Tue Jun 08 16:36:12 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.227391	102.827428	0.000000
-1.489007	98.424276	0.005005
-2.282737	69.458345	0.010010
-4.473180	27.992310	0.015014
-8.459777	22.713370	0.020019
-13.333866	27.000023	0.025024
-18.636858	22.531764	0.030029
-22.887132	20.132849	0.035034
-27.150659	21.043478	0.040038
-30.922967	18.085414	0.045043
-34.583559	24.576080	0.050048
-38.607773	22.739560	0.055053
-41.882522	12.553935	0.060058
-45.251101	29.629178	0.065062
-48.902077	19.463858	0.070067
-52.608335	20.665375	0.075072
-56.849468	18.808835	0.080077
-60.490140	16.091101	0.085082
-64.663975	17.337280	0.090086
-67.928576	19.374064	0.095091
-72.060229	13.840607	0.100096
-76.337723	14.477379	0.105101
-79.299918	12.201042	0.110106
-83.229081	13.921562	0.115110
-87.009229	15.798097	0.120115
-90.879815	16.226170	0.125120
-94.479856	13.418214	0.130125
-98.156333	13.170027	0.135130
-102.070592	18.522088	0.140134
-105.741501	17.431434	0.145139
-109.444458	22.229803	0.150144
-113.233372	23.909720	0.155149
-116.669726	20.650979	0.160154
-120.736730	19.238684	0.165158
-124.593595	16.335461	0.170163
-128.136230	14.809569	0.175168
-132.012388	13.935700	0.180173
-135.939270	12.783976	0.185178
-140.015234	19.588300	0.190182
-143.380565	10.755567	0.195187
-147.035997	17.271478	0.200192
-151.017206	15.321115	0.205197
-154.964767	18.080170	0.210202
-158.974085	31.228678	0.215206
-162.629717	17.491361	0.220211
-166.037974	21.712694	0.225216
-169.974128	19.533584	0.230221
-173.451318	30.106945	0.235226
-177.441403	28.188519	0.240230
-180.741407	20.145077	0.245235
-184.655158	11.356304	0.250240
-188.838298	27.530871	0.255245
-191.999891	12.791556	0.260250
-195.918446	11.680690	0.265254
-200.328575	18.571187	0.270259
-203.858875	13.860314	0.275264
-207.410532	14.814404	0.280269
-210.814362	8.279217	0.285274
-214.954221	19.220442	0.290278
-218.695058	17.079715	0.295283
-222.476070	11.155108	0.300288
-226.631881	19.578869	0.305293
-230.093602	17.743544	0.310298
-233.796271	16.678573	0.315302
-237.454965	11.013243	0.320307
-240.957695	8.793017	0.325312
-245.211735	13.902701	0.330317
-248.800765	6.123221	0.335322
-252.477642	18.296286	0.340326
-255.980166	16.876897	0.345331
-260.245562	14.886172	0.350336
-264.346564	17.932933	0.355341
-267.507318	8.871811	0.360346
-271.364884	11.822749	0.365350
-275.192898	7.774404	0.370355
-279.351665	9.257386	0.375360
-282.591965	18.113858	0.380365
-286.211667	8.259956	0.385370
-290.008382	12.489981	0.390374
-293.863364	13.906267	0.395379
-297.486714	3.250959	0.400384
-301.549792	11.463492	0.405389
-305.537860	6.964242	0.410394
-309.068298	13.800649	0.415398
-312.620244	11.237632	0.420403
-316.413593	17.654966	0.425408
-320.229294	15.652290	0.430413
-323.820577	16.281714	0.435418
-327.844264	19.994956	0.440422
-331.613654	19.018874	0.445427
-335.241853	5.154670	0.450432
-339.189891	17.441012	0.455437
-342.435376	7.846631	0.460442
-346.822890	17.566985	0.465446
-350.979641	17.740048	0.470451
-353.958987	13.722234	0.475456
-357.857720	14.789658	0.480461
-361.234329	6.410592	0.485466
-365.318083	21.834872	0.490470
-369.034526	10.150014	0.495475
-372.819056	11.524678	0.500480
-376.984513	17.582371	0.505485
-380.420997	21.124276	0.510490
-384.362412	14.154910	0.515494
-387.775895	17.190412	0.520499
-391.685261	16.121166	0.525504
-395.610686	19.759193	0.530509
-399.356238	5.707566	0.535514
-403.295254	15.866517	0.540518
-406.959590	15.136142	0.545523
-410.383087	14.922176	0.550528
-414.397606	20.340633	0.555533
-417.834645	9.957790	0.560538
-421.929873	18.410002	0.565542
-425.701690	15.412728	0.570547
-429.307826	16.810910	0.575552
-433.502466	22.056616	0.580557
-437.048785	8.613427	0.585562
-440.512491	19.267533	0.590566
-444.100204	22.240211	0.595571
-447.841377	5.444667	0.600576
-451.725989	19.680723	0.605581
-455.801445	14.098925	0.610586
-459.532973	20.055800	0.615590
-463.275553	19.303766	0.620595
-466.671581	8.543696	0.625600
-470.967549	22.169077	0.630605
-474.470762	18.873150	0.635610
-478.760767	18.352407	0.640614
-482.240793	26.054569	0.645619
-486.003760	6.309210	0.650624
-489.961668	31.315609	0.655629
-493.041840	17.211876	0.660634
-497.026994	22.583527	0.665638
-500.742218	17.347699	0.670643
-504.425135	19.994942	0.675648
-508.252518	17.379482	0.680653
-511.976263	12.056319	0.685658
-516.188262	18.098831	0.690662
-519.342485	15.955209	0.695667
-523.495397	15.894108	0.700672
-527.267655	17.067075	0.705677
-531.092066	6.926838	0.710682
-534.991059	18.827180	0.715686
-538.816881	13.007647	0.720691
-542.083697	12.030378	0.725696
-545.909789	15.787267	0.730701
-549.412023	12.773451	0.735706
-553.262224	18.918905	0.740710
-557.133949	14.499790	0.745715
-560.976385	6.923530	0.750720
-564.899774	16.089212	0.755725
-568.562854	11.544710	0.760730
-572.401767	6.039670	0.765734
-576.507621	9.621578	0.770739
-579.916798	9.574221	0.775744
-584.062985	16.915530	0.780749
-587.200841	16.454151	0.785754
-591.247165	17.324094	0.790758
-595.047408	14.842598	0.795763
-598.326186	14.571579	0.800768
-602.148976	17.208957	0.805773
-605.795853	17.385551	0.810778
-609.952522	15.803979	0.815782
-613.918047	13.209951	0.820787
-617.552754	14.762781	0.825792
-621.320262	18.995958	0.830797
-625.019920	10.012207	0.835802
-628.850975	19.743105	0.840806
-632.721496	12.050161	0.845811
-636.411321	7.974484	0.850816
-640.151364	18.041455	0.855821
-643.614597	9.579607	0.860826
-647.674475	19.715283	0.865830
-651.498403	18.170987	0.870835
-654.693542	19.556054	0.875840
-658.491114	18.428787	0.880845
-662.206111	27.271050	0.885850
-666.337072	20.722479	0.890854
-670.625565	16.867188	0.895859
-674.287597	8.568552	0.900864
-677.960870	13.925514	0.905869
-681.208740	4.013697	0.910874
-684.925161	7.515451	0.915878
-689.170264	17.891746	0.920883
-692.350888	11.120911	0.925888
-696.830416	16.765845	0.930893
-700.242461	14.971711	0.935898
-703.710480	10.593180	0.940902
-707.649097	13.293152	0.945907
-711.139882	7.053551	0.950912
-715.707156	13.744533	0.955917
-718.760702	14.700772	0.960922
-722.451313	14.745638	0.965926
-726.307722	12.875825	0.970931
-730.012223	14.178640	0.975936
-734.103969	18.881208	0.980941
-738.251770	18.640632	0.985946
-741.964088	10.883147	0.990950
-745.638514	14.870336	0.995955
-749.271717	17.601606	1.000960
-753.250487	16.313695	1.005965
-756.416226	13.685554	1.010970
-760.200686	10.572337	1.015974
-764.067364	5.569572	1.020979
-767.724766	2.008276	1.025984
-771.907895	6.330669	1.030989
-775.542400	7.464415	1.035994
-779.281427	9.333678	1.040998
-783.217948	4.928662	1.046003
-786.564030	13.731376	1.051008
-790.399979	17.815004	1.056013
-794.425350	18.684300	1.061018
-798.137471	4.292234	1.066022
-801.990631	13.556962	1.071027
-805.550308	13.625606	1.076032
-809.363893	16.615630	1.081037
-812.938514	15.720606	1.086042
-816.418913	14.637321	1.091046
-820.541795	18.593791	1.096051
-824.077124	18.313692	1.101056
-828.594054	23.442587	1.106061
-832.019493	15.263341	1.111066
-835.683467	16.969387	1.116070
-839.290395	14.393750	1.121075
-842.857286	9.456433	1.126080
-847.252022	16.528422	1.131085
-850.717864	12.937473	1.136090
-854.477994	16.960776	1.141094
-858.292039	20.151826	1.146099
-862.048379	15.836338	1.151104
-865.556916	14.787921	1.156109
-869.196545	9.357891	1.161114
-873.051786	13.823421	1.166118
-877.251613	18.604270	1.171123
-880.726461	9.599934	1.176128
-884.634161	10.368989	1.181133
-888.492749	19.187125	1.186138
-891.989605	16.558299	1.191142
-895.729049	14.517785	1.196147
-899.619322	17.395139	1.201152
-903.551906	15.874458	1.206157
-907.079972	15.897894	1.211162
-910.832924	14.193238	1.216166
-914.902230	15.584093	1.221171
-918.369500	10.300952	1.226176
-922.052854	12.215643	1.231181
-925.725802	14.379583	1.236186
-929.564206	18.239558	1.241190
-933.374961	25.463992	1.246195
-937.144161	11.485643	1.251200
-940.667765	17.608897	1.256205
-944.554130	19.687527	1.261210
-948.343257	16.914333	1.266214
-952.112822	24.349982	1.271219
-956.082239	13.208429	1.276224
-959.970109	22.573580	1.281229
-963.691241	18.983529	1.286234
-967.417848	13.970328	1.291238
-971.000739	12.119698	1.296243
-974.226292	16.626805	1.301248
-978.423479	18.821189	1.306253
-982.450316	22.278595	1.311258
-986.180925	16.994146	1.316262
-990.253648	22.293629	1.321267
-994.063103	10.646667	1.326272
-997.688687	16.565648	1.331277
-1001.267108	19.753864	1.336282
-1004.860797	11.894162	1.341286
-1008.873053	17.755995	1.346291
-1012.322924	15.195777	1.351296
-1016.052279	15.088480	1.356301
-1019.847639	9.047876	1.361306
-1024.081944	12.109132	1.366310
-1027.472298	12.592141	1.371315
-1031.087540	12.865495	1.376320
-1034.947231	23.220524	1.381325
-1038.618405	19.263572	1.386330
-1042.359344	9.047542	1.391334
-1046.512931	9.455178	1.396339
-1050.293589	13.657022	1.401344
-1054.556704	15.536773	1.406349
-1057.416979	18.711458	1.411354
-1061.298549	21.890593	1.416358
-1064.772964	14.399645	1.421363
-1068.607337	11.103849	1.426368
-1072.822717	15.996487	1.431373
-1076.070206	16.172791	1.436378
-1080.423436	12.129322	1.441382
-1083.957650	20.948363	1.446387
-1087.636512	15.089118	1.451392
-1091.267128	13.713721	1.456397
-1095.149775	7.377152	1.461402
-1098.655249	8.372180	1.466406
-1102.882038	18.090088	1.471411
-1106.295976	9.198647	1.476416
-1110.561153	9.777468	1.481421
-1114.005740	1.865826	1.486426
-1117.657240	1.292130	1.491430
-1121.401354	8.504083	1.496435
-1125.490648	12.646891	1.501440
-1129.310875	11.050686	1.506445
-1132.726629	10.520199	1.511450
-1136.128547	12.619224	1.516454
-1140.340863	12.049488	1.521459
-1143.795720	11.461782	1.526464
-1147.528801	18.108624	1.531469
-1151.846721	16.481464	1.536474
-1155.458279	3.016630	1.541478
-1159.526907	7.299591	1.546483
-1162.714724	1.890133	1.551488
-1166.230998	15.762697	1.556493
-1170.071742	14.036643	1.561498
-1173.940316	18.130147	1.566502
-1178.115240	27.128359	1.571507
-1181.677454	9.909725	1.576512
-1185.796894	9.699054	1.581517
-1189.417128	13.709269	1.586522
-1192.908114	15.528396	1.591526
-1196.574093	18.350917	1.596531
-1200.235590	6.894664	1.601536
-1204.214300	10.835015	1.606541
-1207.881909	13.344825	1.611546
-1211.825617	17.512444	1.616550
-1215.855163	25.323320	1.621555
-1219.244986	13.662938	1.626560
-1223.018802	11.411141	1.631565
-1226.915241	10.174665	1.636570
-1230.549771	10.607804	1.641574
-1234.472566	19.136482	1.646579
-1238.003617	12.735722	1.651584
-1242.093350	22.032752	1.656589
-1245.599823	19.873996	1.661594
-1249.359072	9.810909	1.666598
-1252.842592	15.293622	1.671603
-1256.715391	15.489044	1.676608
-1260.879016	22.355173	1.681613
-1264.845966	25.975432	1.686618
-1268.555183	20.061573	1.691622
-1271.746114	20.750901	1.696627
-1275.384677	6.956113	1.701632
-1279.264238	13.465994	1.706637
-1283.376375	17.082785	1.711642
-1287.337281	14.291255	1.716646
-1291.095975	15.016932	1.721651
-1294.579349	8.020323	1.726656
-1298.298736	13.489508	1.731661
-1302.204763	3.558653	1.736666
-1305.711590	4.567503	1.741670
-1309.654835	10.726799	1.746675
-1313.070125	10.866980	1.751680
-1317.127857	16.419950	1.756685
-1320.876919	14.390550	1.761690
-1324.529200	11.349880	1.766694
-1328.568651	16.903667	1.771699
-1331.839302	13.407882	1.776704
-1336.012499	12.697425	1.781709
-1339.701380	15.875285	1.786714
-1343.292700	11.765962	1.791718
-1347.329054	12.395315	1.796723
-1350.909703	8.857670	1.801728
-1354.650802	17.517068	1.806733
-1358.559007	23.752491	1.811738
-1362.215180	22.210025	1.816742
-1366.361919	29.831183	1.821747
-1369.752349	15.057231	1.826752
-1373.448490	20.909296	1.831757
-1377.178785	13.679671	1.836762
-1380.744730	12.012392	1.841766
-1384.991491	15.384006	1.846771
-1388.391839	12.120133	1.851776
-1392.111620	15.473462	1.856781
-1395.997169	21.087315	1.861786
-1400.094543	15.441164	1.866790
-1403.806680	16.496020	1.871795
-1407.158464	16.294608	1.876800
-1411.002291	15.957873	1.881805
-1415.388276	21.461146	1.886810
-1419.020130	22.112653	1.891814
-1422.391909	17.527962	1.896819
-1425.652420	10.773426	1.901824
-1429.604233	13.494468	1.906829
-1433.451158	17.723022	1.911834
-1437.690522	13.281463	1.916838
-1441.262129	20.662582	1.921843
-1445.134476	13.474794	1.926848
-1448.951659	14.700486	1.931853
-1452.586141	19.862345	1.936858
-1456.193890	11.249233	1.941862
-1460.101167	20.799295	1.946867
-1463.751087	11.099714	1.951872
-1467.227721	12.279944	1.956877
-1471.309294	17.142869	1.961882
-1475.232198	13.248906	1.966886
-1479.165788	21.892531	1.971891
-1482.718641	17.469252	1.976896
-1486.286238	12.389357	1.981901
-1490.161986	20.253385	1.986906
-1493.697908	24.112406	1.991910
-1497.685116	20.331343	1.996915
-1501.435027	15.247219	2.006912
-1502.619235	12.398855	2.016909
-1500.055942	21.267178	2.026906
-1497.403158	16.982236	2.036902
-1494.669551	17.440527	2.046899
-1493.196176	17.196074	2.056896
-1491.668586	17.895154	2.066893
-1489.584004	16.466780	2.076890
-1487.493115	21.694204	2.086886
-1485.447450	19.706581	2.096883
-1483.910630	21.117823	2.106880
-1481.733187	20.559160	2.116877
-1479.876842	19.215846	2.126874
-1478.067085	18.100272	2.136870
-1476.099943	20.805008	2.146867
-1474.182088	22.439692	2.156864
-1472.048303	14.666505	2.166861
-1470.431626	19.897550	2.176858
-1468.743807	21.686365	2.186854
-1466.672690	20.187992	2.196851
-1464.811347	20.416358	2.206848
-1462.847601	14.562272	2.216845
-1461.180896	19.608464	2.226842
-1459.319576	20.920101	2.236838
-1457.100313	17.443560	2.246835
-1455.096417	19.716354	2.256832
-1453.490077	17.722015	2.266829
-1451.765443	18.550480	2.276826
-1449.925173	22.747200	2.286822
-1448.005942	18.337347	2.296819
-1445.676532	19.467405	2.306816
-1443.979326	18.533610	2.316813
-1442.369045	20.885886	2.326810
-1440.396636	22.623453	2.336806
-1438.277963	18.452827	2.346803
-1436.286760	17.798134	2.356800
-1434.501036	19.278085	2.366797
-1432.760809	22.166867	2.376794
-1430.928357	14.754911	2.386790
-1429.003418	18.853706	2.396787
-1427.249426	18.739705	2.406784
-1425.237698	23.354358	2.416781
-1423.182920	21.460839	2.426778
-1421.643968	23.727760	2.436774
-1419.655814	20.079502	2.446771
-1417.684304	24.241046	2.456768
-1415.718693	27.861776	2.466765
-1413.862875	21.505363	2.476762
-1412.152803	19.672248	2.486758
-1410.363510	19.327712	2.496755
-1408.136415	21.831721	2.506752
-1406.664238	11.929014	2.516749
-1404.627724	19.036739	2.526746
-1402.543791	24.764159	2.536742
-1400.745642	18.461132	2.546739
-1398.907135	24.639358	2.556736
-1396.960979	19.385479	2.566733
-1395.204547	26.577289	2.576730
-1393.231502	22.527734	2.586726
-1391.440090	24.369925	2.596723
-1389.377763	17.727092	2.606720
-1387.591534	17.020290	2.616717
-1385.600597	16.143955	2.626714
-1383.928835	13.169353	2.636710
-1382.156982	15.934161	2.646707
-1380.108692	18.684683	2.656704
-1378.370076	18.887930	2.666701
-1376.293066	19.126320	2.676698
-1374.300589	18.351689	2.686694
-1372.827773	17.787256	2.696691
-1370.851630	15.808467	2.706688
-1368.598013	9.426032	2.716685
-1367.003734	13.383656	2.726682
-1365.126165	28.870648	2.736678
-1363.273378	18.795072	2.746675
-1361.035583	16.556745	2.756672
-1359.744512	18.026056	2.766669
-1358.016991	14.116703	2.776666
-1355.862298	19.858077	2.786662
-1353.554995	17.496366	2.796659
-1351.752792	13.503445	2.806656
-1350.168873	20.402022	2.816653
-1348.203539	18.406129	2.826650
-1346.563695	19.958207	2.836646
-1344.605425	19.213969	2.846643
-1342.360518	17.703194	2.856640
-1340.474626	20.702948	2.866637
-1338.655585	17.444599	2.876634
-1337.196068	21.025828	2.886630
-1335.381992	24.394794	2.896627
-1333.201635	24.087060	2.906624
-1330.912770	16.198770	2.916621
-1329.407676	18.750955	2.926618
-1327.559323	22.050408	2.936614
-1325.638467	21.216965	2.946611
-1323.771648	21.361064	2.956608
-1322.052515	19.957601	2.966605
-1319.852812	20.448034	2.976602
-1318.111244	21.300127	2.986598
-1316.386356	24.916408	2.996595
-1314.183830	22.835527	3.006592
-1312.490788	21.127891	3.016589
-1310.949440	21.067851	3.026586
-1308.722231	23.282604	3.036582
-1306.945797	18.468930	3.046579
-1305.039317	20.747071	3.056576
-1303.175163	22.118365	3.066573
-1301.151175	19.422385	3.076570
-1299.342989	21.223796	3.086566
-1297.522680	21.514614	3.096563
-1295.604545	22.492893	3.106560
-1293.622591	22.045759	3.116557
-1291.935359	16.136875	3.126554
-1290.207955	18.275840	3.136550
-1288.232768	18.342062	3.146547
-1286.099850	13.107530	3.156544
-1284.306060	14.440726	3.166541
-1282.470885	18.814269	3.176538
-1280.901261	18.890868	3.186534
-1278.587174	14.239378	3.196531
-1276.703806	13.317545	3.206528
-1274.820612	14.595474	3.216525
-1273.057985	16.666745	3.226522
-1271.304744	17.748444	3.236518
-1269.642703	23.693835	3.246515
-1267.376150	20.190690	3.256512
-1265.414590	10.850925	3.266509
-1263.739773	23.249067	3.276506
-1262.033437	15.860016	3.286502
-1260.051425	14.683333	3.296499
-1258.119639	16.933042	3.306496
-1256.030216	14.068552	3.316493
-1254.191187	17.540766	3.326490
-1252.638539	20.579220	3.336486
-1250.609041	14.947892	3.346483
-1248.607273	11.043647	3.356480
-1246.798563	17.396610	3.366477
-1244.970575	15.531059	3.376474
-1243.082049	9.931059	3.386470
-1241.449140	10.923964	3.396467
-1239.330822	18.274224	3.406464
-1237.324096	21.360773	3.416461
-1235.541895	24.249548	3.426458
-1233.899854	16.286244	3.436454
-1231.938949	19.988891	3.446451
-1229.980067	13.772933	3.456448
-1227.995840	14.921688	3.466445
-1226.008430	14.779936	3.476442
-1224.501755	12.938353	3.486438
-1222.347784	9.165670	3.496435
-1220.339238	13.628425	3.506432
-1218.725909	12.878669	3.516429
-1217.062305	14.744072	3.526426
-1215.016093	13.686803	3.536422
-1212.740999	15.562990	3.546419
-1211.319478	18.429141	3.556416
-1209.329403	15.514549	3.566413
-1207.444075	17.300381	3.576410
-1205.675386	18.932749	3.586406
-1203.607562	19.018670	3.596403
-1201.655521	16.386073	3.606400
-1199.785496	15.767319	3.616397
-1198.033506	18.688963	3.626394
-1196.509720	19.271430	3.636390
-1194.010721	23.759449	3.646387
-1192.236483	20.383965	3.656384
-1190.424992	17.454995	3.666381
-1188.579591	14.635998	3.676378
-1186.714599	17.426792	3.686374
-1185.229554	18.421795	3.696371
-1183.142798	17.222813	3.706368
-1181.103227	11.000923	3.716365
-1179.009332	17.808838	3.726362
-1177.355949	14.499563	3.736358
-1175.219798	16.763619	3.746355
-1174.047460	13.290343	3.756352
-1171.982256	17.961946	3.766349
-1169.733181	21.743582	3.776346
-1167.829011	22.372187	3.786342
-1166.072885	18.285285	3.796339
-1163.993385	17.019977	3.806336
-1162.371632	17.707357	3.816333
-1160.692857	14.308758	3.826330
-1158.979150	18.057448	3.836326
-1156.596034	16.641204	3.846323
-1154.846542	15.165012	3.856320
-1152.909745	14.920537	3.866317
-1151.204033	16.292629	3.876314
-1149.233221	12.552222	3.886310
-1147.665142	18.852496	3.896307
-1145.405190	17.154282	3.906304
-1143.625543	13.068093	3.916301
-1141.734921	10.225543	3.926298
-1139.827187	10.721548	3.936294
-1138.009773	12.421458	3.946291
-1136.064872	11.325108	3.956288
-1134.153012	11.074648	3.966285
-1132.250904	12.922448	3.976282
-1130.648338	19.651933	3.986278
-1128.868459	11.011318	3.996275
-1126.383861	9.995401	4.006272
-1124.760934	12.974017	4.016269
-1123.042522	10.809978	4.026266
-1121.124372	14.610129	4.036262
-1119.264248	11.025484	4.046259
-1116.936205	9.410443	4.056256
-1115.215299	10.901665	4.066253
-1113.826192	13.023310	4.076250
-1111.828167	18.638385	4.086246
-1110.135790	15.451672	4.096243
-1107.856346	15.845136	4.106240
-1105.816670	18.532465	4.116237
-1104.275569	17.405872	4.126234
-1102.265048	17.934437	4.136230
-1100.520465	14.935973	4.146227
-1098.498898	13.737949	4.156224
-1096.557020	12.858316	4.166221
-1095.152079	16.341512	4.176218
-1092.905548	18.930491	4.186214
-1091.232323	22.493301	4.196211
-1089.234359	15.595274	4.206208
-1087.032103	18.643187	4.216205
-1085.440423	14.895187	4.226202
-1083.654153	11.311776	4.236198
-1081.749830	11.660190	4.246195
-1079.847497	12.833748	4.256192
-1077.642972	10.413159	4.266189
-1076.096553	12.125638	4.276186
-1074.163995	15.286261	4.286182
-1072.449957	14.842945	4.296179
-1070.450986	10.267006	4.306176
-1068.342244	14.247871	4.316173
-1066.428507	11.415610	4.326170
-1064.921325	11.385239	4.336166
-1062.980785	15.370880	4.346163
-1060.729607	14.777246	4.356160
-1058.879740	13.481068	4.366157
-1057.816722	11.609009	4.376154
-1055.662905	11.763232	4.386150
-1053.538194	10.916646	4.396147
-1051.618971	11.165689	4.406144
-1049.794950	12.944731	4.416141
-1048.004755	13.547905	4.426138
-1046.078136	17.633167	4.436134
-1044.169427	15.187108	4.446131
-1042.359137	12.780870	4.456128
-1040.058327	12.455767	4.466125
-1038.340922	16.997851	4.476122
-1036.625938	19.830676	4.486118
-1034.968084	16.089905	4.496115
-1032.763927	14.200166	4.506112
-1031.214291	13.279620	4.516109
-1029.323893	14.041466	4.526106
-1027.478996	17.004935	4.536102
-1025.310588	17.285112	4.546099
-1023.316514	17.512622	4.556096
-1021.592790	12.432247	4.566093
-1020.119178	17.475035	4.576090
-1017.884985	18.715742	4.586086
-1015.868155	21.807783	4.596083
-1013.926491	17.987466	4.606080
-1012.267373	17.772548	4.616077
-1010.395259	19.860311	4.626074
-1008.511047	15.735668	4.636070
-1006.809966	10.856001	4.646067
-1004.737680	18.541139	4.656064
-1002.799561	14.251531	4.666061
-1001.049385	13.627356	4.676058
-999.285339	15.232945	4.686054
-997.226402	14.032109	4.696051
-995.177100	15.384008	4.706048
-993.417647	16.730341	4.716045
-991.877597	20.089601	4.726042
-989.524061	26.837639	4.736038
-987.627338	20.662086	4.746035
-986.448768	21.892759	4.756032
-984.296481	17.852917	4.766029
-981.993173	24.853031	4.776026
-980.137256	20.206441	4.786022
-978.450550	16.884007	4.796019
-976.754115	20.792246	4.806016
-974.677154	14.980968	4.816013
-972.779786	24.630709	4.826010
-970.996246	22.612049	4.836006
-969.040864	28.403675	4.846003
-967.207432	22.105809	4.856000
-965.368481	21.153796	4.865997
-963.548247	20.918746	4.875994
-961.662841	22.489686	4.885990
-959.702587	15.024338	4.895987
-957.403453	15.201089	4.905984
-955.777145	19.765965	4.915981
-954.529065	11.781852	4.925978
-952.693346	17.853677	4.935974
-950.252810	14.213326	4.945971
-948.211993	17.231329	4.955968
-946.404041	16.490946	4.965965
-944.693576	12.694540	4.975962
-942.774354	14.580198	4.985958
-941.090140	19.118935	4.995955
-939.057699	17.824267	5.005952
-937.018573	19.800793	5.015949
-935.371038	15.420402	5.025946
-933.345918	20.552717	5.035942
-931.572734	22.154791	5.045939
-929.769811	19.770808	5.055936
-927.831751	22.652727	5.065933
-926.042664	18.067032	5.075930
-924.259654	18.584151	5.085926
-922.039842	17.207529	5.095923
-920.223835	17.113523	5.105920
-918.533223	17.403452	5.115917
-916.599517	22.313948	5.125914
-914.830971	28.038081	5.135910
-912.630111	27.888289	5.145907
-910.293700	24.459879	5.155904
-909.306290	23.750104	5.165901
-907.148354	21.609103	5.175898
-905.311554	23.673731	5.185894
-903.350999	21.235033	5.195891
-901.700165	23.827970	5.205888
-899.962847	23.016341	5.215885
-897.586066	21.070162	5.225882
-895.826062	23.183941	5.235878
-894.220816	23.363647	5.245875
-892.069009	15.536233	5.255872
-890.146102	23.919333	5.265869
-888.787697	23.931162	5.275866
-886.715160	27.160329	5.285862
-884.441995	22.419624	5.295859
-882.628043	23.847153	5.305856
-880.733475	22.188872	5.315853
-878.924779	25.913478	5.325850
-877.171104	26.147545	5.335846
-875.693610	15.204249	5.345843
-873.392993	19.072056	5.355840
-871.306641	15.670388	5.365837
-869.572824	22.245462	5.375834
-867.789574	21.743711	5.385830
-865.978718	16.367438	5.395827
-863.728819	20.898031	5.405824
-862.242641	18.625749	5.415821
-860.425436	23.455492	5.425818
-858.414473	24.080529	5.435814
-856.667746	23.399698	5.445811
-854.270863	19.962123	5.455808
-852.752360	15.953669	5.465805
-850.914246	16.638810	5.475802
-849.305799	19.006265	5.485798
-847.128832	18.837684	5.495795
-845.272105	15.929540	5.505792
-843.244499	16.130827	5.515789
-841.478154	16.531883	5.525786
-839.450941	17.083002	5.535782
-837.574857	12.354755	5.545779
-835.878810	14.307620	5.555776
-833.675248	16.454367	5.565773
-831.993672	16.835199	5.575770
-830.591060	13.637461	5.585766
-828.816144	19.724133	5.595763
-826.092533	19.148333	5.605760
-824.797689	13.123973	5.615757
-822.848459	16.575893	5.625754
-820.764900	19.657764	5.635750
-818.795325	15.600352	5.645747
-816.567589	19.994476	5.655744
-815.636409	19.059223	5.665741
-813.457180	26.969568	5.675738
-811.614046	24.540392	5.685734
-809.691716	20.911992	5.695731
-807.482764	16.383114	5.705728
-805.576821	22.691154	5.715725
-803.882134	13.198171	5.725722
-802.530695	19.759864	5.735718
-800.122498	21.081481	5.745715
-798.268716	16.120740	5.755712
-796.548233	17.967068	5.765709
-794.407416	20.778285	5.775706
-792.669323	21.478643	5.785702
-791.138226	20.908752	5.795699
-788.998095	20.727158	5.805696
-786.934249	19.940153	5.815693
-785.111688	18.246451	5.825690
-783.409307	18.432844	5.835686
-781.470836	22.057759	5.845683
-779.524104	22.118430	5.855680
-777.755562	15.138571	5.865677
-775.852245	17.353481	5.875674
-773.879592	19.322922	5.885670
-772.033896	14.643388	5.895667
-770.565954	20.881972	5.905664
-768.101458	23.922598	5.915661
-766.207414	16.789992	5.925658
-764.766801	18.016856	5.935654
-762.970665	19.790142	5.945651
-760.463432	18.764224	5.955648
-758.768046	18.473227	5.965645
-757.011343	18.303707	5.975642
-755.342870	20.623352	5.985638
-752.748341	26.695862	5.995635
-751.640848	18.754490	6.005632
-749.747602	15.985553	6.015629
-747.564018	13.853269	6.025626
-745.817152	19.533775	6.035622
-744.382911	19.857497	6.045619
-742.065810	20.028908	6.055616
-739.933871	19.535342	6.065613
-738.413120	14.045286	6.075610
-736.629234	18.891476	6.085606
-734.603927	15.062846	6.095603
-732.501326	13.932496	6.105600
-730.814970	17.885650	6.115597
-728.737373	19.354944	6.125594
-726.975592	18.671186	6.135590
-725.250424	22.518485	6.145587
-723.188173	20.588437	6.155584
-721.457361	20.723340	6.165581
-719.641123	19.519626	6.175578
-717.805295	24.344265	6.185574
-715.572682	18.339205	6.195571
-714.064601	14.547578	6.205568
-712.224087	12.366691	6.215565
-710.092157	17.889835	6.225562
-708.409948	17.006326	6.235558
-706.415333	18.153547	6.245555
-704.107375	18.016702	6.255552
-702.793494	19.971184	6.265549
-700.942257	21.807760	6.275546
-698.788614	14.409705	6.285542
-696.975113	14.546631	6.295539
-694.869347	11.262644	6.305536
-693.220150	23.356036	6.315533
-691.376261	22.151539	6.325530
-689.769322	16.435663	6.335526
-687.580139	23.597818	6.345523
-685.799275	19.841589	6.355520
-683.752886	17.840377	6.365517
-681.773501	15.431741	6.375514
-680.195146	23.214871	6.385510
-678.346092	17.273675	6.395507
-676.348559	16.784630	6.405504
-674.281118	21.622105	6.415501
-672.720529	26.478981	6.425498
-670.970171	21.068104	6.435494
-668.819338	21.707958	6.445491
-666.816773	22.373652	6.455488
-665.187426	19.079745	6.465485
-663.264504	16.199044	6.475482
-661.405765	18.497932	6.485478
-659.281438	13.277007	6.495475
-657.579282	12.917306	6.505472
-655.788165	21.524705	6.515469
-653.661663	17.581126	6.525466
-651.974241	12.860822	6.535462
-650.062885	14.988649	6.545459
-648.175220	16.394934	6.555456
-646.520708	17.960189	6.565453
-644.461964	17.739673	6.575450
-642.821685	14.791686	6.585446
-640.613887	17.646423	6.595443
-638.699120	17.038017	6.605440
-637.205603	15.024597	6.615437
-635.121235	13.448065	6.625434
-632.984107	12.614174	6.635430
-631.262900	15.355995	6.645427
-629.785154	13.753933	6.655424
-627.515755	9.602073	6.665421
-625.803351	11.104838	6.675418
-623.638201	17.404057	6.685414
-621.982704	13.707701	6.695411
-620.205738	14.062762	6.705408
-617.871740	10.412806	6.715405
-616.154255	13.614903	6.725402
-614.623020	13.736275	6.735398
-612.893489	8.619475	6.745395
-610.850043	8.625290	6.755392
-608.813842	11.677059	6.765389
-606.845822	8.408054	6.775386
-605.120746	20.047412	6.785382
-603.094304	15.677203	6.795379
-601.600053	14.635099	6.805376
-599.363461	9.450266	6.815373
-597.367057	15.310524	6.825370
-595.619572	8.450928	6.835366
-593.931220	14.061315	6.845363
-591.789088	16.975957	6.855360
-589.779946	13.241457	6.865357
-588.175080	15.355112	6.875354
-586.359628	11.194218	6.885350
-584.715089	16.377790	6.895347
-582.685869	12.960760	6.905344
-580.521428	18.004538	6.915341
-578.762068	18.610829	6.925338
-577.044372	11.588384	6.935334
-574.811469	17.598172	6.945331
-572.875178	12.639166	6.955328
-571.283270	17.416803	6.965325
-569.442509	18.237168	6.975322
-567.989553	19.321682	6.985318
-565.720685	12.478945	6.995315
-563.554122	8.587025	7.005312
-561.633775	11.401413	7.015309
-560.179645	12.087354	7.025306
-558.387350	11.591290	7.035302
-556.460464	16.388522	7.045299
-554.155243	16.888912	7.055296
-552.594328	18.832673	7.065293
-550.527389	14.351992	7.075290
-548.546452	19.669539	7.085286
-546.965471	15.210192	7.095283
-545.008252	20.173748	7.105280
-543.148849	19.980764	7.115277
-541.262252	21.352898	7.125274
-539.565698	27.499000	7.135270
-537.694713	19.419549	7.145267
-535.668028	21.673475	7.155264
-533.264897	20.335149	7.165261
-531.889534	17.315275	7.175258
-530.485430	22.751564	7.185254
-528.161283	24.786096	7.195251
-526.012529	13.539584	7.205248
-524.143813	10.403843	7.215245
-522.628174	22.372032	7.225242
-520.490387	20.834208	7.235238
-518.487129	23.180689	7.245235
-516.998027	15.151356	7.255232
-515.178992	19.184594	7.265229
-512.875297	16.808914	7.275226
-511.402730	15.088819	7.285222
-509.423342	11.345230	7.295219
-507.453037	15.975766	7.305216
-505.361933	15.607487	7.315213
-504.063486	21.977224	7.325210
-502.255234	15.452250	7.335206
-499.906382	16.383078	7.345203
-498.000804	12.071985	7.355200
-496.087469	16.139244	7.365197
-494.207915	16.235676	7.375194
-492.625219	14.429111	7.385190
-490.642745	9.856636	7.395187
-488.646823	18.761748	7.405184
-487.058685	16.127467	7.415181
-485.142810	15.899130	7.425178
-482.863126	14.485974	7.435174
-481.209769	14.889568	7.445171
-479.384562	13.678879	7.455168
-477.595517	12.732467	7.465165
-475.557367	21.065980	7.475162
-473.627388	22.959100	7.485158
-471.558074	19.562901	7.495155
-469.912185	11.990422	7.505152
-468.569148	18.863926	7.515149
-466.192883	17.589922	7.525146
-464.324123	18.920490	7.535142
-462.359407	14.327359	7.545139
-460.621282	17.742558	7.555136
-458.545659	12.371594	7.565133
-456.690159	21.160121	7.575130
-454.718988	18.091009	7.585126
-453.186079	16.346747	7.595123
-451.047216	22.193315	7.605120
-449.641731	20.196637	7.615117
-447.443243	21.289243	7.625114
-445.472146	19.774913	7.635110
-443.720342	22.200533	7.645107
-441.882447	18.345291	7.655104
-439.837698	17.345542	7.665101
-437.927069	18.553141	7.675098
-436.370609	21.888858	7.685094
-434.193960	24.424186	7.695091
-432.186599	20.858811	7.705088
-430.480503	17.436810	7.715085
-429.095366	24.513757	7.725082
-426.784252	22.601221	7.735078
-424.911828	21.286020	7.745075
-423.222455	11.080303	7.755072
-421.210818	16.874806	7.765069
-419.448052	25.420004	7.775066
-417.666757	15.173222	7.785062
-415.195431	12.360184	7.795059
-413.855490	20.447542	7.805056
-411.587623	16.717342	7.815053
-409.705822	18.051625	7.825050
-408.242599	19.428865	7.835046
-406.086805	15.502107	7.845043
-404.419643	11.469078	7.855040
-402.363678	17.792685	7.865037
-400.535870	12.357549	7.875034
-398.688759	20.477659	7.885030
-396.900861	15.246186	7.895027
-394.928232	11.042985	7.905024
-393.010927	20.153710	7.915021
-391.109525	18.920895	7.925018
-389.198022	13.588388	7.935014
-387.308953	13.550441	7.945011
-385.487482	18.286799	7.955008
-383.351431	19.501597	7.965005
-381.944350	17.868657	7.975002
-379.866836	17.822891	7.984998
-377.886276	14.996046	7.994995
-376.217190	11.986692	8.004992
-374.198718	13.396744	8.014989
-372.218529	19.853511	8.024986
-370.332432	11.840690	8.034982
-369.095041	18.787289	8.044979
-366.785670	11.200224	8.054976
-364.665457	16.024063	8.064973
-363.107665	18.701945	8.074970
-361.344817	17.520970	8.084966
-359.068526	11.051711	8.094963
-357.203801	13.296749	8.104960
-355.654526	15.255622	8.114957
-353.893524	17.630300	8.124954
-351.829835	15.434589	8.134950
-349.877472	16.244203	8.144947
-347.877559	14.966052	8.154944
-346.066833	10.136961	8.164941
-344.306560	22.709048	8.174938
-342.724992	17.110659	8.184934
-340.274213	18.696741	8.194931
-338.854093	15.739591	8.204928
-336.489148	19.418032	8.214925
-334.973315	17.417083	8.224922
-332.711823	25.931710	8.234918
-331.090899	21.221730	8.244915
-329.230185	22.674278	8.254912
-327.428819	17.322744	8.264909
-325.508213	22.614394	8.274906
-323.537811	22.744717	8.284902
-321.985815	18.819600	8.294899
-319.835917	16.254609	8.304896
-317.665665	18.659883	8.314893
-316.170740	14.426017	8.324890
-314.433466	15.381620	8.334886
-312.258406	14.759136	8.344883
-310.377255	19.417315	8.354880
-308.650640	9.468057	8.364877
-306.719480	17.938577	8.374874
-304.877963	17.591861	8.384870
-302.975708	19.783457	8.394867
-300.987635	19.091481	8.404864
-298.870094	22.845184	8.414861
-297.500874	13.225975	8.424858
-295.477064	17.254619	8.434854
-293.506122	22.213576	8.444851
-291.545950	24.363231	8.454848
-289.829413	18.478495	8.464845
-288.361468	21.005036	8.474842
-286.019376	18.232806	8.484838
-284.303909	23.959223	8.494835
-282.336380	16.401975	8.504832
-280.387083	18.297796	8.514829
-278.638924	20.573139	8.524826
-276.662109	18.853180	8.534822
-274.594077	14.077597	8.544819
-273.035263	22.231807	8.554816
-271.188243	19.538966	8.564813
-268.906786	10.295650	8.574810
-267.206999	15.767477	8.584807
-265.585154	19.886423	8.594803
-263.203186	14.999298	8.604800
-261.921341	17.453827	8.614797
-260.044069	13.514832	8.624794
-257.763027	9.602228	8.634791
-256.185194	9.624437	8.644787
-254.218541	11.242620	8.654784
-252.106213	15.806240	8.664781
-250.426420	15.410613	8.674778
-248.397688	16.679058	8.684775
-246.812142	9.940222	8.694771
-244.952915	14.110546	8.704768
-242.979836	21.208845	8.714765
-240.781737	16.161192	8.724762
-239.296752	17.803898	8.734759
-237.408971	14.301006	8.744755
-234.789374	11.656681	8.754752
-233.105432	1.722277	8.764749
-231.937449	8.981977	8.774746
-229.772171	7.552209	8.784743
-228.076078	6.124264	8.794739
-225.999538	5.342058	8.804736
-223.884269	10.782165	8.814733
-222.349180	11.506502	8.824730
-220.508608	8.885926	8.834727
-218.604915	13.548579	8.844723
-216.604884	13.193288	8.854720
-214.877427	7.264418	8.864717
-212.816085	7.708010	8.874714
-211.053651	11.474837	8.884711
-209.141003	9.443023	8.894707
-207.185167	3.041835	8.904704
-205.624144	2.412868	8.914701
-203.653286	8.785160	8.924698
-201.709268	4.728430	8.934695
-199.737593	9.294461	8.944691
-198.103237	12.705436	8.954688
-195.558110	6.537537	8.964685
-193.921458	7.810411	8.974682
-192.445671	14.750964	8.984679
-190.510454	12.401486	8.994675
-188.398955	16.242832	9.004672
-186.558602	15.477833	9.014669
-184.790863	12.582440	9.024666
-182.965888	15.680524	9.034663
-180.972138	9.186685	9.044659
-179.116911	9.658132	9.054656
-177.200639	11.635149	9.064653
-175.404895	9.606403	9.074650
-173.739044	10.724491	9.084647
-171.544778	9.340761	9.094643
-169.502202	5.464747	9.104640
-167.777250	10.456068	9.114637
-165.932232	11.914538	9.124634
-164.371432	14.760340	9.134631
-162.348758	12.721927	9.144627
-160.300889	7.387461	9.154624
-158.084228	12.933127	9.164621
-156.445010	12.470192	9.174618
-154.892407	16.682471	9.184615
-152.926693	10.015999	9.194611
-151.120524	12.403171	9.204608
-149.329983	12.286579	9.214605
-147.246113	14.982217	9.224602
-144.973859	10.722198	9.234599
-143.562631	12.876345	9.244595
-141.573832	9.794853	9.254592
-139.770572	9.104210	9.264589
-137.804251	11.695914	9.274586
-136.024446	28.380126	9.284583
-133.950904	14.363160	9.294579
-132.197490	18.346961	9.304576
-130.335662	18.584515	9.314573
-128.504465	20.184883	9.324570
-126.717429	17.431640	9.334567
-124.873539	12.010045	9.344563
-122.880770	18.594808	9.354560
-120.902870	15.451168	9.364557
-118.944350	20.605600	9.374554
-117.324235	16.411975	9.384551
-115.470719	14.785947	9.394547
-113.359418	22.275980	9.404544
-111.482567	11.577376	9.414541
-109.917533	20.606778	9.424538
-108.027312	22.642439	9.434535
-105.900372	21.287279	9.444531
-103.855184	12.101934	9.454528
-102.148434	22.033025	9.464525
-100.303951	19.956426	9.474522
-98.516674	22.086020	9.484519
-96.631729	22.077754	9.494515
-94.641140	15.205081	9.504512
-92.785200	15.400187	9.514509
-91.096931	17.048397	9.524506
-89.297480	16.230377	9.534503
-87.162228	14.792782	9.544499
-85.136885	18.749734	9.554496
-83.285258	14.444887	9.564493
-81.350396	22.849287	9.574490
-79.839371	22.351846	9.584487
-77.871921	20.137582	9.594483
-75.807036	11.363055	9.604480
-74.355007	18.457517	9.614477
-72.262610	22.111705	9.624474
-70.251273	20.376427	9.634471
-68.592872	16.769864	9.644467
-66.485100	16.426595	9.654464
-64.501207	17.679892	9.664461
-62.673633	15.938978	9.674458
-60.850196	15.060341	9.684455
-59.057274	16.308446	9.694451
-57.228056	17.604868	9.704448
-55.158996	22.076813	9.714445
-53.611811	18.003211	9.724442
-51.447306	22.823179	9.734439
-49.638809	17.575644	9.744435
-47.634399	19.387425	9.754432
-46.093143	15.445263	9.764429
-44.163331	15.196544	9.774426
-42.511861	15.442144	9.784423
-40.073095	16.608365	9.794419
-38.413769	15.887507	9.804416
-36.384531	20.908918	9.814413
-34.857006	11.696167	9.824410
-32.626083	15.411987	9.834407
-30.864083	17.581117	9.844403
-28.921214	12.847251	9.854400
-27.074428	16.170888	9.864397
-25.236766	16.713782	9.874394
-23.356844	15.639329	9.884391
-21.422739	15.357080	9.894387
-19.489199	17.245050	9.904384
-17.725833	19.470863	9.914381
-15.587032	11.146083	9.924378
-14.342652	10.845751	9.934375
-12.392312	11.074896	9.944371
-10.137266	15.482169	9.954368
-8.213829	16.875882	9.964365
-6.585277	15.265942	9.974362
-4.983473	23.171027	9.984359
-3.504779	46.460412	9.994355
-2.334771	78.671007	10.004352
-1.023083	133.951882	10.014349
0.000000	185.464912	10.019354
1.138303	218.158056	10.024359
1.584819	244.847068	10.029363
2.084947	275.624868	10.034368
2.542397	286.069937	10.039373
2.394292	307.468798	10.044378
3.233691	314.389894	10.049383
3.458743	336.319651	10.054387
3.141106	332.744286	10.059392
3.648697	346.469580	10.064397
4.222118	361.433670	10.069402
4.109466	363.946012	10.074407
3.728980	354.297240	10.079411
4.031019	360.877881	10.084416
4.021484	357.979516	10.089421
3.892138	368.209872	10.094426
4.163514	374.916166	10.099431
4.102345	378.990661	10.104435
4.275369	384.206394	10.109440
4.231544	373.507170	10.114445
4.287028	384.896316	10.119450
4.365738	385.699877	10.124455
4.528143	376.967696	10.129459
4.269907	377.015910	10.134464
4.622245	369.698599	10.139469
4.364730	385.909999	10.144474
4.541409	398.051628	10.149479
4.713733	393.463467	10.154483
4.407122	393.629313	10.159488
4.506842	389.760937	10.164493
4.752970	406.922536	10.169498
4.652133	406.231689	10.174503
4.831499	402.477938	10.179507
4.543902	415.056010	10.184512
5.317244	407.041657	10.189517
4.890964	414.687023	10.194522
4.801384	411.000303	10.199527
5.188493	410.758270	10.204531
5.091852	417.450317	10.209536
4.834833	410.220099	10.214541
4.765227	422.605282	10.219546
5.026018	411.797752	10.224551
5.182285	420.674626	10.229555
5.206936	421.581006	10.234560
5.407320	421.134157	10.239565
5.363852	425.231680	10.244570
5.152122	417.765941	10.249575
5.392000	425.863911	10.254579
5.021139	419.521195	10.259584
5.334140	422.277919	10.264589
5.145055	429.712105	10.269594
5.701042	445.854740	10.274599
5.959239	452.400703	10.279603
5.694684	457.545836	10.284608
5.784645	449.292201	10.289613
5.449566	452.324252	10.294618
6.136057	462.147957	10.299623
6.443582	467.772481	10.304627
6.212547	459.835182	10.309632
6.082304	449.374134	10.314637
5.796164	451.114165	10.319642
6.178883	443.465967	10.324647
5.990702	446.014561	10.329651
5.880210	446.849381	10.334656
6.004798	439.497275	10.339661
6.142030	464.434640	10.344666
6.550559	464.976401	10.349671
6.207857	461.980804	10.354675
6.110138	462.956324	10.359680
6.227983	458.789968	10.364685
6.344416	474.658277	10.369690
6.453101	479.577586	10.374695
6.782937	474.087300	10.379699
6.362548	484.303689	10.384704
6.529429	470.710887	10.389709
6.738063	479.815254	10.394714
7.041604	474.860375	10.399719
6.616865	481.762251	10.404723
6.690533	483.495854	10.409728
6.914937	484.685344	10.414733
6.328760	485.979080	10.419738
6.400156	486.681668	10.424743
6.612002	488.361976	10.429747
6.225699	487.837698	10.434752
6.819498	502.617254	10.439757
6.711777	519.384929	10.444762
6.763877	513.533711	10.449767
7.268318	519.587105	10.454771
6.777637	522.224286	10.459776
7.207393	519.367408	10.464781
7.189707	526.261877	10.469786
7.354588	520.812488	10.474791
7.458119	527.471446	10.479795
7.383308	533.041553	10.484800
7.397226	523.047956	10.489805
7.474287	548.082216	10.494810
7.407974	543.332830	10.499815
7.904321	557.817712	10.504819
7.855845	563.110956	10.509824
7.930148	548.865694	10.514829
7.412094	541.205320	10.519834
7.756628	554.352068	10.524839
7.987494	558.215096	10.529843
7.669771	565.620089	10.534848
7.953471	553.343323	10.539853
8.001698	566.782061	10.544858
7.890557	568.279344	10.549863
8.003718	568.015993	10.554867
8.003390	574.814353	10.559872
8.360496	566.997992	10.564877
7.958049	581.340565	10.569882
8.252624	570.801860	10.574887
8.402751	571.410035	10.579891
7.747310	578.259933	10.584896
8.124554	580.831597	10.589901
7.845628	573.233624	10.594906
7.917366	584.923277	10.599911
8.544994	592.554208	10.604915
8.715822	603.341914	10.609920
9.010886	599.094611	10.614925
8.346789	600.520526	10.619930
8.364896	606.230644	10.624935
8.592394	611.682632	10.629939
8.546035	614.406666	10.634944
9.251268	602.883744	10.639949
8.882396	611.089343	10.644954
9.063223	611.201614	10.649959
9.343267	614.053625	10.654963
8.873886	610.293430	10.659968
9.146502	607.782416	10.664973
9.097572	618.236772	10.669978
9.089361	606.302110	10.674983
9.695114	606.181266	10.679987
9.392973	599.559071	10.684992
9.340096	586.914080	10.689997
8.977988	585.831458	10.695002
9.508972	584.593736	10.700007
9.489217	578.645081	10.705011
9.358423	577.321885	10.710016
9.390089	582.939673	10.715021
9.078397	596.542381	10.720026
9.298526	611.244404	10.725031
9.481768	617.604348	10.730035
9.117569	626.398872	10.735040
9.039448	620.046538	10.740045
9.347653	626.886754	10.745050
9.656136	624.038809	10.750055
9.685223	635.481215	10.755059
9.859785	641.571086	10.760064
10.084235	641.418912	10.765069
9.778339	651.670646	10.770074
9.564031	649.060355	10.775079
10.090891	653.115807	10.780083
10.100125	657.569081	10.785088
10.161977	647.169698	10.790093
9.979603	651.777398	10.795098
9.933359	648.893957	10.800103
10.006557	656.136837	10.805107
9.978769	657.245637	10.810112
10.145433	655.491313	10.815117
10.164401	663.731492	10.820122
10.305472	662.726007	10.825127
10.802291	666.283339	10.830131
10.727057	669.615474	10.835136
10.781033	669.871860	10.840141
10.472610	661.261299	10.845146
10.562296	670.364857	10.850151
10.805255	663.581675	10.855155
10.146652	672.970239	10.860160
10.712955	681.816037	10.865165
10.654696	692.664399	10.870170
10.682132	693.826101	10.875175
11.068126	684.110833	10.880179
10.732978	693.301850	10.885184
10.734875	686.184211	10.890189
10.874665	697.026645	10.895194
11.012250	688.840505	10.900199
11.133907	690.408803	10.905203
10.999562	697.660446	10.910208
11.330483	695.972688	10.915213
11.013620	698.550491	10.920218
10.942223	700.543064	10.925223
11.009737	700.100437	10.930227
11.238599	716.272996	10.935232
11.567252	718.981696	10.940237
11.624821	719.865476	10.945242
11.772274	720.696347	10.950247
11.907484	720.265007	10.955251
11.696072	719.333769	10.960256
11.684371	703.738542	10.965261
11.360309	707.316238	10.970266
11.706081	724.032034	10.975271
12.036814	718.797292	10.980275
11.715818	723.480490	10.985280
11.758104	724.193212	10.990285
11.792584	733.217458	10.995290
11.842746	733.500156	11.000295
11.881244	727.169229	11.005299
11.885754	729.193789	11.010304
12.216808	719.318188	11.015309
12.198155	728.316411	11.020314
12.087693	728.461258	11.025319
12.185153	726.427483	11.030323
11.910192	729.427964	11.035328
12.128545	729.569327	11.040333
12.206188	731.675293	11.045338
12.167824	730.273870	11.050343
12.541166	730.784965	11.055347
12.239600	737.346500	11.060352
12.371275	734.281751	11.065357
12.782927	749.608287	11.070362
12.494903	756.422107	11.075367
12.629052	764.309046	11.080371
12.659209	764.225709	11.085376
12.884741	766.913810	11.090381
12.624395	763.746537	11.095386
12.938655	762.062419	11.100391
12.919138	758.307947	11.105395
12.672359	766.223490	11.110400
13.035560	751.422468	11.115405
12.925921	761.184714	11.120410
13.200795	757.180429	11.125415
13.134617	764.685672	11.130419
13.092453	767.762295	11.135424
13.208964	764.027130	11.140429
12.960808	765.718841	11.145434
12.850197	769.923096	11.150439
12.889709	768.447134	11.155443
12.921173	767.661352	11.160448
13.359570	776.341638	11.165453
13.618698	772.867801	11.170458
13.621982	783.142003	11.175463
13.833709	770.317288	11.180467
13.722675	773.244671	11.185472
13.684501	766.441754	11.190477
13.512783	766.722233	11.195482
13.361415	770.682034	11.200487
13.756549	775.248778	11.205491
13.600419	791.217431	11.210496
13.662721	782.695209	11.215501
14.183130	787.915069	11.220506
14.207820	798.032455	11.225511
14.312023	794.730831	11.230515
14.175963	784.763966	11.235520
13.980851	768.080277	11.240525
13.729717	772.365072	11.245530
13.994482	787.193421	11.250535
13.955446	789.366374	11.255539
13.827081	800.018020	11.260544
14.173923	793.070526	11.265549
13.884894	800.124532	11.270554
13.998256	806.912974	11.275559
14.613792	797.108939	11.280563
14.515923	789.355477	11.285568
14.627635	786.501768	11.290573
14.457087	801.306086	11.295578
14.076744	796.516125	11.300583
14.725471	807.048353	11.305587
14.761854	821.818790	11.310592
15.013089	819.122334	11.315597
14.852491	798.718292	11.320602
14.415362	798.475474	11.325607
15.080356	808.650843	11.330611
14.784917	819.982846	11.335616
14.883668	816.313870	11.340621
15.081812	826.628110	11.345626
15.267247	821.047596	11.350631
15.077480	818.312675	11.355635
15.188405	822.403173	11.360640
15.206916	817.275613	11.365645
15.439561	822.932842	11.370650
15.151734	818.895550	11.375655
15.050955	813.953442	11.380659
14.987812	822.610801	11.385664
15.276777	820.909699	11.390669
15.254064	830.946815	11.395674
15.221177	830.832446	11.400679
15.493360	825.160084	11.405683
15.536865	832.334323	11.410688
15.810943	826.027700	11.415693
15.518260	821.357698	11.420698
15.419328	831.512487	11.425703
15.345453	826.071955	11.430707
15.398707	839.567303	11.435712
15.453925	836.984977	11.440717
16.123423	853.125944	11.445722
16.028213	857.640208	11.450727
16.232535	848.370060	11.455731
15.762910	852.299978	11.460736
16.322554	851.132716	11.465741
16.252715	855.235268	11.470746
16.124996	841.255689	11.475751
16.263501	837.115295	11.480755
15.889588	849.101815	11.485760
16.291908	845.346441	11.490765
16.346723	845.932680	11.495770
16.319991	856.625754	11.500775
16.595835	851.479325	11.505779
16.449537	857.980341	11.510784
16.222363	854.078690	11.515789
16.637616	861.407490	11.520794
16.680902	849.422366	11.525799
16.700568	847.017841	11.530803
16.662167	859.413020	11.535808
16.658490	850.834180	11.540813
16.742761	847.694644	11.545818
16.718131	862.552947	11.550823
16.994084	855.963758	11.555827
16.607422	860.739965	11.560832
16.928723	855.428638	11.565837
16.760173	864.006595	11.570842
16.544493	853.874524	11.575847
16.538317	851.317722	11.580851
16.782992	860.801389	11.585856
17.169987	861.414752	11.590861
17.467611	867.371509	11.595866
16.784642	864.424700	11.600871
17.248257	868.467766	11.605875
17.013744	882.075252	11.610880
17.710723	881.513247	11.615885
17.887504	883.296321	11.620890
17.728126	872.223809	11.625895
17.373490	855.315933	11.630899
17.417038	866.263012	11.635904
17.303776	872.880736	11.640909
17.438278	877.044968	11.645914
17.528149	884.596144	11.650919
17.847841	883.642124	11.655923
17.804456	877.382411	11.660928
18.100303	885.715759	11.665933
18.015586	878.164074	11.670938
17.800134	881.425560	11.675943
18.149916	878.664040	11.680947
17.815318	889.878467	11.685952
17.856866	875.412737	11.690957
17.875587	876.358844	11.695962
17.803270	884.534266	11.700967
18.152245	875.965606	11.705971
18.166146	883.575990	11.710976
18.196670	883.576272	11.715981
18.302406	888.182801	11.720986
18.109058	884.796387	11.725991
18.239578	879.015270	11.730995
18.051712	888.734562	11.736000
18.163301	891.503404	11.741005
18.380374	888.803320	11.746010
18.338366	896.756450	11.751015
18.854525	906.201493	11.756019
18.560659	903.953741	11.761024
18.850613	910.031038	11.766029
18.997029	911.483799	11.771034
18.498918	899.120943	11.776039
18.952194	894.229864	11.781043
18.710124	905.861853	11.786048
18.803669	908.166430	11.791053
18.792745	907.051203	11.796058
18.528956	913.561334	11.801063
18.901793	905.911449	11.806067
18.518961	911.268848	11.811072
19.026561	907.477646	11.816077
18.877926	902.176614	11.821082
18.953156	904.748012	11.826087
19.138313	900.234081	11.831091
18.988334	923.174744	11.836096
19.382574	917.291950	11.841101
19.715765	928.168491	11.846106
19.509350	929.238464	11.851111
19.909164	917.788205	11.856115
19.478918	918.283141	11.861120
19.871296	907.553365	11.866125
19.832818	898.652444	11.871130
19.571662	902.129004	11.876135
19.747985	893.742302	11.881139
19.744490	900.865816	11.886144
19.522487	897.751151	11.891149
19.451852	887.398402	11.896154
19.477774	914.186731	11.901159
19.939529	923.615454	11.906163
19.999933	932.352744	11.911168
19.911274	928.535481	11.916173
20.032870	931.164064	11.921178
20.086596	934.360462	11.926183
20.131915	928.563541	11.931187
19.870112	939.730786	11.936192
20.106920	939.410704	11.941197
20.428006	931.239158	11.946202
20.108465	934.653895	11.951207
20.523009	936.360683	11.956211
20.158094	936.296925	11.961216
20.189049	936.284502	11.966221
20.274970	932.884932	11.971226
20.311848	936.042772	11.976231
20.440850	930.327028	11.981235
20.265928	938.645990	11.986240
20.200681	945.696034	11.991245
20.451716	952.582512	11.996250
20.725607	958.715872	12.001255
20.686604	962.113699	12.006259
20.806909	967.018539	12.011264
20.857466	960.316770	12.016269
21.373657	958.859323	12.021274
20.727169	954.621386	12.026279
21.332826	952.793340	12.031283
21.000768	966.860910	12.036288
21.208008	955.414825	12.041293
21.269669	953.619656	12.046298
20.753341	938.807022	12.051303
20.955007	934.848008	12.056307
20.846222	927.969890	12.061312
20.493443	928.053655	12.066317
20.900238	935.110786	12.071322
20.908061	958.642596	12.076327
21.063499	958.891458	12.081331
20.923956	943.966850	12.086336
21.152476	937.989700	12.091341
21.103814	934.611626	12.096346
20.929198	928.085449	12.101351
21.040319	928.689669	12.106355
20.877872	937.602142	12.111360
21.269249	925.836748	12.116365
20.993978	933.758838	12.121370
21.346332	932.863162	12.126375
21.462035	930.041111	12.131379
21.059966	941.847005	12.136384
20.871830	940.465715	12.141389
21.134743	936.388832	12.146394
20.762258	918.071597	12.151399
21.063595	916.175339	12.156403
20.811865	918.790167	12.161408
20.730636	923.849151	12.166413
21.161230	925.209375	12.171418
20.827253	924.927947	12.176423
21.065855	905.912670	12.181427
20.527863	905.708063	12.186432
20.655578	915.364578	12.191437
20.893774	929.881045	12.196442
20.991482	930.674273	12.201447
21.408411	929.730025	12.206451
21.096571	920.194654	12.211456
20.898170	912.315868	12.216461
20.734703	901.681794	12.221466
20.192364	915.096564	12.226471
20.652645	917.174056	12.231475
20.854936	929.525654	12.236480
20.883869	927.783862	12.241485
21.082131	933.776234	12.246490
20.922861	941.710018	12.251495
21.249205	947.625962	12.256499
21.141360	931.331735	12.261504
20.993137	925.403395	12.266509
20.956563	912.339297	12.271514
20.801989	916.672707	12.276519
21.096815	907.385428	12.281523
20.581933	906.681076	12.286528
20.928208	911.478472	12.291533
20.749035	909.621181	12.296538
20.709658	916.143362	12.301543
21.288339	922.270239	12.306547
21.364067	928.882031	12.311552
21.089270	913.395649	12.316557
21.486600	910.507947	12.321562
20.861698	915.749748	12.326567
20.988001	916.679781	12.331571
20.978725	916.583863	12.336576
21.042400	923.881000	12.341581
20.964655	907.362956	12.346586
21.164776	920.764510	12.351591
21.572952	913.269612	12.356595
21.142144	908.536820	12.361600
20.884330	896.401182	12.366605
20.869621	886.959753	12.371610
20.728861	899.444749	12.376615
20.803978	898.993708	12.381619
20.926472	890.994784	12.386624
20.738653	889.453578	12.391629
20.930357	883.650917	12.396634
20.583530	899.004623	12.401639
21.027239	906.058174	12.406643
21.155096	910.388157	12.411648
20.501382	906.554888	12.416653
21.167888	897.217704	12.421658
20.439811	899.955253	12.426663
20.917654	903.548263	12.431667
21.251676	918.603282	12.436672
21.086701	909.294180	12.441677
20.861633	899.636182	12.446682
20.815495	899.463690	12.451687
20.992763	887.090833	12.456691
20.856609	889.401239	12.461696
21.041224	901.690715	12.466701
21.152005	899.933314	12.471706
20.745855	896.512727	12.476711
20.892056	892.860859	12.481715
21.138716	898.068483	12.486720
20.834310	898.361846	12.491725
20.895663	899.270645	12.496730
20.743161	899.187047	12.501735
20.527459	896.749055	12.506739
20.678500	895.671584	12.511744
20.695910	903.078090	12.516749
21.272042	904.758354	12.521754
20.678161	913.812679	12.526759
20.747922	909.971022	12.531763
21.046458	919.030233	12.536768
21.103784	913.897171	12.541773
21.121258	910.981046	12.546778
20.637867	914.335056	12.551783
20.736280	911.183609	12.556787
20.657000	908.815776	12.561792
20.792174	918.994824	12.566797
21.072997	918.140228	12.571802
21.082237	928.019168	12.576807
21.105113	918.836140	12.581811
21.557231	907.719547	12.586816
21.140962	904.288456	12.591821
21.303363	907.410953	12.596826
21.200679	900.554301	12.601831
21.682751	899.660465	12.606835
21.272337	887.997439	12.611840
21.059401	880.089188	12.616845
21.481275	878.044376	12.621850
20.811755	882.498434	12.626855
20.829000	867.784645	12.631859
21.041836	875.345128	12.636864
21.186256	872.155800	12.641869
21.001406	872.826158	12.646874
20.515341	870.645311	12.651879
20.616914	863.665235	12.656883
20.541758	871.987188	12.661888
20.846426	871.114690	12.666893
20.924641	873.320446	12.671898
21.303405	880.346042	12.676903
21.038464	878.688589	12.681907
20.988427	871.002673	12.686912
20.720376	874.695932	12.691917
21.151348	879.958000	12.696922
20.631576	883.787577	12.701927
20.909356	875.398884	12.706931
20.908793	877.119996	12.711936
20.791489	885.066688	12.716941
20.803715	877.638116	12.721946
20.872506	878.780898	12.726951
20.748569	876.644145	12.731955
20.737565	874.371978	12.736960
20.868745	874.623814	12.741965
20.952853	872.374024	12.746970
20.878548	873.653444	12.751975
20.990811	875.083242	12.756979
20.893152	874.036966	12.761984
20.485154	881.086144	12.766989
20.848408	872.941346	12.771994
20.623375	878.250757	12.776999
20.677939	876.022216	12.782003
21.010357	887.434510	12.787008
20.919649	907.175957	12.792013
20.846706	882.103287	12.797018
20.728338	899.649631	12.802023
21.088231	905.547175	12.807027
21.053971	899.842066	12.812032
20.765196	889.555927	12.817037
21.157116	880.163597	12.822042
20.552626	884.200327	12.827047
20.807128	895.742433	12.832051
20.828257	906.143523	12.837056
21.109539	908.747881	12.842061
21.128532	896.818201	12.847066
20.818138	895.319326	12.852071
20.826395	888.152742	12.857075
20.588813	881.155414	12.862080
20.805216	900.888012	12.867085
21.156757	904.098867	12.872090
21.082745	895.347327	12.877095
20.989732	895.889047	12.882099
20.825987	883.119536	12.887104
20.603664	888.157307	12.892109
20.799840	889.960345	12.897114
20.958178	911.382097	12.902119
20.987343	916.317943	12.907123
20.970787	908.716267	12.912128
20.642286	898.859295	12.917133
20.701157	899.374184	12.922138
20.909162	921.602950	12.927143
21.211380	914.858446	12.932147
20.734636	910.059319	12.937152
21.016720	923.592084	12.942157
21.180280	906.422808	12.947162
20.839108	906.495898	12.952167
20.774616	890.350595	12.957171
20.994225	891.802647	12.962176
20.531545	893.179052	12.967181
20.737229	894.636649	12.972186
20.828876	912.603309	12.977191
21.046284	925.378622	12.982195
21.094700	928.311854	12.987200
20.712915	923.766438	12.992205
21.081059	909.173234	12.997210
20.953290	912.201406	13.002215
20.991047	895.491073	13.007219
21.217364	897.646176	13.012224
20.788267	892.879543	13.017229
20.679199	900.490888	13.022234
20.811002	899.160140	13.027239
20.861860	895.197387	13.032243
20.875113	896.119960	13.037248
20.756104	899.298599	13.042253
21.058367	899.834125	13.047258
20.796180	906.148587	13.052263
20.828862	900.962518	13.057267
20.698474	907.321092	13.062272
21.131355	933.020482	13.067277
21.683948	914.758585	13.072282
21.136912	921.864382	13.077287
21.192050	907.901548	13.082291
21.321514	905.640029	13.087296
20.771294	907.345256	13.092301
21.130881	897.726357	13.097306
21.072160	895.207372	13.102311
20.947860	894.898284	13.107315
21.090907	901.777202	13.112320
21.215264	898.626836	13.117325
20.941348	886.279628	13.122330
20.801245	878.275208	13.127335
20.881966	882.436031	13.132339
20.902332	882.167664	13.137344
20.817916	885.984176	13.142349
20.930626	886.098260	13.147354
20.897260	890.542326	13.152359
20.815016	891.705874	13.157363
20.920052	894.819257	13.162368
20.644666	908.349696	13.167373
21.259756	893.825085	13.172378
20.841131	894.603419	13.177383
20.679626	888.347770	13.182387
20.744304	888.371407	13.187392
21.259922	904.080924	13.192397
21.356409	894.579767	13.197402
20.704485	882.281585	13.202407
20.935108	881.107577	13.207411
20.842926	881.988227	13.212416
20.764673	884.456860	13.217421
20.591470	878.346508	13.222426
20.520807	884.335233	13.227431
20.830362	900.346915	13.232435
21.106885	906.647169	13.237440
20.531831	909.867291	13.242445
21.079593	898.923382	13.247450
20.610172	904.121154	13.252455
20.795069	911.189083	13.257459
20.680314	913.674242	13.262464
20.648860	916.500772	13.267469
21.011050	913.484490	13.272474
20.919529	906.652764	13.277479
21.007304	903.321960	13.282483
20.975026	914.746278	13.287488
20.607869	912.646089	13.292493
21.085976	906.572475	13.297498
21.081300	916.123403	13.302503
21.301738	914.083518	13.307507
21.335127	917.414845	13.312512
20.995851	910.778752	13.317517
20.598574	891.037660	13.322522
20.628117	899.556015	13.327527
20.717045	904.384111	13.332531
21.058458	910.158511	13.337536
20.567199	918.082890	13.342541
21.011652	909.949808	13.347546
20.862707	913.104373	13.352551
20.894694	909.611030	13.357555
21.172542	913.584118	13.362560
21.064381	921.738074	13.367565
21.297328	908.095670	13.372570
20.876356	892.295691	13.377575
20.676873	885.098806	13.382579
20.903087	880.378108	13.387584
20.585571	895.742969	13.392589
21.049575	901.448979	13.397594
21.089535	903.452089	13.402599
20.613055	906.881097	13.407603
20.719831	903.841900	13.412608
20.795953	914.971320	13.417613
21.344236	908.670939	13.422618
20.819025	913.389207	13.427623
20.880158	912.713592	13.432627
21.271945	909.596712	13.437632
21.030079	903.975353	13.442637
21.197735	887.631173	13.447642
20.707086	890.158277	13.452647
20.845663	888.471111	13.457651
20.974231	891.721377	13.462656
20.771240	891.117102	13.467661
21.147787	885.842476	13.472666
20.871092	890.170370	13.477671
20.653502	885.799310	13.482675
21.097009	881.016093	13.487680
20.459119	887.403647	13.492685
20.955362	877.818171	13.497690
20.755773	881.326802	13.502695
20.696869	881.002949	13.507699
21.000381	893.069536	13.512704
20.729125	903.218786	13.517709
21.190216	900.235681	13.522714
20.946955	891.297244	13.527719
20.791083	889.289121	13.532723
20.830360	887.212407	13.537728
20.797202	890.064882	13.542733
21.085934	887.453563	13.547738
20.921220	893.089738	13.552743
20.532721	892.326613	13.557747
20.940733	889.870103	13.562752
20.923564	905.568341	13.567757
21.119450	895.026208	13.572762
20.759198	893.010495	13.577767
20.822325	888.673803	13.582771
21.041951	887.543522	13.587776
20.986788	900.406995	13.592781
20.998508	892.785873	13.597786
20.848512	892.101065	13.602791
20.957511	885.693250	13.607795
20.924745	894.023735	13.612800
20.839469	893.069676	13.617805
21.017274	889.790543	13.622810
21.053320	891.651431	13.627815
20.635998	890.776802	13.632819
20.750697	899.062665	13.637824
20.603884	899.945972	13.642829
20.873091	894.320674	13.647834
21.112600	918.033354	13.652839
20.747637	905.895949	13.657843
20.855351	891.849511	13.662848
20.604055	903.394266	13.667853
21.130301	903.637971	13.672858
21.244615	915.704251	13.677863
21.184714	905.385176	13.682867
21.044094	898.163192	13.687872
21.134364	897.763237	13.692877
21.202266	890.985892	13.697882
21.078311	894.628003	13.702887
21.022541	888.596196	13.707891
21.250703	890.831112	13.712896
20.886481	897.386482	13.717901
21.048914	892.150934	13.722906
21.063218	888.603786	13.727911
20.864777	891.333023	13.732915
20.868388	897.916115	13.737920
20.704399	891.907598	13.742925
20.958766	891.188985	13.747930
21.053299	898.071483	13.752935
21.349736	899.446417	13.757939
20.817163	873.773234	13.762944
20.494509	880.305286	13.767949
21.140929	880.309706	13.772954
20.745504	884.286908	13.777959
20.631520	897.428880	13.782963
20.708337	889.288185	13.787968
20.837685	899.986502	13.792973
20.764136	893.089727	13.797978
20.855736	898.343278	13.802983
20.904362	896.803374	13.807987
