Tue Jun 08 16:33:05 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.128291	104.470110	0.000000
-1.528905	92.611820	0.005005
-2.402653	50.787704	0.010010
-4.850944	9.390769	0.015014
-8.831786	-6.901511	0.020019
-13.992071	-4.404708	0.025024
-19.496153	5.735778	0.030029
-23.792761	-0.668958	0.035034
-27.957684	-0.980648	0.040038
-31.451147	2.671454	0.045043
-34.727914	-1.427393	0.050048
-38.806518	-1.119972	0.055053
-42.614517	-4.274362	0.060058
-46.560961	0.230236	0.065062
-49.921528	-8.720593	0.070067
-53.579289	0.796650	0.075072
-57.312352	6.003565	0.080077
-60.999449	-0.806022	0.085082
-64.752703	1.378917	0.090086
-68.719464	-2.160698	0.095091
-72.568637	-5.796257	0.100096
-76.565356	-0.721342	0.105101
-80.269304	-4.360483	0.110106
-83.851194	-3.399697	0.115110
-87.784641	0.439991	0.120115
-91.212450	1.031755	0.125120
-95.265820	3.817617	0.130125
-98.855505	-4.965604	0.135130
-102.803094	3.262523	0.140134
-106.456164	-0.260198	0.145139
-109.837485	-0.227011	0.150144
-113.827539	4.070006	0.155149
-117.268157	-8.981482	0.160154
-121.397295	-6.368118	0.165158
-125.682863	0.295733	0.170163
-129.108860	-1.968107	0.175168
-132.934810	7.601325	0.180173
-136.165591	-6.029646	0.185178
-139.897591	-1.901590	0.190182
-143.796101	-5.911887	0.195187
-147.690834	-13.910957	0.200192
-151.730179	-7.647706	0.205197
-155.773939	-5.085661	0.210202
-159.390356	0.495640	0.215206
-163.221960	6.581578	0.220211
-166.574653	2.958055	0.225216
-170.347295	6.472230	0.230221
-174.062773	2.358733	0.235226
-178.057908	-0.261378	0.240230
-181.500333	-7.622778	0.245235
-185.869518	-9.534172	0.250240
-189.507791	4.603830	0.255245
-192.860358	-6.715712	0.260250
-196.569328	-1.103512	0.265254
-200.452941	2.714302	0.270259
-204.205731	-9.291666	0.275264
-207.872692	-1.516558	0.280269
-211.916758	1.320700	0.285274
-216.136102	-1.730625	0.290278
-219.547377	-5.315243	0.295283
-222.864165	-5.465922	0.300288
-226.852630	3.673194	0.305293
-230.613817	-5.882936	0.310298
-233.901456	-2.954752	0.315302
-238.068856	0.377725	0.320307
-241.730955	-3.201354	0.325312
-245.706119	5.291728	0.330317
-249.228623	-1.487109	0.335322
-252.876897	-0.115755	0.340326
-256.984949	-3.345590	0.345331
-260.689533	-2.232973	0.350336
-264.708567	6.405007	0.355341
-268.299579	-0.940705	0.360346
-271.945210	-0.073042	0.365350
-275.798126	-7.578281	0.370355
-279.179105	-9.601452	0.375360
-283.025262	2.894759	0.380365
-286.586700	-4.636389	0.385370
-290.755309	-4.825239	0.390374
-294.687933	-2.559616	0.395379
-298.612342	-0.478542	0.400384
-302.257844	4.065432	0.405389
-305.548965	-5.379428	0.410394
-309.232089	-1.977202	0.415398
-313.519386	-7.128066	0.420403
-317.136350	-9.604903	0.425408
-320.992994	2.556448	0.430413
-324.648660	-7.061505	0.435418
-328.443316	0.110774	0.440422
-332.628274	-3.068695	0.445427
-335.897149	-2.252976	0.450432
-339.667780	2.709961	0.455437
-343.143829	1.899504	0.460442
-346.750639	1.911947	0.465446
-350.868504	1.418418	0.470451
-354.561624	-0.526286	0.475456
-358.696435	-3.433300	0.480461
-361.989564	-4.639040	0.485466
-365.997468	-0.569259	0.490470
-370.176376	6.052041	0.495475
-373.803543	-9.080477	0.500480
-377.312255	0.500235	0.505485
-381.214846	-3.620847	0.510490
-385.318416	-3.439478	0.515494
-388.875317	-2.101057	0.520499
-392.265815	-4.403540	0.525504
-396.228689	4.594357	0.530509
-399.555494	0.064671	0.535514
-403.447561	-5.184295	0.540518
-407.347853	-0.064468	0.545523
-411.237893	0.817606	0.550528
-414.980931	8.633551	0.555533
-418.647641	-4.076139	0.560538
-422.351859	-2.865565	0.565542
-426.729558	-2.107434	0.570547
-430.128420	-0.131406	0.575552
-434.111895	5.743975	0.580557
-437.536892	-3.133507	0.585562
-440.996003	-4.519116	0.590566
-445.219266	3.628690	0.595571
-448.703163	1.473317	0.600576
-452.748495	-8.209104	0.605581
-456.343944	-2.373041	0.610586
-459.901544	7.424918	0.615590
-463.748464	6.025338	0.620595
-467.161346	6.169990	0.625600
-471.486930	1.139134	0.630605
-475.205271	-8.884342	0.635610
-478.594123	-7.826899	0.640614
-482.663968	-0.293891	0.645619
-486.692342	-6.054617	0.650624
-490.398260	-2.837796	0.655629
-493.827458	-2.314168	0.660634
-497.781801	1.565366	0.665638
-501.688196	-2.382465	0.670643
-505.082841	-10.525016	0.675648
-508.900881	4.848684	0.680653
-512.515993	-5.151025	0.685658
-516.300514	-0.800125	0.690662
-520.319018	-2.753986	0.695667
-523.878409	-8.874591	0.700672
-528.038032	-5.076250	0.705677
-531.524015	-5.256085	0.710682
-535.520846	1.286357	0.715686
-539.560247	5.582333	0.720691
-543.035299	-6.015074	0.725696
-546.371900	8.757406	0.730701
-550.387485	0.940491	0.735706
-554.341033	-2.303333	0.740710
-558.137733	-8.308986	0.745715
-561.368340	-8.433938	0.750720
-565.450094	-3.667290	0.755725
-568.826891	-12.026778	0.760730
-572.743646	-4.421288	0.765734
-576.480030	-3.721344	0.770739
-579.813891	-9.913754	0.775744
-584.353138	-0.754053	0.780749
-588.483486	-0.794858	0.785754
-591.758536	-1.784858	0.790758
-595.726882	1.060663	0.795763
-598.949052	-3.092109	0.800768
-603.158577	14.216197	0.805773
-606.679387	3.291773	0.810778
-610.596712	2.610929	0.815782
-614.595647	4.092085	0.820787
-617.992546	-4.440744	0.825792
-621.763695	6.547304	0.830797
-625.514929	-8.367111	0.835802
-629.152175	6.622388	0.840806
-633.449196	8.988333	0.845811
-636.917322	-4.053620	0.850816
-641.025899	4.708180	0.855821
-644.497444	7.275087	0.860826
-647.970027	7.706813	0.865830
-652.081013	12.894184	0.870835
-655.406103	2.414210	0.875840
-659.589883	4.858238	0.880845
-663.321559	6.179900	0.885850
-666.789966	2.477560	0.890854
-670.897026	9.748717	0.895859
-674.603338	4.222223	0.900864
-678.327438	7.312854	0.905869
-681.980247	-5.505534	0.910874
-685.354756	4.113146	0.915878
-689.538549	11.549055	0.920883
-693.398646	6.388811	0.925888
-697.488783	10.029737	0.930893
-701.073953	3.575838	0.935898
-704.785302	8.621650	0.940902
-708.528402	10.986545	0.945907
-712.109767	2.949625	0.950912
-715.768672	-2.036323	0.955917
-718.965636	6.275432	0.960922
-722.737337	1.872881	0.965926
-727.425448	1.997399	0.970931
-731.099554	2.742439	0.975936
-735.004353	1.887861	0.980941
-738.544166	2.721956	0.985946
-742.298313	1.355646	0.990950
-746.209492	0.073918	0.995955
-749.621671	-4.726204	1.000960
-753.665533	7.909674	1.005965
-756.902550	8.038183	1.010970
-760.550541	14.115980	1.015974
-764.665446	20.280629	1.020979
-768.372785	13.156622	1.025984
-772.451781	8.789489	1.030989
-775.939990	6.776428	1.035994
-780.069511	-5.679014	1.040998
-783.388068	2.050145	1.046003
-787.328067	-3.060769	1.051008
-791.030073	3.186964	1.056013
-795.051267	-0.119229	1.061018
-798.888889	2.598648	1.066022
-802.289195	8.825001	1.071027
-806.418791	0.991995	1.076032
-809.940994	8.010925	1.081037
-813.518274	2.554378	1.086042
-817.123019	-5.054120	1.091046
-821.346449	5.515167	1.096051
-824.736967	2.068781	1.101056
-828.815602	10.416689	1.106061
-832.724950	11.080623	1.111066
-836.290889	-1.899358	1.116070
-839.869427	5.599356	1.121075
-843.500948	0.969977	1.126080
-847.389762	3.485515	1.131085
-851.577182	3.282664	1.136090
-855.202321	-3.311063	1.141094
-858.897956	3.559659	1.146099
-862.568417	-3.422961	1.151104
-866.232657	3.181871	1.156109
-869.908038	-0.864080	1.161114
-874.079871	7.662876	1.166118
-878.016920	7.436019	1.171123
-881.198682	-0.265159	1.176128
-885.052508	-3.944571	1.181133
-888.720308	0.238190	1.186138
-892.216649	4.771624	1.191142
-896.211985	3.887737	1.196147
-900.408428	2.408033	1.201152
-904.001875	4.113110	1.206157
-907.974949	-9.403961	1.211162
-911.607561	-6.586193	1.216166
-915.342736	-3.024162	1.221171
-918.917721	-1.778916	1.226176
-922.883457	4.330657	1.231181
-926.465026	4.678691	1.236186
-929.775259	3.662228	1.241190
-933.724544	2.407343	1.246195
-937.559379	1.074003	1.251200
-941.835031	3.650507	1.256205
-945.761154	-1.749982	1.261210
-948.968320	6.581041	1.266214
-952.817936	2.451400	1.271219
-956.602686	2.172025	1.276224
-960.716286	3.354258	1.281229
-964.157734	1.087425	1.286234
-967.835205	-1.206379	1.291238
-971.611317	2.477191	1.296243
-975.158278	6.025907	1.301248
-979.213004	4.494716	1.306253
-982.747990	-5.402262	1.311258
-986.507499	-6.652969	1.316262
-990.701217	2.707513	1.321267
-994.091494	-0.207107	1.326272
-997.881172	-16.338114	1.331277
-1001.515350	-4.609946	1.336282
-1005.232203	-1.855789	1.341286
-1009.581008	1.813645	1.346291
-1013.396060	-14.073011	1.351296
-1016.954825	-2.371987	1.356301
-1020.837870	-1.367033	1.361306
-1024.521587	-6.858398	1.366310
-1028.448067	-10.274167	1.371315
-1031.654427	-11.491131	1.376320
-1035.658473	1.254964	1.381325
-1039.415927	-6.967319	1.386330
-1043.125318	-5.627453	1.391334
-1046.804888	-1.709759	1.396339
-1050.450076	0.414025	1.401344
-1054.459413	-0.983580	1.406349
-1058.197331	-4.166457	1.411354
-1061.710004	-2.070942	1.416358
-1065.828631	1.877553	1.421363
-1069.144235	-12.093649	1.426368
-1073.216052	-0.357383	1.431373
-1077.072116	-5.484005	1.436378
-1081.204998	6.684696	1.441382
-1085.040943	5.334314	1.446387
-1088.215385	-6.033171	1.451392
-1091.590954	5.515675	1.456397
-1095.499705	-3.880872	1.461402
-1099.261320	-6.544947	1.466406
-1103.889886	0.403270	1.471411
-1107.013846	-0.545178	1.476416
-1111.211948	-0.136516	1.481421
-1114.423838	-6.358894	1.486426
-1117.866255	-4.429332	1.491430
-1122.409644	-0.668748	1.496435
-1125.658819	-1.480822	1.501440
-1129.945145	1.616733	1.506445
-1133.557121	1.012215	1.511450
-1137.068929	-4.924190	1.516454
-1140.795332	-3.296342	1.521459
-1144.250734	-6.863545	1.526464
-1148.353323	4.535467	1.531469
-1152.356850	4.364092	1.536474
-1155.960438	-0.255198	1.541478
-1159.704289	1.498810	1.546483
-1163.542348	-8.417788	1.551488
-1167.442696	-0.926719	1.556493
-1171.139462	2.555910	1.561498
-1174.606106	-1.713884	1.566502
-1178.693976	5.370093	1.571507
-1182.182172	-5.341901	1.576512
-1186.325323	-2.730682	1.581517
-1189.822798	-2.940771	1.586522
-1193.211478	-5.748533	1.591526
-1197.276903	10.874362	1.596531
-1201.028472	-1.824325	1.601536
-1205.105631	4.005046	1.606541
-1208.792979	2.458748	1.611546
-1212.191925	-7.030359	1.616550
-1216.201112	6.002532	1.621555
-1219.908743	-2.493374	1.626560
-1223.866790	4.083652	1.631565
-1227.026558	7.942226	1.636570
-1230.876868	-7.935384	1.641574
-1235.279842	-1.482055	1.646579
-1238.428845	-5.981197	1.651584
-1242.013896	-2.139569	1.656589
-1246.283932	5.390588	1.661594
-1250.132553	-0.926388	1.666598
-1254.135132	0.671627	1.671603
-1257.675792	-5.446014	1.676608
-1261.261351	-5.576184	1.681613
-1265.413368	-3.567657	1.686618
-1268.595847	-8.774649	1.691622
-1273.048426	3.054415	1.696627
-1276.420555	-5.678251	1.701632
-1280.376289	-0.179905	1.706637
-1283.485110	9.982058	1.711642
-1287.245258	-2.196426	1.716646
-1291.558784	3.929388	1.721651
-1295.383028	-4.697980	1.726656
-1298.796003	-7.585159	1.731661
-1302.676740	-4.545650	1.736666
-1306.359426	-6.269093	1.741670
-1310.254077	-2.478041	1.746675
-1313.909449	-3.789757	1.751680
-1317.515259	3.309038	1.756685
-1321.363120	2.874660	1.761690
-1324.901998	-10.346698	1.766694
-1328.848842	-0.337590	1.771699
-1332.815525	-2.598365	1.776704
-1336.713150	0.650900	1.781709
-1339.886002	1.076304	1.786714
-1343.783274	-0.384872	1.791718
-1347.676148	2.410468	1.796723
-1351.457924	-2.281844	1.801728
-1355.605242	-2.581077	1.806733
-1359.540002	-0.858439	1.811738
-1363.283913	-3.229680	1.816742
-1366.995129	1.725471	1.821747
-1370.054108	-2.772058	1.826752
-1374.104873	-8.555676	1.831757
-1377.742226	-7.700748	1.836762
-1381.383672	-2.420495	1.841766
-1385.424641	4.325244	1.846771
-1389.254178	-9.986814	1.851776
-1392.797544	-4.617225	1.856781
-1396.586580	-5.877489	1.861786
-1400.089552	-2.526237	1.866790
-1404.006905	1.099471	1.871795
-1408.184291	-2.267700	1.876800
-1412.063521	-2.241118	1.881805
-1415.713562	-2.395207	1.886810
-1419.292951	-9.671207	1.891814
-1422.896659	-0.888102	1.896819
-1426.269655	-8.578072	1.901824
-1430.057874	0.585258	1.906829
-1434.371525	-2.152214	1.911834
-1437.799948	-5.322780	1.916838
-1442.012330	-1.522025	1.921843
-1445.581106	-3.075059	1.926848
-1449.652882	-11.172681	1.931853
-1453.228588	-6.082859	1.936858
-1456.853272	-6.484009	1.941862
-1460.858311	0.982666	1.946867
-1464.589210	-4.825418	1.951872
-1468.268600	-5.244789	1.956877
-1471.997449	0.357633	1.961882
-1475.473375	-4.352764	1.966886
-1479.392505	-2.508369	1.971891
-1482.835971	-9.285076	1.976896
-1486.714071	-9.478072	1.981901
-1490.548056	-4.164653	1.986906
-1494.560891	-9.250907	1.991910
-1498.465044	-5.318330	1.996915
-1502.403698	-5.829871	2.006912
-1503.003657	-7.399673	2.016909
-1500.698413	-2.946484	2.026906
-1497.825667	-4.416549	2.036902
-1495.703915	-5.934643	2.046899
-1493.678080	-8.256709	2.056896
-1492.184619	-6.771174	2.066893
-1490.418153	-3.207113	2.076890
-1488.042520	3.635276	2.086886
-1486.008363	-1.950658	2.096883
-1484.343383	2.642970	2.106880
-1482.229229	4.347922	2.116877
-1480.662660	2.725634	2.126874
-1478.667805	1.970363	2.136870
-1476.696893	-4.963425	2.146867
-1474.960012	-4.196298	2.156864
-1472.827778	-9.399518	2.166861
-1471.037297	0.600339	2.176858
-1469.360901	1.454531	2.186854
-1467.185319	0.773343	2.196851
-1465.331391	-0.268740	2.206848
-1463.446822	2.405193	2.216845
-1461.720748	4.541998	2.226842
-1459.772029	3.326341	2.236838
-1457.605891	-4.097839	2.246835
-1455.673151	-3.227609	2.256832
-1454.219362	-3.889917	2.266829
-1452.481094	-0.095725	2.276826
-1450.575928	-0.487791	2.286822
-1448.481006	-4.167388	2.296819
-1446.482656	-6.117562	2.306816
-1444.509226	-1.672942	2.316813
-1442.773551	-5.207432	2.326810
-1440.953630	-2.188038	2.336806
-1438.863621	-3.307419	2.346803
-1436.922156	-4.845099	2.356800
-1435.253483	-7.605325	2.366797
-1433.359462	-3.168399	2.376794
-1431.339954	-1.996896	2.386790
-1430.047485	-4.686170	2.396787
-1427.701743	-3.843005	2.406784
-1425.782062	-2.621153	2.416781
-1423.899656	-8.331959	2.426778
-1422.097202	-5.166886	2.436774
-1420.147971	-2.933632	2.446771
-1418.273621	-2.365172	2.456768
-1416.264289	2.778349	2.466765
-1414.552295	2.598116	2.476762
-1412.794727	-0.936963	2.486758
-1410.792481	-0.497176	2.496755
-1408.999704	-4.970597	2.506752
-1407.178190	0.345885	2.516749
-1405.016757	-2.356702	2.526746
-1403.126142	1.757546	2.536742
-1401.745977	-3.380873	2.546739
-1399.047560	0.242878	2.556736
-1397.329760	2.333313	2.566733
-1395.986884	4.274344	2.576730
-1393.960318	4.988979	2.586726
-1391.981041	4.101659	2.596723
-1389.980848	-1.787848	2.606720
-1388.028491	3.283667	2.616717
-1386.270060	0.787453	2.626714
-1384.576663	2.302314	2.636710
-1382.962849	-2.498021	2.646707
-1380.781243	-6.709803	2.656704
-1378.796968	-2.230652	2.666701
-1376.936117	0.489289	2.676698
-1375.154887	-4.951583	2.686694
-1373.162090	-6.615034	2.696691
-1371.085822	-2.385643	2.706688
-1369.524695	2.720281	2.716685
-1367.449091	1.361146	2.726682
-1365.481654	2.092275	2.736678
-1364.076169	3.828120	2.746675
-1361.991613	2.976479	2.756672
-1360.137617	0.512470	2.766669
-1358.278939	-0.126874	2.776666
-1355.829511	1.992039	2.786662
-1354.793225	-1.651112	2.796659
-1352.686188	-8.451334	2.806656
-1350.677713	-9.642823	2.816653
-1348.451421	-8.216319	2.826650
-1346.997023	-4.194291	2.836646
-1345.147422	-0.370167	2.846643
-1342.988318	-7.792297	2.856640
-1341.452363	-6.342459	2.866637
-1339.499449	-3.118220	2.876634
-1337.404683	-0.543960	2.886630
-1335.651174	-3.625402	2.896627
-1333.997837	0.362857	2.906624
-1331.962476	-4.707075	2.916621
-1329.764031	-4.176853	2.926618
-1328.251641	-4.602178	2.936614
-1326.285270	-7.238024	2.946611
-1324.212222	-0.698062	2.956608
-1322.597929	-1.809976	2.966605
-1320.756594	0.048627	2.976602
-1318.638010	-5.476646	2.986598
-1316.656156	-4.729791	2.996595
-1315.123332	-4.500995	3.006592
-1313.358971	-1.117100	3.016589
-1311.305572	-2.009209	3.026586
-1309.452805	1.136211	3.036582
-1307.397918	-2.254266	3.046579
-1305.682338	-0.702080	3.056576
-1303.813452	-5.690053	3.066573
-1301.687714	-7.112305	3.076570
-1299.901137	-1.924931	3.086566
-1298.106640	-5.214955	3.096563
-1296.232381	-3.923983	3.106560
-1294.284504	-0.168486	3.116557
-1292.516995	-1.205136	3.126554
-1290.737879	1.472369	3.136550
-1288.525531	-4.551940	3.146547
-1286.759276	-6.768860	3.156544
-1285.273979	-8.389766	3.166541
-1283.373836	-5.767033	3.176538
-1281.149079	1.945962	3.186534
-1279.144781	0.189680	3.196531
-1277.513146	5.241643	3.206528
-1275.453274	-6.032510	3.216525
-1273.730174	-6.465551	3.226522
-1271.893214	-4.112954	3.236518
-1269.976126	0.701866	3.246515
-1268.149169	0.494439	3.256512
-1265.924913	-6.589878	3.266509
-1264.076748	-1.709866	3.276506
-1262.494263	-5.467751	3.286502
-1260.924020	-7.166471	3.296499
-1258.877083	-1.060668	3.306496
-1256.691177	-5.733549	3.316493
-1254.824385	-7.320767	3.326490
-1253.232507	-4.213509	3.336486
-1251.237986	-5.234986	3.346483
-1249.134061	-12.565788	3.356480
-1247.258818	-4.275816	3.366477
-1245.726576	-3.746535	3.376474
-1243.685904	-10.084379	3.386470
-1241.471592	-4.447972	3.396467
-1239.972528	-6.920530	3.406464
-1237.906742	-0.702552	3.416461
-1236.644328	2.589739	3.426458
-1234.514174	1.225647	3.436454
-1232.314515	-5.997892	3.446451
-1230.202619	-2.796950	3.456448
-1228.638142	-5.127002	3.466445
-1226.783088	-0.186107	3.476442
-1224.969006	-1.420823	3.486438
-1223.046893	2.665578	3.496435
-1221.012230	1.102503	3.506432
-1219.243513	-1.812358	3.516429
-1217.248994	0.349985	3.526426
-1215.772465	1.870940	3.536422
-1213.585078	-2.887936	3.546419
-1212.018715	-9.100840	3.556416
-1209.964473	-3.587103	3.566413
-1207.965407	1.705705	3.576410
-1206.099957	-6.201049	3.586406
-1204.266082	-1.176673	3.596403
-1202.234728	-5.941945	3.606400
-1200.457780	-1.320390	3.616397
-1198.622194	-0.696562	3.626394
-1197.368505	-0.871115	3.636390
-1194.553305	-6.313221	3.646387
-1192.807636	-3.093234	3.656384
-1190.952412	-5.407204	3.666381
-1189.475048	-2.243499	3.676378
-1187.284087	-2.345437	3.686374
-1185.928716	0.492621	3.696371
-1183.668359	-4.289048	3.706368
-1181.461736	-4.491684	3.716365
-1179.942572	-4.165246	3.726362
-1178.195057	-4.454632	3.736358
-1175.972020	1.406377	3.746355
-1174.174528	-0.512738	3.756352
-1172.345980	-1.480384	3.766349
-1170.450689	1.307250	3.776346
-1168.715143	4.057897	3.786342
-1166.642906	2.526730	3.796339
-1164.881723	-0.142182	3.806336
-1162.888130	-5.087096	3.816333
-1161.231457	-4.403284	3.826330
-1159.459467	0.472868	3.836326
-1157.414254	-5.370525	3.846323
-1155.633617	-4.951446	3.856320
-1153.366026	-7.020439	3.866317
-1151.591181	-6.020988	3.876314
-1149.793209	-7.936223	3.886310
-1147.981437	-6.263351	3.896307
-1146.115248	-7.885197	3.906304
-1144.183870	-2.106482	3.916301
-1142.243748	-5.093033	3.926298
-1140.605004	-5.206433	3.936294
-1138.426173	-1.810636	3.946291
-1136.714898	-3.711374	3.956288
-1135.034739	-0.704195	3.966285
-1132.732520	2.719424	3.976282
-1131.024426	-3.804716	3.986278
-1129.196097	-2.744486	3.996275
-1127.385499	-2.436852	4.006272
-1125.517756	-0.966442	4.016269
-1123.741775	1.002275	4.026266
-1121.820890	4.015550	4.036262
-1119.615276	-5.133238	4.046259
-1117.783737	-6.515949	4.056256
-1115.990465	0.847573	4.066253
-1114.204422	-5.913239	4.076250
-1111.952084	3.296130	4.086246
-1110.752959	-1.860920	4.096243
-1108.746424	-2.835783	4.106240
-1106.587079	-4.545496	4.116237
-1104.911127	1.496441	4.126234
-1103.091946	-4.749171	4.136230
-1101.043187	-5.665676	4.146227
-1098.956121	-1.328915	4.156224
-1097.003760	-1.057465	4.166221
-1095.542822	-2.532640	4.176218
-1093.447336	-1.308806	4.186214
-1091.541852	3.334600	4.196211
-1089.374621	-8.702493	4.206208
-1088.023333	-7.013761	4.216205
-1086.478692	-11.529818	4.226202
-1084.369594	-5.958248	4.236198
-1082.188844	-1.139204	4.246195
-1080.474477	-3.642751	4.256192
-1078.278704	-2.750716	4.266189
-1076.746657	-8.072021	4.276186
-1074.906181	-6.047172	4.286182
-1073.053667	-5.697705	4.296179
-1070.964111	-3.631045	4.306176
-1069.070407	-4.898338	4.316173
-1067.035105	-1.304755	4.326170
-1065.183478	-6.150954	4.336166
-1063.467523	-10.151820	4.346163
-1061.703842	-3.773587	4.356160
-1059.737318	-12.515725	4.366157
-1058.157012	-10.251359	4.376154
-1056.139266	-8.147069	4.386150
-1053.852232	-4.493158	4.396147
-1052.490993	-2.168253	4.406144
-1050.539221	-8.102658	4.416141
-1048.483775	-7.331951	4.426138
-1046.679795	-8.663661	4.436134
-1044.606916	-10.384976	4.446131
-1042.499882	-9.441327	4.456128
-1041.079366	-8.706645	4.466125
-1039.133715	-9.928305	4.476122
-1037.230826	-8.331100	4.486118
-1035.430499	-3.302068	4.496115
-1033.610093	-2.589801	4.506112
-1031.669789	-3.206264	4.516109
-1029.835336	0.455020	4.526106
-1027.823812	-4.650211	4.536102
-1025.928746	-1.175991	4.546099
-1024.137494	-4.147999	4.556096
-1022.199487	-4.928865	4.566093
-1020.494844	-8.591450	4.576090
-1018.640317	-8.758845	4.586086
-1016.819510	-1.054192	4.596083
-1014.542582	-14.638364	4.606080
-1012.579959	-1.974068	4.616077
-1010.630448	-0.575346	4.626074
-1009.038070	-0.610387	4.636070
-1007.199422	-7.687271	4.646067
-1005.501430	-9.303498	4.656064
-1003.635187	-8.196765	4.666061
-1001.699748	-10.440248	4.676058
-999.633105	-8.520589	4.686054
-997.944265	-1.874564	4.696051
-996.001537	-5.517154	4.706048
-994.048696	-8.224832	4.716045
-992.262443	-8.499056	4.726042
-990.483639	-1.590246	4.736038
-988.321226	-3.967541	4.746035
-986.487714	-10.543199	4.756032
-984.412519	-0.293184	4.766029
-982.916004	-8.011239	4.776026
-981.298397	-7.687008	4.786022
-979.034625	-5.356965	4.796019
-977.071067	4.316248	4.806016
-975.326811	-3.933214	4.816013
-973.531969	-6.093266	4.826010
-971.497283	-2.607817	4.836006
-969.616381	-3.078497	4.846003
-967.932267	-3.748961	4.856000
-965.834469	-2.572094	4.865997
-964.111451	-4.230543	4.875994
-962.045358	-5.204893	4.885990
-960.449363	-8.724708	4.895987
-958.383185	-4.668443	4.905984
-956.342783	-6.693590	4.915981
-955.201353	1.270397	4.925978
-952.904472	1.073330	4.935974
-950.919499	-1.175474	4.945971
-949.049346	-6.313707	4.955968
-947.008634	-7.677718	4.965965
-945.182387	1.595813	4.975962
-943.634117	-5.085786	4.985958
-941.537802	-0.232012	4.995955
-939.711494	-2.093932	5.005952
-937.520545	0.406721	5.015949
-935.842816	-1.859680	5.025946
-934.164317	-2.402700	5.035942
-932.245407	-0.939801	5.045939
-930.089596	0.223963	5.055936
-928.734983	-3.338981	5.065933
-926.628848	0.292312	5.075930
-924.442516	-0.127236	5.085926
-922.823526	-2.926172	5.095923
-920.823598	-3.092795	5.105920
-919.068498	-2.042430	5.115917
-917.178089	-7.404260	5.125914
-915.325322	-4.389865	5.135910
-913.402820	0.240827	5.145907
-911.295167	-3.537142	5.155904
-909.770222	0.149665	5.165901
-907.759082	-1.806019	5.175898
-905.751154	0.188582	5.185894
-904.181866	-0.538027	5.195891
-901.876651	-3.360694	5.205888
-900.069970	2.911832	5.215885
-898.504390	-0.707870	5.225882
-896.618721	2.745894	5.235878
-894.820719	-7.024052	5.245875
-892.518574	0.098097	5.255872
-890.706337	-6.026893	5.265869
-889.213691	0.102728	5.275866
-887.093893	-1.868832	5.285862
-885.294066	-0.240823	5.295859
-883.219689	-2.702549	5.305856
-881.582363	-6.882322	5.315853
-879.892222	-1.935870	5.325850
-877.771683	-4.211865	5.335846
-875.800139	-7.643567	5.345843
-873.821949	-10.606107	5.355840
-872.555497	-3.067854	5.365837
-870.265456	0.906164	5.375834
-868.297826	-4.097406	5.385830
-866.389925	-2.286778	5.395827
-864.732332	0.644557	5.405824
-862.913713	-5.134130	5.415821
-860.778638	-2.995739	5.425818
-858.903496	2.426419	5.435814
-857.227027	-6.255191	5.445811
-855.015606	-5.713510	5.455808
-853.205677	-5.165356	5.465805
-851.470229	-0.931329	5.475802
-849.813728	0.700747	5.485798
-847.863919	-2.079858	5.495795
-845.795460	-8.543639	5.505792
-843.999165	-3.100829	5.515789
-841.681321	-2.758416	5.525786
-840.301122	-0.995915	5.535782
-838.410320	-3.025368	5.545779
-836.726596	2.451393	5.555776
-834.577801	-3.580772	5.565773
-832.784812	-4.084124	5.575770
-830.689316	-3.466808	5.585766
-828.914042	-2.219495	5.595763
-827.190821	-1.355296	5.605760
-825.420140	3.407417	5.615757
-823.606197	5.057139	5.625754
-821.230801	1.743470	5.635750
-819.458577	0.763111	5.645747
-817.837833	-3.115805	5.655744
-815.804968	3.847893	5.665741
-814.059945	-3.592653	5.675738
-812.005983	-5.276625	5.685734
-810.253548	-2.870579	5.695731
-808.149294	-1.391614	5.705728
-805.976372	-1.377626	5.715725
-804.608459	-0.604193	5.725722
-802.732472	-0.578758	5.735718
-800.683203	-0.032535	5.745715
-799.070379	-6.597520	5.755712
-796.920325	-5.508975	5.765709
-795.377729	-3.696872	5.775706
-793.463768	3.598673	5.785702
-791.519127	2.341726	5.795699
-789.236163	-5.440125	5.805696
-787.569237	-5.909569	5.815693
-785.691792	-2.383994	5.825690
-784.272829	1.874348	5.835686
-782.025205	1.927696	5.845683
-780.119745	-1.226648	5.855680
-778.442627	-2.983460	5.865677
-776.631583	0.663781	5.875674
-774.325634	1.683688	5.885670
-772.750754	1.723271	5.895667
-770.735547	-1.608385	5.905664
-768.959626	0.599601	5.915661
-767.160299	-3.002871	5.925658
-765.278554	0.732624	5.935654
-763.022206	-4.711716	5.945651
-761.434490	1.526134	5.955648
-759.596751	5.782564	5.965645
-757.533331	0.995771	5.975642
-755.890024	2.401717	5.985638
-753.905120	3.249490	5.995635
-751.869222	0.452568	6.005632
-749.952485	-1.099537	6.015629
-748.034182	4.883977	6.025626
-746.597642	2.436535	6.035622
-744.610449	-0.969739	6.045619
-742.903270	-5.035382	6.055616
-740.593361	-1.650007	6.065613
-738.993355	-6.694768	6.075610
-736.946085	0.636417	6.085606
-735.239081	-2.724927	6.095603
-733.016790	1.369086	6.105600
-731.038266	-0.122082	6.115597
-729.460748	0.691282	6.125594
-727.962371	-5.360421	6.135590
-726.017959	-0.313682	6.145587
-723.924039	-1.609656	6.155584
-721.905118	4.038853	6.165581
-720.203806	-4.480597	6.175578
-718.264522	-0.445900	6.185574
-716.091578	1.977733	6.195571
-714.823488	1.563327	6.205568
-712.733950	1.387744	6.215565
-710.501708	2.336551	6.225562
-708.874842	6.424475	6.235558
-707.080516	2.793242	6.245555
-705.023712	3.613285	6.255552
-703.159656	0.181526	6.265549
-701.368104	1.165655	6.275546
-699.572247	1.391426	6.285542
-697.540001	-4.728572	6.295539
-695.745852	-3.763461	6.305536
-693.761146	-4.061740	6.315533
-692.056478	-2.567892	6.325530
-690.199897	0.768841	6.335526
-688.443446	-2.528649	6.345523
-686.300007	-5.151923	6.355520
-684.208202	-1.838166	6.365517
-682.496916	-0.661619	6.375514
-681.054838	2.115495	6.385510
-678.702060	-5.867989	6.395507
-677.039847	-1.000044	6.405504
-674.993901	1.543813	6.415501
-673.262311	2.697119	6.425498
-671.489141	4.300156	6.435494
-669.405811	1.299896	6.445491
-667.433090	-6.493870	6.455488
-665.892328	-2.287213	6.465485
-663.767357	-4.530672	6.475482
-661.679939	-2.422730	6.485478
-660.218671	0.877519	6.495475
-658.149540	-1.430654	6.505472
-656.294972	-1.157635	6.515469
-654.508838	1.479428	6.525466
-652.581416	-0.200147	6.535462
-650.618225	0.376728	6.545459
-648.528370	2.869589	6.555456
-646.925602	1.369430	6.565453
-645.337380	-5.160461	6.575450
-643.127340	-4.887574	6.585446
-641.352399	-5.156551	6.595443
-639.367875	-3.230919	6.605440
-637.589960	-2.525418	6.615437
-635.881268	-3.377819	6.625434
-633.864050	-1.796886	6.635430
-632.000855	2.396744	6.645427
-630.121502	-4.472000	6.655424
-628.080619	-4.530511	6.665421
-626.549676	-3.697260	6.675418
-624.264552	-0.127350	6.685414
-622.333881	0.819503	6.695411
-620.348614	3.880856	6.705408
-618.833836	6.043215	6.715405
-617.122505	3.081519	6.725402
-615.157373	-1.511294	6.735398
-613.256107	-1.439923	6.745395
-611.315014	-1.421625	6.755392
-609.587127	-2.570556	6.765389
-607.464585	-4.178072	6.775386
-605.663749	-4.523407	6.785382
-603.670266	-0.216563	6.795379
-601.933694	-5.156272	6.805376
-600.092017	-5.754039	6.815373
-598.014714	-3.677528	6.825370
-596.482353	-1.381436	6.835366
-594.480450	-2.966664	6.845363
-592.513875	-1.367141	6.855360
-590.606653	-1.952834	6.865357
-588.623151	2.448606	6.875354
-586.952574	2.399511	6.885350
-585.042406	5.101874	6.895347
-583.287258	-1.220702	6.905344
-581.223102	-6.327272	6.915341
-579.428784	-9.756501	6.925338
-577.381549	0.325452	6.935334
-575.900930	4.138559	6.945331
-573.709106	2.171780	6.955328
-572.108439	2.085681	6.965325
-569.791313	-1.190593	6.975322
-567.972912	-2.333697	6.985318
-566.211472	-1.332489	6.995315
-564.047813	-4.121213	7.005312
-562.387150	0.385825	7.015309
-560.679341	4.921135	7.025306
-559.131650	6.839556	7.035302
-557.235436	3.743007	7.045299
-555.122146	-2.601094	7.055296
-552.921325	-6.621346	7.065293
-551.243037	0.374483	7.075290
-549.545695	0.531063	7.085286
-547.331834	0.149268	7.095283
-545.294612	-4.932116	7.105280
-543.836337	-5.101666	7.115277
-541.741059	-0.161739	7.125274
-539.968260	-3.827946	7.135270
-538.087531	-0.353010	7.145267
-536.593318	-0.336256	7.155264
-534.128799	-4.819484	7.165261
-532.673864	-2.649594	7.175258
-530.903985	-0.787861	7.185254
-528.661609	1.297513	7.195251
-526.491032	-3.574359	7.205248
-525.249136	-0.369608	7.215245
-523.196887	-2.925389	7.225242
-521.146168	-4.401187	7.235238
-519.141707	0.768540	7.245235
-517.274727	-1.361821	7.255232
-515.869700	-3.418454	7.265229
-513.997777	-5.326365	7.275226
-511.855191	-1.949303	7.285222
-509.676975	-2.111154	7.295219
-508.009042	0.183843	7.305216
-506.051311	-1.122652	7.315213
-504.703158	6.252336	7.325210
-502.601812	-0.441039	7.335206
-500.411484	-3.775751	7.345203
-498.747151	-1.628337	7.355200
-496.696864	-1.352470	7.365197
-494.845600	3.803243	7.375194
-493.260283	-1.221534	7.385190
-491.294707	4.672585	7.395187
-489.035608	2.333079	7.405184
-487.392108	4.633463	7.415181
-485.639689	-0.135823	7.425178
-483.630542	-3.647325	7.435174
-481.829587	-3.725071	7.445171
-479.849736	-5.215172	7.455168
-478.155788	-0.402777	7.465165
-476.129445	0.801215	7.475162
-474.206215	1.604763	7.485158
-472.552428	2.261675	7.495155
-470.874846	1.034085	7.505152
-468.575081	0.998419	7.515149
-466.726454	2.649064	7.525146
-464.902818	2.626714	7.535142
-463.068697	2.703742	7.545139
-461.172694	9.568995	7.555136
-459.210557	3.381678	7.565133
-457.143231	3.790594	7.575130
-455.543674	-1.522353	7.585126
-453.846807	5.945382	7.595123
-451.771271	4.547165	7.605120
-450.075504	3.209360	7.615117
-448.163774	-2.040553	7.625114
-446.214128	2.631953	7.635110
-444.136048	9.012669	7.645107
-442.270690	1.682409	7.655104
-440.491713	10.371104	7.665101
-438.804405	6.386829	7.675098
-436.861652	9.222390	7.685094
-434.861301	7.166009	7.695091
-433.150804	9.943009	7.705088
-431.121157	6.652096	7.715085
-429.271883	3.486189	7.725082
-427.067331	8.150545	7.735078
-425.415484	3.840775	7.745075
-424.189547	8.754827	7.755072
-421.804683	5.562646	7.765069
-419.756716	-1.655865	7.775066
-418.191474	4.710481	7.785062
-416.068281	3.596563	7.795059
-414.077968	1.487373	7.805056
-412.451110	2.676141	7.815053
-410.488278	0.455080	7.825050
-408.675290	2.498777	7.835046
-406.671616	6.134482	7.845043
-404.629998	5.305679	7.855040
-403.002943	4.740463	7.865037
-401.172328	0.630443	7.875034
-399.390611	-0.548194	7.885030
-397.492914	2.619188	7.895027
-395.490706	4.531627	7.905024
-393.492144	-0.766360	7.915021
-391.553829	-0.937981	7.925018
-389.795335	1.301612	7.935014
-388.125876	-1.040636	7.945011
-386.255805	2.039011	7.955008
-383.963993	-2.369856	7.965005
-382.485089	-2.595851	7.975002
-380.723112	-0.380170	7.984998
-378.550978	0.742343	7.994995
-376.625295	1.455009	8.004992
-374.864153	0.559722	8.014989
-372.977578	2.164375	8.024986
-371.246958	0.640404	8.034982
-369.241168	-1.120077	8.044979
-367.234702	-3.229646	8.054976
-365.490780	0.085459	8.064973
-363.650421	-5.075112	8.074970
-361.581025	1.340728	8.084966
-359.949611	3.747571	8.094963
-358.198446	1.312671	8.104960
-355.863100	10.715761	8.114957
-354.138264	3.534917	8.124954
-352.483958	1.702340	8.134950
-350.488953	-3.172932	8.144947
-348.725091	-3.620900	8.154944
-346.412026	4.296853	8.164941
-344.813858	-0.495723	8.174938
-343.186640	4.685847	8.184934
-341.135676	5.245434	8.194931
-339.317167	5.176590	8.204928
-337.366876	-0.690106	8.214925
-335.471383	1.458428	8.224922
-333.520285	2.739814	8.234918
-331.420820	2.805764	8.244915
-329.881962	-3.882745	8.254912
-327.981237	-3.784285	8.264909
-326.170049	2.666776	8.274906
-324.388372	-2.027641	8.284902
-322.302539	-1.574016	8.294899
-320.188109	4.454718	8.304896
-318.464943	-2.194264	8.314893
-316.509191	-2.871555	8.324890
-315.311942	-2.459163	8.334886
-313.069401	-2.602311	8.344883
-311.048379	-8.498120	8.354880
-309.226355	-1.897151	8.364877
-307.199943	-5.666848	8.374874
-305.185400	-5.150400	8.384870
-303.640701	-2.117267	8.394867
-301.796774	-1.750188	8.404864
-299.725435	-1.905856	8.414861
-297.704173	-2.809767	8.424858
-296.280274	1.608365	8.434854
-294.328904	1.574847	8.444851
-292.221574	0.691745	8.454848
-290.596517	-2.213144	8.464845
-288.662964	3.125762	8.474842
-286.689511	-1.801513	8.484838
-284.430963	4.091861	8.494835
-282.773954	4.958941	8.504832
-280.904075	4.368323	8.514829
-278.960787	-3.274818	8.524826
-277.597722	11.776695	8.534822
-275.677429	9.004153	8.544819
-273.506260	9.187857	8.554816
-271.214923	2.090486	8.564813
-269.673431	0.554331	8.574810
-268.202126	-5.792570	8.584807
-266.120096	4.680784	8.594803
-264.040725	3.248007	8.604800
-262.260821	3.198067	8.614797
-260.466563	3.793816	8.624794
-258.690477	0.003048	8.634791
-256.472664	0.136867	8.644787
-254.764185	9.703263	8.654784
-252.586378	6.949402	8.664781
-251.098702	1.266024	8.674778
-249.261351	10.876320	8.684775
-247.315731	9.839966	8.694771
-245.357362	17.320653	8.704768
-243.405833	10.915099	8.714765
-241.834799	3.670165	8.724762
-239.779652	3.608596	8.734759
-237.712794	7.250541	8.744755
-235.668107	1.705204	8.754752
-234.144118	-3.490379	8.764749
-232.032680	-0.504228	8.774746
-230.542573	5.423355	8.784743
-228.786475	0.761418	8.794739
-226.531322	-3.313456	8.804736
-224.583944	-4.376976	8.814733
-223.024060	-5.008069	8.824730
-221.287397	0.402183	8.834727
-219.187044	4.131663	8.844723
-217.088340	2.409455	8.854720
-215.067518	4.003406	8.864717
-213.456626	2.281078	8.874714
-211.627371	-1.739716	8.884711
-209.927330	3.090326	8.894707
-207.488279	0.726021	8.904704
-206.310465	3.642293	8.914701
-204.310036	-0.741416	8.924698
-202.277773	-2.188219	8.934695
-200.375062	-2.584062	8.944691
-198.601250	-1.008209	8.954688
-196.387021	1.604639	8.964685
-194.623786	-1.825443	8.974682
-192.823042	-2.289952	8.984679
-191.114677	0.444829	8.994675
-189.050782	-4.258815	9.004672
-187.242935	0.267799	9.014669
-185.325496	-7.802843	9.024666
-183.434770	-0.616428	9.034663
-181.480779	-0.074125	9.044659
-179.892592	-2.706677	9.054656
-177.806260	-1.881174	9.064653
-176.290011	-1.908785	9.074650
-174.220200	-2.513096	9.084647
-172.405225	-2.791520	9.094643
-170.267403	-4.400270	9.104640
-168.158918	-3.713724	9.114637
-166.428082	1.796355	9.124634
-164.834501	5.910368	9.134631
-162.723157	3.328008	9.144627
-160.786570	-2.321671	9.154624
-158.915282	0.210103	9.164621
-157.240297	-0.623691	9.174618
-155.457351	0.589388	9.184615
-153.481919	2.386783	9.194611
-151.842821	-1.535379	9.204608
-149.872734	-5.962473	9.214605
-147.796971	-5.824001	9.224602
-145.952117	-2.345499	9.234599
-144.245765	-1.912870	9.244595
-142.209770	0.397802	9.254592
-140.221148	-4.125738	9.264589
-138.255864	-1.710064	9.274586
-136.359413	3.679938	9.284583
-134.630736	4.326111	9.294579
-133.128689	2.745783	9.304576
-130.834926	0.305258	9.314573
-129.081174	3.650791	9.324570
-127.292622	4.497743	9.334567
-125.353776	2.114923	9.344563
-123.467761	1.474967	9.354560
-121.381045	4.059528	9.364557
-119.496928	5.403083	9.374554
-117.825911	8.617371	9.384551
-116.096615	9.253565	9.394547
-114.131711	3.399067	9.404544
-111.982986	4.617811	9.414541
-110.124711	5.623151	9.424538
-108.742215	9.635455	9.434535
-106.803785	9.485278	9.444531
-104.644096	5.108284	9.454528
-102.748629	12.883198	9.464525
-100.776011	9.327132	9.474522
-98.784899	4.007612	9.484519
-97.235034	2.736057	9.494515
-95.226299	3.398641	9.504512
-93.305058	-2.772041	9.514509
-91.779028	-0.156529	9.524506
-89.861118	2.298118	9.534503
-87.877593	0.034515	9.544499
-85.971566	0.730523	9.554496
-83.810909	4.244219	9.564493
-82.031510	2.095455	9.574490
-80.045344	-3.391568	9.584487
-78.565758	-1.547055	9.594483
-76.287133	1.521956	9.604480
-74.967734	-1.753330	9.614477
-72.877668	-2.695815	9.624474
-70.963530	-1.558156	9.634471
-69.167439	7.030168	9.644467
-67.139304	-2.643438	9.654464
-65.101806	-3.116876	9.664461
-63.340287	-0.267061	9.674458
-61.671678	-5.035664	9.684455
-59.443058	-3.263858	9.694451
-57.685837	-3.089694	9.704448
-56.066890	0.298350	9.714445
-54.077501	5.424262	9.724442
-51.964853	4.885775	9.734439
-50.352163	0.882412	9.744435
-48.051019	-4.960551	9.754432
-46.488078	4.091430	9.764429
-44.852800	-2.067350	9.774426
-43.010464	1.813958	9.784423
-41.091630	1.467980	9.794419
-39.088750	1.137233	9.804416
-36.975766	-5.705761	9.814413
-35.080716	-6.702133	9.824410
-33.272466	-2.519356	9.834407
-31.430512	1.492838	9.844403
-29.690157	-1.770039	9.854400
-27.700422	-3.415777	9.864397
-25.820078	-3.088026	9.874394
-24.182844	-4.870137	9.884391
-22.109838	7.869091	9.894387
-20.084333	-2.086232	9.904384
-18.424509	3.261405	9.914381
-16.036431	-4.699781	9.924378
-14.716479	-3.943170	9.934375
-12.736785	-2.907231	9.944371
-10.743126	-0.916871	9.954368
-8.955755	-7.581903	9.964365
-7.099418	-4.481157	9.974362
-5.655269	3.386992	9.984359
-4.152204	41.360038	9.994355
-3.130591	82.473913	10.004352
-1.382042	129.633000	10.014349
0.000000	183.557026	10.019354
0.212961	212.905018	10.024359
0.636754	258.365116	10.029363
1.181244	270.195744	10.034368
1.359378	301.821071	10.039373
1.543064	322.797220	10.044378
2.318086	339.755618	10.049383
2.302617	356.325386	10.054387
2.942562	363.832556	10.059392
2.724036	374.237321	10.064397
2.867931	375.290644	10.069402
3.300693	377.452542	10.074407
3.153490	381.418276	10.079411
3.365448	385.127044	10.084416
3.053840	391.154955	10.089421
3.738054	398.703892	10.094426
3.438664	395.167248	10.099431
3.360003	399.465034	10.104435
3.993636	405.995194	10.109440
3.673287	406.089611	10.114445
3.362264	405.157737	10.119450
3.679594	406.768668	10.124455
3.915045	417.707833	10.129459
3.629528	408.169859	10.134464
4.000187	411.751558	10.139469
3.870813	414.268386	10.144474
4.109653	408.568361	10.149479
3.685850	416.167160	10.154483
3.826277	420.879342	10.159488
4.396904	433.711360	10.164493
4.063412	434.224855	10.169498
4.058265	436.753543	10.174503
3.816748	447.795430	10.179507
4.187450	436.291318	10.184512
4.148517	442.074741	10.189517
4.042512	448.813048	10.194522
4.555106	438.679547	10.199527
4.240674	451.539389	10.204531
4.347028	450.352405	10.209536
4.320497	461.631771	10.214541
4.308243	465.022568	10.219546
4.739932	455.393171	10.224551
4.608248	463.326365	10.229555
4.784028	460.494517	10.234560
4.597708	460.448327	10.239565
4.577350	460.777875	10.244570
4.838427	464.211014	10.249575
4.704842	462.881624	10.254579
4.907576	464.271034	10.259584
4.783895	466.472302	10.264589
4.592028	469.398127	10.269594
4.778218	473.483556	10.274599
4.943854	495.288000	10.279603
4.958858	498.285725	10.284608
5.238254	503.045943	10.289613
5.086454	506.943816	10.294618
5.223647	514.000439	10.299623
5.240065	507.504071	10.304627
4.910520	507.147319	10.309632
5.185863	505.905305	10.314637
5.061382	510.913978	10.319642
5.086192	512.157064	10.324647
5.058908	516.587384	10.329651
5.415115	519.699500	10.334656
5.753480	540.257856	10.339661
5.608367	540.096052	10.344666
5.861294	546.292876	10.349671
5.714364	547.283579	10.354675
6.181552	540.439919	10.359680
5.914120	528.742795	10.364685
5.673652	524.130267	10.369690
5.676050	514.269320	10.374695
5.678762	540.364365	10.379699
5.964773	545.330297	10.384704
6.160781	550.842170	10.389709
6.232157	555.994507	10.394714
6.362390	560.175209	10.399719
6.056861	550.271907	10.404723
6.165782	544.877519	10.409728
6.088578	555.914203	10.414733
6.387921	554.104405	10.419738
6.507645	566.218477	10.424743
5.970819	562.890261	10.429747
6.540438	550.736191	10.434752
6.656425	561.161485	10.439757
6.610557	555.718636	10.444762
6.378785	559.659837	10.449767
6.293738	568.837545	10.454771
6.463333	568.987689	10.459776
6.300103	560.799134	10.464781
6.252330	563.675797	10.469786
6.722044	557.162870	10.474791
6.309896	565.627739	10.479795
6.559175	564.569788	10.484800
6.757855	579.137354	10.489805
7.167881	596.267165	10.494810
7.264659	584.983983	10.499815
6.763790	587.254281	10.504819
7.052963	596.700595	10.509824
6.910527	600.788720	10.514829
7.110487	601.911391	10.519834
7.150422	599.733184	10.524839
7.054500	609.087248	10.529843
7.287215	604.684872	10.534848
7.258676	611.976397	10.539853
7.191681	611.698174	10.544858
7.356605	613.174210	10.549863
7.166177	617.110706	10.554867
7.176912	607.400634	10.559872
7.555283	610.176215	10.564877
7.290038	623.923788	10.569882
7.512395	609.010484	10.574887
7.506683	626.776066	10.579891
7.771569	635.951049	10.584896
7.692300	644.363228	10.589901
7.757679	646.777624	10.594906
7.932848	644.236366	10.599911
7.776107	648.586291	10.604915
8.209973	642.702352	10.609920
8.317106	643.854362	10.614925
7.980551	642.283844	10.619930
8.008316	645.761369	10.624935
8.025145	641.520336	10.629939
8.046350	648.544804	10.634944
8.586928	643.010452	10.639949
8.069839	651.314549	10.644954
8.369615	647.255127	10.649959
8.296248	658.548981	10.654963
8.304382	658.851938	10.659968
8.518534	660.845708	10.664973
8.523631	648.493888	10.669978
8.626275	650.374148	10.674983
8.363542	662.551896	10.679987
8.340331	655.059264	10.684992
8.373974	654.423532	10.689997
8.298780	657.619905	10.695002
8.611382	659.376538	10.700007
8.578376	660.011803	10.705011
8.613001	658.208699	10.710016
8.509887	668.872942	10.715021
8.640427	678.342951	10.720026
8.856213	681.058003	10.725031
8.999171	690.889828	10.730035
9.115263	692.530557	10.735040
9.028350	691.110646	10.740045
8.656093	701.766191	10.745050
9.064065	696.447973	10.750055
8.733187	691.387883	10.755059
9.257873	695.235732	10.760064
9.395417	697.929466	10.765069
9.141284	705.704966	10.770074
9.361851	701.175570	10.775079
9.113752	706.838643	10.780083
9.297506	707.592267	10.785088
9.182017	713.994428	10.790093
9.388377	733.547804	10.795098
9.672677	722.260003	10.800103
9.667283	728.999732	10.805107
10.186807	723.412911	10.810112
10.136827	725.158694	10.815117
9.924534	723.548309	10.820122
9.850649	710.697626	10.825127
9.763125	713.398374	10.830131
9.751303	724.123580	10.835136
10.000563	724.700978	10.840141
9.948766	729.197928	10.845146
10.211056	729.209421	10.850151
9.952982	732.085858	10.855155
9.994617	727.971203	10.860160
10.029334	735.297729	10.865165
9.917300	735.186696	10.870170
9.897594	734.206432	10.875175
9.816889	740.637771	10.880179
10.093368	728.737504	10.885184
10.207267	739.454979	10.890189
10.607885	748.480839	10.895194
10.327146	740.955348	10.900199
10.260123	755.099304	10.905203
10.460761	757.757757	10.910208
10.545587	762.669046	10.915213
10.660670	768.715519	10.920218
10.580349	769.771787	10.925223
10.539762	770.706771	10.930227
10.882969	772.760137	10.935232
10.943380	767.043997	10.940237
10.853713	771.712054	10.945242
10.938126	775.651201	10.950247
10.657064	787.469434	10.955251
10.321311	777.326832	10.960256
10.961327	777.742894	10.965261
10.728639	776.031397	10.970266
11.046521	785.455140	10.975271
11.558338	798.903848	10.980275
11.618321	797.351375	10.985280
11.772715	784.107025	10.990285
11.481843	774.354221	10.995290
11.735304	770.166921	11.000295
11.630844	786.701880	11.005299
11.244886	783.272749	11.010304
10.772256	786.523082	11.015309
11.034429	783.515708	11.020314
11.273940	784.804503	11.025319
11.295730	802.449914	11.030323
11.566203	816.272379	11.035328
11.832403	808.124931	11.040333
11.437433	807.483341	11.045338
11.919009	804.751761	11.050343
11.458564	803.917322	11.055347
11.572419	805.755021	11.060352
11.905245	805.322192	11.065357
11.557527	808.191908	11.070362
12.043627	813.626111	11.075367
12.460882	814.071684	11.080371
12.002226	809.885684	11.085376
12.258395	811.186624	11.090381
12.037630	810.583453	11.095386
12.276856	803.997051	11.100391
12.504798	801.723030	11.105395
12.502611	801.684345	11.110400
12.463461	809.071727	11.115405
12.057610	814.686887	11.120410
12.189739	810.249595	11.125415
12.697441	834.732130	11.130419
12.830831	830.940394	11.135424
13.018619	815.360990	11.140429
12.395715	813.303902	11.145434
12.543736	806.200646	11.150439
12.263252	819.696404	11.155443
12.498262	829.726083	11.160448
13.103277	829.492106	11.165453
12.528681	837.975106	11.170458
13.113525	837.303675	11.175463
13.074354	851.114131	11.180467
13.009094	844.689259	11.185472
13.156677	840.486936	11.190477
13.256635	836.534750	11.195482
13.458608	840.053501	11.200487
13.282530	839.175435	11.205491
13.343487	837.107273	11.210496
13.465902	828.213559	11.215501
13.034061	831.016783	11.220506
13.482941	826.694122	11.225511
13.490714	834.256625	11.230515
13.306713	833.879252	11.235520
13.163568	834.239729	11.240525
13.147790	848.081303	11.245530
13.189884	847.428325	11.250535
13.406078	854.327481	11.255539
13.407729	852.629086	11.260544
13.323765	846.417415	11.265549
13.265086	847.278139	11.270554
13.308749	856.392895	11.275559
13.704541	874.660305	11.280563
13.815862	873.945720	11.285568
13.838752	880.017517	11.290573
13.900255	872.648017	11.295578
14.417017	868.071736	11.300583
14.135862	865.320528	11.305587
14.208972	874.881424	11.310592
14.407732	864.413043	11.315597
14.018899	871.401337	11.320602
14.157755	870.835582	11.325607
14.051202	870.405456	11.330611
14.045873	875.766442	11.335616
14.425043	870.962307	11.340621
14.324832	881.057390	11.345626
14.529834	867.522059	11.350631
14.417276	871.715262	11.355635
14.415796	875.719688	11.360640
14.609756	876.678805	11.365645
14.231485	875.014363	11.370650
14.534945	876.257464	11.375655
14.330338	874.178778	11.380659
14.403739	876.269340	11.385664
15.063859	885.877620	11.390669
15.005630	880.623879	11.395674
15.063880	868.594740	11.400679
14.992708	870.806798	11.405683
15.003371	872.712329	11.410688
14.742746	865.381089	11.415693
15.057208	869.771073	11.420698
15.381052	868.894920	11.425703
14.984569	874.368366	11.430707
15.062872	861.679751	11.435712
15.434498	877.257665	11.440717
15.165231	886.215701	11.445722
15.426724	886.487854	11.450727
15.424614	881.538302	11.455731
15.389391	879.457810	11.460736
15.764860	876.430599	11.465741
15.162187	867.354873	11.470746
15.621317	877.235237	11.475751
15.745288	881.326705	11.480755
15.518727	884.705786	11.485760
15.859395	885.827247	11.490765
15.772844	885.451321	11.495770
15.835088	878.557342	11.500775
15.562847	877.318003	11.505779
15.905895	881.545986	11.510784
15.869539	881.501712	11.515789
15.778029	895.671704	11.520794
16.192272	894.302031	11.525799
16.089211	898.806241	11.530803
15.842908	897.896396	11.535808
16.291213	899.572160	11.540813
16.090818	903.253859	11.545818
16.402726	892.661061	11.550823
16.389423	893.483613	11.555827
16.274017	901.671208	11.560832
16.491526	893.480749	11.565837
15.902981	893.676807	11.570842
16.153524	891.684684	11.575847
16.189946	905.378019	11.580851
16.079946	896.425037	11.585856
16.363423	898.866420	11.590861
15.978350	903.028594	11.595866
16.050409	900.440632	11.600871
16.451148	910.583657	11.605875
16.588459	924.187870	11.610880
16.864771	917.990188	11.615885
16.853168	918.474953	11.620890
16.929680	916.172801	11.625895
16.729905	921.790955	11.630899
17.220751	912.067454	11.635904
17.006401	911.002921	11.640909
16.775151	919.885775	11.645914
17.143252	915.561545	11.650919
16.813958	917.984048	11.655923
16.846117	918.642098	11.660928
17.246962	916.802226	11.665933
17.285968	917.312656	11.670938
17.358105	922.916952	11.675943
17.245396	911.995106	11.680947
17.342771	913.878275	11.685952
17.505744	906.499650	11.690957
17.011725	917.201876	11.695962
17.645648	917.937932	11.700967
17.487482	924.752097	11.705971
17.505984	931.399792	11.710976
17.679932	921.136546	11.715981
17.269037	923.508305	11.720986
17.613641	936.568966	11.725991
17.889999	955.873781	11.730995
17.786235	953.450165	11.736000
18.131376	947.482248	11.741005
17.642377	959.842704	11.746010
18.171151	948.909135	11.751015
17.917383	950.357914	11.756019
17.882311	955.718896	11.761024
18.137941	955.931661	11.766029
17.837707	962.583098	11.771034
18.060667	956.682704	11.776039
18.056311	950.981548	11.781043
17.887929	949.622161	11.786048
18.368019	943.736500	11.791053
17.866181	949.022380	11.796058
18.086679	948.452098	11.801063
18.074622	958.253829	11.806067
18.125882	965.767098	11.811072
18.475212	974.867410	11.816077
18.532682	982.879356	11.821082
18.875746	972.388530	11.826087
19.274644	976.064204	11.831091
18.848346	966.609628	11.836096
18.983156	950.766411	11.841101
18.467910	954.631183	11.846106
18.751278	947.016767	11.851111
18.845550	948.168243	11.856115
18.609780	964.853797	11.861120
19.131923	967.806897	11.866125
18.989321	972.451328	11.871130
19.282744	971.975515	11.876135
19.282084	968.983960	11.881139
19.523613	963.717085	11.886144
19.553621	949.096960	11.891149
19.018213	957.938827	11.896154
19.460299	940.922288	11.901159
19.323351	952.660279	11.906163
19.222768	946.375234	11.911168
19.454352	939.237854	11.916173
19.251294	955.579110	11.921178
19.324498	951.577798	11.926183
19.240576	950.091825	11.931187
19.547733	964.923782	11.936192
19.763380	969.148765	11.941197
19.354517	979.301173	11.946202
19.467561	978.219581	11.951207
19.837402	984.052328	11.956211
19.783184	984.223484	11.961216
20.142305	972.420177	11.966221
19.737294	982.806794	11.971226
19.845397	978.345153	11.976231
19.749091	984.436639	11.981235
19.759513	976.480983	11.986240
19.901737	979.448698	11.991245
19.881271	991.124905	11.996250
20.348078	981.722848	12.001255
20.188274	982.065658	12.006259
20.031911	980.710918	12.011264
20.237715	977.477122	12.016269
20.363909	984.598213	12.021274
20.272059	984.896609	12.026279
19.817772	987.803182	12.031283
20.043014	980.048322	12.036288
20.369527	979.937885	12.041293
20.066487	989.555055	12.046298
20.427296	998.528677	12.051303
20.221702	997.935134	12.056307
20.427596	1011.504374	12.061312
20.581580	991.861271	12.066317
20.462427	988.142402	12.071322
20.486245	979.705241	12.076327
20.222651	986.128960	12.081331
20.051096	987.016544	12.086336
20.412203	982.434155	12.091341
19.972792	984.213974	12.096346
20.028435	982.530386	12.101351
20.229748	982.585493	12.106355
20.541608	1005.955569	12.111360
20.320848	987.750399	12.116365
20.152042	982.555845	12.121370
20.295419	981.540104	12.126375
20.349914	976.482134	12.131379
20.285715	986.982818	12.136384
20.562374	978.030994	12.141389
20.014171	989.633868	12.146394
19.970060	984.399382	12.151399
20.184088	996.192491	12.156403
20.718418	1012.649349	12.161408
20.981178	996.312045	12.166413
20.279003	995.100227	12.171418
20.341707	986.554948	12.176423
20.560124	986.584623	12.181427
20.563584	990.135076	12.186432
20.427734	985.505261	12.191437
20.450502	982.175348	12.196442
20.109636	982.626175	12.201447
20.402842	981.202643	12.206451
20.383578	983.706209	12.211456
20.368969	979.477579	12.216461
20.181812	983.230843	12.221466
20.381956	987.614804	12.226471
20.404734	985.227118	12.231475
20.677304	987.266178	12.236480
20.788093	980.972510	12.241485
20.288560	977.640570	12.246490
20.528630	972.029734	12.251495
20.272895	961.431584	12.256499
20.262313	966.761924	12.261504
20.387201	963.396743	12.266509
20.271442	963.484898	12.271514
20.278640	960.733574	12.276519
19.861737	954.299868	12.281523
20.138805	965.821622	12.286528
20.622735	971.067177	12.291533
20.264435	973.321373	12.296538
20.380560	965.335757	12.301543
20.792926	969.384513	12.306547
20.176272	967.721064	12.311552
20.213743	963.207986	12.316557
20.025323	973.988905	12.321562
20.171843	965.654660	12.326567
20.205360	964.894201	12.331571
20.073504	971.793085	12.336576
20.405366	983.393878	12.341581
20.451052	999.673583	12.346586
20.545820	977.703428	12.351591
20.408631	969.989399	12.356595
20.243387	972.181679	12.361600
20.434058	965.669849	12.366605
20.260393	976.146663	12.371610
20.536808	970.121837	12.376615
20.525366	971.960118	12.381619
20.095318	970.420989	12.386624
20.431275	960.156387	12.391629
20.253326	964.660035	12.396634
20.366342	968.416697	12.401639
20.352503	963.340448	12.406643
20.273238	965.983771	12.411648
20.429033	960.216469	12.416653
20.110892	963.631005	12.421658
20.175624	966.073983	12.426663
20.490550	966.260793	12.431667
20.386788	970.223964	12.436672
20.675145	969.437575	12.441677
20.444739	967.124880	12.446682
20.451556	967.188467	12.451687
20.590620	973.346565	12.456691
20.338835	972.424235	12.461696
20.467568	960.038733	12.466701
20.507192	974.315391	12.471706
20.613409	971.434589	12.476711
20.586123	950.296577	12.481715
20.153667	956.559369	12.486720
20.047261	941.836720	12.491725
20.034517	947.565709	12.496730
20.035413	949.569239	12.501735
20.452879	958.353915	12.506739
20.295094	973.855724	12.511744
20.659807	965.407095	12.516749
20.071919	951.802375	12.521754
19.924781	947.018193	12.526759
20.511978	969.666803	12.531763
20.269962	981.110201	12.536768
20.493934	973.042144	12.541773
20.138547	957.141258	12.546778
20.317884	951.500185	12.551783
20.269266	958.208741	12.556787
20.421883	957.575887	12.561792
20.435939	940.918128	12.566797
20.501962	947.477551	12.571802
20.321210	945.362003	12.576807
20.395133	939.312696	12.581811
20.221237	942.470394	12.586816
20.242968	948.061631	12.591821
20.505762	952.766021	12.596826
20.227841	945.100212	12.601831
20.342597	951.972199	12.606835
20.325099	960.749744	12.611840
20.307932	949.848595	12.616845
20.094532	952.773464	12.621850
20.348233	953.676554	12.626855
20.274856	955.389270	12.631859
20.077868	951.664808	12.636864
20.354664	946.980834	12.641869
20.165903	953.482892	12.646874
20.288000	948.594127	12.651879
20.135026	953.609801	12.656883
19.991756	953.832540	12.661888
20.409828	961.378441	12.666893
20.274647	972.036942	12.671898
20.437657	970.679943	12.676903
20.181390	970.156273	12.681907
20.222057	966.872636	12.686912
20.732106	960.669598	12.691917
20.360626	964.036438	12.696922
20.507485	957.106996	12.701927
20.209255	962.314154	12.706931
20.210647	967.400075	12.711936
20.381902	955.786490	12.716941
20.090285	962.480659	12.721946
19.988594	957.553683	12.726951
20.196259	955.655350	12.731955
20.229949	959.427980	12.736960
20.486698	972.013081	12.741965
20.537170	961.544007	12.746970
20.467069	963.088400	12.751975
20.867968	962.777316	12.756979
20.379698	966.352468	12.761984
20.349824	960.640684	12.766989
20.125166	965.280629	12.771994
20.057522	967.576963	12.776999
20.288460	958.222862	12.782003
20.555764	968.240384	12.787008
20.415227	960.804825	12.792013
20.127923	960.642921	12.797018
20.520953	962.026198	12.802023
20.445646	956.117339	12.807027
20.471192	961.681480	12.812032
20.405143	964.437010	12.817037
19.899869	961.815789	12.822042
20.407856	953.941807	12.827047
20.326132	956.156080	12.832051
20.037694	959.630259	12.837056
20.215088	961.408136	12.842061
20.199109	961.812733	12.847066
20.285436	964.135956	12.852071
20.391675	957.385582	12.857075
20.296809	960.655257	12.862080
20.045198	962.026694	12.867085
19.978977	962.486878	12.872090
20.139933	959.126566	12.877095
20.003815	969.287862	12.882099
19.998475	960.922025	12.887104
20.393143	964.616975	12.892109
20.102522	966.604569	12.897114
20.608859	981.686600	12.902119
20.513718	964.599120	12.907123
20.022035	972.706795	12.912128
20.675095	963.322947	12.917133
20.600362	964.532610	12.922138
20.293881	973.291815	12.927143
20.279648	967.213797	12.932147
20.706956	972.593402	12.937152
20.467043	966.787761	12.942157
20.345860	969.979846	12.947162
20.863021	965.786360	12.952167
20.583417	961.948562	12.957171
20.335630	969.350082	12.962176
20.650969	965.077122	12.967181
19.983966	950.209004	12.972186
20.107310	965.164846	12.977191
20.353663	973.365452	12.982195
20.061218	966.290671	12.987200
20.129827	963.180268	12.992205
19.774890	966.413615	12.997210
20.304975	964.051057	13.002215
20.659838	967.330072	13.007219
20.381311	970.170586	13.012224
20.507149	964.088290	13.017229
20.802664	971.633499	13.022234
20.566258	961.151244	13.027239
20.331165	947.404329	13.032243
20.372884	955.630933	13.037248
20.400482	944.981452	13.042253
20.489662	944.582105	13.047258
20.395610	943.422340	13.052263
20.837328	944.547401	13.057267
20.376518	950.303873	13.062272
20.355016	939.898470	13.067277
20.174954	942.169865	13.072282
20.114779	950.088281	13.077287
20.054511	943.445803	13.082291
19.635324	952.618264	13.087296
20.174209	934.683959	13.092301
20.326439	940.390581	13.097306
20.341408	954.309872	13.102311
20.568219	950.571169	13.107315
20.502002	953.900668	13.112320
20.291341	950.756045	13.117325
20.183937	950.331194	13.122330
20.343279	953.572282	13.127335
20.418724	955.125272	13.132339
19.882495	952.102785	13.137344
20.147256	951.269522	13.142349
19.743750	954.260933	13.147354
19.844656	958.787425	13.152359
20.404388	956.888728	13.157363
20.167665	972.458938	13.162368
20.536267	969.623543	13.167373
20.539318	975.711411	13.172378
20.216526	980.419106	13.177383
20.176526	968.316342	13.182387
19.977437	978.323047	13.187392
20.534693	969.949956	13.192397
20.309900	976.072546	13.197402
20.392775	984.267635	13.202407
20.507428	976.913841	13.207411
20.394778	973.569648	13.212416
20.477143	958.884484	13.217421
20.492607	958.310672	13.222426
20.198230	957.039991	13.227431
20.660051	951.357195	13.232435
20.360856	956.107811	13.237440
20.477033	950.601119	13.242445
20.551364	958.316480	13.247450
20.198837	963.650184	13.252455
20.484361	949.576375	13.257459
19.930144	958.147128	13.262464
20.491477	955.421979	13.267469
20.254912	960.525013	13.272474
20.439426	960.784314	13.277479
20.521240	954.286021	13.282483
20.594798	961.255471	13.287488
20.904819	947.779826	13.292493
20.794739	958.439935	13.297498
20.373731	937.769311	13.302503
20.744666	923.728249	13.307507
20.208143	927.861528	13.312512
20.197390	923.543438	13.317517
20.436809	927.547625	13.322522
20.071736	928.559964	13.327527
20.266290	923.834835	13.332531
20.090160	929.737487	13.337536
20.277569	917.939189	13.342541
20.151804	932.868632	13.347546
20.191828	927.043035	13.352551
20.048473	928.032754	13.357555
20.067734	946.315860	13.362560
20.111056	954.671267	13.367565
20.014024	963.139952	13.372570
20.121520	959.918673	13.377575
20.308620	960.734499	13.382579
20.145411	958.885149	13.387584
20.594840	962.070187	13.392589
20.764859	966.713120	13.397594
20.690818	963.040602	13.402599
20.355699	943.915624	13.407603
20.136759	939.891380	13.412608
20.181719	932.661659	13.417613
20.066697	942.818926	13.422618
20.306205	952.440944	13.427623
20.391250	947.439324	13.432627
20.197177	959.754346	13.437632
20.395704	955.401154	13.442637
20.545251	960.379171	13.447642
19.835138	953.939686	13.452647
19.911459	953.845303	13.457651
20.252225	966.658361	13.462656
20.265350	953.966241	13.467661
20.564002	968.583347	13.472666
20.252604	962.419704	13.477671
20.588323	961.146383	13.482675
20.417331	965.655154	13.487680
20.846717	957.659252	13.492685
20.399612	950.640995	13.497690
20.292129	940.425989	13.502695
20.377251	934.348318	13.507699
20.406506	944.840845	13.512704
20.216867	934.137040	13.517709
20.064054	937.310858	13.522714
19.915573	934.241630	13.527719
20.152790	933.272170	13.532723
20.435446	955.506006	13.537728
20.097710	944.502326	13.542733
20.140592	948.090615	13.547738
20.181771	962.887648	13.552743
20.513511	970.200463	13.557747
20.222780	973.952931	13.562752
20.790735	961.514621	13.567757
20.393716	952.439109	13.572762
20.140688	953.720788	13.577767
20.559060	933.006516	13.582771
20.081391	942.254918	13.587776
20.065086	935.800298	13.592781
20.221338	941.805044	13.597786
20.164458	948.247383	13.602791
20.554276	951.301720	13.607795
20.200716	951.168149	13.612800
20.143727	939.877523	13.617805
20.489094	959.461824	13.622810
20.188234	951.075609	13.627815
20.792002	947.339775	13.632819
20.086634	948.091910	13.637824
20.273879	938.460315	13.642829
20.216315	936.989165	13.647834
19.946064	948.065936	13.652839
20.508875	956.205960	13.657843
20.237785	952.892094	13.662848
20.231439	943.493028	13.667853
20.454357	950.766071	13.672858
20.163474	949.316372	13.677863
20.259869	944.057019	13.682867
19.928952	954.363809	13.687872
20.257102	963.598008	13.692877
20.441163	974.451246	13.697882
20.640330	977.759328	13.702887
20.408437	961.718843	13.707891
20.067085	956.194280	13.712896
20.171410	958.416917	13.717901
20.608664	961.510491	13.722906
20.789608	959.509372	13.727911
20.537001	943.851401	13.732915
20.317660	954.817212	13.737920
20.084420	945.612966	13.742925
20.201248	949.346865	13.747930
20.126520	947.034718	13.752935
20.127456	948.976268	13.757939
20.379340	951.352813	13.762944
20.456062	945.858414	13.767949
20.555649	951.104729	13.772954
20.432595	947.862587	13.777959
20.540707	943.707662	13.782963
19.967869	945.333908	13.787968
20.548340	949.089759	13.792973
20.404542	946.914585	13.797978
20.288645	948.809852	13.802983
20.488566	937.870306	13.807987
20.467774	945.885388	13.812992
20.426611	950.566104	13.817997
20.627207	948.833193	13.823002
20.268227	947.324117	13.828007
20.579855	947.393468	13.833011
20.438981	949.738670	13.838016
20.315825	951.444525	13.843021
20.233075	936.037700	13.848026
