Tue Jun 08 16:39:24 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.316751	85.859256	0.000000
-1.679087	75.155691	0.005005
-2.641378	42.860565	0.010010
-4.762487	3.226453	0.015014
-9.086494	4.542218	0.020019
-13.883690	1.345111	0.025024
-18.753275	5.814611	0.030029
-23.459180	-3.680319	0.035034
-26.802477	2.222352	0.040038
-31.040914	6.978348	0.045043
-34.711530	0.228722	0.050048
-38.379647	13.767874	0.055053
-41.931746	10.701085	0.060058
-45.479324	0.898613	0.065062
-49.485675	5.399318	0.070067
-52.946890	-3.432761	0.075072
-56.615422	1.434727	0.080077
-60.778728	-1.758929	0.085082
-64.255819	5.192162	0.090086
-68.452295	8.152573	0.095091
-71.796741	4.691411	0.100096
-75.625147	4.612610	0.105101
-79.573460	13.588066	0.110106
-83.460319	6.227845	0.115110
-87.070942	4.825353	0.120115
-91.037569	2.363336	0.125120
-94.650498	6.298096	0.130125
-98.237518	4.938535	0.135130
-101.921803	0.047231	0.140134
-105.787809	10.083776	0.145139
-109.264725	-4.490935	0.150144
-113.089858	-4.087143	0.155149
-117.111385	-5.124297	0.160154
-120.686116	-0.753997	0.165158
-124.989175	-0.176267	0.170163
-128.664222	-3.810802	0.175168
-132.678232	7.949966	0.180173
-137.165467	7.456478	0.185178
-140.041230	4.582838	0.190182
-143.629186	7.066747	0.195187
-147.047286	5.431564	0.200192
-150.930109	4.536035	0.205197
-154.663031	6.144090	0.210202
-158.496665	0.247471	0.215206
-162.505494	8.109239	0.220211
-166.036715	0.040391	0.225216
-169.716777	7.600666	0.230221
-173.823805	15.932413	0.235226
-177.705254	5.596044	0.240230
-181.226939	10.690661	0.245235
-184.703837	1.014340	0.250240
-188.506468	11.092968	0.255245
-192.502180	12.290632	0.260250
-195.964052	-1.608473	0.265254
-199.729117	11.928071	0.270259
-203.611896	7.707955	0.275264
-207.234445	9.144766	0.280269
-211.043791	9.751181	0.285274
-215.426504	5.304212	0.290278
-219.340078	12.881289	0.295283
-222.616262	5.943790	0.300288
-226.262595	13.729624	0.305293
-230.266127	5.489619	0.310298
-233.421569	4.161927	0.315302
-237.780796	10.321091	0.320307
-241.329637	2.009033	0.325312
-244.870339	8.913140	0.330317
-249.248734	13.941608	0.335322
-252.659052	3.142823	0.340326
-256.357609	7.472890	0.345331
-259.862544	-1.375194	0.350336
-263.494633	2.007231	0.355341
-267.977739	4.714243	0.360346
-271.252705	1.522352	0.365350
-275.341400	10.405599	0.370355
-279.333190	8.484476	0.375360
-282.571587	2.210365	0.380365
-286.255925	8.324462	0.385370
-290.386893	10.375087	0.390374
-294.397733	11.073762	0.395379
-297.670280	3.089727	0.400384
-301.473941	3.305666	0.405389
-305.373510	7.381326	0.410394
-309.167591	2.277343	0.415398
-312.983122	4.294799	0.420403
-316.570396	4.982017	0.425408
-320.327558	2.041811	0.430413
-324.484364	11.038616	0.435418
-327.516086	5.743485	0.440422
-331.588039	12.070151	0.445427
-335.338041	6.128164	0.450432
-339.017879	5.276132	0.455437
-342.976299	6.114662	0.460442
-346.644244	-7.080314	0.465446
-350.411094	13.019434	0.470451
-354.293437	7.072931	0.475456
-357.893330	9.100009	0.480461
-362.077582	7.545900	0.485466
-365.556991	1.966835	0.490470
-369.305043	10.168085	0.495475
-373.253621	5.155789	0.500480
-376.932035	4.373802	0.505485
-380.540403	11.696558	0.510490
-384.027294	5.290300	0.515494
-387.931268	7.491136	0.520499
-391.946749	8.899983	0.525504
-395.425285	4.221514	0.530509
-399.390373	7.636306	0.535514
-403.172471	0.692992	0.540518
-406.845425	8.576672	0.545523
-410.649032	7.074142	0.550528
-414.130016	5.104982	0.555533
-418.366985	8.132256	0.560538
-421.678011	2.876429	0.565542
-425.780827	17.074584	0.570547
-429.491480	12.729624	0.575552
-433.239709	1.076805	0.580557
-437.264546	4.939609	0.585562
-440.888134	-2.841590	0.590566
-444.725543	11.730220	0.595571
-448.207445	8.731848	0.600576
-451.608344	8.644360	0.605581
-455.778333	4.350998	0.610586
-459.629132	3.411565	0.615590
-463.740151	14.254570	0.620595
-467.236672	7.887532	0.625600
-470.569563	8.250592	0.630605
-474.581381	3.635266	0.635610
-478.177658	4.770570	0.640614
-482.454577	6.141859	0.645619
-486.024468	1.641760	0.650624
-489.367581	-0.090093	0.655629
-493.165125	4.195569	0.660634
-497.290477	1.384213	0.665638
-501.065959	7.554372	0.670643
-504.830424	6.079548	0.675648
-508.856464	9.622515	0.680653
-512.187733	7.842466	0.685658
-515.629517	7.360232	0.690662
-519.702625	6.816994	0.695667
-523.392097	10.833895	0.700672
-527.086278	0.454691	0.705677
-531.210550	6.524863	0.710682
-534.399482	-5.785485	0.715686
-538.648643	-1.917259	0.720691
-542.441199	6.078615	0.725696
-546.065159	8.407186	0.730701
-550.178590	10.551741	0.735706
-553.643244	7.074087	0.740710
-557.237768	0.517909	0.745715
-561.197100	-0.512144	0.750720
-564.823823	3.123392	0.755725
-568.803460	7.981109	0.760730
-572.326788	5.169541	0.765734
-576.840717	7.985164	0.770739
-580.042607	5.505652	0.775744
-583.686749	6.553736	0.780749
-587.501700	6.115462	0.785754
-590.800282	8.152201	0.790758
-594.701686	9.708219	0.795763
-598.436911	11.097578	0.800768
-602.469006	9.128411	0.805773
-606.186441	9.614399	0.810778
-610.116308	8.375270	0.815782
-614.075583	16.186672	0.820787
-617.504386	15.490727	0.825792
-621.041827	9.540548	0.830797
-624.897066	18.303506	0.835802
-628.480606	9.876568	0.840806
-633.070388	14.106867	0.845811
-636.336470	9.974726	0.850816
-640.354188	6.724675	0.855821
-644.179551	9.731652	0.860826
-647.479043	7.866525	0.865830
-651.622564	12.024206	0.870835
-655.146169	5.954457	0.875840
-658.975522	6.617972	0.880845
-662.990337	14.128707	0.885850
-666.483988	9.501607	0.890854
-670.300573	9.038819	0.895859
-674.058533	10.250578	0.900864
-677.414602	10.383317	0.905869
-681.528282	15.648975	0.910874
-685.074642	10.987124	0.915878
-689.268647	11.624834	0.920883
-692.958037	6.633486	0.925888
-696.675460	12.748447	0.930893
-700.399260	13.699386	0.935898
-703.848746	4.443525	0.940902
-707.644449	14.696999	0.945907
-711.729994	16.657326	0.950912
-715.274979	4.858592	0.955917
-719.676163	8.204439	0.960922
-722.833636	3.398913	0.965926
-726.815035	9.083976	0.970931
-730.288355	7.521884	0.975936
-733.834259	1.543262	0.980941
-737.809028	12.854909	0.985946
-741.506778	2.787549	0.990950
-745.729166	8.544382	0.995955
-749.424707	10.667919	1.000960
-752.599034	8.735211	1.005965
-757.170910	11.447286	1.010970
-760.441354	-1.090439	1.015974
-764.048592	12.439543	1.020979
-767.918265	6.498363	1.025984
-771.769288	-2.119743	1.030989
-775.965281	11.888637	1.035994
-779.377759	0.173005	1.040998
-782.998711	9.356491	1.046003
-786.860596	4.380627	1.051008
-790.125809	8.349787	1.056013
-794.371162	17.099713	1.061018
-798.117484	9.442129	1.066022
-802.251761	8.859923	1.071027
-805.717541	11.655328	1.076032
-809.451571	2.618917	1.081037
-813.403535	4.730078	1.086042
-816.595914	7.236608	1.091046
-820.597771	1.599201	1.096051
-824.549732	12.061937	1.101056
-827.974609	7.642628	1.106061
-831.995912	5.508419	1.111066
-835.573059	1.899139	1.116070
-839.386443	-3.793098	1.121075
-843.331753	1.414985	1.126080
-846.628758	1.547979	1.131085
-850.723364	12.010750	1.136090
-854.603465	1.151843	1.141094
-858.645030	6.876950	1.146099
-862.145864	4.215699	1.151104
-865.545578	1.958639	1.156109
-869.716796	7.183028	1.161114
-873.614973	2.470430	1.166118
-877.155774	3.334847	1.171123
-880.868641	1.897283	1.176128
-884.430974	6.707713	1.181133
-888.287122	10.346974	1.186138
-891.969545	-1.242482	1.191142
-895.723566	4.899441	1.196147
-899.783564	5.783142	1.201152
-903.235506	4.417638	1.206157
-907.583278	2.187980	1.211162
-910.923712	-0.438006	1.216166
-914.643012	-0.172075	1.221171
-918.745790	11.919523	1.226176
-922.314096	5.114060	1.231181
-926.252604	9.732150	1.236186
-929.767030	1.597947	1.241190
-933.522504	5.544410	1.246195
-937.418169	9.830312	1.251200
-941.045717	3.192525	1.256205
-944.862546	-0.199473	1.261210
-948.458270	-2.390054	1.266214
-951.926860	4.615074	1.271219
-955.796589	0.447891	1.276224
-959.752149	-1.535653	1.281229
-963.928534	8.510629	1.286234
-967.424226	-1.042559	1.291238
-971.199947	-6.703243	1.296243
-975.162007	8.401488	1.301248
-978.521615	-6.573422	1.306253
-982.672499	3.359556	1.311258
-986.169891	-2.685979	1.316262
-989.924150	1.080731	1.321267
-993.883638	-2.896151	1.326272
-996.992196	-1.035805	1.331277
-1001.347200	5.786444	1.336282
-1004.710459	-6.958524	1.341286
-1008.700619	-1.065681	1.346291
-1012.513539	-1.612074	1.351296
-1016.218543	-3.282560	1.356301
-1020.327007	0.675243	1.361306
-1024.098994	-4.009141	1.366310
-1028.059156	6.367539	1.371315
-1031.322573	-3.463081	1.376320
-1035.147423	-4.492891	1.381325
-1039.437100	4.909014	1.386330
-1042.556842	-1.307884	1.391334
-1046.021954	-2.553387	1.396339
-1050.214248	11.792845	1.401344
-1053.672406	-5.136226	1.406349
-1057.698952	-5.135152	1.411354
-1061.325489	-8.262106	1.416358
-1065.177665	3.350429	1.421363
-1069.239554	8.138237	1.426368
-1072.531747	-2.853362	1.431373
-1076.723798	3.278270	1.436378
-1079.867533	5.944386	1.441382
-1083.959474	1.282235	1.446387
-1087.872224	4.250127	1.451392
-1091.249287	0.558561	1.456397
-1095.674635	5.147509	1.461402
-1098.904535	0.558384	1.466406
-1102.439759	-4.644567	1.471411
-1106.893979	0.679550	1.476416
-1110.531899	-6.688076	1.481421
-1114.223402	9.501129	1.486426
-1117.814406	1.743376	1.491430
-1121.418702	-3.205350	1.496435
-1125.358973	-5.707237	1.501440
-1128.628545	-1.954964	1.506445
-1133.127044	3.657418	1.511450
-1136.796109	1.227774	1.516454
-1140.508803	-0.327211	1.521459
-1143.907835	6.194839	1.526464
-1147.581141	-1.490335	1.531469
-1151.814652	3.160059	1.536474
-1155.384219	-10.425973	1.541478
-1159.658855	11.165059	1.546483
-1163.333330	10.871713	1.551488
-1166.764408	7.993891	1.556493
-1170.220841	12.556248	1.561498
-1173.822040	2.792835	1.566502
-1177.929272	5.890514	1.571507
-1181.655496	5.975909	1.576512
-1185.608901	3.091102	1.581517
-1189.654233	3.569172	1.586522
-1193.126291	-3.922380	1.591526
-1196.755335	-2.114204	1.596531
-1200.457976	0.642062	1.601536
-1204.228467	1.673288	1.606541
-1208.564367	12.762753	1.611546
-1212.123564	-3.836203	1.616550
-1215.618804	-3.053536	1.621555
-1219.523538	4.035376	1.626560
-1223.012373	0.748348	1.631565
-1226.875330	-0.330002	1.636570
-1230.454807	0.149408	1.641574
-1234.260958	3.009131	1.646579
-1238.081146	13.322083	1.651584
-1241.915468	-3.323135	1.656589
-1245.908754	5.424158	1.661594
-1249.407391	4.859130	1.666598
-1253.161199	4.551070	1.671603
-1257.054807	1.875518	1.676608
-1260.879249	-7.172547	1.681613
-1264.535088	2.051231	1.686618
-1268.340344	0.344905	1.691622
-1272.089608	1.749882	1.696627
-1276.081646	-1.032682	1.701632
-1279.808236	-7.711949	1.706637
-1283.195762	3.278630	1.711642
-1286.784967	-3.685128	1.716646
-1290.551794	0.262400	1.721651
-1294.638274	4.659933	1.726656
-1298.374154	0.033548	1.731661
-1302.337690	3.554650	1.736666
-1306.134693	-1.052940	1.741670
-1310.061050	-11.736067	1.746675
-1313.465450	-0.196699	1.751680
-1316.939285	-1.870308	1.756685
-1321.209129	2.807013	1.761690
-1324.289825	-1.979645	1.766694
-1328.369247	1.905567	1.771699
-1332.444766	3.519388	1.776704
-1335.976102	-1.985181	1.781709
-1339.746951	3.794106	1.786714
-1343.549483	-0.591465	1.791718
-1347.139136	4.053905	1.796723
-1351.008030	5.427401	1.801728
-1354.816878	-5.457432	1.806733
-1359.112491	1.778867	1.811738
-1362.356088	-0.620641	1.816742
-1365.931449	-6.848607	1.821747
-1369.618594	-6.747654	1.826752
-1373.233301	4.116236	1.831757
-1377.501850	4.363248	1.836762
-1380.991754	6.974582	1.841766
-1384.610192	10.260047	1.846771
-1388.558613	2.679200	1.851776
-1392.611409	1.023406	1.856781
-1396.209116	-5.795116	1.861786
-1399.798375	-0.583374	1.866790
-1403.567159	2.771350	1.871795
-1407.438469	9.883498	1.876800
-1411.176380	6.008685	1.881805
-1414.964962	0.810462	1.886810
-1419.119746	7.111654	1.891814
-1422.711867	6.991478	1.896819
-1426.327003	4.811361	1.901824
-1429.434343	4.843942	1.906829
-1433.744032	12.389023	1.911834
-1437.575102	8.413012	1.916838
-1441.356385	10.210449	1.921843
-1445.338228	12.974237	1.926848
-1448.911898	-1.219830	1.931853
-1452.628020	2.003927	1.936858
-1455.873709	3.766989	1.941862
-1460.042804	4.240531	1.946867
-1464.201859	5.183627	1.951872
-1467.815060	-1.345219	1.956877
-1471.500182	-3.893764	1.961882
-1475.332255	-0.534815	1.966886
-1478.881324	2.212278	1.971891
-1482.666045	0.897720	1.976896
-1486.240852	-1.114813	1.981901
-1490.389206	7.766693	1.986906
-1493.975919	-10.448672	1.991910
-1497.169768	-5.858948	1.996915
-1501.849785	2.851254	2.006912
-1502.685948	-2.784521	2.016909
-1500.519486	-0.302477	2.026906
-1497.222867	-4.218961	2.036902
-1494.766668	-1.612011	2.046899
-1493.417524	3.504218	2.056896
-1491.583766	5.643085	2.066893
-1489.372210	3.428252	2.076890
-1487.503978	-0.313561	2.086886
-1485.710263	2.373621	2.096883
-1484.010051	1.261536	2.106880
-1481.710367	1.671948	2.116877
-1479.858954	3.895127	2.126874
-1478.070435	4.441181	2.136870
-1476.124722	-1.736165	2.146867
-1474.479314	0.138662	2.156864
-1472.762238	2.190086	2.166861
-1470.777071	7.661029	2.176858
-1468.435699	1.628726	2.186854
-1466.659445	0.980994	2.196851
-1464.797206	3.553265	2.206848
-1463.258388	-1.238921	2.216845
-1461.303684	7.451878	2.226842
-1459.153048	2.432463	2.236838
-1457.208758	1.296240	2.246835
-1455.335590	3.014570	2.256832
-1453.595681	0.587145	2.266829
-1451.774333	5.107707	2.276826
-1449.725451	4.167326	2.286822
-1447.720391	-0.723924	2.296819
-1446.245620	5.850004	2.306816
-1444.085588	4.023445	2.316813
-1442.235121	2.321602	2.326810
-1440.547322	8.675165	2.336806
-1438.248183	1.670017	2.346803
-1436.585289	2.696902	2.356800
-1434.915755	9.862991	2.366797
-1432.783124	2.222501	2.376794
-1431.010049	-4.736134	2.386790
-1429.326901	8.526461	2.396787
-1427.224742	5.945521	2.406784
-1425.199844	8.845951	2.416781
-1423.458960	8.612563	2.426778
-1421.286435	2.597433	2.436774
-1419.734842	3.822080	2.446771
-1417.969832	2.960122	2.456768
-1415.828064	11.630275	2.466765
-1413.819578	10.441942	2.476762
-1412.125798	13.898014	2.486758
-1410.342017	5.655091	2.496755
-1408.471044	5.510021	2.506752
-1406.580477	11.232004	2.516749
-1404.676230	13.069906	2.526746
-1402.681153	9.257724	2.536742
-1400.764064	7.566981	2.546739
-1399.075672	5.760208	2.556736
-1397.067274	13.588174	2.566733
-1395.191148	7.775336	2.576730
-1393.361187	16.437811	2.586726
-1391.396494	1.150851	2.596723
-1389.310598	2.718059	2.606720
-1387.987708	6.471025	2.616717
-1385.872494	2.383306	2.626714
-1384.108332	4.961397	2.636710
-1382.102058	7.095183	2.646707
-1380.267250	6.104269	2.656704
-1378.560681	7.856392	2.666701
-1376.572079	8.323067	2.676698
-1374.158930	1.270305	2.686694
-1372.481565	0.102512	2.696691
-1370.996575	6.846238	2.706688
-1368.940727	7.397796	2.716685
-1367.275268	5.319119	2.726682
-1365.174461	2.857004	2.736678
-1362.925942	4.404195	2.746675
-1361.392335	-1.469539	2.756672
-1359.635736	7.267994	2.766669
-1358.020192	3.240825	2.776666
-1355.873603	6.467379	2.786662
-1353.825966	4.210030	2.796659
-1351.722462	-1.754480	2.806656
-1350.128683	6.060550	2.816653
-1348.469353	10.711354	2.826650
-1346.414076	6.858426	2.836646
-1344.518376	7.189709	2.846643
-1342.663490	12.602479	2.856640
-1340.860167	10.826968	2.866637
-1338.958415	5.261498	2.876634
-1337.075048	3.791173	2.886630
-1335.244114	2.474107	2.896627
-1333.506849	1.282604	2.906624
-1331.280035	0.221610	2.916621
-1329.454480	2.079782	2.926618
-1327.602070	8.019795	2.936614
-1325.425777	2.715831	2.946611
-1324.071083	4.145461	2.956608
-1321.977891	4.244438	2.966605
-1320.091827	5.655121	2.976602
-1318.165261	2.215570	2.986598
-1316.221668	3.159908	2.996595
-1314.503320	-0.154954	3.006592
-1312.662758	2.104155	3.016589
-1310.672714	0.044443	3.026586
-1308.844083	5.533270	3.036582
-1307.107094	-4.960586	3.046579
-1305.180413	2.135310	3.056576
-1303.193333	5.660798	3.066573
-1301.176471	-0.356784	3.076570
-1299.332521	3.031254	3.086566
-1297.639218	1.757604	3.096563
-1295.758214	2.067326	3.106560
-1293.959613	-5.082580	3.116557
-1291.952128	5.823480	3.126554
-1289.734541	3.751174	3.136550
-1288.122794	1.152174	3.146547
-1286.717312	-0.892094	3.156544
-1284.485976	-1.784295	3.166541
-1282.325394	2.369424	3.176538
-1280.788966	1.327838	3.186534
-1278.988258	0.126250	3.196531
-1276.850963	-1.584475	3.206528
-1275.260232	-1.346612	3.216525
-1273.246795	3.119703	3.226522
-1271.326897	-1.106727	3.236518
-1269.499822	-3.052669	3.246515
-1267.408772	1.058462	3.256512
-1265.580755	6.641476	3.266509
-1263.826647	-2.099002	3.276506
-1261.973344	-1.117791	3.286502
-1259.907898	1.620046	3.296499
-1257.949157	0.051050	3.306496
-1256.257597	5.574906	3.316493
-1254.572861	2.417204	3.326490
-1252.715713	0.909132	3.336486
-1250.775774	-1.879801	3.346483
-1248.838369	0.474548	3.356480
-1246.807959	-0.270886	3.366477
-1245.028999	-1.275862	3.376474
-1243.285291	3.224938	3.386470
-1241.218896	-5.267227	3.396467
-1239.264547	0.163286	3.406464
-1237.648737	-3.060032	3.416461
-1235.831269	6.322366	3.426458
-1233.780525	1.050679	3.436454
-1231.967837	-1.942056	3.446451
-1230.053714	-3.336993	3.456448
-1228.139309	2.179823	3.466445
-1226.059617	-4.574120	3.476442
-1224.273690	-1.498177	3.486438
-1222.547208	-1.671702	3.496435
-1220.894743	0.468389	3.506432
-1218.442508	4.748714	3.516429
-1216.704283	5.610992	3.526426
-1215.026929	4.425478	3.536422
-1213.469201	-3.144241	3.546419
-1211.503399	4.180927	3.556416
-1209.297739	4.404105	3.566413
-1207.431030	-6.668452	3.576410
-1205.807288	1.121342	3.586406
-1203.562717	0.619352	3.596403
-1201.758345	-2.912588	3.606400
-1200.125436	6.635896	3.616397
-1198.174309	6.276783	3.626394
-1195.969738	6.522287	3.636390
-1194.218718	-1.153342	3.646387
-1192.487893	-1.383720	3.656384
-1190.652046	6.653812	3.666381
-1188.652298	12.514847	3.676378
-1187.067688	0.805049	3.686374
-1185.128886	4.434530	3.696371
-1183.285151	7.635333	3.706368
-1181.330648	2.153741	3.716365
-1179.207018	3.427655	3.726362
-1177.251123	2.580835	3.736358
-1175.542298	-3.422130	3.746355
-1173.791978	5.546588	3.756352
-1172.120978	0.373339	3.766349
-1170.013100	-0.345051	3.776346
-1167.835311	-0.862033	3.786342
-1166.347353	0.778332	3.796339
-1164.271242	6.060324	3.806336
-1162.595550	-1.624885	3.816333
-1160.485313	3.482099	3.826330
-1158.804035	-0.854278	3.836326
-1156.842939	-1.580257	3.846323
-1155.046632	-2.580271	3.856320
-1153.207199	-1.866951	3.866317
-1151.072020	-0.375270	3.876314
-1149.258984	1.329816	3.886310
-1147.629098	4.199419	3.896307
-1145.473935	-2.555595	3.906304
-1143.586635	-6.855416	3.916301
-1141.546907	-3.818671	3.926298
-1139.813249	-3.987072	3.936294
-1138.283633	-3.442650	3.946291
-1136.405639	-5.268839	3.956288
-1134.313497	1.089730	3.966285
-1132.544215	-2.423510	3.976282
-1130.378048	1.459803	3.986278
-1128.597392	1.745731	3.996275
-1126.725220	3.510625	4.006272
-1125.035808	3.904306	4.016269
-1122.974587	-0.803193	4.026266
-1121.085751	-0.676928	4.036262
-1119.002365	3.365648	4.046259
-1117.496058	-4.636662	4.056256
-1115.820261	0.965054	4.066253
-1113.862974	-0.505616	4.076250
-1111.778268	0.407472	4.086246
-1109.854639	-1.781044	4.096243
-1107.949436	-2.073344	4.106240
-1106.233935	-0.873561	4.116237
-1104.375256	-0.196327	4.126234
-1102.337764	-2.550224	4.136230
-1100.326612	-4.993261	4.146227
-1098.790586	2.297479	4.156224
-1096.823409	1.408842	4.166221
-1094.934808	1.083435	4.176218
-1093.038768	-4.759578	4.186214
-1091.342989	-2.037614	4.196211
-1089.133538	1.295668	4.206208
-1087.288025	3.471432	4.216205
-1085.619667	1.118089	4.226202
-1083.773179	-1.618763	4.236198
-1081.809785	-2.218635	4.246195
-1079.780736	0.388802	4.256192
-1078.062539	3.679187	4.266189
-1076.165780	-6.766944	4.276186
-1074.267961	4.414171	4.286182
-1072.280684	2.128191	4.296179
-1070.760431	3.529083	4.306176
-1068.601731	8.225870	4.316173
-1066.454981	-2.298755	4.326170
-1064.877646	1.371510	4.336166
-1062.923747	-1.656866	4.346163
-1060.826464	-0.684654	4.356160
-1059.240223	-2.159960	4.366157
-1057.431321	2.289420	4.376154
-1055.572066	6.761378	4.386150
-1053.587997	3.962580	4.396147
-1051.725534	4.274804	4.406144
-1049.883197	4.601947	4.416141
-1047.968005	6.777228	4.426138
-1046.158868	9.473426	4.436134
-1044.444335	7.414503	4.446131
-1042.254092	2.043065	4.456128
-1040.639234	-4.052403	4.466125
-1038.520733	0.811360	4.476122
-1036.564081	-1.136579	4.486118
-1034.608160	1.873509	4.496115
-1033.166839	2.291250	4.506112
-1031.109360	0.261582	4.516109
-1029.456055	0.613681	4.526106
-1027.339047	0.332475	4.536102
-1025.486826	-4.041504	4.546099
-1023.645251	4.568186	4.556096
-1021.845010	5.262209	4.566093
-1019.833878	-2.627172	4.576090
-1017.760858	1.301838	4.586086
-1016.014571	-8.354497	4.596083
-1014.496506	1.616117	4.606080
-1012.300811	6.719181	4.616077
-1010.237382	6.885866	4.626074
-1008.447851	2.094644	4.636070
-1006.983296	5.179626	4.646067
-1004.967854	6.938158	4.656064
-1003.008478	0.841249	4.666061
-1000.932974	2.923027	4.676058
-999.061346	-1.781112	4.686054
-997.022077	-2.908536	4.696051
-995.612902	2.525993	4.706048
-993.797441	1.935751	4.716045
-991.759778	2.387862	4.726042
-989.563649	-2.871927	4.736038
-987.837886	-2.595090	4.746035
-986.258148	2.413764	4.756032
-984.242423	-2.543145	4.766029
-982.279743	-0.547508	4.776026
-980.526425	-4.061902	4.786022
-978.762909	-0.103843	4.796019
-976.658741	-4.093442	4.806016
-974.876126	0.565604	4.816013
-972.778630	1.356027	4.826010
-970.639383	-7.646107	4.836006
-968.997398	2.525361	4.846003
-967.578105	0.631768	4.856000
-965.803921	0.089330	4.865997
-963.574658	0.493938	4.875994
-961.578603	2.231711	4.885990
-959.618050	3.415173	4.895987
-957.915002	2.017465	4.905984
-956.212670	2.367499	4.915981
-954.245497	2.205718	4.925978
-952.204475	-2.631029	4.935974
-950.517271	2.920589	4.945971
-948.315673	7.394293	4.955968
-946.799685	7.164142	4.965965
-944.683278	4.343462	4.975962
-943.033313	1.868441	4.985958
-941.221980	7.787641	4.995955
-939.029283	5.264501	5.005952
-937.376519	3.406320	5.015949
-935.283445	-2.999645	5.025946
-933.475524	-0.050255	5.035942
-931.473111	3.113544	5.045939
-930.089728	4.914226	5.055936
-927.966280	1.615326	5.065933
-925.884486	-3.421272	5.075930
-923.925371	-1.952206	5.085926
-922.323621	-4.218174	5.095923
-920.277185	1.482829	5.105920
-918.586354	3.951202	5.115917
-916.807956	4.832793	5.125914
-914.662320	-1.599972	5.135910
-912.960786	4.464557	5.145907
-911.013046	6.545787	5.155904
-909.167645	3.381575	5.165901
-907.285408	7.748091	5.175898
-904.914423	0.795278	5.185894
-903.758840	5.132012	5.195891
-901.870313	2.925502	5.205888
-899.899443	5.794372	5.215885
-897.880886	5.805198	5.225882
-895.919894	2.717184	5.235878
-893.932602	5.312124	5.245875
-892.217326	3.612378	5.255872
-890.393648	5.049381	5.265869
-888.374646	4.246793	5.275866
-886.512301	3.799121	5.285862
-884.871734	2.139868	5.295859
-882.640110	-6.029968	5.305856
-881.242746	2.581355	5.315853
-879.211955	2.861203	5.325850
-877.270638	0.967738	5.335846
-875.304450	1.201372	5.345843
-873.467098	4.801392	5.355840
-871.725803	2.507534	5.365837
-869.509036	0.573112	5.375834
-867.864743	-2.017495	5.385830
-865.781021	-4.674047	5.395827
-864.215460	-4.065349	5.405824
-862.491071	3.175377	5.415821
-860.262320	2.685766	5.425818
-858.244416	0.294240	5.435814
-856.452504	-6.842510	5.445811
-854.755513	-3.472510	5.455808
-852.863153	2.103612	5.465805
-851.126425	0.061505	5.475802
-849.165206	2.255061	5.485798
-847.165974	-0.917352	5.495795
-845.351946	1.904958	5.505792
-843.303351	3.575279	5.515789
-841.358143	-0.382627	5.525786
-839.706392	-2.701808	5.535782
-837.511630	-2.781668	5.545779
-835.953385	2.320652	5.555776
-834.118972	5.317709	5.565773
-832.259453	0.861927	5.575770
-830.651065	3.590705	5.585766
-828.560596	5.754577	5.595763
-826.644058	3.806105	5.605760
-824.785516	5.096853	5.615757
-822.813385	5.879624	5.625754
-820.874730	2.989129	5.635750
-819.027134	5.049257	5.645747
-817.196629	7.891280	5.655744
-815.431145	4.872032	5.665741
-813.397168	7.296567	5.675738
-811.371854	1.877662	5.685734
-809.764532	2.395033	5.695731
-807.744792	5.489130	5.705728
-805.948383	11.795894	5.715725
-804.115091	7.453307	5.725722
-802.084700	5.658009	5.735718
-800.311425	3.178868	5.745715
-798.707132	9.723725	5.755712
-796.494068	9.173606	5.765709
-794.482888	11.479154	5.775706
-792.983400	9.768268	5.785702
-791.059521	12.610876	5.795699
-788.952360	12.857108	5.805696
-786.898918	8.894081	5.815693
-784.904652	8.671212	5.825690
-783.146187	7.582204	5.835686
-782.056217	2.167351	5.845683
-779.780145	5.509130	5.855680
-777.798458	5.691933	5.865677
-775.789814	5.500984	5.875674
-774.258307	2.659839	5.885670
-772.260545	7.880008	5.895667
-770.250776	7.362029	5.905664
-768.577923	6.635901	5.915661
-766.552564	8.674632	5.925658
-764.369222	9.558318	5.935654
-762.698366	-1.105828	5.945651
-761.081440	6.284207	5.955648
-759.158998	10.918172	5.965645
-757.186179	11.222256	5.975642
-754.947251	3.224713	5.985638
-753.141208	4.731594	5.995635
-751.538130	4.587343	6.005632
-749.539969	2.298845	6.015629
-747.988324	11.671010	6.025626
-746.083217	2.360174	6.035622
-743.801431	6.084743	6.045619
-742.020861	2.744393	6.055616
-740.543919	3.439881	6.065613
-738.491614	4.349231	6.075610
-736.378885	9.606202	6.085606
-734.590990	2.933760	6.095603
-732.762020	7.304760	6.105600
-730.836104	3.995194	6.115597
-728.843406	7.819579	6.125594
-727.216910	3.447698	6.135590
-724.993620	-0.302581	6.145587
-723.334700	4.539454	6.155584
-721.622688	4.129906	6.165581
-719.769678	2.236250	6.175578
-717.895071	8.739097	6.185574
-715.715651	8.586447	6.195571
-714.059311	6.968811	6.205568
-712.149798	7.185768	6.215565
-710.375159	8.575543	6.225562
-708.114479	6.811112	6.235558
-706.486121	7.890854	6.245555
-704.381644	7.801659	6.255552
-702.774673	5.029789	6.265549
-700.930794	4.870313	6.275546
-698.937602	5.631743	6.285542
-697.015766	5.601561	6.295539
-695.283972	5.897637	6.305536
-693.647076	9.525425	6.315533
-691.635767	8.773648	6.325530
-689.380578	8.392222	6.335526
-687.634018	10.329845	6.345523
-685.724634	10.891065	6.355520
-683.938933	11.563225	6.365517
-682.118405	7.283341	6.375514
-680.375429	10.946284	6.385510
-678.343497	8.503026	6.395507
-676.274197	13.516130	6.405504
-674.257379	7.288554	6.415501
-672.767053	3.285079	6.425498
-670.741748	2.742743	6.435494
-668.823450	5.067848	6.445491
-667.388563	2.938890	6.455488
-665.577944	6.622242	6.465485
-663.079504	5.899910	6.475482
-661.372982	5.520573	6.485478
-659.824573	0.992175	6.495475
-657.744185	3.896908	6.505472
-655.627600	4.889327	6.515469
-653.997559	12.493344	6.525466
-652.051515	11.630664	6.535462
-650.264137	7.768686	6.545459
-648.368890	2.685570	6.555456
-646.484978	10.030632	6.565453
-644.287670	7.472063	6.575450
-642.524791	6.442424	6.585446
-640.873720	5.323686	6.595443
-639.127452	6.893437	6.605440
-637.108080	6.727190	6.615437
-635.263541	2.860547	6.625434
-633.313469	5.154527	6.635430
-631.241283	1.874834	6.645427
-629.417744	5.707351	6.655424
-627.731740	1.891629	6.665421
-625.897061	8.981149	6.675418
-623.829216	9.871289	6.685414
-621.755093	4.474911	6.695411
-620.528800	4.786229	6.705408
-618.146375	12.289210	6.715405
-616.495187	5.626829	6.725402
-614.670693	10.490692	6.735398
-612.779661	3.490351	6.745395
-610.823461	5.509014	6.755392
-608.752023	1.879303	6.765389
-606.920801	2.097489	6.775386
-605.143142	8.921341	6.785382
-603.311698	4.721027	6.795379
-601.582915	6.934037	6.805376
-599.075062	6.489540	6.815373
-597.884707	14.015691	6.825370
-595.607842	10.472458	6.835366
-594.052217	10.607917	6.845363
-591.680464	15.417800	6.855360
-590.142321	7.354038	6.865357
-588.322732	9.892540	6.875354
-586.747784	10.500916	6.885350
-584.561926	8.647817	6.895347
-582.471211	6.913009	6.905344
-580.750196	8.792617	6.915341
-578.831903	13.674390	6.925338
-576.933093	12.087521	6.935334
-575.275650	5.498379	6.945331
-573.264871	2.005559	6.955328
-571.390881	6.879918	6.965325
-569.394233	7.653067	6.975322
-567.596689	7.598820	6.985318
-565.480779	1.169326	6.995315
-563.819007	9.555594	7.005312
-561.917278	1.574893	7.015309
-560.379888	3.998211	7.025306
-558.413118	3.696378	7.035302
-556.327278	-0.034189	7.045299
-554.145947	-2.705770	7.055296
-552.675477	1.427652	7.065293
-551.167805	5.329422	7.075290
-549.153274	0.421506	7.085286
-546.786718	7.389765	7.095283
-545.121304	2.889936	7.105280
-542.927749	5.515260	7.115277
-541.281201	2.877350	7.125274
-539.550747	1.948166	7.135270
-537.822173	0.707879	7.145267
-535.429649	6.521228	7.155264
-533.827357	7.278669	7.165261
-532.319863	7.565475	7.175258
-530.134322	7.284213	7.185254
-528.103951	4.275346	7.195251
-526.474850	6.610618	7.205248
-524.476230	9.365436	7.215245
-522.554030	7.407030	7.225242
-520.363649	4.454496	7.235238
-518.873792	2.949281	7.245235
-517.022966	2.720319	7.255232
-515.320236	1.769818	7.265229
-513.247561	5.735510	7.275226
-510.912588	5.847938	7.285222
-509.154764	2.838418	7.295219
-507.703658	5.347303	7.305216
-506.018554	6.053395	7.315213
-504.071208	8.097736	7.325210
-501.728778	8.909205	7.335206
-499.766129	2.834059	7.345203
-498.025963	0.924285	7.355200
-496.636146	7.781141	7.365197
-494.882669	5.527621	7.375194
-492.612141	4.805758	7.385190
-490.490507	6.146364	7.395187
-488.774160	4.752480	7.405184
-486.799274	1.419196	7.415181
-485.066506	7.735847	7.425178
-483.055705	1.086108	7.435174
-481.296396	0.740466	7.445171
-479.742384	5.590726	7.455168
-477.641541	8.062051	7.465165
-475.691412	4.482059	7.475162
-473.625993	7.115968	7.485158
-471.722391	2.652363	7.495155
-470.318034	7.270230	7.505152
-468.092398	2.985735	7.515149
-466.215552	2.791061	7.525146
-464.010192	9.852633	7.535142
-462.544039	7.708098	7.545139
-460.767665	2.572333	7.555136
-459.016999	10.257311	7.565133
-456.857384	5.426109	7.575130
-454.784886	1.837779	7.585126
-453.422119	5.567237	7.595123
-451.708462	7.235536	7.605120
-449.461065	14.383177	7.615117
-446.880418	4.128966	7.625114
-445.454354	0.424694	7.635110
-443.568078	-3.460102	7.645107
-442.087916	2.157696	7.655104
-440.018804	3.021622	7.665101
-438.178118	2.901535	7.675098
-436.283824	3.265871	7.685094
-434.351370	-0.873457	7.695091
-432.397673	3.034831	7.705088
-430.720217	4.367096	7.715085
-428.895807	7.685779	7.725082
-426.764143	3.682613	7.735078
-425.093959	1.440643	7.745075
-423.308841	2.487671	7.755072
-421.320094	-0.246450	7.765069
-419.650690	2.925727	7.775066
-417.651262	0.668377	7.785062
-415.329082	-5.236425	7.795059
-413.577851	-1.188663	7.805056
-411.917536	-6.146413	7.815053
-410.044550	-3.676277	7.825050
