-1423.244704	-3.280224	2.426778
-1421.193060	-4.005692	2.436774
-1419.327197	-6.039005	2.446771
-1417.430855	-7.872833	2.456768
-1415.763301	0.490316	2.466765
-1413.988781	-0.499757	2.476762
-1411.899665	-0.999670	2.486758
-1410.193658	-1.288332	2.496755
-1408.233945	-4.691354	2.506752
-1406.533284	0.322640	2.516749
-1404.101165	-0.998947	2.526746
-1402.434059	-5.397425	2.536742
-1400.800683	-4.696253	2.546739
-1398.906920	-3.877775	2.556736
-1396.659306	0.864817	2.566733
-1395.145646	-7.444772	2.576730
-1393.229420	-4.365995	2.586726
-1391.033687	-3.442092	2.596723
-1389.486066	-5.344448	2.606720
-1387.754156	-7.054772	2.616717
-1385.324178	-2.158938	2.626714
-1383.422718	-4.470649	2.636710
-1381.887870	-5.006544	2.646707
-1380.126362	-9.208607	2.656704
-1377.822051	-6.147087	2.666701
-1376.206117	1.992962	2.676698
-1374.260775	-7.901267	2.686694
-1372.588891	-5.732171	2.696691
-1370.640082	-9.064537	2.706688
-1368.721123	-3.967091	2.716685
-1366.877644	-2.276822	2.726682
-1365.086317	-0.921031	2.736678
-1363.100926	-2.384803	2.746675
-1361.387297	-4.225557	2.756672
-1359.298486	-11.481105	2.766669
-1357.451497	-4.148237	2.776666
-1355.675070	-6.414351	2.786662
-1353.712387	-3.146324	2.796659
-1352.024331	0.567250	2.806656
-1349.658339	0.020994	2.816653
-1348.131794	-1.099954	2.826650
-1345.879526	-5.821826	2.836646
-1344.384090	-1.357462	2.846643
-1342.407626	-2.246242	2.856640
-1340.816186	-3.771963	2.866637
-1338.607753	-0.358416	2.876634
-1336.519327	-4.675900	2.886630
-1335.189057	-9.304999	2.896627
-1333.120951	-6.905167	2.906624
-1330.925127	0.526673	2.916621
-1329.337791	1.579615	2.926618
-1327.371256	-6.534261	2.936614
-1325.670425	-7.463820	2.946611
-1323.739580	0.767994	2.956608
-1321.392213	-2.053828	2.966605
-1319.816931	-5.146145	2.976602
-1318.226695	-5.778081	2.986598
-1316.184978	-6.580045	2.996595
-1314.269277	-6.358901	3.006592
-1312.365146	-4.135216	3.016589
-1310.385887	-3.262615	3.026586
-1308.573371	-4.149303	3.036582
-1306.677210	-11.031463	3.046579
-1304.876875	1.835668	3.056576
-1303.027446	0.068833	3.066573
-1301.027410	-3.361620	3.076570
-1299.153574	-8.369415	3.086566
-1297.322587	-16.084939	3.096563
-1295.304619	-8.455754	3.106560
-1293.707542	-8.921288	3.116557
-1292.041215	-10.087566	3.126554
-1290.003608	-4.475344	3.136550
-1287.916916	-10.929012	3.146547
-1286.140147	-11.277993	3.156544
-1284.076715	-1.793194	3.166541
-1282.261453	-5.120369	3.176538
-1280.530964	-5.467722	3.186534
-1278.509781	-8.428335	3.196531
-1276.863215	-8.325750	3.206528
-1274.989302	-2.221032	3.216525
-1272.999898	-3.630914	3.226522
-1271.041119	-12.615662	3.236518
-1268.928424	-8.212232	3.246515
-1267.638413	-5.964857	3.256512
-1265.398823	-8.835323	3.266509
-1263.596313	-5.868555	3.276506
-1261.823034	-10.056788	3.286502
-1259.588363	-5.988493	3.296499
-1257.978209	-1.899881	3.306496
-1255.970181	0.567616	3.316493
-1254.067890	-1.003559	3.326490
-1252.252331	-1.727128	3.336486
-1250.233818	-7.729993	3.346483
-1248.639536	-5.189852	3.356480
-1246.941613	-4.267716	3.366477
-1244.881728	-3.897806	3.376474
-1242.783883	-7.933894	3.386470
-1241.440887	-2.390467	3.396467
-1239.193557	-8.492303	3.406464
-1237.433351	-8.356262	3.416461
-1235.380597	-7.167433	3.426458
-1233.524855	-8.074160	3.436454
-1231.726524	-7.133693	3.446451
-1229.615086	-6.081802	3.456448
-1228.069618	1.445592	3.466445
-1226.003629	-1.347616	3.476442
-1224.096843	-4.107947	3.486438
-1222.304727	-5.349945	3.496435
-1220.256920	-3.366676	3.506432
-1218.690198	-4.386191	3.516429
-1216.818318	0.422222	3.526426
-1214.538620	-2.715156	3.536422
-1212.878261	-6.629067	3.546419
-1211.031275	-5.000982	3.556416
-1209.116622	-3.839404	3.566413
-1207.289266	-2.599204	3.576410
-1205.420621	-2.542240	3.586406
-1203.543205	-2.074182	3.596403
-1201.652928	2.145377	3.606400
-1199.754909	-7.239141	3.616397
-1197.913605	4.814394	3.626394
-1195.787609	-1.216395	3.636390
-1193.936064	-3.657777	3.646387
-1192.350435	-0.832364	3.656384
-1190.775684	0.379296	3.666381
-1188.347340	-1.086562	3.676378
-1186.500307	-7.687942	3.686374
-1184.897461	-6.360170	3.696371
-1182.975709	-0.543033	3.706368
-1180.892817	-1.050458	3.716365
-1179.122241	-2.947556	3.726362
-1177.214276	-1.569820	3.736358
-1175.362540	-6.521208	3.746355
-1173.305859	-2.773244	3.756352
-1171.880312	-0.937604	3.766349
-1169.413498	2.051870	3.776346
-1168.108108	-4.442655	3.786342
-1165.948964	-4.149429	3.796339
-1164.164349	-9.265155	3.806336
-1162.137264	-4.971059	3.816333
-1160.581725	-8.223548	3.826330
-1158.504181	-9.730321	3.836326
-1156.260766	-14.833537	3.846323
-1154.816448	-11.323053	3.856320
-1153.013252	-5.615172	3.866317
-1150.937483	-8.418323	3.876314
-1148.639627	-5.864591	3.886310
-1147.194601	-3.006321	3.896307
-1145.536243	-3.795329	3.906304
-1143.650211	-1.019508	3.916301
-1141.887452	-0.947889	3.926298
-1139.850195	-4.328939	3.936294
-1137.671031	-3.271242	3.946291
-1135.991755	-2.218204	3.956288
-1133.927194	-3.291166	3.966285
-1132.258538	-0.081219	3.976282
-1130.262446	-4.189497	3.986278
-1128.490725	-3.802849	3.996275
-1126.540686	-8.979770	4.006272
-1124.762862	-2.513060	4.016269
-1122.583146	-1.030203	4.026266
-1120.845862	0.142904	4.036262
-1118.818969	3.323749	4.046259
-1117.453579	-5.369745	4.056256
-1115.218816	-3.181795	4.066253
-1113.623780	-2.945017	4.076250
-1111.555056	-4.805548	4.086246
-1109.719262	-1.322746	4.096243
-1107.611441	-4.460987	4.106240
-1105.794654	-3.281765	4.116237
-1103.993007	-0.441242	4.126234
-1102.051243	-5.039726	4.136230
-1100.329897	-8.010426	4.146227
-1098.760903	-6.579190	4.156224
-1096.800041	-9.166560	4.166221
-1094.678730	-2.910974	4.176218
-1092.482533	0.296537	4.186214
-1090.746008	-12.477204	4.196211
-1089.255189	-9.513747	4.206208
-1087.427362	-5.027313	4.216205
-1085.099537	-9.935529	4.226202
-1083.252872	-6.565241	4.236198
-1081.674543	-5.667161	4.246195
-1079.739018	-8.043873	4.256192
-1077.815207	-5.043309	4.266189
-1076.034171	-6.448148	4.276186
-1073.974334	-9.070288	4.286182
-1072.023482	-5.899681	4.296179
-1070.196155	-5.769563	4.306176
-1068.538245	-3.416538	4.316173
-1066.410982	-5.298956	4.326170
-1064.567499	-11.418708	4.336166
-1062.808624	-9.568731	4.346163
-1060.819800	-0.737708	4.356160
-1059.098532	-4.519749	4.366157
-1056.918159	-3.966901	4.376154
-1055.188279	-4.190357	4.386150
-1053.789644	-4.545847	4.396147
-1051.516736	-5.054218	4.406144
-1049.589040	-7.115776	4.416141
-1047.763692	-4.559107	4.426138
-1045.864229	-7.682490	4.436134
-1043.784042	-6.514084	4.446131
-1042.142171	-5.857701	4.456128
-1040.176784	-8.222530	4.466125
-1038.752063	-9.405719	4.476122
-1036.545839	-5.924833	4.486118
-1034.751430	-13.543878	4.496115
-1033.175621	-2.068707	4.506112
-1030.825483	-6.196630	4.516109
-1028.711672	-3.816344	4.526106
-1026.994379	-0.106065	4.536102
-1025.340426	2.547229	4.546099
-1023.473448	1.945346	4.556096
-1021.466616	-0.820221	4.566093
-1019.367260	-0.537205	4.576090
-1017.702012	-9.470279	4.586086
-1015.752932	-4.500735	4.596083
-1014.048099	-5.572344	4.606080
-1012.233573	-0.335059	4.616077
-1010.374775	-2.954665	4.626074
-1008.255668	-1.829678	4.636070
-1006.661638	-7.069524	4.646067
-1004.630159	-5.174637	4.656064
-1002.547832	-3.267532	4.666061
-1000.689139	-3.969551	4.676058
-999.131209	-3.411375	4.686054
-996.801517	-7.644057	4.696051
-995.411612	-8.014629	4.706048
-993.356900	-10.556414	4.716045
-991.373447	-4.390131	4.726042
-989.297768	-6.475488	4.736038
-987.593656	-6.671966	4.746035
-986.141717	-6.384092	4.756032
-983.958626	-5.604822	4.766029
-982.390266	-1.510498	4.776026
-980.206095	-15.977872	4.786022
-978.198798	-16.413729	4.796019
-976.332837	-10.518539	4.806016
-974.532718	-8.280394	4.816013
-972.922133	-1.180619	4.826010
-970.842246	-6.103123	4.836006
-968.750756	-7.556872	4.846003
-967.095845	-9.914604	4.856000
-965.013748	-4.384538	4.865997
-963.420772	-10.889656	4.875994
-961.808557	-11.186933	4.885990
-959.512310	-5.958422	4.895987
-957.793039	-7.641510	4.905984
-955.570555	0.243634	4.915981
-954.113823	-0.887718	4.925978
-952.033579	-5.670371	4.935974
-950.175749	-6.420040	4.945971
-948.268960	-10.326369	4.955968
-946.155729	-3.532614	4.965965
-945.011781	-4.665594	4.975962
-942.528930	-2.921281	4.985958
-940.958284	-3.595955	4.995955
-938.625760	-5.767671	5.005952
-937.119977	-9.353797	5.015949
-935.353887	-3.931896	5.025946
-933.414817	-5.544816	5.035942
-931.506364	-3.396782	5.045939
-929.081102	-6.100956	5.055936
-927.801851	-1.915875	5.065933
-925.742747	-10.457696	5.075930
-923.761780	-6.920293	5.085926
-922.045634	-9.030448	5.095923
-920.204040	-1.220986	5.105920
-918.484075	-4.285443	5.115917
-916.353747	-4.342437	5.125914
-914.568645	-8.280426	5.135910
-912.411865	-6.944096	5.145907
-910.746510	-4.201024	5.155904
-909.170406	-4.722095	5.165901
-907.208262	0.253958	5.175898
-905.259027	-3.833930	5.185894
-903.393560	-6.752627	5.195891
-901.304150	-5.020975	5.205888
-899.479390	-4.152087	5.215885
-897.608886	-7.596488	5.225882
-895.676632	-3.935701	5.235878
-893.862616	-7.076365	5.245875
-892.081036	-4.987947	5.255872
-890.198030	-5.591338	5.265869
-888.265056	-3.524164	5.275866
-886.109043	-5.277060	5.285862
-884.507563	-12.358251	5.295859
-882.830081	-6.857881	5.305856
-880.783380	-10.404054	5.315853
-878.880338	-8.681897	5.325850
-876.808200	-8.970752	5.335846
-875.216506	-13.508653	5.345843
-873.163862	-11.582556	5.355840
-871.398441	-11.424337	5.365837
-869.309512	-5.478839	5.375834
-867.717764	-5.847658	5.385830
-865.360880	-8.310046	5.395827
-863.636018	-8.045663	5.405824
-862.026794	-19.202807	5.415821
-860.555185	-11.671666	5.425818
-858.184445	-12.993476	5.435814
-856.408057	-13.599101	5.445811
-854.818991	-13.855215	5.455808
-852.690070	-10.526553	5.465805
-850.725986	-9.373295	5.475802
-848.854943	-9.926003	5.485798
-846.367687	-10.413359	5.495795
-845.028265	-6.900560	5.505792
-843.628145	-10.280794	5.515789
-841.200888	-12.125281	5.525786
-839.424949	-6.674990	5.535782
-837.570443	-10.010309	5.545779
-835.602037	-7.803360	5.555776
-833.663298	-0.435776	5.565773
-832.147749	-9.074752	5.575770
-830.399367	-10.148232	5.585766
-828.251520	-11.756631	5.595763
-826.313851	-10.281077	5.605760
-824.038867	-5.315208	5.615757
-822.737942	-11.696643	5.625754
-821.051679	-7.707858	5.635750
-818.884384	-2.913599	5.645747
-816.939636	-11.995763	5.655744
-814.910693	-11.925437	5.665741
-813.082721	-6.500664	5.675738
-811.416542	-13.988940	5.685734
-809.368183	-15.194526	5.695731
-807.642246	-12.800508	5.705728
-805.426528	-8.774546	5.715725
-803.866073	-5.719386	5.725722
-802.396450	-1.715143	5.735718
-800.218856	-8.328068	5.745715
-798.025164	-5.829373	5.755712
-796.323632	-11.208144	5.765709
-794.400105	-6.535253	5.775706
-792.393656	-1.914928	5.785702
-790.708006	-15.326423	5.795699
-788.834576	-1.249948	5.805696
-786.793113	-6.558224	5.815693
-785.188753	4.813766	5.825690
-783.292615	-3.949016	5.835686
-781.063578	-4.628746	5.845683
-779.431891	-1.433250	5.855680
-777.580611	-6.822701	5.865677
-775.916594	-2.206036	5.875674
-773.908848	-2.395658	5.885670
-771.453301	-3.794027	5.895667
-770.089370	-6.849488	5.905664
-768.355596	-9.011618	5.915661
-766.101863	-9.193660	5.925658
-764.656178	-7.291381	5.935654
-762.522894	-8.481485	5.945651
-760.586287	-4.221052	5.955648
-758.774860	-8.827458	5.965645
-756.712688	-11.481076	5.975642
-755.030583	-11.321946	5.985638
-753.125261	-8.294341	5.995635
-751.207095	-17.680973	6.005632
-749.714530	-13.935563	6.015629
-747.623938	-9.754907	6.025626
-745.600123	-7.311208	6.035622
-743.588461	-16.062576	6.045619
-741.740231	-6.340151	6.055616
-739.910891	-5.896834	6.065613
-738.152164	-5.221658	6.075610
-736.492110	-12.166235	6.085606
-734.499044	-11.061766	6.095603
-732.411989	-6.646133	6.105600
-730.332037	-3.543361	6.115597
-729.058771	-6.425955	6.125594
-726.882390	-3.358306	6.135590
-724.950140	-9.395949	6.145587
-723.320156	-11.066389	6.155584
-721.499104	-10.508216	6.165581
-719.251022	-4.982791	6.175578
-717.492337	-8.691297	6.185574
-715.595541	-15.680054	6.195571
-713.491543	-8.836764	6.205568
-711.829298	-8.204301	6.215565
-710.136952	-5.013655	6.225562
-708.261546	-5.608154	6.235558
-705.842651	-6.104645	6.245555
-704.463531	-4.251783	6.255552
-702.718419	-4.691126	6.265549
-700.779436	-3.923565	6.275546
-698.896442	1.363379	6.285542
-696.602936	-7.902302	6.295539
-694.814222	-9.554524	6.305536
-693.132889	-1.208803	6.315533
-691.363266	-0.661946	6.325530
-689.767039	-1.700565	6.335526
-687.548129	-10.309637	6.345523
-685.389839	-8.656094	6.355520
-683.624886	-8.879888	6.365517
-681.921304	-6.966904	6.375514
-679.578501	-11.806750	6.385510
-678.005151	-9.899081	6.395507
-676.154792	-6.110706	6.405504
-674.598615	-7.790990	6.415501
-672.504645	-7.920668	6.425498
-670.618163	-4.878724	6.435494
-668.886559	-13.967731	6.445491
-666.703110	-11.795630	6.455488
-664.979638	-10.097097	6.465485
-663.074109	-13.140741	6.475482
-661.191781	-5.874838	6.485478
-658.924833	-13.656266	6.495475
-657.532929	-9.210221	6.505472
-655.729169	-7.824243	6.515469
-653.613170	-11.308701	6.525466
-651.809418	-13.353956	6.535462
-649.949870	-11.562577	6.545459
-648.215302	-7.594258	6.555456
-646.351995	-2.825988	6.565453
-644.282185	-7.270787	6.575450
-642.598623	-6.306024	6.585446
-640.612768	-6.273671	6.595443
-638.701301	-9.915491	6.605440
-636.723685	-1.154631	6.615437
-635.058138	-0.846779	6.625434
-632.914055	1.043591	6.635430
-631.255139	-6.087697	6.645427
-629.194528	-4.921654	6.655424
-627.582907	-8.279630	6.665421
-625.373512	-8.548052	6.675418
-623.712265	-7.931587	6.685414
-621.807547	-14.449391	6.695411
-619.732446	-7.626779	6.705408
-618.393202	-6.470524	6.715405
-616.536273	-9.712111	6.725402
-614.348025	-5.469099	6.735398
-612.207607	-14.527068	6.745395
-610.465964	-16.850945	6.755392
-608.758040	-11.442626	6.765389
-606.717629	-13.381455	6.775386
-604.943358	-9.224696	6.785382
-602.925902	-11.406198	6.795379
-601.078436	-16.317509	6.805376
-599.252519	-12.476296	6.815373
-597.494751	-15.096973	6.825370
-595.502846	-8.737094	6.835366
-593.809576	-15.028901	6.845363
-591.732069	-15.148206	6.855360
-590.146973	-16.689961	6.865357
-588.227009	-4.886716	6.875354
-586.050169	-6.721293	6.885350
-583.857733	-14.595424	6.895347
-582.465744	-12.831282	6.905344
-580.757120	-8.683403	6.915341
-578.687461	-4.321219	6.925338
-576.549077	-6.730157	6.935334
-575.037172	-2.773395	6.945331
-572.949906	-3.282069	6.955328
-570.918978	-9.012512	6.965325
-569.224563	-1.982270	6.975322
-567.535386	-5.179246	6.985318
-565.234854	-9.575073	6.995315
-563.661935	-12.068378	7.005312
-561.912134	-4.600652	7.015309
-560.036650	-5.321175	7.025306
-558.013515	-4.748601	7.035302
-556.226659	-7.700306	7.045299
-554.271817	-7.936475	7.055296
-552.299186	-4.453972	7.065293
-550.620945	-6.457102	7.075290
-548.586070	2.987583	7.085286
-546.525820	-2.038871	7.095283
-544.712335	-2.067797	7.105280
-542.885574	-9.096251	7.115277
-541.105844	-8.664097	7.125274
-539.376304	-6.518777	7.135270
-537.639019	-4.913065	7.145267
-535.469784	-3.157381	7.155264
-533.570241	-5.090189	7.165261
-531.668008	-0.854176	7.175258
-530.008280	-10.558410	7.185254
-527.936869	-6.932784	7.195251
-525.999076	-8.920366	7.205248
-524.510948	-9.093436	7.215245
-522.602842	-6.577211	7.225242
-520.486607	-1.464178	7.235238
-518.488704	-5.342497	7.245235
-516.708343	-5.790187	7.255232
-514.824774	-1.708654	7.265229
-512.878335	-12.416122	7.275226
-511.096537	-7.926656	7.285222
-509.292306	-8.032232	7.295219
-507.488794	-10.210182	7.305216
-505.478253	-9.378139	7.315213
-503.410772	-9.871531	7.325210
-501.585139	-3.650641	7.335206
-499.986399	-4.452496	7.345203
-497.766477	-6.286520	7.355200
-495.851930	-3.486833	7.365197
-494.250934	-6.026431	7.375194
-492.579522	-2.542804	7.385190
-490.635359	-9.726942	7.395187
-488.476515	-5.346025	7.405184
-486.530888	-2.544948	7.415181
-484.755913	-2.615457	7.425178
-483.190685	-3.157434	7.435174
-481.217343	-11.287182	7.445171
-479.230491	-7.924068	7.455168
-477.208784	-4.018375	7.465165
-475.615948	-1.266238	7.475162
-473.330120	-1.893904	7.485158
-471.576860	-1.097536	7.495155
-469.717150	-4.473127	7.505152
-467.780213	-2.860933	7.515149
-465.953527	3.313951	7.525146
-464.261495	-0.066859	7.535142
-462.389321	-3.365148	7.545139
-460.319766	-1.080522	7.555136
-458.435869	1.235562	7.565133
-457.049915	-0.314270	7.575130
-455.051553	-0.223510	7.585126
-452.888353	-2.700674	7.595123
-450.666407	-6.013517	7.605120
-449.160465	-11.083153	7.615117
-447.406485	-7.159574	7.625114
-445.225793	3.606646	7.635110
-443.518248	0.668587	7.645107
-441.869752	-4.741677	7.655104
-439.937634	-2.042991	7.665101
-437.788591	-1.615664	7.675098
-435.895429	-2.094530	7.685094
-434.254533	-6.096526	7.695091
-432.359193	-0.872435	7.705088
-430.419186	0.897336	7.715085
-428.382394	-1.826481	7.725082
-426.782500	-0.119294	7.735078
-424.948221	0.024132	7.745075
-422.826922	-2.252570	7.755072
-420.979222	2.852443	7.765069
-419.073930	5.362482	7.775066
-417.210682	5.176471	7.785062
-415.583822	-4.108309	7.795059
-413.384218	-10.186959	7.805056
-411.260981	-3.678779	7.815053
-409.785002	-4.014531	7.825050
-408.334394	-8.051059	7.835046
-405.998291	-7.440417	7.845043
-403.948857	-7.467080	7.855040
-402.282317	-11.518518	7.865037
-400.562021	-0.211286	7.875034
-398.477173	-8.758116	7.885030
-396.450326	-5.086441	7.895027
-394.869325	-0.164493	7.905024
-393.015876	-8.412364	7.915021
-390.900636	-7.283639	7.925018
-389.169483	-10.011520	7.935014
-387.201336	-5.716399	7.945011
-385.300790	-4.695488	7.955008
-383.178282	-4.846128	7.965005
-381.662476	-5.095432	7.975002
-379.943699	-9.691339	7.984998
-377.831570	-9.028426	7.994995
-375.647569	-2.855517	8.004992
-374.453901	0.458364	8.014989
-372.451038	-0.301321	8.024986
-370.334134	-2.257518	8.034982
-368.334368	-6.556603	8.044979
-366.652097	-4.195614	8.054976
-364.544214	-5.791010	8.064973
-362.791915	-7.239250	8.074970
-360.911260	-5.692443	8.084966
-359.104251	-3.713680	8.094963
-357.324879	-6.477487	8.104960
-355.383721	-9.286040	8.114957
-353.237102	-3.220527	8.124954
-351.709399	-1.274076	8.134950
-349.673992	-5.879630	8.144947
-348.027044	-4.991466	8.154944
-346.301650	-5.991654	8.164941
-344.202409	1.420979	8.174938
-342.026085	-5.668955	8.184934
-340.160009	-9.479137	8.194931
-338.229451	-1.998045	8.204928
-336.741028	-0.402124	8.214925
-334.915342	-7.473403	8.224922
-332.711888	-4.041060	8.234918
-330.680487	-1.589369	8.244915
-329.044641	-8.522559	8.254912
-327.269057	-4.744514	8.264909
-325.362357	3.001916	8.274906
-323.175293	-3.695034	8.284902
-321.787193	-3.922807	8.294899
-320.222273	-0.727923	8.304896
-317.701933	0.946698	8.314893
-315.883605	1.820891	8.324890
-313.998076	-1.940847	8.334886
-312.302460	-4.271343	8.344883
-310.107919	-0.628390	8.354880
-308.125306	-6.613655	8.364877
-306.796965	-2.079906	8.374874
-304.661621	-2.276974	8.384870
-302.896173	0.310854	8.394867
-300.907161	-5.014312	8.404864
-299.056944	-4.240435	8.414861
-297.172471	-0.364465	8.424858
-295.395452	-0.486233	8.434854
-293.668361	-6.114258	8.444851
-291.710300	-2.095590	8.454848
-289.742968	-1.540985	8.464845
-287.505259	-6.280809	8.474842
-286.124155	-3.132635	8.484838
-284.050387	-5.207071	8.494835
-282.111223	-7.865862	8.504832
-280.271711	-4.941754	8.514829
-278.461927	-6.170203	8.524826
-276.615060	-5.698870	8.534822
-274.362624	-4.358073	8.544819
-272.709446	-3.477272	8.554816
-270.944213	-4.530901	8.564813
-269.272485	-6.132066	8.574810
-267.282948	-1.741750	8.584807
-265.341504	-0.849132	8.594803
-263.332334	0.716777	8.604800
-261.396921	4.742508	8.614797
-259.544716	-1.950335	8.624794
-257.908539	2.851151	8.634791
-255.945123	-0.932224	8.644787
-254.021742	-1.884527	8.654784
-252.052453	-1.070189	8.664781
-250.361459	2.310586	8.674778
-248.257188	0.725347	8.684775
-246.490147	-10.670558	8.694771
-244.434139	-3.318038	8.704768
-242.822259	-5.601345	8.714765
-240.704190	-2.370885	8.724762
-239.247538	-1.843279	8.734759
-237.504418	0.126339	8.744755
-235.363054	-0.184760	8.754752
-233.223448	-6.743506	8.764749
-231.371782	2.876639	8.774746
-229.517661	-1.744806	8.784743
-227.638923	-4.943745	8.794739
-226.027959	-5.594653	8.804736
-223.998381	-5.141199	8.814733
-222.307666	-7.306808	8.824730
-220.274454	-7.814743	8.834727
-218.448994	-7.195857	8.844723
-216.398457	-4.464419	8.854720
-214.424646	-3.759525	8.864717
-212.524702	-13.890998	8.874714
-210.658849	-11.991823	8.884711
-208.843172	-11.741571	8.894707
-207.280158	-13.339482	8.904704
-205.209060	-14.693738	8.914701
-203.538430	-12.364282	8.924698
-201.448504	-12.115614	8.934695
-199.516869	-13.760145	8.944691
-197.329924	-16.843174	8.954688
-196.022430	-15.533136	8.964685
-194.096192	-15.941298	8.974682
-192.163876	-6.977590	8.984679
-190.234096	-15.563745	8.994675
-188.128012	-13.641737	9.004672
-186.571486	-12.155063	9.014669
-184.769419	-15.837224	9.024666
-182.958869	-9.317582	9.034663
-180.890798	-11.070081	9.044659
-178.800848	-12.671802	9.054656
-177.096260	-15.020387	9.064653
-175.226260	-13.052350	9.074650
-173.590155	-12.657070	9.084647
-171.446030	-10.484292	9.094643
-169.546946	-7.708283	9.104640
-167.536449	-7.381162	9.114637
-165.332038	-8.793044	9.124634
-163.860197	-9.501088	9.134631
-162.161412	-8.267631	9.144627
-160.113625	-12.807649	9.154624
-158.718582	-12.882824	9.164621
-156.880251	-14.442568	9.174618
-154.716032	-14.244956	9.184615
-152.547333	-14.395899	9.194611
-150.850287	-18.352101	9.204608
-148.920223	-17.698562	9.214605
-147.071677	-14.101711	9.224602
-144.982870	-15.898062	9.234599
-143.338007	-19.371053	9.244595
-141.747234	-14.764088	9.254592
-139.619732	-13.025552	9.264589
-137.479853	-9.845022	9.274586
-135.860593	-16.004639	9.284583
-133.922984	-10.208666	9.294579
-131.929436	-9.472736	9.304576
-130.250051	-7.792509	9.314573
-128.742116	-11.538032	9.324570
-126.407012	-8.643122	9.334567
-124.230631	-6.445816	9.344563
-122.580993	-8.529651	9.354560
-121.093041	-5.570082	9.364557
-119.140014	-7.199674	9.374554
-116.983943	-9.602741	9.384551
-115.172644	-4.394517	9.394547
-113.118540	-6.447326	9.404544
-111.766019	-6.460260	9.414541
-109.530651	-4.080197	9.424538
-107.668768	-3.719658	9.434535
-105.567427	-4.570020	9.444531
-103.810383	-3.046563	9.454528
-102.253174	-7.176773	9.464525
-100.321787	-4.168747	9.474522
-98.404107	-3.079116	9.484519
-96.336941	-4.775303	9.494515
-94.628137	-7.453402	9.504512
-92.444628	-1.997566	9.514509
-90.678333	-5.643525	9.524506
-88.956857	-0.396567	9.534503
-86.947056	-3.643617	9.544499
-85.130857	2.308763	9.554496
-83.108343	-7.011369	9.564493
-81.431856	-3.727632	9.574490
-79.682460	1.123280	9.584487
-77.828374	-2.846393	9.594483
-75.484936	-2.875107	9.604480
-73.912844	-4.199461	9.614477
-71.877843	0.726971	9.624474
-70.270503	-0.825932	9.634471
-68.511848	-4.388764	9.644467
-66.663098	-4.570564	9.654464
-64.332311	-3.118996	9.664461
-62.589905	-2.453001	9.674458
-60.710609	1.750414	9.684455
-58.888422	4.497768	9.694451
-56.889320	0.716651	9.704448
-55.240858	-4.676099	9.714445
-53.178719	-0.838387	9.724442
-51.509474	1.064536	9.734439
-49.312820	-3.110890	9.744435
-47.697218	-0.054222	9.754432
-45.896064	-4.917874	9.764429
-43.930159	-4.743113	9.774426
-42.000954	-7.025041	9.784423
-40.338962	-7.730479	9.794419
-38.305666	-11.134881	9.804416
-36.220406	-8.406149	9.814413
-34.258983	-8.313611	9.824410
-32.666750	-3.404509	9.834407
-30.853505	-4.258395	9.844403
-28.971909	-1.726728	9.854400
-26.629306	-8.750984	9.864397
-25.377801	-7.205230	9.874394
-23.345201	-4.641752	9.884391
-21.353186	-5.055587	9.894387
-19.535987	-7.397343	9.904384
-17.500804	-6.880337	9.914381
-15.586397	-4.855819	9.924378
-13.882784	-5.162892	9.934375
-12.238887	-2.365582	9.944371
-10.054987	-12.382460	9.954368
-8.170507	-1.864762	9.964365
-6.351949	-4.611053	9.974362
-5.151415	15.640719	9.984359
-3.711856	44.658940	9.994355
-2.410742	96.641777	10.004352
-0.992184	157.036662	10.014349
0.000000	211.253568	10.019354
1.018967	248.560741	10.024359
1.260080	286.575297	10.029363
1.757836	308.109076	10.034368
2.772992	338.095886	10.039373
2.951410	357.909438	10.044378
3.348146	380.619536	10.049383
3.222372	392.064335	10.054387
3.336949	397.326079	10.059392
3.515370	401.467712	10.064397
3.895140	424.303541	10.069402
4.222948	432.178104	10.074407
4.046187	433.897061	10.079411
3.958864	440.804691	10.084416
4.278167	442.699107	10.089421
3.898138	452.932727	10.094426
4.045197	449.432016	10.099431
4.111995	450.021360	10.104435
4.233381	453.121248	10.109440
4.611349	448.791896	10.114445
4.260731	454.273155	10.119450
4.187126	456.065213	10.124455
4.190237	469.530260	10.129459
4.455847	459.722874	10.134464
4.638122	452.111411	10.139469
4.604537	467.453336	10.144474
4.407634	461.636556	10.149479
4.692896	457.550852	10.154483
4.625659	458.647108	10.159488
4.589919	458.068289	10.164493
4.318336	471.869770	10.169498
5.119283	479.164301	10.174503
5.182974	489.898157	10.179507
4.571687	475.262874	10.184512
4.954590	483.124464	10.189517
4.902117	502.141372	10.194522
5.427798	507.124250	10.199527
5.259651	506.501818	10.204531
5.396079	515.911949	10.209536
5.250303	507.456739	10.214541
5.084068	499.781461	10.219546
5.375953	499.731838	10.224551
5.341492	515.122117	10.229555
5.543872	519.579400	10.234560
5.693693	517.970900	10.239565
5.378271	509.294522	10.244570
5.280086	504.997852	10.249575
5.367775	515.026188	10.254579
5.261138	520.499187	10.259584
5.408792	531.606688	10.264589
5.354587	536.460855	10.269594
5.712325	527.770487	10.274599
5.456053	540.276289	10.279603
5.587540	529.351893	10.284608
5.740980	532.653926	10.289613
5.568230	543.962422	10.294618
5.906583	561.126262	10.299623
6.062695	563.897334	10.304627
6.187121	564.792186	10.309632
6.174631	565.920508	10.314637
6.085456	572.275109	10.319642
6.242297	570.263176	10.324647
6.411778	582.039187	10.329651
6.275594	570.880404	10.334656
6.404564	577.681931	10.339661
6.174345	571.815166	10.344666
6.292768	573.012223	10.349671
6.267939	577.485192	10.354675
6.337131	581.484950	10.359680
6.513262	577.267931	10.364685
6.385626	579.219263	10.369690
7.067668	574.660902	10.374695
6.978727	579.861686	10.379699
6.811180	585.362520	10.384704
7.056360	581.415100	10.389709
6.839651	587.055807	10.394714
6.476269	587.727206	10.399719
6.645021	591.973177	10.404723
6.801782	598.237858	10.409728
6.748409	598.953204	10.414733
6.727559	599.635738	10.419738
7.045734	591.894724	10.424743
6.974595	600.661174	10.429747
6.736793	599.408858	10.434752
6.866451	603.728245	10.439757
6.802254	619.884756	10.444762
7.241956	619.079940	10.449767
7.218400	623.703095	10.454771
7.014102	631.644918	10.459776
7.356737	630.974373	10.464781
7.019681	637.804124	10.469786
7.214701	628.472539	10.474791
7.324444	626.353809	10.479795
7.199933	640.997436	10.484800
7.415652	643.474492	10.489805
7.405987	665.584049	10.494810
7.645027	668.701306	10.499815
7.708473	674.692288	10.504819
7.840688	676.419870	10.509824
7.998654	672.546196	10.514829
7.863000	684.725912	10.519834
7.864680	679.573274	10.524839
7.704987	686.124746	10.529843
7.889518	683.253070	10.534848
7.717933	683.040553	10.539853
7.805288	686.701310	10.544858
7.896300	677.307796	10.549863
7.789666	685.969856	10.554867
8.011549	695.577808	10.559872
8.332183	703.142298	10.564877
8.070775	712.070511	10.569882
8.536947	710.179202	10.574887
8.325246	716.224877	10.579891
8.336288	714.474762	10.584896
8.421908	706.535150	10.589901
8.653075	715.028783	10.594906
8.777236	710.252231	10.599911
8.561486	717.155556	10.604915
8.419463	717.877819	10.609920
8.633815	722.748362	10.614925
8.384406	717.174169	10.619930
8.175710	723.462880	10.624935
8.521074	737.208152	10.629939
8.740767	749.815664	10.634944
9.248197	751.771019	10.639949
8.786004	762.880622	10.644954
8.969169	753.766913	10.649959
9.097509	759.608251	10.654963
8.991829	761.547156	10.659968
9.173723	761.235346	10.664973
8.911636	771.669603	10.669978
8.824631	763.381410	10.674983
9.152215	767.453751	10.679987
9.211169	762.662706	10.684992
9.232804	761.652072	10.689997
8.977125	765.895472	10.695002
9.543136	783.340648	10.700007
9.531427	800.233992	10.705011
9.359949	795.218373	10.710016
9.621598	796.702332	10.715021
9.455919	805.286163	10.720026
9.911998	807.021386	10.725031
9.691993	807.737287	10.730035
9.479979	811.855188	10.735040
9.744696	804.054947	10.740045
9.524066	810.354817	10.745050
9.745811	808.023440	10.750055
9.729080	805.183883	10.755059
9.713344	812.188743	10.760064
9.627613	809.963375	10.765069
9.452053	836.076163	10.770074
9.773540	830.681143	10.775079
10.129586	839.280535	10.780083
9.683621	850.582414	10.785088
10.134098	846.096050	10.790093
10.208073	845.408800	10.795098
10.260226	847.566571	10.800103
10.154551	848.217476	10.805107
10.324662	855.046412	10.810112
10.480302	861.737702	10.815117
10.554369	862.350289	10.820122
10.312267	871.761198	10.825127
10.536661	878.208998	10.830131
10.554590	875.619667	10.835136
10.880245	870.626546	10.840141
10.694491	879.885695	10.845146
10.957586	877.102748	10.850151
10.915271	880.407631	10.855155
10.925186	884.363947	10.860160
10.927212	878.686584	10.865165
11.223404	884.919579	10.870170
10.989415	873.083014	10.875175
11.333434	877.043225	10.880179
10.836671	884.721510	10.885184
11.190108	877.769696	10.890189
10.871003	884.890157	10.895194
10.740299	881.891709	10.900199
10.972169	890.284659	10.905203
11.031164	885.272520	10.910208
11.169582	887.359059	10.915213
10.834284	893.111787	10.920218
10.983534	907.246095	10.925223
11.248958	916.126329	10.930227
11.377330	916.005270	10.935232
11.442068	919.880748	10.940237
11.057437	926.827333	10.945242
11.241345	918.510764	10.950247
11.390595	929.767090	10.955251
11.726180	939.793061	10.960256
12.176937	947.842198	10.965261
11.479561	954.716894	10.970266
11.937619	950.264727	10.975271
11.991825	952.349529	10.980275
11.694035	960.590573	10.985280
12.051720	954.080100	10.990285
11.822892	961.445246	10.995290
12.160626	958.461200	11.000295
11.853357	957.079845	11.005299
11.959912	969.229304	11.010304
12.524856	958.088578	11.015309
12.030981	961.225379	11.020314
12.364519	959.642965	11.025319
12.202024	964.837541	11.030323
12.072133	963.484192	11.035328
12.171237	966.936554	11.040333
12.005236	973.604885	11.045338
12.232044	979.436526	11.050343
12.231910	992.062190	11.055347
12.239076	999.224259	11.060352
12.632589	1000.630760	11.065357
12.350907	998.373832	11.070362
13.019590	1000.024071	11.075367
12.711511	1000.985608	11.080371
12.739898	1002.856160	11.085376
13.013463	1003.243494	11.090381
12.727970	1009.798118	11.095386
12.935251	1008.442611	11.100391
13.128080	1007.398265	11.105395
13.131330	1009.140103	11.110400
13.085881	1002.643469	11.115405
12.985978	1008.616798	11.120410
13.009219	1009.651000	11.125415
13.539449	1026.167455	11.130419
13.427423	1024.286433	11.135424
13.168183	1007.532524	11.140429
13.307338	1020.017486	11.145434
13.402150	1027.415591	11.150439
13.612213	1032.079336	11.155443
13.110602	1028.864588	11.160448
13.618678	1028.900266	11.165453
13.331756	1037.939618	11.170458
13.460269	1041.604849	11.175463
13.489633	1041.035371	11.180467
13.336215	1036.472498	11.185472
13.964445	1041.857572	11.190477
13.927038	1039.964149	11.195482
13.655433	1037.306014	11.200487
13.672047	1041.346089	11.205491
13.387473	1041.550045	11.210496
13.756623	1057.168100	11.215501
13.931463	1068.830271	11.220506
13.871170	1065.796424	11.225511
14.275441	1064.819242	11.230515
14.298777	1071.305544	11.235520
14.178051	1071.732065	11.240525
14.086919	1079.446289	11.245530
14.052549	1074.390492	11.250535
14.424388	1068.188598	11.255539
14.344412	1071.312083	11.260544
14.368254	1067.756967	11.265549
14.244062	1070.078033	11.270554
14.257076	1074.455050	11.275559
14.514306	1072.892815	11.280563
14.616242	1070.936811	11.285568
14.898194	1071.252446	11.290573
14.510164	1079.661393	11.295578
14.936950	1077.672585	11.300583
14.869482	1074.634835	11.305587
14.561286	1079.926273	11.310592
14.652894	1074.272164	11.315597
14.738195	1081.371136	11.320602
15.238634	1082.752995	11.325607
15.030533	1078.373171	11.330611
15.073198	1082.117079	11.335616
15.020001	1085.598740	11.340621
14.679920	1092.031704	11.345626
15.162854	1097.869607	11.350631
15.111467	1101.487935	11.355635
14.987360	1113.911926	11.360640
15.105837	1114.237433	11.365645
14.837802	1119.759236	11.370650
14.763287	1111.409111	11.375655
14.953203	1117.979371	11.380659
14.901581	1129.469231	11.385664
15.534749	1138.573118	11.390669
15.395137	1143.629618	11.395674
15.713438	1139.721232	11.400679
16.082158	1140.488573	11.405683
15.798387	1146.345849	11.410688
16.192986	1141.002529	11.415693
16.127789	1138.361091	11.420698
15.920470	1119.683674	11.425703
15.905598	1110.028975	11.430707
15.736383	1106.691690	11.435712
16.262501	1108.505730	11.440717
15.981931	1105.834909	11.445722
15.906414	1107.637632	11.450727
16.334286	1107.844958	11.455731
15.868016	1116.309577	11.460736
16.320642	1124.262170	11.465741
16.410834	1140.740907	11.470746
16.162152	1124.772961	11.475751
16.381829	1125.428487	11.480755
16.102692	1126.022303	11.485760
16.600684	1135.914765	11.490765
16.495106	1146.647306	11.495770
16.571927	1148.526941	11.500775
16.624492	1145.426754	11.505779
16.749751	1144.750435	11.510784
17.214832	1126.321668	11.515789
16.333938	1119.087965	11.520794
16.543977	1114.359329	11.525799
16.672151	1129.094297	11.530803
16.624905	1142.587902	11.535808
17.065508	1141.097245	11.540813
16.585232	1154.149973	11.545818
16.510872	1146.044147	11.550823
16.695287	1146.402165	11.555827
16.238499	1151.530419	11.560832
16.495172	1146.180747	11.565837
16.270404	1163.853520	11.570842
16.941402	1167.454976	11.575847
17.020603	1165.251410	11.580851
16.570246	1171.668183	11.585856
17.191891	1173.616247	11.590861
17.527116	1170.933384	11.595866
17.299168	1172.956462	11.600871
17.314748	1172.326579	11.605875
17.197596	1179.806891	11.610880
17.421739	1168.422081	11.615885
17.564159	1192.593296	11.620890
17.902725	1201.639180	11.625895
17.671241	1183.594651	11.630899
17.780815	1177.903477	11.635904
17.944855	1172.358098	11.640909
17.822180	1162.940931	11.645914
17.845628	1165.422223	11.650919
18.079533	1170.906928	11.655923
18.015518	1177.506147	11.660928
17.810981	1167.242086	11.665933
17.743113	1170.564832	11.670938
17.665105	1163.188312	11.675943
17.949703	1175.333457	11.680947
17.858494	1195.472992	11.685952
18.263284	1199.960898	11.690957
18.292637	1197.971534	11.695962
18.279795	1201.389458	11.700967
18.296102	1197.579813	11.705971
18.329470	1204.697615	11.710976
18.778069	1199.733442	11.715981
18.361768	1199.955248	11.720986
18.542409	1193.242136	11.725991
18.942479	1193.850550	11.730995
18.688922	1187.820578	11.736000
18.297106	1185.162108	11.741005
18.461017	1198.680345	11.746010
18.508432	1208.978535	11.751015
18.681349	1204.694005	11.756019
18.153165	1203.183135	11.761024
19.021404	1201.365332	11.766029
18.692388	1209.888179	11.771034
18.745426	1202.073904	11.776039
19.009664	1206.213275	11.781043
18.442440	1205.967138	11.786048
18.987651	1203.330371	11.791053
18.738225	1204.632787	11.796058
18.593393	1219.512941	11.801063
19.103339	1222.978207	11.806067
18.822272	1235.923819	11.811072
19.350179	1234.082260	11.816077
19.167340	1237.951319	11.821082
19.698745	1224.895737	11.826087
19.714901	1219.875441	11.831091
19.293029	1224.535884	11.836096
19.496164	1227.875730	11.841101
19.550543	1225.545357	11.846106
19.726690	1224.363330	11.851111
19.987921	1225.546215	11.856115
19.634564	1228.892661	11.861120
19.978146	1227.786926	11.866125
19.529043	1234.850096	11.871130
19.633624	1232.088741	11.876135
20.033493	1232.685349	11.881139
19.519570	1233.704693	11.886144
19.924592	1234.329234	11.891149
20.001243	1233.112160	11.896154
20.135841	1234.760054	11.901159
20.029798	1232.442975	11.906163
19.880057	1234.451468	11.911168
19.956454	1231.699682	11.916173
20.003825	1228.315761	11.921178
19.975881	1228.391636	11.926183
19.916607	1226.687073	11.931187
19.949714	1236.279568	11.936192
20.290706	1249.172612	11.941197
20.265582	1262.564631	11.946202
20.481037	1253.634966	11.951207
20.167826	1257.714676	11.956211
20.464340	1266.682939	11.961216
20.608976	1258.880167	11.966221
20.355758	1259.846916	11.971226
20.548076	1263.107702	11.976231
20.856381	1256.769784	11.981235
20.690402	1263.392443	11.986240
20.626060	1263.291794	11.991245
20.842285	1261.510779	11.996250
20.603873	1265.468716	12.001255
20.919622	1263.362342	12.006259
20.509535	1268.391836	12.011264
20.942023	1269.299436	12.016269
20.724979	1281.337648	12.021274
21.030409	1270.720416	12.026279
21.228525	1264.717577	12.031283
20.786465	1271.659554	12.036288
21.236923	1278.920220	12.041293
20.723349	1282.602047	12.046298
21.160065	1284.619335	12.051303
21.074311	1288.017411	12.056307
20.784875	1283.576868	12.061312
21.189610	1284.160407	12.066317
20.967657	1280.770547	12.071322
21.309204	1284.190490	12.076327
21.341785	1265.637556	12.081331
20.954088	1269.042004	12.086336
21.397101	1249.686074	12.091341
21.025134	1266.194843	12.096346
21.056005	1263.344672	12.101351
21.345391	1263.286795	12.106355
21.230753	1261.676985	12.111360
21.323666	1256.449303	12.116365
21.057515	1260.060674	12.121370
21.194917	1264.337864	12.126375
21.553468	1261.823093	12.131379
21.459882	1262.376020	12.136384
21.077436	1245.672585	12.141389
21.356503	1232.785791	12.146394
21.187994	1227.410702	12.151399
21.325780	1222.152837	12.156403
21.165940	1233.225141	12.161408
20.998983	1225.818447	12.166413
21.034517	1231.574031	12.171418
20.798065	1228.404566	12.176423
21.073158	1226.497408	12.181427
21.171411	1229.327467	12.186432
21.247831	1227.822272	12.191437
21.466194	1238.153145	12.196442
21.055234	1231.711981	12.201447
21.034296	1231.885340	12.206451
20.785266	1237.860247	12.211456
21.305328	1231.924589	12.216461
21.287198	1231.842069	12.221466
21.231682	1229.879490	12.226471
21.314137	1229.782882	12.231475
21.123304	1234.567137	12.236480
21.213837	1219.673445	12.241485
21.068012	1212.869062	12.246490
20.999464	1211.463725	12.251495
20.918082	1199.123899	12.256499
20.595751	1209.665883	12.261504
21.082047	1224.668357	12.266509
21.026985	1225.215466	12.271514
21.070633	1235.467740	12.276519
21.061675	1238.916586	12.281523
20.929276	1242.152121	12.286528
20.873633	1233.026974	12.291533
21.085121	1241.622560	12.296538
21.372663	1244.358192	12.301543
21.443524	1235.765176	12.306547
20.738496	1230.350235	12.311552
21.015877	1226.573978	12.316557
20.942076	1236.326911	12.321562
20.843055	1239.518432	12.326567
21.092755	1240.586453	12.331571
21.020594	1236.980258	12.336576
21.397898	1236.753358	12.341581
21.392438	1232.184795	12.346586
20.978709	1222.582230	12.351591
21.292973	1208.976518	12.356595
21.277270	1217.048933	12.361600
21.375916	1212.567922	12.366605
21.442761	1212.777547	12.371610
21.354640	1208.568168	12.376615
21.296975	1205.065286	12.381619
21.071194	1207.475238	12.386624
20.848403	1205.993321	12.391629
21.018172	1215.436449	12.396634
21.055368	1217.873945	12.401639
21.235642	1210.602329	12.406643
20.870943	1218.817875	12.411648
20.946183	1210.304649	12.416653
20.706987	1214.010469	12.421658
21.048751	1222.698182	12.426663
21.194973	1210.573139	12.431667
20.806051	1217.434139	12.436672
20.927173	1212.318478	12.441677
20.894173	1220.854129	12.446682
21.303689	1218.032597	12.451687
21.094453	1221.437226	12.456691
21.090195	1214.088695	12.461696
21.142609	1222.570622	12.466701
20.879772	1225.159432	12.471706
20.891261	1219.695062	12.476711
21.109285	1221.265097	12.481715
21.077122	1228.053878	12.486720
21.255858	1221.991614	12.491725
21.131913	1217.694427	12.496730
21.106607	1217.292213	12.501735
21.109967	1215.349541	12.506739
21.211746	1221.314029	12.511744
21.220743	1219.784474	12.516749
21.074252	1202.157197	12.521754
21.111662	1198.513672	12.526759
21.276584	1191.155881	12.531763
21.180745	1198.321887	12.536768
21.145073	1191.078227	12.541773
21.275583	1194.285648	12.546778
20.966351	1192.174732	12.551783
21.094397	1189.840417	12.556787
21.015400	1192.594282	12.561792
21.190533	1187.834108	12.566797
21.062140	1191.556451	12.571802
21.026079	1191.936879	12.576807
21.012357	1190.133324	12.581811
21.110401	1190.562206	12.586816
20.758144	1189.520125	12.591821
21.168383	1200.633607	12.596826
20.987670	1200.798046	12.601831
21.248355	1194.336474	12.606835
20.600670	1201.498811	12.611840
20.888262	1202.079932	12.616845
21.021211	1202.070193	12.621850
20.750446	1202.120597	12.626855
20.977890	1199.331865	12.631859
20.378416	1204.285652	12.636864
21.068897	1212.771856	12.641869
20.877557	1226.799061	12.646874
21.118022	1232.105820	12.651879
21.427587	1224.180048	12.656883
21.239079	1222.081981	12.661888
21.088596	1204.426965	12.666893
21.181290	1210.243795	12.671898
21.249361	1206.516062	12.676903
21.390615	1201.280110	12.681907
20.594918	1209.638630	12.686912
21.206259	1199.878477	12.691917
21.045379	1203.092835	12.696922
21.084605	1202.615214	12.701927
21.249820	1203.287582	12.706931
21.075835	1199.975174	12.711936
21.090902	1202.841597	12.716941
20.980458	1204.791242	12.721946
21.142710	1208.994681	12.726951
21.060739	1200.104202	12.731955
20.871441	1211.837205	12.736960
21.044108	1210.334851	12.741965
21.285278	1215.371875	12.746970
21.072861	1212.244082	12.751975
21.293458	1210.555482	12.756979
21.255042	1226.497803	12.761984
21.050596	1206.494641	12.766989
20.811618	1210.511478	12.771994
21.084229	1206.127748	12.776999
21.276792	1211.416660	12.782003
20.851367	1216.339029	12.787008
21.052245	1216.223694	12.792013
21.018872	1215.571019	12.797018
20.732656	1205.132645	12.802023
20.829947	1207.662073	12.807027
20.915331	1208.723527	12.812032
21.007840	1210.343898	12.817037
21.095117	1211.735821	12.822042
21.136884	1209.326296	12.827047
21.184658	1204.531507	12.832051
21.253008	1214.612951	12.837056
21.808823	1217.349949	12.842061
21.625549	1207.481298	12.847066
21.258638	1196.821500	12.852071
21.294164	1181.641220	12.857075
21.446501	1184.077915	12.862080
20.975868	1180.422424	12.867085
20.903298	1180.314502	12.872090
20.760454	1185.464333	12.877095
20.872369	1184.384902	12.882099
20.550407	1192.769161	12.887104
20.895239	1184.174198	12.892109
21.143472	1185.546416	12.897114
20.723986	1180.669907	12.902119
20.866604	1185.839478	12.907123
20.946189	1212.477968	12.912128
21.020592	1210.669170	12.917133
21.074830	1214.789287	12.922138
20.905771	1213.765530	12.927143
21.318006	1208.263242	12.932147
21.043229	1220.467623	12.937152
21.155248	1201.161400	12.942157
21.015187	1197.937124	12.947162
20.757261	1201.879839	12.952167
21.068598	1207.258516	12.957171
21.083216	1219.280644	12.962176
21.465075	1209.431937	12.967181
21.275317	1195.797392	12.972186
21.212339	1192.030158	12.977191
21.493614	1182.994905	12.982195
21.000387	1187.028883	12.987200
20.990611	1188.039941	12.992205
21.066913	1184.634884	12.997210
20.986199	1192.548300	13.002215
21.131618	1192.994323	13.007219
21.073555	1190.573892	13.012224
21.429238	1191.283865	13.017229
21.395640	1191.612159	13.022234
20.849600	1189.319608	13.027239
20.906698	1187.186145	13.032243
20.875264	1195.909015	13.037248
21.080368	1190.191193	13.042253
20.901654	1194.202825	13.047258
20.662352	1191.673336	13.052263
20.782243	1184.586166	13.057267
20.590908	1192.850132	13.062272
20.917672	1196.759699	13.067277
21.037143	1190.947611	13.072282
21.402241	1191.464521	13.077287
21.085815	1187.621138	13.082291
21.156890	1193.254562	13.087296
21.029907	1194.839538	13.092301
20.675497	1193.223083	13.097306
20.789996	1206.616378	13.102311
21.148336	1198.183304	13.107315
20.580158	1207.527559	13.112320
20.672373	1201.437111	13.117325
20.859289	1214.961682	13.122330
21.090270	1222.005740	13.127335
21.523581	1226.784425	13.132339
21.400354	1219.159839	13.137344
21.481368	1203.657129	13.142349
21.272770	1195.543109	13.147354
20.732671	1198.320772	13.152359
20.977558	1195.165889	13.157363
20.844762	1203.320348	13.162368
20.634250	1202.103566	13.167373
20.746918	1202.121779	13.172378
20.667685	1220.265061	13.177383
21.569372	1221.674453	13.182387
21.414243	1218.572757	13.187392
21.537762	1210.945737	13.192397
21.516501	1208.091883	13.197402
21.125192	1204.655287	13.202407
21.198920	1208.827720	13.207411
21.021639	1204.751263	13.212416
21.112000	1201.791033	13.217421
21.513262	1203.479649	13.222426
20.831020	1207.833807	13.227431
21.308312	1206.737516	13.232435
20.885585	1201.175497	13.237440
20.744511	1203.164341	13.242445
20.736302	1206.597657	13.247450
20.638575	1201.913475	13.252455
21.226951	1202.004071	13.257459
21.087875	1205.602327	13.262464
20.943012	1193.022334	13.267469
21.217808	1195.881723	13.272474
20.857950	1202.039436	13.277479
21.219442	1204.820804	13.282483
20.911984	1208.018058	13.287488
21.116068	1208.322968	13.292493
21.128937	1204.926415	13.297498
20.934474	1203.377272	13.302503
21.079492	1208.107881	13.307507
20.791430	1199.187212	13.312512
20.549446	1202.641268	13.317517
20.840682	1206.813906	13.322522
20.704948	1206.149176	13.327527
20.652095	1206.388798	13.332531
20.935832	1209.292052	13.337536
21.066346	1216.009908	13.342541
20.768239	1224.866941	13.347546
20.940617	1236.753478	13.352551
21.355063	1228.859459	13.357555
21.011184	1239.908848	13.362560
21.128579	1225.249363	13.367565
21.073767	1227.497765	13.372570
21.167634	1221.943480	13.377575
20.903654	1213.311572	13.382579
21.031154	1219.320597	13.387584
21.206630	1223.315322	13.392589
20.859617	1210.488921	13.397594
20.920317	1207.537329	13.402599
20.921511	1208.396505	13.407603
21.243334	1235.466006	13.412608
21.067900	1225.072572	13.417613
20.916819	1219.196335	13.422618
20.836913	1213.254211	13.427623
21.447082	1222.221959	13.432627
21.530969	1230.669284	13.437632
21.079101	1212.173029	13.442637
21.376982	1205.960473	13.447642
21.470496	1210.054512	13.452647
21.709050	1209.462582	13.457651
21.578007	1218.957684	13.462656
21.465000	1194.730129	13.467661
21.022545	1184.519480	13.472666
20.918885	1187.223888	13.477671
21.335794	1176.718264	13.482675
20.938798	1175.504248	13.487680
21.093554	1174.274971	13.492685
21.006121	1178.777399	13.497690
20.630054	1180.231791	13.502695
21.270526	1175.584072	13.507699
21.099349	1181.767453	13.512704
20.901160	1175.311936	13.517709
20.640892	1173.528946	13.522714
20.741953	1192.892215	13.527719
20.954598	1202.771672	13.532723
21.322383	1211.530313	13.537728
20.807107	1206.757852	13.542733
21.211888	1199.916700	13.547738
21.039425	1205.170696	13.552743
20.865385	1196.823379	13.557747
21.112760	1207.969133	13.562752
20.946536	1205.529745	13.567757
21.064608	1203.755697	13.572762
21.007544	1214.053251	13.577767
21.263498	1207.723934	13.582771
20.601289	1201.235072	13.587776
20.980993	1204.565954	13.592781
21.217169	1212.532810	13.597786
21.319773	1222.842073	13.602791
21.115319	1196.296090	13.607795
20.823396	1188.747812	13.612800
20.867054	1195.625817	13.617805
20.980534	1202.248693	13.622810
20.947942	1215.443003	13.627815
20.909803	1215.134964	13.632819
20.950876	1222.253426	13.637824
21.238595	1216.564851	13.642829
21.790302	1214.012232	13.647834
21.315753	1209.093839	13.652839
21.072721	1194.307496	13.657843
21.449119	1203.927559	13.662848
21.194484	1194.248390	13.667853
21.143031	1191.566691	13.672858
21.153053	1192.323695	13.677863
21.445581	1185.106660	13.682867
20.847873	1195.378085	13.687872
20.649701	1184.739890	13.692877
20.660255	1190.926457	13.697882
21.030440	1189.489713	13.702887
21.412438	1186.147900	13.707891
21.043746	1197.694545	13.712896
20.861334	1198.034934	13.717901
21.223187	1188.116643	13.722906
21.073517	1196.412546	13.727911
21.299763	1192.081375	13.732915
20.727230	1191.873254	13.737920
20.876414	1187.093451	13.742925
20.802820	1187.738079	13.747930
20.785529	1189.422669	13.752935
21.068784	1184.420930	13.757939
21.100015	1189.980656	13.762944
21.440812	1191.658717	13.767949
21.129478	1195.611377	13.772954
21.184918	1191.353309	13.777959
21.340046	1193.718079	13.782963
21.445334	1198.202864	13.787968
21.293085	1194.096854	13.792973
21.294624	1178.602664	13.797978
21.198379	1178.228405	13.802983
20.960512	1163.451469	13.807987
20.960942	1161.471805	13.812992
20.662862	1168.049574	13.817997
20.500221	1169.776058	13.823002
20.613517	1182.753482	13.828007
20.801703	1187.157339	13.833011
20.652848	1186.384333	13.838016
20.938701	1187.361281	13.843021
20.977219	1193.712398	13.848026
21.115277	1200.673299	13.853031
21.664522	1197.212807	13.858035
21.888091	1197.099898	13.863040
21.606290	1195.320597	13.868045
21.162732	1169.510005	13.873050
21.023832	1169.643195	13.878055
20.915012	1155.062431	13.883059
20.799210	1169.609138	13.888064
21.157861	1161.823008	13.893069
21.144970	1161.798407	13.898074
20.829537	1166.845192	13.903079
20.853853	1161.454433	13.908083
20.580224	1169.842235	13.913088
20.559263	1189.559977	13.918093
20.854435	1190.487564	13.923098
20.424125	1195.617214	13.928103
20.941879	1193.655425	13.933107
20.819564	1194.084985	13.938112
21.128958	1192.813007	13.943117
21.207412	1193.821175	13.948122
20.749413	1196.930159	13.953127
21.285493	1198.384472	13.958131
21.179998	1190.598174	13.963136
21.085990	1192.910529	13.968141
21.245789	1197.151886	13.973146
20.958197	1200.470864	13.978151
21.360621	1203.437847	13.983155
21.285150	1198.610111	13.988160
20.964582	1206.480581	13.993165
21.109023	1198.972348	13.998170
20.944498	1210.428337	14.003175
20.669184	1202.500623	14.008179
20.891650	1198.778788	14.013184
21.034094	1206.289208	14.018189
21.131332	1210.254518	14.023207
20.767747	1206.369706	14.028224
21.465692	1197.671000	14.033242
21.300059	1201.522979	14.038259
20.868846	1208.555405	14.043277
21.027780	1197.211093	14.048295
20.752990	1199.622610	14.053312
20.921614	1197.841614	14.058330
20.949934	1209.751176	14.063347
20.915716	1202.695062	14.068365
21.339120	1197.830361	14.073383
21.148289	1203.019843	14.078400
20.967471	1205.318391	14.083418
21.277717	1221.342965	14.088435
21.193985	1229.178493	14.093453
21.427634	1228.399422	14.098471
20.881198	1236.480051	14.103488
21.550705	1238.970237	14.108506
21.267525	1231.922148	14.113523
21.288893	1237.778074	14.118541
21.563530	1234.068889	14.123559
21.081081	1238.822516	14.128576
21.287267	1241.693350	14.133594
21.249389	1243.054323	14.138611
21.496839	1244.651438	14.143629
22.085591	1238.235802	14.148647
21.547292	1234.302192	14.153664
21.765102	1236.788323	14.158682
22.209747	1236.588088	14.163699
21.730811	1217.833193	14.168717
21.519129	1207.722992	14.173735
21.753655	1221.884407	14.178752
22.001473	1208.728631	14.183770
21.479824	1206.365141	14.188787
20.781896	1209.999702	14.193805
21.196086	1211.599329	14.198823
21.346772	1229.501033	14.203840
21.644336	1242.890570	14.208858
21.475072	1236.613961	14.213875
21.038407	1247.439004	14.218893
21.574870	1244.486568	14.223911
21.290060	1250.753689	14.228928
21.947936	1245.190053	14.233946
21.874105	1245.041312	14.238963
21.890464	1253.543214	14.243981
21.837344	1244.662603	14.248999
21.947523	1249.932391	14.254016
21.561812	1245.117423	14.259034
21.923546	1254.426718	14.264051
21.278601	1250.191284	14.269069
21.603406	1258.033950	14.274087
21.879671	1273.071797	14.279104
21.796345	1270.243738	14.284122
22.111141	1276.186387	14.289139
21.861908	1281.501273	14.294157
22.198248	1278.566607	14.299175
21.963232	1282.595871	14.304192
22.098704	1275.222415	14.309210
22.372036	1280.031916	14.314227
22.343266	1278.757239	14.319245
22.221370	1277.905651	14.324263
21.882575	1281.115233	14.329280
22.073601	1275.378855	14.334298
22.083378	1276.148144	14.339315
21.828427	1277.206939	14.344333
22.173541	1271.982772	14.349351
22.149768	1282.914620	14.354368
22.303761	1273.317319	14.359386
22.362915	1272.163799	14.364403
21.957871	1280.690327	14.369421
22.156582	1269.529711	14.374439
22.172280	1282.062019	14.379456
22.141498	1274.745024	14.384474
22.304086	1280.036153	14.389491
21.614256	1285.910487	14.394509
22.460177	1297.517710	14.399527
22.312048	1313.285903	14.404544
22.698326	1309.811912	14.409562
22.913650	1306.975950	14.414579
22.357792	1312.098910	14.419597
22.479268	1308.707334	14.424615
22.308198	1322.551342	14.429632
22.737815	1309.554091	14.434650
22.841427	1305.317470	14.439667
22.699774	1305.690639	14.444685
22.323448	1286.655052	14.449703
22.333371	1296.773186	14.454720
22.255436	1301.885070	14.459738
22.610370	1305.867523	14.464755
22.075872	1305.424505	14.469773
22.330069	1310.516849	14.474791
22.564602	1313.823428	14.479808
22.295253	1306.233515	14.484826
22.632420	1318.634742	14.489843
22.646184	1336.968744	14.494861
22.785670	1339.943168	14.499879
22.976098	1333.357973	14.504896
23.026097	1331.720147	14.509914
23.311905	1312.206792	14.514931
22.808163	1314.285108	14.519949
22.989889	1306.371374	14.524967
22.928233	1304.999962	14.529984
22.710983	1311.298046	14.535002
23.293639	1308.862136	14.540019
22.730339	1307.236153	14.545037
23.092474	1311.315019	14.550055
23.284300	1305.483601	14.555072
23.189726	1306.936986	14.560090
23.027999	1301.521341	14.565107
22.999943	1308.733527	14.570125
23.353841	1301.528531	14.575143
23.220578	1300.674560	14.580160
23.114092	1309.968492	14.585178
23.515866	1311.089506	14.590195
23.188276	1321.082832	14.595213
23.405666	1305.867042	14.600231
23.127693	1302.728226	14.605248
23.233141	1308.787498	14.610266
23.734703	1306.888374	14.615283
23.453663	1309.193490	14.620301
23.813349	1311.561991	14.625319
23.505015	1295.888270	14.630336
22.986515	1283.482383	14.635354
23.342067	1275.686118	14.640371
23.401485	1279.714508	14.645389
23.047112	1269.361779	14.650407
23.310829	1288.262764	14.655424
22.914012	1303.940111	14.660442
23.198011	1305.827055	14.665459
23.031040	1308.835119	14.670477
23.259029	1309.616605	14.675495
23.388240	1312.688463	14.680512
23.209147	1315.240691	14.685530
23.677351	1308.857901	14.690547
23.375741	1318.564462	14.695565
23.204975	1315.837222	14.700583
23.780187	1321.492302	14.705600
23.422068	1320.162664	14.710618
23.871894	1321.847539	14.715635
23.431267	1323.674855	14.720653
23.811812	1330.485860	14.725671
23.666708	1329.706759	14.730688
23.638387	1335.088126	14.735706
24.275837	1341.186915	14.740723
23.756402	1325.409977	14.745741
23.405108	1315.016135	14.750759
23.873868	1318.956237	14.755776
23.579215	1332.954527	14.760794
23.954232	1331.074341	14.765811
23.657519	1338.145974	14.770829
24.030862	1337.209076	14.775847
24.128801	1340.930455	14.780864
23.665688	1339.182950	14.785882
24.250845	1334.875962	14.790899
24.080275	1346.046823	14.795917
23.658114	1325.794130	14.800935
23.905966	1328.702329	14.805952
23.878546	1334.631623	14.810970
24.020818	1333.863490	14.815987
24.054598	1341.011147	14.821005
24.107261	1334.540526	14.826023
23.981310	1343.818916	14.831040
24.119959	1338.013929	14.836058
24.525735	1339.615012	14.841075
24.457013	1345.280501	14.846093
24.420382	1331.353632	14.851111
24.369760	1325.225951	14.856128
24.070758	1310.722376	14.861146
24.197339	1311.081053	14.866163
24.480250	1333.442109	14.871181
24.370874	1328.452557	14.876199
24.247745	1313.358537	14.881216
23.986203	1310.682298	14.886234
24.173456	1313.854845	14.891251
24.163718	1337.492967	14.896269
24.168936	1335.760841	14.901287
24.138455	1339.151057	14.906304
23.961876	1341.720576	14.911322
24.135329	1331.031612	14.916339
23.940576	1342.477903	14.921357
24.253362	1337.435651	14.926375
24.425519	1348.967081	14.931392
24.155356	1371.633671	14.936410
24.626393	1370.213441	14.941427
24.419610	1374.205994	14.946445
24.552362	1370.000190	14.951463
24.822110	1372.908974	14.956480
24.674241	1371.533438	14.961498
24.750816	1362.167881	14.966515
24.760200	1365.605997	14.971533
24.412348	1365.464470	14.976551
24.823425	1362.862677	14.981568
24.596154	1372.059627	14.986586
24.797487	1366.021420	14.991603
24.794752	1374.583754	14.996621
24.865742	1378.784218	15.001639
25.288388	1371.575277	15.006656
24.990373	1370.566069	15.011674
25.212163	1368.464884	15.016691
25.251075	1367.676673	15.021709
25.193819	1354.374245	15.026727
25.070245	1346.174223	15.031744
25.072817	1342.229352	15.036762
25.270468	1337.783667	15.041779
25.237715	1344.935646	15.046797
24.885378	1341.858789	15.051815
24.916681	1334.098010	15.056832
24.778292	1347.386779	15.061850
24.916304	1335.052555	15.066867
25.053299	1347.065646	15.071885
25.364561	1355.661148	15.076903
25.082245	1343.944707	15.081920
24.971557	1352.267246	15.086938
25.336403	1364.368067	15.091955
25.481714	1367.769884	15.096973
25.295864	1349.455176	15.101991
24.890515	1341.686576	15.107008
24.695073	1361.512125	15.112026
25.189385	1360.716311	15.117043
25.101412	1370.667796	15.122061
25.060233	1372.881789	15.127079
25.499581	1372.745460	15.132096
24.827460	1372.980429	15.137114
24.853608	1373.349240	15.142131
25.145559	1381.695287	15.147149
25.086844	1386.075094	15.152167
25.574525	1395.806622	15.157184
25.797637	1404.780686	15.162202
25.708177	1401.674100	15.167219
25.946534	1402.862908	15.172237
25.722246	1390.311600	15.177255
26.054337	1383.776905	15.182272
25.806018	1377.170847	15.187290
26.058942	1374.631211	15.192307
25.966784	1370.188747	15.197325
25.561745	1370.401152	15.202343
25.729202	1368.480166	15.207360
25.584887	1370.172421	15.212378
25.467468	1358.547392	15.217395
25.463927	1366.895666	15.222413
25.463470	1374.877240	15.227431
25.822990	1362.831423	15.232448
25.341407	1375.665233	15.237466
25.773325	1380.088485	15.242483
25.936384	1399.345478	15.247501
25.548825	1405.770449	15.252519
26.135328	1397.999097	15.257536
25.876088	1402.197915	15.262554
26.207371	1398.962885	15.267571
26.234251	1400.933694	15.272589
26.107534	1398.928878	15.277607
26.393109	1394.130668	15.282624
26.276199	1391.782800	15.287642
25.683238	1370.803749	15.292659
26.408629	1386.742351	15.297677
25.962587	1382.249525	15.302695
26.021927	1391.022506	15.307712
25.740121	1403.573241	15.312730
25.936495	1399.149413	15.317747
25.956225	1402.704279	15.322765
25.825201	1411.054355	15.327783
26.236880	1406.428632	15.332800
26.011437	1408.066291	15.337818
26.084878	1402.653207	15.342835
26.023483	1406.786211	15.347853
26.258029	1430.338884	15.352871
26.592828	1424.647885	15.357888
26.824649	1433.348792	15.362906
26.744994	1400.710866	15.367923
26.548442	1399.725602	15.372941
26.161974	1396.679391	15.377959
26.565495	1404.575177	15.382976
26.258890	1405.892467	15.387994
26.273819	1402.525439	15.393011
26.589642	1416.493548	15.398029
26.546536	1432.791545	15.403047
26.582120	1434.495092	15.408064
26.715240	1427.819674	15.413082
26.837005	1432.128781	15.418099
26.960720	1429.017137	15.423117
26.612122	1428.722573	15.428135
26.629539	1413.770122	15.433152
27.032409	1426.640926	15.438170
26.736917	1413.032805	15.443187
26.734672	1410.644799	15.448205
26.661827	1424.789803	15.453223
26.885679	1435.516292	15.458240
26.737997	1428.273604	15.463258
26.793777	1435.901438	15.468275
27.011237	1432.069714	15.473293
26.470918	1438.191330	15.478311
26.675212	1432.934557	15.483328
27.130602	1434.018826	15.488346
27.050079	1433.159742	15.493363
27.555491	1430.230709	15.498381
27.469656	1414.929783	15.503399
27.872942	1397.187299	15.508416
27.483371	1385.919966	15.513434
27.282101	1380.278767	15.518451
27.347959	1372.797504	15.523469
27.285307	1377.399265	15.528487
27.425772	1369.963878	15.533504
27.532464	1367.123695	15.538522
27.821601	1377.348747	15.543539
27.663597	1376.652178	15.548557
27.418313	1376.290289	15.553575
27.161352	1356.934908	15.558592
26.965505	1360.463335	15.563610
27.348923	1365.485112	15.568627
27.768350	1360.928948	15.573645
27.067234	1377.010938	15.578663
27.609959	1373.052585	15.583680
27.228658	1380.038730	15.588698
27.435830	1382.066428	15.593715
27.300458	1376.426926	15.598733
27.276614	1378.214679	15.603751
27.189124	1374.194288	15.608768
26.975665	1375.697199	15.613786
27.042418	1384.563796	15.618803
27.696723	1390.823904	15.623821
27.669787	1405.270497	15.628839