20.370002	939.041447	13.853031
20.322217	924.672707	13.858035
20.170671	934.555970	13.863040
20.415936	927.466381	13.868045
20.326874	923.541055	13.873050
20.241982	921.925779	13.878055
20.441523	914.118517	13.883059
20.111916	919.244989	13.888064
19.901051	923.123092	13.893069
20.281691	939.123071	13.898074
20.493013	947.984532	13.903079
20.604807	936.652732	13.908083
20.320265	936.140622	13.913088
20.540077	917.756574	13.918093
20.445223	909.821371	13.923098
20.414497	917.866563	13.928103
20.884054	917.083845	13.933107
20.432482	920.028623	13.938112
19.947675	914.522750	13.943117
19.939196	906.118797	13.948122
19.799473	914.391488	13.953127
20.260069	919.830892	13.958131
20.146976	923.871045	13.963136
20.566770	923.056202	13.968141
20.419509	921.013466	13.973146
20.099001	919.704242	13.978151
19.941713	915.276675	13.983155
19.822991	916.977424	13.988160
20.007859	943.228226	13.993165
20.180616	946.597670	13.998170
20.350928	942.486159	14.003175
20.615963	942.838232	14.008179
20.339347	955.247929	14.013184
20.804008	951.974492	14.018189
20.593790	947.989973	14.023207
19.803574	932.741033	14.028224
20.151115	932.663746	14.033242
20.420003	949.105328	14.038259
20.669120	943.220527	14.043277
20.533614	949.765851	14.048295
20.124071	936.359242	14.053312
20.566395	941.232556	14.058330
20.353739	940.658366	14.063347
20.393870	944.733655	14.068365
20.359814	951.547430	14.073383
20.143001	948.665143	14.078400
20.527926	950.287462	14.083418
20.192544	952.990430	14.088435
20.272524	955.347754	14.093453
20.187629	952.795627	14.098471
20.434274	957.350505	14.103488
20.485046	948.490854	14.108506
20.740279	955.974762	14.113523
20.800336	955.044739	14.118541
20.793995	962.266392	14.123559
20.339553	962.053757	14.128576
20.610828	951.924721	14.133594
20.500218	951.353902	14.138611
20.354472	959.706614	14.143629
20.731236	956.797362	14.148647
20.247794	982.034281	14.153664
20.901955	984.741619	14.158682
20.711572	997.922405	14.163699
20.812589	995.822286	14.168717
20.959873	986.743296	14.173735
20.736145	998.163540	14.178752
20.744417	994.082732	14.183770
21.141627	993.988660	14.188787
20.976272	994.751725	14.193805
21.216896	992.171734	14.198823
20.818102	989.573808	14.203840
20.959449	984.389405	14.208858
20.904401	989.854344	14.213875
20.645226	985.163837	14.218893
20.888220	988.875987	14.223911
20.777746	998.936960	14.228928
21.161856	986.174600	14.233946
20.925580	991.420989	14.238963
20.942476	994.039940	14.243981
20.844806	991.714422	14.248999
20.736520	996.867210	14.254016
20.687411	995.883455	14.259034
20.760147	998.377077	14.264051
20.811732	1010.602940	14.269069
21.429643	1008.304739	14.274087
21.158371	1015.885248	14.279104
21.215099	1011.391375	14.284122
21.786612	1017.228063	14.289139
21.491839	1018.971652	14.294157
21.637226	1008.305464	14.299175
21.259948	1000.522786	14.304192
21.093343	994.252520	14.309210
21.150574	988.358867	14.314227
21.121435	1013.864031	14.319245
21.351840	1012.421694	14.324263
21.253090	1012.052790	14.329280
21.506736	1015.884782	14.334298
21.282389	1011.344213	14.339315
21.310269	1017.723353	14.344333
21.426830	1016.302503	14.349351
21.198945	1022.861727	14.354368
21.336648	1020.648615	14.359386
21.912862	1020.319902	14.364403
21.597586	1025.392432	14.369421
21.496843	1008.594396	14.374439
21.471345	1017.106061	14.379456
21.632763	1013.391537	14.384474
21.578632	1012.366120	14.389491
21.531585	1030.253784	14.394509
21.796325	1016.640939	14.399527
21.564309	1028.821340	14.404544
21.555469	1020.700659	14.409562
21.462572	1018.475506	14.414579
21.714294	1023.630361	14.419597
21.802501	1015.117428	14.424615
21.583615	1018.880428	14.429632
21.541967	1019.662050	14.434650
21.522512	1022.205737	14.439667
21.586581	1026.035980	14.444685
22.125990	1035.885938	14.449703
21.960442	1045.865827	14.454720
21.820550	1028.449634	14.459738
21.921272	1021.058645	14.464755
21.593221	1035.604892	14.469773
21.919358	1036.401414	14.474791
22.050168	1060.255101	14.479808
22.026701	1051.980207	14.484826
22.075340	1046.990826	14.489843
21.852035	1064.463442	14.494861
22.160381	1053.961029	14.499879
22.023088	1056.835970	14.504896
22.239477	1057.185136	14.509914
22.291308	1057.561335	14.514931
22.205273	1054.822759	14.519949
22.380103	1055.653887	14.524967
21.987619	1044.448354	14.529984
22.038367	1035.944194	14.535002
22.248190	1044.011561	14.540019
21.904476	1053.276674	14.545037
22.380225	1048.639288	14.550055
22.235203	1054.616562	14.555072
22.465189	1048.073932	14.560090
22.240416	1051.508792	14.565107
22.129238	1053.391784	14.570125
22.414806	1049.027968	14.575143
22.238710	1040.877288	14.580160
22.250986	1046.671279	14.585178
22.474642	1051.949862	14.590195
22.585168	1054.891770	14.595213
22.364187	1040.466845	14.600231
22.485429	1049.169131	14.605248
22.306008	1042.549837	14.610266
22.580999	1046.242341	14.615283
22.220341	1047.386162	14.620301
23.018796	1036.788310	14.625319
22.530896	1045.498178	14.630336
22.500114	1047.350848	14.635354
22.740659	1049.675146	14.640371
22.652291	1055.891149	14.645389
22.580696	1042.111917	14.650407
22.673570	1050.119806	14.655424
22.663103	1047.333627	14.660442
22.903601	1046.541570	14.665459
22.502362	1053.700255	14.670477
22.643292	1053.612326	14.675495
22.236178	1056.602827	14.680512
22.781684	1054.985191	14.685530
22.866447	1047.866237	14.690547
22.508434	1051.695621	14.695565
22.564607	1054.420061	14.700583
22.629674	1047.175340	14.705600
22.524072	1051.766229	14.710618
23.250590	1049.424203	14.715635
23.063940	1051.206741	14.720653
22.901972	1046.515693	14.725671
23.351809	1048.305252	14.730688
22.802454	1048.108888	14.735706
23.221477	1048.446935	14.740723
23.184683	1058.770923	14.745741
23.033011	1048.999794	14.750759
22.800668	1048.601823	14.755776
22.739015	1048.771085	14.760794
23.211980	1047.397400	14.765811
22.939446	1053.379999	14.770829
22.901386	1056.057599	14.775847
22.858497	1058.081651	14.780864
22.987017	1073.928096	14.785882
23.481759	1066.979014	14.790899
23.313229	1074.780142	14.795917
23.560900	1068.861288	14.800935
23.253818	1059.920005	14.805952
23.138103	1068.036507	14.810970
23.393897	1061.605990	14.815987
23.259480	1077.018746	14.821005
23.436339	1076.372254	14.826023
23.642905	1074.392227	14.831040
23.206773	1062.364971	14.836058
23.512957	1059.605607	14.841075
23.052653	1069.858111	14.846093
23.500851	1072.538569	14.851111
23.311343	1079.606235	14.856128
23.261161	1075.146423	14.861146
23.876422	1078.150626	14.866163
23.994711	1075.070693	14.871181
24.059664	1067.679515	14.876199
23.924046	1051.118138	14.881216
23.643888	1056.216550	14.886234
23.798159	1044.524331	14.891251
23.713734	1047.953239	14.896269
23.638847	1041.711326	14.901287
23.739435	1043.770622	14.906304
23.464005	1055.413960	14.911322
23.926484	1043.471641	14.916339
23.282703	1048.619795	14.921357
23.532827	1040.577547	14.926375
23.483309	1038.299281	14.931392
23.518195	1047.771937	14.936410
23.616225	1056.895954	14.941427
23.733044	1072.938513	14.946445
23.787368	1071.132237	14.951463
23.859487	1075.519421	14.956480
23.756463	1073.652322	14.961498
24.220108	1074.928456	14.966515
23.833293	1084.456507	14.971533
23.941128	1069.159370	14.976551
23.967515	1078.757921	14.981568
23.656427	1087.043373	14.986586
23.963230	1081.116345	14.991603
23.901719	1082.024613	14.996621
23.811861	1072.962608	15.001639
23.731483	1073.126418	15.006656
23.677840	1082.837519	15.011674
24.309819	1074.861288	15.016691
24.140479	1079.743055	15.021709
23.958517	1081.753549	15.026727
24.026670	1084.817698	15.031744
24.278634	1101.087526	15.036762
24.640761	1106.342386	15.041779
24.489423	1097.019235	15.046797
24.510091	1078.939977	15.051815
24.413493	1078.175399	15.056832
24.448843	1077.381504	15.061850
24.491926	1069.015658	15.066867
24.377947	1075.459304	15.071885
24.313243	1079.291954	15.076903
24.595183	1070.868223	15.081920
24.173859	1073.702096	15.086938
24.394242	1074.060421	15.091955
24.292393	1078.382938	15.096973
24.245230	1081.782628	15.101991
24.586368	1094.927092	15.107008
24.512720	1107.848962	15.112026
24.559614	1109.012287	15.117043
24.911101	1110.939985	15.122061
24.987935	1097.345114	15.127079
24.438551	1083.475704	15.132096
24.457658	1080.832490	15.137114
24.785306	1081.579934	15.142131
24.960796	1085.243047	15.147149
24.823421	1082.181354	15.152167
24.684229	1076.772560	15.157184
24.435677	1078.294829	15.162202
24.935866	1078.081519	15.167219
24.790496	1078.526178	15.172237
24.585890	1071.167828	15.177255
24.948915	1090.364880	15.182272
24.812909	1103.400988	15.187290
24.756822	1100.554112	15.192307
24.536476	1101.422286	15.197325
24.984322	1108.149569	15.202343
25.114804	1101.898012	15.207360
25.041343	1106.883830	15.212378
25.045885	1099.210454	15.217395
25.182230	1102.247952	15.222413
25.086040	1103.415729	15.227431
25.155040	1102.008932	15.232448
24.982399	1105.197053	15.237466
25.212362	1096.143590	15.242483
25.124989	1105.312416	15.247501
24.887320	1104.690143	15.252519
25.299158	1104.764836	15.257536
25.073447	1111.210724	15.262554
25.162278	1110.362379	15.267571
25.251042	1114.079347	15.272589
24.986436	1107.406122	15.277607
24.955067	1104.090406	15.282624
24.943563	1105.425173	15.287642
25.096943	1105.287862	15.292659
24.914197	1107.527251	15.297677
25.580950	1125.615499	15.302695
25.725594	1124.368579	15.307712
25.719762	1126.035865	15.312730
25.649508	1112.135465	15.317747
25.752242	1112.221421	15.322765
25.089537	1111.599181	15.327783
25.691486	1102.902833	15.332800
25.197010	1104.030623	15.337818
25.170391	1107.862655	15.342835
25.672854	1118.235968	15.347853
25.458957	1125.908669	15.352871
26.275303	1122.977960	15.357888
25.995158	1129.961968	15.362906
26.000190	1108.155941	15.367923
25.776279	1106.771803	15.372941
25.580950	1099.063793	15.377959
25.429772	1097.468352	15.382976
25.116394	1106.349132	15.387994
25.730262	1122.633711	15.393011
25.851605	1127.043181	15.398029
25.420290	1133.213676	15.403047
25.504763	1126.536107	15.408064
25.478353	1138.660079	15.413082
25.559709	1132.560252	15.418099
25.816116	1129.986982	15.423117
25.984005	1134.327445	15.428135
26.410363	1126.753006	15.433152
26.122310	1137.430386	15.438170
26.291206	1130.682038	15.443187
26.223275	1130.158229	15.448205
26.121396	1135.799765	15.453223
26.417081	1132.059437	15.458240
26.253288	1131.084312	15.463258
26.286414	1131.748387	15.468275
26.359889	1127.389022	15.473293
26.007551	1141.099702	15.478311
26.432900	1129.951933	15.483328
26.279099	1134.560953	15.488346
26.273515	1132.983856	15.493363
26.351056	1130.433773	15.498381
26.496123	1131.735004	15.503399
26.559870	1125.854751	15.508416
26.545837	1126.558409	15.513434
26.417401	1130.035829	15.518451
26.385529	1124.929901	15.523469
26.004932	1129.173837	15.528487
25.967427	1120.807606	15.533504
26.170361	1129.436872	15.538522
26.029285	1130.068605	15.543539
26.119151	1133.710974	15.548557
26.328727	1152.042611	15.553575
26.386836	1156.935408	15.558592
26.216932	1160.756978	15.563610
26.263891	1161.503335	15.568627
26.325917	1151.535647	15.573645
26.397215	1157.487289	15.578663
26.804464	1143.478612	15.583680
26.732390	1148.594136	15.588698
26.714247	1148.829960	15.593715
26.943175	1153.782453	15.598733
26.825906	1155.642878	15.603751
27.147325	1144.793647	15.608768
26.918382	1157.408300	15.613786
27.211011	1147.140427	15.618803
26.931218	1146.896269	15.623821
26.973346	1154.643600	15.628839
26.871642	1154.918163	15.633856
26.800409	1156.208840	15.638874
27.042505	1152.048921	15.643891
26.949904	1152.878265	15.648909
26.822200	1154.608579	15.653927
26.749861	1151.837714	15.658944
26.920974	1151.294969	15.663962
27.005333	1153.398404	15.668979
27.331192	1163.241354	15.673997
27.310100	1156.786218	15.679015
26.896802	1156.694094	15.684032
27.097569	1163.507073	15.689050
27.340205	1173.195781	15.694067
27.570100	1169.669495	15.699085
27.583592	1159.912895	15.704103
27.855669	1150.498216	15.709120
27.569379	1149.256275	15.714138
27.269725	1143.395799	15.719155
27.819952	1144.214147	15.724173
27.509928	1137.167564	15.729191
27.922390	1147.464589	15.734208
27.589681	1141.951932	15.739226
27.273485	1147.126242	15.744243
27.781287	1142.086453	15.749261
27.379427	1143.473584	15.754279
27.359614	1140.499606	15.759296
27.657187	1139.959197	15.764314
27.679195	1139.614865	15.769331
27.862235	1135.349319	15.774349
27.500626	1141.425576	15.779367
27.562561	1136.377976	15.784384
27.756759	1138.160585	15.789402
27.557341	1141.745854	15.794419
27.607232	1143.470129	15.799437
27.378546	1148.679833	15.804455
27.793673	1141.866426	15.809472
27.651341	1140.574211	15.814490
27.408295	1146.181289	15.819507
27.735376	1143.971126	15.824525
27.806471	1165.533855	15.829543
27.958044	1167.180851	15.834560
28.024452	1165.241380	15.839578
28.124148	1171.525193	15.844595
28.156221	1161.669729	15.849613
27.771718	1153.653942	15.854631
27.867868	1159.572582	15.859648
27.996581	1167.481466	15.864666
27.900568	1173.479124	15.869683
28.276862	1175.452188	15.874701
28.429159	1183.018034	15.879719
28.140101	1166.201717	15.884736
28.084955	1172.129371	15.889754
28.075733	1177.976707	15.894771
28.509634	1169.819805	15.899789
28.369393	1174.922221	15.904807
28.442029	1169.283753	15.909824
28.636161	1177.863763	15.914842
28.371083	1177.317845	15.919859
28.658175	1169.384949	15.924877
28.494009	1174.073717	15.929895
28.521455	1166.447566	15.934912
28.520873	1156.654401	15.939930
28.249524	1156.044593	15.944947
28.435227	1159.222471	15.949965
28.566214	1172.295937	15.954983
28.539324	1166.973770	15.960000
28.622867	1169.358472	15.965018
28.478643	1172.525591	15.970035
28.535029	1171.422549	15.975053
28.297731	1168.318518	15.980071
28.394657	1164.453586	15.985088
28.191074	1170.522446	15.990106
28.275686	1173.519218	15.995123
28.424454	1167.940538	16.000141
28.334218	1180.168800	16.005159
28.875078	1194.548104	16.010176
29.215614	1193.317202	16.015194
28.871406	1196.613503	16.020211
29.123044	1192.666522	16.025229
28.957140	1207.002041	16.030247
28.992486	1201.752269	16.035264
29.392687	1197.474672	16.040282
28.835358	1192.115873	16.045299
29.251325	1173.514363	16.050317
28.875330	1176.513724	16.055335
28.906184	1196.879758	16.060352
29.165353	1199.057567	16.065370
29.064053	1200.312455	16.070387
29.009030	1202.227572	16.075405
29.121047	1206.423292	16.080423
29.363611	1204.748126	16.085440
29.504804	1196.938665	16.090458
29.294678	1194.746185	16.095475
29.431382	1197.245014	16.100493
29.368174	1196.258152	16.105511
29.056372	1203.060598	16.110528
29.384270	1205.355768	16.115546
29.527004	1200.312406	16.120563
29.575057	1193.663496	16.125581
29.511419	1190.140679	16.130599
29.418829	1201.153122	16.135616
29.477148	1192.021151	16.140634
29.478481	1196.542169	16.145651
29.554488	1195.680269	16.150669
29.509453	1195.853376	16.155687
29.350156	1196.351611	16.160704
29.421240	1200.715777	16.165722
29.578453	1195.095479	16.170739
29.375640	1195.212954	16.175757
29.401299	1195.714126	16.180775
29.410963	1193.669804	16.185792
29.846593	1200.114159	16.190810
29.634486	1221.327852	16.195827
30.222175	1211.627115	16.200845
30.136782	1219.705029	16.205863
29.907892	1210.552205	16.210880
29.995158	1203.790653	16.215898
29.404848	1201.213320	16.220915
29.893782	1210.743671	16.225933
30.108299	1220.958926	16.230951
29.940965	1221.518387	16.235968
30.337930	1216.409776	16.240986
30.037017	1232.215040	16.246003
30.253852	1218.195632	16.251021
30.104466	1217.066051	16.256039
30.372159	1224.503856	16.261056
30.381659	1212.185886	16.266074
30.390495	1205.976013	16.271091
30.334116	1188.903619	16.276109
30.167565	1184.770051	16.281127
30.057957	1185.540497	16.286144
30.464550	1182.421349	16.291162
30.087525	1201.324128	16.296179
30.396170	1205.056967	16.301197
30.392335	1214.219409	16.306215
30.155242	1221.640601	16.311232
30.762647	1206.299806	16.316250
30.401390	1210.556591	16.321267
30.636372	1209.213066	16.326285
30.510255	1211.723493	16.331303
30.389280	1207.717155	16.336320
30.795472	1210.946616	16.341338
30.561381	1216.688415	16.346355
30.321916	1212.399611	16.351373
30.880440	1207.995646	16.356391
30.643773	1217.002324	16.361408
30.855138	1210.314775	16.366426
30.672322	1216.795875	16.371443
30.785567	1218.495122	16.376461
30.784960	1212.564447	16.381479
30.374323	1212.571873	16.386496
30.739621	1206.665086	16.391514
30.700017	1211.361644	16.396531
30.822982	1215.230266	16.401549
30.955791	1209.923227	16.406567
30.451762	1222.950087	16.411584
30.575793	1233.812412	16.416602
30.942595	1236.466301	16.421619
31.325861	1235.857649	16.426637
31.111112	1236.520523	16.431655
31.222391	1233.866205	16.436672
31.519964	1229.191595	16.441690
31.512045	1236.890851	16.446707
31.276487	1230.187786	16.451725
31.491076	1236.151902	16.456743
31.254104	1239.561333	16.461760
31.564344	1229.084070	16.466778
31.325811	1234.220682	16.471795
31.717229	1239.114237	16.476813
31.674512	1222.702904	16.481831
31.209679	1213.639354	16.486848
31.469695	1205.611862	16.491866
31.485406	1212.896785	16.496883
31.667631	1226.132392	16.501901
31.690029	1215.634012	16.506919
31.096351	1215.919691	16.511936
31.515559	1220.790365	16.516954
31.801297	1226.396974	16.521971
31.870456	1225.072035	16.526989
31.746391	1227.021436	16.532007
31.703007	1232.980958	16.537024
31.791839	1226.080140	16.542042
31.614560	1227.039370	16.547059
31.885714	1231.786600	16.552077
31.721224	1240.148974	16.557095
31.817367	1234.923023	16.562112
31.711579	1238.832052	16.567130
31.917581	1234.533012	16.572147
31.617675	1240.838118	16.577165
31.775527	1227.557616	16.582183
31.796693	1237.736735	16.587200
31.867495	1239.342859	16.592218
31.815012	1237.408408	16.597235
32.085875	1235.902416	16.602253
32.379551	1238.089276	16.607271
32.370264	1239.890643	16.612288
32.436831	1231.017098	16.617306
32.383276	1240.908612	16.622323
32.237354	1230.383171	16.627341
32.384342	1235.157597	16.632359
31.981311	1231.287021	16.637376
32.474193	1226.239133	16.642394
32.096597	1227.189791	16.647411
31.779280	1238.195511	16.652429
32.055571	1241.855947	16.657447
32.141080	1254.654186	16.662464
32.253241	1254.810186	16.667482
32.599568	1260.117418	16.672499
32.263636	1264.255693	16.677517
32.620398	1257.578238	16.682535
32.532387	1261.651168	16.687552
32.558703	1261.795506	16.692570
32.601131	1257.931626	16.697587
32.806370	1259.572975	16.702605
32.856676	1252.701194	16.707623
32.728326	1259.867125	16.712640
33.157220	1258.358055	16.717658
33.067150	1257.260431	16.722675
33.063854	1258.592229	16.727693
33.108767	1255.745725	16.732711
32.753654	1265.352315	16.737728
32.639872	1262.242444	16.742746
32.919813	1255.591942	16.747763
32.865653	1265.124489	16.752781
33.081557	1257.940431	16.757799
32.930828	1257.567440	16.762816
33.260823	1256.696245	16.767834
32.795110	1254.700346	16.772851
32.797335	1263.926351	16.777869
33.072704	1252.726643	16.782887
32.867381	1261.104299	16.787904
32.943749	1276.913826	16.792922
33.328705	1286.822713	16.797939
33.260625	1286.520597	16.802957
33.570288	1284.893766	16.807975
33.652985	1286.651412	16.812992
33.583522	1279.516271	16.818010
33.409826	1267.712385	16.823027
33.185223	1267.042585	16.828045
33.274728	1269.004984	16.833063
33.665297	1290.177650	16.838080
33.526690	1286.421187	16.843098
33.835355	1285.350480	16.848115
33.710920	1292.004294	16.853133
33.908783	1268.796358	16.858151
33.570600	1261.037162	16.863168
33.352640	1246.795007	16.868186
33.473581	1266.807076	16.873203
33.441965	1282.672528	16.878221
33.671415	1273.775363	16.883239
33.673149	1279.920885	16.888256
33.860072	1279.028151	16.893274
33.698437	1274.135384	16.898291
33.653231	1283.810515	16.903309
33.752793	1285.520777	16.908327
34.007847	1281.190478	16.913344
33.896904	1282.068253	16.918362
33.944117	1280.518706	16.923379
34.072642	1285.851085	16.928397
34.323023	1278.718985	16.933415
34.017832	1282.505507	16.938432
34.177786	1276.882347	16.943450
34.356118	1275.616645	16.948467
33.943402	1282.905365	16.953485
33.950695	1282.541110	16.958503
34.151427	1293.245038	16.963520
34.307777	1301.372893	16.968538
34.453135	1302.244525	16.973555
34.040819	1304.144923	16.978573
34.825367	1299.079685	16.983591
34.303607	1302.289904	16.988608
34.579023	1299.630664	16.993626
34.569690	1302.457331	16.998643
34.527648	1303.513468	17.003661
34.775604	1308.026096	17.008679
34.711184	1308.235602	17.013696
34.709480	1303.329973	17.018714
35.161015	1307.696269	17.023731
34.594459	1308.317093	17.028749
34.603240	1310.161437	17.033767
34.770317	1308.731506	17.038784
34.404578	1311.476749	17.043802
34.883441	1306.319025	17.048819
34.590341	1309.636905	17.053837
35.151330	1303.432727	17.058855
35.386588	1309.970150	17.063872
35.058637	1307.109606	17.068890
35.001457	1311.332789	17.073907
34.753947	1317.311985	17.078925
34.773702	1301.252882	17.083943
35.097760	1306.833658	17.088960
34.652050	1302.577433	17.093978
34.899563	1303.617393	17.098995
34.826943	1312.106193	17.104013
35.088761	1311.878629	17.109031
35.001058	1326.003588	17.114048
34.918860	1332.424961	17.119066
35.259264	1330.455029	17.124083
34.922479	1341.298397	17.129101
34.987602	1338.758284	17.134119
35.150297	1335.678561	17.139136
35.127861	1338.591741	17.144154
35.241593	1334.456145	17.149171
35.403236	1351.464227	17.154189
35.654192	1358.129305	17.159207
35.767085	1362.918278	17.164224
35.785903	1369.640879	17.169242
35.763810	1357.367192	17.174259
35.647166	1356.678484	17.179277
35.723936	1363.273420	17.184295
35.992917	1352.831498	17.189312
35.972056	1347.937802	17.194330
36.081478	1335.667176	17.199347
35.691372	1336.430204	17.204365
35.968911	1331.833414	17.209383
35.717946	1324.233658	17.214400
35.447628	1333.841107	17.219418
35.846435	1344.132729	17.224435
35.743161	1361.444928	17.229453
36.047004	1358.440222	17.234471
36.452219	1353.286842	17.239488
36.141754	1352.942416	17.244506
36.226778	1356.914438	17.249523
36.064693	1353.975837	17.254541
36.285079	1360.412277	17.259559
36.083276	1361.537939	17.264576
36.233588	1363.194229	17.269594
36.298033	1345.740285	17.274611
36.305014	1359.876996	17.279629
36.526031	1351.328509	17.284647
36.644735	1354.646272	17.289664
36.513104	1357.215546	17.294682
36.638850	1360.384058	17.299699
36.429036	1361.850888	17.304717
36.558593	1358.289002	17.309735
36.591412	1361.972311	17.314752
36.518658	1367.474279	17.319770
36.617457	1367.473502	17.324787
36.311206	1365.525845	17.329805
36.527264	1355.245372	17.334823
36.384518	1346.916750	17.339840
36.171745	1362.431418	17.344858
36.550076	1375.693771	17.349875
36.688456	1383.951928	17.354893
36.844252	1385.590743	17.359911
37.005768	1385.894990	17.364928
36.706930	1385.785206	17.369946
36.860406	1389.982530	17.374963
36.746504	1391.513635	17.379981
36.979318	1389.003823	17.384999
36.941224	1388.859572	17.390016
37.083068	1389.637707	17.395034
37.373259	1391.061731	17.400051
37.113014	1391.461913	17.405069
37.316727	1389.366184	17.410087
37.331754	1390.036917	17.415104
37.339832	1386.888803	17.420122
37.574616	1382.671411	17.425139
37.364045	1393.571922	17.430157
37.593586	1384.864461	17.435175
37.643348	1384.875634	17.440192
37.693990	1388.336582	17.445210
37.693258	1373.348339	17.450227
37.341428	1387.849378	17.455245
37.621077	1386.755291	17.460263
37.863384	1376.559681	17.465280
37.506504	1387.552996	17.470298
37.984992	1373.092883	17.475315
37.640662	1378.461086	17.480333
37.489248	1377.525559	17.485351
37.771720	1370.558403	17.490368
37.578798	1377.036577	17.495386
37.717324	1384.437150	17.500403
37.720610	1375.478301	17.505421
37.922576	1380.812690	17.510439
38.182511	1385.037827	17.515456
37.900295	1395.132831	17.520474
38.525253	1399.467452	17.525491
38.238333	1394.051194	17.530509
37.944605	1382.370173	17.535527
38.386327	1376.749066	17.540544
38.002067	1385.865012	17.545562
38.144064	1375.252703	17.550579
37.907782	1380.472448	17.555597
38.019931	1394.360823	17.560615
38.067281	1392.607680	17.565632
37.908605	1402.354312	17.570650
38.113596	1395.454765	17.575667
38.322549	1404.869840	17.580685
38.075433	1398.448238	17.585703
38.145388	1403.254822	17.590720
38.405387	1416.948167	17.595738
38.984057	1428.609928	17.600755
38.898885	1436.665473	17.605773
38.824170	1428.240490	17.610791
39.104595	1397.915959	17.615808
38.449507	1402.890558	17.620826
38.716262	1396.146973	17.625843
38.758887	1397.088197	17.630861
38.934704	1403.783895	17.635879
39.059580	1393.289087	17.640896
38.527351	1392.574377	17.645914
38.701806	1399.101394	17.650931
38.884097	1417.350612	17.655949
38.979343	1420.185751	17.660967
39.034362	1424.667313	17.665984
38.955254	1429.591597	17.671002
39.325461	1426.477460	17.676019
39.533063	1420.407455	17.681037
38.805841	1437.429039	17.686055
39.138237	1434.850173	17.691072
39.127723	1432.133231	17.696090
39.252355	1422.646809	17.701107
39.372343	1425.935624	17.706125
39.091800	1429.664801	17.711143
39.469045	1426.727820	17.716160
39.281966	1432.320285	17.721178
39.286288	1426.573740	17.726195
39.102890	1431.372979	17.731213
38.948760	1430.086306	17.736231
39.462855	1440.114502	17.741248
39.511593	1463.997054	17.746266
39.672089	1459.474237	17.751283
39.695208	1454.261913	17.756301
39.520537	1445.835946	17.761319
39.865288	1444.628321	17.766336
39.796016	1442.938872	17.771354
39.870506	1442.150848	17.776371
40.084476	1442.055908	17.781389
40.070032	1443.379789	17.786407
40.483606	1435.141189	17.791424
40.515988	1442.676141	17.796442
40.313521	1432.365789	17.801459
40.125746	1419.243998	17.806477
39.955546	1417.115119	17.811495
40.008428	1429.936421	17.816512
40.327268	1439.612624	17.821530
40.442694	1443.117994	17.826547
40.530398	1443.351818	17.831565
40.058733	1436.314306	17.836583
40.366413	1427.189448	17.841600
40.510617	1435.873447	17.846618
40.314637	1434.545519	17.851635
40.483550	1438.952040	17.856653
40.097558	1441.119620	17.861671
40.557034	1439.852558	17.866688
40.404175	1449.711226	17.871706
40.325414	1446.457504	17.876723
40.554753	1439.337208	17.881741
40.266662	1442.066010	17.886759
40.507199	1434.877254	17.891776
40.700972	1436.051252	17.896794
41.000163	1442.341132	17.901811
40.828580	1441.670108	17.906829
40.729095	1440.164597	17.911847
40.777781	1440.212572	17.916864
40.776970	1438.735817	17.921882
40.824192	1453.756744	17.926899
41.082823	1459.647247	17.931917
41.398542	1461.300782	17.936935
41.384795	1453.279151	17.941952
40.573360	1444.204017	17.946970
40.610739	1455.327440	17.951987
41.002606	1462.125112	17.957005
41.119827	1474.071555	17.962023
41.524092	1466.230637	17.967040
41.270723	1467.043068	17.972058
40.977014	1468.397901	17.977075
41.405026	1465.067920	17.982093
41.358084	1463.024212	17.987111
41.406744	1460.880641	17.992128
41.280267	1461.053934	17.997146
41.412200	1467.608351	18.002163
41.512244	1474.334396	18.007181
41.331477	1480.564047	18.012199
41.641915	1487.986775	18.017216
41.796741	1494.290797	18.022234
41.647619	1495.934653	18.027251
42.026902	1490.555731	18.032269
41.898576	1490.660042	18.037287
42.120677	1494.828304	18.042304
42.088733	1489.827792	18.047322
42.287063	1492.070804	18.052339
42.111673	1496.209962	18.057357
41.973340	1488.202193	18.062375
42.320264	1473.185748	18.067392
42.169513	1475.066125	18.072410
42.129437	1475.690398	18.077427
42.204156	1469.136021	18.082445
42.116601	1468.684076	18.087463
42.702682	1483.803214	18.092480
42.315560	1476.834661	18.097498
42.125170	1461.932005	18.102515
42.703337	1472.143351	18.107533
42.332816	1478.282294	18.112551
42.493094	1485.572483	18.117568
42.475311	1478.881978	18.122586
42.413809	1480.404894	18.127603
42.587288	1482.997869	18.132621
42.487921	1482.588110	18.137639
42.172599	1482.251601	18.142656
42.622054	1480.553141	18.147674
42.246101	1487.589171	18.152691
42.447342	1467.248755	18.157709
42.541664	1479.138099	18.162727
42.543896	1494.094724	18.167744
42.707915	1499.860899	18.172762
42.786769	1510.317342	18.177779
43.042948	1507.492057	18.182797
42.926235	1514.552163	18.187815
43.154298	1513.834272	18.192832
43.047112	1507.733156	18.197850
42.900665	1505.641929	18.202867
43.112495	1506.881348	18.207885
43.221120	1505.070831	18.212903
43.332109	1506.694504	18.217920
43.694748	1508.684522	18.222938
43.325002	1509.818907	18.227955
43.267749	1503.628515	18.232973
43.243873	1507.127071	18.237991
43.417799	1507.449668	18.243008
43.432539	1504.092099	18.248026
43.251629	1510.853336	18.253043
43.625194	1498.840475	18.258061
43.738761	1509.948118	18.263079
43.940899	1505.788264	18.268096
43.796997	1503.025668	18.273114
43.557890	1504.543995	18.278131
43.759716	1507.869983	18.283149
43.655728	1506.488871	18.288167
43.558544	1519.348181	18.293184
43.888162	1525.776987	18.298202
43.908201	1536.072255	18.303219
43.876378	1534.394881	18.308237
43.725547	1533.523424	18.313255
44.267782	1535.054263	18.318272
44.546015	1531.976743	18.323290
43.968055	1540.582626	18.328307
44.396018	1528.092257	18.333325
44.455780	1529.853469	18.338343
44.003783	1528.391063	18.343360
44.239462	1529.526384	18.348378
44.437930	1531.246097	18.353395
44.385174	1527.168919	18.358413
44.272586	1539.454843	18.363431
44.755991	1529.051246	18.368448
44.835410	1528.450975	18.373466
44.353518	1539.440629	18.378483
44.263149	1531.452176	18.383501
44.312321	1535.867837	18.388519
44.450820	1545.231290	18.393536
45.083068	1548.761866	18.398554
44.417608	1557.619398	18.403571
44.738474	1555.947702	18.408589
44.411306	1563.669961	18.413607
44.788210	1568.281829	18.418624
45.243027	1559.426975	18.423642
45.197531	1562.204372	18.428659
45.424937	1553.240857	18.433677
45.012862	1561.430869	18.438695
45.178777	1564.328729	18.443712
45.101200	1559.277744	18.448730
45.254301	1568.199292	18.453747
45.068015	1555.682705	18.458765
45.291875	1557.829608	18.463783
45.154069	1565.280007	18.468800
45.412039	1552.412817	18.473818
44.950110	1565.676074	18.478835
45.156854	1554.857640	18.483853
45.461351	1569.061654	18.488871
45.184165	1578.211327	18.493888
45.585072	1575.792365	18.498906
45.982847	1581.309021	18.503923
46.177729	1583.044711	18.508941
46.150471	1579.232073	18.513959
46.002350	1569.468276	18.518976
46.091887	1557.044964	18.523994
45.700358	1557.059742	18.529011
45.623251	1561.500604	18.534029
45.405595	1562.396690	18.539047
45.336120	1578.548096	18.544064
45.616499	1578.599661	18.549082
45.750036	1591.338362	18.554099
45.905659	1584.004237	18.559117
46.286737	1584.847283	18.564135
46.199721	1578.156005	18.569152
46.155961	1578.940379	18.574170
45.976402	1588.432807	18.579187
46.146168	1601.121205	18.584205
46.038495	1611.378963	18.589223
46.104276	1625.384560	18.594240
46.417793	1615.084451	18.599258
46.108068	1626.343106	18.604275
46.474706	1613.674975	18.609293
46.759060	1630.026034	18.614311
46.720893	1611.812924	18.619328
46.711257	1611.909880	18.624346
46.601210	1613.648635	18.629363
46.701428	1607.042973	18.634381
46.912563	1610.299663	18.639399
46.573122	1632.465765	18.644416
47.486234	1628.788378	18.649434
47.054892	1627.264540	18.654451
46.963563	1618.496989	18.659469
46.867476	1620.447154	18.664487
46.844529	1634.335281	18.669504
47.250061	1630.653569	18.674522
47.142357	1635.856079	18.679539
47.305412	1640.858609	18.684557
47.745885	1627.920299	18.689575
47.639515	1637.797495	18.694592
47.885634	1627.268356	18.699610
47.355203	1617.089315	18.704627
47.541018	1604.506924	18.709645
47.462650	1605.434649	18.714663
47.047207	1613.620540	18.719680
47.460609	1619.697190	18.724698
47.406760	1627.477355	18.729715
47.429528	1636.188585	18.734733
47.934932	1640.294927	18.739751
47.454347	1647.057990	18.744768
48.013286	1635.097504	18.749786
47.722037	1634.619447	18.754803
47.938612	1636.969207	18.759821
48.018937	1630.852431	18.764839
47.559650	1632.449468	18.769856
47.939282	1628.475316	18.774874
48.298419	1634.830202	18.779891
48.014821	1635.194231	18.784909
48.209106	1631.461721	18.789927
47.945431	1636.076339	18.794944
47.824976	1625.205281	18.799962
47.983415	1644.854282	18.804979
48.327024	1651.460290	18.809997
48.323649	1655.144361	18.815015
47.950540	1659.127676	18.820032
48.411875	1659.539992	18.825050
48.485813	1661.507473	18.830067
48.507909	1655.613686	18.835085
48.551555	1653.098860	18.840103
48.428050	1659.921981	18.845120
48.455273	1664.434758	18.850138
48.509573	1668.735391	18.855155
48.372895	1679.573427	18.860173
48.908535	1678.366526	18.865191
48.824190	1689.307420	18.870208
49.614153	1686.346488	18.875226
49.039245	1688.705168	18.880243
49.035810	1684.508457	18.885261
49.440894	1682.789234	18.890279
49.317329	1683.323881	18.895296
49.487673	1684.938578	18.900314
49.486377	1672.718170	18.905331
49.113415	1661.807693	18.910349
49.087945	1659.748860	18.915367
49.252019	1679.152422	18.920384
49.444507	1685.478021	18.925402
49.306757	1677.533841	18.930419
49.236680	1681.841627	18.935437
49.558579	1676.068892	18.940455
49.349186	1677.829412	18.945472
49.696784	1675.844818	18.950490
49.437755	1682.663228	18.955507
49.158840	1684.538041	18.960525
49.797833	1693.819319	18.965543
49.545446	1712.574559	18.970560
49.529850	1703.208871	18.975578
49.835622	1716.131948	18.980595
49.877120	1715.277511	18.985613
50.022957	1703.963848	18.990631
49.924499	1712.373034	18.995648
50.007927	1717.499489	19.000666
49.897440	1718.626057	19.005683
49.939807	1715.498772	19.010701
49.962700	1713.818298	19.015719
49.955818	1728.553850	19.020736
50.127602	1743.292252	19.025754
49.928036	1741.961369	19.030771
49.926020	1744.222623	19.035789
50.454483	1734.446672	19.040807
50.339646	1731.323106	19.045824
50.687139	1727.268996	19.050842
50.317477	1732.397145	19.055859
50.753979	1745.575818	19.060877
51.208978	1741.890325	19.065895
50.519539	1742.722015	19.070912
50.984487	1747.874812	19.075930
51.342097	1743.799670	19.080947
51.182308	1734.807937	19.085965
51.584988	1722.708802	19.090983
51.081577	1722.591563	19.096000
51.085111	1721.864121	19.101018
51.083829	1720.144085	19.106035
51.000069	1717.762129	19.111053
51.286844	1714.512617	19.116071
51.384686	1719.483829	19.121088
51.123097	1717.104405	19.126106
51.038211	1726.949624	19.131123
51.056439	1736.482255	19.136141
51.565016	1742.174089	19.141159
51.267908	1753.115674	19.146176
51.685221	1748.818853	19.151194
51.552287	1749.198397	19.156211
51.210305	1760.215011	19.161229
51.688034	1748.875126	19.166247
51.412727	1751.974667	19.171264
51.429881	1745.279633	19.176282
51.895980	1744.548089	19.181299
51.814369	1764.098223	19.186317
52.223885	1760.137420	19.191335
52.086702	1768.548550	19.196352
52.290985	1771.037068	19.201370
52.244876	1775.378964	19.206387
52.110756	1772.771354	19.211405
52.700118	1769.262843	19.216423
52.200641	1761.583810	19.221440
52.445767	1764.048000	19.226458
52.471890	1759.707208	19.231475
52.411992	1758.793767	19.236493
52.287087	1763.269655	19.241511
52.674353	1761.773978	19.246528
52.213325	1762.481064	19.251546
52.347987	1759.813200	19.256563
52.406958	1765.646702	19.261581
52.559500	1752.786792	19.266599
52.411573	1768.548649	19.271616
52.272218	1764.944577	19.276634
52.450949	1768.523822	19.281651
52.107561	1799.204825	19.286669
52.664412	1794.893518	19.291687
52.603611	1800.451076	19.296704
52.499031	1800.277270	19.301722
52.847278	1806.884517	19.306739
52.931542	1828.283681	19.311757
53.136443	1825.693144	19.316775
53.027201	1825.566598	19.321792
53.251170	1825.652249	19.326810
53.379190	1820.931328	19.331827
53.221273	1825.044346	19.336845
53.671843	1828.716386	19.341863
53.246214	1828.397204	19.346880
53.341921	1826.082112	19.351898
53.542043	1825.311117	19.356915
53.288665	1828.979817	19.361933
53.504705	1838.847537	19.366951
53.819102	1850.192284	19.371968
53.840810	1850.309068	19.376986
53.992943	1857.201566	19.382003
54.157059	1856.780092	19.387021
54.225598	1846.523801	19.392039
54.004974	1851.262219	19.397056
54.320039	1851.074345	19.402074
54.149557	1851.902903	19.407091
54.119189	1855.032919	19.412109
54.045399	1860.499801	19.417127
54.073525	1859.182238	19.422144
53.688951	1861.704004	19.427162
54.092066	1856.608309	19.432179
54.108509	1854.817100	19.437197
54.134837	1853.352584	19.442215
54.281504	1872.355385	19.447232
54.317383	1877.465632	19.452250
54.843805	1871.440805	19.457267
54.636532	1882.734053	19.462285
54.954753	1874.258391	19.467303
54.994042	1875.797534	19.472320
55.135131	1884.438611	19.477338
55.138036	1880.519928	19.482355
55.442374	1887.341064	19.487373
55.499341	1874.211184	19.492391
55.390723	1864.529023	19.497408
55.024681	1850.446365	19.502426
55.422420	1843.297408	19.507443
54.998088	1850.571843	19.512461
55.283398	1851.784517	19.517479
55.635238	1865.075062	19.522496
55.029352	1868.104122	19.527514
55.459477	1871.194172	19.532531
55.176406	1871.698684	19.537549
55.146435	1880.285611	19.542567
55.337185	1869.164942	19.547584
55.114110	1869.962355	19.552602
55.647950	1866.732272	19.557619
55.738487	1866.832137	19.562637
55.686627	1865.216437	19.567655
55.702922	1873.534373	19.572672
55.736195	1888.334066	19.577690
55.982945	1896.317978	19.582707
55.868222	1902.261241	19.587725
56.118989	1901.289804	19.592743
56.075060	1902.006498	19.597760
55.479821	1894.641493	19.602778
55.703322	1891.296087	19.607795
55.951536	1900.249556	19.612813
55.996106	1908.135443	19.617831
56.904119	1910.987644	19.622848
56.791604	1910.076915	19.627866
56.865116	1891.011550	19.632883
56.864398	1886.205581	19.637901
57.295458	1880.233326	19.642919
57.281516	1885.259586	19.647936
56.573380	1884.089120	19.652954
56.710455	1875.218084	19.657971
56.799052	1882.722349	19.662989
56.741209	1880.606036	19.668007
56.829780	1877.625935	19.673024
56.710721	1875.790625	19.678042
56.807842	1876.117342	19.683059
56.821449	1876.072502	19.688077
57.048122	1891.519834	19.693095
57.289337	1899.283015	19.698112
57.103172	1909.839501	19.703130
57.710177	1899.713326	19.708147
57.299519	1908.901430	19.713165
57.298670	1911.945678	19.718183
57.726412	1907.176101	19.723200
57.298323	1903.552594	19.728218
57.639471	1910.090228	19.733235
57.627608	1914.517247	19.738253
57.705267	1907.982658	19.743271
57.676048	1906.819035	19.748288
57.815640	1908.486278	19.753306
57.860125	1905.660599	19.758323
57.930656	1905.461494	19.763341
57.965648	1916.380905	19.768359
57.978393	1900.105038	19.773376
57.969270	1905.800249	19.778394
57.963373	1905.333503	19.783411
57.776761	1913.057822	19.788429
58.188866	1926.880283	19.793447
58.666864	1928.874204	19.798464
58.606508	1928.971589	19.803482
59.061772	1924.278795	19.808499
58.586733	1918.127185	19.813517
58.375553	1909.823382	19.818535
58.536999	1898.148590	19.823552
58.539863	1921.076200	19.828570
58.334457	1916.141515	19.833587
58.042988	1930.638218	19.838605
58.287260	1932.178448	19.843623
58.284161	1930.340968	19.848640
58.090192	1942.834493	19.853658
58.705102	1956.132777	19.858675
58.969312	1958.075155	19.863693
58.643368	1962.944669	19.868711
59.043259	1957.968014	19.873728
59.010402	1963.272775	19.878746
58.989783	1961.196532	19.883763
59.208853	1976.050292	19.888781
59.075282	1982.489008	19.893799
59.662745	1979.342635	19.898816
59.413737	1977.652048	19.903834
59.718205	1979.185507	19.908851
59.867307	1985.897456	19.913869
59.560723	1989.490658	19.918887
59.921923	1977.133837	19.923904
59.563778	1987.102457	19.928922
60.101520	1991.375026	19.933939
60.315204	1983.779546	19.938957
60.076734	1980.788558	19.943975
60.063821	1982.661113	19.948992
59.650318	1988.815498	19.954010
60.169467	1983.632143	19.959027
60.123452	1982.725758	19.964045
60.081683	1984.633580	19.969063
60.419876	1979.713959	19.974080
60.309902	1982.603285	19.979098
60.374320	1977.318343	19.984115
60.167611	1990.936284	19.989133
60.400552	1974.252855	19.994151
60.339912	1974.140813	19.999168
60.309157	1994.755490	20.004186
60.284986	2000.292663	20.009203
60.733797	1999.325066	20.014221
60.573166	2011.685748	20.019239
60.532918	2009.056492	20.024256
60.499771	2014.481808	20.029274
60.854408	2015.578659	20.034291
60.755711	2022.108669	20.039309
61.169856	2035.402459	20.044327
61.422188	2027.925546	20.049344
61.360874	2039.675048	20.054362
61.363659	2034.343954	20.059379
61.496061	2034.473262	20.064397
61.565482	2029.581198	20.069415
61.857034	2033.471522	20.074432
61.714427	2036.058144	20.079450
61.724500	2027.656494	20.084467
61.603823	2015.830351	20.089485
61.724059	2033.436512	20.094503
61.988568	2022.816149	20.099520
61.724032	2034.442200	20.104538
61.759231	2025.917330	20.109555
61.908624	2035.698164	20.114573
61.799674	2032.571165	20.119591
61.892348	2024.973575	20.124608
61.839690	2029.666317	20.129626
62.033928	2039.102411	20.134643
62.105310	2035.703911	20.139661
61.749901	2037.057556	20.144679
62.006336	2032.930386	20.149696
61.973945	2042.950292	20.154714
62.019664	2059.621494	20.159731
62.346350	2057.154547	20.164749
62.238806	2057.636059	20.169767
62.577058	2055.503789	20.174784
62.251801	2062.510119	20.179802
62.531246	2071.352412	20.184819
62.549384	2083.576581	20.189837
62.697897	2098.198820	20.194855
62.967813	2086.404490	20.199872
62.900209	2097.480219	20.204890
62.736894	2093.814815	20.209907
63.324096	2086.300937	20.214925
63.185152	2088.438453	20.219943
63.163396	2086.169449	20.224960
63.155888	2098.666174	20.229978
63.538812	2085.293200	20.234995
64.089633	2073.914169	20.240013
64.005880	2083.945664	20.245031
64.173267	2081.453262	20.250048
64.088221	2079.414824	20.255066
63.940932	2091.644524	20.260083
64.066568	2080.981386	20.265101
63.678019	2082.475380	20.270119
63.612869	2083.773753	20.275136
63.255560	2084.811936	20.280154
63.441615	2089.111359	20.285171
63.730695	2081.764359	20.290189
63.278500	2094.553098	20.295207
63.975661	2104.751156	20.300224
64.057069	2112.310708	20.305242
63.950501	2113.862675	20.310259
64.009159	2109.654416	20.315277
64.032954	2113.307556	20.320295
64.660224	2135.972895	20.325312
64.979275	2142.212799	20.330330
65.060230	2136.110287	20.335347
64.823632	2116.878492	20.340365
64.633159	2118.005413	20.345383
64.820556	2114.532667	20.350400
64.781380	2112.509987	20.355418
64.893859	2125.929207	20.360435
65.345102	2129.267694	20.365453
64.848643	2127.800248	20.370471
64.970596	2133.241540	20.375488
65.420669	2134.846128	20.380506
65.148287	2140.174689	20.385523
65.653967	2138.205463	20.390541
65.118491	2128.249816	20.395559
65.514712	2131.089397	20.400576
65.549035	2133.459061	20.405594
65.095524	2139.623907	20.410611
65.320617	2124.956513	20.415629
65.029371	2136.545875	20.420647
65.371748	2131.042731	20.425664
65.292588	2131.244536	20.430682
65.180058	2142.148446	20.435699
65.856392	2142.140400	20.440717
65.698287	2155.448926	20.445735
65.599900	2155.765462	20.450752
65.492285	2154.118734	20.455770
65.764007	2171.164752	20.460787
66.134224	2168.442652	20.465805
65.992491	2177.673008	20.470823
65.945834	2182.838456	20.475840
65.967417	2180.276928	20.480858
66.093870	2184.003048	20.485875
65.901668	2196.676418	20.490893
66.191329	2212.053417	20.495911
66.420692	2213.560006	20.500928
66.552848	2206.732443	20.505946
66.860183	2210.638612	20.510963
66.924032	2205.583646	20.515981
66.693112	2207.401465	20.520999
66.906034	2226.484296	20.526016
67.320799	2230.889450	20.531034
67.515944	2231.946723	20.536051
67.581019	2220.567782	20.541069
67.226395	2215.293177	20.546087
67.298874	2202.263135	20.551104
67.594269	2207.681805	20.556122
67.310648	2213.451751	20.561139
67.489164	2218.657358	20.566157
67.656463	2220.768376	20.571175
67.469875	2221.105153	20.576192
67.729019	2221.179658	20.581210
67.654428	2231.040359	20.586227
68.022946	2214.636232	20.591245
67.897610	2228.037641	20.596263
67.619480	2221.661571	20.601280
68.053730	2227.161969	20.606298
67.926607	2225.413445	20.611315
67.867903	2227.784503	20.616333
67.989447	2231.298846	20.621351
68.272333	2243.872691	20.626368
68.629144	2243.932814	20.631386
68.642216	2250.758369	20.636403
68.827374	2247.178088	20.641421
68.861788	2249.091387	20.646439
68.621497	2237.360004	20.651456
68.667659	2230.722003	20.656474
68.216703	2246.396114	20.661491
68.434369	2245.539009	20.666509
68.435891	2244.673285	20.671527
68.564045	2252.202840	20.676544
68.828132	2249.254004	20.681562
68.302865	2261.444291	20.686579
68.503433	2264.170963	20.691597
68.775396	2278.627303	20.696615
69.130262	2282.592280	20.701632
69.566044	2280.355846	20.706650
69.147401	2278.636819	20.711667
69.555767	2274.252009	20.716685
69.284745	2281.655497	20.721703
69.767679	2296.628521	20.726720
69.616005	2302.101821	20.731738
69.703420	2305.986655	20.736755
70.278299	2295.814153	20.741773
69.977319	2297.585717	20.746791
69.682404	2297.821364	20.751808
69.955970	2301.560092	20.756826
69.910972	2295.919730	20.761843
70.161963	2304.525265	20.766861
69.765219	2309.486169	20.771879
69.843988	2302.554315	20.776896
69.935250	2314.959464	20.781914
69.808129	2339.993753	20.786931
70.098190	2336.916806	20.791949
70.575605	2341.123034	20.796967
70.207741	2340.272594	20.801984
70.625398	2336.163382	20.807002
70.617299	2351.787660	20.812019
71.048991	2354.158927	20.817037
71.313639	2359.294687	20.822055
70.922579	2357.553598	20.827072
71.282009	2354.292288	20.832090
71.566523	2362.175462	20.837107
71.585733	2344.713590	20.842125
71.490679	2324.348835	20.847143
71.352548	2322.373805	20.852160
71.321166	2318.106114	20.857178
70.954130	2333.219383	20.862195
71.301813	2338.190485	20.867213
71.448889	2346.072801	20.872231
71.459747	2348.282321	20.877248
71.735783	2342.542802	20.882266
71.581812	2356.276052	20.887283
71.872833	2348.242269	20.892301
71.871229	2346.372197	20.897319
71.715118	2349.953857	20.902336
71.908347	2358.703992	20.907354
72.126624	2374.786410	20.912371
72.307987	2372.496716	20.917389
72.321081	2379.290823	20.922407
72.074274	2378.381038	20.927424
72.519309	2378.718208	20.932442
72.447158	2386.154590	20.937459
72.513977	2372.774140	20.942477
72.578673	2378.556882	20.947495
72.463446	2379.825669	20.952512
72.790425	2370.249250	20.957530
72.696901	2374.352552	20.962547
72.829562	2372.508284	20.967565
73.069359	2374.483252	20.972583
72.832818	2373.962320	20.977600
72.915771	2386.523305	20.982618
72.990586	2409.181773	20.987635
73.232999	2405.916889	20.992653
73.014097	2398.760392	20.997671
72.827909	2411.877069	21.002688
73.245977	2401.734534	21.007706
72.902764	2405.938928	21.012723
73.351301	2424.891041	21.017741
73.683322	2422.985025	21.022759
73.747604	2428.437882	21.027776
73.935568	2421.889680	21.032794
73.773552	2426.443391	21.037811
73.932452	2432.041471	21.042829
74.002617	2427.624035	21.047847
74.028883	2433.274781	21.052864
74.298707	2425.792711	21.057882
74.472598	2425.261263	21.062899
74.271514	2423.313552	21.067917
74.347460	2427.358675	21.072935
74.370644	2438.317881	21.077952
74.629385	2446.671733	21.082970
74.464056	2459.433636	21.087987
74.684147	2457.145954	21.093005
74.879095	2443.526119	21.098023
74.639523	2445.679360	21.103040
74.626065	2440.722625	21.108058
74.723224	2449.938172	21.113075
74.788746	2455.745214	21.118093
75.066018	2460.896958	21.123111
75.164328	2475.385614	21.128128
75.797310	2469.051695	21.133146
75.688077	2471.441691	21.138163
76.041843	2464.021603	21.143181
75.804045	2444.031614	21.148199
75.381100	2440.835117	21.153216
75.547672	2441.828001	21.158234
75.576396	2444.073061	21.163251
75.778330	2461.007325	21.168269
76.262492	2465.858203	21.173287
75.755084	2467.536809	21.178304
75.962680	2462.499642	21.183322
75.906354	2472.425092	21.188339
75.913278	2463.692592	21.193357
76.428176	2457.372623	21.198375
75.869943	2468.130695	21.203392
76.162560	2460.560436	21.208410
76.030046	2470.797419	21.213427
75.981434	2489.126855	21.218445
76.458527	2489.700304	21.223463
76.297938	2494.638891	21.228480
76.472670	2492.516486	21.233498
76.519043	2492.897594	21.238515
76.860384	2493.143078	21.243533
76.724980	2495.002831	21.248551
76.894971	2515.053374	21.253568
77.154770	2518.940207	21.258586
77.187547	2529.078013	21.263603
77.055106	2521.664864	21.268621
77.236298	2523.467979	21.273639
77.224296	2527.466778	21.278656
77.235911	2532.037216	21.283674
77.056821	2524.824220	21.288691
77.138242	2537.477731	21.293709
77.704465	2535.357504	21.298727
77.723643	2544.732170	21.303744
78.194306	2544.850743	21.308762
78.153000	2547.007020	21.313779
77.875446	2549.617254	21.318797
78.282871	2550.516876	21.323815
77.887424	2549.975140	21.328832
77.989545	2542.746214	21.333850
78.078587	2532.691506	21.338867
77.842685	2540.121383	21.343885
78.144635	2561.147952	21.348903
78.531177	2568.493967	21.353920
78.596239	2571.812525	21.358938
78.332990	2571.563137	21.363955
78.279634	2570.928888	21.368973
78.951947	2574.542617	21.373991
78.745094	2580.053825	21.379008
78.694531	2585.710709	21.384026
79.236451	2594.589417	21.389043
79.342704	2605.977094	21.394061
79.722196	2593.713129	21.399079
79.187194	2597.321214	21.404096
79.364424	2598.753301	21.409114
79.498883	2595.467509	21.414131
79.221985	2595.167697	21.419149
79.727268	2590.992994	21.424167
79.656945	2591.509879	21.429184
79.523185	2588.962316	21.434202
79.795461	2593.084864	21.439219
79.428743	2604.500075	21.444237
79.789580	2608.382997	21.449255
80.055785	2623.619516	21.454272
79.888701	2623.724571	21.459290
80.109398	2633.605779	21.464307
80.038706	2627.026233	21.469325
80.424920	2621.164557	21.474343
80.071924	2627.093817	21.479360
80.437833	2636.369716	21.484378
80.714326	2642.717135	21.489395
80.611810	2646.404655	21.494413
80.940548	2645.986834	21.499431
80.986764	2643.737597	21.504448
81.298164	2639.292132	21.509466
81.382546	2635.024983	21.514483
81.441940	2633.537400	21.519501
81.763179	2626.306308	21.524519
81.507268	2612.061929	21.529536
81.446482	2613.754546	21.534554
81.661073	2606.739419	21.539571
81.412912	2604.989552	21.544589
81.811494	2606.542772	21.549607
81.724431	2611.691663	21.554624
81.670157	2616.273421	21.559642
81.259635	2616.237503	21.564659
81.204307	2624.330281	21.569677
81.778184	2639.336084	21.574695
81.522981	2638.688397	21.579712
81.848688	2640.952661	21.584730
81.878118	2641.810775	21.589747
81.751956	2659.959184	21.594765
81.916271	2664.379049	21.599783
81.859491	2672.439811	21.604800
81.751399	2680.110879	21.609818
82.367250	2697.537527	21.614835
81.996162	2703.447078	21.619853
82.405214	2696.156010	21.624871
82.573680	2710.552527	21.629888
82.826838	2718.456221	21.634906
83.045817	2720.422990	21.639923
82.875791	2727.851111	21.644941
83.428280	2713.082939	21.649959
83.830296	2706.570376	21.654976
83.611431	2716.557709	21.659994
83.890306	2715.157709	21.665011
83.995652	2711.658735	21.670029
83.815732	2704.417448	21.675047
83.939021	2689.996944	21.680064
83.517267	2684.006788	21.685082
83.899147	2686.955250	21.690099
83.780717	2708.055663	21.695117
83.687111	2709.723203	21.700135
83.740715	2708.398838	21.705152
83.941092	2708.253460	21.710170
84.345306	2716.591180	21.715187
83.653296	2709.948798	21.720205
84.450521	2729.401443	21.725223
84.143312	2744.717486	21.730240
84.419330	2743.182516	21.735258
84.430178	2735.839205	21.740275
84.384041	2746.270257	21.745293
84.885711	2739.939057	21.750311
85.063091	2743.066710	21.755328
85.030327	2741.209021	21.760346
85.378700	2735.929483	21.765363
85.124147	2745.451216	21.770381
85.431073	2735.359811	21.775399
85.073802	2729.890961	21.780416
84.810272	2734.837033	21.785434
85.278357	2744.631009	21.790451
85.065953	2761.092440	21.795469
85.479822	2770.750819	21.800487
85.549066	2770.288491	21.805504
85.464435	2766.327498	21.810522
85.527850	2766.404062	21.815539
85.472753	2781.161864	21.820557
85.805288	2795.096393	21.825575
85.952967	2791.242837	21.830592
85.764721	2800.760323	21.835610
86.060924	2794.159546	21.840627
85.730188	2797.917729	21.845645
86.129813	2816.404601	21.850663
86.452248	2825.872353	21.855680
86.279266	2833.627862	21.860698
86.523064	2828.932469	21.865715
86.641927	2829.830389	21.870733
86.841548	2828.605414	21.875751
86.982712	2840.683468	21.880768
86.999165	2854.828174	21.885786
87.182649	2851.261433	21.890803
87.189753	2855.652389	21.895821
87.469304	2849.410416	21.900839
87.393849	2850.999254	21.905856
87.666352	2850.971456	21.910874
87.647009	2841.853413	21.915891
87.639395	2854.509842	21.920909
87.723583	2848.947152	21.925927
87.908439	2847.130108	21.930944
87.740383	2858.583898	21.935962
87.963157	2843.646891	21.940979
87.974207	2849.711496	21.945997
87.837933	2846.816225	21.951015
88.169866	2862.946601	21.956032
87.890738	2881.313651	21.961050
88.168390	2878.906571	21.966067
87.934508	2882.935624	21.971085
88.302634	2881.224190	21.976103
88.131786	2886.063064	21.981120
88.141386	2898.791395	21.986138
88.816697	2903.344237	21.991155
89.031534	2900.754973	21.996173
88.929730	2899.210732	22.001191
89.059859	2894.843527	22.006208
89.087057	2911.204971	22.011226
89.527283	2921.768546	22.016243
89.271938	2930.886512	22.021261
89.533082	2937.548554	22.026279
89.662910	2918.647910	22.031296
90.019751	2919.689324	22.036314
90.319455	2906.361426	22.041331
90.459285	2888.093870	22.046349
90.756901	2882.714304	22.051367
90.708631	2876.122146	22.056384
90.250244	2878.409039	22.061402
90.691035	2869.464110	22.066419
90.453185	2862.116911	22.071437
90.391455	2856.145295	22.076455
90.581531	2845.626526	22.081472
90.271512	2862.632455	22.086490
90.483330	2861.270716	22.091507
90.692765	2866.869739	22.096525
90.479311	2864.021561	22.101543
90.814573	2871.767136	22.106560
90.305399	2868.560130	22.111578
90.822171	2863.134336	22.116595
90.690504	2879.886043	22.121613
90.843021	2889.598754	22.126631
91.414806	2892.515487	22.131648
91.068594	2904.717311	22.136666
91.177412	2893.891120	22.141683
91.290948	2896.327255	22.146701
91.150309	2898.766802	22.151719
91.686840	2908.376674	22.156736
91.786891	2921.996776	22.161754
92.020576	2913.659091	22.166771
91.629113	2923.616291	22.171789
91.151942	2925.816630	22.176807
91.618160	2930.334448	22.181824
91.374400	2945.972943	22.186842
91.877102	2961.233038	22.191859
92.133417	2969.319030	22.196877
92.062530	2981.046858	22.201895
92.428267	2982.968812	22.206912
92.434255	2985.702194	22.211930
92.604229	2983.319071	22.216947
92.707988	2987.973863	22.221965
92.894213	3011.680451	22.226983
93.034661	3008.744797	22.232000
93.039966	3006.771866	22.237018
93.177178	3003.476855	22.242035
93.230391	3006.737682	22.247053
93.318064	3018.222563	22.252071
93.680882	3010.060366	22.257088
93.453756	3016.120188	22.262106
93.388543	3019.889606	22.267123
93.465506	3038.672262	22.272141
93.556758	3038.356577	22.277159
94.027765	3028.772396	22.282176
94.105862	3041.053580	22.287194
94.220187	3033.846751	22.292211
94.123916	3032.525215	22.297229
94.255654	3036.091546	22.302247
94.255937	3050.976355	22.307264
94.508756	3062.451070	22.312282
94.547586	3057.842728	22.317299
94.823202	3054.709842	22.322317
94.660566	3064.319178	22.327335
95.129933	3052.759278	22.332352
94.802289	3057.864503	22.337370
94.958884	3059.810509	22.342387
95.016079	3053.049773	22.347405
94.982560	3057.594236	22.352423
95.128821	3065.151005	22.357440
95.246192	3079.003754	22.362458
95.799476	3079.358614	22.367475
95.826020	3079.650992	22.372493
95.600923	3085.183617	22.377511
95.701911	3083.195848	22.382528
95.653045	3083.404284	22.387546
95.506139	3084.009919	22.392563
95.614955	3095.676309	22.397581
95.926449	3113.137486	22.402599
96.129017	3115.596196	22.407616
96.303504	3112.122296	22.412634
96.348607	3111.244327	22.417651
96.374400	3116.662282	22.422669
96.281181	3122.355812	22.427687
96.659464	3135.583447	22.432704
96.762554	3139.660329	22.437722
96.901960	3142.136959	22.442739
97.211495	3142.954955	22.447757
96.876643	3148.450501	22.452775
96.978050	3144.553600	22.457792
97.183084	3158.267743	22.462810
97.376816	3160.401923	22.467827
97.419264	3173.913984	22.472845
97.482433	3171.498740	22.477863
97.650561	3166.818582	22.482880
97.747997	3168.777894	22.487898
97.798037	3174.296458	22.492915
97.857492	3164.591372	22.497933
97.745915	3176.251502	22.502951
97.851086	3182.439498	22.507968
97.967338	3196.238200	22.512986
97.729302	3197.768313	22.518003
98.252319	3195.992489	22.523021
98.596906	3223.124145	22.528039
98.767285	3220.774783	22.533056
98.970315	3230.193945	22.538074
99.035915	3227.924763	22.543091
99.061507	3225.193838	22.548109
98.890574	3222.968358	22.553127
99.167618	3225.020533	22.558144
99.297350	3227.964287	22.563162
99.301241	3225.421373	22.568179
99.228583	3224.360395	22.573197
99.196291	3233.901809	22.578215
99.724649	3243.017909	22.583232
99.687656	3248.199377	22.588250
100.162241	3250.283058	22.593267
100.225688	3244.418996	22.598285
100.087490	3244.264716	22.603303
100.295144	3244.765469	22.608320
100.179187	3247.909648	22.613338
100.217702	3252.869467	22.618355
100.734239	3232.218330	22.623373
100.449005	3242.741106	22.628391
100.339718	3234.184827	22.633408
100.578282	3239.841209	22.638426
100.457299	3245.178837	22.643443
100.569710	3237.847807	22.648461
100.712979	3254.569317	22.653479
100.518509	3258.342049	22.658496
100.826375	3278.762928	22.663514
100.942713	3278.559498	22.668531
101.460922	3275.152647	22.673549
101.378449	3294.543381	22.678567
101.659586	3290.557352	22.683584
102.204806	3288.171283	22.688602
102.031834	3289.987164	22.693619
102.311455	3290.214895	22.698637
102.338443	3296.534475	22.703655
102.275689	3285.409012	22.708672
102.335327	3288.985399	22.713690
102.358410	3287.345678	22.718707
102.648534	3281.866453	22.723725
102.480470	3293.948253	22.728743
102.707732	3287.390594	22.733760
102.571057	3281.256824	22.738778
102.764190	3284.147978	22.743795
102.727838	3287.400591	22.748813
102.513382	3294.179762	22.753831
103.426556	3297.090815	22.758848
103.265928	3299.818162	22.763866
103.346320	3323.779635	22.768883
103.676070	3322.375588	22.773901
103.418376	3323.697226	22.778919
103.518024	3325.660116	22.783936
102.817106	3320.272810	22.788954
103.100266	3321.997108	22.793971
103.186537	3330.672403	22.798989
103.556603	3345.049905	22.804007
103.151757	3347.814403	22.809024
103.465828	3362.670126	22.814042
103.641020	3378.073409	22.819059
104.160691	3380.757386	22.824077
104.386377	3398.917995	22.829095
104.465906	3404.732438	22.834112
104.918887	3392.683654	22.839130
104.717283	3396.730142	22.844147
105.158149	3394.426530	22.849165
105.020250	3393.812254	22.854183
105.336903	3390.885700	22.859200
105.237453	3392.297564	22.864218
105.316130	3404.985322	22.869235
105.405377	3390.334528	22.874253
105.273775	3405.854228	22.879271
105.190019	3416.500881	22.884288
105.629767	3424.504470	22.889306
105.799371	3432.271636	22.894323
106.037711	3422.810588	22.899341
105.699327	3423.265556	22.904359
105.475895	3417.005631	22.909376
106.210788	3433.936998	22.914394
105.999596	3451.552741	22.919411
106.119888	3443.929649	22.924429
106.131612	3447.860033	22.929447
106.162710	3455.606851	22.934464
106.490823	3464.027325	22.939482
106.750892	3476.666717	22.944499
106.882095	3475.955111	22.949517
106.763845	3479.855805	22.954535
106.723839	3469.027168	22.959552
107.244514	3489.182652	22.964570
107.269876	3499.082931	22.969587
107.590844	3500.788954	22.974605
107.440807	3497.191036	22.979623
107.435678	3504.648746	22.984640
107.989032	3506.073931	22.989658
107.589235	3509.305413	22.994675
107.612116	3511.642200	22.999693
107.718190	3535.768135	23.004711
107.875807	3533.791867	23.009728
108.182071	3534.812855	23.014746
108.070283	3552.524294	23.019763
108.667966	3551.060117	23.024781
108.742864	3568.678925	23.029799
108.462287	3569.891881	23.034816
109.256923	3563.466814	23.039834
109.237451	3560.599429	23.044851
109.216745	3554.337772	23.049869
109.453494	3556.863937	23.054887
109.524362	3559.378374	23.059904
109.544079	3559.809758	23.064922
109.321426	3561.931106	23.069939
109.597101	3554.599505	23.074957
109.320179	3573.718336	23.079975
109.245584	3589.459205	23.084992
109.517580	3588.977847	23.090010
109.447604	3598.358974	23.095027
109.922016	3602.024205	23.100045
110.041229	3613.422206	23.105063
110.239472	3616.080208	23.110080
110.459599	3610.460866	23.115098
110.284907	3618.059536	23.120115
110.496292	3630.949187	23.125133
110.629235	3638.769995	23.130151
110.975039	3640.972682	23.135168
110.977075	3636.137352	23.140186
111.065066	3630.411492	23.145203
111.232689	3627.312761	23.150221
110.892304	3631.262600	23.155239
110.849634	3644.564408	23.160256
111.370140	3654.468896	23.165274
111.584051	3668.159122	23.170291
111.857368	3666.638706	23.175309
111.579533	3659.542139	23.180327
111.611813	3669.489381	23.185344
111.895405	3680.948248	23.190362
112.208369	3694.317506	23.195379
112.208465	3692.580872	23.200397
112.088908	3691.119930	23.205415
112.409784	3704.302757	23.210432
112.505724	3687.490967	23.215450
112.649173	3712.569262	23.220467
112.895586	3713.856490	23.225485
112.960626	3717.228851	23.230503
112.986855	3717.363776	23.235520
113.436912	3713.448708	23.240538
113.357338	3712.488905	23.245555
113.404619	3714.698675	23.250573
113.638235	3717.355356	23.255591
113.544391	3723.824199	23.260608
113.872230	3738.103763	23.265626
113.889386	3750.710199	23.270643
113.941263	3743.564946	23.275661
114.305577	3741.017654	23.280679
113.994518	3741.033194	23.285696
114.278994	3741.750771	23.290714
114.005362	3754.915058	23.295731
114.162192	3751.907151	23.300749
114.687253	3748.866045	23.305767
114.691796	3764.156407	23.310784
115.038137	3753.755163	23.315802
114.912367	3759.312736	23.320819
115.122696	3756.745372	23.325837
115.156125	3750.438915	23.330855
115.279249	3764.210947	23.335872
115.628793	3767.299841	23.340890
115.576084	3776.831695	23.345907
115.493044	3777.613854	23.350925
115.593636	3781.985103	23.355943
115.390745	3783.498219	23.360960
115.893642	3793.470397	23.365978