-408.046435	-1.217332	7.835046
-406.031500	-0.591103	7.845043
-404.387662	-1.212128	7.855040
-402.614792	-0.098571	7.865037
-400.780813	0.042163	7.875034
-398.655698	-2.109483	7.885030
-396.915574	-0.752783	7.895027
-395.102910	-3.326265	7.905024
-393.097160	-3.545394	7.915021
-391.230026	6.198451	7.925018
-389.417824	-5.793253	7.935014
-387.428446	3.258946	7.945011
-385.591679	1.024771	7.955008
-383.724583	10.633072	7.965005
-381.735112	5.287673	7.975002
-379.710633	3.744537	7.984998
-378.186732	4.595317	7.994995
-376.286806	1.932176	8.004992
-374.418353	2.302948	8.014989
-372.615529	3.200336	8.024986
-370.727834	0.653117	8.034982
-368.498220	-1.254810	8.044979
-366.862353	3.103245	8.054976
-364.906656	4.228928	8.064973
-362.975543	1.143889	8.074970
-361.349349	5.557751	8.084966
-359.416266	4.017656	8.094963
-357.425905	3.189394	8.104960
-355.353238	9.840639	8.114957
-353.397611	12.874032	8.124954
-352.001694	6.263819	8.134950
-349.893605	0.845918	8.144947
-348.154963	3.306721	8.154944
-346.257247	2.276594	8.164941
-344.469130	5.170364	8.174938
-342.622311	4.385307	8.184934
-340.680224	0.066122	8.194931
-338.470083	-0.139038	8.204928
-336.679382	-0.076220	8.214925
-334.866284	9.497895	8.224922
-332.979182	3.387950	8.234918
-331.032744	-1.923961	8.244915
-329.334733	5.251196	8.254912
-327.779603	8.331169	8.264909
-325.357731	0.776286	8.274906
-323.459487	5.404733	8.284902
-322.050000	5.112047	8.294899
-320.075153	4.839365	8.304896
-318.302368	6.165992	8.314893
-316.134606	11.872196	8.324890
-313.925473	1.235582	8.334886
-312.051977	5.881321	8.344883
-310.639568	5.777840	8.354880
-308.911127	-0.908369	8.364877
-306.760717	-0.016827	8.374874
-305.032413	1.866780	8.384870
-303.295519	4.492705	8.394867
-301.200543	2.313866	8.404864
-299.099650	-0.489238	8.414861
-297.488824	-0.901423	8.424858
-295.626009	2.007615	8.434854
-293.292384	1.775763	8.444851
-291.596697	-1.633250	8.454848
-290.212742	-1.791126	8.464845
-288.272133	0.565895	8.474842
-286.264971	-2.398970	8.484838
-284.206452	-2.985165	8.494835
-282.250450	-5.960223	8.504832
-280.522234	-2.600868	8.514829
-278.775665	1.081787	8.524826
-276.670100	-6.137028	8.534822
-274.681520	-5.326001	8.544819
-272.746638	-1.043700	8.554816
-271.414418	2.370146	8.564813
-269.647044	-2.011918	8.574810
-267.297434	-5.793136	8.584807
-265.283506	-3.296524	8.594803
-263.681164	5.487385	8.604800
-261.978401	1.074512	8.614797
-259.991439	-2.424763	8.624794
-258.073076	-0.961835	8.634791
-255.964243	1.953633	8.644787
-254.250804	7.355626	8.654784
-252.376085	-0.972076	8.664781
-250.345497	-3.642164	8.674778
-248.822269	2.576162	8.684775
-246.540725	-0.483966	8.694771
-244.600652	4.093869	8.704768
-243.260859	3.401745	8.714765
-241.705845	4.359476	8.724762
-238.866232	-1.142351	8.734759
-237.262763	-3.264129	8.744755
-235.733458	3.830928	8.754752
-233.982343	1.973913	8.764749
-231.440559	-1.529613	8.774746
-229.767334	-2.538577	8.784743
-227.810822	-1.170707	8.794739
-226.148402	2.746143	8.804736
-224.515923	1.578575	8.814733
-222.305049	6.744688	8.824730
-220.383340	1.556808	8.834727
-218.527697	-0.615724	8.844723
-216.946931	0.967568	8.854720
-214.878830	0.892748	8.864717
-212.904496	1.719289	8.874714
-210.883694	0.862947	8.884711
-208.651621	-2.175635	8.894707
-207.322840	0.194670	8.904704
-205.517176	-0.155653	8.914701
-203.722462	3.974853	8.924698
-201.816510	2.854846	8.934695
-199.775718	-0.929101	8.944691
-197.907176	-2.809008	8.954688
-195.738582	3.686752	8.964685
-194.475925	2.239182	8.974682
-192.047474	1.376168	8.984679
-190.536724	4.302161	8.994675
-188.656255	0.162754	9.004672
-186.773150	-0.590918	9.014669
-184.886563	4.915780	9.024666
-182.720500	-0.153141	9.034663
-181.010101	-2.749315	9.044659
-179.797775	-1.902731	9.054656
-177.456112	4.110443	9.064653
-175.557818	-0.929941	9.074650
-173.348698	-4.270465	9.084647
-171.568989	-4.365363	9.094643
-169.956546	-2.810804	9.104640
-168.154473	-4.780079	9.114637
-166.033145	-2.140987	9.124634
-164.064681	-0.816240	9.134631
-162.175757	-3.895148	9.144627
-160.373367	-2.703165	9.154624
-158.630765	-2.293330	9.164621
-156.533716	-3.911652	9.174618
-154.631417	-0.283713	9.184615
-153.021793	-4.438704	9.194611
-151.698569	-1.288463	9.204608
-149.311850	-3.820397	9.214605
-147.284528	-3.168510	9.224602
-145.253506	1.504830	9.234599
-143.334485	-4.986762	9.244595
-141.532865	-5.198436	9.254592
-139.900422	4.524926	9.264589
-138.191309	4.219248	9.274586
-136.241104	5.895322	9.284583
-133.946459	0.967593	9.294579
-132.131645	-0.861972	9.304576
-130.595802	4.815958	9.314573
-128.692699	0.320952	9.324570
-126.863584	-5.830746	9.334567
-124.746039	-8.177390	9.344563
-122.715570	-9.606433	9.354560
-121.179910	-5.438581	9.364557
-119.085383	1.945715	9.374554
-117.139046	-5.205025	9.384551
-115.295466	0.162456	9.394547
-113.700607	-2.788938	9.404544
-111.765228	-6.987924	9.414541
-109.630581	-0.434523	9.424538
-107.847140	-3.882236	9.434535
-106.036452	0.645529	9.444531
-104.147358	-1.384490	9.454528
-102.186147	1.478909	9.464525
-100.458475	-3.029475	9.474522
-98.605103	-1.990857	9.484519
-96.851557	-2.167791	9.494515
-94.976975	-0.595713	9.504512
-92.695833	-3.715771	9.514509
-91.061334	0.096842	9.524506
-88.949653	2.522632	9.534503
-87.187303	-2.528000	9.544499
-85.385011	-1.887292	9.554496
-83.821435	2.703411	9.564493
-81.311467	3.848784	9.574490
-79.895269	2.230267	9.584487
-77.967107	10.512589	9.594483
-76.010991	-0.183699	9.604480
-74.308273	2.188921	9.614477
-72.473161	-1.603967	9.624474
-70.460900	0.250012	9.634471
-68.493099	4.593558	9.644467
-66.364039	6.057986	9.654464
-64.879434	6.821552	9.664461
-62.864749	8.338398	9.674458
-60.944892	12.233304	9.684455
-59.181842	12.640858	9.694451
-57.152398	9.806241	9.704448
-55.566436	9.656876	9.714445
-53.251821	0.438083	9.724442
-51.470408	4.483991	9.734439
-49.798037	5.244610	9.744435
-47.774050	5.412188	9.754432
-46.130985	-1.495637	9.764429
-44.274730	9.191260	9.774426
-42.272303	6.628053	9.784423
-40.295783	0.180384	9.794419
-38.526170	1.523872	9.804416
-36.613524	4.292480	9.814413
-34.884891	5.422467	9.824410
-32.720445	-0.353151	9.834407
-30.938764	-3.421130	9.844403
-29.073993	0.694674	9.854400
-27.156626	5.427084	9.864397
-25.513691	-0.660645	9.874394
-23.333850	-0.153417	9.884391
-21.376879	-1.595504	9.894387
-19.777083	3.391737	9.904384
-17.889597	5.901454	9.914381
-15.977479	2.787401	9.924378
-13.827846	-0.648374	9.934375
-12.231631	0.276289	9.944371
-10.477664	-3.974942	9.954368
-8.432066	1.908087	9.964365
-6.648570	0.315930	9.974362
-5.356594	16.090371	9.984359
-3.967170	50.884834	9.994355
-2.603455	98.740940	10.004352
-1.211509	159.500167	10.014349
0.000000	216.360037	10.019354
0.734051	250.769752	10.024359
1.566248	282.479042	10.029363
1.861342	310.125312	10.034368
1.678785	327.647730	10.039373
2.218060	350.165882	10.044378
2.120746	373.032024	10.049383
3.147313	385.003887	10.054387
2.933427	412.613669	10.059392
3.234891	412.400971	10.064397
3.822670	428.208593	10.069402
3.697935	441.822976	10.074407
3.914716	440.849569	10.079411
4.027288	450.490283	10.084416
4.143310	443.401389	10.089421
4.064973	450.290089	10.094426
4.091254	454.893977	10.099431
4.405298	444.571134	10.104435
3.903645	444.939807	10.109440
3.827797	434.321076	10.114445
4.355014	448.922577	10.119450
4.253242	458.094413	10.124455
4.551789	452.402711	10.129459
4.198364	453.097663	10.134464
4.218562	454.459180	10.139469
4.107950	457.855409	10.144474
4.133008	465.590035	10.149479
4.511770	461.998698	10.154483
4.336741	472.263057	10.159488
4.784071	470.530936	10.164493
5.224376	474.013488	10.169498
4.586102	482.661959	10.174503
5.128641	486.832350	10.179507
4.909755	476.327718	10.184512
5.042391	459.721231	10.189517
4.590652	456.662280	10.194522
4.512900	460.749556	10.199527
4.826908	469.011326	10.204531
4.703827	482.033774	10.209536
5.208021	482.961793	10.214541
5.035453	483.108258	10.219546
4.876237	487.942506	10.224551
5.372333	491.236292	10.229555
5.026828	494.945558	10.234560
5.272542	487.197326	10.239565
5.395309	494.171559	10.244570
5.229635	500.163846	10.249575
5.297348	495.347333	10.254579
5.056255	500.277331	10.259584
5.098242	499.934657	10.264589
5.368721	506.102020	10.269594
4.861066	512.364520	10.274599
4.972921	512.869174	10.279603
5.436024	530.690832	10.284608
5.683824	546.620420	10.289613
5.666456	547.072630	10.294618
5.270128	549.192391	10.299623
5.252601	542.537257	10.304627
5.407132	545.152675	10.309632
5.766246	549.610709	10.314637
6.193224	548.689672	10.319642
6.263941	557.851331	10.324647
6.259167	555.196099	10.329651
5.960134	546.956264	10.334656
6.450546	557.269995	10.339661
6.067505	552.673247	10.344666
5.755161	559.169109	10.349671
6.272025	553.365334	10.354675
5.860970	561.183075	10.359680
5.963710	575.498676	10.364685
6.354213	580.002256	10.369690
6.292968	602.526640	10.374695
6.314127	598.918433	10.379699
6.558400	603.260783	10.384704
6.520779	592.547761	10.389709
6.574619	588.302790	10.394714
6.447362	600.622656	10.399719
6.568375	596.197617	10.404723
6.697797	592.131126	10.409728
6.662145	599.520977	10.414733
6.744182	600.157454	10.419738
6.739908	597.063196	10.424743
6.763544	596.411045	10.429747
6.879913	612.441785	10.434752
6.791288	603.608098	10.439757
6.780709	604.635442	10.444762
6.632391	620.751443	10.449767
6.999432	619.912519	10.454771
7.147028	638.149571	10.459776
7.301085	639.888798	10.464781
7.332571	643.316358	10.469786
7.157473	645.374516	10.474791
7.100695	647.074106	10.479795
7.301285	656.581833	10.484800
7.437173	645.913627	10.489805
7.614400	642.580219	10.494810
7.434663	657.097088	10.499815
7.750351	649.084945	10.504819
7.353350	647.742307	10.509824
7.409506	652.131137	10.514829
7.688842	654.468997	10.519834
7.325319	657.993106	10.524839
7.816857	651.272744	10.529843
7.644021	664.918068	10.534848
7.503140	658.263510	10.539853
7.821360	656.638373	10.544858
7.564568	672.250015	10.549863
8.138617	661.281676	10.554867
7.997211	662.449874	10.559872
7.784147	667.397223	10.564877
7.757614	675.026724	10.569882
7.929073	681.071007	10.574887
8.094523	686.955670	10.579891
8.099894	693.849466	10.584896
7.963050	687.465775	10.589901
7.986491	689.665154	10.594906
8.233470	700.454524	10.599911
8.116043	694.684458	10.604915
8.123300	698.400387	10.609920
8.320383	715.781569	10.614925
8.574903	723.453295	10.619930
8.470720	716.465586	10.624935
8.576006	722.452944	10.629939
8.818046	728.266859	10.634944
8.754217	728.826512	10.639949
8.845070	726.970755	10.644954
8.589584	733.252865	10.649959
8.606953	726.760613	10.654963
8.602962	731.545821	10.659968
8.544742	734.150778	10.664973
8.518182	732.235417	10.669978
8.421658	736.965442	10.674983
8.936365	753.612089	10.679987
8.830186	764.025094	10.684992
9.251790	774.772731	10.689997
9.568888	766.866073	10.695002
9.317840	771.215639	10.700007
9.165773	765.212676	10.705011
9.451388	766.666865	10.710016
9.519178	763.332460	10.715021
9.429477	770.503112	10.720026
9.221217	770.088080	10.725031
9.377571	764.196046	10.730035
9.494811	769.964272	10.735040
9.571482	770.425627	10.740045
9.457239	771.650358	10.745050
9.658224	773.217346	10.750055
9.391206	783.871885	10.755059
9.440565	775.556798	10.760064
9.626230	783.081679	10.765069
10.039300	777.369433	10.770074
9.617846	784.634869	10.775079
9.812998	788.649386	10.780083
9.971002	805.817504	10.785088
9.656697	810.481869	10.790093
10.384841	811.098358	10.795098
10.109827	812.460788	10.800103
9.873250	818.525352	10.805107
10.198473	822.591784	10.810112
10.196197	818.068220	10.815117
10.535673	809.804421	10.820122
10.287674	816.560929	10.825127
10.704695	805.823094	10.830131
10.440732	814.083098	10.835136
10.509083	815.011267	10.840141
10.500327	804.651169	10.845146
10.449678	809.841498	10.850151
10.278189	810.580269	10.855155
10.341952	822.932292	10.860160
10.142952	813.914915	10.865165
10.406312	812.989945	10.870170
10.447703	830.485580	10.875175
10.884703	838.678695	10.880179
10.896561	855.871928	10.885184
10.756400	859.942378	10.890189
11.209179	845.508446	10.895194
11.112488	856.560137	10.900199
11.236231	848.961718	10.905203
11.197535	856.808916	10.910208
10.918828	854.817566	10.915213
11.323691	855.474093	10.920218
11.047900	858.969783	10.925223
11.248491	858.580959	10.930227
11.076523	857.807602	10.935232
11.268547	858.257864	10.940237
11.225694	854.191634	10.945242
11.459187	859.223131	10.950247
11.314332	858.903406	10.955251
11.413772	859.054549	10.960256
11.209889	859.032310	10.965261
11.477506	859.006987	10.970266
11.100410	867.749436	10.975271
11.504425	880.873283	10.980275
12.022065	890.215871	10.985280
11.614077	885.057257	10.990285
11.630166	898.076716	10.995290
11.719121	895.264041	11.000295
11.982875	896.301602	11.005299
12.183745	901.880278	11.010304
12.231906	895.700039	11.015309
12.391319	899.874658	11.020314
12.093159	903.394324	11.025319
12.330443	903.322887	11.030323
12.300906	897.931223	11.035328
12.131881	897.488144	11.040333
12.119870	902.283464	11.045338
12.342697	909.100991	11.050343
12.174559	901.564435	11.055347
12.061860	905.878870	11.060352
12.309355	913.339923	11.065357
12.404821	902.260058	11.070362
12.340528	911.508231	11.075367
11.998319	903.171401	11.080371
12.087792	908.520103	11.085376
12.526241	916.442226	11.090381
13.058626	922.298799	11.095386
12.841756	922.141419	11.100391
13.045334	923.939291	11.105395
12.875364	918.218414	11.110400
12.855790	923.290165	11.115405
13.335614	916.770249	11.120410
13.146132	914.414255	11.125415
12.966285	906.085110	11.130419
13.110184	911.082249	11.135424
12.908822	912.349165	11.140429
13.091631	905.358741	11.145434
12.720211	913.801826	11.150439
13.243543	916.441306	11.155443
12.975867	929.043662	11.160448
13.111483	927.739936	11.165453
13.261567	924.005339	11.170458
13.258284	933.468062	11.175463
13.182547	931.301375	11.180467
13.992798	940.128827	11.185472
13.291158	935.146466	11.190477
13.265340	924.758820	11.195482
13.163655	932.191729	11.200487
13.342017	932.258288	11.205491
13.363278	959.167936	11.210496
13.598837	961.714663	11.215501
14.091093	951.057776	11.220506
14.001994	972.649190	11.225511
13.988735	961.762791	11.230515
14.190963	959.217654	11.235520
14.164994	960.240555	11.240525
14.219267	956.622245	11.245530
13.636373	969.809992	11.250535
13.997152	952.604132	11.255539
14.112107	965.353671	11.260544
13.836875	967.356409	11.265549
14.235746	951.222429	11.270554
14.066558	966.360664	11.275559
14.498455	965.366920	11.280563
14.431100	966.792835	11.285568
14.174759	965.412235	11.290573
14.333428	966.244006	11.295578
14.046835	970.763536	11.300583
14.328917	966.721298	11.305587
14.251747	972.794510	11.310592
14.306530	985.336095	11.315597
14.749820	993.281112	11.320602
14.672342	999.819778	11.325607
14.665334	989.366495	11.330611
14.756069	996.959467	11.335616
14.982578	995.648046	11.340621
15.129957	991.221928	11.345626
15.092687	993.710047	11.350631
15.180725	987.497277	11.355635
15.504374	994.603079	11.360640
15.353068	997.341670	11.365645
15.363900	987.336511	11.370650
15.229484	979.182298	11.375655
15.122222	975.254579	11.380659
15.163522	977.554357	11.385664
14.938522	988.112619	11.390669
15.282655	994.534783	11.395674
15.360005	1005.474238	11.400679
15.083817	998.697867	11.405683
15.239039	998.682738	11.410688
15.334151	1003.158934	11.415693
15.371222	998.126864	11.420698
15.526105	1005.016872	11.425703
15.611628	1004.211989	11.430707
15.571834	998.703628	11.435712
15.174763	1011.178237	11.440717
15.708443	1014.446747	11.445722
16.277005	1024.293445	11.450727
16.279191	1017.162232	11.455731
16.334273	1004.651990	11.460736
16.255376	1007.589351	11.465741
16.158551	998.390137	11.470746
16.027159	1002.907144	11.475751
16.012158	1005.842627	11.480755
16.376692	1005.318323	11.485760
16.143641	1003.153336	11.490765
16.320676	1001.081456	11.495770
16.319342	1005.355507	11.500775
15.662064	1008.226250	11.505779
16.041710	1006.530546	11.510784
15.704283	1008.830530	11.515789
16.119733	1020.940437	11.520794
16.448573	1032.644812	11.525799
16.800613	1034.757897	11.530803
16.692534	1038.456579	11.535808
16.854864	1035.343142	11.540813
16.860445	1035.529722	11.545818
16.806827	1041.381818	11.550823
16.911178	1037.610825	11.555827
16.703063	1041.114292	11.560832
16.701799	1040.490076	11.565837
17.174596	1033.450268	11.570842
16.871460	1038.425019	11.575847
16.552604	1032.711075	11.580851
16.601573	1027.225380	11.585856
16.216575	1041.853194	11.590861
16.478534	1034.757168	11.595866
16.461806	1041.268067	11.600871
16.942680	1055.857956	11.605875
17.160139	1057.398070	11.610880
17.034683	1057.392777	11.615885
17.135044	1060.626252	11.620890
17.347886	1069.802528	11.625895
17.786699	1058.343945	11.630899
17.609318	1057.134928	11.635904
17.363254	1057.428208	11.640909
17.146865	1061.965331	11.645914
17.398033	1065.471370	11.650919
17.510932	1062.488771	11.655923
17.525621	1063.573392	11.660928
17.170306	1070.604198	11.665933
17.746721	1076.548412	11.670938
17.945322	1088.132660	11.675943
17.826889	1088.667741	11.680947
17.955527	1090.913481	11.685952
18.060399	1093.384744	11.690957
18.380147	1093.948114	11.695962
18.140858	1090.046556	11.700967
18.085883	1077.185259	11.705971
17.995153	1066.419439	11.710976
17.851128	1094.865945	11.715981
18.043301	1089.671857	11.720986
18.249520	1097.381655	11.725991
18.225179	1096.256526	11.730995
18.376357	1094.386041	11.736000
18.481270	1094.238616	11.741005
18.699440	1088.633888	11.746010
18.363530	1087.987707	11.751015
18.248745	1093.219917	11.756019
18.479877	1084.270736	11.761024
18.434736	1091.656131	11.766029
18.508621	1085.482460	11.771034
18.281766	1085.106922	11.776039
18.391222	1092.772915	11.781043
18.802929	1087.241581	11.786048
18.411984	1097.451792	11.791053
18.977269	1098.539114	11.796058
18.755060	1109.334611	11.801063
18.670072	1116.707508	11.806067
19.423364	1113.786412	11.811072
19.387558	1117.890747	11.816077
19.049184	1110.431042	11.821082
18.862380	1104.646271	11.826087
18.852357	1104.511844	11.831091
19.587719	1116.937631	11.836096
19.242426	1125.711086	11.841101
19.758048	1111.947451	11.846106
19.457052	1104.088182	11.851111
19.452189	1099.649453	11.856115
19.307107	1083.687947	11.861120
19.016809	1093.807478	11.866125
19.088831	1109.627255	11.871130
19.105303	1122.707625	11.876135
19.104095	1126.789845	11.881139
19.450942	1124.639885	11.886144
19.124765	1130.649275	11.891149
19.584655	1131.355986	11.896154
19.408579	1155.643227	11.901159
19.757200	1154.321119	11.906163
20.130400	1157.932965	11.911168
19.956289	1157.836146	11.916173
20.119861	1158.596034	11.921178
20.206309	1166.298377	11.926183
20.064504	1158.150864	11.931187
20.064743	1161.638765	11.936192
20.095799	1159.651104	11.941197
20.208578	1157.173377	11.946202
20.374329	1163.577644	11.951207
20.178811	1159.811064	11.956211
20.095383	1162.581072	11.961216
20.210072	1164.877768	11.966221
20.245838	1151.280849	11.971226
20.305148	1159.202973	11.976231
19.961999	1162.489620	11.981235
20.401419	1161.623259	11.986240
20.190494	1164.586050	11.991245
20.685529	1162.208965	11.996250
20.293133	1159.914567	12.001255
20.452276	1171.218668	12.006259
20.798648	1182.892519	12.011264
21.147668	1184.483510	12.016269
20.846496	1176.885946	12.021274
20.703830	1179.306507	12.026279
20.940245	1177.056264	12.031283
20.649463	1178.000242	12.036288
20.546137	1171.938632	12.041293
21.076812	1174.993349	12.046298
21.014630	1182.316182	12.051303
21.224393	1171.561924	12.056307
21.060122	1166.139979	12.061312
21.096199	1160.699473	12.066317
20.838117	1164.496931	12.071322
20.828120	1165.602371	12.076327
20.709870	1158.826875	12.081331
20.940296	1153.510154	12.086336
20.850648	1166.981784	12.091341
20.775282	1157.217875	12.096346
20.891696	1162.971388	12.101351
20.688369	1169.118018	12.106355
21.264038	1166.305132	12.111360
21.175611	1172.814959	12.116365
21.263524	1167.116483	12.121370
21.045299	1167.077754	12.126375
21.154658	1148.694257	12.131379
20.569839	1131.215729	12.136384
20.711926	1141.843785	12.141389
20.682471	1136.004392	12.146394
21.135067	1134.668800	12.151399
20.892966	1141.730752	12.156403
21.181556	1135.193405	12.161408
20.818305	1136.983886	12.166413
20.917389	1133.529958	12.171418
20.983271	1129.578038	12.176423
20.581701	1125.526269	12.181427
20.698991	1125.799486	12.186432
20.717388	1130.531636	12.191437
20.501458	1124.460931	12.196442
20.757090	1129.517535	12.201447
20.732422	1127.929434	12.206451
20.750107	1117.444989	12.211456
21.036064	1133.747583	12.216461
21.034325	1123.298438	12.221466
20.794817	1128.988624	12.226471
21.038625	1134.388706	12.231475
21.320799	1127.668514	12.236480
21.042966	1142.859496	12.241485
21.063993	1138.175527	12.246490
21.378277	1137.440755	12.251495
21.266847	1140.462667	12.256499
20.592341	1114.771235	12.261504
20.333869	1115.965064	12.266509
20.816786	1121.086511	12.271514
20.697825	1127.849844	12.276519
20.825811	1134.283469	12.281523
20.997869	1136.245061	12.286528
20.502657	1137.642510	12.291533
20.503819	1133.661423	12.296538
20.948289	1129.618932	12.301543
20.539753	1129.410729	12.306547
21.037087	1131.860100	12.311552
20.979863	1144.132071	12.316557
20.836756	1134.761107	12.321562
20.754284	1138.319632	12.326567
20.678830	1151.373551	12.331571
21.516632	1142.156106	12.336576
20.975556	1140.831810	12.341581
21.208643	1135.636218	12.346586
20.878720	1116.964525	12.351591
20.681039	1110.402802	12.356595
20.580476	1104.946665	12.361600
20.386980	1118.246191	12.366605
20.715242	1126.684289	12.371610
21.102917	1136.804838	12.376615
20.823865	1137.229302	12.381619
20.964230	1130.976319	12.386624
20.499093	1124.827553	12.391629
20.604553	1140.468734	12.396634
20.666852	1143.542963	12.401639
20.825733	1150.133929	12.406643
20.723028	1145.686700	12.411648
20.823466	1150.724921	12.416653
20.736559	1136.080495	12.421658
20.990650	1147.945800	12.426663
20.516963	1150.597588	12.431667
21.029500	1146.306975	12.436672
20.582498	1149.424715	12.441677
20.846060	1155.886024	12.446682
20.855903	1155.367267	12.451687
21.001484	1152.075494	12.456691
21.052116	1147.266841	12.461696
20.938245	1153.027863	12.466701
21.062476	1152.049361	12.471706
20.932944	1134.890660	12.476711
20.462736	1125.562365	12.481715
20.829007	1135.841716	12.486720
20.708019	1154.302662	12.491725
21.042741	1149.120823	12.496730
20.745113	1139.028718	12.501735
20.663433	1137.873154	12.506739
20.800866	1139.257261	12.511744
20.850466	1147.195649	12.516749
20.786598	1139.819126	12.521754
20.757993	1140.680649	12.526759
20.731294	1153.033050	12.531763
21.205426	1150.378103	12.536768
20.748121	1139.391664	12.541773
20.797226	1133.701039	12.546778
20.942361	1126.611186	12.551783
20.910754	1122.755721	12.556787
20.912601	1114.221626	12.561792
20.411111	1134.076868	12.566797
20.620238	1127.801439	12.571802
20.838072	1134.852422	12.576807
20.994513	1146.737628	12.581811
21.325133	1138.504385	12.586816
21.038949	1137.273754	12.591821
21.112154	1131.812682	12.596826
21.172709	1132.417732	12.601831
20.843736	1132.435492	12.606835
21.227272	1126.142790	12.611840
20.669462	1131.642027	12.616845
20.669593	1127.625987	12.621850
21.019146	1125.213458	12.626855
20.527530	1131.386214	12.631859
20.815515	1127.363450	12.636864
20.646018	1131.777290	12.641869
20.432457	1130.105523	12.646874
20.703766	1133.775097	12.651879
20.534384	1129.707595	12.656883
20.927798	1126.978861	12.661888
20.739263	1133.717809	12.666893
20.467931	1133.628580	12.671898
20.935963	1133.824685	12.676903
21.083010	1135.660302	12.681907
21.267860	1127.827059	12.686912
21.403624	1135.576194	12.691917
21.217467	1129.764461	12.696922
21.154176	1130.780746	12.701927
20.570321	1121.106020	12.706931
20.826718	1124.045122	12.711936
20.507040	1135.542613	12.716941
20.759408	1131.166349	12.721946
20.957285	1135.225884	12.726951
20.966155	1139.696380	12.731955
20.735422	1137.521898	12.736960
20.937275	1138.433117	12.741965
21.231069	1131.680931	12.746970
21.016782	1111.618101	12.751975
20.828144	1104.135093	12.756979
20.578652	1105.461987	12.761984
20.824801	1104.438900	12.766989
20.270629	1104.748693	12.771994
20.852717	1116.809973	12.776999
20.632112	1136.356136	12.782003
20.931560	1138.927465	12.787008
21.048810	1138.941347	12.792013
20.986718	1126.957546	12.797018
21.158652	1119.203496	12.802023
20.846172	1110.527114	12.807027
20.572760	1112.631794	12.812032
20.789170	1110.337227	12.817037
20.685222	1108.412194	12.822042
20.863789	1108.820167	12.827047
20.583900	1114.028588	12.832051
20.932287	1108.909156	12.837056
20.644832	1113.757690	12.842061
20.706977	1120.261809	12.847066
21.095318	1137.360010	12.852071
20.552549	1127.740208	12.857075
21.175027	1120.142986	12.862080
20.664444	1113.516885	12.867085
20.517831	1111.376536	12.872090
21.061989	1122.437745	12.877095
20.843455	1121.910779	12.882099
20.757123	1112.785883	12.887104
20.650487	1117.489731	12.892109
21.130988	1126.271989	12.897114
20.881616	1119.749914	12.902119
20.755976	1117.462284	12.907123
20.925693	1109.871645	12.912128
20.878187	1108.697197	12.917133
20.867939	1111.458991	12.922138
21.060500	1110.473907	12.927143
20.929257	1120.510526	12.932147
21.017029	1112.148804	12.937152
20.926903	1116.120347	12.942157
20.846891	1122.341736	12.947162
20.963411	1123.780743	12.952167
20.596641	1115.888141	12.957171
20.582794	1114.837001	12.962176
20.542609	1118.227218	12.967181
20.612811	1119.551403	12.972186
20.845096	1122.280693	12.977191
20.677848	1123.287565	12.982195
20.486429	1120.657529	12.987200
20.178155	1124.781741	12.992205
20.415934	1134.840753	12.997210
20.679387	1140.189310	13.002215
20.786843	1146.734618	13.007219
20.924688	1145.898651	13.012224
21.284627	1148.838558	13.017229
21.166659	1146.748556	13.022234
21.032945	1145.511518	13.027239
20.733210	1132.541353	13.032243
20.807051	1124.519909	13.037248
20.663076	1127.007792	13.042253
20.788979	1134.359933	13.047258
20.897139	1136.324191	13.052263
20.553310	1144.473325	13.057267
20.754813	1150.387508	13.062272
20.897772	1164.808466	13.067277
20.766440	1165.074575	13.072282
21.122462	1154.458673	13.077287
21.290943	1142.031115	13.082291
21.289626	1136.374002	13.087296
20.985150	1135.699140	13.092301
21.087997	1128.140090	13.097306
21.045414	1125.258743	13.102311
20.716442	1120.163475	13.107315
20.829942	1110.841685	13.112320
20.705695	1120.502104	13.117325
20.807290	1117.716038	13.122330
20.903274	1123.751330	13.127335
20.631968	1125.539861	13.132339
20.747625	1121.577040	13.137344
20.674776	1123.016148	13.142349
20.854979	1120.625156	13.147354
21.019495	1120.595407	13.152359
20.867323	1132.627464	13.157363
20.876266	1123.886490	13.162368
20.685661	1126.412763	13.167373
20.955837	1125.410028	13.172378
20.983285	1116.108911	13.177383
20.755529	1122.844711	13.182387
20.801612	1122.371058	13.187392
20.924880	1132.757203	13.192397
20.894777	1128.859242	13.197402
20.963597	1112.469451	13.202407
20.913625	1119.184635	13.207411
20.940448	1122.334022	13.212416
21.032589	1124.605367	13.217421
20.630996	1116.114788	13.222426
20.900988	1113.792086	13.227431
20.490821	1119.890872	13.232435
20.960005	1121.218095	13.237440
20.998396	1128.245369	13.242445
20.534521	1116.670335	13.247450
20.968867	1121.257347	13.252455
20.924292	1125.547135	13.257459
20.831937	1107.654983	13.262464
21.074341	1106.235433	13.267469
20.723146	1094.233727	13.272474
20.775378	1088.598240	13.277479
20.781638	1095.743903	13.282483
20.978105	1085.644088	13.287488
20.784402	1096.059689	13.292493
20.876432	1095.624738	13.297498
20.761415	1087.147011	13.302503
20.605205	1086.766071	13.307507
20.390368	1091.181358	13.312512
20.670851	1102.678946	13.317517
20.590340	1119.241334	13.322522
20.823213	1118.841837	13.327527
20.891506	1124.018193	13.332531
20.967613	1121.828207	13.337536
21.006614	1128.892088	13.342541
20.702656	1134.782406	13.347546
21.009683	1124.592951	13.352551
20.579997	1133.425090	13.357555
20.831163	1123.202188	13.362560
20.782996	1128.462856	13.367565
20.847002	1132.145475	13.372570
20.871999	1133.588333	13.377575
21.050007	1133.564166	13.382579
20.854683	1117.999265	13.387584
20.871447	1109.550247	13.392589
20.826166	1104.365684	13.397594
21.038434	1098.122886	13.402599
20.644612	1097.987949	13.407603
20.671300	1102.618801	13.412608
20.894222	1090.138528	13.417613
20.870167	1100.720043	13.422618
21.037796	1094.696084	13.427623
20.648086	1099.512015	13.432627
21.030378	1095.422168	13.437632
20.369796	1097.841914	13.442637
20.564729	1100.609183	13.447642
20.841036	1109.486838	13.452647
20.828436	1126.677063	13.457651
21.039593	1117.324709	13.462656
21.021460	1111.266278	13.467661
21.130150	1098.688743	13.472666
21.129537	1093.562841	13.477671
20.838225	1094.989667	13.482675
20.848573	1093.385302	13.487680
20.753955	1100.329580	13.492685
20.979808	1095.551294	13.497690
21.275109	1094.182675	13.502695
20.641478	1102.413846	13.507699
21.190741	1097.752606	13.512704
21.384021	1103.666603	13.517709
21.328759	1098.267438	13.522714
21.093691	1088.922927	13.527719
20.588022	1073.893255	13.532723
20.580631	1069.771941	13.537728
20.903126	1073.848382	13.542733
20.718689	1073.739518	13.547738
21.045516	1069.974186	13.552743
20.372141	1060.464057	13.557747
20.334447	1073.819330	13.562752
20.642422	1095.422174	13.567757
20.645511	1099.064309	13.572762
20.838296	1104.449049	13.577767
21.037616	1105.683595	13.582771
21.292601	1107.887543	13.587776
21.161922	1098.536969	13.592781
20.856384	1082.538239	13.597786
20.780826	1075.621250	13.602791
20.670787	1084.522107	13.607795
20.649685	1075.932363	13.612800
20.726533	1072.939364	13.617805
20.626553	1078.422451	13.622810
21.031821	1090.003240	13.627815
20.581474	1095.952985	13.632819
20.701963	1103.200250	13.637824
21.132986	1100.362440	13.642829
20.868824	1104.425794	13.647834
21.107669	1084.754250	13.652839
20.901062	1084.368135	13.657843
20.800235	1077.715214	13.662848
20.515117	1080.621631	13.667853
20.448688	1081.918714	13.672858
20.733826	1095.308258	13.677863
20.597764	1115.203451	13.682867
20.616588	1113.217499	13.687872
20.743479	1118.113805	13.692877
20.153498	1113.569345	13.697882
20.526762	1112.613278	13.702887
20.545187	1113.788446	13.707891
20.468748	1109.484355	13.712896
20.424302	1122.205696	13.717901
20.599033	1120.116432	13.722906
21.106929	1131.804786	13.727911
20.713075	1131.397486	13.732915
21.000833	1121.647916	13.737920
20.783290	1119.937359	13.742925
20.632200	1122.981461	13.747930
20.866736	1116.869048	13.752935
20.721655	1120.393304	13.757939
20.734841	1125.671872	13.762944
20.843986	1133.812807	13.767949
20.793463	1141.362965	13.772954