27.940416	1401.110736	15.633856
27.684426	1403.411963	15.638874
27.603226	1406.608902	15.643891
27.782571	1411.721202	15.648909
27.465106	1411.784721	15.653927
27.376329	1401.739942	15.658944
27.674167	1409.626683	15.663962
27.307632	1414.018328	15.668979
27.570817	1409.173553	15.673997
27.680060	1418.099819	15.679015
28.091056	1412.921008	15.684032
27.686554	1406.889802	15.689050
27.804446	1415.632282	15.694067
27.940034	1421.965986	15.699085
27.848821	1437.303637	15.704103
28.333393	1446.494339	15.709120
28.237897	1438.015412	15.714138
28.092834	1446.102139	15.719155
28.313682	1437.139008	15.724173
28.256565	1437.980016	15.729191
28.215427	1414.290678	15.734208
28.156660	1400.086413	15.739226
28.052433	1412.333847	15.744243
28.207096	1414.489068	15.749261
28.227632	1421.287817	15.754279
28.398186	1439.402519	15.759296
28.817019	1437.026571	15.764314
28.196212	1425.207854	15.769331
28.216438	1408.073216	15.774349
28.115219	1414.167177	15.779367
28.466353	1432.220590	15.784384
28.254569	1433.894497	15.789402
28.039919	1445.971501	15.794419
28.564618	1440.140839	15.799437
28.468862	1446.730382	15.804455
28.677704	1438.574508	15.809472
29.167964	1438.989347	15.814490
28.643912	1446.454373	15.819507
28.794476	1430.735695	15.824525
28.711081	1444.116702	15.829543
28.405882	1440.108423	15.834560
28.397136	1444.059951	15.839578
28.503164	1442.866883	15.844595
28.956111	1435.058564	15.849613
28.265120	1445.840728	15.854631
28.540300	1440.369022	15.859648
28.689742	1439.589811	15.864666
28.404071	1443.636070	15.869683
28.438207	1440.514978	15.874701
28.566790	1462.567608	15.879719
28.756483	1465.559434	15.884736
28.961642	1470.479906	15.889754
28.945139	1477.732714	15.894771
29.172881	1471.564729	15.899789
29.166730	1474.775981	15.904807
29.043592	1471.652712	15.909824
29.484331	1473.730542	15.914842
29.242242	1474.743833	15.919859
29.317482	1459.269167	15.924877
28.955772	1458.258668	15.929895
29.250430	1458.047531	15.934912
29.286864	1461.813741	15.939930
29.663040	1473.191766	15.944947
29.704173	1449.261474	15.949965
28.953628	1443.404950	15.954983
29.109446	1433.922604	15.960000
29.313747	1430.095499	15.965018
29.210364	1443.454733	15.970035
29.440987	1454.136369	15.975053
29.414336	1465.758278	15.980071
29.178943	1466.994852	15.985088
29.587647	1461.945172	15.990106
29.403128	1470.953729	15.995123
29.422188	1468.983758	16.000141
29.333705	1470.295154	16.005159
29.610100	1469.365815	16.010176
29.390887	1466.662210	16.015194
29.450454	1469.988979	16.020211
29.332683	1466.548617	16.025229
29.350567	1469.869539	16.030247
29.764917	1475.246321	16.035264
29.648071	1472.478702	16.040282
29.352594	1464.263600	16.045299
29.643029	1459.766535	16.050317
29.602178	1468.338999	16.055335
29.879100	1473.630278	16.060352
29.951277	1482.256606	16.065370
29.742249	1486.929170	16.070387
30.130122	1491.909670	16.075405
29.903528	1487.468566	16.080423
29.984588	1494.279806	16.085440
30.062926	1486.393552	16.090458
29.998249	1494.062543	16.095475
30.070774	1497.854073	16.100493
30.179236	1491.379726	16.105511
30.000422	1496.528264	16.110528
30.345281	1489.643269	16.115546
30.010732	1491.339805	16.120563
30.099613	1487.736040	16.125581
30.187871	1484.757643	16.130599
30.135175	1491.819005	16.135616
30.401603	1492.912841	16.140634
30.044570	1492.787455	16.145651
30.489533	1482.886567	16.150669
30.274571	1489.691075	16.155687
30.109704	1491.732966	16.160704
30.430077	1489.887331	16.165722
30.128352	1498.953012	16.170739
30.195808	1491.604109	16.175757
30.386431	1487.447018	16.180775
30.113872	1491.719805	16.185792
30.284782	1488.561471	16.190810
30.296990	1488.838177	16.195827
30.407712	1496.484576	16.200845
30.926265	1505.081631	16.205863
31.196505	1500.880567	16.210880
31.235775	1485.515597	16.215898
31.007580	1493.068121	16.220915
31.234215	1474.545519	16.225933
31.082507	1478.500306	16.230951
31.002747	1473.291829	16.235968
31.186869	1477.233134	16.240986
30.847910	1465.831068	16.246003
30.731546	1460.097715	16.251021
30.879822	1464.277864	16.256039
30.825407	1470.753231	16.261056
30.999254	1468.888230	16.266074
30.932974	1484.090143	16.271091
30.928064	1473.298580	16.276109
31.018463	1474.095004	16.281127
30.681244	1479.037602	16.286144
30.802174	1473.130474	16.291162
30.643897	1472.524114	16.296179
30.690381	1474.141930	16.301197
30.682067	1476.323922	16.306215
30.652873	1479.995473	16.311232
31.063192	1486.221462	16.316250
30.896691	1505.253173	16.321267
31.194397	1501.545089	16.326285
31.512375	1507.638479	16.331303
31.270635	1501.898653	16.336320
31.056755	1505.786146	16.341338
31.078992	1511.921189	16.346355
31.146992	1498.804269	16.351373
31.471300	1509.022983	16.356391
31.338772	1510.075371	16.361408
31.393923	1506.218304	16.366426
31.157150	1504.117765	16.371443
31.302499	1507.151064	16.376461
31.373661	1522.739334	16.381479
31.794975	1536.554017	16.386496
31.571964	1532.262695	16.391514
31.955880	1536.068173	16.396531
31.830913	1536.670795	16.401549
31.835305	1535.550269	16.406567
31.495063	1538.530992	16.411584
32.049100	1529.099614	16.416602
32.153271	1525.936572	16.421619
31.920799	1506.791002	16.426637
32.122575	1509.186215	16.431655
32.032252	1501.161926	16.436672
31.767646	1504.225747	16.441690
31.705519	1507.232409	16.446707
31.940097	1502.835076	16.451725
32.106864	1511.060517	16.456743
31.806040	1508.707152	16.461760
32.187252	1519.641783	16.466778
32.266967	1525.301179	16.471795
32.154922	1526.262252	16.476813
32.462002	1505.325569	16.481831
31.975652	1513.230272	16.486848
32.025963	1502.350866	16.491866
32.337213	1500.776507	16.496883
32.262410	1507.516830	16.501901
32.438384	1514.873281	16.506919
32.019037	1520.948987	16.511936
32.378010	1519.801135	16.516954
32.300645	1531.699139	16.521971
32.440204	1527.557093	16.526989
32.464578	1525.670464	16.532007
32.226358	1531.502104	16.537024
32.456095	1522.636229	16.542042
32.330715	1531.998893	16.547059
32.079305	1525.436220	16.552077
32.357570	1524.710122	16.557095
32.346559	1528.745140	16.562112
32.772541	1527.515319	16.567130
32.645605	1530.939045	16.572147
32.463759	1531.108852	16.577165
32.967908	1529.319508	16.582183
32.441673	1531.299334	16.587200
32.407931	1521.285598	16.592218
32.717779	1537.308204	16.597235
32.616407	1548.415371	16.602253
32.955114	1553.889805	16.607271
33.164369	1571.592469	16.612288
33.057116	1555.243783	16.617306
32.950132	1550.129328	16.622323
32.761731	1552.415051	16.627341
32.922353	1540.604403	16.632359
32.973339	1557.094293	16.637376
32.988175	1556.420055	16.642394
33.110880	1557.557832	16.647411
33.091178	1557.214353	16.652429
33.533258	1550.737117	16.657447
33.136711	1550.815770	16.662464
33.592004	1554.625158	16.667482
33.627256	1555.876759	16.672499
33.290316	1542.364617	16.677517
33.355341	1528.013406	16.682535
33.282803	1530.363915	16.687552
33.514847	1537.147318	16.692570
32.928998	1529.439102	16.697587
33.392560	1544.803405	16.702605
33.748796	1543.341027	16.707623
33.491341	1563.319998	16.712640
33.423475	1555.402472	16.717658
33.569668	1544.877897	16.722675
33.425530	1545.335364	16.727693
33.981780	1546.277139	16.732711
33.852684	1545.156270	16.737728
33.466885	1549.844592	16.742746
33.640230	1552.732141	16.747763
33.089237	1556.652248	16.752781
33.329378	1545.742627	16.757799
33.155288	1548.994108	16.762816
33.549287	1546.618860	16.767834
33.742739	1559.715465	16.772851
33.542032	1575.700439	16.777869
34.058540	1574.171598	16.782887
34.182448	1577.953156	16.787904
34.251879	1575.269734	16.792922
34.433272	1568.836793	16.797939
34.186378	1564.358592	16.802957
34.206721	1545.451547	16.807975
33.840400	1545.828986	16.812992
33.980435	1547.027184	16.818010
34.019880	1556.760069	16.823027
34.105731	1574.977256	16.828045
34.470005	1572.503152	16.833063
34.007223	1576.273086	16.838080
34.035598	1581.244773	16.843098
34.247041	1576.335583	16.848115
34.401401	1577.842384	16.853133
34.228209	1576.699542	16.858151
34.209462	1584.162255	16.863168
34.128932	1586.818112	16.868186
34.364703	1578.385077	16.873203
34.326445	1582.070805	16.878221
34.567700	1580.482453	16.883239
34.501341	1582.881522	16.888256
34.339813	1576.985773	16.893274
34.270950	1584.615757	16.898291
34.574920	1589.610675	16.903309
34.525805	1599.218598	16.908327
34.786354	1606.200316	16.913344
34.953651	1607.407231	16.918362
35.428567	1608.130647	16.923379
34.837250	1589.555612	16.928397
34.842879	1583.691049	16.933415
34.633631	1583.105630	16.938432
34.639754	1583.989353	16.943450
34.791525	1598.671261	16.948467
34.687755	1609.741871	16.953485
35.015098	1600.059523	16.958503
34.883366	1603.730571	16.963520
35.043717	1610.037662	16.968538
34.854232	1606.783994	16.973555
35.057964	1610.687715	16.978573
35.447547	1604.004080	16.983591
34.942896	1607.565034	16.988608
34.908163	1599.052370	16.993626
35.066033	1605.769379	16.998643
34.905332	1613.135565	17.003661
35.108576	1610.441006	17.008679
35.093139	1627.403434	17.013696
35.353634	1632.075467	17.018714
35.750505	1634.129735	17.023731
35.256699	1643.747783	17.028749
35.582326	1637.785021	17.033767
35.757919	1637.906537	17.038784
35.413909	1640.363457	17.043802
35.295920	1638.364988	17.048819
35.213458	1631.665022	17.053837
35.461128	1631.205219	17.058855
35.956340	1638.184910	17.063872
35.859625	1639.042562	17.068890
35.896644	1631.875603	17.073907
35.632158	1636.822316	17.078925
35.662068	1639.468696	17.083943
35.354627	1646.652948	17.088960
35.650291	1643.659435	17.093978
35.990257	1636.548812	17.098995
36.158573	1640.200316	17.104013
36.247083	1636.526495	17.109031
36.383969	1637.554748	17.114048
36.362753	1634.559656	17.119066
36.708818	1633.043889	17.124083
36.394100	1633.067562	17.129101
36.648450	1620.096956	17.134119
36.528506	1606.223895	17.139136
36.401225	1596.767546	17.144154
36.250644	1601.240731	17.149171
36.029018	1595.161164	17.154189
35.567069	1585.859851	17.159207
35.869271	1598.003489	17.164224
35.948083	1623.696380	17.169242
36.486013	1621.303924	17.174259
36.236403	1622.532710	17.179277
36.288270	1624.291761	17.184295
36.115254	1625.271955	17.189312
36.156560	1629.793754	17.194330
36.411741	1625.771637	17.199347
35.832376	1632.309909	17.204365
36.389329	1645.437185	17.209383
36.756910	1659.494287	17.214400
36.742814	1658.472603	17.219418
36.718059	1652.226566	17.224435
37.009671	1660.799226	17.229453
37.142726	1655.988500	17.234471
36.953719	1658.068807	17.239488
37.064030	1661.399122	17.244506
36.692812	1655.468815	17.249523
36.535987	1666.849777	17.254541
36.905735	1657.525913	17.259559
37.235529	1646.051182	17.264576
36.919386	1660.035336	17.269594
37.230953	1648.103834	17.274611
37.036112	1653.279977	17.279629
37.134600	1649.162659	17.284647
37.057215	1641.309720	17.289664
36.910981	1645.416778	17.294682
37.219960	1652.559917	17.299699
37.131601	1651.124934	17.304717
37.301658	1655.809331	17.309735
37.677161	1653.878233	17.314752
37.372685	1664.061143	17.319770
37.638756	1652.315411	17.324787
37.623913	1660.719724	17.329805
37.516611	1652.574237	17.334823
37.609364	1655.073609	17.339840
37.303130	1661.381578	17.344858
37.885661	1652.829987	17.349875
37.844291	1655.487804	17.354893
37.589592	1665.539724	17.359911
37.754459	1661.660263	17.364928
37.623593	1669.119403	17.369946
37.607348	1657.955204	17.374963
37.042596	1661.646173	17.379981
37.097301	1658.308101	17.384999
37.386024	1673.172527	17.390016
37.667121	1682.525437	17.395034
37.830499	1675.957337	17.400051
37.428378	1686.539330	17.405069
37.783059	1683.298261	17.410087
37.938857	1679.599899	17.415104
37.726491	1684.051808	17.420122
37.977429	1683.751304	17.425139
37.669003	1692.102808	17.430157
37.854217	1696.313305	17.435175
38.066505	1706.720667	17.440192
37.902091	1715.241215	17.445210
38.357623	1713.285758	17.450227
37.878644	1714.941324	17.455245
38.169962	1709.447465	17.460263
38.483272	1714.498308	17.465280
38.639264	1710.826680	17.470298
38.513861	1705.861018	17.475315
38.677890	1716.650327	17.480333
38.941374	1711.538448	17.485351
39.129170	1712.478047	17.490368
38.681717	1716.930504	17.495386
38.728454	1706.683139	17.500403
38.739329	1701.483852	17.505421
38.551567	1705.661438	17.510439
38.768388	1702.341629	17.515456
38.661527	1715.540650	17.520474
38.643559	1715.121664	17.525491
38.981485	1713.662017	17.530509
38.643782	1711.977226	17.535527
38.920818	1710.418164	17.540544
38.527528	1718.462542	17.545562
38.637844	1707.751073	17.550579
38.817046	1711.024306	17.555597
38.864742	1706.821576	17.560615
39.270395	1703.718238	17.565632
38.832434	1718.512004	17.570650
38.929390	1711.293783	17.575667
38.952027	1711.242683	17.580685
39.126485	1729.679924	17.585703
39.423897	1726.280537	17.590720
39.043068	1746.867972	17.595738
39.532983	1739.398483	17.600755
39.467346	1736.553524	17.605773
39.160780	1738.732353	17.610791
39.367144	1738.018575	17.615808
39.443780	1749.943495	17.620826
39.349520	1735.594993	17.625843
39.449993	1740.276384	17.630861
39.413929	1747.335797	17.635879
39.865437	1736.966643	17.640896
39.578586	1741.975104	17.645914
39.726418	1741.734802	17.650931
39.586546	1740.984707	17.655949
39.501043	1745.748386	17.660967
39.544958	1740.415059	17.665984
39.508654	1745.287246	17.671002
39.351894	1742.209455	17.676019
39.648196	1744.162464	17.681037
39.618546	1763.357267	17.686055
40.021038	1767.917190	17.691072
39.685978	1771.156154	17.696090
40.176622	1774.069272	17.701107
40.419051	1774.861695	17.706125
40.061479	1779.827957	17.711143
40.449909	1767.572518	17.716160
40.297074	1773.381339	17.721178
40.284761	1770.934367	17.726195
40.186027	1770.381573	17.731213
39.806652	1769.780034	17.736231
40.253056	1763.318902	17.741248
40.005577	1779.015216	17.746266
40.424438	1765.474092	17.751283
40.617084	1755.877743	17.756301
40.288108	1764.732476	17.761319
40.379084	1758.122024	17.766336
40.439515	1760.624986	17.771354
40.495716	1759.647549	17.776371
40.675904	1763.502977	17.781389
40.587286	1761.341957	17.786407
40.879748	1756.832649	17.791424
40.559876	1756.358326	17.796442
40.619965	1759.059796	17.801459
40.726080	1771.304521	17.806477
40.659660	1795.008179	17.811495
40.959379	1792.903027	17.816512
40.656805	1788.073634	17.821530
41.018845	1787.409943	17.826547
40.897119	1788.354972	17.831565
40.944416	1787.149504	17.836583
41.238862	1785.218507	17.841600
41.157794	1796.501524	17.846618
41.164052	1793.192205	17.851635
41.231795	1790.360593	17.856653
41.196556	1788.672759	17.861671
41.338372	1784.311334	17.866688
41.459278	1794.722610	17.871706
41.277393	1786.642998	17.876723
41.578257	1777.540348	17.881741
40.970213	1781.086780	17.886759
41.531776	1781.831180	17.891776
41.210711	1787.629869	17.896794
41.367809	1785.157392	17.901811
41.559105	1785.105724	17.906829
41.364680	1793.790535	17.911847
41.169712	1780.010901	17.916864
41.514003	1801.137547	17.921882
41.405529	1809.917880	17.926899
41.276590	1814.772502	17.931917
41.120228	1812.684515	17.936935
41.751743	1809.693237	17.941952
41.622532	1816.713920	17.946970
41.581583	1820.007991	17.951987
42.052547	1818.133744	17.957005
41.794625	1829.391983	17.962023
42.542770	1827.869078	17.967040
42.652240	1832.639123	17.972058
42.550404	1810.305427	17.977075
42.814052	1799.212444	17.982093
42.732542	1799.678080	17.987111
42.720054	1794.783592	17.992128
42.507493	1803.031700	17.997146
42.469089	1795.132232	18.002163
42.181902	1774.162025	18.007181
42.335372	1787.556264	18.012199
42.570020	1800.143585	18.017216
42.549366	1789.436403	18.022234
42.375983	1794.314389	18.027251
42.801413	1796.830375	18.032269
42.488089	1808.601703	18.037287
42.649267	1797.875545	18.042304
42.787735	1800.023753	18.047322
42.614449	1800.446850	18.052339
42.891581	1793.966690	18.057357
42.336397	1792.865702	18.062375
42.930114	1799.295048	18.067392
43.019601	1799.569141	18.072410
42.848442	1805.701627	18.077427
42.649470	1794.475735	18.082445
42.424361	1805.943318	18.087463
42.395561	1798.647000	18.092480
42.511133	1806.933743	18.097498
42.717849	1818.931307	18.102515
42.775671	1818.530037	18.107533
42.894060	1829.885980	18.112551
43.170686	1820.026343	18.117568
42.969390	1828.910408	18.122586
42.973063	1832.231087	18.127603
43.133698	1832.058282	18.132621
42.981614	1846.775984	18.137639
43.454791	1850.168156	18.142656
43.598068	1850.136140	18.147674
43.455097	1861.732217	18.152691
43.952361	1859.259287	18.157709
43.819710	1864.151573	18.162727
43.514334	1844.577087	18.167744
43.938677	1844.437030	18.172762
43.789798	1844.725612	18.177779
43.905886	1829.101827	18.182797
43.561386	1832.434953	18.187815
43.548216	1816.770342	18.192832
43.843611	1837.334878	18.197850
43.800789	1851.762558	18.202867
44.191952	1854.201348	18.207885
43.882516	1860.237076	18.212903
44.006936	1851.450105	18.217920
44.277258	1855.929553	18.222938
44.017622	1853.509223	18.227955
44.144203	1850.379286	18.232973
43.897152	1853.616171	18.237991
44.540305	1850.233078	18.243008
44.221852	1856.213650	18.248026
44.057721	1848.984218	18.253043
44.148304	1852.063594	18.258061
44.140399	1848.999241	18.263079
44.155540	1850.895339	18.268096
44.184426	1856.052089	18.273114
44.066504	1853.941756	18.278131
44.197516	1842.026889	18.283149
44.164934	1860.718315	18.288167
44.803837	1869.201227	18.293184
44.873751	1861.963554	18.298202
44.283495	1872.198352	18.303219
44.832841	1862.758918	18.308237
44.743903	1873.680302	18.313255
44.872668	1874.900145	18.318272
45.106972	1868.711586	18.323290
44.980807	1867.923303	18.328307
45.280712	1854.860036	18.333325
45.029365	1867.633114	18.338343
45.114239	1856.393948	18.343360
45.522380	1861.029318	18.348378
45.041421	1866.292781	18.353395
45.195176	1859.160040	18.358413
45.089346	1860.740224	18.363431
45.188809	1868.074130	18.368448
45.544751	1865.339172	18.373466
45.488729	1865.947309	18.378483
45.778432	1854.624594	18.383501
45.215255	1869.289164	18.388519
45.227954	1855.743576	18.393536
45.249703	1857.995280	18.398554
45.037073	1866.343446	18.403571
45.452815	1853.877720	18.408589
45.308155	1864.042807	18.413607
45.402426	1856.432016	18.418624
45.420213	1868.515956	18.423642
45.506614	1884.634325	18.428659
45.901746	1889.838935	18.433677
45.867859	1891.364262	18.438695
45.882825	1888.741313	18.443712
45.797610	1893.861726	18.448730
45.708252	1894.411004	18.453747
45.868797	1892.465546	18.458765
45.835143	1897.785808	18.463783
46.162699	1899.619291	18.468800
46.124796	1892.076032	18.473818
45.860960	1900.001444	18.478835
46.080584	1891.492260	18.483853
45.755071	1898.114298	18.488871
45.933192	1916.276294	18.493888
46.214929	1917.981396	18.498906
46.095775	1925.074035	18.503923
45.962902	1921.846425	18.508941
46.122932	1923.870465	18.513959
46.174292	1924.329074	18.518976
46.287577	1921.886925	18.523994
46.625046	1947.782883	18.529011
46.877338	1948.480700	18.534029
46.871040	1945.693254	18.539047
46.651127	1931.733093	18.544064
46.789601	1927.496234	18.549082
46.871355	1945.392466	18.554099
47.240124	1946.517614	18.559117
46.992545	1927.576506	18.564135
46.598307	1918.844561	18.569152
46.949503	1927.133494	18.574170
46.924273	1943.779005	18.579187
47.382548	1941.212340	18.584205
47.660319	1942.709436	18.589223
47.598164	1933.785488	18.594240
47.611669	1908.489366	18.599258
47.470406	1908.719943	18.604275
47.467690	1897.633184	18.609293
47.235566	1902.013336	18.614311
47.239423	1913.031450	18.619328
47.372423	1899.224222	18.624346
47.301308	1906.588574	18.629363
47.505703	1900.577594	18.634381
47.252180	1900.530923	18.639399
47.447541	1930.701372	18.644416
47.909239	1927.575782	18.649434
47.698649	1939.368574	18.654451
47.936281	1937.395325	18.659469
47.761450	1944.777871	18.664487
47.710218	1944.666985	18.669504
47.965929	1938.273914	18.674522
47.860874	1940.911198	18.679539
47.891447	1935.695855	18.684557
48.114483	1939.408137	18.689575
48.075781	1942.168314	18.694592
48.296736	1939.940803	18.699610
48.177211	1939.138385	18.704627
48.210484	1935.416082	18.709645
48.336036	1936.882970	18.714663
48.203776	1937.667982	18.719680
48.443641	1938.853819	18.724698
47.705022	1939.047821	18.729715
47.840715	1936.315965	18.734733
48.218250	1941.550385	18.739751
47.803223	1943.893132	18.744768
47.981294	1952.244837	18.749786
48.187787	1968.102513	18.754803
48.433946	1971.714762	18.759821
48.249362	1967.392712	18.764839
48.504885	1967.665903	18.769856
48.404187	1978.376356	18.774874
48.384982	1999.770740	18.779891
48.768514	1993.687667	18.784909
48.862730	2003.072024	18.789927
48.742031	2005.641912	18.794944
49.127240	2000.688623	18.799962
49.246319	2007.177384	18.804979
48.837801	2001.091507	18.809997
49.045950	2000.084065	18.815015
49.162480	2000.384632	18.820032
49.224763	1995.779270	18.825050
48.827353	2000.301188	18.830067
49.377680	2004.232997	18.835085
49.468266	2011.140482	18.840103
49.438305	2021.873093	18.845120
49.811277	2013.767530	18.850138
49.529472	2009.987405	18.855155
49.529228	1997.547607	18.860173
49.878629	2004.098860	18.865191
49.534233	2002.950295	18.870208
49.634961	2012.040195	18.875226
49.663841	2010.667372	18.880243
50.053154	2016.088406	18.885261
50.344525	2007.514095	18.890279
49.630663	2009.747043	18.895296
49.961854	2002.413714	18.900314
49.816644	2012.610491	18.905331
49.606655	2022.689231	18.910349
49.866671	2020.944055	18.915367
49.994710	2027.736449	18.920384
50.312639	2015.293666	18.925402
49.887264	2017.676393	18.930419
50.055179	2015.256363	18.935437
50.039892	2013.167392	18.940455
49.936518	2024.262639	18.945472
50.428553	2036.758771	18.950490
50.416105	2048.712975	18.955507
50.516791	2053.399543	18.960525
50.578247	2054.036370	18.965543
50.288838	2049.971279	18.970560
50.472469	2039.693532	18.975578
50.277993	2044.771301	18.980595
50.414765	2049.819842	18.985613
50.577432	2048.333513	18.990631
50.560106	2045.504628	18.995648
50.727038	2044.257759	19.000666
50.761560	2056.829199	19.005683
50.863061	2063.472988	19.010701
50.961554	2068.453284	19.015719
51.209312	2080.337698	19.020736
51.353250	2074.687066	19.025754
51.222803	2075.275684	19.030771
51.167528	2076.344395	19.035789
51.394325	2076.916649	19.040807
51.274274	2083.129469	19.045824
51.312703	2076.541674	19.050842
51.550505	2069.373166	19.055859
51.337845	2074.085114	19.060877
51.602673	2067.445906	19.065895
51.295639	2076.841615	19.070912
51.805952	2068.509692	19.075930
51.295799	2074.749624	19.080947
51.465310	2071.987533	19.085965
51.576347	2077.903213	19.090983
51.774272	2070.695866	19.096000
51.831978	2061.382346	19.101018
51.374070	2065.670920	19.106035
51.694132	2067.069033	19.111053
52.028966	2067.144745	19.116071
51.849353	2072.992130	19.121088
51.852076	2084.291701	19.126106
52.185104	2088.380884	19.131123
52.436488	2083.606835	19.136141
52.612837	2078.303450	19.141159
52.254054	2085.543954	19.146176
52.462208	2078.633711	19.151194
52.546778	2079.504405	19.156211
52.561425	2073.377052	19.161229
52.553464	2061.941815	19.166247
52.456896	2071.336874	19.171264
52.808159	2065.185279	19.176282
52.608629	2063.720887	19.181299
52.635513	2062.342101	19.186317
52.668283	2071.188533	19.191335
52.616768	2083.309721	19.196352
52.740156	2086.146478	19.201370
52.588142	2095.958989	19.206387
52.614269	2089.984801	19.211405
52.902574	2091.167464	19.216423
52.646804	2087.016269	19.221440
52.747114	2083.820703	19.226458
52.981124	2090.218130	19.231475
52.564424	2091.728785	19.236493
53.052042	2102.953501	19.241511
53.169772	2122.338467	19.246528
53.253255	2116.243790	19.251546
53.102191	2123.659751	19.256563
53.275440	2116.353449	19.261581
53.517393	2115.344142	19.266599
53.606324	2117.107131	19.271616
53.951283	2119.075865	19.276634
53.972922	2119.901438	19.281651
53.614539	2125.414874	19.286669
53.871697	2111.417645	19.291687
53.560091	2125.660525	19.296704
53.711064	2117.172046	19.301722
53.508498	2120.782908	19.306739
53.074647	2117.011107	19.311757
53.208726	2125.026304	19.316775
53.291822	2136.427109	19.321792
53.664121	2148.178395	19.326810
54.110789	2146.953646	19.331827
53.621674	2152.254826	19.336845
54.001022	2145.669977	19.341863
54.111375	2166.502140	19.346880
54.340583	2169.809029	19.351898
54.546015	2170.855098	19.356915
54.557911	2174.318162	19.361933
54.799885	2168.812916	19.366951
54.507653	2174.118148	19.371968
54.525752	2168.503234	19.376986
55.110260	2170.127709	19.382003
54.676596	2176.274633	19.387021
54.736235	2157.652280	19.392039
54.813979	2162.806661	19.397056
54.732978	2159.142880	19.402074
54.877142	2169.266913	19.407091
54.707540	2173.501361	19.412109
54.728774	2171.431307	19.417127
54.662183	2173.213092	19.422144
54.869377	2163.612426	19.427162
55.164337	2157.429498	19.432179
54.990546	2170.881750	19.437197
55.231668	2166.348447	19.442215
54.903567	2176.068346	19.447232
55.259233	2181.281397	19.452250
55.662920	2191.424738	19.457267
55.415897	2196.986045	19.462285
55.556830	2204.987507	19.467303
55.662899	2201.843693	19.472320
55.494363	2195.527589	19.477338
55.766238	2196.087394	19.482355
55.615758	2199.105793	19.487373
55.854951	2195.262677	19.492391
55.619313	2190.592966	19.497408
56.061210	2193.734241	19.502426
56.196445	2189.790824	19.507443
55.747993	2198.877732	19.512461
56.017037	2190.646176	19.517479
56.055469	2192.191814	19.522496
55.784015	2190.579087	19.527514
56.218206	2190.560588	19.532531
55.833520	2193.645129	19.537549
55.903174	2193.988388	19.542567
56.243167	2189.928749	19.547584
56.272035	2205.166237	19.552602
56.724527	2214.272727	19.557619
56.478030	2209.940355	19.562637
56.807007	2203.750002	19.567655
56.756358	2203.550024	19.572672
56.348259	2193.769751	19.577690
56.709335	2197.011511	19.582707
56.470056	2210.618354	19.587725
56.866946	2211.443382	19.592743
56.852534	2214.088796	19.597760
56.723832	2218.247729	19.602778
56.650212	2212.491808	19.607795
56.876639	2221.931593	19.612813
56.935877	2211.893991	19.617831
56.968191	2211.223028	19.622848
56.817186	2215.513362	19.627866
57.217568	2207.539636	19.632883
57.247674	2229.358227	19.637901
57.233568	2235.687608	19.642919
57.466717	2236.698216	19.647936
57.449666	2239.354325	19.652954
57.792915	2236.747090	19.657971
57.804116	2244.933045	19.662989
57.795294	2235.279594	19.668007
57.570029	2232.277634	19.673024
57.408482	2239.459192	19.678042
57.939949	2239.464178	19.683059
57.621954	2238.331150	19.688077
57.968094	2239.957914	19.693095
57.687588	2241.049503	19.698112
57.372643	2239.282785	19.703130
57.762184	2233.538798	19.708147
57.711982	2236.170664	19.713165
57.886929	2256.450059	19.718183
58.318881	2258.236942	19.723200
58.311899	2260.154208	19.728218
58.629355	2258.182985	19.733235
58.803755	2254.565957	19.738253
58.494079	2249.758506	19.743271
58.446437	2256.009380	19.748288
58.247752	2251.339616	19.753306
58.759560	2251.941763	19.758323
58.675344	2256.176556	19.763341
58.555094	2252.632886	19.768359
58.858418	2250.219137	19.773376
58.832011	2259.073065	19.778394
59.033106	2244.841197	19.783411
58.502745	2251.515042	19.788429
58.648035	2252.600566	19.793447
59.151468	2249.461853	19.798464
58.801139	2248.817905	19.803482
58.956680	2265.798567	19.808499
58.931380	2275.847772	19.813517
59.180609	2276.748523	19.818535
59.513290	2282.820010	19.823552
59.610398	2287.991588	19.828570
59.872225	2277.461659	19.833587
59.496925	2275.565894	19.838605
59.762806	2277.080419	19.843623
59.245511	2283.895367	19.848640
59.269149	2291.106624	19.853658
59.479343	2283.508827	19.858675
59.356388	2278.318906	19.863693
59.622931	2277.076204	19.868711
59.898373	2283.407937	19.873728
59.704541	2286.219579	19.878746
59.673625	2279.890870	19.883763
59.924429	2297.230881	19.888781
60.054619	2311.623415	19.893799
59.981940	2302.525837	19.898816
59.880388	2309.894021	19.903834
60.385140	2304.444477	19.908851
59.632760	2314.241142	19.913869
59.952952	2306.213388	19.918887
60.254496	2321.815326	19.923904
60.289495	2344.038812	19.928922
60.465717	2336.865778	19.933939
60.459335	2333.565599	19.938957
60.445403	2333.250646	19.943975
60.345003	2335.044547	19.948992
60.513135	2342.203490	19.954010
60.600369	2338.725817	19.959027
60.481772	2352.456996	19.964045
60.924742	2361.330521	19.969063
61.212158	2356.542731	19.974080
61.274458	2368.031535	19.979098
61.369528	2360.339249	19.984115
61.315171	2355.226531	19.989133
61.780408	2358.603247	19.994151
61.763146	2360.621516	19.999168
61.609572	2363.373505	20.004186
61.735536	2335.673570	20.009203
61.649577	2341.590838	20.014221
61.589625	2334.585088	20.019239
61.585265	2325.988462	20.024256
61.474487	2339.995498	20.029274
61.804153	2346.016338	20.034291
61.879971	2351.062433	20.039309
61.698535	2363.005686	20.044327
61.904629	2360.668443	20.049344
61.607818	2366.511617	20.054362
61.866005	2357.833733	20.059379
61.503728	2360.927064	20.064397
61.706229	2356.534995	20.069415
62.274471	2358.433190	20.074432
61.979076	2387.814508	20.079450
62.054894	2381.694266	20.084467
61.924643	2383.726398	20.089485
62.089044	2390.957668	20.094503
62.537178	2390.257931	20.099520
62.169959	2388.552923	20.104538
62.508136	2384.710117	20.109555
62.645507	2385.355993	20.114573
62.566235	2388.637854	20.119591
62.596377	2400.194410	20.124608
62.556482	2412.733219	20.129626
62.916987	2407.607632	20.134643
63.326290	2407.674517	20.139661
63.716476	2401.294036	20.144679
63.628629	2393.477164	20.149696
63.005716	2388.961208	20.154714
63.386158	2381.068778	20.159731
63.351834	2377.827720	20.164749
63.206114	2379.526229	20.169767
63.715375	2365.503664	20.174784
63.481585	2369.981489	20.179802
63.502486	2366.982186	20.184819
63.093711	2368.890388	20.189837
63.329607	2388.565710	20.194855
63.842363	2392.859631	20.199872
63.735855	2403.585939	20.204890
63.733524	2394.306928	20.209907
63.600996	2399.629743	20.214925
63.678988	2398.988742	20.219943
63.781476	2391.866126	20.224960
63.118117	2396.141974	20.229978
63.921751	2411.356295	20.234995
64.071541	2422.701772	20.240013
64.159783	2423.761651	20.245031
64.433161	2423.181653	20.250048
64.135261	2432.583096	20.255066
64.325355	2425.456469	20.260083
64.489432	2425.364579	20.265101
64.288965	2423.065531	20.270119
64.794193	2424.092506	20.275136
64.527010	2419.018619	20.280154
64.770286	2421.771881	20.285171
64.549205	2423.104514	20.290189
64.830498	2444.195975	20.295207
64.964495	2443.255559	20.300224
65.114280	2447.908626	20.305242
65.319678	2443.281352	20.310259
65.396950	2445.169232	20.315277
64.962591	2441.801440	20.320295
65.518042	2440.123303	20.325312
65.559427	2447.567849	20.330330
65.227203	2443.721052	20.335347
65.014602	2435.077378	20.340365
65.415455	2442.212218	20.345383
65.606425	2436.952671	20.350400
65.369514	2441.209755	20.355418
65.581260	2447.546176	20.360435
65.662675	2446.666753	20.365453
65.467749	2457.346829	20.370471
65.360017	2452.696061	20.375488
65.172046	2452.840149	20.380506
65.587246	2467.114658	20.385523
65.609381	2473.413508	20.390541
65.523911	2483.690521	20.395559
66.068532	2471.463672	20.400576
66.100747	2469.827989	20.405594
66.416351	2476.108814	20.410611
66.621461	2474.953021	20.415629
66.293714	2474.050818	20.420647
66.602110	2470.355640	20.425664
66.513121	2469.850370	20.430682
66.356107	2486.583235	20.435699
66.607321	2486.885134	20.440717
66.674304	2502.769241	20.445735
67.069936	2487.987178	20.450752
66.927499	2493.800781	20.455770
66.952978	2485.779363	20.460787
67.227171	2481.419069	20.465805
67.361859	2494.591113	20.470823
67.381522	2475.439714	20.475840
66.881033	2474.305667	20.480858
67.176787	2487.053173	20.485875
67.492336	2484.964907	20.490893
67.095514	2487.571977	20.495911
67.553183	2482.178485	20.500928
67.495165	2484.843234	20.505946
67.548249	2484.932605	20.510963
67.856049	2477.515651	20.515981
67.113895	2479.904716	20.520999
67.435405	2481.070299	20.526016
67.521662	2485.460208	20.531034
67.384475	2484.594635	20.536051
67.419797	2501.385106	20.541069
67.699344	2518.906293	20.546087
68.060170	2518.894862	20.551104
67.895617	2521.043147	20.556122
68.021182	2518.364510	20.561139
67.954220	2509.692675	20.566157
68.209552	2529.124644	20.571175
68.175371	2533.483238	20.576192
68.478754	2538.823505	20.581210
68.757212	2541.087209	20.586227
68.752711	2541.158102	20.591245
68.686726	2540.578795	20.596263
68.990841	2540.822010	20.601280
68.795392	2543.036235	20.606298
68.862705	2548.209858	20.611315
69.181741	2532.228081	20.616333
68.852231	2542.765908	20.621351
68.847717	2529.933046	20.626368
68.926797	2531.797788	20.631386
68.934917	2540.665644	20.636403
69.205080	2538.746596	20.641421
69.051866	2547.005788	20.646439
69.188532	2537.399660	20.651456
69.357513	2547.593713	20.656474
69.324318	2567.848557	20.661491
69.548709	2570.029394	20.666509
69.386549	2568.230930	20.671527
69.331580	2564.519276	20.676544
69.681699	2559.996312	20.681562
69.671256	2559.976082	20.686579
69.621142	2560.077634	20.691597
69.645525	2569.511318	20.696615
69.905341	2559.022498	20.701632
69.955394	2583.168481	20.706650
70.037707	2591.303048	20.711667
70.291096	2592.784308	20.716685
70.058406	2597.336825	20.721703
70.364780	2583.153542	20.726720
70.321932	2586.444162	20.731738
70.184023	2591.615182	20.736755
70.459152	2585.684350	20.741773
70.213062	2586.769272	20.746791
70.188092	2584.508627	20.751808
70.456465	2613.863800	20.756826
70.367972	2623.613771	20.761843
70.692192	2617.330356	20.766861
70.931132	2623.157373	20.771879
71.342466	2614.116025	20.776896
71.241639	2614.950808	20.781914
71.270055	2618.595422	20.786931
71.723450	2610.599803	20.791949
71.679528	2607.859643	20.796967
72.001875	2604.737733	20.801984
72.039126	2606.482074	20.807002
71.813423	2613.049496	20.812019
71.937733	2606.692467	20.817037
71.748986	2611.350071	20.822055
72.090277	2613.508509	20.827072
71.682938	2613.846929	20.832090
71.523072	2613.993287	20.837107
71.943736	2606.452179	20.842125
71.808556	2607.804751	20.847143
72.104852	2610.811207	20.852160
72.213972	2611.195749	20.857178
71.971156	2615.291659	20.862195
72.268135	2606.892864	20.867213
71.907955	2606.454561	20.872231
71.764653	2611.498931	20.877248
72.181588	2620.776351	20.882266
72.193563	2619.974977	20.887283
72.335266	2626.512489	20.892301
72.268006	2632.009264	20.897319
72.419143	2634.624790	20.902336
72.511035	2652.497254	20.907354
72.430042	2655.668422	20.912371
72.569312	2650.416880	20.917389
72.568581	2657.539554	20.922407
72.762912	2651.825735	20.927424
72.934049	2669.447582	20.932442
72.965075	2685.571152	20.937459
73.084922	2688.529907	20.942477
73.410135	2680.112057	20.947495
73.478631	2687.485915	20.952512
73.641441	2684.859930	20.957530
73.937391	2686.001559	20.962547
73.943365	2683.762371	20.967565
73.936815	2678.322396	20.972583
74.009110	2676.589253	20.977600
73.981654	2673.788767	20.982618
73.972765	2675.563078	20.987635
73.787334	2684.605957	20.992653
74.057690	2683.842184	20.997671
73.595317	2675.820044	21.002688
73.966875	2672.808602	21.007706
74.004740	2683.516649	21.012723
74.227022	2694.167884	21.017741
73.723328	2701.207489	21.022759
74.041634	2701.821570	21.027776
74.316335	2703.569315	21.032794
74.088110	2710.123821	21.037811
74.676445	2721.208466	21.042829
74.747038	2735.935288	21.047847
74.409801	2730.403146	21.052864
74.797267	2723.713498	21.057882
74.766389	2737.585120	21.062899
75.093814	2728.852634	21.067917
74.809177	2730.414338	21.072935
74.792000	2748.255208	21.077952
75.191697	2755.264383	21.082970
75.119373	2762.849069	21.087987
75.538912	2756.068065	21.093005
75.382246	2761.731423	21.098023
75.404467	2764.710869	21.103040
75.925908	2755.903364	21.108058
76.074955	2755.626614	21.113075
76.539971	2759.719337	21.118093
75.795679	2753.003989	21.123111
75.743764	2758.383983	21.128128
75.998180	2748.909535	21.133146
75.791803	2758.255314	21.138163
76.227215	2754.072855	21.143181
75.992872	2759.202185	21.148199
75.977228	2774.402967	21.153216
76.240106	2776.837913	21.158234
76.403916	2792.324539	21.163251
76.500898	2793.234886	21.168269
76.377833	2794.256202	21.173287
76.376753	2782.283334	21.178304
76.692995	2777.256574	21.183322
76.683502	2780.104427	21.188339
77.259275	2793.165658	21.193357
76.930928	2789.631554	21.198375
76.591575	2796.872202	21.203392
77.054478	2800.339197	21.208410
77.064128	2819.493903	21.213427
77.209964	2808.129804	21.218445
77.452445	2813.073444	21.223463
77.302770	2816.756513	21.228480
77.538379	2804.669018	21.233498
77.459872	2805.346412	21.238515
77.593573	2797.210987	21.243533
77.542593	2806.119052	21.248551
77.735091	2814.041107	21.253568
77.965677	2796.961422	21.258586
77.876742	2808.650527	21.263603
77.827544	2804.009307	21.268621
78.065344	2808.388288	21.273639
77.968808	2834.626318	21.278656
78.242956	2833.871339	21.283674
78.127804	2836.142717	21.288691
78.382944	2832.436898	21.293709
78.240709	2829.314267	21.298727
78.088024	2832.771041	21.303744
78.324603	2832.139849	21.308762
78.049112	2842.811948	21.313779
78.336714	2855.018530	21.318797
78.529275	2863.324136	21.323815
78.703345	2865.344319	21.328832
78.647892	2861.882331	21.333850
78.914145	2874.528105	21.338867
79.040763	2889.092680	21.343885
79.327370	2890.683257	21.348903
79.163707	2898.964901	21.353920
79.308763	2887.986779	21.358938
79.271309	2899.056771	21.363955
79.521058	2895.384939	21.368973
79.100660	2896.654914	21.373991
79.191148	2902.939855	21.379008
79.269279	2911.514760	21.384026
79.245533	2929.256942	21.389043
79.701513	2927.428850	21.394061
80.116021	2924.299741	21.399079
79.816741	2923.465084	21.404096
80.025806	2920.010498	21.409114
80.095482	2924.482917	21.414131
80.158162	2948.331175	21.419149
80.091168	2945.283827	21.424167
80.251702	2955.051950	21.429184
80.752532	2944.627086	21.434202
80.702232	2958.406938	21.439219
80.352925	2951.200079	21.444237
80.746095	2952.162825	21.449255
80.457214	2957.748113	21.454272
80.814935	2951.472211	21.459290
81.138023	2960.178407	21.464307
81.390372	2965.017234	21.469325
81.189728	2958.008550	21.474343
81.284201	2962.564934	21.479360
81.730657	2955.231880	21.484378
81.289081	2941.194624	21.489395
81.364029	2934.968785	21.494413
81.550910	2945.024568	21.499431
81.639758	2957.945754	21.504448
81.921166	2951.305696	21.509466
81.880319	2960.813804	21.514483
81.959790	2961.774416	21.519501
81.936508	2958.710908	21.524519
81.922638	2967.233100	21.529536
82.184741	2965.750903	21.534554
82.182380	2966.089200	21.539571
82.286656	2964.889231	21.544589
82.213117	2958.034380	21.549607
82.183513	2967.580730	21.554624
82.479956	2972.465553	21.559642
82.400545	2959.350634	21.564659
82.536010	2962.270537	21.569677
82.519481	2961.099943	21.574695
82.409716	2963.661812	21.579712
82.738918	2978.903689	21.584730
83.047798	2984.571578	21.589747
83.448503	2969.180202	21.594765
84.282823	2954.165768	21.599783
83.437181	2946.671492	21.604800
83.905810	2935.905630	21.609818
83.785447	2932.983992	21.614835
83.623602	2930.686909	21.619853
83.754514	2921.838373	21.624871
83.580854	2937.124684	21.629888
83.933844	2926.698401	21.634906
83.652330	2928.613201	21.639923
83.875151	2932.404120	21.644941
84.144514	2923.755512	21.649959
83.713537	2931.942818	21.654976
83.892883	2934.592937	21.659994
83.884519	2920.572782	21.665011
84.005811	2949.436378	21.670029
84.100881	2954.686494	21.675047
84.029002	2970.206617	21.680064
84.531671	2959.086016	21.685082
84.136816	2971.416783	21.690099
84.345279	2964.414349	21.695117
84.270917	2975.560816	21.700135
84.189723	2993.546824	21.705152
84.582901	2997.064409	21.710170
84.767334	3003.655395	21.715187
84.340609	3004.758713	21.720205
85.004994	3012.201460	21.725223
84.806700	3019.495993	21.730240
85.303057	3020.017345	21.735258
85.020135	3023.423247	21.740275
84.786974	3018.766250	21.745293
85.288399	3029.319451	21.750311
85.345463	3044.129213	21.755328
85.329332	3044.907756	21.760346
85.739620	3045.959718	21.765363
85.838349	3038.965826	21.770381
86.059044	3045.983771	21.775399
85.959300	3048.834545	21.780416
85.793151	3046.194806	21.785434
86.384846	3048.901046	21.790451
86.097657	3056.056474	21.795469
86.822233	3057.994114	21.800487
85.962461	3067.262295	21.805504
86.388818	3067.902759	21.810522
86.443487	3075.013762	21.815539
86.171423	3075.048624	21.820557
86.508395	3077.253547	21.825575
86.462835	3078.263955	21.830592
86.577133	3078.796471	21.835610
86.787848	3095.191290	21.840627
86.638798	3100.628220	21.845645
87.188125	3098.445453	21.850663
87.132176	3098.443263	21.855680
87.249505	3098.690949	21.860698
87.561565	3100.032253	21.865715
87.388078	3097.498509	21.870733
87.936577	3109.977162	21.875751
87.604663	3109.900212	21.880768
87.919870	3115.410339	21.885786
88.112004	3128.527388	21.890803
87.969456	3132.728313	21.895821
88.098774	3121.193556	21.900839
87.969307	3124.880320	21.905856
88.184902	3123.992818	21.910874
88.100117	3119.016591	21.915891
87.646787	3124.996349	21.920909
88.251743	3117.672275	21.925927
88.366097	3142.213688	21.930944
88.374937	3153.345229	21.935962
88.670510	3158.128664	21.940979
88.539939	3154.710993	21.945997
88.792744	3144.994801	21.951015
88.840827	3149.480436	21.956032
88.752999	3153.581415	21.961050
89.121743	3162.224768	21.966067
88.921462	3173.478808	21.971085
89.176486	3178.750405	21.976103
89.315327	3176.563185	21.981120
89.628723	3183.544822	21.986138
89.859533	3172.849500	21.991155
89.518845	3179.840104	21.996173
89.751344	3177.276909	22.001191
89.637932	3182.006035	22.006208
89.502715	3188.339237	22.011226
89.774414	3200.897709	22.016243
90.025400	3206.225137	22.021261
89.940721	3213.373482	22.026279
89.980025	3220.309981	22.031296
90.072748	3214.602354	22.036314
90.281906	3209.908057	22.041331
90.094850	3223.781681	22.046349
90.372774	3230.259076	22.051367
90.485206	3236.813675	22.056384
90.513829	3241.903589	22.061402
91.205445	3234.293680	22.066419
91.241559	3236.172173	22.071437
91.619094	3220.972754	22.076455
91.686407	3226.320653	22.081472
91.458364	3225.383983	22.086490
91.858540	3224.545950	22.091507
91.773729	3227.902965	22.096525
91.669465	3210.154102	22.101543
91.634642	3206.223836	22.106560
91.856758	3217.322006	22.111578
91.946947	3229.336695	22.116595
91.935485	3222.242691	22.121613
92.196047	3222.321698	22.126631
91.960762	3221.665856	22.131648
92.024954	3219.775741	22.136666
91.855141	3220.763357	22.141683
91.343835	3223.939895	22.146701
91.712749	3225.312416	22.151719
91.872162	3245.890306	22.156736
91.943573	3250.615331	22.161754
92.089108	3256.638166	22.166771
92.335565	3266.439794	22.171789
92.429602	3275.177561	22.176807
92.482691	3275.910383	22.181824
92.805493	3286.360495	22.186842
92.759763	3279.329046	22.191859
92.835868	3305.502820	22.196877
93.048333	3308.889219	22.201895
93.153305	3313.185581	22.206912
92.987719	3318.617545	22.211930
93.280451	3314.792547	22.216947
93.592382	3329.111539	22.221965
93.725509	3331.916926	22.226983
94.556264	3317.113833	22.232000
94.638421	3307.473265	22.237018
95.153782	3292.488783	22.242035
94.830252	3280.006916	22.247053
94.712366	3267.414983	22.252071
94.838790	3274.634273	22.257088
94.619665	3278.050555	22.262106
94.693216	3266.289769	22.267123
94.990391	3275.205353	22.272141
94.922777	3267.661801	22.277159
94.916927	3259.883993	22.282176
94.823612	3265.272833	22.287194
94.879932	3265.100181	22.292211
94.901413	3278.460045	22.297229
94.844663	3274.402784	22.302247
95.023763	3273.453800	22.307264
94.543563	3283.257947	22.312282
95.085697	3273.343222	22.317299
95.030964	3289.526218	22.322317
95.264583	3297.724207	22.327335
95.414913	3300.157268	22.332352
95.211060	3310.589003	22.337370
95.379420	3302.298525	22.342387
95.104408	3310.927892	22.347405
95.626185	3330.263983	22.352423
96.033146	3336.873664	22.357440
95.680348	3341.129592	22.362458
95.862991	3340.398943	22.367475
96.044052	3353.236126	22.372493
96.286712	3364.492332	22.377511
96.465604	3357.318378	22.382528
96.044730	3372.490766	22.387546
96.632080	3366.198172	22.392563
96.881925	3391.301914	22.397581
96.763278	3401.083527	22.402599
97.190964	3397.199143	22.407616
97.082630	3399.492272	22.412634
97.179462	3397.617018	22.417651
96.972787	3398.439272	22.422669
97.230780	3400.507356	22.427687
97.573224	3394.455996	22.432704
97.231413	3403.282734	22.437722
97.569424	3412.085072	22.442739
97.415240	3420.659918	22.447757
97.542289	3417.201172	22.452775
97.741666	3418.565761	22.457792
97.763143	3427.623997	22.462810
98.108740	3438.338080	22.467827
98.133684	3451.238337	22.472845
98.017143	3450.329003	22.477863
98.436536	3453.908356	22.482880
98.101480	3462.551250	22.487898
98.429188	3448.670690	22.492915
98.502629	3470.109475	22.497933
98.452921	3474.847456	22.502951
99.115580	3479.246722	22.507968
98.625875	3481.893502	22.512986
98.901234	3477.917865	22.518003
98.590003	3479.182555	22.523021
99.183577	3496.026445	22.528039
99.507196	3504.938414	22.533056
99.530303	3517.910711	22.538074
99.511883	3509.709640	22.543091
99.374611	3511.167395	22.548109
99.156376	3510.192796	22.553127
99.764301	3522.848248	22.558144
99.884635	3536.588326	22.563162
99.878167	3532.775980	22.568179
100.001310	3533.483414	22.573197
100.072313	3534.841669	22.578215
100.516548	3533.822012	22.583232
100.529561	3546.130554	22.588250
101.047510	3541.773074	22.593267
101.212274	3531.279429	22.598285
101.090105	3532.031283	22.603303
101.000931	3522.844466	22.608320
101.023895	3526.458722	22.613338
101.170476	3523.729057	22.618355
100.914165	3524.912665	22.623373
100.915525	3526.315151	22.628391
101.355246	3542.349053	22.633408
101.021886	3552.403058	22.638426
101.633030	3550.136390	22.643443
101.452776	3552.887645	22.648461
101.300227	3549.086163	22.653479
101.555063	3556.586000	22.658496
101.565347	3567.923933	22.663514
102.178418	3583.486322	22.668531
101.941666	3586.148821	22.673549
101.540315	3586.877658	22.678567
102.373778	3586.541051	22.683584
102.282756	3590.205580	22.688602
102.819009	3597.695781	22.693619
102.766138	3608.979989	22.698637
102.426894	3622.518551	22.703655
102.697284	3614.593186	22.708672
102.331283	3620.641640	22.713690
102.593097	3611.029156	22.718707
102.586281	3623.701085	22.723725
103.123155	3646.370418	22.728743
103.154769	3631.613468	22.733760
102.836737	3640.617407	22.738778
103.288208	3640.772375	22.743795
103.269042	3657.477336	22.748813
103.516008	3666.373398	22.753831
103.517903	3663.455078	22.758848
103.754878	3669.936526	22.763866
104.150123	3664.328089	22.768883
103.861972	3670.023764	22.773901
104.032584	3687.376699	22.778919
104.567352	3688.827942	22.783936
104.449170	3694.546467	22.788954
104.751459	3683.772388	22.793971
104.589411	3690.527815	22.798989
104.767655	3689.775852	22.804007
104.980555	3686.620516	22.809024
104.838773	3693.307888	22.814042
105.101435	3693.586587	22.819059
105.003089	3699.888470	22.824077
104.654161	3709.901926	22.829095
105.448846	3714.885073	22.834112
105.344860	3728.135300	22.839130
105.629191	3729.571987	22.844147
105.784391	3724.960036	22.849165
105.557803	3725.618750	22.854183
105.714169	3722.909427	22.859200
105.721135	3729.063313	22.864218
105.644994	3729.965592	22.869235
106.108842	3754.781982	22.874253
105.987228	3746.071579	22.879271
106.167798	3751.849956	22.884288
105.958038	3754.937094	22.889306
106.050997	3759.734974	22.894323
106.341318	3776.992664	22.899341
106.633509	3780.725429	22.904359
106.491219	3780.042592	22.909376
106.494289	3792.737378	22.914394
106.896779	3796.587492	22.919411
107.117799	3810.813821	22.924429
107.254436	3808.797015	22.929447
107.715418	3799.665360	22.934464
107.699647	3803.087845	22.939482
107.790863	3804.782113	22.944499
108.157017	3797.147402	22.949517
108.363630	3808.632209	22.954535
108.288245	3799.290860	22.959552
108.323581	3795.012902	22.964570
108.137083	3798.755279	22.969587
108.435981	3794.565240	22.974605
108.302139	3792.570391	22.979623
108.341282	3795.449469	22.984640
108.317864	3800.244473	22.989658
108.719339	3795.106694	22.994675
108.654895	3805.892115	22.999693
108.820998	3818.594413	23.004711
109.270195	3824.770970	23.009728
109.138022	3825.352856	23.014746
108.885384	3826.217665	23.019763
108.853580	3827.441565	23.024781
108.666352	3833.726447	23.029799
108.865174	3834.196456	23.034816
108.727330	3858.370308	23.039834
109.124820	3865.017279	23.044851
109.483363	3869.716104	23.049869
109.969269	3885.544751	23.054887
109.804039	3878.124756	23.059904
110.029127	3888.747181	23.064922
109.980126	3893.845888	23.069939
110.471750	3895.428201	23.074957
110.486306	3914.656646	23.079975
110.423660	3905.162617	23.084992
110.576814	3905.890127	23.090010
110.430412	3913.028892	23.095027
110.763943	3911.265005	23.100045
110.752538	3930.252974	23.105063
111.029708	3928.831117	23.110080
111.062962	3933.773178	23.115098
111.279481	3935.041150	23.120115
111.215633	3926.249071	23.125133
111.367169	3943.952105	23.130151
111.635723	3949.680817	23.135168
111.972783	3957.256537	23.140186
112.047122	3964.898566	23.145203
112.450641	3960.028170	23.150221
112.023971	3957.591249	23.155239
112.190081	3959.276632	23.160256
112.481873	3966.023679	23.165274
112.354496	3958.855491	23.170291
112.646276	3954.290942	23.175309
112.225486	3964.008136	23.180327
112.518443	3959.255146	23.185344
112.835224	3958.302209	23.190362
112.673160	3962.517725	23.195379
113.063805	3980.827221	23.200397
112.845527	3990.902728	23.205415
112.917938	3981.518605	23.210432
113.090514	3990.803294	23.215450
113.190834	3999.136343	23.220467
113.607851	4012.437681	23.225485
113.591161	4024.751689	23.230503
113.838768	4027.435185	23.235520
114.078670	4026.152815	23.240538
113.703492	4016.387017	23.245555
113.743933	4013.792033	23.250573
113.812468	4031.505457	23.255591
114.530525	4034.724999	23.260608
114.612875	4044.752152	23.265626
114.458917	4037.642042	23.270643
114.860175	4027.747851	23.275661
114.836244	4040.979102	23.280679
114.866391	4025.893602	23.285696
115.194031	4042.805726	23.290714
115.347667	4051.426591	23.295731
115.508541	4048.284830	23.300749
115.160551	4050.141847	23.305767
115.527493	4050.912261	23.310784
115.664599	4050.269725	23.315802
115.484214	4059.419638	23.320819
115.572069	4054.085083	23.325837
115.583345	4070.945147	23.330855
115.729080	4080.047826	23.335872
116.048245	4084.907051	23.340890
115.856113	4088.396064	23.345907
116.048205	4100.671974	23.350925
116.129862	4117.495605	23.355943
116.349141	4109.963899	23.360960
116.413741	4105.395724	23.365978
116.731427	4115.688169	23.370995
117.306531	4122.793121	23.376013
117.123446	4136.510917	23.381031
117.360188	4126.299894	23.386048
117.284815	4126.189191	23.391066
117.142235	4136.147060	23.396083
117.578212	4138.928238	23.401101
117.777196	4140.924627	23.406119
117.700839	4129.378714	23.411136
117.683691	4139.672659	23.416154
117.879597	4157.024138	23.421171
118.367689	4155.056514	23.426189
118.277364	4159.088083	23.431207
118.742055	4165.925292	23.436224
118.442865	4162.137774	23.441242
118.383531	4161.821904	23.446259
118.444433	4154.240142	23.451277
118.354312	4161.632433	23.456295
118.427237	4173.815414	23.461312
118.730535	4190.435726	23.466330
118.591742	4198.162452	23.471347
119.055423	4200.947556	23.476365
118.836111	4208.428177	23.481383
119.078797	4220.814438	23.486400
119.176891	4232.524515	23.491418
119.327692	4238.267219	23.496435
119.693530	4250.937987	23.501453
119.793328	4264.056848	23.506471
120.015162	4248.353071	23.511488
120.136880	4247.092520	23.516506
120.136601	4252.732749	23.521523
120.285072	4252.909744	23.526541
120.294067	4264.449242	23.531559
120.305535	4271.442172	23.536576
120.247353	4264.115484	23.541594
120.541720	4285.015786	23.546611
120.861575	4300.333798	23.551629
120.791574	4301.497335	23.556647
120.930364	4303.256750	23.561664
121.139488	4306.172940	23.566682
121.063101	4323.716207	23.571699
121.505253	4330.881854	23.576717
121.554243	4330.019701	23.581735
121.586721	4335.821319	23.586752
121.765088	4339.696603	23.591770
122.429542	4350.134535	23.596787
122.727971	4355.152561	23.601805
122.654721	4356.768756	23.606823
123.024581	4355.218341	23.611840
122.882032	4346.129196	23.616858
122.623313	4357.294066	23.621875
123.150777	4347.878182	23.626893
123.033325	4350.076920	23.631911
123.054290	4353.375083	23.636928
123.310518	4349.719924	23.641946
122.966995	4352.604060	23.646963
123.006290	4352.227170	23.651981
123.235341	4364.853744	23.656999
123.338215	4368.528530	23.662016
123.418032	4382.400736	23.667034
123.310097	4385.022378	23.672051
123.754302	4402.971901	23.677069
123.937282	4416.141214	23.682087
123.973169	4414.862284	23.687104
124.207120	4412.246661	23.692122
124.440935	4425.158376	23.697139
124.514479	4434.811587	23.702157
124.325134	4439.489519	23.707175
124.605676	4444.641387	23.712192
124.766870	4437.995329	23.717210
124.447933	4448.468808	23.722227
124.635255	4458.093075	23.727245
125.331075	4469.220400	23.732263
125.098514	4484.634872	23.737280
125.483499	4479.007432	23.742298
125.704077	4494.901873	23.747315
125.730577	4495.877963	23.752333
126.033413	4506.834822	23.757351
125.813562	4507.138763	23.762368
126.048291	4494.889455	23.767386
125.749597	4506.607899	23.772403
126.107160	4525.773556	23.777421
126.413206	4530.272070	23.782439
126.518992	4526.344936	23.787456
127.110766	4518.139548	23.792474
126.738702	4521.804427	23.797491
127.139859	4517.373768	23.802509
127.464468	4534.924923	23.807527
127.391916	4540.748561	23.812544
127.749155	4542.056257	23.817562
127.748976	4543.396874	23.822579
127.664188	4538.872300	23.827597
127.894438	4538.041284	23.832615
127.881295	4540.830220	23.837632
128.022356	4539.635642	23.842650
127.630574	4550.190989	23.847667
128.185073	4570.060164	23.852685
128.218426	4573.261733	23.857703
128.008733	4580.674718	23.862720
128.446454	4574.313578	23.867738
128.660076	4589.262567	23.872755
129.052499	4592.167078	23.877773
129.227313	4597.768748	23.882791
128.956454	4606.086200	23.887808
129.355296	4599.266222	23.892826
129.154400	4602.765513	23.897843
129.313370	4621.519529	23.902861
129.527061	4632.533503	23.907879
129.670900	4642.455189	23.912896
129.957045	4633.705896	23.917914
129.623002	4638.804087	23.922931
130.258045	4653.632056	23.927949
130.647621	4659.740402	23.932967
130.192079	4664.589271	23.937984
130.521393	4653.634259	23.943002
130.283029	4665.221969	23.948019
130.546371	4679.852189	23.953037
130.513405	4692.087590	23.958055
130.501871	4699.460358	23.963072
130.590334	4697.527313	23.968090
131.017376	4713.421234	23.973107
130.891703	4713.226208	23.978125
131.345315	4716.474691	23.983143
131.151705	4735.423187	23.988160
131.714678	4745.344759	23.993178
132.296087	4739.463013	23.998195
132.238777	4738.628514	24.003213
132.578242	4738.315151	24.008231
132.061179	4739.811346	24.013248
132.705742	4732.568753	24.018266
132.747324	4730.006537	24.023283
132.637095	4734.020397	24.028301
133.092258	4751.843991	24.033319
132.975582	4758.283336	24.038336
133.223759	4752.964382	24.043354
133.085672	4760.562087	24.048371
133.324791	4758.275546	24.053389
133.545067	4757.085487	24.058407
133.117196	4771.388484	24.063424
133.516502	4779.841608	24.068442
133.559379	4789.043457	24.073459
133.478340	4794.793816	24.078477
133.977551	4808.606311	24.083495
134.162826	4820.071885	24.088512
134.408489	4815.213328	24.093530
134.068363	4821.534264	24.098547
133.883926	4836.635219	24.103565
134.443911	4836.253331	24.108583
134.822048	4857.792203	24.113600
135.606228	4867.419155	24.118618
135.571078	4878.334184	24.123635
135.651614	4882.987245	24.128653
135.761163	4880.869403	24.133671
135.990780	4876.386138	24.138688
136.136440	4873.980127	24.143706
135.869504	4873.784111	24.148723
135.682716	4864.193429	24.153741
135.828203	4867.795651	24.158759
136.131026	4876.724568	24.163776
136.216422	4879.441535	24.168794
136.291225	4894.379167	24.173811
136.491487	4890.961111	24.178829
136.732054	4905.957765	24.183847
136.247738	4923.893779	24.188864
136.424605	4923.843009	24.193882
136.935129	4933.136479	24.198899
137.215229	4949.366165	24.203917
137.479325	4947.229696	24.208935
137.690503	4961.747821	24.213952
137.840636	4956.078561	24.218970
137.877239	4954.359166	24.223987
137.813718	4969.794750	24.229005
138.115243	4979.899919	24.234023
138.133614	4978.831101	24.239040
138.320045	4985.358777	24.244058
138.190660	4982.958156	24.249075
138.503190	4999.053946	24.254093
138.819598	5010.231735	24.259111
138.620160	5010.225786	24.264128
138.834053	5007.546555	24.269146
138.885198	5015.716074	24.274163
139.236869	5038.106462	24.279181
139.487645	5046.260676	24.284199
139.420277	5045.818564	24.289216
139.529118	5050.841748	24.294234
139.566848	5057.790352	24.299251
139.788125	5063.236930	24.304269
140.266027	5074.570605	24.309287
140.341698	5086.120537	24.314304
140.645262	5078.458138	24.319322
140.436280	5075.672591	24.324339
140.711018	5088.064277	24.329357
140.973241	5096.274842	24.334375
140.672453	5106.178524	24.339392
140.701381	5103.159997	24.344410
140.810935	5114.607259	24.349427
140.914824	5127.455179	24.354445
141.376317	5133.808159	24.359463
141.636088	5150.205371	24.364480
141.728881	5148.741765	24.369498
142.192924	5152.192558	24.374515
142.592289	5152.289534	24.379533
142.803205	5144.871409	24.384551
142.799696	5145.670733	24.389568
142.515069	5148.480325	24.394586
142.908048	5149.316437	24.399603
142.629675	5150.470860	24.404621
142.737044	5142.884599	24.409639
143.132611	5170.923872	24.414656
143.079976	5169.862488	24.419674
143.420629	5179.274232	24.424691
142.948052	5176.842622	24.429709
143.803515	5184.823930	24.434727
143.618562	5201.328942	24.439744
143.926649	5201.187937	24.444762
144.220711	5201.547931	24.449779
143.953366	5204.345905	24.454797
144.393978	5214.417928	24.459815
144.668867	5228.824554	24.464832
144.788265	5238.289230	24.469850
144.812601	5242.389635	24.474867
144.846092	5248.100045	24.479885
145.338481	5238.782598	24.484903
145.080819	5243.186552	24.489920
145.005278	5258.315711	24.494938
145.397377	5266.080333	24.499955
145.120640	5272.890750	24.504973
145.445429	5284.636784	24.509991
145.586180	5297.981057	24.515008
145.497083	5304.281202	24.520026
145.957716	5302.219692	24.525043
145.785204	5326.207956	24.530061
146.451292	5327.133527	24.535079
146.632509	5322.741928	24.540096
146.404642	5322.222562	24.545114
146.930465	5333.920778	24.550131
147.138469	5357.418512	24.555149
147.273022	5351.426473	24.560167
147.319039	5363.856798	24.565184
147.094460	5362.664192	24.570202
147.285038	5363.244363	24.575219
147.376103	5376.374307	24.580237
147.459614	5384.031991	24.585255
147.358435	5391.077021	24.590272
147.734216	5410.007475	24.595290
148.191113	5417.925688	24.600307
147.986702	5427.993425	24.605325
148.831782	5441.849580	24.610343
148.284771	5450.975711	24.615360
148.204738	5453.755007	24.620378
148.657963	5469.474274	24.625395
148.665670	5486.479813	24.630413
148.860945	5488.885030	24.635431
148.986698	5504.048442	24.640448
149.098287	5513.218452	24.645466
149.534343	5520.317160	24.650483
149.651339	5535.181996	24.655501
150.279017	5533.035108	24.660519
150.165588	5540.443063	24.665536
150.517545	5546.636973	24.670554
151.433650	5547.872580	24.675571
151.658871	5544.973918	24.680589
152.146564	5518.699059	24.685607
152.410834	5502.447207	24.690624
152.146001	5507.963883	24.695642
152.204585	5505.665651	24.700659
151.836304	5498.406520	24.705677
151.885780	5476.868359	24.710695
151.760705	5498.567626	24.715712
152.041742	5501.125131	24.720730
152.343666	5492.786196	24.725747
152.123682	5513.192625	24.730765
152.016943	5503.758759	24.735783
152.217145	5518.497465	24.740800
152.262180	5534.653047	24.745818
152.381208	5535.748034	24.750835
152.235878	5549.507835	24.755853
152.875782	5560.934604	24.760871
152.845815	5576.602906	24.765888
153.045361	5589.782172	24.770906
153.141235	5602.495580	24.775923
152.971439	5605.917290	24.780941
153.564834	5622.212898	24.785959
153.501108	5631.566630	24.790976
153.719549	5625.375788	24.795994
154.013729	5635.320372	24.801011
154.046283	5656.022397	24.806029
154.300766	5651.890689	24.811047
154.398825	5659.538923	24.816064
154.542902	5685.253634	24.821082
154.623095	5690.442621	24.826099
155.023532	5688.480393	24.831117
155.300027	5700.322449	24.836135
155.337412	5706.522300	24.841152
155.989433	5706.152979	24.846170
156.213308	5703.227737	24.851187
155.698549	5709.422207	24.856205
156.302696	5701.460646	24.861223