21.012520	887.516138	13.812992
21.080805	901.570271	13.817997
21.052832	893.050046	13.823002
20.952822	901.638377	13.828007
20.689841	903.722639	13.833011
20.933055	892.099908	13.838016
20.633488	898.165779	13.843021
20.748443	892.641138	13.848026
20.835803	896.968193	13.853031
21.223763	897.411658	13.858035
20.807812	899.251755	13.863040
20.325937	909.899351	13.868045
20.939704	890.985950	13.873050
20.872889	895.936667	13.878055
20.722375	901.470148	13.883059
21.203588	897.721762	13.888064
20.976162	898.984807	13.893069
20.884618	900.177976	13.898074
20.903842	895.249608	13.903079
20.827313	904.052596	13.908083
21.427179	895.978926	13.913088
21.089069	906.751869	13.918093
20.919046	901.575687	13.923098
20.991679	904.887651	13.928103
20.814747	906.985186	13.933107
20.894770	895.584246	13.938112
21.193584	898.470592	13.943117
21.226246	890.438518	13.948122
20.868786	882.273603	13.953127
20.884741	876.225161	13.958131
20.950216	874.404479	13.963136
20.689642	879.234072	13.968141
21.148641	867.596861	13.973146
20.916614	874.873624	13.978151
20.607890	875.318908	13.983155
20.594222	886.030683	13.988160
20.493019	883.323987	13.993165
21.142647	900.199058	13.998170
21.362833	901.737064	14.003175
20.775451	889.758594	14.008179
20.972983	875.764664	14.013184
20.359697	883.541792	14.018189
20.851355	892.504725	14.023207
20.885440	902.291975	14.028224
21.078314	908.015935	14.033242
21.286092	904.227712	14.038259
20.700606	899.966014	14.043277
21.102287	903.937533	14.048295
21.023299	894.426481	14.053312
20.579067	903.742952	14.058330
20.780672	905.163975	14.063347
21.029347	915.594403	14.068365
21.009603	910.674251	14.073383
21.147669	914.967366	14.078400
20.917230	917.528672	14.083418
21.205868	911.081541	14.088435
20.911998	916.668867	14.093453
21.232141	912.533797	14.098471
21.009320	912.157793	14.103488
20.730226	917.034274	14.108506
21.088974	914.653323	14.113523
21.258214	915.383790	14.118541
21.120048	912.656121	14.123559
21.394935	912.700324	14.128576
21.424057	921.401757	14.133594
21.374009	912.669244	14.138611
20.972182	915.431206	14.143629
21.153242	917.060490	14.148647
21.122372	920.071467	14.153664
20.937830	920.670455	14.158682
21.549076	933.219966	14.163699
21.515712	949.573942	14.168717
21.784019	947.793174	14.173735
21.556609	933.012332	14.178752
21.188875	925.238274	14.183770
21.399053	933.753149	14.188787
21.151757	945.597456	14.193805
21.233220	944.166461	14.198823
21.582769	949.029269	14.203840
21.308624	960.750623	14.208858
21.690510	952.640926	14.213875
21.595215	954.766837	14.218893
21.695588	945.723851	14.223911
21.538783	941.909147	14.228928
21.678527	947.805627	14.233946
21.683012	947.932415	14.238963
21.579096	957.701625	14.243981
21.543333	948.362668	14.248999
21.477491	951.446975	14.254016
21.353925	953.373783	14.259034
21.491933	955.205740	14.264051
21.656123	959.444779	14.269069
21.513508	958.038815	14.274087
21.687193	974.350229	14.279104
22.137239	972.943049	14.284122
22.107456	967.932075	14.289139
21.658324	965.223853	14.294157
22.028031	969.830439	14.299175
22.437242	954.110057	14.304192
22.001274	958.231903	14.309210
22.267930	944.290808	14.314227
21.735315	951.721162	14.319245
21.365417	952.964174	14.324263
21.593899	948.089646	14.329280
21.630783	963.199624	14.334298
21.691277	970.271585	14.339315
21.879330	979.794674	14.344333
21.968360	983.793440	14.349351
22.632036	979.708515	14.354368
22.425191	987.318872	14.359386
22.235845	979.574442	14.364403
22.629108	978.456149	14.369421
22.504737	972.676695	14.374439
22.426422	956.405212	14.379456
22.689350	959.908379	14.384474
22.319471	946.455971	14.389491
22.392930	953.965887	14.394509
22.338696	948.068504	14.399527
22.538409	949.807592	14.404544
22.391582	962.113456	14.409562
21.933821	960.046519	14.414579
22.535184	950.917633	14.419597
22.240853	959.113879	14.424615
22.181384	948.079272	14.429632
22.072137	953.174297	14.434650
21.863003	951.504131	14.439667
22.004227	959.938317	14.444685
21.759046	966.663842	14.449703
22.771684	969.379372	14.454720
22.301122	979.374462	14.459738
22.296427	977.154246	14.464755
22.378992	988.080556	14.469773
22.369825	990.723236	14.474791
22.383247	988.148315	14.479808
22.480679	984.517977	14.484826
22.638912	981.845783	14.489843
22.587147	985.277312	14.494861
22.698707	999.131134	14.499879
22.539563	988.020669	14.504896
22.496111	989.376228	14.509914
22.685295	989.856414	14.514931
22.916363	984.890873	14.519949
22.733930	990.260287	14.524967
22.733768	977.027552	14.529984
22.869064	988.707469	14.535002
22.520232	979.704472	14.540019
22.522515	985.400111	14.545037
22.844324	980.658005	14.550055
22.992923	988.439326	14.555072
22.867345	996.281439	14.560090
22.712031	1003.595942	14.565107
22.995139	999.474681	14.570125
23.000924	1012.615499	14.575143
23.218571	1002.165667	14.580160
22.864017	994.499952	14.585178
22.882251	991.008397	14.590195
23.256321	997.615556	14.595213
22.935608	993.822248	14.600231
23.039683	987.777621	14.605248
23.049417	997.803373	14.610266
22.736666	1010.636575	14.615283
23.009370	1005.703655	14.620301
22.934640	1008.547355	14.625319
23.078405	1001.019835	14.630336
23.007178	1010.668505	14.635354
23.000941	1012.378340	14.640371
23.095764	1009.513456	14.645389
22.865474	1013.438230	14.650407
23.423781	1008.346098	14.655424
23.078705	1014.690319	14.660442
22.963228	1004.996073	14.665459
23.390207	1002.206140	14.670477
23.316453	1015.044434	14.675495
23.416640	1017.123844	14.680512
23.415541	1018.061094	14.685530
23.453853	1013.475860	14.690547
23.723616	1003.438380	14.695565
23.265172	1013.875931	14.700583
23.523481	1006.210257	14.705600
23.342940	1008.393314	14.710618
23.112277	1011.925211	14.715635
23.424132	1006.327267	14.720653
23.432924	1011.086698	14.725671
23.672042	1018.153647	14.730688
23.648533	1020.849188	14.735706
23.447633	1027.101761	14.740723
23.624252	1027.495513	14.745741
23.914882	1034.932011	14.750759
23.946089	1008.596917	14.755776
23.450116	1001.623206	14.760794
23.538731	1004.658599	14.765811
23.793697	1020.866357	14.770829
23.703816	1027.538114	14.775847
23.922903	1021.283583	14.780864
23.564710	1027.096951	14.785882
23.927761	1020.437791	14.790899
23.935847	1017.977173	14.795917
23.775665	1025.972095	14.800935
24.120489	1020.151550	14.805952
23.880463	1009.816405	14.810970
23.728195	1011.557971	14.815987
24.029496	1008.883685	14.821005
24.247786	1018.181914	14.826023
23.981060	1001.760786	14.831040
24.164592	1006.661920	14.836058
23.885637	1007.176305	14.841075
23.909855	1011.514558	14.846093
23.727527	1013.852657	14.851111
23.866975	1020.519345	14.856128
23.885553	1030.532971	14.861146
24.052867	1038.650107	14.866163
24.224837	1032.380027	14.871181
24.215048	1045.210136	14.876199
24.428783	1033.995152	14.881216
24.316466	1037.045709	14.886234
24.467560	1026.067078	14.891251
24.471756	1003.362067	14.896269
23.884032	1009.805374	14.901287
24.160002	1019.690998	14.906304
24.003910	1033.282057	14.911322
24.188736	1033.990960	14.916339
24.345667	1032.338341	14.921357
24.004064	1039.791108	14.926375
24.515428	1031.557195	14.931392
24.601830	1036.672643	14.936410
24.176134	1036.059746	14.941427
24.489949	1029.726762	14.946445
24.269047	1037.274982	14.951463
24.817757	1033.981856	14.956480
24.642194	1025.112128	14.961498
24.293402	1030.069103	14.966515
24.481187	1030.440073	14.971533
24.394178	1033.716621	14.976551
24.370686	1039.893109	14.981568
24.486579	1028.375985	14.986586
24.408029	1031.905431	14.991603
24.711138	1019.798696	14.996621
24.256180	1027.501616	15.001639
24.496677	1031.843348	15.006656
24.800270	1029.204101	15.011674
24.548525	1030.567816	15.016691
24.960046	1037.815072	15.021709
24.546682	1040.831807	15.026727
24.826775	1052.759799	15.031744
25.257482	1051.658706	15.036762
25.080395	1050.518898	15.041779
24.947981	1032.057640	15.046797
24.672771	1043.471344	15.051815
24.704575	1030.895728	15.056832
24.599107	1037.913886	15.061850
24.547980	1056.316435	15.066867
24.653685	1053.859942	15.071885
24.605316	1061.070697	15.076903
24.992971	1059.850991	15.081920
24.890925	1063.276590	15.086938
25.048066	1064.812346	15.091955
25.406102	1056.192869	15.096973
24.951619	1056.478670	15.101991
24.852603	1057.863843	15.107008
25.062671	1055.074867	15.112026
24.850988	1056.305329	15.117043
25.221191	1056.982842	15.122061
25.119611	1063.846791	15.127079
25.344292	1057.407416	15.132096
25.588102	1058.006594	15.137114
25.150835	1057.389774	15.142131
25.450893	1055.009809	15.147149
25.239098	1062.145427	15.152167
25.122171	1054.647616	15.157184
25.228083	1060.167235	15.162202
25.325159	1078.755045	15.167219
25.812859	1077.054373	15.172237
25.304874	1066.275335	15.177255
25.349870	1079.616588	15.182272
25.603311	1081.563030	15.187290
25.571978	1075.711282	15.192307
25.523456	1053.825531	15.197325
25.580658	1061.424119	15.202343
25.536436	1062.669573	15.207360
25.445640	1062.756395	15.212378
25.346682	1074.891924	15.217395
25.825088	1078.347936	15.222413
25.884966	1079.659014	15.227431
25.921984	1076.398094	15.232448
26.022955	1062.627438	15.237466
25.415049	1055.970158	15.242483
25.668079	1051.843804	15.247501
25.567522	1060.026565	15.252519
25.806887	1079.155767	15.257536
26.119662	1077.273260	15.262554
25.670352	1078.324371	15.267571
25.654867	1080.976024	15.272589
25.959339	1084.659117	15.277607
25.958914	1082.025133	15.282624
26.284087	1085.266063	15.287642
25.953599	1087.029532	15.292659
25.949459	1075.999129	15.297677
25.899609	1079.077175	15.302695
26.126306	1078.192568	15.307712
26.386942	1077.207252	15.312730
26.027219	1069.392769	15.317747
26.065071	1054.348993	15.322765
25.924072	1051.763921	15.327783
26.169735	1072.509471	15.332800
26.286802	1075.473065	15.337818
25.918166	1081.163038	15.342835
26.414844	1079.569495	15.347853
26.058592	1085.940466	15.352871
25.690044	1086.080422	15.357888
25.990044	1082.832290	15.362906
25.920316	1081.600839	15.367923
26.075700	1082.930583	15.372941
26.208225	1089.888667	15.377959
26.125411	1084.575702	15.382976
26.167911	1085.122775	15.387994
26.062447	1094.045031	15.393011
26.478666	1101.512000	15.398029
26.806053	1101.081028	15.403047
26.554003	1097.163315	15.408064
27.137044	1074.698744	15.413082
26.827141	1079.379757	15.418099
26.845407	1073.290355	15.423117
26.904752	1071.905269	15.428135
26.722476	1083.404257	15.433152
26.848154	1075.872714	15.438170
26.632969	1071.565983	15.443187
26.442368	1069.540632	15.448205
26.958728	1083.075894	15.453223
26.443287	1081.675569	15.458240
26.973676	1082.242936	15.463258
26.681030	1079.585428	15.468275
26.621492	1073.116031	15.473293
26.819340	1069.719262	15.478311
27.127053	1085.709368	15.483328
27.129876	1074.965981	15.488346
26.713056	1074.921680	15.493363
26.700158	1080.985731	15.498381
26.923657	1076.341561	15.503399
26.793493	1078.058870	15.508416
27.112251	1075.400873	15.513434
26.357647	1078.382020	15.518451
26.740986	1082.750460	15.523469
26.830087	1084.733348	15.528487
26.876162	1081.458669	15.533504
26.945651	1081.597542	15.538522
26.934071	1082.157825	15.543539
27.148239	1098.026177	15.548557
27.376637	1102.535763	15.553575
26.990151	1097.653233	15.558592
27.480698	1102.165514	15.563610
27.143202	1100.198418	15.568627
27.085223	1110.492957	15.573645
27.227118	1100.384812	15.578663
27.133210	1105.504817	15.583680
27.411715	1108.051734	15.588698
27.376394	1112.704577	15.593715
27.432113	1110.436974	15.598733
27.641129	1107.654864	15.603751
27.236698	1107.008000	15.608768
27.368642	1103.689458	15.613786
27.569195	1102.572307	15.618803
27.717509	1104.734822	15.623821
27.700852	1103.104872	15.628839
27.613790	1100.401874	15.633856
27.542130	1100.503921	15.638874
27.383821	1103.104469	15.643891
27.473989	1103.470523	15.648909
27.264846	1102.760254	15.653927
27.387830	1096.759983	15.658944
27.577610	1101.764808	15.663962
27.320185	1106.308475	15.668979
27.051597	1104.176797	15.673997
27.946336	1122.679870	15.679015
27.822977	1122.054506	15.684032
27.786188	1105.661566	15.689050
27.460252	1119.968879	15.694067
27.759898	1133.201946	15.699085
28.113542	1132.519602	15.704103
27.670994	1147.225308	15.709120
27.904729	1137.275028	15.714138
27.939987	1135.087313	15.719155
28.470491	1141.225948	15.724173
28.181568	1126.547601	15.729191
27.815312	1114.279947	15.734208
27.782577	1112.464943	15.739226
27.770908	1129.100054	15.744243
27.881689	1137.764377	15.749261
28.073855	1136.604169	15.754279
28.301697	1139.407434	15.759296
28.120645	1141.399637	15.764314
28.479690	1139.230822	15.769331
28.270627	1135.527793	15.774349
28.497002	1135.772850	15.779367
28.577483	1137.747773	15.784384
28.395376	1135.600476	15.789402
28.060327	1135.979982	15.794419
28.221788	1138.307190	15.799437
28.516078	1139.572570	15.804455
28.287955	1131.596111	15.809472
28.238681	1128.699608	15.814490
28.654582	1129.644114	15.819507
28.111515	1132.478364	15.824525
28.710831	1131.266461	15.829543
28.338618	1132.485866	15.834560
28.540083	1129.032161	15.839578
28.660721	1133.281865	15.844595
28.270837	1127.485666	15.849613
28.884991	1121.326364	15.854631
28.627846	1126.080635	15.859648
28.594629	1130.414594	15.864666
28.534991	1126.007158	15.869683
28.431844	1132.372943	15.874701
28.538962	1130.649716	15.879719
28.679872	1138.611971	15.884736
28.908352	1127.381399	15.889754
28.518912	1130.793291	15.894771
28.951306	1146.596322	15.899789
29.021522	1150.417241	15.904807
29.360110	1150.237122	15.909824
28.863298	1137.176418	15.914842
28.827363	1130.009592	15.919859
28.830802	1135.546807	15.924877
28.707639	1148.331474	15.929895
29.019005	1161.343247	15.934912
29.290058	1152.231899	15.939930
29.360261	1151.610751	15.944947
29.057281	1153.128547	15.949965
29.102593	1143.039690	15.954983
29.144624	1146.848510	15.960000
29.175111	1149.977762	15.965018
29.537983	1145.519534	15.970035
29.138255	1150.172264	15.975053
29.434601	1146.412502	15.980071
29.300494	1137.843893	15.985088
29.334083	1143.285778	15.990106
29.511087	1137.684922	15.995123
29.321008	1144.108140	16.000141
29.433049	1131.418677	16.005159
29.460956	1127.938426	16.010176
29.384396	1127.491666	16.015194
29.808135	1130.590894	16.020211
29.477942	1120.421540	16.025229
29.520558	1116.011536	16.030247
29.230806	1117.251450	16.035264
29.479476	1132.491829	16.040282
29.846813	1140.395577	16.045299
29.845544	1150.835943	16.050317
30.107994	1131.491451	16.055335
29.876253	1121.342227	16.060352
29.797536	1122.570764	16.065370
29.756913	1120.592532	16.070387
29.661174	1128.803246	16.075405
29.818125	1119.795738	16.080423
29.676846	1116.992183	16.085440
29.811240	1119.209847	16.090458
29.896252	1113.683044	16.095475
29.309260	1131.740124	16.100493
29.749584	1142.226041	16.105511
30.080173	1144.603393	16.110528
30.124686	1150.389890	16.115546
29.621292	1153.355147	16.120563
29.521770	1151.041314	16.125581
29.609068	1149.701039	16.130599
29.755808	1153.295830	16.135616
29.883626	1150.175245	16.140634
30.201677	1158.480395	16.145651
29.961206	1167.932966	16.150669
30.423329	1168.663628	16.155687
30.765757	1170.320001	16.160704
29.954869	1159.094761	16.165722
29.898338	1156.354234	16.170739
30.055396	1177.150157	16.175757
30.732487	1179.884279	16.180775
30.706555	1177.643659	16.185792
30.682768	1177.252420	16.190810
30.512608	1158.912847	16.195827
30.513909	1158.765359	16.200845
30.259411	1149.303535	16.205863
30.774626	1156.302343	16.210880
30.068226	1155.079250	16.215898
30.431402	1161.001681	16.220915
30.692318	1175.543099	16.225933
30.842454	1180.051164	16.230951
30.849758	1165.068823	16.235968
30.254753	1163.702211	16.240986
30.665649	1162.672623	16.246003
30.946676	1178.302805	16.251021
30.987096	1176.264605	16.256039
30.935739	1159.309495	16.261056
30.349759	1159.250492	16.266074
30.807514	1163.412874	16.271091
30.786636	1179.016861	16.276109
30.961712	1180.484194	16.281127
31.124394	1179.373137	16.286144
30.379290	1167.612949	16.291162
30.636196	1170.695511	16.296179
30.688358	1183.065076	16.301197
30.900430	1180.439528	16.306215
30.900386	1175.314718	16.311232
30.754309	1182.967905	16.316250
30.836927	1175.011774	16.321267
30.824770	1181.866349	16.326285
31.112052	1174.310989	16.331303
31.257418	1181.902789	16.336320
31.109720	1192.010386	16.341338
31.341885	1193.052152	16.346355
31.572621	1194.346151	16.351373
31.787343	1179.738107	16.356391
31.313393	1164.544161	16.361408
31.592255	1173.891945	16.366426
31.507488	1164.202965	16.371443
31.173444	1170.700881	16.376461
31.000343	1165.742370	16.381479
31.590683	1171.770750	16.386496
31.491189	1174.193103	16.391514
31.246683	1169.992166	16.396531
31.507912	1178.322425	16.401549
31.510622	1200.585900	16.406567
31.708331	1195.815004	16.411584
31.301631	1197.635256	16.416602
31.849638	1200.540738	16.421619
31.891778	1199.404673	16.426637
31.841727	1190.351114	16.431655
31.961158	1194.520720	16.436672
31.856924	1196.155244	16.441690
32.003740	1182.423869	16.446707
31.556138	1174.168064	16.451725
31.788486	1183.223019	16.456743
32.107087	1186.874972	16.461760
31.990974	1189.930541	16.466778
31.832949	1192.731464	16.471795
31.811466	1201.281874	16.476813
31.919444	1195.389659	16.481831
32.038191	1198.364014	16.486848
32.029303	1205.366082	16.491866
32.260089	1189.689836	16.496883
32.266226	1190.821540	16.501901
31.889156	1199.708134	16.506919
32.273512	1191.716010	16.511936
32.269396	1202.007281	16.516954
32.155004	1193.848285	16.521971
32.447723	1188.579568	16.526989
32.288962	1202.695289	16.532007
32.390992	1195.614235	16.537024
32.109345	1198.592666	16.542042
32.184815	1196.367337	16.547059
32.332971	1202.282946	16.552077
32.217977	1202.368012	16.557095
32.499019	1202.358796	16.562112
32.317339	1203.382533	16.567130
32.654290	1200.910781	16.572147
32.628606	1193.193700	16.577165
32.687316	1197.873363	16.582183
32.646368	1208.181977	16.587200
32.690990	1203.283771	16.592218
32.467554	1203.497673	16.597235
32.268312	1201.166282	16.602253
32.250354	1200.550798	16.607271
32.570836	1202.309764	16.612288
32.306613	1210.128114	16.617306
32.567620	1221.029111	16.622323
32.586299	1225.792818	16.627341
32.572004	1228.552568	16.632359
32.727148	1221.331677	16.637376
32.817899	1234.527018	16.642394
32.980042	1226.583213	16.647411
33.130692	1226.488864	16.652429
32.461238	1225.378337	16.657447
33.136434	1227.173741	16.662464
33.258258	1227.719425	16.667482
33.163114	1229.925275	16.672499
33.132072	1231.281878	16.677517
32.787137	1228.135630	16.682535
33.205696	1239.096249	16.687552
33.222487	1247.995269	16.692570
33.170923	1247.928897	16.697587
33.458908	1241.546709	16.702605
33.023789	1251.670550	16.707623
33.551651	1244.621591	16.712640
33.413833	1252.508455	16.717658
33.301381	1246.190984	16.722675
33.566123	1246.653498	16.727693
33.707869	1244.749504	16.732711
33.512181	1251.374925	16.737728
33.392762	1248.280960	16.742746
33.813330	1246.317743	16.747763
33.872184	1248.229059	16.752781
33.432925	1252.510219	16.757799
33.606120	1242.486386	16.762816
33.901803	1245.800523	16.767834
33.551475	1249.229752	16.772851
34.054491	1240.299467	16.777869
33.868619	1246.397569	16.782887
33.900536	1243.217024	16.787904
33.756908	1250.980069	16.792922
33.995599	1246.921876	16.797939
34.215040	1245.570748	16.802957
33.609559	1234.872486	16.807975
33.950052	1242.659619	16.812992
33.658889	1252.719801	16.818010
34.170382	1248.160072	16.823027
34.274318	1246.479901	16.828045
34.008567	1252.465706	16.833063
33.947979	1245.988937	16.838080
34.071320	1249.974802	16.843098
34.409493	1245.018771	16.848115
33.994882	1248.294047	16.853133
33.701179	1255.508762	16.858151
33.955446	1250.803356	16.863168
34.002962	1245.983780	16.868186
34.134062	1254.791153	16.873203
34.187977	1247.928972	16.878221
33.885356	1256.220109	16.883239
34.538602	1277.254349	16.888256
34.090942	1279.279286	16.893274
34.353596	1278.762156	16.898291
34.095336	1274.991144	16.903309
34.650607	1285.714559	16.908327
34.541231	1275.372981	16.913344
34.590887	1277.194532	16.918362
34.299546	1281.783831	16.923379
34.553226	1284.345271	16.928397
34.451693	1275.190243	16.933415
34.874326	1272.333286	16.938432
34.534015	1273.333828	16.943450
34.323584	1280.618931	16.948467
34.854579	1284.131334	16.953485
35.487110	1298.301253	16.958503
35.192661	1277.631861	16.963520
35.208118	1273.569018	16.968538
35.066089	1263.924048	16.973555
35.159519	1262.543338	16.978573
34.899868	1275.542471	16.983591
35.073570	1265.709891	16.988608
35.107599	1266.662001	16.993626
34.895487	1270.753420	16.998643
35.289776	1257.605193	17.003661
34.747868	1266.620882	17.008679
34.836111	1271.823107	17.013696
35.544723	1279.746374	17.018714
35.653409	1280.435663	17.023731
35.878046	1271.215265	17.028749
35.215793	1265.553515	17.033767
35.674061	1259.715006	17.038784
35.467374	1258.455444	17.043802
35.127956	1260.013358	17.048819
35.178808	1253.965940	17.053837
35.085332	1268.626479	17.058855
35.421896	1271.850141	17.063872
35.608241	1276.972945	17.068890
35.600908	1284.168105	17.073907
35.948887	1286.036549	17.078925
35.469993	1284.690573	17.083943
36.034434	1284.396134	17.088960
36.115883	1287.461159	17.093978
35.716439	1275.719978	17.098995
35.649067	1261.349216	17.104013
35.515729	1266.908748	17.109031
35.581823	1289.412291	17.114048
35.913388	1288.097059	17.119066
35.783314	1293.811959	17.124083
36.269690	1275.672703	17.129101
35.780215	1283.025729	17.134119
35.743474	1287.278047	17.139136
36.155936	1282.622286	17.144154
35.543515	1289.761336	17.149171
35.652354	1283.205498	17.154189
35.874476	1290.227451	17.159207
35.795516	1294.371251	17.164224
36.015493	1303.687868	17.169242
36.120238	1312.580114	17.174259
36.715080	1316.596583	17.179277
36.758612	1321.002878	17.184295
36.768413	1318.176927	17.189312
36.607741	1288.958256	17.194330
36.448560	1296.692886	17.199347
36.092760	1277.481775	17.204365
36.097105	1286.111275	17.209383
36.301264	1301.861463	17.214400
36.958830	1307.437389	17.219418
37.027346	1313.521432	17.224435
36.497527	1298.791696	17.229453
36.246842	1296.608886	17.234471
36.285992	1306.699091	17.239488
36.517399	1308.899755	17.244506
36.658085	1317.531490	17.249523
36.638321	1317.101760	17.254541
36.605120	1325.553451	17.259559
36.602793	1325.801499	17.264576
36.744510	1315.018777	17.269594
36.703865	1315.304500	17.274611
36.532664	1310.964568	17.279629
36.619491	1328.834293	17.284647
36.887339	1337.350528	17.289664
37.053791	1334.041376	17.294682
36.987537	1344.754454	17.299699
37.473858	1338.181516	17.304717
37.671554	1337.266430	17.309735
37.319948	1338.475623	17.314752
37.391105	1338.006680	17.319770
37.576418	1335.132522	17.324787
37.475490	1321.868735	17.329805
37.442497	1310.560017	17.334823
37.007601	1306.303096	17.339840
37.367915	1311.165749	17.344858
37.129420	1327.811612	17.349875
37.678093	1330.056318	17.354893
37.659461	1334.605570	17.359911
37.525067	1329.330500	17.364928
37.655970	1331.107810	17.369946
37.762381	1334.608368	17.374963
37.640046	1310.743004	17.379981
37.679504	1314.946434	17.384999
37.527382	1317.403818	17.390016
38.081750	1333.338110	17.395034
37.635341	1320.381611	17.400051
37.826224	1317.037957	17.405069
37.849783	1321.420508	17.410087
37.818830	1329.654868	17.415104
37.988463	1327.265332	17.420122
37.695169	1334.806027	17.425139
37.659971	1327.155476	17.430157
37.747714	1331.843589	17.435175
37.828363	1332.613678	17.440192
38.066343	1333.467827	17.445210
38.084798	1337.294910	17.450227
38.127529	1338.453030	17.455245
37.969946	1343.126510	17.460263
37.879610	1338.043901	17.465280
38.063045	1332.276504	17.470298
37.881929	1336.262224	17.475315
38.229193	1351.974147	17.480333
38.450482	1366.322520	17.485351
38.192574	1364.240160	17.490368
37.909362	1363.198451	17.495386
37.742581	1371.607710	17.500403
38.250833	1369.745990	17.505421
38.515577	1360.652534	17.510439
38.218123	1365.567738	17.515456
38.481493	1360.469364	17.520474
38.374289	1379.349667	17.525491
38.552690	1386.950078	17.530509
38.663500	1383.147654	17.535527
38.507537	1380.903706	17.540544
38.647443	1374.780338	17.545562
38.620018	1377.987288	17.550579
38.813995	1373.463063	17.555597
38.845869	1382.464702	17.560615
38.727966	1381.849416	17.565632
38.821386	1377.935004	17.570650
38.940059	1378.479659	17.575667
38.600038	1381.259846	17.580685
39.156691	1396.925677	17.585703
38.801280	1407.083200	17.590720
39.476092	1399.934956	17.595738
39.205660	1406.624836	17.600755
39.686639	1402.734924	17.605773
39.652899	1401.163782	17.610791
39.513042	1383.121926	17.615808
39.142873	1375.789043	17.620826
39.167721	1381.407329	17.625843
38.974825	1378.374759	17.630861
39.344231	1391.145651	17.635879
39.308396	1402.950898	17.640896
39.257071	1402.838417	17.645914
39.451699	1412.951644	17.650931
39.568315	1406.729885	17.655949
39.766292	1403.799995	17.660967
39.464886	1409.278934	17.665984
39.808285	1400.247173	17.671002
39.481142	1403.598437	17.676019
39.658000	1405.886429	17.681037
40.119175	1392.472661	17.686055
40.214561	1392.596073	17.691072
40.248857	1385.812793	17.696090
40.595635	1392.066108	17.701107
39.838974	1375.755357	17.706125
40.187069	1368.854498	17.711143
40.034380	1373.123569	17.716160
40.370430	1358.331550	17.721178
40.164616	1356.060322	17.726195
39.833473	1367.062947	17.731213
39.828509	1359.511143	17.736231
39.793083	1378.665779	17.741248
40.236929	1386.089564	17.746266
40.404214	1386.942843	17.751283
40.514974	1389.595347	17.756301
41.167787	1390.603198	17.761319
40.538833	1384.189956	17.766336
40.481532	1360.614180	17.771354
40.352880	1370.544990	17.776371
40.353963	1365.626242	17.781389
40.790373	1367.103517	17.786407
40.458266	1370.957245	17.791424
40.745578	1372.309282	17.796442
40.367337	1378.477429	17.801459
40.476388	1390.413746	17.806477
40.615171	1395.239991	17.811495
40.723915	1393.294782	17.816512
40.726339	1395.270915	17.821530
40.963973	1400.799571	17.826547
40.548024	1395.557002	17.831565
41.025334	1403.927115	17.836583
40.773329	1396.401505	17.841600
40.806781	1394.086099	17.846618
40.664806	1397.742260	17.851635
40.533865	1390.737678	17.856653
40.735118	1393.684144	17.861671
40.891242	1412.086229	17.866688
41.070564	1422.439904	17.871706
41.153033	1423.643191	17.876723
41.024526	1424.427096	17.881741
41.282280	1418.281143	17.886759
41.136501	1423.556223	17.891776
41.118402	1419.327425	17.896794
41.586847	1420.727553	17.901811
41.302281	1420.453467	17.906829
41.392901	1422.697973	17.911847
41.178714	1424.501779	17.916864
41.271030	1415.887109	17.921882
41.435042	1419.151017	17.926899
41.528417	1432.523652	17.931917
41.738042	1442.872145	17.936935
41.806198	1456.837763	17.941952
41.627209	1447.074201	17.946970
41.884351	1448.869255	17.951987
41.940002	1446.074006	17.957005
41.881711	1438.662421	17.962023
42.005739	1448.630281	17.967040
42.034095	1437.139677	17.972058
41.807945	1435.388508	17.977075
41.863106	1452.464516	17.982093
42.237829	1439.337604	17.987111
42.174197	1449.900684	17.992128
42.132464	1437.804715	17.997146
42.230100	1441.852128	18.002163
41.923576	1448.385601	18.007181
42.054159	1445.871627	18.012199
41.781253	1449.289987	18.017216
41.923422	1446.755127	18.022234
42.071204	1443.686578	18.027251
41.964906	1446.525532	18.032269
42.298026	1456.263041	18.037287
42.142942	1475.635574	18.042304
42.407772	1479.811828	18.047322
42.809935	1471.337329	18.052339
42.702071	1481.969044	18.057357
42.528875	1474.903553	18.062375
42.558967	1471.941011	18.067392
42.598870	1467.501843	18.072410
42.763441	1467.688992	18.077427
42.639037	1472.137509	18.082445
42.626385	1467.945170	18.087463
42.725883	1472.041489	18.092480
42.648342	1474.028980	18.097498
42.952481	1468.381009	18.102515
42.889419	1470.429015	18.107533
42.776732	1461.906559	18.112551
42.955346	1476.841935	18.117568
43.280304	1485.560291	18.122586
43.421530	1493.382502	18.127603
43.574161	1501.779198	18.132621
43.486882	1481.219699	18.137639
43.606236	1471.491987	18.142656
43.296580	1462.681223	18.147674
43.454787	1458.166257	18.152691
43.171361	1460.941479	18.157709
43.326785	1463.830061	18.162727
43.465356	1456.547330	18.167744
43.122261	1464.290738	18.172762
43.686081	1475.496331	18.177779
43.330281	1491.648651	18.182797
43.739443	1486.283486	18.187815
43.822145	1496.701025	18.192832
44.003553	1485.725142	18.197850
44.093053	1478.829591	18.202867
43.775337	1459.913327	18.207885
43.612176	1454.538806	18.212903
43.700527	1464.686432	18.217920
44.081077	1480.037626	18.222938
44.036909	1483.424650	18.227955
44.074394	1493.489274	18.232973
44.200750	1479.847769	18.237991
44.233425	1462.451503	18.243008
44.006274	1459.024358	18.248026
44.188749	1462.373308	18.253043
44.251516	1475.259054	18.258061
44.420418	1470.800524	18.263079
44.111940	1467.216831	18.268096
43.997745	1482.018931	18.273114
44.525430	1478.159974	18.278131
44.572337	1491.483534	18.283149
44.579970	1489.712357	18.288167
44.349574	1491.202778	18.293184
44.246578	1487.442498	18.298202
44.333867	1489.316289	18.303219
44.215855	1490.773267	18.308237
44.321048	1490.706004	18.313255
44.148226	1491.041953	18.318272
44.364703	1495.158384	18.323290
44.617000	1504.620776	18.328307
44.689309	1507.512593	18.333325
44.654036	1509.855475	18.338343
44.949555	1509.942213	18.343360
44.721780	1510.966392	18.348378
45.417246	1504.122464	18.353395
45.315136	1504.757738	18.358413
45.239879	1514.442060	18.363431
45.272008	1505.204526	18.368448
45.139390	1517.313883	18.373466
45.219712	1506.789218	18.378483
44.912655	1511.890777	18.383501
45.431592	1513.320450	18.388519
45.082303	1508.442828	18.393536
45.004352	1505.312565	18.398554
45.182701	1502.161591	18.403571
45.072233	1510.360068	18.408589
45.299079	1500.999379	18.413607
45.412280	1521.000447	18.418624
45.250145	1533.197562	18.423642
45.759746	1528.688478	18.428659
45.490811	1537.558691	18.433677
45.590079	1526.384637	18.438695
45.581148	1529.942419	18.443712
45.693047	1529.918893	18.448730
45.856321	1529.205781	18.453747
45.781959	1530.200902	18.458765
45.506514	1534.587529	18.463783
46.034971	1535.623406	18.468800
45.679512	1533.079747	18.473818
46.020987	1531.445836	18.478835
45.655394	1537.242548	18.483853
45.812055	1542.405178	18.488871
46.429376	1550.991547	18.493888
46.343591	1559.409463	18.498906
46.482605	1551.778939	18.503923
46.428476	1563.563032	18.508941
46.456372	1556.913072	18.513959
46.118510	1545.559986	18.518976
46.300430	1554.535212	18.523994
46.564241	1559.627897	18.529011
46.432117	1561.103837	18.534029
46.359204	1560.541073	18.539047
46.979722	1557.910402	18.544064
46.838717	1559.770187	18.549082
47.204041	1556.436736	18.554099
47.154009	1549.261109	18.559117
46.384530	1536.702373	18.564135
46.481620	1532.016743	18.569152
46.287950	1552.461054	18.574170
46.533240	1557.878994	18.579187
46.563656	1562.395885	18.584205
46.599475	1563.508352	18.589223
46.675532	1554.028194	18.594240
46.825380	1583.541747	18.599258
47.168675	1581.705136	18.604275
47.194273	1590.014985	18.609293
47.209421	1588.333857	18.614311
47.518123	1595.552938	18.619328
47.335908	1598.319493	18.624346
47.425079	1584.909493	18.629363
47.394688	1590.058928	18.634381
47.269492	1588.369575	18.639399
47.459178	1587.174324	18.644416
47.277697	1591.060160	18.649434
47.393477	1581.331418	18.654451
47.564647	1589.700176	18.659469
47.601597	1589.736749	18.664487
47.739947	1586.939502	18.669504
47.520436	1591.059047	18.674522
48.088292	1589.159523	18.679539
47.770727	1589.449416	18.684557
47.581755	1587.469391	18.689575
47.295388	1590.546352	18.694592
47.689346	1611.738506	18.699610
47.881441	1614.227481	18.704627
47.992414	1617.840325	18.709645
48.052911	1622.689513	18.714663
47.873317	1620.209004	18.719680
47.642550	1621.616420	18.724698
47.944295	1617.060262	18.729715
48.098062	1625.335163	18.734733
47.779331	1627.074230	18.739751
48.394267	1637.691982	18.744768
48.660662	1636.961185	18.749786
48.772683	1631.972934	18.754803
48.959056	1632.611121	18.759821
48.718051	1628.805170	18.764839
48.697095	1611.688434	18.769856
48.267499	1609.240158	18.774874
48.780603	1618.567345	18.779891
49.144216	1624.208748	18.784909
48.654672	1616.942284	18.789927
49.028941	1613.453728	18.794944
48.590627	1613.372157	18.799962
48.901325	1625.860364	18.804979
49.026542	1627.658371	18.809997
49.027976	1637.192204	18.815015
48.990862	1636.904037	18.820032
49.250375	1639.907104	18.825050
49.123906	1636.318548	18.830067
49.113079	1642.111566	18.835085
48.753738	1635.875245	18.840103
49.208416	1638.720822	18.845120
49.189690	1637.990480	18.850138
49.120033	1634.085457	18.855155
49.490763	1639.147238	18.860173
49.067461	1644.058511	18.865191
49.403345	1634.325861	18.870208
49.425411	1640.018740	18.875226
49.937643	1637.918882	18.880243
49.949835	1638.485740	18.885261
49.441595	1646.153603	18.890279
49.804317	1642.944609	18.895296
49.593197	1645.186938	18.900314
49.707946	1649.138154	18.905331
50.102488	1659.251129	18.910349
50.413988	1670.209148	18.915367
50.371457	1648.158524	18.920384
49.824364	1640.406981	18.925402
49.969903	1632.139404	18.930419
49.856215	1630.545327	18.935437
50.055732	1646.660479	18.940455
49.957993	1647.046163	18.945472
50.062296	1659.172103	18.950490
50.247967	1657.688921	18.955507
50.054105	1665.663956	18.960525
49.976602	1658.981230	18.965543
50.194392	1653.467303	18.970560
50.173055	1662.432946	18.975578
50.309565	1669.759151	18.980595
50.973787	1675.855783	18.985613
50.624572	1690.616081	18.990631
50.951837	1678.007793	18.995648
50.942298	1680.256515	19.000666
50.810767	1673.175521	19.005683
50.860711	1657.352234	19.010701
50.650610	1661.556414	19.015719
50.796984	1670.197213	19.020736
50.748902	1684.613719	19.025754
51.080659	1687.835538	19.030771
50.943073	1677.496166	19.035789
50.948181	1685.607982	19.040807
50.829811	1680.905700	19.045824
51.208967	1683.089356	19.050842
51.023422	1686.432152	19.055859
51.208488	1678.534587	19.060877
51.134492	1685.985089	19.065895
51.090223	1680.916126	19.070912
51.324879	1683.964413	19.075930
51.548789	1706.164698	19.080947
52.027146	1698.650352	19.085965
51.723200	1692.004072	19.090983
51.986512	1687.026090	19.096000
51.808405	1676.865731	19.101018
51.588950	1680.892367	19.106035
51.850755	1675.008641	19.111053
51.620849	1681.799970	19.116071
51.595613	1678.179479	19.121088
51.687929	1690.297261	19.126106
51.698834	1703.972882	19.131123
52.003298	1698.814199	19.136141
52.047913	1710.194816	19.141159
52.435112	1703.704870	19.146176
52.157319	1703.342599	19.151194
52.285012	1708.089338	19.156211
52.533182	1694.809481	19.161229
52.215886	1705.839106	19.166247
52.253837	1691.288848	19.171264
52.640597	1690.883909	19.176282
52.109515	1700.628384	19.181299
52.198954	1693.830397	19.186317
52.070148	1693.141368	19.191335
52.270067	1703.869694	19.196352
52.617997	1718.938496	19.201370
53.008441	1724.113473	19.206387
53.170674	1726.900927	19.211405
52.875806	1726.902646	19.216423
52.787367	1727.222164	19.221440
53.352897	1723.453127	19.226458
53.217282	1713.313022	19.231475
53.052942	1696.958260	19.236493
52.877026	1691.765390	19.241511
52.663873	1705.691262	19.246528
53.118891	1720.470809	19.251546
53.249029	1719.919294	19.256563
53.293074	1720.049543	19.261581
53.262781	1725.366348	19.266599
53.167529	1726.125272	19.271616
53.479194	1727.275900	19.276634
53.330030	1730.649086	19.281651
53.493453	1721.751947	19.286669
53.304496	1727.390870	19.291687
53.530037	1723.213143	19.296704
53.624714	1726.972523	19.301722
53.679946	1730.237035	19.306739
53.762983	1721.982095	19.311757
53.788149	1734.774491	19.316775
53.699520	1728.368083	19.321792
53.753854	1727.255484	19.326810
53.710534	1733.499826	19.331827
53.769244	1742.015915	19.336845
53.910700	1743.446936	19.341863
53.719242	1747.454220	19.346880
54.037496	1759.348258	19.351898
53.857965	1754.530047	19.356915
53.907780	1746.555231	19.361933
53.819836	1748.037395	19.366951
54.205605	1767.632164	19.371968
54.379902	1766.810448	19.376986
54.096528	1782.233244	19.382003
54.471175	1772.130435	19.387021
54.239676	1770.807752	19.392039
54.420387	1776.847542	19.397056
54.312388	1771.093332	19.402074
54.518988	1788.281555	19.407091
54.675419	1791.892946	19.412109
54.890578	1805.359995	19.417127
54.759628	1803.453075	19.422144
55.275248	1798.157751	19.427162
55.202032	1791.352172	19.432179
55.587044	1789.780465	19.437197
55.267349	1779.886075	19.442215
55.160792	1772.265259	19.447232
55.376641	1764.283230	19.452250
55.151200	1765.894887	19.457267
55.188282	1769.560203	19.462285
55.190315	1775.636532	19.467303
55.275595	1778.330876	19.472320
55.809940	1781.971578	19.477338
55.329637	1796.064606	19.482355
55.387037	1784.887307	19.487373
55.660922	1787.491831	19.492391
55.104337	1788.673986	19.497408
55.427446	1787.796437	19.502426
55.452671	1787.428280	19.507443
55.766541	1786.519240	19.512461
55.914449	1805.277570	19.517479
55.631789	1814.833049	19.522496
56.365096	1809.069247	19.527514
56.410089	1821.472836	19.532531
56.200666	1814.435451	19.537549
56.008503	1799.102007	19.542567
55.914878	1809.827578	19.547584
56.130457	1819.791792	19.552602
56.102544	1824.372309	19.557619
56.292960	1821.448757	19.562637
56.336246	1825.599695	19.567655
56.085431	1822.611223	19.572672
55.999680	1819.813375	19.577690
56.402092	1822.488793	19.582707
56.453219	1822.092176	19.587725
56.345993	1825.367237	19.592743
56.567483	1843.593250	19.597760
56.837405	1837.218643	19.602778
56.574526	1838.481172	19.607795
57.029653	1842.909972	19.612813
56.688519	1841.899816	19.617831
56.747256	1835.712616	19.622848
57.290234	1830.104287	19.627866
57.119929	1837.766673	19.632883
57.222076	1828.935103	19.637901
57.066463	1836.973360	19.642919
57.250646	1834.568654	19.647936
57.340176	1840.709544	19.652954
57.296444	1837.693440	19.657971
57.266213	1839.407479	19.662989
57.185152	1836.516688	19.668007
57.130481	1864.740875	19.673024
57.385867	1864.450593	19.678042
57.812362	1876.235601	19.683059
57.521315	1864.377738	19.688077
58.326578	1858.326352	19.693095
58.424685	1858.168559	19.698112
58.734009	1843.751183	19.703130
58.250218	1830.913277	19.708147
57.874221	1818.317955	19.713165
57.921724	1817.993621	19.718183
57.671127	1829.018985	19.723200
58.008980	1825.576395	19.728218
58.084536	1843.644730	19.733235
58.101354	1852.508260	19.738253
58.143664	1840.919679	19.743271
58.252997	1856.592974	19.748288
58.326013	1850.452539	19.753306
58.303904	1854.208348	19.758323
58.434502	1849.777540	19.763341
58.554173	1849.150641	19.768359
58.062370	1854.830507	19.773376
58.256823	1862.691029	19.778394
58.769686	1873.705624	19.783411
58.698158	1876.775732	19.788429
58.819314	1884.419275	19.793447
58.600798	1893.705113	19.798464
58.938870	1880.368735	19.803482
58.845157	1879.109045	19.808499
59.010127	1873.614728	19.813517
58.966914	1872.362524	19.818535
58.846135	1886.922405	19.823552
59.243467	1898.581705	19.828570
59.419622	1905.155069	19.833587
59.362171	1904.431353	19.838605
59.795811	1901.891336	19.843623
59.682885	1889.887153	19.848640
59.680933	1872.348711	19.853658
59.744508	1871.586135	19.858675
59.746703	1882.836732	19.863693
60.011394	1871.323402	19.868711
59.712066	1877.745175	19.873728
59.892882	1865.779636	19.878746
60.212016	1864.560990	19.883763
59.820141	1865.175083	19.888781
59.741295	1865.622108	19.893799
59.526037	1875.390899	19.898816
60.047361	1885.069637	19.903834
60.007781	1903.181405	19.908851
60.035849	1901.375966	19.913869
60.275701	1894.019361	19.918887
60.014909	1901.995754	19.923904
60.556810	1899.948657	19.928922
60.510574	1900.724386	19.933939
60.248246	1902.417587	19.938957
60.607583	1902.779644	19.943975
60.704293	1906.335151	19.948992
60.549902	1899.445004	19.954010
60.700770	1898.739516	19.959027
60.169369	1905.421194	19.964045
60.597498	1908.684024	19.969063
60.644250	1928.627313	19.974080
60.691140	1926.362288	19.979098
60.539195	1922.142520	19.984115
60.581596	1926.679511	19.989133
60.799189	1927.543096	19.994151
60.589033	1939.144353	19.999168
60.873123	1945.111753	20.004186
61.192340	1948.551946	20.009203
61.370525	1951.415061	20.014221
61.561214	1946.174217	20.019239
61.210629	1953.094633	20.024256
61.437634	1950.539636	20.029274
61.310115	1953.948140	20.034291
61.174952	1965.112489	20.039309
61.678426	1970.598135	20.044327
61.884232	1977.207396	20.049344
61.858723	1973.041143	20.054362
62.337568	1973.121656	20.059379
61.980512	1976.133636	20.064397
62.420919	1982.162056	20.069415
62.276139	1977.605962	20.074432
62.463494	1974.229699	20.079450
62.493189	1957.205882	20.084467
61.991316	1939.864112	20.089485
62.141435	1946.354544	20.094503
62.263047	1964.789974	20.099520
62.099610	1972.878073	20.104538
62.191743	1972.848092	20.109555
62.205235	1978.461453	20.114573
62.497503	1974.273794	20.119591
62.213527	1975.920313	20.124608
62.501957	1977.867173	20.129626
62.512240	1979.095086	20.134643
62.614206	1993.818872	20.139661
62.854142	1994.312835	20.144679
63.192891	2005.790897	20.149696
63.547681	2003.485278	20.154714
63.312570	1990.717217	20.159731
62.773305	1990.488754	20.164749
63.306231	1988.025809	20.169767
63.415726	1994.212555	20.174784
63.403994	2005.202996	20.179802
63.607461	2002.285836	20.184819
63.454439	1997.781156	20.189837
63.511464	2001.843159	20.194855
63.418954	1994.929761	20.199872
63.460765	1994.303998	20.204890
63.664316	2000.825849	20.209907
63.030469	2005.840661	20.214925
63.644271	1994.668621	20.219943
63.285204	1997.533685	20.224960
63.485244	1999.172038	20.229978
63.830216	2009.830425	20.234995
63.795311	2027.234750	20.240013
64.048372	2019.005235	20.245031
63.919998	2027.532292	20.250048
63.727369	2027.557038	20.255066
64.193585	2022.547707	20.260083
64.097255	2029.395035	20.265101
64.404914	2031.863872	20.270119
64.780696	2047.816130	20.275136
64.503953	2049.021988	20.280154
64.795441	2035.499346	20.285171
64.714299	2035.913300	20.290189
64.952440	2041.682682	20.295207
64.675785	2034.462603	20.300224
64.812280	2047.888223	20.305242
65.133758	2048.871425	20.310259
64.676507	2052.868442	20.315277
64.931956	2044.847587	20.320295
65.011273	2045.106062	20.325312
64.836414	2039.887695	20.330330
65.306352	2044.228964	20.335347
65.062025	2046.377029	20.340365
65.305710	2045.342194	20.345383
65.301310	2039.483104	20.350400
65.016652	2041.837715	20.355418
65.821016	2041.028845	20.360435
65.727714	2041.373221	20.365453
65.903302	2041.163556	20.370471
65.657903	2033.774711	20.375488
65.765192	2043.624940	20.380506
65.952806	2037.312008	20.385523
65.277987	2036.796113	20.390541
65.981550	2054.481002	20.395559
66.114591	2065.170249	20.400576
65.828303	2075.094274	20.405594
66.163727	2071.530379	20.410611
65.958893	2074.101655	20.415629
66.035774	2068.168769	20.420647
66.350864	2059.383249	20.425664
66.589692	2061.565033	20.430682
66.594276	2066.646022	20.435699
66.095185	2064.519470	20.440717
65.991664	2062.172323	20.445735
66.113063	2066.268589	20.450752
65.900852	2085.437862	20.455770
66.659246	2082.225521	20.460787
66.214444	2095.732336	20.465805
66.736227	2095.819271	20.470823
67.022642	2097.323518	20.475840
67.152935	2109.308325	20.480858
67.139664	2099.353715	20.485875
67.604813	2100.119742	20.490893
67.491256	2088.743159	20.495911
67.413918	2085.305151	20.500928
67.247967	2088.906125	20.505946
67.387722	2071.886546	20.510963
67.296778	2088.425625	20.515981
67.395127	2092.692014	20.520999
67.562376	2091.408828	20.526016
67.549838	2092.459535	20.531034
67.717001	2090.669996	20.536051
67.639897	2102.819507	20.541069
67.711425	2111.056397	20.546087
67.870814	2104.464380	20.551104
67.341962	2109.481699	20.556122
67.742150	2113.337633	20.561139
67.620707	2127.302100	20.566157
68.017852	2124.608835	20.571175
68.495999	2119.395432	20.576192
68.148273	2128.658279	20.581210
68.737638	2125.522553	20.586227
68.623586	2124.779786	20.591245
68.639665	2122.329043	20.596263
68.782721	2126.456656	20.601280
68.644912	2126.635018	20.606298
68.922593	2123.520441	20.611315
68.709649	2126.258494	20.616333
68.475114	2124.403156	20.621351
68.367882	2126.401331	20.626368
68.716959	2136.594864	20.631386
68.903163	2145.177517	20.636403
68.901046	2156.904707	20.641421
68.880515	2154.122787	20.646439
69.257522	2153.568309	20.651456
69.154526	2158.074775	20.656474
69.287778	2146.764906	20.661491
69.339940	2158.197713	20.666509
69.339265	2155.623835	20.671527
69.245275	2153.180933	20.676544
69.080620	2167.569438	20.681562
69.495279	2171.187046	20.686579
69.486596	2178.832520	20.691597
69.488620	2189.706148	20.696615
70.052202	2178.771755	20.701632
69.791927	2185.303115	20.706650
70.119440	2185.766713	20.711667
69.919572	2177.298582	20.716685
69.839716	2183.730889	20.721703
70.214707	2178.581222	20.726720
70.653310	2183.870163	20.731738
70.677715	2182.196440	20.736755
70.371193	2179.720276	20.741773
70.341628	2179.785580	20.746791
70.275577	2181.244737	20.751808
70.175634	2202.168778	20.756826
70.377898	2203.639031	20.761843
70.626989	2207.178719	20.766861
70.504086	2212.191048	20.771879
70.886783	2204.296744	20.776896
70.546809	2204.036864	20.781914
70.873392	2226.956614	20.786931
70.886620	2235.203564	20.791949
71.581325	2229.038692	20.796967
71.751284	2231.946977	20.801984
71.378255	2237.765300	20.807002
71.450823	2233.267945	20.812019
71.504658	2238.978434	20.817037
71.108963	2233.224945	20.822055
71.414789	2227.649654	20.827072
71.235148	2228.708938	20.832090
71.478235	2224.446956	20.837107
71.946493	2219.565972	20.842125
71.702255	2222.520067	20.847143
72.339928	2216.998927	20.852160
71.574149	2214.599919	20.857178
71.988920	2230.813042	20.862195
72.434338	2245.551422	20.867213
72.490010	2242.421727	20.872231
72.811054	2234.199346	20.877248
72.567311	2226.199013	20.882266
72.357652	2214.704936	20.887283
72.705593	2206.863840	20.892301
72.822305	2214.561465	20.897319
72.788243	2200.394394	20.902336
72.935147	2198.697305	20.907354
73.001581	2198.073219	20.912371
72.972868	2202.585863	20.917389
72.790129	2204.830098	20.922407
73.051423	2202.640101	20.927424
72.640546	2208.723207	20.932442
72.481016	2212.789711	20.937459
72.932614	2227.733343	20.942477
73.019321	2236.570934	20.947495
73.184482	2232.720793	20.952512
73.301027	2239.396263	20.957530
73.314063	2233.904243	20.962547
73.530687	2235.624043	20.967565
73.448882	2238.311675	20.972583
73.660273	2225.001056	20.977600
73.088588	2234.942217	20.982618
73.373501	2252.768409	20.987635
73.706974	2256.967756	20.992653
73.588892	2265.832598	20.997671
73.886270	2261.584924	21.002688
73.690721	2266.655401	21.007706
73.805766	2273.691039	21.012723
74.408007	2281.688190	21.017741
74.397033	2287.383820	21.022759
74.282586	2281.812837	21.027776
74.407317	2287.246583	21.032794
74.478441	2283.025881	21.037811
74.622244	2284.117130	21.042829
74.571072	2297.466462	21.047847
74.801566	2285.507837	21.052864
74.584259	2292.294118	21.057882
74.326321	2300.056804	21.062899
74.490964	2287.746421	21.067917
74.498834	2309.532568	21.072935
74.930413	2318.784378	21.077952
74.748512	2326.452139	21.082970
74.859273	2325.630657	21.087987
75.187590	2325.209737	21.093005
75.436534	2334.083357	21.098023
75.835624	2333.574701	21.103040
75.615964	2338.821802	21.108058
75.368993	2335.705386	21.113075
76.219787	2348.168518	21.118093
75.607160	2349.020897	21.123111
76.448776	2337.127565	21.128128
76.002792	2330.064351	21.133146
75.659739	2318.830111	21.138163
75.774119	2331.020997	21.143181
76.115473	2342.098800	21.148199
75.863251	2332.270454	21.153216
75.693923	2334.915618	21.158234
76.284821	2334.919043	21.163251
76.356359	2343.783708	21.168269
76.139705	2345.432111	21.173287
76.713476	2369.155489	21.178304
76.616466	2376.064511	21.183322
76.712155	2384.688014	21.188339
76.693073	2374.927562	21.193357
76.406429	2379.942816	21.198375
77.083529	2373.383208	21.203392
77.175802	2365.180291	21.208410
76.945533	2364.815760	21.213427
77.668056	2372.345024	21.218445
77.026639	2378.545684	21.223463
77.413904	2381.608110	21.228480
77.466299	2377.386655	21.233498
77.310558	2373.474155	21.238515
77.501158	2369.988968	21.243533
77.132928	2376.170354	21.248551
77.039407	2374.285296	21.253568
76.937064	2373.969710	21.258586
77.189213	2396.806393	21.263603
77.651096	2392.041428	21.268621
77.685547	2400.976273	21.273639
77.657160	2407.864094	21.278656
77.911974	2419.011915	21.283674
77.741914	2430.735027	21.288691
78.049829	2425.839732	21.293709
77.729188	2430.704113	21.298727
77.825102	2429.103157	21.303744
78.324292	2445.939927	21.308762
78.286646	2461.117290	21.313779
78.697565	2453.217236	21.318797
78.476950	2451.614630	21.323815
78.514391	2453.150966	21.328832
78.695430	2446.935471	21.333850
78.965314	2452.152232	21.338867
79.136251	2447.531635	21.343885
79.252564	2449.145015	21.348903
78.920658	2453.217507	21.353920
79.405385	2456.895623	21.358938
79.344158	2472.404652	21.363955
79.452479	2477.836552	21.368973
79.535436	2472.271822	21.373991
79.386276	2480.705822	21.379008
79.742310	2477.526161	21.384026
79.717645	2478.773099	21.389043
79.927327	2475.398808	21.394061
79.955033	2486.902200	21.399079
79.934123	2472.894859	21.404096
80.248099	2470.302030	21.409114
79.976441	2477.155198	21.414131
79.716584	2463.260496	21.419149
80.062560	2473.087794	21.424167
80.178772	2470.708426	21.429184
79.949296	2473.919133	21.434202
80.382297	2490.924018	21.439219
80.314322	2485.407210	21.444237
80.429084	2488.732159	21.449255
80.709233	2488.605366	21.454272
80.698365	2488.081150	21.459290
80.660011	2495.721233	21.464307
81.081408	2499.059767	21.469325
81.230684	2490.271329	21.474343
81.241484	2491.037308	21.479360
80.974610	2487.451756	21.484378
81.010307	2502.792205	21.489395
81.091592	2494.020934	21.494413
81.209820	2500.707253	21.499431
81.380292	2516.564067	21.504448
81.566667	2520.126392	21.509466
81.136262	2524.834001	21.514483
80.961154	2519.327672	21.519501
81.390043	2521.521433	21.524519
81.233642	2532.633518	21.529536
81.331658	2539.330407	21.534554
81.400215	2549.526627	21.539571
81.822054	2549.966191	21.544589
81.845031	2555.560807	21.549607
82.230841	2570.093142	21.554624
82.601337	2567.969428	21.559642
82.419124	2568.762201	21.564659
82.989571	2568.218649	21.569677
82.930847	2561.438600	21.574695
83.081555	2572.167299	21.579712
82.791966	2551.652889	21.584730
82.580546	2552.055328	21.589747
82.887829	2558.653345	21.594765
82.856278	2570.015751	21.599783
82.620876	2566.893367	21.604800
83.300127	2570.824824	21.609818
82.960563	2574.370225	21.614835
83.232537	2569.096731	21.619853
83.254118	2570.747627	21.624871
83.135691	2570.560012	21.629888
83.627433	2585.950725	21.634906
83.868640	2595.725972	21.639923
83.524122	2590.193535	21.644941
83.684367	2595.721317	21.649959
83.416809	2597.312319	21.654976
83.572368	2591.762663	21.659994
83.450866	2599.422565	21.665011
83.765584	2604.963243	21.670029
84.216184	2622.103860	21.675047
84.150472	2630.375577	21.680064
84.809552	2632.032954	21.685082
84.440345	2629.466659	21.690099
84.531541	2621.944224	21.695117
84.419050	2615.631716	21.700135
84.618348	2622.577463	21.705152
84.709842	2614.924250	21.710170
84.582234	2621.630717	21.715187
84.338312	2615.468322	21.720205
84.712011	2623.486719	21.725223
84.722103	2643.821522	21.730240
84.744640	2641.154199	21.735258
84.965920	2654.019254	21.740275
85.090898	2643.465301	21.745293
85.115823	2654.719644	21.750311
85.399308	2669.639757	21.755328
86.022222	2669.977125	21.760346
85.694473	2676.021743	21.765363
85.867039	2669.899755	21.770381
85.845106	2672.427564	21.775399
85.991529	2669.882329	21.780416
86.188688	2667.316584	21.785434
86.028406	2667.401543	21.790451
86.077401	2665.465241	21.795469
85.832175	2664.466148	21.800487
85.903732	2676.177158	21.805504
86.395534	2663.108697	21.810522
85.832308	2673.561368	21.815539
85.888572	2675.917477	21.820557
86.431691	2692.880864	21.825575
86.447660	2693.151392	21.830592
86.730854	2683.323175	21.835610
86.790726	2695.519752	21.840627
87.014242	2688.417985	21.845645
86.975143	2692.082009	21.850663
86.500685	2693.996731	21.855680
86.799301	2702.258790	21.860698
86.917431	2708.779044	21.865715
86.967828	2719.706963	21.870733
87.130544	2713.204689	21.875751
87.697149	2735.727280	21.880768
88.000618	2738.233177	21.885786
88.198832	2733.754302	21.890803
88.236789	2730.366872	21.895821
88.290671	2711.459017	21.900839
87.896349	2714.086902	21.905856
88.148076	2705.062631	21.910874
87.978716	2716.348751	21.915891
87.887719	2728.806694	21.920909
88.047546	2728.595786	21.925927
88.192333	2741.607909	21.930944
88.291227	2732.949255	21.935962
88.261216	2736.555028	21.940979
88.352977	2747.313640	21.945997
88.732913	2750.041117	21.951015
88.545766	2773.606535	21.956032
88.996828	2766.150706	21.961050
88.988485	2769.454293	21.966067
89.096967	2778.158511	21.971085
88.988506	2775.301775	21.976103
89.010368	2772.382533	21.981120
89.379543	2768.775288	21.986138
89.825465	2768.792547	21.991155
89.531532	2762.813502	21.996173
89.980811	2776.558632	22.001191
89.454993	2769.220662	22.006208
89.531530	2785.508100	22.011226
89.869940	2789.291712	22.016243
89.563814	2792.858205	22.021261
90.055079	2795.288600	22.026279
89.765969	2794.438780	22.031296
90.270263	2783.826003	22.036314
90.156772	2791.139680	22.041331
89.856492	2797.009525	22.046349
90.220806	2800.450841	22.051367
90.336527	2817.323828	22.056384
90.438560	2811.563547	22.061402
90.355639	2815.929727	22.066419
90.375082	2822.736288	22.071437
90.372874	2824.078634	22.076455
90.385631	2845.159833	22.081472
90.711690	2838.638954	22.086490
90.932575	2842.229302	22.091507
91.006036	2846.915201	22.096525
91.588798	2857.414089	22.101543
91.423958	2878.748656	22.106560
91.575178	2875.000768	22.111578
91.689691	2876.801937	22.116595
91.555045	2875.030189	22.121613
91.928167	2868.639838	22.126631
91.924334	2879.778777	22.131648
92.439397	2871.036099	22.136666
92.457021	2869.437495	22.141683
92.441195	2871.002693	22.146701
92.455741	2861.310202	22.151719
92.245090	2872.646828	22.156736
92.485699	2873.461633	22.161754
92.417879	2868.658970	22.166771
92.503152	2870.437587	22.171789
92.755691	2873.267256	22.176807
92.689000	2873.450365	22.181824
92.674469	2870.184522	22.186842
92.734951	2871.255446	22.191859
92.882392	2885.035093	22.196877
93.215297	2889.515865	22.201895
93.139829	2894.069013	22.206912
92.997004	2892.886964	22.211930
93.195224	2895.423531	22.216947
92.839121	2904.863496	22.221965
93.387701	2904.978139	22.226983
93.478693	2923.604627	22.232000
93.450941	2927.932241	22.237018
93.595571	2929.388818	22.242035
93.270082	2936.451451	22.247053
93.651335	2946.130453	22.252071
93.570109	2957.492204	22.257088
93.847117	2946.849767	22.262106
94.164790	2940.609078	22.267123
94.043049	2954.041158	22.272141
94.552700	2965.307916	22.277159
94.826091	2980.559254	22.282176
94.735072	2973.591613	22.287194
95.106508	2972.637990	22.292211
94.983558	2981.203223	22.297229
95.404035	2964.624803	22.302247
95.309735	2969.644282	22.307264
95.599898	2966.181273	22.312282
95.656529	2959.377338	22.317299
95.327975	2948.753661	22.322317
95.488068	2936.352195	22.327335
95.438030	2945.106522	22.332352
96.078722	2943.438108	22.337370
95.996312	2934.270165	22.342387
95.389830	2938.140199	22.347405
95.626032	2949.146681	22.352423
95.700880	2962.258396	22.357440
95.695150	2958.093216	22.362458
95.841296	2961.720818	22.367475
95.536399	2957.030439	22.372493
95.786434	2976.418852	22.377511
95.682285	2991.258455	22.382528
96.527486	2987.479771	22.387546
96.423643	2980.169378	22.392563
96.309199	3002.634275	22.397581
96.599791	3009.368443	22.402599
96.522279	3018.927676	22.407616
96.360245	3021.014902	22.412634
96.509823	3021.675997	22.417651
96.625531	3039.850267	22.422669
96.824330	3043.111311	22.427687
96.860334	3052.569986	22.432704
97.492460	3060.063895	22.437722
97.863357	3065.356477	22.442739
97.284347	3077.979478	22.447757
97.559917	3078.136203	22.452775
97.886919	3077.543017	22.457792
97.577239	3074.672682	22.462810
97.701961	3056.866662	22.467827
97.797417	3076.387232	22.472845
97.915190	3090.796679	22.477863
98.383622	3093.735075	22.482880
98.501692	3097.490382	22.487898
98.908336	3092.953622	22.492915
98.764284	3100.001761	22.497933
98.831980	3094.292941	22.502951
98.567980	3094.601236	22.507968
98.985185	3087.776383	22.512986
98.829710	3089.170229	22.518003
98.732683	3100.871080	22.523021
99.266042	3108.449675	22.528039
99.481237	3123.229930	22.533056
99.289181	3122.005111	22.538074
99.254754	3132.299697	22.543091
98.923316	3121.570076	22.548109
99.570506	3121.878095	22.553127
99.501233	3125.012638	22.558144
99.697183	3145.990379	22.563162
100.087903	3150.276239	22.568179
100.096344	3153.024948	22.573197
100.445138	3155.458563	22.578215
100.008538	3159.273536	22.583232
100.208278	3157.605878	22.588250
99.921653	3145.949473	22.593267
100.232689	3152.332883	22.598285
100.378583	3154.115316	22.603303
100.547286	3176.512230	22.608320
100.522433	3186.332671	22.613338
100.921211	3177.137223	22.618355
101.222221	3176.709941	22.623373
101.268478	3192.322537	22.628391
101.546827	3180.305414	22.633408
101.266319	3180.106199	22.638426
101.498608	3176.005689	22.643443
101.272040	3182.101671	22.648461
101.185499	3179.188336	22.653479
101.216975	3180.521000	22.658496
101.259568	3200.729666	22.663514
101.135877	3213.281804	22.668531
101.340899	3220.834048	22.673549
101.559520	3228.514702	22.678567
101.812651	3231.107278	22.683584
102.226533	3231.881372	22.688602
102.311318	3243.017189	22.693619
102.088216	3253.745859	22.698637
102.274057	3259.427789	22.703655
102.418216	3263.522830	22.708672
102.521181	3270.396385	22.713690
102.992232	3263.007779	22.718707
102.879283	3264.065934	22.723725
102.952466	3280.024468	22.728743
103.584771	3291.428737	22.733760
103.112529	3295.972840	22.738778
103.483135	3287.693375	22.743795
103.847444	3293.101362	22.748813
103.450364	3300.489882	22.753831
103.491315	3290.976892	22.758848
103.468370	3305.877689	22.763866
103.581774	3289.918622	22.768883
103.571039	3308.645701	22.773901
103.550486	3312.906818	22.778919
103.836434	3311.067639	22.783936
103.762964	3323.749079	22.788954
104.249902	3331.523183	22.793971
104.255704	3344.010696	22.798989
104.109384	3346.833225	22.804007
104.403912	3337.100318	22.809024
104.378433	3358.391953	22.814042
105.118398	3362.957443	22.819059
104.972195	3367.834732	22.824077
105.043657	3372.051737	22.829095
105.492109	3376.909779	22.834112
105.064094	3370.885755	22.839130
105.999985	3368.185377	22.844147
105.688044	3370.312524	22.849165
105.638429	3376.190014	22.854183
105.587222	3363.748043	22.859200
105.436614	3372.428490	22.864218
105.678193	3377.862273	22.869235
106.058892	3390.656499	22.874253
106.009524	3399.348744	22.879271
106.479234	3394.326181	22.884288
106.462855	3395.771027	22.889306
106.319701	3387.736314	22.894323
106.785596	3392.959955	22.899341
106.487646	3393.341018	22.904359
107.182994	3380.686776	22.909376
106.954572	3387.347057	22.914394
107.000248	3380.242391	22.919411
107.433346	3378.870211	22.924429
107.421430	3377.539670	22.929447
107.210895	3378.467286	22.934464
107.240418	3391.212244	22.939482
107.210290	3384.945161	22.944499
107.603850	3394.842853	22.949517
107.372521	3407.820774	22.954535
108.273900	3409.271313	22.959552
108.090049	3415.215935	22.964570
107.788572	3406.106537	22.969587
107.854752	3412.107527	22.974605
107.519659	3411.356125	22.979623
108.162981	3418.531684	22.984640
108.017123	3437.712885	22.989658
107.938493	3436.362273	22.994675
108.226268	3444.843168	22.999693
108.211828	3452.439449	23.004711
108.887948	3456.807991	23.009728
108.824146	3470.305397	23.014746
108.590961	3462.014367	23.019763
108.606060	3470.142720	23.024781
108.889703	3489.670131	23.029799
109.361138	3490.977802	23.034816
109.286637	3498.519033	23.039834
109.382016	3501.104834	23.044851
109.693306	3495.648663	23.049869
109.737617	3503.052178	23.054887
109.876751	3508.711491	23.059904
110.032823	3512.787228	23.064922
110.135345	3521.933138	23.069939
110.162028	3517.772492	23.074957
109.740288	3521.837815	23.079975
110.225527	3508.133420	23.084992
109.922415	3540.725841	23.090010
110.212262	3549.580539	23.095027
111.123570	3549.088001	23.100045
110.810363	3547.058532	23.105063
111.353985	3533.247233	23.110080
111.574671	3544.037058	23.115098
111.334845	3544.844479	23.120115
111.250504	3541.937788	23.125133
110.897541	3556.609506	23.130151
111.794480	3560.192020	23.135168
111.476950	3573.641652	23.140186
111.591722	3570.128248	23.145203
111.880530	3573.067603	23.150221
112.217943	3576.676736	23.155239
112.161296	3567.849756	23.160256
112.163036	3573.575963	23.165274
112.071168	3575.693761	23.170291
112.233128	3572.925196	23.175309
112.260054	3569.355182	23.180327
112.689312	3579.722572	23.185344
112.616288	3591.880408	23.190362
112.855694	3593.605906	23.195379
113.463071	3590.051365	23.200397
113.313136	3593.556605	23.205415
113.639198	3587.576491	23.210432
113.630257	3584.289064	23.215450
113.641442	3576.979937	23.220467
113.878682	3562.534365	23.225485
113.902684	3561.640272	23.230503
113.806177	3546.546256	23.235520
113.924411	3563.784264	23.240538
113.747703	3566.549822	23.245555
113.908620	3574.453186	23.250573
113.661485	3582.821086	23.255591
113.891041	3581.452281	23.260608
114.017197	3591.949612	23.265626
114.033026	3598.974502	23.270643
113.803283	3599.808550	23.275661
113.931149	3619.833804	23.280679
114.282037	3626.475993	23.285696
114.028285	3639.127949	23.290714
114.841419	3655.052947	23.295731
114.990421	3648.797579	23.300749
115.090032	3667.620368	23.305767
115.526923	3656.865773	23.310784
116.103197	3658.031048	23.315802
116.033674	3659.142428	23.320819
116.132119	3653.261167	23.325837
115.935587	3664.052504	23.330855
115.839737	3650.194789	23.335872
116.258307	3652.689768	23.340890
116.137840	3658.107744	23.345907
116.463822	3654.171408	23.350925