115.920655	3808.687642	23.370995
116.034159	3815.984182	23.376013
116.639342	3809.737990	23.381031
116.289929	3809.486809	23.386048
116.395621	3809.798711	23.391066
116.492569	3824.637750	23.396083
116.593151	3836.998399	23.401101
116.943657	3838.157530	23.406119
116.336133	3848.116907	23.411136
116.382451	3844.290711	23.416154
116.956241	3867.907731	23.421171
117.009427	3876.004601	23.426189
116.961543	3873.919390	23.431207
117.418766	3879.258132	23.436224
117.560224	3891.091213	23.441242
117.264371	3896.288917	23.446259
117.448410	3900.864847	23.451277
117.741575	3898.472283	23.456295
117.853392	3921.246302	23.461312
118.071516	3929.362966	23.466330
118.365209	3927.927244	23.471347
118.065209	3932.229380	23.476365
118.544715	3928.690411	23.481383
118.429567	3944.785131	23.486400
118.837924	3954.470392	23.491418
118.838359	3960.354520	23.496435
118.942464	3976.791309	23.501453
119.537141	3964.310610	23.506471
119.027919	3969.815065	23.511488
119.418662	3969.826070	23.516506
119.445444	3984.277185	23.521523
119.510674	3986.089325	23.526541
120.025816	3986.777610	23.531559
119.561026	3995.455592	23.536576
119.684953	3986.962886	23.541594
119.868322	3994.151443	23.546611
120.230929	4008.087410	23.551629
120.735310	4001.478799	23.556647
120.649310	4010.569928	23.561664
121.112162	4000.856607	23.566682
121.421207	3994.509891	23.571699
121.463197	3995.967657	23.576717
121.717653	3993.543123	23.581735
121.698360	3995.027146	23.586752
121.622558	3977.500991	23.591770
121.657207	3976.683050	23.596787
121.835882	3970.891114	23.601805
121.757794	3965.921350	23.606823
121.515826	3979.419064	23.611840
121.652917	3991.177359	23.616858
121.829895	3990.508290	23.621875
121.863821	3997.643708	23.626893
122.382008	3990.701152	23.631911
121.866055	3997.298391	23.636928
122.182095	4012.096109	23.641946
122.149938	4007.551641	23.646963
122.324947	4023.265116	23.651981
122.680333	4018.003645	23.656999
122.907300	4033.786197	23.662016
123.152991	4038.742251	23.667034
123.110018	4038.623619	23.672051
123.013805	4045.641962	23.677069
123.025853	4042.703714	23.682087
123.044557	4051.531184	23.687104
123.297324	4060.281515	23.692122
123.486943	4068.375573	23.697139
123.264426	4067.390634	23.702157
123.406395	4078.458212	23.707175
123.582500	4098.733408	23.712192
124.123067	4107.014631	23.717210
124.045336	4104.372940	23.722227
123.907070	4114.657655	23.727245
124.351998	4127.488774	23.732263
124.359087	4141.315683	23.737280
124.508338	4133.376187	23.742298
124.799042	4144.461632	23.747315
124.784323	4163.577967	23.752333
125.583260	4161.279811	23.757351
125.307614	4162.955081	23.762368
125.585554	4171.212051	23.767386
125.669955	4168.703227	23.772403
125.695653	4170.603291	23.777421
125.787122	4166.636958	23.782439
126.293234	4164.449647	23.787456
126.067744	4169.718864	23.792474
126.264550	4172.668625	23.797491
126.511226	4186.348960	23.802509
126.706258	4189.755845	23.807527
126.204261	4188.744775	23.812544
126.477266	4183.905356	23.817562
126.875409	4182.779354	23.822579
126.498390	4189.711218	23.827597
126.981699	4198.470148	23.832615
127.043326	4211.168567	23.837632
126.881849	4211.798794	23.842650
126.857160	4209.655217	23.847667
126.905860	4236.675521	23.852685
127.337820	4233.439206	23.857703
127.647792	4237.669147	23.862720
127.706358	4253.890349	23.867738
128.115881	4259.131859	23.872755
128.349007	4266.549872	23.877773
128.481436	4265.761623	23.882791
128.561323	4265.627441	23.887808
128.375919	4262.632425	23.892826
128.667691	4263.976510	23.897843
128.809857	4277.782744	23.902861
129.139824	4272.776010	23.907879
129.233541	4277.368321	23.912896
129.327156	4281.478629	23.917914
129.212962	4276.497629	23.922931
129.302384	4289.192921	23.927949
129.625925	4275.421870	23.932967
129.326322	4289.140022	23.937984
129.796946	4296.077054	23.943002
130.228473	4295.263521	23.948019
130.290063	4301.161708	23.953037
130.776315	4304.202858	23.958055
130.698140	4299.516547	23.963072
130.428831	4304.018302	23.968090
130.871322	4298.396829	23.973107
130.535354	4304.685308	23.978125
130.724914	4306.180814	23.983143
130.995510	4304.843534	23.988160
130.564049	4305.883141	23.993178
131.089051	4324.063604	23.998195
130.774037	4335.288465	24.003213
131.261410	4337.112554	24.008231
131.295199	4333.135590	24.013248
131.837772	4354.365898	24.018266
132.363888	4349.490915	24.023283
132.396733	4361.620212	24.028301
132.588833	4357.675174	24.033319
133.078535	4355.658416	24.038336
132.757699	4352.252620	24.043354
133.120296	4341.363029	24.048371
132.777944	4327.807690	24.053389
132.825522	4333.882356	24.058407
133.107581	4344.212520	24.063424
132.795353	4359.664092	24.068442
133.375136	4344.780248	24.073459
133.054792	4348.920582	24.078477
133.321037	4359.604747	24.083495
133.396783	4357.933045	24.088512
133.067141	4375.842640	24.093530
133.397706	4378.396964	24.098547
133.443483	4400.121278	24.103565
133.599898	4414.357595	24.108583
134.223565	4405.243410	24.113600
133.907272	4415.527335	24.118618
134.178960	4419.082592	24.123635
134.472613	4433.222151	24.128653
134.434214	4436.695886	24.133671
134.840648	4435.796071	24.138688
134.788152	4441.488607	24.143706
135.130263	4457.657472	24.148723
135.290714	4453.817077	24.153741
135.196441	4466.500683	24.158759
135.518211	4457.183030	24.163776
135.524824	4464.075238	24.168794
135.767010	4477.402951	24.173811
135.661685	4490.081381	24.178829
135.602625	4486.417232	24.183847
135.938489	4498.176485	24.188864
135.952718	4516.819644	24.193882
136.191928	4516.471479	24.198899
136.003438	4530.741036	24.203917
136.347563	4535.886733	24.208935
136.985734	4543.255131	24.213952
136.892670	4555.859050	24.218970
137.327706	4550.234829	24.223987
137.259393	4565.054849	24.229005
137.019756	4572.596584	24.234023
137.306995	4573.812302	24.239040
137.648019	4576.961892	24.244058
137.931465	4573.716313	24.249075
137.781843	4577.105966	24.254093
138.059334	4584.798497	24.259111
138.158197	4589.257695	24.264128
137.983792	4599.091304	24.269146
138.082663	4600.827649	24.274163
138.142361	4606.088290	24.279181
138.220641	4628.175958	24.284199
138.418912	4638.817617	24.289216
138.559559	4647.123578	24.294234
138.657855	4664.885311	24.299251
138.885682	4667.275350	24.304269
138.756058	4675.933262	24.309287
139.319209	4685.803527	24.314304
139.167444	4696.583996	24.319322
139.558773	4694.182364	24.324339
139.692112	4712.606062	24.329357
139.805133	4724.647067	24.334375
140.144887	4720.796349	24.339392
139.586725	4735.434279	24.344410
140.279204	4744.123789	24.349427
140.287066	4756.301779	24.354445
140.325279	4764.765562	24.359463
140.968886	4771.897631	24.364480
140.976981	4783.723525	24.369498
141.381948	4773.745557	24.374515
141.611558	4776.470844	24.379533
141.449913	4771.272556	24.384551
141.809329	4794.103843	24.389568
141.922002	4805.717277	24.394586
142.234037	4796.334934	24.399603
142.355665	4803.792006	24.404621
142.469094	4803.414988	24.409639
142.870745	4804.368516	24.414656
142.873735	4798.407123	24.419674
142.861131	4799.164654	24.424691
142.767645	4799.164158	24.429709
142.851247	4784.000285	24.434727
142.884734	4805.527200	24.439744
143.393321	4811.952287	24.444762
143.295416	4817.210084	24.449779
143.303108	4821.352591	24.454797
143.218896	4825.324968	24.459815
143.654337	4839.850161	24.464832
143.793000	4850.051648	24.469850
143.924639	4849.999957	24.474867
143.975848	4859.990387	24.479885
144.004434	4872.672946	24.484903
143.999484	4876.349771	24.489920
144.114299	4886.794814	24.494938
144.584684	4898.146145	24.499955
144.642937	4900.814187	24.504973
144.991407	4913.282049	24.509991
145.268667	4905.231220	24.515008
145.231843	4918.598471	24.520026
145.431406	4930.486169	24.525043
145.547542	4935.103185	24.530061
145.709651	4939.932864	24.535079
145.841927	4940.832547	24.540096
145.945241	4937.279084	24.545114
146.079683	4930.112054	24.550131
146.481193	4935.440233	24.555149
146.845960	4950.020963	24.560167
147.238709	4943.741439	24.565184
146.785494	4954.227980	24.570202
146.905915	4950.440012	24.575219
146.921888	4951.606169	24.580237
147.180837	4953.437985	24.585255
147.475880	4946.047291	24.590272
147.233583	4967.168802	24.595290
147.462772	4975.966218	24.600307
147.478329	4986.537039	24.605325
147.693407	4990.076927	24.610343
147.763326	4988.470746	24.615360
148.009383	5001.064143	24.620378
148.188516	5017.591549	24.625395
148.409587	5010.456891	24.630413
148.478657	5022.899485	24.635431
148.767349	5031.993918	24.640448
148.525363	5039.719012	24.645466
148.753617	5036.059043	24.650483
148.756734	5054.790594	24.655501
148.583124	5070.422308	24.660519
149.067080	5075.109425	24.665536
149.223419	5094.429130	24.670554
149.513851	5103.760392	24.675571
149.702181	5108.588778	24.680589
150.148459	5129.531814	24.685607
150.467615	5125.813707	24.690624
150.605902	5135.477469	24.695642
151.023052	5121.274543	24.700659
151.329520	5119.075648	24.705677
150.916888	5120.698095	24.710695
151.310137	5116.546678	24.715712
151.351658	5122.077624	24.720730
151.514766	5127.635775	24.725747
151.623140	5146.251721	24.730765
151.597483	5156.257878	24.735783
151.878130	5154.098850	24.740800
151.667052	5154.070464	24.745818
151.922091	5147.163071	24.750835
152.724930	5156.698747	24.755853
152.310927	5178.899140	24.760871
152.904553	5177.281143	24.765888
152.767238	5181.464354	24.770906
152.718949	5179.338081	24.775923
153.167682	5172.484115	24.780941
153.127157	5172.791969	24.785959
153.408430	5169.210311	24.790976
153.007010	5178.884703	24.795994
153.279670	5202.710518	24.801011
153.929489	5196.836583	24.806029
153.533533	5208.758840	24.811047
153.875651	5200.569142	24.816064
153.871708	5214.524905	24.821082
154.315987	5228.941031	24.826099
154.464699	5235.258636	24.831117
154.250027	5235.088299	24.836135
154.509241	5237.972426	24.841152
154.483722	5265.315186	24.846170
154.420482	5263.028418	24.851187
155.187825	5273.559561	24.856205
155.016002	5297.960310	24.861223
155.309116	5290.481568	24.866240
155.261355	5290.265288	24.871258
155.525955	5307.325776	24.876275
155.971763	5312.733133	24.881293
155.693178	5323.090732	24.886311
156.238019	5318.515503	24.891328
156.381842	5345.483584	24.896346
156.293655	5348.929821	24.901363
156.644507	5350.805793	24.906381
156.777316	5354.900210	24.911399
157.092760	5362.567711	24.916416
157.177840	5374.688041	24.921434
157.433455	5375.853319	24.926451
157.746628	5375.319171	24.931469
157.452305	5379.686884	24.936487
157.959798	5393.419651	24.941504
157.981074	5402.665688	24.946522
158.125209	5407.626982	24.951539
158.190928	5402.659683	24.956557
158.392618	5417.571268	24.961575
158.684390	5426.173103	24.966592
158.876120	5435.278089	24.971610
158.931597	5441.522752	24.976627
158.954367	5437.656099	24.981645
158.886906	5447.345870	24.986663
159.071202	5464.046933	24.991680
159.305156	5469.478847	24.996698
159.236604	5491.510181	25.001715
159.767495	5483.361233	25.006733
159.879093	5498.857831	25.011751
159.992676	5495.233168	25.016768
160.326655	5506.414552	25.021786
160.362229	5514.897304	25.026803
160.662622	5523.682819	25.031821
160.656804	5528.513896	25.036839
160.748801	5539.888808	25.041856
161.190202	5546.251672	25.046874
161.187011	5548.378980	25.051891
161.593754	5551.258356	25.056909
161.203776	5572.281531	25.061927
161.777204	5571.323100	25.066944
162.156420	5574.911387	25.071962
162.103131	5581.313382	25.076979
161.816218	5573.804759	25.081997
162.000590	5594.542825	25.087015
162.364588	5601.886258	25.092032
162.550118	5602.204992	25.097050
162.399762	5622.785437	25.102067
162.493731	5633.885175	25.107085
162.352505	5643.982342	25.112103
163.055264	5660.531719	25.117120
163.297094	5662.336623	25.122138
163.378631	5670.736749	25.127155
163.884971	5681.617745	25.132173
164.310157	5695.490914	25.137191
164.678639	5686.635578	25.142208
164.682368	5687.051644	25.147226
164.497205	5697.988177	25.152243
164.644537	5693.328961	25.157261
164.706365	5698.088629	25.162279
164.733792	5712.854710	25.167296
164.823745	5721.266810	25.172314
164.795779	5732.853046	25.177331
165.289771	5743.146220	25.182349
165.329888	5756.393071	25.187367
165.541845	5759.112892	25.192384
165.526871	5763.617930	25.197402
165.881856	5791.489499	25.202419
166.282809	5779.867677	25.207437
166.251191	5792.200527	25.212455
166.529827	5810.676212	25.217472
166.816738	5815.977074	25.222490
166.625956	5810.534527	25.227507
166.938533	5818.906941	25.232525
167.561029	5833.772775	25.237543
167.490876	5833.655637	25.242560
168.169353	5827.521350	25.247578
167.659422	5832.599626	25.252595
167.820074	5826.587189	25.257613
168.142467	5846.733208	25.262631
168.559606	5849.522635	25.267648
168.861100	5851.557581	25.272666
168.833619	5857.622067	25.277683
168.730460	5851.675324	25.282701
168.902120	5865.999343	25.287719
169.007100	5878.609745	25.292736
169.608366	5872.687176	25.297754
169.328731	5885.241422	25.302771
169.492935	5881.029036	25.307789
169.842408	5911.203417	25.312807
169.573005	5915.751324	25.317824
169.802473	5910.774701	25.322842
170.172066	5927.535861	25.327859
170.853149	5924.807110	25.332877
171.049443	5924.945198	25.337895
171.123115	5930.750548	25.342912
171.413643	5919.253894	25.347930
171.490479	5916.116721	25.352947
171.530656	5923.691471	25.357965
171.969710	5911.476973	25.362983
171.902718	5918.055534	25.368000
172.216196	5906.729036	25.373018
172.116043	5915.210062	25.378035
172.209265	5909.261929	25.383053
172.057339	5916.254413	25.388071
172.152568	5936.463906	25.393088
172.693630	5942.799608	25.398106
172.532560	5950.244239	25.403123
172.602747	5952.235353	25.408141
173.119313	5970.003254	25.413159
172.785328	5975.710720	25.418176
173.045303	5988.175697	25.423194
173.100619	6008.073102	25.428211
173.418479	6001.917070	25.433229
173.433219	6033.993869	25.438247
173.881623	6034.742538	25.443264
174.168525	6034.651627	25.448282
174.022293	6064.125929	25.453299
174.397679	6072.283695	25.458317
174.375955	6072.018041	25.463335
174.786363	6088.219403	25.468352
174.980442	6092.837575	25.473370
174.841101	6113.784625	25.478387
175.403393	6119.557485	25.483405
175.835585	6132.594076	25.488423
175.851385	6140.568539	25.493440
176.246149	6146.974302	25.498458
176.236204	6149.920493	25.503475
176.235912	6158.185238	25.508493
176.579185	6162.674665	25.513511
176.551359	6180.429780	25.518528
176.899734	6179.423248	25.523546
176.900266	6186.918271	25.528563
177.512477	6201.150531	25.533581
177.819598	6208.088083	25.538599
177.820224	6208.899341	25.543616
178.147249	6214.718079	25.548634
178.368532	6217.052764	25.553651
178.317190	6214.594459	25.558669
178.444159	6222.935888	25.563687
178.321371	6242.891687	25.568704
178.745374	6238.829238	25.573722
178.892645	6248.799348	25.578739
179.142527	6252.958215	25.583757
179.509202	6255.505085	25.588775
179.295097	6271.658508	25.593792
179.332014	6259.444937	25.598810
179.433237	6279.832649	25.603827
179.449270	6293.677228	25.608845
179.855797	6298.068414	25.613863
179.787828	6319.047611	25.618880
179.874281	6321.287265	25.623898
180.569657	6333.980361	25.628915
180.922381	6342.353260	25.633933
181.249364	6347.447352	25.638951
181.335757	6353.609089	25.643968
181.799551	6342.878817	25.648986
181.802687	6343.556526	25.654003
182.029344	6339.991062	25.659021
182.364821	6331.900392	25.664039
182.135965	6342.953560	25.669056
182.380603	6355.704247	25.674074
182.340004	6364.569163	25.679092
182.588924	6362.375242	25.684109
183.172273	6360.854999	25.689127
182.755566	6375.394554	25.694144
183.113412	6376.651880	25.699162
183.032785	6389.682851	25.704180
183.255252	6402.360966	25.709197
183.484868	6418.886691	25.714215
183.162042	6426.801973	25.719232
183.583712	6437.782293	25.724250
183.810125	6466.820077	25.729268
184.138117	6471.032568	25.734285
184.332352	6484.046433	25.739303
184.110142	6496.993056	25.744320
184.674643	6505.690519	25.749338
184.402149	6516.641792	25.754356
184.862356	6527.793595	25.759373
185.559658	6542.068292	25.764391
185.894877	6558.630413	25.769408
185.728101	6556.990603	25.774426
185.943380	6575.938862	25.779444
186.036478	6579.604786	25.784461
186.207675	6584.606711	25.789479
186.587008	6605.495429	25.794496
187.020299	6605.102929	25.799514
186.908701	6605.222907	25.804532
187.089264	6619.969092	25.809549
187.393924	6628.110122	25.814567
187.609961	6642.082992	25.819584
187.645662	6642.404589	25.824602
187.887791	6653.224415	25.829620
188.131965	6662.542469	25.834637
188.568233	6669.771606	25.839655
188.358771	6677.116949	25.844672
188.461993	6682.678823	25.849690
188.712003	6694.004629	25.854708
188.886213	6703.860123	25.859725
189.139244	6713.004962	25.864743
189.239726	6720.643801	25.869760
189.347861	6718.123420	25.874778
189.963042	6729.362234	25.879796
190.042912	6740.947259	25.884813
190.083604	6742.482699	25.889831
189.988279	6759.110167	25.894848
190.513022	6763.135400	25.899866
190.601192	6770.283247	25.904884
190.744261	6789.988555	25.909901
191.307631	6787.828113	25.914919
190.936535	6789.076511	25.919936
191.181374	6801.382444	25.924954
191.635896	6817.187843	25.929972
191.603642	6812.926964	25.934989
192.370074	6817.124261	25.940007
192.218991	6833.183946	25.945024
192.370374	6832.315127	25.950042
192.394220	6836.399459	25.955060
192.614794	6852.762545	25.960077
193.227317	6858.952451	25.965095
193.166508	6869.075993	25.970112
193.015767	6870.255901	25.975130
193.253086	6890.289422	25.980148
193.135981	6896.832074	25.985165
193.309951	6906.421475	25.990183
193.718675	6932.268405	25.995200
193.876181	6939.357965	26.000218
194.737269	6946.154404	26.005236
194.588624	6958.677582	26.010253
194.828704	6957.138930	26.015271
194.696497	6977.946457	26.020288
195.546417	6977.416361	26.025306
195.229779	6985.974451	26.030324
195.780582	7010.058581	26.035341
195.729396	7007.674964	26.040359
196.097639	7020.348276	26.045376
195.935580	7038.353439	26.050394
196.692153	7046.028855	26.055412
196.503593	7044.666868	26.060429
196.761167	7047.743824	26.065447
196.986328	7067.219557	26.070464
196.971353	7077.626843	26.075482
197.375361	7080.794505	26.080500
197.339732	7110.049321	26.085517
197.503043	7106.433890	26.090535
197.850059	7128.935074	26.095552
197.830246	7139.970288	26.100570
198.517027	7148.248538	26.105588
198.408558	7165.476590	26.110605
199.104617	7176.934249	26.115623
198.979458	7180.673962	26.120640
198.778899	7187.276727	26.125658
199.285815	7202.557542	26.130676
199.360906	7211.816673	26.135693
199.690975	7222.662774	26.140711
199.883919	7231.757553	26.145728
200.044387	7235.963516	26.150746
200.351225	7250.256155	26.155764
200.625237	7268.486966	26.160781
200.837285	7273.212689	26.165799
200.731130	7276.879055	26.170816
200.919817	7286.841140	26.175834
201.530871	7292.909366	26.180852
201.139045	7300.798303	26.185869
201.895244	7306.844017	26.190887
202.017830	7321.215569	26.195904
201.517860	7326.364287	26.200922
202.043994	7333.923366	26.205940
202.239434	7354.080450	26.210957
202.671457	7348.969404	26.215975
202.544813	7364.210088	26.220992
202.864547	7368.225717	26.226010
203.291227	7376.636903	26.231028
203.608366	7388.576399	26.236045
204.065339	7393.858094	26.241063
204.311560	7400.271710	26.246080
204.273015	7403.144256	26.251098
204.550472	7407.071034	26.256116
204.902528	7423.555541	26.261133
205.335501	7424.037511	26.266151
205.703060	7420.227081	26.271168
205.829028	7425.330769	26.276186
205.663948	7424.282984	26.281204
205.359690	7431.288846	26.286221
205.504826	7432.722946	26.291239
205.866360	7446.498270	26.296256
205.976864	7452.053649	26.301274
206.385740	7469.262672	26.306292
206.014856	7485.139321	26.311309
206.838936	7491.135658	26.316327
206.674664	7514.552983	26.321344
207.029153	7522.890753	26.326362
207.257035	7529.968513	26.331380
207.154435	7544.519877	26.336397
207.654647	7552.922492	26.341415
208.277086	7567.630834	26.346432
208.387917	7578.757395	26.351450
208.662103	7565.149535	26.356468
208.663005	7576.075147	26.361485
209.386793	7580.691972	26.366503
209.490671	7587.034742	26.371520
209.814731	7586.590047	26.376538
209.679207	7584.479193	26.381556
209.497006	7600.109335	26.386573
209.586608	7617.391365	26.391591
210.150422	7624.071260	26.396608
210.228216	7642.008413	26.401626
210.548328	7652.654842	26.406644
210.704239	7665.856643	26.411661
210.991769	7681.186553	26.416679
211.137370	7689.424718	26.421696
211.311933	7693.993920	26.426714
211.650514	7699.480354	26.431732
211.891384	7729.976151	26.436749
211.818790	7720.921943	26.441767
212.081475	7718.206328	26.446784
211.972303	7739.838860	26.451802
212.461770	7746.829335	26.456820
212.708799	7757.304018	26.461837
212.814233	7769.591266	26.466855
213.099843	7778.260821	26.471872
213.229027	7787.119479	26.476890
213.765161	7793.626149	26.481908
213.845156	7804.083803	26.486925
214.114874	7812.259002	26.491943
214.202404	7815.928529	26.496960
214.102556	7841.782964	26.501978
214.208295	7842.757479	26.506996
214.661510	7873.408585	26.512013
215.081728	7870.273619	26.517031
214.932944	7883.619212	26.522048
215.093671	7898.786722	26.527066
215.808530	7906.601272	26.532084
215.965417	7926.950031	26.537101
215.991378	7936.931748	26.542119
216.529424	7930.500902	26.547136
216.819528	7953.597550	26.552154
217.438678	7952.276650	26.557172
217.359892	7962.016364	26.562189
217.177177	7954.635283	26.567207
217.548855	7966.168023	26.572224
217.651528	7975.940453	26.577242
218.355461	7968.888730	26.582260
218.390963	7973.191938	26.587277
218.383896	7986.936375	26.592295
218.459779	7994.052999	26.597312
218.587199	8004.312005	26.602330
218.698081	8027.502506	26.607348
218.797569	8037.632394	26.612365
219.088636	8048.264370	26.617383
219.709837	8065.552660	26.622400
219.765525	8080.605996	26.627418
220.125945	8090.053855	26.632436
220.100031	8100.117044	26.637453
220.059984	8112.921084	26.642471
220.714001	8127.892386	26.647488
220.683074	8141.880539	26.652506
221.262525	8156.364390	26.657524
221.644020	8160.217587	26.662541
221.539361	8174.684791	26.667559
221.835926	8185.293069	26.672576
221.537257	8196.394927	26.677594
222.126495	8212.173103	26.682612
222.545749	8223.293726	26.687629
222.516288	8235.698203	26.692647
223.103313	8238.876484	26.697664
223.376669	8248.266094	26.702682
223.393745	8255.593807	26.707700
223.514743	8277.665024	26.712717
223.964243	8277.915725	26.717735
224.386679	8283.265877	26.722752
224.475999	8303.542397	26.727770
224.859283	8303.100140	26.732788
224.670036	8312.465879	26.737805
224.652366	8313.229959	26.742823
224.929948	8327.233143	26.747840
224.574746	8350.249535	26.752858
225.246964	8367.195371	26.757876
225.476255	8381.911192	26.762893
225.271760	8391.557691	26.767911
225.683065	8410.904673	26.772928
225.875107	8431.149566	26.777946
226.132743	8448.405262	26.782964
226.441781	8468.375680	26.787981
226.300476	8481.706305	26.792999
227.370606	8487.394565	26.798016
227.163336	8509.062277	26.803034
227.361227	8524.436721	26.808052
227.855467	8531.607925	26.813069
227.880541	8553.309926	26.818087
228.615258	8557.136551	26.823104
228.413031	8566.692165	26.828122
228.929462	8582.220051	26.833140
229.365460	8589.066436	26.838157
229.642137	8600.782151	26.843175
230.318093	8606.031444	26.848192
230.615737	8621.252588	26.853210
230.249254	8620.166764	26.858228
230.475011	8614.873238	26.863245
230.894673	8626.526647	26.868263
230.818869	8640.357479	26.873280
231.126736	8657.329048	26.878298
231.198399	8651.535650	26.883316
231.505526	8666.596068	26.888333
231.215542	8670.737811	26.893351
231.974951	8684.895069	26.898368
232.013136	8712.909548	26.903386
232.197221	8713.300294	26.908404
232.594057	8726.667297	26.913421
232.885116	8745.011103	26.918439
233.477292	8747.621361	26.923456
233.223250	8766.886646	26.928474
233.608130	8770.600752	26.933492
233.623491	8778.933495	26.938509
233.729992	8799.361324	26.943527
233.986516	8803.318035	26.948544
234.225407	8827.129836	26.953562
234.779515	8837.948088	26.958580
234.984446	8859.908023	26.963597
235.162852	8866.515845	26.968615
235.551588	8876.524201	26.973632
235.564896	8895.149777	26.978650
235.591143	8897.521443	26.983668
236.161680	8912.822930	26.988685
236.149702	8931.615179	26.993703
236.383899	8935.090435	26.998720
236.649426	8950.311880	27.003738
236.750142	8958.121133	27.008756
237.197602	8978.435597	27.013773
237.343130	8984.425125	27.018791
237.759990	8980.081962	27.023808
238.024767	8999.315320	27.028826
238.274062	9000.030521	27.033844
238.746947	9004.812106	27.038861
238.744536	9022.036571	27.043879
238.804231	9033.743311	27.048896
239.383428	9037.376901	27.053914
239.374676	9049.364831	27.058932
239.502408	9059.498401	27.063949
239.483458	9072.413037	27.068967
240.216570	9082.739089	27.073984
240.188642	9104.948841	27.079002
240.274815	9116.918975	27.084020
241.116893	9127.347708	27.089037
240.687851	9139.292717	27.094055
241.114462	9152.108985	27.099072
241.403075	9161.413002	27.104090
241.447365	9180.819881	27.109108
241.909897	9196.034578	27.114125
241.823698	9209.649442	27.119143
242.139319	9213.626064	27.124160
242.419665	9235.617705	27.129178
242.725722	9251.056241	27.134196
242.957623	9260.100586	27.139213
242.955065	9286.006051	27.144231
243.526052	9298.750417	27.149248
244.212192	9315.630267	27.154266
244.113272	9321.222191	27.159284
244.455623	9339.295522	27.164301
244.696735	9342.367869	27.169319
244.944719	9354.501107	27.174336
245.060174	9372.069737	27.179354
244.955521	9379.005194	27.184372
245.357672	9398.412449	27.189389
245.641829	9420.384779	27.194407
245.982692	9438.162237	27.199424
246.300416	9451.255830	27.204442
246.302475	9469.849330	27.209460
246.898580	9473.442306	27.214477
246.915934	9498.709671	27.219495
247.291781	9501.314592	27.224512
247.742905	9524.901956	27.229530
247.677243	9540.275271	27.234548
248.100341	9537.691013	27.239565
248.628852	9567.413777	27.244583
248.841052	9565.458149	27.249600
249.241065	9573.594582	27.254618
249.716014	9584.874423	27.259636
249.728273	9587.852104	27.264653
249.695459	9593.360306	27.269671
249.729447	9597.256085	27.274688
250.359714	9606.891012	27.279706
250.143656	9624.593952	27.284724
250.338894	9627.749853	27.289741
250.468392	9656.130863	27.294759
250.789389	9668.110004	27.299776
251.139378	9680.057396	27.304794
250.980565	9697.219568	27.309812
251.369461	9712.948471	27.314829
251.063773	9739.554263	27.319847
251.903346	9741.892222	27.324864
251.770006	9767.545113	27.329882
251.968216	9784.557938	27.334900
252.560711	9808.498097	27.339917
252.738367	9824.731324	27.344935
253.054476	9849.390200	27.349952
253.599981	9860.730628	27.354970
253.670100	9894.643794	27.359988
254.059730	9892.670322	27.365005
254.178874	9908.968815	27.370023
254.791906	9916.969635	27.375040
255.491992	9935.617363	27.380058
255.777721	9931.132544	27.385076
256.097749	9931.027283	27.390093
256.251146	9952.256914	27.395111
256.856311	9946.009176	27.400128
257.307804	9950.719076	27.405146
257.511447	9944.825380	27.410164
257.510379	9932.720322	27.415181
257.865174	9943.794097	27.420199
257.980325	9943.161394	27.425216
258.528620	9949.501408	27.430234
258.242614	9968.135400	27.435252
258.464006	9968.234566	27.440269
258.584409	9971.297784	27.445287
258.586426	9986.283306	27.450304
259.392074	10008.631914	27.455322
259.242477	10009.743301	27.460340
259.741182	10024.022859	27.465357
259.981983	10036.539186	27.470375
260.311842	10043.420936	27.475392
260.595467	10048.679654	27.480410
260.456967	10065.700063	27.485428
260.726341	10067.650458	27.490445
260.828250	10091.873678	27.495463
261.128623	10104.323118	27.500480
261.326028	10112.995661	27.505498
261.336107	10139.711869	27.510516
261.786081	10157.279168	27.515533
261.789577	10169.705480	27.520551
261.867176	10191.971123	27.525568
262.297468	10203.125108	27.530586
262.295649	10227.596379	27.535604
262.771093	10247.920254	27.540621
263.209798	10267.243498	27.545639
263.568732	10284.995153	27.550656
263.710612	10285.213531	27.555674
264.046234	10313.385446	27.560692
264.429645	10324.383664	27.565709
264.553103	10342.139499	27.570727
264.551536	10359.683560	27.575744
265.384399	10378.515477	27.580762
265.299835	10400.490882	27.585780
265.440092	10410.355259	27.590797
265.940486	10414.442337	27.595815
266.569041	10437.300949	27.600832
267.144154	10440.565243	27.605850
267.085993	10453.662619	27.610868
267.774739	10467.222928	27.615885
267.711213	10467.856294	27.620903
267.861353	10474.562596	27.625920
268.598162	10480.118832	27.630938
268.177549	10504.249429	27.635956
268.613904	10509.594005	27.640973
268.852085	10519.556702	27.645991
268.897198	10545.074652	27.651008
269.557425	10547.580577	27.656026
269.597829	10561.874554	27.661044
269.738553	10565.290546	27.666061
270.241388	10589.004549	27.671079
270.396345	10602.784108	27.676096
270.370469	10615.973785	27.681114
270.627681	10638.450361	27.686132
270.979109	10655.626944	27.691149
271.765886	10673.296239	27.696167
271.722668	10681.312220	27.701184
271.959638	10691.199589	27.706202
272.143044	10716.952547	27.711220
272.408435	10724.168692	27.716237
272.718595	10739.382598	27.721255
273.007601	10756.956077	27.726272
273.413496	10767.284149	27.731290
273.839977	10789.207154	27.736308
274.114970	10799.918560	27.741325
274.653210	10807.526070	27.746343
274.570671	10817.328026	27.751360
275.066953	10828.324577	27.756378
274.932956	10847.445681	27.761396
275.321259	10851.389768	27.766413
275.673366	10867.551591	27.771431
275.979556	10876.978082	27.776448
276.530900	10892.198070	27.781466
276.930405	10911.583958	27.786484
277.178691	10927.007208	27.791501
277.341788	10935.646675	27.796519
277.383518	10939.155356	27.801536
277.735247	10944.883342	27.806554
277.907703	10967.920161	27.811572
277.939927	10978.807246	27.816589
278.334749	10993.319789	27.821607
278.258028	11004.680999	27.826624
278.455404	11014.546986	27.831642
278.515816	11045.945933	27.836660
279.072614	11071.594481	27.841677
279.094451	11077.306565	27.846695
279.321799	11104.664758	27.851712
280.010846	11121.837549	27.856730
279.982202	11144.009240	27.861748
280.311057	11164.446066	27.866765
280.787432	11183.759219	27.871783
281.222608	11200.041088	27.876800
282.141523	11193.031519	27.881818
282.695799	11218.051941	27.886836
282.877485	11217.054781	27.891853
282.891025	11223.204868	27.896871
282.976580	11220.503280	27.901888
283.508800	11241.586144	27.906906
283.413086	11242.286518	27.911924
283.735372	11250.177096	27.916941
284.184967	11266.336790	27.921959
284.067991	11282.488023	27.926976
284.260702	11281.871919	27.931994
284.632338	11309.026069	27.937012
284.893577	11326.395326	27.942029
285.163159	11345.173629	27.947047
285.306409	11358.831338	27.952064
285.714441	11372.353847	27.957082
286.259402	11396.977429	27.962100
286.419347	11404.500347	27.967117
286.979630	11429.540553	27.972135
286.474267	11446.146196	27.977152
286.775461	11465.087845	27.982170
287.057200	11490.197949	27.987188
287.222160	11516.465941	27.992205
287.774102	11539.140670	27.997223
288.070118	11557.150352	28.002240
288.627677	11576.588742	28.007258
288.939132	11592.282317	28.012276
288.957453	11617.054807	28.017293
290.930790	11597.108550	28.022311
291.037480	11610.128170	28.027328
291.486920	11606.596659	28.032346
291.652372	11617.437697	28.037364
291.625694	11609.166935	28.042381
292.204599	11610.330074	28.047399
292.086793	11607.455251	28.052416
292.207573	11615.572811	28.057434
292.414300	11628.699801	28.062452
292.483228	11637.625271	28.067469
292.774559	11633.848212	28.072487
292.622154	11664.395986	28.077504
292.675243	11669.860223	28.082522
292.997432	11702.031915	28.087540
293.128232	11724.824790	28.092557
293.628512	11744.219616	28.097575
293.413693	11770.341930	28.102592
293.726084	11787.346741	28.107610
294.017264	11815.254658	28.112628
294.490088	11840.170224	28.117645
294.981760	11863.192996	28.122663
294.787378	11892.355221	28.127680
295.599397	11911.868599	28.132698
295.468523	11932.462409	28.137716
295.772318	11959.463793	28.142733
296.397431	11979.250413	28.147751
296.525795	12007.016356	28.152768
296.525247	12025.732999	28.157786
296.815631	12051.023724	28.162804
297.066914	12081.911269	28.167821
297.952445	12098.313851	28.172839
297.980543	12132.703803	28.177856
298.550309	12148.227559	28.182874
299.076614	12171.006853	28.187892
299.091313	12197.118876	28.192909
299.852844	12204.067827	28.197927
299.514103	12230.489491	28.202944
300.728422	12240.845427	28.207962
300.815189	12266.976730	28.212980
300.924333	12281.878233	28.217997
301.633317	12290.697510	28.223015
301.832298	12303.922508	28.228032
302.053928	12314.926167	28.233050
302.138665	12323.537249	28.238068
302.034246	12362.000781	28.243085
302.432702	12376.843328	28.248103
302.845100	12398.187786	28.253120
302.954557	12421.716569	28.258138
303.380362	12448.136780	28.263156
303.778857	12467.715397	28.268173
304.441425	12485.567141	28.273191
304.458460	12502.553974	28.278208
305.173779	12512.176068	28.283226
305.667642	12519.793571	28.288244
305.960520	12544.046018	28.293261
306.326890	12559.935998	28.298279
306.489561	12568.147720	28.303296
306.225047	12581.403524	28.308314
306.778519	12593.556175	28.313332
307.246271	12612.002523	28.318349
307.802819	12620.137306	28.323367
307.757325	12645.001093	28.328384
308.109577	12662.329380	28.333402
308.356184	12672.227335	28.338420
308.509587	12690.653573	28.343437
308.749087	12702.218661	28.348455
309.027263	12720.651917	28.353472
309.489806	12739.814835	28.358490
309.646027	12757.326548	28.363508
309.996196	12791.229262	28.368525
310.080334	12800.434876	28.373543
310.371993	12821.277324	28.378560
310.867781	12852.349797	28.383578
311.381159	12851.182214	28.388596
311.593268	12880.943207	28.393613
312.316158	12870.678838	28.398631
312.600559	12891.666043	28.403648
312.825096	12909.784033	28.408666
313.471142	12901.466668	28.413684
313.713207	12918.098571	28.418701
314.429518	12925.799498	28.423719
314.475494	12923.689141	28.428736
314.603174	12921.377228	28.433754
314.693606	12937.338510	28.438772
314.845799	12948.345041	28.443789
315.177175	12968.265164	28.448807
315.099967	12985.129954	28.453824
315.474708	13003.698283	28.458842
316.018253	13018.324265	28.463860
316.033531	13047.236683	28.468877
316.667634	13050.805053	28.473895
316.581119	13077.779037	28.478912
316.600336	13109.666563	28.483930
317.595425	13131.572498	28.488948
317.728748	13156.483640	28.493965
318.103872	13175.439821	28.498983
318.126237	13195.370626	28.504000
318.897963	13214.630841	28.509018
319.636022	13213.687939	28.514036
319.660217	13244.580347	28.519053
319.821487	13246.313246	28.524071
320.615391	13252.741715	28.529088
321.069706	13269.410099	28.534106
321.340563	13275.491638	28.539124
322.214592	13279.496503	28.544141
322.337181	13285.866669	28.549159
322.515341	13281.973088	28.554176
322.839587	13297.229525	28.559194
323.161901	13304.555271	28.564212
323.231366	13314.766101	28.569229
323.588702	13322.845543	28.574247
323.984528	13337.921106	28.579264
323.622109	13346.653495	28.584282
324.321886	13368.132797	28.589300
324.327125	13378.562723	28.594317
324.701808	13396.612963	28.599335
324.677646	13419.013927	28.604352
324.891707	13450.794644	28.609370
325.457078	13468.169218	28.614388
325.502251	13502.410957	28.619405
325.836254	13523.812876	28.624423
326.137409	13543.565503	28.629440
326.546450	13564.658300	28.634458
327.084240	13582.628777	28.639476
327.156261	13611.166796	28.644493
327.659432	13630.013293	28.649511
328.495064	13649.608246	28.654528
328.535007	13675.009024	28.659546
328.971824	13685.964117	28.664564
328.632243	13702.236265	28.669581
329.135239	13717.043199	28.674599
329.922558	13740.542809	28.679616
329.523527	13757.138855	28.684634
330.178395	13778.670526	28.689652
330.240848	13806.696693	28.694669
330.791660	13827.633132	28.699687
331.044924	13849.055617	28.704704
331.119428	13875.591929	28.709722
331.515394	13893.038545	28.714740
331.656926	13927.409660	28.719757
332.069438	13948.533878	28.724775
332.622867	13975.256220	28.729792
333.038796	13996.956799	28.734810
333.518592	14015.475170	28.739828
333.865924	14040.503863	28.744845
334.267247	14069.008302	28.749863
334.583124	14084.843793	28.754880
334.937544	14113.827631	28.759898
335.530851	14124.541834	28.764916
335.427814	14146.673589	28.769933
335.959789	14175.576667	28.774951
336.301291	14196.828437	28.779968
336.691011	14217.370560	28.784986
337.204330	14240.210128	28.790004
337.230401	14257.247662	28.795021
337.790191	14274.838414	28.800039
338.392570	14298.493464	28.805056
338.449035	14315.475411	28.810074
338.847996	14330.327525	28.815092
339.152395	14347.118848	28.820109
339.552514	14372.996462	28.825127
340.251380	14395.002149	28.830144
340.614566	14405.773315	28.835162
340.921200	14421.897588	28.840180
341.218968	14446.345883	28.845197
341.193644	14462.360007	28.850215
341.877078	14476.616548	28.855232
342.012859	14496.559437	28.860250
341.956113	14507.959051	28.865268
342.090531	14530.126281	28.870285
342.405444	14562.777702	28.875303
342.999436	14576.327741	28.880320
343.101927	14605.506939	28.885338
343.946230	14626.617924	28.890356
344.680340	14639.811413	28.895373
345.198778	14652.378275	28.900391
345.906572	14665.205877	28.905408
345.986761	14680.265837	28.910426
346.469582	14689.306453	28.915444
346.491032	14702.010545	28.920461
346.494553	14700.671721	28.925479
347.373421	14715.755611	28.930496
347.403031	14726.156992	28.935514
347.720675	14724.819499	28.940532
347.769677	14744.649884	28.945549
347.901391	14756.228588	28.950567
348.115496	14778.250089	28.955584
348.146485	14798.063134	28.960602
348.320641	14820.720467	28.965620
348.805284	14846.177662	28.970637
349.134393	14875.707837	28.975655
349.694994	14893.250247	28.980672
350.282926	14925.924952	28.985690
350.476243	14947.824140	28.990708
350.659986	14977.682055	28.995725
351.096954	14997.922289	29.000743
351.526097	15023.952002	29.005760
351.907452	15059.299497	29.010778
352.774022	15075.810791	29.015796
352.864643	15092.319524	29.020813
353.102237	15121.087133	29.025831
353.728115	15143.402673	29.030848
353.449734	15168.294411	29.035866
353.891917	15189.429323	29.040884
354.431839	15212.773250	29.045901
354.702586	15239.390036	29.050919
355.201190	15261.292488	29.055936
355.339571	15288.973978	29.060954
355.593048	15306.299915	29.065972
356.120323	15328.530145	29.070989
356.254651	15355.326552	29.076007
357.048206	15374.528819	29.081024
357.753411	15393.112570	29.086042
358.053171	15406.445747	29.091060
358.581456	15433.226782	29.096077
358.946685	15438.728628	29.101095
359.894045	15455.554333	29.106112
359.822262	15469.603834	29.111130
360.050896	15480.338863	29.116148
360.751266	15492.053922	29.121165
360.658244	15500.906782	29.126183
361.547447	15513.863169	29.131200
361.641252	15523.957698	29.136218
361.779946	15540.791245	29.141236
362.414999	15560.118627	29.146253
362.401679	15570.560998	29.151271
362.887943	15590.271743	29.156288
362.889839	15616.793341	29.161306
363.214559	15631.615216	29.166324
363.828432	15647.101632	29.171341
363.829654	15686.145932	29.176359
364.043875	15706.108362	29.181376
364.548723	15742.872206	29.186394
364.754452	15769.474189	29.191412
365.170179	15790.967507	29.196429
365.056315	15823.409578	29.201447
365.726920	15835.850380	29.206464
365.813939	15877.795117	29.211482
365.793591	15894.413519	29.216500
366.691376	15925.236884	29.221517
366.998351	15958.970656	29.226535
367.173663	15986.298601	29.231552
366.959768	16014.082658	29.236570
368.011174	16047.444690	29.241588
368.303635	16074.580878	29.246605
368.708728	16109.485156	29.251623
369.109390	16130.978345	29.256640
369.570849	16167.378536	29.261658
369.709955	16194.621597	29.266676
370.248707	16219.018599	29.271693
370.925210	16257.857079	29.276711
371.569176	16279.866810	29.281728
372.229360	16303.505369	29.286746
372.863053	16314.571928	29.291764
373.155526	16328.605443	29.296781
372.858084	16358.209378	29.301799
373.451639	16365.560945	29.306816
373.699182	16388.089611	29.311834
374.297567	16409.211922	29.316852
374.978151	16426.078034	29.321869
375.201125	16457.881916	29.326887
375.657181	16466.872923	29.331904
375.901736	16484.189008	29.336922
376.373121	16500.788376	29.341940
377.138015	16523.149742	29.346957
376.998547	16544.056591	29.351975
377.438908	16562.778481	29.356992
377.468108	16582.917127	29.362010
377.987837	16611.257470	29.367028
378.335178	16637.057813	29.372045
378.293032	16667.373656	29.377063
378.825814	16685.206497	29.382080
379.147761	16726.003293	29.387098
379.286118	16751.678831	29.392116
379.689171	16774.061558	29.397133
379.822174	16818.393832	29.402151
381.768201	16819.089772	29.407168
382.726732	16826.858240	29.412186
382.733724	16831.764565	29.417204
383.401803	16840.473513	29.422221
383.601328	16857.502907	29.427239
383.578384	16858.085418	29.432256
383.829711	16886.406017	29.437274
384.034814	16895.143890	29.442292
384.515374	16916.249205	29.447309
384.632650	16938.567623	29.452327
385.143248	16955.058256	29.457344
385.231439	16975.437925	29.462362
385.216272	17005.770253	29.467380
385.866810	17025.257492	29.472397
385.917574	17061.130962	29.477415
386.132267	17090.328400	29.482432
386.831810	17105.062132	29.487450
386.949238	17137.218034	29.492468
387.390154	17156.418172	29.497485
387.741918	17189.446801	29.502503
388.136346	17219.978903	29.507520
388.315088	17246.300947	29.512538
388.691971	17278.018533	29.517556
389.363378	17301.371244	29.522573
389.680304	17329.361322	29.527591
390.409437	17361.589394	29.532608
390.966048	17386.830057	29.537626
391.328226	17407.128615	29.542644
391.609671	17431.371276	29.547661
392.100943	17453.533275	29.552679
392.610653	17459.742540	29.557696
393.211969	17495.861542	29.562714
393.256634	17517.176323	29.567732
393.573867	17523.305088	29.572749
393.805899	17555.962407	29.577767
393.952062	17591.558962	29.582784
394.888818	17621.084471	29.587802
395.295829	17646.797323	29.592820
395.666734	17662.194835	29.597837
395.794874	17697.462055	29.602855
396.146184	17719.385111	29.607872
396.847772	17740.671154	29.612890
397.109776	17768.983535	29.617908
398.005927	17794.237572	29.622925
397.902054	17822.538648	29.627943
398.183142	17840.630272	29.632960
398.891670	17864.515016	29.637978
399.491022	17894.059417	29.642996
399.784500	17909.837763	29.648013
400.375346	17943.966761	29.653031
400.766513	17968.782608	29.658048
401.409432	17984.091234	29.663066
401.200256	18007.061387	29.668084
401.609899	18019.862292	29.673101
402.098024	18051.792461	29.678119
402.688793	18069.594777	29.683136
403.424209	18094.468482	29.688154
403.504702	18107.357393	29.693172
404.366629	18117.097986	29.698189
404.864236	18138.187737	29.703207
405.330253	18151.384263	29.708224
405.801690	18154.133452	29.713242
406.064507	18184.431310	29.718260
406.384373	18187.885986	29.723277
406.406625	18208.817648	29.728295
406.770725	18224.817524	29.733312
407.166603	18248.111572	29.738330
407.344652	18280.949827	29.743348
408.049119	18292.035537	29.748365
407.846838	18324.358868	29.753383
408.531397	18349.473428	29.758400
409.058496	18364.403374	29.763418
409.154423	18390.498612	29.768436
409.578172	18409.279028	29.773453
409.815916	18449.137458	29.778471
410.112611	18469.336588	29.783488
410.309363	18490.620236	29.788506
410.418495	18531.060597	29.793524
410.965143	18556.164416	29.798541
411.359336	18591.293323	29.803559
412.021116	18629.695242	29.808576
412.650001	18655.948666	29.813594
412.876298	18685.995121	29.818612
413.617764	18713.116984	29.823629
413.980953	18751.133623	29.828647
414.435475	18774.916570	29.833664
414.738772	18807.655557	29.838682
415.237444	18839.322119	29.843700
415.378910	18860.658278	29.848717
416.190580	18896.309100	29.853735
416.118915	18929.000638	29.858752
416.990334	18952.900016	29.863770
417.238488	18992.661773	29.868788
418.042083	19012.599681	29.873805
418.113722	19044.508512	29.878823
417.819043	19070.451008	29.883840
418.211291	19102.163105	29.888858
418.368410	19149.478886	29.893876
419.055958	19198.733084	29.898893
419.690197	19233.374419	29.903911
419.637663	19278.782443	29.908928
420.816287	19314.202561	29.913946
421.537802	19350.997129	29.918964
421.895677	19377.119957	29.923981
422.407210	19418.097361	29.928999
422.743446	19439.940107	29.934016
423.631933	19471.109040	29.939034
424.211520	19505.493839	29.944052
424.692152	19521.238475	29.949069
425.065095	19543.716786	29.954087
425.453062	19566.443248	29.959104
426.344473	19569.874375	29.964122
426.227606	19592.433534	29.969140
426.839524	19607.247566	29.974157
426.912580	19636.696020	29.979175
426.892512	19665.189223	29.984192
427.408932	19699.425994	29.989210
428.033802	19727.698411	29.994228
428.319115	19756.727556	29.999245
428.700608	19792.151263	30.004263
428.794718	19824.216965	30.009280
429.256367	19858.676303	30.014298
429.646897	19901.823136	30.019316
430.249739	19938.877413	30.024333
430.809753	19968.758593	30.029351
431.066253	19995.910447	30.034368
431.320362	20020.292398	30.039386
431.769912	20055.678189	30.044404
432.229401	20082.238802	30.049421
433.005598	20110.563190	30.054439
433.415804	20134.139636	30.059456
433.940944	20155.834256	30.064474
434.666275	20184.539603	30.069492
435.351848	20191.672126	30.074509
436.123906	20203.758235	30.079527
436.379686	20223.704738	30.084544
437.246031	20248.105091	30.089562
437.531337	20266.463501	30.094580
437.978118	20274.589353	30.099597
438.060947	20289.720134	30.104615
438.424062	20314.831223	30.109632
438.742546	20336.935188	30.114650
439.008123	20365.215058	30.119668
439.072666	20381.843847	30.124685
439.811540	20408.281411	30.129703
439.909495	20444.759488	30.134720
440.181917	20468.263827	30.139738
440.079194	20511.728530	30.144756
440.650904	20554.142726	30.149773
441.256726	20584.827624	30.154791
441.629385	20638.957129	30.159808
442.287899	20659.325518	30.164826
442.681172	20690.376584	30.169844
443.077685	20730.262071	30.174861
443.859502	20766.290942	30.179879
443.933544	20799.533507	30.184896
444.380453	20833.382395	30.189914
445.066735	20878.494647	30.194932
445.482614	20910.620796	30.199949
445.660962	20949.468781	30.204967
446.198903	20994.179437	30.209984
446.719767	21035.520258	30.215002
447.473684	21065.108391	30.220020
447.576573	21107.224288	30.225037
448.463738	21140.443292	30.230055
448.774076	21179.395332	30.235072
449.703755	21209.576459	30.240090
450.042637	21224.780883	30.245108
450.616324	21247.794731	30.250125
451.631307	21271.478848	30.255143
451.741512	21303.793733	30.260160
452.040200	21318.855326	30.265178
452.561200	21346.437081	30.270196
453.325579	21377.632382	30.275213
453.555943	21390.422425	30.280231
453.768217	21416.718425	30.285248
454.903984	21436.100839	30.290266
455.793955	21436.520761	30.295284
456.520429	21447.500722	30.300301
457.171834	21455.078016	30.305319
457.062626	21469.359698	30.310336
457.435209	21470.284580	30.315354
457.988908	21481.268939	30.320372
458.427089	21491.162970	30.325389
458.597338	21491.324618	30.330407
458.728302	21504.180664	30.335424
458.886168	21522.464506	30.340442
459.164672	21541.278032	30.345460
459.590289	21564.778138	30.350477
459.621557	21593.641080	30.355495
459.676907	21629.648046	30.360512
460.184125	21669.357501	30.365530
460.663353	21697.618747	30.370548
460.979555	21742.426139	30.375565
461.398011	21773.588408	30.380583
461.314691	21824.398414	30.385600
461.815847	21869.305329	30.390618
461.897712	21913.885249	30.395636
462.593802	21963.590721	30.400653
463.207964	22005.737920	30.405671
463.593993	22074.054261	30.410688
464.143606	22118.433137	30.415706
464.839578	22162.897435	30.420724
465.643471	22201.600082	30.425741
466.223409	22238.720078	30.430759
466.701104	22283.237863	30.435776
467.275777	22321.308274	30.440794
468.063217	22360.824663	30.445812
467.640622	22404.960865	30.450829
468.535619	22428.077374	30.455847
468.881945	22482.250365	30.460864
469.423291	22517.125650	30.465882
470.302842	22564.139484	30.470900
470.706807	22603.870383	30.475917
471.622161	22633.089800	30.480935
471.606406	22675.826001	30.485952
472.411606	22709.082619	30.490970
472.941430	22750.246288	30.495988
473.252510	22773.444400	30.501005
474.321024	22799.029662	30.506023
474.514788	22827.360620	30.511040
475.242777	22841.126235	30.516058
476.380837	22859.817580	30.521076
477.020951	22890.696315	30.526093
477.205264	22901.224476	30.531111
477.494723	22919.632350	30.536128
478.181605	22929.847320	30.541146
478.758802	22945.455589	30.546164
478.633293	22973.387315	30.551181
479.521395	22979.549570	30.556199
480.324044	22997.869592	30.561216
480.707298	23019.147465	30.566234
481.282917	23025.972018	30.571252
481.834995	23050.564310	30.576269
481.773957	23060.891748	30.581287
482.108464	23077.232465	30.586304
483.257787	23073.174958	30.591322
483.798212	23090.338311	30.596340
483.878572	23113.084384	30.601357
484.390600	23109.978211	30.606375
484.536480	23133.034799	30.611392
485.095744	23135.727196	30.616410
485.309440	23160.254620	30.621428
485.328659	23183.247819	30.626445
485.742936	23209.330606	30.631463
486.346736	23241.736474	30.636480
486.985067	23270.260087	30.641498
487.556414	23297.177165	30.646516
487.666678	23322.731861	30.651533
488.211547	23354.763239	30.656551
488.598227	23385.585364	30.661568
488.843210	23421.538370	30.666586
489.473176	23445.168489	30.671604
489.844104	23485.474842	30.676621
490.524915	23514.076744	30.681639
490.644543	23554.539869	30.686656
491.191029	23582.698087	30.691674
491.749371	23624.546581	30.696692
492.202445	23673.235710	30.701709
492.766893	23696.246566	30.706727
493.351636	23741.103069	30.711744
493.985961	23775.737886	30.716762
494.571462	23810.980439	30.721780
495.002880	23856.686764	30.726797
495.562127	23880.878436	30.731815
495.808257	23935.732420	30.736832
496.663628	23960.933284	30.741850
496.751940	23993.542455	30.746868
496.810026	24031.664183	30.751885
497.592693	24068.078401	30.756903
498.078631	24112.239941	30.761920
498.326418	24163.151536	30.766938
498.879590	24204.238993	30.771956
499.089524	24239.770732	30.776973
500.422215	24280.819430	30.781991
500.713813	24329.140642	30.787008
501.252728	24376.974854	30.792026
501.792990	24413.819321	30.797044
501.988696	24457.485780	30.802061
502.689406	24506.052819	30.807079
503.187271	24543.996228	30.812096
503.663687	24583.268223	30.817114
504.150388	24622.305123	30.822132
504.523557	24670.301031	30.827149
504.965337	24710.260592	30.832167
505.329365	24763.317938	30.837184
505.696959	24810.652771	30.842202
506.406181	24854.020897	30.847220
506.364419	24906.110415	30.852237
507.072513	24952.150763	30.857255
507.359654	24998.613505	30.862272
508.141461	25042.004364	30.867290
509.828962	25053.162671	30.872308
510.846141	25087.346530	30.877325
511.655613	25093.482031	30.882343
512.186726	25113.547939	30.887360
512.402406	25128.409453	30.892378
513.025458	25162.175210	30.897396
513.050513	25181.611847	30.902413
513.656974	25202.308457	30.907431
513.888298	25228.643312	30.912448
514.325379	25258.176283	30.917466
514.888669	25284.498504	30.922484
515.034487	25326.399734	30.927501
515.760263	25358.018996	30.932519
516.129109	25395.500592	30.937536
516.399804	25428.696345	30.942554
517.349552	25454.315397	30.947572
517.582947	25499.583672	30.952589
517.927915	25535.839402	30.957607
518.581872	25579.887579	30.962624
518.773985	25618.160181	30.967642
519.393616	25659.384822	30.972660
519.956800	25695.168167	30.977677
520.799728	25734.458841	30.982695
521.318549	25777.189987	30.987712
521.432997	25819.466867	30.992730
521.966074	25861.706820	30.997748
522.232206	25907.267078	31.002765
522.580035	25958.390788	31.007783
523.128208	26011.338383	31.012800
524.051912	26060.010381	31.017818
524.291287	26099.111917	31.022836
524.494379	26161.851118	31.027853
525.783166	26201.946599	31.032871
526.930197	26240.353488	31.037888
526.610574	26282.071782	31.042906
527.852712	26308.452750	31.047924
528.478249	26351.974618	31.052941
529.302326	26375.925668	31.057959
530.468216	26401.783549	31.062976
530.254838	26435.209284	31.067994
530.980102	26468.187176	31.073012
531.327732	26500.135156	31.078029
531.832697	26531.614577	31.083047
532.670343	26559.816097	31.088064
532.678425	26594.103282	31.093082
533.040007	26621.225536	31.098100
533.592835	26668.136205	31.103117
533.985694	26700.956972	31.108135
534.675291	26743.711710	31.113152
534.851571	26789.535743	31.118170
535.483853	26829.915522	31.123188
535.932262	26871.636128	31.128205
536.503564	26901.284553	31.133223
536.929296	26946.028337	31.138240
537.234312	26987.559264	31.143258
537.949345	27020.416919	31.148276
538.223410	27066.792788	31.153293
538.787614	27110.405932	31.158311
539.371801	27146.289622	31.163328
539.761181	27201.832910	31.168346
539.937245	27233.284773	31.173364
540.386200	27287.310117	31.178381
540.941533	27342.935838	31.183399
542.105883	27383.727356	31.188416
542.853561	27427.757846	31.193434
543.688217	27455.939248	31.198452
544.083862	27495.291613	31.203469
545.192082	27523.300057	31.208487
546.111704	27541.251537	31.213504
546.868285	27564.944473	31.218522
547.120905	27596.825559	31.223540
547.576282	27630.277807	31.228557
548.067698	27659.338624	31.233575
548.639778	27686.114132	31.238592
549.026325	27726.317248	31.243610
549.249599	27760.771764	31.248628
549.921005	27799.206806	31.253645
550.250669	27833.173150	31.258663
550.907888	27872.481547	31.263680
551.145236	27912.959895	31.268698
551.930484	27952.101406	31.273716
552.225336	27983.332348	31.278733
552.897293	28034.542267	31.283751
553.601389	28068.564803	31.288768
554.053223	28110.931396	31.293786
554.975225	28142.143506	31.298804
555.451757	28178.278076	31.303821
555.927821	28217.362731	31.308839
556.935969	28256.551918	31.313856
557.333725	28299.474050	31.318874
557.803983	28320.658350	31.323892
558.142555	28365.461714	31.328909
558.711565	28403.817822	31.333927
559.331157	28443.897468	31.338944
559.721020	28486.793015	31.343962
560.110965	28521.570679	31.348980
560.403511	28569.752055	31.353997
560.660660	28613.834871	31.359015
561.602388	28659.352806	31.364032
561.827242	28708.233967	31.369050
562.802126	28752.941915	31.374068
563.039807	28803.499658	31.379085
563.676431	28849.303839	31.384103
564.819816	28886.603434	31.389120
565.048996	28936.932693	31.394138
565.919574	28977.866613	31.399156
566.765522	29010.068241	31.404173
567.247537	29051.062597	31.409191
567.967293	29084.481787	31.414208
568.064955	29120.588555	31.419226
569.052005	29139.243200	31.424244
569.589212	29171.949213	31.429261
569.991425	29206.407457	31.434279
570.638231	29221.473094	31.439296
571.004770	29269.205135	31.444314
571.652715	29298.544750	31.449332
572.783397	29329.906226	31.454349
572.974619	29364.198995	31.459367
573.872383	29385.917137	31.464384
574.298857	29412.900080	31.469402
575.139616	29441.512749	31.474420
576.149019	29461.388137	31.479437
576.748688	29480.737410	31.484455
577.385622	29505.523102	31.489472
577.342876	29533.829787	31.494490
577.824839	29571.913077	31.499508
578.506578	29598.230985	31.504525
578.719994	29629.453562	31.509543
579.357999	29661.584735	31.514560
579.432343	29705.363989	31.519578
580.110246	29741.823818	31.524596
580.508801	29786.181936	31.529613
580.746057	29827.671240	31.534631
581.353534	29872.321929	31.539648
581.742017	29927.627874	31.544666
582.889102	29967.510180	31.549684
583.588961	30013.107770	31.554701
583.894130	30064.304404	31.559719
584.964265	30101.963065	31.564736
585.580005	30160.190513	31.569754
585.880062	30192.746576	31.574772
586.671442	30238.527854	31.579789
586.848789	30287.632938	31.584807
587.098496	30329.465221	31.589824
587.236998	30384.004487	31.594842
588.005773	30431.257395	31.599860
588.693741	30490.748336	31.604877
589.294914	30552.674558	31.609895
590.067802	30606.667215	31.614912
590.726518	30660.588089	31.619930
591.344146	30710.710692	31.624948
592.289703	30763.655033	31.629965
592.508063	30814.928661	31.634983
593.696248	30855.834616	31.640000
594.286713	30902.504013	31.645018
594.945515	30933.289698	31.650036
595.552715	30979.082358	31.655053
595.914533	31024.620560	31.660071
596.517611	31070.426784	31.665088
596.974099	31126.403251	31.670106
597.428169	31170.051638	31.675124
598.021638	31214.269491	31.680141
598.253942	31278.180009	31.685159
599.188353	31318.802335	31.690176
599.891538	31369.868275	31.695194
600.183350	31413.519814	31.700212
601.382014	31455.589767	31.705229
601.571096	31500.698066	31.710247
602.326126	31538.969158	31.715264
602.335119	31583.733006	31.720282
603.319904	31630.604982	31.725300
603.731384	31674.987696	31.730317
604.422548	31737.738867	31.735335
604.967585	31784.355249	31.740352
605.354568	31840.746635	31.745370
605.784030	31893.722808	31.750388
606.461571	31943.696617	31.755405
607.123593	32011.909899	31.760423
608.051684	32066.505224	31.765440
608.476158	32110.574381	31.770458
608.844199	32161.286612	31.775476
609.886727	32219.589691	31.780493
610.422761	32275.878021	31.785511
611.204475	32315.373789	31.790528
611.896040	32381.087233	31.795546
612.293684	32435.749321	31.800564
613.449761	32477.693292	31.805581
614.337827	32518.282116	31.810599
615.504469	32538.481174	31.815616
616.915415	32571.507666	31.820634
617.576988	32607.354492	31.825652
618.386452	32611.255237	31.830669
618.487654	32646.532276	31.835687
619.004472	32672.308652	31.840704
619.423805	32704.375504	31.845722
619.689517	32736.598120	31.850740
620.233466	32768.946695	31.855757
620.593853	32810.661697	31.860775
621.020543	32863.262520	31.865792
621.419265	32908.168039	31.870810
621.712277	32966.223266	31.875828
622.241618	33006.158280	31.880845
622.649779	33067.643459	31.885863
623.211515	33128.569193	31.890880
623.960403	33188.939194	31.895898
624.780541	33240.867786	31.900916
625.467326	33285.917407	31.905933
626.127144	33346.072815	31.910951
626.811619	33394.310581	31.915968
627.307196	33451.991833	31.920986
628.003170	33525.371331	31.926004
628.711007	33562.382999	31.931021
629.029024	33627.369709	31.936039
629.603472	33679.789810	31.941056
630.676661	33742.716104	31.946074
631.259995	33799.761708	31.951092
632.132514	33844.055030	31.956109
632.564761	33891.485221	31.961127
633.068799	33936.375266	31.966144
633.597709	33983.580842	31.971162
633.886921	34038.310570	31.976180
634.857935	34079.463122	31.981197
634.935041	34137.189858	31.986215
635.888468	34187.880115	31.991232
636.764144	34241.989237	31.996250
637.335962	34299.076268	32.001268
637.726462	34344.185613	32.006285
638.471085	34398.961501	32.011303
638.952040	34446.536301	32.016320
639.847444	34500.699630	32.021338
640.164659	34566.617760	32.026356
640.671671	34620.478720	32.031373
640.863703	34692.235519	32.036391
641.726061	34754.885853	32.041408
642.531072	34821.232640	32.046426
643.198640	34882.076736	32.051444
643.968568	34935.031953	32.056461
644.658097	34994.130446	32.061479
645.518378	35053.878464	32.066496
646.200105	35118.568357	32.071514
646.437154	35188.050080	32.076532
647.234322	35241.358181	32.081549
647.868986	35310.646006	32.086567
648.723958	35375.105133	32.091584
649.584342	35435.690806	32.096602
650.167909	35499.369926	32.101620
651.160933	35552.604358	32.106637
651.806814	35603.000926	32.111655
653.325413	35645.243701	32.116672
654.214324	35692.246874	32.121690
653.844993	35738.534608	32.126708
654.968573	35779.923721	32.131725
655.829331	35827.512835	32.136743
656.289557	35879.374959	32.141760
656.971688	35918.081359	32.146778
657.664590	35969.755531	32.151796
657.901336	36015.403554	32.156813
658.643206	36067.135897	32.161831
659.448069	36111.436903	32.166848
659.991969	36156.227778	32.171866
660.626664	36212.265295	32.176884
661.243298	36272.630382	32.181901
661.538701	36326.223329	32.186919
661.850687	36387.335402	32.191936
662.392973	36443.064346	32.196954
663.156225	36514.916713	32.201972
663.815410	36572.914467	32.206989
664.652840	36635.278857	32.212007
665.445136	36694.346338	32.217024
666.856730	36734.728715	32.222042
668.491472	36779.154325	32.227060
669.657141	36793.730294	32.232077
669.900278	36837.886250	32.237095
670.584907	36861.853274	32.242112
670.810713	36885.864209	32.247130
671.493582	36918.104880	32.252148
671.908537	36944.693946	32.257165
672.466858	36982.581027	32.262183
672.910700	37028.136132	32.267200
673.509666	37056.294212	32.272218
673.998478	37110.370849	32.277236
674.143396	37152.767242	32.282253
674.776555	37205.777762	32.287271
674.999671	37272.119546	32.292288
675.742183	37330.042300	32.297306
676.390789	37400.465755	32.302324
676.989847	37456.510042	32.307341
677.258664	37524.186477	32.312359
678.167602	37582.334050	32.317376
679.084749	37642.614305	32.322394
679.193899	37715.688282	32.327412
680.473059	37768.548728	32.332429
681.415902	37833.765421	32.337447
681.919738	37905.124743	32.342464
682.708617	37959.417645	32.347482
683.485546	38019.660027	32.352500
684.780691	38073.797091	32.357517
685.740168	38127.133185	32.362535
686.713907	38176.792529	32.367552
687.532545	38206.837212	32.372570
687.962190	38257.644341	32.377588
688.573498	38291.032973	32.382605
689.662435	38333.260904	32.387623
689.989452	38382.409709	32.392640
691.000656	38437.600350	32.397658
691.415683	38484.963388	32.402676
691.947764	38528.941331	32.407693
692.568721	38586.304867	32.412711
692.794821	38640.806682	32.417728
693.436194	38694.129467	32.422746
693.992779	38762.929197	32.427764
694.760289	38814.320826	32.432781
695.461196	38877.322358	32.437799
695.602962	38943.254773	32.442816
696.364567	39006.805117	32.447834
697.208308	39076.033515	32.452852