156.365522	5702.475482	24.866240
156.223589	5718.106404	24.871258
156.947339	5724.949511	24.876275
156.536036	5728.107811	24.881293
156.932551	5731.617572	24.886311
156.766297	5725.836074	24.891328
156.951466	5749.153982	24.896346
157.343563	5749.301836	24.901363
157.330320	5763.731562	24.906381
157.593610	5764.939680	24.911399
157.764656	5776.135843	24.916416
157.595592	5796.958473	24.921434
157.818629	5798.977734	24.926451
157.711830	5805.271659	24.931469
158.158934	5818.652073	24.936487
158.008453	5829.993978	24.941504
158.467322	5840.715487	24.946522
158.718704	5848.154781	24.951539
158.840404	5866.599216	24.956557
158.790559	5862.899298	24.961575
159.141310	5878.290739	24.966592
159.153182	5886.912489	24.971610
159.295812	5894.235751	24.976627
159.368063	5912.418535	24.981645
159.952780	5924.976718	24.986663
159.953367	5921.964470	24.991680
159.859370	5938.229367	24.996698
160.709661	5942.846880	25.001715
160.595488	5954.404782	25.006733
160.871488	5954.719054	25.011751
160.929796	5950.768990	25.016768
161.145159	5974.479055	25.021786
161.294131	5971.877749	25.026803
161.288376	5980.868855	25.031821
161.289330	5976.023542	25.036839
161.372725	5991.529456	25.041856
161.385663	6005.240462	25.046874
161.710882	6010.957062	25.051891
161.867077	6029.178364	25.056909
162.192235	6042.172628	25.061927
162.368302	6039.863633	25.066944
162.274681	6045.660712	25.071962
162.853592	6054.420083	25.076979
163.066569	6070.894011	25.081997
163.266556	6065.707343	25.087015
163.412161	6060.067614	25.092032
163.226339	6063.013240	25.097050
163.634089	6076.342329	25.102067
163.737197	6086.086001	25.107085
163.792403	6088.274283	25.112103
163.809479	6088.054766	25.117120
163.969606	6098.085638	25.122138
164.260825	6113.182668	25.127155
164.416370	6117.547533	25.132173
164.698565	6112.635848	25.137191
165.011960	6128.295456	25.142208
164.926494	6145.361782	25.147226
165.113660	6141.722783	25.152243
165.897208	6136.721206	25.157261
166.240202	6127.012944	25.162279
166.365241	6127.156172	25.167296
166.372451	6125.603171	25.172314
166.693995	6124.930512	25.177331
166.219196	6128.319546	25.182349
166.705822	6127.029378	25.187367
166.872466	6126.552632	25.192384
166.541800	6132.488843	25.197402
166.873386	6141.664826	25.202419
167.059516	6150.934281	25.207437
167.041512	6164.756283	25.212455
167.172241	6161.387689	25.217472
167.116766	6182.018051	25.222490
167.382229	6190.811540	25.227507
167.955611	6194.406880	25.232525
167.709512	6214.283822	25.237543
168.104691	6220.335888	25.242560
168.049920	6227.607283	25.247578
168.341887	6228.811310	25.252595
168.565350	6246.490408	25.257613
168.565698	6254.215545	25.262631
168.712690	6253.666543	25.267648
168.648658	6281.354896	25.272666
168.989237	6281.699855	25.277683
169.212647	6299.938303	25.282701
169.464947	6319.582631	25.287719
169.988408	6318.050605	25.292736
169.864031	6329.096144	25.297754
170.355170	6326.571612	25.302771
170.370402	6336.329715	25.307789
170.316118	6336.316995	25.312807
171.023945	6334.972349	25.317824
170.738882	6345.395573	25.322842
171.062230	6357.806703	25.327859
171.493300	6366.322190	25.332877
171.386413	6366.669813	25.337895
171.671920	6361.707071	25.342912
171.766256	6356.653428	25.347930
171.812215	6370.781309	25.352947
172.288496	6382.157952	25.357965
171.958234	6393.052925	25.362983
171.952681	6388.648154	25.368000
172.259043	6390.561831	25.373018
172.063561	6406.851693	25.378035
172.512007	6417.139766	25.383053
172.715307	6420.837988	25.388071
173.246859	6441.863535	25.393088
172.931269	6452.236920	25.398106
173.235168	6455.011228	25.403123
173.514870	6472.098803	25.408141
173.563773	6475.380801	25.413159
173.901795	6483.128511	25.418176
174.270221	6486.316350	25.423194
174.652318	6506.945379	25.428211
174.458897	6508.454778	25.433229
174.643142	6510.535134	25.438247
174.864206	6508.234901	25.443264
174.673762	6523.113977	25.448282
175.347450	6529.780902	25.453299
175.480903	6528.201495	25.458317
175.139168	6551.361979	25.463335
175.846349	6556.615493	25.468352
175.673725	6574.503859	25.473370
175.354483	6575.239220	25.478387
175.942304	6601.858496	25.483405
176.111787	6602.681804	25.488423
176.070226	6604.301457	25.493440
176.419939	6621.003015	25.498458
177.127091	6626.945828	25.503475
177.469698	6640.209360	25.508493
177.412245	6651.858873	25.513511
177.699190	6644.414418	25.518528
177.801659	6649.872458	25.523546
177.964213	6649.223096	25.528563
177.974053	6664.119959	25.533581
178.403721	6672.233317	25.538599
178.476484	6671.134581	25.543616
178.716002	6688.456146	25.548634
178.730368	6681.808331	25.553651
178.866991	6695.545204	25.558669
178.795921	6708.350345	25.563687
179.006580	6703.622472	25.568704
179.022028	6726.625874	25.573722
179.650891	6732.908274	25.578739
180.047071	6736.369480	25.583757
179.640466	6743.339848	25.588775
180.221924	6756.634217	25.593792
180.151461	6763.090079	25.598810
180.842914	6763.467856	25.603827
180.798710	6777.394135	25.608845
180.586254	6791.608437	25.613863
180.884456	6799.363915	25.618880
181.170950	6796.122884	25.623898
180.996640	6794.847500	25.628915
181.289246	6820.660682	25.633933
181.334717	6834.254963	25.638951
181.424165	6830.868098	25.643968
182.192183	6848.554557	25.648986
181.918357	6851.022281	25.654003
182.310440	6851.280439	25.659021
182.271647	6872.014391	25.664039
182.622971	6874.958675	25.669056
182.980831	6898.017062	25.674074
182.825356	6897.097655	25.679092
183.101236	6912.178379	25.684109
183.412886	6920.159272	25.689127
183.580384	6919.211282	25.694144
183.821416	6945.106767	25.699162
184.139883	6944.677234	25.704180
184.123174	6945.679001	25.709197
184.036863	6960.179051	25.714215
184.435302	6964.066096	25.719232
185.106205	6955.854576	25.724250
185.142801	6953.522882	25.729268
185.489238	6956.538130	25.734285
185.553841	6982.177178	25.739303
186.153112	6973.144483	25.744320
185.918106	6989.585871	25.749338
185.900735	6981.052758	25.754356
186.257275	6983.610169	25.759373
186.260125	6983.236315	25.764391
186.834499	6994.367345	25.769408
186.987375	7003.286144	25.774426
187.410816	7007.778637	25.779444
187.439112	7008.763240	25.784461
187.286205	7017.675384	25.789479
187.162209	7007.529877	25.794496
187.600377	7021.320898	25.799514
187.913612	7032.340744	25.804532
187.967561	7025.270852	25.809549
187.983710	7038.593043	25.814567
188.076712	7046.750127	25.819584
188.233522	7062.003442	25.824602
188.353568	7062.073486	25.829620
188.346058	7078.673695	25.834637
188.405470	7102.121487	25.839655
188.662994	7115.971916	25.844672
188.955499	7131.262693	25.849690
189.048094	7145.466767	25.854708
189.542063	7163.964687	25.859725
189.520981	7172.868499	25.864743
189.966619	7191.795403	25.869760
189.712414	7199.959304	25.874778
190.231118	7210.041271	25.879796
190.766950	7220.518131	25.884813
190.680116	7231.495622	25.889831
191.113565	7232.174455	25.894848
191.664952	7234.893085	25.899866
191.621139	7237.205636	25.904884
191.750161	7233.258101	25.909901
191.635038	7249.258535	25.914919
192.176813	7248.661521	25.919936
192.601816	7257.513331	25.924954
192.454141	7266.793392	25.929972
192.991585	7261.747010	25.934989
192.638301	7266.910773	25.940007
193.033173	7265.056452	25.945024
193.359643	7276.476749	25.950042
193.347148	7291.848324	25.955060
194.190382	7288.736273	25.960077
193.782821	7300.933904	25.965095
193.937445	7296.677885	25.970112
194.058590	7301.954122	25.975130
194.398764	7322.310160	25.980148
195.055342	7315.905701	25.985165
194.759911	7328.884508	25.990183
194.938180	7320.734408	25.995200
195.000729	7333.846433	26.000218
195.174412	7357.872931	26.005236
195.473991	7353.044546	26.010253
195.772637	7365.116438	26.015271
195.721833	7372.272658	26.020288
195.464271	7389.980337	26.025306
195.399745	7393.020427	26.030324
196.019608	7411.594739	26.035341
196.129754	7424.756974	26.040359
196.052616	7440.041300	26.045376
196.386398	7450.129911	26.050394
197.111168	7472.936377	26.055412
197.071642	7474.339917	26.060429
197.006421	7494.557693	26.065447
197.753610	7495.055925	26.070464
198.019839	7496.377906	26.075482
198.153060	7518.806871	26.080500
198.709416	7514.990837	26.085517
199.013709	7536.876868	26.090535
199.184984	7524.642423	26.095552
199.757880	7524.190533	26.100570
199.734776	7529.930368	26.105588
199.732165	7518.190527	26.110605
199.485006	7549.506326	26.115623
199.675781	7554.507591	26.120640
199.935501	7559.150414	26.125658
199.825591	7570.597673	26.130676
200.271300	7581.955208	26.135693
200.417338	7588.161587	26.140711
200.648585	7604.333033	26.145728
201.261196	7610.134872	26.150746
201.003673	7619.150363	26.155764
201.309591	7613.353411	26.160781
201.456252	7632.349421	26.165799
201.723674	7642.889115	26.170816
202.030994	7642.476446	26.175834
202.004897	7642.691290	26.180852
202.333228	7655.150632	26.185869
202.182079	7673.034965	26.190887
202.503598	7672.344922	26.195904
202.469096	7674.916698	26.200922
202.735750	7699.236584	26.205940
203.372686	7698.531861	26.210957
203.272072	7707.387367	26.215975
203.384114	7723.114571	26.220992
203.933321	7731.273368	26.226010
203.692503	7750.417083	26.231028
203.854049	7749.736340	26.236045
204.027972	7758.884352	26.241063
204.671396	7774.064384	26.246080
204.727240	7780.735341	26.251098
205.166873	7791.737985	26.256116
205.440608	7802.621757	26.261133
205.376548	7812.135166	26.266151
205.775564	7820.334723	26.271168
205.732015	7831.503728	26.276186
206.382420	7854.477109	26.281204
206.394640	7844.696105	26.286221
206.733630	7863.692508	26.291239
206.717135	7867.242037	26.296256
207.305300	7881.216070	26.301274
207.191145	7885.995556	26.306292
207.243508	7883.412868	26.311309
207.481391	7897.688027	26.316327
207.625766	7912.809571	26.321344
207.903841	7909.939242	26.326362
207.724587	7929.364102	26.331380
208.129557	7940.687124	26.336397
208.151200	7955.748603	26.341415
208.157295	7973.929315	26.346432
208.865917	7985.673787	26.351450
208.779951	8011.451371	26.356468
208.909631	8007.324702	26.361485
209.459646	8029.776684	26.366503
209.847114	8036.486225	26.371520
210.128175	8033.248245	26.376538
209.861804	8058.363559	26.381556
210.401259	8063.765293	26.386573
210.934138	8077.697768	26.391591
210.889566	8091.532288	26.396608
210.853356	8098.924247	26.401626
211.095602	8107.235909	26.406644
211.557275	8126.066635	26.411661
211.671357	8136.476954	26.416679
211.784776	8135.116686	26.421696
212.395557	8149.662968	26.426714
212.105677	8171.908546	26.431732
212.325046	8167.939781	26.436749
212.690887	8190.503129	26.441767
212.250417	8197.408234	26.446784
212.748411	8206.400897	26.451802
213.080584	8227.922274	26.456820
213.326492	8228.934250	26.461837
213.236824	8239.719111	26.466855
213.602931	8243.837331	26.471872
214.401622	8253.120389	26.476890
214.677912	8264.787128	26.481908
214.826476	8259.042919	26.486925
215.128874	8252.709839	26.491943
215.418072	8255.360936	26.496960
215.479847	8259.119300	26.501978
216.223451	8270.761873	26.506996
216.377968	8278.036136	26.512013
216.423381	8281.995052	26.517031
216.515162	8283.085449	26.522048
216.563605	8274.949244	26.527066
216.840642	8276.227685	26.532084
217.164534	8275.816889	26.537101
216.970290	8273.868851	26.542119
217.207216	8297.759077	26.547136
217.431550	8299.531064	26.552154
217.605571	8306.475839	26.557172
217.854357	8307.768580	26.562189
218.080425	8318.092067	26.567207
218.379691	8327.531683	26.572224
218.740838	8323.533850	26.577242
218.586424	8350.656705	26.582260
218.873956	8356.798160	26.587277
218.945103	8351.148334	26.592295
219.183751	8374.510538	26.597312
219.335772	8380.460155	26.602330
219.789411	8401.599333	26.607348
220.015141	8416.750736	26.612365
220.080703	8423.557377	26.617383
220.239102	8435.972401	26.622400
220.386880	8441.964524	26.627418
220.445531	8461.797518	26.632436
220.845137	8476.184916	26.637453
220.987471	8487.871630	26.642471
221.188853	8500.633860	26.647488
221.752630	8508.681839	26.652506
221.794843	8524.677843	26.657524
222.306882	8542.775622	26.662541
222.528227	8541.741102	26.667559
222.517316	8547.046690	26.672576
223.226414	8556.086875	26.677594
223.135385	8563.018108	26.682612
223.285346	8565.388234	26.687629
223.588856	8580.547730	26.692647
223.635026	8603.803027	26.697664
224.069817	8604.974095	26.702682
224.343835	8612.442316	26.707700
225.139320	8612.448586	26.712717
225.427688	8609.994712	26.717735
225.320917	8604.685702	26.722752
225.818012	8606.477934	26.727770
225.935577	8609.389348	26.732788
225.727919	8601.401660	26.737805
226.247537	8600.049721	26.742823
226.055848	8606.828843	26.747840
226.361672	8599.167538	26.752858
226.347760	8615.727890	26.757876
226.518451	8621.505012	26.762893
226.539872	8627.645705	26.767911
227.163311	8632.038203	26.772928
227.800926	8637.152294	26.777946
227.855597	8633.636292	26.782964
227.901328	8643.347239	26.787981
228.149327	8641.223294	26.792999
227.986168	8654.116676	26.798016
228.460778	8670.345962	26.803034
228.383895	8675.482486	26.808052
228.535678	8696.177457	26.813069
229.093522	8701.436025	26.818087
229.270333	8719.025010	26.823104
229.585365	8730.158383	26.828122
229.418186	8744.989040	26.833140
229.653624	8756.789984	26.838157
230.326189	8757.990425	26.843175
230.131746	8766.540368	26.848192
230.324160	8776.938462	26.853210
230.311745	8800.013427	26.858228
230.719436	8819.113423	26.863245
230.727338	8829.929224	26.868263
231.017841	8857.632153	26.873280
231.069846	8868.697259	26.878298
231.292428	8883.532139	26.883316
231.510221	8910.414078	26.888333
232.067485	8921.997681	26.893351
232.280321	8947.927233	26.898368
232.622661	8954.904101	26.903386
232.934100	8986.024517	26.908404
233.164316	8994.566392	26.913421
233.479736	9009.595044	26.918439
233.276068	9024.610267	26.923456
233.718930	9038.183203	26.928474
234.145934	9054.864602	26.933492
234.361720	9071.857974	26.938509
234.931176	9081.591287	26.943527
234.836799	9100.613805	26.948544
235.593079	9118.575036	26.953562
235.354999	9123.762181	26.958580
235.328242	9139.182085	26.963597
236.118812	9146.874793	26.968615
236.300729	9157.218207	26.973632
236.434561	9158.331394	26.978650
236.602299	9178.979342	26.983668
236.809962	9187.205312	26.988685
236.885316	9199.787219	26.993703
236.928567	9219.648209	26.998720
237.213536	9227.325200	27.003738
237.347720	9245.793446	27.008756
237.817736	9253.854724	27.013773
238.061165	9268.738385	27.018791
238.246097	9281.703385	27.023808
238.468188	9281.006688	27.028826
238.443954	9300.269535	27.033844
238.770682	9304.409752	27.038861
239.178831	9325.084433	27.043879
239.341001	9345.230887	27.048896
239.665166	9361.720658	27.053914
239.953701	9372.466657	27.058932
239.968259	9382.142423	27.063949
240.647159	9393.770123	27.068967
240.729301	9414.277045	27.073984
240.839481	9421.367972	27.079002
241.391966	9432.892885	27.084020
241.650894	9452.888948	27.089037
241.877308	9454.433801	27.094055
241.793029	9463.100742	27.099072
242.447149	9483.378919	27.104090
242.499452	9494.638221	27.109108
242.741021	9494.462904	27.114125
242.777101	9510.976997	27.119143
242.761662	9529.690245	27.124160
243.433007	9544.158870	27.129178
243.701229	9547.363722	27.134196
243.810266	9572.319338	27.139213
244.697372	9580.098135	27.144231
244.654009	9585.702718	27.149248
245.186753	9584.993730	27.154266
245.313856	9601.744436	27.159284
244.886679	9616.009060	27.164301
245.719544	9630.757352	27.169319
245.577897	9632.912104	27.174336
245.580368	9647.167714	27.179354
246.133245	9666.587348	27.184372
246.183481	9680.661466	27.189389
246.390735	9700.863666	27.194407
246.678642	9708.746811	27.199424
246.572028	9730.488806	27.204442
246.879082	9742.262439	27.209460
247.004105	9763.444766	27.214477
247.682426	9772.639831	27.219495
247.921858	9799.352508	27.224512
247.882639	9802.988298	27.229530
248.521602	9820.395264	27.234548
248.566784	9839.730370	27.239565
249.124449	9857.981753	27.244583
248.926067	9874.862595	27.249600
249.313077	9885.601512	27.254618
249.436376	9901.251699	27.259636
249.803439	9923.049854	27.264653
250.351114	9931.367623	27.269671
250.503503	9955.969725	27.274688
250.991270	9949.010924	27.279706
251.647402	9961.504903	27.284724
251.137649	9965.421511	27.289741
251.286179	9984.373489	27.294759
251.374611	9992.642369	27.299776
251.693932	10016.349255	27.304794
252.337518	10018.468737	27.309812
252.597179	10034.666122	27.314829
253.252316	10042.768553	27.319847
253.119898	10052.652707	27.324864
253.303856	10054.341991	27.329882
253.988627	10065.145024	27.334900
254.021930	10073.253208	27.339917
254.232227	10075.286235	27.344935
254.558648	10081.215255	27.349952
254.522570	10094.943666	27.354970
255.085494	10094.714838	27.359988
254.869813	10117.193043	27.365005
255.563336	10117.140381	27.370023
255.518463	10128.700427	27.375040
255.672951	10148.053409	27.380058
256.206976	10158.077099	27.385076
256.226713	10166.936171	27.390093
256.666508	10187.006144	27.395111
256.688206	10201.039906	27.400128
257.103016	10219.837785	27.405146
257.035954	10223.171156	27.410164
257.367825	10244.490421	27.415181
257.973089	10248.803757	27.420199
257.995242	10259.753592	27.425216
257.762553	10277.170211	27.430234
258.762908	10294.438528	27.435252
258.377812	10318.203566	27.440269
259.048461	10325.677876	27.445287
259.161447	10353.612353	27.450304
259.169900	10375.576592	27.455322
259.626975	10386.407840	27.460340
259.709772	10413.764532	27.465357
260.330396	10425.806388	27.470375
260.794535	10445.426545	27.475392
260.561175	10451.555659	27.480410
260.959862	10472.115243	27.485428
260.959098	10491.273050	27.490445
262.036023	10504.363487	27.495463
261.930850	10520.554555	27.500480
262.072966	10542.691516	27.505498
262.612714	10543.115911	27.510516
262.458088	10564.594629	27.515533
263.132702	10580.302254	27.520551
263.097669	10592.604751	27.525568
263.395282	10615.695344	27.530586
263.756055	10618.320388	27.535604
264.010774	10636.922418	27.540621
264.499855	10647.359116	27.545639
264.488022	10662.524194	27.550656
264.670166	10678.481795	27.555674
264.834365	10677.065337	27.560692
264.982106	10714.641969	27.565709
265.507606	10716.542256	27.570727
265.819809	10729.354228	27.575744
265.764725	10751.909789	27.580762
266.365529	10763.187841	27.585780
266.616855	10771.922449	27.590797
267.042541	10768.210805	27.595815
267.211059	10792.359132	27.600832
267.411056	10798.363667	27.605850
268.248644	10787.759417	27.610868
268.140022	10816.519040	27.615885
268.732016	10820.872628	27.620903
268.903957	10820.351511	27.625920
268.367708	10834.943190	27.630938
269.036831	10850.541709	27.635956
269.262478	10864.646670	27.640973
269.825108	10883.147353	27.645991
269.880039	10894.432390	27.651008
269.785811	10918.153172	27.656026
270.541106	10914.690722	27.661044
270.439943	10935.661206	27.666061
270.538242	10952.796460	27.671079
270.848553	10966.732560	27.676096
270.896205	10993.678639	27.681114
271.692554	11009.803918	27.686132
271.623718	11028.595809	27.691149
272.322770	11036.084494	27.696167
272.767038	11037.623679	27.701184
272.823861	11055.467429	27.706202
273.483117	11060.326452	27.711220
273.553837	11076.442222	27.716237
273.700244	11087.620311	27.721255
274.149881	11098.601448	27.726272
274.340057	11117.582280	27.731290
274.824667	11120.142055	27.736308
274.797403	11123.705175	27.741325
274.850077	11144.482512	27.746343
275.825172	11154.815747	27.751360
275.746959	11171.678910	27.756378
276.037400	11183.946552	27.761396
276.041988	11204.262583	27.766413
276.398685	11215.341677	27.771431
276.822279	11236.241513	27.776448
276.772385	11243.901219	27.781466
277.349741	11256.583059	27.786484
277.235371	11265.451532	27.791501
277.736198	11283.867134	27.796519
278.254609	11295.292061	27.801536
278.112557	11322.460312	27.806554
278.503886	11323.405017	27.811572
278.506145	11355.875247	27.816589
278.651291	11367.852745	27.821607
279.116963	11377.562692	27.826624
279.075184	11394.331587	27.831642
279.246744	11420.760713	27.836660
279.496480	11440.560659	27.841677
279.744313	11456.055467	27.846695
280.200922	11483.334125	27.851712
280.528196	11507.059161	27.856730
280.753170	11524.605115	27.861748
281.407033	11549.342731	27.866765
281.459721	11571.220627	27.871783
281.710034	11573.059447	27.876800
282.068256	11594.946467	27.881818
282.631161	11620.605960	27.886836
282.894297	11631.134029	27.891853
283.466932	11643.653082	27.896871
284.167844	11654.150256	27.901888
284.049324	11659.555680	27.906906
284.416078	11668.682314	27.911924
284.695042	11682.707928	27.916941
285.086867	11684.202584	27.921959
285.166055	11682.865228	27.926976
285.466597	11711.165455	27.931994
285.615618	11711.210862	27.937012
285.675497	11729.384203	27.942029
285.805734	11738.081776	27.947047
286.342149	11748.465369	27.952064
286.237129	11763.286546	27.957082
286.577343	11788.191756	27.962100
286.868568	11803.614843	27.967117
287.386043	11827.044556	27.972135
287.542365	11835.361049	27.977152
288.072440	11865.741901	27.982170
288.445808	11868.376025	27.987188
288.296286	11891.833476	27.992205
288.613765	11911.094427	27.997223
288.913957	11920.924472	28.002240
289.136833	11958.919763	28.007258
289.738565	11976.429994	28.012276
289.709498	11997.578603	28.017293
289.762694	12020.768244	28.022311
290.278824	12038.422447	28.027328
290.218462	12058.901969	28.032346
290.560958	12086.593622	28.037364
291.061905	12111.281078	28.042381
291.401796	12132.536830	28.047399
292.004509	12153.206989	28.052416
291.757216	12175.428672	28.057434
292.526874	12201.794371	28.062452
292.850108	12217.461374	28.067469
292.979286	12236.398802	28.072487
293.549529	12259.944599	28.077504
293.470697	12274.219595	28.082522
294.143274	12290.651052	28.087540
294.429921	12305.203854	28.092557
295.029346	12318.410714	28.097575
295.378866	12320.138056	28.102592
295.360296	12329.375235	28.107610
295.826258	12341.112487	28.112628
296.147431	12350.965988	28.117645
296.160610	12365.137035	28.122663
296.371244	12380.000804	28.127680
296.735814	12386.407977	28.132698
297.079269	12395.412930	28.137716
297.535262	12414.753177	28.142733
297.518560	12426.751312	28.147751
298.046847	12443.916874	28.152768
298.107829	12454.995491	28.157786
298.685126	12464.685382	28.162804
299.167432	12471.644514	28.167821
299.361886	12478.757005	28.172839
299.760502	12485.191479	28.177856
299.906785	12493.079768	28.182874
300.353240	12511.706239	28.187892
300.856962	12526.324476	28.192909
300.984173	12526.045807	28.197927
301.178315	12533.473585	28.202944
301.380035	12551.948196	28.207962
301.952695	12551.905235	28.212980
302.455734	12571.079998	28.217997
302.085740	12589.710956	28.223015
302.829406	12590.029548	28.228032
302.616717	12612.360943	28.233050
303.116091	12617.599309	28.238068
303.491041	12630.829138	28.243085
303.022633	12649.188612	28.248103
303.850696	12676.131365	28.253120
303.517261	12691.928712	28.258138
304.098986	12712.831709	28.263156
304.775029	12743.567432	28.268173
305.063553	12767.447517	28.273191
305.034448	12778.265981	28.278208
305.476724	12800.051951	28.283226
305.747024	12816.875986	28.288244
306.001242	12844.166392	28.293261
305.928421	12871.694147	28.298279
306.698155	12888.940153	28.303296
306.945400	12913.856710	28.308314
307.274893	12927.433430	28.313332
307.933761	12942.832406	28.318349
308.317288	12965.610570	28.323367
308.594702	12968.946924	28.328384
309.437349	12988.694407	28.333402
309.462044	12997.082912	28.338420
310.021150	13002.441981	28.343437
309.887527	13004.819602	28.348455
310.047392	13018.184328	28.353472
310.511155	13036.193753	28.358490
310.567210	13052.668607	28.363508
311.147207	13057.533946	28.368525
311.327831	13080.350200	28.373543
312.084738	13083.356945	28.378560
312.321937	13093.630348	28.383578
312.312462	13102.986187	28.388596
312.324855	13121.867427	28.393613
312.442359	13138.546186	28.398631
312.728299	13151.503265	28.403648
313.188073	13174.768280	28.408666
313.088779	13201.180508	28.413684
313.983315	13215.360415	28.418701
313.649802	13238.914370	28.423719
313.876689	13258.105749	28.428736
313.990099	13286.741815	28.433754
314.494517	13314.109905	28.438772
314.917682	13337.728173	28.443789
314.985435	13362.844822	28.448807
315.524199	13383.234340	28.453824
315.747320	13413.888186	28.458842
316.034701	13441.605763	28.463860
316.894330	13460.287013	28.468877
317.341518	13478.354931	28.473895
317.810867	13489.049025	28.478912
318.401642	13513.573471	28.483930
318.514949	13517.286393	28.488948
318.623102	13528.806851	28.493965
318.998738	13558.946223	28.498983
319.314057	13577.738238	28.504000
319.834282	13591.725716	28.509018
319.940678	13621.090172	28.514036
320.119834	13620.741113	28.519053
320.447513	13645.733260	28.524071
321.546965	13647.649021	28.529088
322.044707	13665.033884	28.534106
322.517867	13675.407487	28.539124
322.759901	13663.678809	28.544141
322.643611	13693.626913	28.549159
323.172781	13700.948940	28.554176
323.062214	13715.673528	28.559194
323.168770	13735.210778	28.564212
323.770651	13748.371094	28.569229
323.678149	13773.591493	28.574247
324.251017	13785.335106	28.579264
323.876002	13805.111019	28.584282
324.439239	13825.534722	28.589300
324.720177	13843.705617	28.594317
324.538398	13877.645125	28.599335
324.745632	13897.556205	28.604352
325.233659	13942.460031	28.609370
325.431010	13968.718616	28.614388
326.033751	13997.525816	28.619405
326.105466	14029.590655	28.624423
326.734795	14062.696422	28.629440
326.960758	14086.831883	28.634458
327.085873	14116.603824	28.639476
328.081854	14150.884247	28.644493
328.164126	14168.872034	28.649511
328.777683	14177.631499	28.654528
329.351984	14203.209554	28.659546
329.576672	14220.813613	28.664564
330.252735	14234.105041	28.669581
330.408240	14246.916686	28.674599
331.318079	14232.300586	28.679616
332.612792	14235.527468	28.684634
332.555342	14241.191226	28.689652
332.835343	14229.963181	28.694669
332.827826	14231.876447	28.699687
333.452527	14234.162101	28.704704
333.790030	14228.492966	28.709722
334.157246	14229.418345	28.714740
334.308217	14228.971651	28.719757
334.255485	14227.804865	28.724775
334.327398	14236.885747	28.729792
334.381806	14256.509788	28.734810
334.485097	14263.109072	28.739828
334.813131	14278.181415	28.744845
334.712942	14298.903831	28.749863
334.955232	14324.045622	28.754880
335.454821	14349.720252	28.759898
335.496723	14383.179542	28.764916
335.603983	14405.499509	28.769933
336.046832	14441.245086	28.774951
336.183794	14470.336279	28.779968
336.933006	14505.148370	28.784986
337.112232	14535.241227	28.790004
337.518821	14566.007634	28.795021
337.688692	14596.534098	28.800039
338.717538	14629.216300	28.805056
338.695063	14649.159777	28.810074
339.216725	14678.960920	28.815092
339.666038	14698.375938	28.820109
340.115048	14720.488013	28.825127
340.449358	14734.059098	28.830144
340.845714	14757.491696	28.835162
340.892673	14785.369383	28.840180
341.699569	14806.643136	28.845197
341.888715	14825.229642	28.850215
342.592189	14837.336236	28.855232
343.399601	14850.648213	28.860250
343.300660	14859.404059	28.865268
343.483505	14876.995498	28.870285
344.106267	14886.754703	28.875303
344.240476	14910.760501	28.880320
344.500041	14925.570898	28.885338
344.713872	14943.037300	28.890356
346.320257	14919.091012	28.895373
346.679431	14930.804294	28.900391
346.823873	14925.726015	28.905408
347.277457	14935.184802	28.910426
347.025715	14957.957962	28.915444
347.416733	14960.576962	28.920461
347.469726	14981.554557	28.925479
347.703090	14990.846202	28.930496
348.010087	15002.994075	28.935514
348.294284	15027.157185	28.940532
348.304037	15033.426025	28.945549
348.246334	15061.678357	28.950567
348.747523	15077.320746	28.955584
348.857270	15097.644056	28.960602
349.157903	15139.096490	28.965620
349.550314	15161.986516	28.970637
349.723280	15189.920527	28.975655
350.187343	15210.842145	28.980672
350.504018	15248.288284	28.985690
350.610175	15271.336287	28.990708
351.179306	15301.508733	28.995725
351.582801	15340.053078	29.000743
351.674480	15359.631054	29.005760
352.702456	15381.617990	29.010778
353.213859	15412.968589	29.015796
353.303395	15435.953463	29.020813
353.782558	15466.773738	29.025831
354.036878	15479.966640	29.030848
354.784380	15497.037929	29.035866
355.019257	15527.066304	29.040884
355.651442	15538.916082	29.045901
355.956442	15552.994139	29.050919
356.556154	15579.209969	29.055936
356.784912	15583.195195	29.060954
356.895091	15610.065609	29.065972
357.400977	15629.339615	29.070989
357.841819	15645.522537	29.076007
357.969846	15663.571891	29.081024
358.421796	15680.028805	29.086042
358.304741	15705.030932	29.091060
359.121001	15729.824273	29.096077
359.193060	15750.208437	29.101095
359.370175	15773.791973	29.106112
359.799473	15795.328765	29.111130
359.946072	15823.597821	29.116148
360.570352	15841.858673	29.121165
361.049999	15864.307524	29.126183
361.231703	15901.078360	29.131200
361.576191	15911.120748	29.136218
362.377242	15945.398906	29.141236
362.570848	15970.531049	29.146253
362.758705	15990.471616	29.151271
362.811835	16020.199414	29.156288
363.110258	16050.017642	29.161306
363.419480	16082.493442	29.166324
363.162519	16111.062304	29.171341
363.786092	16145.916725	29.176359
364.123067	16185.729244	29.181376
364.787280	16209.198388	29.186394
365.574314	16255.630496	29.191412
366.082190	16275.924847	29.196429
366.451709	16295.844105	29.201447
366.754911	16324.345703	29.206464
367.331931	16334.660625	29.211482
367.636322	16359.924128	29.216500
367.887729	16369.412084	29.221517
367.988003	16390.845243	29.226535
368.499240	16415.649324	29.231552
369.156550	16420.355822	29.236570
369.264048	16454.979326	29.241588
369.426928	16474.576363	29.246605
370.152143	16505.703212	29.251623
370.073825	16529.861277	29.256640
370.940736	16545.768698	29.261658
371.568244	16572.309233	29.266676
371.638581	16583.165161	29.271693
371.726530	16599.302298	29.276711
372.196962	16617.702300	29.281728
372.655950	16638.899317	29.286746
372.981417	16667.407145	29.291764
373.417545	16686.163074	29.296781
374.093003	16714.549520	29.301799
374.314590	16734.390610	29.306816
374.957681	16748.848417	29.311834
375.574326	16752.871494	29.316852
375.882803	16774.206407	29.321869
376.449005	16785.615948	29.326887
376.630884	16798.494410	29.331904
377.380624	16802.420597	29.336922
377.763337	16817.093345	29.341940
377.567354	16837.154310	29.346957
377.844888	16851.353258	29.351975
378.076408	16872.135535	29.356992
378.453609	16888.448813	29.362010
378.584287	16918.491251	29.367028
379.168064	16929.658257	29.372045
379.368750	16957.363474	29.377063
379.614297	16979.912283	29.382080
380.136168	17000.968137	29.387098
380.170792	17038.767752	29.392116
380.617621	17064.833989	29.397133
381.107856	17096.426290	29.402151
381.014087	17133.437811	29.407168
381.393244	17157.986597	29.412186
381.657408	17195.969513	29.417204
382.331269	17237.856654	29.422221
382.705896	17267.834263	29.427239
382.905739	17306.574140	29.432256
383.299865	17328.270290	29.437274
383.726733	17366.053870	29.442292
384.357129	17390.531563	29.447309
385.639186	17415.479344	29.452327
385.979940	17446.760552	29.457344
386.505047	17463.583485	29.462362
386.761707	17483.378465	29.467380
386.614618	17500.631941	29.472397
386.980575	17523.143506	29.477415
387.079234	17541.928280	29.482432
387.849887	17560.914792	29.487450
388.009330	17584.311580	29.492468
388.459154	17600.278884	29.497485
389.106001	17620.798577	29.502503
388.838795	17644.213389	29.507520
389.312100	17677.037812	29.512538
389.849668	17701.371064	29.517556
390.140353	17727.966436	29.522573
390.803874	17749.768314	29.527591
390.742053	17787.121065	29.532608
391.327091	17812.428534	29.537626
391.694386	17848.113985	29.542644
391.698252	17870.022765	29.547661
392.629042	17895.296329	29.552679
392.558508	17932.103829	29.557696
392.786147	17973.826497	29.562714
393.524319	18003.703707	29.567732
393.861914	18034.202997	29.572749
394.433742	18060.681347	29.577767
394.570941	18100.367127	29.582784
395.297114	18121.900194	29.587802
395.910174	18148.415760	29.592820
396.165871	18171.131553	29.597837
396.797706	18184.071133	29.602855
397.281216	18219.373266	29.607872
397.842855	18235.251069	29.612890
398.232333	18269.800046	29.617908
398.408475	18285.814909	29.622925
399.003993	18308.873106	29.627943
399.345847	18347.644655	29.632960
399.689818	18359.709816	29.637978
400.277876	18369.461268	29.642996
400.652655	18396.557262	29.648013
401.293766	18410.813473	29.653031
401.543149	18438.154904	29.658048
402.102300	18455.904781	29.663066
402.104168	18477.324368	29.668084
402.426643	18500.068577	29.673101
403.133479	18518.661927	29.678119
403.218139	18546.845299	29.683136
403.662283	18564.608695	29.688154
404.287395	18596.251661	29.693172
404.306156	18616.055641	29.698189
404.561480	18651.347337	29.703207
404.630093	18676.508121	29.708224
405.417111	18704.875681	29.713242
405.929184	18745.217684	29.718260
406.077561	18779.334460	29.723277
406.637043	18803.960391	29.728295
406.843648	18843.054247	29.733312
406.833752	18872.228737	29.738330
407.350630	18907.856119	29.743348
407.564252	18946.070814	29.748365
408.487544	18974.691391	29.753383
408.812886	19008.138178	29.758400
409.033990	19043.972626	29.763418
409.520893	19065.557374	29.768436
410.195328	19093.802985	29.773453
410.523737	19118.133146	29.778471
410.873430	19150.500749	29.783488
411.507133	19169.168846	29.788506
411.888962	19192.498228	29.793524
412.199966	19228.655072	29.798541
413.062826	19249.439315	29.803559
413.380122	19278.145343	29.808576
413.664168	19307.352199	29.813594
413.461050	19330.968068	29.818612
414.143443	19353.576069	29.823629
414.587206	19383.793152	29.828647
414.887063	19425.497582	29.833664
415.066524	19444.185492	29.838682
415.666336	19480.656024	29.843700
415.827658	19523.631614	29.848717
417.154920	19558.158122	29.853735
417.094643	19580.691883	29.858752
417.659268	19608.135707	29.863770
418.100306	19640.259972	29.868788
418.360164	19672.872598	29.873805
418.858916	19688.858738	29.878823
419.380876	19730.754484	29.883840
419.669886	19749.578478	29.888858
420.271988	19779.086409	29.893876
420.438378	19815.989862	29.898893
420.902731	19839.977690	29.903911
421.673163	19874.731144	29.908928
422.164469	19895.617704	29.913946
422.893267	19933.505105	29.918964
422.869942	19956.966471	29.923981
423.752242	19976.519993	29.928999
423.801341	20005.842428	29.934016
424.229846	20031.558490	29.939034
424.748415	20060.073679	29.944052
425.496994	20073.604924	29.949069
426.140726	20075.244845	29.954087
426.300126	20097.647042	29.959104
426.846144	20120.396126	29.964122
427.503273	20139.638385	29.969140
427.841739	20155.018574	29.974157
428.407055	20164.204182	29.979175
428.822626	20198.505089	29.984192
428.963683	20207.134293	29.989210
429.731586	20218.275105	29.994228
429.748814	20251.282049	29.999245
430.357661	20264.551997	30.004263
430.380224	20279.242196	30.009280
430.316066	20309.090712	30.014298
430.619148	20340.998704	30.019316
430.876860	20378.176285	30.024333
431.178875	20403.387942	30.029351
431.847591	20436.438126	30.034368
432.328638	20466.679141	30.039386
432.598784	20497.971813	30.044404
432.875938	20530.799151	30.049421
433.323060	20560.483227	30.054439
433.683744	20596.580872	30.059456
434.192626	20628.626009	30.064474
434.900427	20650.922343	30.069492
434.993268	20693.281910	30.074509
435.569256	20713.357099	30.079527
436.474040	20749.153685	30.084544
437.138536	20772.321702	30.089562
437.754780	20786.257793	30.094580
437.755970	20821.022027	30.099597
438.224964	20846.688240	30.104615
438.708503	20862.310697	30.109632
438.938466	20897.579892	30.114650
439.653403	20925.725445	30.119668
439.703978	20956.816911	30.124685
440.493848	20977.283086	30.129703
441.061310	21010.785377	30.134720
441.106378	21046.545429	30.139738
441.719855	21063.098225	30.144756
442.482189	21099.076072	30.149773
443.157514	21123.942570	30.154791
443.243452	21144.469658	30.159808
443.564913	21171.115647	30.164826
444.459980	21197.076785	30.169844
444.265541	21220.443069	30.174861
444.802571	21250.505587	30.179879
444.859204	21296.247368	30.184896
445.559309	21331.553585	30.189914
445.672184	21360.679781	30.194932
446.044293	21393.262288	30.199949
446.647171	21426.060768	30.204967
446.992359	21467.935913	30.209984
447.391743	21500.132343	30.215002
448.029250	21543.152866	30.220020
448.078476	21594.204562	30.225037
448.463951	21619.656027	30.230055
449.497542	21656.763368	30.235072
449.938755	21697.230208	30.240090
450.668109	21725.830347	30.245108
451.265268	21762.044481	30.250125
451.356113	21789.055802	30.255143
451.635309	21829.713145	30.260160
451.936860	21870.240598	30.265178
452.156265	21898.991494	30.270196
453.051383	21943.178389	30.275213
453.554351	21964.768818	30.280231
454.201152	22006.538406	30.285248
454.135264	22046.354965	30.290266
454.524500	22078.123720	30.295284
455.212478	22127.711373	30.300301
455.355144	22158.402894	30.305319
455.735277	22195.494080	30.310336
456.510739	22238.547911	30.315354
457.426544	22260.222511	30.320372
457.384410	22294.109338	30.325389
458.294683	22313.779050	30.330407
459.291847	22331.333367	30.335424
460.139198	22346.566837	30.340442
460.609981	22364.343858	30.345460
460.851054	22371.957219	30.350477
461.577620	22389.504351	30.355495
461.992824	22396.507556	30.360512
462.299833	22419.841588	30.365530
463.077483	22433.560564	30.370548
463.277301	22449.794510	30.375565
463.549629	22465.388405	30.380583
463.553575	22482.229970	30.385600
463.815280	22513.441059	30.390618
464.451073	22543.326505	30.395636
464.634390	22568.091768	30.400653
464.989217	22601.179452	30.405671
465.469410	22632.706566	30.410688
465.909420	22667.706877	30.415706
466.659793	22699.272972	30.420724
467.745093	22718.017421	30.425741
468.202256	22740.152866	30.430759
468.661161	22756.449942	30.435776
469.158899	22772.125344	30.440794
470.265582	22788.242057	30.445812
470.599967	22802.425237	30.450829
470.849268	22827.819837	30.455847
471.432810	22843.997863	30.460864
471.555592	22862.140980	30.465882
471.849504	22874.959147	30.470900
471.755246	22907.058313	30.475917
472.094860	22939.070573	30.480935
472.881522	22975.828850	30.485952
473.460437	23003.346686	30.490970
473.530177	23030.210611	30.495988
474.065192	23070.191520	30.501005
473.745820	23104.162151	30.506023
474.722523	23143.742673	30.511040
474.774167	23193.388843	30.516058
475.323080	23232.629689	30.521076
475.437619	23287.097451	30.526093
475.812031	23324.292997	30.531111
476.398368	23373.046912	30.536128
476.825389	23418.018058	30.541146
477.620808	23463.774661	30.546164
478.411117	23505.763037	30.551181
478.637413	23553.718076	30.556199
479.353040	23591.637965	30.561216
479.440896	23635.680542	30.566234
480.169307	23670.068880	30.571252
480.741915	23716.299615	30.576269
481.253332	23752.248781	30.581287
481.899250	23781.771923	30.586304
482.368089	23816.984126	30.591322
483.068395	23846.154249	30.596340
483.540450	23873.780112	30.601357
484.145090	23901.884823	30.606375
484.771866	23927.320455	30.611392
484.804849	23959.986467	30.616410
485.413972	23985.463061	30.621428
486.184062	24011.281157	30.626445
486.525412	24038.153736	30.631463
487.249109	24061.819191	30.636480
487.610564	24102.535646	30.641498
487.925631	24128.289948	30.646516
488.096619	24166.020549	30.651533
488.561765	24202.218311	30.656551
489.566251	24227.028200	30.661568
489.814096	24274.987863	30.666586
490.300367	24301.577366	30.671604
490.754416	24341.161893	30.676621
491.248857	24381.607027	30.681639
491.131231	24408.312795	30.686656
491.401631	24454.729781	30.691674
492.302122	24494.143527	30.696692
492.381656	24546.331215	30.701709
492.673049	24593.413698	30.706727
493.604262	24634.595252	30.711744
493.485090	24689.870850	30.716762
494.420105	24731.216010	30.721780
495.429735	24779.478687	30.726797
496.104212	24807.563448	30.731815
496.863179	24838.955364	30.736832
497.199054	24872.558528	30.741850
498.198965	24900.382638	30.746868
498.719880	24945.698132	30.751885
499.040384	24973.645090	30.756903
499.716815	24996.872004	30.761920
500.101665	25026.978272	30.766938
500.597872	25059.033885	30.771956
500.995441	25091.466068	30.776973
501.208199	25130.554339	30.781991
501.961164	25166.758431	30.787008
502.322118	25210.206195	30.792026
502.528774	25248.945633	30.797044
503.121439	25288.262528	30.802061
503.449487	25322.707000	30.807079
503.895241	25361.001943	30.812096
504.485596	25405.426636	30.817114
505.066176	25438.272894	30.822132
505.799015	25472.686157	30.827149
506.242895	25514.470660	30.832167
506.748190	25552.620179	30.837184
506.989019	25598.777164	30.842202
507.530390	25636.497977	30.847220
507.823548	25681.109949	30.852237
508.253013	25718.670307	30.857255
508.514906	25757.549679	30.862272
508.717998	25815.458181	30.867290
509.563646	25859.253540	30.872308
509.656441	25897.764723	30.877325
509.912607	25943.405796	30.882343
510.536840	25993.160628	30.887360
510.879153	26053.525593	30.892378
511.437574	26110.383637	30.897396
512.076958	26154.789229	30.902413
512.573564	26216.371250	30.907431
513.350505	26254.721828	30.912448
513.904735	26312.663300	30.917466
514.814642	26359.597274	30.922484
515.733801	26396.201339	30.927501
516.089368	26450.259190	30.932519
517.136712	26476.938869	30.937536
517.436445	26511.138174	30.942554
517.914120	26548.799325	30.947572
518.243802	26580.176473	30.952589
518.885880	26623.260973	30.957607
519.328977	26655.890179	30.962624
519.682565	26707.040501	30.967642
520.434966	26743.430958	30.972660
521.032361	26783.362450	30.977677
521.336630	26820.618545	30.982695
522.093389	26861.456720	30.987712
522.571856	26901.938865	30.992730
523.601958	26929.849406	30.997748
524.189464	26958.384764	31.002765
524.991047	26981.879984	31.007783
525.957367	27004.066161	31.012800
526.191557	27029.933278	31.017818
526.494293	27057.848777	31.022836
527.051168	27074.098450	31.027853
527.353351	27115.494644	31.032871
527.847353	27144.781403	31.037888
528.347410	27177.373433	31.042906
528.609494	27210.416429	31.047924
528.873275	27251.128616	31.052941
529.245764	27296.551390	31.057959
529.786477	27331.064354	31.062976
530.050048	27382.336189	31.067994
530.109123	27421.566359	31.073012
531.040226	27463.880946	31.078029
531.394468	27523.040633	31.083047
532.132361	27575.257098	31.088064
532.634614	27632.539868	31.093082
533.538393	27670.840283	31.098100
534.168830	27720.138366	31.103117
534.504038	27764.631729	31.108135
535.347910	27792.285312	31.113152
535.587662	27837.104400	31.118170
536.009749	27885.318641	31.123188
536.644542	27921.151197	31.128205
536.795481	27972.866823	31.133223
537.669972	28009.021309	31.138240
538.146267	28049.026926	31.143258
538.418996	28090.925805	31.148276
539.120002	28125.163626	31.153293
539.360386	28182.635039	31.158311
540.309449	28218.777180	31.163328
540.463906	28271.729850	31.168346
540.678549	28317.327447	31.173364
541.286561	28365.605802	31.178381
541.862111	28417.634897	31.183399
542.134285	28463.424938	31.188416
542.733327	28506.584556	31.193434
543.380268	28565.650279	31.198452
544.179397	28617.487057	31.203469
544.611653	28668.247861	31.208487
545.229894	28713.212568	31.213504
546.030836	28780.395951	31.218522
546.315451	28815.665622	31.223540
547.929420	28850.833791	31.228557
548.437906	28886.592152	31.233575
548.950591	28933.430728	31.238592
549.740573	28969.888795	31.243610
550.297703	29005.392962	31.248628
550.753370	29041.829582	31.253645
551.209560	29077.796069	31.258663
552.373162	29100.512735	31.263680
552.936602	29138.309900	31.268698
553.266182	29161.633362	31.273716
553.839631	29191.951141	31.278733
554.309362	29221.494791	31.283751
554.947238	29246.365225	31.288768
555.443459	29283.618905	31.293786
555.755164	29326.353333	31.298804
556.108248	29355.835159	31.303821
556.528066	29399.251698	31.308839
557.053840	29429.177341	31.313856
557.441657	29471.482589	31.318874
557.847365	29517.082106	31.323892
558.386490	29564.867560	31.328909
558.787963	29617.368610	31.333927
559.517526	29669.277202	31.338944
559.845540	29723.476070	31.343962
560.172699	29764.890002	31.348980
561.427271	29817.242318	31.353997
561.637997	29866.580470	31.359015
562.866438	29898.377514	31.364032
563.303708	29943.221758	31.369050
564.154316	29990.017862	31.374068
564.510654	30033.159700	31.379085
564.859261	30061.772598	31.384103
565.182798	30098.129913	31.389120
565.984796	30146.585009	31.394138
566.408623	30192.927830	31.399156
566.653275	30244.801294	31.404173
567.361044	30291.221936	31.409191
567.978246	30331.492579	31.414208
568.282437	30384.050436	31.419226
568.905104	30423.888062	31.424244
569.466251	30453.727341	31.429261
570.052966	30504.037821	31.434279
571.044801	30543.335994	31.439296
571.830834	30583.379490	31.444314
572.286311	30622.438418	31.449332
573.286259	30648.504660	31.454349
573.577964	30688.472165	31.459367
574.157949	30716.677288	31.464384
574.490915	30748.219088	31.469402
574.825318	30799.028024	31.474420
575.743376	30841.974611	31.479437
575.752673	30877.607962	31.484455
576.391712	30929.169725	31.489472
576.869006	30972.479298	31.494490
576.802602	31031.274740	31.499508
577.525132	31078.442772	31.504525
578.206218	31141.360997	31.509543
578.777027	31190.537000	31.514560
579.632347	31244.400879	31.519578
580.130859	31297.344675	31.524596
581.088219	31336.959762	31.529613
581.681236	31387.871226	31.534631
582.205462	31443.793076	31.539648
582.957132	31490.054709	31.544666
583.455627	31543.201198	31.549684
584.477062	31573.623018	31.554701
584.973568	31625.627762	31.559719
585.551461	31667.788923	31.564736
586.195105	31710.992902	31.569754
586.708856	31763.604131	31.574772
587.482588	31802.396538	31.579789
587.626345	31843.155652	31.584807
588.131820	31890.230489	31.589824
588.673366	31944.588886	31.594842
588.837169	31986.184302	31.599860
589.898008	32038.895104	31.604877
590.460585	32089.564487	31.609895
591.168393	32136.245556	31.614912
592.328649	32175.023041	31.619930
592.692981	32223.116991	31.624948
593.640932	32266.377471	31.629965
594.019967	32307.242495	31.634983
594.508882	32347.429234	31.640000
595.767129	32385.814856	31.645018
595.533116	32429.041560	31.650036
596.699574	32463.750833	31.655053
597.212683	32513.707224	31.660071
597.313116	32556.744391	31.665088
597.974964	32597.246044	31.670106
598.736514	32642.574861	31.675124
598.757713	32684.988439	31.680141
599.397511	32739.862597	31.685159
599.524198	32784.416917	31.690176
600.349021	32827.677763	31.695194
600.754440	32876.287140	31.700212
601.961231	32924.525814	31.705229
602.003739	32973.708881	31.710247
602.422060	33024.222588	31.715264
603.419634	33076.092051	31.720282
603.521918	33118.732608	31.725300
604.382011	33178.370466	31.730317
604.657474	33231.351895	31.735335
605.517472	33293.543280	31.740352
606.363600	33333.541637	31.745370
607.418231	33373.264509	31.750388
609.433690	33387.158789	31.755405
610.105037	33417.025180	31.760423
610.289883	33444.380788	31.765440
611.240363	33470.841522	31.770458
611.703187	33503.262229	31.775476
612.362689	33532.042038	31.780493
612.742814	33562.520327	31.785511
612.870259	33598.741640	31.790528
613.643976	33624.942538	31.795546
614.033563	33671.180332	31.800564
614.636170	33713.029638	31.805581
614.695635	33760.858033	31.810599
614.981402	33810.421458	31.815616
615.805984	33849.525196	31.820634
616.460682	33910.418899	31.825652
616.809967	33963.790653	31.830669
616.988429	34021.158977	31.835687
617.970471	34078.771689	31.840704
618.698815	34120.613024	31.845722
619.145702	34184.898151	31.850740
619.704429	34236.596826	31.855757
620.353382	34295.015289	31.860775
620.696464	34361.960480	31.865792
621.242511	34412.071154	31.870810
621.629951	34486.243014	31.875828
622.272160	34558.253761	31.880845
622.985207	34624.423250	31.885863
623.409105	34691.863955	31.890880
624.193267	34756.901308	31.895898
624.735230	34833.068065	31.900916
625.015652	34890.920356	31.905933
625.810670	34961.770297	31.910951
626.405684	35038.244448	31.915968
627.354883	35096.083813	31.920986
627.818022	35173.720529	31.926004
628.954005	35233.665110	31.931021
629.619958	35297.919814	31.936039
630.667202	35362.191484	31.941056
632.070422	35404.816552	31.946074
632.416713	35462.299565	31.951092
633.351482	35500.273832	31.956109
633.763415	35545.868707	31.961127
634.351700	35585.038786	31.966144
634.784739	35621.549516	31.971162
634.909534	35671.903134	31.976180
635.764485	35722.939820	31.981197
636.281437	35770.467883	31.986215
636.867175	35819.275236	31.991232
637.646982	35863.157107	31.996250
638.267430	35922.775653	32.001268
638.605898	35969.719324	32.006285
639.423312	36019.709043	32.011303
639.581211	36079.943937	32.016320
640.450507	36129.454766	32.021338
641.095631	36189.322471	32.026356
641.620318	36253.655261	32.031373
642.119266	36311.682961	32.036391
642.629865	36369.509993	32.041408
643.519533	36418.917113	32.046426
643.995265	36488.116910	32.051444
644.632265	36547.188596	32.056461
645.424392	36603.999099	32.061479
645.932030	36668.891817	32.066496
647.327958	36717.641687	32.071514
647.765254	36777.054513	32.076532
648.912650	36839.451903	32.081549
649.592007	36883.527053	32.086567
650.276787	36938.279986	32.091584
650.890389	36976.807945	32.096602
651.268823	37026.159097	32.101620
651.887425	37082.732512	32.106637
652.635881	37135.802143	32.111655
653.054766	37196.876694	32.116672
653.787944	37250.369102	32.121690
654.760959	37308.233523	32.126708
655.062861	37359.723087	32.131725
655.917888	37405.685472	32.136743
656.307731	37466.907947	32.141760
657.306697	37516.536065	32.146778
657.947468	37583.104340	32.151796
658.533905	37635.777030	32.156813
658.959458	37694.939157	32.161831
659.470426	37770.223848	32.166848
660.183465	37809.604616	32.171866
660.629430	37872.589739	32.176884
661.435281	37947.635235	32.181901
661.938641	37992.030470	32.186919
662.537116	38061.871788	32.191936
663.233940	38122.478801	32.196954
664.002537	38188.503352	32.201972
664.616926	38246.413235	32.206989
665.309123	38304.439400	32.212007
665.778829	38379.989356	32.217024
667.017409	38434.759215	32.222042
667.541281	38498.538121	32.227060
668.328230	38556.643553	32.232077
669.478833	38608.000687	32.237095
669.841872	38665.696091	32.242112
670.584240	38702.500922	32.247130
671.203036	38754.571474	32.252148
671.609264	38803.038719	32.257165
672.159518	38849.767232	32.262183
672.698627	38913.863810	32.267200
673.057724	38964.255784	32.272218
673.828677	39033.989162	32.277236
674.546562	39090.302358	32.282253
674.734479	39157.477961	32.287271
675.104631	39220.910025	32.292288
676.038810	39288.015079	32.297306
676.622497	39350.081927	32.302324
677.251741	39422.227712	32.307341
678.031284	39492.747437	32.312359
678.846752	39555.119377	32.317376
679.845773	39629.535643	32.322394
680.608129	39691.689838	32.327412
681.265583	39760.829784	32.332429
682.041508	39829.015207	32.337447
682.171445	39889.740929	32.342464
683.146723	39954.846104	32.347482
683.937248	40029.429137	32.352500
684.494756	40099.019986	32.357517
685.354426	40164.126760	32.362535
686.037914	40241.090493	32.367552
686.644975	40301.107556	32.372570
687.240161	40366.149850	32.377588
688.346111	40440.528956	32.382605
689.108664	40488.835385	32.387623
689.791732	40560.376519	32.392640
690.787794	40604.952517	32.397658
692.151505	40650.254935	32.402676
692.837635	40709.328403	32.407693
693.455317	40758.418080	32.412711
694.276346	40812.483543	32.417728
694.935001	40861.313895	32.422746
695.721217	40912.408356	32.427764
696.130304	40964.328458	32.432781
696.847047	41006.190690	32.437799
697.746643	41070.798116	32.442816
698.316900	41116.022909	32.447834
699.040086	41183.691921	32.452852
699.382026	41224.779018	32.457869
699.883895	41273.220549	32.462887
700.234777	41339.839384	32.467904
701.262638	41397.186280	32.472922
701.929810	41461.023448	32.477940
702.835898	41531.532394	32.482957
703.697057	41581.400279	32.487975
704.483484	41629.999216	32.492992
705.364581	41674.654308	32.498010
705.909269	41732.397587	32.503028
706.433382	41792.329474	32.508045
707.312944	41840.928792	32.513063
707.758073	41896.100576	32.518080
708.674428	41939.733582	32.523098
709.305188	41992.322670	32.528116
709.631643	42043.454789	32.533133
710.388502	42093.493466	32.538151
710.730671	42157.496042	32.543168
711.198287	42205.519603	32.548186
711.983199	42267.198606	32.553204
712.320884	42329.191235	32.558221
713.252166	42397.173157	32.563239
714.003536	42454.914833	32.568256
714.693318	42522.534422	32.573274
714.778558	42584.084884	32.578292
715.563891	42657.646814	32.583309
716.563484	42722.738553	32.588327
716.873208	42815.100443	32.593344
717.566686	42888.669539	32.598362
718.563042	42954.201537	32.603380
718.930667	43047.732423	32.608397
719.925180	43124.717906	32.613415
720.167738	43210.424388	32.618432
721.036147	43288.530993	32.623450
721.963936	43364.767899	32.628468
722.566097	43442.671300	32.633485
723.307039	43528.293849	32.638503
723.965418	43610.400642	32.643520
724.723652	43709.715924	32.648538
725.584593	43789.565776	32.653556
726.279948	43875.728206	32.658573
727.105365	43942.303397	32.663591
727.806398	44040.695528	32.668608
728.945377	44116.075118	32.673626
730.344862	44178.779272	32.678644
731.165230	44258.802262	32.683661
732.014945	44320.315844	32.688679
732.596282	44389.466979	32.693696
733.373167	44456.582809	32.698714
734.164591	44519.136473	32.703732
734.783292	44576.856853	32.708749
735.477284	44647.047508	32.713767
736.161413	44708.319141	32.718784
736.743205	44780.168441	32.723802
737.731869	44846.804113	32.728820
738.580048	44920.149359	32.733837
739.523967	44983.635278	32.738855
739.937208	45058.912418	32.743872
740.694329	45113.740168	32.748890
741.401481	45183.573707	32.753908
742.066560	45260.292737	32.758925
743.249264	45319.554583	32.763943
743.765252	45400.319809	32.768960
744.286418	45465.073473	32.773978
745.329674	45525.155662	32.778996
745.616525	45596.363810	32.784013
746.627999	45653.192780	32.789031
747.701692	45714.116702	32.794048
748.192638	45770.533063	32.799066
748.973154	45825.055685	32.804084
748.990468	45898.253333	32.809101
750.016249	45957.626159	32.814119
750.669070	46025.580408	32.819136
751.183824	46087.589752	32.824154
752.042246	46160.903287	32.829172
752.477977	46232.754666	32.834189
753.843547	46295.730598	32.839207
754.993875	46359.002577	32.844224
756.492989	46405.183131	32.849242
757.630419	46434.517008	32.854260
758.713692	46476.710746	32.859277
760.205384	46507.913687	32.864295
760.702354	46536.997402	32.869312
761.212631	46578.604198	32.874330
761.808568	46621.633384	32.879348
762.307192	46670.648314	32.884365
763.328709	46710.013936	32.889383
763.754275	46759.025816	32.894400
763.548843	46808.938622	32.899418
764.233387	46863.998600	32.904436
764.590080	46937.423169	32.909453
765.005729	47001.947460	32.914471
765.423533	47079.388864	32.919488
766.259181	47157.046408	32.924506
767.046783	47229.002323	32.929524
767.316188	47319.981250	32.934541
768.334556	47399.895083	32.939559
768.946318	47488.040007	32.944576
769.509089	47571.430952	32.949594
770.320496	47648.519817	32.954612
771.572776	47737.418394	32.959629
772.509196	47824.659646	32.964647
773.134070	47905.299927	32.969664
773.800084	47988.018045	32.974682
775.004453	48070.884341	32.979700
775.630193	48162.084146	32.984717
776.256507	48231.588908	32.989735
777.331313	48310.514579	32.994752
778.200040	48394.867385	32.999770
778.800095	48478.217963	33.004788
779.666272	48564.523891	33.009805
780.028644	48644.302576	33.014823
780.891191	48730.350867	33.019840
781.465487	48814.774890	33.024858
782.659434	48893.331937	33.029876
783.324069	48985.732373	33.034893
784.119336	49068.799371	33.039911
785.288228	49150.899367	33.044928
786.143834	49227.639521	33.049946
787.000964	49307.525703	33.054964
788.338411	49385.674816	33.059981
789.059649	49448.111302	33.064999
789.457406	49515.492996	33.070016
789.932724	49578.161544	33.075034
791.092585	49631.868749	33.080052
791.583804	49708.749030	33.085069
792.257414	49778.958791	33.090087
793.277497	49846.582489	33.095104
793.531945	49917.679496	33.100122
794.298755	49990.262047	33.105140
795.017006	50068.324131	33.110157
795.945363	50140.033025	33.115175
797.297067	50225.536663	33.120192
797.730970	50293.306546	33.125210
798.909743	50352.414021	33.130228
800.002697	50433.559542	33.135245
800.289163	50498.626186	33.140263
801.336546	50573.999468	33.145280
801.812003	50646.128956	33.150298
802.719796	50727.263191	33.155316
802.990762	50806.049249	33.160333
803.875126	50880.225998	33.165351
805.079543	50961.120863	33.170368
805.736558	51041.819208	33.175386
806.484875	51114.788179	33.180404
807.089751	51219.529215	33.185421
807.651576	51294.634647	33.190439
808.992755	51371.717055	33.195456
810.187720	51464.107901	33.200474
811.192866	51542.518446	33.205492
811.491254	51625.454003	33.210509
812.547839	51694.208774	33.215527
812.770204	51784.802822	33.220544
813.493126	51872.904363	33.225562
814.227890	51945.632342	33.230580
814.975627	52045.343065	33.235597
815.694807	52139.770887	33.240615
816.870882	52226.564353	33.245632
817.575476	52315.220696	33.250650
819.238067	52387.507067	33.255668
820.339398	52454.089679	33.260685
821.020014	52532.945178	33.265703
821.665442	52610.789772	33.270720
822.175585	52697.130730	33.275738
823.507308	52778.308245	33.280756
824.143403	52865.020102	33.285773
824.920498	52954.140778	33.290791
826.355824	53012.681594	33.295808
826.991564	53093.859568	33.300826
827.670039	53163.821563	33.305844
828.542038	53239.475224	33.310861
829.340384	53316.462364	33.315879
830.654295	53392.502172	33.320896
830.977646	53472.616823	33.325914
831.431504	53542.353248	33.330932
832.238970	53628.306140	33.335949
832.983898	53710.769579	33.340967
833.604934	53780.610899	33.345984
834.229903	53869.338400	33.351002
835.060082	53929.394658	33.356020
835.957231	54013.482470	33.361037
836.940996	54095.047247	33.366055
837.824613	54167.599941	33.371072
839.404185	54234.397305	33.376090
840.304574	54289.090582	33.381108
840.925536	54368.785060	33.386125
841.671955	54433.665848	33.391143
842.409702	54510.649045	33.396160
843.014810	54588.331385	33.401178
843.872641	54669.951686	33.406196
844.426615	54747.220033	33.411213
844.925849	54830.652771	33.416231
845.932229	54912.096964	33.421248
846.744579	55008.715207	33.426266
847.553282	55090.990191	33.431284
848.451640	55181.610356	33.436301
849.526414	55279.518296	33.441319
850.248221	55363.799821	33.446336
851.041598	55464.113917	33.451354
851.887390	55539.597562	33.456372
852.451722	55634.637266	33.461389
853.369864	55724.978457	33.466407
854.361589	55812.760765	33.471424
855.155137	55914.770667	33.476442
856.087002	55999.973112	33.481460
856.921034	56097.483929	33.486477
856.993780	56198.967832	33.491495
858.709150	56284.473331	33.496512
859.897334	56372.559372	33.501530
861.159630	56448.316353	33.506548
862.391909	56529.892745	33.511565
863.846491	56593.344783	33.516583
865.462963	56653.350397	33.521600
865.913002	56724.381461	33.526618
866.921342	56770.114478	33.531636
868.172618	56843.252195	33.536653
868.787398	56905.231228	33.541671
869.801528	56950.875191	33.546688
870.385184	57018.901519	33.551706
871.182858	57064.525936	33.556724
871.999126	57135.369328	33.561741
872.714391	57216.253410	33.566759
873.258807	57285.557631	33.571776
873.809572	57362.798679	33.576794
874.337326	57435.550564	33.581812
874.847391	57518.916777	33.586829
875.359480	57614.606763	33.591847
876.612096	57700.083783	33.596864
877.387746	57786.420209	33.601882
878.392713	57880.737768	33.606900
879.420076	57968.466492	33.611917
880.172762	58044.569559	33.616935
881.391770	58110.803297	33.621952
881.969337	58190.766851	33.626970
883.128553	58260.879201	33.631988
884.222169	58322.180158	33.637005
884.711245	58395.232838	33.642023
885.461773	58470.794343	33.647040
885.901297	58555.523092	33.652058
886.658979	58636.847993	33.657076
887.613387	58726.735041	33.662093
888.221164	58824.531620	33.667111
888.836890	58915.899569	33.672128
889.453133	59021.317914	33.677146
890.186167	59113.722152	33.682164
891.332980	59220.194638	33.687181