115.974992	3656.046960	23.355943
116.247994	3670.188538	23.360960
116.411480	3679.625735	23.365978
116.467613	3679.165601	23.370995
116.753600	3675.229815	23.376013
116.670835	3689.386720	23.381031
117.063354	3691.806625	23.386048
117.204023	3692.118800	23.391066
116.931832	3702.720724	23.396083
117.284355	3686.322531	23.401101
117.007704	3703.203878	23.406119
116.936017	3712.855469	23.411136
117.337689	3716.877341	23.416154
117.486190	3723.662955	23.421171
118.114745	3723.291346	23.426189
117.563534	3734.196304	23.431207
118.040616	3745.163625	23.436224
117.906632	3750.489440	23.441242
118.024324	3763.609442	23.446259
118.640138	3747.778008	23.451277
118.601962	3757.208080	23.456295
118.970701	3766.481765	23.461312
118.897262	3773.524399	23.466330
119.008092	3774.874225	23.471347
119.386540	3776.613712	23.476365
119.238116	3780.692890	23.481383
119.190059	3779.259035	23.486400
119.658981	3773.892310	23.491418
119.245719	3772.251707	23.496435
119.468835	3765.820557	23.501453
119.180251	3793.281418	23.506471
119.528236	3801.946721	23.511488
119.870511	3795.980289	23.516506
119.954276	3805.009077	23.521523
120.601653	3810.897982	23.526541
120.614468	3813.559422	23.531559
120.875198	3816.802136	23.536576
121.311076	3810.475472	23.541594
121.062474	3815.468115	23.546611
121.690765	3798.451524	23.551629
121.795567	3783.102244	23.556647
121.557651	3771.266114	23.561664
121.575703	3770.457302	23.566682
121.322077	3772.695005	23.571699
121.630769	3764.351085	23.576717
121.823226	3772.481481	23.581735
122.034195	3777.444158	23.586752
122.267169	3775.857375	23.591770
121.606426	3786.681122	23.596787
122.150480	3784.866163	23.601805
122.214267	3808.535813	23.606823
122.472177	3807.603182	23.611840
122.516268	3811.518623	23.616858
122.089801	3812.014662	23.621875
122.473001	3806.883149	23.626893
122.303401	3829.964341	23.631911
122.163007	3833.035607	23.636928
122.878647	3821.309265	23.641946
123.146647	3829.331441	23.646963
123.579415	3830.596941	23.651981
124.033129	3834.574481	23.656999
123.986621	3832.388202	23.662016
124.363170	3822.188856	23.667034
123.797587	3822.943448	23.672051
124.097067	3811.658626	23.677069
124.085247	3815.922319	23.682087
124.026569	3829.780661	23.687104
124.075471	3823.218683	23.692122
124.098544	3838.884727	23.697139
124.154504	3831.355155	23.702157
124.338745	3836.629595	23.707175
124.367307	3850.039033	23.712192
124.277658	3861.065787	23.717210
124.175048	3872.273556	23.722227
124.371027	3869.490445	23.727245
124.935553	3891.213283	23.732263
124.708129	3894.253013	23.737280
125.018622	3898.180300	23.742298
124.878814	3921.252580	23.747315
125.448259	3922.128423	23.752333
125.358366	3934.480802	23.757351
125.343396	3939.371212	23.762368
125.975504	3955.508699	23.767386
125.894216	3964.391815	23.772403
125.871092	3951.653152	23.777421
126.162545	3968.323975	23.782439
125.778426	3979.918749	23.787456
126.549826	3977.348077	23.792474
126.514803	3983.116965	23.797491
126.816745	3996.337892	23.802509
127.300869	4002.737659	23.807527
127.334479	4010.413396	23.812544
127.615704	4012.602760	23.817562
127.522396	4008.438139	23.822579
127.796197	4009.756110	23.827597
127.662620	4011.102963	23.832615
127.529586	4008.598335	23.837632
128.199377	3993.489876	23.842650
127.917004	4007.849833	23.847667
128.315838	4017.646991	23.852685
128.380716	4018.777099	23.857703
128.410048	4032.298399	23.862720
128.698430	4020.297035	23.867738
128.932897	4030.498066	23.872755
128.948358	4028.672886	23.877773
128.834409	4021.649640	23.882791
128.987235	4025.727644	23.887808
129.210729	4019.062407	23.892826
129.309277	4045.411400	23.897843
129.673504	4050.073803	23.902861
129.894014	4051.280410	23.907879
129.641325	4065.477021	23.912896
129.681783	4061.343012	23.917914
129.809185	4063.910815	23.922931
129.725962	4062.326228	23.927949
129.876690	4077.238937	23.932967
129.855624	4085.941673	23.937984
130.007449	4078.300249	23.943002
129.995871	4096.070676	23.948019
130.235881	4107.126150	23.953037
130.406257	4112.844121	23.958055
130.329011	4120.226235	23.963072
130.592670	4135.800921	23.968090
130.598799	4143.171115	23.973107
130.716467	4142.784693	23.978125
130.742024	4164.258481	23.983143
130.988351	4178.663426	23.988160
131.611463	4170.187420	23.993178
131.780766	4189.654966	23.998195
131.773102	4199.262798	24.003213
131.962819	4205.183842	24.008231
131.906510	4207.476780	24.013248
132.370731	4204.500342	24.018266
132.167261	4206.956340	24.023283
131.842049	4221.620764	24.028301
132.311997	4223.365883	24.033319
132.607838	4232.131727	24.038336
133.026588	4239.521806	24.043354
133.036258	4258.911263	24.048371
133.151742	4256.095414	24.053389
133.084713	4256.288047	24.058407
133.139641	4254.155205	24.063424
133.766836	4274.433579	24.068442
133.722435	4280.212846	24.073459
133.763784	4278.877035	24.078477
134.155942	4283.819838	24.083495
133.798191	4289.245628	24.088512
134.152166	4278.993152	24.093530
134.184454	4302.232601	24.098547
134.237687	4312.078163	24.103565
134.518403	4311.388119	24.108583
134.298656	4326.700100	24.113600
134.967672	4335.294911	24.118618
134.854418	4350.978532	24.123635
134.908934	4345.960689	24.128653
135.366173	4340.499690	24.133671
135.368537	4368.725284	24.138688
135.981521	4362.542107	24.143706
136.347477	4359.821924	24.148723
135.729499	4364.778820	24.153741
136.241955	4366.887639	24.158759
136.077090	4365.869928	24.163776
136.221912	4359.754407	24.168794
136.273415	4373.977909	24.173811
136.204873	4389.060034	24.178829
136.857717	4394.259055	24.183847
136.730706	4395.217303	24.188864
136.892449	4391.536566	24.193882
137.073865	4397.603240	24.198899
136.987117	4417.781293	24.203917
137.282228	4425.433668	24.208935
137.400615	4425.081772	24.213952
137.622288	4423.106202	24.218970
137.763778	4425.073054	24.223987
137.746345	4447.569058	24.229005
137.893314	4441.234177	24.234023
137.696653	4445.006743	24.239040
137.928287	4448.513706	24.244058
138.564482	4451.514972	24.249075
138.339645	4474.212758	24.254093
138.405969	4477.781935	24.259111
138.716744	4485.628562	24.264128
139.139624	4476.417206	24.269146
139.033678	4486.446114	24.274163
139.360316	4487.485700	24.279181
139.284366	4488.590364	24.284199
139.095483	4514.547553	24.289216
139.410568	4518.258400	24.294234
139.515641	4527.396580	24.299251
139.601045	4527.736363	24.304269
140.178465	4528.569134	24.309287
139.909526	4545.193286	24.314304
140.054334	4544.527320	24.319322
140.146197	4542.100622	24.324339
140.426711	4563.265025	24.329357
140.687162	4565.064214	24.334375
140.414896	4579.071670	24.339392
140.689509	4581.425289	24.344410
141.332823	4589.128321	24.349427
141.147248	4606.561324	24.354445
141.151658	4607.445071	24.359463
141.240494	4613.274082	24.364480
141.399723	4611.175295	24.369498
141.619427	4622.081023	24.374515
141.936100	4629.773121	24.379533
142.367292	4625.046629	24.384551
142.109809	4621.596021	24.389568
142.200915	4634.354267	24.394586
142.598665	4637.712288	24.399603
142.432906	4650.320034	24.404621
142.273435	4648.296356	24.409639
142.366549	4662.476752	24.414656
142.664154	4674.818415	24.419674
143.444337	4668.948293	24.424691
143.442854	4672.222747	24.429709
143.968348	4673.435406	24.434727
143.905156	4684.395186	24.439744
144.366933	4694.904242	24.444762
144.765155	4691.334123	24.449779
144.850901	4680.473631	24.454797
144.219968	4655.247417	24.459815
144.315788	4666.925031	24.464832
144.542502	4678.699148	24.469850
145.077431	4670.247448	24.474867
144.368963	4682.585154	24.479885
144.901830	4681.403704	24.484903
145.100515	4690.507816	24.489920
144.879146	4707.618621	24.494938
145.447072	4711.060118	24.499955
145.435916	4713.198887	24.504973
145.933756	4710.225258	24.509991
145.644625	4711.493291	24.515008
145.646499	4710.476905	24.520026
146.263071	4724.274620	24.525043
146.276617	4741.622440	24.530061
146.342139	4740.988961	24.535079
146.361251	4736.824566	24.540096
146.427063	4741.653329	24.545114
146.807172	4740.972222	24.550131
146.682407	4753.030338	24.555149
146.635520	4761.614212	24.560167
146.794194	4763.874314	24.565184
146.934644	4776.520247	24.570202
147.574456	4794.511390	24.575219
147.674046	4803.829466	24.580237
147.724139	4799.618786	24.585255
148.016339	4809.157468	24.590272
147.492933	4809.048697	24.595290
148.348546	4822.432177	24.600307
148.332530	4837.196967	24.605325
148.636699	4836.898281	24.610343
148.516764	4843.230239	24.615360
148.508770	4841.695689	24.620378
149.168456	4853.349243	24.625395
148.985402	4864.716430	24.630413
149.182768	4860.674249	24.635431
149.413890	4855.093521	24.640448
149.434953	4864.241572	24.645466
149.720620	4869.169736	24.650483
149.631418	4877.744386	24.655501
149.769010	4884.037727	24.660519
149.716030	4888.615160	24.665536
149.801040	4905.033298	24.670554
150.070350	4911.137876	24.675571
149.937520	4926.956958	24.680589
150.308196	4944.726609	24.685607
150.373773	4949.437328	24.690624
150.278197	4964.160739	24.695642
150.852038	4968.717383	24.700659
150.962210	4973.011672	24.705677
151.147942	4991.065128	24.710695
151.271534	4998.474657	24.715712
151.538513	5005.881663	24.720730
152.190902	5013.456538	24.725747
152.144945	5025.256389	24.730765
152.163347	5033.174676	24.735783
152.512637	5020.987258	24.740800
152.220818	5037.316538	24.745818
152.698879	5029.567535	24.750835
152.834632	5046.945149	24.755853
152.895656	5067.328691	24.760871
153.451901	5064.422964	24.765888
153.221994	5061.436187	24.770906
153.598416	5055.038099	24.775923
153.741553	5055.487721	24.780941
153.976079	5055.445144	24.785959
154.106317	5062.837811	24.790976
154.388483	5082.970796	24.795994
154.479947	5073.982107	24.801011
154.780335	5086.286594	24.806029
154.319111	5078.864781	24.811047
154.585645	5076.105598	24.816064
154.954669	5079.007860	24.821082
154.697699	5077.144194	24.826099
154.545128	5075.495778	24.831117
154.901891	5101.439941	24.836135
155.213993	5110.354719	24.841152
155.353593	5115.845183	24.846170
155.397158	5114.350603	24.851187
155.513363	5126.417316	24.856205
155.825315	5142.418719	24.861223
156.195688	5140.730272	24.866240
156.216813	5138.939438	24.871258
156.420242	5153.000542	24.876275
156.692274	5169.353811	24.881293
156.728606	5168.927749	24.886311
156.638335	5166.676321	24.891328
156.752075	5173.227494	24.896346
157.300378	5181.578025	24.901363
157.178772	5194.899345	24.906381
157.112042	5197.495887	24.911399
157.171527	5197.402975	24.916416
157.325205	5215.701631	24.921434
157.578960	5211.894659	24.926451
157.811488	5225.735020	24.931469
157.892448	5240.800203	24.936487
158.448485	5232.651778	24.941504
158.382203	5254.667373	24.946522
159.131149	5268.801263	24.951539
159.469644	5264.218078	24.956557
159.735192	5254.511811	24.961575
160.092177	5249.830152	24.966592
159.845249	5253.955735	24.971610
160.170711	5259.230074	24.976627
160.327003	5257.940642	24.981645
160.280607	5252.059201	24.986663
160.219524	5243.544748	24.991680
159.960694	5248.155209	24.996698
160.171253	5253.493353	25.001715
160.316893	5244.895415	25.006733
160.376276	5263.462345	25.011751
160.516339	5280.381054	25.016768
160.709337	5282.339972	25.021786
160.968077	5283.907964	25.026803
161.146356	5305.137359	25.031821
161.055288	5309.513498	25.036839
161.495632	5311.412689	25.041856
160.913677	5335.026757	25.046874
161.168490	5345.099124	25.051891
161.460312	5364.339167	25.056909
161.825900	5372.949547	25.061927
161.985855	5375.204792	25.066944
162.487798	5396.237832	25.071962
162.809621	5398.422010	25.076979
162.901583	5400.966963	25.081997
162.577332	5397.337799	25.087015
162.868239	5402.974926	25.092032
163.264710	5408.983071	25.097050
163.730869	5410.063394	25.102067
163.563687	5417.140155	25.107085
163.407767	5420.234079	25.112103
163.770747	5418.285365	25.117120
163.780271	5442.051040	25.122138
163.932574	5441.546802	25.127155
164.581659	5445.746475	25.132173
164.551466	5457.745591	25.137191
164.765089	5476.156362	25.142208
164.910276	5488.828833	25.147226
164.475070	5475.919343	25.152243
165.139699	5485.445002	25.157261
165.491747	5496.238064	25.162279
165.855144	5493.504741	25.167296
165.743387	5497.318924	25.172314
165.943529	5499.309728	25.177331
165.992519	5508.262744	25.182349
166.036539	5525.863768	25.187367
166.427672	5526.892372	25.192384
166.272659	5530.042875	25.197402
166.434220	5542.154904	25.202419
166.728933	5553.361126	25.207437
166.640173	5565.402658	25.212455
167.078408	5573.231916	25.217472
167.334132	5588.478569	25.222490
167.450730	5584.967559	25.227507
167.586522	5586.036000	25.232525
167.831541	5598.360619	25.237543
168.030392	5616.667748	25.242560
168.257534	5629.279809	25.247578
168.382363	5623.348398	25.252595
168.439550	5633.603699	25.257613
168.318359	5651.549045	25.262631
168.746373	5655.889071	25.267648
168.703032	5663.719008	25.272666
169.158262	5672.767893	25.277683
169.742951	5672.152507	25.282701
169.254967	5677.772803	25.287719
169.815289	5686.960431	25.292736
170.192605	5703.990946	25.297754
170.180138	5700.298024	25.302771
170.422607	5698.943372	25.307789
170.466787	5706.573220	25.312807
170.777145	5702.701292	25.317824
170.139241	5710.056584	25.322842
170.467684	5724.566229	25.327859
171.084152	5732.122405	25.332877
170.808938	5750.045428	25.337895
171.466021	5758.760438	25.342912
171.542035	5773.831700	25.347930
171.484617	5771.244511	25.352947
172.184867	5771.508856	25.357965
171.694984	5777.602916	25.362983
172.119131	5788.772151	25.368000
172.004627	5800.252709	25.373018
172.021202	5804.243466	25.378035
172.556373	5818.050581	25.383053
172.744868	5825.895207	25.388071
172.688220	5819.108676	25.393088
173.546993	5836.516815	25.398106
173.429842	5840.361149	25.403123
173.369858	5844.531243	25.408141
173.600008	5848.608280	25.413159
174.071031	5846.032105	25.418176
173.929014	5858.995140	25.423194
173.945951	5874.242828	25.428211
174.420531	5870.745222	25.433229
174.470600	5876.951561	25.438247
174.683900	5889.650486	25.443264
175.115118	5898.573647	25.448282
175.248715	5898.349084	25.453299
175.542747	5896.732726	25.458317
175.229693	5908.805089	25.463335
175.422966	5918.189681	25.468352
175.617324	5930.556325	25.473370
175.703777	5933.642671	25.478387
176.300567	5953.814203	25.483405
176.377811	5966.068617	25.488423
176.287102	5959.519449	25.493440
176.315474	5957.121538	25.498458
176.704936	5982.893759	25.503475
176.956526	5980.496966	25.508493
176.702590	5989.778665	25.513511
177.137115	6012.204136	25.518528
177.242041	6019.208524	25.523546
177.263913	6036.072679	25.528563
177.821011	6047.473735	25.533581
177.819545	6055.189558	25.538599
177.926083	6065.974681	25.543616
178.091645	6075.073452	25.548634
177.867771	6082.675386	25.553651
178.734585	6097.034793	25.558669
179.106614	6110.143075	25.563687
179.300648	6105.778980	25.568704
179.358200	6113.412245	25.573722
179.197790	6135.731131	25.578739
179.476331	6135.101255	25.583757
179.372138	6146.904831	25.588775
179.728753	6169.649511	25.593792
180.073818	6174.319774	25.598810
180.577834	6176.502764	25.603827
180.492240	6176.556024	25.608845
180.673457	6198.952711	25.613863
181.172180	6198.309509	25.618880
181.215719	6203.404844	25.623898
181.124970	6208.397953	25.628915
181.584368	6209.588200	25.633933
181.342135	6218.197681	25.638951
181.197581	6234.994473	25.643968
181.794336	6235.148175	25.648986
181.794254	6254.965531	25.654003
182.303318	6264.345033	25.659021
182.331771	6278.578131	25.664039
182.566684	6270.672496	25.669056
182.985707	6286.298289	25.674074
182.761875	6304.514821	25.679092
182.984351	6308.434173	25.684109
183.285317	6311.806785	25.689127
183.307399	6329.152510	25.694144
183.315690	6324.637445	25.699162
183.429800	6335.282814	25.704180
184.133509	6339.638001	25.709197
184.454534	6346.923729	25.714215
184.175511	6344.580816	25.719232
184.448055	6353.848098	25.724250
185.153598	6373.138967	25.729268
185.073375	6363.616548	25.734285
185.437010	6374.947026	25.739303
185.408707	6383.278880	25.744320
185.990360	6399.318031	25.749338
185.976967	6400.215170	25.754356
186.299658	6400.355988	25.759373
186.354357	6402.424616	25.764391
186.490864	6392.699606	25.769408
186.796130	6397.385422	25.774426
186.910693	6426.972379	25.779444
187.160874	6425.297318	25.784461
186.678848	6418.304595	25.789479
186.586215	6434.443612	25.794496
187.038097	6447.363610	25.799514
187.048888	6454.694690	25.804532
187.424719	6475.633409	25.809549
187.917531	6483.179636	25.814567
187.875823	6499.058704	25.819584
188.467657	6506.863673	25.824602
188.169045	6525.097213	25.829620
188.938366	6517.022653	25.834637
188.915628	6527.612048	25.839655
188.851757	6543.407521	25.844672
189.303091	6543.764971	25.849690
189.636562	6549.597660	25.854708
189.782186	6558.132959	25.859725
189.932250	6562.652435	25.864743
190.120852	6559.675555	25.869760
190.449107	6554.428129	25.874778
190.256326	6578.234115	25.879796
190.626692	6589.435192	25.884813
190.823052	6589.862346	25.889831
190.927962	6596.747256	25.894848
191.045023	6599.579561	25.899866
191.217534	6620.825092	25.904884
191.548113	6618.442235	25.909901
191.526167	6618.417629	25.914919
191.702794	6623.217728	25.919936
191.986654	6640.567758	25.924954
191.959405	6652.408145	25.929972
192.454959	6656.936170	25.934989
192.382532	6667.505817	25.940007
192.419650	6687.759253	25.945024
192.727027	6676.499415	25.950042
192.619232	6707.948620	25.955060
193.172560	6707.429956	25.960077
193.666880	6720.056953	25.965095
193.682703	6736.678686	25.970112
193.993991	6740.875173	25.975130
193.849605	6747.989576	25.980148
194.296749	6755.355492	25.985165
194.555841	6763.011238	25.990183
194.547872	6768.773347	25.995200
194.745833	6776.514414	26.000218
194.834421	6799.198018	26.005236
194.973276	6796.456492	26.010253
195.382798	6815.835667	26.015271
195.198993	6831.139161	26.020288
195.818299	6827.036764	26.025306
195.897102	6851.464610	26.030324
195.823837	6862.184201	26.035341
196.197968	6865.305704	26.040359
196.634010	6879.768813	26.045376
196.778467	6887.049608	26.050394
196.977736	6899.036470	26.055412
197.341550	6913.007832	26.060429
197.803467	6914.278055	26.065447
197.539603	6925.629836	26.070464
197.463649	6926.700793	26.075482
197.805830	6951.911570	26.080500
197.906791	6958.403437	26.085517
198.438715	6974.388675	26.090535
198.273536	6985.399029	26.095552
199.173560	6991.088287	26.100570
199.028016	7009.203971	26.105588
199.113461	7009.370498	26.110605
199.397862	7010.920876	26.115623
199.360266	7025.992315	26.120640
199.693727	7035.700936	26.125658
199.773798	7036.989359	26.130676
199.755162	7052.211972	26.135693
200.332687	7061.499074	26.140711
200.289377	7080.439425	26.145728
200.893246	7101.511609	26.150746
200.691263	7111.479852	26.155764
200.806869	7117.643930	26.160781
201.263006	7131.676858	26.165799
201.360138	7136.315069	26.170816
201.801615	7140.968305	26.175834
201.825763	7132.851019	26.180852
202.258455	7152.254203	26.185869
202.963615	7157.404223	26.190887
203.001792	7158.028665	26.195904
202.695375	7151.988640	26.200922
202.817205	7157.182721	26.205940
203.413415	7164.342090	26.210957
203.549738	7167.043578	26.215975
203.784345	7176.558898	26.220992
203.625453	7171.334119	26.226010
204.010625	7182.166766	26.231028
204.203632	7196.633224	26.236045
204.691274	7207.462504	26.241063
204.718652	7211.205190	26.246080
204.536604	7206.759527	26.251098
204.702177	7220.032521	26.256116
204.684411	7225.319088	26.261133
205.427796	7236.073827	26.266151
205.510977	7259.778378	26.271168
205.332493	7258.068788	26.276186
205.556223	7274.814570	26.281204
205.769460	7291.502298	26.286221
206.313930	7307.503839	26.291239
206.089378	7324.213864	26.296256
206.506710	7332.600594	26.301274
206.766592	7354.567900	26.306292
206.669037	7361.874641	26.311309
207.377037	7372.163662	26.316327
207.250414	7386.015475	26.321344
207.704135	7394.161243	26.326362
207.931918	7409.078840	26.331380
207.823684	7430.490161	26.336397
208.146608	7439.116857	26.341415
208.357564	7459.106714	26.346432
208.471352	7465.482362	26.351450
208.939847	7483.480722	26.356468
208.905578	7494.305127	26.361485
209.439697	7511.006616	26.366503
209.449572	7520.369234	26.371520
209.799211	7514.212674	26.376538
210.283665	7520.642974	26.381556
210.333978	7534.315694	26.386573
210.559837	7531.889998	26.391591
210.801863	7552.359130	26.396608
211.428048	7570.154095	26.401626
211.272194	7574.835799	26.406644
211.738387	7567.453147	26.411661
211.925438	7560.959697	26.416679
211.798363	7581.396026	26.421696
212.054991	7587.721241	26.426714
212.338758	7585.161929	26.431732
212.477859	7600.259551	26.436749
212.898125	7613.161496	26.441767
212.760779	7625.861251	26.446784
212.785393	7622.146561	26.451802
212.952875	7628.391751	26.456820
212.993522	7650.487638	26.461837
213.301273	7651.801683	26.466855
213.255326	7679.202429	26.471872
213.335319	7696.096973	26.476890
214.069918	7700.755275	26.481908
214.251035	7720.012416	26.486925
214.084164	7728.456954	26.491943
214.461293	7742.737150	26.496960
214.740701	7747.905201	26.501978
214.992369	7769.572761	26.506996
215.021728	7785.476372	26.512013
215.416574	7795.256077	26.517031
215.572214	7813.224142	26.522048
215.980478	7826.292177	26.527066
216.358848	7833.751527	26.532084
216.133196	7848.120173	26.537101
216.690268	7863.271657	26.542119
216.845640	7873.350068	26.547136
216.971766	7877.155551	26.552154
217.512611	7900.142909	26.557172
217.769421	7898.070301	26.562189
218.114496	7891.515756	26.567207
218.419117	7911.787910	26.572224
218.752170	7929.036371	26.577242
219.096454	7928.470793	26.582260
219.089781	7931.949269	26.587277
219.084218	7927.521997	26.592295
219.080653	7941.290957	26.597312
219.354271	7953.168966	26.602330
219.897134	7953.803042	26.607348
219.942511	7956.449351	26.612365
220.213043	7968.696591	26.617383
220.507166	7974.721683	26.622400
220.515085	7980.186078	26.627418
221.062136	7995.385099	26.632436
220.878383	8006.419029	26.637453
221.478809	8004.259936	26.642471
221.271018	8016.129912	26.647488
221.430231	8028.852417	26.652506
221.774496	8044.122482	26.657524
221.864780	8063.303432	26.662541
222.462544	8064.863228	26.667559
222.719413	8079.467644	26.672576
222.376786	8085.149723	26.677594
222.428891	8103.135860	26.682612
222.591163	8121.917727	26.687629
223.093965	8128.211990	26.692647
223.339847	8142.708841	26.697664
223.940886	8158.462046	26.702682
224.296646	8159.356668	26.707700
224.111736	8167.351537	26.712717
224.502709	8172.819666	26.717735
224.516602	8182.158346	26.722752
224.675593	8182.297311	26.727770
225.158734	8190.942645	26.732788
225.003977	8216.124786	26.737805
225.570605	8210.140328	26.742823
225.901238	8218.152420	26.747840
225.885034	8245.485220	26.752858
226.228689	8245.895054	26.757876
226.262241	8249.706252	26.762893
226.580755	8266.027948	26.767911
226.892931	8275.675585	26.772928
226.373869	8286.161352	26.777946
227.131610	8288.877837	26.782964
227.417733	8310.233762	26.787981
227.574078	8333.057607	26.792999
228.079975	8339.152893	26.798016
228.006483	8347.164992	26.803034
228.058138	8355.622821	26.808052
228.280731	8370.149080	26.813069
228.510745	8394.816489	26.818087
229.045334	8398.456756	26.823104
229.200833	8415.702300	26.828122
229.627730	8426.921765	26.833140
229.869799	8436.837559	26.838157
230.133844	8448.726242	26.843175
230.294221	8465.762230	26.848192
230.215724	8476.249809	26.853210
230.501516	8482.797275	26.858228
230.360290	8496.727388	26.863245
230.921315	8515.378339	26.868263
231.546796	8520.473140	26.873280
232.054880	8521.997147	26.878298
232.643639	8527.681238	26.883316
232.478338	8540.741815	26.888333
233.293990	8540.336497	26.893351
233.599875	8544.057754	26.898368
233.235159	8541.362859	26.903386
233.575446	8529.823501	26.908404
233.644673	8534.161223	26.913421
233.541449	8546.203532	26.918439
233.758615	8555.401229	26.923456
233.566632	8573.299739	26.928474
234.303533	8582.424909	26.933492
234.425105	8597.780944	26.938509
234.349917	8602.453844	26.943527
235.032861	8618.650407	26.948544
235.014082	8637.277982	26.953562
235.037445	8644.400708	26.958580
235.435015	8660.179830	26.963597
235.734207	8674.525427	26.968615
235.587465	8684.678192	26.973632
235.467963	8703.987253	26.978650
235.921445	8718.679090	26.983668
236.019834	8745.381734	26.988685
236.204828	8760.080237	26.993703
236.894376	8778.411662	26.998720
237.241481	8793.577960	27.003738
237.677231	8802.746210	27.008756
237.832622	8825.593764	27.013773
237.864002	8830.624265	27.018791
238.354137	8836.392338	27.023808
238.144797	8852.174046	27.028826
238.415282	8852.729586	27.033844
238.746303	8875.353297	27.038861
239.000324	8890.482068	27.043879
239.135381	8903.604904	27.048896
239.889601	8896.901828	27.053914
241.038311	8882.671817	27.058932
241.603722	8869.835440	27.063949
241.681128	8866.256378	27.068967
242.012770	8871.988604	27.073984
241.820594	8879.474546	27.079002
242.201349	8867.451365	27.084020
242.477406	8863.882372	27.089037
242.451385	8871.298863	27.094055
242.409785	8862.581394	27.099072
242.388832	8874.768203	27.104090
242.795184	8869.128480	27.109108
243.047039	8888.666400	27.114125
243.168886	8893.400941	27.119143
243.215251	8898.709367	27.124160
243.321977	8919.332642	27.129178
243.527259	8928.040973	27.134196
243.725266	8934.048239	27.139213
243.805480	8959.890086	27.144231
244.055818	8959.224766	27.149248
244.153788	8978.912077	27.154266
244.319444	8991.482972	27.159284
244.482506	9013.889859	27.164301
244.517168	9035.176399	27.169319
245.188747	9060.198522	27.174336
245.053765	9077.097486	27.179354
245.059005	9098.434848	27.184372
245.504999	9121.639545	27.189389
245.744966	9153.449911	27.194407
246.166864	9173.904460	27.199424
246.191221	9190.855018	27.204442
246.702986	9212.884116	27.209460
247.132619	9225.613215	27.214477
247.550724	9248.148465	27.219495
247.749873	9259.295675	27.224512
247.942535	9285.698636	27.229530
248.111630	9298.492936	27.234548
248.792022	9313.695566	27.239565
249.219421	9326.466097	27.244583
249.484610	9319.271531	27.249600
249.569636	9344.211848	27.254618
250.120237	9342.368397	27.259636
250.486452	9344.423404	27.264653
250.525516	9369.256610	27.269671
250.997417	9376.532835	27.274688
251.052272	9378.239402	27.279706
250.972640	9375.590043	27.284724
251.129337	9372.698482	27.289741
251.392120	9398.043318	27.294759
251.656189	9402.605512	27.299776
251.399392	9407.594194	27.304794
252.030964	9432.945206	27.309812
252.224545	9431.148758	27.314829
251.942503	9466.884577	27.319847
252.685544	9469.705430	27.324864
252.950115	9492.662851	27.329882
253.334846	9497.478570	27.334900
253.655175	9521.026835	27.339917
253.690882	9535.306484	27.344935
253.941636	9540.737664	27.349952
253.850642	9562.961950	27.354970
254.278485	9588.806672	27.359988
254.728793	9596.414457	27.365005
254.664523	9618.049630	27.370023
255.092221	9621.611595	27.375040
255.002934	9647.474140	27.380058
255.566502	9668.626735	27.385076
255.411329	9685.941070	27.390093
255.878949	9710.419281	27.395111
256.220795	9724.517410	27.400128
256.274574	9753.393691	27.405146
256.687167	9772.188153	27.410164
257.002992	9788.845133	27.415181
257.191277	9812.799370	27.420199
257.922531	9829.525431	27.425216
258.768033	9831.487320	27.430234
258.898512	9840.558791	27.435252
259.625430	9842.318822	27.440269
259.599722	9852.928247	27.445287
260.366702	9847.303590	27.450304
259.689667	9858.683335	27.455322
259.981369	9873.751419	27.460340
260.334442	9878.834261	27.465357
260.047500	9888.933808	27.470375
260.024902	9897.544630	27.475392
260.291071	9917.941724	27.480410
260.296290	9946.016715	27.485428
261.124305	9967.630206	27.490445
261.394428	9983.634962	27.495463
261.869398	10005.461869	27.500480
262.135304	10014.450345	27.505498
262.003481	10033.886803	27.510516
262.235188	10048.084460	27.515533
262.265916	10074.221789	27.520551
262.652190	10081.839204	27.525568
263.026759	10104.958282	27.530586
263.142344	10123.673269	27.535604
263.738441	10136.125579	27.540621
263.762515	10170.907537	27.545639
263.975461	10174.110905	27.550656
264.200695	10192.053936	27.555674
264.397879	10205.572167	27.560692
264.939576	10226.551176	27.565709
264.939189	10244.446267	27.570727
265.440922	10264.527652	27.575744
265.937689	10271.224847	27.580762
266.093047	10291.613040	27.585780
266.150646	10296.831754	27.590797
266.710433	10310.842613	27.595815
267.632436	10330.883564	27.600832
267.873694	10332.219478	27.605850
267.793893	10333.164462	27.610868
268.558851	10344.228049	27.615885
268.653852	10355.668062	27.620903
268.710724	10353.849247	27.625920
268.981269	10356.144554	27.630938
269.241744	10367.633430	27.635956
269.592100	10370.795951	27.640973
269.421671	10382.475306	27.645991
269.974825	10389.314166	27.651008
270.176880	10406.315906	27.656026
270.026377	10423.559313	27.661044
270.618421	10426.864794	27.666061
270.750834	10439.885326	27.671079
271.137825	10458.098761	27.676096
270.842847	10473.163955	27.681114
271.006767	10498.625163	27.686132
271.482711	10509.122244	27.691149
271.367355	10536.002366	27.696167
271.801162	10547.773679	27.701184
272.688146	10567.923358	27.706202
272.915363	10593.736312	27.711220
273.467466	10598.512646	27.716237
274.265723	10590.450831	27.721255
274.505876	10612.150189	27.726272
274.575106	10619.544850	27.731290
274.876985	10608.539304	27.736308
275.022087	10605.531324	27.741325
275.382519	10627.446465	27.746343
275.478978	10637.802237	27.751360
275.848857	10638.061881	27.756378
275.945628	10643.634865	27.761396
276.337146	10663.948380	27.766413
276.672684	10671.866306	27.771431
276.675780	10676.823436	27.776448
276.863981	10695.673191	27.781466
277.392847	10704.391631	27.786484
277.616759	10713.192286	27.791501
277.953809	10726.166943	27.796519
278.084348	10721.602903	27.801536
278.671866	10742.027902	27.806554
279.286661	10736.290354	27.811572
280.058021	10728.795669	27.816589
280.243040	10727.730176	27.821607
280.171775	10735.687918	27.826624
280.373667	10726.138200	27.831642
279.977894	10724.529300	27.836660
280.360367	10724.239961	27.841677
280.512405	10730.364511	27.846695
280.350385	10747.006678	27.851712
280.761797	10755.072380	27.856730
280.667900	10774.333029	27.861748
281.303010	10788.430676	27.866765
281.160796	10813.533546	27.871783
281.331919	10834.802212	27.876800
281.722922	10855.755864	27.881818
281.643085	10879.253351	27.886836
282.374792	10892.266082	27.891853
282.620987	10919.357497	27.896871
282.801610	10940.601035	27.901888
283.377376	10957.944305	27.906906
283.287041	10985.057264	27.911924
283.869004	11001.474468	27.916941
284.405882	11020.594201	27.921959
284.556591	11039.115115	27.926976
284.785564	11056.387130	27.931994
284.647312	11082.666933	27.937012
285.281531	11091.753623	27.942029
285.764664	11113.451403	27.947047
286.008734	11131.478921	27.952064
286.720639	11145.469162	27.957082
286.752075	11172.140794	27.962100
287.145480	11193.146475	27.967117
287.439525	11193.406521	27.972135
287.666106	11220.055816	27.977152
287.864191	11218.363989	27.982170
288.027382	11238.570799	27.987188
288.347968	11253.056854	27.992205
288.447572	11271.908281	27.997223
288.946495	11289.014504	28.002240
289.060815	11310.633927	28.007258
289.741725	11340.477171	28.012276
289.778143	11347.787960	28.017293
289.867007	11359.924717	28.022311
290.005842	11386.866687	28.027328
290.619431	11409.202819	28.032346
290.466536	11429.724071	28.037364
290.916394	11437.367477	28.042381
290.850513	11475.634708	28.047399
291.089387	11504.580084	28.052416
291.752244	11521.718340	28.057434
292.217011	11558.503254	28.062452
292.573841	11577.473268	28.067469
292.991253	11592.140025	28.072487
293.084132	11611.448446	28.077504
293.407663	11625.319706	28.082522
293.742192	11654.616152	28.087540
294.381166	11666.288501	28.092557
294.854757	11660.819112	28.097575
295.357773	11674.467384	28.102592
295.818902	11684.531229	28.107610
296.021561	11686.778477	28.112628
296.076840	11689.462313	28.117645
296.666574	11683.318986	28.122663
296.575890	11695.464703	28.127680
297.054345	11709.933564	28.132698
297.363259	11718.343541	28.137716
297.546243	11715.921429	28.142733
297.743210	11728.872043	28.147751
297.487436	11758.704817	28.152768
298.187293	11765.002204	28.157786
298.473036	11784.096538	28.162804
298.195546	11794.944227	28.167821
298.853750	11812.950375	28.172839
298.983360	11834.403971	28.177856
299.411638	11842.530366	28.182874
299.314038	11864.194724	28.187892
299.469276	11888.168718	28.192909
300.061873	11919.534801	28.197927
299.926741	11946.817784	28.202944
300.301541	11978.500259	28.207962
300.499244	12000.240264	28.212980
300.613831	12020.191605	28.217997
301.436029	12052.205725	28.223015
301.522038	12082.409180	28.228032
302.234026	12103.082481	28.233050
302.234720	12119.502730	28.238068
302.553001	12135.767700	28.243085
303.007018	12149.773067	28.248103
303.018909	12186.268231	28.253120
303.585137	12208.753844	28.258138
304.026407	12232.975609	28.263156
304.241772	12253.507272	28.268173
304.807359	12272.179122	28.273191
304.974433	12299.942016	28.278208
305.323380	12306.793055	28.283226
305.761567	12335.054845	28.288244
306.158150	12343.174315	28.293261
306.817415	12367.604778	28.298279
306.652610	12384.277454	28.303296
307.121352	12401.854951	28.308314
307.221232	12415.996893	28.313332
307.169999	12446.752513	28.318349
307.494178	12459.205941	28.323367
308.050465	12487.356343	28.328384
308.484679	12503.130573	28.333402
308.658297	12531.680759	28.338420
308.967240	12551.416616	28.343437
309.480277	12571.342892	28.348455
309.640778	12597.895437	28.353472
310.100779	12611.964794	28.358490
310.547562	12629.139678	28.363508
310.473501	12649.138303	28.368525
310.665389	12654.960450	28.373543
310.925845	12682.386472	28.378560
311.777484	12692.226407	28.383578
312.108513	12706.128823	28.388596
312.204444	12724.982555	28.393613
312.939962	12736.100116	28.398631
312.904678	12753.228515	28.403648
313.265764	12766.938280	28.408666
313.431160	12768.199145	28.413684
313.391707	12796.431696	28.418701
313.852580	12798.499303	28.423719
314.282488	12819.223435	28.428736
314.981569	12838.460929	28.433754
315.560167	12846.259458	28.438772
315.786263	12867.639557	28.443789
316.160147	12880.649022	28.448807
316.057041	12899.147776	28.453824
316.237006	12905.801075	28.458842
316.772120	12921.211678	28.463860
317.041952	12934.606248	28.468877
318.015557	12941.399353	28.473895
317.873609	12956.156903	28.478912
318.246472	12977.428458	28.483930
318.382671	12986.689834	28.488948
318.981877	12988.508377	28.493965
319.419138	12993.481634	28.498983
319.737534	13004.674023	28.504000
320.490074	13014.641466	28.509018
321.019887	13017.984953	28.514036
321.065649	13023.764505	28.519053
321.654726	13013.961120	28.524071
321.566893	13022.406672	28.529088
321.813866	13011.689473	28.534106
321.955579	13025.693957	28.539124
321.947612	13041.826614	28.544141
322.780914	13038.977634	28.549159
323.110317	13061.604307	28.554176
323.223555	13065.903390	28.559194
324.459689	13058.198766	28.564212
324.165274	13060.774118	28.569229
324.522914	13076.869367	28.574247
324.676560	13089.563701	28.579264
324.950125	13087.742120	28.584282
325.211233	13095.852088	28.589300
325.443571	13108.435232	28.594317
325.842309	13121.982809	28.599335
326.031296	13147.078199	28.604352
326.064275	13161.050999	28.609370
326.234855	13171.400404	28.614388
326.181567	13192.012387	28.619405
326.612198	13214.724370	28.624423
326.527508	13243.792901	28.629440
326.963963	13264.229624	28.634458
327.264136	13291.079306	28.639476
327.600895	13330.998252	28.644493
327.991315	13347.896699	28.649511
328.051390	13374.786091	28.654528
328.361671	13404.048848	28.659546
328.875785	13420.678718	28.664564
328.871986	13453.809626	28.669581
329.308106	13479.233558	28.674599
329.481654	13501.540800	28.679616
329.683810	13530.800248	28.684634
330.294766	13563.900095	28.689652
330.189457	13603.769376	28.694669
331.211907	13628.010236	28.699687
331.613157	13648.631577	28.704704
332.000328	13673.342321	28.709722
332.388613	13689.659886	28.714740
332.364280	13724.522323	28.719757
332.242993	13747.080600	28.724775
333.111657	13778.398207	28.729792
333.276196	13810.049333	28.734810
334.076701	13821.210091	28.739828
334.273757	13856.450972	28.744845
334.844175	13878.980723	28.749863
335.466364	13897.167151	28.754880
335.963781	13909.108108	28.759898
336.428778	13932.967379	28.764916
336.344604	13946.716617	28.769933
336.747091	13961.332896	28.774951
336.808004	13988.076560	28.779968
336.904011	14007.798651	28.784986
337.510985	14030.684868	28.790004
337.548974	14058.628902	28.795021
337.919312	14081.878865	28.800039
338.430586	14111.162023	28.805056
338.561180	14145.229612	28.810074
339.150435	14166.547585	28.815092
339.313720	14186.855740	28.820109
339.843747	14213.601333	28.825127
340.515304	14233.029604	28.830144
340.931190	14248.599024	28.835162
341.256787	14265.233688	28.840180
341.606155	14274.118795	28.845197
342.004051	14285.649929	28.850215
342.675884	14309.463265	28.855232
342.922305	14330.769278	28.860250
343.150293	14336.566924	28.865268
343.302829	14350.012700	28.870285
343.710306	14369.869413	28.875303
344.213170	14388.128852	28.880320
344.334102	14400.434173	28.885338
344.793238	14412.929007	28.890356
344.829094	14436.123307	28.895373
345.468148	14453.407438	28.900391
345.581021	14471.855177	28.905408
346.039569	14491.313956	28.910426
346.560917	14506.810378	28.915444
346.603671	14523.386594	28.920461
346.809256	14551.638477	28.925479
347.257473	14567.752765	28.930496
347.369657	14587.885752	28.935514
348.072597	14604.845421	28.940532
347.924824	14623.442032	28.945549
348.460364	14640.121483	28.950567
348.943757	14651.174806	28.955584
349.125885	14678.401637	28.960602
349.612726	14679.919659	28.965620
349.585884	14711.077270	28.970637
350.024136	14734.795696	28.975655
350.808979	14751.924327	28.980672
350.707513	14782.122310	28.985690
351.106856	14798.841027	28.990708
351.227373	14828.072633	28.995725
351.475857	14850.584805	29.000743
352.022034	14875.758746	29.005760
351.864123	14902.046444	29.010778
353.185442	14924.023343	29.015796
353.328939	14952.934400	29.020813
353.461975	14975.338850	29.025831
354.134978	14994.257060	29.030848
354.322988	15026.954722	29.035866
354.817401	15045.931972	29.040884
355.019555	15078.759720	29.045901
355.494012	15099.228466	29.050919
356.097024	15116.087568	29.055936
356.268473	15142.418506	29.060954
356.817800	15159.810183	29.065972
357.126197	15177.481189	29.070989
357.915629	15199.525970	29.076007
358.332599	15204.736677	29.081024
358.346395	15223.192777	29.086042
358.606229	15243.376919	29.091060
358.805148	15260.352711	29.096077
358.951320	15281.067101	29.101095
359.574741	15307.908806	29.106112
359.648237	15335.407544	29.111130
359.870539	15353.370924	29.116148
360.808903	15377.527900	29.121165
360.814068	15406.186024	29.126183
361.585968	15420.803343	29.131200
361.615954	15448.427949	29.136218
362.100717	15467.366353	29.141236
362.318764	15486.032071	29.146253
362.432133	15503.268680	29.151271
363.189686	15524.942618	29.156288
363.380987	15549.796934	29.161306
363.859974	15580.209005	29.166324
364.415018	15592.811254	29.171341
364.681382	15613.658365	29.176359
365.043815	15644.189839	29.181376
364.997739	15664.879331	29.186394
365.458686	15685.100480	29.191412
366.347738	15712.628743	29.196429
366.144940	15731.362131	29.201447
366.830217	15743.423557	29.206464
366.608139	15770.765593	29.211482
366.703229	15795.260016	29.216500
367.309595	15815.565172	29.221517
367.444145	15845.915380	29.226535
367.968614	15869.724699	29.231552
367.709836	15898.845066	29.236570
368.242003	15936.068032	29.241588
368.404796	15976.333728	29.246605
369.056552	16011.249052	29.251623
370.123401	16039.983268	29.256640
370.131635	16076.451401	29.261658
370.415935	16104.796482	29.266676
370.879855	16129.639624	29.271693
371.414469	16153.108688	29.276711
372.457407	16181.358566	29.281728
372.590363	16202.472045	29.286746
373.143911	16224.733601	29.291764
373.474623	16242.023583	29.296781
373.635305	16277.031508	29.301799
374.306658	16287.717945	29.306816
374.324392	16311.550108	29.311834
374.378925	16338.563493	29.316852
374.762539	16360.196992	29.321869
375.198159	16396.472774	29.326887
375.699331	16415.527682	29.331904
376.092751	16440.517366	29.336922
376.980195	16455.396405	29.341940
377.544747	16466.438615	29.346957
377.900677	16484.826446	29.351975
378.571724	16492.487918	29.356992
378.732777	16513.844475	29.362010
378.947240	16525.515810	29.367028
379.510763	16539.884501	29.372045
379.683361	16556.848790	29.377063
380.230456	16589.243643	29.382080
380.455298	16612.665553	29.387098
380.810046	16630.937092	29.392116
381.099979	16643.111070	29.397133
381.317957	16661.440763	29.402151
381.763007	16680.422043	29.407168
381.719635	16710.107532	29.412186
382.556236	16725.876759	29.417204
382.917478	16745.496747	29.422221
382.887757	16771.590441	29.427239
383.519724	16785.942887	29.432256
383.913686	16812.055469	29.437274
384.683158	16829.718584	29.442292
385.380340	16837.757241	29.447309
385.489492	16859.493602	29.452327
385.966740	16871.716046	29.457344
386.185781	16892.758894	29.462362
386.656240	16913.195886	29.467380
386.999476	16933.435578	29.472397
386.614670	16959.068608	29.477415
387.436607	16970.577821	29.482432
387.520879	16997.267154	29.487450
387.889282	17014.680752	29.492468
388.464946	17041.049472	29.497485
388.003829	17069.847119	29.502503
388.794401	17103.650028	29.507520
388.773884	17133.529413	29.512538
389.049654	17164.147893	29.517556
389.838175	17196.434764	29.522573
390.146617	17231.704714	29.527591
390.701871	17257.862872	29.532608
390.912327	17299.271282	29.537626
391.652342	17320.085079	29.542644
392.128404	17349.786735	29.547661
392.458742	17378.725165	29.552679
393.251406	17397.411215	29.557696
393.400699	17417.441948	29.562714
393.712712	17445.395163	29.567732
394.157179	17452.690751	29.572749
394.445138	17489.616940	29.577767
394.909789	17513.298555	29.582784
395.344205	17535.989026	29.587802
395.553675	17554.939154	29.592820
396.303485	17582.190116	29.597837
396.293253	17609.424756	29.602855
396.705954	17642.976634	29.607872
397.070851	17667.170594	29.612890
397.893446	17707.954856	29.617908
398.021213	17723.545391	29.622925
398.626593	17757.661987	29.627943
398.991122	17783.539923	29.632960
399.435501	17813.195807	29.637978
399.385283	17846.222030	29.642996
400.059538	17865.769199	29.648013
400.624594	17886.232163	29.653031
401.380721	17901.869684	29.658048
401.616369	17926.699448	29.663066
402.241572	17956.680900	29.668084
402.337536	17977.172338	29.673101
402.624733	18006.489739	29.678119
403.029752	18030.458205	29.683136
403.100137	18060.631094	29.688154
403.140033	18092.748444	29.693172
404.208413	18115.827679	29.698189
404.843429	18153.961846	29.703207
405.144912	18170.267172	29.708224
405.857787	18201.307689	29.713242
405.897952	18224.232197	29.718260
406.178417	18243.790537	29.723277
406.774547	18281.105526	29.728295
407.025870	18300.249552	29.733312
407.693900	18320.808917	29.738330
407.955632	18347.987112	29.743348
408.595522	18371.570543	29.748365
408.690557	18389.959462	29.753383
409.239749	18415.814613	29.758400
409.602050	18430.884749	29.763418
409.929611	18439.484161	29.768436
410.829264	18461.864400	29.773453
410.861883	18485.041238	29.778471
411.107831	18507.066886	29.783488
411.374633	18527.370482	29.788506
411.806474	18554.668062	29.793524
412.115888	18580.544061	29.798541
412.198586	18612.517904	29.803559
412.482905	18644.946010	29.808576
412.924473	18680.834729	29.813594
412.900742	18711.589346	29.818612
413.663090	18750.958048	29.823629
413.963668	18789.589277	29.828647
414.638999	18810.154298	29.833664
415.254153	18838.824135	29.838682
415.368557	18877.880055	29.843700
415.922695	18907.777635	29.848717
416.711490	18946.877387	29.853735
417.009538	18975.772078	29.858752
417.531018	18990.615205	29.863770
417.945660	19027.221926	29.868788
418.111871	19050.092849	29.873805
418.728645	19085.276019	29.878823
419.054114	19116.723603	29.883840
419.527988	19149.545897	29.888858
419.934055	19186.372015	29.893876
420.658523	19215.924043	29.898893
421.046835	19242.430824	29.903911
421.234633	19268.387060	29.908928
422.029651	19296.981132	29.913946
422.453930	19328.751166	29.918964
423.069366	19347.772498	29.923981
423.448853	19377.752875	29.928999
423.746338	19397.773189	29.934016
424.193737	19418.165163	29.939034
424.494306	19466.587653	29.944052
424.954197	19482.914409	29.949069
425.190153	19507.970347	29.954087
425.680695	19537.294988	29.959104
426.421521	19546.413838	29.964122
426.641600	19569.485937	29.969140
428.432619	19566.944810	29.974157
429.284377	19582.640049	29.979175
429.218689	19578.542386	29.984192
430.148308	19584.120724	29.989210
429.846518	19588.640830	29.994228
430.431115	19596.271261	29.999245
430.796201	19615.343682	30.004263
430.622063	19626.170856	30.009280
431.140967	19636.035731	30.014298
431.303541	19665.717952	30.019316
431.534378	19685.920316	30.024333
431.694439	19708.706467	30.029351
431.964363	19734.078572	30.034368
432.440205	19760.301550	30.039386
432.608546	19790.036610	30.044404
432.842661	19822.053021	30.049421
432.987446	19852.167489	30.054439
432.923391	19899.759696	30.059456
433.932609	19926.331440	30.064474
433.986944	19975.254840	30.069492
433.979348	20013.996870	30.074509
434.794795	20053.914539	30.079527
435.172200	20095.561387	30.084544
436.021530	20129.688300	30.089562
436.296859	20173.725860	30.094580
437.072523	20205.550858	30.099597
437.616161	20233.415407	30.104615
438.127379	20274.453205	30.109632
438.554048	20306.822270	30.114650
438.984968	20347.610683	30.119668
439.525522	20379.838960	30.124685
440.340378	20416.380112	30.129703
440.782169	20434.634576	30.134720
441.088093	20454.060246	30.139738
441.734290	20490.816524	30.144756
441.811158	20515.352492	30.149773
442.543398	20543.503746	30.154791
443.222500	20572.277529	30.159808
443.907061	20602.690305	30.164826
443.986865	20621.342861	30.169844
444.494736	20647.028765	30.174861
444.869607	20676.091380	30.179879
444.917467	20706.712788	30.184896
445.490919	20723.800234	30.189914
445.644764	20770.886075	30.194932
445.966051	20802.364319	30.199949
446.545939	20836.871544	30.204967
446.862827	20885.084001	30.209984
447.471579	20913.094618	30.215002
448.074638	20946.538463	30.220020
448.347551	20978.130970	30.225037
448.848505	21012.082838	30.230055
449.279786	21043.258848	30.235072
450.398734	21073.271625	30.240090
450.543612	21108.705446	30.245108
450.989161	21132.333935	30.250125
451.814092	21158.652215	30.255143
452.032214	21187.619572	30.260160
452.577236	21215.383005	30.265178
453.138827	21240.095563	30.270196
453.578673	21261.348873	30.275213
454.182492	21296.712326	30.280231
454.396501	21318.974183	30.285248
454.797610	21342.995338	30.290266
454.636172	21374.812816	30.295284
455.276075	21411.280446	30.300301
455.865715	21431.062300	30.305319
456.372600	21472.043818	30.310336
457.110679	21490.329070	30.315354
457.444003	21516.708495	30.320372
457.670793	21538.468575	30.325389
458.360385	21565.826200	30.330407
458.636897	21594.870974	30.335424
458.907092	21620.062935	30.340442
459.164844	21640.778663	30.345460
459.470487	21677.783522	30.350477
459.981097	21710.580837	30.355495
460.431729	21740.930088	30.360512
460.808387	21781.086287	30.365530
461.142238	21816.907081	30.370548
461.457215	21852.079916	30.375565
462.159455	21897.695095	30.380583
462.369154	21934.493028	30.385600
463.468973	21976.206774	30.390618
463.732386	22013.926064	30.395636
463.898174	22057.011149	30.400653
464.395798	22085.534749	30.405671
464.822052	22126.310885	30.410688
465.382579	22162.449952	30.415706
466.260117	22210.172696	30.420724
466.422693	22256.371743	30.425741
467.077550	22286.234382	30.430759
467.640690	22321.143308	30.435776
467.865687	22355.230299	30.440794
468.803933	22373.639902	30.445812
469.087248	22409.505293	30.450829
470.023869	22424.313422	30.455847
470.196887	22465.565853	30.460864
470.685861	22497.636673	30.465882
471.299902	22530.395764	30.470900
471.855550	22562.294427	30.475917
472.482988	22587.387176	30.480935
472.719086	22620.968160	30.485952
473.083900	22643.636423	30.490970
473.779315	22682.888545	30.495988
474.010929	22705.844651	30.501005
474.783807	22732.578005	30.506023
474.938129	22766.845090	30.511040
475.839186	22790.680112	30.516058
476.168156	22823.876559	30.521076
476.623965	22853.323275	30.526093
477.125328	22874.482899	30.531111
477.190902	22909.929316	30.536128
477.453752	22943.263486	30.541146
478.107692	22981.296477	30.546164
478.662262	23017.261747	30.551181
479.119313	23048.194147	30.556199
479.446093	23094.149686	30.561216
479.513848	23134.283143	30.566234
479.928757	23169.616616	30.571252
480.446718	23221.103544	30.576269
481.242354	23244.727016	30.581287
481.450343	23296.305134	30.586304
482.378544	23302.561532	30.591322
483.427879	23333.386649	30.596340
483.858050	23360.154477	30.601357
484.710832	23372.019237	30.606375
485.356963	23387.565585	30.611392
486.042436	23392.734433	30.616410
486.565935	23414.442906	30.621428
486.839217	23431.194979	30.626445
487.376421	23447.327791	30.631463
487.291468	23462.154172	30.636480
487.992926	23479.876944	30.641498
488.483841	23498.219328	30.646516
488.809165	23530.108797	30.651533
489.800943	23552.620368	30.656551
489.711905	23575.872301	30.661568
489.797270	23611.711045	30.666586
490.299002	23625.181678	30.671604
490.504085	23670.153433	30.676621
491.011704	23700.280338	30.681639
491.353169	23730.577706	30.686656
492.107780	23780.795630	30.691674
492.885563	23810.456928	30.696692
493.020635	23848.186477	30.701709
493.228036	23880.860123	30.706727
493.208367	23926.555524	30.711744
493.808065	23966.792183	30.716762
494.242088	24004.070261	30.721780
494.432094	24062.943207	30.726797
494.946680	24098.677873	30.731815
495.077201	24165.683574	30.736832
495.672975	24222.106062	30.741850
496.328925	24272.872247	30.746868
496.853199	24335.496071	30.751885
497.463051	24381.627347	30.756903
498.000137	24432.997917	30.761920
498.828162	24494.633440	30.766938
499.555917	24546.435363	30.771956
499.729209	24591.642080	30.776973
500.541781	24633.386296	30.781991
500.916162	24680.019253	30.787008
501.416294	24714.347673	30.792026
502.418431	24764.601757	30.797044
502.797925	24807.171344	30.802061
503.715670	24837.125869	30.807079
504.131950	24869.999021	30.812096
504.888208	24901.829806	30.817114
505.378035	24933.091194	30.822132
506.029493	24982.251488	30.827149
506.736544	25000.574215	30.832167
507.117472	25027.718989	30.837184
507.421969	25068.683850	30.842202
508.177216	25095.035916	30.847220
508.556604	25130.912602	30.852237
509.297299	25161.579391	30.857255
509.454230	25185.236118	30.862272
509.762252	25211.914197	30.867290
510.357614	25248.744621	30.872308
510.300373	25279.116180	30.877325
510.829248	25310.702780	30.882343
511.539384	25347.882823	30.887360
511.568926	25385.517095	30.892378
511.993313	25418.768440	30.897396
512.085314	25471.429688	30.902413
512.565294	25507.892430	30.907431
513.320871	25567.831295	30.912448
513.819331	25609.710557	30.917466
514.377008	25658.901461	30.922484
514.568361	25719.133108	30.927501
515.232512	25763.987486	30.932519
515.341520	25815.823523	30.937536
516.118916	25871.340148	30.942554
516.796172	25909.615360	30.947572
518.028649	25955.199354	30.952589
518.273092	25997.665668	30.957607
519.369424	26033.251028	30.962624
519.815379	26082.771428	30.967642
520.195274	26113.927600	30.972660
520.894302	26152.174381	30.977677
521.217709	26191.226948	30.982695
522.235319	26234.211216	30.987712
522.879665	26261.801759	30.992730
523.773217	26299.968216	30.997748
523.721860	26328.132338	31.002765
524.018989	26362.246437	31.007783
524.585492	26387.569692	31.012800
525.219310	26432.724381	31.017818
526.040769	26449.688306	31.022836
526.116859	26497.856810	31.027853
526.556947	26534.555682	31.032871
527.298580	26580.073998	31.037888
527.391280	26625.138930	31.042906
528.010482	26662.879986	31.047924
528.436892	26708.799670	31.052941
528.884170	26753.479242	31.057959
529.391761	26801.262329	31.062976
529.905128	26844.612126	31.067994
530.530976	26885.248591	31.073012
530.849574	26939.771466	31.078029
531.189831	26981.624355	31.083047
532.126272	27031.457760	31.088064
532.454832	27088.638880	31.093082
533.113473	27127.566700	31.098100
533.807856	27172.936921	31.103117
534.485601	27211.066640	31.108135
535.158001	27255.059030	31.113152
535.796778	27293.403826	31.118170
536.738803	27328.103380	31.123188
536.979443	27360.550735	31.128205
538.286364	27381.347561	31.133223
539.195095	27394.407527	31.138240
539.120155	27434.316690	31.143258
539.506094	27446.153850	31.148276
540.284741	27470.215091	31.153293
540.216816	27495.178588	31.158311
540.822931	27524.203687	31.163328
541.019983	27562.586901	31.168346
541.305368	27596.478274	31.173364
541.857950	27634.671379	31.178381
542.302014	27671.327794	31.183399
543.165998	27713.528078	31.188416
543.482754	27755.853775	31.193434
544.087172	27787.308891	31.198452
544.591884	27833.612482	31.203469
544.816514	27875.307492	31.208487
545.294183	27916.861441	31.213504
545.895640	27960.328267	31.218522
546.652969	28005.863391	31.223540
547.112470	28052.408774	31.228557
547.448475	28097.240201	31.233575
548.246549	28141.812737	31.238592
548.957917	28182.813013	31.243610
549.634115	28226.261383	31.248628
549.967449	28268.913599	31.253645
550.925420	28309.316636	31.258663
551.252052	28356.371465	31.263680
551.338179	28404.067084	31.268698
552.138765	28443.263777	31.273716
552.603869	28500.372475	31.278733
552.669432	28547.728106	31.283751
553.497390	28590.233252	31.288768
553.793785	28656.565237	31.293786
554.207325	28697.630366	31.298804
555.132801	28748.931352	31.303821
555.280257	28811.642148	31.308839
556.325678	28869.100638	31.313856
556.329986	28927.242518	31.318874
557.120565	28969.486801	31.323892
557.664855	29029.603115	31.328909
558.090344	29089.834644	31.333927
558.909245	29147.544251	31.338944
559.317810	29206.400268	31.343962
560.130534	29260.047432	31.348980
560.942991	29291.557946	31.353997
561.614189	29350.016063	31.359015
562.236539	29399.818524	31.364032
562.657144	29450.999817	31.369050
563.083475	29493.667463	31.374068
563.758347	29547.692507	31.379085
563.971686	29612.294313	31.384103
564.938080	29651.897563	31.389120
565.139178	29714.741206	31.394138
565.888302	29769.972143	31.399156
566.637939	29814.355282	31.404173
567.142187	29864.832434	31.409191
568.080447	29903.115844	31.414208
568.664257	29938.273204	31.419226
569.648929	29954.862344	31.424244
570.346489	29986.387478	31.429261
571.036471	30018.683867	31.434279
571.913847	30036.831267	31.439296
572.513461	30055.739380	31.444314
573.564058	30080.098392	31.449332
574.057274	30109.904393	31.454349
574.413690	30127.418572	31.459367
574.831974	30147.784068	31.464384
575.150944	30181.419082	31.469402
575.188883	30206.522890	31.474420
575.984375	30243.383193	31.479437
576.165797	30282.809972	31.484455
576.693785	30309.357164	31.489472
577.176005	30360.155044	31.494490
577.565741	30399.798824	31.499508
578.114523	30444.902682	31.504525
578.456243	30502.288275	31.509543
578.756752	30547.592702	31.514560
578.728694	30607.127720	31.519578
579.514078	30661.408601	31.524596
580.255652	30719.224945	31.529613
580.389085	30788.672568	31.534631
581.184573	30846.047790	31.539648
581.815839	30911.406305	31.544666
582.526883	30969.758818	31.549684
583.078243	31029.533614	31.554701
583.284674	31090.894976	31.559719
584.235686	31152.700131	31.564736
584.971647	31214.737988	31.569754
585.562887	31259.202378	31.574772
586.556666	31326.437813	31.579789
586.948091	31388.667840	31.584807
587.757905	31436.862973	31.589824
588.342023	31492.133860	31.594842
588.709411	31552.566739	31.599860
589.546586	31604.900938	31.604877
590.167378	31662.510686	31.609895
590.758677	31699.557314	31.614912
591.744346	31753.542145	31.619930
592.501418	31793.242855	31.624948
593.362742	31832.367242	31.629965
593.915220	31888.588319	31.634983
594.951543	31917.673175	31.640000
595.517462	31959.294091	31.645018
595.805838	31995.045764	31.650036
596.591573	32028.771554	31.655053
596.985870	32078.213528	31.660071
597.209959	32117.488743	31.665088
597.889379	32170.602688	31.670106
598.943834	32208.558761	31.675124
599.845376	32233.981356	31.680141
599.965125	32278.131449	31.685159
600.583811	32300.128148	31.690176
601.708037	32334.601235	31.695194
601.588605	32359.204875	31.700212
602.260436	32393.294845	31.705229
602.566448	32431.294417	31.710247
602.983660	32473.708858	31.715264
603.409068	32515.383546	31.720282
603.904642	32578.224718	31.725300
604.747040	32622.924033	31.730317
604.837174	32670.526285	31.735335
605.645798	32714.742467	31.740352
606.553011	32760.740680	31.745370
606.624786	32812.168139	31.750388
607.806352	32848.917210	31.755405
608.615153	32897.687671	31.760423
609.552348	32922.275158	31.765440
610.051633	32964.967039	31.770458
610.355504	33015.670499	31.775476
611.175845	33056.253131	31.780493
611.481929	33105.047169	31.785511
612.045351	33148.141916	31.790528
612.740166	33193.862045	31.795546
612.831364	33252.015784	31.800564
614.034048	33295.386384	31.805581
614.662344	33354.568783	31.810599
615.098467	33397.812176	31.815616
615.895887	33441.968957	31.820634
616.838320	33479.637645	31.825652
617.810021	33510.399354	31.830669
618.644476	33537.492173	31.835687
619.099750	33575.089883	31.840704
619.921261	33607.887833	31.845722
620.366826	33648.684347	31.850740
620.919861	33677.012234	31.855757
620.903874	33728.018669	31.860775
621.420957	33769.232416	31.865792
621.919607	33816.142829	31.870810
622.336171	33870.815415	31.875828
623.512801	33921.614919	31.880845
623.522043	33986.703055	31.885863
624.535905	34038.906803	31.890880
625.162276	34085.395219	31.895898
625.352001	34144.169324	31.900916
625.797187	34184.922932	31.905933
626.547730	34250.756090	31.910951
627.193742	34314.846303	31.915968
627.461650	34376.101072	31.920986
627.840961	34442.131083	31.926004
628.733982	34507.741934	31.931021
629.495168	34571.068481	31.936039
629.761760	34627.924689	31.941056
630.945752	34689.888358	31.946074
631.507590	34739.327888	31.951092
631.936639	34794.641833	31.956109
632.581717	34848.344005	31.961127
633.418472	34908.221714	31.966144
634.232376	34960.976848	31.971162
634.770815	35015.332181	31.976180
635.524974	35069.672813	31.981197
636.092686	35115.517440	31.986215
636.520470	35166.047905	31.991232
637.211039	35206.045314	31.996250
637.936218	35272.476755	32.001268
638.821664	35312.696669	32.006285
639.337869	35366.050018	32.011303
639.993760	35419.253343	32.016320
640.755974	35458.547811	32.021338
641.001284	35524.803573	32.026356
641.818834	35576.092200	32.031373
642.279165	35632.047227	32.036391
642.481168	35686.651590	32.041408
643.834832	35741.093534	32.046426
643.824907	35797.637804	32.051444
644.165595	35857.777236	32.056461
645.213069	35930.285503	32.061479
645.487917	35987.475975	32.066496
646.361072	36045.741456	32.071514
646.981410	36114.302403	32.076532
647.957439	36174.618112	32.081549
649.017293	36238.647388	32.086567
649.535430	36300.004664	32.091584
650.623188	36355.848117	32.096602
650.665243	36425.311039	32.101620
651.349791	36477.884420	32.106637
652.361636	36546.212629	32.111655
652.707950	36594.336855	32.116672
653.802869	36651.682471	32.121690
653.695814	36725.480686	32.126708
654.194844	36776.293818	32.131725
654.811153	36844.766663	32.136743
655.531597	36913.376596	32.141760
656.245765	36976.782720	32.146778
657.044583	37036.733919	32.151796
658.231807	37094.746932	32.156813
659.003737	37144.573681	32.161831
659.658490	37204.266020	32.166848
660.447553	37255.662115	32.171866
661.128674	37308.693027	32.176884
662.476097	37356.190047	32.181901
663.360730	37410.966719	32.186919
663.656646	37458.047542	32.191936
664.198221	37487.967981	32.196954
664.793039	37537.860868	32.201972
665.319917	37592.134332	32.206989
666.396023	37637.475225	32.212007
666.527169	37691.327495	32.217024
667.286035	37737.486897	32.222042
667.911209	37794.847134	32.227060
668.511500	37847.189513	32.232077
669.357104	37897.949546	32.237095
669.915900	37947.407781	32.242112
670.214592	37984.542688	32.247130
670.641618	38040.365593	32.252148
671.138851	38093.982708	32.257165
671.720361	38155.439525	32.262183
672.444608	38212.806193	32.267200
673.347796	38256.514633	32.272218
673.718209	38318.762626	32.277236
674.596692	38367.431698	32.282253
675.466451	38410.284429	32.287271
675.821222	38477.198218	32.292288
676.536070	38526.432400	32.297306
677.205556	38587.275796	32.302324
678.010054	38643.420998	32.307341
678.923155	38705.441587	32.312359
679.207890	38763.109401	32.317376
680.094902	38817.943536	32.322394
680.518542	38882.299411	32.327412
681.364033	38939.887499	32.332429
681.870812	39003.257235	32.337447
682.230824	39066.734411	32.342464
682.761042	39126.918398	32.347482
683.955607	39190.900201	32.352500
684.347017	39262.179742	32.357517
685.182893	39332.606807	32.362535
685.510640	39402.736040	32.367552
686.458305	39472.462585	32.372570
686.735255	39541.628698	32.377588
687.380367	39620.906997	32.382605
688.719610	39691.211314	32.387623
689.648715	39748.601338	32.392640
690.371166	39795.851843	32.397658
691.639368	39851.728709	32.402676
692.700364	39906.627829	32.407693
693.351799	39957.799337	32.412711
694.189725	40019.111097	32.417728
695.115039	40061.648762	32.422746
695.642417	40107.159206	32.427764
696.422701	40151.963450	32.432781
697.075170	40193.269538	32.437799
697.591017	40249.699542	32.442816
698.091109	40292.714691	32.447834
698.628742	40349.428563	32.452852
699.239927	40407.048734	32.457869