697.608987	39139.718755	32.457869
698.362862	39222.518910	32.462887
698.890247	39296.215719	32.467904
699.772604	39366.815020	32.472922
700.386475	39438.003582	32.477940
701.173426	39502.239510	32.482957
702.020613	39578.610292	32.487975
702.755035	39644.500506	32.492992
703.845054	39696.919041	32.498010
704.246268	39763.662327	32.503028
704.840265	39827.215793	32.508045
705.645522	39895.121582	32.513063
706.101102	39960.009390	32.518080
707.045942	40009.306094	32.523098
707.630752	40082.475280	32.528116
708.166547	40142.197631	32.533133
708.832022	40203.596480	32.538151
709.734598	40270.855555	32.543168
710.204480	40330.899202	32.548186
710.901182	40399.418973	32.553204
711.243986	40470.657937	32.558221
712.219473	40522.706945	32.563239
713.200870	40603.425304	32.568256
714.196943	40670.079419	32.573274
714.876290	40723.303676	32.578292
715.277757	40787.629036	32.583309
716.764759	40841.665595	32.588327
717.235027	40905.158702	32.593344
717.988385	40958.314124	32.598362
718.949102	41020.798543	32.603380
719.520876	41081.452292	32.608397
720.367600	41138.826106	32.613415
720.728618	41197.549365	32.618432
721.884868	41258.491912	32.623450
722.246620	41332.916623	32.628468
722.963173	41386.486863	32.633485
723.636943	41451.579295	32.638503
724.136462	41529.852054	32.643520
725.015654	41589.135032	32.648538
725.841728	41656.071229	32.653556
726.641058	41710.067089	32.658573
727.541626	41774.600833	32.663591
728.288316	41837.932941	32.668608
729.524541	41902.968487	32.673626
729.905966	41961.381226	32.678644
731.033860	42008.558524	32.683661
732.334375	42049.855686	32.688679
732.948576	42098.968294	32.693696
733.667475	42143.614281	32.698714
734.746013	42198.536214	32.703732
735.305996	42242.884444	32.708749
736.149986	42290.919395	32.713767
736.206164	42340.279783	32.718784
737.270621	42386.625862	32.723802
737.739491	42442.726487	32.728820
738.250873	42498.614761	32.733837
739.192287	42553.548596	32.738855
739.382951	42622.630526	32.743872
739.980265	42676.720619	32.748890
740.199719	42751.971039	32.753908
740.912783	42823.758636	32.758925
741.661806	42897.580128	32.763943
742.591694	42972.570803	32.768960
743.124365	43040.092678	32.773978
743.950691	43108.710699	32.778996
744.623098	43178.406818	32.784013
746.135220	43230.813522	32.789031
746.626276	43287.121270	32.794048
747.770660	43336.067359	32.799066
748.252631	43384.694447	32.804084
748.871743	43437.188388	32.809101
749.951350	43489.524653	32.814119
750.561480	43551.793392	32.819136
751.474018	43599.996782	32.824154
752.371994	43651.540459	32.829172
753.030570	43715.509746	32.834189
754.232437	43761.002055	32.839207
755.012443	43824.319371	32.844224
755.211825	43874.783395	32.849242
755.688619	43928.247240	32.854260
756.097151	43980.911391	32.859277
756.887599	44046.194932	32.864295
757.661517	44107.869056	32.869312
758.389553	44172.462702	32.874330
759.197324	44244.498428	32.879348
759.673617	44312.669231	32.884365
760.099212	44383.207842	32.889383
760.632348	44469.811049	32.894400
761.535466	44547.424090	32.899418
762.077012	44625.295169	32.904436
762.790663	44704.990749	32.909453
763.784860	44786.167018	32.914471
764.531153	44871.175558	32.919488
765.363140	44953.163482	32.924506
766.457236	45031.911057	32.929524
767.208907	45110.392348	32.934541
768.461153	45186.833455	32.939559
768.963520	45262.459093	32.944576
769.915038	45332.140604	32.949594
770.671254	45409.365483	32.954612
772.068345	45483.032379	32.959629
772.968893	45529.572169	32.964647
773.819151	45590.189586	32.969664
775.090760	45647.138047	32.974682
775.879997	45699.028045	32.979700
776.316379	45767.703558	32.984717
777.434999	45825.259837	32.989735
777.917589	45875.810146	32.994752
778.402134	45932.208980	32.999770
779.270695	45988.835903	33.004788
779.822034	46056.769569	33.009805
780.841405	46105.248425	33.014823
781.693992	46177.773311	33.019840
782.129131	46243.712677	33.024858
782.771343	46304.803824	33.029876
783.130859	46368.912233	33.034893
784.194655	46435.944671	33.039911
784.907700	46504.862836	33.044928
785.602733	46572.571600	33.049946
786.661798	46650.321259	33.054964
787.230498	46725.938177	33.059981
788.375546	46783.442291	33.064999
788.859115	46856.421418	33.070016
789.375012	46915.972839	33.075034
789.884081	46975.623519	33.080052
790.540309	47045.472408	33.085069
791.304661	47108.279074	33.090087
791.947291	47180.805827	33.095104
792.714314	47250.465938	33.100122
794.082191	47318.400025	33.105140
794.841100	47391.722495	33.110157
795.395376	47459.774333	33.115175
796.124939	47537.533498	33.120192
797.016605	47605.101686	33.125210
798.179257	47675.434625	33.130228
798.419616	47753.906969	33.135245
799.263653	47821.913615	33.140263
800.345565	47901.859502	33.145280
800.877718	47981.520879	33.150298
801.933812	48053.995897	33.155316
802.728828	48142.494362	33.160333
804.204317	48186.683873	33.165351
805.266443	48255.178994	33.170368
806.600798	48304.557004	33.175386
807.753035	48361.145510	33.180404
808.067144	48409.580446	33.185421
809.035424	48467.353613	33.190439
809.643878	48520.501394	33.195456
810.429482	48584.882170	33.200474
811.507687	48639.807014	33.205492
812.351189	48702.643232	33.210509
813.057651	48758.826008	33.215527
813.618261	48811.774323	33.220544
813.480515	48877.779786	33.225562
814.419660	48948.673660	33.230580
815.169957	49026.864843	33.235597
815.714008	49103.152300	33.240615
816.642839	49181.686241	33.245632
817.186570	49268.877869	33.250650
817.707187	49336.155595	33.255668
818.201302	49437.665022	33.260685
819.033647	49530.595009	33.265703
819.757780	49621.073900	33.270720
820.383106	49709.106368	33.275738
823.072698	49767.005536	33.280756
823.832783	49846.126999	33.285773
824.703941	49918.255322	33.290791
826.125795	49980.099550	33.295808
827.253809	50037.401508	33.300826
828.203178	50097.412846	33.305844
828.650490	50163.853134	33.310861
829.737378	50218.780972	33.315879
830.447952	50279.263364	33.320896
830.879883	50342.105895	33.325914
831.461805	50403.545707	33.330932
831.795111	50474.226724	33.335949
832.448334	50553.862140	33.340967
833.589800	50612.313297	33.345984
833.856859	50684.383668	33.351002
834.983540	50743.627461	33.356020
835.793541	50828.739856	33.361037
836.196553	50887.046655	33.366055
837.098569	50958.017397	33.371072
837.781794	51032.115267	33.376090
838.827374	51097.824485	33.381108
839.770333	51183.351579	33.386125
839.868257	51261.170683	33.391143
840.743283	51353.685073	33.396160
841.533556	51438.778229	33.401178
842.453675	51528.019357	33.406196
843.218811	51616.131247	33.411213
843.879470	51703.635944	33.416231
844.917442	51779.173246	33.421248
845.912271	51872.509861	33.426266
847.290451	51945.702399	33.431284
848.118150	52032.131151	33.436301
848.529004	52125.385763	33.441319
849.659424	52208.756009	33.446336
850.773112	52279.524692	33.451354
852.238090	52347.826226	33.456372
852.906323	52420.390264	33.461389
854.510003	52487.790296	33.466407
855.610356	52553.501331	33.471424
856.425631	52626.780184	33.476442
857.391297	52687.194729	33.481460
858.614593	52732.470838	33.486477
859.668187	52795.214757	33.491495
860.375641	52850.214973	33.496512
860.740410	52913.696446	33.501530
861.612037	52968.921611	33.506548
861.776197	53041.896509	33.511565
862.188075	53117.154439	33.516583
862.933120	53188.912024	33.521600
863.320921	53282.713125	33.526618
864.232085	53366.170052	33.531636
864.826576	53455.216626	33.536653
865.506505	53556.443848	33.541671
866.352887	53647.394271	33.546688
867.118467	53751.034168	33.551706
868.491227	53833.996977	33.556724
869.113102	53934.048156	33.561741
869.694493	54037.525215	33.566759
871.158309	54124.511324	33.571776
871.593803	54222.346393	33.576794
873.281723	54302.104100	33.581812
874.424848	54387.320144	33.586829
875.097284	54464.876537	33.591847
876.796007	54554.276024	33.596864
877.518077	54638.680613	33.601882
878.306870	54712.199197	33.606900
879.481580	54788.710347	33.611917
880.011871	54862.160017	33.616935
880.883914	54922.843859	33.621952
881.310275	54986.814293	33.626970
882.703330	55052.508770	33.631988
883.604973	55116.113861	33.637005
884.599222	55184.423668	33.642023
885.199657	55255.290894	33.647040
885.895400	55325.484857	33.652058
886.813074	55390.465652	33.657076
887.775857	55470.428069	33.662093
888.162787	55545.939589	33.667111
889.547977	55623.801805	33.672128
889.878507	55703.696499	33.677146
890.710186	55773.862434	33.682164
891.466745	55852.256595	33.687181
892.259237	55947.037295	33.692199
893.117562	56035.336125	33.697216
894.027891	56135.064563	33.702234
895.225116	56211.286614	33.707252
896.496846	56293.537596	33.712269
897.276817	56374.798824	33.717287
898.698472	56433.263457	33.722304
899.344289	56517.499446	33.727322
900.105019	56601.494923	33.732340
901.255978	56673.852768	33.737357
902.365516	56760.266445	33.742375
903.121520	56832.054221	33.747392
903.873831	56909.764399	33.752410
905.299619	56986.733887	33.757428
905.977737	57054.440645	33.762445
907.064701	57123.025569	33.767463
908.159635	57193.006024	33.772480
908.948688	57277.100584	33.777498
909.703475	57343.569148	33.782516
910.714390	57431.424548	33.787533
911.376421	57512.002744	33.792551
912.584369	57593.328309	33.797568
912.959003	57670.101238	33.802586
913.595729	57757.946302	33.807604
914.361188	57841.933494	33.812621
915.072047	57948.555887	33.817639
915.771412	58033.496869	33.822656
916.527028	58137.382349	33.827674
917.326888	58237.380262	33.832692
918.462704	58339.280363	33.837709
919.185795	58441.182136	33.842727
920.400855	58530.574734	33.847744
921.058562	58641.968950	33.852762
922.194213	58738.871813	33.857780
922.937466	58845.189994	33.862797
923.892501	58947.964700	33.867815
924.918366	59040.874422	33.872832
926.368709	59139.261135	33.877850
927.194716	59230.012786	33.882868
927.968527	59331.739681	33.887885
929.051501	59420.381400	33.892903
930.406498	59501.891684	33.897920
930.903394	59579.409333	33.902938
931.987464	59649.109383	33.907956
933.173646	59737.045868	33.912973
934.016538	59817.014416	33.917991
934.931330	59897.040490	33.923008
935.626565	59985.649936	33.928026
936.307432	60070.710030	33.933044
937.336654	60153.365854	33.938061
938.181912	60246.293028	33.943079
939.236724	60324.255211	33.948096
940.316756	60412.421361	33.953114
941.109407	60506.300513	33.958132
942.162610	60588.732760	33.963149
942.705835	60687.636241	33.968167
944.026096	60770.339524	33.973184
944.831572	60882.403286	33.978202
945.423004	60966.464745	33.983220
946.301923	61066.481926	33.988237
947.247152	61171.349063	33.993255
947.970144	61275.211827	33.998272
949.115117	61381.847314	34.003290
950.030557	61487.953764	34.008308
950.950554	61587.966440	34.013325
951.814396	61693.001873	34.018343
953.040286	61784.638189	34.023360
953.908969	61897.505749	34.028378
954.367772	62003.041962	34.033396
955.604379	62108.685719	34.038413
956.489088	62238.891612	34.043431
957.855572	62330.443057	34.048448
958.670659	62447.292584	34.053466
959.678298	62557.661971	34.058484
960.846726	62652.295668	34.063501
962.224845	62750.560329	34.068519
963.584931	62837.772274	34.073536
964.670732	62932.440363	34.078554
965.673091	63024.177337	34.083572
966.961313	63106.737425	34.088589
968.232928	63193.314894	34.093607
969.449076	63280.104514	34.098624
970.608602	63359.236045	34.103642
971.103825	63442.053377	34.108660
972.208353	63526.460907	34.113677
972.197371	63618.772300	34.118695
973.160552	63709.583389	34.123712
974.037922	63816.195036	34.128730
974.762345	63907.661085	34.133748
975.509727	64009.396580	34.138765
976.544765	64114.250564	34.143783
977.755124	64216.400888	34.148800
978.384112	64319.586913	34.153818
979.313837	64429.404258	34.158836
980.444060	64527.953664	34.163853
981.448060	64626.095251	34.168871
983.020176	64716.155263	34.173888
983.700334	64813.910642	34.178906
984.458306	64907.442629	34.183924
985.243274	64990.861321	34.188941
985.815755	65102.994044	34.193959
986.706249	65180.850883	34.198976
987.605842	65285.493671	34.203994
988.106248	65400.946842	34.209012
989.480417	65506.356641	34.214029
991.020959	65612.389676	34.219047
991.963405	65716.034660	34.224064
993.096473	65824.041564	34.229082
993.724641	65935.220818	34.234100
994.942467	66026.579984	34.239117
995.483270	66133.615076	34.244135
996.473835	66249.855128	34.249152
997.443866	66361.300526	34.254170
998.646260	66480.654196	34.259188
999.660118	66592.497950	34.264205
1000.357667	66715.246115	34.269223
1001.654027	66823.584225	34.274240
1003.335507	66921.095692	34.279258
1004.518673	67028.923128	34.284276
1005.968369	67124.660597	34.289293
1006.888386	67221.538786	34.294311
1007.992590	67315.635446	34.299328
1009.035985	67405.266358	34.304346
1009.919573	67510.302254	34.309364
1010.937076	67602.303187	34.314381
1012.081736	67707.946610	34.319399
1013.266255	67800.754428	34.324416
1014.254760	67893.507693	34.329434
1014.919414	67996.926851	34.334452
1016.417575	68093.861756	34.339469
1017.412505	68185.729964	34.344487
1018.447528	68281.644813	34.349504
1019.242563	68381.660641	34.354522
1019.699453	68494.178838	34.359540
1021.066729	68591.043563	34.364557
1021.817946	68692.282399	34.369575
1022.608255	68803.335042	34.374592
1023.650473	68900.990329	34.379610
1024.479238	69024.671471	34.384628
1025.573555	69134.978205	34.389645
1026.388238	69256.196980	34.394663
1027.500777	69365.856792	34.399680
1028.720514	69477.806870	34.404698
1029.386540	69598.648325	34.409716
1030.644134	69713.160483	34.414733
1031.673034	69831.076545	34.419751
1032.435214	69948.020824	34.424768
1033.751140	70067.286543	34.429786
1034.700602	70185.312996	34.434804
1035.753922	70296.581245	34.439821
1036.707138	70405.489483	34.444839
1038.078971	70516.362841	34.449856
1038.858319	70621.216786	34.454874
1039.629202	70726.793603	34.459892
1041.041072	70831.331569	34.464909
1041.848677	70930.282014	34.469927
1042.520423	71032.924042	34.474944
1043.606781	71149.547367	34.479962
1044.901976	71259.628183	34.484980
1045.913455	71363.826215	34.489997
1046.974350	71480.733933	34.495015
1048.251977	71593.576730	34.500032
1049.618534	71687.413593	34.505050
1050.769134	71799.722689	34.510068
1051.795357	71903.933429	34.515085
1052.698204	72018.575423	34.520103
1053.617343	72129.230962	34.525120
1054.534081	72234.632010	34.530138
1055.550671	72348.984316	34.535156
1056.567857	72458.435765	34.540173
1057.723866	72574.656352	34.545191
1058.455619	72675.746364	34.550208
1060.050919	72783.955735	34.555226
1060.640173	72912.980925	34.560244
1062.215402	73022.440828	34.565261
1063.460086	73133.172185	34.570279
1064.638021	73243.599302	34.575296
1065.912929	73353.238771	34.580314
1067.430883	73458.125332	34.585332
1068.826792	73550.004528	34.590349
1070.087211	73647.321224	34.595367
1071.271584	73733.949987	34.600384
1072.623257	73825.129542	34.605402
1073.269493	73933.102299	34.610420
1073.892309	74022.585942	34.615437
1074.832066	74125.291440	34.620455
1075.467674	74237.271105	34.625472
1076.381300	74352.233344	34.630490
1077.005664	74473.640187	34.635508
1078.000323	74591.606773	34.640525
1079.126275	74712.460993	34.645543
1079.738403	74840.152636	34.650560
1080.983383	74963.960600	34.655578
1081.690434	75105.052934	34.660596
1082.336345	75237.883370	34.665613
1083.735071	75379.997537	34.670631
1084.550663	75527.987368	34.675648
1085.482288	75665.894850	34.680666
1086.523975	75812.557508	34.685684
1087.338132	75949.430533	34.690701
1088.582606	76096.237440	34.695719
1089.455567	76258.176046	34.700736
1090.904444	76401.970694	34.705754
1091.884362	76558.775870	34.710772
1092.867496	76699.647565	34.715789
1094.031648	76840.438544	34.720807
1094.932839	76989.815012	34.725824
1096.119826	77119.135490	34.730842
1097.259234	77267.214208	34.735860
1098.456707	77402.733702	34.740877
1099.716927	77540.501569	34.745895
1100.338463	77677.576256	34.750912
1102.278074	77802.059065	34.755930
1102.971544	77943.430950	34.760948
1104.643488	78084.041548	34.765965
1106.170927	78203.922291	34.770983
1107.322018	78333.610136	34.776000
1108.277041	78454.570745	34.781018
1109.278613	78582.590241	34.786036
1110.725704	78703.860146	34.791053
1111.853590	78836.667283	34.796071
1112.868269	78977.914713	34.801088
1113.819752	79100.201542	34.806106
1114.438704	79235.666588	34.811124
1115.416731	79378.320880	34.816141
1116.917993	79509.701542	34.821159
1118.055738	79650.666370	34.826176
1119.128765	79790.940921	34.831194
1120.676310	79930.793460	34.836212
1122.194571	80057.594030	34.841229
1124.499948	80145.940920	34.846247
1125.969218	80246.894556	34.851264
1128.102551	80343.337989	34.856282
1129.208405	80437.268955	34.861300
1130.303441	80539.015513	34.866317
1131.345736	80626.650515	34.871335
1132.184062	80723.260336	34.876352
1133.088494	80829.077222	34.881370
1134.130696	80925.545435	34.886388
1135.124198	81037.080031	34.891405
1136.206662	81142.051729	34.896423
1136.894859	81246.079121	34.901440
1138.531526	81346.882409	34.906458
1139.453643	81451.155386	34.911476
1140.393902	81562.530820	34.916493
1141.741402	81672.078185	34.921511
1142.617727	81789.995042	34.926528
1143.506413	81891.276759	34.931546
1145.202974	82001.253102	34.936564
1146.193295	82098.696817	34.941581
1147.429927	82211.081252	34.946599
1148.341079	82328.115430	34.951616
1149.554639	82441.460326	34.956634
1150.830635	82562.691379	34.961652
1151.914670	82664.803531	34.966669
1152.611376	82781.965295	34.971687
1153.738115	82901.724124	34.976704
1154.502650	83018.280705	34.981722
1155.502663	83145.743810	34.986740
1156.593119	83279.905450	34.991757
1157.988819	83386.687620	34.996775
1158.386976	83518.488826	35.001792
1159.629352	83636.681421	35.006810
1160.494637	83761.127453	35.011828
1161.368425	83897.575997	35.016845
1162.406878	84025.208169	35.021863
1163.676378	84156.439844	35.026880
1164.806503	84290.049994	35.031898
1165.898004	84427.945020	35.036916
1166.749047	84563.350943	35.041933
1168.286117	84697.070917	35.046951
1168.760647	84846.179207	35.051968
1170.270748	84981.145659	35.056986
1171.591460	85122.118801	35.062004
1172.653374	85273.856540	35.067021
1173.827622	85417.197843	35.072039
1175.013756	85570.390630	35.077056
1176.402501	85707.622123	35.082074
1177.645237	85859.997113	35.087092
1179.006190	86005.664056	35.092109
1180.764443	86143.208175	35.097127
1181.455330	86288.010714	35.102144
1182.907015	86430.930973	35.107162
1184.366089	86558.903535	35.112180
1185.122426	86709.544728	35.117197
1186.786688	86844.894113	35.122215
1187.612887	86999.822107	35.127232
1189.115820	87125.537318	35.132250
1190.361134	87260.998765	35.137268
1191.547069	87419.342201	35.142285
1192.807128	87552.157479	35.147303
1193.552712	87709.204940	35.152320
1194.787816	87847.829405	35.157338
1196.389041	87981.961965	35.162356
1197.399989	88130.676280	35.167373
1199.180868	88258.811717	35.172391
1200.251923	88405.340378	35.177408
1201.241392	88540.403530	35.182426
1202.452620	88692.580512	35.187444
1203.691810	88825.602613	35.192461
1205.176060	88962.437777	35.197479
1206.250842	89100.172905	35.202496
1208.037662	89229.730179	35.207514
1209.565934	89353.389508	35.212532
1210.564345	89492.734853	35.217549
1212.043066	89619.903972	35.222567
1213.633448	89753.871059	35.227584
1215.065434	89860.941980	35.232602
1216.213439	89984.005082	35.237620
1217.378925	90104.356931	35.242637
1218.550193	90219.493129	35.247655
1219.250535	90353.609574	35.252672
1220.348318	90486.424512	35.257690
1221.774037	90604.607657	35.262708
1222.567413	90746.704246	35.267725
1223.904509	90866.815295	35.272743
1224.901545	90997.789436	35.277760
1225.540724	91110.546145	35.282778
1227.134054	91220.582930	35.287796
1228.235464	91348.870055	35.292813
1229.517869	91466.259079	35.297831
1230.510553	91602.275505	35.302848
1231.501763	91743.426237	35.307866
1232.580876	91869.175410	35.312884
1233.584866	92016.110801	35.317901
1234.655335	92150.964954	35.322919
1235.662808	92296.578519	35.327936
1237.056752	92449.868098	35.332954
1237.677896	92599.423412	35.337972
1238.666377	92763.488068	35.342989
1240.015228	92926.371731	35.348007
1241.110979	93100.465809	35.353024
1242.275569	93259.952387	35.358042
1243.683035	93429.779653	35.363060
1244.496087	93605.349932	35.368077
1246.060926	93779.077294	35.373095
1247.013212	93952.220747	35.378112
1248.660525	94117.529909	35.383130
1250.051237	94287.619120	35.388148
1251.068786	94469.750278	35.393165
1252.389926	94630.947026	35.398183
1254.040818	94807.781360	35.403200
1255.232109	94980.118732	35.408218
1256.555087	95145.490232	35.413236
1257.414099	95324.521179	35.418253
1258.888652	95491.837804	35.423271
1260.217140	95683.838208	35.428288
1261.607411	95845.600695	35.433306
1263.311745	96025.523825	35.438324
1264.630978	96196.113037	35.443341
1266.117683	96358.691639	35.448359
1267.562145	96535.029034	35.453376
1268.574039	96697.564483	35.458394
1270.134954	96862.912871	35.463412
1271.328007	97028.274665	35.468429
1272.853984	97185.331289	35.473447
1274.263819	97354.241429	35.478464
1275.408986	97512.143980	35.483482
1277.280374	97671.987131	35.488500
1278.273795	97847.112991	35.493517
1279.461835	97995.191610	35.498535
1280.570998	98157.029651	35.503552
1281.490848	98324.485290	35.508570
1283.215084	98480.205399	35.513588
1284.648061	98639.091331	35.518605
1286.157965	98795.160283	35.523623
1287.537187	98955.545253	35.528640
1288.978351	99104.416380	35.533658
1290.375726	99252.194190	35.538676
1291.668269	99403.422478	35.543693
1293.002566	99540.715085	35.548711
1294.427143	99685.078019	35.553728
1295.485378	99827.307398	35.558746
1296.679961	99961.175428	35.563764
1297.520345	100109.515713	35.568781
1298.627244	100234.022930	35.573799
1299.962999	100387.510018	35.578816
1301.150318	100532.595802	35.583834
1302.214305	100675.417719	35.588852
1303.269783	100844.474815	35.593869
1304.853172	100983.929610	35.598887
1306.092942	101153.615689	35.603904
1307.038420	101312.436904	35.608922
1308.399618	101478.406434	35.613940
1309.412724	101643.056215	35.618957
1310.751894	101805.726260	35.623975
1312.088682	101984.392729	35.628992
1313.311435	102160.192459	35.634010
1314.615690	102320.794724	35.639028
1315.511463	102503.200252	35.644045
1317.252178	102683.917328	35.649063
1318.727084	102861.603620	35.654080
1320.177304	103040.245197	35.659098
1321.542791	103208.327307	35.664116
1322.864330	103389.196967	35.669133
1323.991813	103556.612796	35.674151
1325.614693	103737.040639	35.679168
1326.972408	103907.813540	35.684186
1329.178643	104065.713671	35.689204
1330.654913	104230.097712	35.694221
1332.152465	104389.488939	35.699239
1333.760513	104548.013619	35.704256
1334.835212	104708.365726	35.709274
1336.542192	104868.141940	35.714292
1337.524710	105019.253085	35.719309
1339.142118	105175.728048	35.724327
1340.603405	105324.073813	35.729344
1341.613803	105490.825239	35.734362
1342.907550	105652.766766	35.739380
1344.003862	105809.714614	35.744397
1345.216273	105985.022168	35.749415
1346.623070	106148.771271	35.754432
1347.639324	106321.492674	35.759450
1348.789828	106489.657617	35.764468
1350.115358	106668.851526	35.769485
1351.986664	106834.019937	35.774503
1353.570721	106996.021189	35.779520
1354.793094	107170.169409	35.784538
1356.315256	107328.256549	35.789556
1357.185362	107495.905738	35.794573
1358.929261	107662.177700	35.799591
1360.362167	107836.129488	35.804608
1361.440058	108008.040408	35.809626
1363.062860	108170.979414	35.814644
1364.396385	108340.416566	35.819661
1365.750834	108511.472615	35.824679
1366.928268	108657.681142	35.829696
1368.200335	108817.200489	35.834714
1369.549690	108959.023570	35.839732
1370.934649	109123.453071	35.844749
1372.298270	109281.021293	35.849767
1373.948251	109430.510012	35.854784
1374.729019	109586.431590	35.859802
1376.382842	109746.448381	35.864820
1377.780199	109905.243197	35.869837
1378.940927	110065.130880	35.874855
1380.756486	110220.460879	35.879872
1381.642062	110395.422025	35.884890
1383.063625	110559.397772	35.889908
1384.466329	110734.006509	35.894925
1385.949330	110890.955405	35.899943
1387.484411	111059.297972	35.904960
1388.381950	111236.606054	35.909978
1389.970413	111406.753201	35.914996
1391.543952	111571.773082	35.920013
1393.010677	111739.219305	35.925031
1394.154581	111912.638180	35.930048
1395.816279	112092.253340	35.935066
1397.256573	112260.391334	35.940084
1398.559471	112436.940848	35.945101
1399.705694	112624.629229	35.950119
1401.098812	112790.726052	35.955136
1403.107057	112970.971665	35.960154
1404.827463	113129.729557	35.965172
1405.954196	113299.283065	35.970189
1407.170432	113466.807798	35.975207
1408.897249	113640.150222	35.980224
1409.902684	113823.030837	35.985242
1411.564509	113999.693403	35.990260
1412.689863	114176.474228	35.995277
1413.814970	114373.895691	36.000295
1415.228422	114545.181378	36.005312
1416.687458	114735.668319	36.010330
1418.339832	114919.889658	36.015348
1419.621317	115108.217512	36.020365
1420.982676	115294.011513	36.025383
1422.835962	115477.948650	36.030400
1424.096909	115667.994220	36.035418
1425.645537	115841.177793	36.040436
1426.844624	116032.110633	36.045453
1428.333653	116211.882771	36.050471
1429.816130	116394.571467	36.055488
1431.330935	116581.792009	36.060506
1432.674754	116755.294887	36.065524
1434.258049	116938.818729	36.070541
1436.259622	117127.682771	36.075559
1438.482997	117281.917346	36.080576
1440.318723	117449.764809	36.085594
1441.956738	117602.986191	36.090612
1443.552344	117762.690791	36.095629
1444.672211	117912.010947	36.100647
1446.045809	118054.635818	36.105664
1447.433111	118193.356151	36.110682
1448.671169	118323.169081	36.115700
1450.079947	118469.578816	36.120717
1451.195992	118610.210310	36.125735
1452.807609	118755.484303	36.130752
1453.778426	118912.400230	36.135770
1455.233757	119067.688076	36.140788
1456.791735	119207.714565	36.145805
1458.141890	119374.160855	36.150823
1459.408464	119524.807362	36.155840
1460.799654	119697.407186	36.160858
1462.003247	119856.848116	36.165876
1462.567794	120028.387462	36.170893
1464.266480	120214.079062	36.175911
1465.910484	120384.688041	36.180928
1466.838891	120575.519429	36.185946
1468.100320	120760.921768	36.190964
1469.604298	120960.768874	36.195981
1470.862322	121150.761808	36.200999
1472.083305	121350.343126	36.206016
1473.493693	121550.108801	36.211034
1474.609479	121756.554329	36.216052
1476.106914	121962.834571	36.221069
1477.868431	122176.446959	36.226087
1479.557820	122390.390043	36.231104
1481.377167	122592.944189	36.236122
1483.547619	122779.344042	36.241140
1485.571747	122965.694043	36.246157
1487.010190	123148.267235	36.251175
1488.773606	123340.734921	36.256192
1489.952054	123533.037783	36.261210
1491.603310	123712.929083	36.266228
1493.062071	123902.993695	36.271245
1494.837761	124092.688397	36.276263
1496.746580	124253.945740	36.281280
1498.373569	124449.967225	36.286298
1500.366557	124611.896466	36.291316
1502.230580	124767.587432	36.296333
1503.852026	124943.625351	36.301351
1505.613492	125110.463878	36.306368
1506.995128	125277.419010	36.311386
1508.143790	125443.515007	36.316404
1509.374563	125606.923453	36.321421
1510.644750	125783.444547	36.326439
1512.347778	125973.480156	36.331456
1513.205039	126153.851171	36.336474
1514.169182	126338.552511	36.341492
1515.586532	126523.367517	36.346509
1516.688604	126717.046898	36.351527
1518.228159	126920.564753	36.356544
1519.528800	127125.367014	36.361562
1521.073706	127324.196661	36.366580
1522.285264	127523.109967	36.371597
1523.535833	127729.559895	36.376615
1525.219700	127920.333144	36.381632
1526.698869	128121.295938	36.386650
1527.960468	128323.476107	36.391668
1529.287982	128515.556180	36.396685
1530.693259	128716.624136	36.401703
1532.001843	128911.523942	36.406720
1533.769121	129123.801649	36.411738
1535.183080	129337.193373	36.416756
1537.074591	129539.083345	36.421773
1538.736245	129739.163162	36.426791
1540.741432	129936.903659	36.431808
1542.382823	130142.567164	36.436826
1543.734727	130341.917803	36.441844
1545.235284	130544.286677	36.446861
1546.827828	130762.702719	36.451879
1548.520856	130955.660334	36.456896
1550.186077	131168.577556	36.461914
1551.470383	131377.631449	36.466932
1553.178025	131572.453788	36.471949
1554.470998	131790.775913	36.476967
1556.037403	131994.765295	36.481984
1557.570753	132215.521227	36.487002
1559.055221	132434.347353	36.492020
1560.955175	132649.744270	36.497037
1562.760960	132858.274717	36.502055
1564.434802	133067.653127	36.507072
1566.155067	133291.528430	36.512090
1567.638776	133503.325597	36.517108
1569.954350	133688.028248	36.522125
1571.728665	133899.245753	36.527143
1573.490852	134079.012077	36.532160
1575.372857	134275.088478	36.537178
1576.997097	134474.088131	36.542196
1578.460538	134663.531611	36.547213
1579.901800	134864.961137	36.552231
1581.094072	135062.111097	36.557248
1582.823681	135256.279543	36.562266
1584.348926	135453.717159	36.567284
1586.239712	135648.671741	36.572301
1587.407733	135855.808734	36.577319
1589.424328	136054.940854	36.582336
1591.316508	136241.619295	36.587354
1593.205138	136440.509336	36.592372
1594.812372	136624.664804	36.597389
1596.416592	136817.392947	36.602407
1598.279387	137001.773003	36.607424
1599.935499	137184.984888	36.612442
1601.271057	137370.002377	36.617460
1602.687499	137540.222735	36.622477
1603.995650	137739.967821	36.627495
1605.420737	137932.732943	36.632512
1606.940034	138130.846550	36.637530
1607.704231	138342.581808	36.642548
1609.408245	138546.866631	36.647565
1611.232133	138742.370316	36.652583
1612.924400	138934.296513	36.657600
1614.487729	139121.249890	36.662618
1615.915527	139318.663233	36.667636
1617.448450	139499.486667	36.672653
1618.782985	139698.997693	36.677671
1620.770099	139887.315567	36.682688
1622.339470	140071.407279	36.687706
1623.470322	140265.998366	36.692724
1625.387254	140465.502899	36.697741
1627.207987	140672.303722	36.702759
1628.434195	140881.566110	36.707776
1629.654648	141086.608026	36.712794
1631.160122	141301.620256	36.717812
1632.468916	141509.794380	36.722829
1634.005889	141731.524746	36.727847
1635.586601	141960.261671	36.732864
1637.563318	142191.772901	36.737882
1638.672452	142436.343631	36.742900
1640.530568	142659.292980	36.747917
1642.068341	142895.144835	36.752935
1643.602657	143129.553146	36.757952
1645.502620	143367.616139	36.762970
1646.702237	143608.742700	36.767988
1648.519782	143845.884525	36.773005
1650.105623	144093.276456	36.778023
1651.556208	144337.472011	36.783040
1653.590586	144576.458466	36.788058
1655.263631	144826.275441	36.793076
1657.810152	145060.751401	36.798093
1659.527602	145277.120929	36.803111
1661.844517	145508.874328	36.808128
1664.511697	145712.655233	36.813146
1666.372574	145930.779636	36.818164
1668.366028	146123.213124	36.823181
1670.227513	146338.854067	36.828199
1671.964138	146535.772586	36.833216
1674.068156	146726.731804	36.838234
1675.351535	146937.465467	36.843252
1677.070731	147128.074069	36.848269
1678.873971	147328.359069	36.853287
1680.176543	147524.342478	36.858304
1681.646892	147721.376278	36.863322
1683.132980	147939.513249	36.868340
1684.727037	148141.778944	36.873357
1686.106995	148356.169577	36.878375
1687.396912	148574.026726	36.883392
1689.234464	148787.339539	36.888410
1690.544520	149014.289847	36.893428
1691.995930	149238.236680	36.898445
1693.708458	149462.190899	36.903463
1695.431671	149692.473818	36.908480
1697.102157	149921.245094	36.913498
1698.478887	150151.323714	36.918516
1700.252191	150380.333833	36.923533
1701.974682	150605.713687	36.928551
1703.232201	150828.815167	36.933568
1704.835862	151037.233807	36.938586
1706.298915	151268.674265	36.943604
1708.434413	151490.449727	36.948621
1710.595972	151700.146412	36.953639
1712.272046	151917.931227	36.958656
1714.163059	152132.788405	36.963674
1715.475445	152355.343878	36.968692
1717.126958	152567.365016	36.973709
1718.536411	152784.718280	36.978727
1720.371328	153015.953315	36.983744
1722.451106	153227.600325	36.988762
1724.353973	153461.439458	36.993780
1726.265896	153682.961212	36.998797
1727.906151	153914.361687	37.003815
1729.056075	154140.227849	37.008832
1730.582747	154368.644012	37.013850
1731.937898	154609.205371	37.018868
1733.638638	154861.772930	37.023885
1735.407511	155108.013031	37.028903
1736.998594	155366.133434	37.033920
1739.067675	155605.081739	37.038938
1740.747262	155863.583454	37.043956
1742.718002	156105.050651	37.048973
1744.604995	156358.521825	37.053991
1746.167047	156609.995044	37.059008
1747.976094	156862.087239	37.064026
1749.607254	157124.334993	37.069044
1751.060342	157374.867427	37.074061
1752.867589	157641.008420	37.079079
1754.325277	157906.703486	37.084096
1755.918328	158175.548732	37.089114
1757.471888	158446.609950	37.094132
1758.826304	158710.957709	37.099149
1760.914480	158995.518468	37.104167
1762.995073	159270.338983	37.109184
1764.911677	159542.601234	37.114202
1767.020516	159818.651155	37.119220
1769.062917	160098.114395	37.124237
1770.984360	160356.704430	37.129255
1772.462532	160630.685381	37.134272
1774.485930	160899.766332	37.139290
1776.154689	161171.142644	37.144308
1777.502747	161441.928488	37.149325
1779.502054	161710.016372	37.154343
1781.346637	161994.233024	37.159360
1783.358172	162265.062819	37.164378
1785.093642	162541.371926	37.169396
1786.796419	162804.378803	37.174413
1789.089003	163077.297175	37.179431
1790.233019	163354.182105	37.184448
1792.655996	163612.173079	37.189466
1794.575761	163887.697934	37.194484
1796.191515	164163.860192	37.199501
1798.191403	164420.811741	37.204519
1799.934041	164678.138696	37.209536
1802.117660	164915.077426	37.214554
1803.674489	165154.890757	37.219572
1805.137894	165395.787210	37.224589
1807.330433	165637.384996	37.229607
1808.602628	165880.448479	37.234624
1810.832385	166127.739806	37.239642
1812.604340	166379.754953	37.244660
1814.037592	166630.154508	37.249677
1816.054247	166879.884641	37.254695
1817.717075	167136.427292	37.259712
1819.855564	167389.146710	37.264730
1821.953546	167643.765160	37.269748
1824.129897	167881.862805	37.274765
1826.137407	168121.855913	37.279783
1827.773411	168368.347387	37.284800
1829.944755	168608.010460	37.289818
1831.671548	168853.651489	37.294836
1833.102924	169094.534974	37.299853
1835.336174	169345.738872	37.304871
1837.275440	169593.365134	37.309888
1839.017371	169838.069729	37.314906
1840.764240	170093.269331	37.319924
1842.592308	170328.304711	37.324941
1845.406217	170552.005370	37.329959
1846.920501	170805.091309	37.334976
1848.974168	171031.310033	37.339994
1851.196373	171276.701349	37.345012
1852.321226	171518.791812	37.350029
1853.747301	171765.984266	37.355047
1855.431863	172029.618669	37.360064
1857.548866	172280.591550	37.365082
1859.052908	172533.485347	37.370100
1860.881111	172804.802601	37.375117
1862.610148	173063.219182	37.380135
1864.016659	173334.662294	37.385152
1866.429938	173595.248992	37.390170
1868.582817	173861.859049	37.395188
1870.782776	174112.344938	37.400205
1872.749027	174375.639285	37.405223
1874.304545	174646.264618	37.410240
1876.482957	174897.925761	37.415258
1878.779009	175180.065154	37.420276
1880.191701	175433.928663	37.425293
1882.485962	175692.287710	37.430311
1883.880618	175961.018597	37.435328
1885.734297	176218.440394	37.440346
1887.279482	176482.135152	37.445364
1888.849947	176751.779344	37.450381
1890.877834	177019.074900	37.455399
1892.912662	177293.160777	37.460416
1894.601489	177569.299928	37.465434
1896.341703	177842.004951	37.470452
1897.770654	178126.352450	37.475469
1900.073520	178391.247391	37.480487
1901.766991	178667.061617	37.485504
1903.671151	178913.573062	37.490522
1905.617998	179170.041785	37.495540
1907.528131	179433.448045	37.500557
1909.303221	179688.374829	37.505575
1911.094192	179950.788665	37.510592
1912.559158	180209.781818	37.515610
1914.486317	180488.269108	37.520628
1916.158527	180765.544890	37.525645
1917.981495	181044.611373	37.530663
1919.316265	181343.538142	37.535680
1921.201807	181634.464716	37.540698
1922.899079	181934.944734	37.545716
1924.830688	182238.369177	37.550733
1926.515442	182535.668706	37.555751
1928.493311	182854.041057	37.560768
1930.539669	183168.164004	37.565786
1932.677462	183475.723371	37.570804
1934.312011	183818.226420	37.575821
1936.451365	184151.556735	37.580839
1938.378686	184465.808903	37.585856
1940.721988	184776.665960	37.590874
1943.370529	185089.363865	37.595892
1945.425091	185390.994637	37.600909
1947.353013	185690.439950	37.605927
1949.150779	185991.203859	37.610944
1951.551437	186295.344345	37.615962
1953.808177	186603.166908	37.620980
1955.615890	186906.955041	37.625997
1957.664925	187214.143579	37.631015
1959.485480	187519.709871	37.636032
1961.207407	187825.738918	37.641050
1963.609768	188131.653165	37.646068
1965.634003	188440.858031	37.651085
1968.002649	188742.439717	37.656103
1970.082672	189043.285230	37.661120
1971.889643	189335.508574	37.666138
1973.970911	189635.836354	37.671156
1976.126609	189941.611597	37.676173
1978.698574	190236.285453	37.681191
1980.800105	190521.977107	37.686208
1982.676143	190807.886384	37.691226
1984.884750	191091.137647	37.696244
1987.050016	191379.780281	37.701261
1989.792209	191654.424526	37.706279
1991.978316	191915.784477	37.711296
1993.954743	192179.314159	37.716314
1996.494909	192432.478123	37.721332
1998.435250	192699.634274	37.726349
2001.229861	192939.667961	37.731367
2003.068630	193190.352376	37.736384
2004.680338	193440.873479	37.741402
2006.389383	193693.270529	37.746420
2008.064996	193956.224226	37.751437
2009.493939	194214.676176	37.756455
2011.150409	194474.385185	37.761472
2012.336043	194722.889337	37.766490
2014.450670	194976.758162	37.771508
2015.732428	195249.687046	37.776525
2017.659960	195513.949649	37.781543
2019.371057	195791.365114	37.786560
2020.781911	196076.742618	37.791578
2022.768902	196368.535815	37.796596
2024.334270	196664.820591	37.801613
2026.205051	196961.955845	37.806631
2028.290239	197273.135711	37.811648
2030.224699	197581.143333	37.816666
2032.569184	197889.551968	37.821684
2034.148978	198206.243772	37.826701
2036.505520	198522.004302	37.831719
2038.379305	198839.537441	37.836736
2039.837944	199175.565570	37.841754
2042.569394	199497.309870	37.846772
2043.954575	199832.769631	37.851789
2046.432129	200162.609980	37.856807
2048.181896	200500.676798	37.861824
2050.046159	200842.496545	37.866842
2052.532178	201183.500538	37.871860
2054.067260	201542.723698	37.876877
2056.230374	201885.944637	37.881895
2058.446913	202235.074822	37.886912
2060.089546	202593.281601	37.891930
2062.275844	202956.044247	37.896948
2064.190451	203316.734666	37.901965
2066.012824	203684.527619	37.906983
2068.116524	204049.569694	37.912000
2070.413200	204417.894498	37.917018
2073.308841	204778.233516	37.922036
2075.298790	205141.332062	37.927053
2077.998321	205497.492352	37.932071
2080.224896	205847.589490	37.937088
2082.272789	206197.147323	37.942106
2084.736734	206551.524130	37.947124
2086.880565	206904.649360	37.952141
2088.997868	207257.425112	37.957159
2091.572574	207598.391333	37.962176
2093.703321	207936.907996	37.967194
2095.836249	208278.498563	37.972212
2098.492713	208617.613760	37.977229
2100.976853	208934.639768	37.982247
2103.453910	209256.645823	37.987264
2105.661486	209578.546794	37.992282
2108.170681	209893.895905	37.997300
2110.483219	210207.375055	38.002317
2112.677489	210510.767715	38.007335
2114.594126	210834.323054	38.012352
2116.439572	211140.926713	38.017370
2118.598561	211453.674633	38.022388
2120.351587	211769.312122	38.027405
2122.258601	212069.660770	38.032423
2124.567733	212365.776517	38.037440
2125.996347	212669.739140	38.042458
2127.832210	212966.293308	38.047476
2130.177578	213260.094571	38.052493
2131.909316	213560.325648	38.057511
2134.364757	213876.637527	38.062528
2135.589280	214187.852858	38.067546
2137.835773	214489.014742	38.072564
2140.262260	214804.699696	38.077581
2142.375130	215118.813844	38.082599
2144.651669	215432.393053	38.087616
2146.752318	215755.425992	38.092634
2148.771347	216058.485652	38.097652
2150.762077	216396.956093	38.102669
2153.047029	216722.754429	38.107687
2154.874648	217051.984589	38.112704
2156.644919	217390.724613	38.117722
2158.960825	217734.579128	38.122740
2161.276436	218066.421302	38.127757
2163.353297	218406.788495	38.132775
2165.718109	218740.148285	38.137792
2168.117360	219081.122864	38.142810
2170.618179	219422.055750	38.147828
2172.790955	219760.023319	38.152845
2175.326505	220086.068537	38.157863
2177.475185	220426.251975	38.162880
2179.645590	220764.324595	38.167898
2181.834862	221105.747700	38.172916
2183.936878	221450.971247	38.177933
2185.699666	221794.780665	38.182951
2188.156664	222141.494927	38.187968
2189.950370	222491.904969	38.192986
2192.778275	222836.043284	38.198004
2194.974522	223178.969809	38.203021
2197.110921	223514.033602	38.208039
2199.466239	223854.801243	38.213056
2201.583910	224202.265236	38.218074
2204.195498	224542.355937	38.223092
2206.657090	224889.737618	38.228109
2208.843618	225221.927198	38.233127
2211.621535	225560.595158	38.238144
2213.471673	225898.355827	38.243162
2215.392059	226224.599000	38.248180
2217.496289	226579.920374	38.253197
2219.932351	226928.023014	38.258215
2222.472067	227267.802848	38.263232
2224.301824	227609.025741	38.268250
2226.666797	227945.154023	38.273268
2229.398340	228292.777742	38.278285
2231.427977	228635.340567	38.283303
2233.567922	228971.687539	38.288320
2235.719291	229312.173670	38.293338
2238.055249	229640.512773	38.298356
2240.260589	229988.078074	38.303373
2242.604922	230303.589684	38.308391
2245.440781	230609.314678	38.313408
2247.503293	230915.147101	38.318426
2249.849061	231204.090696	38.323444
2252.489682	231508.910974	38.328461
2254.117005	231800.950429	38.333479
2255.977821	232098.513373	38.338496
2257.788204	232421.232835	38.343514
2260.007162	232734.128911	38.348532
2261.807368	233057.638773	38.353549
2263.430173	233390.197113	38.358567
2265.708828	233719.875177	38.363584
2267.894738	234057.571220	38.368602
2270.110944	234397.472662	38.373620
2272.276858	234753.361011	38.378637
2274.096540	235119.800167	38.383655
2276.306364	235485.258863	38.388672
2278.498308	235847.241257	38.393690
2280.911202	236221.303253	38.398708
2282.992751	236592.069547	38.403725
2285.007651	236978.470143	38.408743
2287.529462	237348.832308	38.413760
2289.729786	237729.868165	38.418778
2292.172716	238125.418641	38.423796
2294.395144	238509.500343	38.428813
2296.598031	238900.698667	38.433831
2299.056987	239287.484689	38.438848
2301.241171	239687.248105	38.443866
2304.052692	240088.149645	38.448884
2306.625755	240479.007861	38.453901
2308.772532	240873.318093	38.458919
2311.752874	241253.032408	38.463936
2313.713082	241642.727051	38.468954
2316.275460	242025.130382	38.473972
2319.137590	242399.049339	38.478989
2321.316151	242791.121507	38.484007
2324.055666	243162.039505	38.489024
2326.463036	243553.463898	38.494042
2329.053348	243928.930014	38.499060
2331.445624	244300.594618	38.504077
2333.255550	244681.605810	38.509095
2335.578848	245054.527783	38.514112
2337.764637	245438.346067	38.519130
2339.960974	245832.171675	38.524148
2342.523491	246217.120298	38.529165
2344.943282	246602.042898	38.534183
2347.422568	246989.089540	38.539200
2349.636443	247376.918599	38.544218
2352.030998	247754.987780	38.549236
2354.334468	248140.922369	38.554253
2356.916368	248529.349970	38.559271
2359.815290	248902.227834	38.564288
2362.205984	249283.474243	38.569306
2364.768836	249656.181461	38.574324
2367.188806	250029.396006	38.579341
2369.533803	250401.328040	38.584359
2372.010856	250745.472125	38.589376
2373.883556	251095.155969	38.594394
2376.129276	251433.370208	38.599412
2378.484121	251778.704221	38.604429
2380.726669	252128.452321	38.609447
2383.147900	252483.479270	38.614464
2385.151400	252840.584615	38.619482
2387.084420	253203.798891	38.624500
2389.370111	253576.479181	38.629517
2391.259901	253950.548226	38.634535
2393.284149	254332.723400	38.639552
2395.613368	254721.400549	38.644570
2398.240865	255099.738483	38.649588
2400.665594	255489.085323	38.654605
2402.750876	255896.678935	38.659623
2405.674856	256280.885266	38.664640
2407.851193	256680.537561	38.669658
2410.423608	257078.775777	38.674676
2412.830106	257474.933877	38.679693
2414.665575	257896.745190	38.684711
2417.321165	258307.950132	38.689728
2419.581499	258729.510872	38.694746
2421.795336	259147.675446	38.699764
2424.661871	259571.672683	38.704781
2426.383243	259993.071209	38.709799
2428.984686	260420.161874	38.714816
2431.561175	260862.244502	38.719834
2434.010309	261292.383822	38.724852
2437.243570	261726.758229	38.729869
2439.214188	262154.489408	38.734887
2442.126965	262567.452502	38.739904
2444.941570	262999.459045	38.744922
2447.484167	263428.768269	38.749940
2450.005139	263842.712041	38.754957
2452.386839	264274.791683	38.759975
2455.315286	264689.046216	38.764992
2457.981201	265116.631056	38.770010
2460.338377	265534.462751	38.775028
2463.496918	265937.702808	38.780045
2466.226612	266347.391939	38.785063
2469.249070	266747.047292	38.790080
2472.081214	267154.025408	38.795098
2474.491114	267544.944475	38.800116
2477.107910	267927.749674	38.805133
2479.708184	268316.323728	38.810151
2482.530815	268696.832072	38.815168
2484.966293	269086.525752	38.820186
2487.133060	269471.971847	38.825204
2490.193530	269834.935764	38.830221
2492.153498	270225.090380	38.835239
2494.623543	270602.837038	38.840256
2496.806739	270995.060905	38.845274
2499.135780	271380.299008	38.850292
2502.082590	271772.975524	38.855309
2503.906069	272157.587685	38.860327
2506.085599	272524.178908	38.865344
2508.504798	272888.620246	38.870362
2510.608443	273263.428351	38.875380
2512.988596	273641.592534	38.880397
2515.245989	274005.678844	38.885415
2518.041305	274383.796288	38.890432
2520.347627	274755.239714	38.895450
2522.573601	275148.161082	38.900468
2525.137950	275533.250871	38.905485
2527.519218	275925.915681	38.910503
2529.113727	276319.831934	38.915520
2531.784581	276725.095954	38.920538
2534.479060	277142.852871	38.925556
2537.158617	277552.381263	38.930573
2539.879001	277969.700175	38.935591
2542.216070	278379.513977	38.940608
2544.556277	278796.438825	38.945626
2547.074879	279217.244092	38.950644
2549.715456	279641.659959	38.955661
2552.387049	280079.024282	38.960679
2554.779743	280516.181166	38.965696
2557.417614	280936.479315	38.970714
2559.523849	281381.684371	38.975732
2562.538672	281818.096506	38.980749
2565.064345	282264.395931	38.985767
2567.746720	282712.851820	38.990784
2570.585971	283144.921350	38.995802
2572.715974	283604.239120	39.000820
2575.750650	284035.231296	39.005837
2578.233438	284489.380491	39.010855
2580.589163	284947.715718	39.015872
2583.331476	285397.372598	39.020890
2585.780268	285852.717150	39.025908
2588.755874	286298.165594	39.030925
2591.437862	286754.788159	39.035943
2594.482606	287195.675194	39.040960
2597.282952	287640.971388	39.045978
2599.415278	288096.692712	39.050996
2602.645425	288543.410987	39.056013
2604.773129	289006.089506	39.061031
2607.198889	289452.332472	39.066048
2610.136634	289905.903072	39.071066
2612.160530	290368.518075	39.076084
2615.113951	290829.397672	39.081101
2617.864978	291293.485020	39.086119
2620.692831	291747.118265	39.091136
2623.466337	292207.083454	39.096154
2625.881584	292660.961429	39.101172
2628.455036	293114.150174	39.106189
2631.369159	293567.202667	39.111207
2633.747466	294023.164156	39.116224
2636.703744	294484.866681	39.121242
2639.173398	294945.024886	39.126260
2641.719402	295406.945956	39.131277
2644.304568	295857.682997	39.136295
2647.357070	296282.050945	39.141312
2650.005811	296698.130132	39.146330
2652.187849	297131.634305	39.151348
2654.824888	297551.318527	39.156365
2657.581916	297971.107470	39.161383
2659.682846	298412.213921	39.166400
2662.204548	298842.325469	39.171418
2664.360335	299290.606109	39.176436
2666.681421	299738.018286	39.181453
2669.496963	300191.566193	39.186471
2672.249101	300663.688096	39.191488
2675.359954	301104.914249	39.196506
2678.196222	301555.632875	39.201524
2681.181468	302009.371427	39.206541
2684.182921	302465.035070	39.211559
2686.862243	302923.011731	39.216576
2689.721390	303375.495051	39.221594
2692.053204	303833.627937	39.226612
2694.691463	304288.760074	39.231629
2697.175721	304762.048875	39.236647
2699.394289	305234.999504	39.241664
2702.309918	305709.148927	39.246682
2704.744085	306192.926670	39.251700
2707.567426	306662.743760	39.256717
2710.647590	307146.659437	39.261735
2713.448370	307627.496360	39.266752
2716.040244	308107.782012	39.271770
2718.535885	308587.674885	39.276788
2721.617193	309075.692619	39.281805
2724.591232	309552.196515	39.286823
2727.208394	310046.610690	39.291840
2730.644684	310519.779113	39.296858
2733.072558	311013.609894	39.301876
2735.714763	311501.077729	39.306893
2738.886502	311973.926683	39.311911
2741.355526	312464.414233	39.316928
2744.127302	312952.612142	39.321946
2746.758351	313449.007420	39.326964
2749.413601	313928.407205	39.331981
2752.624522	314407.759595	39.336999
2755.206657	314899.099955	39.342016
2758.617285	315382.093517	39.347034
2761.608939	315868.938773	39.352052
2764.344433	316357.728774	39.357069
2766.941565	316837.499387	39.362087
2769.704494	317324.398754	39.367104
2772.310587	317813.251159	39.372122
2774.715445	318306.501691	39.377140
2777.692326	318795.943683	39.382157
2780.289756	319294.562244	39.387175
2782.951993	319796.492112	39.392192
2785.580737	320285.880836	39.397210
2788.144818	320792.288464	39.402228
2790.930865	321296.267450	39.407245
2793.889373	321792.951397	39.412263
2796.292001	322270.328562	39.417280
2799.225479	322723.415023	39.422298
2801.903675	323204.901802	39.427316
2804.288625	323678.462683	39.432333
2806.765163	324157.869102	39.437351
2809.220309	324649.005020	39.442368
2812.051747	325131.948256	39.447386
2814.795068	325633.410798	39.452404
2817.425325	326128.947567	39.457421
2820.889825	326627.003344	39.462439
2823.354829	327130.125491	39.467456
2826.620733	327629.755257	39.472474
2829.435824	328131.945668	39.477492
2832.463440	328631.353537	39.482509
2835.788845	329133.828708	39.487527
2838.278840	329644.185067	39.492544
2841.543102	330139.959592	39.497562
2844.446784	330636.222864	39.502580
2847.373532	331143.495237	39.507597
2850.596300	331647.792971	39.512615
2853.276683	332151.137897	39.517632
2856.119977	332657.039593	39.522650
2859.276140	333155.369094	39.527668
2861.829594	333661.260043	39.532685
2864.988800	334159.528835	39.537703
2867.856224	334684.800880	39.542720
2871.115638	335180.250577	39.547738
2873.654506	335688.434406	39.552756
2876.940647	336192.855703	39.557773
2880.121132	336699.549201	39.562791
2882.889526	337217.045093	39.567808
2886.124380	337708.667086	39.572826
2889.162294	338206.282818	39.577844
2892.044646	338714.149234	39.582861
2894.970052	339211.342653	39.587879
2897.455543	339714.570943	39.592896
2901.101591	340209.194505	39.597914
2903.665548	340709.784857	39.602932
2906.816693	341222.503350	39.607949
2909.985658	341713.182884	39.612967
2912.425355	342231.189835	39.617984
2915.214248	342736.822108	39.623002
2917.786108	343248.983317	39.628020
2920.651813	343771.519772	39.633037
2923.500152	344285.906591	39.638055
2925.826459	344812.736509	39.643072
2928.728434	345336.010559	39.648090
2931.985656	345877.059016	39.653108
2934.483637	346406.709094	39.658125
2937.507791	346941.998496	39.663143
2940.347381	347487.464105	39.668160
2943.392962	348011.545616	39.673178
2946.611928	348553.279084	39.678196
2949.761646	349079.360372	39.683213
2953.093272	349592.843009	39.688231
2955.986462	350095.482828	39.693248
2958.695282	350571.960549	39.698266
2961.905509	351056.848165	39.703284
2964.715475	351545.681122	39.708301
2968.211730	352032.589643	39.713319
2970.900017	352518.920157	39.718336
2973.363480	352995.412893	39.723354
2976.279744	353485.880131	39.728372
2979.219471	353987.273728	39.733389
2982.232552	354496.032457	39.738407
2984.071242	355009.654258	39.743424
2987.140870	355521.942992	39.748442
2990.031232	356048.312341	39.753460
2992.635609	356585.938281	39.758477
2995.552498	357115.587729	39.763495
2998.379881	357664.933822	39.768512
3001.138534	358206.545975	39.773530
3004.121978	358769.449242	39.778548
3006.682188	359335.258355	39.783565
3009.823665	359905.501334	39.788583
3012.765068	360478.814609	39.793600
3015.744284	361048.789662	39.798618
3019.293330	361625.508652	39.803636
3022.166197	362208.499139	39.808653
3025.590877	362791.158232	39.813671
3028.526566	363385.916338	39.818688
3031.985270	363970.784009	39.823706
3034.737163	364552.110559	39.828724
3037.659037	365142.099859	39.833741
3040.899157	365733.090897	39.838759
3043.795589	366337.625888	39.843776
3046.724698	366928.600335	39.848794
3050.149972	367528.053922	39.853812
3052.727034	368132.309695	39.858829
3055.951413	368740.325600	39.863847
3059.663168	369342.439776	39.868864
3062.589427	369938.514813	39.873882
3065.656383	370539.958214	39.878900
3069.065923	371137.909039	39.883917
3072.381536	371731.884011	39.888935
3075.279929	372330.130297	39.893952
3078.802601	372931.962494	39.898970
3082.720254	373505.845429	39.903988
3086.031691	374101.226553	39.909005
3089.325405	374672.432512	39.914023
3092.461350	375259.099859	39.919040
3095.914705	375829.853563	39.924058
3099.327673	376395.355388	39.929076
3102.191016	376961.271338	39.934093
3106.130175	377519.665652	39.939111
3108.893226	378085.123434	39.944128
3112.322217	378639.757298	39.949146
3115.612801	379180.332718	39.954164
3118.193266	379742.471874	39.959181
3121.584426	380275.177210	39.964199
3124.427116	380806.598418	39.969216
3127.129021	381313.390137	39.974234
3130.135833	381829.122732	39.979252
3133.309398	382351.258580	39.984269
3136.425277	382865.257332	39.989287
3139.206731	383374.259707	39.994304
3142.429605	383899.734006	39.999322
3145.536031	384425.726597	40.004340
3148.314333	384954.200328	40.009357
3151.367205	385490.223811	40.014375
3154.126804	386024.133433	40.019392
3157.314368	386557.935529	40.024410
3160.695917	387113.927554	40.029428
3163.037932	387667.755032	40.034445
3166.283860	388217.818622	40.039463
3169.504476	388793.504456	40.044480
3172.219291	389358.239351	40.049498
3175.735492	389932.864730	40.054516
3178.679954	390520.428084	40.059533
3181.839438	391091.189000	40.064551
3185.332148	391683.376026	40.069568
3188.550124	392267.386226	40.074586
3191.660499	392854.546255	40.079604
3194.956366	393456.033638	40.084621
3198.034432	394043.936063	40.089639
3201.071977	394646.710616	40.094656
3203.914226	395251.153502	40.099674
3207.444124	395860.180249	40.104692
3210.615937	396467.228050	40.109709
3214.075959	397073.681759	40.114727
3217.235113	397699.788296	40.119744
3220.377864	398321.930863	40.124762
3223.880543	398936.041630	40.129780
3226.898805	399562.460962	40.134797
3230.495122	400169.104622	40.139815
3233.867206	400786.314401	40.144832
3237.024958	401406.055719	40.149850
3240.885178	402011.879803	40.154868
3244.129577	402643.360819	40.159885
3247.646240	403258.363074	40.164903
3250.762741	403874.737466	40.169920
3253.695855	404490.420013	40.174938
3257.044713	405102.141552	40.179956
3260.225353	405734.221350	40.184973
3263.314873	406349.125965	40.189991
3266.543483	406985.576467	40.195008
3269.946209	407612.127977	40.200026
3273.142215	408245.539733	40.205044
3276.863403	408888.168628	40.210061
3279.858648	409518.038138	40.215079
3283.185197	410145.556430	40.220096
3287.025101	410762.891102	40.225114
3290.356781	411376.524115	40.230132
3293.840222	412001.818408	40.235149
3297.416255	412597.448771	40.240167
3300.962102	413166.452056	40.245184
3303.872784	413735.323377	40.250202
3307.611927	414296.088368	40.255220
3310.704339	414871.133722	40.260237
3313.863675	415427.110571	40.265255
3316.818626	415993.467792	40.270272
3319.890978	416569.921784	40.275290
3323.165841	417134.806117	40.280308
3326.001198	417730.165097	40.285325
3328.713023	418312.844862	40.290343
3332.406871	418913.853188	40.295360
3335.087896	419522.236384	40.300378
3338.662901	420126.350202	40.305396
3341.970528	420745.889119	40.310413
3344.825581	421360.046256	40.315431
3348.133630	421982.718848	40.320448
3351.270539	422623.228304	40.325466
3354.661512	423257.348380	40.330484
3357.792458	423913.268148	40.335501
3361.084482	424560.636677	40.340519
3364.348224	425220.396866	40.345536
3367.689991	425888.529861	40.350554
3371.127199	426544.831912	40.355572
3374.487329	427211.051591	40.360589
3377.571015	427888.133263	40.365607
3381.358314	428564.214817	40.370624
3384.278591	429248.777454	40.375642
3387.894803	429930.670309	40.380660
3391.611193	430621.232422	40.385677
3395.013528	431311.979518	40.390695
3398.260554	432008.553251	40.395712
3401.677069	432701.129187	40.400730
3404.909429	433391.843071	40.405748
3408.476946	434094.574731	40.410765
3412.145808	434799.342385	40.415783
3415.716764	435491.908583	40.420800
3419.210633	436205.771666	40.425818
3423.005742	436898.205842	40.430836
3426.582226	437606.190908	40.435853
3430.192754	438297.196486	40.440871
3434.280244	438989.414754	40.445888
3437.716164	439689.565305	40.450906
3441.717093	440365.867656	40.455924
3445.210749	441056.857648	40.460941
3448.632957	441727.398539	40.465959
3452.257922	442396.315896	40.470976
3455.863455	443098.706436	40.475994
3459.850317	443768.379769	40.481012
3463.041465	444448.538459	40.486029
3466.579699	445118.904077	40.491047
3470.276244	445780.521358	40.496064
3473.335151	446461.599874	40.501082
3477.102216	447126.906402	40.506100
3480.214394	447791.899256	40.511117
3483.666664	448441.663544	40.516122
3486.803649	449050.407709	40.521127
3489.994968	449634.990068	40.526132
3493.012426	450154.585536	40.531136
3495.853378	450616.449643	40.536141
3498.167972	451020.189634	40.541146
3500.876912	451378.478603	40.546151
3503.170718	451688.871476	40.551156
3505.501297	451941.964819	40.556160
3507.409608	452139.664217	40.561165
3509.200981	452300.879836	40.566170
3510.966135	452426.154702	40.571175
3512.008050	452515.811271	40.576180
3513.471474	452559.312478	40.581184
3514.283375	452572.050757	40.586189
3515.169699	452568.604174	40.591194
3516.074183	452529.819062	40.596199
3517.041853	452470.997926	40.601204
3517.707068	452390.834211	40.606208
3517.946534	452287.878505	40.611213
3518.511644	452162.002172	40.616218
3518.802607	452012.343947	40.621223
3519.246885	451871.175748	40.626228
3519.471549	451704.187857	40.631232
3519.514075	451536.165044	40.636237
3519.662219	451346.778405	40.641242
3520.259314	451151.888500	40.646247
3519.700966	450958.867166	40.651252
3519.791451	450751.131419	40.656256
3519.505745	450542.088899	40.661261
3519.306868	450324.815754	40.666266
3519.475376	450110.773277	40.671271
3519.316656	449901.499852	40.676276
3519.369778	449673.377190	40.681280
3519.207188	449461.159226	40.686285
3518.631278	449251.037867	40.691290
3519.122145	449015.785390	40.696295
3518.372688	448804.015926	40.701300
3518.489820	448594.733079	40.706304
3518.242596	448386.118846	40.711309
3517.662427	448178.218590	40.716314
3517.847949	447956.342382	40.721319
3517.373550	447749.687539	40.726324
3517.395312	447543.960134	40.731328
3516.913991	447325.284396	40.736333
3516.217423	447130.628794	40.741338
3516.376091	446939.324372	40.746343
3515.924632	446737.726755	40.751348
3515.654956	446552.374408	40.756352
3515.625159	446358.865668	40.761357
3515.357073	446176.653890	40.766362
3515.207000	445992.138355	40.771367
3514.896927	445816.776832	40.776372
3514.985136	445627.501184	40.781376
3514.534988	445456.876950	40.786381
3513.881345	445284.967541	40.791386
3513.846575	445110.415365	40.796391
3513.275975	444956.239162	40.801396
3513.394538	444786.222496	40.806400
3513.209256	444643.642736	40.811405
3512.839141	444488.465353	40.816410
3513.026923	444334.611646	40.821415
3512.287967	444182.030843	40.826420
3512.117447	444025.243832	40.831424
3512.058974	443887.911981	40.836429
3511.522481	443747.972846	40.841434
3511.407297	443631.646114	40.846439
3511.034810	443500.299405	40.851444
3511.242579	443381.735307	40.856448
3511.268676	443258.839772	40.861453
3510.921119	443127.892298	40.866458
3510.933097	442998.657822	40.871463
3510.668707	442876.114035	40.876468
3510.618286	442753.989502	40.881472
3510.457290	442647.048491	40.886477
3510.083675	442538.621647	40.891482
3509.811402	442413.997067	40.896487
3509.670312	442312.782452	40.901492
3509.453845	442217.463891	40.906496
3509.407646	442115.369899	40.911501
3509.249069	442018.468221	40.916506
3509.309698	441911.435038	40.921511
3508.875511	441815.188180	40.926516
3509.253169	441718.802278	40.931520
3509.018171	441625.462467	40.936525
3508.887978	441541.995294	40.941530
3508.524783	441454.002525	40.946535
3508.253068	441374.210925	40.951540
3508.544476	441282.250739	40.956544
3508.340078	441200.620974	40.961549
3507.922536	441110.150652	40.966554
3508.255670	441025.435754	40.971559
3507.910491	440955.495610	40.976564
3507.698687	440874.322413	40.981568
3507.699807	440804.931351	40.986573
3507.377964	440738.131444	40.991578
3507.335661	440662.761847	40.996583
3507.092164	440594.375659	41.001588
3507.113322	440525.944069	41.006592
3506.934663	440459.473942	41.011597
3506.792550	440409.077309	41.016602
3507.086142	440338.924684	41.021607
3506.503304	440287.182711	41.026612
3506.912354	440226.089896	41.031616
3506.768306	440168.185630	41.036621
3506.574931	440107.702608	41.041626
3506.507620	440046.081920	41.046631
3506.403280	439997.504038	41.051636
3506.575491	439940.965512	41.056640
3506.326687	439893.020784	41.061645