891.797424	59330.121731	33.692199
892.702192	59430.095134	33.697216
893.210569	59534.390600	33.702234
894.209614	59646.092372	33.707252
895.238174	59769.122452	33.712269
895.797685	59886.064708	33.717287
897.046058	60000.500452	33.722304
897.523703	60122.603068	33.727322
898.630200	60243.505226	33.732340
900.014249	60358.602369	33.737357
900.981539	60463.569813	33.742375
902.436067	60573.409853	33.747392
904.034077	60654.194327	33.752410
905.314706	60746.234031	33.757428
906.544689	60838.219612	33.762445
907.597129	60925.432120	33.767463
908.866175	61006.362816	33.772480
909.341562	61086.165565	33.777498
910.258245	61168.560500	33.782516
911.239284	61246.779197	33.787533
912.226701	61332.500167	33.792551
913.054146	61412.307094	33.797568
914.005511	61502.718851	33.802586
915.037281	61588.452252	33.807604
915.733242	61668.099374	33.812621
916.871736	61757.152759	33.817639
917.384347	61838.001353	33.822656
918.188826	61928.914222	33.827674
918.841506	62014.107477	33.832692
919.757775	62111.645630	33.837709
920.621329	62201.026150	33.842727
921.598347	62297.941610	33.847744
922.314219	62391.564572	33.852762
923.678693	62477.781994	33.857780
924.786167	62567.577460	33.862797
925.446827	62660.205985	33.867815
926.504875	62750.497457	33.872832
927.228673	62848.824296	33.877850
928.086659	62940.851342	33.882868
928.988594	63038.219302	33.887885
929.683526	63131.147489	33.892903
930.485087	63215.593194	33.897920
931.919894	63286.200205	33.902938
933.400014	63361.781159	33.907956
934.648444	63427.748870	33.912973
935.596258	63488.698278	33.917991
937.423720	63544.755934	33.923008
938.048026	63607.227730	33.928026
938.568238	63668.408938	33.933044
939.374756	63734.826289	33.938061
940.078026	63807.172404	33.943079
941.151370	63876.439888	33.948096
941.599615	63965.526130	33.953114
942.406739	64042.356420	33.958132
943.033511	64131.513943	33.963149
943.156277	64230.531840	33.968167
944.236080	64320.839035	33.973184
944.867681	64432.522104	33.978202
945.705869	64536.969619	33.983220
946.555912	64639.259809	33.988237
947.280229	64748.892987	33.993255
948.152429	64854.834589	33.998272
948.854570	64983.483359	34.003290
949.774255	65099.849600	34.008308
950.687614	65218.032041	34.013325
951.480890	65341.337766	34.018343
952.960625	65453.620709	34.023360
953.883307	65583.209003	34.028378
954.818945	65716.671480	34.033396
956.019085	65823.819942	34.038413
956.780997	65943.524469	34.043431
957.706365	66064.826554	34.048448
959.037827	66186.843778	34.053466
960.065190	66303.520660	34.058484
961.580400	66411.819428	34.063501
962.312650	66531.115067	34.068519
963.260266	66627.581390	34.073536
964.601067	66730.227608	34.078554
965.333167	66849.050860	34.083572
966.654648	66949.235594	34.088589
967.491107	67054.479874	34.093607
968.357994	67165.517464	34.098624
969.363709	67276.670961	34.103642
970.373060	67394.273731	34.108660
971.622029	67492.424837	34.113677
972.239478	67603.431552	34.118695
973.230159	67709.329209	34.123712
973.862740	67826.132640	34.128730
974.905696	67946.363062	34.133748
976.003632	68062.784588	34.138765
977.032445	68176.872717	34.143783
977.701339	68287.848883	34.148800
978.429258	68404.120645	34.153818
979.377375	68530.055109	34.158836
980.710931	68642.923742	34.163853
981.219680	68767.973713	34.168871
982.201844	68872.266150	34.173888
983.758890	68981.746947	34.178906
984.377370	69092.792819	34.183924
985.403291	69191.375640	34.188941
986.335616	69306.491719	34.193959
987.490943	69414.848390	34.198976
988.335887	69519.281287	34.203994
989.225033	69635.114747	34.209012
990.266288	69725.672843	34.214029
991.270868	69851.997437	34.219047
992.258564	69956.186677	34.224064
993.576232	70068.989630	34.229082
994.461939	70191.763707	34.234100
995.625530	70291.459922	34.239117
996.171571	70412.307771	34.244135
997.219043	70521.833066	34.249152
998.328197	70628.957951	34.254170
1000.111270	70739.705351	34.259188
1001.782958	70839.639597	34.264205
1002.904946	70947.902159	34.269223
1003.511694	71037.376557	34.274240
1004.689918	71136.340578	34.279258
1005.308262	71244.273483	34.284276
1006.521373	71333.638939	34.289293
1007.255677	71442.292877	34.294311
1008.458129	71551.841097	34.299328
1009.109571	71656.741144	34.304346
1010.108757	71762.062780	34.309364
1012.361239	71831.729687	34.314381
1013.673972	71916.160280	34.319399
1015.155985	72000.922694	34.324416
1016.664974	72077.162077	34.329434
1017.783951	72164.314611	34.334452
1017.931116	72231.706108	34.339469
1018.957939	72316.256779	34.344487
1019.966941	72398.616288	34.349504
1020.787332	72487.326429	34.354522
1021.295624	72581.832906	34.359540
1022.276961	72665.697035	34.364557
1023.299079	72768.249507	34.369575
1023.952422	72874.375683	34.374592
1024.988754	72971.133465	34.379610
1025.789118	73077.311339	34.384628
1026.894423	73178.535983	34.389645
1027.774807	73282.708915	34.394663
1028.560885	73389.934300	34.399680
1029.594744	73498.028525	34.404698
1030.146593	73622.302111	34.409716
1031.153801	73733.564393	34.414733
1032.267362	73845.846281	34.419751
1033.060584	73968.518272	34.424768
1034.396532	74082.780887	34.429786
1035.532515	74210.790590	34.434804
1037.045366	74316.131392	34.439821
1038.280472	74427.174721	34.444839
1039.045993	74523.504997	34.449856
1039.957739	74617.736066	34.454874
1040.409679	74731.849812	34.459892
1041.272812	74817.665167	34.464909
1042.456910	74926.208700	34.469927
1042.922952	75038.544268	34.474944
1044.539471	75151.568913	34.479962
1045.572967	75272.088063	34.484980
1046.460704	75381.329733	34.489997
1047.379323	75492.976554	34.495015
1048.902136	75606.822862	34.500032
1050.514006	75726.018334	34.505050
1051.390890	75841.235177	34.510068
1052.478924	75941.298902	34.515085
1053.220178	76051.473461	34.520103
1053.799840	76163.592828	34.525120
1055.164416	76271.979184	34.530138
1055.964125	76397.522558	34.535156
1056.951399	76518.859689	34.540173
1057.824284	76643.481039	34.545191
1058.670440	76771.536116	34.550208
1059.666622	76892.481557	34.555226
1060.434312	77032.310855	34.560244
1061.641611	77170.440046	34.565261
1062.555711	77300.143829	34.570279
1063.750383	77438.732280	34.575296
1064.989387	77567.382498	34.580314
1065.873730	77708.979895	34.585332
1067.514623	77839.998298	34.590349
1068.506324	77974.240969	34.595367
1069.352171	78111.362414	34.600384
1070.730678	78224.044787	34.605402
1071.544057	78364.393247	34.610420
1073.013476	78488.789806	34.615437
1074.634546	78619.056994	34.620455
1075.027667	78759.619035	34.625472
1076.761943	78878.019497	34.630490
1077.592153	79015.870273	34.635508
1078.917921	79143.160787	34.640525
1079.326615	79274.430109	34.645543
1080.342166	79408.126797	34.650560
1081.571757	79541.528240	34.655578
1082.257603	79688.599981	34.660596
1083.457729	79815.865157	34.665613
1084.690238	79958.125522	34.670631
1085.766404	80091.050330	34.675648
1087.529743	80221.536411	34.680666
1089.152394	80354.128767	34.685684
1090.204751	80466.669320	34.690701
1091.209043	80574.593890	34.695719
1092.562044	80710.480041	34.700736
1094.083095	80817.380925	34.705754
1095.856751	80914.312428	34.710772
1097.657524	81006.627500	34.715789
1099.136901	81085.882582	34.720807
1099.717315	81164.387132	34.725824
1101.354939	81235.548980	34.730842
1102.312021	81316.944177	34.735860
1103.026326	81383.557417	34.740877
1103.720011	81469.939525	34.745895
1104.445877	81551.071449	34.750912
1105.580813	81639.061592	34.755930
1106.037143	81737.848149	34.760948
1107.265020	81839.312197	34.765965
1107.926453	81938.950271	34.770983
1108.415562	82041.300941	34.776000
1109.589783	82142.617333	34.781018
1110.744749	82259.634969	34.786036
1111.563181	82387.757975	34.791053
1112.614611	82509.957537	34.796071
1113.800789	82620.897583	34.801088
1115.055208	82740.115132	34.806106
1115.820059	82876.570308	34.811124
1117.106964	83005.432726	34.816141
1117.845779	83132.143502	34.821159
1118.826193	83261.743168	34.826176
1120.019734	83386.162890	34.831194
1121.623452	83510.133400	34.836212
1123.011940	83631.097913	34.841229
1124.071481	83763.281078	34.846247
1124.804240	83896.489055	34.851264
1126.055630	84023.642094	34.856282
1126.937851	84167.070355	34.861300
1128.074670	84301.983185	34.866317
1129.366406	84434.839083	34.871335
1130.275391	84574.512940	34.876352
1131.994313	84692.116966	34.881370
1133.454427	84824.395726	34.886388
1134.275727	84946.755017	34.891405
1135.309676	85077.368018	34.896423
1136.282307	85208.814867	34.901440
1137.599866	85347.524798	34.906458
1138.593862	85491.340659	34.911476
1139.646269	85621.409308	34.916493
1141.440683	85747.459890	34.921511
1142.514817	85875.387343	34.926528
1143.349583	86013.386512	34.931546
1144.293127	86149.880746	34.936564
1145.519802	86282.922732	34.941581
1146.641261	86420.843545	34.946599
1147.290688	86565.427355	34.951616
1148.582536	86705.820307	34.956634
1149.968983	86854.886682	34.961652
1150.854612	86993.363787	34.966669
1151.928708	87128.354123	34.971687
1152.750009	87280.892961	34.976704
1154.338981	87433.408920	34.981722
1155.072210	87582.110717	34.986740
1156.335139	87728.039437	34.991757
1157.510063	87873.876529	34.996775
1158.353997	88007.506290	35.001792
1160.280548	88130.072463	35.006810
1161.422762	88258.709870	35.011828
1162.741291	88394.266726	35.016845
1164.194053	88504.954634	35.021863
1165.579943	88643.513856	35.026880
1166.627966	88762.195902	35.031898
1167.572834	88887.427580	35.036916
1168.623014	89007.439527	35.041933
1169.933573	89130.109943	35.046951
1171.376026	89260.131639	35.051968
1172.554366	89384.262658	35.056986
1173.555970	89508.304324	35.062004
1174.703683	89631.486174	35.067021
1176.225228	89754.642623	35.072039
1177.138004	89888.195079	35.077056
1177.955098	90018.410199	35.082074
1179.006777	90154.003642	35.087092
1179.826082	90292.125013	35.092109
1181.305569	90429.532860	35.097127
1181.708163	90587.689762	35.102144
1182.877581	90741.279532	35.107162
1184.277554	90890.552133	35.112180
1185.106046	91049.892332	35.117197
1186.521878	91203.354211	35.122215
1187.301787	91369.990029	35.127232
1188.961536	91525.981954	35.132250
1189.762210	91683.261278	35.137268
1191.026327	91847.013433	35.142285
1192.939561	91999.749524	35.147303
1194.031924	92165.090306	35.152320
1194.863299	92308.582267	35.157338
1196.140708	92475.387274	35.162356
1197.818386	92627.325732	35.167373
1199.524325	92764.581323	35.172391
1201.054083	92925.370780	35.177408
1202.158260	93059.888910	35.182426
1203.797383	93192.113356	35.187444
1204.959471	93327.908016	35.192461
1206.604664	93460.373399	35.197479
1208.006154	93588.152645	35.202496
1209.551614	93710.337407	35.207514
1210.796971	93839.385380	35.212532
1212.371694	93957.109930	35.217549
1213.500767	94073.385755	35.222567
1214.484925	94188.439878	35.227584
1215.663110	94309.120568	35.232602
1216.935130	94433.666248	35.237620
1218.017110	94563.271363	35.242637
1219.079539	94674.155306	35.247655
1220.366674	94808.613606	35.252672
1221.243116	94926.050808	35.257690
1222.432870	95052.493794	35.262708
1223.136588	95193.004664	35.267725
1224.494326	95325.605154	35.272743
1225.110619	95462.441808	35.277760
1226.086289	95586.050067	35.282778
1227.250715	95712.367775	35.287796
1228.124553	95853.650874	35.292813
1229.265738	96002.112311	35.297831
1229.947724	96142.265028	35.302848
1231.105145	96291.852261	35.307866
1232.382132	96447.782364	35.312884
1233.717222	96612.009545	35.317901
1235.032085	96752.677725	35.322919
1236.224178	96916.545181	35.327936
1237.384328	97063.838393	35.332954
1238.814496	97217.987015	35.337972
1239.693955	97382.024958	35.342989
1241.208129	97538.744208	35.348007
1242.351258	97703.448166	35.353024
1244.330000	97853.302872	35.358042
1246.006867	97989.490462	35.363060
1247.461147	98135.422644	35.368077
1249.531755	98269.018166	35.373095
1250.541281	98417.079424	35.378112
1251.551232	98551.896337	35.383130
1252.966642	98694.938625	35.388148
1253.987814	98826.032221	35.393165
1255.356498	98958.922103	35.398183
1256.268747	99104.154846	35.403200
1257.507148	99258.525906	35.408218
1259.147352	99398.690794	35.413236
1259.932609	99553.590739	35.418253
1261.223086	99693.658815	35.423271
1262.019301	99851.293924	35.428288
1263.056615	100010.889533	35.433306
1264.569280	100166.460090	35.438324
1265.401983	100328.093507	35.443341
1266.700623	100490.369993	35.448359
1267.971799	100663.865885	35.453376
1269.248668	100817.543176	35.458394
1270.874237	100985.813739	35.463412
1272.110555	101156.615161	35.468429
1273.149962	101322.544110	35.473447
1274.576738	101497.354979	35.478464
1275.533394	101661.495618	35.483482
1277.146076	101828.982324	35.488500
1278.411245	102000.582179	35.493517
1280.023968	102155.355985	35.498535
1280.949795	102314.794842	35.503552
1282.338806	102481.526150	35.508570
1284.310682	102633.417100	35.513588
1285.759711	102798.050480	35.518605
1287.370358	102947.484806	35.523623
1288.944626	103096.698241	35.528640
1290.142137	103237.200222	35.533658
1291.341559	103380.045648	35.538676
1292.308824	103530.201335	35.543693
1293.805860	103670.223734	35.548711
1294.711715	103817.098628	35.553728
1295.706609	103962.831884	35.558746
1296.745526	104095.475110	35.563764
1298.284598	104243.231864	35.568781
1299.506740	104384.736287	35.573799
1301.049761	104520.119741	35.578816
1302.535150	104662.885132	35.583834
1303.835702	104798.387503	35.588852
1304.970965	104946.103297	35.593869
1306.028609	105082.370639	35.598887
1307.303930	105240.716031	35.603904
1308.673211	105385.620368	35.608922
1309.881267	105522.953481	35.613940
1311.429015	105679.696917	35.618957
1312.853909	105822.086211	35.623975
1314.216063	105975.772607	35.628992
1315.490675	106130.551503	35.634010
1316.997438	106278.147717	35.639028
1317.874586	106433.123054	35.644045
1319.448503	106587.587347	35.649063
1320.750152	106737.995159	35.654080
1321.530893	106891.912973	35.659098
1322.978204	107050.226916	35.664116
1323.967499	107218.386294	35.669133
1325.188480	107384.138348	35.674151
1326.544221	107556.746509	35.679168
1328.169511	107719.023986	35.684186
1329.975788	107889.226402	35.689204
1331.008268	108057.168239	35.694221
1332.740504	108222.812557	35.699239
1333.696571	108379.482919	35.704256
1334.636011	108551.991305	35.709274
1335.970586	108721.025581	35.714292
1337.215139	108895.295355	35.719309
1338.444182	109072.343111	35.724327
1340.411630	109240.030826	35.729344
1341.600120	109426.993989	35.734362
1342.635694	109604.838362	35.739380
1343.413819	109785.122202	35.744397
1344.662515	109964.781943	35.749415
1346.130534	110147.673695	35.754432
1347.392928	110336.315234	35.759450
1348.818831	110509.867424	35.764468
1350.136738	110694.055314	35.769485
1351.569039	110893.161004	35.774503
1353.325838	111082.305738	35.779520
1354.780161	111264.649782	35.784538
1356.425562	111447.507070	35.789556
1357.647044	111630.818183	35.794573
1358.939724	111807.682502	35.799591
1360.237096	111990.476226	35.804608
1361.988464	112173.687528	35.809626
1363.546625	112347.431226	35.814644
1364.892379	112526.318062	35.819661
1366.296261	112697.100391	35.824679
1367.632071	112858.811454	35.829696
1369.095038	113014.395000	35.834714
1370.472626	113169.601263	35.839732
1371.452421	113337.634759	35.844749
1372.658503	113500.283914	35.849767
1373.832048	113671.605684	35.854784
1374.551396	113838.571793	35.859802
1376.204489	114005.708474	35.864820
1377.732165	114197.434703	35.869837
1379.179806	114376.303133	35.874855
1380.892742	114545.624667	35.879872
1382.186221	114723.824808	35.884890
1383.838711	114882.870473	35.889908
1385.286587	115051.619536	35.894925
1386.827480	115219.796173	35.899943
1388.106259	115383.520631	35.904960
1389.689974	115560.067146	35.909978
1391.297140	115722.292881	35.914996
1393.043304	115887.257960	35.920013
1394.482160	116049.919816	35.925031
1395.721530	116222.069211	35.930048
1396.937488	116385.480681	35.935066
1398.417604	116537.646677	35.940084
1399.948719	116712.992843	35.945101
1400.945921	116884.452708	35.950119
1402.193037	117060.825269	35.955136
1403.449520	117249.475815	35.960154
1404.452114	117426.792113	35.965172
1406.091417	117613.529470	35.970189
1407.168313	117797.145706	35.975207
1408.581474	117989.791114	35.980224
1410.540590	118166.517353	35.985242
1412.139536	118343.128902	35.990260
1413.595561	118526.545435	35.995277
1414.767340	118722.810452	36.000295
1416.550956	118893.868730	36.005312
1417.661446	119081.745069	36.010330
1419.201407	119267.901711	36.015348
1420.528682	119466.273996	36.020365
1421.652963	119644.355878	36.025383
1423.017672	119833.169256	36.030400
1424.548167	120033.588842	36.035418
1425.995428	120222.339878	36.040436
1427.279536	120411.855054	36.045453
1428.586413	120613.736167	36.050471
1430.079718	120803.674250	36.055488
1431.289747	121009.858046	36.060506
1432.943652	121200.354120	36.065524
1434.613149	121393.472071	36.070541
1436.130649	121578.126247	36.075559
1437.823508	121760.267586	36.080576
1439.302616	121950.418145	36.085594
1440.780782	122145.233886	36.090612
1442.336458	122335.715955	36.095629
1443.160626	122526.552550	36.100647
1444.937131	122698.457664	36.105664
1446.234264	122871.979322	36.110682
1447.580257	123059.358751	36.115700
1449.122663	123224.285629	36.120717
1450.416846	123407.557064	36.125735
1452.004086	123583.098987	36.130752
1452.962773	123773.742959	36.135770
1454.077301	123944.767170	36.140788
1455.595623	124138.841058	36.145805
1456.622286	124335.116939	36.150823
1458.478558	124534.078482	36.155840
1459.372677	124737.794157	36.160858
1460.807770	124938.237273	36.165876
1462.241758	125145.805044	36.170893
1463.227339	125362.247237	36.175911
1464.943097	125578.756099	36.180928
1466.388869	125801.067104	36.185946
1467.921163	126004.060834	36.190964
1469.377658	126216.765319	36.195981
1471.204472	126436.417261	36.200999
1472.850115	126636.074817	36.206016
1474.070373	126866.176625	36.211034
1475.689311	127085.044812	36.216052
1477.381380	127308.896179	36.221069
1478.669731	127515.528671	36.226087
1480.435430	127733.780514	36.231104
1481.718833	127963.676751	36.236122
1483.274115	128171.231225	36.241140
1484.655780	128385.306879	36.246157
1485.740695	128627.943255	36.251175
1487.695007	128839.971861	36.256192
1488.940535	129076.322153	36.261210
1490.355588	129303.087220	36.266228
1491.954090	129534.715609	36.271245
1493.465087	129758.196970	36.276263
1495.411103	129977.612309	36.281280
1496.781646	130213.214376	36.286298
1498.166542	130435.517756	36.291316
1499.830568	130659.131327	36.296333
1501.381828	130895.265246	36.301351
1503.136373	131112.971681	36.306368
1504.200578	131351.410774	36.311386
1505.987598	131573.285532	36.316404
1507.418206	131791.711185	36.321421
1509.380756	132018.807362	36.326439
1511.243826	132235.539275	36.331456
1512.816362	132447.821810	36.336474
1515.083719	132649.172769	36.341492
1517.043048	132848.866190	36.346509
1518.814864	133052.117352	36.351527
1520.607675	133231.836019	36.356544
1521.911631	133430.529485	36.361562
1523.630028	133617.071058	36.366580
1524.953817	133810.096338	36.371597
1526.280377	133998.799013	36.376615
1527.628647	134166.313700	36.381632
1529.193720	134340.080571	36.386650
1530.683283	134516.764624	36.391668
1532.390943	134686.603969	36.396685
1533.788971	134861.898214	36.401703
1535.740248	135017.345491	36.406720
1536.978366	135197.144399	36.411738
1538.495424	135372.801319	36.416756
1539.706561	135555.751090	36.421773
1540.785822	135735.884368	36.426791
1542.194573	135917.116006	36.431808
1543.423058	136121.569322	36.436826
1544.667619	136309.246735	36.441844
1546.313230	136514.074815	36.446861
1547.385270	136722.197452	36.451879
1548.928128	136931.331215	36.456896
1550.315887	137141.925579	36.461914
1552.023854	137360.898281	36.466932
1553.219840	137577.994680	36.471949
1554.857424	137793.292464	36.476967
1556.338665	138008.390126	36.481984
1557.462441	138246.373898	36.487002
1559.135208	138478.014200	36.492020
1560.838037	138695.804423	36.497037
1562.218911	138932.087874	36.502055
1564.103050	139160.209588	36.507072
1565.827385	139395.904872	36.512090
1567.184494	139617.919179	36.517108
1569.028875	139849.805604	36.522125
1570.453060	140097.933055	36.527143
1571.914531	140325.145683	36.532160
1573.508442	140557.574222	36.537178
1575.095960	140801.988665	36.542196
1577.066278	141033.798001	36.547213
1578.065836	141277.263862	36.552231
1579.812516	141515.746746	36.557248
1581.891353	141759.513124	36.562266
1583.884470	141978.301337	36.567284
1585.889511	142202.275477	36.572301
1587.963808	142432.212068	36.577319
1589.997000	142635.336086	36.582336
1591.192164	142863.434930	36.587354
1592.981798	143078.105223	36.592372
1594.693120	143295.947923	36.597389
1595.794313	143515.760560	36.602407
1597.442820	143730.015050	36.607424
1599.042458	143943.683134	36.612442
1600.413214	144167.587900	36.617460
1602.375418	144382.870555	36.622477
1603.657149	144614.072779	36.627495
1605.494973	144817.293298	36.632512
1606.944448	145044.309819	36.637530
1608.063221	145266.869449	36.642548
1609.553342	145488.314256	36.647565
1611.325855	145714.290444	36.652583
1613.040381	145915.027058	36.657600
1614.737651	146122.210476	36.662618
1616.438611	146328.291040	36.667636
1618.130229	146527.880801	36.672653
1619.667486	146729.565351	36.677671
1620.637069	146937.727621	36.682688
1622.140034	147155.324675	36.687706
1623.333505	147376.298915	36.692724
1624.895106	147601.460309	36.697741
1626.307671	147833.155032	36.702759
1628.004161	148057.230710	36.707776
1629.477439	148300.117246	36.712794
1631.182386	148532.121398	36.717812
1632.738292	148771.432807	36.722829
1634.037058	149022.889860	36.727847
1635.830524	149264.243852	36.732864
1637.358689	149512.760354	36.737882
1638.881672	149760.505657	36.742900
1640.853477	150015.215342	36.747917
1642.307963	150269.089317	36.752935
1643.965849	150520.507517	36.757952
1645.786887	150765.709586	36.762970
1647.460313	151016.697120	36.767988
1649.273471	151259.163892	36.773005
1651.212972	151521.068433	36.778023
1653.694473	151754.773201	36.783040
1655.273504	151996.802653	36.788058
1656.409420	152247.382769	36.793076
1658.804821	152477.948151	36.798093
1660.504165	152713.834760	36.803111
1662.390669	152947.204535	36.808128
1664.086097	153180.456176	36.813146
1665.754411	153418.496091	36.818164
1667.605989	153652.015566	36.823181
1668.912964	153893.583207	36.828199
1670.629656	154133.445822	36.833216
1672.442261	154366.443404	36.838234
1673.910730	154606.884135	36.843252
1676.438624	154828.916027	36.848269
1677.990592	155068.850524	36.853287
1679.806158	155295.548318	36.858304
1681.305560	155535.037919	36.863322
1683.098279	155758.443957	36.868340
1685.074336	155986.500935	36.873357
1686.626405	156208.453714	36.878375
1688.320117	156431.880420	36.883392
1690.422115	156662.253879	36.888410
1691.623773	156899.924976	36.893428
1693.721670	157120.419249	36.898445
1695.290744	157338.708983	36.903463
1696.857847	157567.085843	36.908480
1698.739028	157781.696248	36.913498
1700.570103	158007.493115	36.918516
1702.299750	158218.478026	36.923533
1703.917347	158438.719024	36.928551
1705.556102	158631.034249	36.933568
1707.292136	158832.950247	36.938586
1708.548081	159037.461351	36.943604
1710.619357	159227.485149	36.948621
1711.954874	159430.741258	36.953639
1713.462104	159636.087697	36.958656
1715.107969	159844.951100	36.963674
1716.265815	160063.071801	36.968692
1718.366146	160277.479975	36.973709
1719.281428	160518.671715	36.978727
1720.902100	160737.541383	36.983744
1723.010234	160964.271062	36.988762
1724.386680	161214.903374	36.993780
1726.199053	161442.802701	36.998797
1727.457778	161685.312546	37.003815
1729.065544	161926.888597	37.008832
1730.779517	162168.282896	37.013850
1732.678266	162418.020872	37.018868
1734.753035	162657.453016	37.023885
1736.308077	162919.445725	37.028903
1737.487305	163178.395753	37.033920
1739.498359	163441.683896	37.038938
1740.806909	163699.193826	37.043956
1742.596737	163973.206451	37.048973
1744.302060	164245.623828	37.053991
1745.715005	164523.599678	37.059008
1747.104609	164800.642322	37.064026
1748.751295	165080.497639	37.069044
1750.801881	165354.055498	37.074061
1752.197838	165652.063987	37.079079
1754.295386	165936.910343	37.084096
1756.204168	166225.876624	37.089114
1757.337970	166513.124761	37.094132
1759.462910	166803.796153	37.099149
1760.948952	167099.628989	37.104167
1763.001324	167400.302961	37.109184
1765.113330	167692.276550	37.114202
1766.996985	167985.471183	37.119220
1768.823754	168274.515283	37.124237
1770.442834	168575.283787	37.129255
1772.228483	168869.071842	37.134272
1774.232475	169162.266059	37.139290
1775.875466	169462.515951	37.144308
1778.193359	169750.888815	37.149325
1779.888032	170041.298948	37.154343
1781.330694	170326.969857	37.159360
1783.480752	170625.541502	37.164378
1785.318850	170921.960314	37.169396
1787.420076	171206.534034	37.174413
1789.067848	171497.481431	37.179431
1791.320352	171788.872828	37.184448
1793.129053	172062.575262	37.189466
1794.732490	172350.870423	37.194484
1796.729012	172625.825669	37.199501
1798.308140	172903.658527	37.204519
1800.222835	173169.430105	37.209536
1802.356665	173417.664994	37.214554
1804.138572	173681.139656	37.219572
1806.587563	173921.683271	37.224589
1808.225045	174167.075261	37.229607
1809.614742	174414.274922	37.234624
1812.064450	174651.078105	37.239642
1813.855284	174901.638182	37.244660
1815.802553	175136.841707	37.249677
1818.028831	175379.638789	37.254695
1819.759551	175600.870324	37.259712
1822.061074	175840.585453	37.264730
1823.408151	176077.660183	37.269748
1825.427378	176321.347567	37.274765
1827.278049	176561.244780	37.279783
1828.943324	176800.286426	37.284800
1831.182761	177032.009369	37.289818
1832.994131	177272.221256	37.294836
1835.321098	177516.077473	37.299853
1837.151198	177754.143488	37.304871
1838.506885	177995.908975	37.309888
1840.536510	178234.856896	37.314906
1841.935481	178485.780913	37.319924
1843.840043	178724.701713	37.324941
1845.636328	178973.237443	37.329959
1847.116855	179222.285291	37.334976
1848.785363	179466.707536	37.339994
1850.622148	179738.098854	37.345012
1852.182737	180001.771024	37.350029
1853.872159	180266.755180	37.355047
1855.454551	180539.006431	37.360064
1857.266652	180807.323127	37.365082
1858.899032	181090.687395	37.370100
1860.368556	181373.979471	37.375117
1862.248381	181656.365112	37.380135
1864.025166	181951.221605	37.385152
1865.892357	182232.901598	37.390170
1867.562022	182529.785031	37.395188
1869.567661	182816.572335	37.400205
1871.767725	183108.417840	37.405223
1873.237738	183407.409141	37.410240
1875.613577	183700.484326	37.415258
1877.573680	183994.533400	37.420276
1879.620042	184277.957532	37.425293
1881.593121	184571.575831	37.430311
1883.578007	184870.042587	37.435328
1885.027045	185189.458254	37.440346
1886.668651	185513.894875	37.445364
1888.403484	185820.368352	37.450381
1890.354187	186113.465284	37.455399
1892.576135	186411.594877	37.460416
1894.572779	186710.246917	37.465434
1896.520219	187011.993561	37.470452
1898.633547	187300.993876	37.475469
1900.744456	187578.901312	37.480487
1902.643250	187852.974599	37.485504
1904.691620	188118.010619	37.490522
1906.398913	188379.742162	37.495540
1908.438609	188650.050192	37.500557
1910.375318	188917.711221	37.505575
1911.784976	189186.009462	37.510592
1914.260789	189455.446761	37.515610
1915.433594	189722.899277	37.520628
1917.673180	189999.361448	37.525645
1919.485467	190266.529238	37.530663
1921.503018	190557.542009	37.535680
1923.470027	190823.822509	37.540698
1925.118836	191110.597404	37.545716
1926.919460	191403.352379	37.550733
1928.999190	191682.134529	37.555751
1930.539808	191977.767661	37.560768
1932.631887	192261.628310	37.565786
1934.311783	192562.394589	37.570804
1936.297392	192859.707666	37.575821
1938.357003	193158.152050	37.580839
1940.242376	193466.771244	37.585856
1942.682823	193749.449032	37.590874
1945.075930	194037.557134	37.595892
1947.995361	194323.646761	37.600909
1949.857549	194596.054872	37.605927
1951.624339	194881.861663	37.610944
1953.297937	195164.372051	37.615962
1954.869206	195455.648536	37.620980
1956.427786	195761.135106	37.625997
1958.398217	196045.731362	37.631015
1960.588645	196358.069924	37.636032
1962.425095	196654.295765	37.641050
1964.558757	196964.183809	37.646068
1966.514138	197251.085693	37.651085
1968.532182	197553.492779	37.656103
1970.226842	197857.099166	37.661120
1972.193774	198158.920921	37.666138
1974.591063	198471.106765	37.671156
1976.128552	198790.462171	37.676173
1978.207216	199087.990136	37.681191
1979.591716	199409.367852	37.686208
1981.577539	199722.569151	37.691226
1983.353417	200037.001214	37.696244
1985.622971	200364.580146	37.701261
1987.756185	200679.385575	37.706279
1989.809286	201003.982595	37.711296
1991.868212	201310.715601	37.716314
1993.802631	201629.215809	37.721332
1996.364923	201958.478585	37.726349
1998.819310	202268.639584	37.731367
2000.405273	202584.892624	37.736384
2002.597075	202884.752980	37.741402
2004.384902	203191.781328	37.746420
2006.828836	203507.802595	37.751437
2008.970743	203804.551592	37.756455
2010.066313	204096.795385	37.761472
2012.283396	204382.042679	37.766490
2014.559570	204674.810470	37.771508
2016.136501	204965.172157	37.776525
2017.901622	205250.957024	37.781543
2019.954953	205556.806533	37.786560
2021.464519	205850.052627	37.791578
2023.563673	206154.906176	37.796596
2025.262304	206463.194265	37.801613
2027.265511	206777.907278	37.806631
2029.167166	207094.467352	37.811648
2031.142672	207397.556313	37.816666
2033.473704	207734.260356	37.821684
2035.231748	208069.489215	37.826701
2037.503805	208378.041928	37.831719
2039.922834	208702.798713	37.836736
2041.865896	209033.377674	37.841754
2043.974385	209350.901343	37.846772
2045.824375	209672.762375	37.851789
2048.420656	209978.090869	37.856807
2050.336006	210314.012720	37.861824
2052.342010	210627.241165	37.866842
2054.427428	210952.571368	37.871860
2056.351554	211279.428755	37.876877
2058.992115	211608.501317	37.881895
2060.991454	211936.922833	37.886912
2062.847535	212247.769859	37.891930
2065.040476	212580.655859	37.896948
2066.990720	212909.394017	37.901965
2069.534076	213236.101701	37.906983
2071.355491	213564.026081	37.912000
2073.642679	213888.392481	37.917018
2076.444044	214218.640487	37.922036
2078.544017	214540.171187	37.927053
2080.592650	214851.933592	37.932071
2082.996991	215177.427198	37.937088
2085.184930	215494.907744	37.942106
2087.328379	215799.672510	37.947124
2088.779912	216127.287836	37.952141
2091.465150	216440.114686	37.957159
2093.482530	216751.609019	37.962176
2095.399967	217068.429646	37.967194
2097.628299	217390.455551	37.972212
2099.430040	217726.169002	37.977229
2101.592147	218032.029376	37.982247
2103.946092	218361.453170	37.987264
2106.089222	218674.277873	37.992282
2108.268728	218996.952002	37.997300
2110.741238	219315.005187	38.002317
2112.364069	219620.022556	38.007335
2114.425078	219947.545560	38.012352
2116.862537	220262.889786	38.017370
2119.069623	220572.915075	38.022388
2120.693387	220897.569331	38.027405
2122.925861	221206.195052	38.032423
2124.725708	221507.275776	38.037440
2126.824706	221808.661716	38.042458
2128.576693	222099.389188	38.047476
2130.406243	222404.505663	38.052493
2132.300706	222711.364393	38.057511
2133.968772	223031.699061	38.062528
2136.154157	223345.494569	38.067546
2138.077914	223676.480505	38.072564
2139.745916	224006.622068	38.077581
2141.747797	224346.511792	38.082599
2143.905586	224691.785977	38.087616
2145.804233	225045.055644	38.092634
2147.920808	225382.998110	38.097652
2149.768142	225748.749951	38.102669
2152.292053	226094.752670	38.107687
2154.144748	226464.417215	38.112704
2156.260016	226822.607671	38.117722
2158.886935	227190.719372	38.122740
2160.839503	227547.872720	38.127757
2163.194818	227919.792080	38.132775
2165.445832	228290.104606	38.137792
2166.829894	228664.808268	38.142810
2169.393719	229032.986342	38.147828
2171.643471	229406.400825	38.152845
2173.948769	229777.774666	38.157863
2176.161014	230162.881882	38.162880
2178.380675	230547.302964	38.167898
2180.870883	230918.495533	38.172916
2183.007652	231307.276245	38.177933
2186.216548	231670.727307	38.182951
2188.915733	232035.536407	38.187968
2191.062222	232398.205500	38.192986
2193.739668	232754.713642	38.198004
2195.797127	233111.480956	38.203021
2198.423381	233453.088632	38.208039
2200.525298	233806.496763	38.213056
2202.970594	234163.377706	38.218074
2205.135234	234509.587833	38.223092
2207.286576	234865.326534	38.228109
2209.644156	235219.049308	38.233127
2211.333405	235575.401802	38.238144
2213.078429	235935.911323	38.243162
2215.396293	236292.335450	38.248180
2217.474820	236657.132982	38.253197
2220.273726	237017.591254	38.258215
2221.944834	237376.160030	38.263232
2224.152335	237751.403078	38.268250
2226.531292	238114.983282	38.273268
2229.013811	238479.841891	38.278285
2231.699493	238828.891576	38.283303
2234.555338	239183.297978	38.288320
2236.466730	239541.194112	38.293338
2239.156941	239891.895766	38.298356
2240.899610	240241.591436	38.303373
2243.768548	240567.521588	38.308391
2245.574961	240897.164778	38.313408
2247.226104	241223.939057	38.318426
2249.695851	241533.325473	38.323444
2251.667797	241859.080382	38.328461
2254.037793	242183.370475	38.333479
2255.928794	242509.978271	38.338496
2257.990325	242852.865758	38.343514
2260.148582	243178.310892	38.348532
2261.899864	243526.637561	38.353549
2264.171729	243876.348967	38.358567
2266.398119	244217.584022	38.363584
2268.374892	244573.849737	38.368602
2270.827348	244924.725314	38.373620
2273.303659	245283.726066	38.378637
2275.532920	245638.831980	38.383655
2277.668532	246000.330365	38.388672
2279.944800	246366.834813	38.393690
2282.347332	246730.498289	38.398708
2284.927124	247107.823957	38.403725
2286.756606	247483.195205	38.408743
2288.690387	247855.932432	38.413760
2290.581560	248242.420261	38.418778
2292.865837	248622.947688	38.423796
2295.152913	249017.878439	38.428813
2297.045420	249420.091410	38.433831
2299.187068	249821.322158	38.438848
2301.526439	250219.699629	38.443866
2303.971516	250636.628940	38.448884
2305.829245	251062.118167	38.453901
2308.327013	251467.226518	38.458919
2310.782292	251876.381443	38.463936
2313.078418	252303.523802	38.468954
2315.409456	252720.346705	38.473972
2318.084964	253140.565712	38.478989
2320.332120	253559.283112	38.484007
2323.315363	253976.071170	38.489024
2325.826888	254391.568221	38.494042
2329.020328	254799.454838	38.499060
2331.375041	255208.424849	38.504077
2333.447411	255594.961356	38.509095
2336.195454	255991.213424	38.514112
2338.575519	256396.140120	38.519130
2341.204070	256789.542093	38.524148
2343.420335	257174.555283	38.529165
2346.009025	257565.728567	38.534183
2348.780698	257961.443111	38.539200
2351.095957	258344.610248	38.544218
2353.650848	258732.359738	38.549236
2356.072155	259123.561421	38.554253
2358.657354	259490.500356	38.559271
2361.232540	259872.835235	38.564288
2363.274527	260248.681738	38.569306
2365.932264	260615.633353	38.574324
2368.186647	260998.988023	38.579341
2370.615033	261363.793900	38.584359
2372.904849	261695.827876	38.589376
2375.597033	262039.300540	38.594394
2377.928234	262367.211853	38.599412
2379.647239	262714.178387	38.604429
2381.583702	263060.701116	38.609447
2383.922545	263408.145586	38.614464
2385.951714	263783.890992	38.619482
2388.365016	264138.079515	38.624500
2390.553155	264510.113817	38.629517
2392.579129	264884.766682	38.634535
2394.793651	265256.389480	38.639552
2396.712547	265634.591088	38.644570
2399.155434	266018.215238	38.649588
2401.501857	266418.392839	38.654605
2403.688183	266817.886147	38.659623
2406.321204	267218.140988	38.664640
2407.965889	267626.109018	38.669658
2410.906771	268026.437390	38.674676
2413.254706	268437.942295	38.679693
2415.537555	268851.693281	38.684711
2418.620041	269265.078430	38.689728
2420.749470	269688.939469	38.694746
2422.972666	270092.766621	38.699764
2425.476491	270517.197585	38.704781
2428.028828	270937.758455	38.709799
2430.590889	271358.698082	38.714816
2432.736083	271787.405292	38.719834
2435.417725	272214.165736	38.724852
2437.928059	272650.074238	38.729869
2440.123687	273083.266937	38.734887
2442.441069	273504.524377	38.739904
2445.180430	273939.070549	38.744922
2447.780954	274369.803918	38.749940
2450.641223	274801.889201	38.754957
2452.815077	275240.517735	38.759975
2455.258341	275668.760692	38.764992
2458.114571	276119.311389	38.770010
2460.261867	276547.526962	38.775028
2462.967568	276984.028820	38.780045
2465.608488	277410.811888	38.785063
2468.063439	277840.750244	38.790080
2470.568906	278287.266352	38.795098
2473.019417	278715.476177	38.800116
2475.366963	279161.051928	38.805133
2477.683517	279597.157098	38.810151
2480.416991	280032.986719	38.815168
2482.864134	280485.959370	38.820186
2485.743273	280908.070509	38.825204
2487.699508	281349.592546	38.830221
2490.438236	281795.856685	38.835239
2492.722472	282240.647817	38.840256
2495.572398	282682.369082	38.845274
2498.262823	283120.611026	38.850292
2501.213025	283541.179055	38.855309
2503.908611	283948.276169	38.860327
2506.916263	284338.935300	38.865344
2509.378789	284733.623695	38.870362
2511.848969	285117.260412	38.875380
2514.352105	285509.298075	38.880397
2516.425903	285900.011010	38.885415
2518.622065	286286.028248	38.890432
2520.674879	286693.405247	38.895450
2522.952456	287096.678553	38.900468
2524.873214	287507.047508	38.905485
2527.128616	287934.299900	38.910503
2529.529098	288365.361507	38.915520
2531.724829	288804.610068	38.920538
2534.142176	289245.521022	38.925556
2536.624082	289684.031806	38.930573
2539.173120	290130.174877	38.935591
2542.262753	290566.826049	38.940608
2544.825031	291018.627702	38.945626
2547.646130	291457.861474	38.950644
2550.109380	291910.718016	38.955661
2552.488361	292363.079207	38.960679
2555.090046	292811.616069	38.965696
2557.655589	293268.996193	38.970714
2560.113535	293729.161316	38.975732
2562.993288	294186.814130	38.980749
2565.442925	294647.230800	38.985767
2568.099318	295098.060279	38.990784
2570.754578	295567.352749	38.995802
2573.189781	296029.746972	39.000820
2576.103013	296492.260613	39.005837
2578.553403	296953.149599	39.010855
2581.335166	297424.240657	39.015872
2584.531795	297886.750285	39.020890
2587.498519	298339.468099	39.025908
2590.660053	298784.404227	39.030925
2593.300862	299236.335452	39.035943
2596.003612	299680.482339	39.040960
2598.337648	300135.128469	39.045978
2600.825726	300574.431552	39.050996
2603.759171	301021.834300	39.056013
2606.718776	301465.801810	39.061031
2609.507087	301901.491665	39.066048
2612.462615	302339.487333	39.071066
2615.275211	302781.619531	39.076084
2617.782897	303205.389194	39.081101
2620.331194	303640.578221	39.086119
2622.834935	304064.293594	39.091136
2625.804816	304502.301398	39.096154
2628.716881	304931.123496	39.101172
2631.323405	305360.325785	39.106189
2633.537556	305794.773658	39.111207
2636.369253	306228.783570	39.116224
2638.614784	306666.015012	39.121242
2640.648149	307099.953590	39.126260
2643.165698	307540.663779	39.131277
2645.807985	307982.467608	39.136295
2648.769750	308393.410393	39.141312
2650.974867	308803.693117	39.146330
2653.189339	309224.637827	39.151348
2655.710901	309641.591627	39.156365
2657.863133	310069.779797	39.161383
2660.556208	310500.463341	39.166400
2662.633174	310937.318909	39.171418
2664.849267	311379.557059	39.176436
2667.588518	311828.762636	39.181453
2669.856717	312295.694527	39.186471
2672.350700	312750.954671	39.191488
2674.898934	313230.046961	39.196506
2677.299546	313705.377728	39.201524
2680.428157	314184.923105	39.206541
2682.820245	314673.300821	39.211559
2685.825822	315157.456704	39.216576
2688.175229	315650.837230	39.221594
2690.959580	316138.147343	39.226612
2694.153483	316627.263010	39.231629
2696.336914	317125.028721	39.236647
2699.908056	317609.273768	39.241664
2702.693122	318093.548082	39.246682
2705.825295	318593.578309	39.251700
2709.192409	319071.093476	39.256717
2711.499619	319552.620313	39.261735
2714.113805	320043.130206	39.266752
2716.956379	320546.648051	39.271770
2719.486311	321032.543696	39.276788
2722.149951	321523.693909	39.281805
2725.296166	322029.940984	39.286823
2728.366622	322501.793835	39.291840
2731.886511	322979.685160	39.296858
2735.594625	323459.394024	39.301876
2738.281449	323907.562620	39.306893
2741.304603	324378.520477	39.311911
2744.048761	324828.957443	39.316928
2747.063083	325289.957264	39.321946
2749.935128	325746.484080	39.326964
2752.885346	326197.307057	39.331981
2755.305707	326653.954793	39.336999
2757.904347	327103.155254	39.342016
2760.804320	327569.538893	39.347034
2762.885594	328034.840058	39.352052
2765.795824	328492.633502	39.357069
2768.455599	328966.840630	39.362087
2771.254934	329430.205173	39.367104
2774.064404	329895.798165	39.372122
2776.915646	330358.486083	39.377140
2779.765175	330821.576600	39.382157
2782.167219	331300.453539	39.387175
2784.836944	331779.788250	39.392192
2787.117035	332251.595064	39.397210
2789.284299	332737.455047	39.402228
2792.410872	333223.603626	39.407245
2794.624200	333714.371533	39.412263
2797.652840	334182.377973	39.417280
2800.173344	334643.207172	39.422298
2802.413771	335105.247831	39.427316
2804.909115	335576.912062	39.432333
2807.516490	336069.748139	39.437351
2809.793012	336547.152178	39.442368
2812.639882	337041.613269	39.447386
2814.992317	337547.627073	39.452404
2817.810245	338049.596568	39.457421
2819.900543	338564.198856	39.462439
2822.672926	339105.635021	39.467456
2825.374361	339631.721400	39.472474
2827.982413	340171.574877	39.477492
2830.617300	340718.194582	39.482509
2833.583950	341273.558616	39.487527
2836.615002	341823.549925	39.492544
2839.902282	342370.267823	39.497562
2842.375943	342932.473386	39.502580
2845.529969	343476.917077	39.507597
2848.272478	344052.641488	39.512615
2851.596825	344622.396791	39.517632
2854.318259	345182.045816	39.522650
2857.007959	345760.169010	39.527668
2859.908522	346322.844306	39.532685
2862.660961	346899.165858	39.537703
2866.074820	347471.154365	39.542720
2869.275311	348041.141854	39.547738
2871.797752	348613.547205	39.552756
2875.388437	349188.173407	39.557773
2878.314442	349770.087148	39.562791
2881.336472	350337.994623	39.567808
2884.938206	350904.805979	39.572826
2887.795647	351462.069105	39.577844
2891.133382	352012.975334	39.582861
2893.941419	352575.992510	39.587879
2897.079421	353126.664706	39.592896
2900.528827	353685.675275	39.597914
2903.026755	354243.927515	39.602932
2906.256422	354789.030793	39.607949
2909.119516	355337.513390	39.612967
2911.954841	355890.509755	39.617984
2915.401754	356435.782504	39.623002
2917.452085	356990.293597	39.628020
2920.678400	357539.953199	39.633037
2923.984102	358084.796594	39.638055
2927.445333	358623.212562	39.643072
2930.782731	359146.369377	39.648090
2933.710169	359685.674031	39.653108
2937.494099	360204.605233	39.658125
2939.942596	360730.429921	39.663143
2943.304443	361251.829473	39.668160
2945.898510	361784.591595	39.673178
2948.587733	362315.731915	39.678196
2951.589623	362834.913846	39.683213
2954.521390	363346.338182	39.688231
2957.193291	363838.546168	39.693248
2960.232100	364311.938777	39.698266
2962.663391	364821.374010	39.703284
2965.708511	365303.377798	39.708301
2968.337324	365799.321781	39.713319
2970.870781	366292.764243	39.718336
2973.590274	366807.424605	39.723354
2976.092651	367317.574537	39.728372
2979.363116	367832.506925	39.733389
2982.031903	368361.891091	39.738407
2984.749012	368896.205284	39.743424
2987.771243	369420.998841	39.748442
2989.945703	369971.724019	39.753460
2992.691151	370509.737863	39.758477
2996.179408	371073.105978	39.763495
2998.961914	371631.107529	39.768512
3001.496041	372193.124491	39.773530
3004.675749	372763.898625	39.778548
3007.700113	373335.070408	39.783565
3010.660075	373915.272137	39.788583
3013.637346	374495.309041	39.793600
3017.117308	375078.115945	39.798618
3020.044361	375670.948185	39.803636
3022.821104	376251.649011	39.808653
3026.057141	376848.947175	39.813671
3029.122856	377445.934237	39.818688
3032.280548	378042.311778	39.823706
3035.080152	378651.545095	39.828724
3038.601915	379250.323845	39.833741
3041.684665	379844.932332	39.838759
3044.718724	380438.067803	39.843776
3048.358928	381031.621466	39.848794
3051.185699	381635.698682	39.853812
3054.897805	382226.733547	39.858829
3058.144470	382825.823526	39.863847
3061.239139	383413.189805	39.868864
3064.749506	383995.200944	39.873882
3067.511289	384590.208288	39.878900
3070.874835	385171.589191	39.883917
3074.350734	385761.813167	39.888935
3077.027088	386345.064421	39.893952
3080.332868	386924.952448	39.898970
3083.006638	387518.449145	39.903988
3086.351042	388116.180031	39.909005
3089.109609	388711.287096	39.914023
3092.359487	389294.891933	39.919040
3095.478590	389884.921013	39.924058
3098.906452	390477.446022	39.929076
3102.029388	391064.790077	39.934093
3105.100831	391658.290699	39.939111
3108.049536	392257.224610	39.944128
3111.312160	392848.261178	39.949146
3113.678599	393449.830539	39.954164
3116.631471	394052.934925	39.959181
3119.651991	394637.286300	39.964199
3122.515450	395214.404684	39.969216
3125.891894	395778.676584	39.974234
3129.061411	396362.866722	39.979252
3132.008376	396906.485363	39.984269
3135.781853	397458.568709	39.989287
3138.945038	398017.562446	39.994304
3142.040104	398563.861354	39.999322
3145.283798	399132.170230	40.004340
3148.038303	399702.375769	40.009357
3151.172925	400268.298652	40.014375
3154.443327	400843.055466	40.019392
3157.743044	401398.031937	40.024410
3160.297275	401990.598820	40.029428
3163.430919	402579.659017	40.034445
3166.548653	403174.232774	40.039463
3168.904057	403772.546995	40.044480
3172.318194	404363.421518	40.049498
3175.323851	404975.659574	40.054516
3178.448668	405587.812904	40.059533
3181.734579	406203.142318	40.064551
3184.965165	406828.625739	40.069568
3188.488803	407440.998447	40.074586
3191.210058	408072.822420	40.079604
3194.551324	408698.294118	40.084621
3197.763672	409329.548543	40.089639
3200.619023	409974.273832	40.094656
3203.944773	410606.820955	40.099674
3206.667841	411270.610181	40.104692
3209.808517	411926.814165	40.109709
3213.185072	412593.041696	40.114727
3216.133198	413260.819612	40.119744
3219.688480	413920.904083	40.124762
3222.577426	414587.518135	40.129780
3226.088535	415254.287183	40.134797
3229.679603	415929.736691	40.139815
3232.739230	416599.409309	40.144832
3236.275603	417266.931654	40.149850
3239.699840	417943.875330	40.154868
3242.951685	418613.588270	40.159885
3246.385767	419282.340609	40.164903
3249.884645	419953.494660	40.169920
3253.571400	420624.598464	40.174938
3257.211138	421283.184608	40.179956
3260.663909	421936.772076	40.184973
3264.289558	422594.515274	40.189991
3267.506728	423244.057260	40.195008
3271.034294	423877.984823	40.200026
3274.563152	424533.160493	40.205044
3277.780748	425184.979358	40.210061
3281.378859	425821.628402	40.215079
3284.773716	426461.332825	40.220096
3288.109085	427096.322087	40.225114
3291.139426	427731.143972	40.230132
3294.584914	428363.397418	40.235149
3297.719730	428978.981942	40.240167
3301.010931	429586.019467	40.245184
3304.385373	430160.377963	40.250202
3307.922696	430753.119257	40.255220
3310.709288	431338.279988	40.260237
3314.237386	431916.263829	40.265255
3316.938545	432519.478780	40.270272
3320.480372	433102.238820	40.275290
3323.609914	433710.005677	40.280308
3326.640974	434298.592133	40.285325
3329.836093	434897.611285	40.290343
3332.893232	435518.753435	40.295360
3335.796226	436133.477944	40.300378
3338.935249	436765.401398	40.305396
3341.868846	437399.315659	40.310413
3344.924903	438040.022221	40.315431
3347.886496	438695.451044	40.320448
3351.329640	439357.204275	40.325466
3354.501682	440032.290958	40.330484
3357.484771	440713.663041	40.335501
3360.740441	441390.414019	40.340519
3363.768050	442085.851467	40.345536
3367.557101	442775.167036	40.350554
3371.083886	443477.102112	40.355572
3374.533023	444181.304093	40.360589
3378.385549	444880.254461	40.365607
3381.842382	445578.895557	40.370624
3385.529226	446273.073906	40.375642
3389.080912	446972.057868	40.380660
3392.779235	447669.274092	40.385677
3397.310830	448344.829725	40.390695
3400.577109	449037.674311	40.395712
3404.565090	449712.621351	40.400730
3407.736644	450407.662076	40.405748
3411.541390	451084.871797	40.410765
3415.403038	451751.177389	40.415783
3418.469081	452421.895611	40.420800
3421.823880	453087.385014	40.425818
3425.331492	453769.765731	40.430836
3428.611906	454450.544513	40.435853
3432.276815	455121.021676	40.440871
3435.219693	455798.223258	40.445888
3438.893475	456474.367375	40.450906
3442.606399	457159.683290	40.455924
3445.704000	457838.407829	40.460941
3449.238355	458524.364886	40.465959
3452.376547	459218.605766	40.470976
3456.186431	459899.413460	40.475994
3459.564513	460583.253801	40.481012
3462.906649	461272.838788	40.486029
3466.352615	461960.815079	40.491047
3469.684634	462666.274128	40.496064
3473.043338	463352.245385	40.501082
3476.599137	464050.591220	40.506100
3480.009476	464748.077693	40.511117
3483.178413	465432.621636	40.516122
3486.417266	466079.083076	40.521127
3489.943888	466674.458743	40.526132
3492.762579	467228.548536	40.531136
3495.315432	467723.955619	40.536141
3498.231052	468149.280799	40.541146
3500.421561	468549.797854	40.546151
3502.878362	468878.534332	40.551156
3504.825996	469159.129721	40.556160
3506.649903	469408.843712	40.561165
3508.799919	469608.757963	40.566170
3510.052020	469764.857396	40.571175
3511.446988	469876.864082	40.576180
3512.940015	469958.158493	40.581184
3514.136853	470013.265673	40.586189
3515.384491	470026.019449	40.591194
3515.941198	470014.578494	40.596199
3516.802206	469962.868229	40.601204
3517.692473	469899.148356	40.606208
3518.184954	469816.906911	40.611213
3518.506544	469710.887724	40.616218
3518.744817	469600.526049	40.621223
3519.284563	469466.913219	40.626228
3519.642198	469318.033241	40.631232
3519.691487	469167.887748	40.636237
3519.652799	469004.788623	40.641242
3519.788260	468835.073263	40.646247
3520.030577	468639.909274	40.651252
3520.009886	468457.705385	40.656256
3519.864606	468259.260406	40.661261
3520.497206	468062.656151	40.666266
3519.930971	467868.382175	40.671271
3519.892668	467650.510884	40.676276
3520.099428	467448.501986	40.681280
3519.565660	467235.725745	40.686285
3519.762529	467021.606559	40.691290
3519.636826	466813.416624	40.696295
3519.261636	466604.557783	40.701300
3519.194013	466385.410613	40.706304
3518.570566	466170.104818	40.711309
3518.489654	465956.730470	40.716314
3518.127063	465763.717630	40.721319
3517.780631	465551.448054	40.726324
3517.968044	465349.369754	40.731328
3517.482190	465147.910947	40.736333
3517.690833	464955.451137	40.741338
3516.902381	464746.642750	40.746343
3516.590169	464554.673220	40.751348
3516.136812	464367.640534	40.756352
3516.260151	464191.806291	40.761357
3516.382319	464006.647870	40.766362
3515.725231	463824.711483	40.771367
3515.448291	463642.961828	40.776372
3515.218359	463464.090571	40.781376
3515.093532	463298.981751	40.786381
3515.077960	463126.657796	40.791386
3514.731202	462960.925309	40.796391
3514.751630	462794.774030	40.801396
3514.370117	462632.084923	40.806400
3513.895904	462475.034810	40.811405
3513.885136	462309.796830	40.816410
3513.731965	462160.543501	40.821415
3513.403411	462018.159772	40.826420
3513.356288	461865.896421	40.831424
3512.931125	461723.324361	40.836429
3512.675850	461567.192400	40.841434
3512.245658	461431.916094	40.846439
3512.138307	461282.445586	40.851444
3511.760233	461157.648094	40.856448
3511.571380	461040.266730	40.861453
3511.802759	460913.894060	40.866458
3511.390334	460793.812939	40.871463
3510.968277	460677.229374	40.876468
3511.208953	460559.619788	40.881472
3510.850833	460449.966611	40.886477
3510.849421	460332.903781	40.891482
3510.660956	460237.460640	40.896487
3510.684490	460111.979853	40.901492
3510.360831	460010.832161	40.906496
3510.063856	459912.669392	40.911501
3510.222497	459805.103563	40.916506
3510.336897	459712.342804	40.921511
3509.692268	459610.487703	40.926516
3509.954504	459513.089014	40.931520
3509.939382	459424.960812	40.936525
3509.685480	459319.642003	40.941530
3509.402907	459236.221138	40.946535
3509.338058	459149.012439	40.951540
3509.241788	459064.038647	40.956544
3508.981628	458979.954041	40.961549
3509.240225	458892.638314	40.966554
3509.092256	458808.635192	40.971559
3508.583857	458726.264367	40.976564
3508.697250	458649.716722	40.981568
3508.684759	458576.535243	40.986573
3508.677626	458483.485436	40.991578
3508.340552	458420.951246	40.996583
3508.211092	458349.055950	41.001588
3508.298967	458274.285092	41.006592
3507.614055	458209.326213	41.011597
3507.892738	458141.516423	41.016602
3507.656842	458074.858602	41.021607
3507.629874	458008.925125	41.026612
3508.042944	457945.754538	41.031616
3507.711460	457891.073584	41.036621
3507.928943	457819.370563	41.041626
3507.785757	457767.292646	41.046631
3507.720985	457706.737065	41.051636
3507.647448	457640.202128	41.056640
3507.332283	457584.301144	41.061645
3507.470955	457512.863907	41.066650
3507.343006	457468.385208	41.071655
3507.246349	457410.114961	41.076660
3507.149885	457352.858200	41.081664
3506.966996	457294.348921	41.086669
3507.481122	457243.880686	41.091674
3507.082887	457196.659882	41.096679
3507.218902	457128.921724	41.101684
3506.998336	457073.966183	41.106688
3506.845004	457031.062089	41.111693
3506.670463	456981.775178	41.116698
3506.526316	456943.887175	41.121703
3506.738363	456891.188796	41.126708
3506.727272	456831.229642	41.131712
3506.931427	456792.775026	41.136717
3506.962311	456747.558014	41.141722
3506.462198	456703.242545	41.146727
3506.474103	456642.062439	41.151732
3506.671231	456614.252774	41.156736
3506.560188	456575.496762	41.161741
3506.639518	456527.381864	41.166746
3506.477123	456492.334570	41.171751
3506.306023	456444.363609	41.176756
3506.494436	456394.506423	41.181760
3506.500737	456355.527205	41.186765
3506.386415	456313.577977	41.191770
3505.981099	456278.723853	41.196775
3506.254747	456229.307890	41.201780
3506.152457	456190.346895	41.206784
3506.005140	456158.895247	41.211789
3506.127130	456113.711949	41.216794
3506.212633	456083.335554	41.221799
3505.970016	456046.780560	41.226804
3506.141786	456005.491470	41.231808
3505.858768	455973.353076	41.236813
3505.999018	455931.511651	41.241818
3506.039755	455917.717601	41.246823
3505.580494	455866.347691	41.251828
3505.712928	455842.552374	41.256832
3505.417921	455806.056579	41.261837
3505.843315	455765.331953	41.266842
3505.564393	455743.634294	41.271847
3505.544963	455711.653230	41.276852
3505.516624	455694.474694	41.281856
3505.413497	455659.719971	41.286861
3505.720074	455632.549224	41.291866
3505.743289	455608.417461	41.296871
3505.493847	455574.042396	41.301876
3505.714988	455546.734056	41.306880
3505.304346	455516.036018	41.311885
3505.272495	455479.697457	41.316890
3505.639040	455465.137821	41.321895
3505.622519	455439.846794	41.326900
3505.675517	455404.862220	41.331904
3505.619139	455381.858942	41.336909
3505.858680	455351.151014	41.341914
3505.626522	455328.127001	41.346919
3505.250535	455292.252383	41.351924
3505.603307	455253.516025	41.356928
3505.128437	455237.224382	41.361933
3505.602972	455212.457500	41.366938
3505.470705	455189.213514	41.371943
3505.342374	455153.803262	41.376948
3505.532708	455125.840650	41.381952
3505.512094	455105.770970	41.386957
3505.593806	455066.776402	41.391962
3505.193697	455051.130815	41.396967
3505.486203	455012.961882	41.401972
3505.898943	454981.615541	41.406976
3505.229415	454960.287882	41.411981
3505.431094	454930.802355	41.416986
3505.337940	454907.703440	41.421991
3505.063173	454881.999601	41.426996
3505.464598	454855.065076	41.432000
3505.027480	454836.739040	41.437005
3505.401586	454810.721553	41.442010
3505.428253	454799.311612	41.447015
3505.132088	454768.491515	41.452020
3505.188623	454740.551221	41.457024
3505.276162	454718.840585	41.462029
3505.410692	454693.826985	41.467034
3505.553740	454674.185154	41.472039
3505.486234	454641.602326	41.477044
3505.754708	454614.386038	41.482048
3505.074837	454590.778652	41.487053
3505.203781	454554.968591	41.492058
3505.224350	454527.338295	41.497063
3505.258253	454503.659622	41.502068
3504.919750	454474.316363	41.507072
3504.820271	454458.517604	41.512077
3505.412316	454435.554615	41.517082
3505.238411	454426.763988	41.522087
3504.924658	454393.867970	41.527092
3504.938102	454374.095906	41.532096
3504.921455	454355.849716	41.537101
3505.418214	454317.644609	41.542106
3505.143837	454306.691332	41.547111
3504.953394	454292.276660	41.552116
3505.146140	454268.165056	41.557120
3505.043677	454247.094666	41.562125
3505.002214	454210.958254	41.567130
3505.057369	454207.958026	41.572135
3504.670759	454183.286248	41.577140
3504.774426	454158.682802	41.582144
3504.403822	454156.110111	41.587149
3505.013079	454142.319169	41.592154
3504.767857	454123.097954	41.597159
3505.015580	454101.207233	41.602164
3505.365313	454082.087160	41.607168
3505.104011	454066.011574	41.612173
3505.259620	454038.763100	41.617178
3504.921992	454020.824883	41.622183
3505.101842	453994.383295	41.627188
3504.988677	453972.554058	41.632192
3504.909898	453954.115349	41.637197
3505.373422	453927.422465	41.642202
3505.070432	453906.943587	41.647207
3505.063913	453880.533674	41.652212
3504.639186	453863.674745	41.657216
3504.746313	453842.314686	41.662221
3505.224337	453813.236600	41.667226
3505.130700	453798.703664	41.672231
3504.766712	453776.967741	41.677236
3504.894072	453750.737574	41.682240
3504.911115	453746.729919	41.687245
3505.052249	453714.971777	41.692250
3504.854298	453695.285847	41.697255
3504.712301	453677.972940	41.702260
3505.047588	453663.113201	41.707264
3504.981894	453648.676774	41.712269
3505.347713	453633.254171	41.717274
3505.228750	453624.453817	41.722279
3505.180672	453588.875069	41.727284
3505.434454	453560.088384	41.732288
3505.197044	453542.740961	41.737293
3505.035924	453503.480714	41.742298
3504.776117	453495.261988	41.747303
3504.666437	453467.500420	41.752308
3505.051032	453460.185529	41.757312
3504.489558	453432.805223	41.762317
3504.961139	453416.097045	41.767322
3504.925712	453385.179648	41.772327
3505.066754	453370.859808	41.777332
3505.143488	453349.200260	41.782336
3504.836052	453337.745164	41.787341
3504.841989	453323.144195	41.792346
3504.726993	453302.784696	41.797351
3504.785777	453281.229530	41.802356
3504.641801	453257.123539	41.807360
3504.310012	453244.050323	41.812365
3504.400482	453230.955692	41.817370
3504.346350	453225.439249	41.822375
3504.418318	453197.291437	41.827380
3504.955111	453199.937325	41.832384
3504.405686	453183.352601	41.837389
3504.420345	453176.100776	41.842394
3504.703232	453165.558682	41.847399
3504.626459	453136.574373	41.852404
3504.749467	453133.258233	41.857408
3504.493090	453117.231755	41.862413
3504.680563	453096.212066	41.867418
3504.916022	453076.907792	41.872423
3504.457652	453054.883048	41.877428
3505.032405	453045.710519	41.882432
3504.780076	453036.932685	41.887437
3504.562916	453025.462000	41.892442
3504.425877	452999.985755	41.897447
3504.326008	452990.979088	41.902452
3504.595738	452980.134975	41.907456
3504.534290	452959.918078	41.912461
3504.675268	452947.980636	41.917466
3504.460508	452937.117836	41.922471
3504.372639	452920.048524	41.927476
3504.783557	452912.019210	41.932480
3504.227447	452899.034772	41.937485
3504.467671	452894.380496	41.942490
3504.523086	452884.130577	41.947495
3504.528044	452861.874426	41.952500
3504.693718	452854.951571	41.957504
3504.581108	452834.895375	41.962509
3504.711130	452812.465729	41.967514
3504.572805	452799.055021	41.972519
3504.282038	452788.458599	41.977524
3504.588845	452782.474840	41.982528
3504.434283	452762.983390	41.987533
3504.594437	452751.042559	41.992538
3504.571441	452741.110133	41.997543
3504.575502	452716.623360	42.002548
3504.656238	452699.018117	42.007552
3504.461791	452691.649739	42.012557