20.835950	1131.642417	13.777959
20.653082	1130.114993	13.782963
20.964959	1138.138275	13.787968
21.112609	1132.669964	13.792973
20.527650	1129.781350	13.797978
20.942508	1132.582758	13.802983
20.739902	1128.371348	13.807987
21.066169	1122.258993	13.812992
21.251079	1114.334958	13.817997
20.855689	1128.076871	13.823002
21.199561	1119.254787	13.828007
20.701056	1123.085564	13.833011
20.659289	1125.676711	13.838016
20.946815	1115.959553	13.843021
20.871979	1124.561503	13.848026
20.859432	1117.708296	13.853031
20.861033	1122.965560	13.858035
21.100534	1121.791638	13.863040
20.801681	1124.420550	13.868045
20.716149	1132.934338	13.873050
20.832759	1130.084117	13.878055
20.712909	1124.775359	13.883059
20.539636	1119.573263	13.888064
20.776707	1125.913575	13.893069
20.841097	1128.376390	13.898074
20.743937	1121.599268	13.903079
20.435614	1129.312044	13.908083
20.492959	1116.247903	13.913088
20.749034	1129.260354	13.918093
20.560769	1128.243066	13.923098
20.944977	1122.847488	13.928103
20.921125	1126.092406	13.933107
20.961061	1121.833490	13.938112
20.761072	1128.993216	13.943117
20.533554	1133.770690	13.948122
20.444933	1125.558812	13.953127
20.848323	1142.220622	13.958131
20.920166	1146.810981	13.963136
20.847299	1142.845348	13.968141
20.580545	1142.529544	13.973146
20.962089	1149.477464	13.978151
20.476515	1152.887214	13.983155
20.664746	1161.017761	13.988160
20.972703	1160.921575	13.993165
20.815005	1163.754054	13.998170
21.143414	1156.954081	14.003175
20.748784	1153.887959	14.008179
20.678032	1146.079586	14.013184
20.967201	1153.361899	14.018189
20.869445	1149.357761	14.023207
20.989821	1139.722653	14.028224
20.804783	1133.590176	14.033242
20.788276	1136.309390	14.038259
20.579258	1138.465898	14.043277
20.767838	1157.750813	14.048295
20.915895	1161.945473	14.053312
21.093666	1168.606883	14.058330
20.998955	1163.931068	14.063347
21.158207	1168.055694	14.068365
21.126832	1165.893228	14.073383
20.988998	1147.198936	14.078400
21.002846	1148.225418	14.083418
20.654694	1137.463468	14.088435
21.337173	1157.996870	14.093453
21.015974	1155.476982	14.098471
21.240189	1157.737964	14.103488
20.881316	1168.637768	14.108506
21.323411	1159.478235	14.113523
21.192323	1161.794626	14.118541
21.144935	1168.916722	14.123559
21.400805	1154.768264	14.128576
21.259169	1151.395085	14.133594
20.942524	1148.347605	14.138611
21.151805	1149.335459	14.143629
21.440819	1163.049984	14.148647
21.573245	1167.345759	14.153664
21.473815	1158.345224	14.158682
21.083703	1154.430351	14.163699
21.282126	1139.042844	14.168717
21.088816	1147.673920	14.173735
21.437769	1158.852776	14.178752
21.109912	1163.550723	14.183770
21.470019	1163.565401	14.188787
21.451870	1167.497593	14.193805
21.264301	1173.804292	14.198823
21.325452	1163.073727	14.203840
21.441094	1171.128181	14.208858
21.122982	1168.711706	14.213875
21.032147	1169.317128	14.218893
20.412514	1173.111883	14.223911
20.897542	1184.309949	14.228928
21.568758	1191.315142	14.233946
21.592142	1205.619781	14.238963
22.029330	1203.896302	14.243981
22.052270	1198.476624	14.248999
22.032891	1194.074913	14.254016
21.754252	1180.290542	14.259034
21.814134	1165.427589	14.264051
21.961318	1155.330754	14.269069
21.611090	1166.197181	14.274087
21.557696	1158.515233	14.279104
21.784953	1162.225806	14.284122
21.934754	1157.087169	14.289139
21.891017	1158.358189	14.294157
21.553107	1158.527591	14.299175
21.795261	1166.117796	14.304192
21.912112	1164.373257	14.309210
21.772823	1160.631141	14.314227
21.916609	1156.957821	14.319245
21.422143	1168.056477	14.324263
21.769578	1173.885588	14.329280
22.113065	1176.456856	14.334298
22.265100	1184.824393	14.339315
22.242074	1171.925014	14.344333
21.994725	1170.647282	14.349351
21.985679	1168.754631	14.354368
21.851109	1166.147225	14.359386
21.778713	1170.048164	14.364403
22.221267	1179.635275	14.369421
21.907213	1184.771447	14.374439
22.120613	1185.574725	14.379456
22.107881	1197.233767	14.384474
22.254175	1195.179033	14.389491
22.073848	1183.819334	14.394509
22.414748	1201.145358	14.399527
22.421835	1189.788168	14.404544
21.997767	1169.753841	14.409562
21.805249	1173.997450	14.414579
22.339544	1184.812237	14.419597
22.228846	1196.391218	14.424615
22.439944	1195.264030	14.429632
22.427371	1192.023056	14.434650
22.251893	1196.580309	14.439667
22.550632	1189.507313	14.444685
22.530610	1203.608746	14.449703
22.246979	1199.616939	14.454720
22.498688	1200.060865	14.459738
22.287134	1202.869443	14.464755
22.903207	1192.403976	14.469773
22.401568	1184.090155	14.474791
22.377903	1180.444359	14.479808
22.508819	1187.985533	14.484826
22.301503	1199.033401	14.489843
22.284621	1202.320452	14.494861
22.522306	1202.341946	14.499879
22.726667	1196.763986	14.504896
22.665011	1204.787435	14.509914
22.459108	1202.856873	14.514931
22.729005	1203.472104	14.519949
22.440613	1200.637897	14.524967
22.139508	1202.726732	14.529984
22.234485	1194.605514	14.535002
22.319343	1199.267356	14.540019
22.151128	1200.470345	14.545037
22.685257	1217.275422	14.550055
22.891597	1223.040153	14.555072
22.989594	1226.280344	14.560090
22.766513	1233.486535	14.565107
23.055650	1223.116478	14.570125
22.988866	1229.666290	14.575143
22.926553	1213.827312	14.580160
22.883093	1208.941104	14.585178
22.831916	1213.516423	14.590195
22.994371	1198.129905	14.595213
22.882365	1204.996147	14.600231
22.773046	1208.749084	14.605248
23.270252	1222.540966	14.610266
22.689536	1216.756243	14.615283
23.173253	1227.083630	14.620301
23.302073	1229.833852	14.625319
22.740943	1209.033541	14.630336
23.232140	1215.358925	14.635354
23.489711	1224.770678	14.640371
22.854613	1214.058269	14.645389
23.181876	1209.025025	14.650407
23.105323	1216.991187	14.655424
23.354297	1211.063813	14.660442
23.326904	1215.935078	14.665459
22.994292	1198.193487	14.670477
23.320700	1206.886284	14.675495
23.309224	1219.829087	14.680512
23.531979	1214.427903	14.685530
23.193766	1201.666801	14.690547
23.298353	1202.569845	14.695565
22.913369	1206.176332	14.700583
23.288619	1213.528762	14.705600
23.358162	1223.549571	14.710618
23.398471	1223.365125	14.715635
23.630771	1217.524078	14.720653
23.586490	1225.993020	14.725671
23.527478	1223.317133	14.730688
23.696137	1223.072487	14.735706
23.622692	1225.055356	14.740723
23.452533	1224.102600	14.745741
23.399869	1216.907939	14.750759
23.969612	1222.783997	14.755776
23.751770	1209.620329	14.760794
23.645183	1211.144274	14.765811
22.963510	1196.739962	14.770829
23.438345	1211.284154	14.775847
23.338206	1226.303354	14.780864
23.357970	1229.201812	14.785882
23.356677	1230.222234	14.790899
23.517340	1230.937304	14.795917
23.598023	1226.628672	14.800935
23.595641	1228.980884	14.805952
23.695062	1227.831894	14.810970
23.626672	1250.519524	14.815987
23.993838	1255.463319	14.821005
23.907462	1256.640862	14.826023
23.949404	1254.302020	14.831040
24.022958	1234.342143	14.836058
24.048241	1228.559425	14.841075
24.207820	1220.400737	14.846093
24.410151	1227.461537	14.851111
24.427705	1225.423361	14.856128
24.354644	1222.680193	14.861146
24.242729	1224.945664	14.866163
24.251779	1217.943980	14.871181
24.028294	1221.296777	14.876199
23.977055	1222.141888	14.881216
24.529324	1218.483168	14.886234
24.219568	1225.067157	14.891251
24.352677	1224.188792	14.896269
24.123285	1223.426522	14.901287
24.071659	1227.406992	14.906304
24.560595	1217.720849	14.911322
23.864880	1214.708821	14.916339
24.077925	1226.250820	14.921357
24.170180	1221.300784	14.926375
24.038648	1229.705548	14.931392
24.409231	1221.185851	14.936410
24.321262	1223.502339	14.941427
24.043861	1225.046518	14.946445
24.218294	1223.702762	14.951463
24.250525	1223.965799	14.956480
24.307410	1225.756622	14.961498
24.243815	1235.760894	14.966515
23.966975	1230.718222	14.971533
24.118681	1233.851166	14.976551
24.119838	1255.699253	14.981568
24.485393	1246.831951	14.986586
24.288819	1257.535077	14.991603
24.875296	1255.909234	14.996621
25.047153	1252.733089	15.001639
24.881224	1252.380444	15.006656
24.933783	1247.340741	15.011674
24.460507	1227.276191	15.016691
25.094602	1233.497154	15.021709
25.123508	1224.138723	15.026727
24.624316	1225.174035	15.031744
24.492965	1220.554489	15.036762
24.408929	1215.955179	15.041779
24.287542	1226.835959	15.046797
25.187904	1240.115783	15.051815
24.757443	1241.229083	15.056832
25.173075	1250.826760	15.061850
24.800419	1246.584041	15.066867
24.599242	1254.062493	15.071885
24.844360	1247.287271	15.076903
24.784023	1256.180670	15.081920
25.017095	1251.403740	15.086938
24.986844	1247.219644	15.091955
25.049088	1254.595445	15.096973
25.218543	1251.234657	15.101991
24.673156	1256.927489	15.107008
25.164367	1248.896585	15.112026
25.052338	1260.258501	15.117043
24.825063	1255.012031	15.122061
25.307685	1249.477688	15.127079
25.013374	1260.386172	15.132096
24.684953	1253.819139	15.137114
24.828815	1249.714646	15.142131
24.840592	1241.130859	15.147149
24.734519	1253.667435	15.152167
24.756410	1261.948658	15.157184
25.423021	1268.303834	15.162202
25.210805	1277.209900	15.167219
25.105011	1281.036272	15.172237
25.645518	1277.674855	15.177255
25.517987	1283.839403	15.182272
25.828212	1278.176328	15.187290
25.936349	1274.978424	15.192307
25.071627	1261.908302	15.197325
25.897587	1260.759944	15.202343
25.101612	1256.987475	15.207360
25.724542	1260.369577	15.212378
25.674428	1262.694935	15.217395
25.554995	1265.833427	15.222413
25.666118	1254.286684	15.227431
25.381376	1248.783512	15.232448
25.557204	1256.165037	15.237466
25.731681	1272.286503	15.242483
25.834171	1266.808670	15.247501
25.591507	1260.334812	15.252519
25.517855	1262.312209	15.257536
25.868727	1260.716132	15.262554
25.924673	1276.996520	15.267571
25.633973	1277.970495	15.272589
25.756025	1274.406396	15.277607
25.596397	1281.076882	15.282624
25.935137	1277.147647	15.287642
26.060335	1272.003742	15.292659
25.921953	1283.772195	15.297677
25.971238	1277.638070	15.302695
25.648465	1279.083331	15.307712
25.795472	1276.271315	15.312730
25.949801	1268.738358	15.317747
25.804548	1276.259204	15.322765
25.695519	1270.324682	15.327783
25.727179	1282.928225	15.332800
25.559843	1289.486247	15.337818
25.897885	1282.152118	15.342835
26.049586	1284.976386	15.347853
26.354555	1287.597589	15.352871
25.960417	1285.621332	15.357888
26.290467	1293.902495	15.362906
26.194612	1298.604013	15.367923
26.134835	1312.385168	15.372941
26.485421	1306.443879	15.377959
26.417467	1298.192656	15.382976
25.918708	1282.948170	15.387994
26.298106	1299.325891	15.393011
25.998521	1311.210595	15.398029
26.302486	1317.901618	15.403047
26.111715	1319.172662	15.408064
26.456857	1309.368979	15.413082
26.543767	1312.200030	15.418099
26.549183	1311.660511	15.423117
26.862330	1303.803036	15.428135
26.486093	1301.474465	15.433152
26.348179	1307.434486	15.438170
26.367990	1305.481747	15.443187
26.564271	1308.327906	15.448205
26.572609	1296.030973	15.453223
26.509754	1300.770538	15.458240
26.336915	1306.421953	15.463258
26.793790	1298.474477	15.468275
26.670998	1306.381284	15.473293
26.845853	1306.315118	15.478311
26.837418	1303.814419	15.483328
26.761163	1305.908813	15.488346
26.959806	1309.319970	15.493363
26.617741	1303.022600	15.498381
26.814056	1296.256513	15.503399
26.738351	1304.848218	15.508416
26.438083	1304.380404	15.513434
26.885938	1295.120191	15.518451
26.482351	1305.547007	15.523469
26.733485	1306.552894	15.528487
26.869570	1324.435085	15.533504
27.113673	1329.720899	15.538522
27.055054	1327.085875	15.543539
27.143776	1337.051889	15.548557
27.521832	1330.286912	15.553575
27.226595	1319.326770	15.558592
27.082076	1312.347438	15.563610
27.261904	1307.932801	15.568627
26.814750	1305.010038	15.573645
27.167297	1316.497080	15.578663
27.365685	1337.188138	15.583680
27.212090	1332.484963	15.588698
27.510662	1329.822162	15.593715
27.137611	1323.301731	15.598733
27.561651	1325.266642	15.603751
27.216706	1311.538409	15.608768
26.981566	1324.258603	15.613786
27.445005	1323.577946	15.618803
27.244111	1332.216330	15.623821
27.580233	1330.983437	15.628839
27.891732	1329.770515	15.633856
27.783464	1328.418525	15.638874
27.526246	1314.352778	15.643891
27.426567	1309.231275	15.648909
27.563569	1316.799029	15.653927
27.586194	1327.474069	15.658944
27.583395	1329.183791	15.663962
27.819601	1323.171155	15.668979
27.780453	1328.959512	15.673997
27.351227	1313.531011	15.679015
27.386377	1322.758500	15.684032
27.601079	1331.161044	15.689050
27.744165	1324.094201	15.694067
27.627862	1332.366476	15.699085
27.521187	1332.425753	15.704103
27.636204	1329.961368	15.709120
27.586642	1332.406338	15.714138
27.999981	1334.334105	15.719155
27.496537	1332.236414	15.724173
27.782022	1334.424313	15.729191
27.567301	1335.328566	15.734208
27.765554	1333.913782	15.739226
28.092118	1346.206946	15.744243
28.121191	1366.554994	15.749261
28.089452	1349.645185	15.754279
28.017673	1347.188021	15.759296
28.051952	1361.559838	15.764314
28.128524	1363.800492	15.769331
27.955420	1361.566622	15.774349
28.339001	1366.512758	15.779367
28.341692	1369.782707	15.784384
28.083040	1374.142443	15.789402
28.283997	1367.994876	15.794419
28.343811	1367.581473	15.799437
28.123639	1366.544756	15.804455
28.301474	1356.228343	15.809472
28.065129	1364.079051	15.814490
28.623832	1363.758865	15.819507
28.230361	1366.501410	15.824525
28.341916	1365.777140	15.829543
28.358885	1369.404909	15.834560
28.437471	1371.144387	15.839578
28.613265	1360.733824	15.844595
28.241067	1372.358559	15.849613
28.242696	1366.401483	15.854631
28.700523	1363.075487	15.859648
28.290907	1368.924623	15.864666
28.261035	1360.660144	15.869683
28.327331	1372.415619	15.874701
28.619834	1374.169210	15.879719
28.247130	1374.131174	15.884736
28.578652	1387.519683	15.889754
29.196961	1389.636744	15.894771
29.012034	1383.003315	15.899789
29.030468	1389.830342	15.904807
29.104584	1375.714423	15.909824
29.014546	1372.556384	15.914842
28.962391	1357.895939	15.919859
28.648095	1360.828470	15.924877
28.681785	1359.839573	15.929895
28.768461	1371.950640	15.934912
28.974275	1386.172192	15.939930
28.990968	1380.658238	15.944947
29.351689	1386.460739	15.949965
29.018693	1387.449060	15.954983
29.262181	1388.253883	15.960000
29.157400	1390.222065	15.965018
29.273041	1377.571206	15.970035
29.376761	1367.682885	15.975053
29.279304	1370.665648	15.980071
28.984894	1355.260451	15.985088
28.962412	1360.339600	15.990106
29.316325	1376.138649	15.995123
29.445985	1381.129508	16.000141
29.518210	1375.297344	16.005159
29.331340	1361.727019	16.010176
29.333819	1369.780898	16.015194
29.751207	1365.898399	16.020211
29.497322	1356.658067	16.025229
29.790868	1358.109876	16.030247
29.910487	1357.280277	16.035264
29.667637	1354.904022	16.040282
29.895029	1357.789348	16.045299
29.362405	1362.924861	16.050317
29.142002	1356.818439	16.055335
29.412815	1350.004513	16.060352
28.974880	1356.052611	16.065370
29.471420	1370.245563	16.070387
29.790231	1376.762790	16.075405
29.739822	1378.259401	16.080423
29.767497	1379.052404	16.085440
29.712893	1380.212696	16.090458
30.252068	1375.066287	16.095475
30.021564	1369.921128	16.100493
29.495861	1355.964769	16.105511
30.104965	1359.284298	16.110528
29.551151	1372.621820	16.115546
29.787198	1370.360713	16.120563
29.785500	1384.743052	16.125581
29.616434	1381.167026	16.130599
29.923157	1367.117147	16.135616
29.887298	1385.769901	16.140634
30.108005	1381.891197	16.145651
29.934849	1374.951002	16.150669
29.814122	1381.320346	16.155687
29.889328	1371.290048	16.160704
29.857360	1380.223539	16.165722
29.950183	1389.396293	16.170739
30.456534	1403.708470	16.175757
30.373575	1412.452673	16.180775
30.354803	1397.247441	16.185792
30.077496	1399.270797	16.190810
30.278393	1407.559598	16.195827
30.401014	1405.369513	16.200845
30.315511	1413.505435	16.205863
30.679399	1406.545986	16.210880
30.384354	1417.277917	16.215898
30.357419	1418.903591	16.220915
30.575541	1410.337879	16.225933
30.732523	1417.916038	16.230951
30.943482	1401.079531	16.235968
30.338021	1390.358374	16.240986
30.294351	1397.260625	16.246003
30.548302	1408.032290	16.251021
30.476458	1415.552428	16.256039
30.458363	1406.652382	16.261056
30.411191	1415.355802	16.266074
30.266700	1412.153149	16.271091
30.579567	1417.479964	16.276109
30.332225	1414.259116	16.281127
30.578927	1413.066748	16.286144
30.445928	1428.148080	16.291162
30.601262	1444.597840	16.296179
31.140640	1442.972968	16.301197
30.908097	1450.794719	16.306215
30.884021	1440.120707	16.311232
31.251306	1447.458472	16.316250
31.156263	1449.332069	16.321267
31.351799	1444.071707	16.326285
31.156789	1440.283166	16.331303
31.295095	1442.694366	16.336320
31.077311	1435.482636	16.341338
31.235416	1433.710519	16.346355
31.532954	1422.745527	16.351373
30.919314	1422.500352	16.356391
30.954954	1420.787427	16.361408
31.114107	1434.638643	16.366426
31.504465	1440.800684	16.371443
31.504618	1447.599372	16.376461
31.153735	1452.415536	16.381479
31.326993	1439.477556	16.386496
31.383987	1443.975729	16.391514
31.204108	1440.845286	16.396531
31.454498	1441.714290	16.401549
31.273737	1439.602993	16.406567
31.342384	1437.599340	16.411584
31.352515	1437.883495	16.416602
31.414419	1436.854713	16.421619
31.660154	1433.941481	16.426637
31.345689	1445.729616	16.431655
31.627088	1433.400718	16.436672
31.661438	1439.698217	16.441690
31.467821	1440.171257	16.446707
31.332512	1444.728783	16.451725
31.564355	1466.050557	16.456743
31.987810	1473.064105	16.461760
31.927315	1478.367154	16.466778
31.918487	1465.624956	16.471795
31.925924	1467.760932	16.476813
31.717373	1479.706540	16.481831
32.054695	1468.700833	16.486848
31.798471	1467.780537	16.491866
32.154247	1469.292166	16.496883
31.896730	1462.042744	16.501901
31.999275	1477.204615	16.506919
32.318550	1466.452028	16.511936
32.548277	1465.485816	16.516954
32.019941	1472.080218	16.521971
31.966137	1469.795166	16.526989
31.811758	1476.154568	16.532007
32.097984	1466.392782	16.537024
32.178025	1472.305652	16.542042
32.231712	1466.197472	16.547059
32.465335	1461.876334	16.552077
32.334407	1484.973097	16.557095
32.185700	1478.594467	16.562112
32.777495	1481.064939	16.567130
32.409119	1481.147826	16.572147
32.401717	1473.575171	16.577165
31.987459	1474.015958	16.582183
32.341124	1465.977029	16.587200
32.276500	1468.611628	16.592218
32.658163	1483.173626	16.597235
32.692406	1488.358456	16.602253
32.463038	1483.715869	16.607271
32.460299	1490.752890	16.612288
32.844373	1488.911311	16.617306
32.592137	1494.695316	16.622323
32.749472	1491.223552	16.627341
32.566283	1495.975540	16.632359
32.759969	1497.665373	16.637376
32.794249	1490.681684	16.642394
32.708389	1496.808853	16.647411
32.767821	1489.325923	16.652429
32.823321	1498.638618	16.657447
32.863610	1497.211923	16.662464
32.906355	1491.747011	16.667482
32.929180	1495.746283	16.672499
33.107038	1488.271791	16.677517
32.846340	1499.864116	16.682535
32.938023	1491.324764	16.687552
33.295456	1495.747420	16.692570
32.942910	1494.472341	16.697587
33.343988	1509.896868	16.702605
33.344445	1513.365676	16.707623
33.391984	1505.098478	16.712640
33.311702	1500.860682	16.717658
33.343667	1508.541824	16.722675
33.833263	1496.940247	16.727693
33.127277	1493.494447	16.732711
33.014895	1492.315999	16.737728
33.447932	1504.577646	16.742746
33.489826	1523.349135	16.747763
33.809776	1516.996838	16.752781
33.907534	1522.840147	16.757799
33.992185	1508.063181	16.762816
33.384067	1490.196036	16.767834
33.611609	1482.979982	16.772851
33.491604	1486.019394	16.777869
33.800628	1507.695350	16.782887
33.638334	1500.865846	16.787904
33.767415	1498.134037	16.792922
33.669181	1517.907595	16.797939
33.947377	1520.636982	16.802957
33.827784	1517.633602	16.807975
33.765919	1516.725259	16.812992
33.988614	1510.797947	16.818010
33.850785	1519.807548	16.823027
34.132666	1514.722141	16.828045
34.121503	1511.892710	16.833063
34.055029	1518.286275	16.838080
34.388570	1520.028910	16.843098
34.002638	1508.140784	16.848115
34.010643	1500.491845	16.853133
34.072865	1504.718640	16.858151
33.782187	1515.198683	16.863168
33.908909	1515.085646	16.868186
33.750317	1517.945047	16.873203
33.739772	1521.827594	16.878221
33.505780	1516.540450	16.883239
33.854586	1529.255185	16.888256
34.272705	1534.163167	16.893274
34.304958	1540.451616	16.898291
34.503219	1541.587463	16.903309
34.280258	1538.707325	16.908327
34.454934	1542.430154	16.913344
34.561782	1533.862980	16.918362
34.499750	1541.812642	16.923379
34.330016	1540.199885	16.928397
34.809904	1541.718985	16.933415
34.406035	1539.795155	16.938432
34.348660	1535.588858	16.943450
34.351202	1550.241122	16.948467
34.905825	1557.410190	16.953485
35.213981	1563.512745	16.958503
34.895204	1551.863884	16.963520
35.119134	1532.593664	16.968538
34.735114	1540.754455	16.973555
34.670396	1533.011659	16.978573
34.742394	1541.233252	16.983591
34.781601	1565.669999	16.988608
35.129766	1565.337085	16.993626
34.881715	1566.368338	16.998643
35.171471	1572.301986	17.003661
35.081678	1565.899438	17.008679
35.120224	1572.852637	17.013696
35.225415	1569.984346	17.018714
35.235928	1571.602827	17.023731
35.444990	1569.122674	17.028749
35.466643	1569.799778	17.033767
35.283259	1572.928821	17.038784
35.402469	1562.525858	17.043802
35.236184	1571.938835	17.048819
35.431576	1567.542324	17.053837
35.534857	1565.337422	17.058855
35.500535	1568.274354	17.063872
35.425673	1567.296575	17.068890
35.250279	1563.738129	17.073907
35.612385	1568.419874	17.078925
35.518327	1566.565769	17.083943
35.392218	1565.146337	17.088960
35.747696	1558.833998	17.093978
35.521396	1562.924433	17.098995
35.548256	1558.580445	17.104013
35.646703	1560.192117	17.109031
35.637434	1570.747581	17.114048
36.027359	1567.065432	17.119066
35.997161	1562.796981	17.124083
35.842835	1559.508968	17.129101
36.358064	1554.340620	17.134119
36.253179	1558.054294	17.139136
36.432872	1563.421318	17.144154
36.034451	1570.129720	17.149171
36.034004	1569.869178	17.154189
36.560493	1567.720860	17.159207
36.332467	1556.574598	17.164224
36.298311	1538.861374	17.169242
35.976304	1541.664144	17.174259
36.101502	1537.806896	17.179277
35.915576	1541.599427	17.184295
35.986757	1555.520564	17.189312
36.553817	1557.558632	17.194330
35.852632	1566.264418	17.199347
35.674360	1568.341688	17.204365
36.102376	1563.360356	17.209383
36.022660	1567.505588	17.214400
36.196311	1574.377349	17.219418
36.264913	1582.644433	17.224435
36.116819	1596.367745	17.229453
36.152872	1595.943054	17.234471
36.171662	1597.132121	17.239488
36.724989	1593.844040	17.244506
36.690932	1595.103591	17.249523
36.148245	1603.979486	17.254541
36.484571	1598.321272	17.259559
36.566304	1616.653714	17.264576
36.837051	1623.664771	17.269594
36.783973	1625.376847	17.274611
36.472055	1620.860589	17.279629
36.773147	1620.778290	17.284647
36.820835	1631.411441	17.289664
36.957266	1628.382649	17.294682
37.171925	1622.526365	17.299699
37.002558	1625.452207	17.304717
37.467578	1604.568741	17.309735
37.055957	1622.030167	17.314752
37.293520	1625.774520	17.319770
37.225990	1622.291277	17.324787
37.425289	1621.540926	17.329805
37.445233	1613.969815	17.334823
37.375571	1619.135885	17.339840
37.684796	1615.657739	17.344858
37.702742	1620.995029	17.349875
37.262628	1612.463712	17.354893
37.365083	1596.530339	17.359911
37.173102	1601.527199	17.364928
37.266995	1611.317681	17.369946
37.242292	1620.077998	17.374963
37.309100	1621.820311	17.379981
37.187642	1612.715799	17.384999
37.473707	1618.509926	17.390016
37.834604	1614.194093	17.395034
37.705272	1614.787232	17.400051
37.403152	1618.690659	17.405069
37.565263	1617.869905	17.410087
37.389656	1620.049492	17.415104
37.668514	1632.622352	17.420122
37.658606	1642.232992	17.425139
37.894510	1642.116590	17.430157
38.270503	1642.020662	17.435175
38.317262	1642.269009	17.440192
38.067318	1625.125420	17.445210
38.035088	1612.459957	17.450227
37.724581	1628.751964	17.455245
38.450009	1626.708519	17.460263
37.903880	1635.054257	17.465280
38.194963	1631.655210	17.470298
38.402151	1634.570827	17.475315
38.137367	1641.505585	17.480333
38.277213	1635.216013	17.485351
38.189440	1637.543553	17.490368
38.352157	1631.662310	17.495386
37.999084	1631.489002	17.500403
38.457053	1635.317628	17.505421
38.431561	1630.931017	17.510439
38.445725	1637.217093	17.515456
38.485038	1636.953277	17.520474
38.379182	1633.849871	17.525491
38.420817	1641.541627	17.530509
38.514047	1634.488311	17.535527
38.588882	1636.819470	17.540544
38.632192	1643.567531	17.545562
38.730522	1642.173003	17.550579
38.599970	1636.964549	17.555597
38.483089	1645.782816	17.560615
38.808666	1665.980405	17.565632
38.824645	1670.154537	17.570650
39.269996	1667.605900	17.575667
39.341712	1674.662918	17.580685
39.383241	1643.948960	17.585703
39.169745	1638.193643	17.590720
38.945835	1633.874913	17.595738
38.866273	1631.728126	17.600755
38.834689	1643.265917	17.605773
39.245413	1655.889816	17.610791
39.325621	1667.292697	17.615808
39.571967	1657.096637	17.620826
39.490084	1643.486016	17.625843
39.149490	1641.931680	17.630861
39.146891	1629.948991	17.635879
38.975009	1639.550783	17.640896
39.074949	1661.853812	17.645914
39.405744	1656.935188	17.650931
39.280428	1669.928202	17.655949
39.161487	1669.118227	17.660967
39.246057	1666.580262	17.665984
39.412608	1666.685616	17.671002
39.297878	1663.957782	17.676019
39.138480	1679.504563	17.681037
39.411030	1686.977201	17.686055
39.769945	1693.319558	17.691072
39.574630	1688.384031	17.696090
39.998018	1689.473022	17.701107
39.695542	1691.041231	17.706125
40.227927	1684.119707	17.711143
40.124642	1691.461884	17.716160
39.817937	1679.994735	17.721178
40.394882	1684.286886	17.726195
40.506311	1693.645232	17.731213
40.497777	1675.037991	17.736231
40.289528	1673.442848	17.741248
40.418573	1669.497497	17.746266
40.345825	1653.201544	17.751283
39.562883	1664.637836	17.756301
39.726974	1667.513599	17.761319
39.784567	1683.538590	17.766336
39.817088	1688.147733	17.771354
40.397997	1682.290843	17.776371
40.124385	1690.803688	17.781389
40.266648	1685.317708	17.786407
40.227468	1695.294463	17.791424
40.380595	1706.496266	17.796442
41.093224	1704.421145	17.801459
40.774660	1694.982229	17.806477
40.617791	1690.759087	17.811495
40.716494	1681.789246	17.816512
40.450810	1689.444337	17.821530
40.630795	1698.838181	17.826547
40.747448	1717.493925	17.831565
40.801044	1716.627197	17.836583
40.632553	1714.075914	17.841600
40.781360	1726.406157	17.846618
40.960600	1711.748624	17.851635
40.724219	1722.815231	17.856653
40.955862	1721.512024	17.861671
40.782414	1718.822598	17.866688
41.043512	1716.238608	17.871706
40.973956	1713.273860	17.876723
40.853223	1721.233678	17.881741
40.891996	1714.458592	17.886759
41.065656	1731.843020	17.891776
40.986017	1738.098759	17.896794
41.302239	1739.648304	17.901811
41.012337	1738.097079	17.906829
41.426856	1737.968952	17.911847
41.647257	1728.520686	17.916864
41.521695	1727.859104	17.921882
41.600570	1725.982810	17.926899
41.770651	1731.261373	17.931917
42.148557	1730.192566	17.936935
41.774511	1737.877678	17.941952
41.636231	1723.656114	17.946970
41.795091	1707.686970	17.951987
41.473174	1701.413939	17.957005
41.550226	1726.524052	17.962023
41.475265	1736.529411	17.967040
41.684038	1734.180793	17.972058
41.892599	1728.648387	17.977075
41.946758	1738.085091	17.982093
41.834705	1735.441835	17.987111
41.904423	1727.997582	17.992128
41.680942	1730.034588	17.997146
42.003245	1726.515588	18.002163
41.478677	1733.730782	18.007181
41.818291	1742.868123	18.012199
42.037358	1751.059492	18.017216
41.891258	1757.292378	18.022234
42.236757	1757.515100	18.027251
42.099266	1760.265009	18.032269
42.358699	1762.757078	18.037287
42.582589	1757.587037	18.042304
42.546294	1765.104792	18.047322
42.683897	1747.239033	18.052339
42.545059	1757.767621	18.057357
42.463565	1760.139777	18.062375
42.758189	1760.311372	18.067392
42.649676	1765.053394	18.072410
43.002615	1759.743496	18.077427
42.537789	1765.682173	18.082445
42.979550	1761.894230	18.087463
43.203660	1753.522603	18.092480
42.948961	1766.202408	18.097498
42.847423	1755.595406	18.102515
43.211920	1759.547976	18.107533
43.454748	1754.689291	18.112551
43.658971	1759.876567	18.117568
43.191617	1739.044897	18.122586
43.326846	1723.501884	18.127603
43.255392	1720.860725	18.132621
42.945820	1718.828173	18.137639
42.657332	1713.537312	18.142656
42.501729	1729.386281	18.147674
43.531860	1740.308593	18.152691
43.417785	1753.159969	18.157709
43.457564	1758.884946	18.162727
43.323524	1757.360938	18.167744
43.451074	1756.640602	18.172762
43.711799	1757.179862	18.177779
43.614364	1760.754495	18.182797
43.585777	1757.866976	18.187815
43.565158	1754.701682	18.192832
43.524319	1759.542348	18.197850
43.580807	1747.281691	18.202867
43.546745	1749.503964	18.207885
43.451220	1755.603360	18.212903
43.596004	1750.445309	18.217920
43.538292	1752.800786	18.222938
43.613826	1746.108370	18.227955
43.361779	1757.318255	18.232973
43.563879	1766.039768	18.237991
43.777343	1774.119892	18.243008
43.751810	1785.411446	18.248026
43.780280	1777.991567	18.253043
43.664633	1783.023040	18.258061
43.745182	1778.293758	18.263079
44.137473	1776.155036	18.268096
44.070709	1796.050336	18.273114
44.639852	1803.580458	18.278131
44.040583	1798.381834	18.283149
44.117403	1801.852181	18.288167
44.325787	1806.791486	18.293184
44.130005	1808.292982	18.298202
44.101062	1808.177495	18.303219
43.909781	1803.177453	18.308237
44.030629	1806.236661	18.313255
44.413113	1818.320195	18.318272
44.562017	1825.090392	18.323290
45.010566	1828.874614	18.328307
45.127244	1829.011359	18.333325
44.715799	1829.922593	18.338343
45.234966	1821.696427	18.343360
44.984168	1807.742926	18.348378
44.811638	1800.468536	18.353395
44.799443	1814.181337	18.358413
44.871990	1828.908484	18.363431
45.044662	1832.178523	18.368448
44.743473	1840.069330	18.373466
44.897233	1842.669305	18.378483
45.029454	1831.366186	18.383501
45.054480	1830.440170	18.388519
45.179391	1828.302397	18.393536
45.470037	1825.583386	18.398554
45.526200	1825.610807	18.403571
45.488909	1827.624565	18.408589
45.520444	1828.311405	18.413607
45.749444	1827.515790	18.418624
45.493598	1826.628874	18.423642
45.323207	1824.399590	18.428659
45.421745	1822.377377	18.433677
44.929730	1830.932862	18.438695
45.577804	1825.973568	18.443712
45.542463	1830.451852	18.448730
45.610105	1827.749027	18.453747
45.762987	1839.330146	18.458765
45.794674	1855.086100	18.463783
45.972403	1864.401287	18.468800
46.040788	1872.685493	18.473818
46.244322	1863.302251	18.478835
46.145476	1841.280747	18.483853
45.650459	1836.851731	18.488871
46.193768	1847.515026	18.493888
46.069233	1854.536081	18.498906
45.672727	1864.364341	18.503923
46.243367	1860.391266	18.508941
45.991072	1859.539571	18.513959