3506.207545	439841.097136	41.066650
3506.413565	439789.117845	41.071655
3506.222749	439739.438172	41.076660
3506.038832	439681.590165	41.081664
3506.172035	439631.956380	41.086669
3506.281558	439590.797972	41.091674
3506.646258	439532.957356	41.096679
3506.770308	439487.078632	41.101684
3506.290580	439422.330796	41.106688
3506.272659	439371.352586	41.111693
3505.655590	439324.179693	41.116698
3506.183159	439258.041915	41.121703
3506.029412	439227.885024	41.126708
3505.954134	439176.053782	41.131712
3506.406042	439123.422208	41.136717
3505.878035	439084.197934	41.141722
3506.033609	439031.007998	41.146727
3505.602241	438991.513417	41.151732
3505.241175	438949.571786	41.156736
3505.113368	438912.409479	41.161741
3505.389181	438878.323380	41.166746
3505.576566	438835.983514	41.171751
3505.301388	438805.491681	41.176756
3505.442416	438776.298424	41.181760
3505.658544	438728.576164	41.186765
3505.425654	438698.279879	41.191770
3505.495573	438649.922936	41.196775
3505.462593	438615.889161	41.201780
3505.312906	438571.424981	41.206784
3505.405720	438529.810894	41.211789
3505.211670	438507.218619	41.216794
3504.991704	438469.411822	41.221799
3504.774574	438440.685118	41.226804
3504.364008	438402.301993	41.231808
3504.812767	438380.208591	41.236813
3504.874857	438354.477897	41.241818
3504.865798	438317.801621	41.246823
3504.458088	438297.274820	41.251828
3504.789683	438268.707852	41.256832
3505.078048	438237.459522	41.261837
3504.605627	438216.132011	41.266842
3504.795429	438180.892735	41.271847
3504.669451	438161.839616	41.276852
3504.431789	438134.536476	41.281856
3504.677234	438103.396749	41.286861
3504.851789	438083.429828	41.291866
3504.891267	438046.288242	41.296871
3504.943322	438034.459109	41.301876
3504.999769	438000.967165	41.306880
3505.170229	437965.020619	41.311885
3504.730814	437930.547887	41.316890
3504.916005	437903.273725	41.321895
3504.664294	437880.944316	41.326900
3504.610821	437852.188910	41.331904
3504.518712	437824.556151	41.336909
3504.274962	437793.753178	41.341914
3504.863449	437770.367033	41.346919
3504.652615	437751.023664	41.351924
3504.676131	437720.124223	41.356928
3504.693762	437694.552556	41.361933
3504.552805	437664.594289	41.366938
3504.754385	437634.019447	41.371943
3504.681874	437620.080634	41.376948
3504.011359	437592.241959	41.381952
3504.315516	437569.360739	41.386957
3504.112943	437553.161161	41.391962
3504.255032	437523.661694	41.396967
3503.983435	437523.961747	41.401972
3503.936719	437493.124717	41.406976
3504.372036	437481.280582	41.411981
3504.437378	437466.607887	41.416986
3504.298169	437442.483209	41.421991
3504.664647	437430.549338	41.426996
3504.449183	437396.037542	41.432000
3504.464619	437378.684504	41.437005
3504.469886	437354.230668	41.442010
3504.687549	437326.037077	41.447015
3504.633705	437307.630434	41.452020
3504.319673	437286.427185	41.457024
3504.328351	437259.740436	41.462029
3504.294414	437244.120630	41.467034
3504.534491	437215.567945	41.472039
3504.622735	437197.187683	41.477044
3504.325550	437164.160730	41.482048
3504.174250	437142.371499	41.487053
3504.088236	437131.275723	41.492058
3504.076300	437105.809898	41.497063
3503.893835	437094.375442	41.502068
3503.916834	437082.855165	41.507072
3503.950473	437065.650976	41.512077
3503.773234	437053.150215	41.517082
3504.305948	437032.055810	41.522087
3504.487782	437018.022461	41.527092
3504.534511	437009.694277	41.532096
3504.576875	436972.093820	41.537101
3504.374479	436954.321050	41.542106
3504.488934	436921.020519	41.547111
3504.500839	436906.407316	41.552116
3504.502943	436879.569038	41.557120
3504.061738	436850.421950	41.562125
3504.241179	436835.120559	41.567130
3504.334476	436812.020906	41.572135
3503.934035	436799.405914	41.577140
3503.767714	436772.647000	41.582144
3504.116346	436763.607639	41.587149
3503.739903	436746.929829	41.592154
3503.988811	436732.073110	41.597159
3503.988722	436729.434991	41.602164
3504.020486	436712.788922	41.607168
3504.025662	436682.601457	41.612173
3503.917766	436676.278170	41.617178
3504.033377	436657.537657	41.622183
3504.295293	436653.637179	41.627188
3504.222254	436627.775374	41.632192
3504.193806	436609.059419	41.637197
3503.626032	436594.544992	41.642202
3504.100499	436578.837914	41.647207
3504.052241	436566.974402	41.652212
3503.841581	436542.150679	41.657216
3504.131761	436528.047790	41.662221
3503.966509	436514.022657	41.667226
3503.823317	436500.501091	41.672231
3503.880567	436482.429942	41.677236
3504.024133	436466.677819	41.682240
3504.173034	436443.821965	41.687245
3503.968573	436437.007756	41.692250
3503.984108	436405.803463	41.697255
3503.828558	436401.872755	41.702260
3503.852083	436390.859378	41.707264
3503.884371	436361.021993	41.712269
3503.847940	436365.492871	41.717274
3504.098769	436332.066716	41.722279
3504.057110	436321.622516	41.727284
3503.818677	436302.992895	41.732288
3503.797059	436295.132730	41.737293
3503.849487	436284.368039	41.742298
3503.531653	436260.120387	41.747303
3503.659617	436258.221369	41.752308
3503.837099	436236.425855	41.757312
3503.863352	436228.456023	41.762317
3503.770951	436216.599863	41.767322
3503.991031	436190.941182	41.772327
3504.234457	436194.501815	41.777332
3503.807387	436176.563853	41.782336
3503.893057	436161.430221	41.787341
3503.866683	436151.642888	41.792346
3504.039771	436123.455403	41.797351
3503.797033	436111.675593	41.802356
3503.960166	436093.027967	41.807360
3504.274751	436085.008852	41.812365
3503.613796	436067.161473	41.817370
3503.861368	436055.957472	41.822375
3503.889942	436047.733503	41.827380
3504.036770	436018.231255	41.832384
3503.984765	436002.258524	41.837389
3503.812479	435985.190142	41.842394
3503.808421	435969.970232	41.847399
3503.983780	435951.066725	41.852404
3503.752806	435955.063547	41.857408
3504.077224	435936.388253	41.862413
3503.921662	435920.077998	41.867418
3503.865824	435907.302193	41.872423
3503.698022	435886.377068	41.877428
3503.784616	435876.367383	41.882432
3503.935613	435861.425339	41.887437
3503.877138	435842.206518	41.892442
3504.207039	435821.094878	41.897447
3503.857425	435812.377306	41.902452
3503.800792	435794.933881	41.907456
3503.757147	435775.103641	41.912461
3503.882253	435769.704296	41.917466
3504.084447	435755.159327	41.922471
3503.934624	435744.834801	41.927476
3503.738647	435728.429837	41.932480
3504.044650	435706.662604	41.937485
3503.677699	435697.136171	41.942490
3504.110185	435677.833379	41.947495
3503.795924	435670.682533	41.952500
3503.711713	435641.523659	41.957504
3504.047955	435630.050627	41.962509
3504.052824	435624.468833	41.967514
3504.024198	435600.475507	41.972519
3504.128819	435599.037046	41.977524
3504.320365	435572.570756	41.982528
3504.491432	435556.255204	41.987533
3504.318328	435540.099879	41.992538
3504.466912	435508.262792	41.997543
3504.413137	435494.319463	42.002548
3504.283261	435467.146885	42.007552
3504.238940	435442.141340	42.012557
3504.071889	435424.970167	42.017562
3504.306637	435409.709105	42.022567
3503.818802	435390.867633	42.027572
3503.743507	435368.099710	42.032576
3503.992493	435337.462922	42.037581
3503.795672	435344.193809	42.042586
3504.206699	435302.925309	42.047591
3504.250758	435297.336743	42.052596
3504.082378	435283.159168	42.057600
3503.725604	435265.715847	42.062605
3503.817533	435244.035461	42.067610
3503.822945	435222.623512	42.072615
3503.994266	435217.013196	42.077620
3503.578612	435201.355679	42.082624
3503.927697	435191.300872	42.087629
3503.402931	435178.503250	42.092634
3503.375379	435159.735204	42.097639
3503.569942	435156.099657	42.102644
3503.875406	435154.068766	42.107648
3503.739071	435126.896882	42.112653
3503.501048	435111.564133	42.117658
3503.646800	435098.043127	42.122663
3503.505075	435095.023103	42.127668
3503.694125	435086.365485	42.132672
3504.105681	435073.002029	42.137677
3503.843846	435061.123456	42.142682
3503.900174	435047.059577	42.147687
3503.629281	435034.878113	42.152692
3503.752137	435019.838845	42.157696
3503.713752	435012.589947	42.162701
3503.625988	434991.751803	42.167706
3503.778258	434979.447317	42.172711
3503.772217	434977.672549	42.177716
3503.754841	434946.421126	42.182720
3504.120770	434936.617020	42.187725
3503.710620	434927.300588	42.192730
3503.565447	434899.165924	42.197735
3503.860610	434906.218837	42.202740
3503.660590	434892.350847	42.207744
3503.487680	434879.492977	42.212749
3503.532433	434876.441082	42.217754
3503.242155	434846.656779	42.222759
3503.212618	434836.767942	42.227764
3503.527005	434832.959670	42.232768
3503.827985	434823.369557	42.237773
3503.481015	434825.001698	42.242778
3503.740171	434803.748979	42.247783
3503.391755	434799.089852	42.252788
3503.757583	434794.004339	42.257792
3503.663593	434768.245462	42.262797
3503.351527	434776.366123	42.267802
3503.511410	434760.356337	42.272807
3503.449629	434735.708162	42.277812
3503.002770	434738.625819	42.282816
3503.605564	434733.347617	42.287821
3503.293498	434748.317942	42.292826
3503.446892	434727.133949	42.297831
3503.605870	434701.078110	42.302836
3503.583182	434703.974083	42.307840
3503.993910	434699.692695	42.312845
3503.810274	434678.616943	42.317850
3503.912908	434667.792174	42.322855
3503.751016	434640.522596	42.327860
3503.556640	434634.416458	42.332864
3503.929167	434623.748538	42.337869
3503.579172	434613.001029	42.342874
3503.638381	434610.555492	42.347879
3503.612376	434604.775766	42.352884
3503.633044	434587.977814	42.357888
3503.807081	434566.181285	42.362893
3503.704929	434556.051031	42.367898
3503.963430	434540.683854	42.372903
3503.978171	434535.150846	42.377908
3503.765393	434505.708034	42.382912
3504.806287	434494.317067	42.387917
3504.305729	434487.248395	42.392922
3504.138531	434463.125312	42.397927
3504.147896	434438.008017	42.402932
3503.973390	434414.190563	42.407936
3503.834353	434394.375404	42.412941
3503.595992	434387.058974	42.417946
3504.011714	434367.707197	42.422951
3503.844392	434358.450546	42.427956
3503.873024	434349.160433	42.432960
3503.667119	434324.637900	42.437965
3503.861829	434318.820414	42.442970
3503.703598	434289.266530	42.447975
3503.620123	434280.198488	42.452980
3503.799004	434269.005337	42.457984
3503.959667	434252.792105	42.462989
3503.489915	434258.098476	42.467994
3503.824246	434240.384144	42.472999
3503.806924	434215.575596	42.478004
3503.588029	434210.082402	42.483008
3503.534600	434196.594872	42.488013
3503.381534	434188.249027	42.493018
3503.404026	434173.581513	42.498023
3503.623285	434174.609622	42.503028
3503.545862	434155.392608	42.508032
3503.404064	434132.584064	42.513037
3503.155776	434142.266985	42.518042
3503.397586	434135.223662	42.523047
3503.750063	434134.706840	42.528052
3503.376879	434117.011740	42.533056
3503.698735	434097.320585	42.538061
3503.077931	434103.464616	42.543066
3503.217435	434095.170260	42.548071
3503.661298	434080.481478	42.553076
3503.500163	434058.589475	42.558080
3503.850559	434055.028625	42.563085
3503.436267	434052.968316	42.568090
3503.381028	434026.237929	42.573095
3503.554478	434026.208331	42.578100
3503.504022	434025.506608	42.583104
3503.561831	433996.473593	42.588109
3503.512867	433990.900591	42.593114
3503.530192	433989.933594	42.598119
3503.416676	433984.625311	42.603124
3503.312571	433965.057514	42.608128
3503.629581	433958.254997	42.613133
3503.473645	433957.520542	42.618138
3503.720914	433937.639025	42.623143
3503.889153	433932.130401	42.628148
3503.618148	433926.646036	42.633152
3503.576164	433903.972440	42.638157
3503.376022	433898.120788	42.643162
3503.728853	433887.608110	42.648167
3503.627155	433876.462675	42.653172
3503.392990	433854.633687	42.658176
3503.443328	433855.842874	42.663181
3503.555538	433863.130311	42.668186
3503.967628	433837.537670	42.673191
3503.904321	433822.377180	42.678196
3503.612754	433813.141522	42.683200
3503.968431	433784.615521	42.688205
3503.861274	433781.741639	42.693210
3503.800078	433754.250846	42.698215
3503.845213	433746.378400	42.703220
3503.513326	433735.272201	42.708224
3503.861600	433708.827726	42.713229
3503.480905	433699.252058	42.718234
3503.553838	433700.152952	42.723239
3503.878689	433678.532786	42.728244
3503.636022	433671.216862	42.733248
3503.852370	433653.167038	42.738253
3503.393021	433640.103673	42.743258
3503.482644	433630.396929	42.748263
3503.448825	433628.626800	42.753268
3503.489051	433610.251830	42.758272
3503.613088	433589.832905	42.763277
3503.253205	433597.657703	42.768282
3503.329004	433598.456631	42.773287
3503.668268	433574.246130	42.778292
3503.435525	433559.723286	42.783296
3503.436665	433549.676430	42.788301
3503.398689	433552.575159	42.793306
3503.367199	433540.098311	42.798311
3503.397553	433526.240894	42.803316
3503.816721	433527.437862	42.808321
3503.616134	433505.298361	42.813325
3503.338075	433494.842486	42.818330
3503.556113	433483.693006	42.823335
3503.754589	433479.346153	42.828340
3503.738073	433473.868966	42.833345
3503.340863	433448.211114	42.838349
3503.164602	433461.636860	42.843354
3503.657665	433446.127415	42.848359
3503.727563	433426.833893	42.853364
3503.165947	433427.792405	42.858369
3503.610791	433412.595618	42.863373
3503.621579	433410.767114	42.868378
3503.507291	433383.792353	42.873383
3503.482488	433383.695124	42.878388
3503.625614	433378.393620	42.883393
3503.530846	433357.402956	42.888397
3503.339777	433352.158509	42.893402
3503.386822	433341.393346	42.898407
3503.221163	433345.277987	42.903412
3503.368266	433337.540214	42.908417
3503.375704	433324.802896	42.913421
3503.274166	433323.856167	42.918426
3503.421197	433321.446238	42.923431
3503.285387	433320.556102	42.928436
3503.451577	433302.819015	42.933441
3503.175811	433277.799873	42.938445
3503.194955	433288.756766	42.943450
3503.235052	433285.908420	42.948455
3503.170508	433286.325390	42.953460
3503.062056	433290.961394	42.958465
3503.276915	433274.839699	42.963469
3503.005116	433262.403733	42.968474
3503.219153	433254.705244	42.973479
3503.524462	433253.232370	42.978484
3503.414464	433258.579025	42.983489
3503.657422	433241.640646	42.988493
3503.495538	433231.976677	42.993498
3503.479070	433222.186392	42.998503
3503.459252	433219.754200	43.003508
3503.381816	433204.798680	43.008513
3503.678678	433187.089933	43.013517
3503.303354	433184.058798	43.018522
3503.404805	433174.045391	43.023527
3503.637073	433151.121256	43.028532
3503.528907	433148.145983	43.033537
3503.444313	433135.880950	43.038541
3503.413691	433136.444356	43.043546
3503.245165	433115.313839	43.048551
3503.733997	433100.667495	43.053556
3503.398538	433105.088588	43.058561
3503.701066	433091.844078	43.063565
3503.336934	433084.903898	43.068570
3503.745577	433066.161134	43.073575
3503.928607	433072.168184	43.078580
3503.218369	433040.271331	43.083585
3503.834673	433030.829597	43.088589
3503.660678	433019.290154	43.093594
3503.497348	433001.050937	43.098599
3503.429320	432988.478544	43.103604
3503.552320	432994.749575	43.108609
3503.736397	432968.180058	43.113613
3503.553597	432962.477431	43.118618
3503.741588	432953.463994	43.123623
3503.908544	432932.935674	43.128628
3503.745330	432921.698794	43.133633
3503.720779	432916.324330	43.138637
3503.536324	432903.670286	43.143642
3503.607452	432890.668141	43.148647
3503.935830	432878.383198	43.153652
3503.601465	432861.898313	43.158657
3503.760903	432843.299405	43.163661
3503.627080	432833.528992	43.168666
3503.319814	432812.523371	43.173671
3503.521447	432806.653578	43.178676
3503.377422	432808.098978	43.183681
3503.784022	432785.601393	43.188685
3503.313143	432775.330340	43.193690
3503.269155	432761.891096	43.198695
3503.427024	432754.151288	43.203700
3503.036551	432768.527381	43.208705
3503.402711	432758.367110	43.213709
3503.323510	432744.781640	43.218714
3503.081825	432739.241240	43.223719
3503.248255	432734.189322	43.228724
3503.386380	432740.051899	43.233729
3503.476405	432729.735794	43.238733
3503.305401	432710.076863	43.243738
3503.667805	432699.409780	43.248743
3503.780694	432690.662778	43.253748
3503.874083	432682.426529	43.258753
3503.973401	432665.207796	43.263757
3503.791170	432644.941813	43.268762
3503.474502	432632.310195	43.273767
3503.638471	432619.241301	43.278772
3503.297662	432614.478939	43.283777
3503.585724	432585.962997	43.288781
3503.170669	432586.693544	43.293786
3503.614694	432583.826883	43.298791
3503.617989	432578.346100	43.303796
3503.697773	432557.121927	43.308801
3503.734185	432541.588362	43.313805
3503.874929	432540.549488	43.318810
3503.793454	432516.054515	43.323815
3503.596639	432512.992810	43.328820
3503.652977	432495.324601	43.333825
3503.815926	432465.206091	43.338829
3503.703014	432468.117752	43.343834
3503.112273	432451.879321	43.348839
3503.652818	432437.172984	43.353844
3503.205162	432433.798896	43.358849
3503.354073	432427.887267	43.363853
3503.425829	432426.657194	43.368858
3503.274109	432404.203828	43.373863
3503.363492	432388.661115	43.378868
3503.267362	432393.548912	43.383873
3503.536777	432387.413723	43.388877
3503.475912	432380.624519	43.393882
3503.050938	432365.068130	43.398887
3503.427649	432343.488600	43.403892
3503.503200	432355.755637	43.408897
3503.700402	432341.919761	43.413901
3503.530920	432322.564699	43.418906
3503.448838	432317.910328	43.423911
3503.438084	432315.121289	43.428916
3503.332201	432289.767602	43.433921
3503.680570	432282.096596	43.438925
3503.601963	432280.334010	43.443930
3503.305747	432282.059146	43.448935
3503.560547	432253.700703	43.453940
3503.319576	432243.491643	43.458945
3503.470611	432236.970677	43.463949
3503.266380	432240.253166	43.468954
3503.664782	432219.735435	43.473959
3504.094954	432208.498374	43.478964
3503.621979	432197.161800	43.483969
3503.841959	432171.650855	43.488973
3503.866169	432166.775329	43.493978
3503.643055	432158.542192	43.498983
3503.888836	432142.871121	43.503988
3503.837083	432145.112709	43.508993
3503.487311	432110.869538	43.513997
3503.574532	432108.063744	43.519002
3503.194032	432101.785732	43.524007
3503.541353	432092.440290	43.529012
3503.157598	432073.476815	43.534017
3503.351029	432058.829508	43.539021
3503.355018	432062.736141	43.544026
3503.202902	432063.066598	43.549031
3503.117222	432058.970974	43.554036
3503.195676	432043.023942	43.559041
3503.304708	432027.071678	43.564045
3503.014718	432029.150979	43.569050
3503.263867	432028.601013	43.574055
3503.244873	432026.878973	43.579060
3502.889586	432024.808401	43.584065
3503.399806	432023.097486	43.589069
3503.098959	432012.594082	43.594074
3502.809151	432007.873628	43.599079
3503.229765	431991.868138	43.604084
3503.106762	431999.957494	43.609089
3503.656718	432000.675515	43.614093
3503.254924	432002.520188	43.619098
3503.732558	431978.741084	43.624103
3503.580590	431960.905057	43.629108
3503.037022	431960.947145	43.634113
3503.345172	431958.103609	43.639117
3503.252826	431941.272273	43.644122
3503.250503	431924.730020	43.649127
3503.647872	431914.259584	43.654132
3503.501708	431920.576868	43.659137
3503.559706	431900.066233	43.664141
3503.874986	431884.789077	43.669146
3503.202009	431879.626578	43.674151
3503.453422	431870.754124	43.679156
3503.559372	431866.321278	43.684161
3503.523218	431846.232628	43.689165
3503.366216	431853.312949	43.694170
3503.449317	431838.481363	43.699175
3503.446334	431817.067664	43.704180
3503.013312	431808.159819	43.709185
3503.176865	431799.962020	43.714189
3503.166250	431798.593744	43.719194
3502.887151	431797.220568	43.724199
3503.308990	431792.733770	43.729204
3503.253782	431789.444810	43.734209
3503.151560	431770.940462	43.739213
3503.207468	431766.972844	43.744218
3503.183975	431766.520171	43.749223
3503.160971	431760.434747	43.754228
3503.359503	431759.588950	43.759233
3502.968108	431750.572485	43.764237
3502.594552	431746.170747	43.769242
3502.519252	431761.254820	43.774247
3503.258357	431760.824169	43.779252
3502.998385	431757.874636	43.784257
3503.268669	431734.435155	43.789261
3503.097413	431740.604538	43.794266
3502.935258	431738.856176	43.799271
3503.364753	431736.144128	43.804276
3503.312344	431737.421716	43.809281
3503.078958	431729.748372	43.814285
3502.951476	431725.050889	43.819290
3502.965087	431708.505760	43.824295
3502.956630	431697.343348	43.829300
3503.104062	431698.891284	43.834305
3503.891987	431702.461142	43.839309
3503.804446	431701.511956	43.844314
3503.812913	431679.385746	43.849319
3504.098320	431669.898472	43.854324
3503.744979	431655.090545	43.859329
3503.558931	431633.758681	43.864333
3503.837610	431626.962024	43.869338
3503.261948	431612.344266	43.874343
3503.754670	431586.583126	43.879348
3503.732651	431593.031536	43.884353
3503.739037	431581.562063	43.889357
3503.829842	431566.475262	43.894362
3503.437250	431562.533445	43.899367
3503.382793	431542.447657	43.904372
3502.890901	431522.588779	43.909377
3503.351604	431514.999830	43.914381
3503.124941	431521.280221	43.919386
3503.050004	431520.481111	43.924391
3503.215634	431522.837876	43.929396
3502.738189	431527.740219	43.934401
3502.800130	431525.395379	43.939405
3502.872751	431518.938346	43.944410
3502.872467	431515.944441	43.949415
3503.186458	431511.425259	43.954420
3502.874903	431499.857798	43.959425
3503.117486	431486.419624	43.964429
3503.078931	431482.366597	43.969434
3503.049500	431480.798534	43.974439
3503.217532	431485.387690	43.979444
3503.110348	431484.188121	43.984449
3502.918109	431478.435992	43.989453
3503.217612	431489.345869	43.994458
3503.447118	431477.127812	43.999463
3503.452652	431457.488415	44.004468
3503.030149	431466.897731	44.009473
3503.411702	431455.922336	44.014477
3503.582088	431451.072445	44.019482
3503.096292	431435.678049	44.024487
3503.194701	431418.204816	44.029492
3503.264250	431419.664579	44.034497
3503.112436	431419.538283	44.039501
3503.158524	431426.533311	44.044506
3503.196458	431418.153844	44.049511
3503.559555	431410.023327	44.054516
3502.982201	431391.447567	44.059521
3503.267989	431377.139278	44.064525
3503.173400	431379.692727	44.069530
3503.275981	431380.690142	44.074535
3503.762300	431378.983263	44.079540
3503.532861	431356.846623	44.084545
3503.430428	431346.816492	44.089549
3503.593795	431336.943955	44.094554
3503.247174	431320.764533	44.099559
3503.405841	431298.764551	44.104564
3502.985056	431299.699096	44.109569
3503.458373	431297.791448	44.114573
3503.138151	431298.049127	44.119578
3503.271209	431301.477139	44.124583
3503.714734	431282.726977	44.129588
3503.221626	431279.715699	44.134593
3502.995370	431268.742506	44.139597
3503.278967	431277.980587	44.144602
3503.267193	431269.558809	44.149607
3503.490618	431239.479125	44.154612
3503.398459	431240.306813	44.159617
3503.039211	431231.842861	44.164621
3503.488080	431222.936444	44.169626
3502.869206	431228.776425	44.174631
3503.205377	431219.686266	44.179636
3503.109218	431205.696819	44.184641
3503.355118	431187.234055	44.189645
3503.534888	431178.931776	44.194650
3503.374776	431187.788941	44.199655
3503.246844	431178.879504	44.204660
3503.198005	431174.422210	44.209665
3503.250869	431158.428194	44.214669
3503.101835	431151.805922	44.219674
3502.836442	431158.701978	44.224679
3502.774090	431149.273871	44.229684
3502.904305	431154.072534	44.234689
3503.726972	431158.499230	44.239693
3503.684440	431150.031914	44.244698
3503.704555	431132.115120	44.249703
3503.630077	431127.357718	44.254708
3503.634971	431109.342013	44.259713
3503.535371	431092.409806	44.264717
3503.714050	431088.370363	44.269722
3503.689749	431080.661103	44.274727
3503.508090	431054.963778	44.279732
3503.496681	431048.926934	44.284737
3503.466068	431039.036646	44.289741
3502.991155	431023.792356	44.294746
3502.935899	431008.831625	44.299751
3503.246034	431003.957780	44.304756
3502.847644	431009.455689	44.309761
3503.052477	431007.543115	44.314765
3503.344586	431003.230558	44.319770
3503.072800	431005.459079	44.324775
3503.354210	431005.614033	44.329780
3503.145042	430995.500482	44.334785
3503.178057	430987.070954	44.339789
3503.018453	430989.940026	44.344794
3503.060847	430983.285020	44.349799
3503.309163	430976.493359	44.354804
3503.374994	430983.586642	44.359809
3503.519115	430966.663475	44.364813
3503.345643	430951.722893	44.369818
3503.324419	430949.138462	44.374823
3503.600408	430943.154010	44.379828
3503.158635	430946.527986	44.384833
3503.295124	430922.247841	44.389837
3503.319038	430905.751128	44.394842
3503.481705	430903.135293	44.399847
3503.658590	430893.006526	44.404852
3503.335579	430887.378072	44.409857
3503.131134	430865.541175	44.414861
3503.437086	430861.784442	44.419866
3503.048845	430865.606009	44.424871
3503.340863	430862.409869	44.429876
3503.556229	430860.850712	44.434881
3503.326585	430841.961406	44.439885
3503.307926	430832.880937	44.444890
3503.289727	430835.827376	44.449895
3503.511911	430825.893833	44.454900
3503.362169	430807.295335	44.459905
3503.312469	430795.987291	44.464909
3503.431377	430786.274353	44.469914
3503.446534	430791.853940	44.474919
3503.321254	430778.275183	44.479924
3503.277157	430766.306458	44.484929
3503.583881	430752.247946	44.489933
3503.623978	430749.399288	44.494938
3503.557587	430746.416571	44.499943
3503.788625	430712.630377	44.504948
3503.255390	430711.046792	44.509953
3503.182880	430711.465168	44.514957
3503.171188	430705.529777	44.519962
3503.139107	430685.794657	44.524967
3503.111318	430670.321547	44.529972
3503.194567	430667.008786	44.534977
3503.409909	430671.031807	44.539981
3503.147195	430678.435017	44.544986
3503.018881	430672.062807	44.549991
3503.249793	430659.996323	44.554996
3503.369802	430642.417324	44.560001
3503.387213	430634.142574	44.565005
3503.270234	430636.040214	44.570010
3503.026303	430634.559467	44.575015
3503.224571	430631.176314	44.580020
3503.058364	430610.449087	44.585025
3503.465550	430600.433112	44.590029
3503.608397	430599.140057	44.595034
3503.360704	430595.528563	44.600039
3503.650134	430579.290766	44.605044
3503.451422	430570.951402	44.610049
3503.241656	430556.524236	44.615053
3503.631247	430556.203995	44.620058
3503.275693	430543.121146	44.625063
3503.701766	430525.692790	44.630068
3503.493651	430521.161072	44.635073
3503.485662	430520.705727	44.640077
3503.489474	430496.498540	44.645082
3503.327033	430495.511345	44.650087
3503.083675	430487.940787	44.655092
3503.334580	430485.056102	44.660097
3503.227358	430475.432392	44.665101
3503.160050	430457.530006	44.670106
3502.870598	430461.081033	44.675111
3502.994745	430446.038559	44.680116
3502.997781	430451.062074	44.685121
3503.024844	430443.496075	44.690125
3503.239477	430444.677389	44.695130
3502.538336	430450.227122	44.700135
3503.138416	430445.455896	44.705140
3503.059527	430448.361999	44.710145
3502.977743	430446.193834	44.715149
3503.143583	430440.075819	44.720154
3503.468326	430437.533754	44.725159
3503.623984	430408.022791	44.730164
3503.500503	430402.157159	44.735169
3503.600485	430411.985162	44.740173
3503.595550	430387.982347	44.745178
3503.158880	430380.038779	44.750183
3503.513425	430372.467588	44.755188
3503.153847	430370.702084	44.760193
3503.222287	430356.227290	44.765197
3503.251785	430334.857428	44.770202
3502.970798	430336.021878	44.775207
3503.044721	430325.961193	44.780212
3502.730325	430331.749406	44.785217
3502.870702	430337.459964	44.790221
3503.028072	430334.388240	44.795226
3502.805688	430335.491936	44.800231
3502.947349	430328.819794	44.805236
3502.937657	430332.576810	44.810241
3503.100161	430336.405920	44.815245
3503.229830	430331.917984	44.820250
3502.934746	430319.535154	44.825255
3503.109458	430293.776139	44.830260
3503.197210	430299.952424	44.835265
3502.976988	430292.885332	44.840269
3502.797278	430288.703954	44.845274
3503.138878	430300.419171	44.850279
3503.076426	430295.710294	44.855284
3503.076902	430302.002977	44.860289
3503.127646	430301.943583	44.865293
3503.365841	430295.153452	44.870298
3503.081481	430281.855308	44.875303
3503.069425	430273.534714	44.880308
3503.006213	430259.539072	44.885313
3502.801323	430267.084783	44.890317
3502.950926	430265.993549	44.895322
3502.861228	430270.271716	44.900327
3503.081225	430269.523698	44.905332
3503.034836	430269.836126	44.910337
3503.338385	430268.414117	44.915341
3503.257372	430258.227615	44.920346
3503.069527	430245.166710	44.925351
3503.242913	430240.011568	44.930356
3503.284618	430234.726665	44.935361
3503.099289	430237.752465	44.940365
3503.395962	430243.487107	44.945370
3503.295914	430236.044241	44.950375
3503.035015	430214.926846	44.955380
3502.901122	430201.349224	44.960385
3503.291497	430200.166126	44.965389
3503.338772	430196.554953	44.970394
3503.290096	430190.219760	44.975399
3503.137416	430188.469662	44.980404
3503.238241	430173.532492	44.985409
3503.148319	430160.860806	44.990413
3503.386786	430157.572218	44.995418
3503.164172	430158.371471	45.000423
3503.426168	430149.445808	45.005428
3502.961199	430160.892830	45.010433
3503.096271	430140.062993	45.015437
3503.196426	430123.857199	45.020442
3503.055599	430120.785615	45.025447
3503.507233	430130.198454	45.030452
3503.202052	430121.369625	45.035457
3503.205280	430122.840794	45.040461
3503.885637	430112.574973	45.045466
3502.959056	430098.574410	45.050471
3503.263036	430094.868640	45.055476
3503.294031	430097.654527	45.060481
3503.387023	430084.799322	45.065485
3503.552074	430059.650679	45.070490
3503.117797	430050.691621	45.075495
3503.522662	430036.362179	45.080500
3503.657815	430038.572055	45.085505
3503.766530	430034.189138	45.090509
3503.732167	430013.997102	45.095514
3503.217926	430013.323698	45.100519
3503.592157	429995.497811	45.105524
3503.707280	429982.385027	45.110529
3503.122679	429969.899201	45.115533
3503.575926	429957.946637	45.120538
3503.278574	429954.546517	45.125543
3503.394817	429930.928531	45.130548
3503.492856	429941.416798	45.135553
3503.177474	429936.954030	45.140557
3503.501030	429931.316440	45.145562
3503.383780	429918.294047	45.150567
3503.133141	429896.311883	45.155572
3502.873471	429906.607500	45.160577
3503.076969	429894.646800	45.165581
3503.161362	429886.664841	45.170586
3502.999519	429896.842261	45.175591
3503.426830	429884.386600	45.180596
3503.397410	429870.080462	45.185601
3502.904138	429862.755368	45.190605
3503.244236	429853.258019	45.195610
3503.235400	429853.107299	45.200615
3503.022620	429847.815013	45.205620
3503.399893	429858.001894	45.210625
3503.180003	429841.952049	45.215629
3503.019768	429824.572534	45.220634
3502.611174	429823.678089	45.225639
3503.005773	429815.440142	45.230644
3502.956005	429827.070176	45.235649
3502.972020	429817.323655	45.240653
3503.063905	429822.129139	45.245658
3503.105777	429818.874072	45.250663
3503.174972	429818.913025	45.255668
3503.059606	429831.416990	45.260673
3503.028262	429828.834163	45.265677
3503.512593	429799.469309	45.270682
3503.125980	429798.215866	45.275687
3503.278149	429788.344586	45.280692
3503.261298	429794.792612	45.285697
3503.235074	429789.671454	45.290701
3503.822108	429775.310748	45.295706
3503.173114	429771.006411	45.300711
3503.519763	429755.824004	45.305716
3503.372792	429752.601173	45.310721
3503.507194	429744.204634	45.315725
3503.599990	429719.575455	45.320730
3503.376669	429712.965458	45.325735
3503.451127	429708.943574	45.330740
3503.188708	429692.088901	45.335745
3502.993498	429689.534038	45.340749
3503.383156	429673.126252	45.345754
3503.026287	429674.760434	45.350759
3503.309060	429665.019050	45.355764
3503.077211	429669.372348	45.360769
3503.236916	429668.634607	45.365773
3503.245686	429639.198505	45.370778
3503.107089	429641.556661	45.375783
3503.168174	429631.700868	45.380788
3503.241833	429630.521073	45.385793
3503.276762	429629.956884	45.390797
3503.240896	429631.942253	45.395802
3503.146059	429613.993171	45.400807
3503.541756	429593.981088	45.405812
3503.273425	429599.457117	45.410817
3503.451768	429598.208697	45.415821
3503.526710	429589.213261	45.420826
3503.119619	429570.708470	45.425831
3503.270888	429554.696552	45.430836
3503.293414	429551.394002	45.435841
3503.034960	429558.543090	45.440845
3503.119975	429553.859633	45.445850
3503.076543	429562.088495	45.450855
3503.149926	429539.796922	45.455860
3503.246966	429526.027226	45.460865
3502.935839	429528.820849	45.465869
3502.896021	429509.390553	45.470874
3502.592434	429525.225549	45.475879
3503.175838	429515.382021	45.480884
3503.153413	429518.532346	45.485889
3503.235169	429520.091644	45.490893
3503.569907	429511.863813	45.495898
3503.062156	429500.379605	45.500903
3503.307209	429482.220137	45.505908
3503.432174	429479.965830	45.510913
3503.374368	429485.507439	45.515917
3503.462355	429473.058750	45.520922
3503.295813	429461.973010	45.525927
3503.032552	429442.479312	45.530932
3503.247208	429444.929419	45.535937
3502.986051	429438.884052	45.540941
3503.329091	429439.282245	45.545946
3503.367604	429444.705917	45.550951
3503.335089	429411.927093	45.555956
3503.217073	429413.114509	45.560961
3503.010591	429405.131304	45.565965
3503.449366	429401.402409	45.570970
3503.294595	429400.210857	45.575975
3503.059269	429388.629328	45.580980
3502.822331	429366.441326	45.585985
3502.763329	429363.355671	45.590989
3503.335200	429363.156543	45.595994
3502.880540	429355.723196	45.600999
3503.377458	429360.459615	45.606004
3503.508304	429358.102792	45.611009
3503.310956	429358.136508	45.616013
3503.454277	429339.486801	45.621018
3502.915075	429332.270882	45.626023
3503.261550	429327.136735	45.631028
3503.099368	429324.779194	45.636033
3503.003665	429318.908545	45.641037
3503.171552	429322.736903	45.646042
3503.175051	429332.277334	45.651047
3503.044949	429312.304041	45.656052
3502.838272	429299.398073	45.661057
3502.614405	429301.770822	45.666061
3503.035925	429290.584589	45.671066
3502.825710	429294.782013	45.676071
3502.950311	429287.858737	45.681076
3503.027865	429290.890522	45.686081
3502.893651	429294.110715	45.691085
3503.446550	429288.078561	45.696090
3502.807909	429286.360622	45.701095
3503.209986	429290.605748	45.706100
3503.174699	429290.408791	45.711105
3502.908480	429290.403516	45.716109
3503.209693	429286.647342	45.721114
3503.252629	429269.384974	45.726119
3502.848553	429253.163175	45.731124
3503.391795	429247.081909	45.736129
3503.321615	429252.777935	45.741133
3503.008765	429248.720605	45.746138
3502.782864	429257.437482	45.751143
3503.019890	429260.898793	45.756148
3502.997843	429262.171331	45.761153
3502.921740	429251.070048	45.766157
3502.883699	429224.381931	45.771162
3502.601014	429226.815480	45.776167
3502.831403	429229.567425	45.781172
3502.944012	429243.098533	45.786177
3502.883647	429233.923064	45.791181
3503.011522	429214.210139	45.796186
3502.639954	429226.047669	45.801191
3502.941646	429217.977629	45.806196
3503.050221	429228.159915	45.811201
3502.904887	429225.393484	45.816205
3502.966398	429220.764724	45.821210
3502.882374	429225.904868	45.826215
3502.903440	429229.707560	45.831220
3502.876896	429223.114575	45.836225
3502.964489	429223.657890	45.841229
3503.123261	429221.397786	45.846234
3503.027255	429236.537777	45.851239
3502.888572	429230.217693	45.856244
3502.886833	429231.385265	45.861249
3502.934213	429226.961920	45.866253
3503.397808	429222.163004	45.871258
3503.016178	429214.666392	45.876263
3503.262546	429197.775238	45.881268
3503.272367	429208.177396	45.886273
3503.244492	429211.430194	45.891277
3503.162306	429205.303458	45.896282
3502.637100	429209.503930	45.901287
3502.922015	429207.932790	45.906292
3503.084773	429201.916480	45.911297
3503.063444	429197.860114	45.916301
3503.479276	429164.953639	45.921306
3503.287345	429162.651911	45.926311
3503.018895	429168.635564	45.931316
3503.132750	429161.358834	45.936321
3503.112584	429159.129278	45.941325
3503.225801	429159.668219	45.946330
3503.086206	429137.767882	45.951335
3503.056839	429125.339048	45.956340
3503.334624	429120.216585	45.961345
3503.065687	429124.982321	45.966349
3503.476541	429120.496893	45.971354
3503.035244	429129.352097	45.976359
3503.181140	429118.872603	45.981364
3503.231904	429100.187759	45.986369
3503.272269	429090.081525	45.991373
3503.385315	429084.682680	45.996378
3502.793094	429088.640863	46.001383
3503.012152	429084.746434	46.006388
3503.390396	429082.042837	46.011393
3503.337011	429080.884708	46.016397
3502.961455	429051.462742	46.021402
3502.892778	429055.534539	46.026407
3502.878454	429049.345424	46.031412
3503.163743	429048.839973	46.036417
3503.207246	429058.119932	46.041421
3503.460016	429044.577117	46.046426
3503.314576	429051.757812	46.051431
3503.020448	429022.271155	46.056436
3502.910543	429017.367120	46.061441
3502.899013	429020.972408	46.066445
3503.293062	429013.241784	46.071450
3503.085655	429018.403040	46.076455
3503.093252	429013.580442	46.081460
3503.333528	429007.550847	46.086465
3503.164618	429010.167994	46.091469
3503.075381	428985.366125	46.096474
3503.233119	428977.168330	46.101479
3503.157762	428975.049681	46.106484
3503.577803	428973.607706	46.111489
3503.340767	428973.749700	46.116493
3503.250146	428963.767278	46.121498
3503.141152	428943.130306	46.126503
3502.923737	428926.267397	46.131508
3503.093728	428936.693077	46.136513
3502.767332	428939.134120	46.141517
3503.119152	428927.858115	46.146522
3503.047618	428932.996190	46.151527
3502.879158	428932.974222	46.156532
3503.135898	428935.924706	46.161537
3502.896021	428928.302296	46.166541
3503.340183	428935.331601	46.171546
3502.891941	428924.699714	46.176551
3502.851578	428905.116759	46.181556
3503.136570	428904.408353	46.186561
3502.968008	428911.390034	46.191565
3503.146351	428905.573992	46.196570
3503.222857	428909.215016	46.201575
3502.647719	428907.841461	46.206580
3503.189405	428908.357998	46.211585
3503.048076	428908.331398	46.216589
3503.300582	428910.521343	46.221594
3503.026335	428893.972621	46.226599
3502.853277	428883.953490	46.231604
3503.126364	428866.702280	46.236609
3502.942869	428868.256161	46.241613
3503.089213	428873.407798	46.246618
3502.774512	428871.177754	46.251623
3502.546201	428865.278884	46.256628
3502.793888	428869.550450	46.261633
3502.633802	428868.258275	46.266637
3502.913759	428869.631521	46.271642
3503.196525	428874.252353	46.276647
3502.837945	428867.715963	46.281652
3503.005606	428879.715349	46.286657
3502.786983	428887.517602	46.291661
3503.078651	428875.389076	46.296666
3502.814781	428880.306248	46.301671
3502.873549	428879.179710	46.306676
3503.001160	428870.631765	46.311681
3503.100032	428875.943760	46.316685
3503.189051	428869.432446	46.321690
3502.712635	428858.754588	46.326695
3503.168875	428844.872410	46.331700
3503.168883	428840.457081	46.336705
3502.817858	428844.983133	46.341709
3503.057205	428839.055156	46.346714
3503.114160	428841.329249	46.351719
3503.174153	428844.871601	46.356724
3503.151206	428846.854830	46.361729
3502.960342	428848.156216	46.366733
3503.370387	428836.413466	46.371738
3503.383139	428819.866437	46.376743
3503.352193	428808.198972	46.381748
3503.360646	428806.319754	46.386753
3503.068200	428804.948674	46.391757
3503.214506	428801.675635	46.396762
3503.101166	428786.317390	46.401767
3503.260905	428769.542224	46.406772
3503.183959	428771.788436	46.411777
3503.216065	428769.955927	46.416781
3503.348619	428769.578053	46.421786
3503.154640	428773.316035	46.426791
3503.006565	428753.497590	46.431796
3503.114789	428734.853397	46.436801
3503.350992	428735.320597	46.441805
3503.815573	428727.070323	46.446810
3503.504460	428727.884734	46.451815
3503.330838	428699.798134	46.456820
3503.326445	428688.024572	46.461825
3503.222223	428698.649434	46.466829
3503.309693	428688.940995	46.471834
3503.516932	428688.601119	46.476839
3503.306245	428666.763234	46.481844
3503.418229	428659.385166	46.486849
3503.269967	428649.310950	46.491853
3503.207941	428649.829074	46.496858
3503.322756	428656.102676	46.501863
3502.923701	428635.210452	46.506868
3503.273042	428623.122701	46.511873
3502.993248	428622.155462	46.516877
3503.061984	428617.017834	46.521882
3502.835199	428617.614843	46.526887
3503.243051	428618.001986	46.531892
3503.651019	428620.825184	46.536897
3503.326869	428601.594943	46.541901
3503.412076	428579.655702	46.546906
3503.372822	428585.143603	46.551911
3502.895620	428582.180003	46.556916
3503.120692	428587.115253	46.561921
3502.815773	428581.483151	46.566925
3502.930101	428570.552037	46.571930
3502.812990	428558.949913	46.576935
3502.709283	428551.507136	46.581940
3503.253997	428554.611504	46.586945
3502.950034	428542.635263	46.591949
3503.164322	428538.792310	46.596954
3503.191182	428549.800871	46.601959
3502.846651	428547.423634	46.606964
3502.771122	428546.218508	46.611969
3502.851192	428556.202945	46.616973
3503.038196	428539.219952	46.621978
3502.954250	428545.223011	46.626983
3503.018807	428551.961987	46.631988
3503.323077	428549.118706	46.636993
3503.051548	428536.933917	46.641997
3502.871410	428519.049316	46.647002
3502.889036	428510.773780	46.652007
3503.082399	428503.077256	46.657012
3503.344925	428500.850120	46.662017
3503.101070	428509.367332	46.667021
3503.437979	428512.202677	46.672026
3503.397524	428518.858089	46.677031
3503.197580	428498.033250	46.682036
3503.321345	428478.675675	46.687041
3503.251099	428475.338063	46.692045
3503.611646	428475.631781	46.697050
3503.163480	428474.997797	46.702055
3503.307358	428443.760814	46.707060
3503.412001	428434.455354	46.712065
3502.963017	428437.018883	46.717069
3503.335082	428429.647086	46.722074
3503.224306	428430.630307	46.727079
3503.172784	428428.609043	46.732084
3503.214357	428396.120665	46.737089
3503.024881	428402.497044	46.742093
3502.892563	428393.384285	46.747098
3502.760182	428404.267847	46.752103
3502.908244	428398.659859	46.757108
3503.079921	428389.241431	46.762113
3502.930959	428397.843984	46.767117
3503.281229	428390.222136	46.772122
3503.220967	428400.788873	46.777127
3502.997174	428393.265047	46.782132
3503.191541	428384.045751	46.787137
3503.124808	428371.470643	46.792141
3503.185406	428351.260964	46.797146
3503.061949	428358.082851	46.802151
3502.948742	428360.792063	46.807156
3503.237954	428355.971997	46.812161
3502.939100	428361.047507	46.817165
3503.157211	428357.609889	46.822170
3503.391572	428356.301087	46.827175
3503.116449	428344.015307	46.832180
3503.016082	428323.680832	46.837185
3502.939117	428326.282355	46.842189
3503.343716	428320.833554	46.847194
3503.464647	428322.081729	46.852199
3503.336478	428311.902433	46.857204
3503.688893	428291.896637	46.862209
3503.200863	428283.808867	46.867213
3503.417500	428275.753029	46.872218
3503.598905	428274.757778	46.877223
3503.610637	428261.712443	46.882228
3503.693222	428242.767725	46.887233
3503.343059	428242.726029	46.892237
3503.186981	428214.483598	46.897242
3502.742257	428205.373357	46.902247
3503.076103	428201.103916	46.907252
3503.297583	428192.235183	46.912257
3502.950731	428201.531380	46.917261
3503.524827	428189.151268	46.922266
3503.372410	428199.074049	46.927271
3503.413211	428183.739844	46.932276
3503.361025	428163.803025	46.937281
3503.180580	428156.170217	46.942285
3503.396306	428161.563925	46.947290
3502.713080	428161.832862	46.952295
3502.498502	428167.097033	46.957300
3502.863905	428164.598536	46.962305
3502.574977	428167.033259	46.967309
3502.821678	428161.053104	46.972314
3503.058345	428156.901753	46.977319
3502.740042	428153.606451	46.982324
3503.011998	428155.031858	46.987329
3502.980046	428156.306147	46.992333
3503.212982	428141.497387	46.997338
3503.076956	428134.415265	47.002343
3503.257442	428123.066628	47.007348
3503.268370	428113.523280	47.012353
3503.011386	428121.383088	47.017357
3502.666282	428118.244616	47.022362
3503.087072	428122.842029	47.027367
3502.948782	428117.232115	47.032372
3503.043835	428119.195257	47.037377
3503.255576	428119.209874	47.042381
3503.198887	428101.202371	47.047386
3503.313655	428095.803007	47.052391
3503.157867	428086.694137	47.057396
3503.215396	428085.161750	47.062401
3502.917195	428080.441929	47.067405
3503.213546	428077.853709	47.072410
3503.261987	428084.544818	47.077415
3503.027261	428059.005525	47.082420
3503.361564	428040.017664	47.087425
3502.900556	428042.532535	47.092429
3502.924766	428039.940025	47.097434
3503.091178	428043.718091	47.102439
3502.895018	428037.712017	47.107444
3503.030237	428039.820566	47.112449
3502.768190	428053.720847	47.117453
3503.042324	428040.427573	47.122458
3503.281681	428033.179819	47.127463
3503.104039	428031.738337	47.132468
3503.039981	428011.194382	47.137473
3502.743468	428020.228289	47.142477
3503.204754	428018.271687	47.147482
3503.082781	428021.540716	47.152487
3503.247131	428024.202574	47.157492
3503.358206	428005.151296	47.162497
3503.198148	428018.171383	47.167501
3503.418992	427998.847593	47.172506
3503.670891	427986.623897	47.177511
3503.541603	427975.531094	47.182516
3503.689278	427963.984971	47.187521
3503.491731	427950.619927	47.192525
3503.262690	427933.758293	47.197530
3502.933176	427925.592579	47.202535
3502.808887	427923.888215	47.207540
3503.295294	427929.540277	47.212545
3503.233660	427930.768893	47.217549
3503.018061	427905.936711	47.222554
3502.736173	427894.768421	47.227559
3502.589414	427894.488979	47.232564
3502.782139	427892.324458	47.237569
3502.933573	427898.896527	47.242573
3503.018613	427884.062107	47.247578
3503.269438	427887.165993	47.252583
3503.082909	427895.927402	47.257588
3503.457257	427886.727934	47.262593
3502.948077	427892.093223	47.267597
3503.422699	427887.545922	47.272602
3503.104474	427873.693909	47.277607
3502.765927	427859.642345	47.282612
3502.790836	427856.643670	47.287617
3502.806806	427861.970049	47.292621
3502.986516	427854.732426	47.297626
3502.931165	427857.533322	47.302631
3502.735852	427860.358117	47.307636
3503.166404	427855.057038	47.312641
3502.979660	427856.966812	47.317645
3502.932598	427847.534765	47.322650
3503.086592	427857.405369	47.327655
3502.908009	427846.625442	47.332660
3503.130822	427850.089389	47.337665
3502.705931	427862.799509	47.342669
3502.857255	427863.991766	47.347674
3503.337835	427860.204742	47.352679
3502.875064	427841.251316	47.357684
3503.115702	427833.038970	47.362689
3502.754396	427832.593148	47.367693
3502.839072	427817.657242	47.372698
3503.144824	427822.680383	47.377703
3502.849125	427820.040967	47.382708
3503.138671	427819.281000	47.387713
3503.098110	427826.748678	47.392717
3503.190259	427820.388800	47.397722
3503.182596	427820.745400	47.402727
3502.910909	427818.913937	47.407732
3502.848948	427794.867458	47.412737
3502.637367	427784.499164	47.417741
3502.802265	427802.640728	47.422746
3502.901489	427811.657896	47.427751
3503.166268	427806.994151	47.432756
3503.250342	427788.404089	47.437761
3502.642869	427783.178729	47.442765
3502.843881	427791.620238	47.447770
3503.059369	427786.609632	47.452775
3502.976384	427790.176556	47.457780
3503.177074	427774.967046	47.462785
3502.677598	427785.203026	47.467789
3502.996912	427784.031948	47.472794
3503.182273	427783.239016	47.477799
3503.265673	427795.354848	47.482804
3503.284603	427769.771931	47.487809
3503.174135	427758.219032	47.492813
3503.015983	427746.166735	47.497818
3503.216479	427748.213410	47.502823
3502.934131	427750.139517	47.507828
3502.887757	427743.904779	47.512833
3503.225598	427752.830472	47.517837
3503.223430	427738.010851	47.522842
3503.219395	427726.998052	47.527847
3503.133608	427717.521812	47.532852
3503.439247	427706.405373	47.537857
3503.201752	427715.074044	47.542861
3503.205986	427710.454769	47.547866
3503.030382	427711.144568	47.552871
3502.879153	427717.311585	47.557876
3503.365457	427698.652772	47.562881
3503.013306	427680.746153	47.567885
3503.137104	427672.756717	47.572890
3503.180775	427670.363859	47.577895
3503.106298	427670.173579	47.582900
3503.400769	427661.951983	47.587905
3503.030600	427670.694078	47.592909
3503.125421	427645.605605	47.597914
3503.137555	427634.234726	47.602919
3502.932170	427630.463286	47.607924
3503.227903	427621.632416	47.612929
3503.028502	427632.933806	47.617933
3503.135322	427631.748250	47.622938
3502.822044	427627.690710	47.627943
3502.947970	427622.999885	47.632948
3503.485467	427625.293551	47.637953
3503.162916	427611.797398	47.642957
3503.014713	427598.372976	47.647962
3503.107714	427588.764649	47.652967
3503.344085	427575.274548	47.657972
3503.338193	427575.884619	47.662977
3503.058676	427586.895187	47.667981
3503.259296	427592.342360	47.672986
3503.057071	427571.060308	47.677991
3502.945640	427561.943662	47.682996
3503.252022	427542.198863	47.688001
3502.924091	427550.883036	47.693005
3503.102967	427553.390205	47.698010
3503.336787	427548.985465	47.703015
3503.079039	427541.365657	47.708020
3503.248973	427546.006017	47.713025
3502.783370	427527.103577	47.718029
3503.043427	427509.041540	47.723034
3503.485889	427505.920770	47.728039
3503.346933	427512.085745	47.733044
3503.394500	427502.485141	47.738049
3503.271340	427507.226309	47.743053
3502.889307	427491.862347	47.748058
3502.786973	427480.054154	47.753063
3502.903426	427473.080985	47.758068
3502.890355	427474.453595	47.763073
3502.903594	427472.827223	47.768077
3502.985742	427468.245351	47.773082
3503.063257	427471.987933	47.778087
3502.939345	427477.541300	47.783092
3503.076814	427468.737396	47.788097
3503.133194	427465.682544	47.793101
3502.918593	427465.110157	47.798106
3503.353521	427472.750528	47.803111
3502.892878	427468.515107	47.808116
3503.149427	427456.747131	47.813121
3502.717265	427451.441008	47.818125
3503.089217	427423.361242	47.823130
3502.989835	427424.697838	47.828135
3503.159384	427434.159929	47.833140
3503.201793	427425.524504	47.838145
3503.076504	427431.534903	47.843149
3503.240417	427437.140642	47.848154
3503.425444	427434.571361	47.853159
3503.572324	427427.491475	47.858164
3503.354212	427408.749697	47.863169
3503.244034	427411.763025	47.868173
3503.141623	427410.511676	47.873178
3503.137723	427394.727806	47.878183
3503.248501	427384.608820	47.883188
3503.489806	427362.337272	47.888193
3503.318657	427365.411770	47.893197
3503.042568	427367.641364	47.898202
3503.327051	427366.070180	47.903207
3503.122882	427350.015950	47.908212
3503.212626	427328.379301	47.913217
3503.048324	427337.390893	47.918221
3503.315352	427328.666324	47.923226
3503.147176	427323.974903	47.928231
3503.155872	427329.556416	47.933236
3503.274875	427320.349576	47.938241
3502.931338	427304.725148	47.943245
3502.688076	427291.469046	47.948250
3503.147758	427293.573015	47.953255
3503.138990	427288.752860	47.958260
3503.337783	427283.592736	47.963265
3502.832974	427287.231761	47.968269
3502.832097	427281.547431	47.973274
3502.947959	427280.360314	47.978279
3502.587652	427295.039133	47.983284
3502.915708	427289.755430	47.988289
3502.811377	427292.717020	47.993293
3502.899703	427288.235566	47.998298
3502.927110	427285.693183	48.003303
3502.518001	427294.391310	48.008308
3503.582293	427279.795341	48.013313
3503.169872	427288.291018	48.018317
3503.257908	427264.675180	48.023322
3503.249155	427253.307685	48.028327
3503.172952	427251.493552	48.033332
3502.881081	427255.451505	48.038337
3502.801653	427252.978115	48.043341
3502.840256	427255.001722	48.048346
3502.947802	427260.870899	48.053351
3502.837563	427251.906194	48.058356
3503.250420	427245.034611	48.063361
3503.008427	427257.257033	48.068365
3502.739723	427244.056004	48.073370
3503.134478	427236.882983	48.078375
3502.721600	427233.349927	48.083380
3503.058658	427208.879440	48.088385
3502.858101	427213.126335	48.093389
3502.533583	427212.724973	48.098394
3502.862652	427209.166736	48.103399
3502.863023	427213.988378	48.108404
3503.195179	427214.236209	48.113409
3503.117716	427219.223404	48.118413
3503.149895	427205.209658	48.123418
3503.151241	427210.183398	48.128423
3502.856385	427212.466966	48.133428
3503.016901	427218.327109	48.138433
3503.335157	427214.516946	48.143437
3503.061869	427198.474416	48.148442
3503.106887	427181.971488	48.153447
3502.816908	427176.539516	48.158452
3503.066752	427173.299329	48.163457
3502.952300	427180.830581	48.168461
3502.805474	427180.652652	48.173466
3503.115309	427173.291093	48.178471
3502.737791	427176.857645	48.183476
3503.231079	427172.408533	48.188481
3503.195590	427179.368001	48.193485
3503.024231	427179.498789	48.198490
3503.269844	427152.658389	48.203495
3502.956150	427144.337439	48.208500
3503.492442	427132.470782	48.213505
3503.199624	427136.885709	48.218509
3503.061257	427139.548601	48.223514
3503.103986	427134.668866	48.228519
3502.735393	427134.173519	48.233524
3502.964097	427127.079573	48.238529
3503.164270	427145.926183	48.243533
3503.104507	427113.656369	48.248538
3502.951123	427099.928021	48.253543
3502.771940	427100.821467	48.258548
3503.053404	427097.626625	48.263553
3503.022442	427097.073627	48.268557
3502.829000	427104.567637	48.273562
3502.947682	427096.172842	48.278567
3502.801789	427099.801366	48.283572
3502.881319	427097.554591	48.288577
3502.773026	427100.973675	48.293581
3503.166034	427097.099974	48.298586
3503.433382	427094.415091	48.303591
3502.954482	427104.140301	48.308596
3503.086154	427072.802086	48.313601
3503.049313	427065.499689	48.318605
3502.645512	427064.198273	48.323610
3503.221413	427055.928414	48.328615
3502.739031	427064.080832	48.333620
3503.017983	427060.125091	48.338625
3502.783352	427057.931956	48.343629
3502.922852	427056.487017	48.348634
3503.290992	427053.429634	48.353639
3503.106066	427062.698625	48.358644
3502.924517	427052.172618	48.363649
3502.737098	427064.893370	48.368653
3502.526197	427059.041829	48.373658
3502.991079	427061.094176	48.378663
3503.202967	427061.210279	48.383668
3503.087538	427048.693538	48.388673
3503.125315	427034.678737	48.393677
3503.134934	427014.070583	48.398682
3503.242905	427025.167512	48.403687
3503.014868	427018.202277	48.408692
3503.069956	427019.715540	48.413697
3502.978234	427019.883485	48.418701
3502.951637	427020.547860	48.423706
3503.060877	427023.523771	48.428711
3503.331913	427023.731285	48.433716
3503.112502	426997.173132	48.438721
3502.889729	426988.430562	48.443725
3503.104599	426988.596912	48.448730
3503.380173	426979.972267	48.453735
3502.836973	426983.059587	48.458740
3503.168464	426981.378841	48.463745
3503.255832	426983.241879	48.468749
3502.999366	426981.509261	48.473754
3503.437628	426961.589198	48.478759
3502.912120	426957.770801	48.483764
3502.612151	426948.229315	48.488769
3503.057419	426948.356325	48.493773
3503.238087	426937.057846	48.498778
3503.248454	426940.761222	48.503783
3503.348995	426941.911442	48.508788
3503.101857	426930.939784	48.513793
3503.350626	426918.563809	48.518797
3503.035262	426909.837020	48.523802
3503.287676	426906.291826	48.528807
3502.907479	426904.783350	48.533812
3502.975603	426899.594700	48.538817
3503.000080	426905.731926	48.543821
3503.014137	426900.907794	48.548826
3503.270877	426894.722587	48.553831
3503.089766	426889.728757	48.558836
3503.230558	426863.819525	48.563841
3503.338315	426861.212621	48.568845
3503.374397	426861.511011	48.573850
3503.393056	426863.741079	48.578855
3503.212376	426861.031159	48.583860
3503.302891	426840.510553	48.588865
3503.231339	426832.300414	48.593869
3503.142767	426827.696814	48.598874
3503.442429	426816.174937	48.603879
3502.859417	426831.957932	48.608884
3502.863005	426822.770607	48.613889
3502.837061	426835.819197	48.618893
3502.819634	426823.894668	48.623898
3503.227720	426812.506543	48.628903
3503.115108	426804.201895	48.633908
3503.080833	426790.402274	48.638913
3503.130948	426794.555686	48.643917
3503.383323	426794.005057	48.648922
3502.887616	426792.008741	48.653927
3503.037657	426798.733620	48.658932
3503.144377	426793.132313	48.663937
3503.233440	426780.682025	48.668941
3503.316988	426759.299695	48.673946
3503.681483	426749.695428	48.678951
3503.286470	426755.955075	48.683956
3503.360058	426746.400479	48.688961
3502.891365	426728.919085	48.693965
3502.791917	426718.937223	48.698970
3503.097177	426709.698344	48.703975
3502.895610	426716.127994	48.708980
3503.189410	426704.353286	48.713985
3503.215648	426712.063687	48.718989
3502.963125	426714.796874	48.723994
3503.149650	426702.126881	48.728999
3502.920229	426707.698442	48.734004
3503.567840	426694.188379	48.739009
3503.763495	426685.628030	48.744013
3503.291068	426671.192574	48.749018
3503.473950	426669.587937	48.754023
3503.405782	426656.250828	48.759028
3503.330705	426638.702158	48.764033
3503.381727	426632.348986	48.769037
3503.454951	426631.828943	48.774042
3503.465792	426625.025828	48.779047
3503.168044	426606.246259	48.784052
3503.175351	426591.424305	48.789057
3503.130331	426597.167429	48.794061
3502.713520	426594.700822	48.799066
3503.076693	426586.771661	48.804071
3502.869585	426589.852398	48.809076
3502.580066	426582.745265	48.814081
3502.951739	426592.274692	48.819085
3502.932679	426590.653775	48.824090
3503.147802	426585.541469	48.829095
3502.809154	426589.913565	48.834100
3503.089115	426586.059086	48.839105
3502.909917	426564.467665	48.844109
3502.973179	426553.595099	48.849114
3503.571341	426543.240267	48.854119
3503.148092	426551.179738	48.859124
3503.312136	426545.822364	48.864129
3503.392226	426544.032247	48.869133
3503.410178	426534.284041	48.874138
3503.430931	426522.251331	48.879143
3503.253406	426511.825909	48.884148
3503.289804	426507.403932	48.889153
3503.426061	426501.086928	48.894157
3503.222592	426486.909972	48.899162
3503.109840	426459.571666	48.904167
3503.021237	426470.347126	48.909172
3502.770314	426465.111346	48.914177
3502.942089	426464.675984	48.919181
3502.829931	426469.060186	48.924186
3502.951382	426466.907707	48.929191
3502.864703	426472.810242	48.934196
3502.725462	426472.884792	48.939201
3502.751601	426471.611443	48.944205
3502.408786	426472.837389	48.949210
3502.749138	426466.536282	48.954215
3502.886814	426474.380001	48.959220
3502.941697	426465.437560	48.964225
3503.187243	426465.446408	48.969229
3502.869295	426472.708094	48.974234
3502.909856	426465.240027	48.979239
3502.750234	426473.032997	48.984244
3503.147351	426471.087229	48.989249
3503.224665	426472.850513	48.994253
3503.140182	426450.633742	48.999258
3503.334690	426431.414689	49.004263
3502.861257	426432.206134	49.009268
3502.639978	426425.442596	49.014273
3502.568511	426428.195656	49.019277
3502.850345	426437.486703	49.024282
3502.834970	426430.281958	49.029287
3502.612087	426429.863227	49.034292
3502.666562	426426.757812	49.039297
3502.616159	426430.217863	49.044301
3502.728839	426431.569060	49.049306
3502.985113	426430.002632	49.054311
3502.924542	426430.926606	49.059316
3503.011533	426425.531606	49.064321
3502.936055	426435.340471	49.069325
3502.848381	426439.162179	49.074330
3502.945784	426432.344228	49.079335
3502.815136	426435.056636	49.084340
3502.909523	426437.375325	49.089345
3502.991988	426425.788835	49.094349
3502.831619	426436.018245	49.099354
3502.949656	426423.055261	49.104359
3502.947992	426429.653879	49.109364
3503.116260	426430.944829	49.114369
3502.936586	426424.427968	49.119373
3502.981566	426435.383659	49.124378
3502.986869	426413.811355	49.129383
3502.699448	426398.633555	49.134388
3502.722970	426390.559299	49.139393
3503.091931	426395.064389	49.144397
3502.757278	426401.212309	49.149402
3502.754783	426399.284013	49.154407
3502.790889	426396.283243	49.159412
3502.943251	426398.185986	49.164417
3502.788913	426399.278241	49.169421
3503.130504	426402.519094	49.174426
3503.038109	426392.941942	49.179431
3502.920409	426398.545254	49.184436
3503.072165	426390.601372	49.189441
3503.074344	426397.250099	49.194445
3502.913512	426398.394218	49.199450
3502.892213	426392.662407	49.204455
3503.191882	426398.092942	49.209460
3503.275872	426395.287021	49.214465
3503.135331	426380.693207	49.219469
3502.884759	426361.550095	49.224474
3502.954078	426360.421636	49.229479
3502.871548	426365.257605	49.234484
3502.675758	426360.976760	49.239489
3503.133711	426356.888826	49.244493
3502.957892	426366.714853	49.249498
3503.054103	426359.744815	49.254503
3502.761842	426358.424314	49.259508
3503.072551	426351.366892	49.264513
3503.319929	426359.039648	49.269517
3502.887197	426370.584502	49.274522
3503.183768	426355.916036	49.279527
3503.102216	426347.199873	49.284532
3502.745537	426326.044593	49.289537
3503.123876	426327.756487	49.294541
3502.745868	426323.912801	49.299546
3502.962235	426323.114527	49.304551
3502.827926	426328.111614	49.309556
3502.983448	426321.639004	49.314561
3503.075662	426324.313371	49.319565
3502.822757	426327.300449	49.324570
3503.334518	426326.502493	49.329575
3502.787075	426332.432982	49.334580
3502.694965	426340.366737	49.339585
3502.668532	426330.016950	49.344589
3502.620700	426324.035870	49.349594
3503.382803	426325.276185	49.354599
3503.438861	426336.737595	49.359604
3503.154909	426311.407853	49.364609
3503.252299	426295.149151	49.369613
3503.268610	426290.172242	49.374618
3503.302100	426280.370524	49.379623
3503.358886	426285.182721	49.384628
3503.143114	426274.966753	49.389633
3502.990387	426255.350039	49.394637
3502.611308	426248.562638	49.399642
3502.826631	426247.713784	49.404647
3502.560261	426252.834950	49.409652
3502.841986	426254.461833	49.414657
3503.226793	426237.240396	49.419661
3502.924615	426250.945553	49.424666
3503.140859	426242.178503	49.429671
3502.956169	426246.524373	49.434676
3503.027210	426247.679664	49.439681
3502.949145	426246.728636	49.444685
3502.708603	426257.733162	49.449690
3503.187817	426247.855323	49.454695
3502.689354	426253.625198	49.459700
3502.897802	426250.798008	49.464705
3502.821886	426250.506450	49.469709
3502.701517	426251.998964	49.474714
3502.975898	426245.506037	49.479719
3503.049427	426248.437387	49.484724
3503.496256	426243.589984	49.489729
3503.187264	426219.990146	49.494733
3503.066667	426212.041952	49.499738
3503.319530	426205.857229	49.504743
3503.052403	426210.166425	49.509748