3504.730403	452668.790705	42.017562
3504.959371	452664.543869	42.022567
3504.747616	452647.495485	42.027572
3505.006088	452621.393580	42.032576
3504.654946	452615.775600	42.037581
3504.646485	452595.245121	42.042586
3504.918600	452571.320761	42.047591
3504.461018	452550.714837	42.052596
3504.681069	452530.601543	42.057600
3504.231895	452519.778549	42.062605
3504.451522	452511.731046	42.067610
3504.453535	452488.714549	42.072615
3504.130866	452491.203106	42.077620
3504.334401	452483.056947	42.082624
3504.081077	452469.260088	42.087629
3504.310469	452463.390850	42.092634
3504.437603	452468.185342	42.097639
3504.462543	452457.433449	42.102644
3504.381664	452430.426013	42.107648
3504.643877	452429.012462	42.112653
3504.923617	452412.792500	42.117658
3504.704504	452395.795861	42.122663
3504.558128	452379.243059	42.127668
3504.705291	452361.524793	42.132672
3504.442917	452361.113353	42.137677
3504.733250	452328.516449	42.142682
3504.573884	452330.013900	42.147687
3504.529736	452310.351079	42.152692
3504.726999	452287.554503	42.157696
3504.708240	452281.322010	42.162701
3504.809441	452250.987945	42.167706
3504.554728	452247.127795	42.172711
3504.582200	452215.893721	42.177716
3504.720503	452210.293450	42.182720
3504.925697	452199.307856	42.187725
3505.211781	452173.149974	42.192730
3504.641782	452149.875890	42.197735
3504.129860	452139.468988	42.202740
3504.323452	452128.434640	42.207744
3504.254588	452107.052136	42.212749
3504.586136	452098.833270	42.217754
3504.285882	452094.778078	42.222759
3504.224179	452072.988735	42.227764
3504.735532	452061.950791	42.232768
3504.400904	452055.467980	42.237773
3504.632010	452035.250921	42.242778
3504.192255	452034.312089	42.247783
3504.193830	452023.056984	42.252788
3504.410667	452002.588842	42.257792
3504.119684	451994.932512	42.262797
3504.424636	451983.270700	42.267802
3504.378272	451968.272120	42.272807
3504.072383	451964.268562	42.277812
3504.557839	451954.603822	42.282816
3504.720134	451939.417499	42.287821
3504.685555	451921.577796	42.292826
3504.502529	451924.650949	42.297831
3504.383252	451897.395885	42.302836
3504.560736	451894.120942	42.307840
3504.078446	451873.417164	42.312845
3504.390594	451861.297773	42.317850
3504.419166	451858.098950	42.322855
3504.538530	451849.206445	42.327860
3504.648036	451826.525743	42.332864
3504.180918	451815.147762	42.337869
3504.305633	451809.245515	42.342874
3504.193734	451792.027279	42.347879
3504.233074	451779.041855	42.352884
3504.634996	451772.889471	42.357888
3504.442954	451760.247734	42.362893
3504.540985	451743.855483	42.367898
3504.294369	451749.271642	42.372903
3504.263224	451722.964566	42.377908
3503.997750	451709.625559	42.382912
3504.135346	451710.970951	42.387917
3504.520102	451704.061002	42.392922
3504.439913	451680.905548	42.397927
3504.131821	451676.648816	42.402932
3504.605805	451670.332003	42.407936
3504.490766	451649.058306	42.412941
3504.385474	451630.317852	42.417946
3504.783894	451622.290175	42.422951
3504.945273	451615.671832	42.427956
3505.010446	451585.089452	42.432960
3504.708752	451567.548547	42.437965
3504.616984	451543.330242	42.442970
3504.702685	451529.626963	42.447975
3504.374909	451519.289701	42.452980
3504.836708	451484.431444	42.457984
3504.506967	451486.211541	42.462989
3504.610717	451467.029655	42.467994
3504.384859	451460.578781	42.472999
3504.393614	451446.280198	42.478004
3504.451725	451426.396280	42.483008
3504.281796	451421.051224	42.488013
3504.606354	451404.163734	42.493018
3504.176558	451393.032643	42.498023
3504.343171	451381.749009	42.503028
3504.571555	451369.897131	42.508032
3504.273408	451360.365918	42.513037
3504.260543	451334.105927	42.518042
3504.497392	451330.972858	42.523047
3503.984692	451331.212531	42.528052
3504.303817	451311.131836	42.533056
3504.210056	451308.866405	42.538061
3504.557298	451300.695245	42.543066
3504.752848	451284.083183	42.548071
3504.478079	451278.299697	42.553076
3504.745522	451251.332646	42.558080
3504.493861	451242.199037	42.563085
3504.887028	451233.969309	42.568090
3504.606900	451213.128951	42.573095
3504.352009	451201.055299	42.578100
3504.323483	451169.474313	42.583104
3504.216617	451166.501309	42.588109
3504.550771	451165.430288	42.593114
3504.248837	451151.843649	42.598119
3504.439028	451128.337212	42.603124
3504.599350	451123.645485	42.608128
3504.009168	451103.212857	42.613133
3504.041257	451091.749237	42.618138
3504.129850	451089.655445	42.623143
3504.103965	451091.282292	42.628148
3504.293945	451082.783000	42.633152
3503.826855	451077.894195	42.638157
3504.203736	451058.107595	42.643162
3504.274200	451053.126996	42.648167
3504.161180	451053.602625	42.653172
3504.253971	451035.030610	42.658176
3504.218581	451030.169481	42.663181
3504.630264	451018.691705	42.668186
3504.674976	451000.178569	42.673191
3504.367650	450979.748222	42.678196
3504.653134	450977.671499	42.683200
3504.494069	450963.046337	42.688205
3504.323048	450946.952900	42.693210
3504.176119	450926.343011	42.698215
3504.401644	450913.274555	42.703220
3504.424487	450901.457507	42.708224
3504.317423	450906.292351	42.713229
3504.247208	450878.469867	42.718234
3504.258383	450871.927636	42.723239
3503.960346	450871.370152	42.728244
3504.109774	450864.905712	42.733248
3503.930980	450851.449951	42.738253
3504.328624	450829.580869	42.743258
3504.288254	450828.675184	42.748263
3504.162728	450833.411796	42.753268
3504.166348	450807.959534	42.758272
3504.092899	450806.907394	42.763277
3504.273015	450793.441012	42.768282
3504.298392	450797.695560	42.773287
3504.382952	450783.434278	42.778292
3504.247884	450758.563344	42.783296
3504.163687	450764.002725	42.788301
3504.198599	450756.746595	42.793306
3504.230627	450747.006619	42.798311
3504.310539	450733.912214	42.803316
3504.526323	450728.095512	42.808321
3504.125855	450713.004386	42.813325
3504.480777	450695.806933	42.818330
3504.401011	450703.020103	42.823335
3504.187571	450682.979039	42.828340
3504.535428	450658.532535	42.833345
3504.469992	450661.332290	42.838349
3504.518873	450641.398497	42.843354
3504.367157	450625.757824	42.848359
3504.170090	450619.098968	42.853364
3504.276969	450608.230724	42.858369
3504.254412	450594.697418	42.863373
3504.146939	450582.851740	42.868378
3504.252932	450581.160535	42.873383
3504.249385	450570.159023	42.878388
3504.498750	450542.839235	42.883393
3504.059483	450548.998416	42.888397
3504.234759	450535.684798	42.893402
3504.359935	450517.005390	42.898407
3504.226035	450511.907453	42.903412
3504.270787	450500.187839	42.908417
3504.145884	450495.493973	42.913421
3504.157201	450471.763832	42.918426
3503.717650	450465.298436	42.923431
3504.211291	450466.076100	42.928436
3504.458272	450459.341372	42.933441
3504.232869	450451.876078	42.938445
3504.344144	450435.328431	42.943450
3504.566742	450431.589244	42.948455
3504.322690	450417.130315	42.953460
3504.597162	450400.402670	42.958465
3504.356511	450398.415729	42.963469
3504.288271	450378.045369	42.968474
3504.448570	450369.145242	42.973479
3504.097258	450362.157730	42.978484
3504.610464	450338.189634	42.983489
3504.206186	450322.997472	42.988493
3504.267149	450316.091653	42.993498
3504.347683	450306.951612	42.998503
3504.137591	450297.506278	43.003508
3504.452909	450281.887003	43.008513
3504.404173	450285.495187	43.013517
3504.620057	450258.637061	43.018522
3504.621486	450249.561203	43.023527
3504.423444	450234.587271	43.028532
3504.662352	450207.116724	43.033537
3504.718310	450202.898930	43.038541
3504.502854	450187.218109	43.043546
3504.611660	450162.659737	43.048551
3504.497136	450157.254193	43.053556
3504.442859	450138.250173	43.058561
3504.095520	450139.931982	43.063565
3503.929154	450139.960420	43.068570
3504.099178	450115.999966	43.073575
3503.944317	450110.347786	43.078580
3504.276389	450092.190396	43.083585
3503.708652	450103.036256	43.088589
3504.348425	450097.501899	43.093594
3504.401431	450075.234556	43.098599
3504.145427	450069.092611	43.103604
3504.309487	450062.980342	43.108609
3504.081515	450061.041906	43.113613
3504.267348	450026.836765	43.118618
3504.420882	450028.838679	43.123623
3504.070336	450026.566251	43.128628
3504.358173	450016.680851	43.133633
3504.189324	449997.949780	43.138637
3504.168963	449993.491462	43.143642
3504.013456	449987.839359	43.148647
3503.966863	449972.535164	43.153652
3504.098076	449958.417460	43.158657
3503.951076	449957.175025	43.163661
3504.119736	449954.864638	43.168666
3504.240952	449956.872076	43.173671
3504.109876	449935.092340	43.178676
3504.338806	449912.946892	43.183681
3503.739987	449919.640528	43.188685
3504.143002	449913.132495	43.193690
3504.319134	449908.640609	43.198695
3504.103909	449898.486132	43.203700
3504.194554	449883.817574	43.208705
3504.198535	449880.014213	43.213709
3504.216565	449877.121103	43.218714
3504.183422	449857.758300	43.223719
3504.078353	449851.083490	43.228724
3503.990144	449835.837003	43.233729
3503.733514	449850.229780	43.238733
3504.323578	449832.535142	43.243738
3504.291307	449814.135506	43.248743
3503.807516	449811.378776	43.253748
3504.072809	449804.640711	43.258753
3504.063039	449810.574661	43.263757
3504.211078	449782.713449	43.268762
3504.357132	449772.547925	43.273767
3503.884865	449779.422809	43.278772
3504.188643	449772.475350	43.283777
3504.241879	449760.956686	43.288781
3504.303357	449740.867774	43.293786
3504.019018	449733.919317	43.298791
3503.893998	449737.236402	43.303796
3504.252190	449726.831820	43.308801
3504.524031	449712.132203	43.313805
3504.237738	449704.879851	43.318810
3504.469718	449687.905377	43.323815
3504.136021	449670.875369	43.328820
3504.367095	449652.988361	43.333825
3504.071216	449659.934572	43.338829
3504.439409	449643.190320	43.343834
3504.257966	449626.894830	43.348839
3504.440689	449620.576432	43.353844
3504.351125	449609.994731	43.358849
3504.106565	449594.673359	43.363853
3504.037316	449579.423448	43.368858
3504.251689	449581.617831	43.373863
3504.002009	449568.832492	43.378868
3504.338457	449550.572479	43.383873
3503.818568	449553.551388	43.388877
3504.117946	449552.942559	43.393882
3504.463872	449558.511624	43.398887
3504.548031	449534.413056	43.403892
3504.715679	449514.052281	43.408897
3504.560868	449505.712630	43.413901
3504.455693	449481.899850	43.418906
3504.581758	449477.213605	43.423911
3504.619176	449461.590469	43.428916
3504.489327	449434.688914	43.433921
3504.333054	449434.766332	43.438925
3504.382425	449405.603165	43.443930
3504.507298	449395.542483	43.448935
3504.327844	449407.894225	43.453940
3504.643773	449374.375662	43.458945
3503.885983	449363.096671	43.463949
3503.968924	449363.690988	43.468954
3503.683797	449358.263663	43.473959
3503.763172	449359.365630	43.478964
3504.170966	449349.205913	43.483969
3504.088219	449342.983465	43.488973
3504.275194	449327.283988	43.493978
3504.445356	449328.573271	43.498983
3503.794762	449319.709753	43.503988
3503.810843	449289.740842	43.508993
3503.803088	449289.032337	43.513997
3504.189608	449288.256509	43.519002
3504.123869	449289.231146	43.524007
3504.182736	449288.764786	43.529012
3504.239581	449270.146639	43.534017
3503.961367	449264.363179	43.539021
3504.510500	449256.460978	43.544026
3504.388011	449247.456549	43.549031
3504.170682	449234.614777	43.554036
3504.344281	449214.049877	43.559041
3504.022025	449214.611978	43.564045
3504.163086	449205.156894	43.569050
3504.220268	449188.313273	43.574055
3504.027741	449181.957409	43.579060
3504.074949	449175.002859	43.584065
3504.112057	449182.044482	43.589069
3504.162384	449151.106140	43.594074
3504.386319	449137.834031	43.599079
3504.650252	449141.642546	43.604084
3504.821694	449118.796213	43.609089
3504.507638	449112.156851	43.614093
3504.681385	449086.470627	43.619098
3504.417245	449061.974648	43.624103
3503.924649	449067.991251	43.629108
3504.099484	449043.268180	43.634113
3503.790651	449030.999661	43.639117
3504.120727	449024.351695	43.644122
3503.966936	449020.017364	43.649127
3503.907966	449025.097954	43.654132
3504.204844	449013.587982	43.659137
3503.875875	449001.474999	43.664141
3503.934336	448981.385876	43.669146
3504.115822	448974.002691	43.674151
3503.799679	448977.707464	43.679156
3504.111122	448982.319176	43.684161
3504.044274	448980.403831	43.689165
3504.214076	448975.710007	43.694170
3504.036194	448962.506398	43.699175
3503.988231	448962.007567	43.704180
3504.121019	448953.010129	43.709185
3503.930425	448960.699168	43.714189
3503.852481	448944.588294	43.719194
3504.093520	448928.575058	43.724199
3504.151304	448921.263682	43.729204
3504.282650	448917.387693	43.734209
3504.379054	448911.945810	43.739213
3504.095783	448893.588225	43.744218
3504.030040	448889.999411	43.749223
3503.939545	448892.905091	43.754228
3504.366113	448878.127767	43.759233
3503.873235	448863.355313	43.764237
3504.180469	448852.147717	43.769242
3503.970121	448844.070813	43.774247
3503.971532	448856.239879	43.779252
3504.034281	448849.891031	43.784257
3504.068215	448834.977898	43.789261
3504.022754	448811.103456	43.794266
3504.212482	448810.817563	43.799271
3503.856116	448814.427822	43.804276
3504.212670	448803.566717	43.809281
3504.493055	448776.898503	43.814285
3504.430946	448767.477915	43.819290
3504.209550	448773.853938	43.824295
3503.988355	448761.975941	43.829300
3504.171989	448737.301714	43.834305
3503.935768	448745.252150	43.839309
3504.508974	448738.410463	43.844314
3504.327188	448729.162409	43.849319
3503.678254	448709.954400	43.854324
3504.225632	448696.221139	43.859329
3504.329367	448708.068584	43.864333
3503.935783	448692.670588	43.869338
3504.373659	448677.079901	43.874343
3504.409406	448661.050810	43.879348
3504.251230	448658.136914	43.884353
3504.135783	448652.173374	43.889357
3504.227839	448624.269480	43.894362
3504.193560	448624.579599	43.899367
3504.426995	448618.455066	43.904372
3504.242765	448600.181725	43.909377
3504.188581	448587.565229	43.914381
3503.969141	448578.577069	43.919386
3504.021770	448573.852457	43.924391
3503.724105	448567.514359	43.929396
3504.240010	448545.977650	43.934401
3504.243555	448545.774251	43.939405
3504.427402	448534.486143	43.944410
3504.459514	448532.452447	43.949415
3504.254933	448516.616400	43.954420
3504.417623	448499.196444	43.959425
3504.452102	448505.326032	43.964429
3504.302201	448475.840660	43.969434
3504.195428	448463.588014	43.974439
3504.170190	448465.214953	43.979444
3504.237636	448442.284232	43.984449
3504.092254	448434.348197	43.989453
3504.179570	448422.113091	43.994458
3504.165305	448418.211168	43.999463
3504.205008	448408.265971	44.004468
3504.177175	448382.816135	44.009473
3504.245383	448383.210171	44.014477
3504.325020	448382.283887	44.019482
3504.389474	448371.066785	44.024487
3503.978797	448364.595804	44.029492
3504.014911	448350.949618	44.034497
3503.945076	448354.865975	44.039501
3504.241952	448346.296618	44.044506
3504.241257	448316.937666	44.049511
3504.168638	448323.440540	44.054516
3504.324505	448315.706554	44.059521
3504.312248	448303.539089	44.064525
3504.087102	448279.694725	44.069530
3504.315322	448272.658263	44.074535
3504.068645	448270.012958	44.079540
3504.417934	448252.205990	44.084545
3504.255977	448239.354154	44.089549
3504.180621	448230.746897	44.094554
3504.383693	448227.213482	44.099559
3504.423411	448207.126822	44.104564
3504.421463	448195.008241	44.109569
3504.145884	448189.477568	44.114573
3504.269203	448170.999219	44.119578
3504.258631	448157.259467	44.124583
3504.067362	448159.117608	44.129588
3504.463784	448149.212793	44.134593
3504.125087	448131.928854	44.139597
3504.103319	448127.318260	44.144602
3504.353044	448123.928983	44.149607
3504.009950	448110.043150	44.154612
3504.111268	448085.077974	44.159617
3503.885754	448082.682568	44.164621
3503.946909	448076.790124	44.169626
3504.172532	448084.459119	44.174631
3504.298865	448079.366861	44.179636
3504.404825	448051.611958	44.184641
3504.337829	448054.817984	44.189645
3503.628934	448051.389553	44.194650
3503.877520	448044.501658	44.199655
3503.761882	448027.078131	44.204660
3503.623743	448006.210333	44.209665
3503.575094	448009.362525	44.214669
3503.745060	448007.355948	44.219674
3503.857097	448008.908775	44.224679
3503.490527	448009.377057	44.229684
3503.546612	448008.556193	44.234689
3503.550025	448010.837471	44.239693
3503.470405	448010.648268	44.244698
3504.025247	448008.778801	44.249703
3503.755713	448016.938028	44.254708
3503.981100	448007.011644	44.259713
3503.629174	448016.300501	44.264717
3503.677825	448011.728564	44.269722
3503.968868	448008.078678	44.274727
3503.769209	447984.787410	44.279732
3504.198463	447966.915841	44.284737
3503.894628	447974.168207	44.289741
3503.815490	447971.291427	44.294746
3503.916696	447971.629128	44.299751
3503.994240	447976.483831	44.304756
3503.798313	447968.099883	44.309761
3503.453245	447962.428893	44.314765
3504.029339	447949.248028	44.319770
3503.976028	447937.594437	44.324775
3503.758594	447933.727116	44.329780
3503.764628	447927.793336	44.334785
3503.961908	447935.974299	44.339789
3503.815526	447939.346021	44.344794
3504.205461	447925.233485	44.349799
3503.872318	447912.917756	44.354804
3504.054201	447905.584839	44.359809
3503.784327	447907.405716	44.364813
3503.907021	447903.581727	44.369818
3503.950648	447907.275963	44.374823
3504.012602	447911.271313	44.379828
3504.067447	447894.376350	44.384833
3504.178345	447874.480050	44.389837
3503.909574	447867.122653	44.394842
3503.978768	447866.350254	44.399847
3503.874091	447863.325697	44.404852
3504.315692	447861.019185	44.409857
3504.267291	447840.947223	44.414861
3504.347992	447831.552539	44.419866
3504.470129	447829.554112	44.424871
3504.014700	447810.920732	44.429876
3504.310938	447790.587044	44.434881
3504.109001	447791.635713	44.439885
3503.983478	447788.209042	44.444890
3504.105613	447773.482930	44.449895
3504.198396	447771.895173	44.454900
3504.202809	447762.868440	44.459905
3504.057709	447770.499435	44.464909
3503.885474	447758.206849	44.469914
3504.154217	447740.362496	44.474919
3504.017085	447738.205498	44.479924
3504.041418	447726.741365	44.484929
3504.204913	447720.831348	44.489933
3503.876476	447713.788334	44.494938
3504.021348	447693.987480	44.499943
3503.983016	447690.647321	44.504948
3504.101371	447683.933672	44.509953
3503.719599	447682.629771	44.514957
3503.908653	447686.299213	44.519962
3503.913763	447685.030668	44.524967
3503.752491	447671.468456	44.529972
3503.923901	447645.730171	44.534977
3503.738141	447644.139258	44.539981
3503.725903	447647.285287	44.544986
3503.638910	447641.620852	44.549991
3503.948280	447648.717915	44.554996
3503.817141	447644.987930	44.560001
3503.781590	447652.448137	44.565005
3503.880368	447651.569262	44.570010
3503.656479	447646.384577	44.575015
3503.838224	447639.913630	44.580020
3504.089938	447623.390501	44.585025
3504.330782	447614.526167	44.590029
3503.882079	447617.036812	44.595034
3503.948675	447613.019517	44.600039
3503.980465	447604.292292	44.605044
3504.389289	447585.713974	44.610049
3504.279743	447587.456793	44.615053
3503.799615	447580.135386	44.620058
3504.479710	447579.106539	44.625063
3503.912798	447559.984889	44.630068
3504.366369	447546.723280	44.635073
3504.270743	447545.979012	44.640077
3504.094492	447534.549025	44.645082
3504.200904	447508.720255	44.650087
3503.940186	447501.564190	44.655092
3504.151552	447494.276805	44.660097
3504.144897	447497.776863	44.665101
3504.007018	447490.549110	44.670106
3503.811089	447467.155218	44.675111
3503.707286	447465.093919	44.680116
3503.906330	447466.682639	44.685121
3503.655430	447474.027554	44.690125
3504.041844	447463.617042	44.695130
3504.403270	447457.774572	44.700135
3503.855623	447453.202917	44.705140
3504.206198	447428.549367	44.710145
3503.869790	447421.507616	44.715149
3503.933763	447418.200654	44.720154
3503.873917	447422.977526	44.725159
3503.709757	447425.541024	44.730164
3503.825692	447416.292266	44.735169
3503.994870	447394.915011	44.740173
3503.652692	447385.845881	44.745178
3503.787500	447377.050263	44.750183
3503.699600	447378.637277	44.755188
3503.858280	447376.429732	44.760193
3503.619322	447379.715931	44.765197
3503.787878	447380.498522	44.770202
3504.004130	447376.252793	44.775207
3503.750587	447389.886085	44.780212
3503.962420	447374.383748	44.785217
3503.872810	447353.101348	44.790221
3503.915904	447344.219959	44.795226
3504.148270	447349.504750	44.800231
3503.901250	447353.907926	44.805236
3504.173434	447350.109021	44.810241
3503.986879	447337.970762	44.815245
3503.832617	447324.559258	44.820250
3503.957870	447317.185098	44.825255
3504.105025	447323.955006	44.830260
3504.324526	447311.848816	44.835265
3503.974572	447308.358971	44.840269
3503.944893	447284.074436	44.845274
3504.357290	447274.115777	44.850279
3503.852335	447279.932157	44.855284
3504.091095	447265.084360	44.860289
3504.424244	447270.098417	44.865293
3503.991856	447245.933310	44.870298
3504.099822	447241.249662	44.875303
3503.547246	447232.723483	44.880308
3503.928747	447233.672556	44.885313
3504.024922	447240.654032	44.890317
3503.807118	447217.111472	44.895322
3504.021289	447198.718181	44.900327
3503.769116	447200.485386	44.905332
3503.732334	447195.775734	44.910337
3503.784338	447187.754816	44.915341
3503.741699	447191.920290	44.920346
3503.543775	447187.542407	44.925351
3503.925336	447197.213470	44.930356
3503.884149	447191.997476	44.935361
3503.675360	447202.124305	44.940365
3503.713953	447176.560258	44.945370
3503.907705	447168.870094	44.950375
3503.601968	447173.131206	44.955380
3503.724648	447169.002831	44.960385
3503.654713	447173.071551	44.965389
3503.704334	447172.251759	44.970394
3504.181914	447169.939031	44.975399
3503.763459	447169.706257	44.980404
3503.653301	447166.175443	44.985409
3503.497900	447170.157338	44.990413
3503.640683	447171.147175	44.995418
3503.945441	447165.973523	45.000423
3503.757907	447156.624342	45.005428
3503.835051	447135.972472	45.010433
3503.947318	447132.606510	45.015437
3504.094367	447132.682851	45.020442
3503.920280	447137.884969	45.025447
3503.813221	447136.838382	45.030452
3504.270545	447124.742186	45.035457
3504.142804	447113.252979	45.040461
3503.994221	447100.702425	45.045466
3504.061234	447091.157622	45.050471
3503.646643	447095.843012	45.055476
3503.735204	447090.858386	45.060481
3503.866845	447090.126006	45.065485
3503.493507	447096.934152	45.070490
3503.965565	447087.320185	45.075495
3503.912171	447073.181365	45.080500
3504.016848	447056.835031	45.085505
3503.867563	447058.077583	45.090509
3503.826146	447057.780428	45.095514
3504.061332	447052.263661	45.100519
3503.708338	447060.234666	45.105524
3503.843192	447054.633612	45.110529
3503.925367	447032.560914	45.115533
3503.705817	447027.983852	45.120538
3503.988279	447023.625328	45.125543
3503.653138	447036.207875	45.130548
3503.735243	447022.400852	45.135553
3503.992337	447027.427953	45.140557
3504.073368	447023.408082	45.145562
3504.136658	447015.588011	45.150567
3504.001207	447002.071671	45.155572
3503.918583	446981.954030	45.160577
3504.118676	446988.157198	45.165581
3503.975285	446990.260814	45.170586
3503.747523	446984.417400	45.175591
3503.829286	446967.212843	45.180596
3503.856817	446955.798458	45.185601
3503.931146	446952.793915	45.190605
3503.631066	446953.707252	45.195610
3503.608031	446945.141247	45.200615
3503.622431	446952.643880	45.205620
3504.006430	446941.320749	45.210625
3503.998831	446949.841337	45.215629
3504.029934	446949.988187	45.220634
3504.580152	446927.379071	45.225639
3504.226117	446921.912171	45.230644
3504.354114	446915.602312	45.235649
3503.896322	446896.309300	45.240653
3504.014267	446881.076185	45.245658
3504.162019	446874.864362	45.250663
3504.036247	446881.934564	45.255668
3504.258110	446871.146181	45.260673
3504.537319	446846.909823	45.265677
3503.866209	446841.395623	45.270682
3504.153115	446826.387169	45.275687
3503.845699	446826.338271	45.280692
3504.176909	446815.683320	45.285697
3503.886283	446802.599031	45.290701
3503.825270	446798.045559	45.295706
3503.888424	446788.146308	45.300711
3503.697745	446796.292537	45.305716
3503.723458	446791.876385	45.310721
3504.042802	446796.588650	45.315725
3503.548080	446796.368894	45.320730
3503.884094	446793.776037	45.325735
3503.942630	446775.206115	45.330740
3504.015490	446755.822365	45.335745
3504.062567	446764.080140	45.340749
3504.071513	446753.733736	45.345754
3504.084617	446751.449564	45.350759
3503.885976	446742.609200	45.355764
3504.017355	446725.953790	45.360769
3503.753483	446719.660076	45.365773
3503.788356	446716.053711	45.370778
3504.186189	446713.146027	45.375783
3503.815797	446715.491272	45.380788
3503.990055	446705.674432	45.385793
3504.134896	446693.428508	45.390797
3504.027822	446679.349302	45.395802
3504.182029	446674.454791	45.400807
3503.625419	446679.874468	45.405812
3503.418215	446683.358194	45.410817
3503.903292	446677.190135	45.415821
3503.811447	446678.879296	45.420826
3504.306739	446669.311885	45.425831
3504.026302	446651.560393	45.430836
3504.183040	446639.565959	45.435841
3504.132613	446640.842365	45.440845
3503.910361	446639.054764	45.445850
3503.871415	446604.983884	45.450855
3503.812417	446599.010126	45.455860
3503.867150	446596.972382	45.460865
3503.720392	446602.220675	45.465869
3503.842288	446593.731203	45.470874
3504.017119	446592.839298	45.475879
3503.722205	446599.634211	45.480884
3504.085276	446592.929143	45.485889
3504.464625	446585.714186	45.490893
3504.109903	446581.616504	45.495898
3503.680222	446569.671452	45.500903
3503.988263	446582.043022	45.505908
3503.983674	446576.212099	45.510913
3503.754382	446560.936625	45.515917
3503.946471	446541.075924	45.520922
3503.914507	446532.004169	45.525927
3503.753633	446541.666732	45.530932
3503.966250	446535.747999	45.535937
3504.204259	446539.662836	45.540941
3503.791277	446521.021071	45.545946
3503.933551	446503.197277	45.550951
3503.926934	446505.987539	45.555956
3504.026156	446492.684359	45.560961
3503.629113	446492.650763	45.565965
3503.900288	446498.537672	45.570970
3503.977835	446495.228249	45.575975
3503.991005	446498.065844	45.580980
3504.144068	446470.097988	45.585985
3504.290495	446460.995742	45.590989
3504.272528	446460.745285	45.595994
3504.177172	446454.372006	45.600999
3503.898689	446436.924267	45.606004
3503.645779	446427.078817	45.611009
3503.695072	446423.165674	45.616013
3503.504474	446424.009627	45.621018
3504.033730	446421.079463	45.626023
3503.708851	446423.011279	45.631028
3503.850618	446417.053900	45.636033
3504.295951	446421.491180	45.641037
3503.992439	446399.534394	45.646042
3504.043373	446382.689607	45.651047
3504.000924	446385.587426	45.656052
3503.999385	446374.481960	45.661057
3503.938538	446385.344583	45.666061
3503.912066	446382.965706	45.671066
3504.260245	446362.266807	45.676071
3503.651215	446349.845142	45.681076
3503.890290	446340.067778	45.686081
3504.135417	446342.662941	45.691085
3503.842489	446342.205877	45.696090
3503.955083	446334.427848	45.701095
3503.878075	446325.059428	45.706100
3503.878306	446311.925173	45.711105
3504.175961	446310.657305	45.716109
3503.970704	446307.598988	45.721114
3504.258784	446300.602365	45.726119
3504.248129	446294.823113	45.731124
3504.111886	446278.263762	45.736129
3503.975003	446263.327276	45.741133
3503.929633	446271.956008	45.746138
3504.161379	446262.839109	45.751143
3503.842057	446258.633897	45.756148
3504.062671	446230.806327	45.761153
3504.091517	446223.600386	45.766157
3504.141126	446224.758312	45.771162
3504.365517	446215.034110	45.776167
3503.911616	446209.431943	45.781172
3503.804839	446182.826580	45.786177
3504.032659	446198.914024	45.791181
3503.947097	446184.881530	45.796186
3504.014134	446187.050717	45.801191
3503.906676	446188.894716	45.806196
3504.228756	446167.591545	45.811201
3504.132972	446147.830345	45.816205
3503.949465	446149.028080	45.821210
3504.546230	446140.102361	45.826215
3504.038581	446134.661486	45.831220
3504.039859	446120.918393	45.836225
3504.060041	446108.237012	45.841229
3503.696669	446111.696784	45.846234
3504.135669	446106.144972	45.851239
3503.914306	446107.907005	45.856244
3503.952100	446075.394244	45.861249
3503.794190	446072.733504	45.866253
3503.561380	446076.170989	45.871258
3503.977626	446060.379234	45.876263
3503.718073	446065.494782	45.881268
3503.722659	446063.059854	45.886273
3503.941440	446067.383757	45.891277
3503.888669	446064.705064	45.896282
3503.744923	446052.660185	45.901287
3503.942695	446043.447570	45.906292
3503.908200	446031.029040	45.911297
3503.904984	446030.623923	45.916301
3503.620407	446030.571121	45.921306
3504.000071	446023.203785	45.926311
3503.976721	446027.518329	45.931316
3503.901748	446029.103236	45.936321
3504.063032	446008.588043	45.941325
3503.911683	445995.986597	45.946330
3504.106448	445992.961354	45.951335
3503.780678	445994.284814	45.956340
3504.142137	445990.673274	45.961345
3504.062742	445989.165497	45.966349
3503.824705	445980.940089	45.971354
3503.950208	445963.067996	45.976359
3503.873216	445961.509094	45.981364
3503.958276	445954.648449	45.986369
3504.059443	445966.142881	45.991373
3504.076964	445962.387215	45.996378
3503.795815	445926.784530	46.001383
3503.997124	445929.184378	46.006388
3503.902083	445909.929953	46.011393
3503.995068	445915.543177	46.016397
3503.623886	445917.127957	46.021402
3503.933409	445902.774254	46.026407
3503.863329	445916.529297	46.031412
3503.608519	445895.527209	46.036417
3503.745874	445874.711700	46.041421
3503.868072	445878.494297	46.046426
3503.620942	445864.134192	46.051431
3503.882091	445875.094231	46.056436
3503.826812	445868.054672	46.061441
3503.536268	445878.348225	46.066445
3503.946858	445873.409754	46.071450
3504.347970	445875.978340	46.076455
3504.476578	445854.707893	46.081460
3503.890112	445835.841588	46.086465
3504.072326	445836.165493	46.091469
3503.605449	445833.253205	46.096474
3503.787563	445828.505874	46.101479
3504.020191	445834.044561	46.106484
3503.724829	445812.795753	46.111489
3503.712991	445795.099109	46.116493
3503.907913	445803.585574	46.121498
3504.169656	445791.775585	46.126503
3504.160987	445809.425083	46.131508
3503.985221	445797.588378	46.136513
3503.984036	445775.173624	46.141517
3504.053688	445759.998669	46.146522
3503.927570	445759.107405	46.151527
3503.665213	445759.659361	46.156532
3503.823717	445759.023774	46.161537
3503.956731	445758.493965	46.166541
3503.945715	445762.400755	46.171546
3504.118602	445738.992699	46.176551
3503.849152	445729.403313	46.181556
3503.914937	445717.474605	46.186561
3503.951948	445724.010267	46.191565
3503.922532	445728.376619	46.196570
3504.087633	445720.031562	46.201575
3503.634108	445705.047326	46.206580
3503.689662	445686.426253	46.211585
3503.669752	445681.611960	46.216589
3503.721983	445687.282914	46.221594
3504.238816	445680.652733	46.226599
3504.263778	445682.271314	46.231604
3503.952553	445671.674778	46.236609
3504.134843	445665.355280	46.241613
3504.005389	445647.323605	46.246618
3504.067215	445635.192676	46.251623
3504.087245	445643.303365	46.256628
3503.846513	445636.548960	46.261633
3504.153920	445634.214416	46.266637
3503.589329	445618.437676	46.271642
3503.693172	445600.416839	46.276647
3503.561093	445598.765891	46.281652
3503.771274	445590.007380	46.286657
3503.656304	445597.684720	46.291661
3503.698566	445596.916837	46.296666
3503.949617	445595.758313	46.301671
3503.919622	445600.023364	46.306676
3503.691257	445592.810417	46.311681
3503.831348	445592.330108	46.316685
3503.965954	445589.061516	46.321690
3503.878445	445571.124041	46.326695
3503.664829	445566.697790	46.331700
3503.816388	445556.022175	46.336705
3503.942387	445561.224148	46.341709
3503.600158	445563.006863	46.346714
3503.897375	445560.116205	46.351719
3503.867172	445560.780665	46.356724
3503.855573	445567.527527	46.361729
3504.036665	445559.433242	46.366733
3504.048978	445538.435904	46.371738
3503.883797	445524.923704	46.376743
3503.799589	445521.895317	46.381748
3503.605635	445516.400719	46.386753
3503.923702	445523.699863	46.391757
3503.932209	445527.400509	46.396762
3504.265958	445518.773010	46.401767
3504.049387	445502.176060	46.406772
3503.998385	445489.962887	46.411777
3503.895721	445493.682522	46.416781
3503.888938	445493.785137	46.421786
3504.414159	445492.072658	46.426791
3504.217148	445472.277405	46.431796
3503.930955	445450.519538	46.436801
3504.199656	445451.995090	46.441805
3504.440980	445453.171036	46.446810
3504.652213	445422.909774	46.451815
3504.195340	445412.997254	46.456820
3504.411818	445404.491161	46.461825
3504.067193	445374.324743	46.466829
3503.844617	445374.007784	46.471834
3503.981974	445368.203007	46.476839
3504.233370	445372.724338	46.481844
3504.003184	445352.275361	46.486849
3503.956135	445343.864955	46.491853
3504.179492	445335.053377	46.496858
3503.855796	445336.173667	46.501863
3503.641297	445342.549536	46.506868
3503.879580	445342.458166	46.511873
3503.663632	445344.827899	46.516877
3503.914447	445336.518770	46.521882
3504.001141	445312.820685	46.526887
3503.721315	445308.507112	46.531892
3503.636005	445296.705398	46.536897
3503.962667	445294.570384	46.541901
3503.775696	445298.405875	46.546906
3503.524079	445299.006722	46.551911
3503.798177	445303.727045	46.556916
3503.769890	445300.181941	46.561921
3503.974042	445295.988581	46.566925
3503.709511	445289.390272	46.571930
3504.177811	445271.104071	46.576935
3503.858480	445271.158628	46.581940
3503.970847	445254.911031	46.586945
3504.094016	445264.728524	46.591949
3503.805841	445267.516310	46.596954
3504.075260	445257.783986	46.601959
3503.869026	445234.338687	46.606964
3504.202140	445216.227665	46.611969
3504.155163	445214.562155	46.616973
3504.142109	445228.409330	46.621978
3504.131435	445205.032035	46.626983
3503.929595	445191.576598	46.631988
3503.933610	445187.721675	46.636993
3503.972657	445189.540744	46.641997
3503.575106	445191.586505	46.647002
3503.842953	445173.790876	46.652007
3503.966605	445183.202611	46.657012
3504.281099	445163.928302	46.662017
3504.050902	445152.962674	46.667021
3503.887937	445145.231266	46.672026
3503.979036	445139.992182	46.677031
3503.531654	445141.488601	46.682036
3503.951988	445133.860447	46.687041
3504.125539	445138.496547	46.692045
3503.538700	445121.506099	46.697050
3503.796173	445111.268606	46.702055
3503.601410	445105.368326	46.707060
3503.716720	445105.551524	46.712065
3503.785653	445109.089782	46.717069
3503.391524	445097.137832	46.722074
3503.567711	445099.085634	46.727079
3503.363981	445106.119020	46.732084
3503.554887	445105.021453	46.737089
3503.929861	445107.696026	46.742093
3503.340198	445109.673169	46.747098
3503.785179	445101.584367	46.752103
3503.804057	445105.891886	46.757108
3503.688683	445104.390189	46.762113
3503.686617	445105.506286	46.767117
3503.809437	445110.303198	46.772122
3503.969146	445107.841674	46.777127
3503.712540	445095.764813	46.782132
3503.917712	445079.906951	46.787137
3503.883920	445076.869892	46.792141
3503.727579	445077.708047	46.797146
3503.899943	445071.085784	46.802151
3503.924299	445076.558803	46.807156
3504.175286	445067.336683	46.812161
3503.794243	445056.447477	46.817165
3503.401466	445040.488830	46.822170
3503.722907	445035.818962	46.827175
3503.619686	445036.140904	46.832180
3504.049671	445032.821791	46.837185
3503.710552	445025.323277	46.842189
3503.593199	445034.979087	46.847194
3504.019992	445033.232666	46.852199
3503.612580	445037.815846	46.857204
3503.669425	445029.641148	46.862209
3503.729585	445036.680211	46.867213
3503.876775	445035.235105	46.872218
3503.695608	445028.318194	46.877223
3503.737551	445005.185269	46.882228
3503.578848	444997.199508	46.887233
3503.934769	444996.428761	46.892237
3503.565523	444998.672564	46.897242
3503.932024	444996.885721	46.902247
3503.847140	445003.695989	46.907252
3503.631941	444995.466301	46.912257
3503.663184	444991.809552	46.917261
3503.742828	444989.564544	46.922266
3504.102962	444988.285932	46.927271
3503.971380	444991.757018	46.932276
3503.901288	444971.584629	46.937281
3504.077848	444972.315230	46.942285
3503.641293	444957.733289	46.947290
3503.889721	444946.837973	46.952295
3503.847542	444964.341744	46.957300
3504.250128	444949.007937	46.962305
3504.205408	444931.519053	46.967309
3504.202008	444928.781072	46.972314
3504.408822	444917.943562	46.977319
3504.140455	444909.976494	46.982324
3504.155156	444891.564566	46.987329
3504.254297	444885.563326	46.992333
3504.121107	444871.233814	46.997338
3504.360733	444868.454328	47.002343
3504.068421	444852.376956	47.007348
3504.044734	444834.681542	47.012353
3503.874633	444828.624830	47.017357
3503.289224	444833.948455	47.022362
3503.866161	444827.967044	47.027367
3503.689897	444826.678584	47.032372
3503.571409	444829.893886	47.037377
3504.019420	444832.556022	47.042381
3503.938861	444823.998989	47.047386
3503.859310	444805.755226	47.052391
3503.638004	444798.946525	47.057396
3503.722767	444791.882699	47.062401
3504.045946	444800.246233	47.067405
3503.881057	444792.819317	47.072410
3503.963948	444798.383841	47.077415
3503.800782	444796.180274	47.082420
3503.773404	444777.876864	47.087425
3504.053991	444760.687298	47.092429
3503.925426	444751.428423	47.097434
3503.872484	444744.438810	47.102439
3503.685264	444753.548811	47.107444
3503.748768	444750.951528	47.112449
3503.703271	444756.182981	47.117453
3503.614072	444756.147527	47.122458
3503.599331	444754.273617	47.127463
3503.769371	444750.846702	47.132468
3503.608858	444756.047079	47.137473
3503.711937	444733.309143	47.142477
3503.711211	444727.172766	47.147482
3503.637460	444724.294626	47.152487
3503.485566	444724.269878	47.157492
3503.773108	444723.307937	47.162497
3503.901869	444714.207967	47.167501
3503.625356	444728.049736	47.172506
3503.933655	444723.382045	47.177511
3503.867429	444725.421990	47.182516
3503.650050	444726.372011	47.187521
3503.948569	444729.668268	47.192525
3503.597221	444739.719172	47.197530
3503.625348	444710.756050	47.202535
3504.095058	444697.185634	47.207540
3503.671625	444680.674085	47.212545
3504.229855	444684.433156	47.217549
3503.737735	444689.740887	47.222554
3504.064764	444679.542028	47.227559
3503.774338	444687.046790	47.232564
3503.732306	444684.416805	47.237569
3503.806783	444681.513349	47.242573
3503.898035	444670.492586	47.247578
3503.897663	444650.764429	47.252583
3503.920544	444643.457544	47.257588
3504.160036	444640.880914	47.262593
3504.109148	444634.043061	47.267597
3503.989960	444635.382042	47.272602
3503.631567	444610.085575	47.277607
3503.573011	444597.568892	47.282612
3503.723653	444597.746061	47.287617
3503.664377	444596.437612	47.292621
3503.707043	444597.343235	47.297626
3504.083447	444599.155466	47.302631
3503.898184	444607.910185	47.307636
3503.834871	444605.537401	47.312641
3504.104290	444608.534353	47.317645
3503.710909	444596.429850	47.322650
3503.825621	444573.689759	47.327655
3504.071710	444570.909132	47.332660
3503.599616	444567.743980	47.337665
3503.969375	444564.282933	47.342669
3503.577157	444564.451367	47.347674
3503.971868	444564.637577	47.352679
3503.998091	444576.094836	47.357684
3503.815488	444555.687691	47.362689
3503.771844	444535.916101	47.367693
3503.721044	444530.903961	47.372698
3503.916249	444528.842036	47.377703
3503.930103	444536.193463	47.382708
3503.662090	444527.364027	47.387713
3503.733169	444532.220619	47.392717
3503.587900	444530.318261	47.397722
3504.063572	444530.237070	47.402727
3503.987718	444519.447626	47.407732
3503.997268	444495.457518	47.412737
3504.316003	444489.012946	47.417741
3503.493784	444494.427805	47.422746
3503.981639	444481.107734	47.427751
3504.228905	444483.398466	47.432756
3504.195983	444466.312915	47.437761
3503.958466	444454.688874	47.442765
3503.796024	444453.347316	47.447770
3503.784442	444444.727638	47.452775
3504.232496	444440.796761	47.457780
3504.201389	444437.607007	47.462785
3504.368521	444412.474151	47.467789
3504.381194	444422.919487	47.472794
3504.453930	444402.417881	47.477799
3504.333148	444391.483896	47.482804
3504.458607	444372.697601	47.487809
3504.343171	444365.414240	47.492813
3504.411051	444342.479039	47.497818
3504.304667	444327.028834	47.502823
3504.227952	444323.745418	47.507828
3503.870070	444309.098886	47.512833
3503.707044	444275.349786	47.517837
3503.469463	444286.345082	47.522842
3503.716399	444278.036208	47.527847
3503.479337	444283.351202	47.532852
3503.724400	444280.164983	47.537857
3503.922464	444279.319735	47.542861
3503.775921	444289.792322	47.547866
3504.107709	444279.237449	47.552871
3504.060217	444280.310629	47.557876
3503.693476	444269.621445	47.562881
3503.946470	444249.849658	47.567885
3503.411363	444249.788910	47.572890
3503.710654	444243.753316	47.577895
3503.483151	444246.987318	47.582900
3503.461369	444242.071589	47.587905
3503.812460	444237.193622	47.592909
3503.800111	444252.258496	47.597914
3504.168886	444244.740266	47.602919
3504.324180	444248.314635	47.607924
3504.334355	444235.126694	47.612929
3504.243805	444213.638464	47.617933
3504.015647	444212.967424	47.622938
3503.619458	444209.687825	47.627943
3503.740041	444206.776433	47.632948
3503.777439	444199.669785	47.637953
3504.078919	444201.089112	47.642957
3503.736119	444186.439921	47.647962
3503.669667	444167.280485	47.652967
3503.783648	444165.232394	47.657972
3503.555079	444164.206408	47.662977
3503.755881	444162.802806	47.667981
3503.872562	444166.130200	47.672986
3504.107127	444158.939155	47.677991
3503.981793	444167.633103	47.682996
3504.119762	444154.372575	47.688001
3503.995824	444134.512895	47.693005
3503.544858	444124.142320	47.698010
3503.929777	444123.823042	47.703015
3504.229182	444128.387155	47.708020
3503.661974	444123.108082	47.713025
3504.173038	444119.014239	47.718029
3503.866720	444111.104070	47.723034
3504.243769	444097.904117	47.728039
3504.087315	444095.648614	47.733044
3503.741982	444093.323929	47.738049
3503.882886	444087.366053	47.743053
3503.712845	444097.538446	47.748058
3504.134415	444078.244883	47.753063
3503.950360	444061.996284	47.758068
3503.726869	444052.296866	47.763073
3504.177039	444043.851767	47.768077
3504.304861	444054.125470	47.773082
3504.561590	444033.592096	47.778087
3503.991745	444018.271524	47.783092
3503.452077	444013.697756	47.788097
3503.979023	444006.101719	47.793101
3503.634874	444012.753702	47.798106
3503.723226	444009.391335	47.803111
3504.064387	444017.599954	47.808116
3503.281590	443993.643149	47.813121
3503.645362	443988.154360	47.818125
3503.758165	443986.258604	47.823130
3503.733794	443969.272632	47.828135
3503.677360	443971.818145	47.833140
3503.832622	443970.219440	47.838145
3503.715575	443966.029951	47.843149
3503.753826	443980.477772	47.848154
3503.829041	443971.234481	47.853159
3503.778164	443978.089983	47.858164
3503.521732	443972.605656	47.863169
3503.668086	443969.486964	47.868173
3503.663061	443982.268514	47.873178
3503.775808	443968.707877	47.878183
3503.789891	443976.363758	47.883188
3503.603423	443966.708696	47.888193
3503.842026	443942.628146	47.893197
3503.733397	443938.741517	47.898202
3503.713696	443937.527703	47.903207
3503.555799	443938.112582	47.908212
3503.907955	443929.988477	47.913217
3503.892645	443941.706749	47.918221
3503.822306	443936.596374	47.923226
3503.838934	443935.173489	47.928231
3503.699939	443934.537932	47.933236
3503.674466	443936.520275	47.938241
3504.289312	443924.344670	47.943245
3504.075621	443908.608186	47.948250
3503.863951	443905.804204	47.953255
3503.878028	443899.107175	47.958260
3503.890749	443897.076350	47.963265
3503.829765	443890.848590	47.968269
3503.706579	443877.683202	47.973274
3503.697087	443871.446645	47.978279
3503.631667	443861.821584	47.983284
3503.815219	443860.116606	47.988289
3504.019794	443859.523816	47.993293
3503.842210	443859.909189	47.998298
3503.962341	443855.070574	48.003303
3504.237112	443858.117436	48.008308
3503.709989	443835.841183	48.013313
3503.645191	443824.948069	48.018317
3503.426561	443829.752853	48.023322
3503.680643	443813.226385	48.028327
3503.629984	443817.140297	48.033332
3503.655203	443817.389607	48.038337
3503.725462	443808.147094	48.043341
3503.819636	443819.136696	48.048346
3503.719169	443821.486876	48.053351
3503.708123	443817.279259	48.058356
3503.784106	443812.093151	48.063361
3503.896689	443816.080624	48.068365
3503.649177	443825.150593	48.073370
3504.314430	443809.061086	48.078375
3504.462413	443800.211036	48.083380
3504.150032	443789.410896	48.088385
3504.375366	443779.888305	48.093389
3504.197554	443756.791564	48.098394
3504.356986	443735.818065	48.103399
3504.366985	443744.438357	48.108404
3504.314164	443724.211133	48.113409
3504.402997	443697.924314	48.118413
3504.089094	443701.832479	48.123418
3504.013239	443693.984240	48.128423
3504.091769	443674.495305	48.133428
3504.062939	443662.632332	48.138433
3504.006583	443653.309937	48.143437
3503.883910	443655.359621	48.148442
3504.048286	443651.375606	48.153447
3504.080259	443657.709885	48.158452
3504.033674	443634.235582	48.163457
3504.150687	443614.537152	48.168461
3504.004445	443617.047323	48.173466
3504.105598	443612.566919	48.178471
3503.602956	443610.319760	48.183476
3503.466125	443590.411062	48.188481
3503.588409	443575.783477	48.193485
3503.212364	443581.477399	48.198490
3503.306356	443605.146596	48.203495
3503.650510	443609.145284	48.208500
3503.480104	443611.710299	48.213505
3503.603121	443611.638607	48.218509
3503.220547	443624.941295	48.223514
3503.606230	443616.608477	48.228519
3503.511617	443623.471559	48.233524
3503.479130	443623.680008	48.238529
3503.761829	443620.588702	48.243533
3503.491360	443622.663626	48.248538
3503.486888	443626.772556	48.253543
3504.003088	443630.234685	48.258548
3504.078753	443607.905987	48.263553
3504.191593	443582.781438	48.268557
3503.951004	443584.952698	48.273562
3503.613152	443579.127149	48.278567
3503.427612	443574.594255	48.283572
3503.168199	443576.565859	48.288577
3503.501413	443588.326247	48.293581
3503.451642	443575.553882	48.298586
3503.292788	443568.125512	48.303591
3503.507140	443575.240160	48.308596
3503.474152	443573.267827	48.313601
3503.832320	443570.721524	48.318605
3503.359918	443582.061580	48.323610
3503.662543	443572.931443	48.328615
3503.589770	443570.205135	48.333620
3504.019448	443575.507890	48.338625
3503.678714	443569.479959	48.343629
3503.527438	443576.352730	48.348634
3504.036597	443574.490697	48.353639
3504.184596	443580.957340	48.358644
3503.931699	443564.567968	48.363649
3503.857563	443544.648523	48.368653
3503.565899	443546.524201	48.373658
3503.925716	443540.173770	48.378663
3503.995105	443532.249953	48.383668
3503.816486	443538.772380	48.388673
3503.960062	443532.357434	48.393677
3503.825715	443525.330608	48.398682
3503.813392	443503.473288	48.403687
3503.860614	443502.045151	48.408692
3503.688422	443496.546319	48.413697
3503.970171	443491.629308	48.418701
3503.912480	443503.912953	48.423706
3503.718665	443495.273295	48.428711
3503.796901	443500.382488	48.433716
3503.752680	443495.521138	48.438721
3503.941388	443488.286984	48.443725
3503.526955	443479.684991	48.448730
3503.677647	443462.161548	48.453735
3503.776272	443464.122745	48.458740
3503.859461	443472.172748	48.463745
3504.191086	443463.494076	48.468749
3503.610893	443474.954030	48.473754
3503.796884	443457.475274	48.478759
3503.942043	443462.370176	48.483764
3503.786791	443458.947884	48.488769
3503.913824	443437.776756	48.493773
3503.731322	443435.170604	48.498778
3503.662058	443420.271312	48.503783
3504.096981	443421.870780	48.508788
3503.516797	443419.281812	48.513793
3504.008397	443421.175912	48.518797
3503.872866	443425.408695	48.523802
3503.694313	443422.041095	48.528807
3503.806275	443422.072726	48.533812
3503.655807	443406.832263	48.538817
3503.975257	443384.613863	48.543821
3503.618662	443386.297768	48.548826
3503.929203	443378.231281	48.553831
3503.701460	443387.703803	48.558836
3503.671890	443390.346234	48.563841
3503.941036	443381.678197	48.568845
3503.399327	443380.198458	48.573850
3503.825094	443380.328661	48.578855
3503.755924	443389.114768	48.583860
3503.504338	443390.324278	48.588865
3503.927380	443389.034834	48.593869
3503.584539	443383.260802	48.598874
3503.809229	443358.066175	48.603879
3503.545629	443351.365673	48.608884
3503.531408	443346.093420	48.613889
3503.911166	443334.008346	48.618893
3503.411864	443348.244066	48.623898
3503.772245	443341.690607	48.628903
3503.713293	443344.135187	48.633908
3503.521274	443344.523033	48.638913
3504.160439	443351.311625	48.643917
3503.578503	443355.620647	48.648922
3504.289074	443345.609263	48.653927
3503.484186	443352.187964	48.658932
3503.496683	443351.475803	48.663937
3503.566701	443346.189166	48.668941
3503.846848	443350.553860	48.673946
3503.667738	443338.564216	48.678951
3503.698065	443318.018105	48.683956
3503.992951	443311.475820	48.688961
3504.118741	443305.571029	48.693965
3503.966420	443317.617345	48.698970
3504.217692	443312.857654	48.703975
3504.305757	443310.256005	48.708980
3504.306858	443288.294739	48.713985
3503.665654	443277.956239	48.718989
3503.694536	443272.980920	48.723994
3503.594425	443264.020858	48.728999
3503.595462	443272.186401	48.734004
3503.641873	443268.070303	48.739009
3503.603017	443261.280679	48.744013
3503.283702	443272.087571	48.749018
3503.473545	443266.070394	48.754023
3503.565790	443270.517908	48.759028
3503.880075	443270.159962	48.764033
3503.722687	443271.606987	48.769037
3503.654006	443274.103954	48.774042
3503.741278	443268.459322	48.779047
3503.499615	443260.182770	48.784052
3503.983083	443253.506830	48.789057
3503.989053	443229.718804	48.794061
3503.659198	443245.396499	48.799066
3503.955707	443226.275690	48.804071
3504.288119	443226.523272	48.809076
3504.319148	443222.866261	48.814081
3504.071982	443206.932107	48.819085
3503.566890	443199.258419	48.824090
3503.765728	443196.587123	48.829095
3503.976297	443196.703355	48.834100
3503.985558	443196.651085	48.839105
3503.728223	443192.536120	48.844109
3503.931224	443201.833734	48.849114
3504.008970	443183.206710	48.854119
3504.048023	443166.412154	48.859124
3503.744625	443155.711601	48.864129
3504.006673	443150.290689	48.869133
3503.655059	443155.524080	48.874138
3503.933784	443151.926199	48.879143
3504.124793	443147.734669	48.884148
3503.841511	443127.444802	48.889153
3503.747533	443118.331476	48.894157
3503.614283	443123.679746	48.899162
3503.774459	443113.001453	48.904167
3504.140953	443111.873806	48.909172
3503.480677	443116.399127	48.914177
3503.749064	443112.143659	48.919181
3503.628412	443114.395924	48.924186
3503.591977	443110.141785	48.929191
3503.736584	443120.768098	48.934196
3503.537697	443117.201046	48.939201
3504.217242	443104.912498	48.944205
3503.923250	443085.182329	48.949210
3504.000632	443086.690716	48.954215
3503.820907	443085.098427	48.959220
3503.519083	443079.520186	48.964225
3503.718989	443070.660972	48.969229
3503.731177	443074.006377	48.974234
3503.805120	443074.196658	48.979239
3503.780131	443068.266829	48.984244
3503.690351	443078.578152	48.989249
3503.553869	443071.196510	48.994253
3503.527849	443083.474985	48.999258
3503.699196	443067.621424	49.004263
3503.824570	443056.796889	49.009268
3503.879092	443041.369009	49.014273
3503.694356	443028.112176	49.019277
3503.435551	443030.793792	49.024282
3503.672476	443022.638306	49.029287
3503.771168	443032.004524	49.034292
3503.754190	443035.152039	49.039297
3504.276839	443025.578350	49.044301
3503.458055	443035.912733	49.049306
3503.668964	443034.862369	49.054311
3503.846076	443034.426404	49.059316
3503.650337	443033.597632	49.064321
3503.776242	443022.620832	49.069325
3503.599619	443005.558664	49.074330
3503.869526	442997.042502	49.079335
3503.795761	442993.859818	49.084340
3503.588555	443000.285849	49.089345
3503.726180	442994.074637	49.094349
3503.494374	442991.426131	49.099354
3503.389715	442988.705194	49.104359
3503.608819	442993.841172	49.109364
3503.715651	442997.728340	49.114369
3503.704255	442986.217055	49.119373
3503.583938	442987.962083	49.124378
3503.727512	442986.771056	49.129383
3504.155718	442996.588216	49.134388
3503.849772	443005.414908	49.139393
3504.096089	442987.925474	49.144397
3504.240298	442963.251324	49.149402
3503.750193	442957.350165	49.154407
3504.130447	442955.611530	49.159412
3503.794876	442958.407702	49.164417
3503.850466	442949.522362	49.169421
3503.929439	442933.278722	49.174426
3503.795165	442920.266803	49.179431
3503.980091	442913.540297	49.184436
3503.513247	442916.460329	49.189441
3503.777830	442908.502955	49.194445
3503.630436	442919.940017	49.199450
3503.644239	442924.756031	49.204455
3503.361527	442923.840667	49.209460
3503.835480	442922.441066	49.214465
3504.056197	442911.752337	49.219469
3503.632896	442913.650545	49.224474
3503.384635	442918.308431	49.229479
3503.887925	442913.911376	49.234484
3503.500756	442915.245501	49.239489
3504.062553	442897.600687	49.244493
3503.972116	442891.935582	49.249498
3503.750586	442878.938538	49.254503
3503.686135	442878.290220	49.259508
3503.626632	442873.735657	49.264513
3503.620058	442877.439333	49.269517
3503.655671	442884.787606	49.274522
3503.741120	442879.295343	49.279527
3503.831723	442878.721988	49.284532
3503.893073	442883.631332	49.289537
3504.021521	442866.516963	49.294541
3503.681453	442860.133683	49.299546
3504.195733	442858.017118	49.304551
3503.976127	442849.939521	49.309556
3503.866214	442852.240699	49.314561
3503.814141	442846.873349	49.319565
3504.197576	442847.822298	49.324570
3503.890378	442825.253852	49.329575
3503.991660	442813.723236	49.334580
3503.707343	442812.300945	49.339585
3504.082178	442797.883310	49.344589
3503.836947	442808.069146	49.349594
3503.833234	442802.541368	49.354599
3504.092313	442797.374475	49.359604
3504.398322	442777.896612	49.364609
3504.519997	442762.558508	49.369613
3504.181349	442761.855567	49.374618
3504.137211	442744.466253	49.379623
3504.022749	442725.263019	49.384628
3503.985698	442723.899940	49.389633
3504.305838	442722.830909	49.394637
3504.034655	442717.500941	49.399642
3503.930692	442689.572066	49.404647
3503.949999	442684.091048	49.409652
3503.985950	442682.766221	49.414657
3504.585388	442677.287583	49.419661
3504.141931	442674.472297	49.424666
3504.043252	442651.918786	49.429671
3504.388004	442648.157389	49.434676
3503.901954	442642.965531	49.439681
3504.132840	442625.681321	49.444685
3504.070925	442614.989987	49.449690
3503.869913	442604.525279	49.454695
3504.036008	442595.975967	49.459700
3504.015382	442599.428488	49.464705
3504.094103	442586.177119	49.469709
3503.707040	442573.968960	49.474714
3503.740838	442559.913722	49.479719
3503.844075	442543.462767	49.484724
3503.807040	442552.193004	49.489729
3503.608100	442554.255814	49.494733
3503.755000	442551.288987	49.499738
3503.984271	442552.771476	49.504743
3503.587952	442551.976935	49.509748
3503.658816	442551.609823	49.514753
3504.024108	442551.648920	49.519757
3503.753471	442544.188565	49.524762
3503.284115	442520.886688	49.529767
3503.844575	442517.342037	49.534772
3503.739260	442521.164074	49.539777
3503.704649	442511.533153	49.544781
3503.700083	442524.924128	49.549786
3503.797429	442519.683344	49.554791
3503.812720	442522.571822	49.559796
3503.654450	442529.598279	49.564801
3503.699757	442521.931807	49.569805
3503.601039	442525.549836	49.574810
3503.664326	442520.669911	49.579815
3503.744592	442511.932340	49.584820
3503.425575	442525.224846	49.589825
3503.523105	442517.092973	49.594829
3503.478716	442517.709227	49.599834
3503.603980	442513.579522	49.604839
3503.732004	442520.607817	49.609844
3503.456521	442519.183998	49.614849
3503.657259	442509.715771	49.619853
3503.334563	442525.646363	49.624858
3503.309489	442514.948688	49.629863
3503.363124	442510.983375	49.634868
3503.363194	442512.454283	49.639873
3503.746230	442513.352596	49.644877
3503.474312	442524.151764	49.649882
3503.796569	442518.568255	49.654887
3504.028820	442523.042736	49.659892
3503.937050	442500.792210	49.664897
3503.862743	442481.784785	49.669901
3504.211280	442482.080346	49.674906
3503.899175	442480.003412	49.679911
3504.199989	442469.047187	49.684916
3504.162675	442467.430535	49.689921
3504.171134	442443.134019	49.694925
3503.912497	442432.831229	49.699930
3503.987514	442428.456485	49.704935
3504.011250	442437.480715	49.709940
3504.146823	442428.175741	49.714945
3504.456156	442397.132688	49.719949
3504.032827	442400.704724	49.724954
3503.946027	442393.770854	49.729959
3503.953391	442392.349450	49.734964
3503.908371	442373.032606	49.739969
3503.834313	442353.974307	49.744973
3503.937363	442350.862779	49.749978
3503.894174	442350.312256	49.754983
3503.977192	442346.544778	49.759988
3503.935859	442343.508623	49.764993
3503.957045	442342.034135	49.769997
3503.933411	442321.648459	49.775002
3503.766920	442313.713755	49.780007
3504.140377	442309.541632	49.785012
3503.554348	442311.569118	49.790017
3503.930266	442306.280717	49.795021
3503.186135	442310.566916	49.800026
3503.471565	442312.800644	49.805031
3503.738313	442305.806377	49.810036
3503.571646	442306.950724	49.815041
3503.771678	442301.489471	49.820045
3503.691227	442307.133250	49.825050
3503.478669	442306.002996	49.830055
3503.943175	442304.554249	49.835060
3503.808844	442305.338029	49.840065
3503.755394	442287.696336	49.845069
3503.643648	442276.455415	49.850074
3503.598538	442273.267732	49.855079
3503.632204	442261.697649	49.860084
3503.710616	442272.741447	49.865089
3503.815148	442260.854937	49.870093
3503.713870	442265.741469	49.875098
3503.290684	442273.016126	49.880103
3503.749102	442274.915996	49.885108
3503.790621	442266.134222	49.890113
3504.140208	442255.372446	49.895117
3503.934661	442271.688987	49.900122
3503.968719	442260.828928	49.905127
3503.532422	442243.252571	49.910132
3503.593178	442235.025430	49.915137
3503.537397	442231.687401	49.920141
3503.752670	442237.077818	49.925146
3503.675172	442234.656474	49.930151
3503.530271	442229.913475	49.935156
3503.421967	442232.062280	49.940161
3503.408295	442224.000007	49.945165
3503.697335	442226.638896	49.950170
3503.705622	442230.999517	49.955175
3503.587755	442223.157919	49.960180
3503.626272	442227.411937	49.965185
3503.670354	442234.657541	49.970189
3503.825953	442224.385363	49.975194
3503.459451	442228.353491	49.980199
3503.658031	442221.827326	49.985204
3503.694369	442232.320398	49.990209
3503.809621	442228.344511	49.995213
3503.404406	442232.217807	50.000218
3503.697666	442230.747576	50.005223
3504.071509	442223.379948	50.010228
3503.973193	442226.389305	50.015233
3503.682133	442207.114326	50.020237
3503.627075	442204.638427	50.025242
3503.681951	442201.078614	50.030247
3503.850691	442196.028446	50.035252
3503.585897	442192.117447	50.040257
3503.647019	442193.780837	50.045261
3503.513040	442196.644124	50.050266
3503.547064	442191.059027	50.055271
3504.222901	442185.364338	50.060276
3504.149674	442191.159076	50.065281
3504.180782	442185.422312	50.070285
3504.033503	442169.267456	50.075290
3504.105446	442150.944866	50.080295
3504.030455	442152.885106	50.085300
3503.781761	442160.485054	50.090305
3504.018331	442153.191564	50.095309
3503.746341	442134.724804	50.100314
3503.804870	442117.469622	50.105319
3504.061383	442111.947957	50.110324
3503.984629	442119.822887	50.115329
3503.692405	442106.228797	50.120333
3503.558171	442107.519780	50.125338
3503.781025	442109.257002	50.130343
3504.135428	442112.087630	50.135348
3503.740180	442102.163058	50.140353
3503.851415	442081.754129	50.145357
3503.539119	442078.662762	50.150362
3503.306177	442072.514563	50.155367
3503.567112	442067.144295	50.160372
3503.457184	442066.858768	50.165377
3503.794513	442070.098088	50.170381
3503.474260	442067.312406	50.175386
3503.563836	442069.275274	50.180391
3503.594156	442067.342716	50.185396
3503.386318	442071.790993	50.190401
3503.664613	442057.744405	50.195405
3503.320095	442073.121117	50.200410
3503.233073	442069.788397	50.205415
3503.821662	442062.789819	50.210420
3503.315528	442067.796246	50.215425
3503.815072	442068.421077	50.220429
3503.698109	442066.716553	50.225434
3503.551890	442065.930009	50.230439
3503.550101	442060.097386	50.235444
3503.449733	442072.744176	50.240449
3503.685788	442068.189699	50.245453
3503.657167	442080.164855	50.250458
3503.350457	442066.978984	50.255463
3503.651427	442075.043041	50.260468