46.281163	1851.609390	18.518976
46.340126	1860.144053	18.523994
46.435108	1863.191170	18.529011
46.455293	1850.156642	18.534029
46.334343	1860.352665	18.539047
46.257703	1855.367206	18.544064
46.354044	1853.805657	18.549082
46.106895	1849.619212	18.554099
46.798492	1844.384701	18.559117
46.520568	1863.240571	18.564135
46.740484	1872.385912	18.569152
46.766280	1876.987209	18.574170
46.972680	1876.013948	18.579187
47.046683	1866.222545	18.584205
46.388420	1876.128374	18.589223
46.439102	1872.029065	18.594240
46.639747	1880.730416	18.599258
46.908784	1873.144033	18.604275
47.102398	1868.912724	18.609293
46.509664	1885.992060	18.614311
46.922143	1888.655177	18.619328
46.883333	1899.345472	18.624346
47.124305	1904.957651	18.629363
47.323659	1899.042071	18.634381
47.041435	1903.054375	18.639399
47.464227	1894.875407	18.644416
47.597892	1899.875984	18.649434
47.082794	1898.772065	18.654451
47.724355	1891.580913	18.659469
47.606463	1903.834962	18.664487
48.189541	1894.095252	18.669504
48.091888	1898.952789	18.674522
47.549641	1895.631990	18.679539
47.953414	1891.727680	18.684557
47.731508	1895.191385	18.689575
47.895691	1892.840939	18.694592
48.404738	1893.907777	18.699610
48.338426	1890.165572	18.704627
48.290521	1885.310233	18.709645
48.180553	1890.657341	18.714663
48.213925	1876.768061	18.719680
48.300756	1866.667728	18.724698
48.209538	1868.150120	18.729715
48.201938	1845.894828	18.734733
47.988124	1861.004608	18.739751
48.466485	1868.401491	18.744768
48.268812	1883.916450	18.749786
48.097663	1883.788333	18.754803
48.436634	1879.895136	18.759821
48.146703	1893.989526	18.764839
48.588400	1892.551460	18.769856
48.596220	1885.502045	18.774874
48.262083	1891.029337	18.779891
48.738931	1884.783472	18.784909
48.547440	1881.688399	18.789927
48.277925	1886.522243	18.794944
48.590834	1880.680912	18.799962
48.440604	1882.325017	18.804979
48.769577	1881.787883	18.809997
48.938532	1905.040174	18.815015
48.846644	1909.448639	18.820032
48.880038	1921.345619	18.825050
48.946897	1927.480241	18.830067
49.220878	1907.627284	18.835085
49.519673	1912.016802	18.840103
49.279502	1911.277607	18.845120
49.569603	1906.845077	18.850138
49.199321	1912.947149	18.855155
49.418286	1913.977100	18.860173
49.618502	1920.464885	18.865191
49.274089	1911.277544	18.870208
49.603177	1907.382491	18.875226
49.574484	1914.854127	18.880243
49.535861	1910.597264	18.885261
49.595729	1914.893480	18.890279
49.333631	1908.806589	18.895296
49.276230	1914.514029	18.900314
49.066681	1917.740158	18.905331
49.577360	1913.470619	18.910349
49.818672	1916.341851	18.915367
49.821401	1935.493432	18.920384
50.168177	1935.399364	18.925402
49.527057	1944.174988	18.930419
49.461704	1932.285515	18.935437
49.543812	1930.617724	18.940455
49.771643	1938.615146	18.945472
50.077862	1933.350999	18.950490
49.914169	1950.928963	18.955507
50.245505	1958.610579	18.960525
49.928890	1959.259467	18.965543
49.937462	1961.589829	18.970560
50.308338	1964.187249	18.975578
50.298566	1968.491876	18.980595
50.406514	1956.678984	18.985613
50.580758	1962.357356	18.990631
50.290108	1967.015692	18.995648
50.449687	1959.532297	19.000666
50.381532	1970.056784	19.005683
50.605210	1977.335554	19.010701
50.760504	1984.950897	19.015719
51.007158	1988.657162	19.020736
51.258476	1989.121657	19.025754
51.270455	1985.652263	19.030771
51.078088	1969.535170	19.035789
50.872228	1969.718161	19.040807
50.954412	1970.484917	19.045824
51.488251	1971.297085	19.050842
50.952484	1979.497507	19.055859
51.318915	1982.777276	19.060877
51.200152	1990.928651	19.065895
50.716134	1991.806661	19.070912
51.292941	1987.121381	19.075930
50.812447	1995.408804	19.080947
51.360220	1992.320046	19.085965
51.182860	1985.978802	19.090983
51.186597	1991.809663	19.096000
51.675967	1990.509497	19.101018
51.650632	2019.351110	19.106035
51.624191	2010.660052	19.111053
51.563396	2018.002184	19.116071
51.340435	2018.276701	19.121088
51.948493	2015.652075	19.126106
51.740092	2022.233193	19.131123
51.908427	2015.191637	19.136141
51.870732	2012.715135	19.141159
51.751195	2022.676344	19.146176
51.938373	2017.365249	19.151194
51.817234	2022.742273	19.156211
51.999677	2033.850297	19.161229
52.517003	2047.572921	19.166247
52.326521	2048.360444	19.171264
52.662318	2045.464340	19.176282
52.779599	2032.901266	19.181299
52.775264	2010.160864	19.186317
52.957161	2003.609965	19.191335
52.535117	2007.162740	19.196352
52.772129	2001.894294	19.201370
52.695785	2005.380709	19.206387
52.452691	2005.874848	19.211405
52.889302	1996.223188	19.216423
52.747213	2003.376863	19.221440
52.451759	2000.008215	19.226458
52.665464	2013.158769	19.231475
52.905410	2030.856617	19.236493
53.106908	2031.264686	19.241511
53.010966	2044.682165	19.246528
53.306589	2043.368751	19.251546
52.934453	2041.430358	19.256563
53.222105	2042.630850	19.261581
53.297728	2045.690772	19.266599
53.011710	2045.554785	19.271616
53.373136	2032.517904	19.276634
53.078534	2044.113292	19.281651
53.066369	2037.061722	19.286669
53.369189	2034.726467	19.291687
53.315626	2038.759451	19.296704
53.430920	2035.262488	19.301722
53.173839	2039.097658	19.306739
53.200668	2053.609597	19.311757
53.440840	2058.536839	19.316775
53.510509	2066.474031	19.321792
53.757042	2061.125575	19.326810
53.633353	2058.887068	19.331827
53.625716	2058.043814	19.336845
53.993058	2059.953181	19.341863
53.601854	2062.358008	19.346880
54.060420	2072.997401	19.351898
54.173604	2080.667262	19.356915
54.375207	2084.106827	19.361933
54.423431	2084.053315	19.366951
54.418136	2086.674696	19.371968
54.271849	2080.742708	19.376986
54.339154	2094.812648	19.382003
54.333754	2089.942082	19.387021
54.636188	2085.644808	19.392039
54.505083	2090.179748	19.397056
54.892234	2082.477725	19.402074
54.539812	2080.627692	19.407091
54.849254	2080.694377	19.412109
55.174494	2083.282316	19.417127
54.719328	2084.097502	19.422144
55.280442	2071.015327	19.427162
54.952221	2078.397039	19.432179
55.008847	2080.915269	19.437197
55.224485	2084.766658	19.442215
55.172050	2080.714112	19.447232
55.163459	2077.810899	19.452250
55.059068	2086.814699	19.457267
55.091434	2080.826486	19.462285
55.132770	2079.096369	19.467303
54.587185	2090.361545	19.472320
54.872942	2074.675036	19.477338
54.918441	2085.764051	19.482355
54.964761	2102.622619	19.487373
55.365944	2095.018592	19.492391
55.202253	2101.110515	19.497408
55.194959	2099.747838	19.502426
55.491756	2110.369317	19.507443
55.544421	2109.962633	19.512461
55.809248	2125.671799	19.517479
55.670946	2139.835307	19.522496
55.747681	2133.879630	19.527514
55.588821	2141.577657	19.532531
55.562953	2138.074556	19.537549
55.968244	2144.650125	19.542567
55.834094	2141.683377	19.547584
56.093847	2138.623105	19.552602
56.183392	2145.136259	19.557619
55.836352	2145.009158	19.562637
56.441908	2147.475021	19.567655
56.500739	2156.853689	19.572672
56.818696	2159.643706	19.577690
56.875223	2144.461849	19.582707
56.485740	2137.873014	19.587725
56.695633	2130.349411	19.592743
56.676962	2131.561480	19.597760
56.657315	2122.456933	19.602778
56.529075	2125.199413	19.607795
56.869496	2143.361725	19.612813
57.327805	2151.215788	19.617831
56.794838	2145.902119	19.622848
56.935526	2133.898021	19.627866
56.846884	2139.121462	19.632883
56.756140	2149.440858	19.637901
57.297559	2144.533616	19.642919
57.080194	2154.487269	19.647936
56.972356	2148.311622	19.652954
57.071388	2149.694877	19.657971
56.572071	2148.862679	19.662989
56.978998	2146.588310	19.668007
57.017862	2158.486501	19.673024
57.751058	2172.853029	19.678042
57.514762	2180.886839	19.683059
57.412287	2186.984837	19.688077
57.418587	2181.919296	19.693095
57.710139	2181.686644	19.698112
58.034062	2183.090406	19.703130
57.796378	2180.476489	19.708147
57.519157	2182.620418	19.713165
57.794353	2187.085725	19.718183
57.723710	2178.743539	19.723200
57.864503	2181.882485	19.728218
58.348712	2192.257684	19.733235
58.243280	2212.080997	19.738253
58.628100	2204.098959	19.743271
57.977027	2206.229813	19.748288
58.257854	2206.946379	19.753306
58.546588	2206.840211	19.758323
58.593057	2204.666617	19.763341
59.121878	2206.105341	19.768359
58.659490	2197.444822	19.773376
58.761330	2177.999832	19.778394
58.745561	2173.538556	19.783411
58.361035	2173.778169	19.788429
58.814856	2190.351974	19.793447
58.671713	2202.601923	19.798464
58.924870	2210.817222	19.803482
58.563600	2208.652896	19.808499
58.643150	2207.359584	19.813517
59.092256	2202.389006	19.818535
58.762888	2207.035938	19.823552
58.853721	2204.586195	19.828570
58.816287	2205.217937	19.833587
58.821076	2224.756189	19.838605
59.602645	2234.059813	19.843623
59.192647	2241.331194	19.848640
59.194392	2240.297711	19.853658
59.113689	2240.821896	19.858675
59.126447	2240.316524	19.863693
59.519721	2241.524123	19.868711
59.520093	2244.165427	19.873728
59.293226	2240.459722	19.878746
59.661662	2241.685755	19.883763
59.559655	2259.186942	19.888781
59.725529	2254.291685	19.893799
60.040176	2253.817242	19.898816
60.029183	2251.364474	19.903834
60.375978	2249.998563	19.908851
60.146915	2261.093826	19.913869
59.923572	2249.496593	19.918887
60.156448	2254.973260	19.923904
59.972640	2252.329617	19.928922
60.241894	2250.821860	19.933939
59.968567	2264.273877	19.938957
60.299821	2272.428567	19.943975
60.340265	2279.065961	19.948992
60.414593	2283.454695	19.954010
60.877657	2284.120332	19.959027
60.893933	2284.978337	19.964045
61.131032	2285.333058	19.969063
60.837541	2282.793268	19.974080
60.848102	2293.267068	19.979098
60.928611	2282.553287	19.984115
60.950326	2280.909989	19.989133
60.929446	2281.004959	19.994151
61.230483	2285.535165	19.999168
60.833591	2286.651439	20.004186
61.136452	2290.968704	20.009203
61.082296	2295.896871	20.014221
61.059814	2297.462414	20.019239
61.142366	2287.160939	20.024256
61.451567	2302.911108	20.029274
62.187122	2299.069517	20.034291
62.131917	2296.661336	20.039309
62.103051	2275.702579	20.044327
62.165919	2280.880795	20.049344
62.177680	2273.916369	20.054362
62.219697	2271.796293	20.059379
61.996476	2280.731194	20.064397
62.212105	2267.714391	20.069415
61.973623	2273.312830	20.074432
61.648934	2278.192085	20.079450
62.024124	2279.393338	20.084467
61.805590	2277.401410	20.089485
62.131977	2276.041358	20.094503
61.442858	2284.474165	20.099520
61.449793	2279.721128	20.104538
61.825621	2300.675605	20.109555
61.704202	2307.103720	20.114573
62.400136	2308.146030	20.119591
62.041565	2308.574529	20.124608
61.960551	2331.245415	20.129626
62.348733	2328.064254	20.134643
62.608681	2333.330764	20.139661
62.299574	2339.145303	20.144679
62.512683	2333.454402	20.149696
62.645564	2349.862503	20.154714
63.324940	2354.958667	20.159731
63.171694	2357.327858	20.164749
63.230505	2352.395800	20.169767
63.057224	2353.879313	20.174784
63.065569	2358.466812	20.179802
63.442723	2360.841930	20.184819
63.675179	2352.616608	20.189837
63.694571	2354.174190	20.194855
63.771883	2354.682312	20.199872
63.703501	2360.124827	20.204890
63.913341	2341.218290	20.209907
63.280704	2326.541089	20.214925
63.488745	2336.500672	20.219943
63.680629	2344.162682	20.224960
63.839935	2350.180423	20.229978
63.924709	2353.727888	20.234995
64.018412	2348.209445	20.240013
64.160703	2361.199676	20.245031
64.438239	2353.529703	20.250048
64.107085	2358.953481	20.255066
64.133721	2349.853861	20.260083
64.317530	2350.625657	20.265101
64.300754	2354.065317	20.270119
64.487500	2343.053709	20.275136
64.436870	2358.259236	20.280154
64.662947	2359.063949	20.285171
63.977491	2343.760257	20.290189
64.207398	2350.873149	20.295207
64.307826	2348.554042	20.300224
64.612082	2378.502583	20.305242
64.731184	2366.378761	20.310259
64.518832	2380.197646	20.315277
64.746403	2386.071393	20.320295
64.616939	2383.008111	20.325312
64.778672	2381.524289	20.330330
64.915707	2380.483351	20.335347
64.862079	2393.854498	20.340365
65.091476	2407.482690	20.345383
65.462528	2410.820430	20.350400
65.291238	2422.036630	20.355418
65.509832	2418.560067	20.360435
65.145526	2406.309614	20.365453
65.371036	2412.119934	20.370471
65.515762	2402.614937	20.375488
65.168897	2416.537244	20.380506
65.536193	2415.685208	20.385523
66.048329	2430.323378	20.390541
66.242447	2428.548127	20.395559
65.677349	2409.711370	20.400576
65.574755	2415.664573	20.405594
65.869975	2422.328436	20.410611
65.966041	2432.675841	20.415629
65.935151	2432.953659	20.420647
66.672175	2430.104069	20.425664
66.388536	2436.530122	20.430682
66.563371	2428.587124	20.435699
66.793905	2433.481486	20.440717
66.140972	2437.106624	20.445735
66.039983	2427.876060	20.450752
66.058087	2436.167217	20.455770
66.164427	2435.730847	20.460787
66.162382	2444.266445	20.465805
66.175587	2458.386151	20.470823
66.349734	2461.048887	20.475840
66.324649	2466.239094	20.480858
66.668054	2485.330575	20.485875
66.740926	2486.830174	20.490893
66.845171	2493.075556	20.495911
67.147048	2484.874489	20.500928
67.106357	2480.236661	20.505946
67.461492	2479.645804	20.510963
67.204112	2477.205319	20.515981
67.198234	2498.562568	20.520999
67.829279	2493.394538	20.526016
67.992397	2507.031030	20.531034
67.607040	2495.107791	20.536051
67.741566	2494.366538	20.541069
67.530405	2504.782416	20.546087
68.152852	2506.266545	20.551104
67.881119	2503.256769	20.556122
67.784871	2505.650861	20.561139
68.238845	2500.354107	20.566157
68.045488	2505.789748	20.571175
68.204632	2504.089788	20.576192
68.283983	2503.743884	20.581210
68.169127	2501.494742	20.586227
68.269963	2500.473392	20.591245
68.126081	2503.949840	20.596263
68.249345	2497.637172	20.601280
68.414907	2503.110505	20.606298
68.503037	2517.833266	20.611315
69.087774	2529.917722	20.616333
68.503028	2533.822577	20.621351
68.873953	2529.714261	20.626368
68.804880	2532.373820	20.631386
68.795817	2534.010327	20.636403
68.937203	2525.424877	20.641421
68.762500	2535.750258	20.646439
69.028039	2529.373021	20.651456
68.930102	2537.192707	20.656474
68.983574	2528.238801	20.661491
69.425081	2540.880193	20.666509
68.872079	2537.810743	20.671527
69.504584	2553.393117	20.676544
69.691821	2565.237040	20.681562
69.790003	2566.007777	20.686579
69.917044	2560.351239	20.691597
69.846922	2570.976089	20.696615
69.875059	2557.052453	20.701632
69.803286	2568.266658	20.706650
69.776004	2566.265528	20.711667
69.614679	2559.188108	20.716685
69.188085	2569.571662	20.721703
69.524203	2564.964496	20.726720
69.789579	2578.601631	20.731738
69.682781	2591.877320	20.736755
69.559659	2588.125393	20.741773
69.784454	2605.865474	20.746791
70.090138	2607.206251	20.751808
70.549450	2609.132603	20.756826
70.758284	2619.499386	20.761843
71.096598	2610.613940	20.766861
70.631316	2622.865106	20.771879
70.704093	2612.077610	20.776896
70.758241	2620.590282	20.781914
70.820732	2612.636527	20.786931
71.025781	2607.377691	20.791949
71.103084	2607.903936	20.796967
71.103519	2598.655882	20.801984
71.318053	2602.617450	20.807002
70.947384	2610.190183	20.812019
71.413171	2612.511555	20.817037
71.341374	2641.932060	20.822055
71.668344	2631.428585	20.827072
71.561955	2633.562185	20.832090
71.540806	2638.525751	20.837107
71.587698	2633.486181	20.842125
71.636173	2630.510473	20.847143
71.972585	2622.277425	20.852160
72.246716	2628.075553	20.857178
72.237109	2627.346405	20.862195
72.246215	2626.000558	20.867213
71.986213	2621.145128	20.872231
72.136131	2624.504290	20.877248
72.353028	2629.670389	20.882266
72.327630	2636.608249	20.887283
72.552494	2630.022159	20.892301
72.143716	2626.790145	20.897319
72.532594	2634.384659	20.902336
72.357441	2631.358300	20.907354
72.725755	2638.871287	20.912371
72.932649	2641.978123	20.917389
72.821302	2652.899123	20.922407
72.884102	2657.229298	20.927424
72.923087	2639.621993	20.932442
73.292383	2644.053973	20.937459
72.983011	2638.126502	20.942477
73.052225	2649.636333	20.947495
73.232226	2638.976129	20.952512
73.193453	2640.357853	20.957530
73.215682	2649.413113	20.962547
73.335953	2637.759041	20.967565
73.295386	2649.827156	20.972583
73.517709	2649.006265	20.977600
73.371077	2647.715470	20.982618
73.347345	2648.622094	20.987635
73.673109	2655.572208	20.992653
73.642631	2681.364608	20.997671
73.854716	2670.871353	21.002688
73.881232	2674.707667	21.007706
73.657256	2680.299825	21.012723
73.661778	2681.754459	21.017741
73.720945	2673.417711	21.022759
74.024355	2683.634441	21.027776
74.808728	2693.897873	21.032794
74.687952	2686.903222	21.037811
75.195498	2682.717891	21.042829
75.065630	2674.196192	21.047847
74.596066	2660.400322	21.052864
74.829426	2654.973596	21.057882
74.814385	2655.145533	21.062899
74.828280	2649.730448	21.067917
74.793688	2655.614592	21.072935
74.902361	2672.056321	21.077952
74.979000	2670.402777	21.082970
74.535628	2683.234587	21.087987
75.033147	2680.531548	21.093005
74.964442	2674.979408	21.098023
75.012048	2678.741229	21.103040
75.087232	2683.756810	21.108058
75.386498	2703.761796	21.113075
75.123670	2704.137662	21.118093
75.368745	2712.523933	21.123111
75.395990	2716.849195	21.128128
75.563708	2713.007996	21.133146
75.579747	2736.225918	21.138163
75.979183	2738.038909	21.143181
75.763076	2742.223979	21.148199
75.873205	2734.781771	21.153216
75.926375	2730.112813	21.158234
76.074537	2747.614180	21.163251
76.421169	2731.881141	21.168269
76.192041	2737.623048	21.173287
76.473401	2755.112612	21.178304
76.854299	2759.511923	21.183322
76.665809	2764.571948	21.188339
76.746765	2761.799345	21.193357
76.881612	2761.220259	21.198375
77.022226	2756.685146	21.203392
76.641264	2754.009853	21.208410
76.696052	2767.932911	21.213427
77.051502	2761.156632	21.218445
77.038718	2761.095858	21.223463
76.658096	2761.095000	21.228480
76.906750	2755.452981	21.233498
77.150411	2762.159693	21.238515
77.440418	2766.550175	21.243533
77.438773	2770.973335	21.248551
77.651668	2786.994881	21.253568
77.854318	2786.977501	21.258586
77.615976	2784.997565	21.263603
77.847002	2779.607424	21.268621
78.127760	2789.087028	21.273639
77.979491	2795.370311	21.278656
78.186641	2784.072957	21.283674
77.876836	2791.220304	21.288691
78.008002	2796.538190	21.293709
78.401617	2792.196742	21.298727
78.330291	2795.394624	21.303744
78.827690	2785.877759	21.308762
78.538880	2797.875142	21.313779
78.271592	2789.061923	21.318797
78.348321	2788.550291	21.323815
78.256980	2793.700776	21.328832
78.480950	2784.655276	21.333850
77.815336	2793.716718	21.338867
78.252126	2810.034606	21.343885
78.302145	2815.879891	21.348903
78.496198	2834.947790	21.353920
79.078968	2834.443902	21.358938
78.699957	2847.616843	21.363955
78.678832	2844.253741	21.368973
79.144484	2845.537975	21.373991
79.465959	2861.872538	21.379008
79.885597	2864.653127	21.384026
79.826906	2871.023463	21.389043
79.835995	2872.253667	21.394061
79.838378	2878.863188	21.399079
79.985240	2872.834568	21.404096
80.202099	2864.364364	21.409114
79.912976	2871.733441	21.414131
79.806435	2862.293297	21.419149
79.948499	2870.230298	21.424167
79.803913	2875.714408	21.429184
80.145957	2868.537944	21.434202
79.929971	2862.967673	21.439219
80.639865	2877.087229	21.444237
80.572008	2890.331292	21.449255
80.732447	2894.657394	21.454272
80.671072	2891.705195	21.459290
80.692809	2893.219113	21.464307
80.798959	2891.172226	21.469325
80.845956	2882.469669	21.474343
81.299380	2892.407226	21.479360
81.085852	2885.978884	21.484378
81.192940	2885.699096	21.489395
81.240883	2884.170945	21.494413
81.356174	2884.533966	21.499431
81.408293	2888.475412	21.504448
81.300513	2878.998456	21.509466
81.054254	2895.383138	21.514483
80.923185	2895.687591	21.519501
81.435187	2901.038662	21.524519
81.538857	2914.545518	21.529536
81.896277	2911.176567	21.534554
81.666514	2921.694353	21.539571
81.810947	2913.930372	21.544589
81.848077	2918.583191	21.549607
81.617538	2918.162825	21.554624
81.968102	2928.051098	21.559642
82.057255	2941.237570	21.564659
82.170196	2948.986654	21.569677
82.050773	2945.353714	21.574695
82.123136	2957.517686	21.579712
82.292858	2952.883808	21.584730
82.516202	2979.545165	21.589747
83.229330	2980.173478	21.594765
83.244919	2982.075935	21.599783
82.856593	2979.697984	21.604800
82.948065	2971.836735	21.609818
83.058280	2971.921047	21.614835
83.359777	2977.091658	21.619853
83.505616	2968.474489	21.624871
83.337242	2972.693964	21.629888
83.078816	2966.700140	21.634906
83.031683	2962.890992	21.639923
83.342409	2982.133593	21.644941
83.881500	2991.723390	21.649959
83.727603	3000.787785	21.654976
83.857592	2993.549178	21.659994
83.817118	3003.880992	21.665011
83.952837	3011.871919	21.670029
84.242409	3000.998946	21.675047
84.169612	3006.103793	21.680064
84.473778	2995.755983	21.685082
84.189588	2997.232581	21.690099
84.084260	2991.370798	21.695117
84.273760	2996.305450	21.700135
84.199985	3015.327344	21.705152
84.470181	3013.726424	21.710170
84.700332	3020.196147	21.715187
85.004463	3022.336597	21.720205
85.114291	3026.836012	21.725223
85.044001	3016.027877	21.730240
85.249930	3019.664979	21.735258
85.451361	3021.826974	21.740275
85.423172	3014.181533	21.745293
85.727186	3017.138697	21.750311
85.654945	3016.617946	21.755328
85.819628	3011.334394	21.760346
85.465623	3013.376614	21.765363
85.316168	3020.491848	21.770381
85.716528	3006.274819	21.775399
85.503795	3010.749201	21.780416
85.760360	3009.400273	21.785434
85.776299	3010.135517	21.790451
85.761294	3012.163719	21.795469
86.157020	3017.722992	21.800487
85.934617	3030.790481	21.805504
86.128155	3029.928041	21.810522
86.114222	3036.390002	21.815539
85.681724	3037.484076	21.820557
86.315860	3035.389964	21.825575
86.388712	3049.047130	21.830592
86.429700	3054.234079	21.835610
86.715635	3062.906504	21.840627
86.596205	3070.118207	21.845645
86.988316	3062.346342	21.850663
86.879396	3067.025820	21.855680
87.121806	3065.446198	21.860698
87.110595	3063.002792	21.865715
86.997035	3083.319245	21.870733
87.087393	3081.931077	21.875751
87.334998	3091.611864	21.880768
87.444762	3090.471599	21.885786
87.477422	3095.842704	21.890803
87.310369	3095.184631	21.895821
87.666342	3092.113588	21.900839
87.613983	3108.335300	21.905856
87.899249	3117.706436	21.910874
88.090136	3128.197918	21.915891
87.543289	3125.591166	21.920909
88.332863	3119.144324	21.925927
87.962194	3124.747612	21.930944
88.119958	3139.515723	21.935962
88.557801	3149.178106	21.940979
88.396609	3149.522380	21.945997
88.627223	3144.777986	21.951015
88.728775	3151.298951	21.956032
89.125944	3150.537054	21.961050
89.352776	3141.640496	21.966067
89.082614	3156.921449	21.971085
89.264408	3150.266135	21.976103
89.306813	3150.117141	21.981120
89.371310	3146.467586	21.986138
89.068734	3140.079609	21.991155
89.013275	3146.331368	21.996173
89.327503	3140.200708	22.001191
89.650761	3166.935823	22.006208
89.454750	3167.109653	22.011226
89.809801	3167.674931	22.016243
89.543170	3175.372644	22.021261
90.052896	3168.269680	22.026279
90.040134	3171.682054	22.031296
89.948363	3170.462139	22.036314
89.953914	3169.720129	22.041331
89.906167	3182.460100	22.046349
90.307402	3187.338822	22.051367
90.365539	3197.787743	22.056384
90.461168	3205.951818	22.061402
90.564256	3199.945541	22.066419
90.404002	3203.647830	22.071437
90.369807	3196.810584	22.076455
90.232256	3212.346077	22.081472
90.542207	3228.958647	22.086490
90.815375	3227.973073	22.091507
90.808149	3236.706094	22.096525
90.752569	3237.083454	22.101543
91.189950	3256.384222	22.106560
91.386084	3263.396211	22.111578
91.190082	3257.812922	22.116595
91.337432	3266.045342	22.121613
91.666704	3257.850994	22.126631
91.657491	3257.479304	22.131648
91.936860	3253.477071	22.136666
92.194026	3251.871274	22.141683
91.899647	3270.041346	22.146701
91.971241	3278.275735	22.151719
92.269531	3280.997660	22.156736
92.483235	3286.259034	22.161754
92.616672	3284.327128	22.166771
92.145393	3289.633483	22.171789
92.592848	3282.836483	22.176807
92.896225	3281.677187	22.181824
92.649952	3278.609340	22.186842
92.550425	3272.876407	22.191859
92.320375	3294.329875	22.196877
92.880006	3299.306700	22.201895
92.983912	3308.641313	22.206912
92.870092	3312.449076	22.211930
93.137406	3305.991678	22.216947
93.333878	3315.682158	22.221965
93.380609	3336.719648	22.226983
93.525122	3338.094424	22.232000
93.421338	3341.999708	22.237018
93.925113	3333.409969	22.242035
93.866623	3341.383168	22.247053
93.835167	3337.409788	22.252071
93.782453	3338.543516	22.257088
93.678877	3343.408026	22.262106
94.306508	3349.621510	22.267123
94.580944	3360.753297	22.272141
94.421672	3366.787457	22.277159
94.560159	3371.873525	22.282176
94.145045	3366.362416	22.287194
94.519236	3364.405763	22.292211
94.318657	3371.492904	22.297229
94.531055	3376.185904	22.302247
94.854987	3396.496273	22.307264
94.676701	3401.688640	22.312282
95.038806	3392.219810	22.317299
95.460847	3398.752088	22.322317
95.423159	3391.466439	22.327335
95.525577	3391.581230	22.332352
95.487277	3395.106716	22.337370
95.587082	3383.239019	22.342387
95.518273	3393.772840	22.347405
95.453402	3388.774242	22.352423
95.745609	3399.765972	22.357440
95.725166	3416.409394	22.362458
96.162952	3420.451032	22.367475
96.104680	3420.439009	22.372493
96.276370	3420.815213	22.377511
96.171065	3418.732054	22.382528
96.323977	3413.442511	22.387546
96.779927	3416.428834	22.392563
96.389098	3417.158228	22.397581
96.363109	3422.754507	22.402599
96.608453	3433.970091	22.407616
96.640624	3450.924285	22.412634
96.647140	3444.895881	22.417651
96.871908	3455.720432	22.422669
96.922235	3453.775190	22.427687
97.073236	3454.252601	22.432704
97.046925	3469.583408	22.437722
97.467805	3464.172299	22.442739
97.297405	3473.035811	22.447757
97.426713	3472.902632	22.452775
97.806371	3461.716982	22.457792
97.582290	3472.202656	22.462810
97.763857	3490.137017	22.467827
97.446341	3501.581461	22.472845
97.753267	3505.579400	22.477863
97.977172	3501.453513	22.482880
98.133981	3505.248003	22.487898
98.199558	3517.821538	22.492915
98.135918	3528.174994	22.497933
98.932250	3518.580451	22.502951
99.734159	3509.149562	22.507968
99.423365	3511.996429	22.512986
99.651070	3506.260864	22.518003
99.870193	3490.891528	22.523021
99.481150	3477.742696	22.528039
99.545355	3475.496579	22.533056
99.125248	3476.575955	22.538074
99.677985	3470.987872	22.543091
99.260903	3472.903137	22.548109
99.091077	3478.661134	22.553127
99.829286	3481.889695	22.558144
99.803051	3500.293650	22.563162
99.822434	3502.508976	22.568179
100.139799	3499.307436	22.573197
100.069522	3503.773285	22.578215
100.245661	3505.065471	22.583232
100.216881	3501.818527	22.588250
100.254253	3488.894285	22.593267
100.013189	3496.728746	22.598285
99.737331	3497.658167	22.603303
100.137527	3510.842984	22.608320
100.246450	3522.787691	22.613338
100.356508	3524.083332	22.618355
100.538397	3526.549605	22.623373
100.724573	3546.115107	22.628391
100.866656	3545.123636	22.633408
100.852515	3557.318654	22.638426
101.340314	3555.432287	22.643443
101.077495	3546.167377	22.648461
101.128044	3570.352490	22.653479
101.475207	3566.964684	22.658496
101.603079	3582.722815	22.663514
101.494792	3577.500050	22.668531
101.821740	3588.798627	22.673549
101.781740	3590.754006	22.678567
102.175900	3586.945444	22.683584
102.417244	3609.016322	22.688602
102.657636	3598.731033	22.693619
102.607822	3604.396043	22.698637
102.654881	3606.129363	22.703655
102.760651	3601.170750	22.708672
102.877433	3610.776626	22.713690
103.070077	3592.804825	22.718707
103.243042	3596.999023	22.723725
103.082935	3602.055237	22.728743
103.390754	3604.079362	22.733760
103.326411	3609.117584	22.738778
103.586896	3600.277219	22.743795
103.150262	3602.784963	22.748813
102.950832	3611.622027	22.753831
103.640341	3603.848529	22.758848
103.399840	3608.909864	22.763866
103.584548	3617.314059	22.768883
103.647894	3616.051764	22.773901
103.572174	3632.270932	22.778919
103.874786	3634.532230	22.783936
103.644892	3636.594990	22.788954
104.084198	3653.989172	22.793971
104.239874	3663.973543	22.798989
104.055725	3667.193307	22.804007
105.009291	3659.189429	22.809024
104.708851	3658.769210	22.814042
104.693538	3658.711229	22.819059
105.041880	3659.924288	22.824077
104.996970	3673.781756	22.829095
104.704748	3684.187104	22.834112
105.052012	3680.337731	22.839130
105.208817	3681.915991	22.844147
105.799572	3675.832227	22.849165
105.114533	3675.897729	22.854183
105.411525	3676.156372	22.859200
105.207382	3688.304520	22.864218
105.432638	3706.379705	22.869235
105.807034	3701.601044	22.874253
105.324587	3711.974442	22.879271
105.604356	3708.993530	22.884288
105.999004	3731.562832	22.889306
106.218721	3746.235044	22.894323
106.831728	3738.646292	22.899341
106.444796	3744.595188	22.904359
107.056875	3737.457098	22.909376
106.762803	3743.645252	22.914394
106.636795	3746.135993	22.919411
106.549369	3739.592745	22.924429
106.612299	3750.123908	22.929447
106.829102	3756.457609	22.934464
107.026584	3762.411067	22.939482
106.996764	3761.056045	22.944499
107.290950	3758.875998	22.949517
107.293881	3789.208893	22.954535
107.663175	3790.890138	22.959552
107.592337	3785.997975	22.964570
107.668217	3795.722027	22.969587
108.074507	3783.439980	22.974605
107.847493	3795.479505	22.979623
108.417536	3807.398929	22.984640
108.438156	3817.946055	22.989658
108.372311	3821.431465	22.994675
108.753289	3820.718784	22.999693
108.422280	3827.703261	23.004711
108.820361	3820.528577	23.009728
109.049755	3815.124188	23.014746
108.714193	3825.497680	23.019763
108.732692	3822.358341	23.024781
109.123821	3843.575318	23.029799
109.514809	3844.598357	23.034816
109.301044	3856.649834	23.039834
109.249040	3858.932581	23.044851
109.658806	3853.507495	23.049869
109.466873	3856.075714	23.054887
109.761074	3853.879899	23.059904
109.640017	3860.025047	23.064922
109.834696	3870.232053	23.069939
110.130707	3876.135583	23.074957
109.876089	3878.019103	23.079975
109.969142	3880.219490	23.084992
110.080742	3889.393245	23.090010
110.366794	3902.096260	23.095027
110.470250	3901.289387	23.100045
110.236305	3904.056990	23.105063
110.272517	3913.299604	23.110080
110.811355	3933.929820	23.115098
110.820605	3933.962139	23.120115
111.114970	3934.390572	23.125133
111.030840	3939.112526	23.130151
111.163223	3955.062430	23.135168
111.390014	3964.448036	23.140186
111.032360	3973.851148	23.145203
111.578755	3960.712447	23.150221
111.780980	3969.374524	23.155239
112.025184	3964.495239	23.160256
112.061193	3964.160674	23.165274
112.180079	3984.938564	23.170291
112.494964	3985.848644	23.175309
112.540691	3985.458855	23.180327
112.718512	3980.077429	23.185344
113.574691	3975.572874	23.190362
112.939184	3975.477088	23.195379
113.210392	3958.064778	23.200397
113.084222	3959.837287	23.205415
113.170268	3970.743471	23.210432
113.309670	3971.916766	23.215450
113.161588	3975.638412	23.220467
113.365034	3978.946159	23.225485
113.213139	3981.430349	23.230503
113.061579	3977.986190	23.235520