3502.874899	426221.566258	49.514753
3503.460920	426213.294382	49.519757
3503.128160	426198.631764	49.524762
3503.314346	426184.844907	49.529767
3503.064483	426190.724619	49.534772
3502.683284	426181.602749	49.539777
3503.083362	426180.062507	49.544781
3503.148097	426180.660554	49.549786
3503.516585	426177.399975	49.554791
3503.221988	426178.313161	49.559796
3503.135199	426152.086719	49.564801
3503.450173	426144.114885	49.569805
3502.858852	426143.454518	49.574810
3503.067128	426139.256910	49.579815
3502.925743	426142.580267	49.584820
3502.545898	426138.584593	49.589825
3502.992984	426136.934809	49.594829
3502.889491	426140.911535	49.599834
3503.086493	426135.852984	49.604839
3502.996595	426135.868353	49.609844
3503.052313	426146.213260	49.614849
3502.955300	426140.697345	49.619853
3502.905584	426125.174242	49.624858
3503.184236	426107.970838	49.629863
3503.544154	426105.625338	49.634868
3503.439829	426103.359107	49.639873
3503.237842	426101.617121	49.644877
3503.214643	426092.890902	49.649882
3503.162832	426076.302228	49.654887
3502.984235	426069.785086	49.659892
3503.056556	426056.931224	49.664897
3502.978610	426060.040732	49.669901
3502.593490	426065.994326	49.674906
3503.212592	426063.706081	49.679911
3503.313999	426064.196354	49.684916
3503.393017	426064.030610	49.689921
3503.193157	426047.974766	49.694925
3503.153236	426029.353747	49.699930
3503.535109	426023.756035	49.704935
3503.346978	426027.442689	49.709940
3502.783273	426021.803405	49.714945
3503.042064	426020.338035	49.719949
3502.688181	426024.306778	49.724954
3503.143191	426019.457934	49.729959
3502.920974	426014.115638	49.734964
3502.851204	426002.554938	49.739969
3503.026097	425985.978249	49.744973
3502.785529	425982.669369	49.749978
3503.103055	425980.940182	49.754983
3503.260155	425980.558075	49.759988
3502.841436	425976.416740	49.764993
3503.244357	425971.221479	49.769997
3503.062910	425980.439538	49.775002
3502.976554	425976.393724	49.780007
3502.987112	425981.112361	49.785012
3502.878307	425988.896811	49.790017
3503.149369	425972.100664	49.795021
3502.807977	425960.078749	49.800026
3502.736643	425942.731958	49.805031
3503.098096	425943.279346	49.810036
3502.867872	425945.501239	49.815041
3503.213325	425939.300638	49.820045
3503.104363	425943.735147	49.825050
3502.666705	425938.277349	49.830055
3502.758844	425937.804819	49.835060
3502.984646	425935.431446	49.840065
3503.009627	425933.955236	49.845069
3502.869758	425942.810909	49.850074
3503.075464	425936.634169	49.855079
3502.833555	425944.492118	49.860084
3502.875441	425943.825140	49.865089
3503.063055	425940.595414	49.870093
3502.685204	425944.669776	49.875098
3502.947640	425945.183314	49.880103
3502.801737	425950.131702	49.885108
3502.989654	425941.876953	49.890113
3503.113375	425928.455915	49.895117
3502.871397	425916.518518	49.900122
3502.894207	425903.977572	49.905127
3503.013102	425909.286814	49.910132
3502.568406	425903.728695	49.915137
3502.905417	425905.752222	49.920141
3502.861631	425907.993041	49.925146
3503.147980	425900.330558	49.930151
3502.980459	425905.739464	49.935156
3502.899935	425903.621422	49.940161
3503.046899	425905.220582	49.945165
3502.913585	425914.582720	49.950170
3502.863022	425901.648242	49.955175
3502.883647	425909.055316	49.960180
3503.055561	425907.757046	49.965185
3503.000317	425902.893789	49.970189
3503.063466	425911.765565	49.975194
3503.269082	425904.421413	49.980199
3502.997900	425894.976104	49.985204
3503.024634	425884.972347	49.990209
3502.917640	425878.595199	49.995213
3502.468446	425876.590862	50.000218
3502.827349	425870.235675	50.005223
3502.696433	425875.638337	50.010228
3502.875994	425866.014537	50.015233
3503.217336	425864.738092	50.020237
3503.006434	425870.306685	50.025242
3503.216327	425869.204958	50.030247
3503.065925	425879.991235	50.035252
3503.056350	425870.196702	50.040257
3503.483320	425865.098827	50.045261
3502.997019	425850.157668	50.050266
3503.237567	425838.493143	50.055271
3503.044020	425839.947420	50.060276
3502.771915	425834.512088	50.065281
3503.254033	425826.105549	50.070285
3502.890933	425833.273622	50.075290
3503.236238	425824.687413	50.080295
3503.274988	425835.948988	50.085300
3502.847692	425815.769706	50.090305
3503.214785	425797.332797	50.095309
3502.933683	425794.436872	50.100314
3503.284620	425788.083024	50.105319
3503.228839	425790.884236	50.110324
3503.023039	425785.133025	50.115329
3503.425237	425781.359061	50.120333
3502.961738	425787.326107	50.125338
3503.397937	425766.288736	50.130343
3503.017323	425749.755979	50.135348
3502.858834	425741.154248	50.140353
3503.137004	425737.401454	50.145357
3502.822956	425743.647539	50.150362
3503.230617	425744.643862	50.155367
3503.169362	425746.278586	50.160372
3502.938306	425744.541537	50.165377
3502.977120	425744.940990	50.170381
3503.114344	425740.095594	50.175386
3503.296792	425723.162130	50.180391
3503.068536	425721.424601	50.185396
3503.176103	425710.950150	50.190401
3502.945522	425703.274355	50.195405
3503.081446	425712.793630	50.200410
3503.274233	425704.334936	50.205415
3503.238789	425705.356163	50.210420
3502.918792	425687.341037	50.215425
3502.909028	425660.542568	50.220429
3502.592004	425670.646780	50.225434
3502.689961	425664.945189	50.230439
3502.619809	425678.103475	50.235444
3502.774885	425695.791501	50.240449
3503.008194	425701.944135	50.245453
3502.962779	425696.216275	50.250458
3503.372229	425674.929602	50.255463
3503.419150	425669.896579	50.260468
3503.352408	425658.639743	50.265473
3503.023811	425654.635237	50.270477
3503.130591	425654.160201	50.275482
3503.147403	425655.274023	50.280487
3503.090319	425637.213967	50.285492
3503.123057	425630.508345	50.290497
3503.023203	425621.795043	50.295501
3502.943146	425630.386828	50.300506
3503.030697	425623.164266	50.305511
3503.103891	425624.319220	50.310516
3502.689000	425626.775706	50.315521
3502.976949	425628.756875	50.320525
3502.922445	425631.253340	50.325530
3502.914917	425626.838701	50.330535
3502.913546	425632.016266	50.335540
3502.614099	425630.493918	50.340545
3502.608188	425624.607022	50.345549
3502.883271	425626.184325	50.350554
3502.733439	425633.823621	50.355559
3503.170361	425633.546004	50.360564
3503.157258	425628.117158	50.365569
3503.234811	425604.399953	50.370573
3503.388046	425595.846459	50.375578
3503.271161	425592.059582	50.380583
3502.979447	425584.038881	50.385588
3502.752252	425591.133062	50.390593
3503.017103	425596.468209	50.395597
3502.831042	425591.474952	50.400602
3503.112532	425591.173116	50.405607
3503.275848	425590.180845	50.410612
3503.159655	425566.750475	50.415617
3503.284416	425549.471433	50.420621
3503.247597	425554.858099	50.425626
3503.371532	425550.573273	50.430631
3503.417543	425549.854822	50.435636
3503.027796	425532.156037	50.440641
3503.179443	425516.547399	50.445645
3503.189174	425512.079034	50.450650
3503.182999	425512.790722	50.455655
3502.879409	425504.822780	50.460660
3502.989252	425504.601010	50.465665
3503.366877	425506.414603	50.470669
3502.890584	425513.500582	50.475674
3502.984829	425503.637414	50.480679
3503.006224	425485.411569	50.485684
3502.621179	425476.899185	50.490689
3503.097845	425473.163216	50.495693
3502.937655	425474.967127	50.500698
3503.042833	425473.984779	50.505703
3502.987540	425471.151774	50.510708
3502.823600	425467.220638	50.515713
3503.338728	425465.559191	50.520717
3502.882506	425482.032037	50.525722
3502.861640	425464.879316	50.530727
3503.094059	425443.673424	50.535732
3503.079599	425426.925649	50.540737
3502.949678	425385.478211	50.545741
3502.757693	425352.924046	50.550746
3502.873762	425297.272814	50.555751
3502.448591	425236.688751	50.560756
3502.622275	425157.678303	50.565761
3502.387229	425084.676204	50.570765
3502.140487	425003.300600	50.575770
3501.985933	424913.381389	50.580775
3502.072158	424812.913478	50.585780
3501.373463	424705.828106	50.590785
3501.224445	424584.689360	50.595789
3501.089877	424467.100767	50.600794
3501.193566	424330.384904	50.605799
3500.497109	424195.124680	50.610804
3500.067058	424048.650728	50.615809
3500.060318	423888.093405	50.620813
3499.592562	423734.162030	50.625818
3499.258265	423570.155959	50.630823
3499.121881	423412.917178	50.635828
3498.420733	423229.326304	50.640833
3498.121543	423049.320373	50.645837
3497.583490	422873.059653	50.650842
3497.549200	422685.746590	50.655847
3497.518188	422498.685353	50.660852
3497.030803	422303.070576	50.665857
3496.996573	422086.309236	50.670861
3496.661521	421877.466047	50.675866
3495.865393	421647.631812	50.680871
3495.275509	421428.573527	50.685876
3494.776719	421201.324218	50.690881
3494.057553	420973.958140	50.695885
3493.423175	420746.651641	50.700890
3493.211426	420510.183303	50.705895
3492.373738	420289.202623	50.710900
3491.761036	420046.680649	50.715905
3491.821397	419801.426718	50.720909
3491.482212	419564.945745	50.725914
3490.819775	419308.412383	50.730919
3490.101956	419063.055586	50.735924
3489.687168	418816.857668	50.740929
3489.027927	418555.822698	50.745933
3488.500803	418297.174172	50.750938
3488.133999	418030.143336	50.755943
3487.296046	417770.146180	50.760948
3486.938329	417509.251941	50.765953
3486.409142	417236.782135	50.770957
3485.962024	416968.484381	50.775962
3485.194701	416703.259651	50.780967
3484.625865	416426.294181	50.785972
3483.848579	416151.062327	50.790977
3483.295000	415872.844172	50.795981
3482.491550	415603.018716	50.800986
3482.428962	415321.613218	50.805991
3481.723618	415042.751801	50.810996
3481.046506	414756.671737	50.816001
3480.647699	414461.197296	50.821005
3479.731867	414180.001137	50.826010
3479.246161	413892.583849	50.831015
3478.756117	413601.304632	50.836020
3477.876657	413317.858436	50.841025
3477.692074	413017.455712	50.846029
3476.770747	412727.332159	50.851034
3475.835977	412437.690117	50.856039
3475.455210	412146.223553	50.861044
3474.439285	411851.053249	50.866049
3473.972197	411557.639601	50.871053
3473.521212	411278.643435	50.876058
3473.041054	410976.337785	50.881063
3472.263909	410668.060972	50.886068
3471.262911	410380.972300	50.891073
3470.868720	410080.190746	50.896077
3470.166129	409782.582014	50.901082
3469.395364	409481.299272	50.906087
3469.106461	409186.355897	50.911092
3468.266889	408890.842995	50.916097
3467.784832	408582.643912	50.921101
3467.220885	408296.118367	50.926106
3466.499871	407985.362775	50.931111
3466.159749	407680.633812	50.936116
3465.155777	407370.401962	50.941121
3464.873544	407058.849611	50.946125
3463.926125	406750.023228	50.951130
3463.254215	406442.517770	50.956135
3462.937309	406130.351092	50.961140
3461.570730	405828.519545	50.966145
3461.301964	405508.971894	50.971149
3460.534827	405208.148668	50.976154
3460.034588	404905.701784	50.981159
3460.117581	404599.773792	50.986164
3458.916783	404285.196970	50.991169
3458.147658	403965.234150	50.996173
3457.259607	403658.496290	51.001178
3456.488058	403337.002557	51.006183
3456.124245	403028.110705	51.011188
3455.180646	402721.422748	51.016193
3454.808123	402415.624561	51.021197
3453.368966	402117.574987	51.026202
3453.025605	401794.669391	51.031207
3452.317232	401491.306257	51.036212
3451.469842	401182.374931	51.041217
3451.098542	400883.875847	51.046221
3450.327976	400578.887677	51.051226
3449.589068	400276.812239	51.056231
3449.239435	399964.734119	51.061236
3448.305714	399661.745434	51.066241
3447.736024	399351.781305	51.071245
3446.979431	399044.894301	51.076250
3446.045113	398736.637061	51.081255
3445.903376	398429.155750	51.086260
3444.721810	398122.483846	51.091265
3444.113825	397819.699455	51.096269
3443.324095	397511.531387	51.101274
3442.823950	397209.713014	51.106279
3441.984540	396904.113003	51.111284
3441.267062	396604.535818	51.116289
3440.853015	396294.232665	51.121293
3439.848671	395998.560128	51.126298
3439.496130	395687.681045	51.131303
3438.786845	395383.211597	51.136308
3438.298014	395075.042536	51.141313
3437.868588	394773.059799	51.146317
3436.798691	394470.446475	51.151322
3436.480668	394160.434637	51.156327
3435.909146	393855.620946	51.161332
3434.805956	393545.762155	51.166337
3434.361285	393240.488515	51.171341
3433.695509	392939.594643	51.176346
3432.533194	392623.485435	51.181351
3431.705762	392313.210983	51.186356
3431.225493	392018.527197	51.191361
3430.573775	391712.663447	51.196365
3429.338110	391417.086310	51.201370
3428.871543	391115.352360	51.206375
3428.446639	390816.683134	51.211380
3427.644118	390525.114636	51.216385
3427.258765	390223.586647	51.221389
3426.164320	389930.258007	51.226394
3425.628304	389627.479211	51.231399
3424.750967	389331.591860	51.236404
3423.984407	389041.324522	51.241409
3423.580370	388747.587098	51.246413
3422.721409	388455.830602	51.251418
3422.414497	388161.333999	51.256423
3421.601684	387856.399407	51.261428
3420.568382	387559.835483	51.266433
3420.222277	387267.675231	51.271437
3419.345209	386977.305724	51.276442
3418.545568	386683.743368	51.281447
3417.702250	386391.812315	51.286452
3417.336693	386099.796956	51.291457
3416.467841	385808.093574	51.296461
3415.688483	385522.624625	51.301466
3415.062913	385230.086441	51.306471
3414.516926	384942.818657	51.311476
3413.670060	384655.650484	51.316481
3413.238892	384358.089317	51.321485
3412.706447	384068.574596	51.326490
3412.196173	383775.139132	51.331495
3411.254476	383488.230814	51.336500
3410.257577	383201.837717	51.341505
3410.093699	382900.963826	51.346509
3409.172161	382620.373502	51.351514
3408.729290	382326.226996	51.356519
3408.284250	382026.892689	51.361524
3407.260315	381737.161312	51.366529
3406.743379	381441.468853	51.371533
3405.832263	381165.338005	51.376538
3405.214289	380864.954916	51.381543
3404.790090	380571.882431	51.386548
3403.744178	380281.913116	51.391553
3403.387732	379982.036537	51.396557
3402.508991	379696.660088	51.401562
3401.838963	379398.890858	51.406567
3401.475867	379101.930864	51.411572
3400.182192	378823.913691	51.416577
3399.729575	378526.658790	51.421581
3399.396046	378247.176329	51.426586
3398.476411	377955.995703	51.431591
3397.862471	377657.057336	51.436596
3396.726551	377380.323191	51.441601
3396.418501	377085.395139	51.446605
3395.602634	376802.296715	51.451610
3394.613759	376515.335700	51.456615
3394.631288	376222.937718	51.461620
3393.824299	375942.703470	51.466625
3392.968907	375653.017467	51.471629
3392.276609	375368.208027	51.476634
3391.514710	375071.509485	51.481639
3391.213919	374786.145291	51.486644
3390.298405	374509.019656	51.491649
3389.809348	374218.470828	51.496653
3389.218629	373934.293234	51.501658
3388.611757	373650.472027	51.506663
3387.678778	373347.355263	51.511668
3386.867266	373063.284536	51.516673
3386.276841	372770.859412	51.521677
3385.511808	372494.937909	51.526682
3384.906268	372205.866928	51.531687
3384.229404	371916.322648	51.536692
3383.290466	371634.016566	51.541697
3382.980118	371341.658882	51.546701
3381.841456	371068.943002	51.551706
3381.095506	370785.986959	51.556711
3380.815999	370502.974441	51.561716
3380.124058	370240.219882	51.566721
3379.754144	369944.580717	51.571725
3378.732247	369657.314668	51.576730
3378.154097	369364.605127	51.581735
3377.868063	369075.199920	51.586740
3376.855378	368808.548238	51.591745
3376.296312	368513.667101	51.596749
3375.675588	368223.879969	51.601754
3374.715159	367947.829633	51.606759
3374.356975	367663.129979	51.611764
3373.276929	367380.916375	51.616769
3372.981142	367089.360971	51.621773
3372.092401	366798.591143	51.626778
3371.711145	366521.159669	51.631783
3371.155303	366226.971671	51.636788
3370.284812	365954.527636	51.641793
3369.435192	365657.638770	51.646797
3368.692290	365383.541184	51.651802
3368.234107	365092.964237	51.656807
3367.581964	364805.215650	51.661812
3366.913597	364529.344313	51.666817
3366.046065	364243.332154	51.671821
3365.532396	363963.183113	51.676826
3364.822210	363681.921105	51.681831
3364.342036	363393.725498	51.686836
3363.360915	363119.168950	51.691841
3363.162571	362823.748862	51.696845
3362.505569	362539.493698	51.701850
3361.413224	362254.878414	51.706855
3361.133737	361973.555739	51.711860
3360.228292	361688.014183	51.716865
3359.330464	361392.244779	51.721869
3358.923629	361113.226666	51.726874
3358.005618	360818.066765	51.731879
3357.385600	360541.370060	51.736884
3356.341956	360256.680957	51.741889
3356.175878	359973.671231	51.746893
3355.431481	359693.810443	51.751898
3354.770651	359410.855741	51.756903
3354.290412	359125.757038	51.761908
3353.665762	358848.286193	51.766913
3353.326031	358556.597037	51.771917
3352.616780	358282.824895	51.776922
3351.707729	357980.189568	51.781927
3350.806345	357677.677833	51.786932
3350.123075	357407.252885	51.791937
3349.793573	357123.386023	51.796941
3348.956764	356843.470213	51.801946
3347.845919	356552.508732	51.806951
3347.416436	356279.845347	51.811956
3346.656515	355991.160156	51.816961
3346.029367	355701.076629	51.821965
3345.478121	355422.272447	51.826970
3344.406749	355140.960543	51.831975
3344.134047	354852.692920	51.836980
3343.247040	354574.754386	51.841985
3342.780131	354292.672102	51.846989
3342.319649	354013.563129	51.851994
3341.446656	353734.777132	51.856999
3340.686764	353442.029429	51.862004
3339.932752	353166.450087	51.867009
3339.561903	352883.527874	51.872013
3338.573566	352606.662058	51.877018
3337.619276	352330.195655	51.882023
3337.354118	352041.118834	51.887028
3336.421754	351768.918930	51.892033
3335.654526	351487.657855	51.897037
3335.367363	351202.929395	51.902042
3334.415444	350940.013278	51.907047
3333.751231	350660.891649	51.912052
3333.162653	350387.581239	51.917057
3332.726454	350105.465969	51.922061
3332.020336	349827.287459	51.927066
3331.031080	349549.944213	51.932071
3330.563184	349258.517397	51.937076
3330.059436	348989.483360	51.942081
3328.932888	348711.802095	51.947085
3328.393705	348437.326219	51.952090
3327.675569	348156.213393	51.957095
3326.991829	347877.408158	51.962100
3326.422647	347617.281752	51.967105
3326.071998	347327.450547	51.972109
3325.046940	347052.285865	51.977114
3324.449198	346778.751192	51.982119
3323.892775	346495.564917	51.987124
3323.206306	346225.324200	51.992129
3322.426481	345946.981412	51.997133
3321.507388	345666.727009	52.002138
3321.085233	345388.167072	52.007143
3320.418174	345127.152574	52.012148
3319.665965	344844.625602	52.017153
3319.019659	344568.796046	52.022157
3318.397203	344304.894107	52.027162
3317.629991	344019.540362	52.032167
3317.005352	343740.547093	52.037172
3316.146795	343478.919920	52.042177
3316.071358	343203.213794	52.047181
3315.322641	342919.020650	52.052186
3314.187022	342648.428668	52.057191
3313.991454	342366.097004	52.062196
3312.902133	342098.191174	52.067201
3312.595806	341820.938828	52.072205
3311.684995	341543.228310	52.077210
3311.087186	341266.964033	52.082215
3310.665779	340994.663062	52.087220
3310.000865	340714.030371	52.092225
3309.123727	340436.969334	52.097229
3308.875700	340156.923827	52.102234
3308.389591	339883.787948	52.107239
3307.845829	339595.545050	52.112244
3306.994744	339309.821295	52.117249
3306.279413	339023.996358	52.122253
3305.404524	338745.194986	52.127258
3304.601387	338460.476023	52.132263
3304.620726	338175.589514	52.137268
3303.655351	337895.119308	52.142273
3302.894629	337605.120582	52.147277
3302.232134	337328.056373	52.152282
3300.826640	337046.104286	52.157287
3300.343509	336766.716050	52.162292
3299.412359	336497.963835	52.167297
3298.755079	336215.955702	52.172301
3298.311173	335951.265489	52.177306
3297.348560	335685.084687	52.182311
3297.080450	335403.590951	52.187316
3295.832078	335136.947153	52.192321
3295.368906	334853.575075	52.197325
3294.754322	334589.492380	52.202330
3294.295442	334337.902835	52.207335
3293.740283	334055.789164	52.212340
3292.680696	333788.037367	52.217345
3292.119075	333520.937205	52.222349
3291.312913	333247.769497	52.227354
3290.328712	332977.888395	52.232359
3289.887531	332713.028658	52.237364
3289.771851	332446.076000	52.242369
3288.874399	332177.524914	52.247373
3288.149848	331910.062783	52.252378
3287.688224	331646.219316	52.257383
3287.362527	331366.673690	52.262388
3286.474684	331100.202594	52.267393
3285.268049	330815.256316	52.272397
3284.809710	330544.662453	52.277402
3283.780533	330287.297609	52.282407
3283.432305	330017.802216	52.287412
3282.854862	329755.521989	52.292417
3282.254157	329485.329048	52.297421
3281.595324	329218.682523	52.302426
3280.953129	328941.978405	52.307431
3280.191352	328675.448697	52.312436
3279.301614	328402.474753	52.317441
3278.721538	328137.209540	52.322445
3278.078474	327872.921040	52.327450
3277.465344	327607.582656	52.332455
3276.747463	327324.087794	52.337460
3275.888270	327062.199571	52.342465
3275.324411	326796.492703	52.347469
3274.666253	326533.600551	52.352474
3274.115402	326271.808820	52.357479
3273.654314	326004.960862	52.362484
3272.724836	325736.079070	52.367489
3272.075350	325469.515397	52.372493
3271.800608	325196.064979	52.377498
3270.970156	324934.976867	52.382503
3270.150774	324649.959206	52.387508
3269.368892	324399.983749	52.392513
3268.895670	324122.235170	52.397517
3268.164912	323856.696353	52.402522
3267.418139	323591.490013	52.407527
3266.910410	323313.921808	52.412532
3266.205785	323051.964077	52.417537
3265.415213	322790.274454	52.422541
3264.933652	322521.276370	52.427546
3264.230218	322248.573167	52.432551
3263.545750	321983.781987	52.437556
3262.863878	321713.109145	52.442561
3261.999578	321442.975394	52.447565
3261.363978	321174.837837	52.452570
3260.592057	320913.595353	52.457575
3260.318162	320637.935344	52.462580
3259.548963	320378.930274	52.467585
3259.058540	320107.276016	52.472589
3258.341415	319831.917340	52.477594
3257.891385	319573.490903	52.482599
3256.890639	319292.578093	52.487604
3256.238675	319026.801752	52.492609
3255.348292	318760.428650	52.497613
3254.687381	318497.960990	52.502618
3254.249616	318239.374447	52.507623
3253.764576	317966.437538	52.512628
3252.869325	317699.322753	52.517633
3252.730829	317424.542478	52.522637
3251.512379	317151.116546	52.527642
3250.671341	316890.633494	52.532647
3250.386312	316608.925202	52.537652
3249.617003	316348.224161	52.542657
3249.180766	316075.627660	52.547661
3248.409386	315816.121433	52.552666
3247.618226	315543.277957	52.557671
3247.164063	315260.727472	52.562676
3246.402259	315002.362145	52.567681
3245.792894	314723.094557	52.572685
3245.055122	314466.759762	52.577690
3244.319676	314191.763044	52.582695
3243.912688	313910.217382	52.587700
3243.127957	313650.145338	52.592705
3242.265075	313375.294524	52.597709
3241.765302	313105.217702	52.602714
3241.129652	312828.034748	52.607719
3240.353695	312557.952142	52.612724
3239.945053	312293.915840	52.617729
3238.929379	312021.988270	52.622733
3238.708800	311760.081909	52.627738
3237.063810	311483.600904	52.632743
3236.768005	311209.001510	52.637748
3235.865846	310945.528413	52.642753
3235.381283	310685.827383	52.647757
3235.083071	310417.488436	52.652762
3233.817666	310154.711102	52.657767
3233.463364	309888.162015	52.662772
3232.702172	309628.504624	52.667777
3232.389653	309366.223771	52.672781
3231.618129	309097.808290	52.677786
3230.640643	308824.615184	52.682791
3229.908638	308547.789366	52.687796
3229.370427	308304.281877	52.692801
3228.926707	308037.283444	52.697805
3228.110977	307766.681412	52.702810
3227.220476	307502.405340	52.707815
3227.097990	307236.011320	52.712820
3225.990268	306973.934729	52.717825
3225.373058	306703.778957	52.722829
3224.898434	306447.321110	52.727834
3224.256682	306176.913184	52.732839
3223.670472	305916.297214	52.737844
3222.734286	305649.324111	52.742849
3222.233930	305373.746352	52.747853
3221.849019	305108.535994	52.752858
3220.876874	304852.107279	52.757863
3220.533601	304574.284972	52.762868
3219.405528	304310.726712	52.767873
3218.944022	304039.313591	52.772877
3218.721040	303771.194295	52.777882
3217.823823	303504.818859	52.782887
3217.489811	303230.402451	52.787892
3216.411397	302963.114240	52.792897
3215.602131	302693.258551	52.797901
3215.416850	302418.661440	52.802906
3214.021208	302156.008074	52.807911
3213.382985	301889.456219	52.812916
3212.624600	301624.426350	52.817921
3211.886639	301361.505559	52.822925
3211.345971	301096.284191	52.827930
3210.794475	300843.565788	52.832935
3210.109135	300569.634122	52.837940
3209.218125	300308.595203	52.842945
3208.744597	300052.041994	52.847949
3208.482361	299781.575005	52.852954
3207.372615	299511.888568	52.857959
3206.886978	299250.089990	52.862964
3205.975316	298993.837920	52.867969
3205.449336	298737.010037	52.872973
3205.447816	298471.841970	52.877978
3204.367653	298205.558825	52.882983
3203.761561	297933.541228	52.887988
3203.172733	297674.276857	52.892993
3202.371690	297395.670724	52.897997
3202.163626	297131.221841	52.903002
3201.167483	296859.929981	52.908007
3200.656607	296586.110040	52.913012
3199.703946	296317.813964	52.918017
3199.277299	296045.149500	52.923021
3198.785219	295776.722418	52.928026
3197.462545	295510.066183	52.933031
3197.366666	295238.769064	52.938036
3196.011789	294974.204981	52.943041
3195.603675	294708.154411	52.948045
3194.701969	294441.168943	52.953050
3193.952620	294181.337576	52.958055
3193.370373	293913.150369	52.963060
3192.634862	293653.850122	52.968065
3192.014439	293389.309494	52.973069
3191.442278	293127.179074	52.978074
3190.683147	292869.663511	52.983079
3190.002167	292609.154706	52.988084
3189.587485	292354.227402	52.993089
3188.738393	292082.465468	52.998093
3188.160251	291818.677870	53.003098
3187.115483	291567.828884	53.008103
3186.856250	291297.135714	53.013108
3185.847039	291043.376588	53.018113
3185.462450	290788.618965	53.023117
3185.150495	290513.986011	53.028122
3184.060013	290258.864013	53.033127
3183.451446	289996.936478	53.038132
3183.004563	289742.492867	53.043137
3182.061963	289480.468500	53.048141
3181.801708	289216.391696	53.053146
3181.262306	288952.718526	53.058151
3180.233235	288678.331301	53.063156
3179.587152	288420.863236	53.068161
3178.845810	288149.685250	53.073165
3178.034098	287882.593137	53.078170
3177.408343	287624.941761	53.083175
3177.052477	287361.539566	53.088180
3176.371184	287107.640057	53.093185
3175.599761	286833.077615	53.098189
3175.137223	286576.847856	53.103194
3174.076965	286315.117323	53.108199
3173.605132	286049.542353	53.113204
3172.943925	285788.022776	53.118209
3172.345100	285520.533110	53.123213
3171.531536	285261.355946	53.128218
3170.452436	285006.731090	53.133223
3170.069837	284736.019809	53.138228
3169.633970	284486.937549	53.143233
3168.567317	284223.243383	53.148237
3168.178873	283960.909916	53.153242
3167.521391	283703.231270	53.158247
3166.950460	283438.763460	53.163252
3166.150982	283182.381480	53.168257
3165.791152	282915.279176	53.173261
3164.936383	282655.773446	53.178266
3164.251928	282401.229550	53.183271
3163.552243	282135.915666	53.188276
3163.014390	281864.487279	53.193281
3162.510202	281613.502069	53.198285
3161.608693	281342.822518	53.203290
3160.672390	281087.275456	53.208295
3160.515947	280819.956664	53.213300
3159.494957	280558.795199	53.218305
3159.084616	280298.114750	53.223309
3158.506480	280024.933068	53.228314
3157.544475	279774.023324	53.233319
3156.955170	279495.316493	53.238324
3156.189629	279239.686588	53.243329
3155.728551	278980.388053	53.248333
3155.218478	278710.376057	53.253338
3154.435421	278451.844843	53.258343
3153.565746	278186.070050	53.263348
3152.925654	277919.084195	53.268353
3152.339465	277664.822158	53.273357
3151.743315	277397.828074	53.278362
3150.720609	277139.692561	53.283367
3150.459740	276873.098899	53.288372
3149.756731	276610.986190	53.293377
3148.847719	276345.623096	53.298381
3148.108358	276084.738340	53.303386
3147.467509	275823.174288	53.308391
3147.365507	275557.545005	53.313396
3146.380611	275301.896510	53.318401
3145.793166	275035.101625	53.323405
3144.974743	274768.244007	53.328410
3144.465405	274514.601673	53.333415
3143.415038	274256.314577	53.338420
3143.213048	273991.668264	53.343425
3142.692474	273725.446169	53.348429
3142.393734	273465.170697	53.353434
3140.886517	273198.403476	53.358439
3139.950781	272926.597678	53.363444
3139.521701	272664.968388	53.368449
3138.802602	272411.054058	53.373453
3137.971580	272150.333327	53.378458
3137.378283	271903.858968	53.383463
3136.902944	271634.876451	53.388468
3136.176127	271378.848649	53.393473
3135.436503	271118.798929	53.398477
3135.041322	270862.459325	53.403482
3134.108472	270606.033067	53.408487
3133.638230	270334.068730	53.413492
3132.864205	270083.370560	53.418497
3132.032926	269829.931459	53.423501
3131.406725	269568.103726	53.428506
3130.496791	269312.793034	53.433511
3129.938421	269047.948099	53.438516
3130.001627	268804.924473	53.443521
3128.793284	268545.512922	53.448525
3128.394559	268281.888028	53.453530
3127.611493	268029.152395	53.458535
3127.096570	267759.842181	53.463540
3126.525890	267506.025721	53.468545
3125.840582	267246.422006	53.473549
3125.490768	266976.395392	53.478554
3124.405426	266722.513525	53.483559
3123.753202	266457.708195	53.488564
3122.914422	266186.924141	53.493569
3122.315233	265931.914557	53.498573
3121.613477	265660.495536	53.503578
3120.884801	265415.389329	53.508583
3120.035233	265146.822193	53.513588
3119.639847	264892.668592	53.518593
3118.520160	264643.222827	53.523597
3118.302046	264381.296416	53.528602
3117.699554	264125.955347	53.533607
3116.776180	263866.746899	53.538612
3116.297287	263608.812206	53.543617
3115.659431	263357.933733	53.548621
3114.962188	263094.051128	53.553626
3114.096241	262849.221872	53.558631
3113.593952	262585.102008	53.563636
3113.093374	262326.202706	53.568641
3112.048192	262062.710217	53.573645
3111.555110	261807.757003	53.578650
3110.598415	261561.516593	53.583655
3110.210992	261303.157911	53.588660
3109.584017	261041.045326	53.593665
3108.773198	260787.419489	53.598669
3108.407545	260528.623912	53.603674
3107.717736	260278.593749	53.608679
3107.241125	260022.465691	53.613684
3106.493829	259756.400304	53.618689
3105.933120	259499.013096	53.623693
3105.317836	259243.137786	53.628698
3104.193621	258979.581585	53.633703
3103.540299	258713.347147	53.638708
3102.693580	258458.046087	53.643713
3102.177720	258203.987352	53.648717
3101.904512	257942.628709	53.653722
3100.750104	257689.723207	53.658727
3100.508139	257422.679782	53.663732
3099.236962	257176.874350	53.668737
3098.636889	256917.685341	53.673741
3098.359059	256659.765622	53.678746
3097.490587	256418.602994	53.683751
3096.758712	256159.029006	53.688756
3096.187363	255899.936966	53.693761
3095.395900	255656.316255	53.698765
3094.714459	255399.407843	53.703770
3093.930924	255153.060715	53.708775
3093.582259	254891.052796	53.713780
3093.070222	254650.134992	53.718785
3092.132837	254391.105608	53.723789
3091.635306	254128.053553	53.728794
3091.234985	253883.322006	53.733799
3090.686268	253627.231585	53.738804
3089.958786	253361.875877	53.743809
3089.056316	253103.986816	53.748813
3088.613783	252843.192275	53.753818
3087.565622	252588.893760	53.758823
3086.873907	252316.222833	53.763828
3086.175870	252068.588223	53.768833
3085.257952	251816.738070	53.773837
3084.647958	251537.711857	53.778842
3084.331718	251300.148549	53.783847
3083.704142	251045.167394	53.788852
3083.117962	250794.814446	53.793857
3082.105462	250534.372659	53.798861
3081.831045	250283.228061	53.803866
3080.720534	250024.254898	53.808871
3079.995473	249762.312637	53.813876
3079.531420	249511.404491	53.818881
3078.855560	249267.154323	53.823885
3078.411143	249014.154665	53.828890
3077.364426	248759.577134	53.833895
3076.487919	248507.211831	53.838900
3076.078459	248260.955580	53.843905
3075.616120	248009.589428	53.848909
3074.948416	247741.627929	53.853914
3074.165170	247503.483795	53.858919
3073.317369	247246.530029	53.863924
3072.881859	246992.103705	53.868929
3072.284747	246749.445832	53.873933
3071.859701	246496.087671	53.878938
3070.895029	246242.847325	53.883943
3070.442904	245978.313732	53.888948
3069.601707	245718.711143	53.893953
3068.961652	245476.570745	53.898957
3069.033831	245221.473068	53.903962
3067.689872	244964.554616	53.908967
3067.626474	244697.739838	53.913972
3066.746609	244443.569405	53.918977
3066.316969	244190.697502	53.923981
3065.675074	243918.353811	53.928986
3064.599845	243658.334325	53.933991
3063.284263	243402.074390	53.938996
3062.915741	243145.423663	53.944001
3062.426397	242887.724154	53.949005
3061.951767	242633.918893	53.954010
3060.951195	242377.606013	53.959015
3060.361844	242119.211174	53.964020
3059.837621	241867.859944	53.969025
3058.697080	241618.065881	53.974029
3058.261681	241365.834040	53.979034
3057.927327	241122.982656	53.984039
3057.396747	240864.528029	53.989044
3056.581594	240603.651938	53.994049
3055.889869	240354.189872	53.999053
3055.109339	240072.909058	54.004058
3054.147727	239837.984528	54.009063
3053.448862	239577.242447	54.014068
3052.833632	239326.724196	54.019073
3052.175199	239079.218724	54.024077
3051.388987	238830.487451	54.029082
3050.560904	238579.013146	54.034087
3050.133716	238326.910353	54.039092
3049.580977	238078.012682	54.044097
3048.592077	237826.108290	54.049101
3048.292698	237576.174687	54.054106
3047.459984	237338.251060	54.059111
3046.872708	237089.334959	54.064116
3046.309750	236845.533860	54.069121
3045.155424	236593.379056	54.074125
3044.828729	236339.962623	54.079130
3043.766069	236092.860695	54.084135
3043.257243	235840.571084	54.089140
3042.623712	235605.824267	54.094145
3042.054643	235357.976796	54.099149
3041.910915	235102.187751	54.104154
3041.035662	234861.778588	54.109159
3039.936105	234614.684850	54.114164
3039.530266	234361.844794	54.119169
3038.872317	234119.565867	54.124173
3038.519040	233856.530885	54.129178
3037.185337	233609.402110	54.134183
3037.154057	233365.871139	54.139188
3036.267304	233117.240568	54.144193
3035.091396	232869.780275	54.149197
3034.658402	232621.684087	54.154202
3034.066205	232374.786910	54.159207
3033.263343	232130.472718	54.164212
3032.698013	231890.523969	54.169217
3032.231925	231653.232568	54.174221
3031.997223	231402.455821	54.179226
3031.005700	231155.374025	54.184231
3030.526170	230891.626688	54.189236
3029.769283	230651.024914	54.194241
3028.779932	230403.765652	54.199245
3028.893765	230147.710795	54.204250
3027.858758	229906.546501	54.209255
3026.967067	229651.020786	54.214260
3026.354812	229393.104900	54.219265
3025.480846	229151.226714	54.224269
3025.224576	228897.707383	54.229274
3024.306034	228651.508444	54.234279
3023.711673	228402.275045	54.239284
3023.029431	228144.245970	54.244289
3022.047868	227905.749694	54.249293
3022.027894	227649.671078	54.254298
3020.901762	227400.148293	54.259303
3020.403231	227157.776392	54.264308
3019.779276	226907.557521	54.269313
3018.822371	226661.979760	54.274317
3018.069253	226408.778951	54.279322
3017.676942	226168.733462	54.284327
3017.174530	225909.659203	54.289332
3016.672199	225665.100599	54.294337
3015.834397	225411.126725	54.299341
3015.164058	225156.589965	54.304346
3014.601471	224916.677701	54.309351
3014.079430	224664.764937	54.314356
3013.372245	224409.650251	54.319361
3012.488342	224158.895303	54.324365
3011.943481	223905.638303	54.329370
3011.139795	223652.375107	54.334375
3010.496315	223405.145668	54.339380
3010.356121	223157.754343	54.344385
3009.191984	222902.389773	54.349389
3008.924815	222647.891077	54.354394
3008.060962	222392.654533	54.359399
3007.432670	222136.257850	54.364404
3007.065312	221870.980984	54.369409
3006.115712	221622.279642	54.374413
3005.479316	221368.585240	54.379418
3004.730984	221109.715807	54.384423
3004.345690	220860.410400	54.389428
3003.535814	220597.249187	54.394433
3002.750355	220342.462099	54.399437
3002.182675	220078.649574	54.404442
3001.301894	219831.570068	54.409447
3000.680068	219575.509033	54.414452
2999.868624	219337.356618	54.419457
2998.760757	219075.395782	54.424461
2998.205727	218821.871475	54.429466
2997.442087	218580.733290	54.434471
2996.879791	218334.162956	54.439476
2996.508882	218083.588175	54.444481
2995.290611	217843.929826	54.449485
2994.876374	217605.687919	54.454490
2994.684254	217359.795049	54.459495
2993.737019	217105.043219	54.464500
2992.919000	216859.360326	54.469505
2992.639489	216615.826775	54.474509
2991.892694	216363.359689	54.479514
2991.157065	216119.828864	54.484519
2990.813434	215868.108948	54.489524
2990.107746	215612.224672	54.494529
2989.298030	215367.002315	54.499533
2988.824836	215105.299545	54.504538
2988.116249	214852.524190	54.509543
2987.023391	214605.034997	54.514548
2986.484071	214353.963476	54.519553
2985.973852	214109.686140	54.524557
2985.211049	213847.068657	54.529562
2984.270031	213607.220293	54.534567
2983.769445	213356.654014	54.539572
2983.505341	213111.598776	54.544577
2982.343312	212862.980108	54.549581
2981.646063	212625.104110	54.554586
2980.973994	212372.329092	54.559591
2980.637192	212129.656831	54.564596
2979.894251	211871.293651	54.569601
2979.379197	211629.671648	54.574605
2978.976774	211377.031537	54.579610
2978.030923	211140.347652	54.584615
2977.394340	210881.790888	54.589620
2976.651561	210628.574493	54.594625
2976.139784	210377.458119	54.599629
2975.345855	210123.564444	54.604634
2974.373314	209875.990982	54.609639
2973.520839	209623.203600	54.614644
2973.174303	209390.928652	54.619649
2972.204866	209147.939757	54.624653
2971.793638	208898.439975	54.629658
2971.285785	208644.985509	54.634663
2970.671924	208413.497250	54.639668
2970.057633	208163.321408	54.644673
2969.075964	207915.818811	54.649677
2968.756973	207661.011063	54.654682
2967.834687	207421.239844	54.659687
2967.492125	207175.005120	54.664692
2966.831391	206916.388038	54.669697
2965.819405	206666.093691	54.674701
2965.535067	206426.089064	54.679706
2964.808765	206172.883128	54.684711
2963.835125	205917.988951	54.689716
2963.313875	205667.817515	54.694721
2962.709534	205430.416531	54.699725
2962.029325	205174.850809	54.704730
2961.788068	204927.778155	54.709735
2960.500230	204676.798798	54.714740
2959.927256	204430.739121	54.719745
2959.396763	204181.757831	54.724749
2958.445235	203925.440548	54.729754
2957.856939	203680.506077	54.734759
2957.470521	203446.969155	54.739764
2956.577273	203190.300653	54.744769
2955.812476	202946.900777	54.749773
2955.455251	202702.299109	54.754778
2954.814612	202452.502089	54.759783
2953.989821	202204.774079	54.764788
2953.312691	201954.692169	54.769793
2952.710359	201716.271176	54.774797
2952.186529	201462.282255	54.779802
2951.315426	201211.446764	54.784807
2950.598826	200965.117350	54.789812
2950.139445	200724.498424	54.794817
2949.254147	200475.526342	54.799821
2949.168100	200218.437375	54.804826
2948.449449	199977.508803	54.809831
2947.816541	199722.717171	54.814836
2947.148609	199459.887694	54.819841
2946.437524	199207.351558	54.824845
2945.894983	198951.363442	54.829850
2944.625921	198708.891162	54.834855
2943.887256	198460.295624	54.839860
2942.925189	198195.573583	54.844865
2942.511319	197968.117719	54.849869
2942.292747	197721.205236	54.854874
2941.343065	197483.404980	54.859879
2940.851182	197227.567259	54.864884
2940.288526	196978.692373	54.869889
2939.176403	196739.522305	54.874893
2938.656254	196486.059685	54.879898
2938.252614	196242.964494	54.884903
2937.326962	195996.751820	54.889908
2936.931742	195743.830682	54.894913
2936.214630	195494.338492	54.899917
2935.531689	195248.494397	54.904922
2934.580496	194999.565913	54.909927
2934.308022	194759.597554	54.914932
2933.804254	194499.711942	54.919937
2932.733051	194266.551374	54.924941
2932.190261	194005.834334	54.929946
2931.305608	193762.894046	54.934951
2930.715753	193508.818298	54.939956
2930.078902	193264.526563	54.944961
2929.500979	193030.407923	54.949965
2928.632117	192784.044841	54.954970
2927.999707	192536.776821	54.959975
2926.968127	192304.265679	54.964980
2926.301961	192041.528524	54.969985
2925.637702	191807.760046	54.974989
2924.984810	191564.572137	54.979994
2923.963753	191325.088131	54.984999
2923.241002	191105.536107	54.990004
2923.181508	190859.627696	54.995009
2922.422315	190626.236221	55.000013
2921.773230	190383.968634	55.005018
2921.199222	190150.152769	55.010023
2920.551402	189900.454175	55.015028
2919.860694	189647.493059	55.020033
2918.986825	189427.336477	55.025037
2918.227819	189183.297908	55.030042
2917.432839	188946.648109	55.035047
2916.889806	188716.141469	55.040052
2916.444734	188481.342746	55.045057
2916.014017	188239.746369	55.050061
2915.223951	188002.984909	55.055066
2914.733991	187755.775387	55.060071
2913.350934	187521.687967	55.065076
2913.015063	187284.431787	55.070081
2912.356722	187055.936631	55.075085
2911.866075	186807.674893	55.080090
2911.206575	186572.984010	55.085095
2910.479315	186342.009033	55.090100
2909.975815	186095.521494	55.095105
2909.018850	185855.615628	55.100109
2908.485784	185615.587422	55.105114
2908.068663	185386.421301	55.110119
2907.348867	185148.552229	55.115124
2907.159838	184893.565948	55.120129
2905.986553	184666.720810	55.125133
2905.369112	184424.243176	55.130138
2904.821396	184175.404430	55.135143
2904.141851	183940.918639	55.140148
2903.430752	183693.967917	55.145153
2902.426614	183460.290424	55.150157
2902.030452	183214.675113	55.155162
2901.537690	182983.330123	55.160167
2900.960574	182742.341783	55.165172
2900.505973	182494.779904	55.170177
2899.547604	182252.229982	55.175181
2899.085766	181995.980080	55.180186
2898.659543	181756.611855	55.185191
2897.573947	181521.467628	55.190196
2897.172585	181270.110049	55.195201
2896.479817	181029.238091	55.200205
2895.988843	180776.536521	55.205210
2894.948208	180528.867392	55.210215
2893.888135	180277.028922	55.215220
2893.104752	180026.607729	55.220225
2892.345594	179802.040579	55.225229
2891.636385	179570.683497	55.230234
2891.446973	179334.365006	55.235239
2890.676171	179102.435156	55.240244
2890.146727	178855.742629	55.245249
2889.537229	178624.258138	55.250253
2888.667294	178375.208376	55.255258
2888.299792	178137.093369	55.260263
2887.734912	177897.969774	55.265268
2887.481564	177644.975365	55.270273
2886.127738	177405.836164	55.275277
2885.644724	177159.983551	55.280282
2884.808769	176912.449209	55.285287
2883.937356	176667.148847	55.290292
2883.570038	176427.642051	55.295297
2882.715992	176188.855754	55.300301
2882.375953	175950.262676	55.305306
2881.518900	175712.471607	55.310311
2880.333944	175473.096316	55.315316
2879.821310	175230.082792	55.320321
2879.203999	174997.190966	55.325325
2878.367114	174762.174723	55.330330
2877.853445	174525.615696	55.335335
2877.211648	174294.423576	55.340340
2876.452804	174057.336117	55.345345
2875.735143	173826.248212	55.350349
2875.118906	173581.199257	55.355354
2874.692257	173349.109613	55.360359
2873.642667	173126.300970	55.365364
2873.388312	172885.774020	55.370369
2872.646601	172662.724037	55.375373
2872.299327	172419.708813	55.380378
2871.339297	172179.980263	55.385383
2870.408826	171949.408362	55.390388
2869.966241	171712.087411	55.395393
2869.368328	171480.417654	55.400397
2868.782615	171241.800313	55.405402
2867.825526	171007.726009	55.410407
2867.551523	170775.711696	55.415412
2866.725928	170538.322073	55.420417
2865.791084	170304.514605	55.425421
2865.174714	170069.814193	55.430426
2864.853281	169828.779701	55.435431
2863.709521	169607.771924	55.440436
2863.403865	169371.266225	55.445441
2862.838901	169138.940741	55.450445
2862.127033	168889.606608	55.455450
2861.254489	168658.264796	55.460455
2860.615833	168423.741841	55.465460
2859.944496	168187.571810	55.470465
2859.382781	167961.230971	55.475469
2858.674660	167722.003645	55.480474
2858.138235	167486.590187	55.485479
2857.239705	167259.089082	55.490484
2856.380906	167023.376892	55.495489
2855.969197	166800.590926	55.500493
2855.695399	166561.817044	55.505498
2855.111161	166321.227424	55.510503
2854.272396	166100.337039	55.515508
2853.942552	165849.682050	55.520513
2852.855042	165620.898457	55.525517
2852.572861	165379.409935	55.530522
2851.931991	165136.126737	55.535527
2851.119989	164897.619040	55.540532
2850.358363	164647.922322	55.545537
2849.206335	164415.746734	55.550541
2848.387099	164172.143114	55.555546
2847.969581	163945.696041	55.560551
2846.974377	163712.098080	55.565556
2846.651127	163481.210505	55.570561
2845.953586	163259.356074	55.575565
2845.345776	163025.313961	55.580570
2844.772230	162787.438414	55.585575
2844.251250	162553.892813	55.590580
2843.518642	162320.384635	55.595585
2842.622237	162098.582833	55.600589
2842.158497	161860.668172	55.605594
2841.706699	161622.689185	55.610599
2840.758507	161390.367691	55.615604
2840.134830	161153.120281	55.620609
2839.243992	160928.601515	55.625613
2838.445677	160682.304607	55.630618
2838.016601	160454.745727	55.635623
2837.057094	160237.657928	55.640628
2836.687956	159994.000957	55.645633
2836.224946	159773.205626	55.650637
2835.875528	159530.044025	55.655642
2834.978870	159298.958968	55.660647
2834.261742	159069.523451	55.665652
2833.768775	158829.493949	55.670657
2832.727234	158595.613879	55.675661
2832.334610	158363.366743	55.680666
2831.485941	158125.704237	55.685671
2831.062315	157903.245878	55.690676
2830.563500	157658.454554	55.695681
2829.891517	157418.145846	55.700685
2829.179415	157177.565587	55.705690
2828.780869	156943.267029	55.710695
2827.792513	156705.840094	55.715700
2826.913153	156466.653485	55.720705
2826.459848	156239.656009	55.725709
2825.595069	156001.614301	55.730714
2825.034178	155766.790650	55.735719
2824.244934	155524.745308	55.740724
2823.973531	155291.083179	55.745729
2822.320872	155061.982582	55.750733
2822.362968	154820.053771	55.755738
2821.773051	154587.658374	55.760743
2821.001993	154361.285370	55.765748
2820.648986	154121.526745	55.770753
2819.594796	153879.358578	55.775757
2819.092206	153643.609025	55.780762
2818.941153	153411.285396	55.785767
2817.758192	153177.333604	55.790772
2817.703266	152924.406905	55.795777
2816.559589	152698.018071	55.800781
2815.815877	152460.625404	55.805786
2815.017585	152211.912554	55.810791
2814.076102	151980.266589	55.815796
2813.911142	151745.157454	55.820801
2812.904884	151514.072164	55.825805
2812.259049	151271.799450	55.830810
2811.811038	151041.575339	55.835815
2810.799244	150812.568013	55.840820
2810.420757	150574.768399	55.845825
2809.398359	150360.707557	55.850829
2808.495187	150117.837537	55.855834
2808.137813	149898.884252	55.860839
2807.696746	149665.144778	55.865844
2806.913287	149433.817747	55.870849
2806.392722	149203.299177	55.875853
2805.749378	148959.412998	55.880858
2805.046523	148724.999234	55.885863
2803.739074	148500.417897	55.890868
2803.357115	148269.538004	55.895873
2803.011878	148045.697765	55.900877
2802.109811	147817.783287	55.905882
2801.558217	147584.622347	55.910887
2800.983375	147360.062511	55.915892
2800.417742	147120.739851	55.920897
2799.570105	146896.114992	55.925901
2798.997575	146662.543795	55.930906
2798.650812	146428.859197	55.935911
2797.537045	146196.031913	55.940916
2797.234478	145959.202103	55.945921
2796.623918	145733.259578	55.950925
2795.710038	145498.953041	55.955930
2795.021737	145264.164435	55.960935
2794.268918	145035.237121	55.965940
2794.192085	144794.447415	55.970945
2793.291881	144576.139445	55.975949
2792.299907	144329.813095	55.980954
2791.707973	144093.871262	55.985959
2790.813029	143871.027609	55.990964
2790.689383	143643.209404	55.995969
2789.790484	143408.672211	56.000973
2788.957066	143175.918038	56.005978
2788.563671	142942.797753	56.010983
2787.532511	142714.657394	56.015988
2786.933189	142488.644177	56.020993
2786.103312	142258.832251	56.025997
2785.767467	142023.928206	56.031002
2785.194115	141786.180326	56.036007
2784.554002	141566.625708	56.041012
2784.042200	141323.301916	56.046017
2783.224028	141091.207146	56.051021
2782.501154	140856.300711	56.056026
2781.661931	140623.971068	56.061031
2780.621072	140396.966051	56.066036
2780.378349	140168.898056	56.071041
2779.245136	139939.458188	56.076045
2779.109092	139715.519321	56.081050
2778.766595	139480.824078	56.086055
2777.550508	139259.106762	56.091060
2776.761518	139022.469614	56.096065
2776.343401	138797.161068	56.101069
2775.471437	138575.046087	56.106074
2774.991116	138355.026695	56.111079
2773.973548	138118.460233	56.116084
2773.423764	137895.900494	56.121089
2773.023671	137680.638759	56.126093
2772.148878	137455.213656	56.131098
2771.647910	137226.560894	56.136103
2771.019482	137009.372068	56.141108
2770.233405	136757.991634	56.146113
2769.564310	136550.155799	56.151117
2769.043321	136317.114349	56.156122
2768.433670	136100.716245	56.161127
2767.346061	135877.651469	56.166132
2767.302213	135634.834400	56.171137
2766.122898	135417.940606	56.176141
2765.348612	135190.136407	56.181146
2765.245803	134965.879776	56.186151
2764.159950	134746.686367	56.191156
2763.728684	134519.616188	56.196161
2762.666984	134298.909002	56.201165
2762.388494	134069.095677	56.206170
2761.835022	133844.084704	56.211175
2761.067623	133620.980264	56.216180
2760.678847	133385.229293	56.221185
2759.693938	133164.923268	56.226189
2758.800520	132938.629259	56.231194
2758.461349	132707.920625	56.236199
2757.763383	132491.001819	56.241204
2757.051766	132259.546544	56.246209
2756.913379	132032.888252	56.251213
2755.679185	131799.771576	56.256218
2755.137596	131581.637355	56.261223
2754.545946	131357.870069	56.266228
2754.250330	131116.705192	56.271233
2753.406741	130899.377028	56.276237
2752.684728	130667.477311	56.281242
2751.959206	130441.388000	56.286247
2751.232858	130210.712397	56.291252
2750.700497	129976.840727	56.296257
2749.986902	129749.902725	56.301261
2748.988297	129524.171551	56.306266
2749.132156	129303.444626	56.311271
2747.953734	129057.349808	56.316276
2747.559456	128821.238951	56.321281
2746.692399	128602.036766	56.326285
2745.856030	128371.405940	56.331290
2745.316867	128129.047007	56.336295
2744.604965	127910.788918	56.341300
2744.146730	127674.049406	56.346305
2743.068711	127446.808872	56.351309
2742.197458	127222.482897	56.356314
2741.340009	126994.292960	56.361319
2740.956735	126781.959245	56.366324
2740.463826	126549.732692	56.371329
2740.041512	126330.495708	56.376333
2738.836239	126105.561313	56.381338
2738.536159	125878.694794	56.386343
2737.858710	125662.339877	56.391348
2736.984248	125436.273658	56.396353
2736.481377	125218.354418	56.401357
2735.803746	124993.363316	56.406362
2735.344923	124766.493941	56.411367
2734.280542	124549.043892	56.416372
2733.628837	124312.706057	56.421377
2732.784478	124104.205265	56.426381
2732.389606	123876.378518	56.431386
2732.284239	123661.756903	56.436391
2731.082876	123434.897204	56.441396
2730.421788	123208.416987	56.446401
2729.762472	122988.672467	56.451405
2729.012066	122759.580658	56.456410
2728.625047	122542.270527	56.461415
2728.048349	122324.765664	56.466420
2727.378600	122088.549788	56.471425
2726.668892	121864.679906	56.476429
2725.735058	121644.776051	56.481434
2725.299012	121414.776709	56.486439
2724.484638	121199.874400	56.491444
2723.938319	120965.742640	56.496449
2723.073631	120748.374611	56.501453
2722.186400	120521.838842	56.506458
2721.957805	120298.228747	56.511463
2721.215004	120089.166541	56.516468
2720.731027	119853.266842	56.521473
2719.980850	119635.429975	56.526477
2719.185042	119406.079300	56.531482
2718.933898	119181.426961	56.536487
2717.851849	118962.864072	56.541492
2717.069257	118734.443778	56.546497
2716.553257	118517.553363	56.551501
2715.616606	118292.770864	56.556506
2715.484244	118075.437010	56.561511
2714.443319	117853.839033	56.566516
2714.123111	117623.658702	56.571521
2713.227344	117405.926723	56.576525
2712.696530	117179.050787	56.581530
2712.103952	116952.123653	56.586535
2711.034449	116738.974271	56.591540
2710.463737	116514.142911	56.596545
2709.905780	116295.954989	56.601549
2709.392308	116073.657941	56.606554
2709.151002	115842.576282	56.611559
2708.022854	115626.307424	56.616564
2707.261568	115390.846763	56.621569
2706.945543	115183.245608	56.626573
2706.145738	114948.061917	56.631578
2705.239277	114721.460005	56.636583
2704.842609	114505.099972	56.641588
2704.140764	114274.859084	56.646593
2703.058595	114048.864147	56.651597
2702.178233	113827.536363	56.656602
2701.960540	113619.447064	56.661607
2700.825249	113399.969895	56.666612
2700.215484	113175.476221	56.671617
2699.475459	112964.826276	56.676621
2699.037968	112752.093899	56.681626
2698.558267	112529.488395	56.686631
2697.631350	112321.301222	56.691636
2697.430289	112102.144417	56.696641
2696.532689	111879.082016	56.701645
2695.763625	111660.698912	56.706650
2695.559264	111442.005071	56.711655
2694.491386	111225.937249	56.716660
2693.634852	111004.614851	56.721665
2693.387646	110792.106120	56.726669
2692.109840	110570.262230	56.731674
2691.592501	110352.964004	56.736679
2690.928751	110132.936463	56.741684
2690.524679	109920.727917	56.746689
2690.107923	109712.650808	56.751693
2688.990331	109488.083001	56.756698
2688.669713	109276.487450	56.761703
2688.146404	109052.355025	56.766708
2687.580645	108833.159295	56.771713
2686.535838	108614.517089	56.776717
2686.049879	108401.305537	56.781722
2685.630376	108174.698761	56.786727
2684.526276	107953.595517	56.791732
2684.213556	107735.406686	56.796737
2683.360872	107518.734227	56.801741
2682.325223	107301.028021	56.806746
2682.248849	107073.101813	56.811751
2681.384371	106854.036513	56.816756
2680.755421	106644.799864	56.821761
2679.923469	106425.465790	56.826765
2679.265531	106210.027688	56.831770
2678.828037	105991.734511	56.836775
2677.883314	105776.171109	56.841780
2677.145784	105548.624723	56.846785
2676.785751	105336.609379	56.851789
2676.035927	105124.294081	56.856794
2675.331210	104900.912622	56.861799
2674.555518	104680.427626	56.866804
2673.983845	104466.715701	56.871809
2673.336625	104252.281922	56.876813
2672.513417	104031.937385	56.881818
2671.783179	103809.775711	56.886823
2671.056171	103595.056122	56.891828
2670.344888	103387.179523	56.896833
2669.696548	103175.281425	56.901837
2668.949084	102959.288051	56.906842
2668.532158	102743.633557	56.911847
2668.136838	102544.077016	56.916852
2667.405003	102324.048501	56.921857
2666.484033	102111.062822	56.926861
2665.804719	101895.993387	56.931866
2665.390676	101673.554405	56.936871
2664.796591	101474.395467	56.941876
2664.059915	101247.939651	56.946881
2663.684154	101032.400094	56.951885
2662.874022	100813.261001	56.956890
2661.826922	100586.045084	56.961895
2661.266227	100385.638182	56.966900
2660.598973	100168.073454	56.971905
2660.064079	99947.885286	56.976909
2659.512638	99736.550724	56.981914
2658.661077	99522.793544	56.986919
2658.100044	99308.804390	56.991924
2657.528578	99093.593688	56.996929
2656.783984	98873.844073	57.001933
2655.665055	98661.117276	57.006938
2655.231562	98443.057408	57.011943
2654.389459	98228.312798	57.016948
2653.687900	98026.278912	57.021953
2653.512624	97817.352272	57.026957
2652.559649	97605.634151	57.031962
2651.681636	97390.331459	57.036967
2650.867111	97188.824942	57.041972
2650.617344	96971.596752	57.046977
2649.849705	96754.541449	57.051981
2649.755047	96553.577023	57.056986
2648.872590	96333.517398	57.061991
2648.179916	96124.229767	57.066996
2647.142431	95897.053765	57.072001
2646.589919	95688.399519	57.077005
2645.378935	95490.693534	57.082010
2644.953166	95277.533840	57.087015
2644.198009	95080.057813	57.092020
2643.710374	94865.585728	57.097025
2643.332994	94648.868979	57.102029
2642.401114	94446.820524	57.107034
2642.189275	94232.985792	57.112039
2641.331131	94033.422243	57.117044
2640.707521	93822.879047	57.122049
2640.479145	93603.448685	57.127053
2639.514180	93407.113303	57.132058
2639.004471	93184.428320	57.137063
2638.002856	92970.809229	57.142068
2637.697857	92754.102930	57.147073
2636.960276	92537.846886	57.152077
2636.498388	92323.011533	57.157082
2635.656093	92095.271980	57.162087
2634.807345	91897.754713	57.167092
2634.008644	91676.808020	57.172097
2633.686175	91468.422685	57.177101
2632.910099	91257.648169	57.182106
2632.350497	91029.013500	57.187111
2631.602496	90826.157280	57.192116
2630.461616	90619.257980	57.197121
2630.277930	90402.545316	57.202125
2629.517318	90197.646877	57.207130
2628.870224	89981.575564	57.212135
2628.179660	89761.871381	57.217140
2627.822062	89552.645424	57.222145
2626.920545	89335.081446	57.227149
2625.787886	89122.596991	57.232154
2625.567937	88900.345555	57.237159
2624.456030	88699.009625	57.242164
2624.424654	88488.747270	57.247169
2623.752533	88280.709137	57.252173
2622.724903	88065.316399	57.257178
2622.249985	87851.087389	57.262183
2621.496934	87646.317129	57.267188
2620.894406	87437.551094	57.272193
2620.194510	87219.318251	57.277197
2619.374056	87006.729324	57.282202
2619.142919	86787.747764	57.287207
2618.382125	86576.085121	57.292212
2617.744331	86369.199725	57.297217
2617.142167	86154.798292	57.302221
2616.623770	85943.797718	57.307226
2615.647700	85722.453625	57.312231
2615.041322	85512.912068	57.317236
2614.303697	85295.940424	57.322241
2613.322763	85084.747419	57.327245
2613.214887	84886.456749	57.332250
2612.667023	84657.119382	57.337255
2611.393044	84449.154147	57.342260
2610.921935	84234.411487	57.347265
2610.177812	84025.940729	57.352269
2609.406732	83826.129307	57.357274
2608.699616	83611.794276	57.362279
2608.149050	83397.770659	57.367284
2607.428688	83188.351745	57.372289
2607.025339	82985.135234	57.377293
2606.246110	82782.048178	57.382298
2605.056229	82559.051341	57.387303
2604.940675	82359.844524	57.392308
2604.069768	82152.566645	57.397313
2603.747145	81937.978286	57.402317
2602.678480	81742.739284	57.407322
2602.094315	81527.203554	57.412327
2601.296222	81325.172738	57.417332
2600.748922	81109.818546	57.422337
2600.058841	80904.690240	57.427341
2598.966243	80711.861680	57.432346
2598.759247	80496.106189	57.437351
2598.204503	80295.939304	57.442356
2597.577885	80091.162598	57.447361
2596.539235	79875.409213	57.452365
2596.235770	79680.152032	57.457370
2595.720105	79478.520456	57.462375
2594.614019	79215.126861	57.467380
2594.298278	79013.262256	57.472385
2593.475619	78808.226108	57.477389
2592.854691	78601.673219	57.482394
2592.237412	78388.379759	57.487399
2591.546635	78180.967401	57.492404
2590.754600	77978.527461	57.497409
2590.128788	77772.826451	57.502413
2589.443977	77566.446113	57.507418
2589.131720	77363.054463	57.512423
2587.887583	77164.593059	57.517428
2587.571561	76961.643260	57.522433
2587.194232	76746.751472	57.527437
2585.922077	76545.123075	57.532442
2585.534912	76326.495354	57.537447
2584.824013	76129.112459	57.542452
2584.420703	75929.763567	57.547457
2583.669482	75726.677355	57.552461
2582.687272	75512.883711	57.557466
2582.527462	75301.088577	57.562471
2581.571979	75107.130126	57.567476
2581.144025	74906.221920	57.572481
2580.381184	74693.368843	57.577485
2579.696413	74481.652207	57.582490
2579.104694	74275.533552	57.587495
2578.338522	74070.905072	57.592500
2577.040416	73859.666994	57.597505
2576.849919	73664.144625	57.602509
2576.244159	73458.727127	57.607514
2575.905446	73248.212267	57.612519
2575.134893	73038.819456	57.617524
2574.377938	72838.988063	57.622529
2573.460499	72632.870652	57.627533
2572.954296	72434.635948	57.632538
2572.668176	72220.006892	57.637543
2571.472366	72019.395661	57.642548
2570.835898	71816.522236	57.647553
2570.119476	71603.063323	57.652557
2569.676369	71400.369932	57.657562
2569.198053	71198.736915	57.662567
2568.203916	70996.927650	57.667572
2567.782154	70790.844287	57.672577
2567.051199	70587.675085	57.677581
2566.041811	70387.433727	57.682586
2565.279044	70184.001117	57.687591
2564.930807	69982.211314	57.692596
2564.190936	69786.899874	57.697601
2563.564342	69581.928083	57.702605
2562.946882	69380.227948	57.707610
2562.470315	69170.796631	57.712615
2561.551769	68979.041523	57.717620
2560.653028	68769.527782	57.722625
2560.432309	68573.720159	57.727629
2559.421031	68368.064928	57.732634
2558.804424	68166.965566	57.737639
2558.200537	67963.133690	57.742644
2557.357153	67778.806060	57.747649
2557.027312	67579.577626	57.752653
2556.038552	67380.210122	57.757658
2555.900428	67171.786385	57.762663
2555.031890	66970.310276	57.767668
2554.131198	66767.383617	57.772673
2553.358585	66561.381672	57.777677
2552.803911	66368.053738	57.782682
2552.105328	66161.028808	57.787687
2551.370167	65972.305554	57.792692
2551.099288	65769.768831	57.797697
2550.653244	65569.685315	57.802701
2549.750384	65376.571724	57.807706
2549.138477	65172.717218	57.812711
2548.311161	64966.721103	57.817716
2547.785910	64760.377460	57.822721
2547.012644	64555.745195	57.827725
2546.088985	64361.921889	57.832730
2545.882905	64157.843028	57.837735
2544.942405	63962.555837	57.842740
2543.970519	63758.256842	57.847745
2543.589067	63560.608818	57.852749
2542.820479	63369.512501	57.857754
2542.429932	63160.524987	57.862759
2541.325451	62974.217724	57.867764
2540.822522	62776.242964	57.872769
2540.426740	62576.331457	57.877773
2539.258728	62383.613957	57.882778
2538.946508	62181.758987	57.887783
2538.111699	61992.315355	57.892788
2537.570939	61791.460203	57.897793
2537.249315	61598.592619	57.902797
2535.967971	61400.453497	57.907802
2535.647590	61201.980890	57.912807
2534.962361	61011.411639	57.917812
2534.393559	60813.999171	57.922817
2534.155832	60610.657546	57.927821
2533.585195	60415.220028	57.932826
2532.730326	60199.244280	57.937831
2532.039323	60004.236803	57.942836
2530.919167	59788.716279	57.947841
2530.544919	59595.939775	57.952845
2529.592943	59410.335580	57.957850
2529.010799	59193.056457	57.962855
2528.099109	59000.890694	57.967860
2527.595994	58802.630885	57.972865
2527.055773	58611.805641	57.977869
2526.182409	58417.997674	57.982874
2525.744417	58231.137757	57.987879