3503.432666	442069.602519	50.265473
3503.730592	442064.327377	50.270477
3503.552278	442074.958619	50.275482
3503.631227	442064.953061	50.280487
3503.565664	442069.579931	50.285492
3503.596132	442080.479849	50.290497
3503.771331	442068.581168	50.295501
3503.769978	442069.595857	50.300506
3503.419287	442076.046659	50.305511
3503.717887	442076.604359	50.310516
3503.628902	442079.510701	50.315521
3503.629464	442066.525969	50.320525
3503.494839	442076.896144	50.325530
3503.498923	442075.221672	50.330535
3503.685970	442076.052027	50.335540
3503.798860	442075.982060	50.340545
3503.761074	442070.510636	50.345549
3503.773204	442072.638893	50.350554
3503.811254	442059.647755	50.355559
3504.076813	442044.335299	50.360564
3503.823307	442037.683388	50.365569
3503.696232	442034.002451	50.370573
3503.525787	442032.712828	50.375578
3503.496470	442027.138505	50.380583
3503.580701	442027.732810	50.385588
3503.540963	442039.253394	50.390593
3503.625471	442030.616349	50.395597
3503.655796	442028.024408	50.400602
3503.474983	442030.692828	50.405607
3503.427339	442032.324080	50.410612
3503.666148	442037.304756	50.415617
3503.632863	442032.846984	50.420621
3503.798380	442041.492117	50.425626
3503.605933	442036.655751	50.430631
3504.126783	442030.784601	50.435636
3503.647627	442021.026484	50.440641
3503.833216	442011.662072	50.445645
3504.021763	441998.797365	50.450650
3503.796877	441992.191274	50.455655
3503.620947	441993.337219	50.460660
3503.831249	441996.141746	50.465665
3503.438000	441994.940887	50.470669
3503.603162	441994.659108	50.475674
3503.607032	441980.253556	50.480679
3503.873399	441985.584590	50.485684
3503.758061	441993.821205	50.490689
3504.254434	441990.439579	50.495693
3504.110195	441973.269628	50.500698
3504.107823	441960.488220	50.505703
3504.203176	441960.877742	50.510708
3503.891635	441956.315301	50.515713
3504.084422	441941.268807	50.520717
3503.992991	441930.582177	50.525722
3503.784644	441919.154679	50.530727
3504.172395	441903.770538	50.535732
3503.737313	441892.838238	50.540737
3503.728161	441842.675941	50.545741
3503.782701	441794.582255	50.550746
3503.300289	441746.022206	50.555751
3503.184477	441680.559666	50.560756
3503.087782	441621.383244	50.565761
3503.060077	441532.420731	50.570765
3502.910326	441466.811178	50.575770
3502.484360	441361.126733	50.580775
3502.493560	441250.193700	50.585780
3502.063672	441154.044897	50.590785
3502.027213	441035.915840	50.595789
3501.782210	440909.655187	50.600794
3501.506055	440790.449809	50.605799
3501.389397	440643.368728	50.610804
3500.930187	440494.062529	50.615809
3501.103407	440340.893652	50.620813
3500.475171	440187.556208	50.625818
3500.143551	440024.123285	50.630823
3500.141449	439841.864085	50.635828
3499.174065	439676.913902	50.640833
3499.177461	439485.672166	50.645837
3499.022661	439304.347703	50.650842
3498.972990	439104.082196	50.655847
3498.475418	438909.775885	50.660852
3497.898869	438695.443361	50.665857
3497.327144	438479.028032	50.670861
3496.827670	438270.968729	50.675866
3496.392810	438053.460562	50.680871
3496.104440	437827.453168	50.685876
3495.641378	437607.966963	50.690881
3495.079819	437380.733410	50.695885
3494.826775	437146.900360	50.700890
3493.786834	436904.929729	50.705895
3493.642894	436669.956949	50.710900
3492.904315	436421.131328	50.715905
3492.935811	436171.004561	50.720909
3492.125718	435934.260665	50.725914
3491.504516	435679.927398	50.730919
3491.274001	435418.827337	50.735924
3490.463286	435168.681080	50.740929
3490.165487	434904.440882	50.745933
3489.594989	434646.079076	50.750938
3488.610334	434373.273742	50.755943
3488.198673	434106.303816	50.760948
3487.808516	433845.263681	50.765953
3487.532876	433566.391043	50.770957
3486.737775	433297.193810	50.775962
3485.940328	433023.071854	50.780967
3485.645578	432736.936301	50.785972
3484.841875	432458.597051	50.790977
3484.425168	432173.185719	50.795981
3483.838145	431896.172758	50.800986
3483.252487	431606.977450	50.805991
3482.606353	431324.893242	50.810996
3481.757875	431044.261047	50.816001
3481.627623	430749.750423	50.821005
3480.826924	430464.941831	50.826010
3480.368180	430172.103913	50.831015
3479.819693	429865.778475	50.836020
3478.828927	429568.405697	50.841025
3478.575882	429275.572177	50.846029
3477.964395	428983.455970	50.851034
3477.028175	428668.401224	50.856039
3476.593938	428382.185194	50.861044
3475.512529	428084.149337	50.866049
3475.041672	427776.413093	50.871053
3474.412609	427480.931562	50.876058
3473.613962	427181.008907	50.881063
3473.015756	426870.440398	50.886068
3472.295563	426572.729903	50.891073
3471.966155	426266.726407	50.896077
3471.302978	425977.272057	50.901082
3470.334506	425673.958714	50.906087
3469.735741	425362.304779	50.911092
3469.081931	425067.812763	50.916097
3468.632926	424758.663382	50.921101
3468.053209	424452.425697	50.926106
3467.367811	424140.872271	50.931111
3467.059827	423833.108271	50.936116
3466.120565	423527.681702	50.941121
3465.246078	423213.204429	50.946125
3464.108967	422904.098113	50.951130
3463.725755	422606.890256	50.956135
3463.161714	422294.886333	50.961140
3462.377839	421991.292275	50.966145
3462.033685	421683.862677	50.971149
3461.307852	421379.134279	50.976154
3460.358975	421067.129693	50.981159
3459.943239	420767.341359	50.986164
3459.035169	420464.003504	50.991169
3458.397513	420153.609596	50.996173
3457.616274	419851.613352	51.001178
3457.025902	419543.006063	51.006183
3456.590453	419230.687586	51.011188
3455.144698	418930.570628	51.016193
3454.825221	418624.291983	51.021197
3454.410588	418317.645043	51.026202
3453.525657	418020.747036	51.031207
3453.204964	417710.446326	51.036212
3452.317015	417411.282186	51.041217
3451.619622	417097.484018	51.046221
3450.718998	416789.479743	51.051226
3450.206376	416490.697596	51.056231
3449.563688	416177.234119	51.061236
3448.950568	415880.315324	51.066241
3448.226475	415567.848409	51.071245
3447.557626	415261.410951	51.076250
3446.651356	414961.027759	51.081255
3445.918500	414653.375237	51.086260
3445.145945	414364.768649	51.091265
3444.796230	414044.322790	51.096269
3443.855460	413755.458797	51.101274
3442.937777	413453.155611	51.106279
3442.782622	413148.865088	51.111284
3441.867465	412851.556600	51.116289
3441.418275	412542.535495	51.121293
3440.644202	412245.830791	51.126298
3440.039032	411948.357476	51.131303
3439.375069	411643.069737	51.136308
3438.620545	411344.497760	51.141313
3438.120046	411041.460503	51.146317
3437.071457	410737.243647	51.151322
3436.066381	410439.212048	51.156327
3435.868029	410141.344055	51.161332
3434.870170	409841.526858	51.166337
3434.524723	409544.032788	51.171341
3433.992400	409247.481532	51.176346
3433.063515	408946.601232	51.181351
3432.588101	408635.608679	51.186356
3431.649950	408341.605450	51.191361
3431.019918	408042.721026	51.196365
3430.309438	407739.478750	51.201370
3429.420189	407445.787502	51.206375
3429.040517	407142.761373	51.211380
3428.199984	406857.157160	51.216385
3427.519774	406554.074154	51.221389
3426.870004	406260.989465	51.226394
3426.348469	405969.352824	51.231399
3425.617940	405670.103710	51.236404
3424.722297	405378.321430	51.241409
3424.201345	405075.702725	51.246413
3423.341546	404785.736746	51.251418
3422.542805	404490.042298	51.256423
3422.388357	404196.495253	51.261428
3421.576984	403901.355432	51.266433
3420.658145	403603.004913	51.271437
3419.855013	403306.485683	51.276442
3418.901095	403026.398228	51.281447
3418.830901	402723.295679	51.286452
3417.894284	402447.670095	51.291457
3416.891580	402143.983829	51.296461
3416.938052	401865.720611	51.301466
3415.989568	401568.623424	51.306471
3415.547528	401277.965127	51.311476
3415.118733	400986.488661	51.316481
3414.336964	400688.972649	51.321485
3413.932902	400389.712355	51.326490
3413.054545	400090.783926	51.331495
3412.565131	399791.023796	51.336500
3411.678959	399487.314353	51.341505
3410.884779	399186.126425	51.346509
3409.530168	398888.257450	51.351514
3408.880281	398609.522177	51.356519
3408.412112	398313.807708	51.361524
3407.771816	398028.053226	51.366529
3407.371450	397739.866765	51.371533
3406.392730	397445.958157	51.376538
3405.600683	397161.161015	51.381543
3405.119529	396862.308854	51.386548
3404.261697	396587.171861	51.391553
3403.864056	396294.549708	51.396557
3403.192621	395999.583063	51.401562
3402.366027	395716.276685	51.406567
3402.018399	395417.691774	51.411572
3400.961905	395138.611381	51.416577
3400.330543	394847.208831	51.421581
3399.719824	394557.476844	51.426586
3398.861740	394272.662782	51.431591
3398.716080	393976.645871	51.436596
3397.736435	393695.328071	51.441601
3397.138730	393402.533398	51.446605
3396.401377	393124.649946	51.451610
3395.967241	392837.793126	51.456615
3395.390022	392534.847736	51.461620
3394.520875	392247.271809	51.466625
3393.710425	391951.983569	51.471629
3393.377502	391666.063853	51.476634
3392.515482	391376.191355	51.481639
3391.788672	391080.092520	51.486644
3391.067269	390797.661497	51.491649
3390.463049	390507.939940	51.496653
3389.438038	390211.629418	51.501658
3388.402186	389927.515953	51.506663
3388.305243	389657.521554	51.511668
3386.928557	389364.083683	51.516673
3386.652745	389093.098324	51.521677
3385.623486	388804.246406	51.526682
3385.047879	388523.395907	51.531687
3384.884238	388240.642680	51.536692
3384.109078	387973.189056	51.541697
3383.507614	387686.845875	51.546701
3382.482946	387405.426546	51.551706
3381.997829	387124.471655	51.556711
3381.430314	386833.997590	51.561716
3380.539723	386555.572097	51.566721
3380.265462	386269.871646	51.571725
3379.319466	385992.568900	51.576730
3378.594088	385722.139219	51.581735
3377.969140	385429.349082	51.586740
3377.145368	385154.407220	51.591745
3376.456439	384874.102408	51.596749
3376.235206	384594.172752	51.601754
3375.063335	384320.630209	51.606759
3374.452644	384044.422311	51.611764
3373.939079	383752.487293	51.616769
3373.398053	383477.050542	51.621773
3372.635786	383204.191022	51.626778
3371.859754	382922.841801	51.631783
3371.482699	382634.762313	51.636788
3370.544750	382365.255521	51.641793
3369.559472	382080.071027	51.646797
3369.441313	381804.115640	51.651802
3368.832910	381532.639200	51.656807
3367.955410	381241.684140	51.661812
3367.213043	380960.896791	51.666817
3366.406504	380685.710417	51.671821
3366.061162	380404.723394	51.676826
3364.892473	380122.578132	51.681831
3364.576917	379840.818589	51.686836
3363.610345	379579.860500	51.691841
3363.233970	379293.403796	51.696845
3362.546992	379020.369323	51.701850
3361.961580	378742.154674	51.706855
3360.970334	378457.956615	51.711860
3360.415017	378185.350404	51.716865
3360.146739	377894.261819	51.721869
3359.149623	377626.480474	51.726874
3358.817380	377342.312938	51.731879
3358.015215	377054.384404	51.736884
3357.152989	376792.573195	51.741889
3356.741856	376501.751211	51.746893
3355.976850	376230.258197	51.751898
3355.091201	375951.131080	51.756903
3354.933960	375671.826430	51.761908
3353.651922	375390.703088	51.766913
3353.304392	375099.400646	51.771917
3352.804485	374837.131175	51.776922
3351.970259	374559.687381	51.781927
3351.369354	374272.743423	51.786932
3350.389516	373990.946833	51.791937
3350.125177	373709.585115	51.796941
3349.434269	373430.226314	51.801946
3348.790307	373159.629149	51.806951
3347.972536	372867.727174	51.811956
3347.081392	372594.726955	51.816961
3346.666372	372306.590875	51.821965
3345.875760	372038.120486	51.826970
3344.806777	371753.854705	51.831975
3344.790311	371477.467239	51.836980
3343.836465	371204.619525	51.841985
3343.490534	370914.858389	51.846989
3342.661015	370636.569048	51.851994
3341.781490	370363.625912	51.856999
3341.622218	370071.791831	51.862004
3340.232850	369808.060183	51.867009
3340.032368	369511.829516	51.872013
3339.055707	369242.301850	51.877018
3338.369085	368970.561193	51.882023
3338.111589	368684.428701	51.887028
3337.016945	368409.142609	51.892033
3336.249598	368126.703745	51.897037
3335.499394	367860.356673	51.902042
3335.191224	367581.242732	51.907047
3334.512946	367310.912342	51.912052
3333.540766	367040.197847	51.917057
3332.962209	366760.615254	51.922061
3332.818277	366486.322151	51.927066
3331.844316	366222.239326	51.932071
3331.337048	365936.051790	51.937076
3330.764904	365657.527885	51.942081
3329.694254	365376.950816	51.947085
3329.391957	365094.180470	51.952090
3328.417532	364822.687271	51.957095
3328.124322	364537.240863	51.962100
3327.461876	364264.825679	51.967105
3326.635470	363983.280948	51.972109
3325.948196	363700.896528	51.977114
3324.863640	363431.014386	51.982119
3324.652880	363144.220917	51.987124
3323.522718	362868.798247	51.992129
3322.883987	362591.458481	51.997133
3322.390018	362319.738181	52.002138
3321.056435	362050.016006	52.007143
3320.590982	361774.548274	52.012148
3320.184684	361514.430514	52.017153
3319.551920	361228.076361	52.022157
3319.161101	360963.094371	52.027162
3318.090642	360695.734091	52.032167
3317.401931	360416.250813	52.037172
3316.874478	360149.658840	52.042177
3315.933561	359884.585464	52.047181
3315.728225	359618.621623	52.052186
3315.073426	359341.566691	52.057191
3314.489847	359065.489640	52.062196
3313.618190	358795.259187	52.067201
3312.691492	358517.151216	52.072205
3312.277489	358250.170993	52.077210
3311.320539	357974.557138	52.082215
3310.829455	357702.779013	52.087220
3310.069781	357438.294316	52.092225
3309.632650	357162.687871	52.097229
3309.035579	356903.182916	52.102234
3307.997036	356633.551488	52.107239
3307.427544	356357.046452	52.112244
3306.682216	356094.000465	52.117249
3306.302122	355827.507227	52.122253
3305.647935	355555.793486	52.127258
3304.675554	355280.164002	52.132263
3304.236538	355005.815231	52.137268
3303.672130	354740.542031	52.142273
3303.075602	354471.456878	52.147277
3302.507915	354200.075600	52.152282
3301.704186	353933.311823	52.157287
3300.830039	353647.097705	52.162292
3299.891332	353378.521857	52.167297
3298.975799	353105.157783	52.172301
3298.702162	352847.887124	52.177306
3297.846286	352581.937744	52.182311
3297.652027	352312.948143	52.187316
3296.685772	352046.378274	52.192321
3296.473382	351778.787586	52.197325
3295.475059	351516.163072	52.202330
3295.050797	351241.354798	52.207335
3294.255617	350962.359577	52.212340
3293.263992	350707.539184	52.217345
3293.103120	350438.175968	52.222349
3292.641839	350167.971962	52.227354
3291.368788	349893.020251	52.232359
3290.670845	349621.555787	52.237364
3290.139071	349353.215985	52.242369
3289.492612	349076.116819	52.247373
3288.772037	348824.292120	52.252378
3287.981485	348557.899795	52.257383
3287.295971	348281.972641	52.262388
3286.849612	348015.594600	52.267393
3286.354579	347748.002052	52.272397
3285.754153	347474.523266	52.277402
3284.742487	347212.027908	52.282407
3284.398235	346933.718874	52.287412
3283.513747	346665.957413	52.292417
3283.001910	346394.187051	52.297421
3282.197033	346128.367927	52.302426
3281.664667	345861.635634	52.307431
3280.959683	345586.255044	52.312436
3279.847436	345319.440527	52.317441
3279.254156	345052.128720	52.322445
3279.000099	344788.090575	52.327450
3278.051822	344526.103242	52.332455
3277.922782	344246.367116	52.337460
3277.183882	343991.770714	52.342465
3276.531371	343713.189457	52.347469
3275.768456	343435.999410	52.352474
3274.543989	343162.957725	52.357479
3274.317319	342887.428543	52.362484
3273.773660	342626.455596	52.367489
3273.186648	342355.234190	52.372493
3272.470394	342079.402252	52.377498
3271.542494	341805.513283	52.382503
3271.240979	341526.070385	52.387508
3270.008018	341258.464581	52.392513
3269.698365	340994.618264	52.397517
3268.745532	340722.686720	52.402522
3267.681424	340462.605154	52.407527
3267.460646	340193.166568	52.412532
3266.657184	339930.238538	52.417537
3266.022614	339666.923995	52.422541
3265.522403	339403.076154	52.427546
3264.746142	339144.414326	52.432551
3264.553171	338866.260863	52.437556
3263.710981	338602.238131	52.442561
3262.917723	338320.952348	52.447565
3262.447872	338051.697292	52.452570
3261.771728	337789.652248	52.457575
3261.088893	337517.707808	52.462580
3260.177049	337244.706757	52.467585
3259.313001	336989.077061	52.472589
3259.145529	336716.302291	52.477594
3258.295651	336440.843306	52.482599
3257.892447	336169.378289	52.487604
3257.115472	335900.953155	52.492609
3256.001646	335629.657557	52.497613
3255.424918	335353.738902	52.502618
3254.746856	335097.100943	52.507623
3254.238526	334822.491124	52.512628
3253.008723	334561.898360	52.517633
3252.739803	334298.493443	52.522637
3251.926522	334024.186013	52.527642
3251.539936	333767.008201	52.532647
3250.748632	333495.748220	52.537652
3249.979680	333240.974536	52.542657
3249.571397	332976.925139	52.547661
3248.979083	332705.932543	52.552666
3248.257228	332442.544870	52.557671
3247.890389	332173.063534	52.562676
3246.979565	331909.247423	52.567681
3245.735796	331629.834773	52.572685
3245.491786	331370.915918	52.577690
3244.813816	331112.426268	52.582695
3244.592265	330843.269834	52.587700
3244.178771	330592.036987	52.592705
3242.911987	330305.826064	52.597709
3242.569394	330034.828419	52.602714
3241.679396	329774.052636	52.607719
3240.829561	329490.718663	52.612724
3240.122815	329229.272745	52.617729
3239.727688	328956.751738	52.622733
3239.248111	328691.624907	52.627738
3238.424535	328425.715672	52.632743
3237.651321	328141.343743	52.637748
3237.048768	327879.924696	52.642753
3235.783707	327609.938335	52.647757
3235.178043	327342.332424	52.652762
3234.332807	327086.143537	52.657767
3234.068704	326820.080383	52.662772
3233.281947	326563.599217	52.667777
3232.498804	326295.458824	52.672781
3231.943575	326046.928089	52.677786
3231.398863	325786.049686	52.682791
3230.848280	325511.426321	52.687796
3229.895104	325255.426027	52.692801
3229.257754	324985.371216	52.697805
3228.924780	324723.001115	52.702810
3227.914016	324476.730625	52.707815
3227.240376	324200.747737	52.712820
3226.910764	323949.420683	52.717825
3225.929895	323679.545949	52.722829
3225.027218	323420.067448	52.727834
3224.686462	323157.615519	52.732839
3224.197791	322898.216813	52.737844
3223.080070	322644.473557	52.742849
3222.084463	322376.606511	52.747853
3222.243700	322125.672115	52.752858
3221.401258	321872.056859	52.757863
3220.820555	321599.482811	52.762868
3220.150046	321345.530594	52.767873
3219.598822	321074.400174	52.772877
3218.847650	320814.146708	52.777882
3218.016779	320552.480285	52.782887
3217.788682	320279.662133	52.787892
3216.852206	320021.957182	52.792897
3215.978714	319755.330935	52.797901
3215.528332	319482.445548	52.802906
3214.500011	319235.724611	52.807911
3214.021370	318968.849494	52.812916
3213.378156	318698.030241	52.817921
3212.688655	318451.248470	52.822925
3212.227399	318182.967096	52.827930
3211.072858	317922.770925	52.832935
3210.755684	317657.237567	52.837940
3209.776080	317410.221456	52.842945
3209.274969	317143.215538	52.847949
3208.623947	316884.914948	52.852954
3208.097470	316643.317300	52.857959
3207.848678	316374.203237	52.862964
3207.013587	316100.631435	52.867969
3206.421464	315835.367008	52.872973
3205.687928	315573.104222	52.877978
3204.857292	315301.437783	52.882983
3204.163024	315035.398557	52.887988
3203.381966	314780.167169	52.892993
3202.951648	314511.000492	52.897997
3202.613651	314245.457482	52.903002
3201.869020	313985.380010	52.908007
3200.893293	313704.898291	52.913012
3199.998016	313451.081809	52.918017
3199.224229	313186.500326	52.923021
3198.660903	312927.177242	52.928026
3197.503345	312663.906854	52.933031
3197.128365	312413.052854	52.938036
3196.141966	312158.890990	52.943041
3195.932591	311900.140257	52.948045
3195.088420	311647.607142	52.953050
3194.147939	311403.541940	52.958055
3193.684933	311141.445862	52.963060
3193.211101	310891.520106	52.968065
3192.537507	310635.950270	52.973069
3191.928222	310383.601896	52.978074
3191.391231	310126.123028	52.983079
3190.882983	309862.069876	52.988084
3189.779864	309607.461030	52.993089
3189.176352	309347.852317	52.998093
3188.741721	309087.093665	53.003098
3187.723270	308836.312212	53.008103
3187.408372	308567.766173	53.013108
3186.763601	308314.500542	53.018113
3185.639404	308059.304659	53.023117
3185.057278	307802.665980	53.028122
3184.418901	307555.201708	53.033127
3184.020886	307287.200190	53.038132
3183.431119	307043.290459	53.043137
3182.743802	306785.138881	53.048141
3182.250495	306520.002654	53.053146
3181.011030	306269.811023	53.058151
3180.385012	306002.837177	53.063156
3179.941874	305748.179638	53.068161
3179.490039	305492.860824	53.073165
3178.797484	305238.931771	53.078170
3177.585749	304981.296966	53.083175
3177.326929	304718.380947	53.088180
3176.641407	304470.915460	53.093185
3176.004385	304208.597149	53.098189
3175.782062	303947.225644	53.103194
3174.930154	303696.680079	53.108199
3174.316451	303437.639939	53.113204
3173.378452	303164.956190	53.118209
3173.026917	302906.226150	53.123213
3172.458132	302648.194461	53.128218
3171.544008	302389.839088	53.133223
3170.660000	302121.038522	53.138228
3170.336324	301871.084997	53.143233
3169.668259	301614.976917	53.148237
3169.158035	301348.198067	53.153242
3168.219740	301083.834064	53.158247
3167.453888	300826.085442	53.163252
3166.876407	300570.519127	53.168257
3166.207474	300303.866207	53.173261
3165.992236	300040.266885	53.178266
3164.746540	299781.171448	53.183271
3164.417245	299515.171217	53.188276
3163.514082	299256.576007	53.193281
3162.713882	298998.802773	53.198285
3162.279613	298732.767372	53.203290
3161.200373	298480.922290	53.208295
3160.765211	298217.711990	53.213300
3159.988754	297967.468942	53.218305
3159.127427	297700.408779	53.223309
3158.840682	297450.080768	53.228314
3158.513333	297199.886380	53.233319
3157.549903	296934.802265	53.238324
3156.732117	296675.396324	53.243329
3156.000829	296412.766578	53.248333
3155.618411	296145.391319	53.253338
3154.738012	295895.059029	53.258343
3154.260494	295640.863265	53.263348
3153.364119	295382.511495	53.268353
3152.425549	295124.268153	53.273357
3152.017831	294868.378005	53.278362
3151.205277	294614.287927	53.283367
3150.832636	294358.339638	53.288372
3150.229702	294096.191456	53.293377
3148.978836	293835.375590	53.298381
3148.861797	293580.018404	53.303386
3147.939926	293331.367815	53.308391
3147.533335	293070.864268	53.313396
3146.694542	292819.448230	53.318401
3145.775624	292562.112175	53.323405
3145.437378	292300.321964	53.328410
3144.721470	292061.055137	53.333415
3144.077124	291799.825358	53.338420
3143.465040	291541.008594	53.343425
3142.638742	291294.145196	53.348429
3142.290482	291032.888586	53.353434
3141.549838	290787.817475	53.358439
3140.633869	290521.996713	53.363444
3140.163826	290278.380744	53.368449
3139.433812	290016.244938	53.373453
3139.252858	289759.413300	53.378458
3137.837502	289500.169123	53.383463
3137.489019	289249.043691	53.388468
3136.522707	288988.881399	53.393473
3136.235295	288726.310747	53.398477
3135.384007	288479.445926	53.403482
3134.587239	288234.481194	53.408487
3134.234424	287971.538191	53.413492
3133.316851	287720.761614	53.418497
3132.645291	287463.245185	53.423501
3132.580322	287208.654994	53.428506
3131.478939	286948.384348	53.433511
3130.763428	286693.980706	53.438516
3130.136764	286447.099165	53.443521
3129.265216	286191.753555	53.448525
3128.613660	285925.776247	53.453530
3128.079133	285681.602402	53.458535
3127.543566	285419.144023	53.463540
3126.890788	285163.173451	53.468545
3126.189807	284912.354719	53.473549
3125.827661	284653.659693	53.478554
3124.626383	284403.027407	53.483559
3124.148991	284134.826954	53.488564
3123.367939	283885.853676	53.493569
3122.811039	283626.935458	53.498573
3122.176869	283379.438736	53.503578
3121.511153	283127.159396	53.508583
3120.999784	282864.386741	53.513588
3120.418614	282605.139883	53.518593
3119.394509	282356.867755	53.523597
3119.154186	282102.960656	53.528602
3118.166264	281849.206334	53.533607
3117.825172	281578.838999	53.538612
3116.931011	281323.692662	53.543617
3116.246559	281069.401425	53.548621
3115.803514	280806.028007	53.553626
3114.838283	280554.559786	53.558631
3114.530393	280294.625912	53.563636
3113.604139	280036.045139	53.568641
3112.863067	279779.011268	53.573645
3112.005475	279514.738965	53.578650
3111.302125	279261.772545	53.583655
3111.083561	279012.695741	53.588660
3110.079444	278758.175601	53.593665
3109.161067	278502.519927	53.598669
3109.037772	278244.054070	53.603674
3108.022259	277987.777619	53.608679
3107.619122	277737.890238	53.613684
3106.917197	277494.522146	53.618689
3106.075840	277235.337193	53.623693
3105.340503	276973.587101	53.628698
3104.607764	276730.045063	53.633703
3103.868577	276476.418925	53.638708
3103.314619	276223.270169	53.643713
3102.770836	275981.732319	53.648717
3102.376536	275721.577721	53.653722
3101.470928	275472.537394	53.658727
3101.133001	275213.085626	53.663732
3100.370799	274959.690806	53.668737
3099.438308	274713.964934	53.673741
3099.226655	274452.020390	53.678746
3098.280868	274200.897190	53.683751
3097.665090	273944.929500	53.688756
3096.821067	273703.873404	53.693761
3096.160613	273445.289677	53.698765
3095.441254	273180.578113	53.703770
3094.795705	272937.348092	53.708775
3094.111402	272680.244739	53.713780
3093.642607	272425.905722	53.718785
3092.701832	272178.803429	53.723789
3092.013620	271910.876322	53.728794
3091.320802	271668.162525	53.733799
3090.870820	271407.146834	53.738804
3090.555677	271166.125325	53.743809
3090.034392	270909.629096	53.748813
3089.414502	270642.376704	53.753818
3088.818564	270386.529450	53.758823
3087.848537	270122.927329	53.763828
3086.590464	269870.630877	53.768833
3086.158255	269605.663045	53.773837
3085.773736	269362.843713	53.778842
3084.599941	269107.068644	53.783847
3083.823691	268847.761849	53.788852
3083.304649	268609.396317	53.793857
3082.973713	268365.319175	53.798861
3082.016895	268100.159607	53.803866
3081.373942	267864.004958	53.808871
3081.097240	267602.217915	53.813876
3080.645989	267353.601900	53.818881
3079.483605	267098.994931	53.823885
3078.840566	266845.088573	53.828890
3077.845305	266592.974041	53.833895
3077.692576	266338.830791	53.838900
3077.177808	266087.194155	53.843905
3075.907419	265841.824229	53.848909
3075.641516	265580.135893	53.853914
3074.993640	265334.888548	53.858919
3074.111671	265086.446636	53.863924
3073.510920	264834.747588	53.868929
3072.688405	264585.098268	53.873933
3072.393786	264331.614844	53.878938
3071.595445	264083.107211	53.883943
3070.908852	263822.992425	53.888948
3070.158002	263580.334095	53.893953
3069.153364	263330.969992	53.898957
3068.824168	263085.463406	53.903962
3068.028197	262828.677716	53.908967
3067.512827	262583.712104	53.913972
3066.960683	262336.205879	53.918977
3066.282854	262086.123294	53.923981
3066.145922	261830.701789	53.928986
3064.658952	261580.018698	53.933991
3064.458571	261334.973390	53.938996
3063.694386	261085.236327	53.944001
3063.351762	260825.927564	53.949005
3062.556764	260567.230847	53.954010
3061.635813	260320.041711	53.959015
3060.919894	260056.110389	53.964020
3060.371701	259796.479937	53.969025
3059.756063	259552.141846	53.974029
3059.214465	259297.985821	53.979034
3058.189018	259041.543876	53.984039
3057.987164	258785.572420	53.989044
3056.513136	258522.407036	53.994049
3056.284317	258282.561470	53.999053
3055.605837	258019.718537	54.004058
3055.000959	257774.410578	54.009063
3054.332291	257524.376418	54.014068
3053.588068	257274.915450	54.019073
3052.764648	257032.522688	54.024077
3052.317750	256771.295543	54.029082
3051.400910	256525.633335	54.034087
3051.131815	256272.627499	54.039092
3050.374664	256026.021158	54.044097
3049.699800	255774.510877	54.049101
3049.569510	255516.234906	54.054106
3048.017483	255266.428071	54.059111
3047.672936	255009.946046	54.064116
3047.128124	254762.208374	54.069121
3046.382307	254507.577729	54.074125
3045.700363	254251.204368	54.079130
3044.479672	254006.307354	54.084135
3043.917760	253745.609444	54.089140
3043.716153	253510.954878	54.094145
3042.618361	253260.816021	54.099149
3042.524354	253008.442800	54.104154
3041.516608	252761.497650	54.109159
3041.235034	252514.097404	54.114164
3040.555598	252261.289546	54.119169
3039.386040	252010.093579	54.124173
3038.887029	251768.028044	54.129178
3038.169926	251524.471751	54.134183
3037.840732	251268.369891	54.139188
3036.931870	251024.439024	54.144193
3036.273566	250773.003283	54.149197
3035.667294	250507.169283	54.154202
3034.860284	250275.878902	54.159207
3034.333712	250020.116832	54.164212
3033.911228	249765.126591	54.169217
3032.989990	249513.303301	54.174221
3032.651737	249271.440384	54.179226
3031.785220	249016.933822	54.184231
3031.260199	248764.049923	54.189236
3030.572496	248516.363939	54.194241
3030.024597	248270.003992	54.199245
3029.366866	248015.640527	54.204250
3028.518433	247760.774951	54.209255
3027.585600	247508.190581	54.214260
3026.947663	247255.581436	54.219265
3026.265335	247006.621930	54.224269
3025.511731	246756.324948	54.229274
3024.938131	246522.908027	54.234279
3024.181008	246266.728865	54.239284
3023.793564	246021.183200	54.244289
3022.923150	245772.180179	54.249293
3022.523875	245513.979353	54.254298
3021.569037	245278.692761	54.259303
3020.723807	245029.787806	54.264308
3020.510290	244787.065631	54.269313
3019.850898	244539.198919	54.274317
3019.197427	244284.480560	54.279322
3018.021999	244037.084399	54.284327
3017.724570	243794.937564	54.289332
3016.802114	243544.315099	54.294337
3016.029354	243311.087120	54.299341
3015.563255	243051.677150	54.304346
3015.064240	242814.811846	54.309351
3014.497561	242560.895017	54.314356
3013.829483	242308.829396	54.319361
3013.059330	242062.893643	54.324365
3012.309000	241809.543674	54.329370
3011.410156	241569.080388	54.334375
3011.097665	241317.082244	54.339380
3010.601853	241076.856146	54.344385
3009.400255	240826.436550	54.349389
3009.078167	240574.186080	54.354394
3008.369465	240332.468999	54.359399
3007.890364	240077.189765	54.364404
3007.236817	239840.251595	54.369409
3006.749766	239585.636378	54.374413
3006.117645	239329.747386	54.379418
3004.647178	239092.592985	54.384423
3004.169249	238834.258798	54.389428
3003.799084	238597.451721	54.394433
3002.958032	238351.175162	54.399437
3002.329153	238107.969611	54.404442
3001.790069	237856.905119	54.409447
3001.179305	237606.922779	54.414452
3000.479069	237360.903405	54.419457
2999.575176	237124.469240	54.424461
2999.168562	236875.726227	54.429466
2998.178220	236633.806520	54.434471
2997.556941	236390.346960	54.439476
2997.240728	236143.728609	54.444481
2996.369704	235905.023680	54.449485
2995.770001	235646.943362	54.454490
2994.783787	235407.265511	54.459495
2994.578594	235158.693950	54.464500
2993.580976	234914.511046	54.469505
2992.965524	234667.461826	54.474509
2992.568031	234427.710090	54.479514
2991.679511	234181.726837	54.484519
2991.279685	233937.544946	54.489524
2990.661035	233684.462012	54.494529
2989.707639	233441.801504	54.499533
2989.103281	233194.726923	54.504538
2988.377522	232945.024923	54.509543
2987.514895	232701.331274	54.514548
2987.083209	232461.689895	54.519553
2986.291505	232218.392281	54.524557
2986.108807	231963.582062	54.529562
2985.144412	231719.092298	54.534567
2984.490637	231469.176451	54.539572
2983.970521	231219.747475	54.544577
2983.061325	230976.064312	54.549581
2982.651831	230731.124701	54.554586
2981.644708	230489.929228	54.559591
2981.256291	230233.068670	54.564596
2980.713161	229987.465471	54.569601
2979.780886	229748.855890	54.574605
2979.488298	229490.757832	54.579610
2978.399489	229250.724223	54.584615
2978.035632	229006.441671	54.589620
2977.220339	228762.211187	54.594625
2976.391966	228519.587686	54.599629
2976.030884	228262.165575	54.604634
2975.225190	228020.812317	54.609639
2974.770954	227775.070261	54.614644
2974.092638	227522.083767	54.619649
2973.132904	227277.167448	54.624653
2972.672371	227022.438455	54.629658
2971.801663	226786.751755	54.634663
2971.296638	226542.191956	54.639668
2970.442893	226287.811629	54.644673
2970.363674	226040.862634	54.649677
2969.593417	225795.152637	54.654682
2968.452847	225552.180212	54.659687
2968.014181	225289.556541	54.664692
2967.816559	225047.824517	54.669697
2966.852031	224801.945851	54.674701
2965.947983	224546.737134	54.679706
2965.033803	224297.616779	54.684711
2964.657611	224064.447876	54.689716
2963.942700	223813.970253	54.694721
2963.142715	223562.616400	54.699725
2962.352171	223318.595291	54.704730
2961.931796	223077.083351	54.709735
2961.425207	222823.083481	54.714740
2960.508318	222577.302916	54.719745
2959.647670	222332.837401	54.724749
2959.338681	222087.157689	54.729754
2958.748935	221847.281419	54.734759
2957.854313	221606.821121	54.739764
2957.440497	221356.373541	54.744769
2956.538597	221116.221071	54.749773
2955.785112	220863.922774	54.754778
2955.077701	220625.087702	54.759783
2954.575155	220370.048418	54.764788
2953.878199	220128.717123	54.769793
2953.183157	219886.443853	54.774797
2952.581318	219636.312290	54.779802
2951.977798	219400.441354	54.784807
2951.367496	219155.659742	54.789812
2950.862628	218906.277185	54.794817
2949.894433	218660.284650	54.799821
2949.585980	218405.216741	54.804826
2948.814442	218175.131962	54.809831
2948.206398	217918.333955	54.814836
2947.815184	217674.511358	54.819841
2946.713449	217430.377853	54.824845
2946.388079	217179.491790	54.829850
2945.484831	216921.167939	54.834855
2945.099161	216677.092097	54.839860
2944.273477	216430.214682	54.844865
2943.307625	216181.070137	54.849869
2942.844811	215934.692112	54.854874
2942.306097	215694.693406	54.859879
2941.044141	215441.985541	54.864884
2940.533892	215193.504025	54.869889
2939.626455	214953.621038	54.874893
2939.284990	214704.551733	54.879898
2938.097240	214469.377508	54.884903
2937.833778	214224.573831	54.889908
2937.335464	213981.771519	54.894913
2936.529405	213740.193680	54.899917
2935.952234	213494.274194	54.904922
2934.947604	213264.622438	54.909927
2934.452257	213025.310401	54.914932
2933.883456	212777.456219	54.919937
2932.762748	212547.927901	54.924941
2932.365564	212300.223900	54.929946
2931.678731	212078.210312	54.934951
2931.509035	211831.690877	54.939956
2931.163018	211593.299115	54.944961
2930.313477	211343.026960	54.949965
2929.676740	211087.728633	54.954970
2928.662511	210855.130966	54.959975
2927.871887	210605.207262	54.964980
2927.569910	210355.226226	54.969985
2926.701381	210110.995150	54.974989
2926.320265	209868.896608	54.979994
2924.995048	209623.319086	54.984999
2924.531824	209385.640724	54.990004
2923.883307	209144.659260	54.995009
2922.953275	208903.573807	55.000013
2922.331884	208662.639981	55.005018
2921.722445	208437.745207	55.010023
2921.062839	208194.400444	55.015028
2920.646803	207959.391376	55.020033
2919.836159	207725.239676	55.025037
2919.119915	207481.715698	55.030042
2918.554835	207247.841635	55.035047
2918.182825	207017.677942	55.040052
2917.379747	206762.331764	55.045057
2917.043745	206524.117792	55.050061
2916.353412	206272.738428	55.055066
2915.549463	206031.410587	55.060071
2915.189122	205792.362731	55.065076
2914.586073	205536.540672	55.070081
2913.619932	205294.173434	55.075085
2913.152835	205039.831875	55.080090
2912.701641	204788.225347	55.085095
2911.913926	204545.422551	55.090100
2911.193626	204296.893288	55.095105
2910.249798	204046.442622	55.100109
2910.021466	203801.853488	55.105114
2909.134072	203553.215126	55.110119
2908.152596	203291.545723	55.115124
2907.350150	203050.455899	55.120129
2906.574004	202815.370712	55.125133
2906.022137	202568.231227	55.130138
2905.184889	202330.955770	55.135143
2904.861258	202090.474573	55.140148
2904.293222	201840.857990	55.145153
2903.311225	201604.093285	55.150157
2902.816848	201353.269186	55.155162
2902.203733	201119.943564	55.160167
2901.421641	200876.846020	55.165172
2900.483667	200628.684230	55.170177
2899.733956	200399.126633	55.175181
2898.899047	200157.555282	55.180186
2898.249744	199939.260002	55.185191
2898.025390	199692.914292	55.190196
2897.571931	199454.907894	55.195201
2896.539027	199217.154050	55.200205
2896.159490	198977.698237	55.205210
2895.403271	198735.443599	55.210215
2894.530590	198500.261473	55.215220
2894.013082	198262.919189	55.220225
2893.017399	198022.617246	55.225229
2892.758040	197784.786966	55.230234
2891.825816	197550.763794	55.235239
2891.298200	197304.694634	55.240244
2890.497675	197070.115983	55.245249
2889.731288	196844.455008	55.250253
2889.681078	196599.095967	55.255258
2889.379185	196375.495555	55.260263
2888.214635	196134.427172	55.265268
2887.847035	195880.991510	55.270273
2886.731326	195647.057133	55.275277
2885.940080	195400.899903	55.280282
2885.028843	195174.161898	55.285287
2884.574608	194931.067229	55.290292
2883.985919	194692.565827	55.295297
2883.008362	194464.250568	55.300301
2882.674317	194227.947478	55.305306
2882.231299	193994.693125	55.310311
2881.627281	193743.024315	55.315316
2881.243163	193510.423484	55.320321
2880.324765	193273.129112	55.325325
2879.418164	193017.480097	55.330330
2878.579964	192787.428661	55.335335
2877.784015	192549.772386	55.340340
2877.224502	192308.563759	55.345345
2876.273972	192079.845020	55.350349
2875.789119	191845.320123	55.355354
2875.071100	191622.736179	55.360359
2874.700851	191385.736997	55.365364
2873.815837	191150.264875	55.370369
2873.388755	190920.709987	55.375373
2872.941462	190677.082965	55.380378
2871.963782	190438.345722	55.385383
2871.270047	190205.657226	55.390388
2871.083367	189969.459350	55.395393
2870.115762	189733.357649	55.400397
2869.422450	189492.730052	55.405402
2868.651104	189259.002070	55.410407
2867.934539	189025.011088	55.415412
2867.241332	188793.180600	55.420417
2866.522523	188561.139022	55.425421
2866.157037	188321.516398	55.430426
2865.359056	188097.291700	55.435431
2864.787395	187855.720797	55.440436
2864.352898	187618.110892	55.445441
2863.541615	187379.764548	55.450445
2863.070151	187141.284737	55.455450
2862.298667	186905.224298	55.460455
2861.470406	186665.801993	55.465460
2860.816362	186434.661261	55.470465
2860.050128	186202.204348	55.475469
2859.469253	185958.377529	55.480474
2858.748399	185729.987182	55.485479
2858.101493	185499.103490	55.490484
2857.518474	185258.703352	55.495489
2856.611575	185026.007972	55.500493
2856.096224	184787.430815	55.505498
2855.530260	184561.996560	55.510503
2855.027930	184327.427807	55.515508
2854.488590	184088.641348	55.520513
2853.478426	183852.354272	55.525517
2852.835175	183619.874136	55.530522
2852.336533	183383.959752	55.535527
2851.834693	183142.816649	55.540532
2851.244301	182896.243148	55.545537
2850.378310	182661.438107	55.550541
2850.116761	182413.283493	55.555546
2849.058639	182179.340498	55.560551
2848.375317	181930.738393	55.565556
2847.788501	181697.785850	55.570561
2846.532666	181464.732299	55.575565
2846.043313	181215.756724	55.580570
2845.198364	180989.099431	55.585575
2844.698815	180758.668321	55.590580
2844.354145	180529.382438	55.595585
2843.559034	180292.883064	55.600589
2842.628875	180057.871187	55.605594
2841.977174	179832.750925	55.610599
2841.468835	179603.471535	55.615604
2840.888978	179367.499379	55.620609
2840.164138	179134.416123	55.625613
2839.697371	178897.574183	55.630618
2838.793915	178668.620868	55.635623
2838.188929	178434.502263	55.640628
2838.071227	178199.207125	55.645633
2837.067772	177960.577911	55.650637
2836.232436	177723.829727	55.655642
2835.992935	177489.614744	55.660647
2835.267811	177248.879901	55.665652
2834.405461	177000.751406	55.670657
2833.137249	176770.545490	55.675661
2832.854110	176536.647688	55.680666
2832.065547	176309.670153	55.685671
2831.202326	176071.343854	55.690676
2830.822156	175838.547385	55.695681
2830.150966	175614.123143	55.700685
2829.516105	175386.334601	55.705690
2828.682692	175157.792149	55.710695
2828.194294	174920.157940	55.715700
2827.759311	174691.129647	55.720705
2827.149107	174451.024651	55.725709
2826.538023	174231.431304	55.730714
2825.762096	173986.827296	55.735719
2824.956929	173752.573631	55.740724
2824.336502	173516.279219	55.745729
2823.271534	173277.084662	55.750733
2822.781404	173048.607784	55.755738
2822.139084	172821.939226	55.760743
2821.495164	172589.737442	55.765748
2821.266361	172356.918736	55.770753
2820.107541	172129.158434	55.775757
2819.690397	171890.534305	55.780762
2819.053767	171662.254388	55.785767
2818.515864	171427.380993	55.790772
2818.321784	171180.147100	55.795777
2817.101751	170942.644545	55.800781
2816.562990	170704.861355	55.805786
2815.788054	170468.595531	55.810791
2814.963310	170232.899187	55.815796
2814.549065	169998.520611	55.820801
2813.808154	169777.175835	55.825805
2813.361799	169533.288735	55.830810
2812.834811	169294.263854	55.835815
2812.059993	169047.941858	55.840820
2811.079838	168816.871888	55.845825
2810.201106	168580.480644	55.850829
2809.855198	168341.862256	55.855834
2808.726679	168108.467608	55.860839
2808.270638	167884.971310	55.865844
2807.715926	167646.392204	55.870849
2806.841186	167425.921146	55.875853
2806.629751	167191.700179	55.880858
2805.711374	166955.145961	55.885863
2804.787790	166741.110962	55.890868
2804.359410	166489.374978	55.895873
2803.358373	166268.905667	55.900877
2802.871330	166038.961249	55.905882
2802.206996	165813.793335	55.910887
2801.422540	165574.208515	55.915892
2801.254743	165345.536091	55.920897
2800.020237	165122.389983	55.925901
2799.459817	164893.977785	55.930906
2798.782461	164666.795234	55.935911
2798.015551	164437.860948	55.940916
2797.562926	164211.850805	55.945921
2796.893847	163985.141007	55.950925
2796.633020	163743.746548	55.955930
2796.083321	163520.885826	55.960935
2795.436864	163279.407177	55.965940
2794.463305	163038.685390	55.970945
2793.900745	162820.702375	55.975949
2793.245088	162580.183201	55.980954
2792.274470	162343.802393	55.985959
2791.623031	162110.713741	55.990964
2791.170751	161882.756683	55.995969
2790.294481	161658.104188	56.000973
2789.545381	161426.142577	56.005978
2788.704240	161200.265357	56.010983
2787.859166	160981.818402	56.015988
2787.450950	160749.013576	56.020993
2786.840027	160528.328405	56.025997
2786.459244	160300.749153	56.031002
2785.586969	160079.513160	56.036007
2785.256307	159852.029512	56.041012
2784.607525	159621.141766	56.046017
2783.535070	159392.947889	56.051021
2783.113207	159149.978696	56.056026
2782.232554	158934.321219	56.061031
2781.533978	158708.725499	56.066036
2780.999628	158483.013900	56.071041
2780.228750	158259.111896	56.076045
2779.688830	158025.441618	56.081050
2779.065177	157799.570935	56.086055
2778.024988	157572.424480	56.091060
2777.639675	157346.719046	56.096065
2777.030275	157120.709745	56.101069
2776.733878	156892.193502	56.106074
2776.162793	156669.054553	56.111079
2774.839083	156434.064645	56.116084
2774.544301	156197.424911	56.121089
2773.631421	155973.826733	56.126093
2773.091819	155741.504859	56.131098
2772.431732	155510.947302	56.136103
2771.569164	155286.186975	56.141108
2771.228600	155059.799806	56.146113
2770.412542	154841.087808	56.151117
2769.533719	154598.579820	56.156122
2769.081084	154379.248648	56.161127
2768.249875	154147.939667	56.166132
2767.827791	153917.248864	56.171137
2767.190501	153707.580236	56.176141
2766.434923	153474.100261	56.181146
2765.664991	153249.055797	56.186151
2765.321844	153013.778481	56.191156
2764.598165	152799.067921	56.196161
2763.425473	152563.477251	56.201165
2763.107303	152330.323541	56.206170
2762.371325	152105.190809	56.211175
2761.420220	151893.016639	56.216180
2761.019560	151663.200156	56.221185
2759.992686	151449.706076	56.226189
2759.683901	151219.240675	56.231194
2759.083684	150997.804467	56.236199
2758.296559	150779.059254	56.241204
2757.626576	150553.377441	56.246209
2756.490556	150332.964939	56.251213
2756.354396	150105.872004	56.256218
2755.667040	149885.576142	56.261223
2754.978387	149672.123138	56.266228
2754.633609	149440.504662	56.271233
2753.802279	149217.312540	56.276237
2753.167224	148997.864858	56.281242
2752.418585	148775.920093	56.286247
2751.739767	148540.282373	56.291252
2751.392887	148308.455007	56.296257
2750.336098	148090.534282	56.301261
2749.966987	147861.536371	56.306266
2749.324030	147642.072504	56.311271
2748.620275	147415.334315	56.316276
2747.784218	147180.520372	56.321281
2747.030838	146961.257398	56.326285
2746.448157	146743.225358	56.331290
2745.942160	146510.190243	56.336295
2745.189012	146278.737368	56.341300
2744.703888	146058.098800	56.346305
2744.042686	145844.879058	56.351309
2743.577138	145612.453017	56.356314
2742.783083	145387.293904	56.361319
2741.758460	145153.542262	56.366324
2741.569870	144918.555767	56.371329
2740.421765	144699.437298	56.376333
2739.677228	144469.113258	56.381338
2739.073612	144247.285265	56.386343
2738.515353	144028.197179	56.391348
2737.820396	143806.730782	56.396353
2736.978870	143585.990075	56.401357
2736.541138	143356.930239	56.406362
2735.745601	143142.363457	56.411367
2735.001281	142915.647362	56.416372
2734.102364	142688.348857	56.421377
2733.710564	142476.107272	56.426381
2732.790964	142252.387658	56.431386
2732.125451	142038.809659	56.436391
2731.224774	141820.213132	56.441396
2731.322510	141599.158880	56.446401
2730.336834	141387.724534	56.451405
2729.842082	141159.514927	56.456410
2729.305215	140943.315311	56.461415
2728.487469	140718.291227	56.466420
2727.775288	140493.771779	56.471425
2727.435216	140278.051144	56.476429
2726.773796	140052.953757	56.481434
2725.876482	139829.805067	56.486439
2725.061039	139606.681950	56.491444
2724.656775	139373.586798	56.496449
2723.741991	139161.988502	56.501453
2723.419896	138929.441643	56.506458
2722.715268	138708.784302	56.511463
2722.085614	138491.941979	56.516468
2721.495257	138264.441406	56.521473
2720.640384	138043.292800	56.526477
2719.739569	137816.903364	56.531482
2719.093001	137599.078018	56.536487
2718.533114	137372.035787	56.541492
2718.009267	137150.798230	56.546497
2717.256882	136947.334121	56.551501
2716.614837	136706.924842	56.556506
2716.239857	136484.878045	56.561511
2715.336261	136259.173146	56.566516
2714.836812	136034.277769	56.571521
2713.768741	135823.641544	56.576525
2713.101749	135597.188794	56.581530
2712.648239	135380.641242	56.586535
2712.195880	135151.637990	56.591540
2711.322297	134932.622903	56.596545
2710.392125	134708.750627	56.601549
2710.173799	134485.635235	56.606554
2709.099243	134267.993499	56.611559
2708.533535	134036.360710	56.616564
2707.859406	133814.916556	56.621569
2707.087105	133604.370872	56.626573
2706.749471	133372.385976	56.631578
2706.125816	133155.665890	56.636583
2705.283554	132939.912442	56.641588
2704.863507	132712.814306	56.646593
2703.834492	132490.206808	56.651597
2703.375834	132268.685368	56.656602
2702.619866	132042.361050	56.661607
2702.167508	131830.462916	56.666612
2701.953790	131607.861881	56.671617
2700.877809	131389.553098	56.676621
2700.281424	131153.802517	56.681626
2699.683569	130924.828059	56.686631
2698.620340	130705.733710	56.691636
2698.154992	130473.435352	56.696641
2697.206041	130252.176675	56.701645
2696.839531	130033.628687	56.706650
2695.876728	129811.778076	56.711655
2694.978510	129594.366098	56.716660
2694.730502	129368.380349	56.721665
2693.985487	129156.384559	56.726669
2693.395852	128929.125883	56.731674
2692.556788	128715.954478	56.736679
2691.537790	128493.893868	56.741684
2691.190672	128281.060676	56.746689
2690.233468	128070.430068	56.751693
2690.161186	127855.023798	56.756698
2689.093409	127637.247510	56.761703
2688.609728	127418.496033	56.766708
2688.111089	127194.487515	56.771713
2687.360703	126985.976452	56.776717
2686.850689	126756.317978	56.781722
2685.925810	126544.650009	56.786727
2685.261354	126325.937042	56.791732
2684.980066	126098.785830	56.796737
2683.941449	125882.020647	56.801741
2683.324454	125664.956177	56.806746
2682.529735	125452.549055	56.811751
2682.036167	125229.011229	56.816756
2681.416637	125016.450081	56.821761
2680.445562	124802.425637	56.826765
2679.882318	124584.304870	56.831770
2679.292631	124361.120132	56.836775
2678.480168	124141.380503	56.841780
2678.010890	123920.351241	56.846785
2677.152071	123718.424609	56.851789
2676.656446	123495.763764	56.856794
2675.799437	123280.879095	56.861799
2675.246848	123065.638955	56.866804
2674.607635	122852.105069	56.871809
2673.707644	122642.950049	56.876813
2673.682855	122418.768097	56.881818
2672.666964	122201.300769	56.886823
2671.905832	121996.865792	56.891828
2671.068843	121771.823694	56.896833
2670.331695	121569.534786	56.901837
2670.186808	121350.056979	56.906842
2669.247148	121141.960989	56.911847
2668.633439	120926.517821	56.916852
2668.200157	120713.827826	56.921857
2667.018188	120501.800934	56.926861
2666.705677	120275.930792	56.931866
2665.929821	120065.285971	56.936871
2665.336649	119857.546258	56.941876
2664.827288	119637.101509	56.946881
2663.892175	119429.639219	56.951885
2663.383793	119210.480655	56.956890
2662.813161	118998.474332	56.961895
2661.966364	118784.318856	56.966900
2661.367535	118564.075255	56.971905
2660.670403	118357.240446	56.976909
2659.928327	118140.429255	56.981914
2659.660733	117924.288106	56.986919
2658.911526	117708.065719	56.991924
2658.015078	117487.042600	56.996929
2657.152756	117279.087575	57.001933
2656.791234	117060.644057	57.006938
2656.031814	116848.558499	57.011943
2655.359070	116638.250875	57.016948
2654.708499	116417.727392	57.021953
2653.875008	116214.653182	57.026957
2653.410397	115986.860265	57.031962
2652.799027	115781.134256	57.036967
2651.706532	115581.602143	57.041972
2651.443458	115363.675412	57.046977
2650.474060	115147.916232	57.051981
2650.236425	114942.742068	57.056986
2649.331640	114730.379337	57.061991
2648.716120	114513.116331	57.066996
2648.364575	114303.456780	57.072001
2647.228743	114083.453311	57.077005
2646.713568	113861.706849	57.082010
2646.315628	113660.189456	57.087015
2645.202718	113441.025383	57.092020
2645.104446	113228.408958	57.097025
2644.244155	113022.046726	57.102029
2643.693102	112802.740741	57.107034
2642.590403	112597.515404	57.112039
2641.857597	112381.419203	57.117044
2641.626795	112162.190471	57.122049
2641.075903	111953.369869	57.127053
2640.397499	111733.090560	57.132058
2639.879955	111516.113221	57.137063
2639.105742	111314.575281	57.142068
2638.389566	111094.574174	57.147073
2637.704099	110873.007330	57.152077
2637.053375	110656.745281	57.157082
2636.397273	110428.674092	57.162087
2635.497224	110224.206260	57.167092
2634.825546	109996.052381	57.172097
2634.191067	109788.468823	57.177101
2633.523888	109579.800176	57.182106
2632.564668	109366.014001	57.187111
2631.660199	109153.998152	57.192116
2631.210691	108936.559422	57.197121
2630.366303	108730.251616	57.202125
2629.706953	108535.877054	57.207130
2628.982659	108324.357503	57.212135
2628.454913	108113.009184	57.217140
2628.288462	107909.766601	57.222145
2626.953190	107704.452105	57.227149
2626.418610	107495.357550	57.232154
2625.976533	107294.439863	57.237159
2625.092748	107085.230358	57.242164
2624.872988	106879.515518	57.247169
2623.917557	106676.632889	57.252173
2623.405297	106469.117098	57.257178
2622.508637	106268.729175	57.262183
2622.111627	106065.438203	57.267188
2621.260497	105854.175430	57.272193
2620.487974	105644.881855	57.277197
2619.765527	105445.244887	57.282202
2619.647210	105230.115699	57.287207
2618.617068	105028.997920	57.292212
2618.176850	104818.815894	57.297217
2617.628090	104616.818940	57.302221
2617.250742	104403.073970	57.307226
2616.606413	104189.935056	57.312231
2615.349991	103975.988236	57.317236
2615.127854	103762.386944	57.322241
2614.280183	103555.687501	57.327245
2613.490235	103345.107069	57.332250
2612.998732	103138.337299	57.337255
2612.171834	102930.851943	57.342260
2611.751577	102711.071323	57.347265
2611.034635	102509.169939	57.352269
2610.228151	102298.359433	57.357274
2609.582451	102092.055916	57.362279
2608.934073	101881.539147	57.367284
2608.222497	101661.956751	57.372289
2607.056686	101461.092401	57.377293
2606.638371	101260.139907	57.382298
2606.212144	101047.649307	57.387303
2605.699686	100845.573421	57.392308
2604.888333	100638.617731	57.397313
2604.270708	100431.681356	57.402317
2603.612713	100215.980616	57.407322
2602.822159	100007.712363	57.412327
2601.853566	99804.554523	57.417332
2601.608003	99598.583201	57.422337
2600.732747	99392.429162	57.427341
2600.231735	99187.323649	57.432346
2599.854183	98981.113208	57.437351
2599.067713	98775.939159	57.442356
2598.512762	98552.941264	57.447361
2597.607705	98357.572440	57.452365
2597.059579	98152.476884	57.457370
2596.303374	97935.707546	57.462375
2595.661356	97729.933210	57.467380
2595.106503	97512.003214	57.472385
2594.440248	97306.128532	57.477389
2593.637842	97099.510776	57.482394
2593.049288	96885.603337	57.487399
2592.404396	96675.445775	57.492404
2591.923683	96461.701190	57.497409
2590.872356	96261.676617	57.502413
2590.267473	96051.111185	57.507418
2589.412215	95842.024706	57.512423
2588.978028	95631.465327	57.517428
2588.249441	95424.677253	57.522433
2587.455391	95232.550351	57.527437
2587.090250	95028.851387	57.532442
2586.350085	94821.936969	57.537447
2585.632090	94615.509155	57.542452
2585.287970	94407.388072	57.547457
2584.212536	94198.048279	57.552461
2583.563032	93996.405462	57.557466
2582.879937	93781.575895	57.562471
2582.023663	93577.991739	57.567476
2581.414808	93375.617170	57.572481
2580.958004	93172.761328	57.577485
2579.978816	92973.232989	57.582490
2579.361905	92767.177633	57.587495
2578.724354	92570.012012	57.592500
2578.339885	92366.274650	57.597505
2577.381388	92167.707520	57.602509
2576.720648	91963.995321	57.607514
2575.937584	91760.191492	57.612519
2575.448238	91556.218571	57.617524
2575.264198	91356.415078	57.622529
2574.699645	91166.621977	57.627533
2574.091463	90957.439138	57.632538
2573.425860	90746.357877	57.637543
2572.672335	90536.924273	57.642548
2571.981511	90317.506640	57.647553
2571.107945	90123.516640	57.652557
2570.415640	89906.679206	57.657562
2569.892921	89703.336600	57.662567
2568.798582	89497.834495	57.667572
2568.205030	89291.347503	57.672577
2567.859605	89092.909938	57.677581
2567.165768	88878.581947	57.682586
2566.340467	88672.019297	57.687591
2565.614139	88473.188744	57.692596
2565.125497	88267.885417	57.697601
2563.949552	88064.579424	57.702605
2563.227476	87869.058822	57.707610
2562.655724	87673.704457	57.712615
2562.053900	87468.598613	57.717620
2561.297741	87262.765890	57.722625
2560.433289	87075.670114	57.727629
2559.995898	86879.207981	57.732634
2559.262317	86686.065531	57.737639
2558.543852	86488.842560	57.742644
2558.290737	86285.387577	57.747649
2557.199593	86086.049170	57.752653
2556.909671	85893.757235	57.757658
2556.318065	85702.248021	57.762663
2555.622893	85500.740539	57.767668
2554.740757	85295.720348	57.772673
2553.793508	85101.605896	57.777677
2553.604142	84903.125649	57.782682
2552.914358	84715.212909	57.787687
2552.070530	84508.626033	57.792692
2551.653645	84314.230731	57.797697
2550.940838	84113.201213	57.802701
2550.240349	83926.279898	57.807706
2549.865139	83722.442806	57.812711
2548.839072	83524.358285	57.817716
2548.430090	83316.870190	57.822721
2547.394238	83126.815397	57.827725
2546.818854	82930.580965	57.832730
2546.321513	82739.542829	57.837735
2544.970161	82540.437530	57.842740
2544.753897	82339.268597	57.847745
2544.029520	82154.040194	57.852749
2543.221171	81957.200431	57.857754
2542.970573	81756.638678	57.862759
2542.456655	81572.736382	57.867764
2541.564072	81316.195771	57.872769
2540.879790	81124.904756	57.877773
2540.538565	80921.524056	57.882778
2539.824685	80717.669708	57.887783
2538.752539	80533.553974	57.892788
2538.491347	80330.082355	57.897793
2537.877704	80136.567488	57.902797
2536.761392	79938.294360	57.907802
2536.199772	79743.822507	57.912807
2535.883855	79552.316690	57.917812
2535.083690	79351.990333	57.922817
2534.117686	79160.624302	57.927821
2533.706793	78960.406079	57.932826
2533.054556	78761.740357	57.937831
2532.384965	78572.827483	57.942836
2531.599522	78370.744065	57.947841
2530.899555	78183.507634	57.952845
2530.239714	77971.810526	57.957850
2529.671184	77780.147157	57.962855
2529.064401	77581.407883	57.967860
2528.551009	77388.114843	57.972865
2527.549027	77200.240555	57.977869
2527.102224	76996.240636	57.982874
2526.220103	76802.501955	57.987879
2525.579898	76606.662508	57.992884
2524.876249	76416.942686	57.997889
2524.227369	76230.284469	58.002893
2523.376304	76029.983513	58.007898
2522.502154	75837.906947	58.012903
2522.151747	75652.413750	58.017908
2521.936163	75461.236127	58.022913
2521.160869	75269.572417	58.027917
2520.592313	75070.709296	58.032922
2519.566955	74873.657211	58.037927
2518.917730	74680.099995	58.042932
2518.486846	74483.165338	58.047937
2517.696973	74298.456057	58.052941
2517.122707	74102.430702	58.057946
2516.340637	73910.532554	58.062951
2515.581911	73703.299660	58.067956
2515.111970	73520.070338	58.072961
2514.268447	73324.402264	58.077965
2513.730986	73132.798767	58.082970
2513.240583	72936.959624	58.087975
2512.272247	72738.731065	58.092980
2511.989497	72550.589134	58.097985
2510.931405	72360.577747	58.102989
2510.555564	72167.534733	58.107994
2509.759926	71966.088005	58.112999
2508.834125	71769.775735	58.118004
2508.450414	71579.909436	58.123009
2507.397046	71396.562954	58.128013
2506.972483	71204.627284	58.133018
2506.268336	71009.564674	58.138023
2505.868621	70829.446137	58.143028
2504.946216	70628.838604	58.148033
2504.566806	70440.014916	58.153037
2503.603969	70242.302565	58.158042
2503.168272	70058.741289	58.163047
2502.260097	69867.977868	58.168052
2501.879575	69667.717683	58.173057
2501.190006	69487.418917	58.178061
2500.653527	69290.682073	58.183066
2500.108832	69085.396291	58.188071
2498.838470	68898.659259	58.193076
2498.459573	68702.845427	58.198081
2497.822986	68510.240810	58.203085
2496.830430	68320.006311	58.208090
2496.215961	68131.845211	58.213095
2495.431973	67946.275808	58.218100
2495.646575	67749.088663	58.223105
2494.362707	67568.362405	58.228109
2493.662314	67371.683820	58.233114
2492.878996	67184.878437	58.238119
2492.137950	66996.216477	58.243124
2491.884742	66804.740701	58.248129
2491.013185	66613.575204	58.253133
2490.323144	66421.588039	58.258138
2489.527145	66236.270085	58.263143
2488.801309	66052.722931	58.268148
2488.348508	65857.860557	58.273153
2487.734325	65679.298742	58.278157
2486.955822	65500.246764	58.283162
2486.907565	65302.201772	58.288167
2485.704009	65119.162721	58.293172
2485.161220	64921.706577	58.298177
2484.342093	64739.695294	58.303181
2483.531261	64548.690171	58.308186
2483.199708	64360.260548	58.313191
2482.145111	64179.542991	58.318196
2482.070019	63992.492561	58.323201
2480.805080	63811.478215	58.328205
2480.080567	63621.455497	58.333210
2479.657816	63433.968784	58.338215
2478.609254	63252.092012	58.343220
2477.866205	63070.310360	58.348225
2477.392774	62882.932319	58.353229
2476.907927	62705.070800	58.358234
2476.285787	62532.076235	58.363239
2475.388301	62335.674746	58.368244
2474.959832	62151.445375	58.373249
2473.813537	61979.723798	58.378253
2473.306952	61795.745422	58.383258
2472.893088	61616.068574	58.388263
2471.891925	61444.244231	58.393268
2471.475852	61258.759537	58.398273
2470.904244	61071.091412	58.403277
2470.464036	60885.297332	58.408282
2469.510194	60711.272000	58.413287
2468.837753	60533.720990	58.418292
2468.423864	60348.592631	58.423297
2467.319654	60166.847476	58.428301
2467.017151	59985.055577	58.433306
2466.118645	59809.501220	58.438311
2465.402986	59635.526641	58.443316
2464.725211	59458.549798	58.448321
2463.886137	59273.218668	58.453325
2463.385390	59104.933845	58.458330
2463.062550	58914.980693	58.463335
2462.074409	58744.443984	58.468340
2461.476850	58558.463400	58.473345
2460.795607	58390.823615	58.478349
2459.909115	58207.499882	58.483354
2459.542240	58023.487015	58.488359
2458.401127	57855.607111	58.493364
2458.132573	57683.612977	58.498369
2457.415440	57507.312409	58.503373
2457.101529	57328.010843	58.508378
2456.386980	57148.209121	58.513383
2455.521453	56968.586870	58.518388
2455.087639	56795.475381	58.523393
2454.090598	56607.946298	58.528397
2453.795376	56434.871224	58.533402
2453.239049	56259.669125	58.538407