700.329610	40465.610027	32.462887
700.495457	40526.312455	32.467904
701.150785	40578.034352	32.472922
701.496354	40648.102098	32.477940
702.404499	40707.595047	32.482957
703.045718	40768.223144	32.487975
703.347994	40836.676219	32.492992
703.915238	40906.646977	32.498010
704.512450	40972.988367	32.503028
704.992773	41042.949269	32.508045
706.066555	41114.778894	32.513063
706.665924	41187.466753	32.518080
707.219961	41232.015578	32.523098
708.073960	41302.216538	32.528116
708.890988	41362.822768	32.533133
709.847756	41414.166993	32.538151
710.499819	41487.702624	32.543168
711.143378	41545.317615	32.548186
711.733583	41602.310458	32.553204
712.441129	41666.374764	32.558221
713.157796	41728.148647	32.563239
713.596505	41808.387263	32.568256
714.398167	41874.712624	32.573274
715.176012	41939.517281	32.578292
715.500309	42020.098458	32.583309
716.269926	42085.214454	32.588327
716.989805	42164.077158	32.593344
717.991147	42227.666807	32.598362
718.451417	42301.187972	32.603380
719.155312	42371.952273	32.608397
720.131916	42441.994427	32.613415
720.523116	42520.460258	32.618432
721.372978	42591.437194	32.623450
722.619508	42674.439721	32.628468
723.272712	42747.768552	32.633485
724.468418	42797.837900	32.638503
725.053909	42867.171887	32.643520
725.611205	42929.769577	32.648538
726.474970	42991.089841	32.653556
727.086907	43073.347138	32.658573
727.931393	43130.755762	32.663591
728.585715	43214.269450	32.668608
729.095884	43277.542625	32.673626
729.736764	43351.497971	32.678644
730.015317	43432.449850	32.683661
730.883059	43497.383424	32.688679
731.761081	43578.602686	32.693696
732.596606	43652.667967	32.698714
733.615749	43736.017269	32.703732
734.267666	43808.807331	32.708749
735.160282	43868.423510	32.713767
736.041562	43947.783911	32.718784
736.755591	44012.919267	32.723802
737.607054	44087.207722	32.728820
738.264695	44156.152004	32.733837
739.131739	44225.733272	32.738855
739.928737	44286.197644	32.743872
740.934958	44343.095958	32.748890
741.472613	44411.209119	32.753908
742.286234	44474.838524	32.758925
743.015909	44524.635467	32.763943
743.740591	44590.806755	32.768960
744.681533	44643.877232	32.773978
745.794534	44697.834163	32.778996
746.431841	44759.858961	32.784013
747.538264	44797.548009	32.789031
748.020722	44844.312379	32.794048
748.839330	44895.152952	32.799066
749.546517	44943.047487	32.804084
750.440687	44990.834325	32.809101
750.779377	45034.680629	32.814119
751.345353	45089.070274	32.819136
751.812598	45146.094907	32.824154
752.119031	45198.798782	32.829172
752.947953	45262.380842	32.834189
754.114277	45335.208659	32.839207
754.289031	45409.731904	32.844224
754.677875	45473.336367	32.849242
755.627435	45533.936486	32.854260
755.915307	45620.378383	32.859277
756.854848	45691.528457	32.864295
757.354445	45771.122931	32.869312
757.761044	45856.825531	32.874330
758.746801	45939.937603	32.879348
759.595084	46016.343738	32.884365
760.218405	46099.967036	32.889383
760.853174	46181.937054	32.894400
761.884443	46270.247313	32.899418
762.954841	46352.914025	32.904436
763.370008	46440.067352	32.909453
764.483291	46524.214943	32.914471
765.238084	46610.076031	32.919488
765.650949	46697.846769	32.924506
766.713151	46771.196901	32.929524
767.730616	46853.742200	32.934541
768.642366	46934.126791	32.939559
769.334865	47014.337674	32.944576
770.262501	47090.519750	32.949594
771.383604	47165.933114	32.954612
771.960233	47246.085857	32.959629
772.888211	47304.961404	32.964647
773.710429	47386.872888	32.969664
774.496242	47459.426575	32.974682
775.299607	47526.845262	32.979700
775.805086	47604.826132	32.984717
776.937507	47687.007911	32.989735
777.580428	47757.695352	32.994752
777.962314	47829.211039	32.999770
778.886775	47898.912738	33.004788
779.473473	47994.754551	33.009805
780.848753	48057.901739	33.014823
781.813317	48132.034974	33.019840
782.738340	48195.635590	33.024858
783.627181	48263.787608	33.029876
784.209093	48343.691341	33.034893
785.160674	48397.815882	33.039911
785.979872	48468.709463	33.044928
786.385444	48544.241321	33.049946
787.032924	48606.478990	33.054964
787.629557	48682.831457	33.059981
788.715359	48750.111293	33.064999
789.607390	48799.869456	33.070016
790.576371	48860.505198	33.075034
791.563739	48920.512588	33.080052
791.864321	48985.249294	33.085069
792.741281	49031.447785	33.090087
793.429067	49093.503239	33.095104
794.190644	49157.611967	33.100122
795.048805	49221.584337	33.105140
795.626843	49289.970092	33.110157
796.729251	49356.510081	33.115175
797.283058	49416.940722	33.120192
797.661146	49499.733222	33.125210
798.362868	49569.210618	33.130228
798.949013	49646.149870	33.135245
799.668381	49725.410345	33.140263
800.487930	49803.093591	33.145280
800.897714	49896.805103	33.150298
801.754959	49984.641014	33.155316
802.618354	50075.496017	33.160333
802.962413	50157.665397	33.165351
803.803783	50256.920969	33.170368
804.389447	50358.640470	33.175386
805.304647	50441.168081	33.180404
806.138907	50543.850463	33.185421
806.962500	50643.963928	33.190439
808.144777	50727.975879	33.195456
808.922485	50816.915803	33.200474
809.839852	50918.461368	33.205492
810.439691	51005.145593	33.210509
811.430129	51097.202921	33.215527
812.666117	51192.131144	33.220544
813.368629	51281.174508	33.225562
815.089968	51348.284988	33.230580
816.443418	51420.948968	33.235597
817.509524	51485.057423	33.240615
818.650884	51545.179213	33.245632
819.028213	51613.032560	33.250650
820.104043	51674.284250	33.255668
820.935955	51752.137402	33.260685
821.724708	51811.467474	33.265703
822.522728	51867.333849	33.270720
823.142925	51942.147130	33.275738
824.182978	52010.242151	33.280756
824.780885	52071.431625	33.285773
825.168629	52136.820934	33.290791
825.924704	52208.857251	33.295808
827.159672	52280.514854	33.300826
828.258597	52334.246022	33.305844
828.937106	52410.434781	33.310861
830.046061	52475.253094	33.315879
831.056600	52528.551337	33.320896
831.704370	52598.478379	33.325914
832.368989	52663.701969	33.330932
833.514881	52725.286128	33.335949
833.775301	52777.487769	33.340967
834.474756	52833.348499	33.345984
835.447124	52903.682268	33.351002
835.703818	52960.093070	33.356020
836.407585	53025.930354	33.361037
837.013621	53093.294704	33.366055
837.738460	53162.452333	33.371072
838.446853	53238.272701	33.376090
839.729409	53308.289407	33.381108
840.930380	53381.163675	33.386125
841.199601	53457.211746	33.391143
842.072618	53521.486285	33.396160
842.322892	53604.621289	33.401178
843.168344	53691.129948	33.406196
843.877140	53775.027511	33.411213
844.548859	53870.899364	33.416231
845.844204	53953.168098	33.421248
846.291779	54043.316511	33.426266
846.993625	54131.519833	33.431284
848.030638	54216.791089	33.436301
848.862105	54311.721483	33.441319
849.804355	54397.869107	33.446336
850.573663	54493.607192	33.451354
851.562670	54578.445900	33.456372
853.103762	54661.692825	33.461389
854.152215	54750.995894	33.466407
855.201487	54823.370651	33.471424
855.783474	54907.901335	33.476442
856.789697	54984.486195	33.481460
857.762523	55066.827417	33.486477
858.847410	55157.042330	33.491495
859.534677	55228.014528	33.496512
859.961009	55314.690498	33.501530
860.152194	55392.888878	33.506548
861.044814	55485.773298	33.511565
861.585882	55591.647500	33.516583
863.154958	55685.826180	33.521600
863.658152	55774.765910	33.526618
864.466230	55871.300189	33.531636
865.257554	55967.755651	33.536653
866.275738	56068.602607	33.541671
867.649710	56155.044075	33.546688
868.109328	56261.649856	33.551706
869.068185	56351.007014	33.556724
870.030832	56450.329769	33.561741
870.782499	56544.595607	33.566759
872.039482	56626.199425	33.571776
873.129367	56730.298314	33.576794
874.154086	56806.583634	33.581812
874.943849	56885.614288	33.586829
875.535085	56975.631229	33.591847
876.484916	57057.586427	33.596864
877.200850	57155.735216	33.601882
878.108130	57249.465804	33.606900
878.758146	57334.393200	33.611917
879.654278	57418.273952	33.616935
880.936423	57500.951372	33.621952
882.146107	57585.449020	33.626970
882.877923	57644.995831	33.631988
883.749147	57727.156807	33.637005
884.223177	57805.436190	33.642023
885.146541	57886.236418	33.647040
886.031174	57964.844252	33.652058
886.918444	58043.148579	33.657076
887.864668	58131.472989	33.662093
888.086363	58214.297026	33.667111
889.050702	58295.053947	33.672128
889.857806	58396.953586	33.677146
890.630635	58494.391269	33.682164
891.912715	58587.716255	33.687181
892.477174	58682.997431	33.692199
893.268714	58769.891145	33.697216
894.297382	58875.319842	33.702234
895.354738	58968.217365	33.707252
896.670963	59053.929023	33.712269
897.885955	59141.782015	33.717287
898.977921	59216.244644	33.722304
899.902652	59302.795484	33.727322
900.610259	59390.654280	33.732340
901.515356	59473.480162	33.737357
902.201624	59567.885032	33.742375
903.365382	59649.466440	33.747392
904.083731	59743.506359	33.752410
904.917165	59827.584774	33.757428
906.747178	59909.539800	33.762445
907.248429	59983.379530	33.767463
908.755097	60060.308778	33.772480
909.453947	60141.466122	33.777498
910.086802	60221.510010	33.782516
911.419596	60295.600337	33.787533
911.876898	60388.942086	33.792551
912.757298	60473.230013	33.797568
913.126506	60564.166799	33.802586
913.909346	60643.409190	33.807604
915.072571	60731.537034	33.812621
915.782948	60834.855982	33.817639
916.938645	60920.147859	33.822656
918.188148	61001.618836	33.827674
918.628147	61099.094327	33.832692
919.619804	61190.824855	33.837709
920.495443	61283.675514	33.842727
921.492024	61378.699275	33.847744
922.287790	61478.005616	33.852762
923.154365	61569.708683	33.857780
924.325452	61666.378972	33.862797
925.157396	61765.699464	33.867815
925.881386	61857.598899	33.872832
927.072618	61947.977490	33.877850
928.055765	62046.432717	33.882868
928.971906	62137.605153	33.887885
929.557298	62229.106450	33.892903
930.320829	62309.686021	33.897920
931.718980	62388.696994	33.902938
932.906641	62465.961695	33.907956
934.125993	62530.161285	33.912973
934.857944	62614.388564	33.917991
935.754994	62681.178702	33.923008
936.684803	62758.602439	33.928026
937.374467	62846.978451	33.933044
938.363105	62917.179904	33.938061
938.988267	63010.182349	33.943079
939.897859	63105.924305	33.948096
940.608045	63211.151617	33.953114
941.169482	63297.345269	33.958132
942.073417	63394.948075	33.963149
942.751469	63501.117957	33.968167
943.597136	63602.233919	33.973184
944.645883	63707.235068	33.978202
945.243648	63814.861650	33.983220
946.419651	63914.753027	33.988237
947.657565	64031.924486	33.993255
948.632890	64134.095530	33.998272
949.796076	64237.575142	34.003290
950.473401	64348.105235	34.008308
951.556711	64443.444259	34.013325
952.973753	64547.406652	34.018343
954.194135	64638.487358	34.023360
955.151132	64739.077666	34.028378
956.065995	64840.763068	34.033396
957.061520	64939.255130	34.038413
957.680263	65046.669492	34.043431
958.509347	65143.382881	34.048448
959.618961	65249.923947	34.053466
960.317034	65359.539089	34.058484
961.672588	65455.961445	34.063501
962.389851	65567.692341	34.068519
963.286291	65686.537376	34.073536
964.183040	65787.851115	34.078554
965.081377	65902.315644	34.083572
966.007027	66014.677070	34.088589
967.106102	66128.450915	34.093607
967.564770	66244.111663	34.098624
968.613056	66349.176671	34.103642
969.738584	66476.117685	34.108660
970.873664	66583.710665	34.113677
971.460906	66705.358379	34.118695
972.705878	66823.359782	34.123712
973.770015	66932.914065	34.128730
974.692000	67046.982397	34.133748
975.504521	67168.290691	34.138765
976.691951	67288.403691	34.143783
977.136466	67396.941013	34.148800
977.965151	67522.073871	34.153818
978.433555	67668.324471	34.158836
979.776784	67787.907773	34.163853
980.684596	67913.086280	34.168871
981.776878	68024.727945	34.173888
982.958346	68140.161402	34.178906
983.628206	68263.593284	34.183924
985.043939	68370.622416	34.188941
985.955703	68489.859883	34.193959
986.428033	68601.907913	34.198976
987.718475	68709.314292	34.203994
989.017304	68832.085296	34.209012
989.822629	68944.615569	34.214029
991.131602	69072.242501	34.219047
991.727185	69191.639185	34.224064
992.768521	69312.212231	34.229082
993.344790	69430.020046	34.234100
994.888278	69558.608809	34.239117
995.695025	69693.161105	34.244135
996.567356	69811.799275	34.249152
997.642150	69934.317726	34.254170
998.126507	70072.051441	34.259188
999.140410	70201.310172	34.264205
1000.229898	70328.046222	34.269223
1001.553176	70470.931755	34.274240
1002.743871	70592.656268	34.279258
1003.643119	70725.890125	34.284276
1004.507215	70850.663180	34.289293
1005.653297	70978.449426	34.294311
1006.972347	71110.013809	34.299328
1008.379656	71226.519166	34.304346
1009.256588	71352.007508	34.309364
1010.206542	71477.016091	34.314381
1011.342286	71600.248133	34.319399
1012.233677	71723.497419	34.324416
1013.630182	71848.747873	34.329434
1014.684774	71969.346082	34.334452
1016.004691	72089.210185	34.339469
1017.067602	72209.093658	34.344487
1018.175895	72319.477273	34.349504
1019.386297	72420.838145	34.354522
1020.332261	72526.652831	34.359540
1021.930587	72632.046426	34.364557
1022.974419	72730.148583	34.369575
1023.992592	72851.263843	34.374592
1025.153942	72932.163306	34.379610
1025.986764	73039.884532	34.384628
1027.128724	73139.521215	34.389645
1028.588118	73234.468106	34.394663
1029.648620	73334.720455	34.399680
1030.993134	73423.198825	34.404698
1032.007946	73521.663666	34.409716
1033.279773	73613.583196	34.414733
1034.058288	73694.848283	34.419751
1034.653204	73795.233052	34.424768
1035.191688	73889.638421	34.429786
1035.903332	73994.621162	34.434804
1036.849416	74102.973319	34.439821
1037.989907	74205.435935	34.444839
1038.809202	74317.321130	34.449856
1039.957352	74412.611014	34.454874
1040.327088	74518.964040	34.459892
1041.606419	74612.847169	34.464909
1043.030315	74709.659700	34.469927
1043.867108	74819.128297	34.474944
1045.091407	74911.598993	34.479962
1046.148416	75004.642674	34.484980
1047.207460	75119.071483	34.489997
1048.027374	75209.885919	34.495015
1048.853447	75317.435976	34.500032
1049.998596	75420.029913	34.505050
1051.032780	75536.160270	34.510068
1051.907769	75639.465624	34.515085
1053.462319	75747.753254	34.520103
1053.784440	75864.557546	34.525120
1055.144088	75984.783903	34.530138
1055.825325	76096.847177	34.535156
1056.927112	76227.448304	34.540173
1057.804356	76353.129505	34.545191
1058.531720	76476.718044	34.550208
1059.211351	76614.655349	34.555226
1060.577803	76747.339559	34.560244
1061.164131	76885.357760	34.565261
1062.654158	77010.792233	34.570279
1063.904163	77154.353547	34.575296
1064.957469	77283.596459	34.580314
1066.418847	77413.757054	34.585332
1067.498885	77539.815020	34.590349
1068.826409	77660.777002	34.595367
1069.848366	77796.107316	34.600384
1071.139119	77915.229816	34.605402
1072.380344	78050.625326	34.610420
1072.893714	78156.502919	34.615437
1074.618706	78280.423965	34.620455
1075.420734	78410.589343	34.625472
1076.233702	78529.961368	34.630490
1077.264551	78660.474890	34.635508
1078.343721	78790.449496	34.640525
1079.523850	78915.201140	34.645543
1080.564770	79044.285435	34.650560
1081.793185	79176.988589	34.655578
1082.884688	79306.932408	34.660596
1083.990668	79438.614220	34.665613
1085.645725	79562.649142	34.670631
1086.414224	79690.448893	34.675648
1087.148207	79809.354029	34.680666
1088.278615	79943.451257	34.685684
1089.020745	80076.736375	34.690701
1089.993936	80218.624715	34.695719
1090.682544	80348.396714	34.700736
1092.057721	80496.354695	34.705754
1093.153241	80647.917079	34.710772
1094.060004	80787.504769	34.715789
1095.181384	80923.728715	34.720807
1096.275731	81066.354433	34.725824
1096.969705	81197.104628	34.730842
1098.325584	81330.513377	34.735860
1099.080451	81468.479909	34.740877
1100.352725	81598.323527	34.745895
1101.005691	81751.291272	34.750912
1102.317858	81885.849568	34.755930
1103.350579	82019.330287	34.760948
1104.369947	82165.835114	34.765965
1105.828819	82301.958801	34.770983
1106.765968	82457.312155	34.776000
1107.946420	82596.825966	34.781018
1109.576337	82734.068123	34.786036
1110.337274	82872.149545	34.791053
1111.844440	83007.142856	34.796071
1113.150273	83151.276422	34.801088
1114.393260	83282.672034	34.806106
1115.837836	83411.237170	34.811124
1116.861019	83540.938171	34.816141
1118.620194	83660.807570	34.821159
1119.652439	83798.626572	34.826176
1120.527087	83925.906406	34.831194
1122.043026	84046.952062	34.836212
1123.170245	84171.912073	34.841229
1124.712155	84285.013394	34.846247
1125.723340	84404.021240	34.851264
1127.147061	84519.415557	34.856282
1128.141726	84642.698628	34.861300
1128.728524	84761.489874	34.866317
1130.017059	84884.072139	34.871335
1130.991892	85016.573816	34.876352
1131.933281	85144.880272	34.881370
1133.273063	85274.897352	34.886388
1134.143017	85399.300464	34.891405
1135.662984	85527.838998	34.896423
1136.399781	85661.460806	34.901440
1137.655761	85781.072832	34.906458
1139.018959	85905.052447	34.911476
1140.323618	86033.820440	34.916493
1141.728331	86149.972718	34.921511
1142.796941	86289.413757	34.926528
1143.559045	86414.030517	34.931546
1145.035887	86536.317012	34.936564
1146.156332	86666.499535	34.941581
1147.344298	86792.918535	34.946599
1148.081293	86927.933343	34.951616
1149.215300	87052.844165	34.956634
1150.283454	87183.829516	34.961652
1151.249051	87322.977834	34.966669
1152.425569	87451.155264	34.971687
1153.172780	87599.215088	34.976704
1154.064235	87742.004773	34.981722
1155.387810	87892.454851	34.986740
1156.499884	88039.125927	34.991757
1157.707063	88172.744588	34.996775
1158.618534	88311.566174	35.001792
1159.847302	88437.695774	35.006810
1161.200109	88564.070608	35.011828
1161.934215	88688.963507	35.016845
1163.121747	88815.583140	35.021863
1164.271834	88959.791418	35.026880
1165.266640	89099.596916	35.031898
1166.813441	89231.910197	35.036916
1168.383180	89372.422620	35.041933
1169.671773	89495.813407	35.046951
1170.729410	89632.035347	35.051968
1172.127104	89771.351712	35.056986
1173.443185	89895.594259	35.062004
1174.212911	90028.880385	35.067021
1175.657409	90159.121312	35.072039
1177.010117	90291.068552	35.077056
1177.933616	90422.596310	35.082074
1179.464035	90552.552481	35.087092
1180.126025	90691.588683	35.092109
1181.435424	90824.451324	35.097127
1182.464517	90952.602985	35.102144
1183.419340	91094.262348	35.107162
1184.886932	91238.113349	35.112180
1185.695676	91390.059484	35.117197
1186.986676	91531.689147	35.122215
1188.275639	91674.414993	35.127232
1189.458827	91814.583631	35.132250
1190.922723	91958.743324	35.137268
1191.978433	92098.669565	35.142285
1193.584823	92235.236196	35.147303
1194.180522	92369.913119	35.152320
1196.074831	92516.755841	35.157338
1198.049119	92650.001955	35.162356
1199.356529	92782.894551	35.167373
1200.465707	92906.345963	35.172391
1201.567870	93034.337743	35.177408
1202.608813	93173.392761	35.182426
1204.087849	93295.200309	35.187444
1205.131180	93421.191230	35.192461
1206.251445	93545.966912	35.197479
1207.400693	93685.512669	35.202496
1208.798372	93816.679917	35.207514
1210.238626	93936.895743	35.212532
1211.285354	94069.922173	35.217549
1212.502132	94197.267321	35.222567
1213.720247	94330.227822	35.227584
1214.520301	94467.482899	35.232602
1215.660581	94594.703911	35.237620
1216.880944	94747.011696	35.242637
1218.133623	94872.765232	35.247655
1219.476975	94998.573514	35.252672
1220.069517	95146.382670	35.257690
1221.557036	95284.803299	35.262708
1222.490703	95434.005435	35.267725
1223.176696	95575.419952	35.272743
1224.158979	95725.951249	35.277760
1224.930980	95873.847916	35.282778
1226.043184	96023.497785	35.287796
1227.318607	96187.953464	35.292813
1228.411759	96329.327837	35.297831
1231.156626	96439.734940	35.302848
1232.679293	96572.344991	35.307866
1234.167260	96703.043433	35.312884
1235.145227	96835.817755	35.317901
1236.290168	96973.546617	35.322919
1237.683121	97105.440955	35.327936
1238.636236	97241.703679	35.332954
1240.124965	97368.765118	35.337972
1240.852432	97520.199086	35.342989
1241.874569	97659.491140	35.348007
1243.048336	97799.220170	35.353024
1244.422479	97943.809647	35.358042
1246.026003	98070.272476	35.363060
1247.526127	98210.682313	35.368077
1249.076514	98363.430269	35.373095
1249.881755	98495.761653	35.378112
1251.510635	98634.068784	35.383130
1252.465431	98767.756202	35.388148
1253.606083	98915.550500	35.393165
1254.605827	99063.046868	35.398183
1255.788920	99209.024803	35.403200
1256.732618	99369.524697	35.408218
1258.324330	99513.591943	35.413236
1259.643011	99660.201377	35.418253
1260.733410	99810.269796	35.423271
1261.999641	99961.948885	35.428288
1263.468055	100124.459434	35.433306
1264.651797	100276.382432	35.438324
1265.789225	100434.658679	35.443341
1266.906948	100595.263040	35.448359
1268.673547	100748.551679	35.453376
1269.596979	100911.135132	35.458394
1270.722736	101074.223179	35.463412
1271.695777	101229.429772	35.468429
1272.637330	101399.434231	35.473447
1274.120985	101569.600281	35.478464
1275.009708	101746.682607	35.483482
1276.182728	101915.067779	35.488500
1277.700641	102096.654557	35.493517
1278.490388	102273.896701	35.498535
1279.800199	102448.822063	35.503552
1281.284204	102641.689837	35.508570
1282.325549	102820.387023	35.513588
1284.056650	102997.130958	35.518605
1285.228968	103183.470378	35.523623
1287.122268	103355.578943	35.528640
1288.440856	103538.438302	35.533658
1289.840298	103704.731779	35.538676
1291.038816	103880.673577	35.543693
1292.660067	104042.029773	35.548711
1294.223116	104190.490926	35.553728
1295.366418	104346.548019	35.558746
1296.474550	104485.475643	35.563764
1297.806319	104632.585654	35.568781
1299.061510	104790.133399	35.573799
1300.380688	104938.767134	35.578816
1301.501773	105093.781157	35.583834
1302.972529	105241.428033	35.588852
1304.434977	105391.724323	35.593869
1305.762539	105545.553025	35.598887
1307.440562	105689.709083	35.603904
1308.631961	105848.616591	35.608922
1309.894835	105998.190479	35.613940
1311.152203	106148.652782	35.618957
1311.875234	106310.315776	35.623975
1313.097653	106481.470075	35.628992
1313.995678	106647.867716	35.634010
1315.307541	106825.848803	35.639028
1316.556210	107002.410546	35.644045
1317.686886	107189.418379	35.649063
1319.149980	107361.917733	35.654080
1320.264177	107545.168790	35.659098
1321.645943	107731.453366	35.664116
1322.828389	107915.581929	35.669133
1324.300245	108111.024663	35.674151
1325.521107	108288.866248	35.679168
1326.728369	108479.860036	35.684186
1328.669765	108654.477165	35.689204
1330.011300	108838.939415	35.694221
1331.468561	109032.503778	35.699239
1332.915950	109197.910907	35.704256
1334.432938	109376.367591	35.709274
1336.239145	109534.659382	35.714292
1338.284646	109708.036624	35.719309
1339.385315	109868.541310	35.724327
1340.714431	110032.200182	35.729344
1342.032813	110200.409728	35.734362
1343.631645	110362.719572	35.739380
1344.981659	110520.474366	35.744397
1346.082304	110694.184219	35.749415
1347.316863	110852.822116	35.754432
1348.611818	111035.406765	35.759450
1349.914082	111202.434307	35.764468
1351.418480	111368.566783	35.769485
1352.555612	111545.708922	35.774503
1353.675740	111717.698876	35.779520
1355.032211	111901.393526	35.784538
1356.606625	112072.864495	35.789556
1358.547274	112223.863949	35.794573
1359.606526	112401.873667	35.799591
1360.950318	112567.179252	35.804608
1362.471833	112741.843342	35.809626
1363.456224	112910.481142	35.814644
1365.099653	113081.072269	35.819661
1365.783533	113257.149872	35.824679
1366.785302	113421.302735	35.829696
1368.178245	113597.235750	35.834714
1369.063507	113769.379807	35.839732
1370.628922	113926.660802	35.844749
1371.677821	114112.614394	35.849767
1372.853604	114289.957227	35.854784
1374.098336	114481.999323	35.859802
1375.326598	114670.890660	35.864820
1377.024916	114850.225449	35.869837
1378.106549	115044.339155	35.874855
1379.776902	115240.177952	35.879872
1380.846889	115435.094536	35.884890
1381.985507	115623.019204	35.889908
1383.602873	115814.917772	35.894925
1384.174788	116024.824316	35.899943
1385.928748	116223.975249	35.904960
1387.239158	116440.613348	35.909978
1388.955673	116647.857678	35.914996
1390.259791	116858.481243	35.920013
1391.650554	117074.121981	35.925031
1393.115618	117273.912465	35.930048
1394.594091	117479.885669	35.935066
1395.972800	117682.190002	35.940084
1398.123457	117882.082732	35.945101
1399.435922	118090.787710	35.950119
1401.320031	118281.769935	35.955136
1402.839624	118481.610044	35.960154
1404.017123	118678.620870	35.965172
1405.666472	118875.691649	35.970189
1407.389152	119067.720381	35.975207
1408.869380	119259.107566	35.980224
1410.219321	119451.836206	35.985242
1411.347840	119648.570440	35.990260
1412.897772	119837.592390	35.995277
1414.339605	120038.292744	36.000295
1415.955723	120239.509548	36.005312
1417.517962	120422.893823	36.010330
1419.206452	120612.074409	36.015348
1420.967292	120785.770301	36.020365
1421.944837	120984.414798	36.025383
1423.670417	121169.549918	36.030400
1425.171179	121359.920617	36.035418
1426.505506	121545.784028	36.040436
1428.062604	121725.463953	36.045453
1429.346356	121921.324839	36.050471
1431.121021	122088.233037	36.055488
1433.204582	122258.460429	36.060506
1434.238740	122433.418178	36.065524
1436.028516	122606.929564	36.070541
1437.235593	122787.169999	36.075559
1439.036066	122946.816524	36.080576
1440.891457	123105.149093	36.085594
1442.134623	123271.115542	36.090612
1443.834122	123430.794573	36.095629
1445.020250	123598.217398	36.100647
1446.204615	123756.427400	36.105664
1447.091623	123904.169588	36.110682
1448.325197	124055.325904	36.115700
1449.938405	124210.727241	36.120717
1451.111656	124372.491126	36.125735
1452.419275	124535.779144	36.130752
1453.480051	124707.944371	36.135770
1454.977296	124883.825548	36.140788
1456.397722	125049.353056	36.145805
1457.576014	125228.674909	36.150823
1458.892586	125406.655964	36.155840
1460.175286	125596.786319	36.160858
1461.452677	125796.424927	36.165876
1462.640173	125984.571322	36.170893
1464.117377	126196.016740	36.175911
1464.956738	126392.476655	36.180928
1466.762289	126593.386235	36.185946
1468.125840	126791.229280	36.190964
1470.288687	126994.044967	36.195981
1471.438215	127198.822633	36.200999
1472.924391	127404.241180	36.206016
1474.836572	127602.426429	36.211034
1476.076656	127808.130571	36.216052
1477.199170	128012.423813	36.221069
1479.284340	128215.057875	36.226087
1480.689363	128414.995576	36.231104
1482.518509	128612.187312	36.236122
1483.722066	128822.962057	36.241140
1486.489897	128998.839111	36.246157
1488.392247	129184.271049	36.251175
1490.002501	129362.782069	36.256192
1491.698973	129537.197532	36.261210
1492.868824	129737.361276	36.266228
1494.337958	129918.701064	36.271245
1495.412483	130105.015269	36.276263
1496.985252	130293.717247	36.281280
1498.155309	130481.449757	36.286298
1499.521837	130690.244037	36.291316
1501.173999	130880.190881	36.296333
1502.589115	131074.185348	36.301351
1503.780031	131279.147004	36.306368
1505.136751	131480.886935	36.311386
1506.033093	131694.496756	36.316404
1507.609218	131910.121441	36.321421
1508.886547	132131.047144	36.326439
1510.673816	132342.214136	36.331456
1512.425914	132558.535617	36.336474
1513.897788	132775.933378	36.341492
1515.122873	132980.646344	36.346509
1516.702846	133199.549746	36.351527
1517.930696	133421.177230	36.356544
1519.763890	133633.967463	36.361562
1520.720970	133871.086127	36.366580
1522.517695	134088.842671	36.371597
1523.811126	134313.469650	36.376615
1524.998347	134534.262107	36.381632
1526.438420	134744.781262	36.386650
1527.932880	134956.674399	36.391668
1529.687000	135166.774802	36.396685
1531.174489	135374.158206	36.401703
1532.833301	135589.146185	36.406720
1534.603805	135799.919737	36.411738
1536.216360	136005.510609	36.416756
1537.954708	136212.425185	36.421773
1539.696942	136424.538785	36.426791
1541.070170	136635.131972	36.431808
1542.160391	136847.435880	36.436826
1544.078877	137071.657401	36.441844
1545.238096	137290.444081	36.446861
1546.757964	137507.027622	36.451879
1548.298479	137734.335909	36.456896
1550.087440	137951.434125	36.461914
1551.517549	138182.961252	36.466932
1553.055913	138400.168598	36.471949
1554.492892	138624.064287	36.476967
1556.120606	138853.292420	36.481984
1558.036407	139074.446309	36.487002
1559.602514	139315.594628	36.492020
1561.408784	139532.205342	36.497037
1563.428749	139749.427537	36.502055
1564.484055	139971.647391	36.507072
1566.482193	140189.827104	36.512090
1567.791108	140429.898614	36.517108
1569.452599	140646.414238	36.522125
1570.817519	140874.267778	36.527143
1572.554061	141103.010265	36.532160
1574.013027	141330.394164	36.537178
1575.408286	141565.475091	36.542196
1577.317103	141788.118376	36.547213
1579.265995	142010.794250	36.552231
1580.598705	142233.868633	36.557248
1582.307369	142461.838464	36.562266
1583.609256	142696.600483	36.567284
1585.203423	142929.665448	36.572301
1586.357760	143158.609612	36.577319
1587.819446	143406.448969	36.582336
1589.360656	143638.766718	36.587354
1590.916616	143889.307159	36.592372
1592.516522	144130.507970	36.597389
1594.312826	144368.354116	36.602407
1595.890560	144618.946626	36.607424
1597.735572	144853.629799	36.612442
1599.476235	145095.941667	36.617460
1601.226253	145333.903523	36.622477
1602.733934	145571.489882	36.627495
1604.412534	145814.070789	36.632512
1606.131008	146046.348261	36.637530
1607.556739	146288.493639	36.642548
1608.979971	146529.157162	36.647565
1610.510344	146755.269459	36.652583
1611.613667	146991.386888	36.657600
1613.481861	147214.425666	36.662618
1614.854811	147445.426678	36.667636
1616.132815	147674.263879	36.672653
1617.775780	147909.508452	36.677671
1619.112397	148147.280160	36.682688
1621.125952	148378.532466	36.687706
1623.315994	148609.908201	36.692724
1625.078629	148846.609459	36.697741
1626.933133	149059.476757	36.702759
1628.318082	149288.736751	36.707776
1629.722864	149525.224457	36.712794
1631.782450	149755.982676	36.717812
1633.344555	149986.852788	36.722829
1635.192799	150214.884873	36.727847
1636.843495	150454.456530	36.732864
1638.707783	150676.793503	36.737882
1640.128804	150917.751872	36.742900
1641.658766	151146.249860	36.747917
1643.618601	151371.136725	36.752935
1645.238440	151603.579556	36.757952
1647.075015	151830.595799	36.762970
1648.616775	152058.665896	36.767988
1650.263069	152302.067844	36.773005
1652.018501	152532.323970	36.778023
1653.577954	152767.384465	36.783040
1654.932138	153006.160104	36.788058
1656.559214	153248.302753	36.793076
1658.000159	153498.102435	36.798093
1660.242832	153722.066528	36.803111
1661.612135	153963.382409	36.808128
1663.654520	154203.075053	36.813146
1665.354864	154445.034916	36.818164
1666.904651	154684.484933	36.823181
1669.039553	154915.501923	36.828199
1670.373068	155162.729953	36.833216
1672.368207	155386.568190	36.838234
1674.210130	155614.480627	36.843252
1676.010694	155849.873348	36.848269
1677.786482	156084.383675	36.853287
1679.113857	156320.507081	36.858304
1680.890567	156550.897035	36.863322
1682.274973	156792.696755	36.868340
1683.984263	157033.046850	36.873357
1686.057413	157265.711696	36.878375
1686.950683	157509.972019	36.883392
1688.636466	157747.742338	36.888410
1690.764819	157995.067310	36.893428
1692.173309	158239.548292	36.898445
1694.337640	158483.431998	36.903463
1695.866883	158733.667637	36.908480
1697.646951	158963.055632	36.913498
1699.799401	159198.026806	36.918516
1700.889349	159444.104489	36.923533
1702.487563	159675.252933	36.928551
1704.554393	159900.828998	36.933568
1706.250199	160117.715673	36.938586
1708.018999	160339.792705	36.943604
1709.342931	160567.339085	36.948621
1711.485594	160774.370845	36.953639
1712.958042	160998.570068	36.958656
1714.443708	161218.441806	36.963674
1716.160746	161439.975217	36.968692
1717.719348	161668.692656	36.973709
1719.049034	161896.092910	36.978727
1720.548605	162135.505908	36.983744
1721.825393	162380.629779	36.988762
1723.813897	162620.926094	36.993780
1725.120044	162875.449427	36.998797
1726.933014	163123.124856	37.003815
1728.695468	163396.465563	37.008832
1730.071801	163653.937761	37.013850
1731.639089	163916.834730	37.018868
1733.451503	164187.025161	37.023885
1735.022710	164450.685954	37.028903
1736.449586	164729.459559	37.033920
1738.308431	165005.902462	37.038938
1740.810378	165271.883175	37.043956
1742.682358	165540.371416	37.048973
1744.502788	165809.187311	37.053991
1746.733220	166077.972744	37.059008
1748.607261	166337.266026	37.064026
1750.099756	166599.772942	37.069044
1751.691258	166872.847102	37.074061
1753.372138	167138.205326	37.079079
1754.667560	167418.997653	37.084096
1756.337346	167709.917147	37.089114
1758.667559	167983.480679	37.094132
1760.034897	168275.673688	37.099149
1762.051593	168546.477160	37.104167
1763.789531	168825.273587	37.109184
1765.178553	169119.980768	37.114202
1766.951918	169410.741005	37.119220
1768.408269	169703.143517	37.124237
1770.366696	169986.947042	37.129255
1772.068920	170280.973474	37.134272
1773.507178	170574.057077	37.139290
1776.181394	170865.294025	37.144308
1777.697618	171157.987203	37.149325
1779.964663	171445.325335	37.154343
1782.275357	171728.101892	37.159360
1783.636606	172013.225302	37.164378
1785.912455	172290.998419	37.169396
1787.822648	172571.132689	37.174413
1790.286161	172832.163323	37.179431
1791.917772	173115.356085	37.184448
1793.697249	173384.806446	37.189466
1795.655880	173649.087846	37.194484
1796.912476	173920.496167	37.199501
1798.197428	174177.471466	37.204519
1800.461267	174439.915477	37.209536
1802.335286	174690.916711	37.214554
1804.138913	174941.652052	37.219572
1805.669639	175205.926153	37.224589
1807.462038	175457.833608	37.229607
1808.932400	175711.396537	37.234624
1810.688332	175969.214297	37.239642
1812.346634	176226.821630	37.244660
1813.659115	176514.187751	37.249677
1815.301507	176801.410219	37.254695
1816.873763	177070.966721	37.259712
1818.998708	177353.350349	37.264730
1820.914778	177622.800175	37.269748
1823.001688	177906.805220	37.274765
1825.127689	178180.042321	37.279783
1826.700489	178475.777007	37.284800
1828.305789	178757.521069	37.289818
1830.771847	179023.698368	37.294836
1832.865229	179305.108043	37.299853
1834.766801	179586.069727	37.304871
1836.752121	179861.332382	37.309888
1838.625661	180132.388995	37.314906
1840.345120	180407.573039	37.319924
1842.383588	180706.756426	37.324941
1844.444749	180966.019132	37.329959
1846.001260	181240.753013	37.334976
1847.485984	181530.795401	37.339994
1849.406833	181810.140804	37.345012
1850.592170	182107.383575	37.350029
1852.160772	182391.069735	37.355047
1854.206528	182702.397416	37.360064
1855.616510	183003.858801	37.365082
1857.764091	183309.765215	37.370100
1859.350989	183623.702533	37.375117
1862.347038	183908.180462	37.380135
1864.515223	184202.550002	37.385152
1866.192533	184504.773470	37.390170
1868.154973	184780.344096	37.395188
1869.883008	185142.082381	37.400205
1871.651095	185447.557614	37.405223
1873.734875	185739.664719	37.410240
1875.403360	186047.216579	37.415258
1877.011212	186338.938469	37.420276
1878.620463	186648.534688	37.425293
1880.934664	186945.876477	37.430311
1883.746067	187234.858187	37.435328
1885.811040	187525.708104	37.440346
1888.387578	187800.731128	37.445364
1890.479157	188087.085515	37.450381
1892.178373	188365.320554	37.455399
1894.508420	188633.052281	37.460416
1896.140215	188904.319453	37.465434
1897.673214	189176.721866	37.470452
1899.276451	189461.186024	37.475469
1900.940110	189729.087397	37.480487
1902.922801	190004.247513	37.485504
1904.335852	190275.228182	37.490522
1906.005228	190538.358910	37.495540
1907.557428	190811.704765	37.500557
1908.980414	191095.991546	37.505575
1910.900302	191365.912806	37.510592
1912.804360	191641.436443	37.515610
1915.036729	191931.644114	37.520628
1917.105822	192215.698526	37.525645
1919.326557	192494.891413	37.530663
1921.162442	192777.414035	37.535680
1922.969810	193064.284580	37.540698
1925.088596	193349.706656	37.545716
1927.139304	193623.449173	37.550733
1928.690813	193912.398534	37.555751
1930.473119	194203.277513	37.560768
1932.193238	194500.541607	37.565786
1933.951875	194789.535604	37.570804
1936.124606	195100.309330	37.575821
1938.124002	195404.817073	37.580839
1940.095167	195703.122788	37.585856
1941.835678	196016.374239	37.590874
1944.055164	196311.136133	37.595892
1945.649173	196628.389316	37.600909
1947.283373	196946.894019	37.605927
1948.974406	197254.979684	37.610944
1951.099562	197584.423601	37.615962
1953.387003	197909.537317	37.620980
1954.758720	198242.579310	37.625997
1956.965024	198563.482103	37.631015
1959.070071	198874.018033	37.636032
1961.249845	199209.732319	37.641050
1963.456330	199524.697521	37.646068
1965.942875	199851.627172	37.651085
1967.564641	200174.110047	37.656103
1969.075237	200487.789184	37.661120
1971.049396	200826.796569	37.666138
1973.369078	201154.712915	37.671156
1975.510286	201478.776015	37.676173
1977.328355	201802.705356	37.681191
1979.942274	202119.021479	37.686208
1981.438695	202456.949950	37.691226
1983.715505	202763.333900	37.696244
1986.262348	203083.182652	37.701261
1987.925238	203409.697593	37.706279
1990.372025	203727.826652	37.711296
1992.434860	204046.886114	37.716314
1994.612668	204349.687333	37.721332
1997.083004	204647.779760	37.726349
1998.697287	204956.952227	37.731367
2000.969735	205264.197601	37.736384
2002.794005	205582.783534	37.741402
2004.814484	205883.243125	37.746420
2007.406057	206171.606910	37.751437
2009.235380	206468.901584	37.756455
2011.811271	206742.261439	37.761472
2013.534217	207017.164846	37.766490
2014.873569	207289.163494	37.771508
2016.605518	207567.216255	37.776525
2018.659087	207857.696967	37.781543
2020.504246	208135.516404	37.786560
2021.811280	208425.847414	37.791578
2023.083156	208725.023256	37.796596
2025.611892	209022.867766	37.801613
2027.377656	209338.392591	37.806631
2029.239143	209648.137240	37.811648
2031.037518	209952.027223	37.816666
2033.455419	210276.231091	37.821684
2035.546603	210591.247677	37.826701
2037.208016	210913.246784	37.831719
2039.082249	211232.417015	37.836736
2041.049567	211564.575656	37.841754
2043.009866	211895.873225	37.846772
2045.041173	212230.944016	37.851789
2047.350183	212578.489332	37.856807
2049.541823	212911.681194	37.861824
2051.406655	213246.860338	37.866842
2053.168709	213582.058257	37.871860
2054.990523	213925.247361	37.876877
2057.178721	214273.784731	37.881895
2059.661307	214630.247896	37.886912
2061.639957	214987.433503	37.891930
2063.790580	215340.324162	37.896948
2066.022706	215687.563798	37.901965
2067.689838	216042.317506	37.906983
2070.286299	216402.221751	37.912000
2072.217631	216744.259076	37.917018
2074.573659	217095.292119	37.922036
2077.103923	217448.684014	37.927053
2078.775498	217790.439063	37.932071
2080.949432	218144.122842	37.937088
2083.457283	218504.278157	37.942106
2085.061714	218854.480486	37.947124
2087.441654	219191.166149	37.952141
2089.645500	219541.674578	37.957159
2092.065297	219894.331510	37.962176
2094.240862	220239.132224	37.967194
2096.559045	220583.503228	37.972212
2098.359993	220922.833094	37.977229
2100.555328	221286.352857	37.982247
2102.937223	221613.901748	37.987264
2105.454249	221968.605863	37.992282
2107.372433	222300.376093	37.997300
2109.585247	222637.608579	38.002317
2112.124725	222985.733411	38.007335
2113.865353	223310.374102	38.012352
2115.979138	223643.206780	38.017370
2118.176712	223975.187833	38.022388
2120.260520	224310.999219	38.027405
2122.267632	224641.033416	38.032423
2124.319928	224942.917468	38.037440
2126.262781	225274.513697	38.042458
2128.275660	225578.818993	38.047476
2130.822572	225876.353409	38.052493
2132.842719	226188.863156	38.057511
2134.964852	226494.752100	38.062528
2137.721333	226794.945169	38.067546
2139.945372	227088.829032	38.072564
2141.789292	227382.880128	38.077581
2143.954423	227693.057090	38.082599
2146.068251	228003.040307	38.087616
2148.133512	228315.216966	38.092634
2149.762592	228635.546332	38.097652
2151.600904	228953.529153	38.102669
2153.661056	229288.493307	38.107687
2155.015173	229620.226027	38.112704
2156.941947	229975.484466	38.117722
2159.035451	230326.219238	38.122740
2161.041178	230670.340131	38.127757
2162.933923	231046.842172	38.132775
2164.791326	231404.274836	38.137792
2166.586609	231767.307196	38.142810
2168.716218	232149.435795	38.147828
2171.294038	232527.068790	38.152845
2173.515030	232909.208903	38.157863
2175.952146	233293.319631	38.162880
2177.854118	233674.372922	38.167898
2180.342119	234063.353736	38.172916
2183.058629	234441.297397	38.177933
2185.016981	234826.839585	38.182951
2187.311331	235202.850260	38.187968
2189.704582	235562.765421	38.192986
2192.357425	235949.334225	38.198004
2195.001994	236320.816471	38.203021
2197.484312	236673.529703	38.208039
2200.131217	237032.235679	38.213056
2203.276835	237375.641179	38.218074
2205.397272	237719.959198	38.223092
2208.440430	238040.394411	38.228109
2211.541978	238365.062273	38.233127
2213.889636	238684.474253	38.238144
2216.458250	239000.876845	38.243162
2218.477885	239314.808112	38.248180
2220.352358	239620.356462	38.253197
2222.428340	239948.478823	38.258215
2224.562429	240266.125918	38.263232
2226.315686	240590.951210	38.268250
2227.989850	240921.455185	38.273268
2230.507398	241238.860122	38.278285
2232.428153	241578.442252	38.283303
2234.629464	241915.665211	38.288320
2236.322182	242245.253168	38.293338
2238.497789	242592.998002	38.298356
2240.636798	242934.297249	38.303373
2242.287369	243272.200242	38.308391
2244.291878	243596.884512	38.313408
2246.703104	243924.751125	38.318426
2248.204881	244272.155856	38.323444
2250.457402	244607.163064	38.328461
2252.070031	244951.755250	38.333479
2254.209153	245306.901534	38.338496
2256.190901	245651.609116	38.343514
2258.136769	246016.391407	38.348532
2260.478926	246380.013968	38.353549
2262.237513	246764.516215	38.358567
2264.343012	247142.634182	38.363584
2266.466331	247518.513979	38.368602
2268.784574	247920.500421	38.373620
2271.176139	248306.521600	38.378637
2272.813430	248710.860605	38.383655
2275.276255	249116.557564	38.388672
2277.491293	249521.560508	38.393690
2279.891443	249935.575585	38.398708
2282.153427	250334.499737	38.403725
2284.762402	250753.738098	38.408743
2287.211186	251167.186793	38.413760
2289.387249	251582.714601	38.418778
2291.596991	252004.536847	38.423796
2294.578042	252405.422248	38.428813
2297.306484	252810.313904	38.433831
2300.324550	253210.456614	38.438848
2303.131079	253604.234031	38.443866
2305.638616	253996.970349	38.448884
2307.796380	254385.117790	38.453901
2310.520568	254787.673701	38.458919
2312.378948	255175.466039	38.463936
2314.368360	255568.367480	38.468954
2316.816658	255973.815905	38.473972
2319.001758	256365.871062	38.478989
2321.379630	256776.005764	38.484007
2324.010581	257184.852441	38.489024
2326.745419	257575.746675	38.494042
2328.549037	257972.236372	38.499060
2330.721709	258364.954059	38.504077
2333.136031	258771.449710	38.509095
2335.562350	259171.058964	38.514112
2338.316250	259568.046398	38.519130
2340.349762	259978.366535	38.524148
2343.064710	260379.145464	38.529165
2345.504805	260779.209145	38.534183
2347.715900	261182.283988	38.539200
2349.669187	261578.747108	38.544218
2352.582692	261981.498275	38.549236
2354.900407	262385.138589	38.554253
2356.817884	262799.389386	38.559271
2359.023273	263193.014215	38.564288
2362.053888	263584.998938	38.569306
2364.110094	263998.437741	38.574324
2366.636147	264390.406568	38.579341
2369.088319	264774.436597	38.584359
2371.624609	265162.008375	38.589376
2373.894211	265524.374886	38.594394
2376.138148	265901.428406	38.599412
2378.027969	266269.168466	38.604429
2380.043086	266655.151479	38.609447
2382.324829	267032.045124	38.614464
2384.942779	267430.397152	38.619482
2386.535692	267826.307509	38.624500
2388.812030	268223.015107	38.629517
2390.723644	268624.179293	38.634535
2392.915284	269033.398613	38.639552
2395.222219	269445.569835	38.644570
2397.563407	269865.634905	38.649588
2400.214179	270291.768520	38.654605
2402.755149	270723.712097	38.659623
2405.345588	271155.138527	38.664640
2407.586671	271571.331704	38.669658
2409.873687	272013.858775	38.674676
2412.338239	272433.289349	38.679693
2415.013252	272863.987336	38.684711
2417.542943	273302.558762	38.689728
2420.049452	273734.681184	38.694746
2422.263565	274182.932446	38.699764
2425.058044	274627.324111	38.704781
2427.405693	275069.987741	38.709799
2429.394425	275508.672912	38.714816
2431.975879	275942.429483	38.719834
2434.093410	276408.728240	38.724852
2436.718924	276854.439740	38.729869
2439.406527	277306.083691	38.734887
2441.495261	277761.918683	38.739904
2444.191686	278225.955105	38.744922
2447.016840	278685.929517	38.749940
2449.395239	279144.378857	38.754957
2452.141895	279606.345716	38.759975
2454.248113	280059.250911	38.764992
2457.155927	280515.802725	38.770010
2459.754095	280974.920993	38.775028
2462.338624	281419.028165	38.780045
2464.829447	281871.989797	38.785063
2467.602764	282313.953971	38.790080
2470.197167	282765.701528	38.795098
2472.658640	283213.914363	38.800116
2475.357395	283660.129462	38.805133
2477.910917	284105.758452	38.810151
2480.446730	284554.183227	38.815168
2483.109660	284996.006116	38.820186
2485.466982	285448.751368	38.825204
2488.237112	285880.900960	38.830221
2490.906143	286319.264219	38.835239
2493.349769	286769.221799	38.840256
2496.014349	287192.139580	38.845274
2498.932190	287627.001651	38.850292
2501.585191	288048.597877	38.855309
2505.003541	288450.986460	38.860327
2507.546539	288835.489408	38.865344
2510.476047	289188.607014	38.870362
2513.356136	289557.225990	38.875380
2515.478257	289916.067517	38.880397
2518.274718	290282.184049	38.885415
2520.125600	290644.549562	38.890432
2522.796060	291007.713679	38.895450
2524.867923	291377.532070	38.900468
2526.979407	291758.391265	38.905485
2529.202551	292134.658254	38.910503
2531.212572	292529.222486	38.915520
2533.729965	292921.692099	38.920538
2535.463879	293324.682473	38.925556
2538.214870	293734.177471	38.930573
2541.654749	294113.379356	38.935591
2544.658652	294510.382787	38.940608
2547.401996	294901.282813	38.945626
2550.585930	295282.962614	38.950644
2552.705717	295673.940983	38.955661
2555.633567	296058.811156	38.960679
2557.594017	296459.744586	38.965696
2560.499156	296852.946322	38.970714
2562.683126	297255.794088	38.975732
2564.610338	297667.090866	38.980749
2566.901882	298074.209217	38.985767
2568.909599	298513.147027	38.990784
2571.241816	298928.813935	38.995802
2573.855323	299373.587374	39.000820
2575.719433	299811.121575	39.005837
2578.212107	300255.886148	39.010855
2580.543778	300727.622551	39.015872
2582.785425	301180.603513	39.020890
2585.557903	301654.291603	39.025908
2587.445746	302128.763340	39.030925
2590.292061	302607.563966	39.035943
2592.456837	303101.487845	39.040960
2594.874379	303593.334041	39.045978
2597.739646	304099.957733	39.050996
2600.047194	304596.566127	39.056013
2602.916085	305095.742260	39.061031
2605.125354	305606.380091	39.066048
2608.240108	306105.000286	39.071066
2611.099669	306616.765149	39.076084
2614.207975	307120.154636	39.081101
2616.913232	307612.055082	39.086119
2619.895786	308115.942347	39.091136
2622.522437	308608.916672	39.096154
2625.474099	309106.352613	39.101172
2627.961160	309592.259486	39.106189
2630.894227	310080.144018	39.111207
2633.184052	310580.578526	39.116224
2636.198400	311072.226541	39.121242
2639.516073	311543.453620	39.126260
2642.248684	312030.039318	39.131277
2645.515226	312491.822647	39.136295
2647.769650	312940.342937	39.141312
2650.447499	313375.735972	39.146330
2653.209464	313807.937864	39.151348
2655.174513	314247.865820	39.156365
2658.266748	314686.912805	39.161383
2660.267075	315130.485794	39.166400
2662.842780	315575.887459	39.171418
2665.761800	316024.680938	39.176436
2668.138423	316477.474569	39.181453
2670.433516	316936.779465	39.186471
2672.832958	317406.118552	39.191488
2675.050094	317876.932837	39.196506
2677.474242	318358.017329	39.201524
2679.812150	318853.230575	39.206541
2682.201027	319340.585551	39.211559
2684.864420	319842.185000	39.216576
2687.009061	320359.306706	39.221594
2690.080678	320868.445577	39.226612
2692.765430	321388.259591	39.231629
2696.034397	321900.276312	39.236647
2698.822775	322412.726430	39.241664
2701.547401	322941.838774	39.246682
2704.568116	323453.224981	39.251700
2707.065705	323967.412945	39.256717
2710.362703	324467.699135	39.261735
2712.878510	324982.611625	39.266752
2715.558886	325498.811756	39.271770
2718.424399	326012.360762	39.276788
2721.580882	326536.721650	39.281805
2724.839427	327043.898218	39.286823
2727.276226	327565.656321	39.291840
2730.031492	328075.194722	39.296858
2732.701699	328589.439737	39.301876
2736.090210	329105.131331	39.306893
2739.314564	329602.364748	39.311911
2741.871119	330106.968388	39.316928
2745.181416	330608.138433	39.321946
2748.267339	331094.262981	39.326964
2750.735138	331602.345996	39.331981
2753.809232	332099.430270	39.336999
2756.590065	332590.873779	39.342016
2759.119470	333095.251373	39.347034
2762.054454	333585.770932	39.352052
2764.832855	334088.091163	39.357069
2767.630484	334582.254941	39.362087
2770.042388	335064.194055	39.367104
2773.022498	335545.955458	39.372122
2776.040724	336039.560021	39.377140
2778.464412	336540.140334	39.382157
2781.396202	337025.195964	39.387175
2784.190717	337528.419190	39.392192
2787.106627	338021.006705	39.397210
2789.919422	338523.912252	39.402228
2792.234927	339027.506867	39.407245
2795.455875	339500.534143	39.412263
2798.275939	339960.731493	39.417280
2801.001073	340427.742957	39.422298
2803.983601	340872.700478	39.427316
2805.911428	341338.468835	39.432333
2808.661369	341791.757194	39.437351
2811.207410	342271.421011	39.442368
2813.718233	342744.385645	39.447386
2816.389747	343222.064146	39.452404
2818.720394	343721.318007	39.457421
2821.469510	344220.444283	39.462439
2823.598955	344720.457844	39.467456
2826.258811	345237.455336	39.472474
2828.859301	345745.117856	39.477492
2831.396350	346281.056972	39.482509
2834.225407	346808.362129	39.487527
2837.180389	347350.637818	39.492544
2839.791250	347884.362841	39.497562
2842.549659	348424.121392	39.502580
2845.197714	348992.567947	39.507597
2848.271943	349542.358839	39.512615
2850.904963	350106.504963	39.517632
2853.868158	350670.866509	39.522650
2857.368713	351223.227820	39.527668
2860.577224	351778.397834	39.532685
2863.895377	352338.084003	39.537703
2867.222261	352887.890668	39.542720
2870.243812	353442.284328	39.547738
2873.415596	353991.570263	39.552756
2876.414389	354531.667988	39.557773
2880.138501	355058.643741	39.562791
2882.929114	355596.910938	39.567808
2885.513328	356143.173314	39.572826
2888.794396	356670.026530	39.577844
2891.965421	357218.762216	39.582861
2894.386347	357743.185922	39.587879
2897.544621	358280.771291	39.592896
2900.387818	358825.456357	39.597914
2903.296625	359355.940702	39.602932
2905.945481	359910.183395	39.607949
2908.717199	360440.981051	39.612967
2911.748710	360986.213060	39.617984
2914.426519	361530.863659	39.623002
2918.029390	362074.080138	39.628020
2920.871581	362619.727454	39.633037
2923.599501	363171.398752	39.638055
2926.706275	363704.555125	39.643072
2929.377837	364259.391260	39.648090
2932.422020	364791.223959	39.653108
2935.532595	365348.404301	39.658125
2938.961398	365880.866117	39.663143
2942.089288	366416.872210	39.668160
2945.325004	366953.410172	39.673178
2949.070253	367459.237683	39.678196
2952.090685	367996.329892	39.683213
2954.493488	368494.027488	39.688231
2957.830513	368977.202656	39.693248
2960.422730	369449.998070	39.698266
2963.560009	369921.654273	39.703284
2966.241329	370395.842390	39.708301
2968.927717	370872.153821	39.713319
2971.760979	371347.419298	39.718336
2974.474375	371849.785468	39.723354
2977.080254	372348.206453	39.728372
2979.865724	372852.955365	39.733389
2982.175937	373352.249524	39.738407
2985.065732	373871.675199	39.743424
2987.318817	374408.979312	39.748442
2990.299690	374938.669624	39.753460
2993.016990	375488.988569	39.758477
2995.902181	376020.402962	39.763495
2999.451315	376562.828030	39.768512
3001.909862	377126.934397	39.773530
3005.348810	377671.186304	39.778548
3008.460954	378221.697756	39.783565
3011.200549	378783.015092	39.788583
3014.170731	379348.416670	39.793600
3016.597171	379923.080354	39.798618
3019.917296	380507.824989	39.803636
3022.396459	381095.720126	39.808653
3025.428754	381684.169416	39.813671
3028.805792	382275.946623	39.818688
3031.453154	382877.446701	39.823706
3034.292288	383476.646357	39.828724
3037.787362	384078.435502	39.833741
3040.848269	384686.955102	39.838759
3043.872521	385288.953903	39.843776
3047.025667	385900.223134	39.848794
3050.228968	386517.226541	39.853812
3053.787109	387126.729544	39.858829
3056.636281	387735.530537	39.863847
3059.869930	388345.318571	39.868864
3062.818233	388961.683283	39.873882
3066.145539	389582.001259	39.878900
3069.108771	390187.616455	39.883917
3072.204008	390815.021019	39.888935
3075.375087	391431.323124	39.893952
3078.416137	392053.211004	39.898970
3081.255900	392674.207938	39.903988
3084.484589	393303.818907	39.909005
3087.622331	393938.551686	39.914023
3090.600844	394562.552176	39.919040
3093.406674	395203.168942	39.924058
3096.213544	395829.630172	39.929076
3100.047950	396468.066790	39.934093
3103.147804	397092.347389	39.939111
3106.673816	397717.783443	39.944128
3110.132676	398340.860689	39.949146
3113.633140	398950.208229	39.954164
3116.939970	399561.805723	39.959181
3119.769824	400167.896918	39.964199
3123.209899	400740.322590	39.969216
3125.904032	401308.531231	39.974234
3129.004746	401878.229853	39.979252
3132.531045	402437.379956	39.984269
3135.976778	402989.311665	39.989287
3139.364258	403548.919170	39.994304
3142.335007	404100.631157	39.999322
3145.608412	404660.843636	40.004340
3148.778562	405219.288889	40.009357
3151.659666	405778.329444	40.014375
3154.872078	406341.937955	40.019392
3157.760671	406903.766085	40.024410
3160.800016	407474.676452	40.029428
3163.566426	408056.159386	40.034445
3166.224510	408633.772515	40.039463
3169.804678	409228.339254	40.044480
3172.882582	409833.262542	40.049498
3175.901485	410425.036023	40.054516
3178.638345	411022.796730	40.059533
3181.449182	411647.404698	40.064551
3184.645340	412255.570161	40.069568
3187.613878	412887.947835	40.074586
3190.626639	413517.238033	40.079604
3193.672225	414156.004560	40.084621
3196.575379	414800.984284	40.089639
3199.981039	415453.915221	40.094656
3202.955198	416108.929088	40.099674
3206.078505	416758.304136	40.104692
3209.566645	417413.120584	40.109709
3212.660913	418081.357368	40.114727
3216.514344	418744.154535	40.119744
3220.039553	419395.140078	40.124762
3222.969310	420048.818276	40.129780
3226.788452	420698.807949	40.134797
3230.443599	421357.796687	40.139815
3233.936550	422000.946355	40.144832
3237.365234	422642.976153	40.149850
3241.053468	423286.970077	40.154868
3244.780560	423920.307547	40.159885
3247.751505	424565.909002	40.164903
3251.278260	425199.854732	40.169920
3254.716592	425843.924475	40.174938
3257.780168	426481.560665	40.179956
3261.186354	427110.211214	40.184973
3264.130453	427753.098802	40.189991
3267.850033	428378.169153	40.195008
3271.209546	429006.372333	40.200026
3274.459157	429645.207695	40.205044
3278.043491	430261.392527	40.210061
3281.401528	430875.423178	40.215079
3285.045281	431493.792402	40.220096
3288.633894	432116.203698	40.225114
3291.552771	432742.356736	40.230132
3295.124209	433355.424626	40.235149
3297.922973	433966.786082	40.240167
3301.294050	434531.472897	40.245184
3304.164595	435112.577573	40.250202
3307.223672	435685.538085	40.255220
3310.779876	436258.348567	40.260237
3313.590619	436840.937186	40.265255
3317.283614	437426.446796	40.270272
3320.190312	438006.205589	40.275290
3322.976342	438595.938162	40.280308
3326.161986	439184.271281	40.285325
3328.924344	439788.902859	40.290343
3332.344399	440393.506762	40.295360
3335.339389	441030.749601	40.300378
3338.371774	441654.661544	40.305396
3341.681144	442287.159563	40.310413
3344.645400	442933.205741	40.315431
3348.127481	443581.876055	40.320448
3351.127953	444241.839508	40.325466
3353.942482	444899.133473	40.330484
3357.469391	445573.838332	40.335501
3360.476667	446268.641279	40.340519
3363.542325	446952.789663	40.345536
3367.319718	447636.541576	40.350554
3370.813387	448343.534893	40.355572
3374.559160	449023.757453	40.360589
3378.153667	449717.385958	40.365607
3381.708189	450405.384762	40.370624
3384.995424	451088.096576	40.375642
3388.562374	451784.492994	40.380660
3392.501270	452491.118216	40.385677
3395.733323	453188.839244	40.390695
3399.382865	453875.594046	40.395712
3403.105668	454568.229090	40.400730
3406.537852	455263.569954	40.405748
3410.352219	455945.221456	40.410765
3413.399022	456635.373572	40.415783
3416.803800	457330.951507	40.420800
3420.740627	458014.130009	40.425818
3424.364963	458707.752277	40.430836
3428.308127	459402.104821	40.435853
3431.373802	460088.596334	40.440871
3435.316953	460770.870530	40.445888
3438.825525	461449.455060	40.450906
3442.191632	462141.030134	40.455924
3445.765561	462815.159131	40.460941
3449.210358	463493.784983	40.465959
3452.263477	464190.496118	40.470976
3456.032160	464873.415369	40.475994
3459.229442	465569.547015	40.481012
3462.711468	466248.171250	40.486029
3465.963494	466942.576387	40.491047
3469.578539	467625.828583	40.496064
3473.061261	468327.824464	40.501082
3476.448750	469020.008858	40.506100
3479.591888	469710.643514	40.511117
3483.337587	470389.378317	40.516122
3486.280222	471038.155988	40.521127
3489.977490	471624.384962	40.526132
3492.557068	472175.891456	40.531136
3495.962109	472654.110102	40.536141
3498.191472	473081.975152	40.541146
3501.077747	473449.555102	40.546151
3503.517249	473779.020387	40.551156
3505.929408	474054.704064	40.556160
3508.325002	474262.883194	40.561165
3510.361441	474442.712446	40.566170
3512.058218	474550.284996	40.571175
3513.546664	474632.269075	40.576180
3514.393484	474682.206569	40.581184
3515.924747	474688.578823	40.586189
3516.640639	474678.835161	40.591194
3517.430683	474626.238113	40.596199
3518.172050	474555.064577	40.601204
3518.512556	474457.981083	40.606208
3519.230529	474350.805921	40.611213
3519.678460	474215.267046	40.616218
3519.743478	474071.639406	40.621223
3520.241414	473920.695058	40.626228
3520.490642	473755.713594	40.631232
3520.285982	473577.945084	40.636237
3520.449825	473396.820190	40.641242
3520.378754	473202.617089	40.646247
3520.359795	473006.782471	40.651252
3520.489710	472812.135837	40.656256
3520.747160	472599.132017	40.661261
3520.238855	472392.688470	40.666266
3519.919109	472180.487466	40.671271
3520.020420	471971.757415	40.676276
3519.422811	471771.754360	40.681280
3519.442417	471555.335283	40.686285
3519.495624	471341.187142	40.691290
3519.395767	471123.719882	40.696295
3519.445257	470908.351879	40.701300
3519.063099	470694.473311	40.706304
3518.730445	470471.821336	40.711309
3518.799218	470260.190771	40.716314
3518.138263	470046.555066	40.721319
3518.134893	469840.807710	40.726324
3517.812235	469635.315245	40.731328
3517.503235	469423.486562	40.736333
3517.331088	469227.790712	40.741338
3517.132025	469021.004144	40.746343
3517.042064	468819.870044	40.751348
3516.604554	468638.650071	40.756352
3516.552201	468440.240928	40.761357
3516.306882	468240.900195	40.766362
3515.704391	468059.095002	40.771367
3515.437766	467882.904355	40.776372
3515.048712	467708.860617	40.781376
3515.329744	467518.844831	40.786381
3514.957029	467355.281358	40.791386
3514.741122	467186.421157	40.796391
3514.254150	467013.603638	40.801396
3513.889345	466860.571801	40.806400
3514.210781	466687.309354	40.811405
3513.625544	466531.576864	40.816410
3513.253637	466386.698874	40.821415
3513.574998	466234.102165	40.826420
3513.130259	466086.042660	40.831424
3513.078546	465935.280460	40.836429
3512.526481	465790.631399	40.841434
3512.497671	465654.757979	40.846439
3512.216062	465516.292260	40.851444
3511.974267	465392.865943	40.856448
3512.244873	465254.202733	40.861453
3512.115426	465116.822788	40.866458
3511.325393	464997.034080	40.871463
3511.258482	464875.499872	40.876468
3511.116701	464759.094912	40.881472
3511.272847	464630.731896	40.886477
3510.862205	464516.499355	40.891482
3510.777779	464396.383793	40.896487
3510.796976	464288.257833	40.901492
3510.202795	464198.628148	40.906496
3509.925945	464077.428796	40.911501
3509.979985	463973.601863	40.916506
3509.680302	463880.475030	40.921511
3509.815768	463783.118666	40.926516
3509.670208	463694.626095	40.931520
3509.683068	463596.428372	40.936525
3509.224754	463515.284668	40.941530
3508.943545	463416.680231	40.946535
3509.274954	463324.861724	40.951540
3508.814352	463244.578662	40.956544
3508.840885	463156.003597	40.961549
3508.727864	463072.366947	40.966554
3508.459543	463005.781630	40.971559
3508.428930	462925.170488	40.976564
3508.214151	462852.495065	40.981568
3508.506615	462771.726787	40.986573
3507.950602	462710.408673	40.991578
3507.936678	462631.262929	40.996583
3508.094901	462553.252912	41.001588
3507.893403	462494.711184	41.006592
3507.461452	462432.357588	41.011597
3507.641879	462358.548750	41.016602
3507.648225	462298.602811	41.021607
3507.568326	462232.641431	41.026612
3507.177712	462176.816669	41.031616
3507.676632	462104.574010	41.036621
3507.331935	462040.836115	41.041626
3507.334181	461985.146420	41.046631
3507.366030	461921.141153	41.051636
3506.944341	461868.361197	41.056640
3507.112489	461813.808171	41.061645
3506.876548	461767.330379	41.066650
3506.732292	461715.364089	41.071655