113.294572	3982.761690	23.240538
113.063156	4007.200590	23.245555
113.613042	4000.581051	23.250573
113.542696	4009.288304	23.255591
113.205173	4032.186763	23.260608
113.959465	4036.333398	23.265626
113.907683	4038.279037	23.270643
114.161211	4054.671385	23.275661
114.243254	4076.107851	23.280679
114.380501	4081.822873	23.285696
114.399718	4072.812529	23.290714
114.641413	4097.888756	23.295731
115.021272	4089.646714	23.300749
115.185543	4097.784520	23.305767
115.305056	4096.888247	23.310784
115.351571	4094.348935	23.315802
114.975499	4102.627423	23.320819
115.474378	4121.643049	23.325837
115.690289	4123.605814	23.330855
115.993961	4128.760684	23.335872
116.075799	4127.868506	23.340890
116.358493	4129.732398	23.345907
116.723541	4125.440382	23.350925
115.892187	4132.202029	23.355943
116.245527	4133.213429	23.360960
116.565707	4136.635878	23.365978
116.703707	4160.026378	23.370995
116.636873	4150.336857	23.376013
116.780448	4156.352477	23.381031
116.920533	4151.073551	23.386048
117.189616	4147.413107	23.391066
116.899442	4154.365523	23.396083
117.265168	4160.209164	23.401101
117.436044	4177.475883	23.406119
117.406867	4183.435280	23.411136
117.537738	4182.233825	23.416154
117.378453	4184.747666	23.421171
117.838765	4177.068319	23.426189
117.690329	4181.958105	23.431207
117.563500	4195.566224	23.436224
117.935001	4196.808436	23.441242
118.072656	4207.649227	23.446259
118.123175	4208.293537	23.451277
118.144467	4224.521097	23.456295
118.507439	4239.325944	23.461312
118.645012	4230.201494	23.466330
118.460349	4238.640991	23.471347
118.995869	4235.638191	23.476365
118.896179	4258.509591	23.481383
118.977316	4260.595507	23.486400
118.982052	4269.061621	23.491418
119.202700	4275.653211	23.496435
119.518321	4268.772855	23.501453
119.726935	4289.453063	23.506471
119.593038	4295.271356	23.511488
119.973804	4288.223087	23.516506
119.941427	4299.986252	23.521523
120.158410	4286.622578	23.526541
119.995562	4287.197930	23.531559
120.143782	4309.459030	23.536576
120.694920	4310.863421	23.541594
120.492437	4311.859069	23.546611
120.935951	4306.364248	23.551629
120.703046	4311.997103	23.556647
120.994540	4327.007254	23.561664
121.126272	4335.984851	23.566682
121.193297	4340.638479	23.571699
121.196466	4338.406643	23.576717
121.456991	4339.113407	23.581735
121.648787	4341.272514	23.586752
122.202888	4339.470782	23.591770
121.770178	4345.845187	23.596787
122.092544	4357.132501	23.601805
122.281339	4361.608522	23.606823
122.009661	4369.221825	23.611840
122.297404	4362.495069	23.616858
122.539789	4368.685223	23.621875
122.307599	4365.258740	23.626893
122.658545	4366.090988	23.631911
122.613811	4389.561202	23.636928
123.126337	4385.065831	23.641946
122.891984	4395.438883	23.646963
123.145454	4381.008732	23.651981
123.376948	4379.785285	23.656999
123.558825	4380.075493	23.662016
123.561844	4371.692341	23.667034
123.794607	4383.854332	23.672051
123.736819	4398.720438	23.677069
124.231113	4397.936325	23.682087
124.023880	4402.614148	23.687104
124.401475	4398.472708	23.692122
124.227547	4410.726496	23.697139
124.004432	4411.404336	23.702157
124.338341	4406.485122	23.707175
124.453041	4407.788706	23.712192
124.428172	4410.726909	23.717210
124.549865	4425.670963	23.722227
124.536021	4434.864967	23.727245
124.629146	4432.184501	23.732263
124.666216	4446.192417	23.737280
125.113434	4453.279250	23.742298
125.263317	4461.867870	23.747315
125.261409	4462.543232	23.752333
125.674342	4462.263756	23.757351
126.111419	4488.228632	23.762368
126.105637	4490.947768	23.767386
125.922549	4498.263187	23.772403
126.229253	4498.533572	23.777421
126.309158	4490.372677	23.782439
126.004949	4496.881062	23.787456
126.247856	4492.402743	23.792474
126.481399	4510.404179	23.797491
126.526945	4507.105692	23.802509
127.229982	4508.959003	23.807527
127.057895	4509.809254	23.812544
127.336373	4497.041335	23.817562
127.077046	4504.744739	23.822579
127.308796	4522.277069	23.827597
127.822134	4524.863895	23.832615
127.472250	4538.385314	23.837632
127.602399	4534.143700	23.842650
127.722682	4536.558472	23.847667
127.481303	4550.551994	23.852685
128.329579	4556.542258	23.857703
128.166559	4563.425007	23.862720
128.432525	4563.558241	23.867738
128.467034	4566.458727	23.872755
128.629633	4583.848605	23.877773
129.118749	4591.570239	23.882791
128.729697	4605.117333	23.887808
129.207257	4593.993656	23.892826
129.206612	4603.598215	23.897843
129.148784	4600.664778	23.902861
129.455521	4597.704284	23.907879
129.477471	4620.910578	23.912896
129.598657	4627.381531	23.917914
129.588766	4623.568746	23.922931
129.600501	4626.854363	23.927949
129.832314	4635.685801	23.932967
129.768222	4645.111442	23.937984
130.129123	4656.397091	23.943002
130.327001	4646.487028	23.948019
130.389172	4666.792717	23.953037
130.764337	4674.964765	23.958055
130.849393	4686.748254	23.963072
130.868666	4683.395950	23.968090
130.800122	4683.621976	23.973107
130.578442	4691.361548	23.978125
131.288963	4696.890298	23.983143
130.988698	4712.715867	23.988160
131.537515	4713.546507	23.993178
131.846808	4715.012090	23.998195
131.472583	4721.073376	24.003213
131.846522	4724.091343	24.008231
132.058052	4735.594840	24.013248
132.722947	4732.129479	24.018266
132.688841	4728.013641	24.023283
133.105030	4714.856474	24.028301
132.908701	4710.650304	24.033319
133.165270	4713.233136	24.038336
133.066560	4717.066999	24.043354
133.268932	4715.341280	24.048371
133.091461	4722.425848	24.053389
133.082524	4714.617179	24.058407
133.266369	4717.044712	24.063424
133.539335	4730.501260	24.068442
133.328527	4739.303881	24.073459
133.488429	4750.899731	24.078477
133.572912	4748.245898	24.083495
133.701990	4768.914378	24.088512
133.987748	4773.197461	24.093530
134.148291	4779.040279	24.098547
134.088661	4779.152934	24.103565
134.438337	4792.789357	24.108583
134.491191	4810.951286	24.113600
134.788585	4808.448402	24.118618
134.907489	4812.323746	24.123635
134.932276	4813.373404	24.128653
135.430869	4832.915298	24.133671
135.244210	4832.551150	24.138688
135.510606	4823.119147	24.143706
135.651148	4828.334508	24.148723
135.905032	4824.148006	24.153741
136.088780	4837.571107	24.158759
136.060302	4852.672058	24.163776
136.233134	4846.595703	24.168794
136.455540	4851.515060	24.173811
136.075023	4854.975090	24.178829
136.555843	4863.500894	24.183847
136.413288	4859.136601	24.188864
136.785477	4882.361998	24.193882
137.143605	4879.056318	24.198899
137.213948	4866.894042	24.203917
137.414337	4869.455812	24.208935
137.366624	4878.619648	24.213952
137.640930	4880.489008	24.218970
138.280350	4893.012521	24.223987
138.142657	4894.993472	24.229005
138.453710	4891.579287	24.234023
138.257683	4893.603319	24.239040
137.975265	4901.185636	24.244058
138.652320	4900.381985	24.249075
138.230522	4901.321536	24.254093
138.545028	4890.442210	24.259111
138.805908	4896.074109	24.264128
138.730166	4901.461261	24.269146
138.758062	4905.455413	24.274163
138.612188	4920.788432	24.279181
138.837853	4918.542787	24.284199
138.834420	4925.355801	24.289216
138.976114	4953.705890	24.294234
139.542925	4957.291029	24.299251
139.524007	4969.388711	24.304269
139.615319	4968.830402	24.309287
139.840963	4980.332446	24.314304
139.564214	4993.673943	24.319322
140.101489	4999.278187	24.324339
139.920231	5019.106208	24.329357
140.324897	5015.781494	24.334375
140.432309	5021.127836	24.339392
140.368446	5042.640246	24.344410
140.910312	5047.990095	24.349427
141.084102	5055.777832	24.354445
141.153929	5057.156901	24.359463
141.408420	5077.259224	24.364480
141.509886	5083.004373	24.369498
142.468245	5065.830646	24.374515
142.410255	5064.091238	24.379533
142.479700	5057.756848	24.384551
142.610562	5066.167109	24.389568
142.452573	5062.535564	24.394586
142.866949	5052.480224	24.399603
142.739655	5063.256753	24.404621
142.962802	5064.198381	24.409639
143.024262	5061.671318	24.414656
143.144308	5064.461925	24.419674
143.285132	5076.435421	24.424691
143.346358	5089.092870	24.429709
143.473818	5086.391443	24.434727
143.463284	5086.263323	24.439744
143.777136	5094.887978	24.444762
143.660633	5088.517715	24.449779
143.805641	5122.537105	24.454797
143.882291	5123.466044	24.459815
144.216166	5116.585345	24.464832
144.633324	5121.298115	24.469850
144.891962	5129.065828	24.474867
144.705794	5147.396721	24.479885
145.083736	5146.147324	24.484903
144.718113	5142.958577	24.489920
144.345692	5143.213075	24.494938
144.912014	5154.105479	24.499955
144.562599	5170.531462	24.504973
144.664186	5190.289940	24.509991
144.897104	5197.319330	24.515008
145.291002	5204.586568	24.520026
145.261401	5221.068837	24.525043
145.840929	5243.532206	24.530061
145.789688	5237.944661	24.535079
146.016260	5255.390474	24.540096
146.329964	5259.940645	24.545114
147.161827	5255.702206	24.550131
146.870059	5250.957736	24.555149
147.032938	5248.814967	24.560167
147.434880	5257.137899	24.565184
147.231771	5257.596521	24.570202
147.489156	5272.692187	24.575219
147.776806	5285.945048	24.580237
147.710907	5277.847341	24.585255
147.913951	5276.565692	24.590272
148.168526	5280.609296	24.595290
148.308993	5278.937452	24.600307
148.179649	5276.230395	24.605325
148.561860	5284.949771	24.610343
148.525862	5306.020605	24.615360
148.503142	5314.947258	24.620378
148.697369	5312.832976	24.625395
148.576711	5317.694717	24.630413
149.418975	5325.462509	24.635431
149.710458	5330.202400	24.640448
149.806191	5326.302024	24.645466
149.728420	5327.898612	24.650483
149.887069	5331.213538	24.655501
149.918769	5329.765917	24.660519
150.142841	5322.621180	24.665536
150.093094	5330.875079	24.670554
150.578016	5342.177767	24.675571
150.419401	5351.602703	24.680589
150.345754	5360.984722	24.685607
150.524569	5351.925024	24.690624
150.595807	5377.643737	24.695642
150.848227	5387.191996	24.700659
150.746740	5396.175520	24.705677
150.836511	5401.151658	24.710695
151.039039	5410.863657	24.715712
151.194772	5424.657539	24.720730
151.691792	5437.250008	24.725747
151.675026	5449.273645	24.730765
151.971930	5454.417510	24.735783
152.386184	5464.038895	24.740800
152.283452	5477.139867	24.745818
152.775681	5479.294889	24.750835
152.784810	5478.078763	24.755853
152.562855	5485.394208	24.760871
152.667908	5489.543054	24.765888
152.388433	5514.159498	24.770906
152.919602	5518.553525	24.775923
153.204528	5524.944788	24.780941
153.495641	5530.094397	24.785959
153.991573	5529.834552	24.790976
154.039059	5531.581401	24.795994
154.160401	5528.593445	24.801011
154.189114	5529.440043	24.806029
154.267628	5541.745947	24.811047
154.621274	5544.491078	24.816064
154.803805	5551.018059	24.821082
154.896715	5551.878859	24.826099
155.025278	5545.287595	24.831117
155.413754	5548.845157	24.836135
155.347216	5541.391748	24.841152
155.385909	5549.923616	24.846170
155.739213	5572.486887	24.851187
155.750740	5571.943023	24.856205
155.985909	5571.918499	24.861223
156.181444	5575.012116	24.866240
155.947757	5573.144448	24.871258
156.039973	5577.449904	24.876275
156.162563	5594.899739	24.881293
156.436870	5603.195899	24.886311
156.660789	5606.502844	24.891328
156.743180	5621.547711	24.896346
157.050468	5626.760744	24.901363
157.097657	5639.803853	24.906381
157.377495	5639.721260	24.911399
157.475189	5651.356003	24.916416
157.721465	5666.561862	24.921434
157.698366	5666.332704	24.926451
157.853062	5665.759568	24.931469
157.828211	5684.451753	24.936487
158.392099	5678.052045	24.941504
158.249483	5691.134824	24.946522
158.064260	5691.267439	24.951539
158.924841	5710.746001	24.956557
158.963057	5722.235030	24.961575
159.154017	5722.856902	24.966592
159.061009	5733.976953	24.971610
159.112329	5744.429513	24.976627
159.816039	5743.399918	24.981645
159.540671	5755.396439	24.986663
159.872441	5766.583114	24.991680
159.907731	5783.781882	24.996698
160.115930	5788.268374	25.001715
160.153940	5782.046998	25.006733
160.482034	5794.977487	25.011751
160.874929	5802.705188	25.016768
160.547176	5809.067691	25.021786
161.017156	5812.434898	25.026803
161.096540	5825.501785	25.031821
160.879964	5835.813647	25.036839
161.335953	5841.402985	25.041856
161.653438	5848.722218	25.046874
161.540030	5864.434975	25.051891
161.658594	5879.221033	25.056909
161.479397	5875.957640	25.061927
162.164727	5885.246878	25.066944
162.445547	5907.452832	25.071962
162.519958	5901.103077	25.076979
162.852297	5899.474683	25.081997
162.660738	5907.605104	25.087015
163.056359	5920.458741	25.092032
162.988530	5932.500948	25.097050
162.912788	5932.129573	25.102067
163.217188	5940.300233	25.107085
163.120507	5958.099197	25.112103
163.658198	5964.147193	25.117120
163.491395	5975.594356	25.122138
163.808914	5993.075014	25.127155
163.913637	5991.833797	25.132173
163.859347	6012.227338	25.137191
164.219999	6019.538462	25.142208
164.704254	6028.087941	25.147226
164.684789	6039.894292	25.152243
164.894180	6045.932433	25.157261
164.933254	6048.787508	25.162279
165.560699	6057.766175	25.167296
166.024827	6073.691276	25.172314
166.041798	6067.930265	25.177331
166.242536	6066.029813	25.182349
166.064267	6081.608966	25.187367
166.540472	6071.740104	25.192384
166.268061	6076.688743	25.197402
166.192821	6093.737436	25.202419
166.746957	6104.069376	25.207437
166.570223	6105.519951	25.212455
166.992398	6113.880828	25.217472
167.223970	6125.072330	25.222490
167.182094	6127.772727	25.227507
167.806001	6140.370788	25.232525
167.836283	6150.009577	25.237543
168.066612	6155.588874	25.242560
168.325227	6158.823033	25.247578
168.318303	6157.847495	25.252595
168.663024	6165.547398	25.257613
168.497375	6184.169780	25.262631
168.707374	6172.548144	25.267648
168.899237	6176.603518	25.272666
168.852529	6195.875079	25.277683
169.426015	6198.114739	25.282701
169.175751	6212.563388	25.287719
169.216942	6209.181010	25.292736
169.489464	6235.047776	25.297754
169.470091	6248.947225	25.302771
169.824133	6254.330476	25.307789
170.137433	6273.278894	25.312807
170.293236	6271.365640	25.317824
170.413805	6277.382073	25.322842
170.606291	6292.138513	25.327859
171.484149	6285.382259	25.332877
171.064560	6300.232605	25.337895
171.474905	6291.607679	25.342912
171.459831	6285.435381	25.347930
171.773359	6296.546786	25.352947
172.409682	6313.965269	25.357965
171.916389	6317.515835	25.362983
172.130970	6312.674001	25.368000
172.357538	6319.018088	25.373018
172.120604	6316.293061	25.378035
172.847968	6322.889230	25.383053
172.698908	6346.196677	25.388071
172.823024	6358.644274	25.393088
172.992549	6355.402136	25.398106
173.014479	6354.569732	25.403123
173.084754	6366.773706	25.408141
172.965649	6386.322583	25.413159
173.270818	6400.533607	25.418176
173.417681	6420.622998	25.423194
173.514354	6422.656910	25.428211
174.215992	6436.980390	25.433229
174.231070	6446.050864	25.438247
174.495999	6451.855138	25.443264
174.881292	6467.163968	25.448282
174.585364	6480.290216	25.453299
175.144000	6477.945527	25.458317
175.492692	6481.087113	25.463335
176.169916	6497.004467	25.468352
176.388173	6500.478783	25.473370
175.985577	6506.789009	25.478387
176.260384	6492.846411	25.483405
175.841205	6503.548700	25.488423
175.925479	6512.567963	25.493440
176.393315	6528.181732	25.498458
176.444176	6536.627756	25.503475
176.884117	6545.703439	25.508493
177.199888	6563.800243	25.513511
177.040178	6560.173374	25.518528
177.250999	6567.419060	25.523546
177.241555	6588.602834	25.528563
177.545764	6599.656181	25.533581
177.699741	6608.654097	25.538599
178.349695	6616.938383	25.543616
178.307252	6625.756505	25.548634
178.278764	6627.626782	25.553651
178.660891	6636.104297	25.558669
178.449653	6654.084372	25.563687
178.683321	6654.947886	25.568704
179.120799	6672.868766	25.573722
179.437526	6687.449089	25.578739
179.459869	6686.949022	25.583757
179.369228	6700.049711	25.588775
179.776375	6711.134329	25.593792
180.214131	6710.933286	25.598810
180.128531	6718.150295	25.603827
180.784795	6735.231033	25.608845
180.439148	6751.259394	25.613863
180.738121	6746.966986	25.618880
180.944216	6743.994210	25.623898
181.094438	6755.656203	25.628915
181.561995	6766.931378	25.633933
181.495642	6771.462852	25.638951
181.595770	6775.605002	25.643968
181.790750	6783.095339	25.648986
181.817841	6789.598273	25.654003
182.046541	6789.860812	25.659021
182.236591	6802.906377	25.664039
182.173378	6813.047632	25.669056
182.866492	6814.343641	25.674074
182.497559	6830.397342	25.679092
183.303585	6819.004704	25.684109
183.455453	6827.538337	25.689127
183.230960	6846.612714	25.694144
183.627636	6850.128993	25.699162
183.723755	6848.065991	25.704180
184.231054	6871.233327	25.709197
184.182937	6875.887743	25.714215
184.334524	6886.761852	25.719232
184.496608	6879.818472	25.724250
184.515970	6891.332844	25.729268
184.612782	6902.416440	25.734285
184.930875	6911.115409	25.739303
185.174538	6927.632947	25.744320
185.192538	6936.904863	25.749338
185.283704	6947.930378	25.754356
185.516402	6956.657401	25.759373
185.258374	6963.692961	25.764391
186.017440	6984.074353	25.769408
186.762381	6983.910453	25.774426
186.652256	6997.337704	25.779444
186.796088	6995.561123	25.784461
187.196269	7002.872229	25.789479
187.222297	7023.746425	25.794496
187.380444	7028.036246	25.799514
187.247332	7024.609527	25.804532
187.991415	7030.540629	25.809549
188.091280	7045.136399	25.814567
187.987012	7050.485839	25.819584
188.331390	7043.774249	25.824602
188.441401	7058.309997	25.829620
188.686373	7065.516184	25.834637
188.670971	7075.789630	25.839655
188.849929	7079.333830	25.844672
189.399500	7095.424130	25.849690
189.252751	7109.307562	25.854708
189.661024	7108.993407	25.859725
189.735261	7105.475195	25.864743
189.835625	7125.538783	25.869760
190.338517	7129.412678	25.874778
190.112671	7134.253613	25.879796
190.489801	7137.900925	25.884813
190.816078	7162.930471	25.889831
190.608396	7171.194275	25.894848
191.152942	7168.905474	25.899866
190.596226	7179.618396	25.904884
191.075782	7187.747857	25.909901
191.459273	7197.552818	25.914919
191.116057	7215.927183	25.919936
191.467261	7222.970281	25.924954
191.837326	7241.792743	25.929972
191.970245	7249.379806	25.934989
192.339457	7254.024237	25.940007
193.297611	7242.864400	25.945024
194.024933	7234.193299	25.950042
193.822993	7227.689511	25.955060
194.280280	7226.664267	25.960077
194.910568	7218.903921	25.965095
194.394814	7217.145065	25.970112
194.845847	7215.548978	25.975130
194.646591	7214.707967	25.980148
194.442191	7208.580372	25.985165
194.970371	7206.860773	25.990183
194.674426	7220.120760	25.995200
194.732311	7214.424010	26.000218
195.063707	7228.680120	26.005236
195.234232	7239.110075	26.010253
195.248304	7237.426611	26.015271
195.244516	7249.723520	26.020288
195.883685	7257.065463	26.025306
195.645814	7276.924896	26.030324
195.525240	7284.162334	26.035341
196.016311	7311.236478	26.040359
195.858620	7320.793971	26.045376
196.338783	7331.217384	26.050394
196.291083	7349.590086	26.055412
196.618716	7367.318668	26.060429
197.312356	7378.118309	26.065447
197.379047	7395.928680	26.070464
197.799873	7400.234231	26.075482
197.786667	7411.008539	26.080500
197.419690	7429.951266	26.085517
197.661045	7441.061664	26.090535
198.043096	7459.771253	26.095552
198.177348	7467.261294	26.100570
198.482307	7483.298598	26.105588
198.659285	7503.578768	26.110605
199.309990	7515.955117	26.115623
199.297314	7536.293837	26.120640
199.471837	7541.631887	26.125658
199.925676	7557.819419	26.130676
200.261396	7553.256592	26.135693
200.686131	7548.298798	26.140711
200.533492	7560.404823	26.145728
201.065280	7567.604610	26.150746
200.987563	7585.355653	26.155764
201.316350	7581.250133	26.160781
201.495885	7571.818013	26.165799
201.430369	7597.403038	26.170816
201.704367	7605.165394	26.175834
201.928092	7612.050116	26.180852
201.966047	7610.073403	26.185869
202.392321	7621.933708	26.190887
202.256768	7638.778532	26.195904
202.653422	7641.121195	26.200922
202.829877	7644.174374	26.205940
202.732318	7654.500088	26.210957
203.014021	7671.010299	26.215975
202.976629	7679.026955	26.220992
203.623914	7694.696977	26.226010
203.484235	7717.950452	26.231028
203.564558	7716.547063	26.236045
203.516788	7732.949957	26.241063
204.134570	7739.565510	26.246080
204.513013	7763.605469	26.251098
205.091443	7762.210436	26.256116
204.741535	7773.135664	26.261133
205.602469	7784.636400	26.266151
205.131515	7800.772368	26.271168
205.504972	7808.282224	26.276186
205.984497	7825.776512	26.281204
205.848166	7827.045421	26.286221
206.269761	7833.248754	26.291239
206.311439	7854.188311	26.296256
206.595744	7864.054015	26.301274
207.028646	7864.136616	26.306292
206.606118	7879.159083	26.311309
207.426460	7874.487883	26.316327
207.094927	7889.629475	26.321344
207.217885	7906.425538	26.326362
207.566800	7917.945604	26.331380
207.755341	7942.257873	26.336397
207.899746	7946.659802	26.341415
208.406401	7974.108964	26.346432
208.491599	7971.704210	26.351450
209.093913	7985.671125	26.356468
208.982040	8008.107242	26.361485
209.356865	8006.377613	26.366503
209.487234	8019.925204	26.371520
209.707332	8032.161488	26.376538
210.086120	8038.310002	26.381556
210.246472	8053.331190	26.386573
210.452644	8060.507451	26.391591
210.500551	8077.274804	26.396608
210.850000	8083.370855	26.401626
210.831550	8099.058495	26.406644
211.015049	8107.725256	26.411661
211.537591	8118.457044	26.416679
211.702400	8134.703373	26.421696
211.748026	8141.048479	26.426714
211.878633	8148.335421	26.431732
212.049933	8166.870831	26.436749
212.356770	8164.947222	26.441767
212.462746	8182.115180	26.446784
212.511674	8191.275377	26.451802
212.974120	8201.177716	26.456820
213.167965	8220.493984	26.461837
213.710419	8219.094841	26.466855
213.630413	8230.095434	26.471872
213.834402	8242.498505	26.476890
214.473568	8255.699099	26.481908
214.414545	8260.112350	26.486925
214.861253	8253.347269	26.491943
214.955708	8267.551960	26.496960
214.971725	8276.803719	26.501978
215.535063	8290.513664	26.506996
215.404237	8294.597321	26.512013
215.749351	8287.972539	26.517031
215.419992	8310.644100	26.522048
215.623704	8315.813540	26.527066
216.229572	8337.996304	26.532084
216.246494	8348.907883	26.537101
216.649394	8345.986164	26.542119
216.649059	8360.709027	26.547136
216.936469	8373.556411	26.552154
217.412265	8380.958395	26.557172
217.329814	8407.307069	26.562189
217.837444	8400.938787	26.567207
218.162025	8422.081905	26.572224
217.958759	8435.888720	26.577242
218.164606	8436.073275	26.582260
218.347054	8456.077186	26.587277
218.584266	8461.706534	26.592295
219.233398	8468.450163	26.597312
219.400554	8489.449396	26.602330
219.525947	8480.554658	26.607348
219.389903	8500.993740	26.612365
219.998454	8518.973242	26.617383
220.026851	8523.347945	26.622400
219.895875	8541.533023	26.627418
220.283010	8557.885841	26.632436
220.423680	8572.270382	26.637453
221.225882	8575.563909	26.642471
221.313222	8582.526789	26.647488
221.496100	8594.706068	26.652506
221.837458	8601.768010	26.657524
222.228124	8617.722430	26.662541
222.254501	8626.913527	26.667559
222.651503	8639.013592	26.672576
222.530792	8644.035488	26.677594
222.804973	8647.426633	26.682612
223.010279	8668.860748	26.687629
223.158377	8671.357258	26.692647
223.493746	8685.265763	26.697664
223.659589	8697.093514	26.702682
223.975340	8698.608009	26.707700
224.133587	8721.466790	26.712717
224.455870	8727.603197	26.717735
224.339276	8729.417128	26.722752
224.573326	8737.457899	26.727770
224.815281	8755.539899	26.732788
225.057516	8768.410312	26.737805
225.330127	8774.346475	26.742823
225.387984	8786.097473	26.747840
225.683381	8789.738696	26.752858
226.204226	8799.124027	26.757876
225.962319	8818.973445	26.762893
226.359855	8817.514010	26.767911
226.778596	8827.802394	26.772928
226.985413	8839.936000	26.777946
227.067596	8854.717650	26.782964
227.224313	8874.793459	26.787981
227.226470	8874.574107	26.792999
227.718658	8886.542230	26.798016
227.898167	8909.100615	26.803034
228.455152	8920.698398	26.808052
228.406466	8950.605603	26.813069
228.447962	8956.196981	26.818087
228.903406	8968.480300	26.823104
228.523906	8985.714212	26.828122
228.996180	9000.898688	26.833140
229.281250	9018.600151	26.838157
229.408778	9028.498962	26.843175
229.703967	9043.474325	26.848192
229.807585	9075.561643	26.853210
230.540144	9071.003640	26.858228
230.571806	9092.930555	26.863245
231.133589	9099.505856	26.868263
231.356024	9105.854125	26.873280
231.318718	9130.325082	26.878298
231.808413	9134.123740	26.883316
232.000336	9148.410982	26.888333
232.563783	9157.099057	26.893351
232.429659	9160.097041	26.898368
232.879964	9184.331651	26.903386
233.558950	9193.792529	26.908404
233.457161	9197.577563	26.913421
233.548158	9190.234902	26.918439
233.815105	9207.645020	26.923456
234.065644	9203.966922	26.928474
234.127991	9214.983177	26.933492
234.476408	9235.481959	26.938509
234.827002	9242.952290	26.943527
235.354427	9248.953676	26.948544
234.895953	9249.085878	26.953562
235.573127	9260.189012	26.958580
235.417018	9279.100910	26.963597
235.951060	9278.111240	26.968615
236.438324	9284.496123	26.973632
236.453250	9303.701757	26.978650
236.329479	9302.656241	26.983668
236.914698	9316.193924	26.988685
237.090585	9325.588272	26.993703
237.113463	9324.448285	26.998720
237.093501	9332.213809	27.003738
237.466875	9348.257009	27.008756
237.365376	9357.342807	27.013773
237.595120	9369.701364	27.018791
237.877228	9392.553259	27.023808
237.700884	9409.891462	27.028826
238.158080	9421.632774	27.033844
238.067342	9444.889014	27.038861
238.860723	9464.390003	27.043879
239.040632	9474.395138	27.048896
239.093562	9486.440580	27.053914
239.584314	9507.020884	27.058932
239.748121	9521.959335	27.063949
239.920137	9547.914069	27.068967
240.635896	9549.092991	27.073984
240.818073	9570.504693	27.079002
240.717839	9576.872216	27.084020
241.107936	9595.512796	27.089037
241.312935	9611.227421	27.094055
241.855103	9620.292852	27.099072
241.949737	9645.741006	27.104090
242.373468	9644.540163	27.109108
242.621008	9659.465964	27.114125
242.239654	9677.868571	27.119143
243.328709	9672.568565	27.124160
243.510235	9697.365296	27.129178
243.906018	9696.391424	27.134196
244.274900	9697.722788	27.139213
244.451864	9693.212579	27.144231
244.814820	9708.789920	27.149248
244.661693	9720.938615	27.154266
245.004327	9716.727763	27.159284
245.446223	9721.842647	27.164301
245.272854	9739.609304	27.169319
245.729553	9741.604776	27.174336
245.862563	9747.686565	27.179354
245.991852	9757.968435	27.184372
246.389664	9781.853666	27.189389
246.570092	9786.777023	27.194407
246.779803	9789.936793	27.199424
246.978975	9810.662013	27.204442
246.776068	9810.151611	27.209460
247.263880	9835.860432	27.214477
247.453300	9846.946731	27.219495
247.785257	9860.517256	27.224512
247.815231	9881.180173	27.229530
247.713241	9894.829837	27.234548
248.310402	9912.515030	27.239565
248.393680	9939.538231	27.244583
248.923612	9949.625485	27.249600
248.880171	9972.858617	27.254618
249.408652	9991.209624	27.259636
249.873113	10010.663655	27.264653
249.786441	10020.730582	27.269671
250.191105	10033.609619	27.274688
250.377619	10039.531069	27.279706
250.297319	10057.973898	27.284724
250.673913	10069.184270	27.289741
250.976207	10086.857166	27.294759
251.308270	10101.075532	27.299776
251.492073	10114.298198	27.304794
251.869121	10137.431125	27.309812
252.238109	10146.767639	27.314829
252.050242	10169.575125	27.319847
252.534464	10176.014465	27.324864
253.148803	10191.635852	27.329882
253.722553	10200.143087	27.334900
253.442216	10210.183446	27.339917
253.191166	10228.031711	27.344935
254.191225	10233.534862	27.349952
254.035427	10259.132486	27.354970
254.382874	10264.093545	27.359988
255.078393	10274.491422	27.365005
255.066517	10294.575832	27.370023
255.710976	10287.553824	27.375040
255.956801	10309.098995	27.380058
255.975506	10307.423872	27.385076
256.025229	10314.604320	27.390093
256.221446	10327.375922	27.395111
256.582128	10336.067878	27.400128
256.985132	10358.668769	27.405146
257.343166	10360.843545	27.410164
257.710806	10365.219692	27.415181
257.496126	10388.909822	27.420199
257.775227	10395.627089	27.425216
257.857056	10413.842400	27.430234
258.091042	10432.266450	27.435252
258.798249	10449.074536	27.440269
258.898557	10468.496987	27.445287
259.586540	10457.627115	27.450304
259.465874	10474.350210	27.455322
259.586376	10485.836419	27.460340
260.091889	10494.040337	27.465357
260.218143	10519.630997	27.470375
260.593090	10524.754463	27.475392
260.762357	10543.739705	27.480410
260.909813	10547.899931	27.485428
261.068549	10559.863425	27.490445
261.326256	10587.195039	27.495463
261.974518	10591.203248	27.500480
262.506964	10617.017546	27.505498
262.424668	10628.582741	27.510516
263.155220	10615.792373	27.515533
262.860973	10643.374702	27.520551
263.371721	10652.119900	27.525568
263.642469	10656.188107	27.530586
263.728677	10673.200575	27.535604
263.981930	10677.765031	27.540621
263.724932	10693.430677	27.545639
264.184000	10706.915515	27.550656
264.385708	10712.341361	27.555674
264.189133	10733.802188	27.560692
264.781019	10752.708931	27.565709
264.805361	10778.720890	27.570727
264.985649	10788.515607	27.575744
265.224804	10806.463282	27.580762
265.573457	10830.539713	27.585780
265.907544	10839.661988	27.590797
266.556910	10856.067532	27.595815
267.013998	10868.255893	27.600832
267.181652	10880.599459	27.605850
267.332966	10904.137779	27.610868
267.746851	10906.462222	27.615885
267.998506	10924.789250	27.620903
268.083041	10927.583032	27.625920
268.512970	10953.637639	27.630938
268.814071	10966.628151	27.635956
268.939964	10975.701090	27.640973
269.033310	11003.926743	27.645991
269.300659	11015.871956	27.651008
269.576698	11034.439193	27.656026
269.507936	11053.421705	27.661044
270.235704	11067.398169	27.666061
270.316259	11100.642281	27.671079
270.419642	11108.236225	27.676096
270.795112	11128.242663	27.681114
271.036106	11155.228246	27.686132
271.385762	11167.109033	27.691149
271.603684	11193.146782	27.696167
272.103128	11203.421279	27.701184
272.921164	11215.819091	27.706202
272.747135	11233.267578	27.711220
273.350638	11246.591004	27.716237
273.860846	11263.225684	27.721255
273.921974	11264.624118	27.726272
274.319411	11286.629983	27.731290
274.258732	11294.958149	27.736308
274.461937	11294.305595	27.741325
274.797069	11316.553840	27.746343
274.751509	11329.265237	27.751360
275.185591	11344.906031	27.756378
275.237154	11367.979885	27.761396
275.383246	11375.821935	27.766413
275.427205	11407.224376	27.771431
276.091495	11420.387813	27.776448
276.320303	11448.772251	27.781466
276.238777	11473.364632	27.786484
277.209214	11480.392508	27.791501
277.433458	11499.416721	27.796519
277.517019	11512.312577	27.801536
278.348587	11534.253820	27.806554
278.373247	11548.456806	27.811572
279.013232	11562.554334	27.816589