2452.412664	56071.266867	58.543412
2451.754808	55889.413904	58.548417
2450.981958	55720.094937	58.553421
2450.528188	55539.958850	58.558426
2449.727394	55354.549278	58.563431
2448.385455	55184.521191	58.568436
2447.967316	54997.909125	58.573441
2447.582793	54830.153114	58.578445
2446.725116	54649.010755	58.583450
2446.253959	54476.679496	58.588455
2445.711516	54307.478778	58.593460
2445.396877	54119.520503	58.598465
2444.300961	53942.739444	58.603469
2443.821424	53761.071702	58.608474
2443.358501	53588.277924	58.613479
2442.195889	53419.931953	58.618484
2441.698744	53226.863102	58.623489
2441.074165	53063.318594	58.628493
2440.109052	52877.649731	58.633498
2439.963784	52695.206098	58.638503
2438.773273	52525.244506	58.643508
2438.303251	52348.237610	58.648513
2437.850653	52175.391030	58.653517
2437.261767	51994.993370	58.658522
2436.560511	51813.280034	58.663527
2435.623017	51641.084792	58.668532
2434.780452	51463.009367	58.673537
2433.762445	51288.170620	58.678541
2433.038943	51118.711378	58.683546
2432.605976	50949.457285	58.688551
2431.630958	50785.852219	58.693556
2431.191321	50621.200559	58.698561
2430.503302	50463.807021	58.703565
2430.092717	50286.751500	58.708570
2429.738041	50116.078775	58.713575
2429.072019	49953.897261	58.718580
2428.282275	49764.978602	58.723585
2427.522085	49599.364301	58.728589
2426.653502	49425.447680	58.733594
2425.830145	49263.894156	58.738599
2425.428254	49098.324189	58.743604
2424.792979	48926.785167	58.748609
2423.894567	48758.376973	58.753613
2423.284382	48594.702570	58.758618
2422.503922	48423.129489	58.763623
2421.739315	48266.685110	58.768628
2421.336185	48105.037713	58.773633
2420.745271	47933.009080	58.778637
2420.099901	47765.370550	58.783642
2419.559273	47600.305734	58.788647
2418.950507	47432.727160	58.793652
2418.062233	47267.328828	58.798657
2417.401747	47109.403635	58.803661
2416.301711	46937.154290	58.808666
2415.990256	46776.259104	58.813671
2414.958199	46610.669356	58.818676
2414.405874	46448.124127	58.823681
2413.565752	46296.762022	58.828685
2413.029783	46136.670480	58.833690
2412.133126	45979.003931	58.838695
2411.302232	45823.322125	58.843700
2411.129516	45665.683186	58.848705
2410.415158	45513.419248	58.853709
2409.629898	45351.736843	58.858714
2409.037524	45194.395170	58.863719
2408.258932	45051.792915	58.868724
2407.677107	44894.683032	58.873729
2406.466207	44738.742613	58.878733
2405.833250	44589.185394	58.883738
2405.094284	44436.079457	58.888743
2404.401090	44306.977270	58.893748
2403.831821	44151.042773	58.898753
2402.847026	44009.021796	58.903757
2401.761909	43861.326841	58.908762
2401.179421	43726.166074	58.913767
2400.352478	43599.516595	58.918772
2399.898798	43468.210591	58.923777
2398.896719	43333.292160	58.928781
2398.404784	43198.129179	58.933786
2397.570224	43064.000788	58.938791
2396.483673	42953.133641	58.943796
2396.165871	42823.483538	58.948801
2394.931013	42709.974516	58.953805
2394.398279	42587.222765	58.958810
2394.008331	42460.018704	58.963815
2393.461692	42340.838583	58.968820
2392.157157	42223.628004	58.973825
2391.719533	42109.438648	58.978829
2391.224016	41993.354233	58.983834
2390.689097	41874.095929	58.988839
2389.717203	41761.674597	58.993844
2389.248495	41639.820250	58.998849
2388.766158	41520.469735	59.003853
2387.917989	41414.575494	59.008858
2387.642451	41285.577684	59.013863
2386.569168	41177.152960	59.018868
2386.077802	41055.777931	59.023873
2385.275178	40940.448931	59.028877
2384.825192	40822.417290	59.033882
2384.227066	40700.600683	59.038887
2383.060602	40587.798690	59.043892
2382.965126	40478.887970	59.048897
2382.429376	40364.580431	59.053901
2381.613864	40251.308984	59.058906
2380.897189	40118.732477	59.063911
2380.162769	40005.594259	59.068916
2379.559398	39886.325527	59.073921
2378.778938	39773.845454	59.078925
2378.194153	39656.401316	59.083930
2377.737982	39530.272998	59.088935
2376.662001	39430.737065	59.093940
2376.121343	39308.020859	59.098945
2375.538761	39192.358056	59.103949
2375.061407	39080.352595	59.108954
2374.119818	38962.831431	59.113959
2373.451952	38849.445178	59.118964
2373.141964	38736.637753	59.123969
2372.558929	38622.247748	59.128973
2371.664928	38497.540105	59.133978
2370.783525	38391.747890	59.138983
2370.072363	38284.923897	59.143988
2369.802840	38172.470631	59.148993
2369.398477	38050.198373	59.153997
2368.075042	37937.616591	59.159002
2367.226938	37827.986126	59.164007
2366.444234	37724.589299	59.169012
2366.035142	37602.286010	59.174017
2365.465976	37500.300239	59.179021
2364.910130	37398.388710	59.184026
2364.097565	37279.656775	59.189031
2363.590009	37175.877360	59.194036
2362.921186	37066.603712	59.199041
2362.341711	36957.976855	59.204045
2361.726013	36842.831311	59.209050
2361.229705	36731.824410	59.214055
2360.233516	36621.815066	59.219060
2359.557294	36499.957212	59.224065
2358.887115	36392.763793	59.229069
2358.286042	36295.255403	59.234074
2357.786746	36178.261854	59.239079
2356.865240	36080.451808	59.244084
2356.356834	35958.312543	59.249089
2355.380751	35856.446644	59.254093
2354.950815	35747.788747	59.259098
2354.484353	35633.476544	59.264103
2353.803379	35521.043436	59.269108
2352.964872	35408.087351	59.274113
2352.442964	35307.640462	59.279117
2351.565078	35196.360060	59.284122
2351.371818	35088.545321	59.289127
2350.322921	34985.586060	59.294132
2350.130351	34868.466199	59.299137
2349.430693	34752.943170	59.304141
2348.628764	34647.541897	59.309146
2347.718774	34524.019031	59.314151
2346.787261	34413.917043	59.319156
2346.530276	34304.570543	59.324161
2345.916747	34212.157181	59.329165
2344.833100	34098.558207	59.334170
2344.229411	33980.308827	59.339175
2343.562891	33886.466498	59.344180
2342.802637	33775.639835	59.349185
2342.564168	33680.209767	59.354189
2341.559555	33560.057291	59.359194
2340.968927	33458.246534	59.364199
2340.384233	33353.037146	59.369204
2339.689990	33245.252598	59.374209
2338.915614	33152.286819	59.379213
2337.973708	33048.371094	59.384218
2337.816461	32946.046164	59.389223
2336.557977	32843.986058	59.394228
2336.338100	32742.596871	59.399233
2335.785133	32640.372985	59.404237
2334.797666	32536.344618	59.409242
2334.190396	32427.227588	59.414247
2333.294194	32333.078273	59.419252
2333.227998	32230.988624	59.424257
2332.396162	32134.820298	59.429261
2331.555054	32039.017912	59.434266
2330.875504	31930.979303	59.439271
2329.797847	31837.616606	59.444276
2329.443461	31728.969952	59.449281
2329.033242	31629.188830	59.454285
2328.189690	31541.248277	59.459290
2327.563767	31431.922200	59.464295
2326.707924	31347.062998	59.469300
2326.250401	31235.947145	59.474305
2325.722682	31142.095422	59.479309
2324.651469	31045.581594	59.484314
2323.887790	30951.989512	59.489319
2322.930750	30860.933401	59.494324
2322.501612	30767.085776	59.499329
2321.511380	30681.218230	59.504333
2321.002248	30595.028399	59.509338
2320.218103	30506.959412	59.514343
2319.433297	30417.467385	59.519348
2318.978411	30328.953862	59.524353
2317.970400	30243.815915	59.529357
2317.118923	30170.074961	59.534362
2316.439786	30075.922586	59.539367
2315.672541	30000.507111	59.544372
2315.004896	29926.855946	59.549377
2313.861329	29864.915248	59.554381
2313.538827	29783.743118	59.559386
2313.173462	29713.011603	59.564391
2312.377468	29641.980726	59.569396
2311.714226	29561.434129	59.574401
2311.149746	29486.020969	59.579405
2310.609780	29408.291528	59.584410
2310.333894	29328.660390	59.589415
2309.287198	29254.918671	59.594420
2308.435674	29179.128856	59.599425
2307.955888	29104.177338	59.604429
2307.211899	29035.294213	59.609434
2307.064390	28953.260859	59.614439
2305.923103	28876.772196	59.619444
2304.952008	28792.672470	59.624449
2304.322498	28734.272912	59.629453
2303.506426	28670.565933	59.634458
2303.351783	28593.030409	59.639463
2302.272993	28521.173030	59.644468
2301.718757	28447.375783	59.649473
2300.922156	28380.750071	59.654477
2300.344387	28301.232127	59.659482
2299.830992	28231.322645	59.664487
2298.847069	28180.722576	59.669492
2298.575180	28106.324929	59.674497
2297.830669	28032.384825	59.679501
2296.950290	27961.128428	59.684506
2296.469699	27891.739760	59.689511
2295.724515	27833.815293	59.694516
2295.091431	27755.536547	59.699521
2294.221885	27696.555198	59.704525
2293.548221	27639.767328	59.709530
2293.050010	27566.723326	59.714535
2292.359302	27502.970676	59.719540
2291.721477	27427.360624	59.724545
2291.163166	27367.808427	59.729549
2290.236367	27306.690514	59.734554
2289.763365	27242.515701	59.739559
2289.475406	27172.489648	59.744564
2288.729605	27102.184755	59.749569
2287.840093	27041.194237	59.754573
2287.118840	26966.422803	59.759578
2286.791948	26891.097163	59.764583
2285.905040	26831.198134	59.769588
2285.348991	26758.774667	59.774593
2284.066288	26692.716093	59.779597
2283.632335	26632.401861	59.784602
2283.208710	26576.523540	59.789607
2282.536577	26515.133960	59.794612
2282.077242	26446.398927	59.799617
2281.817751	26379.821815	59.804621
2280.970680	26305.435287	59.809626
2280.321101	26230.778094	59.814631
2279.269987	26165.146847	59.819636
2278.754412	26085.928787	59.824641
2278.304912	26028.301318	59.829645
2277.099496	25953.481021	59.834650
2276.401727	25894.776844	59.839655
2275.775611	25834.880921	59.844660
2275.183465	25761.332356	59.849665
2274.703839	25699.001876	59.854669
2273.646069	25644.155330	59.859674
2273.466916	25575.227174	59.864679
2272.760239	25523.727156	59.869684
2272.249348	25461.247905	59.874689
2271.241319	25387.009847	59.879693
2270.385636	25328.827957	59.884698
2269.918249	25261.253334	59.889703
2269.005232	25203.881807	59.894708
2268.188526	25141.639434	59.899713
2267.776598	25086.883450	59.904718
2266.804817	25026.018430	59.909722
2267.015413	24975.207584	59.914727
2266.453072	24909.661952	59.919732
2265.714085	24841.417515	59.924737
2264.967221	24772.722454	59.929742
2264.094353	24711.964962	59.934746
2263.623583	24641.123305	59.939751
2262.517828	24574.232940	59.944756
2261.948525	24515.049742	59.949761
2261.180847	24460.834106	59.954766
2260.848353	24399.343324	59.959770
2260.186420	24331.704398	59.964775
2259.279180	24279.423311	59.969780
2258.770685	24214.835644	59.974785
2258.267961	24143.691572	59.979790
2257.660781	24085.164616	59.984794
2257.031832	24018.251789	59.989799
2256.283990	23950.774516	59.994804
2255.524305	23881.734168	59.999809
2254.902038	23835.717750	60.004814
2254.075936	23770.003346	60.009818
2253.459417	23703.870710	60.014823
2252.474098	23638.626759	60.019828
2252.528666	23575.810955	60.024833
2251.495670	23523.873059	60.029838
2250.542767	23468.228082	60.034842
2250.139626	23401.845081	60.039847
2248.941448	23350.767632	60.044852
2248.992924	23285.755646	60.049857
2248.365603	23236.747050	60.054862
2247.754372	23169.515105	60.059866
2247.200735	23105.293484	60.064871
2246.375110	23048.141863	60.069876
2246.075640	22978.760809	60.074881
2245.125378	22910.253414	60.079886
2243.783986	22848.975481	60.084890
2243.479119	22781.869742	60.089895
2242.990587	22729.853787	60.094900
2243.107504	22666.236939	60.099905
2242.150337	22602.468826	60.104910
2241.058490	22542.243409	60.109914
2240.781644	22467.013817	60.114919
2240.091405	22407.573957	60.119924
2239.188944	22339.389526	60.124929
2238.325029	22270.610632	60.129934
2237.326673	22211.733236	60.134938
2237.099029	22147.778817	60.139943
2236.161466	22097.264490	60.144948
2235.730034	22032.029951	60.149953
2235.195154	21967.297138	60.154958
2234.179571	21909.372332	60.159962
2233.597161	21841.457676	60.164967
2232.707354	21798.515330	60.169972
2232.309198	21732.741869	60.174977
2231.697129	21673.831886	60.179982
2230.904092	21609.595155	60.184986
2230.489202	21565.056030	60.189991
2229.729178	21501.806905	60.194996
2229.246138	21434.408075	60.200001
2228.019675	21382.857577	60.205006
2227.477921	21317.002770	60.210010
2227.088334	21254.212922	60.215015
2226.399842	21199.415432	60.220020
2225.987050	21135.847428	60.225025
2224.866028	21085.822780	60.230030
2224.406332	21023.874172	60.235034
2223.488915	20947.878663	60.240039
2222.611682	20897.134669	60.245044
2222.115536	20842.664298	60.250049
2221.386437	20790.331783	60.255054
2220.876405	20744.603273	60.260058
2220.700803	20682.374932	60.265063
2220.097107	20628.733050	60.270068
2219.432150	20570.212178	60.275073
2218.639966	20510.760004	60.280078
2217.764412	20441.726476	60.285082
2217.263085	20377.967770	60.290087
2216.621639	20331.679511	60.295092
2215.869650	20262.826346	60.300097
2215.071224	20206.220243	60.305102
2214.471066	20151.700318	60.310106
2213.513100	20082.911566	60.315111
2212.697536	20028.168040	60.320116
2212.628292	19972.035565	60.325121
2211.797687	19925.679593	60.330126
2210.994790	19874.339467	60.335130
2210.260528	19796.311747	60.340135
2209.710332	19751.509646	60.345140
2208.864595	19693.865281	60.350145
2208.635551	19643.833036	60.355150
2207.907896	19595.552354	60.360154
2207.184802	19536.479075	60.365159
2206.238801	19480.463394	60.370164
2205.988530	19423.342518	60.375169
2205.804800	19364.231343	60.380174
2204.783407	19300.805908	60.385178
2204.473461	19241.106579	60.390183
2203.730415	19172.708413	60.395188
2202.684847	19104.166250	60.400193
2202.227100	19044.377499	60.405198
2201.771234	18995.824426	60.410202
2201.047259	18926.067736	60.415207
2200.268853	18861.816779	60.420212
2199.621484	18782.754575	60.425217
2198.740639	18736.212874	60.430222
2197.702619	18677.405114	60.435226
2197.162448	18612.782417	60.440231
2195.918843	18563.755164	60.445236
2195.861121	18511.142586	60.450241
2194.965569	18457.127562	60.455246
2194.338713	18403.672154	60.460250
2193.731356	18340.829179	60.465255
2193.414598	18296.259732	60.470260
2192.957800	18237.420496	60.475265
2192.080990	18183.844146	60.480270
2191.247190	18124.271554	60.485274
2190.999849	18056.436465	60.490279
2190.248675	18008.455192	60.495284
2189.614929	17940.054403	60.500289
2188.916116	17881.216707	60.505294
2187.870734	17829.525967	60.510298
2187.368040	17775.019183	60.515303
2186.881818	17717.893856	60.520308
2185.931433	17655.984603	60.525313
2185.834666	17593.989651	60.530318
2184.798916	17540.602179	60.535322
2184.497358	17485.249513	60.540327
2183.485371	17426.136633	60.545332
2182.761546	17357.647726	60.550337
2182.137219	17304.557336	60.555342
2181.561200	17243.666688	60.560346
2180.849616	17178.413408	60.565351
2179.994778	17128.140035	60.570356
2179.717055	17067.036216	60.575361
2178.870855	17017.763762	60.580366
2177.850486	16963.876052	60.585370
2177.428281	16899.464209	60.590375
2176.660455	16846.943516	60.595380
2176.248034	16788.428939	60.600385
2176.134378	16733.988607	60.605390
2175.595250	16680.275550	60.610394
2175.263593	16616.091129	60.615399
2174.130983	16548.840276	60.620404
2173.159621	16474.476789	60.625409
2172.542222	16411.590609	60.630414
2171.899181	16354.866587	60.635418
2171.234481	16278.927944	60.640423
2170.235854	16228.097101	60.645428
2169.559924	16171.045851	60.650433
2169.122367	16110.586082	60.655438
2168.431961	16051.359853	60.660442
2167.709578	15988.313054	60.665447
2166.864435	15934.131610	60.670452
2166.186712	15871.401605	60.675457
2165.635216	15816.569759	60.680462
2164.846692	15768.462230	60.685466
2164.137672	15698.624756	60.690471
2163.227514	15651.132606	60.695476
2162.763348	15597.677306	60.700481
2162.687126	15544.233267	60.705486
2161.607659	15482.524840	60.710490
2161.081391	15427.201620	60.715495
2160.021865	15376.563964	60.720500
2159.790247	15317.837140	60.725505
2158.896872	15256.118273	60.730510
2158.365315	15203.156200	60.735514
2157.761544	15136.536519	60.740519
2156.887884	15086.473239	60.745524
2156.182342	15021.693576	60.750529
2155.741270	14976.324559	60.755534
2155.043488	14920.185298	60.760538
2154.331617	14863.144686	60.765543
2153.908671	14805.694539	60.770548
2153.203479	14743.234248	60.775553
2152.157753	14688.026043	60.780558
2151.750759	14633.116498	60.785562
2151.198000	14574.606841	60.790567
2150.418593	14522.093894	60.795572
2149.600407	14461.586701	60.800577
2149.099260	14400.624112	60.805582
2148.273390	14353.549528	60.810586
2148.111403	14298.338442	60.815591
2147.311056	14241.405182	60.820596
2146.799467	14176.126313	60.825601
2146.416212	14112.698364	60.830606
2145.604946	14061.884791	60.835610
2144.801757	13992.364539	60.840615
2143.952131	13940.293699	60.845620
2143.150959	13867.730072	60.850625
2142.208653	13809.000566	60.855630
2141.757339	13763.186261	60.860634
2141.302299	13696.319386	60.865639
2140.290340	13654.382749	60.870644
2139.824965	13597.113141	60.875649
2138.980884	13539.186348	60.880654
2138.474017	13486.857631	60.885658
2137.997048	13427.420976	60.890663
2136.919546	13367.989275	60.895668
2136.527215	13323.041532	60.900673
2135.641241	13263.160283	60.905678
2135.225147	13204.786963	60.910682
2134.900599	13152.371239	60.915687
2133.775926	13098.501305	60.920692
2133.344775	13041.509045	60.925697
2132.699957	12988.352221	60.930702
2131.854050	12932.720683	60.935706
2131.396118	12871.734230	60.940711
2130.406817	12823.263524	60.945716
2130.074118	12763.633935	60.950721
2129.324971	12712.910292	60.955726
2128.705807	12644.046875	60.960730
2128.415553	12586.371602	60.965735
2127.584244	12531.429439	60.970740
2126.868712	12470.322623	60.975745
2126.489743	12404.963305	60.980750
2125.486567	12345.159173	60.985754
2124.870645	12290.052992	60.990759
2124.136171	12233.959180	60.995764
2123.683955	12179.473205	61.000769
2122.806976	12119.373380	61.005774
2121.768437	12054.447445	61.010778
2121.315170	12004.193651	61.015783
2120.305046	11963.779465	61.020788
2119.829930	11894.091891	61.025793
2119.640039	11841.687340	61.030798
2118.173879	11785.472145	61.035802
2118.188365	11731.636235	61.040807
2117.155715	11682.787634	61.045812
2116.435975	11624.928496	61.050817
2116.152828	11576.138463	61.055822
2115.137526	11524.362752	61.060826
2114.885199	11456.991576	61.065831
2113.854472	11402.468095	61.070836
2113.583572	11344.351482	61.075841
2113.016650	11299.445466	61.080846
2111.796983	11241.439356	61.085850
2111.215952	11192.638217	61.090855
2110.602179	11132.252109	61.095860
2109.691246	11075.445126	61.100865
2109.676535	11028.596839	61.105870
2108.934932	10967.631236	61.110874
2108.355363	10910.442680	61.115879
2107.523123	10864.987598	61.120884
2106.818045	10803.055753	61.125889
2106.115127	10742.264491	61.130894
2105.448354	10688.273629	61.135898
2105.008372	10635.269529	61.140903
2104.193192	10582.878010	61.145908
2103.446273	10516.657019	61.150913
2102.776239	10463.416342	61.155918
2102.269196	10418.398239	61.160922
2102.087787	10354.672231	61.165927
2101.080713	10313.530130	61.170932
2100.006270	10243.547659	61.175937
2099.257298	10187.096831	61.180942
2098.875523	10133.612024	61.185946
2098.522117	10082.604525	61.190951
2097.578098	10027.979191	61.195956
2097.124762	9967.615778	61.200961
2096.410541	9914.750986	61.205966
2095.615403	9861.985519	61.210970
2095.077074	9790.268676	61.215975
2094.436866	9736.214820	61.220980
2093.497041	9677.248546	61.225985
2092.942209	9626.543925	61.230990
2092.239218	9573.392376	61.235994
2091.465926	9513.521411	61.240999
2090.648216	9468.581198	61.246004
2090.001865	9412.009669	61.251009
2089.495286	9359.472949	61.256014
2088.880320	9311.086117	61.261018
2088.522586	9257.124567	61.266023
2087.731909	9205.420519	61.271028
2087.113630	9148.636577	61.276033
2086.420703	9092.326897	61.281038
2085.670275	9030.894565	61.286042
2084.898330	8970.200739	61.291047
2084.146189	8919.260363	61.296052
2083.561212	8867.364237	61.301057
2083.124306	8806.473120	61.306062
2082.162891	8760.943354	61.311066
2081.731596	8702.757775	61.316071
2080.776052	8659.506858	61.321076
2080.398215	8611.040489	61.326081
2079.793299	8554.513845	61.331086
2079.076603	8500.818423	61.336090
2078.792348	8435.528346	61.341095
2077.739552	8388.527172	61.346100
2076.603487	8331.536893	61.351105
2076.178858	8270.472720	61.356110
2075.819579	8226.781342	61.361114
2075.675598	8173.650941	61.366119
2074.881683	8110.686194	61.371124
2073.848723	8050.609950	61.376129
2073.228649	8008.190392	61.381134
2071.979240	7944.196858	61.386138
2071.184138	7890.134604	61.391143
2070.380223	7849.551675	61.396148
2070.142238	7793.805316	61.401153
2069.782755	7743.245377	61.406158
2068.997766	7699.028771	61.411162
2068.502776	7648.116355	61.416167
2067.567411	7593.003360	61.421172
2066.748709	7539.063217	61.426177
2066.337246	7488.659876	61.431182
2066.073284	7441.994111	61.436186
2065.374680	7383.094486	61.441191
2064.556098	7338.451806	61.446196
2064.097823	7274.874533	61.451201
2063.832960	7217.083657	61.456206
2062.384875	7164.083298	61.461210
2061.885968	7097.622236	61.466215
2061.037325	7049.947173	61.471220
2060.462745	6992.649205	61.476225
2059.724928	6931.695812	61.481230
2059.153098	6894.581453	61.486234
2058.701354	6833.385214	61.491239
2057.869475	6786.737150	61.496244
2057.245001	6733.968534	61.501249
2057.011999	6677.778182	61.506254
2055.628771	6627.361330	61.511258
2055.556427	6567.657844	61.516263
2054.646046	6516.527070	61.521268
2054.170324	6464.627910	61.526273
2053.522285	6406.219197	61.531278
2052.146642	6354.986879	61.536282
2051.747166	6294.402928	61.541287
2050.988391	6254.788506	61.546292
2050.362693	6199.828726	61.551297
2050.015426	6146.434168	61.556302
2049.177951	6096.401070	61.561306
2048.646811	6038.002138	61.566311
2047.839234	5987.237709	61.571316
2047.264262	5937.236024	61.576321
2046.667115	5884.929902	61.581326
2045.889512	5848.079826	61.586330
2044.922896	5779.006524	61.591335
2044.350904	5742.980743	61.596340
2043.927858	5690.361178	61.601345
2043.352971	5634.710753	61.606350
2042.325258	5588.202355	61.611354
2042.058088	5530.081544	61.616359
2041.315541	5484.098794	61.621364
2040.708959	5426.510246	61.626369
2040.026421	5384.628748	61.631374
2038.956379	5323.765961	61.636378
2038.852234	5269.525672	61.641383
2038.066092	5216.111375	61.646388
2037.351551	5165.726922	61.651393
2037.376865	5111.511617	61.656398
2035.928328	5061.836631	61.661402
2035.908828	5005.048643	61.666407
2034.552058	4952.764174	61.671412
2034.238790	4894.444300	61.676417
2033.617886	4838.865334	61.681422
2032.821421	4792.234427	61.686426
2032.033659	4736.547747	61.691431
2031.240290	4690.250643	61.696436
2030.369539	4632.800180	61.701441
2030.150737	4582.891863	61.706446
2029.257963	4532.498844	61.711450
2028.241226	4472.156123	61.716455
2027.823727	4433.309112	61.721460
2027.233947	4384.742547	61.726465
2026.901583	4339.408379	61.731470
2026.135183	4281.878955	61.736474
2025.479767	4228.465363	61.741479
2024.909432	4184.530543	61.746484
2024.139287	4125.412766	61.751489
2023.501837	4073.654878	61.756494
2022.465233	4023.492601	61.761498
2021.764713	3970.602440	61.766503
2021.253381	3923.236754	61.771508
2020.931238	3868.215736	61.776513
2020.215550	3814.907816	61.781518
2019.407962	3769.095934	61.786522
2018.776675	3715.344355	61.791527
2017.772575	3665.499822	61.796532
2017.261705	3612.522354	61.801537
2016.593202	3569.810993	61.806542
2016.018782	3523.299819	61.811546
2015.616551	3472.159833	61.816551
2014.782097	3429.894154	61.821556
2014.151044	3379.736405	61.826561
2013.668708	3323.118093	61.831566
2012.582531	3274.218992	61.836570
2012.243472	3217.970560	61.841575
2011.346290	3176.419035	61.846580
2010.804291	3128.796461	61.851585
2010.239129	3075.522930	61.856590
2009.282209	3034.714740	61.861594
2008.833014	2986.925908	61.866599
2008.255371	2939.313952	61.871604
2007.640738	2884.040034	61.876609
2006.931077	2842.181750	61.881614
2005.778913	2796.107121	61.886618
2005.301941	2737.786083	61.891623
2004.662897	2698.332993	61.896628
2004.020990	2643.213026	61.901633
2003.422055	2601.570945	61.906638
2002.571652	2554.981138	61.911642
2002.086143	2502.089125	61.916647
2001.477687	2459.805552	61.921652
2000.734867	2409.977939	61.926657
2000.197144	2366.397116	61.931662
1999.233694	2316.245925	61.936666
1998.593172	2262.938292	61.941671
1997.971267	2227.993374	61.946676
1997.218263	2188.485263	61.951681
1996.916284	2141.063853	61.956686
1995.865277	2097.486309	61.961690
1995.512794	2054.880541	61.966695
1994.718012	2011.144134	61.971700
1993.953630	1962.582524	61.976705
1993.843527	1920.655716	61.981710
1993.074526	1875.743606	61.986714
1992.315202	1825.067189	61.991719
1991.622339	1778.022842	61.996724
1990.885164	1722.739232	62.001729
1990.408019	1678.407803	62.006734
1989.176475	1635.796434	62.011738
1988.721236	1586.090017	62.016743
1987.695923	1548.402571	62.021748
1987.077077	1509.086394	62.026753
1986.342934	1468.396155	62.031758
1985.719702	1436.903003	62.036762
1985.318030	1387.737946	62.041767
1984.283870	1347.035395	62.046772
1983.658801	1309.000575	62.051777
1983.207826	1278.240542	62.056782
1982.969312	1238.696951	62.061786
1982.199387	1197.561944	62.066791
1981.460404	1151.585693	62.071796
1980.369807	1118.461900	62.076801
1979.691581	1063.985687	62.081806
1979.058526	1041.552460	62.086810
1978.363357	998.527781	62.091815
1977.795260	962.114749	62.096820
1977.211058	925.974955	62.101825
1976.467745	872.041869	62.106830
1975.885463	846.621126	62.111834
1975.305940	812.737920	62.116839
1974.412959	767.698624	62.121844
1973.593397	733.727178	62.126849
1973.328919	691.106908	62.131854
1972.729053	655.565683	62.136858
1972.228993	615.314465	62.141863
1971.271794	580.340984	62.146868
1970.128212	542.274761	62.151873
1969.550721	509.666064	62.156878
1969.253258	468.898994	62.161882
1968.638364	432.383100	62.166887
1967.928304	404.064334	62.171892
1967.583840	374.659940	62.176897
1966.887645	325.985573	62.181902
1965.615563	289.434416	62.186906
1965.140273	249.473583	62.191911
1964.451848	227.315864	62.196916
1963.489244	189.118104	62.201921
1963.541164	156.188929	62.206926
1962.257603	130.357239	62.211930
1961.826308	101.590693	62.216935
1960.747958	72.483331	62.221940
1959.727146	47.461008	62.226945
1959.370313	29.345227	62.231950
1957.823951	18.584091	62.236954
1955.620355	39.803872	62.241959
1954.715780	46.147465	62.246964
1954.057954	63.726801	62.251969
1954.130067	55.886793	62.256974
1953.484935	56.700579	62.261978
1953.975011	50.220329	62.266983
1952.949085	58.343559	62.271988
1952.017353	52.751512	62.276993
1951.145359	61.362337	62.281998
1950.140381	63.228431	62.287002
1949.326905	57.869563	62.292007
1949.787084	60.382209	62.297012
1949.226999	65.555740	62.302017
1948.660617	62.895144	62.307022
1947.400703	66.859767	62.312026
1947.019646	59.621866	62.317031
1946.287987	64.197932	62.322036
1945.201985	66.989693	62.327041
1944.742157	65.675813	62.332046
1943.852877	57.735021	62.337050
1943.068463	55.057255	62.342055
1942.399018	60.316990	62.347060
1941.910378	67.229279	62.352065
1941.909313	58.405120	62.357070
1940.959111	58.577178	62.362074
1940.331136	52.859751	62.367079
1939.878907	74.722955	62.372084
1938.660928	69.348420	62.377089
1938.079674	56.498688	62.382094
1937.717982	67.832627	62.387098
1936.911107	63.141681	62.392103
1935.946332	65.106291	62.397108
1935.770779	73.035503	62.402113
1935.415493	64.609031	62.407118
1934.442029	67.910862	62.412122
1933.760308	65.027246	62.417127
1932.907464	69.885351	62.422132
1932.672422	75.217218	62.427137
1932.357540	65.992023	62.432142
1931.006902	76.543876	62.437146
1929.797626	70.314862	62.442151
1929.750880	75.670171	62.447156
1929.053476	83.402492	62.452161
1928.559308	64.800194	62.457166
1928.235836	78.822753	62.462170
1927.606252	68.782221	62.467175
1926.838237	65.808374	62.472180
1925.973893	69.794536	62.477185
1925.204227	66.462959	62.482190
1924.478860	70.324297	62.487194
1924.001365	72.907361	62.492199
1923.279002	63.333476	62.497204
1922.570182	69.974368	62.502209
1922.053041	56.711451	62.507214
1921.457990	73.574691	62.512218
1919.879620	61.203820	62.517223
1920.144412	71.761138	62.522228
1919.461967	69.367101	62.527233
1918.961918	64.120400	62.532238
1918.022190	63.509123	62.537242
1917.083638	68.801480	62.542247
1916.712965	70.996416	62.547252
1915.834163	74.110353	62.552257
1915.691070	61.673931	62.557262
1914.762590	72.611042	62.562266
1913.525721	67.866168	62.567271
1913.360853	67.111673	62.572276
1912.898304	73.232034	62.577281
1912.923403	55.796917	62.582286
1911.475750	72.507609	62.587290
1910.760048	66.574279	62.592295
1909.398716	69.203158	62.597300
1908.662857	72.248432	62.602305
1909.142411	54.038888	62.607310
1908.670732	72.090047	62.612314
1907.791756	66.132942	62.617319
1906.701934	70.851994	62.622324
1905.808018	72.272404	62.627329
1905.207788	65.445014	62.632334
1904.886684	70.264650	62.637338
1904.284511	65.294753	62.642343
1903.432612	68.138440	62.647348
1902.477116	71.297866	62.652353
1902.309711	66.361742	62.657358
1901.502252	74.667471	62.662362
1900.705997	69.559073	62.667367
1900.315535	67.142718	62.672372
1899.478313	63.553505	62.677377
1899.359425	61.911313	62.682382
1898.376573	77.260836	62.687386
1898.229837	73.455206	62.692391
1897.268508	70.059323	62.697396
1896.705069	66.919435	62.702401
1895.993861	66.524056	62.707406
1894.746129	65.016176	62.712410
1893.886700	63.762772	62.717415
1893.705510	55.868608	62.722420
1893.116971	71.261186	62.727425
1892.428050	59.439973	62.732430
1891.394617	61.615669	62.737434
1890.968491	63.958639	62.742439
1890.331902	59.674737	62.747444
1889.929266	66.991505	62.752449
1889.168464	57.628674	62.757454
1888.740318	67.464175	62.762458
1887.974287	63.588849	62.767463
1887.735466	64.187083	62.772468
1886.690119	65.829578	62.777473
1885.545223	64.378708	62.782478
1884.921263	71.144816	62.787482
1883.930038	66.856062	62.792487
1884.066082	67.994874	62.797492
1883.080520	69.675298	62.802497
1882.697404	57.964000	62.807502
1882.208122	72.185041	62.812506
1881.423728	62.844796	62.817511
1880.727754	51.880157	62.822516
1879.830211	65.207527	62.827521
1879.418058	62.719494	62.832526
1878.139202	69.234896	62.837530
1877.979625	53.825511	62.842535
1877.167524	65.932395	62.847540
1875.850986	62.710179	62.852545
1876.012980	59.887876	62.857550
1875.751913	67.130690	62.862554
1874.592176	60.960718	62.867559
1873.975818	61.860376	62.872564
1873.205188	64.600167	62.877569
1872.916403	57.737265	62.882574
1872.057414	60.959521	62.887578
1871.854922	60.350012	62.892583
1870.723004	69.206229	62.897588
1869.128316	68.040728	62.902593
1869.586340	55.823568	62.907598
1868.677959	64.366813	62.912602
1867.876818	56.818312	62.917607
1867.511507	56.530332	62.922612
1866.481413	56.341877	62.927617
1866.270232	59.375542	62.932622
1865.575040	56.521480	62.937626
1865.257307	57.265446	62.942631
1864.712210	56.553902	62.947636
1863.044825	67.259813	62.952641
1862.305500	61.030549	62.957646
1861.677110	63.720744	62.962650
1861.595035	58.305047	62.967655
1860.903120	62.206058	62.972660
1860.549804	68.244180	62.977665
1859.960379	61.567708	62.982670
1859.213672	64.563134	62.987674
1858.042583	67.834843	62.992679
1857.119260	72.201352	62.997684
1857.014454	71.542368	63.002689
1856.443280	66.271135	63.007694
1855.535898	73.317831	63.012698
1854.875091	58.980212	63.017703
1854.945165	62.172985	63.022708
1853.341517	71.116229	63.027713
1852.526766	58.823549	63.032718
1851.632800	57.122923	63.037722
1851.409639	59.914701	63.042727
1851.021387	59.479073	63.047732
1849.946253	56.888957	63.052737
1849.533220	60.339641	63.057742
1849.022369	57.389703	63.062746
1848.703291	58.354944	63.067751
1848.314036	57.569372	63.072756
1847.160787	54.392647	63.077761
1846.515012	52.524433	63.082766
1845.644176	61.845958	63.087770
1845.179609	57.769070	63.092775
1844.676346	57.880072	63.097780
1843.366773	58.126658	63.102785
1842.358011	55.102838	63.107790
1841.922833	60.063957	63.112794
1842.000797	55.071256	63.117799
1840.877495	55.126902	63.122804
1840.297947	57.672957	63.127809
1839.803706	54.109547	63.132814
1839.134963	62.646134	63.137818
1838.678603	66.049761	63.142823
1838.160535	58.772954	63.147828
1836.735027	59.430150	63.152833
1835.690433	54.412021	63.157838
1835.795179	62.470890	63.162842
1835.525730	58.024318	63.167847
1834.364108	56.871968	63.172852
1833.787670	64.107556	63.177857
1833.409374	50.620392	63.182862
1832.933032	52.901300	63.187866
1831.795569	52.628201	63.192871
1831.118469	47.538516	63.197876
1830.342677	65.599850	63.202881
1830.005354	49.552234	63.207886
1829.181279	54.351742	63.212890
1828.628483	55.633670	63.217895
1828.217849	58.308319	63.222900
1826.406730	61.478758	63.227905
1826.250690	58.470879	63.232910
1825.425383	58.662245	63.237914
1825.212029	51.044373	63.242919
1824.620540	50.313536	63.247924
1823.856258	61.294389	63.252929
1823.746103	56.147568	63.257934
1823.279915	57.740322	63.262938
1822.226439	54.119841	63.267943
1821.096945	47.727620	63.272948
1820.444302	68.315802	63.277953
1819.778852	52.584447	63.282958
1819.182772	53.424196	63.287962
1818.795259	55.869110	63.292967
1818.257494	54.090178	63.297972
1817.218072	54.195817	63.302977
1816.940730	54.359347	63.307982
1816.136860	56.418018	63.312986
1815.280715	50.681630	63.317991
1814.956107	61.023597	63.322996
1813.481431	58.593819	63.328001
1813.288866	54.974060	63.333006
1812.459579	63.482856	63.338010
1811.913904	55.929737	63.343015
1811.471528	57.489209	63.348020
1810.757366	62.249784	63.353025
1810.817424	58.262342	63.358030
1810.096954	56.189027	63.363034
1809.160223	55.956585	63.368039
1808.416306	55.256960	63.373044
1806.846356	62.430835	63.378049
1806.095350	61.483356	63.383054
1806.036132	62.399006	63.388058
1805.411750	52.039873	63.393063
1804.381208	54.599545	63.398068
1803.905725	56.639924	63.403073
1803.563471	61.606460	63.408078
1802.798244	59.381338	63.413082
1802.417807	58.110729	63.418087
1802.045682	62.167021	63.423092
1800.586427	63.026967	63.428097
1800.116458	58.222751	63.433102
1799.642488	63.116697	63.438106
1798.838095	56.450969	63.443111
1798.411228	58.432506	63.448116
1797.164839	67.983288	63.453121
1796.644391	51.095864	63.458126
1795.516381	57.542836	63.463130
1794.800086	62.691787	63.468135
1795.248639	57.947113	63.473140
1794.671402	71.139164	63.478145
1794.271053	64.411011	63.483150
1793.255162	64.540653	63.488154
1792.285676	51.753441	63.493159
1791.477270	56.738158	63.498164
1790.570076	59.317385	63.503169
1790.477264	51.352854	63.508174
1790.103609	60.792594	63.513178
1788.950032	60.612651	63.518183
1788.443156	56.205525	63.523188
1787.222556	55.108671	63.528193
1786.766384	47.782210	63.533198
1786.575747	50.198175	63.538202
1785.752256	58.776633	63.543207
1785.535200	56.244177	63.548212
1784.225910	67.540121	63.553217
1783.423500	51.533410	63.558222
1782.642645	63.039710	63.563226
1782.519568	55.435209	63.568231
1782.097475	56.590177	63.573236
1780.587118	59.042092	63.578241
1780.182812	55.418699	63.583246
1779.257709	55.653593	63.588250
1778.842758	61.855805	63.593255
1778.509982	58.950403	63.598260
1777.644500	58.241190	63.603265
1777.575044	59.169644	63.608270
1777.182810	52.788648	63.613274
1775.959532	55.661554	63.618279
1774.978947	51.018525	63.623284
1774.383922	50.327771	63.628289
1773.707351	58.161912	63.633294
1772.715460	59.383983	63.638298
1772.085975	55.858722	63.643303
1771.396722	51.148873	63.648308
1770.583030	58.981609	63.653313
1770.668732	59.379063	63.658318
1770.148104	59.746848	63.663322
1769.741763	65.681547	63.668327
1769.059164	56.029456	63.673332
1767.747485	68.568389	63.678337
1767.441894	58.366283	63.683342
1767.023672	59.511511	63.688346
1765.626843	62.522664	63.693351
1764.811792	54.367517	63.698356
1763.902327	56.852798	63.703361
1763.773972	46.980754	63.708366
1763.258695	59.849969	63.713370
1762.977774	53.872278	63.718375
1762.088633	50.768011	63.723380
1761.421504	51.076394	63.728385
1760.800501	53.367849	63.733390
1759.922193	54.556277	63.738394
1759.586776	50.517697	63.743399
1758.930419	47.416230	63.748404
1757.552556	49.911792	63.753409
1756.743231	49.526117	63.758414
1756.110804	47.099079	63.763418
1755.722459	55.515847	63.768423
1755.495081	53.498690	63.773428
1755.250312	60.018740	63.778433
1754.669003	49.673960	63.783438
1753.496377	57.964412	63.788442
1752.773883	52.528049	63.793447
1752.757199	59.901532	63.798452
1750.972284	54.979706	63.803457
1750.056486	48.282926	63.808462
1749.397871	60.915758	63.813466
1749.000165	55.405663	63.818471
1748.919656	48.845813	63.823476
1747.876874	58.818447	63.828481
1747.906200	51.986786	63.833486
1746.883830	53.564982	63.838490
1745.868572	54.892893	63.843495
1745.342347	51.944811	63.848500
1744.558156	54.509312	63.853505
1744.602874	40.370347	63.858510
1743.720178	46.057747	63.863514
1743.043145	48.884557	63.868519
1742.436781	46.725022	63.873524
1741.121381	55.459491	63.878529
1740.591965	44.009703	63.883534
1740.358447	45.471470	63.888538
1739.292325	54.410773	63.893543
1738.691540	45.013501	63.898548
1737.852324	54.722759	63.903553
1737.750142	49.379196	63.908558
1736.722392	51.390136	63.913562
1736.313091	50.622609	63.918567
1735.018667	46.784444	63.923572
1734.484910	51.853611	63.928577
1734.194693	45.564110	63.933582
1733.427078	55.407557	63.938586
1732.876613	54.123025	63.943591
1733.015266	52.485323	63.948596
1731.622902	55.480324	63.953601
1730.700562	51.077592	63.958606
1729.834340	56.356407	63.963610
1729.686864	53.919413	63.968615
1729.285514	45.301928	63.973620
1728.102130	61.417956	63.978625
1727.461755	50.019125	63.983630
1726.700079	46.405972	63.988634
1726.381326	58.870915	63.993639
1726.130002	53.473534	63.998644
1725.299935	54.362409	64.003649
1724.248435	51.914325	64.008654
1723.360517	50.318869	64.013658
1722.965635	57.159458	64.018663
1722.736147	56.398267	64.023668
1721.576525	52.332178	64.028673
1720.800288	50.026459	64.033678
1720.111664	55.735127	64.038682
1719.679906	49.476162	64.043687
1719.696627	50.798009	64.048692
1718.239548	55.087320	64.053697
1717.243089	47.574256	64.058702
1716.745219	58.645701	64.063706
1716.188894	55.484493	64.068711
1715.971523	48.075341	64.073716
1715.391735	60.781522	64.078721
1714.457129	48.610447	64.083726
1713.399000	47.185429	64.088730
1712.876385	53.911301	64.093735
1712.804676	47.549677	64.098740
1711.971505	49.494565	64.103745
1711.026662	52.471016	64.108750
1709.999118	55.739108	64.113754
1709.297754	56.030462	64.118759
1709.084166	43.306560	64.123764
1708.745482	54.550096	64.128769
1708.471763	49.573768	64.133774
1707.494776	50.924741	64.138778
1706.466426	55.191610	64.143783
1705.747677	48.649008	64.148788
1705.227322	56.419317	64.153793
1704.162481	44.338426	64.158798
1702.966619	51.837894	64.163802
1702.759966	52.479575	64.168807
1702.831460	53.199971	64.173812
1701.959478	62.748271	64.178817
1701.526205	49.815652	64.183822
1701.131609	50.744088	64.188826
1699.897602	51.871423	64.193831
1699.475316	49.922753	64.198836
1698.850335	51.265201	64.203841
1698.497786	54.154906	64.208846
1697.653344	54.856781	64.213850
1696.731820	54.474526	64.218855
1695.927603	51.537706	64.223860
1694.731337	57.381006	64.228865
1694.305182	57.771314	64.233870
1693.533800	55.191622	64.238874
1693.137235	57.252451	64.243879
1693.148987	48.122195	64.248884
1692.244928	52.264381	64.253889
1691.256242	42.405759	64.258894
1690.708050	52.079032	64.263898
1690.059166	55.776124	64.268903
1689.661608	47.570478	64.273908
1688.454200	56.424628	64.278913
1687.727310	47.636287	64.283918
1686.980894	36.214176	64.288922
1686.154507	46.474632	64.293927
1686.049438	47.984680	64.298932
1685.576218	54.969325	64.303937
1685.066002	46.283244	64.308942
1683.975455	47.987586	64.313946
1683.177063	50.776751	64.318951
1682.801342	50.394254	64.323956
1682.193002	53.474172	64.328961
1681.527110	51.387987	64.333966
1680.665171	44.338604	64.338970
1679.845405	54.657929	64.343975
1679.641384	54.436305	64.348980
1678.544441	56.327261	64.353985
1678.155337	50.733998	64.358990
1676.789746	42.806504	64.363994
1676.698087	60.455899	64.368999
1676.323162	49.325064	64.374004
1675.369320	53.796283	64.379009
1674.931205	47.298424	64.384014
1673.589859	44.315769	64.389018
1673.173842	52.259660	64.394023
1672.782290	48.072807	64.399028
1672.049131	56.646077	64.404033
1671.954694	52.098525	64.409038
1671.376912	52.065987	64.414042
1670.109729	48.605267	64.419047
1669.546059	44.995344	64.424052
1668.951061	51.552033	64.429057
1668.415034	47.704890	64.434062
1667.112669	41.012314	64.439066
1666.523688	49.397494	64.444071
1666.475944	46.776472	64.449076
1665.459654	56.045136	64.454081
1664.994133	42.890297	64.459086
1664.455799	50.647497	64.464090
1663.201651	55.955204	64.469095
1662.903756	48.293008	64.474100
1662.229462	56.644635	64.479105
1661.560947	40.970704	64.484110
1661.072181	54.679282	64.489114
1660.361647	53.815290	64.494119
1659.674985	45.253352	64.499124
1659.003886	52.048843	64.504129
1658.469831	45.522013	64.509134
1657.049731	46.430952	64.514138
1656.303545	50.527179	64.519143
1656.377280	48.216932	64.524148
1655.447504	47.248756	64.529153
1655.304802	48.018831	64.534158
1654.641177	55.256708	64.539162
1653.802084	45.264738	64.544167
1653.187026	45.758031	64.549172
1652.296585	53.541147	64.554177
1652.340785	46.635901	64.559182
1650.925747	50.254904	64.564186
1649.781193	43.772157	64.569191
1649.824701	38.338940	64.574196
1648.951658	48.935394	64.579201
1648.838365	42.696546	64.584206
1647.687118	52.306053	64.589210
1646.837048	41.889274	64.594215
1646.369511	45.437708	64.599220
1645.852623	53.683453	64.604225
1645.552969	41.085209	64.609230
1644.611562	44.305807	64.614234
1643.653731	44.623296	64.619239
1643.471591	46.581119	64.624244
1642.442112	49.360100	64.629249
1641.220143	40.856225	64.634254
1640.833198	43.147107	64.639258
1639.956864	45.098996	64.644263
1640.098783	44.766465	64.649268
1639.352157	46.769575	64.654273
1638.459049	39.048990	64.659278
1637.750616	51.818622	64.664282
1637.148290	53.501000	64.669287
1636.894415	46.498350	64.674292
1636.252449	56.702782	64.679297
1634.933946	53.063361	64.684302
1634.038416	44.304289	64.689306
1633.620503	47.449513	64.694311
1633.466230	52.645972	64.699316
1632.887997	52.514441	64.704321
1631.958538	49.290001	64.709326
1631.020198	50.248733	64.714330
1630.597870	57.652547	64.719335
1630.394861	49.538742	64.724340
1628.908568	58.849556	64.729345
1628.214749	49.228238	64.734350
1627.641720	51.968580	64.739354
1626.828237	49.996474	64.744359
1626.580766	42.794187	64.749364
1626.051298	48.682061	64.754369
1625.913426	46.123436	64.759374
1624.789569	52.652611	64.764378
1624.054830	46.218549	64.769383
1623.415585	46.074961	64.774388
1622.754629	56.017391	64.779393
1621.727194	47.767188	64.784398
1620.717931	53.077202	64.789402
1620.323414	42.865089	64.794407
1620.370903	45.729360	64.799412
1619.611536	43.823385	64.804417
1618.466876	42.640555	64.809422
1618.007480	52.076010	64.814426
1617.615447	46.216824	64.819431
1617.123774	48.812592	64.824436
1615.468496	49.826918	64.829441
1615.098960	51.922201	64.834446
1614.462501	44.115069	64.839450
1614.084177	48.556090	64.844455
1614.065914	39.024029	64.849460
1612.987990	46.053345	64.854465
1611.701200	42.863617	64.859470
1611.017504	46.078799	64.864474
1610.763687	44.087098	64.869479
1610.520010	29.959624	64.874484
1609.386052	45.422213	64.879489
1608.673496	49.278227	64.884494
1608.016329	44.706202	64.889498
1607.221822	46.828425	64.894503
1607.042661	36.987207	64.899508
1606.184951	48.256797	64.904513
1605.203162	49.460984	64.909518
1604.588168	53.372931	64.914522
1604.073876	44.753877	64.919527
1604.176605	41.842645	64.924532
1602.748092	45.327787	64.929537
1602.020814	34.098995	64.934542
1601.484592	44.539916	64.939546
1601.452484	47.336102	64.944551
1600.612500	43.645195	64.949556
1599.795682	51.206119	64.954561
1598.952848	42.467643	64.959566
1598.043509	37.577611	64.964570
1597.105792	49.493233	64.969575
1596.580381	38.897362	64.974580
1595.430389	45.588109	64.979585
1595.288283	48.450486	64.984590
1594.695037	43.398204	64.989594
1594.368237	45.803922	64.994599
1594.386328	49.539237	64.999604
1593.466498	45.533984	65.004609
1592.351908	48.406483	65.009614
1592.000340	52.387421	65.014618
1590.574327	47.389241	65.019623
1590.090240	44.791979	65.024628
1589.313035	47.638711	65.029633
1589.316380	49.455848	65.034638
1588.754371	46.350893	65.039642
1587.410058	57.151161	65.044647
1587.225844	43.925698	65.049652
1586.309589	50.287118	65.054657
1585.874661	45.963234	65.059662
1584.367797	50.468322	65.064666
1583.996140	46.233868	65.069671
1583.920014	44.080317	65.074676
1583.471077	54.617222	65.079681
1582.661775	42.737761	65.084686
1581.915540	53.758946	65.089690
1580.787730	55.272326	65.094695
1580.608920	50.203983	65.099700
1579.385812	45.203843	65.104705
1578.431579	47.706285	65.109710
1577.741284	48.828224	65.114714
1577.089724	51.276498	65.119719
1577.066843	49.676703	65.124724
1576.127109	55.836496	65.129729
1575.858048	50.116919	65.134734
1575.585607	47.440413	65.139738
1574.791536	50.992237	65.144743
1574.257550	50.118569	65.149748
1573.394305	51.959286	65.154753
1572.783019	47.993596	65.159758
1571.247487	49.722408	65.164762
1570.680195	51.097231	65.169767
1570.481370	48.684429	65.174772
1569.943674	59.481253	65.179777
1569.823069	52.097791	65.184782
1568.262654	49.704474	65.189786
1567.390766	51.254974	65.194791
1567.229008	42.387708	65.199796
1566.801683	47.904829	65.204801
1566.083509	46.350218	65.209806
1564.645797	50.573094	65.214810
1564.018311	48.111293	65.219815
1564.321695	44.241684	65.224820
1563.490534	55.732517	65.229825
1562.472664	47.532007	65.234830
1561.699138	51.011241	65.239834
1560.850498	51.398080	65.244839
1560.700914	45.770554	65.249844
1560.089803	47.452863	65.254849
1559.595934	45.120951	65.259854
1558.410734	51.533929	65.264858
1557.412907	47.143762	65.269863
1557.548397	40.204744	65.274868
1556.632845	50.445339	65.279873
1556.238670	47.347583	65.284878
1555.291276	46.787423	65.289882
1554.830427	46.626337	65.294887
1554.003110	40.985732	65.299892
1552.560486	50.376314	65.304897
1552.370024	45.362862	65.309902
1551.716502	46.343121	65.314906
1551.269054	42.665170	65.319911
1551.172711	43.139563	65.324916
1550.356157	49.322483	65.329921
1549.731651	43.206662	65.334926
1549.346181	44.966401	65.339930
1547.927759	49.478071	65.344935
1547.230670	39.818261	65.349940
1546.303983	43.540408	65.354945
1546.138938	41.559176	65.359950
1545.816209	46.979847	65.364954
1544.603039	46.833053	65.369959
1544.314970	35.428847	65.374964
1543.599287	48.055645	65.379969
1542.671494	44.045451	65.384974
1541.632991	45.772490	65.389978
1540.398581	54.060913	65.394983
1540.528277	47.737855	65.399988
1540.211725	51.877794	65.404993
1539.737166	45.511320	65.409998
1539.495049	45.135572	65.415002
1538.246216	47.034787	65.420007
1537.751593	42.206020	65.425012
1537.074452	48.086014	65.430017
1536.107537	47.397757	65.435022
1535.083455	38.781106	65.440026
1534.520931	43.423777	65.445031
1534.081851	35.134879	65.450036
1533.199004	49.263376	65.455041
1533.437156	37.304524	65.460046
1532.195881	51.239380	65.465050
1531.345268	47.265714	65.470055
1531.303519	43.135453	65.475060
1530.266872	42.188750	65.480065
1528.869158	42.481683	65.485070
1528.453129	32.914297	65.490074
1527.795318	43.910475	65.495079
1527.870203	35.991880	65.500084
1527.451394	41.242686	65.505089
1526.714322	40.899154	65.510094
1525.503576	44.369147	65.515098
1524.910668	48.727297	65.520103
1524.518087	33.077632	65.525108
1523.180767	44.459703	65.530113
1522.250281	39.165563	65.535118
1522.388780	40.974960	65.540122
1521.629735	39.562345	65.545127
1521.244862	25.751545	65.550132
1520.520687	47.108981	65.555137
1519.456189	47.248575	65.560142
1519.380507	41.803001	65.565146
1518.728246	41.375088	65.570151
1517.386390	37.680496	65.575156
1516.077749	40.482804	65.580161
1516.048869	38.711941	65.585166
1515.864245	35.574380	65.590170
1515.031419	46.049488	65.595175
1515.098553	34.264772	65.600180
1513.592955	42.697893	65.605185
1513.136269	45.843048	65.610190
1512.533773	49.306829	65.615194
1511.269903	52.619743	65.620199
1510.681883	47.987744	65.625204
1509.905288	57.357497	65.630209
1509.494054	46.558554	65.635214
1508.998132	49.138873	65.640218
1508.540113	48.433386	65.645223
1508.418549	53.572930	65.650228
1507.086050	54.725061	65.655233
1506.464104	51.568800	65.660238
1506.106681	48.464365	65.665242
1504.877970	51.988752	65.670247
1504.047277	43.021260	65.675252
1503.532582	49.436321	65.680257
1503.042316	42.866895	65.685262
1502.694372	37.545288	65.690266
1501.990005	45.123678	65.695271
1501.103468	37.945137	65.700276
1500.320395	45.581208	65.705281
1499.783060	45.398483	65.710286
1499.655732	48.758044	65.715290
1498.335567	49.096526	65.720295
1497.907917	45.916879	65.725300
1497.547397	49.545289	65.730305
1496.976083	48.735253	65.735310
1496.001035	42.914692	65.740314
1495.676823	43.096129	65.745319
1494.417653	43.577322	65.750324
1493.246653	40.805158	65.755329
1492.921124	39.765563	65.760334
1492.851462	48.394607	65.765338
1492.189388	45.644672	65.770343
1491.609855	40.502434	65.775348
1490.142995	46.929290	65.780353
1489.375867	47.972421	65.785358
1489.258762	46.736897	65.790362
1488.814605	47.720011	65.795367
1488.543312	39.130046	65.800372
1487.100111	47.799588	65.805377
1486.871214	47.695908	65.810382
1486.129372	45.233957	65.815386
1484.956296	57.781557	65.820391
1483.933448	39.674104	65.825396
1483.245596	48.378563	65.830401
1483.091665	41.396327	65.835406
1483.096558	36.429180	65.840410
1482.436548	49.632211	65.845415
1482.268853	48.308245	65.850420
1481.039065	47.340140	65.855425
1479.785159	49.794421	65.860430
1478.994037	42.999007	65.865434
1478.493051	48.581236	65.870439
1478.076858	46.694306	65.875444
1477.403128	50.159231	65.880449
1476.906571	48.513414	65.885454
1475.636870	43.179455	65.890458
1474.951718	49.857761	65.895463
1475.175713	45.372164	65.900468
1474.633055	52.237650	65.905473
1473.851078	53.588048	65.910478
1472.752043	49.154832	65.915482
1471.789976	47.806183	65.920487
1471.295067	48.160121	65.925492
1470.220796	47.564460	65.930497
1469.193856	43.763481	65.935502
1469.238823	43.857652	65.940506
1468.239061	45.642412	65.945511
1468.440975	34.736958	65.950516
1467.820462	43.797767	65.955521
1466.890702	42.146762	65.960526
1466.164435	35.717603	65.965530
1465.374238	40.468717	65.970535
1465.233517	39.692346	65.975540
1464.460277	55.273992	65.980545
1463.635690	44.269508	65.985550
1462.919938	41.033000	65.990554
1461.933680	49.331849	65.995559
1461.675147	43.960206	66.000564
1460.749141	38.160471	66.005569
1459.892156	49.628881	66.010574
1459.078053	45.139795	66.015578
1458.656976	45.562014	66.020583
1458.602736	47.246906	66.025588
1457.623336	49.098838	66.030593
1456.780714	49.829648	66.035598
1456.368299	52.613562	66.040602
1455.694672	45.846591	66.045607
1454.931890	44.796583	66.050612
1453.776916	48.599265	66.055617
1453.458069	53.138658	66.060622
1453.042565	51.545678	66.065626
1452.437359	50.148187	66.070631
1451.773159	41.291941	66.075636
1450.873197	46.969698	66.080641
1450.123211	51.549336	66.085646
1449.854691	44.690922	66.090650
1448.858943	54.861573	66.095655
1448.114619	49.181520	66.100660
1447.587084	50.464291	66.105665
1447.264046	43.839409	66.110670
1446.602004	43.511860	66.115674
1445.316596	49.967270	66.120679
1444.857921	36.556724	66.125684
1444.219335	42.936941	66.130689
1443.791609	39.903755	66.135694
1443.710908	34.898764	66.140698
1442.361366	38.493183	66.145703
1441.849531	28.628415	66.150708
1441.270828	45.564183	66.155713
1440.462046	41.562852	66.160718
1439.929754	46.299034	66.165722
1439.064443	42.682755	66.170727
1438.646957	41.363261	66.175732
1437.532928	48.930072	66.180737
1436.849924	56.116807	66.185742
1435.759386	51.360450	66.190746
1435.397673	58.272333	66.195751
1435.033994	51.361525	66.200756
1434.854993	57.481511	66.205761
1433.869047	56.189454	66.210766
1433.120141	45.980406	66.215770
1432.763931	47.020704	66.220775
1431.844832	46.777814	66.225780
1430.679961	51.613198	66.230785
1430.110749	51.362125	66.235790
1429.470066	50.640546	66.240794
1428.888470	50.742498	66.245799
1428.644780	34.520291	66.250804
1428.165519	51.358126	66.255809
1427.339565	42.757720	66.260814
1426.717519	41.940193	66.265818
1425.881668	47.258048	66.270823
1425.397550	46.201001	66.275828
1423.876931	51.356610	66.280833
1423.228706	41.907928	66.285838
1423.645802	44.388413	66.290842
1422.887364	48.445710	66.295847
1422.263591	43.780375	66.300852
1421.283701	50.420719	66.305857
1420.789136	50.381464	66.310862
1420.369244	42.374285	66.315866
1418.473925	58.369439	66.320871
1418.260063	47.059514	66.325876
1417.864236	58.608461	66.330881
1417.558676	48.631406	66.335886
1417.213306	42.038377	66.340890
1415.983527	49.864598	66.345895
1415.673343	42.546764	66.350900
1414.540626	44.877688	66.355905
1413.410494	47.452106	66.360910
1412.872206	56.799229	66.365914
1411.710769	51.297156	66.370919
1411.830702	42.869168	66.375924
1411.607948	55.602244	66.380929
1410.959133	45.664607	66.385934
1410.587525	46.006129	66.390938
1409.141272	60.679084	66.395943
1408.791411	45.967078	66.400948
1408.392432	50.275068	66.405953
1406.804618	45.284516	66.410958
1406.201323	47.912825	66.415962
1405.783987	50.872444	66.420967
1405.525942	48.470579	66.425972
1404.970220	54.492030	66.430977
1404.339401	51.450982	66.435982
1403.432037	39.004969	66.440986
1402.617587	46.063815	66.445991
1402.629737	45.492977	66.450996
1401.288395	51.549833	66.456001
1400.989166	47.576147	66.461006
1400.126000	43.974113	66.466010
1399.658978	45.603749	66.471015
1399.000002	38.355098	66.476020
1398.034011	44.794915	66.481025
1397.159775	48.438636	66.486030
1396.838694	46.360574	66.491034
1396.295252	51.342604	66.496039
1395.273559	49.414469	66.501044
1394.554160	51.428738	66.506049
1394.231717	50.495195	66.511054
1394.100028	51.306414	66.516058
1392.123896	56.643423	66.521063
1392.334067	50.871437	66.526068
1391.426910	51.820136	66.531073
1391.122524	55.323684	66.536078
1390.508920	55.119292	66.541082
1389.374929	59.496264	66.546087
1388.778022	44.759056	66.551092
1388.295476	56.377316	66.556097
1387.008999	55.368018	66.561102
1386.257474	51.155982	66.566106
1385.686347	43.665331	66.571111
1385.069816	53.281228	66.576116
1384.951559	56.111103	66.581121
1384.754768	56.909389	66.586126
1384.233111	50.773227	66.591130
1383.039925	53.851842	66.596135
1382.551465	52.779754	66.601140
1381.712711	49.185780	66.606145
1380.832909	43.335129	66.611150
1380.098578	43.607303	66.616154
1379.594366	51.466820	66.621159
1379.142109	43.575708	66.626164
1378.424553	57.357383	66.631169
1377.248849	52.458129	66.636174
1376.819953	44.188431	66.641178
1376.413996	44.953841	66.646183
1376.293042	46.197412	66.651188
1375.357782	52.504875	66.656193
1374.373891	53.868141	66.661198
1374.156122	41.671176	66.666202
1372.502664	47.569896	66.671207
1372.099731	44.776015	66.676212
1371.761958	49.000900	66.681217
1371.259734	49.210449	66.686222
1370.388721	41.278924	66.691226
1368.766798	50.890881	66.696231
1368.483475	42.356278	66.701236
1368.055940	47.847783	66.706241
1367.847967	42.412630	66.711246
1367.436540	42.715579	66.716250
1366.806983	46.903574	66.721255
1366.095562	39.661539	66.726260
1365.165781	55.753509	66.731265
1364.697586	43.062203	66.736270
1363.891725	47.964819	66.741274
1362.761052	47.005038	66.746279
1362.138837	45.370878	66.751284
1361.700141	45.882169	66.756289
1361.254683	48.018881	66.761294
1360.865623	45.311043	66.766298
1359.958380	56.135993	66.771303
1359.443863	40.943398	66.776308
1358.423691	45.606005	66.781313
1357.226370	54.563468	66.786318
1357.082516	49.679810	66.791322
1356.239970	60.872616	66.796327
1356.143716	50.654093	66.801332
1355.342920	40.810381	66.806337
1354.700273	54.785273	66.811342
1354.420949	45.623568	66.816346
1353.486232	51.159268	66.821351
1352.034187	40.413802	66.826356
1351.156937	44.972210	66.831361
1350.758193	51.854114	66.836366
1350.845735	46.245616	66.841370
1350.521154	54.349108	66.846375
1349.529772	37.982161	66.851380
1348.549108	42.119740	66.856385
1347.856920	49.306865	66.861390
1347.607868	43.193122	66.866394
1346.269661	46.849568	66.871399
1345.735493	49.689065	66.876404
1345.236353	42.879617	66.881409
1344.589386	44.120082	66.886414
1344.275877	47.305470	66.891418
1342.884952	47.741758	66.896423
1342.353247	39.575322	66.901428
1341.872627	44.390685	66.906433
1341.827559	54.262422	66.911438
1340.582245	44.915577	66.916442
1339.475322	52.253040	66.921447
1339.457815	43.163356	66.926452
1338.509024	47.504682	66.931457
1338.673111	44.967404	66.936462
1337.524171	45.340954	66.941466
1336.769042	44.003090	66.946471
1336.378534	40.587775	66.951476
1334.872707	49.233727	66.956481
1333.850797	43.690427	66.961486
1334.098768	42.488722	66.966490
1332.986378	44.799999	66.971495
1332.767087	41.755223	66.976500
1332.904835	49.796538	66.981505
1331.669215	40.474486	66.986510
1330.881626	39.865302	66.991514
1330.373005	46.033814	66.996519
1329.411208	36.361746	67.001524
1328.564404	41.232296	67.006529
1327.940449	38.547307	67.011534
1327.589076	39.741512	67.016538
1326.898767	43.679002	67.021543
1326.118799	36.467263	67.026548
1325.389839	44.243679	67.031553
1324.730281	38.450861	67.036558
1324.552939	38.433885	67.041562
1323.108922	40.607339	67.046567
1322.157979	30.900263	67.051572
1321.644767	36.852068	67.056577
1321.394818	47.256216	67.061582
1321.212790	36.865688	67.066586
1320.437358	41.223520	67.071591
1319.591931	42.017591	67.076596
1318.389129	42.793505	67.081601
1318.254459	41.963211	67.086606
1318.204011	35.146429	67.091610
1317.068401	43.670585	67.096615
1316.583805	26.302344	67.101620
1316.301024	37.330233	67.106625
1314.996104	29.924961	67.111630
1314.432287	28.857888	67.116634
1313.660224	34.115096	67.121639
1312.938321	28.536236	67.126644
1312.009570	35.061259	67.131649
1311.237602	38.498807	67.136654
1311.317867	27.899971	67.141658
1310.359260	41.256342	67.146663
1309.556515	29.642677	67.151668
1309.105387	38.271088	67.156673
1308.539074	33.119515	67.161678
1307.336342	33.580830	67.166682
1306.468855	34.870102	67.171687
1306.163775	37.748140	67.176692
1305.713098	36.522758	67.181697
1304.734547	38.343388	67.186702
1304.809980	31.195600	67.191706
1303.202905	37.804384	67.196711
1302.713264	34.822472	67.201716
1302.509904	43.775950	67.206721
1301.671039	38.378552	67.211726
1301.549718	39.408644	67.216730
1300.186156	40.724031	67.221735
1299.805412	34.394827	67.226740
1299.277910	31.046785	67.231745
1298.102333	39.020048	67.236750
1297.110635	33.601451	67.241754
1296.239274	41.237649	67.246759
1296.214827	45.449945	67.251764
1295.870825	44.670094	67.256769
1295.243754	44.583276	67.261774
1295.377822	38.868139	67.266778
1293.640776	35.640330	67.271783
1293.406399	42.559220	67.276788
1292.511029	38.844703	67.281793
1290.932839	36.725695	67.286798
1290.824478	34.154933	67.291802
1290.136195	46.630994	67.296807
1289.950710	34.482205	67.301812
1289.533734	37.421635	67.306817
1288.735961	48.051798	67.311822
1287.964436	42.513801	67.316826
1286.898223	42.250335	67.321831
1286.926063	40.120838	67.326836
1286.234122	46.887549	67.331841
1285.003345	40.217973	67.336846
1284.849176	34.824539	67.341850
1283.834736	44.244488	67.346855
1282.691480	41.972077	67.351860
1281.657621	37.266060	67.356865
1281.230740	41.391338	67.361870
1281.330233	36.671677	67.366874
1280.677120	41.330661	67.371879
1280.681013	41.822632	67.376884
1279.969750	42.630844	67.381889
1278.584132	37.829925	67.386894
1278.106012	33.921617	67.391898
1276.699122	37.457210	67.396903
1276.138662	37.686212	67.401908
1275.789200	37.828962	67.406913
1275.134514	44.016955	67.411918
1275.014485	35.627694	67.416922
1274.015950	44.706649	67.421927
1273.389622	39.099984	67.426932
1273.065850	35.676015	67.431937
1271.949807	38.898146	67.436942
1271.288011	33.252163	67.441946
1270.808858	45.431512	67.446951
1270.495222	35.515475	67.451956
1269.034022	39.538766	67.456961
1268.489194	43.898964	67.461966
1268.037133	39.600556	67.466970
1267.665590	44.315936	67.471975
1266.981608	32.692211	67.476980
1265.845472	33.804468	67.481985
1264.915237	40.528690	67.486990
1264.634282	39.247414	67.491994
1264.057251	38.713503	67.496999
1263.640016	43.424075	67.502004
1262.276928	36.241924	67.507009