2524.835764	58023.786201	57.992884
2524.213216	57826.506738	57.997889
2523.255313	57636.737808	58.002893
2522.653379	57457.022168	58.007898
2522.234120	57258.978481	58.012903
2521.905045	57055.827208	58.017908
2520.831626	56868.809673	58.022913
2520.281213	56672.073996	58.027917
2519.404347	56482.016921	58.032922
2519.124249	56279.308580	58.037927
2518.378299	56094.155621	58.042932
2517.660495	55891.000154	58.047937
2517.316788	55697.476130	58.052941
2516.425981	55504.744398	58.057946
2515.956319	55318.106864	58.062951
2515.202175	55115.168186	58.067956
2514.403459	54914.127093	58.072961
2513.996680	54721.041394	58.077965
2512.978805	54527.187778	58.082970
2512.312832	54328.283832	58.087975
2511.681781	54138.789748	58.092980
2510.996355	53937.359012	58.097985
2510.727017	53740.261936	58.102989
2509.826879	53541.716280	58.107994
2509.200371	53348.193649	58.112999
2508.818024	53155.556030	58.118004
2507.702591	52955.038605	58.123009
2507.050143	52758.453853	58.128013
2506.219697	52561.882479	58.133018
2505.708600	52367.583210	58.138023
2505.089155	52178.865979	58.143028
2504.180096	51979.710394	58.148033
2503.762350	51784.900485	58.153037
2502.812294	51605.898697	58.158042
2502.389279	51406.032392	58.163047
2501.524600	51220.774035	58.168052
2500.653329	51028.981827	58.173057
2500.545048	50828.320172	58.178061
2499.621728	50650.411960	58.183066
2499.282473	50459.623798	58.188071
2498.480565	50267.611828	58.193076
2497.673612	50075.228916	58.198081
2497.336891	49877.206550	58.203085
2496.461816	49694.054519	58.208090
2495.749513	49496.435907	58.213095
2495.190692	49296.234336	58.218100
2494.448043	49113.894804	58.223105
2493.873332	48919.304899	58.228109
2493.203552	48723.802203	58.233114
2492.593681	48523.503317	58.238119
2491.808196	48331.380963	58.243124
2491.022905	48142.778516	58.248129
2490.698738	47940.511549	58.253133
2489.622192	47766.367051	58.258138
2489.155306	47562.469199	58.263143
2488.746430	47373.581920	58.268148
2487.790394	47185.239661	58.273153
2487.227921	46985.600882	58.278157
2486.125173	46797.556639	58.283162
2485.385834	46605.009793	58.288167
2485.017840	46416.181910	58.293172
2484.384017	46235.380243	58.298177
2483.647729	46040.330881	58.303181
2482.525694	45862.915378	58.308186
2481.887915	45673.621680	58.313191
2481.511355	45490.253317	58.318196
2480.632446	45312.006667	58.323201
2480.449183	45121.858705	58.328205
2479.188064	44947.233118	58.333210
2478.892853	44765.475646	58.338215
2478.381117	44582.357572	58.343220
2477.239717	44388.730380	58.348225
2477.094794	44201.915604	58.353229
2476.003558	44026.848361	58.358234
2475.869390	43833.463028	58.363239
2474.907624	43646.723719	58.368244
2474.051422	43467.999776	58.373249
2473.543345	43278.555776	58.378253
2472.640892	43093.116079	58.383258
2472.552562	42913.249907	58.388263
2471.645576	42732.015394	58.393268
2471.027374	42549.109287	58.398273
2470.504929	42358.201800	58.403277
2469.838237	42184.851777	58.408282
2469.254297	41988.368176	58.413287
2468.311981	41806.657959	58.418292
2467.589904	41626.665516	58.423297
2467.186256	41441.065021	58.428301
2466.555629	41251.254031	58.433306
2466.237763	41061.746016	58.438311
2465.208377	40874.672263	58.443316
2464.182332	40692.673802	58.448321
2463.621578	40499.902096	58.453325
2462.716945	40323.777056	58.458330
2462.247757	40142.233185	58.463335
2461.460975	39957.440928	58.468340
2461.238111	39785.711639	58.473345
2460.378967	39590.670804	58.478349
2459.608592	39418.301043	58.483354
2459.033521	39231.697861	58.488359
2458.328645	39046.941806	58.493364
2457.499430	38863.044410	58.498369
2456.894545	38678.854126	58.503373
2456.035515	38507.498632	58.508378
2455.486680	38318.187822	58.513383
2454.991888	38137.323087	58.518388
2454.032814	37960.410105	58.523393
2453.557204	37775.197148	58.528397
2452.874914	37604.623687	58.533402
2452.229995	37428.386841	58.538407
2451.461232	37249.593611	58.543412
2450.615752	37072.093771	58.548417
2450.312227	36896.566349	58.553421
2449.349578	36721.552040	58.558426
2448.878840	36543.483742	58.563431
2448.179204	36362.370857	58.568436
2447.571762	36184.224995	58.573441
2446.677142	36015.845005	58.578445
2445.883335	35838.022352	58.583450
2445.227345	35670.104740	58.588455
2444.761093	35500.086705	58.593460
2443.798334	35326.104727	58.598465
2443.364692	35150.426455	58.603469
2442.578878	34977.857337	58.608474
2441.907963	34798.555575	58.613479
2441.348339	34631.757558	58.618484
2440.441930	34470.200222	58.623489
2439.976133	34292.146747	58.628493
2439.000356	34124.168359	58.633498
2438.609188	33953.253337	58.638503
2437.905546	33780.070890	58.643508
2437.028696	33626.654145	58.648513
2436.339193	33456.278934	58.653517
2435.640177	33294.247349	58.658522
2435.074954	33125.198730	58.663527
2434.168648	32961.601426	58.668532
2433.655851	32801.254145	58.673537
2432.732799	32636.393918	58.678541
2431.531758	32488.724692	58.683546
2430.822770	32339.083724	58.688551
2430.151344	32186.318037	58.693556
2429.387539	32046.522095	58.698561
2428.937435	31893.996309	58.703565
2427.781840	31745.468049	58.708570
2426.747893	31602.570654	58.713575
2426.078732	31461.304619	58.718580
2425.103365	31333.177062	58.723585
2424.755336	31198.125468	58.728589
2424.037290	31074.811994	58.733594
2423.162674	30936.195245	58.738599
2422.399165	30808.478140	58.743604
2421.835455	30690.186875	58.748609
2421.367968	30549.051757	58.753613
2420.633531	30422.170793	58.758618
2419.771193	30289.276637	58.763623
2419.364974	30173.245928	58.768628
2418.577461	30043.944020	58.773633
2417.805116	29919.607056	58.778637
2416.984358	29799.625774	58.783642
2416.332092	29675.428161	58.788647
2416.003702	29549.692422	58.793652
2414.982715	29422.994127	58.798657
2414.727846	29307.189946	58.803661
2413.617961	29180.271339	58.808666
2412.943286	29064.458277	58.813671
2412.397194	28943.660829	58.818676
2411.740140	28824.319290	58.823681
2411.342573	28710.764007	58.828685
2410.430741	28587.099225	58.833690
2409.929741	28472.747052	58.838695
2408.930516	28349.418361	58.843700
2408.381850	28237.808830	58.848705
2407.853237	28108.128864	58.853709
2407.149223	27998.176417	58.858714
2406.587518	27877.907685	58.863719
2405.796080	27761.534815	58.868724
2405.551803	27649.146308	58.873729
2404.956341	27527.636347	58.878733
2404.643780	27407.113154	58.883738
2403.945898	27280.684991	58.888743
2403.411066	27152.597784	58.893748
2402.195006	27029.647541	58.898753
2401.836575	26900.889940	58.903757
2401.016145	26779.246508	58.908762
2399.985353	26657.835987	58.913767
2399.461179	26539.455076	58.918772
2398.809723	26421.030310	58.923777
2398.309047	26289.322164	58.928781
2397.279626	26179.708764	58.933786
2396.325326	26059.778986	58.938791
2396.043192	25941.205771	58.943796
2395.149284	25825.179570	58.948801
2394.538851	25717.426686	58.953805
2393.989883	25604.331713	58.958810
2393.295231	25483.124910	58.963815
2392.584795	25369.157721	58.968820
2391.898321	25256.787456	58.973825
2391.473767	25137.643170	58.978829
2390.437922	25030.138062	58.983834
2389.957269	24912.187711	58.988839
2389.668927	24799.641642	58.993844
2388.699726	24694.261920	58.998849
2388.278426	24579.352329	59.003853
2387.328200	24464.669924	59.008858
2387.231552	24343.239171	59.013863
2386.412651	24227.818008	59.018868
2385.354500	24110.838354	59.023873
2384.992140	23994.499492	59.028877
2384.282561	23872.085830	59.033882
2383.663713	23757.958622	59.038887
2383.220034	23641.756207	59.043892
2381.992332	23530.605980	59.048897
2381.575877	23418.426002	59.053901
2380.885804	23310.369668	59.058906
2380.437058	23183.071741	59.063911
2379.781427	23068.424134	59.068916
2378.778820	22954.076944	59.073921
2378.622724	22839.573126	59.078925
2377.617459	22732.826526	59.083930
2376.959238	22612.730877	59.088935
2376.661758	22491.075554	59.093940
2375.749229	22380.435402	59.098945
2375.223098	22266.526738	59.103949
2374.424301	22151.995102	59.108954
2374.033647	22034.602391	59.113959
2373.162405	21904.100854	59.118964
2372.489566	21797.518253	59.123969
2371.790754	21671.267147	59.128973
2370.993176	21553.297535	59.133978
2370.328917	21448.546393	59.138983
2369.913943	21334.903168	59.143988
2369.078160	21227.629492	59.148993
2368.781761	21105.253437	59.153997
2368.337047	20996.437770	59.159002
2367.634528	20867.979963	59.164007
2366.574068	20745.460477	59.169012
2365.916081	20629.697688	59.174017
2365.377343	20516.240746	59.179021
2364.837565	20395.051206	59.184026
2363.961120	20279.799244	59.189031
2363.118717	20165.601401	59.194036
2362.161932	20041.415712	59.199041
2361.607630	19929.781707	59.204045
2360.924552	19817.416414	59.209050
2360.399509	19702.667888	59.214055
2359.611013	19589.971192	59.219060
2358.730002	19487.267289	59.224065
2358.361929	19375.639866	59.229069
2357.726267	19274.924992	59.234074
2356.908660	19161.828291	59.239079
2356.350457	19047.390213	59.244084
2355.974165	18945.311465	59.249089
2355.555602	18813.448984	59.254093
2354.397693	18721.066926	59.259098
2353.650202	18595.430270	59.264103
2353.442742	18478.087681	59.269108
2352.502631	18373.984368	59.274113
2351.796360	18262.736674	59.279117
2351.285407	18147.901451	59.284122
2350.492910	18040.931379	59.289127
2349.666036	17925.255476	59.294132
2348.915805	17817.002458	59.299137
2348.398795	17699.700833	59.304141
2347.522269	17600.497619	59.309146
2346.904973	17492.342507	59.314151
2346.414976	17384.477696	59.319156
2345.681719	17286.717029	59.324161
2345.128502	17172.237097	59.329165
2344.437432	17062.862957	59.334170
2343.826462	16948.218990	59.339175
2343.197748	16842.412366	59.344180
2342.479062	16729.558497	59.349185
2341.943651	16622.686268	59.354189
2341.363363	16513.380540	59.359194
2340.674156	16414.485802	59.364199
2339.989883	16294.600591	59.369204
2339.102944	16196.675010	59.374209
2338.856772	16068.242091	59.379213
2337.901395	15964.004630	59.384218
2336.928068	15857.749523	59.389223
2336.668787	15752.989764	59.394228
2335.604997	15638.422729	59.399233
2335.512739	15526.612508	59.404237
2334.502688	15427.127362	59.409242
2333.605505	15321.940479	59.414247
2333.414389	15206.193631	59.419252
2332.656651	15109.110490	59.424257
2331.962723	14989.095669	59.429261
2331.441509	14896.142278	59.434266
2330.696345	14777.917203	59.439271
2329.766623	14667.423817	59.444276
2329.326009	14560.347905	59.449281
2328.696504	14445.629499	59.454285
2327.587002	14348.840099	59.459290
2327.214534	14245.452432	59.464295
2326.598574	14133.780638	59.469300
2325.493477	14036.086824	59.474305
2325.183125	13917.028697	59.479309
2324.469947	13815.223751	59.484314
2323.773036	13708.688624	59.489319
2323.459710	13606.527409	59.494324
2322.385943	13509.234309	59.499329
2321.755866	13388.951531	59.504333
2321.205394	13296.348707	59.509338
2320.680539	13193.832751	59.514343
2320.198012	13082.875283	59.519348
2319.421281	12981.963336	59.524353
2318.804032	12870.916561	59.529357
2317.716966	12765.653570	59.534362
2316.876804	12656.695790	59.539367
2316.628733	12553.141016	59.544372
2316.003137	12457.510879	59.549377
2315.476263	12346.668664	59.554381
2314.660615	12239.114163	59.559386
2313.905439	12134.724390	59.564391
2313.285696	12033.399564	59.569396
2312.489953	11930.103533	59.574401
2311.968371	11823.160357	59.579405
2311.220909	11714.791814	59.584410
2310.468242	11617.957455	59.589415
2310.040779	11506.906411	59.594420
2309.389143	11400.830376	59.599425
2308.803383	11305.348667	59.604429
2307.726894	11210.790401	59.609434
2306.883044	11112.358305	59.614439
2306.423749	10997.753322	59.619444
2306.152042	10899.689180	59.624449
2305.647376	10790.458929	59.629453
2304.743241	10690.064761	59.634458
2303.956974	10592.711367	59.639463
2303.513814	10481.110684	59.644468
2302.532565	10384.103121	59.649473
2302.142354	10281.716645	59.654477
2301.336514	10180.692650	59.659482
2300.588013	10081.746490	59.664487
2299.974217	9977.885060	59.669492
2298.869688	9881.873189	59.674497
2298.374754	9781.729042	59.679501
2298.051124	9683.774307	59.684506
2297.059219	9585.804892	59.689511
2296.274919	9488.118111	59.694516
2295.212436	9400.386457	59.699521
2294.624391	9310.632576	59.704525
2293.552932	9224.216225	59.709530
2292.516665	9147.857531	59.714535
2292.098686	9062.009605	59.719540
2291.165870	8986.735084	59.724545
2290.418318	8911.105382	59.729549
2289.417404	8847.816157	59.734554
2288.836269	8765.672211	59.739559
2288.266483	8693.689196	59.744564
2287.268746	8641.709587	59.749569
2286.828693	8564.242247	59.754573
2286.070792	8504.565138	59.759578
2284.972518	8434.664099	59.764583
2284.510665	8369.031900	59.769588
2283.549933	8316.047850	59.774593
2283.119493	8259.719908	59.779597
2282.672223	8197.735800	59.784602
2281.954512	8142.338070	59.789607
2281.327297	8074.781276	59.794612
2280.543019	8030.424630	59.799617
2279.672419	7961.974763	59.804621
2279.066303	7906.161476	59.809626
2278.519742	7849.941705	59.814631
2278.116273	7780.768227	59.819636
2277.431592	7734.833882	59.824641
2276.480506	7672.392973	59.829645
2275.856018	7615.949611	59.834650
2275.124995	7556.085026	59.839655
2274.508422	7499.146296	59.844660
2273.734264	7444.360090	59.849665
2273.365830	7389.609734	59.854669
2272.629815	7327.937409	59.859674
2272.223604	7277.020490	59.864679
2271.546200	7214.433467	59.869684
2270.635745	7156.350457	59.874689
2269.832733	7099.670118	59.879693
2269.366465	7050.746563	59.884698
2268.726958	6996.301374	59.889703
2268.046052	6924.718051	59.894708
2267.215211	6884.489674	59.899713
2266.983701	6830.990934	59.904718
2266.149071	6775.553152	59.909722
2265.372270	6725.799933	59.914727
2264.533075	6666.933325	59.919732
2263.775345	6621.956857	59.924737
2263.229468	6560.813335	59.929742
2262.805954	6512.519873	59.934746
2261.915897	6457.666828	59.939751
2261.335864	6397.064441	59.944756
2260.378411	6354.763825	59.949761
2259.819802	6306.615709	59.954766
2259.312500	6259.059964	59.959770
2258.627221	6208.240759	59.964775
2257.827157	6145.965569	59.969780
2257.292660	6097.950584	59.974785
2257.023754	6049.189037	59.979790
2255.902684	6003.348502	59.984794
2255.451323	5960.703352	59.989799
2255.180865	5892.208662	59.994804
2254.309769	5847.282983	59.999809
2254.124294	5786.530147	60.004814
2253.539554	5731.238843	60.009818
2252.667730	5677.314869	60.014823
2252.114902	5614.701747	60.019828
2251.272385	5562.586343	60.024833
2250.505517	5485.505635	60.029838
2249.833999	5437.030400	60.034842
2248.825265	5384.010569	60.039847
2248.704172	5324.591772	60.044852
2247.483916	5276.436721	60.049857
2247.320912	5223.885603	60.054862
2246.749183	5171.894956	60.059866
2245.683997	5114.543930	60.064871
2244.781438	5053.444279	60.069876
2243.871563	5009.506026	60.074881
2243.389745	4955.855000	60.079886
2242.807796	4908.850667	60.084890
2242.079950	4857.011728	60.089895
2241.784459	4802.290137	60.094900
2240.869829	4761.533416	60.099905
2240.212229	4712.660014	60.104910
2239.798567	4667.410698	60.109914
2238.790671	4624.211246	60.114919
2238.226313	4564.008773	60.119924
2237.322303	4516.737704	60.124929
2236.789217	4461.911830	60.129934
2236.160536	4417.342782	60.134938
2235.266847	4373.180053	60.139943
2235.078655	4322.890689	60.144948
2234.248238	4284.363414	60.149953
2233.855415	4227.300969	60.154958
2233.447266	4175.017132	60.159962
2232.539097	4126.762460	60.164967
2232.204693	4071.483078	60.169972
2230.957658	4019.257935	60.174977
2230.362087	3966.381444	60.179982
2229.923017	3913.228053	60.184986
2229.096265	3870.116549	60.189991
2228.582938	3811.158196	60.194996
2227.809369	3770.278836	60.200001
2227.253091	3711.683531	60.205006
2226.556604	3669.223847	60.210010
2226.047936	3622.717735	60.215015
2225.444809	3568.292266	60.220020
2224.877069	3518.702055	60.225025
2224.626711	3450.901408	60.230030
2223.654459	3411.471937	60.235034
2222.673689	3347.216442	60.240039
2222.235427	3292.101251	60.245044
2221.442280	3247.839988	60.250049
2220.648984	3192.040481	60.255054
2220.142000	3135.809254	60.260058
2219.182071	3092.873463	60.265063
2218.732292	3036.616225	60.270068
2217.660879	2991.996630	60.275073
2217.116416	2938.566867	60.280078
2216.577318	2890.763720	60.285082
2215.498831	2845.112189	60.290087
2215.160905	2795.707611	60.295092
2214.470361	2757.423866	60.300097
2214.066502	2704.495129	60.305102
2213.419979	2655.013488	60.310106
2212.564041	2605.238566	60.315111
2212.283101	2560.869531	60.320116
2210.826965	2529.854159	60.325121
2210.208046	2477.394857	60.330126
2210.171910	2423.629617	60.335130
2209.124482	2379.151362	60.340135
2208.780520	2334.422651	60.345140
2208.092193	2277.327779	60.350145
2207.510364	2230.446668	60.355150
2207.199151	2182.778823	60.360154
2205.990143	2133.191317	60.365159
2205.328789	2077.632169	60.370164
2204.659722	2034.408720	60.375169
2204.107480	1987.208251	60.380174
2203.322397	1945.942411	60.385178
2202.327225	1896.890708	60.390183
2201.751010	1840.644368	60.395188
2201.351010	1800.927248	60.400193
2200.759502	1762.801899	60.405198
2200.314425	1722.549098	60.410202
2198.973785	1674.259851	60.415207
2198.521487	1625.703953	60.420212
2198.019101	1578.138931	60.425217
2197.535565	1536.150723	60.430222
2197.269726	1488.920931	60.435226
2196.481632	1441.303734	60.440231
2195.628149	1382.112637	60.445236
2194.946873	1336.537314	60.450241
2194.284528	1297.468728	60.455246
2193.741218	1243.539252	60.460250
2192.552112	1197.628407	60.465255
2191.937206	1144.932868	60.470260
2191.168282	1111.176935	60.475265
2190.636676	1065.170613	60.480270
2190.106467	1021.983451	60.485274
2189.435273	971.357110	60.490279
2188.362228	931.505850	60.495284
2187.683640	886.755206	60.500289
2186.882599	855.303108	60.505294
2186.314114	811.891755	60.510298
2185.729437	781.653336	60.515303
2185.088915	740.631221	60.520308
2184.330377	695.633483	60.525313
2183.792625	665.643447	60.530318
2183.191528	622.162411	60.535322
2182.448661	590.312875	60.540327
2182.110472	545.697230	60.545332
2181.212501	508.728657	60.550337
2180.372950	472.462276	60.555342
2179.785765	435.095338	60.560346
2178.842025	397.650919	60.565351
2178.132193	360.868413	60.570356
2177.550492	328.588438	60.575361
2176.981715	285.666879	60.580366
2176.399642	249.752102	60.585370
2175.565258	227.002374	60.590375
2174.972098	187.349626	60.595380
2174.050835	156.772894	60.600385
2173.178920	128.590455	60.605390
2172.865262	105.955919	60.610394
2171.820156	78.759994	60.615399
2171.480640	47.995172	60.620404
2170.301908	27.599136	60.625409
2169.097651	9.453443	60.630414
2167.326370	23.265652	60.635418
2165.662135	56.068872	60.640423
2165.518477	52.019951	60.645428
2164.936247	58.453616	60.650433
2165.203839	56.206122	60.655438
2164.472240	48.441603	60.660442
2163.628496	55.889030	60.665447
2163.529517	52.889528	60.670452
2162.768253	57.530996	60.675457
2161.672522	62.203618	60.680462
2160.919482	59.127300	60.685466
2159.852116	69.806660	60.690471
2160.021280	58.457174	60.695476
2159.411373	63.100389	60.700481
2158.406227	67.060839	60.705486
2158.045820	60.185291	60.710490
2156.685263	65.806722	60.715495
2156.743040	57.801804	60.720500
2156.588359	66.544091	60.725505
2155.865657	73.049154	60.730510
2155.169782	62.524162	60.735514
2153.957615	74.061544	60.740519
2153.551366	64.035679	60.745524
2152.785210	59.573375	60.750529
2151.823588	58.173189	60.755534
2151.153190	62.685440	60.760538
2150.289445	74.285990	60.765543
2149.993174	62.123643	60.770548
2149.508265	76.477309	60.775553
2148.962809	71.380834	60.780558
2148.627174	68.684688	60.785562
2147.691887	72.659244	60.790567
2146.973770	63.292615	60.795572
2146.184403	67.759297	60.800577
2145.497980	68.157755	60.805582
2144.979966	70.827840	60.810586
2144.196322	73.670061	60.815591
2143.666681	72.249675	60.820596
2142.849183	71.487180	60.825601
2141.983198	72.552638	60.830606
2141.667627	67.777622	60.835610
2141.540287	71.096123	60.840615
2140.741087	71.330720	60.845620
2139.513023	75.477715	60.850625
2138.744403	73.098376	60.855630
2138.805944	68.884099	60.860634
2138.070791	72.242610	60.865639
2137.192467	69.960979	60.870644
2136.176203	75.626948	60.875649
2135.949834	75.358195	60.880654
2135.738519	68.292944	60.885658
2134.058815	69.364950	60.890663
2133.478538	64.375483	60.895668
2133.277568	59.550477	60.900673
2132.607986	65.796990	60.905678
2132.483570	69.141041	60.910682
2131.019810	68.927220	60.915687
2130.838017	68.646897	60.920692
2129.845908	69.705114	60.925697
2129.051516	66.976121	60.930702
2128.737914	64.265157	60.935706
2128.037010	73.239414	60.940711
2127.133593	70.440256	60.945716
2126.454730	68.951056	60.950721
2126.205666	76.850973	60.955726
2125.844834	70.309432	60.960730
2124.053470	75.752723	60.965735
2123.942634	62.855273	60.970740
2123.804709	67.109490	60.975745
2122.447656	71.438016	60.980750
2121.965354	65.616302	60.985754
2121.270413	65.999642	60.990759
2121.022487	69.394816	60.995764
2119.624508	77.023099	61.000769
2119.613951	77.941464	61.005774
2118.542610	71.310269	61.010778
2117.771024	76.101928	61.015783
2117.960372	71.187267	61.020788
2116.700537	69.893353	61.025793
2115.545603	73.476025	61.030798
2115.689590	72.240021	61.035802
2115.037500	83.126249	61.040807
2114.272863	74.340711	61.045812
2113.361091	66.958706	61.050817
2112.646768	67.165765	61.055822
2112.202238	75.057666	61.060826
2111.514569	80.162197	61.065831
2110.875400	73.958776	61.070836
2110.399492	78.627235	61.075841
2109.582502	78.126358	61.080846
2108.824961	72.001998	61.085850
2108.075511	77.554839	61.090855
2107.675077	78.237531	61.095860
2107.071487	78.984969	61.100865
2106.393007	76.663241	61.105870
2106.452626	67.786860	61.110874
2105.594637	77.324807	61.115879
2104.225857	76.986989	61.120884
2103.723440	78.429988	61.125889
2102.428791	79.097869	61.130894
2102.081410	77.997615	61.135898
2101.211376	85.888092	61.140903
2100.982960	75.203812	61.145908
2100.353063	76.552568	61.150913
2099.524416	77.126930	61.155918
2099.193154	73.883747	61.160922
2098.481081	72.744427	61.165927
2098.031527	70.029482	61.170932
2097.390422	72.650363	61.175937
2096.850167	71.184431	61.180942
2096.026498	66.947490	61.185946
2094.385066	76.420103	61.190951
2094.240693	80.815157	61.195956
2094.159106	71.246115	61.200961
2092.837311	71.997191	61.205966
2092.346852	66.808428	61.210970
2091.307242	66.420628	61.215975
2091.499243	55.627352	61.220980
2091.011592	62.196418	61.225985
2089.948310	70.200858	61.230990
2089.913460	59.061134	61.235994
2088.941787	75.322446	61.240999
2087.651435	70.483251	61.246004
2086.631131	69.664273	61.251009
2086.147242	79.363226	61.256014
2086.380075	64.736149	61.261018
2085.394522	73.196224	61.266023
2084.912003	69.628797	61.271028
2084.318063	72.721987	61.276033
2083.537799	77.619339	61.281038
2082.743321	62.306698	61.286042
2081.289377	72.630626	61.291047
2081.340970	68.751196	61.296052
2080.296980	65.959120	61.301057
2079.500945	72.627908	61.306062
2079.714707	60.694508	61.311066
2078.022243	73.943846	61.316071
2077.604322	64.317869	61.321076
2077.662443	68.450136	61.326081
2076.735268	76.516166	61.331086
2076.328148	69.202583	61.336090
2075.373879	69.951981	61.341095
2074.573206	62.825710	61.346100
2074.162708	72.924194	61.351105
2073.571444	73.590583	61.356110
2073.050306	64.563289	61.361114
2071.757378	74.869152	61.366119
2070.932999	72.404235	61.371124
2070.307839	70.487849	61.376129
2070.130060	70.439331	61.381134
2069.815019	70.545339	61.386138
2068.907872	75.242957	61.391143
2068.279653	68.554535	61.396148
2067.965293	67.229567	61.401153
2067.011815	71.411710	61.406158
2066.037181	66.595492	61.411162
2065.181975	72.278129	61.416167
2064.463266	60.416598	61.421172
2063.983742	64.396493	61.426177
2063.581646	70.003996	61.431182
2063.294401	66.325413	61.436186
2062.368227	75.730557	61.441191
2061.903708	70.077907	61.446196
2061.162584	65.484237	61.451201
2059.756394	69.867363	61.456206
2059.648941	64.878346	61.461210
2058.648784	73.776297	61.466215
2058.259748	72.058725	61.471220
2057.764061	67.010987	61.476225
2057.101802	69.240376	61.481230
2056.883994	62.411500	61.486234
2055.503178	67.314868	61.491239
2054.427699	74.466043	61.496244
2053.839790	73.498115	61.501249
2053.381893	72.676889	61.506254
2053.416037	65.884255	61.511258
2052.384468	66.697798	61.516263
2051.991024	67.072206	61.521268
2051.591818	74.037447	61.526273
2050.489594	77.010747	61.531278
2049.739690	65.461644	61.536282
2048.891972	75.715042	61.541287
2048.793385	67.850158	61.546292
2048.049751	71.300914	61.551297
2046.387496	73.120324	61.556302
2045.779895	61.819241	61.561306
2045.902284	71.647765	61.566311
2044.870902	69.895994	61.571316
2044.707066	69.206831	61.576321
2043.792403	66.524082	61.581326
2043.300340	66.874309	61.586330
2042.628712	69.112011	61.591335
2041.753687	75.448540	61.596340
2040.564122	71.713913	61.601345
2039.667635	73.932055	61.606350
2040.414737	63.805637	61.611354
2039.045558	72.316335	61.616359
2038.742311	76.210427	61.621364
2038.255022	71.608867	61.626369
2037.082081	73.149196	61.631374
2036.695060	63.640304	61.636378
2035.429300	64.966783	61.641383
2034.851614	74.099959	61.646388
2034.352873	76.885172	61.651393
2034.257813	78.599930	61.656398
2033.722455	75.487580	61.661402
2032.839816	80.411528	61.666407
2031.634179	76.710440	61.671412
2030.922960	65.820617	61.676417
2029.880131	74.227734	61.681422
2029.553620	68.419646	61.686426
2028.891928	71.195628	61.691431
2028.505534	63.025125	61.696436
2028.293794	72.066496	61.701441
2027.528157	73.018495	61.706446
2027.276246	69.385973	61.711450
2026.050576	81.262773	61.716455
2025.192021	72.258860	61.721460
2024.651745	70.172835	61.726465
2023.671076	76.898079	61.731470
2023.518820	67.985319	61.736474
2022.892131	79.579274	61.741479
2021.909828	66.126329	61.746484
2021.016153	68.785683	61.751489
2020.444393	68.521940	61.756494
2020.006389	60.593942	61.761498
2019.148106	67.503107	61.766503
2018.981148	65.558087	61.771508
2018.987159	67.361340	61.776513
2017.737243	68.745110	61.781518
2017.024189	66.313264	61.786522
2016.413504	69.591288	61.791527
2015.304076	61.431182	61.796532
2014.284537	66.641033	61.801537
2013.426752	77.725067	61.806542
2013.638449	64.039863	61.811546
2012.458729	67.481536	61.816551
2012.052949	68.050680	61.821556
2011.478027	69.750814	61.826561
2010.924910	67.506732	61.831566
2010.375331	63.781848	61.836570
2009.554448	66.291389	61.841575
2008.228418	74.049087	61.846580
2007.969340	65.114736	61.851585
2007.054922	66.578877	61.856590
2006.802674	69.177458	61.861594
2006.191160	71.357910	61.866599
2005.583571	73.088105	61.871604
2005.502662	64.838509	61.876609
2004.459862	74.506753	61.881614
2003.934794	68.843155	61.886618
2002.916475	70.865440	61.891623
2002.381917	71.164126	61.896628
2001.397525	64.013248	61.901633
2000.419952	74.293991	61.906638
2000.064083	67.516366	61.911642
1999.524581	65.056809	61.916647
1998.526741	66.205235	61.921652
1998.404260	67.276159	61.926657
1997.661280	66.122405	61.931662
1997.397424	62.997172	61.936666
1996.387985	72.242885	61.941671
1995.390539	68.699213	61.946676
1995.325312	52.794517	61.951681
1994.242865	65.899648	61.956686
1993.799286	67.443506	61.961690
1992.760813	75.746072	61.966695
1991.826951	76.565412	61.971700
1991.137471	64.444303	61.976705
1990.556937	65.474375	61.981710
1990.441127	63.293644	61.986714
1989.756893	68.397591	61.991719
1989.444855	61.494452	61.996724
1989.340669	65.316598	62.001729
1987.555245	71.105472	62.006734
1986.914920	56.317527	62.011738
1986.374917	61.016686	62.016743
1985.676085	64.529254	62.021748
1985.610961	62.957588	62.026753
1983.894790	74.824349	62.031758
1983.211171	59.906050	62.036762
1982.555810	68.205443	62.041767
1982.018730	57.062834	62.046772
1981.887955	61.305561	62.051777
1981.296327	58.787821	62.056782
1981.194887	59.383850	62.061786
1980.549454	61.276829	62.066791
1979.753723	60.699313	62.071796
1978.977737	59.012417	62.076801
1977.344179	71.551462	62.081806
1976.927868	59.128644	62.086810
1976.373070	69.100628	62.091815
1975.821937	70.250799	62.096820
1975.410482	59.039334	62.101825
1974.648099	68.802102	62.106830
1973.789617	64.898364	62.111834
1973.050367	64.160405	62.116839
1972.139956	65.612418	62.121844
1971.932927	67.590266	62.126849
1971.132888	69.859415	62.131854
1971.204645	65.820626	62.136858
1969.801344	68.918465	62.141863
1968.754612	68.427701	62.146868
1968.270936	66.450419	62.151873
1967.855009	72.482245	62.156878
1967.593529	53.359821	62.161882
1967.377591	70.338522	62.166887
1966.004956	72.479448	62.171892
1965.756069	70.108727	62.176897
1964.256672	74.525976	62.181902
1964.001212	67.355407	62.186906
1962.804890	70.417842	62.191911
1961.786965	70.166088	62.196916
1961.979970	65.853148	62.201921
1961.073496	71.277341	62.206926
1960.148362	73.516183	62.211930
1959.704397	68.760783	62.216935
1959.416231	66.621377	62.221940
1959.348562	66.779413	62.226945
1958.140792	71.237955	62.231950
1957.699699	63.612455	62.236954
1956.657584	69.095376	62.241959
1956.248382	67.783482	62.246964
1955.903081	64.210363	62.251969
1954.320083	72.366091	62.256974
1953.746667	71.812914	62.261978
1953.030274	70.111090	62.266983
1952.458908	77.727071	62.271988
1952.472461	68.038751	62.276993
1951.628815	71.236637	62.281998
1951.342503	65.318267	62.287002
1950.442898	62.292715	62.292007
1949.795246	65.407338	62.297012
1948.599867	61.262435	62.302017
1947.626104	68.170047	62.307022
1947.030244	63.426424	62.312026
1946.203679	67.074526	62.317031
1945.849442	63.619773	62.322036
1945.475247	61.244045	62.327041
1944.980282	65.496970	62.332046
1944.715423	57.867379	62.337050
1943.908321	63.887570	62.342055
1942.660362	64.163834	62.347060
1942.407009	62.127024	62.352065
1941.907902	70.346402	62.357070
1940.848836	69.517111	62.362074
1939.817882	66.673496	62.367079
1939.227451	66.950169	62.372084
1938.910397	65.214374	62.377089
1938.417940	71.530069	62.382094
1938.137222	65.326151	62.387098
1936.550544	66.122577	62.392103
1935.689725	69.722464	62.397108
1935.486682	59.483072	62.402113
1934.972184	72.493422	62.407118
1934.509133	57.028220	62.412122
1933.867121	71.208225	62.417127
1932.395326	76.399146	62.422132
1931.782088	64.622626	62.427137
1931.424175	66.354719	62.432142
1930.773732	65.721173	62.437146
1930.517768	65.787479	62.442151
1930.242466	67.328210	62.447156
1929.233143	58.474458	62.452161
1928.330620	62.213710	62.457166
1927.856378	62.215123	62.462170
1927.352599	58.248349	62.467175
1926.089823	63.881515	62.472180
1925.656128	58.854378	62.477185
1924.840166	68.832752	62.482190
1924.282213	60.316238	62.487194
1923.895385	61.237393	62.492199
1922.940363	68.173379	62.497204
1921.659018	57.988200	62.502209
1920.990589	63.418643	62.507214
1920.645340	60.269448	62.512218
1920.246847	65.590558	62.517223
1919.805884	71.454964	62.522228
1919.532284	64.847218	62.527233
1919.008643	70.717084	62.532238
1918.055838	66.660553	62.537242
1916.960466	63.282067	62.542247
1916.214902	72.436858	62.547252
1916.056779	56.923443	62.552257
1915.101642	66.701030	62.557262
1913.977120	59.420998	62.562266
1913.212305	63.175771	62.567271
1912.495542	64.028638	62.572276
1912.433230	56.620574	62.577281
1911.988575	72.205962	62.582286
1911.711082	63.540028	62.587290
1910.811305	67.347494	62.592295
1909.908116	63.126564	62.597300
1909.422610	56.281139	62.602305
1908.746761	65.185589	62.607310
1907.809253	61.411432	62.612314
1906.913575	66.850360	62.617319
1905.959540	64.914079	62.622324
1905.981730	58.813867	62.627329
1905.250043	68.561913	62.632334
1905.026889	65.567876	62.637338
1904.340763	71.009245	62.642343
1902.915278	77.577714	62.647348
1902.377972	68.376778	62.652353
1901.676225	71.324616	62.657358
1901.229525	72.765204	62.662362
1900.826190	80.275471	62.667367
1899.654786	76.486460	62.672372
1899.301007	64.277552	62.677377
1898.320653	72.387823	62.682382
1898.321843	66.074106	62.687386
1897.752334	67.286240	62.692391
1896.643626	65.348791	62.697396
1895.884906	57.070307	62.702401
1895.335723	74.828348	62.707406
1894.763678	64.957205	62.712410
1893.600442	67.384020	62.717415
1893.160680	73.614127	62.722420
1892.544702	59.840415	62.727425
1892.248824	67.739643	62.732430
1892.017159	62.624264	62.737434
1890.397122	66.990722	62.742439
1889.511167	66.830480	62.747444
1889.083056	67.636337	62.752449
1888.475285	68.631213	62.757454
1888.052306	62.572819	62.762458
1887.966154	67.709844	62.767463
1886.978447	78.392182	62.772468
1886.024623	65.471230	62.777473
1885.022664	65.704238	62.782478
1884.670858	62.791815	62.787482
1884.478851	63.314133	62.792487
1883.685147	70.266339	62.797492
1882.755735	61.536290	62.802497
1882.193682	64.917314	62.807502
1881.746905	64.859957	62.812506
1880.795893	69.492472	62.817511
1879.724301	75.660154	62.822516
1879.439859	60.822403	62.827521
1878.692107	67.969238	62.832526
1878.376651	66.423034	62.837530
1877.542922	67.865496	62.842535
1876.663220	73.230647	62.847540
1876.089775	66.679334	62.852545
1875.605535	66.955214	62.857550
1875.194494	69.097039	62.862554
1874.316904	71.703532	62.867559
1873.525700	67.989610	62.872564
1873.173206	56.969387	62.877569
1872.555612	65.901766	62.882574
1871.345775	64.187273	62.887578
1870.511051	66.742619	62.892583
1869.663542	71.595049	62.897588
1869.595714	58.580554	62.902593
1868.939773	71.726804	62.907598
1868.569444	69.866713	62.912602
1867.878792	79.868261	62.917607
1866.992560	66.865885	62.922612
1866.777392	74.117388	62.927617
1865.466635	68.750459	62.932622
1864.130551	66.456409	62.937626
1863.714000	68.680489	62.942631
1863.182508	78.065097	62.947636
1862.732061	68.175918	62.952641
1862.209147	72.783746	62.957646
1861.996063	69.678256	62.962650
1861.881344	65.251788	62.967655
1860.570833	73.653800	62.972660
1860.220376	64.178550	62.977665
1859.218235	64.586850	62.982670
1858.064842	64.722224	62.987674
1857.286416	68.437887	62.992679
1856.506107	70.218960	62.997684
1856.406409	79.662321	63.002689
1855.799695	72.710535	63.007694
1855.652292	73.232723	63.012698
1854.504170	69.444479	63.017703
1853.520107	73.532415	63.022708
1853.387219	68.021998	63.027713
1852.380809	78.305715	63.032718
1851.038318	78.445417	63.037722
1850.511515	74.008925	63.042727
1849.954525	71.986964	63.047732
1849.970375	57.945308	63.052737
1849.242843	69.423486	63.057742
1848.864764	64.512363	63.062746
1848.237689	59.716074	63.067751
1847.097703	73.969828	63.072756
1846.785788	67.130629	63.077761
1846.066238	70.407951	63.082766
1845.232925	67.808820	63.087770
1844.808788	67.331559	63.092775
1843.964077	70.703712	63.097780
1842.919536	64.671932	63.102785
1841.716640	66.950418	63.107790
1841.347412	69.485730	63.112794
1840.908363	67.087556	63.117799
1840.395043	76.057362	63.122804
1840.117959	69.905330	63.127809
1839.727622	75.516747	63.132814
1838.808658	73.194364	63.137818
1837.944278	69.474022	63.142823
1837.102229	69.864803	63.147828
1836.982836	63.896181	63.152833
1835.740286	65.874756	63.157838
1834.853633	74.107549	63.162842
1834.579163	63.946702	63.167847
1833.812952	69.244679	63.172852
1833.740875	62.731539	63.177857
1832.664390	63.239401	63.182862
1831.545869	61.538504	63.187866
1831.033750	73.163375	63.192871
1830.454537	74.867023	63.197876
1830.150758	66.712415	63.202881
1829.521138	67.201058	63.207886
1828.430343	71.351071	63.212890
1828.091920	67.444829	63.217895
1827.454238	64.781049	63.222900
1826.927613	67.861952	63.227905
1825.800433	71.927800	63.232910
1825.067365	62.567753	63.237914
1824.438144	66.187631	63.242919
1824.039291	73.375432	63.247924
1823.831834	64.678976	63.252929
1822.989091	67.463847	63.257934
1822.070275	67.833425	63.262938
1821.487830	65.462155	63.267943
1820.495490	71.198278	63.272948
1819.686039	59.244580	63.277953
1818.674255	73.377326	63.282958
1818.622599	66.303349	63.287962
1818.029270	63.920521	63.292967
1817.278231	69.139723	63.297972
1817.332027	65.437944	63.302977
1816.609807	68.681779	63.307982
1815.902406	66.297943	63.312986
1815.316924	69.042354	63.317991
1813.849088	70.247937	63.322996
1813.203654	64.588781	63.328001
1812.535492	68.057041	63.333006
1812.155929	71.726177	63.338010
1811.990627	68.436076	63.343015
1810.436165	71.587446	63.348020
1809.723407	62.337607	63.353025
1809.407113	65.802504	63.358030
1808.814768	59.584030	63.363034
1808.757523	61.183769	63.368039
1807.402717	60.480892	63.373044
1806.572195	61.758612	63.378049
1806.141597	61.893090	63.383054
1805.820373	55.200751	63.388058
1805.439746	58.565343	63.393063
1803.690716	68.184704	63.398068
1803.680486	63.760098	63.403073
1802.683988	72.179836	63.408078
1802.189648	62.090561	63.413082
1801.686649	57.769213	63.418087
1800.863435	65.508410	63.423092
1800.768694	55.569839	63.428097
1799.669707	62.463364	63.433102
1798.610282	58.133013	63.438106
1797.903119	67.758056	63.443111
1797.301996	70.395017	63.448116
1797.236009	57.764281	63.453121
1796.528691	61.052538	63.458126
1796.044531	53.463648	63.463130
1794.971222	58.528787	63.468135
1793.900575	58.400555	63.473140
1793.532185	51.392226	63.478145
1793.174517	64.046929	63.483150
1792.714909	58.888855	63.488154
1791.891260	59.791208	63.493159
1791.017670	66.414078	63.498164
1790.344012	54.473472	63.503169
1789.132994	54.057826	63.508174
1788.567339	62.986449	63.513178
1788.172585	52.074919	63.518183
1787.379428	53.549133	63.523188
1787.507693	53.746669	63.528193
1786.847272	59.451264	63.533198
1785.969838	59.129720	63.538202
1785.511781	57.713312	63.543207
1784.006845	57.328615	63.548212
1783.014465	49.470254	63.553217
1782.896583	63.834899	63.558222
1782.158822	52.056837	63.563226
1781.994699	62.557602	63.568231
1781.060036	62.800826	63.573236
1781.169688	58.810821	63.578241
1779.502898	70.304450	63.583246
1778.997560	62.982459	63.588250
1778.600695	63.594303	63.593255
1777.941643	68.331212	63.598260
1777.654233	53.234273	63.603265
1776.357342	58.259909	63.608270
1775.213755	58.601640	63.613274
1775.341449	62.729089	63.618279
1774.540155	65.830939	63.623284
1773.957707	62.765367	63.628289
1772.993749	59.822306	63.633294
1772.297401	59.482412	63.638298
1772.441519	56.617379	63.643303
1771.005961	60.546138	63.648308
1770.590316	52.919478	63.653313
1769.910816	57.974078	63.658318
1769.233678	51.789464	63.663322
1768.886149	49.564711	63.668327
1767.875763	53.093501	63.673332
1767.168176	54.277169	63.678337
1766.643554	58.533201	63.683342
1766.036329	52.113215	63.688346
1765.218708	56.975142	63.693351
1763.925307	59.953570	63.698356
1763.769738	55.570810	63.703361
1763.263624	58.167043	63.708366
1763.085047	59.272040	63.713370
1762.325531	64.116528	63.718375
1760.921562	65.330933	63.723380
1760.891490	53.179170	63.728385
1760.223230	60.867776	63.733390
1758.744305	66.052453	63.738394
1758.314667	56.146321	63.743399
1757.659209	61.902566	63.748404
1757.502765	57.280756	63.753409
1756.964603	57.118262	63.758414
1755.863464	56.390943	63.763418
1755.371746	55.748814	63.768423
1754.420109	59.078879	63.773428
1754.127819	57.182949	63.778433
1753.867848	62.320499	63.783438
1752.695079	59.299886	63.788442
1751.920986	57.307192	63.793447
1751.483267	57.895240	63.798452
1751.005737	55.865618	63.803457
1750.020002	60.986039	63.808462
1749.116362	64.519857	63.813466
1748.681329	58.568148	63.818471
1748.115337	60.650049	63.823476
1747.787335	53.974272	63.828481
1746.477002	58.525789	63.833486
1745.913774	57.881292	63.838490
1745.760417	56.021982	63.843495
1745.059143	57.372329	63.848500
1744.160375	58.605290	63.853505
1743.228954	65.442918	63.858510
1742.603449	54.158397	63.863514
1742.290422	52.465349	63.868519
1741.594731	55.422427	63.873524
1740.486172	60.853983	63.878529
1739.874088	58.981984	63.883534
1739.606828	62.122717	63.888538
1739.178647	63.209637	63.893543
1738.164457	57.823978	63.898548
1737.100738	51.771435	63.903553
1736.515339	58.057640	63.908558
1736.007847	63.945272	63.913562
1735.829244	60.106033	63.918567
1735.084425	54.231018	63.923572
1734.187154	54.479298	63.928577
1733.703560	54.221816	63.933582
1733.120388	54.770019	63.938586
1732.648274	52.634478	63.943591
1731.328266	60.834849	63.948596
1730.574643	54.246111	63.953601
1729.878351	61.873203	63.958606
1729.509595	63.746102	63.963610
1729.455127	54.781524	63.968615
1727.930020	63.732219	63.973620
1727.831555	55.150547	63.978625
1726.824136	60.416385	63.983630
1726.245087	59.208177	63.988634
1725.964313	58.247339	63.993639
1724.632195	68.107208	63.998644
1724.344771	58.648436	64.003649
1723.771582	61.723891	64.008654
1723.118361	54.595763	64.013658
1722.434951	50.392531	64.018663
1721.337407	57.198980	64.023668
1721.113493	46.219158	64.028673
1720.765767	55.604674	64.033678
1719.424562	53.413381	64.038682
1718.997502	53.277273	64.043687
1718.370922	56.092665	64.048692
1718.107158	58.803347	64.053697
1716.839385	57.783643	64.058702
1715.995377	54.309701	64.063706
1715.383109	52.418791	64.068711
1714.951109	65.570133	64.073716
1714.806545	60.975501	64.078721
1713.959169	60.602645	64.083726
1712.729585	60.757009	64.088730
1712.359986	64.666008	64.093735
1711.978401	60.899792	64.098740
1711.384848	54.853246	64.103745
1710.456002	66.069438	64.108750
1709.644937	67.364369	64.113754
1709.424818	64.229307	64.118759
1708.732406	65.472752	64.123764
1707.639328	63.258344	64.128769
1707.389651	67.479967	64.133774
1706.769364	63.764463	64.138778
1706.069364	57.623637	64.143783
1704.761613	60.126135	64.148788
1704.452369	59.756326	64.153793
1703.912496	57.462259	64.158798
1702.945889	59.900462	64.163802
1702.034787	61.136331	64.168807
1701.380123	63.957321	64.173812
1700.978305	63.735978	64.178817
1700.329778	62.809255	64.183822
1699.799543	61.681904	64.188826
1699.866822	59.150530	64.193831
1698.750942	64.923988	64.198836
1697.927093	60.115609	64.203841
1697.333256	58.441800	64.208846
1696.578559	64.383970	64.213850
1695.893617	55.270712	64.218855
1694.783330	65.573786	64.223860
1694.641934	62.373942	64.228865
1694.128733	56.939673	64.233870
1693.612561	68.431420	64.238874
1692.718456	62.821154	64.243879
1691.721606	64.848108	64.248884
1691.241750	62.687844	64.253889
1690.749978	55.734586	64.258894
1689.726888	62.004115	64.263898
1689.278893	60.802696	64.268903
1688.318212	63.372908	64.273908
1688.094253	62.303671	64.278913
1687.781940	59.952509	64.283918
1686.826197	67.979249	64.288922
1686.315303	56.199098	64.293927
1685.879531	59.661548	64.298932
1684.557757	60.882828	64.303937
1683.759432	69.486155	64.308942
1682.966536	72.328829	64.313946
1683.050714	65.418322	64.318951
1681.988398	60.788509	64.323956
1681.076651	61.264659	64.328961
1680.752008	65.473058	64.333966
1679.628887	70.637920	64.338970
1679.679885	65.784047	64.343975
1679.099297	64.250861	64.348980
1677.908461	60.012891	64.353985
1677.193900	56.260633	64.358990
1676.749217	66.300215	64.363994
1676.548726	60.345485	64.368999
1675.260458	68.615040	64.374004
1674.656872	55.751069	64.379009
1674.206353	58.854086	64.384014
1673.534471	54.843486	64.389018
1673.199167	59.799724	64.394023
1671.986818	70.673268	64.399028
1671.722457	67.130931	64.404033
1670.911824	61.640591	64.409038
1669.976781	70.497041	64.414042
1669.374854	62.769644	64.419047
1668.636646	71.364660	64.424052
1668.019498	68.639761	64.429057
1667.659829	68.344896	64.434062
1666.691065	72.325245	64.439066
1666.541225	63.443302	64.444071
1665.683511	66.692575	64.449076
1664.922360	64.201520	64.454081
1664.098721	63.440944	64.459086
1663.036369	68.611199	64.464090
1662.964304	50.793355	64.469095
1662.522141	65.655955	64.474100
1662.069054	65.900867	64.479105
1660.713882	65.099017	64.484110
1659.811305	65.633204	64.489114
1659.694668	66.457617	64.494119
1658.818755	69.063064	64.499124
1658.530756	60.515408	64.504129
1657.833573	56.334674	64.509134
1656.756491	65.228454	64.514138
1656.709537	62.093368	64.519143
1655.492099	71.265763	64.524148
1654.786542	64.106734	64.529153
1654.195068	60.275787	64.534158
1653.837046	67.567908	64.539162
1653.523870	63.891828	64.544167
1652.264444	62.518624	64.549172
1651.805264	68.947046	64.554177
1651.159935	57.350952	64.559182
1650.026353	59.871814	64.564186
1649.323068	55.853960	64.569191
1648.458303	66.744995	64.574196
1647.910992	74.359629	64.579201
1647.810386	66.268170	64.584206
1647.394896	65.328417	64.589210
1646.874947	67.579281	64.594215
1645.624224	64.843601	64.599220
1644.679902	65.635580	64.604225
1644.478067	58.949672	64.609230
1644.025486	60.975070	64.614234
1643.045396	58.555036	64.619239
1642.532236	64.792177	64.624244
1641.898465	61.279114	64.629249
1641.228063	56.820655	64.634254
1639.912985	64.374441	64.639258
1639.580545	60.346413	64.644263
1639.215938	67.962541	64.649268
1638.861815	59.735268	64.654273
1638.194648	63.294553	64.659278
1637.082872	67.794354	64.664282
1636.690852	56.632921	64.669287
1635.769329	63.433735	64.674292
1635.000284	57.186718	64.679297
1634.253286	67.656568	64.684302
1633.650499	59.778940	64.689306
1633.675036	66.190502	64.694311
1632.785787	59.797484	64.699316
1631.750586	60.977236	64.704321
1631.246272	63.093195	64.709326
1630.525998	65.594252	64.714330
1629.914116	54.138093	64.719335
1628.872937	57.303508	64.724340
1628.673789	53.024528	64.729345
1627.800500	55.952012	64.734350
1627.385648	59.457066	64.739354
1627.110250	55.561379	64.744359
1625.949912	56.291648	64.749364
1625.634889	65.061731	64.754369
1624.566252	51.608313	64.759374
1623.404798	64.012153	64.764378
1623.180960	64.575056	64.769383
1622.166221	68.701035	64.774388
1621.481783	55.985907	64.779393
1621.476757	52.274073	64.784398
1620.682062	69.863713	64.789402
1619.755362	50.160914	64.794407
1619.139368	58.779219	64.799412
1618.716578	64.222118	64.804417
1618.441765	64.620069	64.809422
1616.958621	69.808659	64.814426
1616.785547	59.990877	64.819431
1616.190785	66.248300	64.824436
1615.449666	62.000489	64.829441
1614.787754	58.010296	64.834446
1613.743694	65.712698	64.839450
1613.078667	64.515665	64.844455
1612.783039	65.380972	64.849460
1612.142438	57.133654	64.854465
1611.211267	64.107430	64.859470
1610.706587	53.195404	64.864474
1610.711443	51.524937	64.869479
1609.615086	52.429383	64.874484
1608.444261	53.615770	64.879489
1607.925302	54.675998	64.884494
1607.196979	65.842880	64.889498
1606.919493	48.506236	64.894503
1605.825468	62.562270	64.899508
1605.085283	53.778998	64.904513
1604.852596	48.391868	64.909518
1604.144724	56.367113	64.914522
1603.943800	48.048901	64.919527
1602.603183	59.349771	64.924532
1602.018640	56.886528	64.929537
1602.154575	54.185126	64.934542
1600.930794	63.117041	64.939546
1600.001137	64.294920	64.944551
1598.840134	71.413027	64.949556
1598.555228	60.381287	64.954561
1598.909095	52.514420	64.959566
1597.561449	56.664214	64.964570
1596.785215	51.719033	64.969575
1595.997535	61.864674	64.974580
1595.760612	53.278687	64.979585
1595.109800	53.218774	64.984590
1594.165198	55.760197	64.989594
1593.653092	56.979904	64.994599
1592.848254	58.434040	64.999604
1592.286007	60.409923	65.004609
1591.337548	59.184824	65.009614
1590.236498	64.351842	65.014618
1590.042244	54.376648	65.019623
1589.935676	51.821741	65.024628
1589.083999	56.549390	65.029633
1588.264399	52.828940	65.034638
1587.193637	63.891407	65.039642
1587.037553	53.730084	65.044647
1586.635190	51.312242	65.049652
1585.628398	51.606526	65.054657
1584.986205	46.563413	65.059662
1584.075001	55.376310	65.064666
1583.602559	52.975592	65.069671
1583.285811	50.924790	65.074676
1582.453167	53.947951	65.079681
1581.836009	52.386696	65.084686
1580.931135	59.937786	65.089690
1580.290004	57.219770	65.094695
1579.537984	62.295480	65.099700
1579.035157	64.836300	65.104705
1578.664935	57.156503	65.109710
1577.856809	60.751758	65.114714
1576.844155	60.046438	65.119719
1576.310329	63.333052	65.124724
1575.493666	59.764461	65.129729
1575.480632	59.764736	65.134734
1574.184385	60.665505	65.139738
1573.863464	51.178943	65.144743
1572.989964	59.176615	65.149748
1572.604871	61.835831	65.154753
1571.845659	48.272247	65.159758
1570.669513	49.605992	65.164762
1570.503322	51.234241	65.169767
1569.756646	62.823453	65.174772
1569.474723	51.938443	65.179777
1568.186816	50.021873	65.184782
1567.563726	57.602893	65.189786
1567.118778	51.657647	65.194791
1566.552428	56.423701	65.199796
1565.738604	58.817622	65.204801
1565.078504	54.816471	65.209806
1564.354602	50.674669	65.214810
1564.350052	49.712356	65.219815
1563.434646	53.964622	65.224820
1562.479417	45.691829	65.229825
1562.046861	46.260061	65.234830
1561.582241	55.631631	65.239834
1560.300668	48.475688	65.244839
1559.576919	55.296341	65.249844
1559.263234	58.341606	65.254849
1558.697446	54.393786	65.259854
1557.768925	53.371718	65.264858
1556.865381	49.656958	65.269863
1556.162394	52.405313	65.274868
1555.572864	56.595495	65.279873
1555.725257	53.611421	65.284878
1555.275538	52.681876	65.289882
1554.619092	53.760903	65.294887
1553.567399	50.536868	65.299892
1552.341253	53.310420	65.304897
1551.857376	66.021837	65.309902
1550.606229	56.154108	65.314906
1550.294368	52.470711	65.319911
1550.014981	52.579726	65.324916
1549.322632	52.430616	65.329921
1548.846110	46.030539	65.334926
1547.462543	54.510222	65.339930
1547.131183	59.581438	65.344935
1546.972769	58.123642	65.349940
1545.938217	60.592446	65.354945
1545.239674	53.931957	65.359950
1544.378680	57.212988	65.364954
1544.164721	54.762906	65.369959
1543.790962	59.040892	65.374964
1542.637310	56.370730	65.379969
1541.756396	59.869503	65.384974
1541.220216	61.115439	65.389978
1541.016753	52.721882	65.394983
1540.107914	56.753171	65.399988
1539.082225	56.894390	65.404993
1538.884443	54.767181	65.409998
1537.827859	62.317795	65.415002
1537.798820	56.911604	65.420007
1536.923665	52.808323	65.425012
1536.133144	54.430534	65.430017
1535.982821	59.627075	65.435022
1534.535798	59.020182	65.440026
1534.048221	56.978095	65.445031
1533.422262	60.700853	65.450036
1533.185798	55.253983	65.455041
1532.111400	63.087895	65.460046
1530.833310	56.371471	65.465050
1530.693409	54.044103	65.470055
1530.588295	64.291604	65.475060
1529.952650	57.481411	65.480065
1528.791526	57.924087	65.485070
1527.890427	62.248908	65.490074
1527.504057	60.823021	65.495079
1527.153082	63.593237	65.500084
1525.888954	59.268384	65.505089
1525.463622	56.639358	65.510094
1525.092920	73.066224	65.515098
1524.555966	61.456348	65.520103
1523.634253	64.043995	65.525108
1522.394516	58.420297	65.530113
1522.406078	55.612292	65.535118
1522.144421	62.128087	65.540122
1520.689402	54.341476	65.545127
1519.914606	55.817717	65.550132
1519.324421	66.657816	65.555137
1519.191467	57.808135	65.560142
1518.332396	57.516651	65.565146
1517.225796	55.605378	65.570151
1516.471301	60.837431	65.575156
1515.825829	63.955667	65.580161
1516.102821	56.398783	65.585166
1515.427911	58.792620	65.590170
1514.110738	62.555527	65.595175
1513.685533	56.390603	65.600180
1513.050771	63.524437	65.605185
1512.799918	56.792069	65.610190
1511.381058	58.076978	65.615194
1510.643303	55.669574	65.620199
1509.985104	56.022231	65.625204
1509.429042	60.821264	65.630209
1509.336630	56.997290	65.635214
1508.018304	61.648115	65.640218
1507.662430	58.723006	65.645223
1507.169183	63.527867	65.650228
1506.682787	66.174426	65.655233
1506.026345	54.176083	65.660238
1505.014944	56.129378	65.665242
1504.142235	58.190771	65.670247
1503.844059	54.280442	65.675252
1502.894433	60.440322	65.680257
1502.164291	55.574502	65.685262
1501.402563	55.260046	65.690266
1501.072764	59.423146	65.695271
1501.026895	50.760662	65.700276
1500.162654	55.009706	65.705281
1499.304708	56.937527	65.710286
1498.718281	58.880848	65.715290
1497.926938	47.054409	65.720295
1496.828175	55.938492	65.725300
1496.359545	62.853639	65.730305
1495.988442	55.963047	65.735310
1494.746555	64.763478	65.740314
1493.743766	52.393782	65.745319
1493.581800	53.566990	65.750324
1492.749666	60.469750	65.755329
1492.692024	47.771722	65.760334
1492.495238	56.661289	65.765338
1491.643495	48.844067	65.770343
1490.734405	62.010341	65.775348
1490.000795	66.664905	65.780353
1489.303506	63.911515	65.785358
1488.236216	66.645657	65.790362
1487.888414	50.422731	65.795367
1487.336316	56.972049	65.800372
1486.275163	60.416025	65.805377
1485.691873	53.038358	65.810382
1484.981530	61.387041	65.815386
1484.414842	62.057180	65.820391
1484.246992	55.238771	65.825396
1483.102910	60.076872	65.830401
1482.344652	46.930762	65.835406
1481.723268	50.920752	65.840410
1481.288335	55.745235	65.845415
1481.147966	46.853020	65.850420
1480.382918	53.999677	65.855425
1479.657425	52.984715	65.860430
1478.891797	57.112284	65.865434
1477.976282	54.567951	65.870439
1477.172544	56.986209	65.875444
1476.292545	62.763536	65.880449
1476.056643	50.739407	65.885454
1475.186174	63.716713	65.890458
1474.142280	63.718963	65.895463
1473.604425	58.541567	65.900468
1473.266662	57.968638	65.905473
1472.812202	58.651542	65.910478
1472.352806	64.276753	65.915482
1471.776495	62.706942	65.920487
1470.967410	57.921347	65.925492
1470.153537	62.529652	65.930497
1469.458700	52.794884	65.935502
1468.311054	57.775300	65.940506
1467.617745	56.290644	65.945511
1467.545234	60.737718	65.950516
1467.081160	57.035384	65.955521
1466.579869	55.785086	65.960526
1465.498617	58.567407	65.965530
1464.889288	53.281859	65.970535
1464.398884	56.371978	65.975540
1463.207201	55.576540	65.980545
1462.813883	51.995906	65.985550
1462.470048	53.323395	65.990554
1461.502250	53.505639	65.995559
1460.819045	46.580849	66.000564
1459.915351	59.094520	66.005569
1459.566033	44.889659	66.010574
1458.426315	59.060882	66.015578
1457.577496	59.585508	66.020583
1456.774640	57.502266	66.025588
1456.390470	54.019930	66.030593
1456.090867	54.889476	66.035598
1455.699916	65.953619	66.040602
1455.373587	60.795675	66.045607
1454.368884	59.716012	66.050612
1453.330189	63.703623	66.055617
1453.097665	56.396574	66.060622
1452.296943	61.985475	66.065626
1451.350572	63.096770	66.070631
1450.801116	62.548235	66.075636
1450.260467	67.953683	66.080641
1450.078407	60.077498	66.085646
1448.873455	61.725264	66.090650
1447.730252	60.374060	66.095655
1447.146908	63.256285	66.100660
1446.814910	62.442383	66.105665
1446.700873	67.266811	66.110670
1445.961597	65.227948	66.115674
1444.710365	65.425552	66.120679
1444.287154	52.985879	66.125684
1443.809474	62.619806	66.130689
1443.186827	49.469046	66.135694
1442.367717	60.308853	66.140698
1441.746779	62.058359	66.145703
1441.432356	60.609114	66.150708
1439.910553	69.167745	66.155713
1440.122970	52.626318	66.160718
1439.303544	60.581985	66.165722
1438.353534	61.912973	66.170727
1437.619988	58.010857	66.175732
1436.703543	66.256277	66.180737
1436.557327	50.733033	66.185742
1435.700724	67.032668	66.190746
1434.791764	55.613590	66.195751
1434.530044	51.176793	66.200756
1433.747341	61.043708	66.205761
1433.319610	60.526443	66.210766
1431.815198	59.229569	66.215770
1431.169342	60.567310	66.220775
1431.073197	55.212874	66.225780
1430.700377	56.164030	66.230785
1430.202937	56.321426	66.235790
1429.180059	57.417401	66.240794
1428.407448	51.745355	66.245799
1428.139451	50.187512	66.250804
1426.634639	59.147816	66.255809
1425.872754	51.620740	66.260814
1425.051609	59.860898	66.265818
1425.009796	55.959588	66.270823
1424.823526	55.468885	66.275828
1424.486232	56.417907	66.280833
1423.494394	51.249548	66.285838
1422.759054	44.116596	66.290842
1422.276120	41.457972	66.295847
1421.361361	48.030682	66.300852
1420.358373	56.116447	66.305857
1420.041949	54.373482	66.310862
1418.982344	56.109265	66.315866
1418.341726	52.882397	66.320871
1417.737384	53.653720	66.325876
1417.363575	54.294404	66.330881
1416.789751	47.571546	66.335886
1415.893704	52.737050	66.340890
1415.155184	58.040978	66.345895
1414.766387	56.348294	66.350900
1413.803239	58.008360	66.355905
1413.089978	52.438652	66.360910
1412.055797	52.443594	66.365914
1411.756823	55.209649	66.370919
1411.544039	51.179719	66.375924
1410.871138	53.574800	66.380929
1409.984717	51.609287	66.385934
1409.221451	49.662956	66.390938
1408.555183	58.774189	66.395943
1408.286077	53.585538	66.400948
1407.056080	62.717087	66.405953
1406.553183	53.442875	66.410958
1405.843378	59.190287	66.415962
1405.341674	56.408171	66.420967
1404.900171	56.564284	66.425972
1403.462617	62.651388	66.430977
1403.457376	55.614505	66.435982
1402.533160	61.680447	66.440986
1402.104345	57.521713	66.445991
1401.470650	53.481336	66.450996
1400.320011	54.468928	66.456001
1400.059732	57.992137	66.461006
1399.652837	56.629772	66.466010
1398.936726	57.233922	66.471015
1398.428811	51.732090	66.476020
1397.638936	54.419155	66.481025
1396.621869	55.848861	66.486030
1395.463246	66.161819	66.491034
1395.069127	60.597481	66.496039
1394.488504	51.964571	66.501044
1393.919445	58.026164	66.506049
1393.943715	53.871583	66.511054
1392.884796	57.942792	66.516058
1391.840241	53.628551	66.521063
1391.658126	54.221424	66.526068
1391.020764	54.666051	66.531073
1390.488603	53.156586	66.536078
1389.197682	57.580123	66.541082
1388.348430	65.896146	66.546087
1388.301229	58.817896	66.551092
1387.654953	54.908352	66.556097
1386.758484	57.065008	66.561102
1386.402615	63.717710	66.566106
1385.920867	59.933942	66.571111
1384.827058	54.770810	66.576116
1383.526287	62.744537	66.581121
1383.390666	60.791029	66.586126
1383.068196	54.295136	66.591130
1382.577999	55.353618	66.596135
1381.716444	46.685123	66.601140
1381.120315	53.961943	66.606145
1380.475311	51.223702	66.611150
1379.400702	55.833228	66.616154
1378.954181	55.796791	66.621159
1378.076102	50.288856	66.626164
1377.509447	62.126714	66.631169
1376.899443	54.934815	66.636174
1375.931418	57.849737	66.641178
1374.966005	56.491405	66.646183
1375.290777	49.738677	66.651188
1374.567132	56.268419	66.656193
1373.997246	44.191753	66.661198
1372.600255	56.107402	66.666202
1371.896439	47.345990	66.671207
1371.720374	47.902303	66.676212
1371.096561	53.692230	66.681217
1370.183627	47.825940	66.686222
1369.548934	53.762591	66.691226
1369.147388	48.829105	66.696231
1368.765303	44.445286	66.701236
1367.564858	50.597589	66.706241
1367.109196	51.410569	66.711246
1366.199501	49.767585	66.716250
1365.843138	52.236769	66.721255
1365.384245	57.630591	66.726260
1363.918233	55.699172	66.731265
1363.707584	48.197351	66.736270
1363.320123	52.862929	66.741274
1361.964405	47.700825	66.746279
1361.255602	52.356676	66.751284
1360.623035	53.507423	66.756289
1360.340392	49.131844	66.761294
1359.840592	48.086555	66.766298
1359.687836	54.087543	66.771303
1358.495840	49.138191	66.776308
1357.665281	50.607420	66.781313
1357.410013	43.410067	66.786318
1355.887359	49.458851	66.791322
1355.240537	55.812426	66.796327
1355.004900	42.950297	66.801332
1354.934084	51.698296	66.806337
1354.482878	39.609612	66.811342
1353.523308	53.566062	66.816346
1352.544434	51.207855	66.821351
1352.218163	50.073260	66.826356
1350.791496	54.551619	66.831361
1350.222155	53.357981	66.836366
1349.526239	52.888210	66.841370
1349.097104	41.839377	66.846375
1349.016284	51.095509	66.851380
1347.618453	49.358071	66.856385
1347.538716	39.825531	66.861390
1346.966634	51.657205	66.866394
1345.631805	48.202625	66.871399
1345.040195	38.505881	66.876404
1343.782969	51.384395	66.881409
1343.423575	38.546615	66.886414
1343.503390	45.870740	66.891418
1342.874408	43.859594	66.896423
1342.474196	48.187108	66.901428
1341.502316	57.866158	66.906433
1341.173603	41.219637	66.911438
1340.241479	49.927585	66.916442
1339.109465	52.513761	66.921447
1338.884243	46.446864	66.926452
1337.529443	46.131725	66.931457
1336.745291	47.717349	66.936462
1336.310474	47.176439	66.941466
1335.629444	50.720359	66.946471
1335.529346	44.028523	66.951476
1334.920826	52.436748	66.956481
1333.974285	44.636586	66.961486
1333.420133	45.629051	66.966490
1332.792879	46.043930	66.971495
1332.189993	41.662785	66.976500
1330.887324	52.523398	66.981505
1330.393083	43.179835	66.986510
1329.839257	47.477597	66.991514
1329.303492	51.221639	66.996519
1329.153613	41.709790	67.001524
1327.991071	49.922739	67.006529
1327.381199	38.036477	67.011534
1326.837545	39.978410	67.016538
1326.075623	54.564939	67.021543
1325.587914	46.615184	67.026548
1324.650525	49.897480	67.031553
1324.223405	43.212288	67.036558
1323.531844	48.453711	67.041562
1322.326925	53.064238	67.046567
1321.538609	43.993243	67.051572
1321.029802	48.790114	67.056577
1320.735197	49.110156	67.061582
1320.442507	55.061286	67.066586
1319.444035	51.920561	67.071591
1318.916297	46.123732	67.076596
1318.102497	50.814139	67.081601
1317.886449	51.577025	67.086606
1316.520955	38.080210	67.091610
1315.708797	51.407114	67.096615
1315.526258	43.019879	67.101620
1314.775924	47.446013	67.106625
1314.801196	40.712588	67.111630
1313.782644	51.944544	67.116634
1312.671695	48.544012	67.121639
1312.414696	55.498321	67.126644
1311.667687	46.936939	67.131649
1311.074549	45.038865	67.136654
1310.262251	42.354932	67.141658
1309.460733	54.977818	67.146663
1308.887956	52.508262	67.151668
1308.216880	57.066086	67.156673
1307.715137	49.284911	67.161678
1307.369408	47.086734	67.166682
1305.894912	57.600211	67.171687
1305.430376	49.235591	67.176692
1304.718335	58.731223	67.181697
1304.547831	51.526862	67.186702
1303.366905	47.989109	67.191706
1302.645142	45.745575	67.196711
1302.408212	45.414331	67.201716
1302.014791	54.478462	67.206721
1301.608942	48.890887	67.211726
1300.340448	51.850942	67.216730
1299.322016	58.516809	67.221735
1299.413829	59.785122	67.226740
1298.109049	52.549161	67.231745
1297.417469	58.776594	67.236750
1296.975704	59.328267	67.241754
1296.454919	54.608218	67.246759
1295.775552	48.214881	67.251764
1294.475424	56.670459	67.256769
1293.754516	55.679607	67.261774
1293.839198	57.044267	67.266778
1293.266894	56.831224	67.271783
1293.183353	48.995036	67.276788
1292.201641	54.172852	67.281793