279.378789	11575.587868	27.821607
279.078031	11576.126426	27.826624
279.551628	11592.720441	27.831642
279.464359	11607.818893	27.836660
280.064138	11600.647971	27.841677
280.082402	11630.925288	27.846695
280.153541	11646.526146	27.851712
280.813487	11665.023571	27.856730
280.690523	11676.588599	27.861748
281.365535	11683.752305	27.866765
281.717827	11705.080930	27.871783
281.715267	11707.380739	27.876800
282.016694	11726.458178	27.881818
282.286521	11742.820935	27.886836
282.771793	11759.135749	27.891853
282.745857	11770.997830	27.896871
282.909660	11798.300295	27.901888
283.609138	11799.849395	27.906906
283.588891	11817.935632	27.911924
283.704328	11837.762149	27.916941
284.064309	11860.536407	27.921959
284.368431	11879.206960	27.926976
285.011726	11884.174547	27.931994
284.675194	11907.619848	27.937012
285.383826	11929.626826	27.942029
285.701586	11954.131004	27.947047
285.953530	11962.806227	27.952064
286.677974	11969.321736	27.957082
286.725291	11980.960232	27.962100
287.600591	12004.703854	27.967117
287.767115	12010.493917	27.972135
287.794697	12012.930441	27.977152
288.062884	12017.428102	27.982170
288.690099	12026.511835	27.987188
289.723817	12031.459829	27.992205
289.694413	12018.091013	27.997223
290.093980	12018.892513	28.002240
290.151093	12024.149736	28.007258
290.536192	12046.235968	28.012276
290.660485	12045.789182	28.017293
290.626016	12049.988857	28.022311
290.647750	12051.392536	28.027328
290.804746	12070.824518	28.032346
290.744263	12085.392436	28.037364
291.206057	12100.288489	28.042381
291.287363	12122.039196	28.047399
291.379223	12146.952746	28.052416
291.749981	12162.201724	28.057434
291.770484	12183.185962	28.062452
291.752546	12209.904047	28.067469
292.237546	12242.794328	28.072487
292.598198	12273.677652	28.077504
292.870581	12294.495931	28.082522
293.117121	12323.504531	28.087540
293.658559	12347.023771	28.092557
293.998810	12370.996751	28.097575
294.441135	12383.801858	28.102592
295.208500	12398.127294	28.107610
295.117406	12420.445375	28.112628
295.333176	12431.916627	28.117645
295.742368	12451.676203	28.122663
295.948958	12471.152169	28.127680
296.039910	12480.206718	28.132698
296.155692	12507.505990	28.137716
296.772640	12526.126818	28.142733
297.167562	12546.443721	28.147751
297.028807	12571.063321	28.152768
297.497326	12589.205326	28.157786
297.786412	12617.289894	28.162804
298.257675	12639.418897	28.167821
298.551388	12648.522317	28.172839
298.461446	12686.172430	28.177856
299.250411	12698.763917	28.182874
299.153971	12719.923341	28.187892
299.624820	12741.727884	28.192909
300.261940	12754.066477	28.197927
300.666760	12781.586171	28.202944
301.101675	12779.629840	28.207962
301.524084	12806.200921	28.212980
301.719133	12818.273327	28.217997
302.286588	12835.459310	28.223015
302.012722	12847.066787	28.228032
302.557181	12855.039854	28.233050
302.446208	12878.422662	28.238068
302.759923	12899.212561	28.243085
303.425314	12911.674091	28.248103
303.596104	12941.513179	28.253120
303.956597	12956.555040	28.258138
304.143912	12970.296381	28.263156
304.298684	12986.735268	28.268173
304.695240	13003.326589	28.273191
304.698268	13023.176961	28.278208
305.255162	13040.418558	28.283226
305.677657	13062.246001	28.288244
306.211415	13070.011388	28.293261
306.760364	13093.230956	28.298279
306.616426	13109.092302	28.303296
306.991795	13117.089751	28.308314
307.664490	13132.877346	28.313332
308.020095	13157.893804	28.318349
308.231988	13154.035472	28.323367
308.081363	13188.806565	28.328384
308.798055	13195.883420	28.333402
309.087747	13209.192898	28.338420
309.375165	13236.005317	28.343437
309.568510	13239.980267	28.348455
309.858262	13265.334431	28.353472
309.954910	13273.912456	28.358490
310.364697	13297.294865	28.363508
310.380090	13317.247496	28.368525
310.812194	13337.467595	28.373543
310.823592	13353.896749	28.378560
311.326409	13362.753528	28.383578
311.341922	13394.338027	28.388596
311.691782	13409.873879	28.393613
312.209460	13427.346415	28.398631
312.320075	13462.174181	28.403648
312.551000	13483.923116	28.408666
312.990334	13500.220752	28.413684
313.073415	13518.023208	28.418701
313.615733	13541.428957	28.423719
314.001926	13566.573190	28.428736
314.338895	13589.358528	28.433754
314.388718	13612.379100	28.438772
314.993514	13632.757525	28.443789
315.497045	13650.448657	28.448807
315.610267	13675.904637	28.453824
316.129120	13695.925899	28.458842
316.776534	13705.695893	28.463860
317.116462	13741.247806	28.468877
317.762455	13743.599085	28.473895
317.834043	13754.555353	28.478912
318.454453	13763.108486	28.483930
318.367840	13773.992584	28.488948
318.224765	13796.034577	28.493965
318.702892	13808.651832	28.498983
318.935612	13828.014599	28.504000
319.365996	13844.809029	28.509018
319.801385	13878.445592	28.514036
319.834815	13887.994663	28.519053
320.322070	13892.215718	28.524071
320.291485	13922.132081	28.529088
320.884118	13930.800396	28.534106
321.238869	13950.131358	28.539124
321.954298	13952.183903	28.544141
322.661592	13967.045886	28.549159
323.319699	13974.382163	28.554176
323.271694	13972.423353	28.559194
323.659281	13995.331403	28.564212
323.772218	14003.506666	28.569229
324.222336	14000.158974	28.574247
324.239650	14029.337549	28.579264
324.719204	14035.829672	28.584282
324.845601	14037.500872	28.589300
324.918292	14063.394698	28.594317
325.492981	14074.690522	28.599335
325.681177	14099.108206	28.604352
325.600374	14116.509097	28.609370
326.031188	14140.500667	28.614388
326.021042	14166.107797	28.619405
326.264455	14181.736706	28.624423
326.471508	14206.958333	28.629440
327.232389	14232.931498	28.634458
327.566077	14257.058100	28.639476
327.765772	14286.248428	28.644493
328.061674	14302.812606	28.649511
328.314166	14338.535263	28.654528
328.393323	14357.827248	28.659546
329.003665	14372.275909	28.664564
329.232525	14399.424962	28.669581
329.620353	14407.141917	28.674599
329.669759	14440.861547	28.679616
330.439441	14457.672533	28.684634
330.582770	14486.540291	28.689652
330.863943	14510.742467	28.694669
331.346916	14526.611213	28.699687
331.647803	14546.967204	28.704704
332.007218	14577.148919	28.709722
332.381807	14594.558955	28.714740
332.600654	14617.569297	28.719757
332.959376	14640.183705	28.724775
333.345200	14668.672902	28.729792
333.776039	14689.147081	28.734810
333.964110	14712.013087	28.739828
334.245270	14737.840714	28.744845
334.492329	14753.710707	28.749863
335.017307	14780.987751	28.754880
335.295731	14802.342526	28.759898
335.448990	14834.531947	28.764916
335.709820	14854.606726	28.769933
336.342248	14871.714356	28.774951
336.486315	14902.825742	28.779968
336.474634	14932.833693	28.784986
337.071249	14953.918179	28.790004
337.641985	14994.578197	28.795021
337.993156	15009.492706	28.800039
338.331332	15026.375080	28.805056
338.360616	15057.539532	28.810074
338.729884	15088.622127	28.815092
339.278387	15108.535993	28.820109
339.406378	15139.581223	28.825127
340.232479	15171.244567	28.830144
340.303130	15192.417927	28.835162
340.869640	15208.366015	28.840180
341.005647	15248.662956	28.845197
341.390962	15259.273260	28.850215
342.037907	15287.148147	28.855232
342.223910	15301.827985	28.860250
342.872414	15323.674865	28.865268
343.405680	15343.066715	28.870285
343.774688	15348.856357	28.875303
344.714277	15374.488585	28.880320
344.296677	15385.195598	28.885338
344.874726	15397.412328	28.890356
344.981133	15420.135676	28.895373
345.294427	15425.086834	28.900391
345.779858	15451.347156	28.905408
346.172585	15463.676089	28.910426
346.583610	15477.180987	28.915444
346.472372	15502.364562	28.920461
346.797516	15504.372286	28.925479
347.162148	15530.376004	28.930496
347.427195	15550.955330	28.935514
347.773522	15562.223537	28.940532
348.155608	15584.616122	28.945549
348.509004	15595.555262	28.950567
348.799781	15601.741452	28.955584
349.230981	15634.824289	28.960602
349.594136	15651.576913	28.965620
349.722664	15683.898330	28.970637
349.822507	15694.858923	28.975655
350.633055	15708.973366	28.980672
350.981792	15728.256999	28.985690
351.520998	15735.973858	28.990708
352.030789	15746.749152	28.995725
352.818291	15757.158433	29.000743
353.222313	15767.408027	29.005760
353.180733	15791.785620	29.010778
353.395408	15801.522269	29.015796
353.248635	15814.278116	29.020813
353.933943	15823.059238	29.025831
354.520749	15849.841933	29.030848
354.572537	15874.060195	29.035866
355.152614	15885.652701	29.040884
355.249939	15913.206683	29.045901
355.626788	15931.106415	29.050919
355.836882	15947.789413	29.055936
356.049825	15973.249178	29.060954
356.660610	15987.024497	29.065972
356.885301	16017.678043	29.070989
357.180214	16032.150697	29.076007
357.674541	16056.482545	29.081024
357.437986	16075.770736	29.086042
358.312760	16094.023539	29.091060
358.467514	16127.656029	29.096077
358.729626	16162.132471	29.101095
359.315882	16184.984286	29.106112
359.154741	16206.089893	29.111130
359.946703	16226.239251	29.116148
360.125846	16259.487915	29.121165
360.587684	16285.955382	29.126183
360.872104	16313.302981	29.131200
361.386298	16345.234846	29.136218
361.867975	16364.323031	29.141236
362.267282	16399.474801	29.146253
362.266182	16422.396079	29.151271
362.796843	16441.999327	29.156288
362.955400	16468.760256	29.161306
363.413326	16502.604805	29.166324
363.929658	16527.157423	29.171341
364.318914	16558.385954	29.176359
364.833808	16581.608395	29.181376
365.000451	16612.728573	29.186394
365.367742	16620.874149	29.191412
365.632763	16650.640722	29.196429
366.204031	16672.288227	29.201447
366.239476	16689.659277	29.206464
366.709376	16715.435566	29.211482
367.244974	16741.153342	29.216500
367.467160	16776.744563	29.221517
367.379264	16787.619819	29.226535
367.975117	16815.301097	29.231552
368.012546	16847.391305	29.236570
368.669397	16870.960288	29.241588
369.354285	16899.477733	29.246605
369.413547	16933.618492	29.251623
369.710509	16954.603968	29.256640
370.174040	16989.886282	29.261658
370.345554	17015.070975	29.266676
370.708218	17037.910259	29.271693
371.489496	17071.300122	29.276711
372.106651	17093.715937	29.281728
371.903553	17116.415820	29.286746
372.726144	17150.456153	29.291764
373.195477	17170.412869	29.296781
373.534058	17195.099408	29.301799
374.008650	17215.555022	29.306816
374.164165	17243.430716	29.311834
374.583197	17265.671044	29.316852
374.563455	17290.969332	29.321869
375.183151	17326.001730	29.326887
375.994592	17347.895875	29.331904
375.936988	17374.030017	29.336922
376.218946	17399.562110	29.341940
376.642742	17426.250738	29.346957
376.954223	17454.322340	29.351975
377.803095	17476.367891	29.356992
377.910967	17505.371511	29.362010
378.430553	17530.654978	29.367028
378.550119	17555.515166	29.372045
379.301972	17585.319786	29.377063
379.769184	17609.318023	29.382080
379.891830	17633.345392	29.387098
380.304862	17654.321314	29.392116
380.731838	17671.895869	29.397133
381.224558	17697.017081	29.402151
381.920813	17715.420509	29.407168
382.131882	17740.262136	29.412186
382.663588	17756.623815	29.417204
382.899551	17776.167207	29.422221
383.521141	17801.990124	29.427239
383.574130	17815.143656	29.432256
383.931872	17845.965366	29.437274
384.233840	17861.482078	29.442292
384.921528	17892.565790	29.447309
385.018737	17906.752341	29.452327
385.621816	17927.416986	29.457344
385.243244	17961.721588	29.462362
386.113731	17986.376470	29.467380
386.511046	18008.192685	29.472397
386.500044	18033.183164	29.477415
386.886171	18058.696833	29.482432
387.101943	18087.441753	29.487450
387.489176	18113.038874	29.492468
388.013273	18138.242083	29.497485
388.407385	18171.306356	29.502503
388.910415	18183.716156	29.507520
388.917836	18214.491375	29.512538
389.497222	18234.824648	29.517556
390.008980	18272.184072	29.522573
390.233437	18306.143234	29.527591
390.864181	18323.409226	29.532608
390.983030	18346.817090	29.537626
391.180041	18379.560819	29.542644
392.308991	18401.699913	29.547661
392.501339	18426.020756	29.552679
393.096179	18452.982840	29.557696
393.665075	18470.705763	29.562714
393.853500	18494.584352	29.567732
394.594280	18519.872399	29.572749
394.564752	18543.387950	29.577767
395.178147	18560.294539	29.582784
395.656534	18582.923755	29.587802
396.095982	18599.231124	29.592820
396.363485	18619.569440	29.597837
396.646077	18641.161764	29.602855
397.355397	18656.639357	29.607872
397.547242	18679.016675	29.612890
397.843033	18704.890514	29.617908
398.504434	18727.338781	29.622925
398.785991	18759.767625	29.627943
399.271832	18771.599031	29.632960
399.242542	18795.710861	29.637978
399.062432	18817.392168	29.642996
399.794691	18847.640704	29.648013
400.091988	18874.913029	29.653031
400.500931	18909.828773	29.658048
401.028374	18944.081008	29.663066
401.254523	18984.604852	29.668084
401.745164	19009.457204	29.673101
402.234610	19049.858825	29.678119
402.585974	19073.798605	29.683136
403.290518	19102.143009	29.688154
403.818344	19130.397920	29.693172
404.271592	19155.857608	29.698189
404.871841	19175.969293	29.703207
405.434437	19194.195444	29.708224
405.476498	19222.322484	29.713242
406.166721	19244.432249	29.718260
406.673324	19259.658186	29.723277
406.886822	19291.092218	29.728295
407.371208	19309.156886	29.733312
407.785205	19332.450896	29.738330
407.767912	19357.072319	29.743348
408.332579	19380.482476	29.748365
408.394515	19404.530664	29.753383
408.919402	19422.571169	29.758400
409.222561	19442.904371	29.763418
409.372413	19474.144681	29.768436
409.766724	19492.453604	29.773453
410.130763	19530.755629	29.778471
411.078772	19551.240183	29.783488
411.237354	19581.555244	29.788506
411.400310	19608.277856	29.793524
412.113294	19632.676773	29.798541
411.996156	19675.846923	29.803559
412.906082	19704.854057	29.808576
412.982127	19729.251899	29.813594
413.092669	19758.564830	29.818612
413.441978	19779.264212	29.823629
414.262345	19816.996744	29.828647
414.699414	19845.771387	29.833664
415.396986	19879.007755	29.838682
415.681196	19913.535426	29.843700
416.460869	19934.514436	29.848717
416.593347	19961.900333	29.853735
416.690669	19987.926834	29.858752
417.268083	20019.066496	29.863770
417.636871	20056.747659	29.868788
418.321884	20093.859114	29.873805
418.600253	20128.299926	29.878823
419.017986	20151.567622	29.883840
419.267615	20184.990155	29.888858
419.603079	20222.535489	29.893876
420.201390	20250.780200	29.898893
420.256366	20298.160805	29.903911
421.078589	20330.738105	29.908928
421.104171	20361.318603	29.913946
421.444211	20396.728574	29.918964
422.285127	20424.153066	29.923981
422.089909	20468.052898	29.928999
422.898533	20503.836907	29.934016
423.912864	20535.763576	29.939034
424.517857	20566.048048	29.944052
424.927231	20584.913763	29.949069
425.069309	20619.490883	29.954087
425.529094	20642.167052	29.959104
425.968669	20666.073474	29.964122
426.511657	20694.632732	29.969140
427.285878	20720.118616	29.974157
427.694291	20746.040933	29.979175
428.007709	20769.573340	29.984192
428.370885	20794.232565	29.989210
428.538814	20829.262961	29.994228
429.003802	20845.987567	29.999245
429.385410	20882.818461	30.004263
429.848718	20909.600455	30.009280
430.346983	20935.654310	30.014298
430.619008	20972.710743	30.019316
431.218364	20993.364031	30.024333
431.570056	21027.608037	30.029351
432.100138	21052.907618	30.034368
432.394320	21071.093496	30.039386
432.364469	21095.412108	30.044404
432.913253	21113.786198	30.049421
433.154299	21149.544268	30.054439
433.758056	21179.677094	30.059456
434.275638	21206.835011	30.064474
434.382878	21232.229398	30.069492
435.032178	21269.724845	30.074509
435.300179	21308.578752	30.079527
435.829184	21341.438472	30.084544
436.837801	21361.217867	30.089562
437.124581	21395.585697	30.094580
438.029409	21420.870491	30.099597
438.109634	21452.534789	30.104615
438.978149	21477.732854	30.109632
439.197099	21502.094562	30.114650
439.221776	21521.273241	30.119668
439.661530	21544.487039	30.124685
440.135151	21579.012447	30.129703
440.180354	21605.113433	30.134720
440.537669	21642.528858	30.139738
440.468668	21685.109251	30.144756
441.143511	21715.252922	30.149773
441.707777	21764.849469	30.154791
442.014526	21797.730812	30.159808
443.401106	21831.360705	30.164826
443.878814	21863.225726	30.169844
444.840369	21886.648610	30.174861
445.279195	21916.883547	30.179879
445.854647	21925.270421	30.184896
446.145679	21940.120988	30.189914
445.969566	21970.852480	30.194932
446.423155	22000.291838	30.199949
446.947188	22025.723214	30.204967
447.831736	22046.510261	30.209984
448.346911	22074.188790	30.215002
448.734808	22103.478736	30.220020
449.354707	22117.870981	30.225037
449.750148	22137.493015	30.230055
450.195236	22158.579435	30.235072
450.565421	22178.767239	30.240090
450.751485	22205.051584	30.245108
450.946584	22234.422103	30.250125
451.454570	22263.581357	30.255143
451.644085	22294.864212	30.260160
452.041841	22327.921794	30.265178
451.846842	22362.815685	30.270196
452.736953	22404.292059	30.275213
453.239181	22439.946576	30.280231
453.384001	22481.755864	30.285248
454.070402	22515.240593	30.290266
454.316660	22560.407432	30.295284
454.513589	22595.799195	30.300301
455.045152	22635.744815	30.305319
455.319843	22674.261631	30.310336
456.466293	22704.589596	30.315354
456.488410	22746.505715	30.320372
457.165043	22778.992814	30.325389
457.416771	22802.778307	30.330407
457.946118	22852.167947	30.335424
458.439485	22881.942643	30.340442
458.895436	22923.195045	30.345460
459.592697	22943.296163	30.350477
459.928250	22979.721568	30.355495
461.039578	23002.918468	30.360512
462.597698	23006.161964	30.365530
462.923203	23030.020290	30.370548
463.850783	23023.764577	30.375565
463.992240	23042.885524	30.380583
464.315770	23065.905259	30.385600
464.952125	23069.354037	30.390618
464.974872	23080.922455	30.395636
465.090515	23104.804232	30.400653
465.632340	23130.852407	30.405671
465.521854	23144.566394	30.410688
466.089718	23169.190828	30.415706
466.031301	23204.832621	30.420724
466.308275	23242.795206	30.425741
466.751433	23272.787358	30.430759
466.733469	23315.361480	30.435776
467.379348	23361.755138	30.440794
467.753440	23414.910639	30.445812
468.213427	23457.917334	30.450829
468.868049	23509.129416	30.455847
469.264016	23557.745946	30.460864
469.621474	23589.614290	30.465882
470.146782	23642.631033	30.470900
470.601193	23688.664112	30.475917
471.080158	23732.649193	30.480935
471.113097	23781.505199	30.485952
472.051844	23821.355419	30.490970
472.826402	23871.585996	30.495988
473.300454	23915.676476	30.501005
473.819170	23953.611821	30.506023
474.172070	24001.830089	30.511040
475.537122	24032.542470	30.516058
475.758647	24082.161881	30.521076
476.272028	24112.055146	30.526093
476.810564	24139.789790	30.531111
477.059510	24169.438277	30.536128
477.566405	24201.654352	30.541146
477.840495	24236.030057	30.546164
478.623135	24275.977478	30.551181
479.046154	24308.731738	30.556199
479.415600	24348.516714	30.561216
479.941526	24382.430035	30.566234
480.355040	24419.526463	30.571252
480.885139	24446.802518	30.576269
481.585333	24474.267118	30.581287
481.929621	24512.391300	30.586304
482.731082	24540.469519	30.591322
483.299629	24564.152692	30.596340
483.152744	24597.525626	30.601357
483.619445	24620.680626	30.606375
483.902170	24655.093540	30.611392
484.847786	24679.216954	30.616410
485.470605	24711.925125	30.621428
485.171450	24751.333520	30.626445
486.060023	24784.873207	30.631463
486.046344	24826.229577	30.636480
487.020988	24861.521122	30.641498
487.456142	24894.460524	30.646516
487.631623	24921.028424	30.651533
488.260713	24955.597083	30.656551
489.165250	25006.045278	30.661568
489.689688	25028.039568	30.666586
490.175531	25075.115080	30.671604
490.120406	25105.441857	30.676621
490.729706	25139.168885	30.681639
490.834318	25184.429970	30.686656
491.712133	25223.770242	30.691674
492.416341	25262.802825	30.696692
492.829844	25310.831405	30.701709
493.282486	25338.872910	30.706727
493.563041	25379.315853	30.711744
494.427298	25406.782216	30.716762
494.872229	25448.910045	30.721780
495.507757	25483.516511	30.726797
496.138335	25518.754798	30.731815
496.351547	25559.922621	30.736832
497.150548	25589.280554	30.741850
498.064213	25619.101531	30.746868
498.473304	25644.592669	30.751885
499.119606	25673.125185	30.756903
499.204843	25706.999904	30.761920
499.848248	25738.646564	30.766938
500.087625	25772.141687	30.771956
500.596026	25805.704340	30.776973
501.234790	25832.885102	30.781991
501.607353	25871.064216	30.787008
502.383764	25899.208879	30.792026
502.604125	25939.628742	30.797044
502.835766	25980.696614	30.802061
503.768254	26020.082958	30.807079
503.684009	26055.050499	30.812096
504.398040	26088.389187	30.817114
504.893821	26131.345934	30.822132
505.023737	26181.914520	30.827149
505.908765	26211.403881	30.832167
506.269842	26259.011883	30.837184
506.698471	26301.119337	30.842202
507.532895	26343.687342	30.847220
507.707297	26384.551457	30.852237
508.268443	26426.134914	30.857255
508.488384	26467.682296	30.862272
509.274046	26501.520563	30.867290
509.635671	26542.876647	30.872308
509.983271	26580.392800	30.877325
510.551286	26619.092138	30.882343
511.339590	26653.097447	30.887360
511.878196	26697.685554	30.892378
511.783763	26736.258907	30.897396
512.409523	26774.260963	30.902413
512.979180	26821.033456	30.907431
513.491541	26874.869935	30.912448
514.103832	26914.429903	30.917466
514.487327	26949.678731	30.922484
514.550542	27005.747287	30.927501
515.439151	27043.796380	30.932519
515.603838	27091.881980	30.937536
516.467485	27130.840968	30.942554
517.690934	27174.139356	30.947572
518.059434	27206.387890	30.952589
519.207283	27233.508851	30.957607
519.924642	27262.230558	30.962624
520.335568	27288.862687	30.967642
521.018821	27312.047276	30.972660
521.413910	27353.090374	30.977677
521.894136	27381.016875	30.982695
522.369907	27414.575605	30.987712
522.221066	27444.474521	30.992730
522.966061	27480.252437	30.997748
523.414591	27524.242892	31.002765
523.764732	27555.719117	31.007783
524.148254	27605.986516	31.012800
524.633494	27647.585893	31.017818
524.948733	27697.423569	31.022836
525.513541	27752.092971	31.027853
526.094896	27794.799379	31.032871
526.452653	27843.036946	31.037888
526.998399	27894.788590	31.042906
527.852438	27939.445707	31.047924
528.293727	27995.228646	31.052941
528.841079	28039.282336	31.057959
528.947082	28082.641947	31.062976
529.486865	28131.454873	31.067994
530.340382	28179.800872	31.073012
531.046904	28235.886178	31.078029
531.263000	28276.917941	31.083047
532.169000	28328.236844	31.088064
532.806971	28367.360307	31.093082
533.369868	28400.991185	31.098100
533.518105	28449.260009	31.103117
534.373201	28487.573551	31.108135
534.971243	28533.339299	31.113152
535.445078	28570.532049	31.118170
535.925201	28609.869249	31.123188
536.345266	28659.322551	31.128205
537.086007	28690.935810	31.133223
538.115422	28709.566944	31.138240
538.875278	28741.003489	31.143258
539.886975	28776.583758	31.148276
539.788544	28794.023146	31.153293
540.100136	28816.184904	31.158311
540.608487	28850.337118	31.163328
540.960633	28890.662342	31.168346
541.872917	28911.762137	31.173364
542.446934	28956.088056	31.178381
543.083937	28980.595322	31.183399
543.624131	29014.471057	31.188416
544.053822	29043.456377	31.193434
543.915295	29082.320092	31.198452
543.941742	29128.586036	31.203469
544.573214	29164.838035	31.208487
545.068015	29215.867147	31.213504
545.343027	29267.252741	31.218522
546.072543	29305.706329	31.223540
546.420587	29372.726344	31.228557
547.125272	29424.032461	31.233575
548.105082	29466.763009	31.238592
548.603737	29518.363432	31.243610
549.287726	29557.080945	31.248628
549.675191	29609.464254	31.253645
550.673718	29643.202715	31.258663
550.789455	29688.785912	31.263680
551.373387	29743.716963	31.268698
552.639240	29777.520312	31.273716
552.898750	29830.995843	31.278733
553.236112	29864.668165	31.283751
553.397577	29912.749409	31.288768
553.990362	29958.437724	31.293786
554.634256	30007.102334	31.298804
555.276350	30067.451580	31.303821
556.021623	30105.440380	31.308839
556.444238	30151.432866	31.313856
557.098574	30195.483088	31.318874
557.801180	30229.068278	31.323892
558.486344	30284.289734	31.328909
559.065036	30326.740849	31.333927
559.625453	30370.826533	31.338944
559.699014	30420.214769	31.343962
560.335656	30471.270533	31.348980
560.894909	30516.006791	31.353997
561.828021	30558.476620	31.359015
562.394804	30601.403748	31.364032
562.891473	30641.534656	31.369050
564.093815	30674.981425	31.374068
564.332246	30717.898832	31.379085
565.252841	30753.463999	31.384103
565.787045	30791.414708	31.389120
566.083545	30827.727517	31.394138
566.855613	30854.451474	31.399156
566.862251	30910.119309	31.404173
567.708851	30938.392586	31.409191
568.017878	30968.042303	31.414208
568.331168	31016.334031	31.419226
568.917054	31051.136716	31.424244
569.622359	31095.101555	31.429261
570.126779	31136.472372	31.434279
570.836691	31179.379530	31.439296
571.037694	31228.180180	31.444314
571.661063	31259.127093	31.449332
571.797167	31319.125519	31.454349
572.423511	31363.795619	31.459367
572.540146	31408.846632	31.464384
572.754961	31469.819772	31.469402
573.586386	31520.813625	31.474420
573.899605	31580.422845	31.479437
574.599592	31648.306279	31.484455
575.558010	31703.557908	31.489472
575.944408	31767.254369	31.494490
576.505315	31822.678612	31.499508
577.366511	31890.311296	31.504525
577.872705	31949.178661	31.509543
578.532873	31997.798605	31.514560
578.960751	32055.417469	31.519578
579.582536	32109.276419	31.524596
580.203501	32172.536517	31.529613
580.986599	32218.945941	31.534631
581.440863	32275.929853	31.539648
582.362006	32336.396775	31.544666
583.322315	32380.381054	31.549684
583.985597	32426.874664	31.554701
584.811752	32467.395040	31.559719
585.725496	32518.156739	31.564736
586.017200	32564.193669	31.569754
586.904588	32592.380542	31.574772
587.624491	32631.136480	31.579789
588.070342	32672.915370	31.584807
588.384351	32721.299949	31.589824
588.758215	32761.664958	31.594842
589.241338	32807.417252	31.599860
589.852469	32859.891730	31.604877
590.208552	32905.776495	31.609895
591.063080	32962.198546	31.614912
591.043503	33012.663962	31.619930
591.830004	33065.191046	31.624948
592.397571	33121.486037	31.629965
592.798171	33178.920681	31.634983
593.757998	33222.610464	31.640000
594.053326	33285.087663	31.645018
595.022143	33331.477622	31.650036
595.653839	33382.410022	31.655053
595.863139	33440.440033	31.660071
596.987956	33479.627068	31.665088
597.399962	33538.986030	31.670106
597.903471	33598.345290	31.675124
598.563544	33646.916079	31.680141
598.937474	33687.377836	31.685159
599.558556	33739.225141	31.690176
600.436248	33796.927176	31.695194
600.989227	33831.876626	31.700212
601.264468	33888.672256	31.705229
601.666027	33939.093362	31.710247
602.573411	33983.646108	31.715264
602.524674	34031.121152	31.720282
603.617099	34080.439603	31.725300
604.267491	34135.558999	31.730317
604.707429	34190.367454	31.735335
605.224190	34241.037931	31.740352
605.892394	34301.643187	31.745370
606.664587	34351.175050	31.750388
607.040617	34408.794568	31.755405
608.063431	34460.164826	31.760423
608.989372	34497.125230	31.765440
609.583433	34558.469957	31.770458
609.984735	34605.954620	31.775476
611.221261	34646.349643	31.780493
612.064598	34685.357140	31.785511
612.368547	34718.836028	31.790528
612.860327	34765.816405	31.795546
613.713572	34803.417969	31.800564
613.921894	34840.741897	31.805581
614.425494	34888.850480	31.810599
615.341022	34944.842214	31.815616
616.440161	34982.200025	31.820634
617.453369	35009.513817	31.825652
618.154486	35038.721189	31.830669
618.413059	35073.960205	31.835687
618.800440	35116.824742	31.840704
619.508211	35151.150548	31.845722
620.456510	35188.080134	31.850740
621.319456	35223.357924	31.855757
621.229010	35270.054303	31.860775
621.414547	35305.773408	31.865792
621.999458	35359.462194	31.870810
622.724436	35408.522140	31.875828
623.301486	35459.416112	31.880845
623.780708	35514.439634	31.885863
624.433889	35564.979980	31.890880
624.313553	35625.456487	31.895898
624.796650	35683.090123	31.900916
625.253341	35743.951079	31.905933
625.767292	35812.096733	31.910951
626.715987	35865.115514	31.915968
626.869041	35945.582772	31.920986
627.786373	36011.586331	31.926004
628.582248	36065.540916	31.931021
628.921359	36138.556488	31.936039
629.775760	36199.167757	31.941056
630.296850	36279.712317	31.946074
631.136101	36335.939210	31.951092
631.857820	36400.876101	31.956109
632.104828	36468.069351	31.961127
632.399983	36525.810454	31.966144
633.257671	36588.186919	31.971162
634.111975	36650.100174	31.976180
635.167547	36707.440114	31.981197
635.697827	36765.930817	31.986215
636.509856	36817.703718	31.991232
636.626506	36878.812956	31.996250
637.104552	36934.563814	32.001268
638.257754	36982.841265	32.006285
638.814974	37061.950015	32.011303
639.367725	37115.523228	32.016320
640.272837	37175.040039	32.021338
641.094917	37224.735344	32.026356
641.594213	37274.220933	32.031373
642.211400	37332.547044	32.036391
643.067795	37378.089110	32.041408
644.053816	37433.252559	32.046426
644.692547	37479.744434	32.051444
645.489484	37525.022427	32.056461
645.962550	37575.403495	32.061479
646.933167	37622.261863	32.066496
647.500959	37674.363136	32.071514
647.981271	37723.531211	32.076532
648.575305	37775.227377	32.081549
649.200941	37825.431474	32.086567
649.694388	37874.701876	32.091584
650.434057	37934.006435	32.096602
650.841585	37991.414081	32.101620
651.457035	38043.309363	32.106637
651.729819	38110.371641	32.111655
652.200370	38160.912586	32.116672
652.852574	38226.710721	32.121690
653.477242	38295.844201	32.126708
654.139654	38362.979545	32.131725
654.552042	38431.275474	32.136743
655.128529	38502.236297	32.141760
656.244037	38573.272358	32.146778
657.254008	38640.099781	32.151796
658.213824	38688.231770	32.156813
658.808830	38760.588895	32.161831
659.574064	38808.419909	32.166848
660.408496	38864.346026	32.171866
660.814280	38922.517680	32.176884
661.544539	38973.925544	32.181901
661.649156	39038.106203	32.186919
662.453458	39100.828685	32.191936
663.355026	39168.955147	32.196954
663.949205	39232.358087	32.201972
664.837353	39291.076493	32.206989
665.137945	39359.076159	32.212007
665.714163	39413.548626	32.217024
666.615758	39474.304708	32.222042
667.129574	39543.828067	32.227060
667.679827	39600.379671	32.232077
668.154647	39670.762576	32.237095
668.727392	39725.716423	32.242112
669.652695	39785.771767	32.247130
670.097207	39857.132936	32.252148
671.067131	39896.306681	32.257165
672.096629	39961.048739	32.262183
672.374760	40009.670339	32.267200
673.462471	40064.293874	32.272218
674.114323	40117.802022	32.277236