3506.953842	461658.521209	41.076660
3506.710023	461616.148968	41.081664
3506.727323	461568.968709	41.086669
3506.628246	461518.362379	41.091674
3506.380636	461468.034651	41.096679
3506.558443	461415.809884	41.101684
3506.348664	461384.174267	41.106688
3506.747277	461331.455506	41.111693
3506.613054	461285.820677	41.116698
3506.504043	461239.826714	41.121703
3506.684874	461196.722293	41.126708
3506.613174	461160.096610	41.131712
3506.566563	461103.399269	41.136717
3506.314589	461062.294107	41.141722
3506.237008	461015.331427	41.146727
3506.144506	460967.813754	41.151732
3506.177529	460933.348811	41.156736
3506.014196	460886.147088	41.161741
3506.073569	460849.599801	41.166746
3506.479719	460807.317547	41.171751
3506.352455	460766.798585	41.176756
3506.195829	460727.703482	41.181760
3506.300743	460674.678388	41.186765
3506.650638	460632.810777	41.191770
3506.124442	460591.903487	41.196775
3506.313719	460549.049596	41.201780
3506.071420	460521.016179	41.206784
3505.846504	460476.104437	41.211789
3505.861345	460448.635131	41.216794
3505.821474	460413.370902	41.221799
3505.840737	460375.613346	41.226804
3505.443805	460338.180166	41.231808
3505.612573	460306.174127	41.236813
3505.890801	460276.328465	41.241818
3505.932180	460238.009422	41.246823
3505.958489	460201.973359	41.251828
3505.882916	460172.846757	41.256832
3505.848266	460131.955942	41.261837
3505.716307	460095.287901	41.266842
3505.667243	460057.642762	41.271847
3505.958861	460018.925825	41.276852
3505.518607	459990.368001	41.281856
3505.643658	459959.027680	41.286861
3505.749816	459931.846135	41.291866
3505.325789	459901.866428	41.296871
3505.546656	459866.607386	41.301876
3505.450688	459840.980576	41.306880
3505.467988	459807.175178	41.311885
3505.509656	459775.595414	41.316890
3505.329769	459748.259746	41.321895
3505.500728	459720.762777	41.326900
3505.359404	459693.065699	41.331904
3505.462230	459663.755854	41.336909
3505.456339	459627.572211	41.341914
3505.540936	459596.846373	41.346919
3505.610185	459567.846194	41.351924
3505.174378	459543.645358	41.356928
3505.393685	459508.791382	41.361933
3505.472407	459485.009412	41.366938
3505.225714	459463.310146	41.371943
3505.235614	459431.583223	41.376948
3505.075991	459408.450010	41.381952
3505.200313	459385.065570	41.386957
3504.950553	459368.992141	41.391962
3504.826837	459338.757589	41.396967
3505.065832	459323.006106	41.401972
3505.226031	459297.132138	41.406976
3505.343792	459279.120736	41.411981
3505.417476	459255.795470	41.416986
3505.288544	459220.088215	41.421991
3505.412676	459187.530522	41.426996
3505.036960	459171.782519	41.432000
3505.494610	459149.658568	41.437005
3505.470961	459111.348460	41.442010
3505.655302	459086.737100	41.447015
3505.599682	459059.024506	41.452020
3505.420406	459024.237741	41.457024
3505.131603	458985.111098	41.462029
3505.138838	458958.401241	41.467034
3504.992016	458940.992197	41.472039
3504.929150	458917.081684	41.477044
3504.800127	458890.648405	41.482048
3505.165475	458869.401477	41.487053
3505.278085	458848.755169	41.492058
3504.828530	458822.224486	41.497063
3505.351632	458801.406677	41.502068
3504.754992	458787.317881	41.507072
3504.968386	458765.336574	41.512077
3504.781365	458742.612715	41.517082
3504.653418	458721.399176	41.522087
3504.828587	458703.833584	41.527092
3504.672088	458694.889729	41.532096
3504.974272	458674.413597	41.537101
3504.740033	458648.200687	41.542106
3504.835455	458634.348385	41.547111
3504.554602	458600.794578	41.552116
3504.698776	458599.198827	41.557120
3505.030296	458570.811276	41.562125
3504.950400	458552.478199	41.567130
3504.532529	458536.990300	41.572135
3504.960284	458514.161211	41.577140
3504.821309	458505.417005	41.582144
3504.743322	458481.255145	41.587149
3504.798722	458457.577298	41.592154
3504.798955	458445.717708	41.597159
3505.026200	458415.472516	41.602164
3504.643034	458386.547870	41.607168
3504.739458	458374.114312	41.612173
3504.705938	458348.474921	41.617178
3504.106232	458355.672795	41.622183
3504.939141	458320.205157	41.627188
3504.747225	458314.358789	41.632192
3504.457141	458291.854743	41.637197
3504.903257	458275.458886	41.642202
3504.456301	458257.390941	41.647207
3504.613118	458239.574665	41.652212
3504.613805	458244.642770	41.657216
3504.617875	458220.770679	41.662221
3504.627400	458203.638391	41.667226
3504.259041	458185.556961	41.672231
3504.966886	458168.964281	41.677236
3504.474301	458155.110683	41.682240
3504.614565	458140.844923	41.687245
3504.774931	458114.715985	41.692250
3504.759695	458105.088871	41.697255
3504.723081	458081.527657	41.702260
3504.583939	458078.257027	41.707264
3504.444736	458048.327264	41.712269
3504.963577	458038.203465	41.717274
3504.619933	458014.643913	41.722279
3505.200474	457986.719847	41.727284
3505.329178	457979.855659	41.732288
3505.313154	457948.586958	41.737293
3505.363633	457922.577899	41.742298
3505.175786	457894.582172	41.747303
3505.311533	457869.217367	41.752308
3504.998310	457831.207669	41.757312
3504.803098	457802.300770	41.762317
3505.274785	457784.024860	41.767322
3504.595349	457758.697737	41.772327
3504.895553	457739.589447	41.777332
3505.003703	457729.941086	41.782336
3504.713190	457707.436457	41.787341
3504.903582	457679.527898	41.792346
3504.859714	457661.086487	41.797351
3505.035609	457636.221371	41.802356
3504.649344	457636.135262	41.807360
3504.850013	457607.008435	41.812365
3504.674170	457587.575812	41.817370
3504.338116	457576.330652	41.822375
3504.644790	457558.184081	41.827380
3504.713946	457530.954909	41.832384
3504.527116	457517.403451	41.837389
3504.709495	457493.804156	41.842394
3504.406116	457488.838209	41.847399
3504.619784	457462.851376	41.852404
3504.426525	457452.189976	41.857408
3504.360051	457425.592032	41.862413
3504.600209	457416.883984	41.867418
3504.374528	457414.895132	41.872423
3504.792053	457388.315867	41.877428
3504.388875	457373.077979	41.882432
3504.344132	457354.332329	41.887437
3504.513722	457338.692510	41.892442
3504.524345	457333.926333	41.897447
3504.376879	457298.573610	41.902452
3504.347409	457302.684093	41.907456
3504.537509	457281.414726	41.912461
3504.741137	457266.073148	41.917466
3504.197193	457254.356456	41.922471
3504.393513	457231.818854	41.927476
3504.379939	457223.914320	41.932480
3504.345361	457200.858575	41.937485
3504.426455	457197.296772	41.942490
3504.291056	457189.007546	41.947495
3504.733150	457171.851205	41.952500
3504.425095	457154.721564	41.957504
3504.335410	457141.761486	41.962509
3504.435016	457118.632051	41.967514
3504.529830	457122.011757	41.972519
3504.366834	457093.554505	41.977524
3504.444384	457092.426178	41.982528
3504.272904	457077.148505	41.987533
3504.435305	457059.026119	41.992538
3504.278184	457054.288518	41.997543
3504.548166	457031.383318	42.002548
3504.512843	457028.703014	42.007552
3504.213803	457003.462042	42.012557
3504.581829	456987.940127	42.017562
3504.050058	456986.814462	42.022567
3504.274943	456967.971730	42.027572
3504.225710	456946.894932	42.032576
3504.537034	456947.145878	42.037581
3504.322054	456927.313816	42.042586
3504.332083	456922.142157	42.047591
3504.508029	456907.311890	42.052596
3504.268038	456889.815602	42.057600
3504.284475	456885.048326	42.062605
3504.388676	456863.438386	42.067610
3504.273218	456850.381150	42.072615
3504.373854	456839.719930	42.077620
3504.430963	456820.956393	42.082624
3504.417001	456806.462593	42.087629
3504.573065	456797.616581	42.092634
3504.478108	456775.026832	42.097639
3504.498078	456766.862962	42.102644
3504.274075	456748.958333	42.107648
3504.226376	456738.930620	42.112653
3504.412255	456722.425880	42.117658
3504.431121	456715.934820	42.122663
3504.513350	456695.646293	42.127668
3504.515452	456674.104270	42.132672
3504.288018	456669.226524	42.137677
3504.414180	456660.993793	42.142682
3504.069291	456638.345194	42.147687
3504.585609	456618.337274	42.152692
3504.269580	456615.248667	42.157696
3504.354096	456599.977608	42.162701
3504.394157	456589.427972	42.167706
3504.278908	456574.748554	42.172711
3504.388240	456553.847019	42.177716
3504.024751	456554.162506	42.182720
3504.242562	456540.490613	42.187725
3504.436263	456528.444799	42.192730
3504.210057	456525.949081	42.197735
3504.579503	456503.381107	42.202740
3504.395867	456498.039661	42.207744
3504.185976	456493.006817	42.212749
3504.376259	456466.566516	42.217754
3504.310229	456463.435199	42.222759
3504.171171	456449.925552	42.227764
3504.572193	456426.490425	42.232768
3504.497261	456419.559104	42.237773
3504.979682	456400.671870	42.242778
3504.559661	456395.624194	42.247783
3504.968901	456366.916150	42.252788
3504.480360	456348.245342	42.257792
3503.937780	456333.486653	42.262797
3504.267386	456311.584201	42.267802
3504.255384	456301.296740	42.272807
3504.375830	456283.130136	42.277812
3504.321777	456272.292281	42.282816
3504.158124	456273.536708	42.287821
3504.396297	456241.410961	42.292826
3503.929934	456243.619449	42.297831
3504.333622	456227.888113	42.302836
3504.559971	456208.132051	42.307840
3503.970559	456199.413064	42.312845
3504.559388	456195.460267	42.317850
3504.093897	456180.688303	42.322855
3504.353746	456159.760661	42.327860
3504.602119	456163.722559	42.332864
3504.211241	456134.745303	42.337869
3504.411057	456122.242016	42.342874
3504.221055	456120.348317	42.347879
3504.648887	456087.936504	42.352884
3503.960017	456080.501641	42.357888
3504.236800	456084.154578	42.362893
3504.212180	456060.690330	42.367898
3504.258514	456055.968442	42.372903
3503.760931	456042.519740	42.377908
3504.119271	456015.898092	42.382912
3503.763964	456008.710375	42.387917
3504.189001	456008.587104	42.392922
3504.026829	456019.005809	42.397927
3504.163714	455997.135924	42.402932
3504.257004	455979.987445	42.407936
3504.274547	455983.329848	42.412941
3504.516223	455970.363128	42.417946
3504.108356	455963.539186	42.422951
3504.063917	455941.396074	42.427956
3504.183248	455936.661694	42.432960
3504.057223	455926.241447	42.437965
3503.826176	455919.336611	42.442970
3503.773062	455929.584675	42.447975
3503.915216	455922.565429	42.452980
3503.842966	455905.698594	42.457984
3503.801306	455894.351538	42.462989
3504.184874	455880.397457	42.467994
3504.090513	455885.938578	42.472999
3503.945607	455877.701125	42.478004
3503.998382	455860.610151	42.483008
3503.926625	455857.023523	42.488013
3504.029824	455844.435186	42.493018
3503.726087	455856.652237	42.498023
3504.068496	455847.317798	42.503028
3504.015813	455832.120275	42.508032
3503.808286	455825.464833	42.513037
3504.018785	455817.977685	42.518042
3503.887129	455822.612800	42.523047
3504.039757	455802.007227	42.528052
3503.801137	455795.813280	42.533056
3503.914753	455783.425880	42.538061
3504.467619	455782.419077	42.543066
3504.153807	455779.887535	42.548071
3503.761498	455754.711617	42.553076
3504.393919	455758.760086	42.558080
3503.956200	455760.304783	42.563085
3504.104099	455738.382051	42.568090
3504.251828	455737.596488	42.573095
3504.217647	455719.810602	42.578100
3504.114734	455716.127892	42.583104
3504.294791	455695.720283	42.588109
3504.433111	455687.333015	42.593114
3504.314047	455676.151120	42.598119
3504.546917	455654.669988	42.603124
3504.815419	455642.813633	42.608128
3504.503484	455629.282268	42.613133
3504.641291	455605.688383	42.618138
3504.449882	455596.140843	42.623143
3504.380788	455582.973494	42.628148
3503.829666	455557.672381	42.633152
3504.217820	455541.334899	42.638157
3504.142170	455540.384713	42.643162
3503.780377	455542.372664	42.648167
3503.757692	455527.068413	42.653172
3503.749040	455508.771092	42.658176
3503.790860	455502.731927	42.663181
3504.153023	455494.458427	42.668186
3503.829846	455503.181453	42.673191
3504.035976	455495.137352	42.678196
3504.567232	455480.549511	42.683200
3504.214395	455480.711124	42.688205
3504.288617	455464.072359	42.693210
3503.521406	455446.157949	42.698215
3503.836062	455438.095295	42.703220
3503.913028	455437.524561	42.708224
3503.804997	455436.377141	42.713229
3503.986667	455430.162008	42.718234
3503.919516	455423.837290	42.723239
3503.843257	455414.675518	42.728244
3504.056702	455405.008071	42.733248
3504.151188	455412.798100	42.738253
3504.692766	455392.683286	42.743258
3504.223983	455390.076776	42.748263
3504.226328	455379.583640	42.753268
3503.887477	455358.554641	42.758272
3504.119288	455341.939558	42.763277
3504.760103	455333.922552	42.768282
3504.455281	455316.790800	42.773287
3504.565831	455304.809150	42.778292
3504.786864	455292.453800	42.783296
3504.405094	455276.754466	42.788301
3504.686329	455258.001905	42.793306
3504.199039	455243.638496	42.798311
3504.367501	455235.904864	42.803316
3504.617659	455220.198966	42.808321
3504.124774	455205.177517	42.813325
3503.989846	455183.454549	42.818330
3503.996072	455167.080601	42.823335
3503.990928	455149.339949	42.828340
3503.974065	455145.439681	42.833345
3503.494301	455153.277171	42.838349
3504.315869	455141.174022	42.843354
3503.621734	455126.389637	42.848359
3503.827147	455113.884776	42.853364
3503.497723	455118.046917	42.858369
3503.322753	455115.238133	42.863373
3503.682466	455109.043193	42.868378
3503.551538	455121.383248	42.873383
3504.071913	455116.428131	42.878388
3504.311743	455119.631341	42.883393
3504.443672	455113.424605	42.888397
3504.335027	455097.222285	42.893402
3504.257633	455086.843994	42.898407
3504.356923	455061.583277	42.903412
3504.629282	455050.080752	42.908417
3503.684966	455040.509435	42.913421
3504.119945	455014.228226	42.918426
3503.913502	455011.475492	42.923431
3504.464582	455004.690250	42.928436
3504.609168	454985.504557	42.933441
3504.349011	454974.751891	42.938445
3504.530666	454960.730277	42.943450
3504.498154	454946.289007	42.948455
3504.169458	454932.709348	42.953460
3504.164069	454914.360246	42.958465
3504.396447	454894.601880	42.963469
3504.762305	454893.779040	42.968474
3504.293998	454879.361442	42.973479
3503.856329	454863.215115	42.978484
3504.232321	454855.192450	42.983489
3504.005626	454836.475538	42.988493
3504.301764	454828.415807	42.993498
3504.072512	454828.252177	42.998503
3504.135019	454822.513424	43.003508
3504.042386	454807.169884	43.008513
3504.161318	454807.605785	43.013517
3504.410297	454789.770739	43.018522
3504.181614	454781.242999	43.023527
3504.011039	454762.313673	43.028532
3504.106827	454758.343406	43.033537
3503.936397	454742.455499	43.038541
3503.734594	454721.909353	43.043546
3504.127160	454727.266265	43.048551
3504.355410	454723.222683	43.053556
3504.111568	454707.651431	43.058561
3503.747560	454696.358746	43.063565
3504.305467	454689.014632	43.068570
3504.091943	454692.751540	43.073575
3503.917259	454676.458778	43.078580
3504.151479	454650.971750	43.083585
3503.837345	454649.910168	43.088589
3503.769249	454653.825016	43.093594
3503.940135	454650.247436	43.098599
3504.049977	454632.486701	43.103604
3504.130306	454616.707954	43.108609
3504.145736	454616.401161	43.113613
3504.117628	454604.746924	43.118618
3504.029887	454591.125895	43.123623
3503.833697	454578.385130	43.128628
3503.975805	454568.171862	43.133633
3503.892240	454579.541018	43.138637
3504.207191	454556.676046	43.143642
3503.930739	454548.105673	43.148647
3504.028414	454539.319341	43.153652
3503.752771	454538.656713	43.158657
3503.736781	454535.719321	43.163661
3503.868451	454515.876401	43.168666
3503.679421	454505.009959	43.173671
3503.880734	454506.547018	43.178676
3503.467043	454501.700550	43.183681
3504.374717	454508.541010	43.188685
3504.298094	454499.277505	43.193690
3504.348194	454488.522299	43.198695
3504.252229	454483.773652	43.203700
3504.454936	454459.711134	43.208705
3504.306674	454448.077324	43.213709
3504.016263	454438.799603	43.218714
3504.044758	454426.527297	43.223719
3503.737215	454415.478275	43.228724
3503.948463	454397.395870	43.233729
3503.523155	454401.016915	43.238733
3503.861858	454395.991263	43.243738
3503.785537	454401.276246	43.248743
3503.788810	454383.178647	43.253748
3503.896133	454375.759281	43.258753
3503.566858	454372.520513	43.263757
3504.117011	454357.675187	43.268762
3504.180251	454366.484793	43.273767
3503.927416	454355.730549	43.278772
3504.195039	454333.785866	43.283777
3503.627102	454337.228507	43.288781
3503.915111	454331.045576	43.293786
3503.529003	454335.623090	43.298791
3503.818016	454335.421656	43.303796
3503.958321	454319.784516	43.308801
3503.608572	454311.682788	43.313805
3504.035044	454301.877062	43.318810
3504.065474	454300.046938	43.323815
3503.879908	454301.548686	43.328820
3504.233433	454279.285124	43.333825
3503.977091	454275.476272	43.338829
3503.816633	454264.706208	43.343834
3503.897396	454268.494328	43.348839
3504.020912	454261.984617	43.353844
3504.043927	454241.703754	43.358849
3503.934007	454248.312514	43.363853
3504.045507	454240.436155	43.368858
3504.121386	454246.404884	43.373863
3503.555484	454222.625402	43.378868
3503.808762	454203.166955	43.383873
3503.636872	454205.477453	43.388877
3503.843012	454198.395997	43.393882
3503.976287	454201.566855	43.398887
3504.113247	454206.004393	43.403892
3504.031567	454182.547725	43.408897
3503.637557	454177.241586	43.413901
3503.753949	454171.087910	43.418906
3503.860598	454172.843928	43.423911
3503.433385	454174.133483	43.428916
3503.853623	454180.296896	43.433921
3503.911520	454165.231326	43.438925
3503.898218	454133.753506	43.443930
3503.916845	454140.999356	43.448935
3504.116784	454134.831404	43.453940
3504.198322	454136.794483	43.458945
3503.993706	454118.225220	43.463949
3504.040734	454106.253714	43.468954
3503.984098	454110.420172	43.473959
3503.814270	454104.061884	43.478964
3504.006261	454077.314035	43.483969
3503.895790	454069.424819	43.488973
3503.715559	454063.169679	43.493978
3503.890396	454065.674455	43.498983
3503.908866	454074.136982	43.503988
3504.694907	454053.877727	43.508993
3504.066946	454044.201227	43.513997
3504.167385	454033.183722	43.519002
3504.117420	454015.500431	43.524007
3504.204200	454001.038124	43.529012
3504.013947	453992.351413	43.534017
3503.805536	453999.433307	43.539021
3503.732747	453984.035068	43.544026
3503.953454	453958.143942	43.549031
3503.933371	453960.428547	43.554036
3504.014505	453953.216272	43.559041
3503.804372	453955.077091	43.564045
3503.892768	453944.365753	43.569050
3503.891988	453933.061318	43.574055
3503.774837	453918.329615	43.579060
3503.973934	453911.806888	43.584065
3503.972877	453922.452617	43.589069
3503.929410	453904.058416	43.594074
3504.583812	453889.803271	43.599079
3504.423404	453889.070252	43.604084
3504.616660	453863.994785	43.609089
3504.418918	453863.065366	43.614093
3504.010551	453839.714779	43.619098
3504.009487	453826.230521	43.624103
3504.150784	453811.049065	43.629108
3503.804547	453802.845147	43.634113
3504.160158	453803.189965	43.639117
3503.952382	453779.298125	43.644122
3504.132416	453774.907735	43.649127
3503.572489	453776.980376	43.654132
3504.070714	453762.194181	43.659137
3503.596444	453768.561146	43.664141
3503.732157	453755.965971	43.669146
3504.057929	453734.973896	43.674151
3503.935410	453728.049783	43.679156
3503.994715	453720.638379	43.684161
3503.732343	453729.554550	43.689165
3503.799225	453718.491912	43.694170
3503.750741	453712.264863	43.699175
3503.883007	453695.107811	43.704180
3503.963627	453692.914207	43.709185
3503.724231	453704.209069	43.714189
3503.543408	453699.829584	43.719194
3503.597783	453698.907804	43.724199
3503.749757	453694.623576	43.729204
3504.041180	453678.047658	43.734209
3503.717231	453675.872436	43.739213
3503.617673	453671.022827	43.744218
3503.739324	453673.536732	43.749223
3503.821466	453671.647028	43.754228
3504.286303	453666.346193	43.759233
3504.087287	453662.780907	43.764237
3503.900745	453636.401280	43.769242
3503.781395	453643.924334	43.774247
3503.256420	453633.165482	43.779252
3503.800249	453630.183067	43.784257
3503.602758	453651.710957	43.789261
3503.782329	453634.647164	43.794266
3503.856771	453617.347838	43.799271
3503.563557	453613.950710	43.804276
3504.318386	453604.443444	43.809281
3504.155767	453609.996836	43.814285
3504.002757	453587.616238	43.819290
3503.975881	453572.463320	43.824295
3504.090116	453569.250083	43.829300
3504.165198	453555.549870	43.834305
3503.665578	453550.413682	43.839309
3504.345571	453530.983127	43.844314
3504.328884	453530.732496	43.849319
3504.345549	453523.987325	43.854324
3504.674925	453504.058975	43.859329
3504.434138	453497.560531	43.864333
3504.445875	453484.580805	43.869338
3504.470021	453458.671917	43.874343
3504.484724	453445.438188	43.879348
3504.632679	453417.885892	43.884353
3504.079338	453415.851199	43.889357
3504.223151	453393.267624	43.894362
3504.251557	453384.391237	43.899367
3504.132098	453380.660234	43.904372
3504.241658	453355.497049	43.909377
3504.034841	453349.398314	43.914381
3504.188835	453330.310855	43.919386
3504.345635	453330.131988	43.924391
3504.507995	453305.872229	43.929396
3504.416922	453290.121729	43.934401
3503.882466	453282.963634	43.939405
3504.163782	453266.693279	43.944410
3503.968209	453258.564807	43.949415
3503.885264	453261.164393	43.954420
3503.945081	453246.452685	43.959425
3503.910787	453228.512566	43.964429
3503.752430	453223.368721	43.969434
3503.808501	453218.897990	43.974439
3503.771692	453225.646680	43.979444
3503.872682	453221.624533	43.984449
3503.902012	453220.808397	43.989453
3504.059417	453194.268085	43.994458
3503.873941	453187.151759	43.999463
3503.710284	453184.492861	44.004468
3503.716478	453175.670871	44.009473
3503.887222	453175.895182	44.014477
3504.058289	453157.362292	44.019482
3503.927326	453152.467226	44.024487
3503.842536	453143.508673	44.029492
3503.831718	453147.414028	44.034497
3503.857952	453153.898502	44.039501
3503.901273	453136.452001	44.044506
3503.976396	453113.879848	44.049511
3503.792168	453111.072368	44.054516
3503.935371	453100.503317	44.059521
3503.770978	453113.965588	44.064525
3503.607339	453110.951811	44.069530
3503.598948	453101.067682	44.074535
3503.508158	453085.215586	44.079540
3503.535816	453074.209994	44.084545
3503.444923	453089.180587	44.089549
3503.739736	453085.733661	44.094554
3503.776640	453084.206494	44.099559
3503.739786	453087.761440	44.104564
3503.848448	453085.816459	44.109569
3503.547964	453087.236526	44.114573
3503.817687	453088.204365	44.119578
3503.941488	453071.149628	44.124583
3503.551601	453051.445043	44.129588
3503.737428	453045.127089	44.134593
3503.767331	453057.795791	44.139597
3503.754281	453051.055539	44.144602
3503.491758	453045.523873	44.149607
3503.777556	453050.189725	44.154612
3503.680181	453045.947938	44.159617
3503.547756	453029.241088	44.164621
3503.817156	453018.954620	44.169626
3503.759801	453019.319271	44.174631
3503.811883	453016.978381	44.179636
3503.828838	453006.532230	44.184641
3503.333455	453017.161442	44.189645
3503.567432	453015.854097	44.194650
3503.521952	453013.884733	44.199655
3503.867814	453020.517456	44.204660
3504.012714	453006.399393	44.209665
3504.225551	452988.518259	44.214669
3504.016523	452973.700174	44.219674
3504.317023	452972.077296	44.224679
3503.794152	452951.280021	44.229684
3504.053003	452935.773674	44.234689
3503.970302	452936.700305	44.239693
3504.400324	452935.866436	44.244698
3504.346548	452906.015904	44.249703
3503.963903	452905.675664	44.254708
3503.857361	452904.882716	44.259713
3504.052408	452889.488620	44.264717
3503.829266	452869.958172	44.269722
3503.798800	452859.266564	44.274727
3503.768240	452865.355261	44.279732
3504.138029	452865.748372	44.284737
3504.023318	452855.476713	44.289741
3503.929780	452829.435040	44.294746
3503.948054	452824.818590	44.299751
3504.036367	452834.131531	44.304756
3503.677986	452816.601261	44.309761
3504.023496	452818.874265	44.314765
3503.780528	452804.264637	44.319770
3503.900764	452795.220228	44.324775
3503.982089	452794.243110	44.329780
3504.042445	452785.563793	44.334785
3503.816222	452773.638168	44.339789
3504.168736	452751.271735	44.344794
3503.875269	452748.584248	44.349799
3503.868144	452750.157031	44.354804
3504.242883	452755.770988	44.359809
3503.993908	452737.867098	44.364813
3503.826971	452717.667861	44.369818
3503.761967	452714.941361	44.374823
3503.804606	452715.491728	44.379828
3503.696353	452710.440591	44.384833
3503.793932	452693.643500	44.389837
3503.649664	452669.435348	44.394842
3504.035416	452670.434093	44.399847
3503.903339	452673.751888	44.404852
3504.018086	452663.238169	44.409857
3503.961983	452662.031028	44.414861
3503.894522	452640.192451	44.419866
3503.707537	452636.016576	44.424871
3503.580749	452641.107843	44.429876
3503.931287	452634.457462	44.434881
3503.960380	452636.936603	44.439885
3503.679612	452625.121597	44.444890
3504.034392	452608.128432	44.449895
3503.770934	452598.794577	44.454900
3504.053273	452595.653879	44.459905
3503.966476	452597.240277	44.464909
3504.072414	452588.654487	44.469914
3504.356449	452572.180336	44.474919
3504.070891	452560.771683	44.479924
3504.259082	452555.112230	44.484929
3504.041653	452525.948145	44.489933
3504.222225	452525.308944	44.494938
3504.271061	452512.879933	44.499943
3504.026919	452502.985074	44.504948
3503.928973	452489.820663	44.509953
3503.958610	452490.170469	44.514957
3504.166216	452486.738335	44.519962
3504.184157	452469.903964	44.524967
3503.355088	452457.320638	44.529972
3503.985050	452443.879819	44.534977
3503.877043	452449.221411	44.539981
3503.826165	452446.948734	44.544986
3503.981011	452444.184659	44.549991
3503.756549	452431.548780	44.554996
3503.934669	452405.916459	44.560001
3503.702380	452411.989037	44.565005
3503.664883	452412.603791	44.570010
3503.886086	452406.837268	44.575015
3503.523038	452406.493672	44.580020
3503.729346	452411.223939	44.585025
3503.845579	452388.998853	44.590029
3503.915805	452378.087015	44.595034
3503.957613	452374.024112	44.600039
3504.165881	452373.177390	44.605044
3503.772518	452358.086155	44.610049
3503.989571	452348.822233	44.615053
3504.062294	452336.084855	44.620058
3504.242627	452328.956468	44.625063
3503.618320	452338.543402	44.630068
3503.886780	452310.107200	44.635073
3503.773811	452306.983259	44.640077
3504.213429	452302.700326	44.645082
3504.010216	452295.383932	44.650087
3503.756488	452289.901257	44.655092
3503.886992	452263.668524	44.660097
3503.739695	452261.665776	44.665101
3503.609581	452258.747544	44.670106
3503.880043	452255.659520	44.675111
3503.470074	452257.250428	44.680116
3503.819591	452249.535456	44.685121
3503.791061	452256.790022	44.690125
3503.833799	452249.685102	44.695130
3504.173509	452227.472381	44.700135
3504.105898	452225.760208	44.705140
3503.812306	452221.957332	44.710145
3503.886176	452221.184249	44.715149
3503.823425	452208.520622	44.720154
3504.025938	452188.663363	44.725159
3503.580227	452194.823143	44.730164
3503.802586	452186.977768	44.735169
3503.898476	452185.136279	44.740173
3503.966126	452178.128475	44.745178
3504.285420	452159.772171	44.750183
3504.289925	452158.402561	44.755188
3504.533747	452143.810741	44.760193
3504.258300	452131.436872	44.765197
3504.187917	452113.045667	44.770202
3504.187508	452103.463883	44.775207
3504.126520	452079.646401	44.780212
3503.914296	452072.280767	44.785217
3504.298539	452070.998405	44.790221
3504.055183	452055.019474	44.795226
3504.131466	452025.145462	44.800231
3504.102695	452031.132703	44.805236
3504.098653	452012.375197	44.810241
3504.052379	451995.297915	44.815245
3504.118927	451987.022788	44.820250
3503.824945	451977.288280	44.825255
3503.795632	451980.183056	44.830260
3503.965823	451968.848351	44.835265
3504.056235	451953.775613	44.840269
3503.498078	451949.257391	44.845274
3503.761549	451953.825910	44.850279
3503.617665	451954.154655	44.855284
3503.960895	451945.528082	44.860289
3503.980375	451941.367510	44.865293
3503.756845	451918.185971	44.870298
3503.662275	451908.062496	44.875303
3503.563735	451917.002171	44.880308
3503.746859	451911.191314	44.885313
3503.704181	451913.784192	44.890317
3503.799074	451909.864228	44.895322
3503.681062	451907.856445	44.900327
3503.706906	451903.187798	44.905332
3503.743187	451883.358631	44.910337
3503.847129	451888.562781	44.915341
3503.604820	451892.203711	44.920346
3503.723365	451880.827078	44.925351
3503.816967	451894.195391	44.930356
3504.052427	451891.620272	44.935361
3503.872349	451867.518691	44.940365
3503.544334	451854.545253	44.945370
3503.778949	451849.333965	44.950375
3503.658394	451851.179675	44.955380
3504.084117	451841.525009	44.960385
3503.849642	451855.152159	44.965389
3503.965976	451850.062464	44.970394
3504.011972	451823.995699	44.975399
3503.822781	451820.225620	44.980404
3503.758974	451816.991814	44.985409
3503.715069	451809.698744	44.990413
3503.671385	451809.249908	44.995418
3503.904473	451794.608978	45.000423
3503.870849	451783.156877	45.005428
3504.046672	451779.273768	45.010433
3503.899693	451764.393522	45.015437
3503.629672	451773.159745	45.020442
3503.786250	451763.855189	45.025447
3504.032510	451761.227511	45.030452
3504.116998	451745.344458	45.035457
3503.589109	451744.876899	45.040461
3503.658376	451738.679847	45.045466
3503.644657	451740.456626	45.050471
3503.440453	451747.690667	45.055476
3503.490359	451746.363976	45.060481
3503.663646	451745.016217	45.065485
3503.461284	451726.951396	45.070490
3503.834349	451705.087310	45.075495
3503.586466	451702.493299	45.080500
3503.821134	451704.379767	45.085505
3503.960588	451697.207445	45.090509
3503.441266	451698.766366	45.095514
3503.784396	451700.076630	45.100519
3503.548452	451712.994343	45.105524
3504.029102	451710.478733	45.110529
3503.994507	451683.208786	45.115533
3503.738054	451674.025412	45.120538
3503.896980	451668.015824	45.125543
3503.709528	451666.831053	45.130548
3503.945895	451662.227804	45.135553
3504.113813	451651.400301	45.140557
3503.904879	451637.747310	45.145562
3504.281480	451629.773992	45.150567
3503.864039	451628.983380	45.155572
3504.150239	451618.034266	45.160577
3504.047260	451604.667355	45.165581
3503.853207	451592.279264	45.170586
3504.029975	451593.161650	45.175591
3504.131494	451586.705552	45.180596
3504.187753	451559.115736	45.185601
3503.805355	451561.665266	45.190605
3503.749850	451557.923012	45.195610
3504.078613	451540.223631	45.200615
3503.879236	451529.053186	45.205620
3503.924318	451510.895227	45.210625
3503.815667	451511.015167	45.215629
3503.777642	451508.841590	45.220634
3503.718979	451506.620838	45.225639
3503.562943	451516.229591	45.230644
3503.769583	451500.883183	45.235649
3504.161534	451476.176484	45.240653
3503.727716	451484.869398	45.245658
3504.349366	451473.254542	45.250663
3504.007133	451466.164387	45.255668
3504.047232	451445.117369	45.260673
3503.965595	451440.517669	45.265677
3503.606423	451440.173393	45.270682
3503.894032	451433.938968	45.275687
3503.659440	451427.844406	45.280692
3503.792619	451410.279707	45.285697
3503.777352	451400.700135	45.290701
3503.503578	451398.516101	45.295706
3503.973600	451387.636877	45.300711
3503.763183	451392.539932	45.305716
3503.707151	451395.794247	45.310721
3504.171639	451397.540103	45.315725
3503.779769	451377.580760	45.320730
3503.709768	451364.157364	45.325735
3503.783746	451352.128959	45.330740
3503.512186	451355.724277	45.335745
3503.280682	451360.935137	45.340749
3503.416443	451363.599015	45.345754
3503.847134	451356.528946	45.350759
3503.515708	451368.297090	45.355764
3503.823858	451369.106354	45.360769
3504.208921	451348.963625	45.365773
3503.974171	451326.797330	45.370778
3504.147286	451316.577159	45.375783
3504.258462	451327.458561	45.380788
3504.324306	451300.677957	45.385793
3504.423698	451297.771101	45.390797
3504.114724	451295.745164	45.395802
3504.423993	451268.111761	45.400807
3504.134489	451249.960004	45.405812
3504.048387	451251.799884	45.410817
3504.198208	451225.004844	45.415821
3504.332477	451220.469630	45.420826
3504.361860	451204.240674	45.425831
3504.081308	451190.143319	45.430836
3503.759022	451170.121195	45.435841
3504.072899	451169.104294	45.440845
3503.791437	451169.760741	45.445850
3504.194911	451155.647967	45.450855
3504.103966	451141.011205	45.455860
3504.099544	451134.573055	45.460865
3503.955746	451124.660402	45.465869
3503.950256	451109.400627	45.470874
3504.078300	451097.007943	45.475879
3503.804827	451094.367524	45.480884
3503.828478	451095.630977	45.485889
3504.331332	451086.875394	45.490893
3504.064679	451072.268585	45.495898
3503.810622	451049.344788	45.500903
3503.690137	451055.652171	45.505908
3503.625408	451056.423716	45.510913
3503.452337	451057.264459	45.515917
3503.522992	451059.077590	45.520922
3503.887592	451052.322905	45.525927
3503.848949	451033.469022	45.530932
3503.594669	451014.144939	45.535937
3503.623353	451013.328827	45.540941
3503.427370	451019.851913	45.545946
3504.072490	451008.232792	45.550951
3503.714270	451024.061726	45.555956
3503.780138	451013.555518	45.560961
3503.823566	451007.362660	45.565965
3504.002906	450995.214658	45.570970
3503.808106	450980.696917	45.575975
3503.709097	450988.065360	45.580980
3504.011217	450979.090505	45.585985
3504.211539	450974.949563	45.590989
3503.530475	450961.579543	45.595994
3503.531205	450935.265890	45.600999
3503.485726	450943.081513	45.606004
3503.577614	450932.621522	45.611009
3503.834248	450931.563683	45.616013
3503.654392	450941.379570	45.621018
3504.112089	450933.189338	45.626023
3503.602104	450935.608627	45.631028
3503.538508	450925.530083	45.636033
3503.767439	450905.768489	45.641037
3503.487613	450904.599446	45.646042
3503.777102	450889.644046	45.651047
3503.612039	450894.336671	45.656052
3503.461048	450890.103596	45.661057
3503.621460	450891.952116	45.666061
3503.422103	450897.715308	45.671066
3503.500318	450891.009470	45.676071
3503.766006	450900.698600	45.681076
3503.347149	450896.511263	45.686081
3503.999224	450897.515325	45.691085
3503.697378	450889.911071	45.696090
3503.614660	450861.177945	45.701095
3503.462460	450859.429401	45.706100
3503.800839	450864.999384	45.711105
3503.814971	450863.070337	45.716109
3503.766102	450857.755104	45.721114
3504.030459	450865.872758	45.726119
3503.633044	450862.797166	45.731124
3503.165045	450841.075783	45.736129
3503.629077	450843.835779	45.741133
3503.569832	450844.454293	45.746138
3503.619290	450830.756652	45.751143
3503.583563	450829.343122	45.756148
3503.634625	450818.433738	45.761153
3503.545983	450821.186703	45.766157
3503.358930	450829.837754	45.771162
3503.867086	450817.937709	45.776167
3503.456160	450834.029290	45.781172
3503.478402	450830.577835	45.786177
3504.113394	450822.560090	45.791181
3503.607973	450823.609693	45.796186
3503.687656	450805.546611	45.801191
3503.481028	450798.838679	45.806196
3503.431185	450790.430847	45.811201
3503.791654	450789.608776	45.816205
3503.590568	450793.749866	45.821210
3503.885823	450795.828875	45.826215
3503.482259	450790.979795	45.831220
3503.643492	450788.974924	45.836225
3503.674938	450788.868143	45.841229
3503.748091	450791.137178	45.846234
3503.621416	450776.810465	45.851239
3503.599368	450773.265161	45.856244
3503.707578	450761.889681	45.861249
3503.852821	450753.448525	45.866253
3503.863989	450756.336558	45.871258
3503.801375	450755.536025	45.876263
3503.701699	450760.978029	45.881268
3503.874954	450752.177183	45.886273
3503.875938	450727.434952	45.891277
3503.726453	450720.920041	45.896282
3503.802672	450712.997663	45.901287
3503.327601	450716.019428	45.906292
3503.128208	450709.766540	45.911297
3503.197666	450709.805371	45.916301
3503.515932	450721.057338	45.921306
3503.995286	450713.978745	45.926311
3503.868015	450719.476172	45.931316
3503.865077	450714.051658	45.936321
3503.976800	450712.359439	45.941325
3504.018858	450703.023263	45.946330
3504.054960	450687.705375	45.951335
3503.925621	450690.465306	45.956340
3503.688076	450682.647192	45.961345
3503.573682	450662.436979	45.966349
3503.558655	450654.124550	45.971354
3503.792681	450640.344568	45.976359
3503.658916	450643.612273	45.981364
3503.385773	450648.627614	45.986369
3503.537820	450648.145332	45.991373
3503.343314	450651.778315	45.996378
3503.587448	450649.759275	46.001383
3504.258242	450660.241266	46.006388
3504.280789	450645.888984	46.011393
3504.278015	450625.862481	46.016397
3503.573386	450621.774584	46.021402
3503.550525	450610.979115	46.026407
3503.885372	450607.220740	46.031412
3503.802740	450610.327615	46.036417
3503.782325	450585.386065	46.041421
3503.560118	450580.100358	46.046426
3503.749097	450572.919194	46.051431
3503.958032	450578.562057	46.056436
3504.230748	450567.817501	46.061441
3504.040251	450563.743208	46.066445
3503.857970	450549.831444	46.071450
3504.186953	450538.975863	46.076455
3503.948078	450531.867739	46.081460
3503.728892	450530.485514	46.086465
3503.889250	450503.383538	46.091469
3503.506991	450493.004285	46.096474
3503.710717	450485.009348	46.101479
3503.700496	450496.165421	46.106484
3503.359761	450493.333603	46.111489
3504.031755	450487.641684	46.116493
3503.652156	450502.916945	46.121498
3503.961169	450481.214619	46.126503
3503.447666	450462.542704	46.131508
3503.601802	450459.220771	46.136513
3503.786440	450449.809435	46.141517
3503.612793	450447.608202	46.146522
3503.739354	450446.268340	46.151527
3503.851980	450450.710843	46.156532
3503.405202	450453.271498	46.161537
3503.745793	450442.768796	46.166541
3504.065675	450450.268712	46.171546
3504.314699	450430.401835	46.176551
3504.075674	450411.125288	46.181556
3503.894278	450413.488530	46.186561
3503.847812	450410.403649	46.191565
3503.726955	450385.631115	46.196570
3503.771965	450375.736568	46.201575
3503.873579	450384.794830	46.206580
3503.522635	450377.857895	46.211585
3503.823606	450377.147371	46.216589
3503.770075	450380.198609	46.221594
3503.834089	450374.458365	46.226599
3503.638049	450354.971620	46.231604
3503.796146	450341.407213	46.236609
3503.769082	450335.023385	46.241613
3503.847215	450335.618456	46.246618
3503.821468	450332.783535	46.251623
3503.724251	450337.109787	46.256628
3503.661450	450334.636107	46.261633
3504.020490	450321.950012	46.266637
3503.770824	450321.079996	46.271642
3503.539233	450304.894901	46.276647
3503.458450	450303.894644	46.281652
3503.438128	450307.193733	46.286657
3503.979145	450298.025690	46.291661
3503.758111	450303.032216	46.296666
3504.042630	450290.713741	46.301671
3503.768962	450272.710532	46.306676
3503.539968	450262.051484	46.311681
3503.933114	450246.621607	46.316685
3503.441421	450260.800738	46.321690
3503.903308	450252.457420	46.326695
3503.658770	450265.022581	46.331700
3503.908374	450257.323936	46.336705
3504.109622	450241.014184	46.341709
3503.749700	450231.695731	46.346714
3503.739377	450223.433030	46.351719
3504.040478	450223.178799	46.356724
3503.888892	450216.258471	46.361729
3504.195808	450183.705921	46.366733
3503.989344	450179.684981	46.371738
3503.868158	450172.049617	46.376743
3503.712148	450177.704200	46.381748
3503.644447	450177.107322	46.386753
3504.006142	450171.164087	46.391757
3503.716835	450156.306991	46.396762
3503.793903	450142.857696	46.401767
3503.791036	450144.176437	46.406772
3503.542113	450146.094917	46.411777
3503.749438	450130.037552	46.416781
3504.203775	450140.962385	46.421786
3504.290189	450119.551204	46.426791
3504.222983	450104.504041	46.431796
3503.744017	450100.377507	46.436801
3504.028548	450083.799900	46.441805
3503.807164	450079.223760	46.446810
3503.898445	450068.053604	46.451815
3503.974260	450073.465822	46.456820
3503.513940	450075.014784	46.461825
3503.779083	450069.544329	46.466829
3503.320798	450064.095990	46.471834
3503.354051	450061.250958	46.476839
3503.298377	450072.769935	46.481844
3503.371749	450074.379879	46.486849
3503.259253	450075.108913	46.491853
3503.569150	450079.467109	46.496858
3503.652015	450061.149329	46.501863
3503.250871	450043.826822	46.506868
3503.296583	450057.660817	46.511873
3503.552925	450060.304274	46.516877
3503.163224	450063.159445	46.521882
3503.659442	450070.325174	46.526887
3503.706945	450051.759910	46.531892
3503.217896	450042.362016	46.536897
3503.480925	450030.959704	46.541901
3503.842467	450035.359794	46.546906
3503.653667	450035.239913	46.551911
3503.647577	450030.677705	46.556916
3503.285722	450030.485967	46.561921
3504.104467	450022.639355	46.566925
3503.897163	450030.330843	46.571930
3503.711918	450028.739978	46.576935
3503.556168	450010.513598	46.581940
3503.592596	450013.296016	46.586945
3503.826259	449991.910265	46.591949
3503.811773	449991.912728	46.596954
3503.962454	449987.627959	46.601959
3503.673894	449992.189764	46.606964
3503.352660	450000.914771	46.611969
3503.814782	449994.498014	46.616973
3503.635122	449985.097969	46.621978
3503.669573	449969.019295	46.626983
3503.784356	449963.016755	46.631988
3503.635796	449959.340806	46.636993
3503.548433	449946.781409	46.641997
3503.665984	449955.177999	46.647002
3503.601439	449958.281882	46.652007
3503.863272	449954.890779	46.657012
3503.914253	449961.067808	46.662017
3503.536346	449946.377799	46.667021
3504.063523	449933.713464	46.672026
3504.017209	449920.285093	46.677031
3503.914793	449919.440621	46.682036
3503.862024	449922.643904	46.687041
3503.878900	449906.770996	46.692045
3503.756821	449886.459937	46.697050
3503.730203	449882.661747	46.702055
3503.990756	449884.797478	46.707060
3503.520097	449879.503312	46.712065
3503.598936	449883.596784	46.717069
3503.960682	449884.751879	46.722074
3504.334607	449868.108134	46.727079
3504.121470	449849.080164	46.732084
3503.965122	449848.397007	46.737089
3504.241235	449839.679621	46.742093
3504.062578	449818.972533	46.747098
3503.986365	449800.935202	46.752103
3504.119456	449796.551991	46.757108
3504.043251	449801.990236	46.762113
3503.973072	449766.002904	46.767117
3503.590340	449764.496442	46.772122
3503.449214	449763.912089	46.777127
3503.781983	449758.734226	46.782132
3503.665845	449768.894706	46.787137
3503.771268	449763.045816	46.792141
3503.939349	449769.912754	46.797146
3503.648293	449741.720695	46.802151
3503.654718	449725.697323	46.807156
3503.478388	449723.648582	46.812161
3503.823011	449721.713703	46.817165
3503.611672	449716.273811	46.822170
3503.634254	449723.723345	46.827175
3503.562887	449719.222918	46.832180
3503.490666	449730.694205	46.837185
3503.753992	449719.494487	46.842189
3503.309194	449718.404247	46.847194
3503.629969	449716.067812	46.852199
3503.631898	449703.594430	46.857204
3503.392140	449687.714471	46.862209
3503.414050	449681.829115	46.867213
3503.131966	449686.694102	46.872218
3503.352726	449689.749310	46.877223
3503.359928	449693.753644	46.882228
3503.154373	449712.498302	46.887233
3503.579030	449720.436922	46.892237
3503.327014	449724.434808	46.897242
3503.576517	449724.392196	46.902247
3503.526132	449712.891116	46.907252
3503.313526	449701.214914	46.912257
3503.492677	449694.897086	46.917261
3503.490458	449690.993288	46.922266
3503.355444	449685.388245	46.927271
3503.654165	449684.171049	46.932276
3503.564268	449686.214528	46.937281
3503.932415	449693.655772	46.942285
3503.270353	449700.106739	46.947290
3503.240805	449693.571028	46.952295
3503.720871	449688.672219	46.957300
3503.545214	449692.454259	46.962305
3504.028036	449686.642316	46.967309
3503.817239	449694.081005	46.972314
3503.966216	449679.655769	46.977319
3503.686507	449663.630503	46.982324
3503.470279	449651.245043	46.987329
3503.728273	449647.144695	46.992333
3503.249184	449651.688402	46.997338
3503.750302	449651.754939	47.002343
3503.847634	449654.577709	47.007348
3503.534176	449654.783332	47.012353
3503.851497	449646.261644	47.017357
3503.937285	449644.066732	47.022362
3503.519295	449629.434047	47.027367
3503.533290	449613.358594	47.032372
3503.299361	449617.353411	47.037377
3503.722560	449608.255890	47.042381
3503.322351	449619.529722	47.047386
3503.313602	449611.165103	47.052391
3503.379577	449611.914383	47.057396
3503.488299	449610.526810	47.062401
3503.837941	449615.993798	47.067405
3503.868113	449623.036443	47.072410
3503.655179	449625.557269	47.077415
3504.224864	449619.274143	47.082420
3503.722871	449601.106527	47.087425
3503.977202	449582.657643	47.092429
3503.683917	449582.961229	47.097434
3503.888556	449574.560160	47.102439
3503.702001	449573.324410	47.107444
3503.465499	449580.564714	47.112449
3503.512473	449574.218715	47.117453
3503.522353	449583.952136	47.122458
3503.681496	449575.001094	47.127463
3503.759232	449558.255566	47.132468
3503.578951	449550.123026	47.137473
3503.907073	449534.044580	47.142477
3503.611736	449543.982246	47.147482
3503.639552	449549.047868	47.152487
3504.140868	449541.965133	47.157492
3503.947616	449538.803778	47.162497
3503.701270	449507.460130	47.167501
3503.523831	449507.743937	47.172506
3503.902115	449502.761056	47.177511
3503.852364	449503.023060	47.182516
3503.528902	449505.664180	47.187521
3503.759302	449503.900897	47.192525
3503.916286	449510.617703	47.197530
3503.589811	449490.746792	47.202535
3503.718588	449480.178368	47.207540
3503.721894	449474.752467	47.212545
3503.895623	449466.863673	47.217549
3503.903265	449479.335542	47.222554
3504.214430	449465.135985	47.227559
3504.443307	449441.215289	47.232564
3503.825310	449439.292637	47.237569
3503.754112	449431.597762	47.242573
3504.053089	449434.234019	47.247578
3503.870726	449415.555329	47.252583
3504.080732	449394.781458	47.257588
3503.849350	449401.767429	47.262593
3503.876635	449397.199384	47.267597
3503.782536	449398.432341	47.272602
3503.806897	449375.459166	47.277607
3504.131062	449359.178444	47.282612
3503.546805	449357.351432	47.287617
3504.185124	449349.180449	47.292621
3504.026275	449350.982212	47.297626
3503.663636	449332.080707	47.302631
3503.800763	449321.257256	47.307636
3503.701674	449313.414987	47.312641
3503.684549	449309.260141	47.317645
3503.737916	449312.800326	47.322650
3503.549484	449319.626877	47.327655
3503.760610	449307.269652	47.332660
3503.509565	449319.582968	47.337665
3503.375750	449300.743773	47.342669
3503.580226	449301.722937	47.347674
3503.580728	449294.674927	47.352679
3503.725527	449288.210730	47.357684
3503.627804	449284.171049	47.362689
3503.965919	449272.197757	47.367693
3503.969927	449273.211152	47.372698
3503.617734	449272.409302	47.377703
3504.036105	449271.932220	47.382708
3503.931349	449261.910607	47.387713
3504.053086	449239.174178	47.392717
3503.957928	449237.770688	47.397722
3503.843817	449234.747888	47.402727
3503.878441	449220.037634	47.407732
3503.740723	449202.872270	47.412737
3503.596625	449193.415092	47.417741
3503.426465	449195.066686	47.422746
3503.637382	449196.399688	47.427751
3503.732323	449192.732731	47.432756
3503.396270	449200.750733	47.437761
3503.428021	449192.024099	47.442765
3503.386068	449207.546878	47.447770
3503.650698	449201.873467	47.452775
3503.581189	449201.733212	47.457780
3503.858686	449196.463240	47.462785
3503.706778	449183.508769	47.467789
3503.480280	449178.527667	47.472794
3503.606902	449165.677741	47.477799
3503.526775	449155.854690	47.482804
3503.623090	449164.458043	47.487809
3503.789564	449163.973265	47.492813
3503.571485	449163.199216	47.497818
3503.451293	449162.864795	47.502823
3503.862304	449153.312816	47.507828
3503.674584	449157.756173	47.512833
3503.541817	449155.598528	47.517837
3503.388314	449160.390975	47.522842
3503.482340	449164.634109	47.527847
3503.828474	449142.467718	47.532852
3503.666926	449134.331818	47.537857
3503.975652	449130.679052	47.542861
3503.701463	449128.799075	47.547866
3503.459442	449121.893826	47.552871
3503.851551	449120.102900	47.557876
3503.836886	449124.618125	47.562881
3503.739871	449111.350008	47.567885
3503.845164	449095.258569	47.572890
3503.912364	449086.323019	47.577895
3504.024692	449070.990934	47.582900
3503.651013	449077.950603	47.587905
3503.776366	449081.377126	47.592909
3504.135195	449068.031147	47.597914
3503.651935	449047.578127	47.602919
3503.810019	449035.990375	47.607924
3503.474226	449037.416737	47.612929
3503.589707	449040.794247	47.617933
3503.528732	449045.013166	47.622938
3503.181690	449046.847089	47.627943
3503.650066	449043.674098	47.632948
3503.655667	449041.949160	47.637953
3503.804866	449041.213804	47.642957
3503.839045	449043.489685	47.647962
3503.952329	449026.382728	47.652967
3504.023572	449009.688577	47.657972
3504.118737	449004.703216	47.662977
3503.992238	448994.026020	47.667981
3503.978604	448975.774475	47.672986
3503.657743	448965.992439	47.677991
3504.044009	448961.312300	47.682996
3504.095435	448958.007669	47.688001
3503.880270	448957.385229	47.693005
3503.924873	448936.689854	47.698010
3503.627137	448924.165765	47.703015
3504.078463	448917.142062	47.708020
3503.732727	448919.280004	47.713025
3503.893160	448915.551111	47.718029
3503.913025	448905.913692	47.723034
3503.602470	448893.239657	47.728039
3503.719730	448883.484187	47.733044
3503.683964	448882.780407	47.738049
3503.748295	448879.169328	47.743053
3503.894074	448879.702186	47.748058
3503.794460	448883.420681	47.753063
3503.806870	448873.987341	47.758068
3503.781392	448863.242125	47.763073
3503.801011	448848.432762	47.768077
3504.052220	448853.308293	47.773082
3503.798599	448854.517814	47.778087
3503.825172	448852.332930	47.783092
3503.726704	448831.154825	47.788097
3503.712977	448809.455174	47.793101
3503.465484	448805.948030	47.798106
3503.715772	448807.325041	47.803111
3503.794177	448797.069109	47.808116
3503.584101	448810.592662	47.813121
3503.633010	448807.187025	47.818125
3503.619391	448808.811920	47.823130
3503.598701	448802.882887	47.828135
3503.965371	448798.206057	47.833140
3503.661360	448790.297171	47.838145
3503.888415	448768.809893	47.843149
3503.482950	448766.191713	47.848154
3503.708253	448761.386897	47.853159
3503.977147	448766.867896	47.858164
3503.728412	448777.964197	47.863169
3504.019226	448755.451905	47.868173
3504.209599	448733.108857	47.873178
3503.966763	448731.679842	47.878183
3504.058739	448723.044142	47.883188
3504.207179	448716.934089	47.888193
3504.052957	448688.565132	47.893197
3503.824360	448695.246625	47.898202
3503.829790	448686.929923	47.903207
3504.076532	448668.887182	47.908212
3503.574696	448654.724486	47.913217
3503.941785	448644.520600	47.918221
3503.849159	448643.522285	47.923226
3503.687770	448646.237250	47.928231
3503.765898	448645.209780	47.933236
3503.515969	448651.590692	47.938241
3503.516257	448637.038012	47.943245
3503.457421	448631.166150	47.948250
3503.355750	448625.605836	47.953255
3503.552376	448604.224998	47.958260
3503.545381	448608.536200	47.963265
3503.721850	448599.429667	47.968269
3503.891878	448597.473794	47.973274
3503.212739	448601.747645	47.978279
3503.415331	448604.603290	47.983284
3503.510104	448610.976065	47.988289
3503.620783	448609.233150	47.993293
3503.578720	448606.654311	47.998298
3503.214418	448608.541924	48.003303
3503.547703	448602.907337	48.008308
3503.261169	448609.294512	48.013313
3503.395185	448607.750437	48.018317
3503.743387	448607.893797	48.023322
3503.589719	448615.221700	48.028327
3503.916960	448609.283910	48.033332
3503.613367	448613.138693	48.038337
3503.492943	448578.577676	48.043341
3503.847457	448568.832256	48.048346
3503.506821	448568.788996	48.053351
3503.824299	448559.049895	48.058356
3503.839504	448569.847707	48.063361
3503.275705	448568.017129	48.068365
3503.743050	448570.320512	48.073370
3503.589858	448573.338323	48.078375
3503.503556	448567.978194	48.083380
3503.418455	448571.237910	48.088385
3503.739230	448571.183128	48.093389
3503.723437	448570.881578	48.098394
3503.508304	448546.072261	48.103399
3503.912947	448530.182809	48.108404
3503.544504	448537.040349	48.113409
3503.583311	448530.999668	48.118413
3503.617952	448530.943036	48.123418
3503.732448	448535.487040	48.128423
3503.991560	448527.735435	48.133428
3503.739140	448527.778525	48.138433
3503.344268	448501.935014	48.143437
3503.813156	448498.964682	48.148442
3503.320841	448500.062860	48.153447
3503.457463	448485.436090	48.158452
3503.508807	448491.714903	48.163457
3503.568751	448490.183467	48.168461
3503.586764	448489.876142	48.173466
3503.590552	448489.267009	48.178471
3503.703652	448487.118020	48.183476
3503.418928	448495.330350	48.188481
3503.426802	448502.884241	48.193485
3503.700345	448486.966435	48.198490
3503.482624	448501.961976	48.203495
3503.579240	448490.536539	48.208500
3503.558559	448502.861704	48.213505
3503.707301	448488.790637	48.218509
3503.857729	448465.642824	48.223514
3503.602966	448459.449422	48.228519
3503.848825	448446.984351	48.233524
3503.713368	448453.142952	48.238529
3503.497257	448452.977016	48.243533
3503.682355	448456.241321	48.248538
3503.363385	448455.991535	48.253543
3503.496689	448456.830773	48.258548
3503.595631	448456.560337	48.263553
3503.557253	448455.248512	48.268557
3503.776505	448446.236021	48.273562
3503.631683	448431.353031	48.278567
3503.892762	448416.704963	48.283572
3503.895845	448422.383559	48.288577
3503.883408	448413.410615	48.293581
3503.557522	448409.612550	48.298586
3503.681828	448415.929634	48.303591
3503.748856	448400.401971	48.308596
3503.879929	448388.311410	48.313601
3503.591009	448377.763048	48.318605
3503.907172	448381.106398	48.323610
3503.483783	448376.615083	48.328615
3503.773717	448374.030236	48.333620
3503.722617	448375.357324	48.338625
3503.940781	448372.886144	48.343629
3503.708939	448349.904889	48.348634
3503.567634	448344.047028	48.353639
3503.477048	448335.391634	48.358644
3503.424897	448340.268375	48.363649
3503.562993	448335.478353	48.368653
3503.537870	448335.938993	48.373658
3503.227871	448341.671068	48.378663
3503.561093	448335.478647	48.383668
3503.280062	448341.357896	48.388673
3503.655185	448343.119277	48.393677
3503.944315	448339.469721	48.398682
3503.549578	448345.064144	48.403687
3503.660223	448343.371920	48.408692
3504.005468	448342.450946	48.413697
3503.454105	448311.664663	48.418701
3503.606475	448307.429972	48.423706
3503.613971	448307.073734	48.428711
3503.730618	448297.267391	48.433716
3503.762516	448313.437407	48.438721
3503.617078	448301.444717	48.443725
3503.923979	448307.730656	48.448730
3503.734757	448321.301668	48.453735
3503.921190	448286.332830	48.458740
3503.659339	448275.222018	48.463745
3503.344374	448263.359667	48.468749
3503.845428	448255.363823	48.473754
3503.489282	448261.205213	48.478759
3503.753405	448256.951430	48.483764
3503.537410	448269.005839	48.488769
3503.615822	448262.654077	48.493773
3503.735281	448260.656100	48.498778
3503.680923	448263.657079	48.503783
3503.931742	448245.309040	48.508788
3503.859381	448233.506661	48.513793
3503.894573	448235.224680	48.518797
3503.925746	448226.396331	48.523802
3503.541412	448231.887593	48.528807
3503.698961	448233.179063	48.533812
3503.414065	448210.663078	48.538817
3503.672892	448188.662715	48.543821
3503.732490	448174.606660	48.548826
3503.582201	448194.103838	48.553831
3503.685191	448183.133511	48.558836
3503.643088	448186.487359	48.563841
3503.573740	448191.975555	48.568845
3503.470601	448187.987296	48.573850
3503.279162	448188.932701	48.578855
3503.625545	448188.569305	48.583860
3503.610656	448196.684970	48.588865
3503.440812	448198.184465	48.593869
3503.814705	448188.435562	48.598874
3504.030364	448181.603977	48.603879
3503.718214	448152.754194	48.608884
3503.770007	448146.609771	48.613889
3503.849590	448148.269510	48.618893
3504.136591	448145.887965	48.623898
3503.942032	448147.645219	48.628903
3504.062931	448123.893588	48.633908
3504.011159	448111.884797	48.638913
3503.773843	448107.310945	48.643917
3503.797162	448103.858858	48.648922
3503.747763	448110.763473	48.653927
3503.710998	448089.067015	48.658932
3503.792567	448081.193439	48.663937
3503.687706	448059.914237	48.668941
3503.887682	448067.384775	48.673946
3503.469384	448071.817022	48.678951
3503.498008	448065.220166	48.683956
3503.474968	448078.509421	48.688961
3503.508417	448076.019039	48.693965
3503.616450	448066.214059	48.698970
3503.629904	448076.403934	48.703975
3503.798905	448059.692339	48.708980
3503.974714	448040.494904	48.713985
3503.643788	448032.590328	48.718989
3503.520680	448027.540591	48.723994
3503.240084	448040.265358	48.728999
3503.599795	448023.622586	48.734004
3503.379374	448036.184958	48.739009
3503.348637	448034.060483	48.744013
3503.531104	448029.567060	48.749018
3503.844410	448031.693975	48.754023
3503.756153	448028.970831	48.759028
3503.846894	448031.338578	48.764033
3503.453882	448019.641538	48.769037
3503.465204	447994.894322	48.774042
3503.407323	447994.752072	48.779047
3503.382580	447988.113596	48.784052
3503.381384	447982.333126	48.789057
3503.165472	447987.085787	48.794061
3503.339560	447982.238832	48.799066
3503.480847	447987.944654	48.804071
3503.681548	447991.054244	48.809076
3503.517241	447984.490304	48.814081
3503.632673	447985.332613	48.819085
3503.766802	447981.658755	48.824090
3503.308359	447987.872640	48.829095
3503.425831	447993.126159	48.834100
3503.308150	447988.988222	48.839105
3502.905253	447998.792856	48.844109
3503.387741	447990.546547	48.849114
3503.479904	447993.370423	48.854119
3503.379358	447990.345127	48.859124
3503.248966	447989.809598	48.864129
3503.071260	447990.499129	48.869133
3503.715587	447984.963392	48.874138
3503.278192	447989.297502	48.879143
3503.274934	447984.683659	48.884148
3503.519417	447987.025160	48.889153
3503.574547	447994.419041	48.894157
3503.790904	447987.181615	48.899162
3503.773324	447989.263617	48.904167
3503.792366	447988.702572	48.909172
3503.743268	447995.150806	48.914177
3503.748888	447993.070826	48.919181
3503.966403	447993.540752	48.924186
3503.671861	447964.434167	48.929191
3503.691290	447960.678475	48.934196
3503.581708	447951.772629	48.939201
3503.906565	447955.317394	48.944205
3503.974811	447953.277425	48.949210
3503.694500	447953.173154	48.954215
3503.616806	447936.402170	48.959220
3503.827260	447922.776558	48.964225
3503.617454	447918.603630	48.969229
3504.013945	447915.392040	48.974234
3503.964738	447923.310839	48.979239
3503.858634	447914.353676	48.984244
3503.924478	447912.364821	48.989249
3503.765837	447888.407117	48.994253
3503.876480	447870.082688	48.999258
3503.771120	447875.982778	49.004263
3503.645083	447868.195279	49.009268
3503.712776	447881.671997	49.014273
3503.897775	447867.797158	49.019277
3503.893198	447847.565483	49.024282
3503.608022	447839.500899	49.029287
3503.858633	447827.338899	49.034292
3503.867288	447829.467145	49.039297
3503.656006	447830.466662	49.044301
3503.916913	447826.517590	49.049306
3503.607849	447816.479466	49.054311
3504.006933	447792.375716	49.059316
3503.721570	447794.706292	49.064321
3503.553533	447793.467273	49.069325
3503.817029	447788.858548	49.074330
3503.453514	447792.165922	49.079335
3503.817533	447789.872602	49.084340
3503.656980	447786.756107	49.089345
3503.617194	447773.223835	49.094349
3503.721877	447761.644504	49.099354
3503.791492	447760.466321	49.104359
3503.469781	447759.152122	49.109364
3503.536175	447758.937943	49.114369
3503.612743	447758.316362	49.119373
3504.039032	447740.292881	49.124378
3503.582428	447751.222380	49.129383
3503.620268	447755.779641	49.134388
3503.679436	447753.791911	49.139393
3503.520268	447736.831846	49.144397
3503.786372	447711.635131	49.149402
3503.448836	447718.639781	49.154407
3503.667851	447715.204924	49.159412
3503.616638	447711.156999	49.164417
3503.693423	447715.099120	49.169421
3503.688043	447705.871130	49.174426
3503.791525	447712.749771	49.179431
3503.789115	447710.113344	49.184436
3503.859858	447696.460735	49.189441
3503.660741	447681.637195	49.194445
3504.170351	447672.422673	49.199450
3504.234623	447677.381104	49.204455
3503.811357	447669.441450	49.209460
3504.148671	447645.956581	49.214465
3503.980050	447642.993567	49.219469
3503.992158	447629.452343	49.224474
3503.901322	447628.352257	49.229479
3503.922599	447627.993655	49.234484
3503.877177	447605.385427	49.239489
3503.735180	447603.837699	49.244493
3503.970924	447600.501384	49.249498
3503.798201	447596.575602	49.254503
3503.992959	447589.443145	49.259508
3503.889615	447566.844766	49.264513
3503.509932	447560.723138	49.269517
3504.113698	447547.486506	49.274522
3504.158890	447554.932947	49.279527
3503.663402	447542.898178	49.284532
3503.914613	447525.259370	49.289537
3503.714521	447522.352421	49.294541
3503.650017	447509.736958	49.299546
3503.532902	447517.464669	49.304551
3503.600268	447508.274880	49.309556
3503.720133	447514.795827	49.314561
3503.472338	447519.249784	49.319565
3503.803856	447512.702454	49.324570
3503.781826	447516.306524	49.329575
3503.595681	447498.793079	49.334580
3503.920002	447481.293878	49.339585
3503.526841	447479.281938	49.344589
3503.643530	447468.106067	49.349594
3503.657195	447469.168609	49.354599
3503.755740	447468.847520	49.359604
3503.904091	447468.416508	49.364609
3503.716591	447469.919069	49.369613
3503.976422	447446.396500	49.374618
3503.736623	447441.670801	49.379623
3503.520201	447428.929103	49.384628
3503.542797	447436.683696	49.389633
3503.282558	447432.265738	49.394637
3503.658168	447423.175407	49.399642
3503.583316	447436.676747	49.404647
3503.414965	447437.871787	49.409652
3503.704900	447427.781909	49.414657
3503.127495	447437.109509	49.419661
3503.526940	447442.467146	49.424666
3503.624884	447435.554004	49.429671
3503.534704	447435.417265	49.434676
3503.381937	447434.530579	49.439681
3503.052716	447436.767265	49.444685
3503.740310	447437.765446	49.449690
3503.678811	447446.041484	49.454695
3503.394011	447421.749831	49.459700
3503.456983	447418.240152	49.464705
3503.461306	447416.819554	49.469709
3503.490372	447393.894128	49.474714
3503.783839	447397.697892	49.479719
3503.694535	447395.583353	49.484724
3503.286737	447402.701522	49.489729
3503.390829	447395.280227	49.494733
3504.043570	447394.610964	49.499738
3503.219018	447399.670516	49.504743
3503.592883	447393.876554	49.509748
3503.727832	447393.853501	49.514753
3503.665109	447394.523418	49.519757
3503.694848	447389.498139	49.524762
3503.589255	447398.035270	49.529767
3503.407479	447381.078781	49.534772