1261.927015	36.545401	67.512014
1262.172842	37.638551	67.517018
1260.440727	37.248320	67.522023
1259.804527	31.856102	67.527028
1259.222830	34.066667	67.532033
1258.870593	39.913552	67.537038
1258.941719	42.404306	67.542042
1257.438725	42.259045	67.547047
1256.299489	40.349488	67.552052
1255.917337	32.672969	67.557057
1255.780237	48.155955	67.562062
1254.985314	37.944969	67.567066
1254.113145	38.256943	67.572071
1253.576247	34.696184	67.577076
1252.949000	39.688224	67.582081
1251.583471	42.932153	67.587086
1251.522530	38.516656	67.592090
1250.673121	45.028895	67.597095
1250.106157	34.623367	67.602100
1249.975115	43.108957	67.607105
1248.821490	40.850567	67.612110
1248.633276	36.445809	67.617114
1247.296995	44.293445	67.622119
1246.429423	46.554141	67.627124
1245.779288	52.125602	67.632129
1245.221449	48.127132	67.637134
1245.367736	38.497075	67.642138
1244.455916	37.928516	67.647143
1244.189215	38.930212	67.652148
1243.423096	44.653757	67.657153
1242.115463	48.201972	67.662158
1241.150735	44.655647	67.667162
1240.012455	41.132722	67.672167
1239.869310	38.176359	67.677172
1239.421865	32.147517	67.682177
1239.013642	47.682840	67.687182
1238.356309	36.667948	67.692186
1238.142100	43.328002	67.697191
1237.325232	35.491449	67.702196
1236.469649	37.692070	67.707201
1235.795917	43.969769	67.712206
1234.756809	44.408218	67.717210
1233.634344	44.596873	67.722215
1233.262845	42.026167	67.727220
1232.878921	53.211502	67.732225
1232.478832	53.224377	67.737230
1232.360215	39.843679	67.742234
1231.178233	46.989937	67.747239
1230.641910	36.059718	67.752244
1229.941093	36.313940	67.757249
1228.589294	47.758135	67.762254
1228.099804	48.236688	67.767258
1227.490252	54.809704	67.772263
1227.126572	55.707223	67.777268
1226.485615	46.673766	67.782273
1225.102800	55.801947	67.787278
1224.771500	39.767667	67.792282
1223.997944	46.900443	67.797287
1223.559636	43.590819	67.802292
1223.511954	46.311508	67.807297
1222.751199	38.968220	67.812302
1222.224450	40.540203	67.817306
1221.408607	46.959072	67.822311
1220.771184	41.857974	67.827316
1219.807090	51.292208	67.832321
1218.925289	42.870751	67.837326
1218.952866	35.731160	67.842330
1217.392264	36.278635	67.847335
1216.466774	33.776336	67.852340
1216.115503	39.653449	67.857345
1215.505362	43.799054	67.862350
1215.498657	34.988971	67.867354
1215.150576	50.927661	67.872359
1214.358560	33.447874	67.877364
1213.720949	35.513682	67.882369
1212.643940	42.214490	67.887374
1211.946589	40.623609	67.892378
1210.852004	47.002971	67.897383
1210.755873	40.466766	67.902388
1209.714767	40.770964	67.907393
1208.493982	40.365042	67.912398
1208.368280	33.076443	67.917402
1207.408460	43.861845	67.922407
1207.324740	38.083347	67.927412
1207.153023	38.453024	67.932417
1206.431947	38.550857	67.937422
1205.573239	32.911760	67.942426
1204.856995	40.589694	67.947431
1203.729499	41.199196	67.952436
1202.695772	41.814352	67.957441
1202.094926	43.214296	67.962446
1202.159714	45.614954	67.967450
1201.115033	45.776483	67.972455
1201.235084	44.775877	67.977460
1200.530918	41.745843	67.982465
1199.742421	48.814473	67.987470
1198.445554	42.890413	67.992474
1197.634011	44.727465	67.997479
1196.380869	33.749864	68.002484
1196.078337	37.151653	68.007489
1195.596123	41.632574	68.012494
1195.539745	35.083646	68.017498
1195.395756	37.002575	68.022503
1194.785632	42.436139	68.027508
1193.944257	39.112247	68.032513
1192.746863	41.419159	68.037518
1191.768546	38.905780	68.042522
1190.733898	40.618014	68.047527
1190.980708	46.028797	68.052532
1190.539315	38.984503	68.057537
1189.821842	44.107649	68.062542
1188.856794	31.009647	68.067546
1188.071850	46.859322	68.072551
1187.081183	36.213737	68.077556
1186.256429	44.301416	68.082561
1185.189239	35.649623	68.087566
1185.536925	34.125724	68.092570
1184.773377	39.952249	68.097575
1184.239504	28.985707	68.102580
1184.157471	38.617050	68.107585
1182.640925	45.788626	68.112590
1182.227780	37.503639	68.117594
1181.811801	43.576165	68.122599
1180.967507	39.696225	68.127604
1179.812651	40.378307	68.132609
1178.974707	42.828140	68.137614
1178.871915	43.755593	68.142618
1178.446484	42.430775	68.147623
1177.888576	39.256893	68.152628
1176.863348	39.857179	68.157633
1175.934526	45.860024	68.162638
1175.347841	40.666567	68.167642
1175.120928	51.073869	68.172647
1174.194066	40.922992	68.177652
1173.390844	31.203297	68.182657
1173.285940	36.220768	68.187662
1172.702518	24.809975	68.192666
1171.454516	31.339152	68.197671
1170.955387	39.818289	68.202676
1170.582779	36.227833	68.207681
1169.239232	45.822165	68.212686
1168.522200	37.045688	68.217690
1168.030784	36.748564	68.222695
1167.668347	40.452307	68.227700
1167.310032	31.472314	68.232705
1166.182465	43.814389	68.237710
1165.507133	31.024797	68.242714
1164.701092	39.235975	68.247719
1164.786648	32.440918	68.252724
1164.156086	31.094780	68.257729
1163.011423	46.112409	68.262734
1162.444405	28.729903	68.267738
1161.624867	46.789201	68.272743
1160.543532	41.605447	68.277748
1160.070704	36.514072	68.282753
1159.530779	39.174576	68.287758
1158.748365	32.391565	68.292762
1158.382638	45.856026	68.297767
1157.958466	39.236661	68.302772
1156.842139	42.763584	68.307777
1155.960168	42.314266	68.312782
1155.971496	38.135467	68.317786
1155.286490	43.362788	68.322791
1154.730453	35.371075	68.327796
1153.685022	36.606766	68.332801
1152.944608	41.947384	68.337806
1152.770536	37.836644	68.342810
1151.241844	39.511117	68.347815
1151.113430	43.395042	68.352820
1150.385651	41.516501	68.357825
1149.941183	47.330631	68.362830
1149.374725	33.187468	68.367834
1148.081808	40.019195	68.372839
1147.455508	52.178742	68.377844
1147.446515	41.694271	68.382849
1146.729811	39.313729	68.387854
1145.585055	37.017138	68.392858
1144.712489	42.518931	68.397863
1144.280221	42.179710	68.402868
1144.299913	45.605271	68.407873
1143.579989	47.319280	68.412878
1142.968074	38.351134	68.417882
1142.051309	45.663561	68.422887
1141.221661	33.073678	68.427892
1140.099504	33.442686	68.432897
1139.422544	42.744076	68.437902
1139.060290	30.968987	68.442906
1138.745462	44.537224	68.447911
1138.324364	38.642430	68.452916
1137.367962	38.699256	68.457921
1136.387946	41.390121	68.462926
1135.831155	36.401938	68.467930
1135.484369	40.306675	68.472935
1134.708876	34.622164	68.477940
1133.353979	42.187233	68.482945
1132.911664	47.700616	68.487950
1132.993043	38.603102	68.492954
1131.866092	39.473433	68.497959
1130.943090	36.366811	68.502964
1130.533297	36.302412	68.507969
1129.977511	48.325941	68.512974
1130.032931	42.914392	68.517978
1128.697334	41.002570	68.522983
1128.057018	37.167842	68.527988
1127.733701	41.502354	68.532993
1126.439997	46.945611	68.537998
1126.052549	45.223919	68.543002
1125.477380	50.992935	68.548007
1124.707360	46.173492	68.553012
1124.267189	44.285969	68.558017
1122.919043	48.580451	68.563022
1122.474602	37.720571	68.568026
1121.863363	42.885134	68.573031
1121.674215	45.009155	68.578036
1120.784225	39.835278	68.583041
1120.008921	45.708031	68.588046
1119.739427	38.750360	68.593050
1118.936104	40.018019	68.598055
1117.726821	40.984158	68.603060
1117.142464	45.587964	68.608065
1116.250360	39.951841	68.613070
1116.199652	44.563343	68.618074
1115.835042	36.512412	68.623079
1114.900609	44.495332	68.628084
1114.156076	48.757507	68.633089
1113.339214	40.244438	68.638094
1113.546829	36.493454	68.643098
1112.464560	44.751543	68.648103
1111.351816	41.830959	68.653108
1110.712567	36.153910	68.658113
1109.640883	47.144389	68.663118
1108.775246	37.102649	68.668122
1108.554579	45.169390	68.673127
1107.875323	42.761916	68.678132
1107.569742	33.873555	68.683137
1107.174761	51.913840	68.688142
1106.932661	38.716538	68.693146
1105.803524	40.011965	68.698151
1105.019052	43.461547	68.703156
1103.942262	44.783140	68.708161
1103.153167	47.849851	68.713166
1102.610078	33.038786	68.718170
1102.353297	41.853775	68.723175
1102.106058	38.948006	68.728180
1101.214646	44.604997	68.733185
1100.174641	40.667013	68.738190
1099.704630	46.031989	68.743194
1098.613900	42.457935	68.748199
1097.888351	44.445662	68.753204
1097.360772	33.430298	68.758209
1096.815988	52.185408	68.763214
1096.886548	45.138719	68.768218
1096.060064	43.119597	68.773223
1095.039940	37.340412	68.778228
1094.557726	48.746242	68.783233
1093.175702	52.099213	68.788238
1092.436335	38.374071	68.793242
1091.488896	37.932423	68.798247
1091.415792	43.586651	68.803252
1091.149335	35.392609	68.808257
1090.549232	41.623368	68.813262
1090.412855	41.064940	68.818266
1089.467994	44.697507	68.823271
1088.702800	43.582450	68.828276
1087.918416	42.024648	68.833281
1086.332725	43.703769	68.838286
1085.890937	42.560567	68.843290
1085.442206	42.605466	68.848295
1085.065526	42.079504	68.853300
1084.919076	26.303735	68.858305
1083.504186	42.966633	68.863310
1082.873813	36.541661	68.868314
1082.473250	41.722647	68.873319
1081.630539	35.112207	68.878324
1081.680782	37.040505	68.883329
1080.630763	38.070954	68.888334
1079.956591	32.708167	68.893338
1079.462583	42.015728	68.898343
1077.998101	40.899635	68.903348
1077.314949	40.227611	68.908353
1076.664641	49.319981	68.913358
1076.459017	39.076811	68.918362
1076.059887	37.524090	68.923367
1075.235063	37.801542	68.928372
1074.568987	31.222828	68.933377
1073.689065	44.853487	68.938382
1073.481494	36.841984	68.943386
1072.037987	39.572362	68.948391
1071.470043	41.171543	68.953396
1071.301693	33.580409	68.958401
1070.845659	48.928916	68.963406
1070.506855	39.965330	68.968410
1069.346446	44.510686	68.973415
1068.821197	45.135897	68.978420
1067.851726	32.258944	68.983425
1066.848426	47.722874	68.988430
1066.375548	31.906691	68.993434
1065.811262	47.454908	68.998439
1065.286325	34.672743	69.003444
1065.336823	36.932954	69.008449
1064.243466	39.749813	69.013454
1063.426571	42.815762	69.018458
1062.143366	36.111819	69.023463
1061.492155	44.082558	69.028468
1061.415381	43.088814	69.033473
1060.787716	37.907528	69.038478
1060.764535	42.336295	69.043482
1059.295396	41.430995	69.048487
1058.530920	39.583621	69.053492
1057.565900	41.604072	69.058497
1057.263152	41.584897	69.063502
1056.246661	33.372466	69.068506
1055.646337	44.457878	69.073511
1055.113341	46.748935	69.078516
1054.623999	43.137036	69.083521
1053.657828	49.023141	69.088526
1053.937418	43.886612	69.093530
1052.341380	43.444731	69.098535
1051.530562	42.693132	69.103540
1051.353086	33.276027	69.108545
1050.630231	44.983180	69.113550
1050.835923	41.463038	69.118554
1049.622301	42.866492	69.123559
1049.253954	48.165906	69.128564
1048.346537	39.948215	69.133569
1046.743154	50.389129	69.138574
1046.350691	41.569333	69.143578
1046.010675	41.509965	69.148583
1045.501969	38.325310	69.153588
1045.091837	37.784159	69.158593
1044.021369	37.071894	69.163598
1043.600113	37.950863	69.168602
1042.484873	45.576748	69.173607
1042.234007	40.169499	69.178612
1041.308582	41.841348	69.183617
1040.382884	44.495298	69.188622
1040.248650	37.130416	69.193626
1039.796226	47.691582	69.198631
1039.299964	39.187970	69.203636
1038.421615	35.177321	69.208641
1037.506726	46.004383	69.213646
1036.961188	37.946556	69.218650
1035.937208	44.234119	69.223655
1035.435662	42.307382	69.228660
1035.390319	37.375702	69.233665
1034.017479	41.179458	69.238670
1033.005275	30.452750	69.243674
1032.607213	35.391347	69.248679
1032.280289	35.718927	69.253684
1031.829152	33.504100	69.258689
1031.022213	40.607476	69.263694
1030.121275	34.776715	69.268698
1029.526300	44.403526	69.273703
1029.074490	41.850542	69.278708
1028.494115	35.473463	69.283713
1027.435190	44.521340	69.288718
1026.875265	36.919113	69.293722
1026.567500	34.771703	69.298727
1025.482359	40.698312	69.303732
1024.963118	37.723874	69.308737
1023.770212	33.577239	69.313742
1023.914362	32.953010	69.318746
1023.316007	35.509853	69.323751
1022.415452	39.370882	69.328756
1021.493141	36.640329	69.333761
1020.783776	45.136528	69.338766
1020.507625	34.022469	69.343770
1019.220488	41.547931	69.348775
1019.115772	43.599471	69.353780
1018.361100	33.029179	69.358785
1018.231430	40.485493	69.363790
1017.279641	23.593251	69.368794
1016.353388	38.936222	69.373799
1015.323753	31.616534	69.378804
1015.412309	34.083766	69.383809
1014.230608	34.043811	69.388814
1013.454629	24.028593	69.393818
1013.001474	33.950041	69.398823
1012.494029	29.641025	69.403828
1012.161082	27.973956	69.408833
1010.604833	38.731255	69.413838
1010.249452	34.235547	69.418842
1009.800283	29.765375	69.423847
1009.217952	34.649087	69.428852
1008.647155	24.389927	69.433857
1007.412250	30.012596	69.438862
1006.856379	30.033221	69.443866
1006.403306	31.091711	69.448871
1006.049445	31.138922	69.453876
1004.790748	22.344340	69.458881
1004.018684	27.605918	69.463886
1003.935593	30.433711	69.468890
1003.283755	26.888728	69.473895
1002.540925	32.410550	69.478900
1001.957916	34.658467	69.483905
1001.030408	31.439758	69.488910
1001.141588	30.894197	69.493914
1000.453345	25.519233	69.498919
999.288746	23.918411	69.503924
998.803018	21.257565	69.508929
997.504633	31.106273	69.513934
996.658813	28.935361	69.518938
996.030444	25.890411	69.523943
995.670754	21.777926	69.528948
995.622084	24.797970	69.533953
995.073513	38.576737	69.538958
994.520662	22.583631	69.543962
993.621843	22.748249	69.548967
992.393615	25.005222	69.553972
991.263448	23.733620	69.558977
990.384856	36.932622	69.563982
990.221518	24.279205	69.568986
989.887387	34.198425	69.573991
989.399305	35.223046	69.578996
989.299528	37.615958	69.584001
987.968474	32.993283	69.589006
987.643146	35.608760	69.594010
986.816544	35.181963	69.599015
985.598531	34.493006	69.604020
985.139307	29.918776	69.609025
984.073233	41.344462	69.614030
983.776213	27.772146	69.619034
983.497211	29.991288	69.624039
982.877041	33.246964	69.629044
981.974065	37.467999	69.634049
981.336332	41.295470	69.639054
981.478141	29.856828	69.644058
980.520616	35.542126	69.649063
979.342891	39.073675	69.654068
978.828940	35.443899	69.659073
978.128497	35.259957	69.664078
977.114711	31.436325	69.669082
976.638879	40.562361	69.674087
976.478120	34.152111	69.679092
975.563725	26.863619	69.684097
974.451075	37.076820	69.689102
974.368285	39.952323	69.694106
973.447639	32.585956	69.699111
972.320448	33.900813	69.704116
971.525870	30.962486	69.709121
971.073276	36.253826	69.714126
970.825546	26.813639	69.719130
969.687331	23.956270	69.724135
969.366376	28.037759	69.729140
969.454064	25.997093	69.734145
968.063657	30.740135	69.739150
967.657443	23.006607	69.744154
967.129653	28.498708	69.749159
966.468243	34.598663	69.754164
965.064243	26.371318	69.759169
964.689387	31.184763	69.764174
964.202293	22.135687	69.769178
964.028239	29.374212	69.774183
962.802820	38.295089	69.779188
962.148923	26.685243	69.784193
961.351983	28.118796	69.789198
961.224675	22.168982	69.794202
960.251199	30.966185	69.799207
959.404103	30.756444	69.804212
959.040668	30.662806	69.809217
958.459744	38.165612	69.814222
957.191246	37.257952	69.819226
956.723947	34.822098	69.824231
955.817406	44.806596	69.829236
956.135053	25.665757	69.834241
955.183379	37.562481	69.839246
954.011880	33.201422	69.844250
953.506872	33.977511	69.849255
953.156955	31.505371	69.854260
952.736077	25.223752	69.859265
951.599628	30.156185	69.864270
950.745292	28.118575	69.869274
950.579725	32.645138	69.874279
949.807991	32.699582	69.879284
948.966479	32.945177	69.884289
947.884699	37.791676	69.889294
947.729661	27.092263	69.894298
947.028934	24.230627	69.899303
945.959996	32.221594	69.904308
945.709838	33.909643	69.909313
945.355265	37.953474	69.914318
944.684609	21.451246	69.919322
943.964582	34.667694	69.924327
942.935646	33.197986	69.929332
942.560458	24.518146	69.934337
941.693075	31.464123	69.939342
940.966536	22.415800	69.944346
940.145195	23.348694	69.949351
939.538350	31.479192	69.954356
939.132689	33.295315	69.959361
938.505153	30.183920	69.964366
937.493739	22.466423	69.969370
936.844618	28.838600	69.974375
936.130789	36.249701	69.979380
936.300164	18.999298	69.984385
935.431973	37.100066	69.989390
934.594649	37.292844	69.994394
934.424076	31.585690	69.999399
932.972715	39.565586	70.004404
932.410274	27.470373	70.009409
931.517743	36.668564	70.014414
931.301226	30.091827	70.019418
930.674274	32.245045	70.024423
929.467260	30.423360	70.029428
928.943642	27.114573	70.034433
927.878657	23.896139	70.039438
927.914500	33.591736	70.044442
927.359190	31.531730	70.049447
926.650815	32.585008	70.054452
926.264722	27.943791	70.059457
925.220597	36.702576	70.064462
924.944537	30.826790	70.069466
923.866130	32.712350	70.074471
922.916346	31.638409	70.079476
922.801138	30.223381	70.084481
922.430910	34.668161	70.089486
921.175757	29.603453	70.094490
920.900044	32.774088	70.099495
920.115149	38.258916	70.104500
918.658378	27.529052	70.109505
917.939897	40.892469	70.114510
917.489903	28.224214	70.119514
916.760447	29.533326	70.124519
917.010220	31.722297	70.129524
916.599898	30.392945	70.134529
915.496202	30.490436	70.139534
914.618703	27.969721	70.144538
913.929017	23.283010	70.149543
913.437493	33.857176	70.154548
912.356577	26.872338	70.159553
911.993151	31.651460	70.164558
911.652055	30.324067	70.169562
911.557584	40.252763	70.174567
909.850542	34.108149	70.179572
909.757098	29.624036	70.184577
908.816929	32.258379	70.189582
908.102047	20.700443	70.194586
907.508386	28.789211	70.199591
906.949068	29.363829	70.204596
905.997786	31.580888	70.209601
904.485583	31.890841	70.214606
904.332774	30.009780	70.219610
903.807200	29.857079	70.224615
903.672873	36.857498	70.229620
903.442212	31.754685	70.234625
902.525135	39.068766	70.239630
901.495127	36.372869	70.244634
900.783739	22.058039	70.249639
899.540677	34.343733	70.254644
898.473888	29.627670	70.259649
898.745300	38.525855	70.264654
898.107312	29.770644	70.269658
897.645910	34.064471	70.274663
897.401853	41.316962	70.279668
896.270832	29.319141	70.284673
895.439210	34.332395	70.289678
895.229697	28.622837	70.294682
894.056045	37.688402	70.299687
893.062375	31.756724	70.304692
892.522348	30.893249	70.309697
891.866548	39.679866	70.314702
891.166697	36.227987	70.319706
891.188514	32.771312	70.324711
890.487224	40.662613	70.329716
889.594669	34.386002	70.334721
888.867647	33.546662	70.339726
888.393301	35.794530	70.344730
887.588284	40.726655	70.349735
886.299788	51.605485	70.354740
885.971589	31.212712	70.359745
885.412759	46.659331	70.364750
885.538892	32.668783	70.369754
884.535838	34.520919	70.374759
883.631800	33.876495	70.379764
883.439832	22.977773	70.384769
882.313093	33.956380	70.389774
881.472138	36.175072	70.394778
880.797504	30.412557	70.399783
880.162165	35.178258	70.404788
879.978718	39.255540	70.409793
879.114920	36.009367	70.414798
878.764272	37.437934	70.419802
878.062297	39.854653	70.424807
876.819587	39.875705	70.429812
876.268251	34.207328	70.434817
875.410389	34.367715	70.439822
874.629370	38.380386	70.444826
874.508630	32.138152	70.449831
873.851752	35.588010	70.454836
872.486483	29.167386	70.459841
871.959532	29.717911	70.464846
871.705068	33.428035	70.469850
871.602453	32.024668	70.474855
870.377342	35.979990	70.479860
869.815159	31.593929	70.484865
868.936395	38.644886	70.489870
868.345958	32.886503	70.494874
867.528414	35.566556	70.499879
866.534025	33.201260	70.504884
866.670442	23.131640	70.509889
865.732384	39.867217	70.514894
865.557204	31.279833	70.519898
864.373082	32.644331	70.524903
863.587865	35.218590	70.529908
863.544134	29.442747	70.534913
862.567682	33.355084	70.539918
861.827907	33.770758	70.544922
861.234039	36.460656	70.549927
860.575428	36.022474	70.554932
860.265905	28.703430	70.559937
859.091447	37.813345	70.564942
858.366437	30.179830	70.569946
857.837903	30.139740	70.574951
856.876020	39.339160	70.579956
856.317970	36.468098	70.584961
855.732904	38.703356	70.589966
855.234040	41.761435	70.594970
855.161007	38.450473	70.599975
853.696415	33.799401	70.604980
853.332906	25.871482	70.609985
852.722433	30.465170	70.614990
851.828717	37.485534	70.619994
851.126767	29.661371	70.624999
850.298109	32.270703	70.630004
850.035487	30.715148	70.635009
849.446291	32.651919	70.640014
848.511269	34.159270	70.645018
847.842937	38.238689	70.650023
846.804944	32.862480	70.655028
846.614049	25.139851	70.660033
846.389341	35.875145	70.665038
845.169659	32.511132	70.670042
844.636247	27.069417	70.675047
843.888057	33.118721	70.680052
843.801293	26.682394	70.685057
842.691414	30.490095	70.690062
841.856079	23.193230	70.695066
841.194084	29.277503	70.700071
840.696202	32.034246	70.705076
840.273148	21.828368	70.710081
839.157823	41.151272	70.715086
838.695677	32.505683	70.720090
838.294407	35.087991	70.725095
836.857757	29.921774	70.730100
836.435712	32.660396	70.735105
835.917466	40.264965	70.740110
835.577817	26.605251	70.745114
835.287711	33.149612	70.750119
833.921786	35.405737	70.755124
833.396303	29.567555	70.760129
832.601921	34.509704	70.765134
832.417902	38.563006	70.770138
831.182599	25.116314	70.775143
830.448051	39.499662	70.780148
830.182721	30.686159	70.785153
829.308982	37.167475	70.790158
829.148790	33.881708	70.795162
828.467396	28.785456	70.800167
827.429950	34.480912	70.805172
826.928731	29.339588	70.810177
825.748046	34.564607	70.815182
825.081251	32.430163	70.820186
824.550710	31.727300	70.825191
823.942870	38.264907	70.830196
824.141367	32.241927	70.835201
822.817504	35.476058	70.840206
822.393089	29.326898	70.845210
822.631846	32.339940	70.850215
821.316161	34.606408	70.855220
820.404847	30.296342	70.860225
819.329623	38.363402	70.865230
818.463241	36.672071	70.870234
817.686658	23.098261	70.875239
817.355459	36.850047	70.880244
816.922988	36.340374	70.885249
816.767682	38.197695	70.890254
815.662973	26.075406	70.895258
815.219232	28.993787	70.900263
814.392595	34.257630	70.905268
813.526223	23.110120	70.910273
812.642259	31.554918	70.915278
811.967566	26.362397	70.920282
811.656748	33.665000	70.925287
810.746938	37.593166	70.930292
810.674437	25.796145	70.935297
809.241289	30.121042	70.940302
808.506748	30.977119	70.945306
807.876500	34.605964	70.950311
807.466451	32.122824	70.955316
807.089070	20.303036	70.960321
806.700226	29.705463	70.965326
805.638106	23.505685	70.970330
804.876788	29.938535	70.975335
804.473453	36.248885	70.980340
803.962090	20.394775	70.985345
803.021481	25.913783	70.990350
802.641641	28.272566	70.995354
801.638785	30.055608	71.000359
800.535878	33.498986	71.005364
800.113237	27.955413	71.010369
799.459513	33.147403	71.015374
799.068843	34.420602	71.020378
798.897046	28.681700	71.025383
797.591733	37.184865	71.030388
797.221375	29.050506	71.035393
796.388186	43.244713	71.040398
796.171432	35.596774	71.045402
795.115664	32.076810	71.050407
793.969095	37.651235	71.055412
793.908647	28.321091	71.060417
793.413258	31.999463	71.065422
792.417020	30.982451	71.070426
791.656555	25.447410	71.075431
790.768054	30.652776	71.080436
790.679505	26.801746	71.085441
789.971399	32.532759	71.090446
788.998064	28.643433	71.095450
788.364934	24.698989	71.100455
787.993955	36.647032	71.105460
787.652969	25.960156	71.110465
786.566885	37.292975	71.115470
785.591772	27.774533	71.120474
785.577315	26.180025	71.125479
784.550293	32.041849	71.130484
783.584830	21.570891	71.135489
783.049008	24.560702	71.140494
782.325008	24.867507	71.145498
782.291873	33.746003	71.150503
780.901194	36.388860	71.155508
779.975769	20.050717	71.160513
779.628481	31.142114	71.165518
779.209504	29.920041	71.170522
779.124318	16.324517	71.175527
777.858185	23.822733	71.180532
777.331816	15.728530	71.185537
776.695265	28.112431	71.190542
776.145912	25.940906	71.195546
775.084535	30.137789	71.200551
774.254613	31.187830	71.205556
774.062226	23.921757	71.210561
773.549251	30.400484	71.215566
773.066501	34.928092	71.220570
771.993244	27.925406	71.225575
771.308102	35.269238	71.230580
771.066811	24.858956	71.235585
769.815796	34.270138	71.240590
769.173789	30.551415	71.245594
768.644180	24.354368	71.250599
767.847060	38.059656	71.255604
767.963310	32.100896	71.260609
766.887178	31.427952	71.265614
766.156626	28.594349	71.270618
765.499950	28.653979	71.275623
764.315645	37.416273	71.280628
763.848323	24.228028	71.285633
763.463585	26.748300	71.290638
762.863312	21.175958	71.295642
762.888956	26.112235	71.300647
761.363391	24.115441	71.305652
760.827789	24.786269	71.310657
759.778203	28.440376	71.315662
758.897534	24.110867	71.320666
758.685855	27.954574	71.325671
758.086914	28.257722	71.330676
757.973941	24.021295	71.335681
756.877972	34.549406	71.340686
755.759888	28.814333	71.345690
755.549599	32.645567	71.350695
754.702148	26.832951	71.355700
754.149902	28.506048	71.360705
753.142964	30.388083	71.365710
752.462131	29.386913	71.370714
752.165291	28.352724	71.375719
751.709911	27.951582	71.380724
751.226511	24.563304	71.385729
750.043380	32.815820	71.390734
749.643243	32.220092	71.395738
749.537103	25.668678	71.400743
748.515569	36.699538	71.405748
747.698857	19.369024	71.410753
747.118992	31.931100	71.415758
745.760217	24.068703	71.420762
745.028742	26.942042	71.425767
744.150229	26.843110	71.430772
744.391625	22.324149	71.435777
743.613214	23.742717	71.440782
743.108301	18.782428	71.445786
742.230827	20.977792	71.450791
740.920454	22.527752	71.455796
740.697202	17.927741	71.460801
740.382044	24.125883	71.465806
740.160782	21.650277	71.470810
739.134119	16.770686	71.475815
737.988547	28.931542	71.480820
738.024454	29.870763	71.485825
737.160802	18.227447	71.490830
736.366024	23.620829	71.495834
735.715831	24.783368	71.500839
735.128489	29.948991	71.505844
734.421365	30.996159	71.510849
733.437338	35.424523	71.515854
732.616778	33.344461	71.520858
732.143263	30.473146	71.525863
731.651001	36.418227	71.530868
731.443861	29.742808	71.535873
730.212467	33.932511	71.540878
729.850880	25.090914	71.545882
729.654052	30.730002	71.550887
728.156258	42.324403	71.555892
727.734932	31.843918	71.560897
726.864397	33.595622	71.565902
726.385615	40.172307	71.570906
725.921498	30.792514	71.575911
724.986296	39.825938	71.580916
724.488248	30.807201	71.585921
724.230767	34.592445	71.590926
722.769220	39.501672	71.595930
722.138078	32.586671	71.600935
721.472051	35.663922	71.605940
721.405468	28.448534	71.610945
720.647477	34.724516	71.615950
720.131495	38.608516	71.620954
719.613030	33.412140	71.625959
718.519346	31.044152	71.630964
717.882892	29.472128	71.635969
716.800933	26.534535	71.640974
716.492381	28.887424	71.645978
716.103902	14.918763	71.650983
715.191707	26.740051	71.655988
714.529571	20.108640	71.660993
713.645716	30.421215	71.665998
713.398784	30.930101	71.671002
712.659495	31.557281	71.676007
711.302640	31.464912	71.681012
711.105525	21.516389	71.686017
710.352844	23.346978	71.691022
709.980423	34.031781	71.696026
709.514129	28.338604	71.701031
708.379976	32.960838	71.706036
707.814114	35.898569	71.711041
707.745192	37.372035	71.716046
706.412741	39.371025	71.721050
705.698310	34.006130	71.726055
704.814709	40.789923	71.731060
704.469365	23.792721	71.736065
704.088095	38.271457	71.741070
703.391112	34.257443	71.746074
702.723857	35.771443	71.751079
701.745104	40.182331	71.756084
701.512001	27.628935	71.761089
700.931740	27.054203	71.766094
700.001029	31.088196	71.771098
699.211525	26.979515	71.776103
698.991883	26.942968	71.781108
698.080385	26.765621	71.786113
697.085776	36.298274	71.791118
696.308077	31.820092	71.796122
696.063883	32.390480	71.801127
695.616134	23.695879	71.806132
694.529370	18.615424	71.811137
693.998103	23.943142	71.816142
693.073758	27.698955	71.821146
693.176054	28.683639	71.826151
691.874902	29.819162	71.831156
691.136647	34.956962	71.836161
690.345364	26.379238	71.841166
689.981213	33.908859	71.846170
689.707680	25.491500	71.851175
688.759088	32.792054	71.856180
688.282334	37.094048	71.861185
687.755646	35.352442	71.866190
686.865200	31.134353	71.871194
685.883808	30.368227	71.876199
684.839613	36.483258	71.881204
685.006283	27.566560	71.886209
684.585324	30.653141	71.891214
683.686176	32.421991	71.896218
682.698686	32.736454	71.901223
681.753677	27.281208	71.906228
681.575699	22.739757	71.911233
681.336078	32.944728	71.916238
680.149747	27.012172	71.921242
680.003187	26.875084	71.926247
679.326730	41.824368	71.931252
678.591546	31.955791	71.936257
677.517346	33.520171	71.941262
676.680830	34.023495	71.946266
675.807002	29.431136	71.951271
674.997089	37.952470	71.956276
674.620629	26.458976	71.961281
674.418729	34.739570	71.966286
673.977312	38.846837	71.971290
673.718996	21.537911	71.976295
672.195030	36.108997	71.981300
671.647619	33.738611	71.986305
669.958060	30.234901	71.991310
669.738143	32.596290	71.996314
669.862662	25.088051	72.001319
668.833207	33.571210	72.006324
668.615064	34.691710	72.011329
668.001272	37.418195	72.016334
666.404552	39.997704	72.021338
666.116998	36.029598	72.026343
665.673785	37.753889	72.031348
665.084883	33.597820	72.036353
664.740371	35.203759	72.041358
663.537910	36.227255	72.046362
662.787746	30.218397	72.051367
661.957780	41.286706	72.056372
662.099167	29.237150	72.061377
661.115837	43.976922	72.066382
659.921480	36.451491	72.071386
659.673166	30.660979	72.076391
658.992053	38.819214	72.081396
658.867079	32.805476	72.086401
657.538683	35.160605	72.091406
656.477556	38.618563	72.096410
656.390899	34.895102	72.101415
656.004470	36.482567	72.106420
655.187799	24.726228	72.111425
654.327072	29.175317	72.116430
654.065222	32.993281	72.121434
653.572178	32.268620	72.126439
651.983949	39.675217	72.131444
651.618947	25.343349	72.136449
650.795636	26.888433	72.141454
650.883084	32.198173	72.146458
650.480195	31.621478	72.151463
649.469448	40.174460	72.156468
648.564047	21.199795	72.161473
647.409826	33.072031	72.166478
646.569611	31.855041	72.171482
646.648076	30.070546	72.176487
645.802612	30.552120	72.181492
645.576896	25.378230	72.186497
644.791914	28.591914	72.191502
643.931103	29.393073	72.196506
643.149099	21.204542	72.201511
642.021928	38.523936	72.206516
641.646850	28.096729	72.211521
641.096163	25.858744	72.216526
640.652617	35.726043	72.221530
640.274499	25.094896	72.226535
639.194255	23.816012	72.231540
638.346028	22.762624	72.236545
637.882857	25.466067	72.241550
637.608875	30.853519	72.246554
636.750585	17.137067	72.251559
636.160013	30.264232	72.256564
634.935395	26.644168	72.261569
634.552866	26.566062	72.266574
633.905068	34.620305	72.271578
632.971018	20.824469	72.276583
632.102368	33.430496	72.281588
631.959934	30.472866	72.286593
631.803342	22.007458	72.291598
630.411983	23.312784	72.296602
629.855631	19.442447	72.301607
629.051425	27.660055	72.306612
629.100488	26.283601	72.311617
628.205402	28.746855	72.316622
627.145894	27.293114	72.321626
626.799968	34.521997	72.326631
625.667875	33.142268	72.331636
625.683998	21.017874	72.336641
624.638990	26.019167	72.341646
623.623613	29.939000	72.346650
623.493551	22.847388	72.351655
622.613036	37.937018	72.356660
622.173261	28.682148	72.361665
621.176492	37.805467	72.366670
620.662409	32.032469	72.371674
620.347844	24.177514	72.376679
619.416505	26.923674	72.381684
618.702868	23.461974	72.386689
618.012507	28.543024	72.391694
617.251273	31.582522	72.396698
617.223428	27.993059	72.401703
615.940698	38.172289	72.406708
615.432730	36.797726	72.411713
615.102059	36.833097	72.416718
614.438758	37.196629	72.421722
613.389739	22.222934	72.426727
612.921079	34.465580	72.431732
612.413009	28.766945	72.436737
611.021808	29.423340	72.441742
610.476013	29.707927	72.446746
609.639572	23.524009	72.451751
609.130106	35.837985	72.456756
608.999610	26.373427	72.461761
608.975735	32.814936	72.466766
607.402228	29.276761	72.471770
607.345705	30.313127	72.476775
606.412329	36.731269	72.481780
605.852166	26.719049	72.486785
604.875588	26.888377	72.491790
604.240545	33.110937	72.496794
603.105262	25.233982	72.501799
601.981082	35.039093	72.506804
601.999891	31.518605	72.511809
601.668750	40.167506	72.516814
601.251564	29.336229	72.521818
600.555591	17.034263	72.526823
599.173463	34.248925	72.531828
599.104795	28.983397	72.536833
598.508143	26.964860	72.541838
597.893366	28.025433	72.546842
597.214377	29.155426	72.551847
596.188029	36.622465	72.556852
595.624462	35.830161	72.561857
595.209321	29.303285	72.566862
594.124074	32.016219	72.571866
593.721969	25.315016	72.576871
592.693253	33.033497	72.581876
592.726165	24.667457	72.586881
591.670304	24.270933	72.591886
590.650094	25.535571	72.596890
590.579109	24.107059	72.601895
590.138748	27.896403	72.606900
589.324152	27.264736	72.611905
588.511406	23.514120	72.616910
587.799243	26.354566	72.621914
587.065431	20.610149	72.626919
585.681917	32.866263	72.631924
585.527712	17.641771	72.636929
585.143706	29.110083	72.641934
584.639538	30.776143	72.646938
584.170379	21.752490	72.651943
582.742288	31.159700	72.656948
582.210813	27.528645	72.661953
581.811203	31.527310	72.666958
581.380396	24.242904	72.671962
580.216033	19.424446	72.676967
579.634461	30.269413	72.681972
579.345042	24.050981	72.686977
578.483035	35.654486	72.691982
577.348878	35.951867	72.696986
576.771487	28.604160	72.701991
576.239346	36.434917	72.706996
575.971680	27.746190	72.712001
575.690344	32.710190	72.717006
574.346466	28.681524	72.722010
573.987293	31.596088	72.727015
573.186814	39.525321	72.732020
572.596979	29.076901	72.737025
571.501023	27.855985	72.742030
570.899763	25.423398	72.747034
570.518134	31.573329	72.752039
570.118548	35.897631	72.757044
569.412143	28.843199	72.762049
568.375841	23.567037	72.767054
567.936544	35.934512	72.772058
567.591831	24.819263	72.777063
566.663227	25.291019	72.782068
566.082433	28.927200	72.787073
565.184857	24.104478	72.792078
564.927579	34.669289	72.797082
563.578443	28.788347	72.802087
562.923527	29.898826	72.807092
562.637590	24.221346	72.812097
562.522513	20.803141	72.817102
560.925392	36.516844	72.822106
560.260657	27.015550	72.827111
559.558716	28.497223	72.832116
559.187335	30.866411	72.837121
559.238724	28.983536	72.842126
558.449654	29.673739	72.847130
557.909969	27.044693	72.852135
556.603805	30.722670	72.857140
555.447835	30.760914	72.862145
554.929461	32.588481	72.867150
554.336463	32.159625	72.872154
554.348455	24.686068	72.877159
553.656216	32.035075	72.882164
552.737090	24.352006	72.887169
552.017214	24.022256	72.892174
551.313281	32.742134	72.897178
551.096876	23.593471	72.902183
549.819685	28.999277	72.907188
549.362094	26.972314	72.912193
549.034998	29.318520	72.917198
548.298837	35.241061	72.922202
547.242685	27.994736	72.927207
546.674317	31.987584	72.932212
546.397838	29.824594	72.937217
545.647074	33.832513	72.942222
544.455510	34.662734	72.947226
544.244201	29.514804	72.952231
543.370285	40.818005	72.957236
543.036188	36.307655	72.962241
541.960218	36.521657	72.967246
540.654294	38.091433	72.972250
540.724230	26.382142	72.977255
540.007060	32.132096	72.982260
540.117810	31.077027	72.987265
539.199841	26.883031	72.992270
537.976593	31.682395	72.997274
537.583396	32.533702	73.002279
536.751251	39.616967	73.007284
536.052128	32.160265	73.012289
535.158165	34.126397	73.017294
534.664764	34.773835	73.022298
534.719059	33.608840	73.027303
533.824194	46.413574	73.032308
532.967441	41.094019	73.037313
532.109519	26.805985	73.042318
531.604300	39.437768	73.047322
531.171054	36.198415	73.052327
530.019826	32.836974	73.057332
529.348427	29.603302	73.062337
528.819403	33.090097	73.067342
528.266914	32.200383	73.072346
527.470328	24.924983	73.077351
527.169240	39.086036	73.082356
526.356725	32.379775	73.087361
526.123377	35.639470	73.092366
524.630672	36.858778	73.097370
524.487687	27.492680	73.102375
524.006329	38.324032	73.107380
523.188865	28.393812	73.112385
522.082489	28.035563	73.117390
521.344175	41.401985	73.122394
521.517689	21.085589	73.127399
520.219733	34.387254	73.132404
519.161262	29.308707	73.137409
518.964990	35.742255	73.142414
518.298500	37.161415	73.147418
518.060788	25.240782	73.152423
516.785219	37.215535	73.157428
516.259920	33.031620	73.162433
515.889377	30.100849	73.167438
515.152602	31.391930	73.172442
514.282765	24.387227	73.177447
513.022905	34.410587	73.182452
512.904004	35.234234	73.187457
512.524237	31.216819	73.192462
512.012094	35.181484	73.197466
511.326425	28.177589	73.202471
510.023257	38.587298	73.207476
509.492937	36.429914	73.212481
509.166618	33.062906	73.217486
508.588544	42.328033	73.222490
507.458968	37.014186	73.227495
506.471846	32.187874	73.232500
506.175873	30.794760	73.237505
506.089918	37.668851	73.242510
505.337997	36.154931	73.247514
505.532053	23.657055	73.252519
503.827534	32.270910	73.257524
503.446366	33.293043	73.262529
502.513557	36.002373	73.267534
501.736217	39.032016	73.272538
501.396965	32.031518	73.277543
500.745834	36.098155	73.282548
499.745118	29.317185	73.287553
498.963192	27.929981	73.292558
498.655362	36.023074	73.297562
498.431951	35.026055	73.302567
496.988880	38.366740	73.307572
496.352698	35.201243	73.312577
495.747326	31.214595	73.317582
494.854813	39.954953	73.322586
494.601350	33.829835	73.327591
493.727049	33.585762	73.332596
492.781512	34.814731	73.337601
492.500288	30.672675	73.342606
491.998348	38.347479	73.347610
491.525011	26.576957	73.352615
490.307959	30.511242	73.357620
489.956302	29.833814	73.362625
489.371348	33.908452	73.367630
488.748156	31.625679	73.372634
488.569332	25.622766	73.377639
487.323221	39.946941	73.382644
486.903643	37.171408	73.387649
485.845991	35.329380	73.392654
484.388595	31.351773	73.397658
484.078859	26.980539	73.402663
483.791475	34.756725	73.407668
483.400030	34.421622	73.412673
482.632190	32.646371	73.417678
482.119626	39.305820	73.422682
481.866210	31.534741	73.427687
480.759501	35.768654	73.432692
480.284889	29.182518	73.437697
479.167740	31.773449	73.442702
478.569121	44.743327	73.447706
478.764673	35.226065	73.452711
477.641464	40.279074	73.457716
476.271084	39.075998	73.462721
475.916610	31.648270	73.467726
474.995548	41.633713	73.472730
474.829738	36.614561	73.477735
474.432599	35.317334	73.482740
473.683321	32.251744	73.487745
473.124463	34.063362	73.492750
472.101446	39.510100	73.497754
471.002081	32.710518	73.502759
470.432623	44.823211	73.507764
469.781344	35.661845	73.512769
469.513475	35.870796	73.517774
469.325941	31.070093	73.522778
468.395805	26.801230	73.527783
467.488387	35.410730	73.532788
466.691564	37.416672	73.537793
466.590303	31.760446	73.542798
465.304620	43.275918	73.547802
465.162064	38.788803	73.552807
464.421701	37.825508	73.557812
463.810910	33.563889	73.562817
462.826463	33.235283	73.567822
462.053468	36.363259	73.572826
462.013013	26.750666	73.577831
460.634647	32.864973	73.582836
459.899918	27.402957	73.587841
459.561826	37.847411	73.592846
459.036482	33.033550	73.597850
458.418260	25.149740	73.602855
457.327935	28.831013	73.607860
456.675564	35.186808	73.612865
456.314896	33.037462	73.617870
455.811931	37.772224	73.622874
454.943672	30.431757	73.627879
453.649758	38.359117	73.632884
453.102120	34.329031	73.637889
453.151367	29.073305	73.642894
452.706068	38.944061	73.647898
451.960276	31.219866	73.652903
451.069607	39.589672	73.657908
450.536020	34.800118	73.662913
449.678532	37.789821	73.667918
448.647414	36.483617	73.672922
448.419196	35.493345	73.677927
447.734590	36.879305	73.682932
447.164907	33.418228	73.687937
446.488069	33.943171	73.692942
445.310778	39.984738	73.697946
444.908864	30.957873	73.702951
444.475819	38.484301	73.707956
443.965037	42.291249	73.712961
442.927223	38.519629	73.717966
442.410362	43.851608	73.722970
442.004673	32.057658	73.727975
440.680777	38.432226	73.732980
440.102203	29.081579	73.737985
439.662597	31.499963	73.742990
439.248517	31.308866	73.747994
438.855474	20.402443	73.752999
437.363243	28.450229	73.758004
436.893786	31.546714	73.763009
436.566824	30.324696	73.768014
435.949915	34.838605	73.773018
435.728295	27.403117	73.778023
434.476494	35.371417	73.783028
434.046176	30.471017	73.788033
432.903133	34.277771	73.793038
432.054100	29.397026	73.798042
431.664171	26.299861	73.803047
430.668670	37.228006	73.808052
430.423103	36.914483	73.813057
430.334416	27.946831	73.818062
429.317754	34.243091	73.823066
428.561104	25.333864	73.828071
427.597119	35.177066	73.833076
427.198180	36.130412	73.838081
426.191568	26.906805	73.843086
425.438788	32.989300	73.848090
424.791607	25.891992	73.853095
424.802293	26.158991	73.858100
424.617577	30.627646	73.863105
423.610552	33.912964	73.868110
422.542743	40.833745	73.873114
422.081526	33.909815	73.878119
421.040926	37.603890	73.883124
420.152329	36.821919	73.888129
420.163866	31.472794	73.893134
419.262413	37.515248	73.898138
418.825603	33.532486	73.903143
417.982423	29.023746	73.908148
417.399642	25.683728	73.913153
417.012371	27.584754	73.918158
415.719465	28.161600	73.923162
415.442444	22.008561	73.928167
414.782152	25.856919	73.933172
413.909184	30.452998	73.938177
414.117496	32.106700	73.943182
412.741729	40.947253	73.948186
412.058091	28.259161	73.953191
411.294319	32.659696	73.958196
410.557576	29.604996	73.963201
409.778237	23.144121	73.968206
409.126377	27.553105	73.973210
409.178806	28.837624	73.978215
408.318477	32.274240	73.983220
407.183678	32.981484	73.988225
406.822567	27.172440	73.993230
406.032963	28.116954	73.998234
405.843910	27.007085	74.003239
404.559267	30.253541	74.008244
403.453702	29.172857	74.013249
403.129190	30.902480	74.018254
402.727329	33.805421	74.023258
402.718489	29.841680	74.028263
401.315241	33.824078	74.033268
400.302747	23.806143	74.038273
400.311636	32.723582	74.043278
399.087937	38.081574	74.048282
398.592059	32.169713	74.053287
398.133292	35.413176	74.058292
397.805661	28.744237	74.063297
397.408995	32.126653	74.068302
395.828536	34.494260	74.073306
395.113706	29.268044	74.078311
394.556450	32.559173	74.083316
394.531182	35.700714	74.088321
393.758510	27.100932	74.093326
392.411062	23.244245	74.098330
392.075813	27.013215	74.103335
391.903465	34.586537	74.108340
391.096901	31.046073	74.113345
390.129619	24.887000	74.118350
388.944306	36.611053	74.123354
389.241821	25.648651	74.128359
388.578680	39.735171	74.133364
387.538428	37.916235	74.138369
386.758936	36.492320	74.143374
386.379160	34.833331	74.148378
385.966505	24.823907	74.153383
384.576369	30.457118	74.158388
383.714745	30.913483	74.163393
383.500033	32.663366	74.168398
383.227092	30.984095	74.173402
382.774511	29.883078	74.178407
381.418831	36.868594	74.183412
381.228322	37.363879	74.188417
380.524208	29.772682	74.193422
379.684692	32.014097	74.198426
378.735987	26.486541	74.203431
378.348876	30.198879	74.208436
377.596833	30.030974	74.213441
377.224179	34.434741	74.218446
376.304893	29.539604	74.223450
375.763234	28.037432	74.228455
375.346962	29.156769	74.233460
374.266231	36.395935	74.238465
373.780107	28.632388	74.243470
373.275375	41.374209	74.248474
372.723021	31.415566	74.253479
371.460459	36.187759	74.258484
370.709858	29.073452	74.263489
369.981392	31.526348	74.268494
369.468178	39.190062	74.273498
369.384260	37.468132	74.278503
368.056089	35.937348	74.283508
367.382212	33.244490	74.288513
367.080407	32.075794	74.293518
366.666664	37.726397	74.298522
366.111196	36.043840	74.303527
364.750504	38.642592	74.308532
364.592602	34.943989	74.313537
364.376315	36.553625	74.318542
363.175543	38.961163	74.323546
362.586663	29.920965	74.328551
361.984441	32.447746	74.333556
361.353253	25.672560	74.338561
360.510195	38.068177	74.343566
359.505787	30.582528	74.348570
359.701390	29.123332	74.353575
358.040079	29.066272	74.358580
357.294305	39.400210	74.363585
356.807765	34.423409	74.368590
356.088770	35.432009	74.373594
356.034681	26.334102	74.378599
355.781251	35.532141	74.383604
354.720240	45.440141	74.388609
354.085245	39.346878	74.393614
353.350379	36.223975	74.398618
352.669265	25.998084	74.403623
351.485214	38.761600	74.408628
350.710487	35.490013	74.413633
350.372260	32.196901	74.418638
349.657456	42.276075	74.423642
349.917566	30.534604	74.428647
348.774191	33.281233	74.433652
347.792684	40.384195	74.438657
347.468418	32.288587	74.443662
346.557617	35.604398	74.448666
345.973005	30.597832	74.453671
345.224578	28.848884	74.458676
344.406722	26.246625	74.463681
344.126739	36.291531	74.468686
343.402453	46.358124	74.473690
342.617991	37.866548	74.478695
341.903887	32.516672	74.483700
341.458302	34.917931	74.488705
341.009439	36.040093	74.493710
339.873885	41.764678	74.498714
339.318173	29.849237	74.503719
338.884307	36.933333	74.508724
337.876429	38.260643	74.513729
337.300076	33.921700	74.518734
336.440287	40.604354	74.523738
336.198648	31.018755	74.528743
335.594249	30.255192	74.533748
334.436094	31.509975	74.538753
334.280058	28.871649	74.543758
333.241415	37.445632	74.548762
332.924587	28.213559	74.553767
331.845829	39.432283	74.558772
331.352035	38.346229	74.563777
330.657612	32.882463	74.568782
330.342349	31.858962	74.573786
330.046536	33.564330	74.578791
328.597505	40.207854	74.583796
328.219565	26.670073	74.588801
327.572130	35.890249	74.593806
326.438700	41.732096	74.598810
326.156872	28.507031	74.603815
325.273612	28.226239	74.608820
324.787541	24.759141	74.613825
324.371886	32.014972	74.618830
323.070321	30.743310	74.623834
322.802685	19.567931	74.628839
322.014987	28.137976	74.633844
321.934610	24.930929	74.638849
321.662880	29.253059	74.643854
320.004327	35.664090	74.648858
319.875471	27.904053	74.653863
318.574584	32.862024	74.658868
317.791147	27.796785	74.663873
317.323127	27.444429	74.668878
316.591827	31.968874	74.673882
316.746035	29.724978	74.678887
316.159839	26.953159	74.683892
314.701797	36.532917	74.688897
314.606757	26.555509	74.693902
313.359615	37.598239	74.698906
312.715107	31.895014	74.703911
311.718906	27.935126	74.708916
311.344673	31.101346	74.713921
310.975999	30.331723	74.718926
310.721817	30.836740	74.723930
310.210998	28.889186	74.728935
309.156579	28.910480	74.733940
308.500268	28.623553	74.738945
307.330536	20.625505	74.743950
306.280849	32.724583	74.748954
305.926298	27.390453	74.753959
305.553817	25.839164	74.758964
305.308218	29.046884	74.763969
304.892108	32.259359	74.768974
303.847559	37.236947	74.773978
303.117269	21.097628	74.778983
302.630320	34.910405	74.783988
301.553251	40.812065	74.788993
301.050322	26.151047	74.793998
300.403174	37.491966	74.799002
300.019721	27.598729	74.804007
298.824563	30.025843	74.809012
298.388031	27.366917	74.814017
297.794141	30.260148	74.819022
297.271833	32.324845	74.824026
296.151769	29.749133	74.829031
295.391446	32.097769	74.834036
294.612659	36.804031	74.839041
294.549446	21.702936	74.844046
293.959600	37.068388	74.849050
293.544286	26.783137	74.854055
292.425611	30.948088	74.859060
291.914501	34.007910	74.864065
291.378971	35.474516	74.869070
290.250628	37.973070	74.874074
289.395835	32.795337	74.879079
289.076256	34.742792	74.884084
288.972149	29.718609	74.889089
288.628622	24.871642	74.894094
287.597418	37.163335	74.899098
286.585203	30.462155	74.904103
284.975810	29.679819	74.909108
284.195869	36.203931	74.914113
284.096078	33.132046	74.919118
283.904466	32.739420	74.924122
283.175163	33.171148	74.929127
282.864774	36.425500	74.934132
282.404103	30.206459	74.939137
281.014367	27.045041	74.944142
280.492367	33.684403	74.949146
280.245872	27.734160	74.954151
279.494624	30.853695	74.959156
278.314644	30.675873	74.964161
278.343605	30.785406	74.969166
277.545161	32.400493	74.974170
277.055792	24.526609	74.979175
275.861411	33.703966	74.984180
275.409994	29.346384	74.989185
274.604201	31.709132	74.994190
273.514837	17.910443	74.999194
273.158378	20.213933	75.004199
272.621561	40.532224	75.009204
272.025775	24.013826	75.014209
271.658684	24.015993	75.019214
270.120751	29.506418	75.024218
270.114116	19.974101	75.029223
269.838175	24.074335	75.034228
268.895586	23.328884	75.039233
267.614943	19.655382	75.044238
267.153650	26.771016	75.049242
266.825455	22.779134	75.054247
266.131669	29.875808	75.059252
265.035124	37.288218	75.064257
264.612665	33.934163	75.069262
263.833457	39.967920	75.074266
263.464198	28.709313	75.079271
263.128473	27.810502	75.084276
262.124560	27.004516	75.089281
261.565202	29.645136	75.094286
260.738576	31.966855	75.099290
260.059760	27.627334	75.104295
259.491715	34.954285	75.109300
258.958087	27.127066	75.114305
258.535146	28.207688	75.119310
257.322404	36.416415	75.124314
256.563252	22.840189	75.129319
255.998566	33.101248	75.134324
255.930819	31.940990	75.139329
255.123296	15.927028	75.144334
254.180222	33.653009	75.149338
253.741628	26.604847	75.154343
252.469883	20.508660	75.159348
251.486292	24.711642	75.164353
251.375349	30.240082	75.169358
250.565904	31.900872	75.174362
250.340877	20.709519	75.179367
249.994100	28.750860	75.184372
248.474272	23.754237	75.189377
247.979147	27.289712	75.194382
247.490729	37.475731	75.199386
247.426695	26.852398	75.204391
246.475310	28.093073	75.209396
245.533888	26.896271	75.214401
245.233665	20.612635	75.219406
243.467375	30.945856	75.224410
243.030673	26.517472	75.229415
242.417724	27.195692	75.234420
241.890141	25.179185	75.239425
241.758916	27.503670	75.244430
241.420599	28.836219	75.249434
240.946075	19.281089	75.254439
239.533942	23.504640	75.259444
238.856541	28.355358	75.264449
238.710282	27.366050	75.269454
237.517922	28.278582	75.274458
236.480169	20.854739	75.279463
236.232354	23.085927	75.284468
235.920206	26.891203	75.289473
235.463870	24.542767	75.294478
234.406510	35.799275	75.299482
233.833335	19.966975	75.304487
233.316956	27.911475	75.309492
231.888133	25.818154	75.314497
231.944863	23.545970	75.319502
230.929578	29.358894	75.324506
230.815045	26.257569	75.329511
229.478242	31.739579	75.334516
228.642252	29.751072	75.339521
228.607295	19.428270	75.344526
228.213815	29.937462	75.349530
227.018453	26.543808	75.354535
226.315777	29.261100	75.359540
225.730828	24.746822	75.364545
225.415670	20.174852	75.369550
223.574908	26.625036	75.374554
223.198594	19.626597	75.379559
222.851287	31.112681	75.384564
222.251580	31.367082	75.389569
222.245480	24.552270	75.394574
221.765971	34.155743	75.399578
220.543089	32.026333	75.404583
219.837127	29.196511	75.409588
219.521802	33.058383	75.414593
218.370407	27.333128	75.419598
217.133454	29.591384	75.424602
216.869674	21.796072	75.429607
216.660958	23.739523	75.434612
216.140088	27.519398	75.439617
215.236739	18.353158	75.444622
214.206914	26.015828	75.449626
213.910961	22.631017	75.454631
213.600744	26.293867	75.459636
212.620200	30.858680	75.464641
211.731670	18.315507	75.469646
211.220878	22.697563	75.474650
210.959257	28.292881	75.479655
209.852888	26.149028	75.484660
208.928695	29.885155	75.489665
208.578982	14.326384	75.494670
208.210771	27.275297	75.499674
207.442959	13.867147	75.504679
206.539833	19.637951	75.509684
205.770459	19.012417	75.514689
205.473012	15.994553	75.519694
204.333403	25.369750	75.524698
203.678013	22.051294	75.529703
203.047698	9.878314	75.534708
202.568500	21.492782	75.539713
202.490514	17.470253	75.544718
200.998019	21.640093	75.549722
200.368482	22.067362	75.554727
199.600332	23.472017	75.559732
199.558546	16.784109	75.564737
199.505168	16.777107	75.569742
198.020437	18.346835	75.574746
197.461894	14.787188	75.579751
196.868850	14.843883	75.584756
195.969031	20.651225	75.589761
195.199524	22.860536	75.594766
194.527443	19.913998	75.599770
194.166532	13.683403	75.604775
193.763200	17.309322	75.609780
192.716394	25.765118	75.614785
192.299419	19.013245	75.619790
191.352981	21.704042	75.624794
190.712373	22.473847	75.629799
189.660726	21.326740	75.634804
189.370287	22.777786	75.639809
189.219645	14.088801	75.644814
188.248072	26.398691	75.649818
187.367638	23.069871	75.654823
186.504527	27.113272	75.659828
186.152293	27.608657	75.664833
185.763623	19.129805	75.669838
184.309282	24.609868	75.674842
184.125306	26.261335	75.679847
183.322490	23.960460	75.684852
182.512538	36.158578	75.689857
182.821859	32.230694	75.694862
181.419710	27.491010	75.699866
180.952614	18.299333	75.704871
180.343318	28.021756	75.709876
179.090840	24.127545	75.714881
178.522187	24.456754	75.719886
177.868270	20.336785	75.724890
177.345513	21.392685	75.729895
177.333952	29.097499	75.734900
176.470025	24.369755	75.739905
175.865081	12.799498	75.744910
174.899385	30.401467	75.749914
174.254312	27.626342	75.754919
173.172095	22.377898	75.759924
172.426421	20.478914	75.764929
172.248772	26.325082	75.769934
171.738630	27.818530	75.774938
171.657379	31.326479	75.779943
170.480438	30.867129	75.784948
169.530842	25.402541	75.789953
169.393749	20.697032	75.794958
168.095903	33.492703	75.799962
167.245333	25.561557	75.804967
166.922191	23.968668	75.809972
166.179211	29.071410	75.814977
166.045258	21.053336	75.819982
164.831498	25.228689	75.824986
164.133858	26.462194	75.829991
163.528829	24.369768	75.834996
163.142498	26.508265	75.840001
162.423167	20.769353	75.845006
161.699648	20.899732	75.850010
161.285499	23.425868	75.855015
160.636742	17.668543	75.860020
159.375906	25.216490	75.865025
158.710109	22.244013	75.870030
158.290893	24.296179	75.875034
158.217250	15.966210	75.880039
157.135901	16.757501	75.885044
156.058522	30.105469	75.890049
155.790804	22.181770	75.895054
154.974107	24.151298	75.900058
154.614436	24.491654	75.905063
153.613046	22.744268	75.910068
152.966749	25.146002	75.915073
152.443487	16.839826	75.920078
152.002438	24.952980	75.925082
151.026132	28.108350	75.930087
150.019744	29.005600	75.935092
149.740765	24.235605	75.940097
149.311580	12.461946	75.945102
148.545931	19.703173	75.950106
147.472302	25.850169	75.955111
147.097170	22.918253	75.960116
146.445758	28.466323	75.965121
146.336529	20.296785	75.970126
145.276099	23.588148	75.975130
144.422817	19.940099	75.980135
143.979319	16.591248	75.985140
143.212163	17.992189	75.990145
142.676718	10.749091	75.995150
141.945403	23.138970	76.000154
141.448789	19.952374	76.005159
140.784095	22.616983	76.010164
139.942303	15.193523	76.015169
139.272110	14.676516	76.020174
138.632861	21.682930	76.025178
137.521647	14.627745	76.030183
136.925143	18.002196	76.035188
136.182243	21.580155	76.040193
135.860324	14.382156	76.045198
135.568808	23.843664	76.050202
135.049945	23.674505	76.055207
133.866039	21.030447	76.060212
132.852593	16.133362	76.065217
132.742059	17.315557	76.070222
131.788595	27.949560	76.075226
131.215815	17.967643	76.080231
130.442964	8.723012	76.085236
130.180642	25.804944	76.090241
130.151683	20.032152	76.095246
129.000660	29.377348	76.100250
128.183141	23.665537	76.105255
126.970469	20.197913	76.110260
126.058966	25.383230	76.115265
125.710494	6.288055	76.120270
124.818959	19.627049	76.125274
124.568619	12.167324	76.130279
124.418718	18.604745	76.135284
123.767191	16.137823	76.140289
122.944617	12.683845	76.145294
122.240734	22.514844	76.150298
121.753159	20.600040	76.155303
120.254006	20.082267	76.160308
119.996399	20.763131	76.165313
119.577816	13.359880	76.170318
119.058453	22.822556	76.175322
117.972182	14.326746	76.180327
117.547618	12.792299	76.185332
116.479720	18.070345	76.190337
116.396747	9.666593	76.195342
115.412546	18.532030	76.200346
114.951968	15.579245	76.205351
114.443545	15.526712	76.210356
113.613566	15.360766	76.215361
112.817275	13.435737	76.220366
112.091938	21.757092	76.225370
111.555624	13.740908	76.230375
110.794707	19.026717	76.235380
109.885520	23.072107	76.240385
108.919360	16.338618	76.245390
108.707168	19.907694	76.250394
108.209322	21.134977	76.255399
107.938920	15.951835	76.260404
107.199303	25.145188	76.265409
106.475072	19.350291	76.270414
105.396417	26.472303	76.275418
104.849008	14.501040	76.280423
104.138368	23.484175	76.285428
102.962297	19.531498	76.290433
103.014094	16.511001	76.295438
102.443070	22.254487	76.300442
101.474918	15.723039	76.305447
100.336341	17.059777	76.310452
99.840165	24.432431	76.315457
99.529715	15.000378	76.320462
98.992955	24.676814	76.325466
98.561726	16.677351	76.330471
97.827940	20.294801	76.335476
97.124326	30.033003	76.340481
96.781866	16.158828	76.345486
95.304486	18.976588	76.350490
94.706057	7.413528	76.355495
94.321548	19.824073	76.360500
93.581604	22.082405	76.365505
93.451632	19.960647	76.370510
92.237455	22.506718	76.375514
91.852607	23.761601	76.380519
91.248734	22.064884	76.385524
90.064974	18.539423	76.390529
89.479329	17.547300	76.395534
88.784049	17.590355	76.400538
88.414904	23.058851	76.405543
88.036421	25.719788	76.410548
86.663410	22.480968	76.415553
85.980692	14.384502	76.420558
85.597264	20.707628	76.425562
85.478246	21.512750	76.430567
84.938334	13.157738	76.435572
83.548888	28.779465	76.440577
83.205061	16.217943	76.445582
82.484285	28.536946	76.450586
81.454849	16.499524	76.455591
80.943509	17.337569	76.460596
80.104916	30.950506	76.465601
80.074175	26.292291	76.470606
79.359518	26.799692	76.475610
78.214268	22.155335	76.480615
77.796185	13.991790	76.485620
77.171124	24.158993	76.490625
77.265024	17.156929	76.495630
75.735157	24.738781	76.500634
74.882741	29.263097	76.505639
74.508053	29.579194	76.510644
74.059683	25.412555	76.515649
72.954486	15.637586	76.520654
72.024663	25.501406	76.525658
71.844178	16.127201	76.530663
71.181824	18.052517	76.535668
70.929521	28.723802	76.540673
70.013240	17.768228	76.545678
69.305501	24.172220	76.550682
68.738975	21.989924	76.555687
67.533184	18.014329	76.560692
66.826559	24.186435	76.565697
66.324461	20.525163	76.570702
65.959108	19.039776	76.575706
65.435856	18.964925	76.580711
64.930344	11.365023	76.585716
63.716476	21.747642	76.590721
63.728630	9.680455	76.595726
62.704541	24.262235	76.600730
61.403356	20.463249	76.605735
61.126428	18.245513	76.610740
60.406875	20.214187	76.615745
60.148680	15.206184	76.620750
59.261288	24.541316	76.625754
58.913086	21.723208	76.630759
58.287215	16.108813	76.635764
57.446930	22.376462	76.640769
56.905223	21.834280	76.645774
55.843613	18.796274	76.650778
55.438992	21.506297	76.655783
54.983329	18.390450	76.660788
53.977504	28.886212	76.665793
53.527235	16.483858	76.670798
52.659904	22.183419	76.675802
52.287666	25.417987	76.680807
51.084208	25.440421	76.685812
50.263405	21.115025	76.690817
49.946254	9.980560	76.695822
49.191849	20.847261	76.700826
49.246488	18.294010	76.705831
47.899277	26.015857	76.710836
46.860637	23.923589	76.715841
46.460415	19.840273	76.720846
46.480654	24.149843	76.725850
46.048758	15.444365	76.730855
45.098140	18.017491	76.735860
44.332869	21.870858	76.740865
43.405231	16.344914	76.745870
42.379913	21.776321	76.750874
41.879382	13.452457	76.755879
41.528782	20.078619	76.760884
40.857699	23.414949	76.765889
40.813942	17.381429	76.770894
39.513348	24.454272	76.775898
38.959318	25.240040	76.780903
37.990399	19.138581	76.785908
37.016517	26.004235	76.790913
36.754834	24.256749	76.795918
36.187032	32.328092	76.800922
35.422166	17.717591	76.805927
35.648507	18.542047	76.810932
34.172937	20.698768	76.815937
33.283287	23.263811	76.820942
32.832382	14.307797	76.825946
32.286789	14.974889	76.830951
31.643051	16.112332	76.835956
30.959612	19.838782	76.840961
30.601321	16.084574	76.845966
29.436015	26.814115	76.850970
28.926249	25.024699	76.855975
28.371233	23.676828	76.860980
27.596853	26.415517	76.865985
26.817467	20.591412	76.870990
25.986211	19.169730	76.875994
25.640969	19.006734	76.880999
25.198848	17.240060	76.886004
24.477286	20.403085	76.891009
23.516629	15.981289	76.896014
22.512118	17.090203	76.901018
22.202743	17.920465	76.906023
21.570124	20.977852	76.911028
21.206556	26.048315	76.916033
20.796405	22.391413	76.921038
19.518334	22.431780	76.926042
19.080799	22.376577	76.931047
18.457716	13.720070	76.936052
17.355821	20.597410	76.941057
16.888189	19.301265	76.946062
16.047954	22.922374	76.951066
16.315498	18.362616	76.956071
15.476433	22.133909	76.961076
14.254164	22.271676	76.966081
13.795968	15.804778	76.971086
12.861548	20.969173	76.976090
12.300279	18.942290	76.981095
11.373760	17.423664	76.986100
10.739709	26.229079	76.991105
10.656910	11.888064	76.996110
10.179136	20.550241	77.001114
9.091738	21.374179	77.006119
8.533834	13.308038	77.011124
7.998376	14.405604	77.016129
7.286461	11.695653	77.021134
6.101361	17.641534	77.026139
5.708465	12.838596	77.031143
5.225728	17.689506	77.036148
4.928091	20.767214	77.041153
4.140302	16.802461	77.046158