674.784929	40164.977147	32.282253
675.205050	40214.604170	32.287271
675.855862	40271.620475	32.292288
676.517282	40327.924787	32.297306
676.785726	40396.195806	32.302324
677.742752	40457.532845	32.307341
678.214578	40521.782017	32.312359
678.855523	40589.765772	32.317376
679.573708	40658.955213	32.322394
680.044093	40719.795569	32.327412
680.834486	40788.057536	32.332429
681.594914	40845.410429	32.337447
682.104136	40911.413102	32.342464
683.222444	40981.693894	32.347482
683.779946	41063.986451	32.352500
684.416421	41113.821917	32.357517
685.158085	41185.393016	32.362535
685.963677	41254.503393	32.367552
686.629322	41311.191989	32.372570
687.544190	41377.136290	32.377588
688.412567	41432.893853	32.382605
689.479872	41492.841989	32.387623
690.220686	41540.617940	32.392640
690.973887	41602.110495	32.397658
691.453618	41653.164569	32.402676
692.663416	41694.842682	32.407693
692.371821	41760.354080	32.412711
693.183181	41818.061182	32.417728
693.913329	41872.104029	32.422746
694.569191	41940.626911	32.427764
695.415583	41998.552743	32.432781
696.186932	42071.306178	32.437799
696.653920	42117.210809	32.442816
697.448940	42184.188867	32.447834
697.931956	42252.537268	32.452852
698.836829	42315.644899	32.457869
699.028642	42392.404632	32.462887
699.569819	42450.081032	32.467904
700.248097	42521.156595	32.472922
700.870166	42605.241483	32.477940
701.379525	42676.093969	32.482957
701.848005	42761.844619	32.487975
702.510149	42843.621871	32.492992
703.362235	42920.668498	32.498010
703.393171	43010.139053	32.503028
704.338745	43088.591259	32.508045
705.499139	43166.230223	32.513063
706.091217	43238.024249	32.518080
706.938587	43306.244597	32.523098
707.341799	43383.385804	32.528116
708.198165	43452.227193	32.533133
709.294090	43521.978249	32.538151
710.045616	43595.909317	32.543168
710.886964	43655.205239	32.548186
711.235123	43731.927859	32.553204
712.274605	43797.941429	32.558221
712.874043	43870.784960	32.563239
713.445255	43932.954186	32.568256
713.885745	44003.886617	32.573274
714.697105	44082.564891	32.578292
715.221283	44156.799196	32.583309
715.905339	44237.950347	32.588327
716.710799	44315.503275	32.593344
717.661620	44394.771568	32.598362
718.147332	44470.014713	32.603380
719.183249	44543.739723	32.608397
719.961095	44621.232320	32.613415
720.580664	44693.226110	32.618432
721.481186	44764.565735	32.623450
721.737139	44839.249711	32.628468
722.628509	44923.027211	32.633485
723.868358	44993.943255	32.638503
724.676495	45063.502986	32.643520
726.313374	45124.517773	32.648538
727.433127	45188.602431	32.653556
728.145483	45235.277891	32.658573
729.135102	45288.032388	32.663591
730.017646	45341.234857	32.668608
731.130648	45377.499727	32.673626
731.823780	45432.042295	32.678644
732.305457	45468.017583	32.683661
733.147614	45509.782933	32.688679
733.357207	45573.923754	32.693696
734.187396	45619.746263	32.698714
734.367210	45672.195273	32.703732
734.836162	45728.422418	32.708749
735.397084	45792.541686	32.713767
735.997366	45869.204492	32.718784
736.676964	45928.762620	32.723802
737.231929	46000.156607	32.728820
737.687520	46073.121658	32.733837
738.355821	46145.166285	32.738855
738.648294	46225.540319	32.743872
739.635483	46294.079074	32.748890
740.510697	46386.484283	32.753908
741.075109	46463.111404	32.758925
742.216283	46535.550219	32.763943
742.412282	46613.586426	32.768960
743.435981	46686.219636	32.773978
744.323336	46768.265783	32.778996
745.035444	46850.162284	32.784013
746.043810	46920.926195	32.789031
746.809702	46981.363438	32.794048
748.555940	47021.388642	32.799066
749.870544	47066.253657	32.804084
750.973457	47108.729505	32.809101
751.582009	47146.865417	32.814119
752.737358	47192.658113	32.819136
753.291091	47216.389247	32.824154
753.691795	47249.826726	32.829172
754.646579	47285.493843	32.834189
755.097286	47325.122590	32.839207
755.463987	47383.036532	32.844224
756.004909	47429.554073	32.849242
756.121016	47484.135022	32.854260
756.280367	47548.584786	32.859277
757.634974	47619.686759	32.864295
758.093767	47688.693707	32.869312
758.695511	47757.834332	32.874330
758.873346	47831.096848	32.879348
759.746146	47913.718895	32.884365
760.218002	47985.513518	32.889383
761.135500	48068.289649	32.894400
761.980251	48147.651712	32.899418
762.583844	48238.823734	32.904436
763.133677	48328.381953	32.909453
764.193940	48406.962772	32.914471
765.064470	48491.789132	32.919488
766.191050	48566.913347	32.924506
766.605339	48649.127520	32.929524
767.174517	48739.009653	32.934541
768.139591	48820.675381	32.939559
768.969664	48908.087858	32.944576
770.051756	48979.266801	32.949594
770.869785	49068.615103	32.954612
771.554264	49147.740249	32.959629
772.284355	49220.029023	32.964647
772.734435	49309.991061	32.969664
773.609908	49389.002352	32.974682
774.412486	49489.145093	32.979700
775.300968	49566.228107	32.984717
776.143355	49644.165846	32.989735
776.678809	49731.733581	32.994752
777.683237	49807.490000	32.999770
778.472627	49893.069211	33.004788
779.263919	49980.095165	33.009805
780.161982	50056.951058	33.014823
780.831090	50138.938367	33.019840
781.855072	50227.208017	33.024858
782.667929	50314.724540	33.029876
783.563511	50383.363024	33.034893
784.903868	50459.279237	33.039911
785.349400	50542.582694	33.044928
786.313291	50607.963014	33.049946
786.668007	50679.828738	33.054964
787.718433	50749.383319	33.059981
788.912460	50812.210465	33.064999
789.901387	50878.111772	33.070016
790.764413	50933.863297	33.075034
791.267113	50982.765073	33.080052
792.057678	51045.857933	33.085069
792.843421	51095.128480	33.090087
793.375062	51168.071308	33.095104
794.255188	51221.476814	33.100122
794.974504	51279.035572	33.105140
795.795527	51344.196434	33.110157
796.638377	51414.395457	33.115175
797.373009	51479.344122	33.120192
798.218083	51546.826534	33.125210
798.664894	51616.405463	33.130228
799.355784	51691.768014	33.135245
800.153084	51747.918516	33.140263
800.741706	51831.588346	33.145280
801.828982	51899.725469	33.150298
802.526991	51976.490502	33.155316
802.677120	52055.478882	33.160333
803.963371	52137.886943	33.165351
804.431711	52227.227470	33.170368
804.888062	52306.556130	33.175386
805.629846	52392.748341	33.180404
806.615115	52489.166366	33.185421
807.585771	52564.825527	33.190439
808.551199	52657.861185	33.195456
809.388746	52737.802343	33.200474
810.786470	52821.754801	33.205492
810.900167	52908.404360	33.210509
811.774379	52993.654031	33.215527
813.075174	53080.878174	33.220544
813.317662	53164.853053	33.225562
814.446128	53245.965901	33.230580
815.318956	53333.182323	33.235597
816.174708	53414.576361	33.240615
816.616566	53505.190912	33.245632
817.650798	53587.414414	33.250650
818.744347	53663.675959	33.255668
819.421088	53738.195740	33.260685
820.789603	53815.459666	33.265703
821.480384	53892.258661	33.270720
822.606744	53972.648200	33.275738
823.597169	54046.205515	33.280756
824.075148	54127.281744	33.285773
825.089125	54192.229409	33.290791
825.684807	54276.559217	33.295808
826.403598	54350.183142	33.300826
827.427466	54430.592091	33.305844
828.176780	54511.465439	33.310861
828.918275	54589.459030	33.315879
829.930659	54668.076336	33.320896
830.634461	54747.947410	33.325914
831.803871	54830.784806	33.330932
831.748760	54901.491254	33.335949
833.053407	54976.243034	33.340967
833.769683	55054.369145	33.345984
834.446114	55118.891085	33.351002
834.923267	55189.741190	33.356020
835.763904	55274.342900	33.361037
836.496978	55337.926933	33.366055
837.269933	55427.886886	33.371072
837.885795	55515.182169	33.376090
839.129467	55599.602476	33.381108
839.320063	55687.647509	33.386125
840.749373	55775.227988	33.391143
841.262965	55864.242198	33.396160
841.938779	55948.325207	33.401178
842.721503	56030.570279	33.406196
843.462196	56131.345037	33.411213
844.238665	56223.399680	33.416231
845.010316	56326.925387	33.421248
845.955361	56427.015722	33.426266
846.698116	56509.636132	33.431284
847.591326	56610.608353	33.436301
849.048632	56707.452570	33.441319
849.912154	56793.851531	33.446336
850.369628	56895.715043	33.451354
852.105412	56978.729742	33.456372
852.649791	57074.809422	33.461389
853.339599	57161.789527	33.466407
854.469336	57238.368190	33.471424
855.358399	57324.872488	33.476442
856.806567	57414.529772	33.481460
857.258359	57507.416910	33.486477
858.551577	57586.989774	33.491495
859.214136	57681.181419	33.496512
860.139773	57766.284649	33.501530
860.976480	57839.111195	33.506548
861.577142	57932.126462	33.511565
862.299465	58012.184299	33.516583
863.068308	58111.453651	33.521600
863.727159	58206.008611	33.526618
865.061678	58300.764290	33.531636
865.570978	58398.973488	33.536653
866.708996	58483.480864	33.541671
867.325903	58571.136803	33.546688
867.600392	58671.321503	33.551706
868.636853	58768.936582	33.556724
869.688641	58875.372579	33.561741
870.318683	58975.662205	33.566759
870.958367	59084.249250	33.571776
871.648383	59191.703230	33.576794
872.392188	59289.099151	33.581812
873.294741	59408.336988	33.586829
874.113006	59514.500297	33.591847
874.721552	59622.880643	33.596864
875.518166	59742.157534	33.601882
876.953907	59844.038931	33.606900
877.794756	59956.217833	33.611917
878.764346	60061.713363	33.616935
879.760753	60164.708186	33.621952
880.435257	60271.538429	33.626970
882.240318	60356.128939	33.631988
882.832826	60453.619523	33.637005
883.553137	60537.840346	33.642023
884.555663	60629.528605	33.647040
885.611314	60721.947710	33.652058
886.480085	60799.102781	33.657076
887.625945	60894.705563	33.662093
888.473624	60981.087091	33.667111
889.363018	61077.638539	33.672128
889.986207	61170.335998	33.677146
890.989602	61250.838779	33.682164
891.679352	61337.849346	33.687181
892.702678	61428.538884	33.692199
893.970243	61521.949297	33.697216
894.465800	61620.789437	33.702234
895.867084	61707.376286	33.707252
896.490950	61804.374843	33.712269
897.319437	61894.278048	33.717287
898.230940	61991.209254	33.722304
898.886083	62091.617257	33.727322
900.187592	62180.290224	33.732340
900.473501	62282.178353	33.737357
901.553329	62384.108005	33.742375
902.520528	62480.475686	33.747392
903.470291	62588.212665	33.752410
904.210269	62681.389962	33.757428
905.282068	62786.072784	33.762445
906.123282	62881.755902	33.767463
906.945741	62986.318078	33.772480
908.132873	63088.024199	33.777498
909.173256	63181.070106	33.782516
909.691368	63297.722252	33.787533
910.572641	63401.157514	33.792551
911.387340	63495.564701	33.797568
912.121013	63607.326617	33.802586
913.284138	63718.231686	33.807604
914.076428	63824.023326	33.812621
914.754885	63935.353930	33.817639
915.851337	64038.521590	33.822656
916.783378	64148.962774	33.827674
917.796528	64250.514705	33.832692
918.537630	64366.129440	33.837709
919.580077	64480.827093	33.842727
920.734349	64590.650925	33.847744
921.388319	64707.565830	33.852762
922.536707	64808.218538	33.857780
923.426023	64919.929192	33.862797
924.381922	65028.980063	33.867815
925.446882	65137.987532	33.872832
926.399939	65246.717589	33.877850
927.291288	65340.000929	33.882868
928.526731	65441.166503	33.887885
929.640860	65552.469000	33.892903
930.534652	65639.513150	33.897920
931.076344	65728.887682	33.902938
932.623988	65806.836498	33.907956
933.603915	65883.093596	33.912973
935.001515	65969.698773	33.917991
936.203311	66038.774110	33.923008
937.225914	66123.471542	33.928026
938.388674	66179.770018	33.933044
939.044984	66275.310615	33.938061
940.086372	66333.495426	33.943079
940.761757	66396.459695	33.948096
941.286859	66483.304919	33.953114
942.041833	66567.980417	33.958132
942.908571	66657.025009	33.963149
943.409487	66743.350663	33.968167
944.454802	66832.005016	33.973184
944.997018	66951.107512	33.978202
945.928101	67039.953010	33.983220
946.180197	67142.262509	33.988237
947.101109	67267.201057	33.993255
948.076441	67360.491567	33.998272
948.732726	67490.908056	34.003290
949.675102	67604.501688	34.008308
950.617104	67728.927176	34.013325
951.899261	67852.378304	34.018343
952.830719	67963.313745	34.023360
954.150497	68086.038959	34.028378
955.256753	68194.966555	34.033396
956.596621	68303.949545	34.038413
957.353538	68420.892588	34.043431
958.499166	68520.039523	34.048448
959.273094	68629.171675	34.053466
960.049711	68740.485438	34.058484
961.108458	68853.509330	34.063501
962.086526	68961.539580	34.068519
963.276205	69064.349003	34.073536
964.375504	69178.626005	34.078554
965.380519	69281.436475	34.083572
966.498240	69387.857780	34.088589
967.498968	69497.025057	34.093607
968.707130	69589.842769	34.098624
969.685367	69698.490070	34.103642
970.764934	69799.140249	34.108660
971.456352	69898.276477	34.113677
972.317811	69990.440724	34.118695
973.235048	70103.558650	34.123712
974.338317	70217.536947	34.128730
975.466941	70316.511689	34.133748
976.369410	70418.858217	34.138765
977.291854	70526.045807	34.143783
978.325270	70617.525608	34.148800
979.278342	70727.851872	34.153818
980.152464	70834.233488	34.158836
981.066245	70934.708657	34.163853
981.788377	71050.369194	34.168871
982.747801	71149.180674	34.173888
983.667433	71249.789101	34.178906
984.450824	71344.938419	34.183924
985.840980	71444.784179	34.188941
987.247583	71534.154952	34.193959
988.409964	71612.096042	34.198976
990.030994	71704.156469	34.203994
990.893712	71786.475187	34.209012
992.443568	71851.607676	34.214029
993.401970	71936.117700	34.219047
994.883102	71998.018100	34.224064
995.577851	72070.153098	34.229082
996.487671	72137.894112	34.234100
997.607955	72210.551179	34.239117
998.014447	72299.565125	34.244135
998.720212	72371.218585	34.249152
999.472292	72466.637457	34.254170
1000.516124	72558.825636	34.259188
1001.042633	72652.993781	34.264205
1002.189509	72755.941880	34.269223
1003.015890	72853.341899	34.274240
1003.651980	72961.830095	34.279258
1004.472405	73073.076362	34.284276
1005.384087	73180.234571	34.289293
1006.235081	73305.371766	34.294311
1007.785205	73414.565812	34.299328
1008.389038	73527.875340	34.304346
1008.933187	73639.924414	34.309364
1010.302816	73756.367501	34.314381
1011.369965	73876.417496	34.319399
1012.880424	73985.912107	34.324416
1013.106605	74106.923261	34.329434
1014.363831	74229.251174	34.334452
1015.235577	74343.783975	34.339469
1016.265411	74470.086222	34.344487
1017.421961	74598.625491	34.349504
1018.286008	74716.033054	34.354522
1019.541283	74842.501218	34.359540
1020.326967	74963.471835	34.364557
1021.202479	75086.217724	34.369575
1022.224513	75212.215604	34.374592
1023.062395	75342.616405	34.379610
1024.177456	75468.523905	34.384628
1024.867558	75595.194336	34.389645
1025.796293	75732.811584	34.394663
1027.136727	75873.275142	34.399680
1028.260836	76006.040747	34.404698
1029.057345	76142.424422	34.409716
1030.107694	76272.016251	34.414733
1031.165417	76413.853629	34.419751
1032.384129	76538.724692	34.424768
1033.740530	76671.435491	34.429786
1034.670358	76804.593331	34.434804
1036.025707	76928.747359	34.439821
1036.929076	77051.511925	34.444839
1038.076095	77163.545077	34.449856
1039.094770	77273.399425	34.454874
1039.575857	77385.933585	34.459892
1040.511867	77504.330287	34.464909
1041.589957	77630.490325	34.469927
1043.170354	77738.359343	34.474944
1043.885698	77868.928670	34.479962
1044.534220	77987.307552	34.484980
1045.980211	78094.752153	34.489997
1047.188916	78222.936409	34.495015
1048.372290	78342.054262	34.500032
1049.625381	78459.857645	34.505050
1050.629930	78582.973802	34.510068
1052.061373	78696.509420	34.515085
1052.879988	78815.306332	34.520103
1054.206521	78928.361312	34.525120
1055.216219	79043.160200	34.530138
1055.909574	79162.796455	34.535156
1056.712549	79276.379328	34.540173
1057.671852	79414.722372	34.545191
1058.921156	79533.727644	34.550208
1059.863525	79672.574932	34.555226
1060.514833	79806.804024	34.560244
1061.645048	79934.859548	34.565261
1062.442891	80076.068488	34.570279
1063.684195	80212.305649	34.575296
1064.754925	80339.842200	34.580314
1065.738139	80489.341352	34.585332
1066.881277	80621.289353	34.590349
1067.839989	80758.944704	34.595367
1068.610689	80903.965713	34.600384
1070.102852	81045.384395	34.605402
1071.099343	81185.806944	34.610420
1072.513708	81319.249918	34.615437
1073.607136	81458.917298	34.620455
1075.076409	81583.773198	34.625472
1076.798067	81711.218557	34.630490
1077.634706	81844.447153	34.635508
1079.317569	81961.353507	34.640525
1080.176416	82090.625354	34.645543
1081.045612	82217.213478	34.650560
1082.362657	82335.063823	34.655578
1083.042993	82457.459104	34.660596
1084.581344	82579.866293	34.665613
1085.421590	82714.832920	34.670631
1086.095097	82830.195499	34.675648
1087.327168	82962.426385	34.680666
1088.278583	83089.201333	34.685684
1089.538483	83207.521461	34.690701
1090.637822	83349.242954	34.695719
1091.897511	83462.698673	34.700736
1093.096852	83590.300751	34.705754
1094.526260	83708.309664	34.710772
1095.503685	83826.618029	34.715789
1096.443218	83955.835809	34.720807
1097.388519	84055.149271	34.725824
1098.462701	84164.982841	34.730842
1099.205356	84288.421119	34.735860
1100.729339	84411.023894	34.740877
1101.310823	84525.493099	34.745895
1102.320963	84644.825081	34.750912
1103.091119	84758.143108	34.755930
1103.881192	84888.366092	34.760948
1105.252692	85021.122614	34.765965
1106.058774	85164.480933	34.770983
1106.726222	85299.030125	34.776000
1107.857407	85437.120256	34.781018
1108.357926	85584.323874	34.786036
1109.438045	85732.435319	34.791053
1110.367749	85897.450350	34.796071
1111.677055	86055.795005	34.801088
1113.316714	86210.723916	34.806106
1114.446965	86365.703094	34.811124
1115.530169	86507.281854	34.816141
1116.366011	86666.831751	34.821159
1117.784694	86811.202596	34.826176
1119.679125	86949.721422	34.831194
1121.022342	87081.431188	34.836212
1122.921564	87218.685089	34.841229
1124.540894	87352.215956	34.846247
1125.559940	87475.851368	34.851264
1127.191228	87590.022741	34.856282
1128.475142	87699.545711	34.861300
1129.217931	87808.250523	34.866317
1130.287576	87941.334547	34.871335
1131.473374	88061.913044	34.876352
1132.712966	88184.179018	34.881370
1133.507099	88309.211580	34.886388
1134.936933	88427.294601	34.891405
1135.774904	88547.688275	34.896423
1136.570587	88681.785285	34.901440
1137.480112	88802.148995	34.906458
1138.350252	88942.487582	34.911476
1139.344070	89077.293346	34.916493
1140.353268	89225.704425	34.921511
1141.467115	89361.883592	34.926528
1142.623784	89514.214140	34.931546
1143.359231	89659.257090	34.936564
1144.808631	89799.893880	34.941581
1146.350695	89948.958666	34.946599
1147.227194	90088.486360	34.951616
1148.845600	90222.273839	34.956634
1149.930618	90365.083917	34.961652
1151.453394	90502.857742	34.966669
1152.374296	90642.058221	34.971687
1153.398061	90773.906185	34.976704
1154.737492	90908.181928	34.981722
1155.632656	91054.800863	34.986740
1156.934953	91199.642021	34.991757
1158.443901	91319.320630	34.996775
1159.344628	91444.547336	35.001792
1160.626335	91568.886614	35.006810
1161.907271	91686.226152	35.011828
1162.721195	91805.013405	35.016845
1163.552523	91940.919909	35.021863
1164.736024	92074.671749	35.026880
1165.842216	92187.739431	35.031898
1166.688629	92320.391987	35.036916
1167.969118	92453.167163	35.041933
1168.722864	92591.375592	35.046951
1169.860198	92741.944595	35.051968
1171.534092	92870.882083	35.056986
1172.199594	93016.374698	35.062004
1173.863234	93162.089734	35.067021
1174.942773	93306.892835	35.072039
1175.936920	93453.116669	35.077056
1177.241547	93587.786493	35.082074
1178.478006	93727.469492	35.087092
1179.966941	93874.174476	35.092109
1181.238962	94018.581633	35.097127
1182.214448	94169.471886	35.102144
1183.531154	94305.498199	35.107162
1184.400169	94452.281079	35.112180
1185.927602	94587.279000	35.117197
1187.176910	94731.751156	35.122215
1188.052493	94879.928103	35.127232
1189.858091	95023.528069	35.132250
1190.621016	95161.559318	35.137268
1191.924150	95316.812740	35.142285
1193.088217	95464.532275	35.147303
1194.355731	95611.038492	35.152320
1195.463523	95750.406664	35.157338
1196.547370	95909.537643	35.162356
1197.626486	96060.522848	35.167373
1199.023434	96200.350462	35.172391
1200.364758	96359.237619	35.177408
1201.561165	96499.221510	35.182426
1202.390704	96659.913824	35.187444
1203.634861	96809.906640	35.192461
1204.901670	96967.082050	35.197479
1206.042002	97133.580253	35.202496
1207.389643	97280.823173	35.207514
1208.775969	97434.872507	35.212532
1210.494443	97573.209194	35.217549
1212.078348	97713.633611	35.222567
1212.927741	97863.674919	35.227584
1214.361286	97996.573600	35.232602
1215.612202	98138.798442	35.237620
1216.556310	98288.053626	35.242637
1217.773092	98425.607125	35.247655
1218.839919	98579.870034	35.252672
1220.144516	98727.331288	35.257690
1221.297583	98874.547083	35.262708
1222.815025	99009.899581	35.267725
1224.714543	99135.557250	35.272743
1225.405223	99262.454519	35.277760
1226.702183	99390.350302	35.282778
1227.871048	99514.666004	35.287796
1228.873350	99645.931230	35.292813
1229.778599	99771.521629	35.297831
1230.754919	99913.841318	35.302848
1232.089942	100051.471929	35.307866
1232.883532	100196.262151	35.312884
1233.951367	100334.231270	35.317901
1234.912757	100486.130259	35.322919
1235.784085	100651.772936	35.327936
1237.080465	100802.590676	35.332954
1238.150098	100961.799878	35.337972
1238.786001	101140.244743	35.342989
1240.422422	101308.527682	35.348007
1241.856688	101486.869906	35.353024
1243.071067	101647.711180	35.358042
1244.268222	101826.716861	35.363060
1245.233338	102008.549636	35.368077
1246.852522	102170.705237	35.373095
1247.820942	102353.578320	35.378112
1249.508116	102516.066360	35.383130
1250.219743	102693.679332	35.388148
1251.595373	102873.028879	35.393165
1253.157616	103051.562483	35.398183
1254.250070	103232.558721	35.403200
1255.770499	103410.190041	35.408218
1256.907449	103593.714131	35.413236
1258.169880	103772.240612	35.418253
1259.745960	103937.137482	35.423271
1261.043901	104121.220269	35.428288
1262.096487	104300.014203	35.433306
1263.579005	104476.924577	35.438324
1264.734857	104655.259931	35.443341
1266.504491	104824.182156	35.448359
1267.781339	104998.889389	35.453376
1269.068100	105167.503815	35.458394
1270.535517	105338.013593	35.463412
1271.770927	105503.383796	35.468429
1273.654680	105659.600478	35.473447
1274.969392	105830.253528	35.478464
1276.262769	105976.250236	35.483482
1277.744103	106144.723511	35.488500
1278.603119	106313.190377	35.493517
1280.264058	106478.202414	35.498535
1281.112563	106644.874521	35.503552
1282.345002	106805.161309	35.508570
1283.856668	106962.449919	35.513588
1285.487685	107133.462412	35.518605
1287.311964	107274.941917	35.523623
1288.407747	107434.090481	35.528640
1289.497505	107585.197501	35.533658
1290.961464	107746.387583	35.538676
1291.935209	107909.828610	35.543693
1293.408391	108060.049272	35.548711
1294.487182	108216.266542	35.553728
1295.621997	108352.726791	35.558746
1296.907371	108490.314680	35.563764
1297.696270	108646.356023	35.568781
1299.026230	108787.877349	35.573799
1299.912052	108955.342616	35.578816
1300.993518	109114.883467	35.583834
1301.917523	109268.194344	35.588852
1302.913988	109443.168273	35.593869
1304.017858	109618.580973	35.598887
1305.144783	109799.463403	35.603904
1306.551255	109985.911111	35.608922
1307.868014	110170.918601	35.613940
1308.911830	110359.166443	35.618957
1310.401872	110542.145173	35.623975
1311.716242	110729.779146	35.628992
1313.137712	110924.591750	35.634010
1314.648985	111109.673556	35.639028
1315.759109	111301.919707	35.644045
1316.882152	111497.332156	35.649063
1318.133855	111696.727299	35.654080
1319.287131	111894.379734	35.659098
1320.996981	112096.043049	35.664116
1322.373144	112294.268266	35.669133
1323.951180	112483.452534	35.674151
1324.955005	112692.715815	35.679168
1325.991823	112900.505356	35.684186
1327.703967	113091.178411	35.689204
1328.973139	113300.464129	35.694221
1330.671566	113502.494231	35.699239
1331.751948	113695.255970	35.704256
1333.269664	113906.594131	35.709274
1334.738003	114099.368227	35.714292
1336.018203	114302.717272	35.719309
1337.893120	114494.296820	35.724327
1339.213123	114696.488887	35.729344
1340.706693	114877.784760	35.734362
1343.614009	115036.096546	35.739380
1345.492806	115206.913565	35.744397
1347.426410	115363.797374	35.749415
1348.880565	115513.529235	35.754432
1350.285401	115670.378528	35.759450
1351.645729	115818.138754	35.764468
1352.545180	115979.409611	35.769485
1353.913316	116122.760648	35.774503
1355.243502	116290.535664	35.779520
1355.951385	116449.966653	35.784538
1357.392233	116609.539150	35.789556
1358.545265	116783.442111	35.794573
1359.613222	116954.129531	35.799591
1360.662126	117127.672245	35.804608
1362.244610	117301.073978	35.809626
1363.813359	117472.819145	35.814644
1364.320104	117653.680493	35.819661
1365.743822	117812.578276	35.824679
1366.699390	117983.176925	35.829696
1367.601294	118157.739322	35.834714
1369.001085	118333.256622	35.839732
1369.773770	118522.808671	35.844749
1370.779466	118702.805443	35.849767
1372.024147	118897.778737	35.854784
1373.194227	119095.186461	35.859802
1374.556814	119291.485422	35.864820
1375.707374	119502.433103	35.869837
1377.020025	119703.977000	35.874855
1378.125573	119929.090450	35.879872
1379.290231	120147.238264	35.884890
1380.909440	120360.646345	35.889908
1382.196370	120582.274070	35.894925
1383.934344	120796.856188	35.899943
1385.519989	121019.500550	35.904960
1387.195601	121232.144844	35.909978
1388.654668	121442.647941	35.914996
1389.891910	121670.730173	35.920013
1391.699468	121876.905803	35.925031
1393.188812	122088.599535	35.930048
1394.541088	122303.448558	35.935066
1396.198534	122514.242037	35.940084
1397.916142	122725.698393	35.945101
1399.320032	122919.732867	35.950119
1400.972067	123124.904399	35.955136
1402.251505	123334.323474	35.960154
1404.271183	123530.499733	35.965172
1405.631980	123721.099383	35.970189
1407.650781	123914.692762	35.975207
1409.300131	124110.568591	35.980224
1410.364215	124300.893117	35.985242
1412.130688	124475.952742	35.990260
1413.801282	124670.447012	35.995277
1415.405573	124862.659776	36.000295
1416.630232	125040.882592	36.005312
1417.875472	125226.948536	36.010330
1419.513651	125404.963259	36.015348
1420.580429	125601.480644	36.020365
1422.305611	125787.087572	36.025383
1423.415998	125965.854954	36.030400
1424.852685	126165.113770	36.035418
1426.404657	126338.496872	36.040436
1427.489932	126528.920231	36.045453
1428.838422	126719.717987	36.050471
1430.518972	126907.075756	36.055488
1432.238592	127101.881116	36.060506
1434.032259	127278.181451	36.065524
1434.990844	127472.079977	36.070541
1436.230164	127651.633511	36.075559
1438.170538	127839.129845	36.080576
1439.252704	128030.817765	36.085594
1440.830723	128208.389783	36.090612
1442.120964	128394.923248	36.095629
1443.517490	128591.048052	36.100647
1445.049075	128764.422700	36.105664
1446.371366	128936.122835	36.110682
1448.005678	129098.390082	36.115700
1449.296845	129271.757945	36.120717
1450.750818	129440.091722	36.125735
1452.696715	129613.463476	36.130752
1453.696187	129782.041640	36.135770
1455.198258	129950.496644	36.140788
1456.245234	130126.129342	36.145805
1457.539811	130300.021946	36.150823
1459.145939	130483.268341	36.155840
1460.160105	130676.023323	36.160858
1461.495822	130860.611188	36.165876
1462.333270	131052.016877	36.170893
1463.856914	131267.925156	36.175911
1464.923684	131463.933850	36.180928
1466.289320	131675.992681	36.185946
1467.891770	131887.657402	36.190964
1469.409030	132111.394304	36.195981
1470.790458	132315.543895	36.200999
1472.489367	132531.075605	36.206016
1473.523683	132766.182699	36.211034
1474.981482	132982.519308	36.216052
1476.516810	133204.992827	36.221069
1478.098808	133431.250566	36.226087
1479.903208	133649.801598	36.231104
1481.264938	133875.060485	36.236122
1483.160293	134089.655976	36.241140
1484.747359	134308.540161	36.246157
1486.408776	134529.264106	36.251175
1487.895361	134745.581987	36.256192
1489.411737	134961.718676	36.261210
1491.190832	135171.586615	36.266228
1493.117846	135389.925271	36.271245
1494.889058	135604.323565	36.276263
1496.006231	135818.721055	36.281280
1497.129112	136030.431005	36.286298
1498.804654	136235.987145	36.291316
1500.279946	136460.876363	36.296333
1501.739220	136671.429689	36.301351
1503.296425	136884.921829	36.306368
1504.444642	137113.117244	36.311386
1506.347308	137317.347797	36.316404
1507.974482	137535.764344	36.321421
1509.378233	137748.831714	36.326439
1511.586727	137957.768607	36.331456
1512.873856	138170.592295	36.336474
1514.205738	138374.597189	36.341492
1515.823182	138593.288435	36.346509
1517.241309	138805.066570	36.351527
1518.855672	139007.733525	36.356544
1520.094547	139227.875711	36.361562
1521.807984	139424.112023	36.366580
1523.699274	139635.408511	36.371597
1524.948852	139849.605780	36.376615
1526.654265	140045.618739	36.381632
1528.086560	140238.496743	36.386650
1529.561274	140424.089924	36.391668
1531.367582	140620.722879	36.396685
1532.551455	140812.251699	36.401703
1534.596154	140985.412016	36.406720
1535.790324	141184.955342	36.411738
1537.171786	141364.279781	36.416756
1539.183549	141558.486149	36.421773
1540.344379	141758.101834	36.426791
1541.930922	141939.156764	36.431808
1543.617112	142139.166576	36.436826
1545.061867	142332.421696	36.441844
1546.444568	142536.328097	36.446861
1547.831747	142734.274656	36.451879
1549.433637	142923.955317	36.456896
1550.317534	143142.496159	36.461914
1551.844103	143348.956933	36.466932
1553.482397	143569.831512	36.471949
1554.545708	143798.072486	36.476967
1555.894895	144011.757979	36.481984
1557.669518	144249.061725	36.487002
1558.807975	144474.149006	36.492020
1560.409385	144710.331361	36.497037
1561.653717	144950.634649	36.502055
1563.664408	145194.714507	36.507072
1564.805965	145435.241497	36.512090
1566.417789	145681.396676	36.517108
1567.994229	145925.416227	36.522125
1569.218712	146178.197876	36.527143
1570.920673	146424.938702	36.532160
1573.045012	146675.477140	36.537178
1574.333201	146926.058902	36.542196
1576.066534	147177.834477	36.547213
1577.465726	147432.750911	36.552231
1579.141014	147680.113456	36.557248
1580.783008	147934.839582	36.562266
1582.493234	148194.109061	36.567284
1584.353194	148438.718127	36.572301
1585.811649	148698.630296	36.577319
1587.353527	148942.802421	36.582336
1589.442147	149203.244414	36.587354
1590.541822	149452.277223	36.592372
1592.300869	149695.617978	36.597389
1593.710530	149947.695833	36.602407
1595.750822	150190.357436	36.607424
1597.353099	150446.172757	36.612442
1598.872121	150699.454532	36.617460
1600.786388	150940.049583	36.622477
1602.122996	151199.910912	36.627495