3503.688924	447367.542110	49.539777
3503.537948	447371.117512	49.544781
3503.895453	447354.880266	49.549786
3503.795517	447354.846611	49.554791
3503.704016	447351.819679	49.559796
3503.791440	447352.362541	49.564801
3503.637633	447348.484193	49.569805
3503.834298	447345.965857	49.574810
3503.627234	447321.001597	49.579815
3503.852374	447308.285849	49.584820
3503.858020	447312.037355	49.589825
3503.617433	447318.619909	49.594829
3503.758133	447305.969287	49.599834
3503.736046	447312.920207	49.604839
3503.601202	447309.342869	49.609844
3503.939072	447306.546872	49.614849
3503.679332	447287.017450	49.619853
3503.738538	447282.037824	49.624858
3503.413457	447277.022394	49.629863
3503.657708	447274.495924	49.634868
3504.122626	447268.077869	49.639873
3504.013656	447278.796124	49.644877
3503.745634	447249.633319	49.649882
3503.511060	447241.559866	49.654887
3503.451720	447231.884498	49.659892
3503.837672	447226.696940	49.664897
3503.653016	447231.393723	49.669901
3503.716716	447220.581735	49.674906
3503.958036	447232.609356	49.679911
3503.769506	447232.083734	49.684916
3503.618321	447217.708069	49.689921
3503.470898	447205.461549	49.694925
3503.878418	447192.714591	49.699930
3503.627361	447199.501807	49.704935
3503.609020	447193.926887	49.709940
3503.765619	447188.829191	49.714945
3503.225672	447189.682017	49.719949
3503.641966	447187.126161	49.724954
3503.698954	447198.881019	49.729959
3503.369348	447196.807490	49.734964
3503.395679	447188.790887	49.739969
3503.164075	447197.096067	49.744973
3503.713718	447187.570245	49.749978
3503.536149	447194.902719	49.754983
3503.672729	447193.713070	49.759988
3503.753053	447183.810996	49.764993
3503.364362	447170.135076	49.769997
3504.169674	447153.922634	49.775002
3503.898398	447155.135264	49.780007
3503.872053	447150.271633	49.785012
3504.114806	447146.426955	49.790017
3503.948018	447144.274911	49.795021
3504.082786	447114.840307	49.800026
3504.117903	447117.978300	49.805031
3503.794280	447110.427098	49.810036
3504.187652	447100.522242	49.815041
3503.857302	447083.590884	49.820045
3503.657195	447068.310696	49.825050
3503.537781	447070.714435	49.830055
3503.406671	447070.939650	49.835060
3503.275770	447077.047162	49.840065
3503.462180	447074.733384	49.845069
3503.769353	447062.662709	49.850074
3504.132236	447076.444505	49.855079
3503.826901	447068.585907	49.860084
3503.777771	447043.442224	49.865089
3503.678460	447039.199545	49.870093
3503.493568	447041.969436	49.875098
3503.604603	447034.141151	49.880103
3503.312266	447029.424330	49.885108
3503.535349	447029.284809	49.890113
3503.344639	447032.714923	49.895117
3503.199164	447019.149506	49.900122
3503.289617	447029.783126	49.905127
3503.327581	447023.387190	49.910132
3503.347478	447028.708319	49.915137
3503.501287	447036.643494	49.920141
3503.601414	447032.620309	49.925146
3503.293729	447031.912187	49.930151
3503.359685	447025.511472	49.935156
3503.497762	447023.358071	49.940161
3503.599683	447028.360936	49.945165
3503.543614	447024.820808	49.950170
3503.843760	447025.682327	49.955175
3503.686557	447026.621936	49.960180
3503.715883	447016.677782	49.965185
3503.648208	446995.492581	49.970189
3503.641606	446993.008910	49.975194
3503.693211	446992.695829	49.980199
3503.367115	446985.956364	49.985204
3503.579574	446982.015410	49.990209
3503.178993	446989.943843	49.995213
3503.384749	446980.172386	50.000218
3503.692105	446990.008340	50.005223
3503.248886	446988.816259	50.010228
3503.408910	446974.285871	50.015233
3503.395181	446984.886592	50.020237
3503.641084	446987.684353	50.025242
3503.384344	446994.928994	50.030247
3503.634285	446983.780826	50.035252
3503.452933	446984.775271	50.040257
3503.401312	446997.005174	50.045261
3503.646666	446980.736083	50.050266
3503.606216	446989.414385	50.055271
3503.452083	446982.442717	50.060276
3503.595296	446984.903042	50.065281
3503.564809	446994.796679	50.070285
3503.741925	446987.971293	50.075290
3503.748067	446977.270430	50.080295
3503.390757	446964.653928	50.085300
3503.811641	446954.490757	50.090305
3503.364399	446967.548879	50.095309
3503.579563	446967.664261	50.100314
3503.492286	446964.433712	50.105319
3503.369480	446956.645326	50.110324
3503.855637	446968.935552	50.115329
3503.786760	446958.703878	50.120333
3503.606389	446959.191056	50.125338
3503.556427	446958.793896	50.130343
3503.896579	446946.666815	50.135348
3504.113898	446927.207736	50.140353
3503.583362	446927.501154	50.145357
3503.952029	446918.817475	50.150362
3503.775752	446914.080811	50.155367
3503.734450	446911.653766	50.160372
3503.443571	446892.332139	50.165377
3503.422535	446883.664276	50.170381
3503.347239	446877.287634	50.175386
3503.411636	446883.361855	50.180391
3503.306186	446878.308829	50.185396
3503.650883	446877.235758	50.190401
3503.378154	446880.324929	50.195405
3503.638006	446873.079697	50.200410
3503.498312	446883.701977	50.205415
3503.489856	446883.703410	50.210420
3503.906907	446872.171679	50.215425
3503.554431	446886.481426	50.220429
3503.557743	446880.395625	50.225434
3503.417011	446882.803024	50.230439
3503.366748	446880.580347	50.235444
3503.838731	446882.376025	50.240449
3503.483143	446879.546248	50.245453
3503.566487	446883.335274	50.250458
3503.490870	446887.557122	50.255463
3503.627217	446879.217356	50.260468
3503.583938	446863.149589	50.265473
3503.347580	446856.800443	50.270477
3503.759498	446837.713737	50.275482
3503.550372	446843.276859	50.280487
3503.122693	446848.877296	50.285492
3503.594463	446833.380798	50.290497
3503.272583	446837.543284	50.295501
3503.631552	446832.461659	50.300506
3503.519045	446842.014399	50.305511
3503.331580	446845.748251	50.310516
3503.633425	446837.836603	50.315521
3503.238369	446841.960873	50.320525
3503.329004	446833.071081	50.325530
3503.314575	446841.795710	50.330535
3503.015746	446849.199718	50.335540
3503.274871	446841.751759	50.340545
3503.298057	446843.066258	50.345549
3503.580127	446837.389240	50.350554
3503.671717	446844.016642	50.355559
3503.536617	446844.090411	50.360564
3503.614032	446835.659270	50.365569
3503.196127	446848.306773	50.370573
3503.581957	446841.344282	50.375578
3503.667381	446839.047722	50.380583
3503.188699	446845.265393	50.385588
3503.251690	446843.682608	50.390593
3503.339125	446845.188978	50.395597
3503.544528	446846.066681	50.400602
3503.530759	446845.308367	50.405607
3503.378404	446844.776558	50.410612
3503.927215	446835.859245	50.415617
3503.705807	446845.024897	50.420621
3504.121804	446839.984246	50.425626
3504.144846	446826.187091	50.430631
3503.435595	446813.782723	50.435636
3503.978531	446804.308587	50.440641
3503.749704	446808.404480	50.445645
3503.481149	446804.190651	50.450650
3503.408222	446800.095550	50.455655
3503.492663	446805.811398	50.460660
3503.387002	446809.886261	50.465665
3503.566752	446819.946924	50.470669
3503.746500	446803.587479	50.475674
3503.718727	446784.575801	50.480679
3503.660747	446777.080543	50.485684
3503.712070	446767.081806	50.490689
3503.509546	446771.122504	50.495693
3503.892546	446766.493154	50.500698
3503.472514	446765.398522	50.505703
3503.415363	446760.235799	50.510708
3503.633213	446764.762537	50.515713
3503.705604	446766.880007	50.520717
3503.457621	446765.096762	50.525722
3503.549515	446744.188327	50.530727
3503.294371	446735.966062	50.535732
3503.301539	446708.378263	50.540737
3503.318910	446693.060671	50.545741
3503.294362	446650.569272	50.550746
3503.049670	446601.066565	50.555751
3503.292399	446554.523177	50.560756
3503.175137	446464.936671	50.565761
3502.832376	446398.309843	50.570765
3502.556585	446306.873420	50.575770
3502.682787	446217.345726	50.580775
3502.233637	446122.388287	50.585780
3502.498256	446004.183754	50.590785
3501.744491	445897.765632	50.595789
3501.790277	445767.628989	50.600794
3501.594173	445640.271368	50.605799
3501.545858	445503.962183	50.610804
3501.416428	445337.237674	50.615809
3501.062126	445189.263824	50.620813
3501.081678	445016.019958	50.625818
3500.796294	444853.984070	50.630823
3500.087400	444675.029607	50.635828
3499.802633	444484.336583	50.640833
3499.452907	444301.057548	50.645837
3499.040473	444103.840549	50.650842
3498.734600	443893.264912	50.655847
3498.172020	443695.207626	50.660852
3497.724344	443479.631116	50.665857
3497.163241	443270.208796	50.670861
3496.727866	443061.118021	50.675866
3496.315259	442834.167995	50.680871
3495.757871	442627.934189	50.685876
3495.451633	442394.114175	50.690881
3494.920701	442166.720906	50.695885
3494.323464	441928.887885	50.700890
3494.039885	441693.687005	50.705895
3493.268409	441457.603169	50.710900
3493.083260	441216.141427	50.715905
3492.247742	440976.309799	50.720909
3491.919141	440732.026677	50.725914
3491.527238	440481.563175	50.730919
3491.042734	440236.692473	50.735924
3490.567488	439968.990605	50.740929
3489.839132	439710.662478	50.745933
3489.444884	439452.020645	50.750938
3488.865898	439178.746891	50.755943
3488.074096	438915.448955	50.760948
3487.848851	438636.578684	50.765953
3486.854625	438369.149027	50.770957
3486.520044	438097.747992	50.775962
3486.329400	437817.339641	50.780967
3485.100930	437543.446475	50.785972
3485.059691	437256.511896	50.790977
3484.310121	436984.711624	50.795981
3483.884997	436693.624543	50.800986
3483.496487	436408.057503	50.805991
3482.330096	436112.878520	50.810996
3481.565118	435822.700714	50.816001
3481.025412	435536.285949	50.821005
3480.784411	435241.850833	50.826010
3480.760100	434957.979086	50.831015
3479.665855	434655.614757	50.836020
3479.103206	434354.728548	50.841025
3478.225519	434057.596163	50.846029
3477.576821	433751.744199	50.851034
3477.258428	433456.842561	50.856039
3476.198932	433168.406389	50.861044
3475.883336	432850.358240	50.866049
3475.078962	432553.396795	50.871053
3474.335139	432252.107964	50.876058
3473.966286	431947.249806	50.881063
3473.084681	431650.239178	50.886068
3472.752234	431338.820673	50.891073
3471.567246	431031.197305	50.896077
3471.021753	430719.705380	50.901082
3470.672275	430420.406027	50.906087
3469.781024	430120.434117	50.911092
3469.609022	429805.973555	50.916097
3468.679912	429499.453510	50.921101
3467.743724	429181.816324	50.926106
3467.204980	428878.063527	50.931111
3466.338773	428573.449195	50.936116
3465.722119	428269.042075	50.941121
3465.169535	427965.076868	50.946125
3464.618743	427652.530073	50.951130
3464.214868	427342.085755	50.956135
3463.237412	427038.434986	50.961140
3462.507538	426723.622567	50.966145
3462.179406	426423.659758	50.971149
3461.478018	426105.484400	50.976154
3460.816312	425787.196518	50.981159
3460.190144	425482.247787	50.986164
3459.461397	425158.582628	50.991169
3458.330406	424851.834015	50.996173
3457.972333	424534.645170	51.001178
3457.443461	424213.725011	51.006183
3456.686328	423911.570625	51.011188
3455.856495	423596.632791	51.016193
3455.273456	423283.120856	51.021197
3454.637931	422976.416167	51.026202
3454.211075	422656.828634	51.031207
3453.214816	422343.628999	51.036212
3452.681061	422027.858867	51.041217
3451.582394	421706.139952	51.046221
3451.224212	421403.175654	51.051226
3450.715578	421087.186075	51.056231
3449.744488	420785.461109	51.061236
3449.107535	420470.856292	51.066241
3448.133583	420158.158105	51.071245
3447.292878	419847.387869	51.076250
3447.010403	419540.935472	51.081255
3446.229495	419239.032290	51.086260
3445.537907	418921.802471	51.091265
3444.894105	418615.654270	51.096269
3444.471968	418307.890506	51.101274
3443.892004	417991.112184	51.106279
3442.840458	417689.414242	51.111284
3442.181391	417380.004024	51.116289
3441.789971	417078.541475	51.121293
3440.966157	416763.439577	51.126298
3440.369363	416451.646271	51.131303
3439.475066	416138.681276	51.136308
3438.638396	415821.234112	51.141313
3438.491026	415519.457489	51.146317
3437.593860	415216.078839	51.151322
3436.954646	414893.914730	51.156327
3436.249124	414603.749678	51.161332
3435.453438	414281.299915	51.166337
3434.733872	413983.081435	51.171341
3434.020654	413666.119716	51.176346
3433.486809	413355.192052	51.181351
3432.534935	413050.959303	51.186356
3432.176671	412740.400553	51.191361
3431.475952	412441.043843	51.196365
3430.531023	412134.463081	51.201370
3430.147634	411826.767107	51.206375
3429.438370	411526.030140	51.211380
3428.338206	411205.574860	51.216385
3428.278355	410899.691883	51.221389
3427.176322	410597.081411	51.226394
3426.913748	410292.851235	51.231399
3426.147706	409989.160638	51.236404
3425.331258	409669.577845	51.241409
3424.683269	409367.332877	51.246413
3423.691767	409062.273422	51.251418
3423.550177	408752.443274	51.256423
3422.281604	408452.808102	51.261428
3422.154624	408152.796852	51.266433
3421.303497	407846.023366	51.271437
3420.273186	407540.140475	51.276442
3419.644257	407234.490333	51.281447
3418.793559	406936.544696	51.286452
3418.558273	406627.848936	51.291457
3418.067609	406319.421852	51.296461
3416.955508	406021.764769	51.301466
3416.316351	405713.381558	51.306471
3415.493733	405413.026904	51.311476
3415.027622	405110.779310	51.316481
3414.103195	404814.397764	51.321485
3413.311257	404517.787188	51.326490
3412.901465	404216.942518	51.331495
3412.125877	403920.348105	51.336500
3411.696864	403617.010919	51.341505
3410.924487	403313.932248	51.346509
3410.171670	403024.258812	51.351514
3409.636657	402715.925801	51.356519
3409.040348	402421.901087	51.361524
3408.291724	402116.112694	51.366529
3407.527781	401825.717425	51.371533
3406.835775	401518.591902	51.376538
3405.947875	401217.161325	51.381543
3405.135340	400924.453351	51.386548
3404.324156	400631.335647	51.391553
3403.501396	400326.099288	51.396557
3402.937763	400049.115453	51.401562
3402.434096	399749.737518	51.406567
3401.725316	399460.248413	51.411572
3401.247082	399170.589967	51.416577
3400.573429	398876.134992	51.421581
3399.738658	398584.245026	51.426586
3399.064478	398288.971125	51.431591
3398.223005	398012.141974	51.436596
3397.585799	397722.470617	51.441601
3397.050330	397432.194629	51.446605
3396.203337	397135.388616	51.451610
3396.059657	396843.159718	51.456615
3395.421205	396552.460572	51.461620
3394.769715	396258.051271	51.466625
3394.028192	395965.432899	51.471629
3393.241368	395663.875759	51.476634
3392.653478	395370.259689	51.481639
3391.945176	395079.481569	51.486644
3391.394782	394778.611784	51.491649
3390.709309	394486.502650	51.496653
3389.977655	394184.184033	51.501658
3389.350628	393885.350954	51.506663
3388.387672	393596.126258	51.511668
3388.068668	393295.430546	51.516673
3386.949402	393017.813830	51.521677
3386.299852	392727.053373	51.526682
3385.805547	392429.250236	51.531687
3385.042149	392143.128281	51.536692
3383.901964	391848.351923	51.541697
3383.424178	391552.265218	51.546701
3382.699568	391276.496237	51.551706
3382.726391	390984.129528	51.556711
3381.784365	390703.360897	51.561716
3380.921524	390409.209251	51.566721
3380.465717	390119.279976	51.571725
3379.931493	389824.634546	51.576730
3379.207791	389530.247349	51.581735
3378.140232	389238.609853	51.586740
3377.483196	388947.204439	51.591745
3377.090719	388656.843876	51.596749
3375.780648	388365.341162	51.601754
3375.241826	388090.731549	51.606759
3374.793037	387799.330552	51.611764
3374.144002	387510.172098	51.616769
3373.334986	387230.695965	51.621773
3372.473883	386945.406137	51.626778
3372.079468	386658.661568	51.631783
3371.231653	386385.843339	51.636788
3370.887724	386096.924675	51.641793
3370.121664	385806.499644	51.646797
3369.373983	385534.190658	51.651802
3369.398068	385235.238031	51.656807
3368.346400	384947.675113	51.661812
3368.054783	384649.584213	51.666817
3367.063909	384354.990433	51.671821
3366.163255	384067.114164	51.676826
3365.871377	383777.250421	51.681831
3364.920708	383495.096535	51.686836
3364.304301	383200.580670	51.691841
3363.761646	382907.091668	51.696845
3362.796873	382625.796785	51.701850
3362.068740	382335.994549	51.706855
3361.018146	382040.372970	51.711860
3360.306109	381767.263257	51.716865
3359.849376	381477.889974	51.721869
3359.463978	381203.626709	51.726874
3358.892099	380917.623532	51.731879
3358.613384	380633.270945	51.736884
3357.504105	380337.313493	51.741889
3356.900284	380053.443557	51.746893
3356.123690	379773.896812	51.751898
3355.546774	379473.061558	51.756903
3354.784243	379198.617194	51.761908
3354.335172	378903.373052	51.766913
3353.708125	378610.724285	51.771917
3352.915756	378329.363126	51.776922
3352.482461	378036.625397	51.781927
3351.133966	377758.405079	51.786932
3350.620050	377457.312088	51.791937
3349.944659	377173.251881	51.796941
3349.163032	376897.647887	51.801946
3348.558563	376616.291156	51.806951
3347.788360	376339.358659	51.811956
3347.297952	376053.020202	51.816961
3346.619457	375771.897940	51.821965
3346.022551	375492.462846	51.826970
3345.314618	375200.230572	51.831975
3344.785538	374928.508296	51.836980
3344.196247	374640.318925	51.841985
3343.355614	374359.670434	51.846989
3342.572202	374080.967629	51.851994
3342.032818	373787.728448	51.856999
3340.892191	373515.362171	51.862004
3340.359057	373223.744405	51.867009
3339.824826	372949.922585	51.872013
3338.505491	372670.232124	51.877018
3338.440657	372385.977273	51.882023
3337.518818	372116.817323	51.887028
3336.877089	371840.843956	51.892033
3336.336669	371560.782815	51.897037
3335.479373	371292.749779	51.902042
3335.039633	371012.489124	51.907047
3334.136872	370741.179562	51.912052
3333.933104	370458.407777	51.917057
3333.365598	370178.187818	51.922061
3332.304139	369913.713778	51.927066
3331.974971	369622.997808	51.932071
3331.112526	369350.755419	51.937076
3330.084561	369058.857390	51.942081
3329.697837	368787.419522	51.947085
3329.340967	368512.948459	51.952090
3328.468104	368226.865954	51.957095
3328.031518	367943.987108	51.962100
3327.680324	367659.947153	51.967105
3326.811521	367376.527428	51.972109
3325.837329	367108.941053	51.977114
3325.646117	366821.841120	51.982119
3324.502955	366532.511066	51.987124
3323.919114	366256.256337	51.992129
3323.534936	365976.761162	51.997133
3322.710839	365690.650646	52.002138
3321.944162	365404.706150	52.007143
3321.646718	365124.299688	52.012148
3320.994428	364846.698355	52.017153
3320.067142	364550.627549	52.022157
3319.127260	364266.484207	52.027162
3318.081070	363977.092411	52.032167
3317.811937	363705.775320	52.037172
3316.693078	363425.827165	52.042177
3316.328426	363140.407258	52.047181
3315.562960	362877.612735	52.052186
3314.936536	362586.282087	52.057191
3313.974509	362321.737007	52.062196
3313.690817	362041.381773	52.067201
3313.171783	361770.297138	52.072205
3311.882727	361487.311885	52.077210
3311.581731	361216.567652	52.082215
3311.140482	360944.115962	52.087220
3310.116654	360670.134065	52.092225
3309.900991	360400.590455	52.097229
3308.942682	360125.906832	52.102234
3308.418661	359840.744220	52.107239
3307.640846	359574.902732	52.112244
3306.567998	359295.578261	52.117249
3306.253996	359020.293641	52.122253
3305.577569	358752.674280	52.127258
3304.920779	358469.966319	52.132263
3304.057189	358203.316369	52.137268
3303.445804	357928.710920	52.142273
3302.827422	357654.613519	52.147277
3302.203192	357381.888827	52.152282
3301.832621	357108.610240	52.157287
3300.783370	356835.140480	52.162292
3300.216031	356558.330634	52.167297
3299.754305	356288.139985	52.172301
3298.836595	356008.740783	52.177306
3298.339737	355733.312371	52.182311
3297.774239	355468.552245	52.187316
3296.853761	355188.155868	52.192321
3296.582935	354917.542042	52.197325
3295.390823	354633.855918	52.202330
3295.084918	354358.411175	52.207335
3294.191009	354086.651878	52.212340
3293.482277	353810.254776	52.217345
3292.886710	353545.970881	52.222349
3292.235729	353267.270842	52.227354
3291.552979	352989.312125	52.232359
3290.861244	352723.996496	52.237364
3290.206201	352454.399095	52.242369
3289.465720	352178.581848	52.247373
3288.685346	351915.489569	52.252378
3288.248646	351627.812780	52.257383
3287.614003	351362.021008	52.262388
3286.966096	351093.202457	52.267393
3286.833633	350814.957527	52.272397
3285.498802	350546.329217	52.277402
3285.376330	350270.216102	52.282407
3284.361892	349990.615513	52.287412
3283.730976	349711.227484	52.292417
3283.251932	349430.081724	52.297421
3282.471284	349158.017406	52.302426
3281.898032	348879.224832	52.307431
3281.084907	348605.076436	52.312436
3280.125260	348325.735766	52.317441
3279.660788	348051.524404	52.322445
3278.872993	347785.762529	52.327450
3278.409521	347502.388405	52.332455
3278.095070	347233.947283	52.337460
3277.296968	346967.368158	52.342465
3276.590978	346675.888574	52.347469
3275.900778	346400.230001	52.352474
3275.494722	346119.458025	52.357479
3274.732945	345838.745075	52.362484
3273.317368	345555.343279	52.367489
3273.158264	345265.389653	52.372493
3272.672681	345005.132034	52.377498
3271.708190	344730.782446	52.382503
3270.847998	344451.502700	52.387508
3270.362903	344174.396307	52.392513
3269.835327	343898.796742	52.397517
3268.826169	343639.715005	52.402522
3268.888029	343357.472323	52.407527
3267.968338	343080.102897	52.412532
3266.961556	342801.321792	52.417537
3266.460672	342529.271947	52.422541
3265.593103	342251.125403	52.427546
3265.177173	341976.742362	52.432551
3264.292100	341705.262338	52.437556
3263.607813	341421.888757	52.442561
3262.947315	341142.377223	52.447565
3262.156877	340881.589114	52.452570
3261.873444	340598.473031	52.457575
3260.999078	340332.301708	52.462580
3260.065577	340055.909545	52.467585
3259.725246	339784.427493	52.472589
3258.769342	339511.216910	52.477594
3258.252399	339238.311540	52.482599
3257.511551	338968.547443	52.487604
3256.468481	338702.039841	52.492609
3256.201850	338433.387857	52.497613
3255.339064	338167.966286	52.502618
3254.910502	337882.492779	52.507623
3254.242410	337623.676894	52.512628
3253.449739	337351.698963	52.517633
3252.873357	337081.769362	52.522637
3252.014609	336817.103421	52.527642
3251.661646	336546.725646	52.532647
3250.821011	336283.937013	52.537652
3250.008599	336008.519738	52.542657
3249.712739	335731.587634	52.547661
3248.353991	335472.547953	52.552666
3248.140513	335197.812962	52.557671
3247.406480	334931.003743	52.562676
3246.402321	334658.742267	52.567681
3246.088322	334395.141513	52.572685
3245.092210	334137.407516	52.577690
3244.799813	333865.020352	52.582695
3244.177445	333605.234851	52.587700
3243.266192	333332.441652	52.592705
3242.844988	333072.364685	52.597709
3241.717276	332801.896238	52.602714
3241.363887	332535.798857	52.607719
3240.754507	332266.129933	52.612724
3240.012967	332009.945534	52.617729
3239.772137	331740.211037	52.622733
3238.724944	331472.343579	52.627738
3238.400945	331193.483770	52.632743
3237.572288	330928.961282	52.637748
3236.813472	330662.669466	52.642753
3236.297392	330386.816147	52.647757
3235.314281	330126.591994	52.652762
3234.857790	329860.270128	52.657767
3234.038519	329588.562314	52.662772
3233.149024	329321.497385	52.667777
3232.658102	329060.140673	52.672781
3232.214495	328794.829615	52.677786
3231.397315	328526.654132	52.682791
3230.855836	328258.710266	52.687796
3229.973474	327991.128791	52.692801
3229.818904	327718.713055	52.697805
3228.692540	327459.391906	52.702810
3228.032730	327187.263571	52.707815
3227.323076	326922.931019	52.712820
3226.472263	326658.545015	52.717825
3226.584123	326395.189674	52.722829
3225.245124	326128.390259	52.727834
3224.631757	325861.465689	52.732839
3224.640322	325594.739122	52.737844
3223.500483	325326.756659	52.742849
3223.033223	325055.985480	52.747853
3222.399931	324795.499272	52.752858
3221.588167	324512.210345	52.757863
3220.857820	324249.982032	52.762868
3220.089480	323984.271866	52.767873
3219.556683	323717.578499	52.772877
3218.606139	323457.853421	52.777882
3218.089513	323193.369518	52.782887
3217.738537	322921.296201	52.787892
3216.721973	322652.542646	52.792897
3216.539996	322383.110821	52.797901
3215.262250	322120.355969	52.802906
3214.691400	321843.300875	52.807911
3214.081474	321576.942343	52.812916
3213.329368	321318.930798	52.817921
3213.142133	321045.268560	52.822925
3212.010015	320782.992345	52.827930
3211.669032	320519.739885	52.832935
3210.855336	320249.414072	52.837940
3210.267117	319989.918176	52.842945
3209.785209	319705.609153	52.847949
3208.943838	319446.790710	52.852954
3208.066369	319172.347427	52.857959
3207.454044	318902.999831	52.862964
3206.402859	318646.123257	52.867969
3206.099552	318385.884986	52.872973
3205.294576	318124.865863	52.877978
3204.440654	317855.478887	52.882983
3204.150224	317592.180527	52.887988
3203.222899	317338.790745	52.892993
3202.670768	317066.345157	52.897997
3201.853106	316812.858296	52.903002
3201.577362	316547.669537	52.908007
3200.985346	316288.948954	52.913012
3200.139911	316016.676543	52.918017
3199.684870	315744.794602	52.923021
3198.951851	315478.177835	52.928026
3198.242340	315209.646718	52.933031
3197.463127	314945.479718	52.938036
3196.602754	314676.666829	52.943041
3196.381186	314409.016686	52.948045
3195.208401	314146.874160	52.953050
3195.008616	313890.012470	52.958055
3194.440534	313621.934847	52.963060
3194.002527	313353.579421	52.968065
3193.210520	313076.118494	52.973069
3191.940918	312813.885794	52.978074
3191.516414	312543.641139	52.983079
3190.989110	312281.356103	52.988084
3190.239498	312018.471638	52.993089
3189.616111	311738.838302	52.998093
3189.026734	311484.835117	53.003098
3188.157692	311212.803023	53.008103
3187.674097	310941.773378	53.013108
3186.817205	310678.367866	53.018113
3186.276494	310414.780131	53.023117
3185.606490	310147.700189	53.028122
3185.072098	309869.012147	53.033127
3183.947152	309602.084388	53.038132
3183.420202	309348.267049	53.043137
3182.994252	309078.799430	53.048141
3182.194734	308817.541790	53.053146
3181.640009	308547.712438	53.058151
3180.958565	308281.239049	53.063156
3180.224060	308017.854478	53.068161
3179.550820	307747.100620	53.073165
3178.670944	307496.138191	53.078170
3178.214005	307225.472922	53.083175
3177.553740	306961.282929	53.088180
3176.556019	306702.369092	53.093185
3176.308512	306424.129107	53.098189
3175.493308	306169.612525	53.103194
3174.846156	305910.152554	53.108199
3174.092732	305643.097176	53.113204
3173.327808	305375.406388	53.118209
3173.095944	305114.981875	53.123213
3172.402599	304858.148994	53.128218
3171.842428	304590.293430	53.133223
3170.951069	304312.538309	53.138228
3170.428157	304057.736250	53.143233
3169.735564	303788.882352	53.148237
3169.152326	303526.374271	53.153242
3168.203193	303259.039310	53.158247
3167.569013	302991.700657	53.163252
3166.887446	302721.950439	53.168257
3166.191064	302461.469964	53.173261
3165.359073	302197.981950	53.178266
3164.700505	301929.371180	53.183271
3164.230672	301667.423840	53.188276
3163.473297	301406.288718	53.193281
3163.080610	301139.106982	53.198285
3162.276475	300879.175056	53.203290
3161.298788	300619.373893	53.208295
3160.658854	300356.738926	53.213300
3159.990508	300096.959851	53.218305
3159.719651	299835.940890	53.223309
3158.739749	299577.410333	53.228314
3158.348297	299307.244041	53.233319
3157.445617	299045.643351	53.238324
3156.816432	298788.884058	53.243329
3156.488705	298524.051838	53.248333
3155.666065	298253.650702	53.253338
3154.875190	297994.854453	53.258343
3154.197252	297735.172495	53.263348
3153.277554	297469.292725	53.268353
3153.014846	297196.119441	53.273357
3152.390979	296945.822061	53.278362
3151.765481	296672.938502	53.283367
3151.099777	296403.371304	53.288372
3150.029625	296146.935165	53.293377
3149.659689	295872.045147	53.298381
3148.832116	295619.436700	53.303386
3148.089940	295356.729508	53.308391
3147.544380	295101.245193	53.313396
3147.026824	294836.206618	53.318401
3146.518883	294569.459677	53.323405
3145.528809	294310.866443	53.328410
3144.587148	294038.488398	53.333415
3144.203022	293771.132674	53.338420
3143.440311	293517.285930	53.343425
3142.683388	293250.934793	53.348429
3141.876565	293000.150083	53.353434
3141.624983	292730.833947	53.358439
3140.802213	292480.789265	53.363444
3139.729829	292218.258272	53.368449
3139.803916	291950.514371	53.373453
3138.907708	291704.198327	53.378458
3138.160173	291438.146921	53.383463
3137.506495	291166.578554	53.388468
3136.857080	290914.591049	53.393473
3136.138804	290650.111671	53.398477
3135.458538	290398.179277	53.403482
3134.892861	290127.051880	53.408487
3134.443552	289870.317043	53.413492
3133.315897	289607.484139	53.418497
3132.890812	289343.995899	53.423501
3132.204288	289086.765198	53.428506
3131.550717	288822.729200	53.433511
3130.901476	288563.530264	53.438516
3130.156701	288306.384326	53.443521
3129.451368	288048.874626	53.448525
3129.133156	287786.841884	53.453530
3128.245934	287521.977321	53.458535
3127.354507	287267.884748	53.463540
3126.670767	287014.290984	53.468545
3126.292343	286744.575950	53.473549
3125.301829	286492.408739	53.478554
3124.552299	286242.517253	53.483559
3124.360854	285981.732610	53.488564
3123.453234	285720.000266	53.493569
3122.907326	285459.682649	53.498573
3122.324002	285200.415036	53.503578
3121.486900	284934.849351	53.508583
3121.019314	284668.303287	53.513588
3120.239632	284420.043543	53.518593
3119.536610	284159.928680	53.523597
3118.659175	283902.135083	53.528602
3117.840844	283645.909832	53.533607
3117.406012	283383.939728	53.538612
3116.543695	283124.410537	53.543617
3115.899676	282871.897710	53.548621
3115.268677	282626.181690	53.553626
3114.779060	282360.679430	53.558631
3113.714917	282104.035228	53.563636
3113.249279	281869.240234	53.568641
3113.118699	281605.432556	53.573645
3112.512366	281348.072294	53.578650
3111.447851	281090.229642	53.583655
3111.270664	280836.360560	53.588660
3110.315884	280569.916202	53.593665
3109.683627	280305.326314	53.598669
3108.643824	280047.656121	53.603674
3107.868313	279784.566965	53.608679
3107.034823	279527.497427	53.613684
3106.252003	279288.347333	53.618689
3105.950720	279029.734569	53.623693
3105.683987	278775.877800	53.628698
3104.976094	278526.196180	53.633703
3104.493132	278263.691509	53.638708
3103.784550	278006.929568	53.643713
3103.295408	277737.039865	53.648717
3102.457044	277477.803643	53.653722
3101.771954	277221.418649	53.658727
3101.403960	276953.442652	53.663732
3100.287570	276696.570390	53.668737
3099.930097	276429.254041	53.673741
3098.779569	276172.718026	53.678746
3098.265149	275910.088278	53.683751
3097.872832	275648.074023	53.688756
3097.227436	275399.421965	53.693761
3096.361429	275132.674727	53.698765
3095.565804	274881.628369	53.703770
3094.986251	274611.317105	53.708775
3094.823318	274356.240134	53.713780
3093.452239	274096.224891	53.718785
3093.052667	273834.006013	53.723789
3092.594638	273575.769729	53.728794
3091.525936	273319.955015	53.733799
3091.010959	273052.687007	53.738804
3090.347350	272796.547875	53.743809
3089.475192	272533.007631	53.748813
3088.780020	272279.318239	53.753818
3087.738028	272020.492491	53.758823
3087.417064	271766.407601	53.763828
3086.413898	271520.996091	53.768833
3086.085525	271268.058037	53.773837
3085.465085	271017.308922	53.778842
3084.776100	270760.459082	53.783847
3084.420368	270496.930512	53.788852
3083.346404	270244.144394	53.793857
3083.014934	269996.401148	53.798861
3082.555020	269739.944241	53.803866
3081.574605	269477.845818	53.808871
3081.249561	269216.959538	53.813876
3080.286048	268961.963291	53.818881
3079.797227	268694.992325	53.823885
3079.194241	268441.920573	53.828890
3078.229738	268183.078278	53.833895
3078.114352	267930.024727	53.838900
3077.042356	267672.219136	53.843905
3076.659987	267406.960822	53.848909
3075.621473	267149.352893	53.853914
3074.908259	266890.746910	53.858919
3074.284417	266627.184725	53.863924
3073.711921	266378.053888	53.868929
3073.497480	266113.580994	53.873933
3072.336931	265855.814822	53.878938
3071.510857	265597.940423	53.883943
3070.853057	265340.801169	53.888948
3069.891769	265084.987018	53.893953
3069.612793	264832.265132	53.898957
3069.295314	264577.053833	53.903962
3068.056431	264314.741438	53.908967
3067.822254	264061.323883	53.913972
3066.659730	263815.730681	53.918977
3066.198341	263561.282058	53.923981
3065.436921	263295.449432	53.928986
3064.514911	263045.077764	53.933991
3064.246372	262796.733677	53.938996
3063.541853	262545.382342	53.944001
3062.958605	262292.940539	53.949005
3062.290203	262033.229321	53.954010
3061.541740	261783.744398	53.959015
3061.142051	261529.360872	53.964020
3060.405067	261283.312028	53.969025
3059.782235	261016.054138	53.974029
3059.191588	260763.791399	53.979034
3058.072400	260498.349994	53.984039
3057.651608	260248.961477	53.989044
3056.726752	260000.219317	53.994049
3056.107064	259734.081162	53.999053
3055.715939	259489.195282	54.004058
3055.083374	259241.600046	54.009063
3054.135464	258975.772504	54.014068
3053.561651	258725.365655	54.019073
3053.041807	258480.527083	54.024077
3052.070319	258221.172380	54.029082
3051.604438	257954.752992	54.034087
3051.282428	257698.521741	54.039092
3050.273889	257441.007010	54.044097
3049.862753	257188.254626	54.049101
3049.177143	256931.143130	54.054106
3048.487738	256676.859245	54.059111
3047.648880	256418.908006	54.064116
3046.875945	256163.212176	54.069121
3046.565491	255903.642583	54.074125
3046.062242	255643.138148	54.079130
3045.129407	255403.030725	54.084135
3044.703104	255134.745387	54.089140
3043.682429	254883.497952	54.094145
3042.982863	254615.870589	54.099149
3042.400870	254362.816433	54.104154
3041.335408	254110.175996	54.109159
3041.308728	253848.036784	54.114164
3040.302914	253604.070880	54.119169
3039.826589	253348.834043	54.124173
3038.943792	253088.267455	54.129178
3038.239722	252839.538543	54.134183
3037.577877	252584.893869	54.139188
3037.075881	252339.135792	54.144193
3036.523229	252083.784952	54.149197
3036.225502	251820.266306	54.154202
3035.239800	251570.439775	54.159207
3034.586754	251306.065144	54.164212
3033.777877	251053.559885	54.169217
3032.790105	250793.725003	54.174221
3032.425436	250540.099844	54.179226
3031.913346	250296.661721	54.184231
3031.331706	250031.282115	54.189236
3030.662720	249784.585615	54.194241
3030.244182	249519.254772	54.199245
3028.840961	249259.313221	54.204250
3028.028249	249004.542783	54.209255
3027.696277	248743.679888	54.214260
3027.032982	248511.805349	54.219265
3026.255517	248255.679453	54.224269
3025.332202	247997.617576	54.229274
3024.744441	247753.429473	54.234279
3024.147177	247501.042452	54.239284
3023.359596	247250.190695	54.244289
3022.852365	246994.732431	54.249293
3022.309391	246748.881818	54.254298
3021.507274	246507.226886	54.259303
3021.133249	246250.600270	54.264308
3020.371361	246004.099879	54.269313
3019.601927	245746.598839	54.274317
3018.995502	245500.326892	54.279322
3018.165944	245251.011630	54.284327
3017.833240	245003.012382	54.289332
3016.984863	244758.972506	54.294337
3016.233568	244498.897019	54.299341
3015.947786	244258.021252	54.304346
3015.144634	243999.457608	54.309351
3014.721182	243742.637503	54.314356
3013.514687	243475.738862	54.319361
3013.382229	243238.810618	54.324365
3012.695722	242985.474209	54.329370
3011.664993	242728.529493	54.334375
3011.588556	242470.785271	54.339380
3010.702933	242229.911700	54.344385
3010.036912	241970.434996	54.349389
3009.703363	241708.635124	54.354394
3008.533502	241451.333322	54.359399
3007.884937	241190.300859	54.364404
3006.984864	240940.466351	54.369409
3005.986488	240682.040899	54.374413
3005.798087	240441.126208	54.379418
3005.080772	240192.585506	54.384423
3004.471736	239941.759963	54.389428
3003.646624	239688.450331	54.394433
3002.920008	239435.811752	54.399437
3002.213381	239176.141071	54.404442
3001.403284	238932.456293	54.409447
3001.250169	238682.802075	54.414452
3000.872604	238443.678944	54.419457
3000.363405	238183.873786	54.424461
2999.344197	237930.752044	54.429466
2998.449503	237680.334298	54.434471
2997.897113	237413.151985	54.439476
2996.807219	237169.287747	54.444481
2996.133510	236920.921433	54.449485
2995.096516	236674.960443	54.454490
2994.897005	236434.332048	54.459495
2994.545450	236190.622957	54.464500
2993.619129	235951.596396	54.469505
2993.158141	235695.198650	54.474509
2992.370798	235441.021675	54.479514
2991.739319	235195.196967	54.484519
2990.853557	234937.013729	54.489524
2990.295319	234696.627032	54.494529
2989.644421	234448.540080	54.499533
2989.235066	234201.558191	54.504538
2988.167891	233959.629545	54.509543
2987.516880	233707.341634	54.514548
2987.080470	233462.835634	54.519553
2986.253136	233207.369780	54.524557
2985.939720	232977.282934	54.529562
2985.426391	232724.157986	54.534567
2984.678200	232468.603302	54.539572
2984.229559	232211.597177	54.544577
2983.205553	231960.241401	54.549581
2982.603738	231709.043069	54.554586
2981.681974	231453.646929	54.559591
2981.407786	231198.930001	54.564596
2980.541470	230955.443343	54.569601
2980.166562	230707.849455	54.574605
2979.331446	230447.499695	54.579610
2978.614531	230208.496156	54.584615
2978.046129	229954.009767	54.589620
2977.244096	229702.237641	54.594625
2976.597213	229449.471720	54.599629
2975.949340	229193.497697	54.604634
2975.174322	228940.474404	54.609639
2974.427863	228698.804392	54.614644
2973.719119	228447.298569	54.619649
2973.261940	228200.206693	54.624653
2972.880191	227948.875060	54.629658
2971.608296	227702.305228	54.634663
2971.009760	227437.285595	54.639668
2970.661336	227197.078042	54.644673
2969.861999	226953.968489	54.649677
2968.972740	226699.033321	54.654682
2968.455200	226460.689455	54.659687
2967.962015	226205.280094	54.664692
2966.960036	225954.058056	54.669697
2966.367857	225704.472642	54.674701
2965.845787	225466.997137	54.679706
2964.780323	225229.742231	54.684711
2964.644259	224973.382952	54.689716
2963.893237	224726.042008	54.694721
2963.260820	224471.780271	54.699725
2962.456037	224234.228012	54.704730
2962.179530	223984.082689	54.709735
2961.768983	223731.745329	54.714740
2960.476375	223485.670734	54.719745
2959.587749	223230.360309	54.724749
2959.270833	222974.163330	54.729754
2958.322250	222735.594466	54.734759
2957.734839	222490.063470	54.739764
2957.183091	222252.751919	54.744769
2956.631577	221998.023116	54.749773
2956.560607	221748.382029	54.754778
2955.460363	221495.836151	54.759783
2955.092605	221238.352918	54.764788
2954.235306	220988.618635	54.769793
2953.553809	220732.896242	54.774797
2952.800309	220483.068936	54.779802
2951.811650	220233.129578	54.784807
2951.195011	219977.321419	54.789812
2950.575462	219740.230344	54.794817
2950.049007	219490.162750	54.799821
2949.311437	219245.810230	54.804826
2948.784202	218999.206970	54.809831
2947.928556	218738.578947	54.814836
2947.274141	218489.655916	54.819841
2946.565606	218241.964963	54.824845
2945.626026	217991.029267	54.829850
2945.045538	217749.403370	54.834855
2944.930850	217501.994635	54.839860
2944.443352	217253.071456	54.844865
2943.316548	217012.151731	54.849869
2942.558318	216749.755012	54.854874
2941.721058	216512.199059	54.859879
2941.351501	216262.876178	54.864884
2940.353498	216026.571056	54.869889
2939.740782	215776.934440	54.874893
2939.660525	215531.001444	54.879898
2938.858354	215283.537319	54.884903
2938.219907	215031.131519	54.889908
2937.651901	214777.797674	54.894913
2936.681950	214531.535397	54.899917
2935.882309	214276.689211	54.904922
2935.135918	214036.399169	54.909927
2934.669706	213784.374582	54.914932
2933.612049	213555.164184	54.919937
2933.094410	213305.339421	54.924941
2932.239497	213056.107655	54.929946
2931.743566	212821.990690	54.934951
2931.296816	212574.625594	54.939956
2930.785575	212333.484923	54.944961
2929.889345	212086.427092	54.949965
2929.400004	211836.652362	54.954970
2928.378243	211600.565926	54.959975
2928.036511	211345.878642	54.964980
2927.356653	211109.989685	54.969985
2926.565969	210852.223254	54.974989
2926.064859	210603.727030	54.979994
2925.410837	210363.481699	54.984999
2924.901825	210122.091940	54.990004
2924.295371	209877.384054	54.995009
2923.539223	209627.279172	55.000013
2923.011283	209371.356317	55.005018
2921.901007	209131.497867	55.010023
2921.554765	208875.876431	55.015028
2920.875364	208636.098511	55.020033
2920.312668	208387.517301	55.025037
2919.164696	208136.236131	55.030042
2918.429904	207888.755150	55.035047
2917.775635	207642.445065	55.040052
2917.337176	207405.837526	55.045057
2916.448408	207158.334102	55.050061
2915.967812	206924.968628	55.055066
2915.010541	206672.729987	55.060071
2914.682086	206441.376727	55.065076
2913.976088	206201.330302	55.070081
2913.402457	205948.404576	55.075085
2912.962368	205707.143015	55.080090
2911.629502	205457.760218	55.085095
2911.283783	205210.984661	55.090100
2910.582738	204972.723264	55.095105
2910.317597	204729.627118	55.100109
2909.361766	204476.567694	55.105114
2908.307746	204242.467835	55.110119
2907.985219	203988.028797	55.115124
2907.149091	203752.340149	55.120129
2906.296409	203516.069482	55.125133
2905.798701	203274.736130	55.130138
2905.181530	203050.468915	55.135143
2904.777130	202799.535714	55.140148
2903.954172	202560.984328	55.145153
2903.252116	202315.704590	55.150157
2902.892341	202074.669722	55.155162
2901.607092	201828.511060	55.160167
2901.454765	201588.206080	55.165172
2901.011807	201344.374595	55.170177
2900.050701	201106.233340	55.175181
2899.749759	200848.860719	55.180186
2898.803127	200613.824526	55.185191
2898.200144	200368.114247	55.190196
2897.021622	200127.658437	55.195201
2896.550765	199879.330498	55.200205
2895.954247	199637.974941	55.205210
2895.245158	199399.681661	55.210215
2894.434842	199156.849510	55.215220
2894.148788	198917.887295	55.220225
2893.351132	198679.280613	55.225229
2892.773132	198443.195698	55.230234
2891.895505	198203.433244	55.235239
2891.290384	197955.325915	55.240244
2890.451147	197714.272981	55.245249
2889.816791	197483.177862	55.250253
2889.209808	197235.633486	55.255258
2888.600360	197008.074256	55.260263
2887.742100	196753.955705	55.265268
2887.296264	196524.473579	55.270273
2886.330032	196288.398728	55.275277
2885.865512	196038.657792	55.280282
2885.031992	195807.678753	55.285287
2884.430686	195565.701772	55.290292
2883.879250	195342.554944	55.295297
2883.293739	195098.260419	55.300301
2882.988756	194854.886196	55.305306
2882.324949	194627.369762	55.310311
2881.562596	194375.509446	55.315316
2880.854274	194139.423597	55.320321
2880.267580	193899.868539	55.325325
2879.630061	193645.864134	55.330330
2878.726294	193412.538093	55.335335
2878.236999	193156.359271	55.340340
2877.565270	192919.927959	55.345345
2876.647988	192684.519514	55.350349
2876.183341	192428.695764	55.355354
2875.636727	192193.913087	55.360359
2874.876656	191952.625778	55.365364
2874.465471	191710.516123	55.370369
2873.528757	191471.768164	55.375373
2872.912370	191211.953390	55.380378
2872.269032	190976.733597	55.385383
2871.973263	190739.915294	55.390388
2871.120952	190500.991177	55.395393
2870.040703	190240.967002	55.400397
2869.893768	189999.086126	55.405402
2868.821795	189764.224195	55.410407
2868.696487	189507.285374	55.415412
2867.486583	189267.816271	55.420417
2866.721683	189026.770290	55.425421
2866.603138	188785.742092	55.430426
2865.327679	188546.541592	55.435431
2865.065053	188297.547495	55.440436
2864.242426	188054.160820	55.445441
2863.169762	187823.824574	55.450445
2862.788773	187573.224712	55.455450
2862.118015	187344.705198	55.460455
2861.158307	187101.294957	55.465460
2860.814058	186860.338585	55.470465
2860.308348	186631.093687	55.475469
2859.548218	186386.621472	55.480474
2858.650068	186151.324122	55.485479
2858.192369	185903.277063	55.490484
2857.306584	185670.537543	55.495489
2856.510122	185435.009390	55.500493
2855.734562	185186.497965	55.505498
2855.495622	184956.068779	55.510503
2854.818689	184719.746858	55.515508
2853.921614	184484.494343	55.520513
2853.204524	184253.640676	55.525517
2852.672178	184013.313781	55.530522
2852.143441	183785.064106	55.535527
2851.634925	183544.047953	55.540532
2851.171752	183304.335840	55.545537
2850.469028	183065.709198	55.550541
2849.706507	182809.354304	55.555546
2849.040486	182579.771391	55.560551
2848.404741	182335.180898	55.565556
2847.769583	182097.501308	55.570561
2846.651158	181855.324194	55.575565
2846.218621	181611.453006	55.580570
2845.444302	181381.295535	55.585575
2844.841457	181137.557379	55.590580
2844.140000	180899.499871	55.595585
2843.136615	180667.564884	55.600589
2842.761445	180424.821780	55.605594
2842.280935	180190.967096	55.610599
2841.638471	179954.010777	55.615604
2841.148517	179712.384870	55.620609
2840.145481	179481.256646	55.625613
2839.941060	179235.613975	55.630618
2838.777732	179007.161969	55.635623
2838.550684	178766.411642	55.640628
2838.428174	178520.911007	55.645633
2837.136940	178275.471274	55.650637
2836.786736	178029.362911	55.655642
2835.641348	177794.232799	55.660647
2834.999746	177542.705045	55.665652
2834.245326	177306.047044	55.670657
2833.567107	177072.494547	55.675661
2832.922772	176821.874205	55.680666
2832.446516	176589.918091	55.685671
2831.622600	176342.626335	55.690676
2830.639733	176108.977619	55.695681
2830.546846	175866.360206	55.700685
2830.062834	175621.647738	55.705690
2829.016903	175386.130009	55.710695
2828.011742	175149.423109	55.715700
2827.916233	174921.341228	55.720705
2827.041030	174676.611156	55.725709
2826.542573	174424.412788	55.730714
2825.428785	174193.174680	55.735719
2824.985985	173949.710267	55.740724
2824.585364	173707.461292	55.745729
2823.670579	173463.138410	55.750733
2823.136259	173234.770310	55.755738
2822.377539	172996.937393	55.760743
2822.102256	172751.872620	55.765748
2821.243042	172509.606159	55.770753
2819.938790	172273.740296	55.775757
2819.856712	172029.549489	55.780762
2818.947116	171798.847635	55.785767
2818.599813	171561.587604	55.790772
2817.933528	171326.482513	55.795777
2816.836673	171090.803300	55.800781
2816.426250	170844.613558	55.805786
2815.823128	170607.681881	55.810791
2815.129736	170369.176501	55.815796
2814.329174	170129.532896	55.820801
2813.526978	169895.946639	55.825805
2812.599519	169650.156808	55.830810
2812.381525	169422.579779	55.835815
2811.846965	169188.480586	55.840820
2810.997433	168952.591686	55.845825
2810.409943	168714.585508	55.850829
2810.012522	168477.960209	55.855834
2809.109605	168242.274874	55.860839
2808.593722	168005.392357	55.865844
2807.831823	167764.062309	55.870849
2806.891068	167529.061349	55.875853
2806.126240	167292.021509	55.880858
2805.599953	167058.580511	55.885863
2805.003864	166820.165800	55.890868
2804.611124	166579.236903	55.895873
2803.531239	166354.379347	55.900877
2803.038904	166111.892506	55.905882
2802.545341	165883.286079	55.910887
2801.232606	165644.949154	55.915892
2800.564556	165406.808633	55.920897
2800.086460	165182.871789	55.925901
2799.383164	164943.912891	55.930906
2798.622869	164724.428044	55.935911
2798.039357	164489.089310	55.940916
2797.920398	164258.938849	55.945921
2796.935575	164033.822321	55.950925
2796.524204	163793.725761	55.955930
2795.466682	163554.402408	55.960935
2795.017615	163323.206564	55.965940
2794.166599	163088.595227	55.970945
2793.526081	162868.870205	55.975949
2793.385489	162626.049780	55.980954
2792.541390	162397.534027	55.985959
2791.954779	162159.791499	55.990964
2791.476241	161922.451576	55.995969
2790.706841	161683.547221	56.000973
2789.953590	161441.614082	56.005978
2789.464959	161213.896103	56.010983
2788.530019	160970.928203	56.015988
2788.006059	160725.474698	56.020993
2787.042989	160491.698013	56.025997
2786.628916	160251.367226	56.031002
2785.798224	160027.606263	56.036007
2785.064117	159784.470924	56.041012
2784.519354	159544.420888	56.046017
2783.537740	159319.621050	56.051021
2783.350399	159077.363035	56.056026
2782.039517	158843.311527	56.061031
2781.443260	158608.732194	56.066036
2780.917425	158391.490940	56.071041
2780.388607	158158.479787	56.076045
2780.249551	157914.019909	56.081050
2779.048047	157682.805294	56.086055
2778.553241	157450.873423	56.091060
2778.245941	157215.540360	56.096065
2777.342660	156980.246907	56.101069
2776.538513	156738.108006	56.106074
2775.744823	156502.862167	56.111079
2774.950463	156267.337998	56.116084
2774.492242	156035.522374	56.121089
2773.619752	155811.893121	56.126093
2773.269942	155573.295504	56.131098
2772.401435	155344.619041	56.136103
2771.708286	155120.225324	56.141108
2771.281439	154870.923731	56.146113
2770.116800	154648.419183	56.151117
2769.482015	154411.263423	56.156122
2768.849091	154190.934327	56.161127
2768.312353	153960.263263	56.166132
2768.094247	153738.047158	56.171137
2767.088789	153500.693112	56.176141
2766.619514	153260.183952	56.181146
2765.603634	153048.053110	56.186151
2765.122075	152805.386874	56.191156
2764.582499	152568.976208	56.196161
2763.868728	152347.323195	56.201165
2763.225667	152107.334051	56.206170
2762.327340	151876.050283	56.211175
2761.672982	151640.364293	56.216180
2761.491795	151410.283297	56.221185
2760.625517	151192.630582	56.226189
2760.027017	150949.105722	56.231194
2759.347247	150721.263157	56.236199
2759.057406	150489.107977	56.241204
2758.025589	150242.609674	56.246209
2757.466369	150008.252630	56.251213
2756.590015	149772.628726	56.256218
2755.405024	149540.403393	56.261223
2754.760203	149317.268221	56.266228
2754.628154	149079.308798	56.271233
2753.618571	148860.206067	56.276237
2753.326334	148613.363038	56.281242
2752.655463	148387.185982	56.286247
2751.609536	148164.088020	56.291252
2751.439847	147931.711770	56.296257
2750.410065	147709.974327	56.301261
2750.073187	147474.298000	56.306266
2749.458250	147249.262650	56.311271
2748.709298	147013.354490	56.316276
2747.997777	146779.984489	56.321281
2747.190489	146544.178289	56.326285
2746.519217	146315.572538	56.331290
2745.828024	146088.103248	56.336295
2745.099357	145851.194542	56.341300
2744.487405	145615.831347	56.346305
2743.676647	145399.435991	56.351309
2743.464022	145166.079951	56.356314
2742.458773	144940.209933	56.361319
2741.961453	144707.935364	56.366324
2741.166299	144471.491968	56.371329
2740.319283	144254.067019	56.376333
2740.039675	144012.007738	56.381338
2739.434637	143790.551918	56.386343
2738.346318	143558.474721	56.391348
2738.041620	143334.961531	56.396353
2736.987924	143102.054946	56.401357
2736.676222	142872.443107	56.406362
2736.005331	142651.297981	56.411367
2735.466876	142423.609427	56.416372
2734.647929	142180.103589	56.421377
2733.891135	141962.537247	56.426381
2733.426786	141730.835676	56.431386
2732.586483	141496.822460	56.436391
2731.735244	141274.356386	56.441396
2731.325160	141038.836067	56.446401
2730.660370	140812.221944	56.451405
2730.021400	140577.328638	56.456410
2729.065001	140347.868763	56.461415
2728.448752	140124.327338	56.466420
2727.710458	139893.714428	56.471425
2727.289199	139674.337802	56.476429
2726.678858	139438.938743	56.481434
2725.825452	139220.299898	56.486439
2725.079791	138998.275197	56.491444
2724.546394	138779.063231	56.496449
2723.609808	138555.993444	56.501453
2722.970483	138323.962987	56.506458
2722.284061	138100.166934	56.511463
2721.804152	137877.341301	56.516468
2721.441556	137645.064740	56.521473
2720.512165	137425.407891	56.526477
2719.554702	137203.990305	56.531482
2718.953770	136975.000561	56.536487
2718.314099	136758.298476	56.541492
2717.786699	136531.828778	56.546497
2717.125615	136313.823896	56.551501
2716.500766	136079.708824	56.556506
2716.099066	135864.675119	56.561511
2715.171679	135643.173611	56.566516
2714.505352	135404.735772	56.571521
2713.873216	135191.093142	56.576525
2713.381421	134967.665822	56.581530
2712.411274	134738.767071	56.586535
2711.696852	134522.753118	56.591540
2711.363274	134295.566262	56.596545
2710.322153	134074.425063	56.601549
2710.028110	133843.167124	56.606554
2709.352801	133614.645167	56.611559
2708.512078	133389.127298	56.616564
2708.208399	133161.116928	56.621569
2707.136891	132939.645332	56.626573
2706.456061	132705.881282	56.631578
2706.048702	132491.035579	56.636583
2705.407448	132270.664286	56.641588
2704.729640	132041.098756	56.646593
2703.505747	131820.779237	56.651597
2703.134757	131588.978362	56.656602
2702.252437	131372.835832	56.661607
2701.707261	131158.962967	56.666612
2701.716291	130932.134809	56.671617
2700.940733	130707.424999	56.676621
2700.276577	130480.575261	56.681626
2699.877119	130260.608391	56.686631
2699.092933	130029.677271	56.691636
2698.392145	129791.819851	56.696641
2697.622388	129559.161223	56.701645
2697.050447	129329.406217	56.706650
2696.163963	129100.647068	56.711655
2695.694247	128879.087677	56.716660
2695.158926	128644.324136	56.721665
2694.135795	128419.316847	56.726669
2693.345908	128191.233986	56.731674
2692.548647	127976.764605	56.736679
2691.559662	127735.095778	56.741684
2691.221653	127521.694730	56.746689
2690.503998	127299.235658	56.751693
2689.788154	127071.440520	56.756698
2689.207260	126857.577174	56.761703
2688.306519	126634.760159	56.766708
2688.324884	126409.220693	56.771713
2687.404540	126190.641845	56.776717
2686.532544	125968.421927	56.781722
2686.135383	125742.450003	56.786727
2685.606905	125525.613297	56.791732
2684.608521	125292.097619	56.796737
2683.722255	125077.574375	56.801741
2683.466720	124861.419974	56.806746
2682.674375	124635.536377	56.811751
2681.584624	124423.022038	56.816756
2681.316410	124193.151102	56.821761
2680.603226	123978.440742	56.826765
2680.039104	123756.425544	56.831770
2679.427433	123533.937237	56.836775
2678.343998	123314.974614	56.841780
2677.978934	123092.167836	56.846785
2677.361321	122871.883563	56.851789
2676.622275	122650.312911	56.856794
2676.436504	122430.046974	56.861799
2675.330116	122203.714087	56.866804
2675.004108	121982.751134	56.871809
2674.309436	121765.677236	56.876813
2674.105691	121534.201734	56.881818
2673.066961	121308.245172	56.886823
2672.502673	121083.289180	56.891828
2671.962650	120848.179154	56.896833
2670.871066	120624.295046	56.901837
2670.566779	120400.290755	56.906842
2669.872894	120169.570233	56.911847
2668.779180	119945.691581	56.916852
2668.078869	119718.393291	56.921857
2667.373601	119501.045423	56.926861
2666.670017	119270.930661	56.931866
2666.142335	119053.987679	56.936871
2665.431455	118835.260861	56.941876
2664.881708	118605.036059	56.946881
2664.120668	118397.755012	56.951885
2663.351207	118169.819830	56.956890
2662.876142	117948.772539	56.961895
2661.939594	117731.159651	56.966900
2661.447863	117507.793702	56.971905
2660.830086	117287.067992	56.976909
2660.130386	117059.396315	56.981914
2659.556248	116839.720942	56.986919
2658.792641	116630.534617	56.991924
2658.245687	116403.261188	56.996929
2657.259699	116189.390379	57.001933
2656.676210	115961.516900	57.006938
2656.136567	115739.887668	57.011943
2655.490014	115521.759047	57.016948
2655.120050	115293.676503	57.021953
2653.949024	115079.566089	57.026957
2653.328996	114858.249552	57.031962
2652.685413	114649.107894	57.036967
2651.991059	114416.159142	57.041972
2651.566178	114199.603206	57.046977
2650.412814	113989.270565	57.051981
2650.005260	113773.235703	57.056986
2649.775013	113552.637500	57.061991
2648.484806	113335.385000	57.066996
2647.806971	113112.478733	57.072001
2647.327640	112910.155439	57.077005
2646.956950	112692.458561	57.082010
2646.165258	112464.458047	57.087015
2645.254943	112252.851992	57.092020
2644.571263	112031.530258	57.097025
2643.930641	111817.480803	57.102029
2643.114749	111608.492652	57.107034
2642.855350	111392.349074	57.112039
2641.937588	111178.758308	57.117044
2641.266913	110957.709558	57.122049
2640.863648	110746.091725	57.127053
2640.072689	110529.524949	57.132058
2639.404634	110318.793878	57.137063
2638.614516	110104.859315	57.142068
2637.993765	109884.915514	57.147073
2637.203246	109677.601286	57.152077
2636.719027	109457.929652	57.157082
2636.317819	109247.110327	57.162087
2635.449311	109039.572919	57.167092
2634.817541	108814.775383	57.172097
2634.201022	108599.476616	57.177101
2633.564424	108384.030572	57.182106
2633.160810	108168.521000	57.187111
2632.327821	107952.692829	57.192116
2631.534011	107725.925385	57.197121
2630.583411	107517.359484	57.202125
2630.241008	107297.922202	57.207130
2629.419194	107079.787761	57.212135
2628.659267	106869.098871	57.217140
2628.250091	106660.015236	57.222145
2627.140972	106441.973132	57.227149
2626.846375	106225.698383	57.232154
2626.429466	106013.662244	57.237159
2625.626182	105802.925581	57.242164
2625.063417	105575.908064	57.247169
2624.114930	105366.964728	57.252173
2623.527602	105150.494683	57.257178
2622.806852	104935.560279	57.262183
2621.681599	104719.160272	57.267188
2621.314315	104505.108568	57.272193
2620.765722	104306.517517	57.277197
2620.162519	104081.119525	57.282202
2619.652860	103872.849335	57.287207
2618.868951	103662.253205	57.292212
2618.765078	103443.530388	57.297217
2617.660238	103220.904613	57.302221
2617.121732	103007.541801	57.307226
2616.600407	102786.153160	57.312231
2615.344519	102570.554829	57.317236
2614.833228	102350.679080	57.322241
2614.281421	102157.488208	57.327245
2613.556364	101933.424429	57.332250
2613.083527	101706.056412	57.337255
2612.350905	101504.331016	57.342260
2611.733524	101284.907666	57.347265
2610.778890	101066.769004	57.352269
2610.069505	100858.398089	57.357274
2609.668741	100643.558189	57.362279
2608.809510	100437.304774	57.367284
2608.230075	100209.955317	57.372289
2607.818706	100002.194163	57.377293
2607.032799	99789.217276	57.382298
2606.663059	99568.985289	57.387303
2605.449457	99355.209089	57.392308
2605.040958	99129.572841	57.397313
2604.218023	98925.128024	57.402317
2603.411274	98708.247126	57.407322
2602.959287	98504.891156	57.412327
2602.372144	98287.316131	57.417332
2601.565127	98066.479870	57.422337
2600.770844	97856.357719	57.427341
2600.236175	97654.806247	57.432346
2599.770694	97444.345651	57.437351
2598.709588	97229.304353	57.442356
2598.390196	97014.880706	57.447361
2597.423118	96803.413090	57.452365
2596.745699	96591.878682	57.457370
2596.432662	96387.862089	57.462375
2595.196627	96180.317328	57.467380
2595.038722	95965.602030	57.472385
2593.995147	95757.456623	57.477389
2593.552049	95547.496654	57.482394
2593.012374	95337.034509	57.487399
2592.488135	95127.269624	57.492404
2591.846117	94903.322833	57.497409
2591.171383	94691.899104	57.502413
2590.478539	94486.921991	57.507418
2589.815902	94268.531273	57.512423
2588.820526	94063.222213	57.517428
2588.307278	93837.073437	57.522433
2587.321818	93637.350999	57.527437
2586.861700	93426.865938	57.532442
2586.425353	93211.904516	57.537447
2585.419349	93002.385798	57.542452
2584.574666	92797.753162	57.547457
2583.979921	92595.148307	57.552461
2583.286569	92396.915326	57.557466
2583.040060	92187.172150	57.562471
2582.283275	91977.556058	57.567476
2581.975287	91765.789943	57.572481
2581.116328	91558.822061	57.577485
2580.417045	91351.276550	57.582490
2580.249202	91129.123037	57.587495
2579.279216	90922.255654	57.592500
2578.580779	90698.445355	57.597505
2578.154927	90489.356510	57.602509
2577.410089	90271.491110	57.607514
2576.644139	90057.812883	57.612519
2575.995642	89847.371617	57.617524
2575.729006	89625.185222	57.622529
2574.808417	89407.890604	57.627533
2573.517809	89197.793160	57.632538
2573.089097	88991.604739	57.637543
2572.233365	88771.240057	57.642548
2571.497124	88560.583854	57.647553
2570.958222	88354.933649	57.652557
2569.801708	88156.376510	57.657562
2569.621658	87946.588679	57.662567
2568.946956	87737.965850	57.667572
2568.359333	87522.572807	57.672577
2567.632940	87323.619103	57.677581
2566.909771	87121.405364	57.682586
2566.417938	86903.806272	57.687591
2565.709426	86694.798605	57.692596
2565.425782	86490.802052	57.697601
2564.580825	86282.963323	57.702605
2563.503624	86070.261930	57.707610
2562.994263	85852.815009	57.712615
2562.221479	85658.533500	57.717620
2561.624457	85443.972908	57.722625
2560.889844	85246.585949	57.727629
2560.282907	85036.680990	57.732634
2559.810145	84828.892893	57.737639
2559.222598	84619.933584	57.742644
2558.310726	84412.458948	57.747649
2557.413996	84210.337761	57.752653
2557.045712	84004.924362	57.757658
2556.439973	83812.767360	57.762663
2555.653386	83546.402775	57.767668
2554.987658	83329.316701	57.772673
2554.544304	83128.148665	57.777677
2553.892436	82923.224593	57.782682
2553.568171	82713.628292	57.787687
2552.181165	82505.357358	57.792692
2552.010391	82299.322561	57.797697
2551.725433	82095.345299	57.802701
2551.182254	81875.067503	57.807706
2550.162364	81661.933222	57.812711
2549.516604	81460.027665	57.817716
2548.359923	81232.972248	57.822721
2547.643867	81031.488407	57.827725
2547.024322	80821.249275	57.832730
2546.753336	80612.982193	57.837735
2545.758459	80414.519873	57.842740
2545.258781	80193.292923	57.847745
2544.478129	79998.362205	57.852749
2543.576554	79794.237956	57.857754
2543.053647	79582.851962	57.862759
2542.300467	79377.114078	57.867764
2541.857940	79162.363034	57.872769
2541.001226	78963.724767	57.877773
2540.440946	78763.997410	57.882778
2540.103147	78550.084106	57.887783
2539.022816	78343.466476	57.892788
2538.505116	78136.538911	57.897793
2537.796668	77942.006642	57.902797
2537.209054	77737.193917	57.907802
2536.536293	77530.583785	57.912807
2535.569526	77328.706164	57.917812
2535.366391	77117.529423	57.922817
2534.280221	76921.840177	57.927821
2533.767909	76721.285509	57.932826
2533.156646	76505.244026	57.937831
2532.138749	76302.014536	57.942836
2531.862115	76103.416374	57.947841
2531.162584	75904.505428	57.952845
2530.270371	75708.616034	57.957850
2529.605786	75499.721197	57.962855
2529.086130	75297.760030	57.967860
2528.701816	75097.077524	57.972865
2527.907922	74885.318898	57.977869
2527.072270	74694.774418	57.982874
2526.539215	74487.198234	57.987879
2525.715206	74281.455574	57.992884
2525.424423	74081.387665	57.997889
2524.264475	73879.035211	58.002893
2523.501357	73673.928219	58.007898
2523.296381	73470.281223	58.012903
2522.136473	73276.646617	58.017908