1291.327148	47.257161	67.286798
1289.739313	41.597611	67.291802
1288.914159	46.546529	67.296807
1288.605598	50.465614	67.301812
1288.033419	51.214867	67.306817
1287.827097	45.505906	67.311822
1287.709669	49.580154	67.316826
1286.831476	54.903267	67.321831
1285.958419	49.471857	67.326836
1285.561601	50.056097	67.331841
1284.387561	44.564117	67.336846
1283.691440	49.057944	67.341850
1282.731690	48.323498	67.346855
1282.465210	48.619386	67.351860
1281.740258	50.771958	67.356865
1281.024267	50.297345	67.361870
1280.348782	48.735855	67.366874
1279.510151	53.002646	67.371879
1279.392571	49.589554	67.376884
1278.930307	58.008270	67.381889
1278.026932	46.904063	67.386894
1277.166640	46.663749	67.391898
1276.553391	46.196415	67.396903
1276.203332	52.904167	67.401908
1274.761522	57.820508	67.406913
1274.026157	52.055677	67.411918
1273.637617	54.542610	67.416922
1273.037961	57.964060	67.421927
1272.965041	50.871280	67.426932
1271.781269	55.824757	67.431937
1271.428517	50.611761	67.436942
1271.185712	43.872523	67.441946
1269.879327	45.820704	67.446951
1269.172465	45.025600	67.451956
1268.722789	50.185357	67.456961
1268.295362	45.939570	67.461966
1267.323309	51.978978	67.466970
1266.409967	52.364294	67.471975
1266.082611	45.384940	67.476980
1265.352607	49.899173	67.481985
1264.442682	49.226066	67.486990
1263.919376	49.678023	67.491994
1263.344354	60.648146	67.496999
1263.348290	49.456503	67.502004
1261.791906	62.751363	67.507009
1260.949836	60.692238	67.512014
1260.620974	52.871210	67.517018
1259.895411	51.174225	67.522023
1259.797958	41.507366	67.527028
1258.517452	52.412745	67.532033
1257.932033	41.099782	67.537038
1257.436493	52.379564	67.542042
1256.450072	50.745395	67.547047
1255.622905	45.215749	67.552052
1254.933561	50.634026	67.557057
1254.635328	53.798620	67.562062
1254.598264	45.341488	67.567066
1253.455492	54.824812	67.572071
1252.724048	50.012949	67.577076
1251.874872	55.163738	67.582081
1251.493141	48.371316	67.587086
1250.948190	49.809427	67.592090
1250.327318	56.521704	67.597095
1249.500817	54.693588	67.602100
1248.818284	55.541866	67.607105
1248.112665	48.483596	67.612110
1247.540989	51.403309	67.617114
1246.545427	55.332648	67.622119
1245.909918	51.817186	67.627124
1245.322548	55.431129	67.632129
1245.076162	55.622137	67.637134
1244.309008	51.458196	67.642138
1243.451236	57.784344	67.647143
1243.267632	52.010315	67.652148
1241.908839	54.896637	67.657153
1241.109313	61.902383	67.662158
1241.304617	57.755630	67.667162
1240.485830	56.854961	67.672167
1239.890843	49.507371	67.677172
1238.161522	52.605147	67.682177
1237.655061	52.915283	67.687182
1237.409856	53.104116	67.692186
1236.959415	50.530340	67.697191
1236.627155	42.213745	67.702196
1235.622635	55.140584	67.707201
1234.621766	51.922530	67.712206
1234.558389	44.799308	67.717210
1234.041952	51.871447	67.722215
1233.333594	46.557899	67.727220
1232.329895	51.670806	67.732225
1231.186269	50.434590	67.737230
1230.485352	47.219656	67.742234
1229.636023	55.818711	67.747239
1229.340682	48.067737	67.752244
1229.153436	58.696352	67.757249
1228.906355	52.491110	67.762254
1227.955710	52.325875	67.767258
1226.882866	54.032384	67.772263
1226.684927	50.937379	67.777268
1225.781267	55.390564	67.782273
1224.553261	52.931361	67.787278
1224.263544	47.372861	67.792282
1223.308330	57.706663	67.797287
1223.280560	43.705740	67.802292
1222.623575	48.317996	67.807297
1221.609571	42.664433	67.812302
1221.138718	48.309764	67.817306
1220.416427	50.990806	67.822311
1220.341583	49.984483	67.827316
1218.937022	52.324464	67.832321
1218.605745	47.960385	67.837326
1218.183837	53.395639	67.842330
1216.710191	55.764422	67.847335
1216.387956	58.946548	67.852340
1215.997081	40.459880	67.857345
1215.110315	54.396371	67.862350
1214.315683	53.041201	67.867354
1213.256304	58.283639	67.872359
1213.202064	47.465893	67.877364
1212.705233	49.624019	67.882369
1212.204582	48.722964	67.887374
1211.520669	44.958047	67.892378
1210.262182	54.559867	67.897383
1209.997095	49.368578	67.902388
1208.945218	55.995973	67.907393
1208.145707	44.133520	67.912398
1207.888466	52.562524	67.917402
1206.823386	57.331096	67.922407
1206.763787	54.635147	67.927412
1205.707237	62.579328	67.932417
1204.961787	57.563432	67.937422
1204.732232	42.876309	67.942426
1203.718583	57.113196	67.947431
1203.503244	47.435341	67.952436
1202.215949	58.937521	67.957441
1201.653334	55.911268	67.962446
1201.932153	42.937405	67.967450
1200.475365	59.304658	67.972455
1199.680251	51.136780	67.977460
1199.139222	54.753844	67.982465
1198.632391	50.724938	67.987470
1198.544196	53.551221	67.992474
1197.374121	48.471064	67.997479
1196.691612	45.241539	68.002484
1195.986610	52.765546	68.007489
1194.832541	52.741325	68.012494
1194.137778	49.188256	68.017498
1193.867015	54.243573	68.022503
1193.673046	39.557467	68.027508
1193.033589	42.711013	68.032513
1191.980207	48.390164	68.037518
1191.354429	48.928747	68.042522
1190.605252	53.512584	68.047527
1190.088541	35.369166	68.052532
1188.944847	48.964401	68.057537
1188.253740	43.364504	68.062542
1188.348529	41.002895	68.067546
1187.384067	55.100708	68.072551
1186.695198	45.475513	68.077556
1185.686348	48.975711	68.082561
1185.393037	44.615793	68.087566
1185.140980	43.388379	68.092570
1184.155966	51.729234	68.097575
1183.357095	45.664656	68.102580
1182.635782	46.932453	68.107585
1182.161880	47.780148	68.112590
1181.736345	48.947175	68.117594
1180.490762	47.195562	68.122599
1179.960847	47.977457	68.127604
1179.538779	52.505682	68.132609
1179.082506	53.199578	68.137614
1177.947480	44.757161	68.142618
1177.350591	49.056385	68.147623
1177.131345	39.155010	68.152628
1176.487396	51.698816	68.157633
1175.582044	55.801790	68.162638
1174.426571	49.256719	68.167642
1174.263586	47.582630	68.172647
1173.561172	48.424058	68.177652
1172.565990	42.989510	68.182657
1171.789734	50.194157	68.187662
1171.566499	46.991388	68.192666
1171.150073	43.563949	68.197671
1170.299473	46.390906	68.202676
1169.457603	48.623506	68.207681
1168.603252	42.344628	68.212686
1168.466505	39.853724	68.217690
1167.289848	49.551267	68.222695
1166.844399	44.347052	68.227700
1166.279722	45.742367	68.232705
1165.693527	49.902005	68.237710
1165.353943	47.417410	68.242714
1163.710359	46.449565	68.247719
1163.326849	44.572459	68.252724
1163.049134	49.775799	68.257729
1162.386228	53.155984	68.262734
1161.248370	46.511986	68.267738
1160.526871	57.286145	68.272743
1160.451317	50.316583	68.277748
1159.876454	48.355009	68.282753
1159.276920	46.618700	68.287758
1158.148331	46.551048	68.292762
1157.622856	45.613594	68.297767
1157.125598	48.571885	68.302772
1156.423869	42.364768	68.307777
1155.434344	43.624416	68.312782
1155.049586	44.872485	68.317786
1154.158296	51.076095	68.322791
1154.043230	46.796971	68.327796
1152.916037	39.597367	68.332801
1151.708053	46.326095	68.337806
1152.048976	40.475690	68.342810
1151.396295	44.993272	68.347815
1150.517818	42.186498	68.352820
1149.891768	48.664413	68.357825
1148.902934	44.669494	68.362830
1148.428391	42.522992	68.367834
1147.366079	49.423744	68.372839
1146.649113	35.962006	68.377844
1146.140102	41.414539	68.382849
1145.733743	46.549120	68.387854
1145.791936	48.775237	68.392858
1144.649556	45.524992	68.397863
1143.678035	43.973555	68.402868
1143.319012	46.878180	68.407873
1142.148262	53.343973	68.412878
1141.468343	38.709112	68.417882
1140.829834	56.232505	68.422887
1140.641757	47.347318	68.427892
1140.284917	49.366617	68.432897
1139.247963	45.502302	68.437902
1138.707108	42.057490	68.442906
1137.677871	41.311684	68.447911
1137.321833	34.727243	68.452916
1136.373747	43.164006	68.457921
1135.421277	49.003115	68.462926
1135.087232	47.301478	68.467930
1134.756402	55.042460	68.472935
1134.275045	45.182810	68.477940
1133.372251	49.112465	68.482945
1132.555629	47.210053	68.487950
1132.238830	47.128927	68.492954
1130.980078	58.455317	68.497959
1130.552755	39.678483	68.502964
1130.031949	50.606948	68.507969
1129.355145	47.327118	68.512974
1128.190790	49.065892	68.517978
1127.211515	45.889955	68.522983
1126.953885	43.662106	68.527988
1127.146911	43.745514	68.532993
1126.202002	43.510242	68.537998
1125.008026	34.918082	68.543002
1124.181779	43.555026	68.548007
1124.015591	44.713964	68.553012
1123.649326	42.329068	68.558017
1122.241496	42.571328	68.563022
1121.758913	37.596495	68.568026
1121.229627	54.174786	68.573031
1120.745727	46.777413	68.578036
1120.557023	49.810367	68.583041
1119.489433	41.881790	68.588046
1119.065253	33.824497	68.593050
1118.268316	48.109926	68.598055
1117.172855	46.808257	68.603060
1116.441181	48.019025	68.608065
1115.595349	50.126792	68.613070
1115.484001	50.866231	68.618074
1114.768096	53.361071	68.623079
1113.898973	50.004047	68.628084
1113.157105	45.773834	68.633089
1112.496803	50.635732	68.638094
1112.330608	41.930742	68.643098
1111.495585	44.174808	68.648103
1110.685346	41.678051	68.653108
1110.110109	38.837914	68.658113
1109.055484	45.451974	68.663118
1109.262537	43.871229	68.668122
1108.150051	48.107962	68.673127
1107.523612	46.233775	68.678132
1106.930134	51.589073	68.683137
1106.042880	38.454118	68.688142
1105.355443	39.281544	68.693146
1104.450708	52.162487	68.698151
1104.255699	51.508698	68.703156
1103.912587	45.140717	68.708161
1102.554438	45.200801	68.713166
1102.165122	43.475476	68.718170
1101.262825	50.274628	68.723175
1101.083418	40.942332	68.728180
1100.194311	46.416929	68.733185
1099.284634	55.087113	68.738190
1099.096877	47.554170	68.743194
1098.660983	46.626646	68.748199
1097.490819	47.100571	68.753204
1097.086720	48.333798	68.758209
1096.340339	52.334960	68.763214
1095.573594	40.966642	68.768218
1093.724488	50.959725	68.773223
1093.561149	46.798206	68.778228
1093.268410	45.421851	68.783233
1092.861540	51.995259	68.788238
1092.598831	45.961255	68.793242
1092.190211	54.465514	68.798247
1091.162348	53.895525	68.803252
1090.540648	49.675526	68.808257
1089.481402	52.371652	68.813262
1088.944057	45.767341	68.818266
1087.962181	50.718646	68.823271
1087.413795	48.710314	68.828276
1087.196111	42.243889	68.833281
1086.308618	49.398119	68.838286
1085.849114	40.958082	68.843290
1085.278278	49.983510	68.848295
1084.728442	53.238952	68.853300
1083.528239	48.636856	68.858305
1082.954948	51.503968	68.863310
1082.439507	46.794091	68.868314
1081.749274	56.578874	68.873319
1080.950707	53.002944	68.878324
1080.444481	49.133022	68.883329
1079.377052	53.465066	68.888334
1079.156187	50.305713	68.893338
1078.103166	53.802441	68.898343
1077.256223	53.447777	68.903348
1076.481871	41.189500	68.908353
1075.888953	56.545203	68.913358
1076.305190	46.177805	68.918362
1076.227239	50.535799	68.923367
1075.044034	51.134718	68.928372
1074.045110	40.873473	68.933377
1072.637020	53.600230	68.938382
1071.794330	38.643150	68.943386
1070.874898	53.226649	68.948391
1071.028990	48.380416	68.953396
1070.637607	48.366538	68.958401
1070.560143	49.738430	68.963406
1070.037379	40.262050	68.968410
1068.981089	54.179023	68.973415
1067.557236	46.879065	68.978420
1066.999223	42.673034	68.983425
1066.246459	52.436550	68.988430
1066.291036	39.077705	68.993434
1064.892597	47.966180	68.998439
1064.185216	51.681998	69.003444
1063.660621	40.828377	69.008449
1063.362295	53.056435	69.013454
1063.259145	45.924645	69.018458
1061.744178	48.935641	69.023463
1060.755097	44.774611	69.028468
1060.288927	44.846957	69.033473
1059.834019	51.411618	69.038478
1059.399964	48.647963	69.043482
1058.120617	42.039278	69.048487
1057.710318	41.791021	69.053492
1057.539202	41.266162	69.058497
1057.092242	49.865006	69.063502
1056.068558	46.888126	69.068506
1055.282228	48.579551	69.073511
1054.942693	40.634079	69.078516
1054.035273	41.731274	69.083521
1053.004280	56.607417	69.088526
1052.461436	44.195823	69.093530
1051.792180	51.711349	69.098535
1051.317993	49.659528	69.103540
1050.498635	43.793479	69.108545
1049.923212	53.347428	69.113550
1049.511012	48.854338	69.118554
1048.793496	48.968541	69.123559
1048.175020	43.063751	69.128564
1047.526673	42.795077	69.133569
1046.852046	48.267689	69.138574
1046.360106	41.386811	69.143578
1045.418610	58.171076	69.148583
1044.508197	52.142600	69.153588
1044.347820	50.074146	69.158593
1043.274640	48.900908	69.163598
1042.795805	38.092350	69.168602
1042.590856	44.967080	69.173607
1041.632161	42.268796	69.178612
1040.732872	43.768789	69.183617
1039.334073	55.033122	69.188622
1039.351437	44.802315	69.193626
1038.734262	40.592210	69.198631
1037.917515	45.325386	69.203636
1037.319666	42.625702	69.208641
1036.416123	51.567192	69.213646
1036.130786	44.343058	69.218650
1035.731478	56.693403	69.223655
1034.349570	43.309640	69.228660
1034.048150	50.493376	69.233665
1033.330453	49.851733	69.238670
1032.767744	50.110735	69.243674
1032.121917	50.288054	69.248679
1031.330953	53.294282	69.253684
1030.832976	53.454572	69.258689
1029.882134	49.643823	69.263694
1029.689745	44.823769	69.268698
1028.931241	46.404254	69.273703
1027.970396	45.306910	69.278708
1027.568854	44.031687	69.283713
1026.964076	48.668175	69.288718
1026.439124	39.408483	69.293722
1025.114771	50.480471	69.298727
1024.665370	44.575941	69.303732
1023.897841	46.201391	69.308737
1023.781065	46.813084	69.313742
1023.445470	46.973987	69.318746
1022.533918	42.200119	69.323751
1022.063830	39.039638	69.328756
1020.995535	45.296071	69.333761
1019.665765	45.750375	69.338766
1019.656988	37.112384	69.343770
1018.978769	44.732464	69.348775
1018.304916	43.489664	69.353780
1017.298442	48.530450	69.358785
1016.227372	54.453434	69.363790
1016.261343	43.568902	69.368794
1015.790065	51.478397	69.373799
1015.476071	48.910096	69.378804
1014.610122	42.205766	69.383809
1013.507377	48.972941	69.388814
1013.179985	38.664610	69.393818
1012.060160	39.340316	69.398823
1011.005262	49.898821	69.403828
1010.814848	40.993135	69.408833
1010.167327	49.964989	69.413838
1009.827925	45.648507	69.418842
1009.506810	49.545274	69.423847
1008.683956	49.993688	69.428852
1007.874561	46.930784	69.433857
1007.088014	56.023944	69.438862
1006.186753	45.830856	69.443866
1005.518434	52.269443	69.448871
1004.892780	49.835431	69.453876
1004.581770	51.051539	69.458881
1003.906776	44.470817	69.463886
1002.772243	39.395291	69.468890
1002.127796	40.379964	69.473895
1001.952495	45.474585	69.478900
1001.489844	43.020949	69.483905
1000.551936	49.504123	69.488910
1000.008424	44.861827	69.493914
999.242462	45.799419	69.498919
998.312416	40.870839	69.503924
997.606283	39.480422	69.508929
996.933417	43.937134	69.513934
996.884334	40.364314	69.518938
996.169343	44.127622	69.523943
994.717042	49.562110	69.528948
994.561535	39.461569	69.533953
993.679506	44.499991	69.538958
993.376790	40.411690	69.543962
992.306822	47.052473	69.548967
991.493526	42.300073	69.553972
991.108293	41.991874	69.558977
990.571799	46.929284	69.563982
990.241266	44.336978	69.568986
989.084242	48.402948	69.573991
988.163181	39.984740	69.578996
987.989002	34.320438	69.584001
987.440366	46.498593	69.589006
987.124251	47.541508	69.594010
986.014438	45.430005	69.599015
985.424625	43.032883	69.604020
984.489241	38.669268	69.609025
983.653063	51.206126	69.614030
983.310801	44.470142	69.619034
983.063329	48.302195	69.624039
981.692601	47.450308	69.629044
980.878797	47.077354	69.634049
980.237757	51.056541	69.639054
979.773653	39.883124	69.644058
979.582243	48.929227	69.649063
978.951269	42.564381	69.654068
978.170778	39.059585	69.659073
977.086560	52.888193	69.664078
977.066782	46.542615	69.669082
975.916000	46.021331	69.674087
975.109752	45.086195	69.679092
974.803720	34.260297	69.684097
974.410285	50.128900	69.689102
973.343415	53.777615	69.694106
972.557515	48.864219	69.699111
971.852233	50.518093	69.704116
971.642905	43.099777	69.709121
970.514006	52.538525	69.714126
970.119859	42.185976	69.719130
969.237599	44.785107	69.724135
968.563821	50.465989	69.729140
968.473725	39.470878	69.734145
967.281520	37.684132	69.739150
966.763105	42.895140	69.744154
966.211343	49.142461	69.749159
965.496651	49.185143	69.754164
964.563020	42.565833	69.759169
963.712605	53.356152	69.764174
963.209737	42.417126	69.769178
962.711556	45.587155	69.774183
962.549083	51.869644	69.779188
961.897340	41.234390	69.784193
960.996798	55.850972	69.789198
960.438019	43.352926	69.794202
959.292361	47.122103	69.799207
958.436688	49.368939	69.804212
958.162835	49.119427	69.809217
957.454646	51.729404	69.814222
957.095631	47.800739	69.819226
956.036056	50.031577	69.824231
955.464540	49.788045	69.829236
955.152913	46.206902	69.834241
953.920134	49.477084	69.839246
953.610014	48.918011	69.844250
953.070015	51.061841	69.849255
952.471450	53.897374	69.854260
951.806263	47.783112	69.859265
950.725552	49.792584	69.864270
950.497800	46.388514	69.869274
949.892498	41.932457	69.874279
948.774702	45.523190	69.879284
948.207014	40.801760	69.884289
947.356839	51.989120	69.889294
947.354624	45.547778	69.894298
946.365045	40.300215	69.899303
945.396480	45.313992	69.904308
945.208197	39.635925	69.909313
944.227338	47.221004	69.914318
943.489126	49.136296	69.919322
943.321382	49.935130	69.924327
942.687487	49.477296	69.929332
941.722191	47.802475	69.934337
940.631245	53.525202	69.939342
939.970783	52.368536	69.944346
939.708132	47.560918	69.949351
939.376309	44.899368	69.954356
938.529265	49.157772	69.959361
937.495797	48.792448	69.964366
936.692467	44.505695	69.969370
936.311852	44.932852	69.974375
935.613581	47.910586	69.979380
934.468227	38.610727	69.984385
934.025210	51.177746	69.989390
933.992421	40.938176	69.994394
933.756454	43.105722	69.999399
932.547805	46.509135	70.004404
932.031544	36.238297	70.009409
931.103681	45.890496	70.014414
930.866123	44.048018	70.019418
929.778475	45.516739	70.024423
928.843574	50.587909	70.029428
928.783742	39.877736	70.034433
927.536852	50.990943	70.039438
926.925144	46.882940	70.044442
926.218655	45.018938	70.049447
925.488755	60.156137	70.054452
925.440550	43.398128	70.059457
924.643745	43.605265	70.064462
923.687683	42.225298	70.069466
922.778603	38.103100	70.074471
922.125907	40.541348	70.079476
921.975869	35.266448	70.084481
921.088761	46.539469	70.089486
920.269294	39.668133	70.094490
919.867067	45.585914	70.099495
919.511769	49.796019	70.104500
919.041694	41.409926	70.109505
917.926659	47.699248	70.114510
917.004999	48.546288	70.119514
916.802438	47.519612	70.124519
915.676272	48.528381	70.129524
914.960650	47.076842	70.134529
914.115058	55.898294	70.139534
913.924124	39.830619	70.144538
913.674871	36.468129	70.149543
912.779977	52.051186	70.154548
911.872141	45.003942	70.159553
911.062147	44.727448	70.164558
910.800580	45.409728	70.169562
910.050251	49.831956	70.174567
909.152787	54.559238	70.179572
908.949174	42.772437	70.184577
908.206568	50.925365	70.189582
907.135015	38.499765	70.194586
906.551276	34.046340	70.199591
906.187701	38.950979	70.204596
905.945364	37.172081	70.209601
904.594507	35.953282	70.214606
903.546115	37.138590	70.219610
903.723569	33.944584	70.224615
902.355897	35.981108	70.229620
901.784824	31.957727	70.234625
901.323656	42.433100	70.239630
900.781417	36.327795	70.244634
900.671419	33.378405	70.249639
899.552182	50.706232	70.254644
898.684492	42.364559	70.259649
898.088138	58.834332	70.264654
897.331975	45.996311	70.269658
896.540894	43.346716	70.274663
895.577149	48.698736	70.279668
895.090814	41.597858	70.284673
894.612628	53.792370	70.289678
894.503919	39.740633	70.294682
894.146520	41.589918	70.299687
893.030077	40.613589	70.304692
892.407958	33.349272	70.309697
891.285644	40.963317	70.314702
890.637658	36.924691	70.319706
890.171592	35.591853	70.324711
889.571610	46.679522	70.329716
888.840396	37.213228	70.334721
887.389468	45.836793	70.339726
887.045320	38.550522	70.344730
886.722324	33.106709	70.349735
886.303826	42.430498	70.354740
886.191904	37.431293	70.359745
884.764421	37.706985	70.364750
884.221664	41.297524	70.369754
883.727362	39.890974	70.374759
882.300373	46.837249	70.379764
881.899789	39.152510	70.384769
881.313952	45.552503	70.389774
881.009009	41.198558	70.394778
880.552810	43.424745	70.399783
879.126354	42.374024	70.404788
878.631055	35.594011	70.409793
878.155359	43.601359	70.414798
877.642725	46.548883	70.419802
877.195374	41.645810	70.424807
876.517388	45.399240	70.429812
876.046314	33.724573	70.434817
875.348647	44.659246	70.439822
874.304381	45.156656	70.444826
873.270905	42.482666	70.449831
872.572254	44.969447	70.454836
872.564070	38.421379	70.459841
871.557103	43.616207	70.464846
870.811402	45.614891	70.469850
870.145847	39.242965	70.474855
869.521091	36.579099	70.479860
869.273376	33.871969	70.484865
868.303910	48.118269	70.489870
867.658433	41.209645	70.494874
866.916938	28.990414	70.499879
866.491152	33.047205	70.504884
866.548882	37.758901	70.509889
865.195453	41.377772	70.514894
864.762758	36.636787	70.519898
863.808140	44.482232	70.524903
862.819618	51.193159	70.529908
862.135186	45.527056	70.534913
861.792446	39.876637	70.539918
861.323308	50.220361	70.544922
860.351168	37.912348	70.549927
859.630805	34.030195	70.554932
859.391238	39.714468	70.559937
858.133513	34.101566	70.564942
857.096028	40.696936	70.569946
856.689548	37.216520	70.574951
856.274383	39.028336	70.579956
856.508570	36.516545	70.584961
855.244024	45.606322	70.589966
854.471736	34.679527	70.594970
854.019406	41.745823	70.599975
853.226162	39.937348	70.604980
852.402440	36.462482	70.609985
851.523523	45.003868	70.614990
851.063981	44.221726	70.619994
850.723385	42.260726	70.624999
850.129247	39.877786	70.630004
849.225102	34.635747	70.635009
848.622725	35.912425	70.640014
847.977169	31.160144	70.645018
846.864715	42.568074	70.650023
846.077448	39.459969	70.655028
845.703056	32.039159	70.660033
845.536930	35.987138	70.665038
845.174505	45.279615	70.670042
844.173369	39.468433	70.675047
842.932377	40.459782	70.680052
842.512747	35.596965	70.685057
841.816227	43.388731	70.690062
841.150985	40.241569	70.695066
840.626274	37.887394	70.700071
839.501885	35.335953	70.705076
839.849177	38.363146	70.710081
838.299140	33.183192	70.715086
837.198594	34.828998	70.720090
837.121646	38.865118	70.725095
836.471872	33.342290	70.730100
836.448513	29.721656	70.735105
835.555402	36.768322	70.740110
834.795295	34.493545	70.745114
834.048171	32.942028	70.750119
833.520914	38.330203	70.755124
833.063476	38.124380	70.760129
831.889948	41.861251	70.765134
831.600673	31.720892	70.770138
831.058813	30.827728	70.775143
829.511877	40.332959	70.780148
829.268978	28.006628	70.785153
828.596974	38.068532	70.790158
828.266859	38.435734	70.795162
827.323403	36.250781	70.800167
826.053417	38.164020	70.805172
825.989859	26.736523	70.810177
825.576154	42.180311	70.815182
825.610350	41.587533	70.820186
824.536604	36.302712	70.825191
823.569866	43.575139	70.830196
822.322689	38.584878	70.835201
821.273302	41.859987	70.840206
821.029791	36.418749	70.845210
820.793070	32.732430	70.850215
819.862164	44.986320	70.855220
820.134629	31.607428	70.860225
819.234593	33.377568	70.865230
818.229899	44.580345	70.870234
817.608447	40.241940	70.875239
816.637163	45.788670	70.880244
815.711745	33.386625	70.885249
815.203814	39.757485	70.890254
814.788869	41.062454	70.895258
814.393931	36.297642	70.900263
814.027590	44.877147	70.905268
813.327960	41.495104	70.910273
812.514460	44.329571	70.915278
811.184305	44.778470	70.920282
810.763396	38.919619	70.925287
809.573193	42.782502	70.930292
809.479193	37.192899	70.935297
809.069109	40.144175	70.940302
808.467227	39.594828	70.945306
807.482516	36.024396	70.950311
806.502123	41.010614	70.955316
806.785664	31.527623	70.960321
806.139583	32.299849	70.965326
805.146120	30.450684	70.970330
804.190278	28.760461	70.975335
803.565793	38.884880	70.980340
803.081035	27.054693	70.985345
802.153136	40.993492	70.990350
801.367470	37.371205	70.995354
801.356073	24.461708	71.000359
800.305073	29.406731	71.005364
799.482656	24.651600	71.010369
798.687605	40.885005	71.015374
798.096800	38.535052	71.020378
798.083231	40.476228	71.025383
796.954442	40.831037	71.030388
796.124361	31.338286	71.035393
795.790829	36.817220	71.040398
795.094135	37.766264	71.045402
794.729769	33.459613	71.050407
793.384964	46.357923	71.055412
793.045886	36.328723	71.060417
792.388963	38.675346	71.065422
791.867508	44.450140	71.070426
791.075528	36.979690	71.075431
790.243803	42.863680	71.080436
790.254757	37.023220	71.085441
789.094857	40.128987	71.090446
788.378779	39.348166	71.095450
787.939446	41.743565	71.100455
786.942893	46.017730	71.105460
786.109026	38.001067	71.110465
785.394227	40.116040	71.115470
784.814357	41.811213	71.120474
784.893576	36.393640	71.125479
784.325682	40.653584	71.130484
783.570721	35.413242	71.135489
782.842330	36.949130	71.140494
781.371117	40.710163	71.145498
780.601263	39.113603	71.150503
780.058026	41.990590	71.155508
779.859226	36.307633	71.160513
779.230337	33.332271	71.165518
778.820090	39.686400	71.170522
778.368512	35.631912	71.175527
777.315102	38.338147	71.180532
777.286373	33.556792	71.185537
776.201103	38.638343	71.190542
774.897988	38.340559	71.195546
774.283034	31.453571	71.200551
773.881906	42.145222	71.205556
772.818956	30.132651	71.210561
772.237197	32.668099	71.215566
771.673944	36.859357	71.220570
771.497619	33.253480	71.225575
770.951830	32.815707	71.230580
769.789692	36.936668	71.235585
768.959180	34.072025	71.240590
768.166363	38.620747	71.245594
768.160951	32.378907	71.250599
767.948778	45.856840	71.255604
767.119828	40.156702	71.260609
766.343368	38.230112	71.265614
765.038858	38.873961	71.270618
764.429552	39.370303	71.275623
763.691138	41.127372	71.280628
763.381468	34.456100	71.285633
762.679510	42.132361	71.290638
761.852814	31.610417	71.295642
761.442218	36.147346	71.300647
760.471444	34.169575	71.305652
760.177828	36.566460	71.310657
759.709817	32.446899	71.315662
758.614827	34.446223	71.320666
758.077659	32.563508	71.325671
757.093501	35.004477	71.330676
756.774752	26.058849	71.335681
756.111316	30.295687	71.340686
755.287283	33.761926	71.345690
754.896362	33.867987	71.350695
754.325351	31.763320	71.355700
753.218000	30.234448	71.360705
752.654810	36.509387	71.365710
751.754356	35.103353	71.370714
751.744162	39.318682	71.375719
750.916200	45.397810	71.380724
749.918422	38.044723	71.385729
749.597018	36.672911	71.390734
748.947737	45.822694	71.395738
747.720433	33.353970	71.400743
747.353130	38.462528	71.405748
747.355604	31.988431	71.410753
746.625197	36.325949	71.415758
745.645230	36.848291	71.420762
744.837960	31.840327	71.425767
744.109357	39.879157	71.430772
742.985531	40.302203	71.435777
742.016441	39.137651	71.440782
741.656368	43.259767	71.445786
741.318796	39.447843	71.450791
740.572290	50.403520	71.455796
740.290518	39.397857	71.460801
739.928518	34.570180	71.465806
739.031716	33.507319	71.470810
738.423886	33.349371	71.475815
737.845441	43.552744	71.480820
737.104398	38.229111	71.485825
735.812519	35.147868	71.490830
735.250848	45.785712	71.495834
735.065905	37.479882	71.500839
734.835761	40.053385	71.505844
733.873858	32.721000	71.510849
733.400142	43.130629	71.515854
732.480076	40.139631	71.520858
731.627415	33.873994	71.525863
730.891480	45.884109	71.530868
730.394256	38.327655	71.535873
729.812978	34.410254	71.540878
728.780833	37.269161	71.545882
728.302001	34.590978	71.550887
727.923840	38.882761	71.555892
726.864804	26.340624	71.560897
726.160193	31.518014	71.565902
725.550066	45.978271	71.570906
725.251445	44.813728	71.575911
724.380568	41.491430	71.580916
723.642502	32.867488	71.585921
722.917466	40.449816	71.590926
722.121054	43.057960	71.595930
721.858877	37.549671	71.600935
720.934678	38.345079	71.605940
719.984937	36.611593	71.610945
719.434513	37.504014	71.615950
718.952592	35.853799	71.620954
718.681490	35.210301	71.625959
717.810666	41.644911	71.630964
717.290185	36.170215	71.635969
716.440109	40.060108	71.640974
715.629293	45.764878	71.645978
715.470037	40.930495	71.650983
714.278561	47.381357	71.655988
713.588680	40.905478	71.660993
713.270700	37.334924	71.665998
712.388984	43.305639	71.671002
711.892896	36.676571	71.676007
710.760902	46.738736	71.681012
710.546460	38.886357	71.686017
710.412065	42.440503	71.691022
708.823400	41.210398	71.696026
708.475014	27.084507	71.701031
707.752659	41.288080	71.706036
707.227138	32.745751	71.711041
706.573321	39.376461	71.716046
705.700080	36.407842	71.721050
705.420318	38.008193	71.726055
704.852698	36.787110	71.731060
703.928951	29.813308	71.736065
702.917899	43.462429	71.741070
702.229314	32.684750	71.746074
702.355902	38.228536	71.751079
701.274047	40.764011	71.756084
700.255146	33.920186	71.761089
699.911156	41.397766	71.766094
699.450975	39.618705	71.771098
699.044785	36.416532	71.776103
697.903371	44.353992	71.781108
697.225098	38.838440	71.786113
696.457827	41.269500	71.791118
695.983986	38.703747	71.796122
695.313114	35.944000	71.801127
694.380575	37.717756	71.806132
693.836419	34.047013	71.811137
693.653268	34.166034	71.816142
692.514541	37.443050	71.821146
691.978473	34.361017	71.826151
690.970463	43.183858	71.831156
690.959457	35.959750	71.836161
690.221517	27.841031	71.841166
689.393159	37.848018	71.846170
688.978586	37.435930	71.851175
688.385651	39.518987	71.856180
687.435934	35.931142	71.861185
686.803970	32.022432	71.866190
685.922448	37.901542	71.871194
685.558326	33.412900	71.876199
684.263392	40.833536	71.881204
683.818349	36.072194	71.886209
683.491463	33.726385	71.891214
682.770013	41.099298	71.896218
682.404060	25.918593	71.901223
681.656902	35.352361	71.906228
681.040337	34.293209	71.911233
679.820736	30.452016	71.916238
678.783724	33.110856	71.921242
678.437988	34.956970	71.926247
677.985434	33.258311	71.931252
677.697180	31.748991	71.936257
677.294992	34.109614	71.941262
675.961292	31.059238	71.946266
675.659426	28.043658	71.951271
675.086158	45.151252	71.956276
674.309013	39.590673	71.961281
673.143344	30.301888	71.966286
672.554252	36.426935	71.971290
672.302600	30.164923	71.976295
671.841991	37.486833	71.981300
670.897310	34.747158	71.986305
669.930756	35.319713	71.991310
669.327741	36.090499	71.996314
669.166865	27.681487	72.001319
668.166896	38.475330	72.006324
667.605363	32.224962	72.011329
667.082181	34.599209	72.016334
666.311664	27.391153	72.021338
665.343025	32.765352	72.026343
664.750743	37.027113	72.031348
664.425168	27.937019	72.036353
663.792747	29.500690	72.041358
662.866649	41.178666	72.046362
662.184064	35.506371	72.051367
661.340062	39.420886	72.056372
660.874559	38.963451	72.061377
660.588392	35.138388	72.066382
659.259220	41.140376	72.071386
658.866908	37.423493	72.076391
657.848678	42.449766	72.081396
657.975807	37.660662	72.086401
657.577214	34.644287	72.091406
656.292176	35.083130	72.096410
655.994569	42.988133	72.101415
654.623295	38.571387	72.106420
653.786094	38.492218	72.111425
653.164756	34.388284	72.116430
652.556216	44.419193	72.121434
652.464312	31.777304	72.126439
652.023912	44.487137	72.131444
651.471787	32.240654	72.136449
650.679016	35.920618	72.141454
649.824041	36.817857	72.146458
649.463911	24.791103	72.151463
648.403438	32.635755	72.156468
647.672721	27.321822	72.161473
647.144090	28.740615	72.166478
646.261748	34.880380	72.171482
645.640811	29.729601	72.176487
645.030566	31.315920	72.181492
644.768405	35.263772	72.186497
644.137129	36.804750	72.191502
642.517869	38.096598	72.196506
642.298693	32.895934	72.201511
641.724147	32.214828	72.206516
641.339853	34.534100	72.211521
640.719073	29.972996	72.216526
639.567623	44.549673	72.221530
638.889956	41.028513	72.226535
638.409744	34.239248	72.231540
637.966684	38.842135	72.236545
637.343417	33.416640	72.241550
636.674666	35.484666	72.246554
636.357073	28.816350	72.251559
634.922161	41.668146	72.256564
634.146387	36.227335	72.261569
633.685177	36.270056	72.266574
633.270590	38.165467	72.271578
633.023608	22.028926	72.276583
631.999521	34.714811	72.281588
631.375308	39.735947	72.286593
630.984723	41.195824	72.291598
629.567933	40.288778	72.296602
628.894225	29.865392	72.301607
627.961558	37.340805	72.306612
627.762753	33.698531	72.311617
627.569224	34.249569	72.316622
626.827816	35.805865	72.321626
626.029476	27.725929	72.326631
625.398871	31.077340	72.331636
624.632378	29.439578	72.336641
623.699224	38.009219	72.341646
622.720543	38.428345	72.346650
622.395156	32.381854	72.351655
621.948809	39.301083	72.356660
621.812463	29.235212	72.361665
621.131447	33.137990	72.366670
620.224737	35.345070	72.371674
619.736005	24.706062	72.376679
618.592877	37.787323	72.381684
617.529718	36.033030	72.386689
617.448085	39.612080	72.391694
616.690437	44.670685	72.396698
616.218915	24.168015	72.401703
615.171788	40.160412	72.406708
614.477037	38.453521	72.411713
614.120575	31.406232	72.416718
613.431103	38.385272	72.421722
612.958254	32.895330	72.426727
611.699912	39.888946	72.431732
611.467058	34.464457	72.436737
611.309637	33.413092	72.441742
609.816907	37.163251	72.446746
608.983440	28.225707	72.451751
608.863814	32.769626	72.456756
608.283844	33.098734	72.461761
608.077299	27.747893	72.466766
606.664387	37.603606	72.471770
606.279923	32.438369	72.476775
605.452408	35.996010	72.481780
604.271495	26.773411	72.486785
603.582688	32.643589	72.491790
603.087651	44.296662	72.496794
603.039787	34.241286	72.501799
602.571115	36.576991	72.506804
601.666289	34.152194	72.511809
601.141503	27.710423	72.516814
600.379774	38.739753	72.521818
600.018962	36.402922	72.526823
598.973812	29.022080	72.531828
597.885812	35.425231	72.536833
597.941028	27.129590	72.541838
596.540442	26.129784	72.546842
596.138359	24.926930	72.551847
595.581380	31.051609	72.556852
595.091046	29.519291	72.561857
594.251653	26.941979	72.566862
593.135020	32.841251	72.571866
592.913921	29.527253	72.576871
592.509983	24.893482	72.581876
591.583909	28.445511	72.586881
590.687162	30.862849	72.591886
589.816250	35.026705	72.596890
589.521516	33.939266	72.601895
589.386424	32.274245	72.606900
588.329242	33.119697	72.611905
587.532708	25.137351	72.616910
586.978155	37.247824	72.621914
586.814069	32.861097	72.626919
585.562230	32.369460	72.631924
584.631396	26.676563	72.636929
584.060637	32.412050	72.641934
583.401951	37.656977	72.646938
583.361677	25.570697	72.651943
582.528211	38.949015	72.656948
581.921090	35.656949	72.661953
581.457692	32.813914	72.666958
580.271301	38.232146	72.671962
579.686011	29.771133	72.676967
578.874247	33.703817	72.681972
578.217499	37.965184	72.686977
578.110742	35.868624	72.691982
576.896243	47.356040	72.696986
576.383924	29.515205	72.701991
575.797751	31.391073	72.706996
575.257413	36.608618	72.712001
574.176526	28.289360	72.717006
573.012976	33.965768	72.722010
572.912667	28.037027	72.727015
572.523881	34.023160	72.732020
572.183637	25.942113	72.737025
571.448660	24.204230	72.742030
570.264780	28.165543	72.747034
569.984089	25.569872	72.752039
569.373961	42.290637	72.757044
568.119570	40.566359	72.762049
567.901592	35.619296	72.767054
567.384563	39.062958	72.772058
566.187944	34.793545	72.777063
565.437504	41.131760	72.782068
565.082061	34.137984	72.787073
564.714652	31.970435	72.792078
564.181536	38.320358	72.797082
563.638496	31.014142	72.802087
562.402442	29.464740	72.807092
562.018817	30.392541	72.812097
561.861533	24.071747	72.817102
560.566166	28.566869	72.822106
560.314540	39.346967	72.827111
558.928356	33.658283	72.832116
557.607520	37.019421	72.837121
557.351764	33.384542	72.842126
556.734905	47.866473	72.847130
556.720306	31.835772	72.852135
556.345287	33.530209	72.857140
555.920458	36.154439	72.862145
555.108389	29.172989	72.867150
554.139449	38.343600	72.872154
553.190404	25.712026	72.877159
551.993722	41.244161	72.882164
551.532986	39.297459	72.887169
551.443314	37.789252	72.892174
550.736954	41.555470	72.897178
550.345375	29.568462	72.902183
549.305984	36.037102	72.907188
548.399588	37.373800	72.912193
548.478651	33.319207	72.917198
547.520820	36.452369	72.922202
546.583675	35.662100	72.927207
546.059031	31.825020	72.932212
545.257070	37.010426	72.937217
544.673262	42.194767	72.942222
543.722467	46.079049	72.947226
543.323900	44.863754	72.952231
542.926131	36.190232	72.957236
542.017360	44.861489	72.962241
541.234894	29.352339	72.967246
540.427242	35.019479	72.972250
540.175090	37.824900	72.977255
539.749194	31.384746	72.982260
539.061655	40.847385	72.987265
538.142715	31.457164	72.992270
537.557011	47.243016	72.997274
536.895937	32.650112	73.002279
535.667413	41.938227	73.007284
534.891009	40.209816	73.012289
534.741834	40.234211	73.017294
534.343721	44.933211	73.022298
533.942353	40.461625	73.027303
532.952901	41.137993	73.032308
531.879188	44.789933	73.037313
531.700464	40.222175	73.042318
530.325865	43.932775	73.047322
529.878371	34.191395	73.052327
529.272210	45.752989	73.057332
528.567435	45.810615	73.062337
528.425902	46.926659	73.067342
528.101116	54.024792	73.072346
527.279619	41.332283	73.077351
526.507366	38.659799	73.082356
525.578284	38.967821	73.087361
524.625415	35.576333	73.092366
523.709491	43.849763	73.097370
523.663761	34.126380	73.102375
523.317446	35.551049	73.107380
522.348036	39.609037	73.112385
521.481043	33.706675	73.117390
520.918652	43.584030	73.122394
520.607976	30.766110	73.127399
519.701363	29.131852	73.132404
518.787648	36.984533	73.137409
518.719882	32.441579	73.142414
517.217354	38.619343	73.147418
516.564652	32.294630	73.152423
516.055911	35.433342	73.157428
515.361324	40.811129	73.162433
515.273864	34.217862	73.167438
515.026886	43.341740	73.172442
513.904652	36.538173	73.177447
513.165950	33.926650	73.182452
512.512243	38.283812	73.187457
511.603372	32.923463	73.192462
510.882972	41.059186	73.197466
510.473467	37.780635	73.202471
509.864572	39.803290	73.207476
508.216755	39.943568	73.212481
508.100966	38.296163	73.217486
507.478950	42.743811	73.222490
507.470003	39.635029	73.227495
506.682401	31.026736	73.232500
505.590482	40.554326	73.237505
505.211264	40.123961	73.242510
504.860096	42.708733	73.247514
504.434290	29.533595	73.252519
503.260837	42.908996	73.257524
502.442607	42.433864	73.262529
501.994312	39.144198	73.267534
500.738176	37.117889	73.272538
500.226781	29.602987	73.277543
499.974808	38.634171	73.282548
498.673492	40.022760	73.287553
498.059473	30.320581	73.292558
497.332579	41.971145	73.297562
496.638910	34.213545	73.302567
496.389099	28.759216	73.307572
496.358906	34.766794	73.312577
495.728932	27.618375	73.317582
494.485226	34.712128	73.322586
493.863032	34.374712	73.327591
493.434259	35.031192	73.332596
492.590968	36.703643	73.337601
491.963498	35.876898	73.342606
491.186840	37.555694	73.347610
490.347014	37.198337	73.352615
489.322479	40.449512	73.357620
488.473337	33.710468	73.362625
488.672878	31.033697	73.367630
487.787749	35.719839	73.372634
487.844829	35.608241	73.377639
486.986075	27.100563	73.382644
485.927806	34.063074	73.387649
485.247164	32.435492	73.392654
484.524729	41.575713	73.397658
483.702182	35.278137	73.402663
483.069289	35.506598	73.407668
482.536098	45.714061	73.412673
482.326246	32.145102	73.417678
481.167011	41.667258	73.422682
480.309503	41.897106	73.427687
480.320086	35.800561	73.432692
479.594175	43.508180	73.437697
478.930751	37.302540	73.442702
477.820574	40.308277	73.447706
477.449357	36.820287	73.452711
476.935089	42.897003	73.457716
475.969738	40.717062	73.462721
475.015531	25.025408	73.467726
474.105559	32.369456	73.472730
473.853547	32.382661	73.477735
473.752847	25.853639	73.482740
472.618611	34.598662	73.487745
472.242031	31.082385	73.492750
471.308085	36.638156	73.497754
470.524610	35.966034	73.502759
470.029292	35.473466	73.507764
469.221902	37.398700	73.512769
469.025121	35.453748	73.517774
468.238307	44.984717	73.522778
467.563219	36.811069	73.527783
466.848268	33.762486	73.532788
465.995599	45.513154	73.537793
465.599103	37.105857	73.542798
464.406318	39.631574	73.547802
463.761099	37.333230	73.552807
463.269728	46.270844	73.557812
462.497120	47.614629	73.562817
462.534662	42.326570	73.567822
461.770500	44.015860	73.572826
460.698072	49.112635	73.577831
460.454844	41.454288	73.582836
459.671858	47.007089	73.587841
458.784842	40.036133	73.592846
457.761672	42.304248	73.597850
457.157126	47.790553	73.602855
456.973116	36.771744	73.607860
456.362328	46.111902	73.612865
455.439715	34.946127	73.617870
454.643394	41.830997	73.622874
454.422608	32.385500	73.627879
453.783623	37.522068	73.632884
452.720169	45.918677	73.637889
452.198342	36.483320	73.642894
451.623341	44.015880	73.647898
451.075707	45.490841	73.652903
449.951451	37.095766	73.657908
449.118352	45.594997	73.662913
448.920267	36.528479	73.667918
448.587886	40.619017	73.672922
447.695472	33.583470	73.677927
446.902183	33.205515	73.682932
446.273395	41.355936	73.687937
446.087301	38.798929	73.692942
444.717532	38.464503	73.697946
443.775658	41.837697	73.702951
443.669415	39.089781	73.707956
442.996072	34.986506	73.712961
442.829584	33.006366	73.717966
441.821471	43.521383	73.722970
441.123896	35.453431	73.727975
440.558280	31.063688	73.732980
439.263715	47.088634	73.737985
438.626274	30.747083	73.742990
438.122685	46.288346	73.747994
437.809257	42.196809	73.752999
437.586475	40.935613	73.758004
436.954328	45.896156	73.763009
436.461095	30.375368	73.768014
435.082194	46.876579	73.773018
433.471015	43.685155	73.778023
433.363035	33.486165	73.783028
432.169095	35.535669	73.788033
432.392182	43.059349	73.793038
432.092402	48.101085	73.798042
431.633214	43.492588	73.803047
430.750989	38.133217	73.808052
430.141083	46.117390	73.813057
429.104744	38.318664	73.818062
427.835886	42.755596	73.823066
427.398937	41.150599	73.828071
426.999368	34.171116	73.833076
426.512764	41.969562	73.838081
426.251333	38.099234	73.843086
425.452627	37.267898	73.848090
424.910058	45.450517	73.853095
423.822270	45.013305	73.858100
422.485007	48.713982	73.863105
422.430111	45.875560	73.868110
421.901863	48.231752	73.873114
421.741267	44.884898	73.878119
420.635657	37.842868	73.883124
419.645334	53.153357	73.888129
419.222646	49.514728	73.893134
418.911584	37.406978	73.898138
417.694708	43.123342	73.903143
416.918757	44.875840	73.908148
416.378534	47.462622	73.913153
416.288755	39.017375	73.918158
415.405062	49.134916	73.923162
414.423067	38.578107	73.928167
413.633569	44.861456	73.933172
413.183130	53.500761	73.938177
412.997177	39.731935	73.943182
411.670400	48.814295	73.948186
411.636314	45.524309	73.953191
411.130083	49.330058	73.958196
409.522259	58.051270	73.963201
408.857471	44.392525	73.968206
408.596609	40.020817	73.973210
407.943115	39.686012	73.978215
407.741068	40.540867	73.983220
406.396546	44.857753	73.988225
405.858616	38.093813	73.993230
405.508716	36.979133	73.998234
404.703435	45.455838	74.003239
404.048552	38.919559	74.008244
403.225486	42.800524	74.013249
402.802755	31.600415	74.018254
402.288196	45.339328	74.023258
401.288220	42.440252	74.028263
400.425794	43.995611	74.033268
399.774062	49.686968	74.038273
399.310656	38.787886	74.043278
399.213734	43.260416	74.048282
397.954000	40.771756	74.053287
397.435313	38.846845	74.058292
396.541354	48.328291	74.063297
396.327520	43.199361	74.068302
395.311129	43.443033	74.073306
394.625370	42.583267	74.078311
394.530704	41.399585	74.083316
393.552354	49.044297	74.088321
392.837349	36.453971	74.093326
391.947377	52.743121	74.098330
391.740988	48.194719	74.103335
391.172711	35.751737	74.108340
389.980606	44.271447	74.113345
389.473738	34.563164	74.118350
388.856440	35.868502	74.123354
388.245145	41.695418	74.128359
387.381493	38.801009	74.133364
386.462725	46.394459	74.138369
386.589896	38.044659	74.143374
385.803543	43.118074	74.148378
384.533088	40.847557	74.153383
384.099148	34.370124	74.158388
383.506498	42.879858	74.163393
383.027790	47.706354	74.168398
382.062925	48.629576	74.173402
381.577494	40.108069	74.178407
381.202966	35.867153	74.183412
380.484636	43.125087	74.188417
379.345835	40.653599	74.193422
378.498099	47.020744	74.198426
377.630949	43.254622	74.203431
377.702220	37.602390	74.208436
377.192151	41.606548	74.213441
376.202529	38.453879	74.218446
375.568416	45.773166	74.223450
375.085606	47.239393	74.228455
374.719653	34.831212	74.233460
373.517942	46.548157	74.238465
372.799048	42.698605	74.243470
372.322469	28.810668	74.248474
371.938246	32.084750	74.253479
371.095087	35.574054	74.258484
369.993646	45.127768	74.263489
369.722888	45.431542	74.268494
369.145977	41.058742	74.273498
367.986342	48.329551	74.278503
367.269491	41.260776	74.283508
366.564765	47.689855	74.288513
366.453463	38.909640	74.293518
366.005252	45.158580	74.298522
365.642309	46.475195	74.303527
364.418838	42.896845	74.308532
363.815567	39.098134	74.313537
363.361374	33.444387	74.318542
362.277933	39.017506	74.323546
361.548711	45.444862	74.328551
361.221308	31.517149	74.333556
359.952706	38.243377	74.338561
359.574782	37.296914	74.343566
358.930092	38.797596	74.348570
358.227647	38.939711	74.353575
358.284951	36.504011	74.358580
356.971438	41.817371	74.363585
355.952488	48.211099	74.368590
355.691884	41.009268	74.373594
355.068810	42.123771	74.378599
355.133699	44.205035	74.383604
353.854214	55.958607	74.388609
353.568863	42.225772	74.393614
352.929077	41.772975	74.398618
351.704006	45.240113	74.403623
351.201114	46.171792	74.408628
350.350846	48.098078	74.413633
350.173274	44.155362	74.418638
348.912504	40.739716	74.423642
348.514413	47.971584	74.428647
348.111584	45.411466	74.433652
347.398355	52.033441	74.438657
346.290995	40.523595	74.443662
345.447944	44.359443	74.448666
345.020355	51.146792	74.453671
344.870359	37.933493	74.458676
344.250679	43.089656	74.463681
343.472248	37.092822	74.468686
342.713492	42.437415	74.473690
342.043173	39.314893	74.478695
341.014510	37.504628	74.483700
340.056726	43.105160	74.488705
339.582135	39.794366	74.493710
339.160152	36.508502	74.498714
338.601806	51.073159	74.503719
338.548648	43.240945	74.508724
337.665527	53.893625	74.513729
337.144960	42.603718	74.518734
335.940706	46.240570	74.523738
334.698608	44.789365	74.528743
334.489639	47.136630	74.533748
333.570785	52.244209	74.538753
333.549224	39.447819	74.543758
332.825579	45.773175	74.548762
331.759362	45.392283	74.553767
331.628020	40.115415	74.558772
331.120343	47.585919	74.563777
330.018366	52.574104	74.568782
329.638486	42.846039	74.573786
328.702486	47.235418	74.578791
328.269874	39.122474	74.583796
326.981130	43.753482	74.588801
326.321940	45.795040	74.593806
326.083408	46.683781	74.598810
325.709222	47.713396	74.603815
324.942432	42.455048	74.608820
323.700034	51.985960	74.613825
323.666603	39.407513	74.618830
323.067112	45.627123	74.623834
322.075865	42.688678	74.628839
321.343815	36.848890	74.633844
320.502492	39.052313	74.638849
320.237452	33.532721	74.643854
319.776535	36.800215	74.648858
318.693001	40.208761	74.653863
318.504088	38.932689	74.658868
317.878074	42.143618	74.663873
316.580639	40.531782	74.668878
315.916677	41.858941	74.673882
315.291294	34.364399	74.678887
315.373165	38.705236	74.683892
314.184113	35.388224	74.688897
313.470077	40.723971	74.693902
312.559026	40.421482	74.698906
312.335795	41.687314	74.703911
311.690562	31.631735	74.708916
310.522601	39.136462	74.713921
309.970318	31.365331	74.718926
309.436733	34.967365	74.723930
308.836167	35.368324	74.728935
308.535682	28.192681	74.733940
307.608390	39.891805	74.738945
307.153268	38.913581	74.743950
306.781598	33.471868	74.748954
305.388480	44.580221	74.753959
304.688316	34.716020	74.758964
303.999314	40.278777	74.763969
303.565823	39.035153	74.768974
303.208934	44.182592	74.773978
302.359955	39.394228	74.778983
301.772751	27.429358	74.783988
300.916841	41.635295	74.788993
300.578504	42.852965	74.793998
299.696788	36.943708	74.799002
299.043770	43.078552	74.804007
298.469086	39.053124	74.809012
297.144213	38.419750	74.814017
296.793889	32.680320	74.819022
296.197736	31.743243	74.824026
295.528055	39.295192	74.829031
295.720875	35.740942	74.834036
294.368260	42.760645	74.839041
294.062923	35.453605	74.844046
293.262050	40.595830	74.849050
291.826536	30.636238	74.854055
291.134960	36.334428	74.859060
290.790415	34.502439	74.864065
290.054386	34.573746	74.869070
289.984708	35.473018	74.874074
289.358797	38.203962	74.879079
288.453387	40.272332	74.884084
287.830870	38.671133	74.889089
287.212203	36.682063	74.894094
286.596285	32.771068	74.899098
285.838314	33.623717	74.904103
285.461726	32.982539	74.909108
284.755665	37.618677	74.914113
283.831695	38.556223	74.919118
283.178589	28.429771	74.924122
282.118636	38.071506	74.929127
281.999255	36.177243	74.934132
280.640183	41.138057	74.939137
279.550348	37.021731	74.944142
279.317209	29.677059	74.949146
278.884159	43.545275	74.954151
278.665716	25.298530	74.959156
278.334017	41.172265	74.964161
277.908538	35.731095	74.969166
276.605233	34.828785	74.974170
275.751716	38.875633	74.979175
275.478413	34.616986	74.984180
274.175738	35.508925	74.989185
273.701220	38.126690	74.994190
273.521289	31.317995	74.999194
273.002568	30.974714	75.004199
272.042624	27.618052	75.009204
271.018506	32.360018	75.014209
270.737645	33.964127	75.019214
270.221305	34.345523	75.024218
268.821272	39.256127	75.029223
268.286797	33.836799	75.034228
267.779544	39.825483	75.039233
267.580058	42.170728	75.044238
266.846288	31.288813	75.049242
265.697354	43.712729	75.054247
265.131198	38.620125	75.059252
264.763643	39.084565	75.064257
264.245609	43.180090	75.069262
263.312190	38.757502	75.074266
262.573531	40.910971	75.079271
262.224937	29.619244	75.084276
261.349420	42.302196	75.089281
260.450153	43.769163	75.094286
259.919565	33.779598	75.099290
259.397650	43.138077	75.104295
259.035037	33.893354	75.109300
257.797534	44.087337	75.114305
257.304562	39.847792	75.119310
256.954516	39.092336	75.124314
256.146094	42.812532	75.129319
255.373074	34.186805	75.134324
254.426153	42.933308	75.139329
254.086983	32.589245	75.144334
253.730431	30.981541	75.149338
252.293399	42.226104	75.154343
251.534045	34.043270	75.159348
250.965957	31.148358	75.164353
250.918689	28.199700	75.169358
250.447425	32.864273	75.174362
249.795456	37.372335	75.179367
249.488908	28.341809	75.184372
248.720220	41.841264	75.189377
247.990409	38.685143	75.194382
247.070754	34.345064	75.199386
245.974825	49.546957	75.204391
244.577957	45.000139	75.209396
244.107272	42.893742	75.214401
243.819130	37.034324	75.219406
243.739355	35.657450	75.224410
243.032363	40.365195	75.229415
242.814686	34.792497	75.234420
241.707093	40.025589	75.239425
240.941344	37.283761	75.244430
240.676329	37.193424	75.249434
239.010918	41.970326	75.254439
238.577110	31.535522	75.259444
238.132655	36.434697	75.264449
237.722297	41.356448	75.269454
237.591865	34.973453	75.274458
236.281400	36.583138	75.279463
235.656418	36.444380	75.284468
235.065084	36.209465	75.289473
234.140419	37.325154	75.294478
233.717583	33.965244	75.299482
232.993356	38.927769	75.304487
232.483856	28.638171	75.309492
231.050372	37.176779	75.314497
230.396571	34.491549	75.319502
230.090810	36.163083	75.324506
229.125043	43.593696	75.329511
229.427953	29.767563	75.334516
228.717733	35.294097	75.339521
227.737781	33.029487	75.344526
227.481604	33.500889	75.349530
226.533763	41.153808	75.354535
225.356760	31.554906	75.359540
224.446296	31.552314	75.364545
223.939655	38.569511	75.369550
223.817863	34.631061	75.374554
223.325277	40.035034	75.379559
222.692076	30.181482	75.384564
221.601539	40.649073	75.389569
221.067547	26.561820	75.394574
220.801617	32.705309	75.399578
219.585393	33.474688	75.404583
219.282329	26.609349	75.409588
218.689242	36.795102	75.414593
217.177808	36.422268	75.419598
216.606028	42.814359	75.424602
216.123003	44.643376	75.429607
215.911928	42.078825	75.434612
215.129020	38.153047	75.439617
214.816551	42.509766	75.444622
214.094011	41.195706	75.449626
213.265350	44.370334	75.454631
212.714738	31.188238	75.459636
211.658206	38.702694	75.464641
210.647991	36.045012	75.469646
210.634002	38.685676	75.474650
209.882993	36.538920	75.479655
209.720956	39.519152	75.484660
208.749621	33.161495	75.489665
207.547938	32.507821	75.494670
207.356023	33.565800	75.499674
206.513041	39.289162	75.504679
206.259273	28.160392	75.509684
205.596373	35.244633	75.514689
204.255860	37.961116	75.519694
203.620093	30.022751	75.524698
203.137536	39.037004	75.529703
202.763011	32.026425	75.534708
201.997724	33.487802	75.539713
200.903249	33.002844	75.544718
200.478146	33.363082	75.549722
199.798639	33.970600	75.554727
199.715586	31.672639	75.559732
198.566605	29.169002	75.564737
198.107835	31.278448	75.569742
197.464531	31.595174	75.574746
196.500360	41.845725	75.579751
195.928109	31.458344	75.584756
195.053065	32.897486	75.589761
194.592764	33.980948	75.594766
193.823529	33.801795	75.599770
193.230778	32.893357	75.604775
192.487368	34.064425	75.609780
191.586439	38.277296	75.614785
191.443215	36.133324	75.619790
190.782981	21.669857	75.624794
189.972406	32.484560	75.629799
189.439589	34.205674	75.634804
188.989412	33.409761	75.639809
188.068292	33.371112	75.644814
187.265541	33.788982	75.649818
186.200768	36.753050	75.654823
185.950068	32.378047	75.659828
185.118898	39.560211	75.664833
184.845610	36.300979	75.669838
184.903504	37.364292	75.674842
183.840000	41.626742	75.679847
183.085048	29.156614	75.684852
181.835732	36.963445	75.689857
181.083724	46.280059	75.694862
180.686824	31.656583	75.699866
179.900684	41.669394	75.704871
179.737143	20.257951	75.709876
178.450160	32.068470	75.714881
177.980180	34.129316	75.719886
177.735961	37.068771	75.724890
176.960293	37.794611	75.729895
176.001089	30.775324	75.734900
175.334099	38.475624	75.739905
174.281588	35.289973	75.744910
174.079351	37.967248	75.749914
173.707214	37.832914	75.754919
173.124361	35.949031	75.759924
172.209109	38.985754	75.764929
171.517416	39.511292	75.769934
171.244070	36.212994	75.774938
169.935586	39.432383	75.779943
169.246905	33.649137	75.784948
168.584422	46.556087	75.789953
168.650908	41.949879	75.794958
167.938849	42.487592	75.799962
166.804274	46.630397	75.804967
166.167377	33.421264	75.809972
165.727055	30.740895	75.814977
164.644918	36.545518	75.819982
164.196058	35.292702	75.824986
163.453490	46.896626	75.829991
163.255180	40.125825	75.834996
162.660582	41.377565	75.840001
161.707238	45.274580	75.845006
161.197132	31.911487	75.850010
160.350033	43.578719	75.855015
159.485467	32.136267	75.860020
158.784787	38.839384	75.865025
157.904568	31.773406	75.870030
157.400064	32.012268	75.875034
156.939492	41.816911	75.880039
156.474338	32.496240	75.885044
155.428548	33.695861	75.890049
155.044891	37.963343	75.895054
154.665587	33.718145	75.900058
153.369582	34.053220	75.905063
153.177451	30.733109	75.910068
152.630794	38.884856	75.915073
151.910753	40.741089	75.920078
151.286995	32.818044	75.925082
150.004253	40.286031	75.930087
150.013231	36.602255	75.935092
149.256271	49.474091	75.940097
148.075220	44.259957	75.945102
147.741270	30.332626	75.950106
147.096098	54.238383	75.955111
146.694398	42.532643	75.960116
145.687435	42.086772	75.965121
144.811892	46.750797	75.970126
144.590609	41.237537	75.975130
143.697116	45.119559	75.980135
142.928322	40.302093	75.985140
142.238542	35.550025	75.990145
141.737163	36.081623	75.995150
141.670003	32.774823	76.000154
140.687252	34.550181	76.005159
139.901166	40.281165	76.010164
139.473112	40.546789	76.015169
138.738162	39.010279	76.020174
138.134477	38.486986	76.025178
137.152413	40.051847	76.030183
136.383762	34.102330	76.035188
135.410322	37.647948	76.040193
134.444017	34.867501	76.045198
133.957007	28.853916	76.050202
133.553408	31.746488	76.055207
133.419842	25.438250	76.060212
132.899810	29.003632	76.065217
131.916658	44.736025	76.070222
131.406444	36.470644	76.075226
130.503467	34.838607	76.080231
130.075608	36.923419	76.085236
129.240148	40.142247	76.090241
128.425768	35.572585	76.095246
128.006677	31.574984	76.100250
127.475952	40.974444	76.105255
127.068310	33.066062	76.110260
125.862955	37.246663	76.115265
125.121507	37.011051	76.120270
124.985718	36.320317	76.125274
123.722896	39.327823	76.130279
123.527644	38.389537	76.135284
123.215410	32.568607	76.140289
121.891402	40.516931	76.145294
121.195305	34.434593	76.150298
120.210881	43.718821	76.155303
119.886923	38.881149	76.160308
119.598320	35.322201	76.165313
118.408455	37.380553	76.170318
117.921007	36.096070	76.175322
116.989405	43.566232	76.180327
117.294406	30.436020	76.185332
116.240423	40.097673	76.190337
115.094371	38.326533	76.195342
114.857643	42.362790	76.200346
114.345981	37.969771	76.205351
113.441108	32.632521	76.210356
112.360317	43.293047	76.215361
111.672569	43.647402	76.220366
111.834530	39.691495	76.225370
110.874883	46.533746	76.230375
109.977913	35.485257	76.235380
109.430936	46.887900	76.240385
108.910288	43.822649	76.245390
108.230740	36.570316	76.250394
107.174552	39.262946	76.255399
106.831109	40.803192	76.260404
106.148656	35.884887	76.265409
105.367174	49.589425	76.270414
104.657463	32.580282	76.275418
103.776580	36.858409	76.280423
103.416883	36.974958	76.285428
102.788098	39.497218	76.290433
102.220841	37.854996	76.295438
101.524503	25.544572	76.300442
100.659970	48.082753	76.305447
100.249797	38.831606	76.310452
99.926354	42.544462	76.315457
99.175447	35.867223	76.320462
98.086969	29.693486	76.325466
97.665188	37.880269	76.330471
96.992843	35.770177	76.335476
95.905698	36.231688	76.340481
95.061093	39.491165	76.345486
94.791717	34.681243	76.350490
94.126010	41.076417	76.355495
93.841203	35.988896	76.360500
92.886734	34.179391	76.365505
92.033667	43.567410	76.370510
91.734820	28.741634	76.375514
90.932041	39.163459	76.380519
90.299543	36.030551	76.385524
89.862945	34.402245	76.390529
89.062934	36.326272	76.395534
88.409263	33.150419	76.400538
87.213115	38.823034	76.405543
86.680255	39.337536	76.410548
86.415958	37.084468	76.415553
85.851161	41.229071	76.420558
85.415178	39.485404	76.425562
84.371186	46.775116	76.430567
83.978962	38.845544	76.435572
83.229099	41.724068	76.440577
81.675763	37.757124	76.445582
81.269781	44.928376	76.450586
80.622552	44.826608	76.455591
80.798163	44.283396	76.460596
80.225619	37.174555	76.465601
78.915248	34.078530	76.470606
78.363387	34.325914	76.475610
77.430923	46.626299	76.480615
77.105267	39.529996	76.485620
76.718667	29.818927	76.490625
75.515380	39.079104	76.495630
75.131036	30.110888	76.500634
74.264877	36.930402	76.505639
73.628165	45.232585	76.510644
73.059961	40.855975	76.515649
72.712109	46.940886	76.520654
72.413248	35.387262	76.525658
70.913011	41.275031	76.530663
70.157755	41.862004	76.535668
69.899589	41.869181	76.540673
69.093360	37.210903	76.545678
68.411896	33.103566	76.550682
67.391214	44.236524	76.555687
67.208069	37.998757	76.560692
66.703521	36.631955	76.565697
66.116176	40.193096	76.570702
65.016474	37.121742	76.575706
64.244495	45.821301	76.580711
64.343740	31.484215	76.585716
63.346115	36.171547	76.590721
62.541147	41.477911	76.595726
62.120305	40.541991	76.600730
61.413434	43.642474	76.605735
60.293423	43.576374	76.610740
59.496965	41.126011	76.615745
58.783461	45.662799	76.620750
58.728509	34.139988	76.625754
58.108205	35.891113	76.630759
57.301362	36.405622	76.635764
56.494167	33.941708	76.640769
55.767982	39.487969	76.645774
55.411563	38.788093	76.650778
54.998607	39.355458	76.655783
53.885689	36.918303	76.660788
53.490380	44.319814	76.665793
52.475625	36.695914	76.670798
51.680955	35.749093	76.675802
50.903257	39.780211	76.680807
50.352401	37.364711	76.685812
50.360052	38.402689	76.690817
49.781626	31.731021	76.695822
48.589362	27.775209	76.700826
47.992474	34.380411	76.705831
47.337728	36.270460	76.710836
47.082900	41.821956	76.715841
45.678496	43.815273	76.720846
45.361732	41.559361	76.725850
44.660421	39.219391	76.730855
44.160714	34.135960	76.735860
43.027651	29.404262	76.740865
42.295430	37.150882	76.745870
42.169854	31.315722	76.750874
41.488246	39.737304	76.755879
40.971085	35.221696	76.760884
40.119010	33.430172	76.765889
39.310725	38.175829	76.770894
38.971497	44.084404	76.775898
38.400147	44.971013	76.780903
37.339979	45.881040	76.785908
37.050632	36.309605	76.790913
36.074640	36.591031	76.795918
35.406363	32.522489	76.800922
34.544425	40.282274	76.805927
34.295398	36.752467	76.810932
33.702192	34.019779	76.815937
32.732021	36.696492	76.820942
32.156317	33.983302	76.825946
31.428864	34.257245	76.830951
30.980785	36.670772	76.835956
30.236382	32.589233	76.840961
29.603262	44.007037	76.845966
29.170318	31.805011	76.850970
28.324987	33.949566	76.855975
27.155246	36.687337	76.860980
26.518834	28.500457	76.865985
25.905205	39.812292	76.870990
25.957077	26.904294	76.875994
25.178094	36.576828	76.880999
24.128388	31.988332	76.886004
23.736847	37.939030	76.891009
22.798443	36.677012	76.896014
22.718091	29.781015	76.901018
21.367832	38.895491	76.906023
20.853520	37.507475	76.911028
20.485847	40.545858	76.916033
19.361197	38.328604	76.921038
18.776928	31.402566	76.926042
18.229887	35.510973	76.931047
17.573279	34.962827	76.936052
17.304741	32.588921	76.941057
15.923591	28.166986	76.946062
15.411132	31.987245	76.951066
15.013750	30.838507	76.956071
14.441356	32.789435	76.961076
13.897649	25.794476	76.966081
12.891564	36.077489	76.971086
12.189702	26.146560	76.976090
11.826870	32.105358	76.981095
10.831923	39.592313	76.986100
10.120809	39.219291	76.991105
9.351409	33.841077	76.996110
9.091766	30.474136	77.001114
8.619361	31.481536	77.006119
7.803667	28.824104	77.011124
7.233064	31.933988	77.016129
6.146485	39.599274	77.021134
6.428065	26.029436	77.026139
5.014990	33.041802	77.031143
4.331479	30.509722	77.036148
3.892931	35.846416	77.041153
3.322537	35.463477	77.046158