2521.785062	73072.096227	58.022913
2521.081855	72867.487401	58.027917
2520.125858	72676.682857	58.032922
2519.735488	72476.792338	58.037927
2518.793563	72274.487082	58.042932
2518.320014	72067.322917	58.047937
2517.971528	71881.696685	58.052941
2517.061367	71683.227398	58.057946
2516.430761	71484.864289	58.062951
2515.584571	71284.460239	58.067956
2515.106833	71081.959847	58.072961
2514.321444	70882.151415	58.077965
2513.768694	70686.020317	58.082970
2513.524549	70485.837691	58.087975
2512.811173	70287.791265	58.092980
2512.167288	70082.107890	58.097985
2511.605306	69872.995301	58.102989
2510.754021	69671.522879	58.107994
2510.028027	69471.628518	58.112999
2509.360886	69268.625860	58.118004
2508.933689	69058.464743	58.123009
2508.017047	68851.349901	58.128013
2506.936620	68650.274857	58.133018
2506.647374	68452.572124	58.138023
2505.733900	68253.481839	58.143028
2505.172704	68046.624610	58.148033
2504.399614	67849.580679	58.153037
2503.506867	67651.601803	58.158042
2503.309843	67451.287134	58.163047
2501.872507	67265.151301	58.168052
2501.262852	67065.620762	58.173057
2500.790451	66872.052576	58.178061
2500.341172	66680.890968	58.183066
2499.669186	66480.685623	58.188071
2498.709870	66296.752168	58.193076
2498.334346	66095.054534	58.198081
2497.644949	65914.520162	58.203085
2496.917633	65722.406863	58.208090
2496.585939	65520.022636	58.213095
2495.694570	65333.239927	58.218100
2495.015523	65134.937361	58.223105
2494.211407	64941.234331	58.228109
2493.626569	64738.431829	58.233114
2493.069534	64548.765689	58.238119
2492.451476	64355.549633	58.243124
2491.926151	64166.705479	58.248129
2491.409329	63968.627008	58.253133
2490.499581	63774.090807	58.258138
2490.058553	63573.886213	58.263143
2489.198901	63384.808371	58.268148
2488.390780	63184.505474	58.273153
2487.824552	62982.065343	58.278157
2487.148501	62792.733311	58.283162
2486.792877	62586.059117	58.288167
2485.715261	62394.017134	58.293172
2485.507603	62200.389576	58.298177
2484.610629	61999.359093	58.303181
2483.776579	61810.512969	58.308186
2483.325472	61605.037269	58.313191
2482.333343	61419.460116	58.318196
2481.705364	61221.097215	58.323201
2481.035647	61029.181914	58.328205
2480.345385	60838.342880	58.333210
2479.897034	60645.480755	58.338215
2479.038900	60453.469941	58.343220
2478.672408	60261.921841	58.348225
2478.008347	60068.347902	58.353229
2477.245531	59865.287449	58.358234
2476.824388	59676.428281	58.363239
2475.802383	59477.287735	58.368244
2475.138411	59279.792468	58.373249
2474.404229	59091.055577	58.378253
2473.680619	58903.319790	58.383258
2473.056912	58707.375612	58.388263
2472.449902	58515.384369	58.393268
2472.002647	58324.146990	58.398273
2471.197606	58129.620685	58.403277
2470.276543	57951.457175	58.408282
2469.882418	57754.507132	58.413287
2468.990204	57557.029552	58.418292
2468.554168	57369.227062	58.423297
2467.880264	57174.763514	58.428301
2466.742216	56982.472038	58.433306
2466.544561	56801.375473	58.438311
2465.538883	56622.084988	58.443316
2465.224317	56423.296901	58.448321
2464.688109	56230.048033	58.453325
2463.670678	56045.417371	58.458330
2463.335718	55849.749215	58.463335
2462.548625	55668.206066	58.468340
2461.754122	55471.973930	58.473345
2461.003244	55284.422061	58.478349
2460.419026	55095.570053	58.483354
2459.816172	54903.365322	58.488359
2458.919176	54722.223306	58.493364
2458.278612	54538.074241	58.498369
2457.638532	54356.517842	58.503373
2456.962701	54168.944592	58.508378
2456.500984	53968.596881	58.513383
2455.596017	53799.241308	58.518388
2455.230066	53599.774156	58.523393
2454.753100	53414.682609	58.528397
2453.960110	53222.545585	58.533402
2453.118881	53036.107200	58.538407
2452.419016	52850.476232	58.543412
2451.630502	52666.724519	58.548417
2451.357419	52478.046838	58.553421
2450.310624	52292.607106	58.558426
2449.849193	52102.799672	58.563431
2448.739142	51915.448651	58.568436
2448.599989	51740.215531	58.573441
2448.037699	51559.697581	58.578445
2447.020317	51360.510055	58.583450
2446.443119	51166.056848	58.588455
2445.554944	50999.300354	58.593460
2444.813798	50806.614256	58.598465
2444.782681	50623.790872	58.603469
2443.710217	50445.726593	58.608474
2443.268971	50249.834112	58.613479
2442.168025	50064.234655	58.618484
2441.815486	49883.309916	58.623489
2441.359227	49698.186412	58.628493
2440.650835	49522.975420	58.633498
2440.296346	49328.002049	58.638503
2439.838988	49138.558285	58.643508
2438.878209	48949.683771	58.648513
2438.491058	48759.737693	58.653517
2437.664058	48569.216351	58.658522
2437.160317	48375.386368	58.663527
2436.076263	48185.324404	58.668532
2435.483048	47988.404038	58.673537
2434.614119	47799.395203	58.678541
2433.828593	47613.619576	58.683546
2433.221906	47427.245204	58.688551
2432.288681	47239.858219	58.693556
2431.322964	47052.709758	58.698561
2431.046863	46869.004172	58.703565
2430.263138	46696.728835	58.708570
2429.610682	46506.264504	58.713575
2428.779173	46330.429065	58.718580
2428.194434	46151.817436	58.723585
2427.648944	45975.781203	58.728589
2426.839936	45800.535689	58.733594
2426.208764	45615.427381	58.738599
2425.454952	45446.545925	58.743604
2425.033586	45277.001238	58.748609
2424.350515	45088.091796	58.753613
2423.165910	44918.025423	58.758618
2423.019641	44740.273328	58.763623
2421.856447	44566.777674	58.768628
2421.704292	44386.041233	58.773633
2420.983832	44212.827698	58.778637
2419.915350	44041.065060	58.783642
2419.568144	43862.443758	58.788647
2418.917524	43697.783409	58.793652
2417.875503	43512.920923	58.798657
2417.332545	43330.763940	58.803661
2416.576505	43167.031637	58.808666
2416.126329	43000.769722	58.813671
2415.434198	42835.778917	58.818676
2414.700623	42650.900622	58.823681
2414.313660	42486.702754	58.828685
2413.080071	42318.494666	58.833690
2412.600651	42141.248119	58.838695
2412.157101	41980.030466	58.843700
2411.397524	41805.421216	58.848705
2410.638388	41637.844009	58.853709
2409.752059	41470.166594	58.858714
2409.564222	41300.278921	58.863719
2408.502049	41142.083250	58.868724
2407.962677	40973.825507	58.873729
2407.360056	40804.465899	58.878733
2406.033743	40649.370933	58.883738
2405.494437	40480.541539	58.888743
2404.565274	40309.463375	58.893748
2403.616927	40169.485105	58.898753
2402.986419	40024.348093	58.903757
2402.220344	39885.733478	58.908762
2401.415560	39731.598331	58.913767
2400.460118	39595.759269	58.918772
2399.624440	39453.706637	58.923777
2398.982450	39310.200860	58.928781
2398.190126	39182.642077	58.933786
2397.754466	39039.989327	58.938791
2396.856349	38907.782118	58.943796
2395.864538	38774.455647	58.948801
2395.209575	38641.885937	58.953805
2394.734155	38513.983239	58.958810
2394.352365	38379.286180	58.963815
2393.461979	38253.209599	58.968820
2392.907693	38123.750139	58.973825
2392.425054	38000.722960	58.978829
2391.592581	37874.854275	58.983834
2391.257209	37735.188378	58.988839
2390.248367	37610.959371	58.993844
2389.306498	37478.953443	58.998849
2389.266801	37344.917525	59.003853
2388.056446	37220.358506	59.008858
2387.397089	37086.401941	59.013863
2386.579248	36969.011994	59.018868
2386.059387	36839.903801	59.023873
2385.653840	36720.672749	59.028877
2384.727838	36606.936605	59.033882
2384.259070	36477.752607	59.038887
2383.348229	36352.635619	59.043892
2382.465862	36225.840578	59.048897
2382.039041	36105.012754	59.053901
2381.322988	35997.488100	59.058906
2380.785573	35864.155698	59.063911
2380.293200	35741.445968	59.068916
2379.722802	35623.924254	59.073921
2379.169460	35508.985707	59.078925
2378.307967	35384.202353	59.083930
2377.430771	35259.818085	59.088935
2376.933036	35132.537695	59.093940
2376.095106	35019.356487	59.098945
2375.551699	34903.391662	59.103949
2374.789016	34771.428462	59.108954
2373.998876	34654.029697	59.113959
2373.269028	34540.905771	59.118964
2372.822745	34423.133282	59.123969
2372.071566	34307.198302	59.128973
2371.229796	34196.880162	59.133978
2370.787030	34080.507870	59.138983
2370.176231	33968.471460	59.143988
2369.367220	33846.262166	59.148993
2369.065890	33723.273955	59.153997
2368.213185	33615.460876	59.159002
2367.497301	33480.493210	59.164007
2366.964978	33371.503567	59.169012
2366.482001	33251.631405	59.174017
2365.762891	33144.314036	59.179021
2365.146101	33019.688655	59.184026
2364.484410	32905.291401	59.189031
2364.062995	32778.055661	59.194036
2363.123413	32658.129474	59.199041
2362.443278	32536.634729	59.204045
2361.753019	32422.147354	59.209050
2361.391719	32298.078099	59.214055
2360.844266	32185.491439	59.219060
2360.127407	32065.736778	59.224065
2359.645293	31933.499595	59.229069
2358.802358	31811.205525	59.234074
2357.945192	31683.115580	59.239079
2357.344804	31559.351747	59.244084
2356.414827	31446.873102	59.249089
2356.145481	31318.457474	59.254093
2355.397426	31200.020543	59.259098
2354.990520	31080.067629	59.264103
2354.290812	30958.412942	59.269108
2353.321011	30833.360115	59.274113
2353.007583	30708.518619	59.279117
2352.250668	30591.305222	59.284122
2351.687196	30462.806848	59.289127
2351.105275	30337.491879	59.294132
2350.149407	30219.046388	59.299137
2349.568719	30088.554340	59.304141
2348.766663	29979.530245	59.309146
2348.221788	29848.375843	59.314151
2347.397322	29724.422655	59.319156
2346.794028	29597.759464	59.324161
2345.980272	29479.123793	59.329165
2345.640123	29366.785213	59.334170
2344.801150	29241.113871	59.339175
2344.068262	29120.828180	59.344180
2343.404677	29007.579218	59.349185
2342.905003	28883.092406	59.354189
2342.482339	28769.341942	59.359194
2341.817566	28638.232823	59.364199
2340.991966	28519.289300	59.369204
2339.975953	28397.516479	59.374209
2339.419501	28270.595412	59.379213
2338.692949	28157.748574	59.384218
2338.528930	28031.135377	59.389223
2337.899864	27922.853537	59.394228
2337.146721	27800.603394	59.399233
2336.530676	27676.002669	59.404237
2335.483270	27547.927693	59.409242
2335.272908	27425.565208	59.414247
2334.366941	27297.793660	59.419252
2333.309767	27182.922064	59.424257
2333.107571	27055.965008	59.429261
2332.363939	26956.334000	59.434266
2331.654795	26826.308718	59.439271
2330.763774	26712.186706	59.444276
2330.188986	26587.118563	59.449281
2329.596781	26458.654273	59.454285
2328.911060	26347.554812	59.459290
2328.386753	26213.760899	59.464295
2327.900017	26099.213207	59.469300
2327.140225	25982.742580	59.474305
2326.457952	25857.856177	59.479309
2325.853536	25744.112127	59.484314
2325.073069	25623.773152	59.489319
2324.427263	25494.559764	59.494324
2323.527073	25377.396113	59.499329
2322.275859	25260.713901	59.504333
2321.716793	25145.302489	59.509338
2321.538007	25039.320799	59.514343
2321.007403	24930.325931	59.519348
2319.984103	24811.049282	59.524353
2319.347707	24693.756589	59.529357
2318.591209	24580.776696	59.534362
2318.014907	24461.068663	59.539367
2317.597602	24353.718333	59.544372
2317.027445	24226.810022	59.549377
2316.421230	24116.416447	59.554381
2315.553488	24004.468140	59.559386
2314.822539	23890.928646	59.564391
2314.131559	23774.948075	59.569396
2313.568329	23667.592172	59.574401
2312.674634	23540.601922	59.579405
2312.171427	23435.387551	59.584410
2311.636059	23323.140174	59.589415
2311.047362	23208.331765	59.594420
2310.335356	23088.542611	59.599425
2310.006875	22966.671243	59.604429
2308.921566	22859.551946	59.609434
2308.200422	22742.372381	59.614439
2307.842052	22625.005098	59.619444
2306.715746	22506.131969	59.624449
2306.344662	22384.724190	59.629453
2305.590338	22276.236518	59.634458
2305.036917	22162.646450	59.639463
2304.243171	22044.054833	59.644468
2303.721096	21927.814365	59.649473
2303.233218	21816.011394	59.654477
2302.375950	21704.250184	59.659482
2301.489989	21584.335278	59.664487
2300.977258	21472.323792	59.669492
2300.390419	21368.684139	59.674497
2299.542664	21246.741466	59.679501
2299.353145	21142.665306	59.684506
2298.478357	21015.720557	59.689511
2297.590701	20904.559458	59.694516
2296.826428	20799.880172	59.699521
2295.999118	20685.592674	59.704525
2295.567752	20569.861303	59.709530
2295.105733	20452.180443	59.714535
2294.612388	20345.547950	59.719540
2293.547716	20231.599709	59.724545
2293.145360	20115.302112	59.729549
2292.370979	20008.330910	59.734554
2291.961466	19894.789823	59.739559
2291.144369	19779.956549	59.744564
2290.552431	19667.431431	59.749569
2290.379426	19549.198392	59.754573
2289.334035	19437.155440	59.759578
2288.858702	19319.770822	59.764583
2287.643358	19198.599653	59.769588
2286.851074	19087.800874	59.774593
2286.479553	18971.425233	59.779597
2285.562338	18871.651027	59.784602
2285.188976	18747.305737	59.789607
2284.941396	18640.681463	59.794612
2283.834707	18530.853738	59.799617
2283.641307	18403.886314	59.804621
2282.543309	18304.370832	59.809626
2281.868888	18173.477279	59.814631
2281.621310	18065.807091	59.819636
2280.569283	17951.443707	59.824641
2279.730493	17835.503542	59.829645
2278.955106	17733.718674	59.834650
2278.282773	17617.974410	59.839655
2277.719826	17505.215338	59.844660
2276.671419	17407.011732	59.849665
2275.993050	17291.122180	59.854669
2275.339695	17185.968980	59.859674
2274.502157	17083.953695	59.864679
2274.314536	16972.932673	59.869684
2273.498610	16867.309825	59.874689
2272.845134	16762.761479	59.879693
2272.127646	16663.038935	59.884698
2271.607736	16558.257239	59.889703
2270.991873	16460.573161	59.894708
2270.339312	16350.122562	59.899713
2269.552098	16243.428767	59.904718
2268.836050	16133.295487	59.909722
2268.016744	16039.634557	59.914727
2267.502092	15925.046138	59.919732
2266.898881	15817.928491	59.924737
2266.493375	15720.920797	59.929742
2265.316141	15614.441539	59.934746
2264.982311	15499.869372	59.939751
2264.552899	15397.824624	59.944756
2263.357051	15300.475678	59.949761
2262.902543	15189.856665	59.954766
2262.046936	15086.108806	59.959770
2261.710938	14991.177962	59.964775
2261.288014	14881.663417	59.969780
2259.995459	14783.779343	59.974785
2259.921445	14678.585545	59.979790
2259.262171	14583.555862	59.984794
2258.353252	14462.470882	59.989799
2257.879019	14362.181642	59.994804
2256.457736	14255.974075	59.999809
2255.848232	14154.329649	60.004814
2255.336620	14066.997261	60.009818
2254.451769	13971.050456	60.014823
2253.985207	13863.688171	60.019828
2253.267596	13771.323181	60.024833
2252.989918	13673.902634	60.029838
2251.869298	13582.362963	60.034842
2251.352511	13484.363402	60.039847
2250.628494	13391.205215	60.044852
2249.564121	13303.464151	60.049857
2249.266339	13201.644285	60.054862
2248.529408	13111.319975	60.059866
2247.370045	13017.080093	60.064871
2246.863312	12934.937345	60.069876
2245.891281	12853.152681	60.074881
2245.305022	12755.752404	60.079886
2244.458589	12682.261750	60.084890
2243.658588	12601.044628	60.089895
2243.119640	12527.925552	60.094900
2242.235264	12458.463759	60.099905
2241.824844	12372.725264	60.104910
2241.064775	12301.449475	60.109914
2240.440591	12222.787597	60.114919
2239.769383	12151.020082	60.119924
2238.687892	12068.531216	60.124929
2237.973994	11990.950755	60.129934
2237.494863	11936.242795	60.134938
2236.813163	11855.271424	60.139943
2235.877935	11784.029421	60.144948
2234.885681	11715.428227	60.149953
2234.488141	11638.277245	60.154958
2233.902660	11589.192967	60.159962
2233.535211	11514.829309	60.164967
2232.719103	11451.909252	60.169972
2231.750775	11401.326807	60.174977
2231.077818	11322.636516	60.179982
2230.191783	11269.011568	60.184986
2229.732008	11193.748769	60.189991
2229.012203	11139.132034	60.194996
2227.847147	11091.462905	60.200001
2227.515449	11016.991121	60.205006
2226.897537	10961.910427	60.210010
2226.492875	10911.841391	60.215015
2225.919600	10850.250364	60.220020
2225.091605	10787.519757	60.225025
2224.673424	10725.581951	60.230030
2223.877745	10661.299550	60.235034
2223.023033	10609.780619	60.240039
2222.461686	10546.637218	60.245044
2221.677169	10497.776694	60.250049
2221.087998	10431.418642	60.255054
2220.504864	10379.010329	60.260058
2219.997758	10314.793701	60.265063
2219.117519	10257.772746	60.270068
2218.687560	10206.463674	60.275073
2217.765294	10139.721410	60.280078
2217.340710	10095.077268	60.285082
2216.517257	10033.293558	60.290087
2215.888552	9975.900386	60.295092
2215.298293	9919.109086	60.300097
2214.627719	9855.393025	60.305102
2213.880058	9796.771170	60.310106
2213.106884	9741.583716	60.315111
2212.771832	9685.427339	60.320116
2212.069093	9629.452524	60.325121
2211.526605	9564.808880	60.330126
2210.702461	9516.774856	60.335130
2209.876044	9459.733286	60.340135
2209.326511	9402.094793	60.345140
2208.599329	9352.357445	60.350145
2207.870572	9290.896869	60.355150
2207.288459	9243.280406	60.360154
2206.598992	9179.363283	60.365159
2206.022073	9118.788929	60.370164
2205.288043	9072.451712	60.375169
2204.538607	9008.615029	60.380174
2203.740125	8962.393416	60.385178
2203.009186	8905.686600	60.390183
2202.837602	8857.238044	60.395188
2201.727401	8810.035440	60.400193
2201.229383	8750.415778	60.405198
2200.863660	8698.305887	60.410202
2199.746816	8643.958184	60.415207
2199.410569	8587.635210	60.420212
2198.991863	8543.578839	60.425217
2198.807222	8479.413860	60.430222
2198.040367	8429.032139	60.435226
2197.148137	8365.036017	60.440231
2196.678575	8296.333825	60.445236
2195.605406	8244.361394	60.450241
2194.300548	8181.862239	60.455246
2194.371116	8131.873745	60.460250
2193.373319	8074.021255	60.465255
2192.878881	8028.751836	60.470260
2192.018576	7979.997187	60.475265
2191.324709	7918.393703	60.480270
2190.769071	7868.280121	60.485274
2190.002125	7816.876717	60.490279
2189.493273	7757.268109	60.495284
2188.526885	7714.671693	60.500289
2188.266707	7654.213743	60.505294
2187.545412	7605.399336	60.510298
2186.909259	7553.028211	60.515303
2186.781514	7495.123786	60.520308
2185.580018	7443.330698	60.525313
2184.829062	7382.698646	60.530318
2184.303142	7321.518126	60.535322
2183.608088	7281.940881	60.540327
2183.240178	7219.252856	60.545332
2182.531234	7168.538998	60.550337
2181.608824	7105.184100	60.555342
2181.167765	7056.246039	60.560346
2180.429532	7008.635242	60.565351
2179.811311	6945.633322	60.570356
2179.422132	6902.811615	60.575361
2178.751396	6842.876317	60.580366
2177.615747	6777.489970	60.585370
2176.728563	6731.002469	60.590375
2176.556071	6669.216682	60.595380
2175.620947	6619.028954	60.600385
2175.133599	6565.199024	60.605390
2174.363931	6513.741823	60.610394
2173.427713	6457.467318	60.615399
2172.967724	6406.714087	60.620404
2172.069385	6357.350135	60.625409
2171.646906	6304.559569	60.630414
2171.063520	6259.102654	60.635418
2170.103465	6207.754816	60.640423
2169.853811	6146.603402	60.645428
2169.097038	6099.379931	60.650433
2168.335533	6048.857885	60.655438
2168.050373	6007.541820	60.660442
2167.433768	5957.607326	60.665447
2166.620482	5895.061464	60.670452
2165.638525	5849.240320	60.675457
2165.479620	5784.113499	60.680462
2164.942954	5738.256005	60.685466
2163.567058	5683.792866	60.690471
2163.342106	5628.089068	60.695476
2162.744552	5577.860311	60.700481
2162.184406	5526.229894	60.705486
2161.271903	5464.692199	60.710490
2160.652509	5402.928508	60.715495
2160.119232	5345.813523	60.720500
2159.318577	5296.812840	60.725505
2158.734063	5235.259422	60.730510
2158.482519	5190.544026	60.735514
2157.405331	5138.634506	60.740519
2156.736486	5084.054870	60.745524
2156.020134	5036.283544	60.750529
2155.444483	4978.704101	60.755534
2154.713814	4928.939224	60.760538
2154.183090	4864.186937	60.765543
2153.236666	4820.509822	60.770548
2152.488441	4766.148591	60.775553
2151.568742	4706.010419	60.780558
2151.039796	4658.186069	60.785562
2150.190551	4613.857220	60.790567
2149.870418	4567.520697	60.795572
2149.135338	4515.580766	60.800577
2148.579229	4462.876014	60.805582
2147.959733	4408.696145	60.810586
2147.160339	4366.079335	60.815591
2146.880930	4311.254131	60.820596
2145.849112	4268.054302	60.825601
2145.487598	4211.131174	60.830606
2144.965219	4165.555311	60.835610
2144.246204	4121.490629	60.840615
2143.765212	4067.874151	60.845620
2142.803232	4017.572891	60.850625
2142.288080	3957.018566	60.855630
2141.511907	3901.896766	60.860634
2140.859062	3848.559157	60.865639
2140.531272	3792.345591	60.870644
2139.180816	3741.514694	60.875649
2138.644024	3688.254901	60.880654
2137.734237	3637.468995	60.885658
2137.100766	3586.776546	60.890663
2136.479804	3534.560535	60.895668
2135.792043	3494.212915	60.900673
2135.379651	3441.441187	60.905678
2134.712094	3395.835520	60.910682
2133.925452	3354.163629	60.915687
2133.583261	3298.485684	60.920692
2132.831233	3252.604306	60.925697
2132.124667	3202.205901	60.930702
2131.354079	3151.063755	60.935706
2130.357707	3106.042613	60.940711
2130.125115	3062.635962	60.945716
2129.463445	3012.954537	60.950721
2128.857971	2965.651361	60.955726
2128.177391	2922.030360	60.960730
2127.484474	2868.443935	60.965735
2127.073212	2803.603058	60.970740
2126.287021	2763.563129	60.975745
2125.733488	2713.700711	60.980750
2125.133077	2648.438820	60.985754
2123.923349	2601.240876	60.990759
2123.595815	2548.895830	60.995764
2123.303149	2506.337922	61.000769
2122.030393	2455.457628	61.005774
2121.277989	2408.040717	61.010778
2120.415985	2364.588886	61.015783
2120.088028	2312.855813	61.020788
2119.347542	2271.162317	61.025793
2118.923956	2219.527230	61.030798
2118.842916	2176.045781	61.035802
2117.699039	2127.449191	61.040807
2116.914395	2071.590708	61.045812
2115.874348	2034.056264	61.050817
2115.583580	1979.144776	61.055822
2114.597884	1939.915605	61.060826
2113.635594	1895.021593	61.065831
2113.575078	1846.802728	61.070836
2112.622428	1805.380065	61.075841
2112.187739	1757.982625	61.080846
2111.532090	1703.526902	61.085850
2110.689626	1656.212936	61.090855
2110.362428	1606.794954	61.095860
2109.333744	1571.222811	61.100865
2108.922329	1521.597253	61.105870
2108.207939	1464.731368	61.110874
2107.955133	1426.940573	61.115879
2107.201929	1381.152895	61.120884
2106.299431	1331.379029	61.125889
2105.493210	1268.963966	61.130894
2104.481022	1227.801710	61.135898
2103.750941	1188.595050	61.140903
2103.432403	1143.983100	61.145908
2102.291648	1104.472278	61.150913
2101.921907	1066.589456	61.155918
2101.277032	1026.792698	61.160922
2100.628501	990.031447	61.165927
2100.415634	937.862823	61.170932
2099.352341	904.293934	61.175937
2099.061487	853.277757	61.180942
2098.070819	810.042122	61.185946
2096.897296	765.830514	61.190951
2096.345828	726.889729	61.195956
2095.847915	690.714474	61.200961
2095.328988	651.945151	61.205966
2094.950555	609.632850	61.210970
2094.202868	571.416797	61.215975
2093.270254	526.070468	61.220980
2092.599538	486.471742	61.225985
2092.046802	444.016021	61.230990
2091.577621	405.189858	61.235994
2090.725479	368.281351	61.240999
2090.374073	326.259267	61.246004
2089.554742	288.107084	61.251009
2088.904615	250.841024	61.256014
2088.041944	212.849591	61.261018
2087.412672	172.244349	61.266023
2086.947260	126.836641	61.271028
2085.613651	93.145223	61.276033
2085.232372	56.996489	61.281038
2084.522169	18.834986	61.286042
2083.543280	-5.868762	61.291047
2083.074423	-39.898447	61.296052
2080.575918	-22.342767	61.301057
2075.023923	86.200377	61.306062
2075.925114	83.497914	61.311066
2076.548868	82.997680	61.316071
2077.734429	74.113821	61.321076
2077.935108	74.645909	61.326081
2077.207994	72.334847	61.331086
2076.605162	72.838587	61.336090
2075.449393	82.243491	61.341095
2074.747337	75.200586	61.346100
2073.557263	82.567895	61.351105
2072.754188	84.966989	61.356110
2072.450038	78.617834	61.361114
2071.768646	88.574338	61.366119
2071.869229	84.441776	61.371124
2071.011644	83.403501	61.376129
2070.514851	83.266632	61.381134
2069.859872	73.622369	61.386138
2068.489374	77.705683	61.391143
2067.928897	72.433355	61.396148
2066.961629	83.155169	61.401153
2066.539477	83.902336	61.406158
2066.703367	85.319363	61.411162
2066.135260	93.394206	61.416167
2065.179233	85.198738	61.421172
2063.917012	86.478394	61.426177
2063.246060	86.119088	61.431182
2062.848269	88.035590	61.436186
2061.687375	84.604698	61.441191
2061.137007	77.462826	61.446196
2061.108045	83.834991	61.451201
2060.394731	88.517187	61.456206
2060.092018	82.769338	61.461210
2059.129883	88.321821	61.466215
2058.692521	84.095754	61.471220
2057.929398	93.139045	61.476225
2056.734227	93.601610	61.481230
2056.198523	88.752128	61.486234
2055.329976	85.926072	61.491239
2054.687743	80.450236	61.496244
2054.091317	80.894070	61.501249
2053.902404	82.315786	61.506254
2053.334266	82.170990	61.511258
2052.326610	93.426277	61.516263
2052.308523	81.100291	61.521268
2051.073454	87.276933	61.526273
2050.549846	86.915715	61.531278
2050.275065	75.642938	61.536282
2048.898566	83.785001	61.541287
2048.492298	76.730190	61.546292
2048.086400	83.018019	61.551297
2047.361990	87.049641	61.556302
2046.858573	89.084471	61.561306
2045.555140	92.545691	61.566311
2045.045232	91.774779	61.571316
2044.557016	87.191901	61.576321
2043.906840	90.898210	61.581326
2043.699775	83.067250	61.586330
2042.990267	84.668798	61.591335
2042.174339	82.942118	61.596340
2041.092091	89.483000	61.601345
2040.419695	89.498533	61.606350
2039.958613	82.249027	61.611354
2039.355975	92.621913	61.616359
2039.098826	81.569135	61.621364
2038.451177	79.698019	61.626369
2037.164304	85.836552	61.631374
2037.059999	78.001834	61.636378
2035.485356	85.977670	61.641383
2035.578411	81.626143	61.646388
2034.691487	87.476013	61.651393
2034.463131	84.202971	61.656398
2033.682014	72.376179	61.661402
2031.947145	84.011234	61.666407
2032.185875	75.361558	61.671412
2031.397283	87.116583	61.676417
2030.849951	86.603905	61.681422
2030.631497	71.486800	61.686426
2029.673873	88.271832	61.691431
2028.841020	81.814967	61.696436
2027.836998	81.906568	61.701441
2027.626210	86.370577	61.706446
2027.145937	81.903576	61.711450
2025.848059	96.390343	61.716455
2025.565010	88.610668	61.721460
2024.979330	77.582908	61.726465
2024.132912	85.386815	61.731470
2023.492264	75.229738	61.736474
2022.807341	90.140970	61.741479
2022.758362	81.759969	61.746484
2021.787225	88.962740	61.751489
2020.727033	87.152718	61.756494
2020.414172	87.183330	61.761498
2019.608286	89.542651	61.766503
2018.767780	87.719919	61.771508
2018.239540	90.353049	61.776513
2017.573982	83.911383	61.781518
2016.916696	80.615402	61.786522
2016.202380	88.202907	61.791527
2015.996434	88.158786	61.796532
2015.282352	87.296492	61.801537
2014.603587	80.136724	61.806542
2014.100264	75.053171	61.811546
2013.300822	84.576334	61.816551
2012.835362	87.174648	61.821556
2011.707117	85.209698	61.826561
2010.504085	90.723265	61.831566
2010.631241	84.659138	61.836570
2010.168524	91.432721	61.841575
2009.293359	82.315977	61.846580
2008.399473	86.341068	61.851585
2007.802632	87.802170	61.856590
2007.479991	79.293517	61.861594
2006.392237	93.029109	61.866599
2006.352392	86.168583	61.871604
2005.406100	83.771081	61.876609
2004.410381	80.928107	61.881614
2003.836475	81.047581	61.886618
2002.551576	88.436255	61.891623
2002.847730	83.619743	61.896628
2001.883876	85.883330	61.901633
2000.722086	84.147137	61.906638
2001.070147	84.907815	61.911642
2000.152119	91.860726	61.916647
1999.278248	84.733938	61.921652
1998.932690	84.269640	61.926657
1998.241319	83.857391	61.931662
1997.653691	89.668305	61.936666
1996.941439	93.999025	61.941671
1995.484444	86.062551	61.946676
1994.860007	87.023529	61.951681
1994.815616	88.932081	61.956686
1994.062530	84.051902	61.961690
1993.232306	93.305218	61.966695
1992.491837	84.931587	61.971700
1991.764269	86.462419	61.976705
1991.512065	93.247754	61.981710
1991.025620	87.328060	61.986714
1990.085804	89.253999	61.991719
1989.678473	84.090082	61.996724
1988.927913	85.774840	62.001729
1988.285033	83.447803	62.006734
1987.548204	85.179552	62.011738
1986.338141	91.788883	62.016743
1985.804814	87.848439	62.021748
1985.274244	83.229002	62.026753
1984.359928	93.661914	62.031758
1984.330516	76.979780	62.036762
1983.509236	78.140212	62.041767
1983.382146	82.155711	62.046772
1982.935369	88.994459	62.051777
1981.706028	86.908657	62.056782
1981.224761	88.855627	62.061786
1980.354713	87.745292	62.066791
1979.137093	84.023348	62.071796
1979.038485	85.321465	62.076801
1978.291651	85.464997	62.081806
1978.037134	88.855745	62.086810
1976.322417	89.323128	62.091815
1975.897353	87.241846	62.096820
1975.957096	80.527309	62.101825
1975.209710	86.009909	62.106830
1974.511991	85.839923	62.111834
1973.598829	86.849502	62.116839
1972.830214	81.152548	62.121844
1972.502661	84.541974	62.126849
1971.355078	90.803924	62.131854
1971.211644	81.243875	62.136858
1970.148803	88.694038	62.141863
1969.272380	89.145516	62.146868
1968.544795	91.001998	62.151873
1967.609800	94.177587	62.156878
1967.941318	86.970919	62.161882
1966.958368	89.503819	62.166887
1966.561098	89.347171	62.171892
1966.239279	84.489536	62.176897
1965.975510	91.845638	62.181902
1964.755758	80.713208	62.186906
1963.226258	81.703096	62.191911
1962.864175	81.841601	62.196916
1962.483906	87.725987	62.201921
1961.522395	90.170750	62.206926
1961.403370	83.098390	62.211930
1960.832596	87.095845	62.216935
1959.966721	80.476494	62.221940
1958.683876	80.508441	62.226945
1957.900488	86.767299	62.231950
1957.351161	77.430234	62.236954
1956.717753	83.938554	62.241959
1956.558439	81.818130	62.246964
1955.890621	81.763814	62.251969
1955.259153	92.914098	62.256974
1955.289813	78.557641	62.261978
1954.144655	83.488578	62.266983
1953.065768	80.909305	62.271988
1952.477242	74.726834	62.276993
1951.372537	82.968464	62.281998
1951.242979	80.234688	62.287002
1950.464396	88.004893	62.292007
1950.191914	81.739936	62.297012
1949.792287	77.696894	62.302017
1948.615629	84.689313	62.307022
1947.686252	74.760453	62.312026
1946.644540	80.145778	62.317031
1946.291495	75.827149	62.322036
1945.970456	76.990429	62.327041
1945.349831	83.151577	62.332046
1945.120499	74.660131	62.337050
1944.558206	84.279697	62.342055
1943.465516	86.261003	62.347060
1942.758851	74.485048	62.352065
1941.813496	81.602890	62.357070
1941.734734	74.647985	62.362074
1940.777566	75.946137	62.367079
1939.546800	81.271046	62.372084
1938.918391	78.883912	62.377089
1938.746434	86.451663	62.382094
1937.900560	81.528557	62.387098
1936.870609	83.775040	62.392103
1936.710528	77.128900	62.397108
1936.507355	82.506958	62.402113
1935.621861	87.856484	62.407118
1935.030937	85.210317	62.412122
1933.840634	81.762779	62.417127
1933.362588	81.481801	62.422132
1932.462940	80.496139	62.427137
1931.925174	86.002091	62.432142
1931.651366	75.063497	62.437146
1930.970873	82.035772	62.442151
1930.446104	70.279231	62.447156
1929.469873	72.846904	62.452161
1928.260535	83.110423	62.457166
1927.893415	73.500629	62.462170
1927.370817	77.264853	62.467175
1926.835411	75.968208	62.472180
1926.577490	82.299799	62.477185
1925.923776	84.624020	62.482190
1925.510838	87.342427	62.487194
1924.237828	86.524449	62.492199
1923.576615	85.706805	62.497204
1922.999679	80.338634	62.502209
1922.363059	78.021588	62.507214
1921.381902	80.930354	62.512218
1920.416205	84.095017	62.517223
1919.844024	77.413198	62.522228
1919.646682	83.593906	62.527233
1919.005622	86.427519	62.532238
1918.966340	77.462661	62.537242
1917.466482	81.904045	62.542247
1916.529098	74.626312	62.547252
1916.031171	73.817051	62.552257
1915.384713	82.929591	62.557262
1915.067622	85.107414	62.562266
1914.548953	81.985490	62.567271
1914.236026	79.632412	62.572276
1912.995726	74.706528	62.577281
1911.919378	80.203568	62.582286
1911.776920	76.192717	62.587290
1910.762875	83.027065	62.592295
1910.195513	87.824824	62.597300
1909.803618	81.525828	62.602305
1909.010759	87.105815	62.607310
1908.767993	80.505399	62.612314
1907.293656	85.419240	62.617319
1906.640689	87.198229	62.622324
1906.375594	73.585112	62.627329
1905.711162	88.662563	62.632334
1905.461227	81.747204	62.637338
1904.720542	88.873853	62.642343
1903.652689	84.772244	62.647348
1903.221098	80.045497	62.652353
1902.280866	74.741061	62.657358
1902.088147	76.871950	62.662362
1901.746049	81.584989	62.667367
1900.114206	77.950114	62.672372
1899.416428	76.593624	62.677377
1898.313479	89.246340	62.682382
1898.274138	78.238428	62.687386
1897.892472	79.030389	62.692391
1897.254345	81.066565	62.697396
1896.754023	80.573885	62.702401
1895.850828	82.699616	62.707406
1894.841963	76.731163	62.712410
1894.441001	77.649577	62.717415
1894.046982	83.322377	62.722420
1893.757707	85.379001	62.727425
1892.657109	86.193301	62.732430
1891.765582	79.037985	62.737434
1890.755949	76.548322	62.742439
1890.274324	78.568382	62.747444
1889.939822	71.774860	62.752449
1889.667904	80.224535	62.757454
1889.198873	72.260398	62.762458
1887.643477	79.250119	62.767463
1887.015754	84.692124	62.772468
1886.640248	85.531977	62.777473
1885.950054	84.964417	62.782478
1885.828730	76.033335	62.787482
1884.466424	85.866737	62.792487
1883.130711	86.286677	62.797492
1883.109870	80.762984	62.802497
1882.302548	91.573895	62.807502
1881.857404	75.565246	62.812506
1881.050851	80.283930	62.817511
1881.082268	84.822943	62.822516
1880.835302	80.152636	62.827521
1879.738311	85.489405	62.832526
1878.799996	79.006409	62.837530
1878.174838	80.506707	62.842535
1877.314379	75.637819	62.847540
1876.142977	79.209899	62.852545
1875.516266	80.049704	62.857550
1875.143906	79.590001	62.862554
1874.794917	84.373295	62.867559
1874.731739	79.284722	62.872564
1874.429339	75.013882	62.877569
1872.862813	88.409036	62.882574
1872.257195	80.690097	62.887578
1871.735575	78.417724	62.892583
1870.535795	78.282726	62.897588
1869.852879	75.066151	62.902593
1868.892938	81.231276	62.907598
1868.793868	75.910829	62.912602
1868.279642	84.651817	62.917607
1867.599612	78.386335	62.922612
1867.155243	77.729356	62.927617
1865.928088	85.440129	62.932622
1865.405045	77.444184	62.937626
1864.821549	80.022832	62.942631
1864.039898	88.647740	62.947636
1863.949787	75.598745	62.952641
1862.681642	79.848138	62.957646
1862.260256	72.450959	62.962650
1861.476053	69.380788	62.967655
1860.550328	78.533210	62.972660
1860.221045	74.484856	62.977665
1859.753366	81.435725	62.982670
1858.869047	81.500563	62.987674
1858.097175	87.799693	62.992679
1857.466626	79.727013	62.997684
1857.222491	81.125419	63.002689
1856.418869	83.669495	63.007694
1855.685471	82.132007	63.012698
1854.797407	80.872417	63.017703
1854.045957	80.292053	63.022708
1853.897186	77.428549	63.027713
1852.853641	84.927920	63.032718
1852.222769	80.688016	63.037722
1851.432526	79.055654	63.042727
1850.367332	79.619181	63.047732
1850.075586	72.606780	63.052737
1849.543274	80.261831	63.057742
1849.352919	76.262338	63.062746
1848.933625	82.068929	63.067751
1847.944455	82.271702	63.072756
1847.288588	73.672857	63.077761
1846.397082	81.619483	63.082766
1845.532545	84.013727	63.087770
1844.608070	81.640945	63.092775
1843.639072	84.032930	63.097780
1843.206685	83.164702	63.102785
1842.940477	94.599058	63.107790
1842.825263	80.985173	63.112794
1842.603137	79.817300	63.117799
1841.416420	82.064568	63.122804
1840.470500	79.153508	63.127809
1839.921604	88.330278	63.132814
1839.292030	74.714403	63.137818
1838.255070	77.694699	63.142823
1837.186385	79.335617	63.147828
1836.872770	76.803462	63.152833
1836.165074	87.815606	63.157838
1836.167607	82.415410	63.162842
1835.583415	81.007523	63.167847
1834.275308	75.600654	63.172852
1833.994399	71.862565	63.177857
1832.832551	76.704011	63.182862
1832.098190	85.298328	63.187866
1831.782899	76.803841	63.192871
1831.167842	80.843219	63.197876
1830.941594	82.112255	63.202881
1829.484171	93.625682	63.207886
1829.163794	84.669055	63.212890
1828.321946	91.569871	63.217895
1827.864289	89.940608	63.222900
1827.831535	74.660724	63.227905
1826.090372	85.635744	63.232910
1825.709583	80.542305	63.237914
1824.798301	84.018579	63.242919
1824.431912	81.266516	63.247924
1824.107482	82.723658	63.252929
1823.631405	86.761759	63.257934
1822.657760	84.745535	63.262938
1821.852042	78.381177	63.267943
1821.353469	84.347774	63.272948
1820.999425	72.778747	63.277953
1819.643414	80.446838	63.282958
1819.028283	72.911506	63.287962
1818.557089	79.236953	63.292967
1817.958825	75.086999	63.297972
1817.612090	74.539235	63.302977
1816.998276	88.091908	63.307982
1815.928140	76.540796	63.312986
1815.383865	78.135810	63.317991
1814.648762	88.227029	63.322996
1814.596118	75.112030	63.328001
1813.055599	78.533336	63.333006
1812.495764	77.163125	63.338010
1811.832169	78.131611	63.343015
1811.177281	82.516869	63.348020
1811.459533	80.283801	63.353025
1809.653726	72.367214	63.358030
1809.056386	74.559833	63.363034
1808.314902	76.187799	63.368039
1807.961624	70.861511	63.373044
1807.710607	71.632704	63.378049
1807.147375	74.001057	63.383054
1805.942195	76.726732	63.388058
1805.411329	76.844784	63.393063
1804.837789	79.144248	63.398068
1804.516108	69.769455	63.403073
1803.309807	79.727745	63.408078
1802.539281	73.296980	63.413082
1801.843463	71.772413	63.418087
1801.411200	76.307072	63.423092
1800.983434	62.559983	63.428097
1800.430140	78.392447	63.433102
1799.639243	68.826764	63.438106
1798.470273	71.854914	63.443111
1797.979788	72.511559	63.448116
1797.609941	71.096214	63.453121
1797.202665	73.276839	63.458126
1796.143839	73.133136	63.463130
1795.451945	72.861129	63.468135
1794.725616	76.194844	63.473140
1794.363136	71.888506	63.478145
1793.692746	74.949373	63.483150
1792.708513	69.272379	63.488154
1791.620913	77.699774	63.493159
1791.354669	79.493130	63.498164
1790.933674	77.222497	63.503169
1790.521509	78.802804	63.508174
1789.800415	77.543472	63.513178
1788.876079	75.868541	63.518183
1788.077866	81.208674	63.523188
1787.701444	80.594152	63.528193
1787.230394	80.133578	63.533198
1786.581341	78.020381	63.538202
1785.750674	75.028433	63.543207
1784.772627	81.287451	63.548212
1784.612166	76.995493	63.553217
1783.181379	82.261893	63.558222
1782.328853	80.738484	63.563226
1781.823700	66.059682	63.568231
1781.910504	84.346324	63.573236
1781.455442	69.771443	63.578241
1780.612720	78.321144	63.583246
1779.719939	72.422462	63.588250
1778.695423	78.245768	63.593255
1778.040566	80.998468	63.598260
1777.820249	68.593452	63.603265
1777.102735	71.143724	63.608270
1776.588502	75.207694	63.613274
1775.650678	80.090948	63.618279
1774.763344	77.636830	63.623284
1774.708596	75.747987	63.628289
1773.890505	79.806320	63.633294
1773.377822	77.742815	63.638298
1772.361939	70.176593	63.643303
1771.524987	75.957544	63.648308
1770.973697	66.955976	63.653313
1770.930717	73.041188	63.658318
1769.537939	70.283967	63.663322
1769.030222	65.677236	63.668327
1768.036530	68.240421	63.673332
1767.907389	68.865636	63.678337
1767.748850	72.497712	63.683342
1766.292551	69.614788	63.688346
1765.595819	70.721968	63.693351
1764.838683	76.613205	63.698356
1764.681109	71.524609	63.703361
1764.071987	76.589242	63.708366
1763.153901	71.330785	63.713370
1762.510170	72.358243	63.718375
1761.510615	81.981969	63.723380
1761.217337	68.239109	63.728385
1760.929979	82.281024	63.733390
1760.017623	74.678144	63.738394
1759.361949	73.342890	63.743399
1757.933820	73.891958	63.748404
1757.909574	75.580753	63.753409
1757.440616	78.843990	63.758414
1756.376850	72.493802	63.763418
1756.076571	76.673527	63.768423
1755.373896	73.834940	63.773428
1755.050361	64.336534	63.778433
1753.644299	81.915885	63.783438
1753.034224	67.481609	63.788442
1752.255171	70.974342	63.793447
1751.875605	74.248334	63.798452
1751.517507	68.474875	63.803457
1751.081624	77.705720	63.808462
1749.928565	75.571007	63.813466
1749.412375	78.822196	63.818471
1748.752773	83.374836	63.823476
1748.331597	78.017542	63.828481
1746.918004	84.770281	63.833486
1746.625149	76.312623	63.838490
1746.182402	78.129865	63.843495
1745.531707	74.691098	63.848500
1744.379494	73.264761	63.853505
1743.579666	76.583033	63.858510
1742.758637	72.958684	63.863514
1742.686757	73.020313	63.868519
1742.078082	75.360133	63.873524
1742.471662	73.960606	63.878529
1741.588278	69.758798	63.883534
1740.651842	72.607441	63.888538
1739.309144	78.328491	63.893543
1738.098595	82.754361	63.898548
1737.812886	79.082229	63.903553
1737.353567	78.470054	63.908558
1736.830905	80.809763	63.913562
1736.573427	80.635530	63.918567
1735.116311	83.542084	63.923572
1734.705379	68.742570	63.928577
1733.774427	86.933362	63.933582
1733.525098	81.155105	63.938586
1733.383844	73.346084	63.943591
1731.751044	75.056705	63.948596
1731.203445	77.729480	63.953601
1730.305514	80.202871	63.958606
1730.135353	84.953990	63.963610
1729.703988	80.961798	63.968615
1728.972051	81.548848	63.973620
1728.358342	76.074508	63.978625
1727.368320	77.142277	63.983630
1726.758200	73.721832	63.988634
1726.340227	71.938166	63.993639
1725.690127	82.186541	63.998644
1724.670308	73.625526	64.003649
1724.056798	74.185208	64.008654
1723.673263	72.426832	64.013658
1723.449277	72.843682	64.018663
1722.115304	83.687868	64.023668
1721.324081	79.681861	64.028673
1721.046214	79.132583	64.033678
1720.303690	81.777137	64.038682
1719.996790	74.639852	64.043687
1718.445124	78.559251	64.048692
1718.049156	79.845489	64.053697
1717.671899	73.496259	64.058702
1717.202907	76.382153	64.063706
1716.774054	73.894200	64.068711
1715.011376	76.588582	64.073716
1714.607253	64.447915	64.078721
1714.368723	76.210260	64.083726
1713.810592	83.222791	64.088730
1713.189868	77.585056	64.093735
1712.170405	73.087606	64.098740
1711.523518	72.312143	64.103745
1711.447525	72.332242	64.108750
1710.689981	71.413880	64.113754
1709.571754	72.409646	64.118759
1708.431645	79.788193	64.123764
1707.802673	73.487956	64.128769
1707.308923	70.747437	64.133774
1707.003193	80.464409	64.138778
1707.207938	74.001383	64.143783
1706.217861	76.617248	64.148788
1705.133305	67.452743	64.153793
1704.189170	78.256668	64.158798
1703.898298	76.801765	64.163802
1703.074489	66.893599	64.168807
1701.900149	78.023085	64.173812
1701.854798	68.806279	64.178817
1701.053402	77.040639	64.183822
1700.822726	70.797377	64.188826
1699.700661	75.077065	64.193831
1698.891982	81.757091	64.198836
1698.979098	73.086800	64.203841
1698.245232	80.372546	64.208846
1696.917658	77.604582	64.213850
1696.478002	65.503550	64.218855
1695.661350	75.552274	64.223860
1695.284549	65.840372	64.228865
1694.632815	75.725093	64.233870
1693.402740	78.727011	64.238874
1692.700819	67.851852	64.243879
1691.992584	77.275344	64.248884
1692.164030	79.237349	64.253889
1691.793041	75.309433	64.258894
1690.804836	76.404133	64.263898
1690.091313	66.064619	64.268903
1689.284749	79.423695	64.273908
1688.625506	74.606071	64.278913
1687.415392	80.734293	64.283918
1686.806895	80.865642	64.288922
1686.723627	73.169462	64.293927
1686.004997	84.990280	64.298932
1685.612764	74.291851	64.303937
1684.678565	77.552600	64.308942
1683.889191	77.080589	64.313946
1683.303158	71.744411	64.318951
1682.908339	83.221674	64.323956
1681.887236	72.817164	64.328961
1680.676896	80.564952	64.333966
1679.986365	77.873502	64.338970
1679.714392	74.901229	64.343975
1679.471592	87.614001	64.348980
1679.290494	78.035571	64.353985
1678.333809	76.743153	64.358990
1677.339481	71.115675	64.363994
1676.970148	63.251357	64.368999
1676.043622	78.544156	64.374004
1675.369734	65.199588	64.379009
1674.771617	70.069325	64.384014
1673.706443	68.196685	64.389018
1673.306020	66.299502	64.394023
1672.720638	69.081372	64.399028
1671.713820	72.343891	64.404033
1670.975301	73.617700	64.409038
1670.183225	79.952666	64.414042
1670.010126	73.611532	64.419047
1669.691184	81.865571	64.424052
1669.471711	73.690224	64.429057
1668.315635	67.855177	64.434062
1667.291895	75.483406	64.439066
1667.294757	71.762298	64.444071
1665.965000	79.518681	64.449076
1665.179048	73.904099	64.454081
1664.550229	76.188165	64.459086
1663.936105	80.847498	64.464090
1663.697208	70.458347	64.469095
1662.817811	77.367965	64.474100
1662.086890	70.996767	64.479105
1661.532257	71.720056	64.484110
1660.522497	73.261717	64.489114
1660.435847	72.122775	64.494119
1659.800539	74.019550	64.499124
1658.790970	64.885649	64.504129
1658.283755	71.699604	64.509134
1657.610140	69.313539	64.514138
1656.512222	71.399997	64.519143
1655.717196	75.927267	64.524148
1655.298123	69.122199	64.529153
1654.688145	77.788389	64.534158
1654.251678	79.720610	64.539162
1654.121647	78.953415	64.544167
1653.025162	84.183953	64.549172
1652.602364	70.895493	64.554177
1651.969852	69.203019	64.559182
1650.888848	71.722352	64.564186
1650.293332	70.633780	64.569191
1649.810486	75.801543	64.574196
1649.363947	64.748491	64.579201
1647.788222	72.766427	64.584206
1646.912378	75.739709	64.589210
1646.750365	74.248945	64.594215
1645.820612	77.061724	64.599220
1645.911008	70.682608	64.604225
1645.518585	78.610551	64.609230
1644.857298	75.557278	64.614234
1643.694636	73.085963	64.619239
1643.016980	81.216263	64.624244
1642.581014	69.692870	64.629249
1641.662088	72.583529	64.634254
1640.653735	72.321488	64.639258
1640.509659	67.973453	64.644263
1640.007072	75.351854	64.649268
1638.968903	73.068436	64.654273
1637.983281	76.570480	64.659278
1637.549880	82.304888	64.664282
1637.213005	68.465703	64.669287
1636.666048	74.747277	64.674292
1635.659189	72.346403	64.679297
1635.168237	75.219481	64.684302
1634.264680	68.788626	64.689306
1634.099219	74.837162	64.694311
1632.656343	78.310881	64.699316
1631.693087	67.125608	64.704321
1631.901811	71.824910	64.709326
1631.370296	76.827721	64.714330
1631.054609	70.372447	64.719335
1629.886705	71.742633	64.724340
1629.334319	71.608609	64.729345
1628.880595	78.051064	64.734350
1627.791682	72.118879	64.739354
1627.492923	64.697995	64.744359
1626.255352	70.993546	64.749364
1626.016007	66.722207	64.754369
1624.963104	68.500982	64.759374
1623.646011	69.409619	64.764378
1623.130279	71.336459	64.769383
1622.617823	74.993574	64.774388
1622.594210	71.496066	64.779393
1622.019907	71.504734	64.784398
1621.543877	71.780782	64.789402
1621.186051	69.091221	64.794407
1619.889558	76.682057	64.799412
1619.336358	73.071108	64.804417
1618.924344	69.404420	64.809422
1617.716060	72.855760	64.814426
1617.075571	67.349317	64.819431
1616.377130	67.050825	64.824436
1616.064021	65.599340	64.829441
1615.712627	68.701944	64.834446
1614.511435	72.242855	64.839450
1614.057971	70.566322	64.844455
1612.992579	72.303819	64.849460
1612.862054	71.041340	64.854465
1611.858295	67.689067	64.859470
1610.878777	71.152966	64.864474
1610.274192	65.864581	64.869479
1609.822952	72.323581	64.874484
1609.712235	74.832001	64.879489
1608.893795	70.598976	64.884494
1607.630779	63.679409	64.889498
1607.476953	61.082433	64.894503
1606.973141	68.842732	64.899508
1605.927360	70.355832	64.904513
1605.135948	72.080390	64.909518
1604.152545	69.754452	64.914522
1604.667473	64.593810	64.919527
1603.789824	67.430439	64.924532
1602.863138	64.154974	64.929537
1602.153446	66.354206	64.934542
1601.183361	69.835439	64.939546
1601.099599	59.646325	64.944551
1599.779390	66.342842	64.949556
1598.948230	70.608287	64.954561
1598.765228	69.019675	64.959566
1598.413381	74.067525	64.964570
1598.048878	67.657319	64.969575
1596.719125	71.919279	64.974580
1596.003595	70.383512	64.979585
1595.690702	71.881713	64.984590
1594.631021	71.782011	64.989594
1593.622045	68.949688	64.994599
1592.959872	73.814605	64.999604
1592.489820	69.257897	65.004609
1592.463735	69.472341	65.009614
1591.568995	66.935059	65.014618
1591.565685	67.588082	65.019623
1590.235248	68.887018	65.024628
1589.884677	64.931939	65.029633
1589.081562	73.127127	65.034638
1587.410577	73.627017	65.039642
1587.238424	66.016716	65.044647
1586.273934	77.362920	65.049652
1585.952351	71.094967	65.054657
1585.825936	70.041776	65.059662
1585.213722	76.761605	65.064666
1584.374722	70.314977	65.069671
1583.182509	76.606327	65.074676
1583.025502	74.670257	65.079681
1582.550352	68.003476	65.084686
1581.184546	71.240212	65.089690
1580.932195	67.943686	65.094695
1580.279733	74.729610	65.099700
1579.744352	71.146010	65.104705
1579.508628	65.957523	65.109710
1578.480223	75.924865	65.114714
1578.172968	63.565951	65.119719
1576.610696	76.354521	65.124724
1575.391142	68.934127	65.129729
1574.879733	67.178309	65.134734
1574.259030	74.966510	65.139738
1574.656144	62.908611	65.144743
1574.247388	66.148527	65.149748
1573.533273	67.157658	65.154753
1572.493440	63.257385	65.159758
1571.549789	70.854945	65.164762
1571.437611	60.821084	65.169767
1570.076965	65.554495	65.174772
1569.200988	71.270699	65.179777
1568.669256	59.788979	65.184782
1568.193534	71.053901	65.189786
1567.922538	57.506215	65.194791
1567.029877	66.351430	65.199796
1566.476119	73.420841	65.204801
1565.811341	61.908604	65.209806
1565.062384	72.839386	65.214810
1564.731499	64.520107	65.219815
1563.795521	76.312593	65.224820
1562.671645	77.561186	65.229825
1562.422285	74.487953	65.234830
1561.584564	71.018069	65.239834
1561.831385	72.156022	65.244839
1560.474340	77.426427	65.249844
1559.405416	72.902745	65.254849
1559.343475	72.400597	65.259854
1558.529696	77.612369	65.264858
1558.042321	74.533293	65.269863
1556.826760	74.914201	65.274868
1556.292455	65.009817	65.279873
1556.188872	66.389307	65.284878
1555.147054	79.670626	65.289882
1554.422682	65.344780	65.294887
1554.024494	72.548611	65.299892
1553.222274	74.588036	65.304897
1553.127737	74.798011	65.309902
1551.690157	77.626666	65.314906
1551.246669	71.671671	65.319911
1550.617074	74.397175	65.324916
1549.802614	72.720065	65.329921
1549.092461	69.564650	65.334926
1548.057291	73.035716	65.339930
1547.932417	69.365288	65.344935
1547.378028	73.491008	65.349940
1547.343548	74.506191	65.354945
1546.173721	65.824070	65.359950
1545.252866	78.539977	65.364954
1544.777037	70.554172	65.369959
1543.354507	79.936110	65.374964
1542.538391	78.199682	65.379969
1542.294841	72.892541	65.384974
1542.048962	79.054701	65.389978
1541.784197	70.795944	65.394983
1540.895242	79.214635	65.399988
1540.105669	76.405165	65.404993
1539.470136	75.692910	65.409998
1538.858427	77.089105	65.415002
1537.759860	74.072005	65.420007
1536.813297	83.494060	65.425012
1536.163481	76.878886	65.430017
1535.971277	76.111678	65.435022
1535.127288	75.918235	65.440026
1535.186133	66.856108	65.445031
1534.524382	77.608951	65.450036
1533.555477	73.884432	65.455041
1532.834463	69.592515	65.460046
1531.800453	75.113545	65.465050
1531.116532	69.631524	65.470055
1530.611714	71.497295	65.475060
1530.377424	73.057438	65.480065
1530.181539	71.026978	65.485070
1528.567755	69.852970	65.490074
1528.090428	58.282217	65.495079
1527.117064	73.050555	65.500084
1526.733304	71.861024	65.505089
1526.194153	70.563095	65.510094
1524.966324	83.650870	65.515098
1524.645018	71.609349	65.520103
1524.167564	75.314556	65.525108
1523.824761	74.209195	65.530113
1523.088678	77.135286	65.535118
1521.680498	71.398292	65.540122
1521.384400	68.110443	65.545127
1520.994127	70.644997	65.550132
1520.398322	72.171096	65.555137
1519.379397	63.484474	65.560142
1518.574560	76.772994	65.565146
1518.238838	59.153836	65.570151
1518.048785	69.538985	65.575156
1516.634960	69.473464	65.580161
1515.848354	65.310008	65.585166
1515.313588	73.533480	65.590170
1515.233041	67.281125	65.595175
1514.566102	68.437708	65.600180
1513.443892	68.107157	65.605185
1512.991708	69.105018	65.610190
1512.227721	67.922935	65.615194
1511.697062	65.063633	65.620199
1510.710397	69.296495	65.625204
1509.829784	64.339566	65.630209
1509.665036	66.896308	65.635214
1509.085285	72.680629	65.640218
1508.464718	64.285023	65.645223
1507.615669	59.624652	65.650228
1506.926209	62.836038	65.655233
1506.564521	63.884327	65.660238
1505.622643	63.914079	65.665242
1504.773982	62.151258	65.670247
1504.217881	66.491603	65.675252
1503.702653	71.027444	65.680257
1503.482951	62.342190	65.685262
1502.122205	68.080187	65.690266
1501.566784	59.517127	65.695271
1501.129641	65.043761	65.700276
1500.391663	71.302772	65.705281
1499.531977	63.599376	65.710286
1498.637073	72.522349	65.715290
1498.445207	63.245781	65.720295
1498.036908	65.488568	65.725300
1497.221791	67.543232	65.730305
1496.488645	62.677904	65.735310
1495.352613	67.144742	65.740314
1495.222856	57.916755	65.745319
1494.934277	65.823365	65.750324
1494.110984	72.511431	65.755329
1493.380488	58.210736	65.760334
1492.163829	64.900997	65.765338
1491.406431	64.181583	65.770343
1490.522502	66.646294	65.775348
1489.784175	66.973562	65.780353
1489.904866	63.808188	65.785358
1489.128211	65.409451	65.790362
1488.980743	60.988592	65.795367
1488.059079	60.905157	65.800372
1487.052796	62.104428	65.805377
1487.078514	55.921124	65.810382
1485.753373	61.112662	65.815386
1484.888963	56.442690	65.820391
1484.074497	64.086035	65.825396
1483.642227	59.394597	65.830401
1483.441107	59.692285	65.835406
1482.836833	76.937458	65.840410
1482.002629	70.833832	65.845415
1481.178899	73.439419	65.850420
1480.466285	70.675602	65.855425
1479.798754	66.758207	65.860430
1478.736906	69.639405	65.865434
1478.324544	60.340585	65.870439
1477.504322	65.269662	65.875444
1477.356546	70.071411	65.880449
1477.076799	63.147796	65.885454
1476.220576	70.709481	65.890458
1475.639966	61.884302	65.895463
1474.685129	64.512724	65.900468
1473.769089	71.164957	65.905473
1472.869357	65.198071	65.910478
1472.315128	68.138433	65.915482
1471.861005	61.272295	65.920487
1471.478728	67.802777	65.925492
1470.824123	67.996909	65.930497
1470.171602	63.949453	65.935502
1469.544143	61.085017	65.940506
1468.676337	58.899974	65.945511
1467.761126	70.785613	65.950516
1466.891831	69.096983	65.955521
1466.369080	64.087102	65.960526
1466.176658	72.785242	65.965530
1465.685299	69.233201	65.970535
1465.051965	63.774114	65.975540
1463.762278	75.908973	65.980545
1463.486640	60.699158	65.985550
1462.833604	67.138227	65.990554
1462.041587	63.433975	65.995559
1461.491562	60.415767	66.000564
1460.695484	64.042096	66.005569
1460.514029	64.508910	66.010574
1459.200632	69.400830	66.015578
1458.497018	64.288097	66.020583
1458.534295	64.712343	66.025588
1457.849448	56.343148	66.030593
1456.963274	60.404480	66.035598
1455.838410	67.698742	66.040602
1455.939364	67.942754	66.045607
1454.596699	64.869567	66.050612
1453.320305	67.005953	66.055617
1453.451314	58.280021	66.060622
1452.463370	60.017711	66.065626
1452.403923	59.056084	66.070631
1451.716303	62.778318	66.075636
1450.833842	74.268375	66.080641
1450.177918	71.256451	66.085646
1449.374698	67.010593	66.090650
1448.907496	65.591416	66.095655
1448.154422	61.615647	66.100660
1447.015476	70.110680	66.105665
1446.804559	62.720969	66.110670
1446.002259	76.474031	66.115674
1445.511951	63.439931	66.120679
1445.227865	71.907455	66.125684
1444.070135	70.469504	66.130689
1443.976101	61.988132	66.135694
1442.931607	61.485620	66.140698
1442.537352	63.018279	66.145703
1441.620782	66.490770	66.150708
1440.906714	62.541876	66.155713
1440.787486	55.828808	66.160718
1439.287256	64.520275	66.165722
1438.868354	62.047229	66.170727
1438.268336	70.125956	66.175732
1437.487873	63.496855	66.180737
1436.527406	62.234343	66.185742
1435.902832	64.721772	66.190746
1435.216652	61.805026	66.195751
1434.799765	63.744959	66.200756
1434.564536	71.063390	66.205761
1434.283035	59.570448	66.210766
1433.157545	64.725062	66.215770
1432.550711	62.902309	66.220775
1432.044150	62.749806	66.225780
1430.478404	63.655659	66.230785
1429.821792	60.430316	66.235790
1429.149948	62.166402	66.240794
1428.750832	58.222021	66.245799
1428.407441	54.739789	66.250804
1427.821665	64.044037	66.255809
1427.782945	59.798770	66.260814
1426.999164	67.245037	66.265818
1426.055693	62.143369	66.270823
1424.998977	57.323572	66.275828
1423.853048	58.177304	66.280833
1423.610994	59.668913	66.285838
1423.006863	64.752840	66.290842
1422.961455	55.581081	66.295847
1421.775274	58.890127	66.300852
1421.045372	58.596258	66.305857
1420.647709	61.175894	66.310862
1419.275154	65.735727	66.315866
1418.450921	60.192884	66.320871
1418.232365	58.872065	66.325876
1417.459831	65.689598	66.330881
1417.409330	60.130758	66.335886
1416.919188	59.486788	66.340890
1416.152197	59.605825	66.345895
1415.493881	55.256626	66.350900
1414.542616	63.988732	66.355905
1414.133159	54.984282	66.360910
1412.913927	63.923299	66.365914
1412.344337	63.114121	66.370919
1411.875372	66.163045	66.375924
1411.402883	62.393058	66.380929
1410.924163	61.943701	66.385934
1409.190916	65.572564	66.390938
1409.371357	61.794232	66.395943
1409.153095	54.727875	66.400948
1407.887891	62.020506	66.405953
1407.203489	49.323976	66.410958
1406.216690	58.488849	66.415962
1406.282057	61.713533	66.420967
1405.415612	61.511719	66.425972
1404.510944	67.771638	66.430977
1404.048267	58.907738	66.435982
1403.207454	70.619601	66.440986
1402.009794	73.156975	66.445991
1401.282525	63.921147	66.450996
1400.644495	66.605873	66.456001
1400.513949	61.620838	66.461006
1399.929435	67.619520	66.466010
1399.489428	61.468177	66.471015
1399.217195	60.901376	66.476020
1398.091513	68.932721	66.481025
1397.820951	65.594726	66.486030
1396.800385	62.945607	66.491034
1395.384702	53.806310	66.496039
1394.976634	63.378545	66.501044
1394.417383	59.875241	66.506049
1394.146409	52.741335	66.511054
1393.688927	64.070620	66.516058
1392.752356	60.214688	66.521063
1392.402505	53.016130	66.526068
1391.564184	63.289216	66.531073
1390.990642	55.202942	66.536078
1389.802749	65.692175	66.541082
1389.277496	60.061452	66.546087
1388.937767	56.056782	66.551092
1388.026127	69.138985	66.556097
1387.169815	61.608322	66.561102
1386.356518	61.783841	66.566106
1385.763403	64.457327	66.571111
1385.727916	61.206194	66.576116
1384.947414	68.147851	66.581121
1384.293756	55.706178	66.586126
1382.954553	58.222784	66.591130
1382.875919	59.230523	66.596135
1382.546019	58.791615	66.601140
1381.484210	59.500306	66.606145
1380.695982	58.527647	66.611150
1380.205723	57.811073	66.616154
1379.691374	57.443604	66.621159
1378.831805	59.820482	66.626164
1377.814575	61.458598	66.631169
1377.358181	58.721202	66.636174
1376.760939	66.644725	66.641178
1376.536718	59.893189	66.646183
1375.553125	59.459999	66.651188
1374.671505	61.621979	66.656193
1374.380805	59.219359	66.661198
1373.918256	65.096906	66.666202
1372.874529	58.210928	66.671207
1372.287281	56.732183	66.676212
1371.601356	60.239013	66.681217
1371.022515	52.791118	66.686222
1370.375964	61.786049	66.691226
1369.704146	57.697708	66.696231
1369.272759	67.262095	66.701236
1368.264147	65.346293	66.706241
1367.462555	62.407474	66.711246
1366.824176	66.205757	66.716250
1366.622685	67.141375	66.721255
1365.624443	64.349107	66.726260
1364.272914	66.831121	66.731265
1363.800686	54.643382	66.736270
1363.176930	60.699304	66.741274
1363.026031	61.797173	66.746279
1362.627473	58.037037	66.751284
1361.983465	58.956435	66.756289
1361.548474	48.970764	66.761294
1360.589135	60.220567	66.766298
1359.405218	61.686309	66.771303
1358.625038	57.523761	66.776308
1358.036891	74.061593	66.781313
1357.978200	56.785827	66.786318
1357.397123	57.543276	66.791322
1356.344146	63.289799	66.796327
1355.361330	60.880926	66.801332
1354.768725	64.061933	66.806337
1354.531813	58.627766	66.811342
1354.232766	64.979009	66.816346
1352.950738	63.805898	66.821351
1352.753503	59.927621	66.826356
1351.819110	60.099402	66.831361
1351.146870	58.689284	66.836366
1350.296469	59.698484	66.841370
1349.443882	65.636878	66.846375
1349.057709	57.325916	66.851380
1348.725635	65.668629	66.856385
1347.665508	56.965825	66.861390
1346.960556	69.155721	66.866394
1346.598829	70.506775	66.871399
1346.140116	67.056921	66.876404
1344.737175	66.427903	66.881409
1344.361226	68.564509	66.886414
1343.478421	64.541102	66.891418
1343.080184	58.186445	66.896423
1342.930675	59.377229	66.901428
1341.623159	67.400236	66.906433
1341.046120	60.106369	66.911438
1340.631246	63.511149	66.916442
1339.923855	65.028737	66.921447
1339.412879	63.187615	66.926452
1338.264104	63.059009	66.931457
1337.694569	63.169520	66.936462
1337.016889	61.144973	66.941466
1336.808924	63.408734	66.946471
1336.308955	62.774349	66.951476
1335.469409	67.970815	66.956481
1335.137062	61.227530	66.961486
1334.063840	65.725483	66.966490
1333.246862	62.664575	66.971495
1332.587676	53.574608	66.976500
1331.704454	65.888566	66.981505
1331.418491	53.194896	66.986510
1330.411239	55.576536	66.991514
1329.705436	64.651083	66.996519
1329.469217	63.933261	67.001524
1328.851239	61.815999	67.006529
1327.891857	52.223242	67.011534
1326.873447	68.643678	67.016538
1326.229506	65.066464	67.021543
1326.053638	52.042914	67.026548
1325.428093	58.752398	67.031553
1325.169502	54.107432	67.036558
1324.255334	56.453797	67.041562
1323.559904	58.781270	67.046567
1322.703429	63.316327	67.051572
1321.488624	57.224215	67.056577
1321.037944	50.393437	67.061582
1320.812416	63.115435	67.066586
1320.338929	60.658062	67.071591
1319.430300	55.534273	67.076596
1318.330682	65.395409	67.081601
1318.024462	58.635814	67.086606
1317.472740	62.843585	67.091610
1316.898155	60.402335	67.096615
1316.225407	58.269979	67.101620
1315.352424	60.582455	67.106625
1315.134286	57.530742	67.111630
1313.723606	63.360215	67.116634
1312.834468	53.063894	67.121639
1312.691099	53.440513	67.126644
1312.291388	61.416664	67.131649
1311.812986	59.036313	67.136654
1311.502725	55.760779	67.141658
1309.941243	62.017493	67.146663
1309.342475	63.493991	67.151668
1308.938697	66.778064	67.156673
1307.967754	51.764686	67.161678
1307.283522	56.538663	67.166682
1306.427887	57.181681	67.171687
1306.299104	57.197402	67.176692
1305.643130	65.606613	67.181697
1305.198422	58.238392	67.186702
1303.869480	63.083269	67.191706
1303.845505	60.040946	67.196711
1303.264659	58.540983	67.201716
1302.133500	57.908082	67.206721
1301.441418	54.247542	67.211726
1300.917466	62.332588	67.216730
1300.367331	64.939517	67.221735
1299.353755	58.091423	67.226740
1298.324731	62.185126	67.231745
1297.778033	59.676739	67.236750
1297.722952	53.223874	67.241754
1297.243367	65.168750	67.246759
1297.071763	58.766619	67.251764
1295.778732	52.671725	67.256769
1295.352847	57.223855	67.261774
1294.222863	57.301243	67.266778
1293.130611	56.716943	67.271783
1293.101936	50.256401	67.276788
1292.450821	65.138116	67.281793
1292.016069	61.326555	67.286798
1291.125745	59.349470	67.291802
1290.248884	56.937868	67.296807
1289.884495	56.379746	67.301812
1288.893163	62.677405	67.306817
1287.922736	62.097907	67.311822
1287.186718	58.373052	67.316826
1286.752922	58.766630	67.321831
1286.330452	58.015962	67.326836
1285.753264	63.855112	67.331841
1284.721569	57.304583	67.336846
1283.984407	71.267531	67.341850
1283.543167	64.924584	67.346855
1283.397515	58.413411	67.351860
1282.823100	64.571808	67.356865
1282.014916	53.451285	67.361870
1281.230634	58.348967	67.366874
1280.408717	53.561246	67.371879
1279.696259	54.584735	67.376884
1278.852876	65.110129	67.381889
1278.612709	63.231731	67.386894
1278.100716	58.448186	67.391898
1277.461484	56.613240	67.396903
1276.676705	53.120145	67.401908
1275.997469	62.495655	67.406913
1274.858696	54.346705	67.411918
1274.068480	54.200544	67.416922
1273.227718	63.208992	67.421927
1273.356034	55.315201	67.426932
1272.463263	59.116780	67.431937
1272.064983	56.208799	67.436942
1271.264451	55.777052	67.441946
1270.221967	55.561980	67.446951
1269.943877	51.853861	67.451956
1269.323740	58.792146	67.456961
1268.914606	57.452649	67.461966
1268.353502	56.549673	67.466970
1266.853185	58.490764	67.471975
1266.696335	51.184583	67.476980
1265.412977	58.126679	67.481985
1264.561027	54.292604	67.486990
1264.242628	57.437725	67.491994
1263.792467	57.765821	67.496999
1263.666087	51.451080	67.502004
1262.684493	58.341120	67.507009
1262.174465	61.512339	67.512014
1260.950156	59.179170	67.517018
1260.465625	61.705795	67.522023
1260.206155	54.512703	67.527028
1259.145979	60.199290	67.532033
1258.361516	51.199074	67.537038
1258.165945	56.948814	67.542042
1257.662638	57.117860	67.547047
1257.128548	61.846403	67.552052
1255.861027	60.022712	67.557057
1255.397104	59.829772	67.562062
1254.834078	61.902887	67.567066
1253.438371	61.212661	67.572071
1253.444330	64.888012	67.577076
1252.584935	61.076527	67.582081
1252.254333	61.983728	67.587086
1251.221248	60.891177	67.592090
1250.137826	59.877504	67.597095
1250.148052	57.731648	67.602100
1249.450961	64.700874	67.607105
1249.147074	64.082662	67.612110
1248.187260	64.564324	67.617114
1246.802379	60.262968	67.622119
1246.736129	59.091337	67.627124
1246.271262	66.721822	67.632129
1245.959803	61.814348	67.637134
1244.822738	63.277226	67.642138
1244.218256	68.269652	67.647143
1243.336341	56.002877	67.652148
1242.288991	65.419307	67.657153
1241.589739	55.111812	67.662158
1241.193199	64.153151	67.667162
1240.627274	67.627215	67.672167
1240.531390	62.361932	67.677172
1239.898156	65.240446	67.682177
1239.019114	55.572778	67.687182
1238.475907	55.934568	67.692186
1237.378209	65.646971	67.697191
1236.332051	53.999997	67.702196
1235.864397	60.743636	67.707201
1235.517659	60.320251	67.712206
1235.160883	58.772857	67.717210
1233.919026	66.331902	67.722215
1233.208036	53.746148	67.727220
1232.407196	65.389988	67.732225
1232.166837	62.208276	67.737230
1231.972995	54.921850	67.742234
1231.086238	52.659578	67.747239
1230.172132	53.303935	67.752244
1229.849416	69.438304	67.757249
1229.177026	62.271303	67.762254
1228.235916	55.975661	67.767258
1227.212175	59.761381	67.772263
1227.057282	54.210562	67.777268
1226.229561	61.732255	67.782273
1225.960723	55.053111	67.787278
1224.530978	57.282904	67.792282
1223.935532	58.745422	67.797287
1223.473686	56.416719	67.802292
1223.096372	66.234725	67.807297
1222.528448	59.390481	67.812302
1221.511395	60.976098	67.817306
1220.884199	61.083468	67.822311
1220.759788	55.050219	67.827316
1219.624119	54.479290	67.832321
1219.003920	65.957607	67.837326
1218.353639	65.417254	67.842330
1217.592007	64.011803	67.847335
1217.438825	60.224278	67.852340
1215.972947	63.968863	67.857345
1215.508787	67.832458	67.862350
1215.243845	61.468418	67.867354
1214.508427	62.841223	67.872359
1213.748112	63.083483	67.877364
1213.251659	62.469824	67.882369
1212.719808	57.248397	67.887374
1211.472378	59.568552	67.892378
1210.379733	65.735550	67.897383
1210.266620	59.006851	67.902388
1209.553001	61.167329	67.907393
1209.375366	64.597810	67.912398
1209.002050	57.542629	67.917402
1207.688469	55.555531	67.922407
1207.192559	48.915664	67.927412
1206.663633	59.802065	67.932417
1205.600759	62.333769	67.937422
1204.921124	60.249975	67.942426
1203.800031	63.165443	67.947431
1203.722040	58.894151	67.952436
1203.815783	62.206725	67.957441
1202.718814	57.460191	67.962446
1201.917341	61.740727	67.967450
1201.046397	58.509885	67.972455
1200.642677	55.558635	67.977460
1199.325969	60.172503	67.982465
1198.861594	56.704692	67.987470
1198.600199	54.014060	67.992474
1197.926672	63.067691	67.997479
1198.020335	59.256852	68.002484
1196.709414	65.026247	68.007489
1196.008794	66.395070	68.012494
1195.202943	63.841861	68.017498
1194.049915	65.284985	68.022503
1193.518622	63.971541	68.027508
1193.116504	70.362535	68.032513
1192.779734	59.062644	68.037518
1192.673516	62.577207	68.042522
1191.111590	61.259836	68.047527
1190.661762	57.742170	68.052532
1189.856549	68.655751	68.057537
1189.246803	66.300665	68.062542
1188.537799	64.651747	68.067546
1187.876259	59.782904	68.072551
1187.488665	54.724274	68.077556
1187.035256	66.780317	68.082561
1185.892932	63.908949	68.087566
1185.339152	57.532792	68.092570
1184.647626	67.470512	68.097575
1184.105239	55.177596	68.102580
1183.181809	59.857547	68.107585
1182.457129	58.511298	68.112590
1182.358072	55.447101	68.117594
1181.213741	68.048522	68.122599
1180.548986	63.989791	68.127604
1179.704463	68.017585	68.132609
1179.144922	55.115799	68.137614
1179.209990	56.332607	68.142618
1178.148395	70.927780	68.147623
1177.542996	55.290968	68.152628
1176.730966	68.740182	68.157633
1176.255148	66.774251	68.162638
1175.438029	66.870725	68.167642
1174.158429	63.879977	68.172647
1173.749935	60.693902	68.177652
1173.293412	68.674650	68.182657
1173.037646	61.132003	68.187662
1171.857912	53.230482	68.192666
1171.012791	59.271029	68.197671
1170.779592	59.925517	68.202676
1170.333385	66.441684	68.207681
1169.780064	67.243742	68.212686
1168.774999	60.450670	68.217690
1167.820030	60.841128	68.222695
1167.542207	52.548751	68.227700
1166.969806	65.385387	68.232705
1166.299130	54.936841	68.237710
1165.432851	53.426165	68.242714
1164.354411	54.742056	68.247719
1164.331948	51.210036	68.252724
1163.514060	51.912136	68.257729
1162.726426	58.330846	68.262734
1162.189210	56.400297	68.267738
1161.525747	62.393954	68.272743
1161.383806	57.091172	68.277748
1160.414751	59.825098	68.282753
1159.517058	52.233297	68.287758
1159.187581	52.098262	68.292762
1158.147704	57.690604	68.297767
1157.368277	50.100264	68.302772
1156.618520	49.754969	68.307777
1156.019572	58.394010	68.312782
1155.865719	52.086351	68.317786
1155.013070	58.792494	68.322791
1154.395128	52.066956	68.327796
1153.921707	63.448301	68.332801
1153.001191	60.010047	68.337806
1152.230577	58.000257	68.342810
1151.296913	66.613723	68.347815
1150.760652	61.279382	68.352820
1149.881904	60.521197	68.357825
1149.944556	64.015135	68.362830
1149.204664	63.967740	68.367834
1148.042836	67.294382	68.372839
1147.803021	56.386431	68.377844
1147.239152	60.972851	68.382849
1146.260657	57.136785	68.387854
1145.457386	53.186249	68.392858
1145.074509	60.098916	68.397863
1144.869048	52.471089	68.402868
1143.941455	52.990672	68.407873
1143.139993	57.009911	68.412878
1142.721193	57.083187	68.417882
1141.489380	63.502169	68.422887
1140.799577	53.394387	68.427892
1139.800649	60.227020	68.432897
1139.548764	61.513490	68.437902
1139.182888	53.541703	68.442906
1138.543825	64.669584	68.447911
1138.204267	57.593635	68.452916
1136.988536	57.865729	68.457921
1136.147573	59.785929	68.462926
1136.180646	55.500756	68.467930
1134.630507	58.865862	68.472935
1134.252678	59.210003	68.477940
1133.841949	59.871998	68.482945
1133.006644	63.776251	68.487950
1133.029143	57.901003	68.492954
1132.125399	61.779476	68.497959
1131.785187	60.859220	68.502964
1130.695524	58.098450	68.507969
1129.608616	53.345477	68.512974
1129.194404	61.954864	68.517978
1128.376506	62.433168	68.522983
1127.714586	60.569368	68.527988
1126.455210	72.000824	68.532993
1126.011617	64.511658	68.537998
1125.885086	58.257739	68.543002
1125.184858	61.704283	68.548007
1125.281817	64.261608	68.553012
1124.323742	62.072748	68.558017
1123.156566	70.692651	68.563022
1123.186631	62.759640	68.568026
1121.839339	69.231162	68.573031
1121.139580	67.087672	68.578036
1120.551522	64.068919	68.583041
1119.811256	67.184839	68.588046
1119.015797	60.665743	68.593050
1118.078495	67.255737	68.598055
1117.806867	61.998451	68.603060
1116.961196	69.260744	68.608065
1116.610606	68.269638	68.613070
1116.406164	61.077007	68.618074
1114.964319	68.015878	68.623079
1114.669815	65.347103	68.628084
1113.778796	66.729987	68.633089
1113.520708	66.936791	68.638094
1112.842956	62.854247	68.643098
1111.562149	70.092765	68.648103
1111.335896	67.738338	68.653108
1110.899388	68.624999	68.658113
1110.096525	68.239859	68.663118
1108.987960	59.347670	68.668122
1108.300055	68.825720	68.673127
1107.864676	66.165673	68.678132
1107.831734	59.789157	68.683137
1107.092583	63.950092	68.688142
1106.461303	61.449110	68.693146
1105.503065	67.621135	68.698151
1104.995737	53.469049	68.703156
1103.631156	59.010820	68.708161
1102.904932	61.297409	68.713166
1102.889577	52.395657	68.718170
1101.995193	67.406254	68.723175
1101.448836	53.717932	68.728180
1100.987811	54.084216	68.733185
1099.779169	59.839273	68.738190
1099.707022	50.160186	68.743194
1098.943988	54.059961	68.748199
1098.215253	51.900124	68.753204
1097.683822	52.435560	68.758209
1096.965669	58.448058	68.763214
1096.100414	53.808316	68.768218
1094.966219	59.444053	68.773223
1094.714582	51.526525	68.778228
1094.111030	59.494158	68.783233
1093.656463	51.793341	68.788238
1092.888899	47.883674	68.793242
1092.045646	57.770403	68.798247
1091.268982	54.556202	68.803252
1091.206133	53.866729	68.808257
1090.277895	54.259729	68.813262
1089.575782	49.680866	68.818266
1088.952311	59.961780	68.823271
1088.701603	49.121626	68.828276
1087.769092	56.491939	68.833281
1086.574715	61.669062	68.838286
1086.429325	51.635828	68.843290
1085.583944	60.612711	68.848295
1084.818264	47.550474	68.853300
1084.063659	54.210624	68.858305
1083.302016	60.283463	68.863310
1083.130253	57.657223	68.868314
1082.414607	59.157311	68.873319
1081.351578	57.579689	68.878324
1080.799509	60.118285	68.883329
1080.501543	60.289290	68.888334
1079.953464	59.199775	68.893338
1078.975414	66.747619	68.898343
1078.294312	54.276783	68.903348
1077.656276	59.593892	68.908353
1077.115967	51.648433	68.913358
1076.397699	48.234774	68.918362
1075.465585	57.350053	68.923367
1074.856628	62.031035	68.928372
1074.508288	51.809540	68.933377
1073.697888	51.114662	68.938382
1072.875632	55.047475	68.943386
1071.942432	58.923895	68.948391
1071.620369	53.186991	68.953396
1071.419631	49.627084	68.958401
1070.310021	58.841833	68.963406
1069.905849	54.052095	68.968410
1068.845611	58.727857	68.973415
1068.849245	54.579563	68.978420
1067.722636	52.438918	68.983425
1066.929121	57.878566	68.988430
1066.454363	48.242375	68.993434
1065.805367	56.968142	68.998439
1064.881642	60.289156	69.003444
1064.424635	52.219704	69.008449
1063.755227	50.972557	69.013454
1063.703014	56.528411	69.018458
1062.118523	60.090856	69.023463
1061.231682	57.147749	69.028468
1060.792708	57.216987	69.033473
1060.297978	59.862997	69.038478
1060.178462	51.090397	69.043482
1059.661203	56.445242	69.048487
1058.536983	51.658418	69.053492
1058.098094	49.921034	69.058497
1057.393710	56.130902	69.063502
1056.489480	58.834009	69.068506
1055.273522	58.851571	69.073511
1054.908184	53.947428	69.078516
1055.157675	57.615406	69.083521
1054.217007	50.685035	69.088526
1053.220042	47.320288	69.093530
1052.589897	56.170714	69.098535
1052.404565	41.275527	69.103540
1051.164339	52.546604	69.108545
1050.163537	57.513753	69.113550
1050.029063	46.258989	69.118554
1049.354942	55.448900	69.123559
1048.789838	55.305672	69.128564
1047.748798	57.524999	69.133569
1046.981255	59.351723	69.138574
1046.879251	51.948547	69.143578
1045.540222	61.160747	69.148583
1045.057191	53.538624	69.153588
1044.318137	52.642071	69.158593
1043.829493	60.040191	69.163598
1043.966714	47.014395	69.168602
1042.769582	58.660181	69.173607
1042.042157	57.276927	69.178612
1041.517031	58.558484	69.183617
1040.364505	53.677043	69.188622
1040.041394	56.526942	69.193626
1038.966324	64.899384	69.198631
1038.328511	60.850670	69.203636
1038.195198	57.334083	69.208641
1037.809212	65.285384	69.213646
1036.837349	57.379885	69.218650
1035.908498	59.293046	69.223655
1035.697789	54.828583	69.228660
1034.303365	60.502972	69.233665
1033.803355	58.321740	69.238670
1033.062538	52.052243	69.243674
1032.889915	53.374088	69.248679
1032.658266	50.507860	69.253684
1031.845620	53.666575	69.258689
1030.610878	58.130266	69.263694
1030.188290	52.773719	69.268698
1029.321359	48.676224	69.273703
1028.043493	53.252293	69.278708
1027.401927	47.476168	69.283713
1026.969106	58.037442	69.288718
1027.082748	49.056376	69.293722
1026.328539	59.665582	69.298727
1026.138509	54.424334	69.303732
1024.980359	51.545853	69.308737
1024.450073	62.410383	69.313742
1023.720753	41.672246	69.318746
1022.489784	61.076806	69.323751
1021.449909	51.962108	69.328756
1021.523875	44.108829	69.333761
1020.812075	54.138828	69.338766
1021.042102	49.698363	69.343770
1019.913541	53.066301	69.348775
1018.829929	49.009862	69.353780
1018.302657	50.754392	69.358785
1017.052376	58.414380	69.363790
1016.642521	52.537395	69.368794
1015.965407	62.516068	69.373799
1015.695130	61.479246	69.378804
1015.473024	60.177215	69.383809
1014.372856	50.069482	69.388814
1013.858874	52.027646	69.393818
1012.935545	55.319390	69.398823
1011.898269	56.252890	69.403828
1011.537503	55.165646	69.408833
1010.543844	55.111996	69.413838
1010.246177	53.241491	69.418842
1009.886370	52.635636	69.423847
1009.061725	48.259341	69.428852
1008.582217	55.459327	69.433857
1007.677094	56.518214	69.438862
1007.197639	47.974620	69.443866
1006.262668	52.647490	69.448871
1005.702768	47.075661	69.453876
1005.306865	48.784671	69.458881
1004.108085	50.385266	69.463886
1003.485607	51.254442	69.468890
1002.612618	55.731184	69.473895
1002.554228	50.422793	69.478900
1002.117316	49.435823	69.483905
1001.062984	45.936842	69.488910
1000.356179	51.335201	69.493914
999.514356	55.858313	69.498919
999.277010	52.048906	69.503924
998.300966	49.033069	69.508929
997.539000	51.410259	69.513934
997.169266	44.752374	69.518938
996.378413	59.006725	69.523943
995.755993	51.152708	69.528948
995.420078	49.662944	69.533953
994.382882	62.281160	69.538958
994.097656	51.163528	69.543962
992.860653	53.343796	69.548967
991.843752	54.036192	69.553972
991.575057	47.122597	69.558977
990.859543	49.543935	69.563982
990.395965	45.938263	69.568986
990.334182	49.474814	69.573991
989.111503	48.229669	69.578996
988.417224	53.522864	69.584001
987.886471	56.259121	69.589006
987.697142	49.297199	69.594010
986.584042	52.056215	69.599015
986.012451	50.154075	69.604020
985.664291	44.910311	69.609025
984.050268	52.737588	69.614030
983.601653	44.163852	69.619034
983.075342	52.244171	69.624039
982.646551	55.093223	69.629044
981.970843	51.888595	69.634049
980.604604	54.061394	69.639054
980.139448	48.870427	69.644058
979.875638	54.506721	69.649063
979.468271	46.598908	69.654068
978.950934	40.457724	69.659073
978.114918	45.254562	69.664078
977.305184	49.119718	69.669082
976.703812	54.626727	69.674087
975.835198	51.469740	69.679092
975.048269	46.024424	69.684097
974.371513	52.646778	69.689102
974.023026	43.755914	69.694106
973.376702	47.013249	69.699111
972.716294	51.208865	69.704116
972.008318	50.037806	69.709121
971.190717	54.938857	69.714126
970.939896	51.038213	69.719130
969.830101	56.983194	69.724135
969.185773	45.671689	69.729140
969.004176	49.358619	69.734145
968.256171	51.822232	69.739150
966.933367	45.380858	69.744154
966.233767	50.191440	69.749159
966.000139	49.331098	69.754164
965.494685	49.344628	69.759169
964.862165	57.602604	69.764174
964.515798	47.777482	69.769178
963.515568	46.994351	69.774183
963.103535	50.390764	69.779188
962.156557	47.659678	69.784193
960.710811	49.068907	69.789198
960.428120	51.705844	69.794202
960.043266	50.082368	69.799207
959.599530	52.846354	69.804212
959.180093	42.732188	69.809217
957.992140	44.467905	69.814222
957.544793	48.211004	69.819226
956.635488	45.157696	69.824231
955.310146	50.085706	69.829236
955.096068	47.097666	69.834241
954.332849	51.656265	69.839246
954.625756	51.820816	69.844250
954.232519	48.941217	69.849255
953.367102	51.068909	69.854260
952.599729	38.154238	69.859265
951.481183	55.122708	69.864270
950.689016	39.464678	69.869274
949.703869	58.359797	69.874279
949.488180	47.703923	69.879284
949.010343	48.195461	69.884289
947.882903	57.789440	69.889294
947.020249	56.421467	69.894298
946.362008	57.963843	69.899303
945.782867	54.525589	69.904308
946.088083	47.584760	69.909313
945.420761	55.021374	69.914318
944.766584	51.539923	69.919322
943.577474	56.620254	69.924327
943.051449	51.753908	69.929332
942.438973	59.641368	69.934337
941.416205	60.103477	69.939342
940.966688	47.601312	69.944346
940.561182	54.360361	69.949351
939.690790	56.898226	69.954356
938.906332	58.556555	69.959361
937.895414	59.729094	69.964366
937.601823	55.161210	69.969370
936.986498	50.366603	69.974375
935.769703	55.707451	69.979380
935.103149	59.145484	69.984385
934.720444	64.791487	69.989390
934.279574	53.027137	69.994394
934.112128	49.463119	69.999399
933.246252	48.740663	70.004404
932.346211	40.193334	70.009409
931.672835	54.792277	70.014414
931.540572	47.559288	70.019418
930.027586	53.081118	70.024423
929.306412	50.961855	70.029428
929.281817	55.046610	70.034433
928.564724	57.189953	70.039438
927.808624	39.247860	70.044442
926.621058	52.441662	70.049447
926.138069	60.674031	70.054452
925.677545	46.917775	70.059457
925.215089	59.381511	70.064462
924.926828	46.608984	70.069466
924.008218	62.246981	70.074471
923.127136	53.637192	70.079476
922.457995	43.720922	70.084481
921.685339	53.152303	70.089486
921.197411	49.130440	70.094490
920.740043	48.281184	70.099495
920.148583	50.625630	70.104500
919.477353	52.082606	70.109505
918.751872	56.875917	70.114510
918.158592	57.249869	70.119514
916.808237	46.221918	70.124519
916.217023	53.995215	70.129524
915.589515	52.514743	70.134529
915.163032	55.968105	70.139534
914.332894	52.154843	70.144538
913.624992	53.957160	70.149543
913.071820	51.007463	70.154548
912.813710	46.069187	70.159553
912.046304	56.122135	70.164558
911.103306	56.611243	70.169562
910.383131	60.002808	70.174567
909.919912	56.656410	70.179572
909.576922	53.768210	70.184577
908.271983	55.298592	70.189582
907.753066	50.103423	70.194586
907.120235	51.111744	70.199591
906.704507	50.507186	70.204596
906.080170	51.660886	70.209601
904.595508	46.719537	70.214606
904.400532	50.860311	70.219610
904.314726	48.598683	70.224615
903.504221	55.910227	70.229620
902.886444	52.441494	70.234625
902.048671	50.487066	70.239630
901.542173	48.184997	70.244634
900.802559	51.215175	70.249639
899.533388	55.505588	70.254644
899.322865	51.572787	70.259649
898.731618	58.199054	70.264654
897.875516	52.246157	70.269658
896.922555	51.081149	70.274663
896.320039	47.974127	70.279668
896.263167	39.297791	70.284673
895.921421	53.836381	70.289678
894.903849	41.696376	70.294682
894.129188	41.819570	70.299687
893.255106	52.062093	70.304692
893.059840	49.274112	70.309697
891.913419	56.367680	70.314702
891.118109	49.897955	70.319706
890.854264	44.223340	70.324711
890.236903	52.397408	70.329716
889.231989	46.021213	70.334721
888.290017	43.533219	70.339726
888.013565	43.798440	70.344730
887.575617	48.505008	70.349735
887.028435	54.108129	70.354740
885.971781	49.068217	70.359745
885.270821	50.320302	70.364750
884.909549	42.283040	70.369754
884.443949	45.216159	70.374759
883.133096	53.260336	70.379764
882.604369	50.996416	70.384769
882.462329	56.708163	70.389774
881.615181	51.761835	70.394778
880.466636	49.499870	70.399783
879.297224	54.778142	70.404788
879.339972	43.233727	70.409793
878.999793	52.716162	70.414798
878.571682	46.405378	70.419802
878.166511	48.376099	70.424807
877.090347	49.852702	70.429812
876.368667	46.099815	70.434817
875.375019	55.531553	70.439822
874.499280	54.614230	70.444826
873.997288	45.926505	70.449831
873.480975	53.800258	70.454836
873.417414	39.535136	70.459841
872.428334	55.079413	70.464846
871.526237	52.689586	70.469850
870.736948	50.083082	70.474855
870.501001	50.681609	70.479860
869.477466	50.048533	70.484865
868.686722	49.660174	70.489870
868.575872	41.050319	70.494874
868.006806	42.967011	70.499879
866.909496	51.848904	70.504884
866.225170	47.120995	70.509889
865.391180	51.583179	70.514894
864.931763	46.510450	70.519898
864.401663	49.782626	70.524903
863.223788	50.380652	70.529908
863.157732	53.871751	70.534913
862.194890	51.906780	70.539918
861.821907	54.459718	70.544922
860.793397	51.485265	70.549927
860.209298	54.381055	70.554932
860.093011	41.493437	70.559937
859.506862	53.599821	70.564942
858.476906	48.020113	70.569946
857.951636	48.659117	70.574951
857.154435	51.711005	70.579956
856.117363	50.349636	70.584961
855.105117	48.956385	70.589966
854.699211	52.764625	70.594970
854.496756	50.819013	70.599975
853.760630	58.336494	70.604980
853.672758	44.308416	70.609985
852.450597	58.007468	70.614990
851.756083	46.803661	70.619994
851.527208	49.249421	70.624999
850.476319	50.569340	70.630004
849.955212	44.296594	70.635009
849.279655	46.291524	70.640014
848.822788	41.594525	70.645018
847.631930	50.623094	70.650023
846.729706	50.065555	70.655028
846.334363	45.926009	70.660033
845.734803	55.621809	70.665038
844.559897	59.618211	70.670042
844.192907	47.687688	70.675047
843.295470	50.179280	70.680052
843.113836	52.028431	70.685057
842.570357	63.147835	70.690062
842.464548	51.100342	70.695066
841.368750	51.027512	70.700071
840.270373	46.042125	70.705076
840.306865	45.249596	70.710081
839.273743	52.504938	70.715086
838.263577	56.455361	70.720090
837.987168	50.833029	70.725095
837.131737	60.047296	70.730100
836.976106	46.109373	70.735105
836.210503	52.322242	70.740110
835.018547	50.940436	70.745114
835.235797	50.966368	70.750119
833.657312	49.412757	70.755124
832.989849	43.896092	70.760129
832.277000	51.761668	70.765134
831.838619	50.108296	70.770138
831.753013	46.954190	70.775143
830.335894	48.993251	70.780148
830.059330	47.157434	70.785153
829.519764	49.839163	70.790158
828.988536	45.028595	70.795162
827.564392	44.581376	70.800167
826.956293	57.838955	70.805172
826.698704	46.525976	70.810177
826.188910	53.560242	70.815182
825.511606	50.957458	70.820186
824.957548	53.463655	70.825191
824.059750	56.489360	70.830196
823.716543	45.674966	70.835201
822.208604	55.224799	70.840206
821.566162	51.194286	70.845210
821.271967	49.444380	70.850215
820.567767	55.192419	70.855220
820.420867	52.449445	70.860225
819.470347	53.521667	70.865230
818.641241	54.287713	70.870234
818.223855	50.895191	70.875239
817.705809	53.775329	70.880244
816.646858	49.476707	70.885249
815.442858	52.259616	70.890254
815.158858	44.388724	70.895258
814.846261	49.347754	70.900263
814.341512	49.431439	70.905268
813.909146	39.214130	70.910273
812.848361	53.622075	70.915278
812.378119	52.479000	70.920282
811.329660	46.780508	70.925287
810.406844	47.687337	70.930292
810.081680	46.657958	70.935297
809.910025	48.207391	70.940302
809.386042	46.475137	70.945306
808.479180	46.660855	70.950311
807.236613	48.889484	70.955316
807.157681	41.743292	70.960321
806.000606	48.166893	70.965326
805.019356	47.279892	70.970330
804.667943	47.833467	70.975335
803.953217	55.504380	70.980340
803.864027	48.171664	70.985345
802.743885	49.233077	70.990350
801.719469	46.680281	70.995354
801.289486	42.529703	71.000359
800.748753	53.856644	71.005364
800.554575	43.798656	71.010369
799.894400	46.531044	71.015374
799.071629	50.199519	71.020378
798.558360	46.248327	71.025383
797.719260	60.701986	71.030388
796.474542	45.279406	71.035393
795.973148	46.941765	71.040398
795.873104	52.849197	71.045402
795.430904	53.107290	71.050407
794.269031	52.632523	71.055412
793.527135	48.727993	71.060417
792.947693	50.362277	71.065422
792.675286	41.355392	71.070426
791.762222	49.784971	71.075431
790.675868	53.698323	71.080436
790.691777	46.999672	71.085441
790.056294	48.811308	71.090446
788.794401	59.174347	71.095450
788.392318	52.926613	71.100455
787.513287	63.271044	71.105460
787.313747	54.298643	71.110465
786.320354	60.252135	71.115470
785.561839	55.255516	71.120474
785.028322	47.856816	71.125479
784.281783	52.811236	71.130484
784.053421	43.375649	71.135489
783.324326	57.056559	71.140494
782.693495	46.724046	71.145498
782.000397	46.478045	71.150503
780.496635	42.375227	71.155508
780.229014	52.307044	71.160513
779.691767	56.681700	71.165518
778.940704	56.006707	71.170522
778.869349	46.709214	71.175527
777.560223	54.929157	71.180532
777.286536	46.132873	71.185537
776.514390	54.146367	71.190542
775.877655	57.772322	71.195546
775.149138	48.800148	71.200551
774.231958	53.974447	71.205556
773.833506	52.227404	71.210561
773.649121	60.920567	71.215566
772.292437	54.271914	71.220570
772.295138	48.325482	71.225575
770.800564	58.031317	71.230580
770.708232	49.707227	71.235585
769.515876	51.212833	71.240590
768.759616	55.428835	71.245594
768.599157	43.927135	71.250599
767.776015	49.343467	71.255604
767.850384	48.110264	71.260609
766.965204	51.397879	71.265614
766.197104	54.953185	71.270618
765.009026	52.430406	71.275623
763.984151	48.500149	71.280628
763.647104	43.780268	71.285633
763.053440	49.781728	71.290638
762.189963	60.663462	71.295642
762.451987	48.239966	71.300647
761.711749	56.791911	71.305652
760.621212	52.881190	71.310657
759.711164	46.883099	71.315662
759.736557	50.525098	71.320666
758.918540	48.718883	71.325671
757.575233	51.343705	71.330676
757.591292	54.202615	71.335681
756.704502	48.453945	71.340686
755.555953	50.165985	71.345690
755.203580	52.323842	71.350695
754.499388	50.115652	71.355700
754.242741	47.490556	71.360705
753.601497	53.738575	71.365710
752.803429	58.819452	71.370714
752.248068	50.970973	71.375719
751.562698	57.812306	71.380724
750.414185	50.695002	71.385729
749.791708	49.549593	71.390734
748.733764	61.520104	71.395738
748.831420	50.185359	71.400743
748.338319	52.808218	71.405748
747.567811	49.062930	71.410753
746.475614	53.098468	71.415758
745.849359	43.739729	71.420762
745.722868	42.744607	71.425767
744.734909	55.582151	71.430772
743.888358	45.768547	71.435777
743.516439	46.928365	71.440782
743.070496	49.849048	71.445786
742.361892	47.660563	71.450791
741.536773	48.233319	71.455796
740.866159	46.581057	71.460801
740.519724	45.884912	71.465806
739.741351	53.466474	71.470810
738.853853	46.201049	71.475815
738.253459	56.427488	71.480820
737.365472	47.346071	71.485825
736.550384	56.344234	71.490830
736.182041	51.627347	71.495834
735.997535	45.158810	71.500839
734.381562	49.772729	71.505844
733.576208	39.551440	71.510849
733.167702	49.647510	71.515854
732.313197	53.254725	71.520858
732.556196	51.619631	71.525863
731.993977	56.506170	71.530868
731.272414	48.829448	71.535873
730.432489	51.859857	71.540878
729.920801	59.136412	71.545882
729.019666	44.207603	71.550887
727.798062	54.517959	71.555892
727.933595	48.834152	71.560897
727.384318	55.151677	71.565902
725.804176	47.633877	71.570906
725.446270	43.184006	71.575911
724.730241	54.760041	71.580916
724.597224	41.053124	71.585921
723.977882	39.309982	71.590926
722.763321	40.606257	71.595930
722.404645	43.748819	71.600935
721.088275	47.860655	71.605940
720.873128	52.544061	71.610945
720.815687	51.244234	71.615950
719.472497	52.528600	71.620954
719.020548	53.410042	71.625959
718.172886	54.454005	71.630964
717.878675	57.966819	71.635969
716.581817	50.534696	71.640974
715.905266	51.765648	71.645978
715.629921	47.073884	71.650983
715.142733	49.542188	71.655988
714.850465	49.957750	71.660993
713.810761	46.802895	71.665998
712.799210	50.413726	71.671002
712.642594	46.005947	71.676007
711.495396	42.258493	71.681012
710.664811	47.966219	71.686017
710.253160	44.458263	71.691022
709.761790	45.262780	71.696026
709.577565	43.545752	71.701031
708.788693	59.863718	71.706036
708.186509	47.930490	71.711041
707.538511	40.921266	71.716046
705.725938	49.907554	71.721050
705.047440	45.810218	71.726055
704.561679	50.330786	71.731060
704.247796	52.079839	71.736065
704.057191	57.310062	71.741070
703.388968	54.820209	71.746074
703.218702	52.177161	71.751079
702.262440	56.653997	71.756084
701.480504	47.433246	71.761089
700.662528	50.791458	71.766094
699.832409	54.747767	71.771098
699.531707	49.050672	71.776103
698.251352	59.171771	71.781108
697.285531	47.855413	71.786113
697.443475	51.975988	71.791118
696.745325	55.243020	71.796122
696.374545	47.129263	71.801127
694.782508	57.739124	71.806132
693.984423	49.937370	71.811137
693.858630	49.545250	71.816142
693.438868	47.959357	71.821146
693.084198	38.867905	71.826151
691.782178	48.521027	71.831156
691.261102	54.148895	71.836161
690.807335	46.185927	71.841166
689.741224	47.647030	71.846170
689.133083	56.710000	71.851175
688.342643	58.378074	71.856180
687.967211	53.329269	71.861185
687.616776	51.473357	71.866190
686.796575	53.809252	71.871194
685.941971	48.604921	71.876199
685.119261	55.877525	71.881204
684.759275	52.940946	71.886209
684.482584	49.884316	71.891214
683.318106	51.905397	71.896218
682.878425	54.072295	71.901223
682.061975	56.853573	71.906228
680.838737	60.349108	71.911233
680.319324	51.156408	71.916238
679.488047	53.484333	71.921242
679.547388	45.129535	71.926247
678.848549	53.239812	71.931252
678.281489	49.199174	71.936257
677.402950	55.461799	71.941262
676.689836	56.821777	71.946266
676.230631	40.794578	71.951271
675.390729	53.492294	71.956276
674.526850	49.273573	71.961281
674.018037	54.364110	71.966286
673.361809	60.179335	71.971290
673.239008	45.974914	71.976295
672.103721	55.529615	71.981300
671.305431	55.734652	71.986305
671.122632	54.966665	71.991310
669.927828	53.510394	71.996314
669.409178	45.937469	72.001319
668.486114	48.032451	72.006324
668.106571	55.372020	72.011329
667.920418	44.453781	72.016334
666.752405	52.319982	72.021338
665.799589	43.056680	72.026343
665.162579	52.681534	72.031348
664.756575	49.761920	72.036353
664.288111	43.962922	72.041358
663.883546	55.066020	72.046362
663.171172	49.614314	72.051367
662.488157	55.338607	72.056372
661.347926	48.593312	72.061377
660.478658	56.332945	72.066382
659.897420	53.817935	72.071386
659.675713	46.580958	72.076391
659.036021	48.273732	72.081396
658.488840	49.497133	72.086401
657.587944	44.073386	72.091406
657.007910	50.173958	72.096410
656.581849	47.520660	72.101415
655.438358	43.046710	72.106420
654.638056	45.132898	72.111425
654.506746	45.926653	72.116430
653.853117	48.555310	72.121434
653.101835	49.193190	72.126439
652.496528	57.200609	72.131444
651.592751	52.019708	72.136449
651.546897	47.953330	72.141454
650.154429	59.756963	72.146458
649.932276	55.299628	72.151463
649.065498	58.551743	72.156468
647.989996	58.108396	72.161473
647.429352	51.236178	72.166478
647.055444	60.371516	72.171482
646.445669	51.445735	72.176487
645.704872	67.838757	72.181492
644.861033	55.128701	72.186497
643.808925	53.599835	72.191502
643.228350	67.644891	72.196506
642.994652	57.120033	72.201511
642.530023	60.353775	72.206516
641.846171	56.723521	72.211521
640.966838	56.767194	72.216526
640.280375	55.819857	72.221530
639.999481	55.549043	72.226535
639.232789	53.484204	72.231540
638.363044	51.369130	72.236545
637.551221	52.588928	72.241550
637.217196	56.171718	72.246554
636.870936	53.918015	72.251559
636.035461	54.901090	72.256564
635.035130	44.279442	72.261569
634.726755	50.059147	72.266574
633.350431	51.717086	72.271578
632.720406	46.124576	72.276583
632.057570	50.800214	72.281588
631.427079	49.448971	72.286593
631.205639	46.515504	72.291598
630.586960	47.156719	72.296602
630.585107	47.148738	72.301607
629.510251	58.086823	72.306612
628.535184	49.653474	72.311617
627.550201	41.179989	72.316622
626.285721	44.241310	72.321626
626.263760	44.232431	72.326631
625.959031	47.717443	72.331636
625.648061	48.954848	72.336641
625.275658	48.182245	72.341646
624.081862	54.495336	72.346650
623.703350	41.174686	72.351655
622.510407	51.824729	72.356660
621.321230	47.960156	72.361665
621.149529	44.726476	72.366670
620.197233	46.601093	72.371674
620.577523	43.726366	72.376679
619.204798	50.203130	72.381684
618.212691	48.594126	72.386689
617.903273	50.868570	72.391694
617.417873	54.405852	72.396698
617.372298	50.091943	72.401703
615.957322	48.626043	72.406708
615.425571	53.614336	72.411713
614.851813	44.482671	72.416718
613.664452	55.424243	72.421722
613.247953	44.697837	72.426727
612.402263	50.907870	72.431732
612.083696	54.551955	72.436737
611.584719	41.327338	72.441742
610.432370	48.638660	72.446746
609.918873	37.377860	72.451751
609.436104	43.056397	72.456756
608.870740	56.352830	72.461761
608.358023	52.094484	72.466766
607.482811	56.252335	72.471770
606.911212	47.096223	72.476775
605.838873	51.235746	72.481780
604.750417	48.538453	72.486785
604.822008	40.667455	72.491790
604.231350	48.217259	72.496794
603.868077	54.364376	72.501799
602.693336	49.505028	72.506804
601.855886	52.285968	72.511809
601.462446	47.709969	72.516814
600.907988	52.056403	72.521818
600.530762	45.524985	72.526823
599.555371	50.336671	72.531828
598.627532	44.673623	72.536833
598.500448	53.076314	72.541838
597.046188	54.448818	72.546842
596.173372	47.847978	72.551847
595.790493	52.622487	72.556852
595.522327	44.719310	72.561857
594.989881	49.250644	72.566862
593.910881	55.416580	72.571866
593.236382	48.807419	72.576871
592.650106	56.191091	72.581876
592.173253	53.778594	72.586881
591.993441	39.473047	72.591886
591.057986	56.795009	72.596890
590.225672	48.030522	72.601895
589.943822	49.491478	72.606900
589.019991	58.355529	72.611905
588.317902	53.017727	72.616910
587.184775	56.608757	72.621914
586.921075	46.287991	72.626919
586.582927	49.210344	72.631924
585.486508	49.301879	72.636929
585.119943	43.342155	72.641934
584.423925	54.319933	72.646938
583.768027	52.929631	72.651943
582.657757	50.629215	72.656948
581.844882	53.835395	72.661953
581.664904	35.949445	72.666958
581.063504	51.237053	72.671962
580.146144	49.245012	72.676967
579.306955	49.535223	72.681972
578.800082	51.305112	72.686977
578.581947	51.801527	72.691982
578.000737	53.826507	72.696986
577.091971	42.686721	72.701991
576.529772	45.091313	72.706996
575.785606	53.407507	72.712001
575.015688	55.378772	72.717006
573.761086	55.592143	72.722010
573.583858	44.294651	72.727015
572.750311	40.413369	72.732020
572.753178	44.475245	72.737025
572.462609	40.594477	72.742030
571.021233	46.179516	72.747034
570.583897	45.381335	72.752039
569.383834	52.780178	72.757044
568.626191	53.507576	72.762049
568.351788	49.189064	72.767054
567.367039	56.108149	72.772058
567.298338	54.953140	72.777063
566.610976	50.839586	72.782068
566.132986	53.947339	72.787073
565.648707	42.379979	72.792078
564.339074	58.591392	72.797082
563.783644	49.200032	72.802087
563.248426	52.467186	72.807092
562.668353	48.840482	72.812097
562.208603	44.204804	72.817102
561.018794	49.779109	72.822106
560.503229	56.943049	72.827111
559.863829	55.217971	72.832116
558.964939	53.783655	72.837121
558.254443	50.469411	72.842126
557.945272	55.093932	72.847130
557.598856	55.560621	72.852135
556.391513	47.837314	72.857140
555.278226	48.609862	72.862145
554.647485	51.907988	72.867150
554.350894	54.953083	72.872154
554.104041	48.196846	72.877159
553.978677	47.468363	72.882164
552.614826	56.521488	72.887169
552.156751	54.837575	72.892174
551.408749	63.992407	72.897178
550.829757	59.910019	72.902183
549.833184	57.005165	72.907188
549.283717	58.044243	72.912193
548.726722	53.662843	72.917198
547.194127	59.433248	72.922202
546.528980	54.799212	72.927207
546.088329	56.553416	72.932212
545.434888	53.422412	72.937217
545.417092	51.607012	72.942222
545.123430	53.924546	72.947226
544.624048	50.904506	72.952231
543.580886	54.050682	72.957236
542.635401	58.270712	72.962241
542.420847	45.876793	72.967246
541.263729	50.688838	72.972250
540.539774	46.720499	72.977255
540.018073	48.687130	72.982260
539.570817	51.979080	72.987265
538.647877	49.318176	72.992270
537.738548	48.000910	72.997274
537.504515	47.660497	73.002279
536.975540	45.437323	73.007284
536.140622	54.798479	73.012289
536.012239	47.926819	73.017294
534.867078	58.567507	73.022298
533.743416	49.946502	73.027303
533.087349	55.353181	73.032308
532.432469	50.631736	73.037313
532.289689	46.986158	73.042318
531.733653	54.056775	73.047322
530.718009	56.173171	73.052327
529.548366	59.406150	73.057332
529.005109	66.840087	73.062337
529.107107	54.684010	73.067342
528.354965	59.043009	73.072346
527.572932	55.007652	73.077351
526.752996	49.590194	73.082356
526.052486	50.577002	73.087361
525.696879	49.519705	73.092366
524.370011	55.118688	73.097370
523.749018	52.951542	73.102375
523.315028	54.794995	73.107380
523.150751	60.013994	73.112385
523.259647	51.345207	73.117390
521.696751	55.609062	73.122394
520.874154	52.663354	73.127399
519.995338	54.614605	73.132404
519.133751	62.679760	73.137409
518.808005	56.303729	73.142414
518.080436	64.524726	73.147418
517.410502	62.024934	73.152423
517.050807	55.812211	73.157428
515.636848	57.571756	73.162433
515.330900	48.291597	73.167438
514.877261	61.189569	73.172442
514.390937	59.992443	73.177447
513.944477	53.523027	73.182452
512.827237	57.173319	73.187457
512.610844	41.214684	73.192462
511.840756	54.123455	73.197466
510.922817	51.001071	73.202471
510.090789	51.364274	73.207476
509.483797	54.020481	73.212481
508.973033	53.821430	73.217486
508.593462	51.789354	73.222490
507.513105	52.329311	73.227495
506.966299	55.468990	73.232500
506.366765	58.699410	73.237505
505.790879	55.589069	73.242510
504.648440	54.552921	73.247514
503.939344	60.031450	73.252519
503.630886	59.394732	73.257524
503.311283	62.665208	73.262529
503.008065	48.642510	73.267534
501.552257	58.219792	73.272538
500.943294	57.498391	73.277543
500.407464	49.487548	73.282548
499.518070	54.803955	73.287553
498.963238	55.880272	73.292558
498.052416	58.582227	73.297562
497.881783	50.873915	73.302567
497.578726	49.922477	73.307572
496.182133	59.098848	73.312577
495.713147	48.536185	73.317582
495.001284	55.057226	73.322586
494.628252	48.452873	73.327591
493.680084	49.450151	73.332596
492.870352	55.093940	73.337601
492.624971	45.280020	73.342606
492.230290	58.185647	73.347610
491.032324	58.739050	73.352615
490.186144	57.617406	73.357620
489.280209	59.874475	73.362625
489.607575	45.744913	73.367630
488.326475	52.916092	73.372634
487.398615	52.837459	73.377639
487.157566	51.854082	73.382644
486.698414	49.982083	73.387649
486.647448	44.277353	73.392654
485.241708	50.942949	73.397658
484.827847	50.315217	73.402663
484.365112	62.533079	73.407668
482.964687	61.815074	73.412673
482.402039	55.267288	73.417678
481.530905	62.057190	73.422682
481.088505	65.267792	73.427687
480.879449	59.245168	73.432692
479.476066	51.836118	73.437697
479.247742	58.025636	73.442702
478.438586	59.694185	73.447706
478.246393	55.202524	73.452711
477.477570	57.932252	73.457716
476.372798	67.560306	73.462721
476.041918	49.542339	73.467726
475.560810	61.434159	73.472730
474.533761	59.381203	73.477735
474.012959	60.608786	73.482740
473.203970	64.464408	73.487745
473.052880	48.812721	73.492750
472.207758	60.158666	73.497754
471.197564	56.630942	73.502759
470.915878	53.007985	73.507764
469.728850	58.840371	73.512769
468.694507	56.035161	73.517774
468.472796	53.668558	73.522778
468.156981	55.143234	73.527783
467.981994	56.159989	73.532788
466.564535	52.454966	73.537793
465.779822	49.059911	73.542798
465.040978	47.463593	73.547802
464.903565	47.468184	73.552807
464.443560	51.944089	73.557812
463.131948	56.444752	73.562817
462.570376	51.088818	73.567822
462.011049	59.636226	73.572826
461.498240	53.936430	73.577831
460.777637	54.687890	73.582836
459.812150	50.325982	73.587841
459.611486	47.647504	73.592846
459.020737	54.796700	73.597850
458.195977	48.852355	73.602855
457.677611	45.502050	73.607860
457.003845	52.207605	73.612865
456.029344	42.312202	73.617870
455.307970	57.082377	73.622874
454.494703	57.139236	73.627879
454.315114	50.572786	73.632884
453.499831	59.618764	73.637889
453.243367	52.106732	73.642894
452.306425	53.899808	73.647898
451.555041	45.599093	73.652903
450.990788	48.528226	73.657908
449.631398	55.730197	73.662913
449.042124	58.934392	73.667918
448.784188	55.745497	73.672922
448.039339	56.149426	73.677927
448.011496	54.353906	73.682932
446.917221	55.729893	73.687937
446.317098	55.682337	73.692942
445.703344	54.505478	73.697946
444.887001	54.005927	73.702951
444.051504	51.137046	73.707956
443.499149	56.739104	73.712961
443.449987	51.845198	73.717966
442.089529	60.114261	73.722970
441.499398	60.649957	73.727975
441.027822	54.559833	73.732980
440.396636	59.000738	73.737985
440.040262	55.049157	73.742990
438.698869	52.250787	73.747994
437.945217	58.050752	73.752999
437.844507	52.291787	73.758004
436.826103	71.760214	73.763009
435.986909	58.372494	73.768014
435.091060	64.038945	73.773018
434.535377	56.626344	73.778023
434.758416	57.696858	73.783028
434.327306	68.488736	73.788033
433.416510	60.295068	73.793038
432.527846	56.855467	73.798042
431.418697	61.536166	73.803047
430.765489	59.832025	73.808052
429.605365	62.638290	73.813057
429.495210	47.972694	73.818062
428.851995	55.486122	73.823066
428.565491	54.144640	73.828071
428.332688	50.242145	73.833076
427.046929	56.668920	73.838081
426.788075	45.150585	73.843086
425.864371	53.371644	73.848090
424.801991	64.134733	73.853095
424.220851	50.498735	73.858100
423.520573	61.532907	73.863105
423.444951	56.375920	73.868110
422.464355	50.398292	73.873114
421.248222	55.345204	73.878119
421.041978	45.653659	73.883124
420.331748	56.730977	73.888129
420.300317	49.486684	73.893134
419.460256	55.955889	73.898138
418.420038	57.705884	73.903143
418.044579	47.183654	73.908148
417.418496	58.111957	73.913153
416.331721	55.625199	73.918158
415.713565	56.474760	73.923162
415.172622	56.294311	73.928167
414.702312	59.447730	73.933172
413.452133	53.599981	73.938177
412.782680	49.706794	73.943182
412.112920	56.372591	73.948186
411.871218	55.418144	73.953191
411.765179	53.753650	73.958196
410.923988	52.708924	73.963201
410.289119	54.727723	73.968206
409.391960	53.931389	73.973210
407.818036	53.239588	73.978215
407.495824	55.123890	73.983220
406.913484	59.890749	73.988225
406.655254	48.435463	73.993230
406.609423	55.807441	73.998234
405.569475	51.019783	74.003239
404.853894	49.159373	74.008244
403.716460	53.724535	74.013249
403.423639	52.086919	74.018254
402.662553	46.480997	74.023258
401.544498	52.613000	74.028263
401.459036	46.366327	74.033268
400.991220	58.608342	74.038273
399.985924	49.572780	74.043278
399.014132	59.764591	74.048282
398.450439	55.378442	74.053287
398.143731	45.650042	74.058292
397.230419	58.054056	74.063297
396.480449	52.622268	74.068302
395.900109	52.332528	74.073306
395.289514	57.049759	74.078311
395.186826	40.236060	74.083316
394.174006	55.623381	74.088321
392.909181	54.577053	74.093326
392.675317	56.359773	74.098330
392.305715	49.862208	74.103335
391.687693	43.273017	74.108340
390.427926	54.127558	74.113345
389.574834	54.617147	74.118350
389.321145	53.778038	74.123354
389.023044	56.175281	74.128359
388.483652	47.686681	74.133364
387.300452	51.297383	74.138369
387.106064	52.369172	74.143374
386.497946	58.825078	74.148378
385.561738	54.449881	74.153383
385.141635	51.471142	74.158388
384.272411	56.427684	74.163393
383.174724	49.973586	74.168398
382.813260	53.433594	74.173402
382.102145	55.840044	74.178407
381.578012	52.127208	74.183412
380.098281	54.179886	74.188417
379.987194	46.423493	74.193422
379.701747	48.087166	74.198426
378.946307	52.659889	74.203431
378.832724	45.324687	74.208436
377.728785	63.288124	74.213441
377.298841	62.119244	74.218446
376.092459	50.531605	74.223450
374.962128	62.874533	74.228455
374.398168	54.529082	74.233460
373.742127	63.370946	74.238465
373.645219	54.473376	74.243470
373.423145	55.083757	74.248474
372.163050	59.272474	74.253479
371.517153	44.750414	74.258484
371.335792	55.573290	74.263489
370.624509	53.662810	74.268494
369.527440	54.250659	74.273498
368.674013	48.200730	74.278503
368.115568	49.463982	74.283508
367.579337	50.535940	74.288513
367.186728	53.200812	74.293518
366.298702	49.794669	74.298522
365.524762	57.668773	74.303527
365.337073	49.909720	74.308532
363.755846	65.216450	74.313537
363.273545	46.721211	74.318542
362.926749	56.039380	74.323546
362.429270	51.097584	74.328551
362.392902	48.150576	74.333556
360.905093	61.892052	74.338561
360.364433	55.460119	74.343566
359.885803	51.430429	74.348570
359.081748	49.579269	74.353575
358.184419	48.164857	74.358580
357.435376	54.715964	74.363585
357.124625	49.144574	74.368590
356.597106	46.675269	74.373594
355.808177	53.310969	74.378599
355.109892	45.251031	74.383604
354.400112	42.765993	74.388609
354.058834	42.629485	74.393614
353.029495	46.744315	74.398618
351.865097	48.493105	74.403623
352.286644	40.815949	74.408628
351.719188	52.130095	74.413633
350.137252	53.811508	74.418638
349.475363	50.999334	74.423642
348.955104	54.696545	74.428647
348.665090	45.106205	74.433652
347.351960	58.520131	74.438657
347.012414	56.262147	74.443662
346.346629	49.125000	74.448666
345.787531	48.125487	74.453671
345.480152	39.879356	74.458676
344.788399	50.163293	74.463681
343.920725	47.795706	74.468686
343.716777	29.646314	74.473690
341.893189	44.413945	74.478695
341.526713	47.435105	74.483700
340.897288	53.117871	74.488705
340.612370	55.838099	74.493710
340.636748	45.227229	74.498714
339.069868	48.744235	74.503719
338.275438	44.143845	74.508724
337.736235	51.300788	74.513729
337.525366	46.851815	74.518734
336.999862	48.465849	74.523738
335.528698	46.282610	74.528743
335.050801	44.609620	74.533748
334.759242	52.605116	74.538753
333.948845	47.254354	74.543758
333.191038	40.828861	74.548762
332.489315	47.724729	74.553767
332.402737	44.183999	74.558772
331.064205	54.492349	74.563777
330.151393	51.945407	74.568782
329.510294	50.406959	74.573786
328.739725	52.142333	74.578791
328.613615	42.868489	74.583796
328.258940	45.979594	74.588801
327.714011	51.455260	74.593806
326.905032	51.850463	74.598810
326.134273	52.292006	74.603815
325.540722	43.404573	74.608820
324.680329	58.965104	74.613825
323.917277	51.584912	74.618830
323.616433	43.262667	74.623834
322.888230	54.481610	74.628839
322.130925	52.812301	74.633844
321.172330	49.593909	74.638849
320.893561	51.210260	74.643854
320.451230	39.252111	74.648858
319.088873	57.946236	74.653863
318.461437	49.055136	74.658868
317.639863	54.673343	74.663873
317.384005	53.279252	74.668878
317.467601	47.381350	74.673882
316.052136	56.620591	74.678887
315.566971	53.076337	74.683892
314.818080	56.155937	74.688897
313.718710	47.484663	74.693902
312.974608	46.841315	74.698906
312.271336	52.687126	74.703911
312.253896	47.008633	74.708916
311.770214	53.399401	74.713921
311.158315	41.495576	74.718926
310.135746	43.585570	74.723930
309.590903	51.097536	74.728935
309.253201	45.838253	74.733940
307.826186	47.389712	74.738945
307.075265	51.034491	74.743950
306.821222	40.351751	74.748954
306.094190	50.222553	74.753959
306.221277	49.967487	74.758964
305.171084	46.259175	74.763969
304.217168	50.340167	74.768974
304.113779	44.122232	74.773978
302.484679	52.625246	74.778983
301.694406	52.386893	74.783988
301.284266	48.869255	74.788993
301.036761	47.820289	74.793998
300.597744	39.882893	74.799002
299.646173	47.970983	74.804007
299.198445	45.074748	74.809012
298.545629	47.860005	74.814017
297.431131	51.704856	74.819022
296.686365	41.452386	74.824026
295.992057	59.263512	74.829031
295.914523	47.650574	74.834036
295.276519	42.576965	74.839041
294.141540	43.075414	74.844046
293.642126	43.611366	74.849050
292.931337	56.483140	74.854055
292.456588	43.180243	74.859060
291.757251	49.591790	74.864065
290.768975	46.629925	74.869070
290.380176	41.864897	74.874074
289.631657	54.309349	74.879079
288.870167	48.160397	74.884084
288.027999	49.827133	74.889089
287.618034	55.057054	74.894094
287.433364	49.415908	74.899098
286.547642	54.348449	74.904103
285.774680	45.438488	74.909108
285.121145	55.151444	74.914113
284.420054	44.901357	74.919118
283.740980	54.749734	74.924122
282.509947	54.627585	74.929127
282.058307	48.283036	74.934132
281.833486	48.594700	74.939137
281.848819	49.119001	74.944142
280.633970	48.501085	74.949146
279.914421	53.602501	74.954151
279.588017	48.117483	74.959156
278.171755	48.314433	74.964161
277.435372	53.651613	74.969166
277.060486	47.858347	74.974170
276.485595	50.964966	74.979175
276.116177	51.612446	74.984180
275.232115	52.516679	74.989185
274.221112	44.447996	74.994190
273.850186	39.065738	74.999194
273.133871	54.833266	75.004199
272.292157	51.448020	75.009204
271.317549	50.670910	75.014209
270.924485	47.795702	75.019214
270.877839	46.849276	75.024218
270.291807	47.985828	75.029223
269.191916	45.980538	75.034228
268.306471	47.593514	75.039233
268.160671	46.780918	75.044238
267.883736	47.029283	75.049242
266.384141	58.097836	75.054247
266.160132	48.890116	75.059252
265.219617	54.276891	75.064257
264.388065	50.115482	75.069262
263.661687	44.864408	75.074266
262.635058	52.094243	75.079271
262.481744	47.631464	75.084276
261.861571	50.614012	75.089281
261.817667	50.318784	75.094286
260.991823	50.655708	75.099290
260.121301	59.166862	75.104295
259.168521	51.024652	75.109300
258.152473	46.101895	75.114305
257.458786	52.165131	75.119310
257.475400	41.783747	75.124314
257.399622	49.300178	75.129319
256.371932	42.832546	75.134324
255.703203	53.173722	75.139329
255.120698	45.844703	75.144334
253.977602	50.244295	75.149338
253.048278	53.658362	75.154343
252.794421	44.897049	75.159348
252.146867	52.938563	75.164353
251.239968	47.669489	75.169358
250.490305	43.223277	75.174362
249.348804	45.574048	75.179367
249.342482	44.661760	75.184372
248.924182	49.058690	75.189377
248.007855	55.222060	75.194382
247.089464	46.277830	75.199386
246.289102	63.794921	75.204391
246.292183	44.636297	75.209396
245.775217	39.655629	75.214401
244.754785	48.377593	75.219406
244.009991	36.916541	75.224410
242.989951	46.819806	75.229415
243.049135	44.897278	75.234420
242.465804	58.724905	75.239425
241.479768	60.160536	75.244430
240.639092	42.319229	75.249434
240.295284	54.519060	75.254439
239.861309	50.379898	75.259444
238.785774	46.806991	75.264449
237.960521	54.096649	75.269454
237.858971	45.474615	75.274458
236.467207	49.074127	75.279463
235.973786	42.863058	75.284468
235.628224	44.775841	75.289473
235.095349	55.308455	75.294478
234.785158	43.148868	75.299482
233.308113	50.726289	75.304487
232.523802	45.300033	75.309492
232.205352	49.180144	75.314497
231.813776	50.746760	75.319502
230.704891	39.703753	75.324506
229.939983	54.013259	75.329511
229.719183	49.456267	75.334516
229.314168	51.554494	75.339521
228.242833	50.516887	75.344526
227.457536	51.419197	75.349530
226.819916	47.591242	75.354535
226.626205	39.432612	75.359540
225.446939	56.688218	75.364545
224.807205	47.435324	75.369550
224.632707	42.646992	75.374554
224.045876	50.511530	75.379559
222.822508	47.426174	75.384564
222.201221	52.954407	75.389569
221.270541	49.403645	75.394574
221.309894	35.282830	75.399578
220.201182	50.318325	75.404583
219.530364	47.238907	75.409588
218.993055	47.128117	75.414593
218.412864	60.001191	75.419598
218.343554	50.062795	75.424602
216.938615	54.666742	75.429607
216.059746	49.926520	75.434612
215.703581	47.327211	75.439617
214.894402	53.145792	75.444622
214.084151	48.597085	75.449626
213.356535	54.825606	75.454631
212.703531	51.351582	75.459636
212.928446	52.820813	75.464641
212.193822	48.397687	75.469646
211.507905	47.127449	75.474650
210.468706	57.238074	75.479655
209.783524	46.866076	75.484660
209.014247	50.497041	75.489665
208.618020	44.794280	75.494670
207.830170	43.302322	75.499674
207.012606	54.043594	75.504679
206.320952	49.978999	75.509684
205.723922	42.039101	75.514689
204.940498	49.216991	75.519694
204.662290	44.350918	75.524698
203.928511	55.498985	75.529703
203.297595	45.326094	75.534708
202.454548	43.843204	75.539713
201.714195	48.330075	75.544718
201.221331	41.908536	75.549722
200.287193	45.369616	75.554727
199.533696	47.711515	75.559732
199.145265	47.504949	75.564737
198.677595	45.951003	75.569742
198.272697	43.184799	75.574746
196.974990	52.720040	75.579751
196.391732	47.317744	75.584756
195.949042	39.277976	75.589761
195.174712	48.740472	75.594766
194.291992	37.048093	75.599770
193.809403	50.279797	75.604775
193.427567	37.541622	75.609780
193.113778	42.308243	75.614785
191.769742	46.600590	75.619790
191.284664	38.502568	75.624794
190.628572	45.113931	75.629799
189.992043	42.561896	75.634804
189.109334	54.408078	75.639809
188.298892	40.097430	75.644814
188.149890	39.760223	75.649818
187.627859	42.402290	75.654823
186.806425	45.396846	75.659828
185.689722	50.484645	75.664833
184.834843	48.346988	75.669838
184.597492	44.165446	75.674842
184.114688	51.526660	75.679847
183.353874	41.230791	75.684852
182.456083	49.428090	75.689857
181.859156	51.055962	75.694862
181.904824	42.071223	75.699866
180.697222	48.503199	75.704871
179.670652	45.037565	75.709876
179.298097	52.033325	75.714881
178.639424	53.189050	75.719886
178.390067	54.734843	75.724890
177.291840	46.625882	75.729895
176.202331	43.872044	75.734900
176.169352	45.769534	75.739905
175.748400	43.257910	75.744910
174.826606	45.021202	75.749914
173.948481	51.638264	75.754919
173.597188	52.826556	75.759924
173.173015	43.849731	75.764929
171.862795	45.443572	75.769934
171.080693	45.254759	75.774938
170.779656	47.074261	75.779943
170.385987	49.146470	75.784948
169.817930	45.959057	75.789953
168.592315	52.304525	75.794958
168.281287	49.596832	75.799962
167.247397	51.258166	75.804967
167.208257	50.499522	75.809972
166.328030	41.647849	75.814977
165.271040	42.504776	75.819982
165.188066	34.753461	75.824986
163.578309	54.168117	75.829991
163.200696	50.968188	75.834996
163.002261	46.880233	75.840001
162.274032	63.481859	75.845006
161.966223	44.239188	75.850010
160.928195	48.231998	75.855015
160.107328	43.844587	75.860020
159.641152	45.466624	75.865025
158.984282	52.000368	75.870030
158.352862	49.883616	75.875034
157.319356	53.933280	75.880039
156.845185	54.887260	75.885044
156.467187	46.855747	75.890049
155.395581	56.356974	75.895054
154.977157	47.214570	75.900058
154.319790	54.849642	75.905063
153.872323	51.975089	75.910068
152.890697	55.019611	75.915073
151.920399	55.300402	75.920078
151.310891	44.489161	75.925082
150.817106	54.238283	75.930087
150.642784	46.418945	75.935092
150.085353	47.860850	75.940097
148.928494	45.872067	75.945102
148.479557	48.445560	75.950106
147.897023	43.318264	75.955111
146.992750	46.106383	75.960116
146.357567	50.876791	75.965121
145.517667	55.765578	75.970126
145.183914	51.574908	75.975130
144.460484	52.382552	75.980135
143.678218	45.278446	75.985140
143.165899	55.636627	75.990145
142.391744	57.839191	75.995150
141.270200	51.991586	76.000154
140.577217	58.022742	76.005159
140.546949	60.460128	76.010164
140.330548	56.449458	76.015169
139.064957	58.924941	76.020174
138.464997	49.067657	76.025178
137.959872	54.467043	76.030183
137.352812	59.370781	76.035188
136.189853	46.928351	76.040193
135.046165	52.308529	76.045198
135.154347	49.645414	76.050202
134.634562	48.808520	76.055207
134.443126	60.710666	76.060212
133.223263	51.849725	76.065217
132.207938	52.407037	76.070222
132.135511	51.088085	76.075226
131.378588	59.235589	76.080231
130.546599	48.412757	76.085236
130.015858	54.443729	76.090241
129.269121	54.047162	76.095246
128.508186	47.507785	76.100250
127.307855	47.650001	76.105255
126.630329	52.890665	76.110260
126.449374	51.323889	76.115265
125.921062	50.977899	76.120270
125.357283	43.132179	76.125274
124.398864	56.671232	76.130279
123.505346	50.228790	76.135284
123.512305	47.589343	76.140289
122.971068	51.809604	76.145294
122.143110	48.691226	76.150298
121.067345	55.545848	76.155303
120.446535	46.839568	76.160308
120.495004	43.821978	76.165313
118.985717	52.500275	76.170318
118.832317	45.808989	76.175322
118.221574	51.599482	76.180327
116.948748	53.614399	76.185332
116.229808	47.800407	76.190337
115.614112	55.513990	76.195342
115.459058	46.217109	76.200346
114.847655	44.392966	76.205351
114.415847	46.251073	76.210356
113.533434	43.526086	76.215361
112.515110	47.367115	76.220366
112.288104	43.651934	76.225370
111.319837	52.558382	76.230375
110.323207	56.803035	76.235380
109.994216	56.853110	76.240385
109.458847	52.567149	76.245390
109.208978	60.798243	76.250394
107.863713	45.570424	76.255399
107.221905	51.807135	76.260404
106.894371	46.301809	76.265409
105.616811	45.703770	76.270414
104.815619	51.080891	76.275418
104.521840	50.713247	76.280423
103.936134	57.814231	76.285428
103.811253	49.339096	76.290433
103.269339	50.523759	76.295438
102.323186	46.144024	76.300442
101.807771	51.948569	76.305447
101.170963	50.162727	76.310452
99.943469	45.552166	76.315457
98.927179	61.142981	76.320462
99.016217	49.882409	76.325466
98.342879	47.509187	76.330471
97.122852	48.881152	76.335476
96.789423	44.344274	76.340481
96.046725	52.757346	76.345486
95.794025	46.441878	76.350490
94.953102	49.581885	76.355495
93.862393	50.083054	76.360500
93.629223	45.196246	76.365505
93.189425	55.083735	76.370510
91.930519	46.362128	76.375514
91.265980	50.841541	76.380519
90.562728	51.955976	76.385524
90.459903	45.567054	76.390529
89.418870	54.930819	76.395534
89.131851	45.958914	76.400538
88.367781	51.316648	76.405543
87.759146	55.515707	76.410548
87.253535	49.729880	76.415553
85.883838	57.399454	76.420558
85.702214	44.123323	76.425562
85.070747	51.921709	76.430567
84.250208	46.954824	76.435572
83.259224	41.285370	76.440577
82.473167	54.101368	76.445582
82.211226	56.383878	76.450586
81.791338	45.420153	76.455591
81.036822	48.179846	76.460596
80.389394	42.463728	76.465601
79.475918	53.982846	76.470606
79.356977	54.120456	76.475610
78.265012	49.324439	76.480615
77.202542	47.803408	76.485620
77.029045	46.845183	76.490625
76.666566	53.136632	76.495630
76.070376	48.774268	76.500634
74.960300	43.638751	76.505639
74.239899	47.182806	76.510644
73.828847	44.919742	76.515649
72.830254	49.274071	76.520654
71.987232	42.338679	76.525658
71.598573	60.499603	76.530663
71.371186	57.126701	76.535668
70.480294	47.288526	76.540673
69.627244	53.327788	76.545678
69.125784	46.128587	76.550682
68.536424	49.678596	76.555687
68.000144	46.013678	76.560692
67.130490	43.343352	76.565697
66.271463	48.233058	76.570702
66.007111	47.494081	76.575706
65.475825	52.577450	76.580711
64.179749	49.339223	76.585716
63.894374	47.532608	76.590721
62.729312	58.700942	76.595726
62.757612	44.822415	76.600730
61.486188	49.655729	76.605735
60.589952	55.346369	76.610740
60.054623	56.032178	76.615745
59.492471	57.722781	76.620750
59.350970	58.818274	76.625754
59.277000	64.679369	76.630759
58.214222	55.174194	76.635764
57.463364	56.384817	76.640769
56.755145	60.443069	76.645774
55.744119	50.863503	76.650778
54.977390	53.763443	76.655783
54.213381	51.907845	76.660788
54.417404	54.026788	76.665793
52.863104	60.511918	76.670798
52.151335	53.675594	76.675802
51.408648	57.250709	76.680807
51.018395	59.357075	76.685812
51.126693	53.720982	76.690817
50.533037	56.524150	76.695822
49.394572	53.102994	76.700826
48.926739	57.694335	76.705831
47.596525	60.025405	76.710836
46.576763	57.373318	76.715841
46.122462	60.649534	76.720846
45.710433	57.413284	76.725850
45.620255	60.033032	76.730855
44.899491	55.685320	76.735860
44.444736	53.903798	76.740865
43.376570	48.548355	76.745870
43.036126	49.688219	76.750874
42.252665	54.693650	76.755879
40.878530	58.448471	76.760884
40.599074	54.125354	76.765889
39.807629	57.181892	76.770894
39.617898	47.318242	76.775898
38.583262	63.759256	76.780903
38.087092	56.355873	76.785908
37.685859	50.536765	76.790913
37.300903	60.007119	76.795918
36.193107	52.760309	76.800922
35.673975	50.754973	76.805927
34.735678	57.416710	76.810932
34.062502	46.235913	76.815937
33.416605	47.102118	76.820942
32.913052	55.701942	76.825946
32.389052	51.179981	76.830951
30.799370	55.648688	76.835956
30.826387	58.730284	76.840961
30.073030	55.280997	76.845966
29.870933	48.191517	76.850970
28.745794	45.565004	76.855975
27.926973	56.625033	76.860980
27.973280	50.611966	76.865985
26.533626	52.822471	76.870990
25.832820	49.039331	76.875994
25.387917	49.346506	76.880999
24.605210	58.126422	76.886004
24.448593	45.736479	76.891009
23.266569	49.137071	76.896014
22.626379	52.602648	76.901018
21.994655	46.761093	76.906023
21.653357	47.661516	76.911028
21.260419	42.754350	76.916033
19.934387	56.335913	76.921038
19.439670	52.886492	76.926042
18.915073	49.013145	76.931047
18.533373	55.850222	76.936052
17.529053	56.911690	76.941057
16.283770	53.648586	76.946062
15.930680	53.578071	76.951066
15.763298	49.201797	76.956071
14.995542	52.013109	76.961076
14.331160	45.204591	76.966081
13.373004	50.177217	76.971086
12.792554	57.457292	76.976090
12.568833	53.443153	76.981095
11.433789	49.700918	76.986100
10.804116	50.081219	76.991105
10.162541	51.883333	76.996110
10.045995	48.464593	77.001114
9.301676	46.802983	77.006119
7.952440	57.974483	77.011124
7.852368	52.605814	77.016129
7.279022	55.861393	77.021134
6.260461	55.591974	77.026139
5.695462	47.166658	77.031143
4.948698	56.907450	77.036148
4.777021	49.468570	77.041153
3.611431	63.966384	77.046158