1603.453882	151450.058760	36.632512
1605.407059	151698.896722	36.637530
1607.030397	151946.689174	36.642548
1609.516297	152189.984795	36.647565
1610.693775	152428.761768	36.652583
1612.607177	152655.947265	36.657600
1614.174401	152872.994731	36.662618
1615.821979	153088.444041	36.667636
1617.850677	153301.951946	36.672653
1619.037878	153517.710720	36.677671
1620.685323	153725.615961	36.682688
1622.272693	153950.416521	36.687706
1623.869612	154163.609740	36.692724
1625.826716	154377.059606	36.697741
1627.084509	154607.742842	36.702759
1628.857334	154816.685241	36.707776
1630.364205	155051.869813	36.712794
1631.530206	155279.807200	36.717812
1633.363236	155511.653099	36.722829
1634.486477	155751.956314	36.727847
1636.047749	155994.773916	36.732864
1637.199873	156235.760105	36.737882
1638.643550	156483.104250	36.742900
1640.675901	156732.201337	36.747917
1642.132572	156995.936747	36.752935
1644.351957	157251.056286	36.757952
1645.745729	157496.956217	36.762970
1647.387429	157753.509796	36.767988
1648.833209	158008.157477	36.773005
1650.270057	158259.763497	36.778023
1651.930755	158523.334261	36.783040
1653.574405	158792.161901	36.788058
1654.728847	159053.323384	36.793076
1656.505303	159326.229574	36.798093
1658.523699	159600.491712	36.803111
1660.266668	159857.434273	36.808128
1662.351414	160131.345984	36.813146
1663.759166	160403.637174	36.818164
1665.866518	160654.977967	36.823181
1667.646003	160928.160473	36.828199
1669.606740	161173.642515	36.833216
1671.603085	161437.174147	36.838234
1673.470986	161689.361342	36.843252
1675.692942	161938.571293	36.848269
1677.114385	162187.856224	36.853287
1678.997895	162434.119978	36.858304
1680.587063	162672.327974	36.863322
1682.285686	162923.346027	36.868340
1683.977119	163163.797677	36.873357
1685.848034	163418.240243	36.878375
1687.626381	163650.724305	36.883392
1689.140504	163903.378283	36.888410
1690.952964	164142.342788	36.893428
1692.331680	164393.043384	36.898445
1693.890051	164647.622697	36.903463
1695.763538	164893.990869	36.908480
1697.421209	165138.557499	36.913498
1698.932191	165385.294951	36.918516
1700.724009	165635.589306	36.923533
1702.309124	165884.308959	36.928551
1703.714055	166119.293444	36.933568
1705.008712	166354.323405	36.938586
1706.841488	166595.048687	36.943604
1708.814679	166817.605925	36.948621
1710.403494	167056.903483	36.953639
1712.353717	167293.260030	36.958656
1714.044027	167531.832133	36.963674
1715.218497	167779.071702	36.968692
1717.172546	168009.099351	36.973709
1718.524603	168256.970961	36.978727
1720.025855	168502.711924	36.983744
1721.888114	168761.906811	36.988762
1723.390173	169013.842862	36.993780
1725.162160	169270.670392	36.998797
1726.953988	169528.549195	37.003815
1729.005647	169789.773157	37.008832
1730.360064	170046.739851	37.013850
1731.975268	170303.853683	37.018868
1733.748335	170565.929099	37.023885
1735.832746	170833.295242	37.028903
1737.889427	171095.540803	37.033920
1739.909217	171358.466707	37.038938
1741.373913	171612.720016	37.043956
1743.322699	171866.688807	37.048973
1745.197461	172135.214883	37.053991
1746.878709	172399.701903	37.059008
1748.594532	172645.364293	37.064026
1750.088548	172915.102005	37.069044
1752.102024	173181.757326	37.074061
1753.815247	173444.823216	37.079079
1755.914823	173706.339589	37.084096
1757.671507	173962.040116	37.089114
1759.272200	174225.751307	37.094132
1761.241944	174487.636707	37.099149
1762.857442	174757.224171	37.104167
1764.536909	175024.923855	37.109184
1766.178919	175285.854241	37.114202
1767.673140	175566.368644	37.119220
1769.347308	175840.266981	37.124237
1770.896386	176127.641192	37.129255
1772.419014	176404.995226	37.134272
1774.401370	176683.947423	37.139290
1776.040817	176972.630894	37.144308
1777.872103	177263.440779	37.149325
1779.420475	177552.333481	37.154343
1781.201765	177849.513858	37.159360
1783.220822	178151.617838	37.164378
1784.935667	178448.089579	37.169396
1786.945733	178738.686811	37.174413
1788.565045	179026.090615	37.179431
1790.315374	179319.883181	37.184448
1792.091817	179609.865216	37.189466
1793.843151	179913.383260	37.194484
1795.686461	180202.874795	37.199501
1797.870447	180491.751151	37.204519
1799.388732	180770.779245	37.209536
1801.292135	181035.374783	37.214554
1802.981179	181300.706396	37.219572
1804.570863	181572.529647	37.224589
1806.792242	181841.072974	37.229607
1808.625783	182114.888084	37.234624
1810.560385	182388.522271	37.239642
1811.785170	182662.596584	37.244660
1814.285068	182918.264870	37.249677
1816.173334	183204.312232	37.254695
1817.715147	183472.510159	37.259712
1820.077028	183734.755550	37.264730
1821.360011	184013.167705	37.269748
1823.529022	184290.084162	37.274765
1825.255700	184566.722239	37.279783
1826.706775	184836.516216	37.284800
1828.905794	185098.872000	37.289818
1830.367370	185457.090953	37.294836
1832.432113	185738.398962	37.299853
1834.240319	186019.904563	37.304871
1835.961181	186314.018819	37.309888
1837.996834	186590.842334	37.314906
1839.737174	186874.178941	37.319924
1841.451133	187165.353680	37.324941
1843.444438	187457.764188	37.329959
1845.122572	187747.335790	37.334976
1846.676027	188040.700336	37.339994
1848.715940	188348.492732	37.345012
1850.936107	188631.463738	37.350029
1852.807493	188923.978503	37.355047
1854.566112	189220.601616	37.360064
1857.004224	189502.320772	37.365082
1858.790605	189796.834666	37.370100
1861.044561	190085.544693	37.375117
1863.136029	190370.742045	37.380135
1864.918341	190651.931270	37.385152
1866.818752	190929.229641	37.390170
1869.333102	191213.114457	37.395188
1871.115705	191488.010750	37.400205
1872.948175	191774.680718	37.405223
1874.350204	192063.228333	37.410240
1876.103990	192336.292486	37.415258
1878.043724	192622.909882	37.420276
1879.748685	192916.513043	37.425293
1882.162340	193206.593978	37.430311
1883.874503	193501.239608	37.435328
1885.894660	193765.707625	37.440346
1887.595613	194054.860577	37.445364
1889.374248	194327.713141	37.450381
1891.622593	194614.680178	37.455399
1893.408439	194898.414020	37.460416
1895.139519	195185.865600	37.465434
1896.939801	195466.222354	37.470452
1898.718665	195758.936987	37.475469
1900.811672	196041.912213	37.480487
1902.562231	196302.094547	37.485504
1904.386217	196565.566278	37.490522
1906.369284	196847.954289	37.495540
1907.839454	197106.892684	37.500557
1909.742132	197375.356346	37.505575
1911.401581	197647.595338	37.510592
1913.043044	197925.513694	37.515610
1914.551274	198209.512079	37.520628
1916.203399	198493.169599	37.525645
1918.318737	198798.561418	37.530663
1920.033885	199089.549080	37.535680
1921.667199	199396.562210	37.540698
1923.605540	199711.231293	37.545716
1925.412034	200007.450762	37.550733
1927.732612	200317.384779	37.555751
1929.447096	200634.406989	37.560768
1931.672487	200942.569729	37.565786
1933.454154	201260.471947	37.570804
1934.523059	201577.748342	37.575821
1936.758155	201903.701774	37.580839
1938.811816	202233.293614	37.585856
1940.402479	202568.768650	37.590874
1942.208413	202910.798152	37.595892
1943.994194	203255.587929	37.600909
1946.260627	203598.697203	37.605927
1947.715123	203955.050475	37.610944
1949.846568	204285.209291	37.615962
1952.028077	204632.261159	37.620980
1953.807145	204987.522462	37.625997
1956.261627	205337.222615	37.631015
1957.695258	205691.606554	37.636032
1960.174343	206018.272140	37.641050
1961.960777	206376.509625	37.646068
1964.135298	206729.819091	37.651085
1966.471690	207069.769745	37.656103
1968.492075	207425.546554	37.661120
1971.037019	207763.458146	37.666138
1973.234692	208099.703593	37.671156
1975.433523	208444.076897	37.676173
1977.765230	208769.254858	37.681191
1979.870650	209109.532686	37.686208
1982.099902	209417.029529	37.691226
1984.303609	209749.369457	37.696244
1985.831454	210067.248704	37.701261
1988.956395	210389.681282	37.706279
1990.810234	210707.710268	37.711296
1992.511461	211025.639515	37.716314
1994.680287	211343.972458	37.721332
1996.641273	211659.091277	37.726349
1998.417401	211969.747548	37.731367
2000.267939	212292.430359	37.736384
2002.492855	212598.516729	37.741402
2004.312445	212918.616521	37.746420
2006.391663	213234.279273	37.751437
2008.287677	213536.589991	37.756455
2010.087548	213841.153100	37.761472
2012.081086	214140.960115	37.766490
2013.708469	214439.941777	37.771508
2015.232679	214738.307070	37.776525
2017.397840	215045.706864	37.781543
2018.746950	215367.063645	37.786560
2020.848273	215673.968369	37.791578
2022.791295	215992.787400	37.796596
2024.287901	216314.045825	37.801613
2026.660888	216649.657761	37.806631
2028.026949	216993.164102	37.811648
2030.233932	217323.523800	37.816666
2032.077065	217663.344213	37.821684
2034.132475	218007.751962	37.826701
2036.339969	218352.109429	37.831719
2037.992603	218698.924989	37.836736
2040.447311	219053.833703	37.841754
2042.806903	219399.997238	37.846772
2044.549470	219749.264476	37.851789
2046.972153	220101.718377	37.856807
2048.577154	220451.239948	37.861824
2050.865464	220810.018044	37.866842
2052.820168	221172.054639	37.871860
2055.226558	221529.875033	37.876877
2057.902979	221870.785132	37.881895
2059.942564	222224.860485	37.886912
2062.397938	222570.941120	37.891930
2064.816363	222911.034763	37.896948
2067.377218	223249.225429	37.901965
2069.751246	223583.054824	37.906983
2072.047682	223909.710236	37.912000
2074.054771	224235.907995	37.917018
2075.911150	224577.042171	37.922036
2077.998657	224913.286326	37.927053
2079.759872	225241.052726	37.932071
2081.756795	225576.272700	37.937088
2083.937726	225911.055660	37.942106
2085.982681	226245.100714	37.947124
2088.505835	226588.259759	37.952141
2090.689475	226915.653263	37.957159
2092.233903	227253.113866	37.962176
2094.174849	227594.977981	37.967194
2096.423716	227939.076327	37.972212
2098.397612	228283.095533	37.977229
2100.507863	228627.905069	37.982247
2102.004716	228978.103696	37.987264
2103.988552	229333.960472	37.992282
2106.077576	229700.925720	37.997300
2107.569597	230063.777392	38.002317
2109.909842	230429.685400	38.007335
2112.203170	230797.786792	38.012352
2114.273200	231163.971343	38.017370
2116.287971	231524.603316	38.022388
2118.408573	231909.019003	38.027405
2120.589822	232267.998470	38.032423
2122.227137	232618.714670	38.037440
2123.917845	232969.092247	38.042458
2126.126929	233311.761442	38.047476
2127.813695	233685.891552	38.052493
2130.326263	234039.153521	38.057511
2132.216346	234407.306401	38.062528
2134.206929	234771.988205	38.067546
2136.347054	235136.772161	38.072564
2138.265944	235507.716491	38.077581
2140.380155	235881.549350	38.082599
2142.775665	236250.152832	38.087616
2144.840453	236641.827721	38.092634
2147.063269	237021.207176	38.097652
2149.248406	237393.404992	38.102669
2151.603110	237770.781898	38.107687
2154.099447	238150.396037	38.112704
2156.295438	238536.082511	38.117722
2158.520529	238902.585997	38.122740
2160.690594	239284.391642	38.127757
2163.152350	239655.123432	38.132775
2165.463472	240044.780900	38.137792
2167.499879	240414.875329	38.142810
2170.146703	240793.274124	38.147828
2172.304946	241179.199948	38.152845
2174.714017	241549.079880	38.157863
2177.037156	241910.947819	38.162880
2178.721915	242289.005217	38.167898
2181.471735	242684.866033	38.172916
2183.350343	243052.781062	38.177933
2185.593845	243432.751216	38.182951
2187.715050	243824.275576	38.187968
2190.176680	244198.519166	38.192986
2192.672314	244563.358356	38.198004
2194.813034	244941.366466	38.203021
2197.309062	245312.099838	38.208039
2200.148693	245677.008400	38.213056
2201.781043	246050.430497	38.218074
2204.546311	246411.719884	38.223092
2207.068830	246772.746277	38.228109
2209.300641	247132.044495	38.233127
2211.922842	247497.728611	38.238144
2213.918581	247837.380504	38.243162
2216.497248	248183.563151	38.248180
2218.383078	248547.494201	38.253197
2220.606843	248908.090745	38.258215
2222.634827	249256.222723	38.263232
2224.639551	249615.739469	38.268250
2227.260065	249979.850713	38.273268
2228.608657	250335.059959	38.278285
2231.025003	250700.502097	38.283303
2233.250358	251072.937543	38.288320
2235.359707	251441.125294	38.293338
2237.546760	251810.646302	38.298356
2239.475013	252183.133088	38.303373
2241.513362	252541.299230	38.308391
2243.949042	252895.358463	38.313408
2245.636170	253251.603465	38.318426
2248.152603	253596.783410	38.323444
2250.257000	253942.668980	38.328461
2252.574272	254290.931537	38.333479
2254.874375	254643.134599	38.338496
2256.579732	255014.263188	38.343514
2258.917762	255364.732469	38.348532
2261.105395	255728.233948	38.353549
2263.094095	256105.614223	38.358567
2265.496032	256479.494432	38.363584
2267.511618	256855.879418	38.368602
2269.843343	257230.609944	38.373620
2272.072395	257619.380580	38.378637
2274.042782	257998.237355	38.383655
2276.356821	258381.582502	38.388672
2278.236779	258785.273560	38.393690
2280.788461	259178.967845	38.398708
2283.088532	259575.474006	38.403725
2285.282035	259986.579702	38.408743
2287.762375	260379.828602	38.413760
2289.505714	260801.248462	38.418778
2292.120691	261206.591343	38.423796
2294.506891	261619.060635	38.428813
2296.888597	262029.752275	38.433831
2299.493346	262439.795888	38.438848
2301.765937	262860.031892	38.443866
2304.695778	263251.322768	38.448884
2307.357242	263654.878159	38.453901
2309.660094	264056.665569	38.458919
2312.516853	264452.032634	38.463936
2314.663580	264856.056212	38.468954
2317.322616	265250.948413	38.473972
2319.426599	265650.202886	38.478989
2321.623186	266056.223764	38.484007
2324.127394	266459.194128	38.489024
2325.939472	266867.845673	38.494042
2328.469707	267261.462541	38.499060
2330.557139	267681.345041	38.504077
2332.429410	268093.846235	38.509095
2335.000373	268517.455530	38.514112
2337.051269	268935.310592	38.519130
2339.283061	269360.450187	38.524148
2341.380056	269787.161833	38.529165
2343.546394	270201.286735	38.534183
2346.173634	270630.650045	38.539200
2348.690559	271077.584765	38.544218
2350.684539	271502.939833	38.549236
2352.748982	271943.422085	38.554253
2354.866833	272385.850472	38.559271
2357.663044	272827.603282	38.564288
2360.183520	273278.013864	38.569306
2362.832116	273707.698837	38.574324
2365.340936	274144.062334	38.579341
2367.916406	274556.433930	38.584359
2370.420691	274971.916019	38.589376
2372.462638	275367.865938	38.594394
2375.128331	275769.703397	38.599412
2377.763458	276158.361674	38.604429
2379.850364	276542.184971	38.609447
2382.759644	276951.014881	38.614464
2384.365361	277344.343053	38.619482
2386.671705	277744.307555	38.624500
2388.974103	278159.436773	38.629517
2391.014509	278567.395787	38.634535
2393.417054	278965.131332	38.639552
2395.989999	279387.374846	38.644570
2398.334517	279803.153625	38.649588
2400.514892	280223.277744	38.654605
2402.765900	280650.958399	38.659623
2405.687774	281079.590152	38.664640
2407.877693	281515.966332	38.669658
2410.225606	281943.449317	38.674676
2412.840195	282378.277324	38.679693
2415.061408	282819.775678	38.684711
2417.969385	283237.481629	38.689728
2420.323299	283676.236954	38.694746
2422.754987	284108.678295	38.699764
2425.485772	284537.612743	38.704781
2427.738454	284981.588700	38.709799
2430.030920	285411.255926	38.714816
2432.628484	285856.465652	38.719834
2435.082938	286290.039604	38.724852
2437.816199	286730.346443	38.729869
2440.197077	287173.582335	38.734887
2443.031854	287612.040124	38.739904
2445.290125	288059.993071	38.744922
2447.838714	288494.102611	38.749940
2449.923201	288935.198818	38.754957
2452.129978	289381.047766	38.759975
2454.881969	289839.603424	38.764992
2457.226268	290288.702180	38.770010
2459.489257	290743.172497	38.775028
2462.030387	291207.702554	38.780045
2464.205278	291663.809991	38.785063
2466.364622	292122.661432	38.790080
2468.982071	292593.827554	38.795098
2471.249004	293069.598085	38.800116
2474.062237	293539.710835	38.805133
2476.073081	294013.946380	38.810151
2478.512015	294481.401417	38.815168
2481.722642	294956.723100	38.820186
2483.692934	295427.708349	38.825204
2486.646618	295911.705186	38.830221
2489.279652	296371.676977	38.835239
2492.028152	296828.934766	38.840256
2494.608093	297291.451323	38.845274
2497.483737	297758.791619	38.850292
2500.237000	298215.686722	38.855309
2502.726139	298663.303881	38.860327
2505.573371	299093.612782	38.865344
2507.923278	299516.080746	38.870362
2510.543483	299930.856017	38.875380
2512.827148	300342.842496	38.880397
2514.713647	300767.365067	38.885415
2517.556286	301190.731773	38.890432
2519.897552	301613.953655	38.895450
2521.500839	302053.121933	38.900468
2524.039628	302484.839311	38.905485
2526.623611	302930.565784	38.910503
2528.827314	303387.961184	38.915520
2531.256589	303840.439545	38.920538
2533.517768	304294.975969	38.925556
2536.011597	304761.711109	38.930573
2537.794516	305241.136169	38.935591
2540.042743	305712.860239	38.940608
2542.607606	306215.230797	38.945626
2545.198295	306702.483593	38.950644
2548.256274	307192.040767	38.955661
2550.729240	307690.837220	38.960679
2553.447225	308180.065570	38.965696
2555.996582	308680.874368	38.970714
2559.044104	309170.421176	38.975732
2561.472762	309665.911417	38.980749
2563.792613	310172.285844	38.985767
2566.711778	310655.420394	38.990784
2569.020427	311167.402218	38.995802
2571.515837	311673.812771	39.000820
2575.002419	312167.201270	39.005837
2577.449432	312681.231290	39.010855
2580.221035	313177.325325	39.015872
2582.849560	313677.808027	39.020890
2585.647764	314181.000671	39.025908
2588.492686	314672.551876	39.030925
2591.271404	315182.444413	39.035943
2594.058822	315661.429182	39.040960
2596.488083	316167.870067	39.045978
2598.773391	316663.159323	39.050996
2601.424780	317154.573628	39.056013
2604.076174	317662.235023	39.061031
2606.687461	318167.614190	39.066048
2609.265417	318656.236962	39.071066
2612.223196	319160.025848	39.076084
2614.386041	319661.737706	39.081101
2616.868935	320179.514072	39.086119
2619.584499	320683.104000	39.091136
2622.466974	321193.008996	39.096154
2624.953819	321708.563318	39.101172
2628.000612	322206.625642	39.106189
2630.737934	322716.720798	39.111207
2633.110441	323212.935282	39.116224
2635.764472	323726.184605	39.121242
2638.230312	324225.497793	39.126260
2641.529717	324726.644720	39.131277
2644.097673	325217.071528	39.136295
2647.307180	325685.931438	39.141312
2650.153810	326141.825488	39.146330
2652.452371	326581.205896	39.151348
2655.245853	327030.348894	39.156365
2657.596186	327499.061857	39.161383
2660.145390	327953.875483	39.166400
2662.990098	328420.160793	39.171418
2665.067023	328879.617455	39.176436
2667.880700	329350.800108	39.181453
2670.146707	329820.320730	39.186471
2672.903180	330295.744764	39.191488
2675.318536	330780.336647	39.196506
2677.498439	331258.567250	39.201524
2680.075310	331748.225556	39.206541
2682.404577	332267.902007	39.211559
2685.135321	332762.728864	39.216576
2687.788002	333258.351429	39.221594
2690.241527	333788.298215	39.226612
2693.352407	334289.823642	39.231629
2696.172968	334811.599762	39.236647
2698.521420	335324.287726	39.241664
2701.713547	335844.010041	39.246682
2704.267579	336366.628344	39.251700
2707.159171	336884.081595	39.256717
2709.721594	337415.825676	39.261735
2712.462579	337940.248811	39.266752
2715.462875	338460.687875	39.271770
2717.948976	339008.038322	39.276788
2721.004990	339514.344350	39.281805
2723.768818	340061.635657	39.286823
2726.676784	340591.763810	39.291840
2729.485339	341125.862611	39.296858
2732.797763	341665.605453	39.301876
2735.795888	342179.406309	39.306893
2738.646636	342705.383938	39.311911
2741.779237	343211.105132	39.316928
2744.434784	343728.170992	39.321946
2747.165862	344251.055495	39.326964
2750.280671	344759.859286	39.331981
2753.085736	345274.953604	39.336999
2756.712869	345762.543605	39.342016
2759.824764	346243.973396	39.347034
2762.623442	346738.876585	39.352052
2765.483532	347226.988013	39.357069
2768.388368	347719.146894	39.362087
2770.822739	348210.441802	39.367104
2773.358917	348703.388768	39.372122
2775.573606	349199.760274	39.377140
2778.687166	349705.158814	39.382157
2780.895916	350213.725883	39.387175
2783.123484	350725.100508	39.392192
2785.880893	351244.777823	39.397210
2788.362097	351768.099335	39.402228
2790.865628	352288.923910	39.407245
2793.788299	352799.343080	39.412263
2796.386404	353302.579920	39.417280
2799.175059	353792.939002	39.422298
2801.635054	354290.072517	39.427316
2804.763623	354777.088787	39.432333
2807.077552	355267.689275	39.437351
2809.556627	355774.671852	39.442368
2812.850008	356273.745085	39.447386
2815.070812	356796.413917	39.452404
2817.788078	357311.836375	39.457421
2820.522211	357841.152917	39.462439
2823.340078	358375.420922	39.467456
2825.784746	358903.986415	39.472474
2828.055077	359447.035806	39.477492
2830.419758	359998.383005	39.482509
2833.510879	360561.978765	39.487527
2836.065173	361131.975105	39.492544
2838.618385	361700.923172	39.497562
2841.112949	362285.220884	39.502580
2844.098220	362859.126424	39.507597
2847.281605	363457.900677	39.512615
2849.603594	364055.113100	39.517632
2852.609072	364659.758688	39.522650
2855.381296	365266.844259	39.527668
2858.631200	365865.036330	39.532685
2861.825078	366461.503505	39.537703
2864.540998	367061.441706	39.542720
2868.110254	367660.717046	39.547738
2871.130335	368260.811996	39.552756
2874.488567	368854.878737	39.557773
2877.795004	369463.503344	39.562791
2880.874393	370050.217278	39.567808
2884.028965	370637.720386	39.572826
2887.166722	371224.861628	39.577844
2890.110816	371797.189486	39.582861
2893.223546	372383.529584	39.587879
2895.643905	372973.351238	39.592896
2898.846683	373545.505002	39.597914
2901.789632	374138.717457	39.602932
2904.794706	374722.678143	39.607949
2907.233656	375315.423952	39.612967
2910.568775	375900.145110	39.617984
2913.755884	376485.160479	39.623002
2916.154596	377078.617937	39.628020
2919.340007	377668.329771	39.633037
2922.809382	378251.085574	39.638055
2925.394818	378844.632104	39.643072
2928.504264	379423.904327	39.648090
2931.219818	380008.710596	39.653108
2934.177113	380601.731070	39.658125
2937.088540	381182.933238	39.663143
2939.826644	381775.158547	39.668160
2942.918095	382359.275456	39.673178
2945.926301	382950.748591	39.678196
2948.902326	383541.607883	39.683213
2951.876525	384111.971620	39.688231
2954.732130	384669.770705	39.693248
2958.305705	385208.398115	39.698266
2961.096212	385753.107711	39.703284
2964.049556	386280.820276	39.708301
2966.884106	386831.613235	39.713319
2969.395817	387373.072109	39.718336
2972.380615	387924.732683	39.723354
2975.222208	388471.414106	39.728372
2978.026973	389023.694199	39.733389
2981.453741	389577.455034	39.738407
2983.973565	390147.862201	39.743424
2986.853915	390706.866837	39.748442
2989.710134	391275.750562	39.753460
2992.936823	391842.532565	39.758477
2996.040961	392425.748953	39.763495
2999.127468	392979.809779	39.768512
3002.280400	393553.846107	39.773530
3005.063344	394141.721907	39.778548
3008.273097	394711.772353	39.783565
3011.260754	395290.897304	39.788583
3013.914191	395881.218794	39.793600
3016.628322	396466.120041	39.798618
3019.508885	397063.854765	39.803636
3022.760229	397666.252632	39.808653
3025.890415	398262.019301	39.813671
3028.863594	398870.901352	39.818688
3032.261596	399464.417972	39.823706
3034.926103	400081.359598	39.828724
3038.101390	400686.722109	39.833741
3041.401219	401293.646648	39.838759
3044.340926	401910.703941	39.843776
3047.414539	402519.996948	39.848794
3050.514376	403143.359209	39.853812
3053.358961	403752.765645	39.858829
3056.612708	404363.963544	39.863847
3059.571248	405000.153013	39.868864
3062.354563	405618.269035	39.873882
3065.605980	406252.757904	39.878900
3068.233933	406890.606395	39.883917
3071.627055	407516.681552	39.888935
3074.515268	408170.617364	39.893952
3077.466078	408805.908111	39.898970
3080.769246	409448.165434	39.903988
3083.656904	410090.224904	39.909005
3086.797294	410741.065552	39.914023
3089.502552	411398.524576	39.919040
3093.434608	412040.712682	39.924058
3096.630800	412690.735559	39.929076
3098.991302	413343.316310	39.934093
3102.347135	414003.384423	39.939111
3105.452941	414664.035503	39.944128
3108.227503	415327.866447	39.949146
3111.566073	415982.745664	39.954164
3114.875073	416636.600139	39.959181
3117.913588	417278.177019	39.964199
3120.744385	417910.884959	39.969216
3124.043368	418514.149212	39.974234
3127.077040	419136.232469	39.979252
3130.431102	419744.395223	39.984269
3134.196649	420356.169499	39.989287
3136.861517	420975.636457	39.994304
3140.017283	421575.458102	39.999322
3143.081235	422194.674312	40.004340
3146.459176	422806.631123	40.009357
3149.070865	423426.146553	40.014375
3151.934527	424066.767305	40.019392
3155.170444	424692.877799	40.024410
3158.326507	425322.529724	40.029428
3161.291022	425968.753200	40.034445
3164.779572	426610.515831	40.039463
3167.423935	427257.974146	40.044480
3170.689948	427904.903637	40.049498
3173.606813	428562.961379	40.054516
3176.577254	429234.760495	40.059533
3180.195064	429899.444316	40.064551
3183.321539	430567.888276	40.069568
3186.777371	431231.397597	40.074586
3190.036893	431901.450822	40.079604
3193.378637	432572.077937	40.084621
3196.580001	433240.330712	40.089639
3199.973775	433913.541609	40.094656
3203.075662	434586.073984	40.099674
3206.461445	435269.823513	40.104692
3209.487308	435948.603872	40.109709
3212.804038	436611.323061	40.114727
3215.821622	437308.686385	40.119744
3219.341226	437995.568937	40.124762
3222.354487	438686.362426	40.129780
3225.406856	439380.366071	40.134797
3228.984914	440067.377007	40.139815
3231.677604	440774.907650	40.144832
3234.432230	441472.488588	40.149850
3238.318176	442171.220058	40.154868
3241.639177	442891.931246	40.159885
3245.258100	443594.760419	40.164903
3248.581150	444297.162005	40.169920
3251.765287	444995.062322	40.174938
3255.267780	445696.122942	40.179956
3258.442423	446399.846842	40.184973
3262.118089	447094.306874	40.189991
3265.509092	447792.434473	40.195008
3268.915118	448495.695322	40.200026
3272.344933	449195.034328	40.205044
3274.902712	449910.277963	40.210061
3278.547688	450608.774427	40.215079
3281.730441	451304.848467	40.220096
3285.001409	452007.913137	40.225114
3288.755963	452709.404878	40.230132
3291.546657	453412.756562	40.235149
3295.297692	454096.908294	40.240167
3298.074360	454764.012542	40.245184
3301.239982	455415.000965	40.250202
3304.626740	456070.986620	40.255220
3307.497499	456726.280794	40.260237
3310.944260	457383.376424	40.265255
3313.832274	458062.435713	40.270272
3316.973711	458725.858748	40.275290
3320.725399	459395.322659	40.280308
3323.563062	460079.933047	40.285325
3326.468141	460754.954976	40.290343
3329.969095	461439.961102	40.295360
3332.918974	462145.456977	40.300378
3336.334625	462835.432851	40.305396
3339.481954	463553.530222	40.310413
3342.421395	464264.561380	40.315431
3345.980563	464991.783761	40.320448
3349.225596	465714.939230	40.325466
3352.765869	466433.317700	40.330484
3355.844078	467159.782525	40.335501
3359.460100	467894.313530	40.340519
3362.952761	468629.595231	40.345536
3366.062686	469374.968198	40.350554
3369.802820	470103.885543	40.355572
3373.219539	470846.318910	40.360589
3376.787549	471590.162186	40.365607
3380.264263	472334.597743	40.370624
3383.575666	473089.336787	40.375642
3387.132756	473824.404539	40.380660
3390.223173	474588.061137	40.385677
3394.136734	475338.969115	40.390695
3397.774575	476093.833038	40.395712
3400.989047	476853.586600	40.400730
3404.692139	477598.933140	40.405748
3408.395556	478357.581100	40.410765
3411.842737	479104.273173	40.415783
3415.219805	479856.500941	40.420800
3418.515057	480612.801290	40.425818
3422.211621	481371.929796	40.430836
3425.355885	482128.595982	40.435853
3428.737941	482884.129270	40.440871
3432.491964	483646.988245	40.445888
3435.877061	484419.620560	40.450906
3439.496835	485171.481994	40.455924
3443.000508	485939.029929	40.460941
3446.791328	486685.042877	40.465959
3450.723108	487439.782415	40.470976
3454.235663	488191.330651	40.475994
3458.087043	488936.429336	40.481012
3462.054806	489683.595715	40.486029
3465.343783	490418.733958	40.491047
3469.237383	491149.397707	40.496064
3472.686712	491884.496284	40.501082
3476.572976	492604.754635	40.506100
3479.690265	493341.209540	40.511117
3483.590993	494034.602248	40.516122
3486.693076	494714.662904	40.521127
3489.538213	495341.833640	40.526132
3492.633054	495898.988964	40.531136
3495.749045	496418.644994	40.536141
3498.162816	496864.919171	40.541146
3500.787741	497258.801347	40.546151
3503.006306	497617.342588	40.551156
3504.941814	497912.557793	40.556160
3506.864551	498176.921512	40.561165
3508.724986	498381.416157	40.566170
3510.162303	498563.830854	40.571175
3511.242303	498687.087555	40.576180
3513.012818	498774.422325	40.581184
3513.727138	498841.405884	40.586189
3514.738829	498869.197934	40.591194
3515.802058	498873.061961	40.596199
3516.628409	498840.455498	40.601204
3517.588923	498783.350495	40.606208
3517.769537	498714.899165	40.611213
3518.293993	498612.861028	40.616218
3518.996634	498507.049644	40.621223
3519.018529	498389.065173	40.626228
3519.606178	498241.196951	40.631232
3519.887334	498094.138321	40.636237
3520.113255	497926.049888	40.641242
3520.492269	497754.039538	40.646247
3520.365959	497571.240491	40.651252
3520.851290	497368.307840	40.656256
3520.117957	497180.702515	40.661261
3520.279168	496963.204323	40.666266
3519.819786	496758.200279	40.671271
3519.554762	496571.570248	40.676276
3519.825187	496356.928376	40.681280
3519.699455	496150.747246	40.686285
3519.431417	495948.785856	40.691290
3519.173151	495731.039846	40.696295
3519.049423	495519.539876	40.701300
3519.066287	495299.566401	40.706304
3518.373087	495098.476679	40.711309
3518.255158	494894.504373	40.716314
3518.083392	494678.803826	40.721319
3517.524761	494482.286728	40.726324
3517.685111	494281.749695	40.731328
3517.792492	494081.219332	40.736333
3517.750584	493867.762537	40.741338
3517.380443	493671.102674	40.746343
3517.334581	493473.424041	40.751348
3516.782926	493279.066971	40.756352
3516.411542	493090.494349	40.761357
3516.273687	492890.295318	40.766362
3516.516996	492697.161717	40.771367
3515.892631	492522.942314	40.776372
3515.776066	492332.243674	40.781376
3515.611739	492156.171370	40.786381
3515.361971	491975.154038	40.791386
3515.121485	491799.647553	40.796391
3514.379802	491621.492939	40.801396
3514.528544	491455.832278	40.806400
3514.335753	491295.489883	40.811405
3514.394832	491128.020059	40.816410
3514.179488	490963.681621	40.821415
3513.492375	490804.633271	40.826420
3513.415650	490656.660440	40.831424
3513.451755	490496.271502	40.836429
3513.322032	490344.763446	40.841434
3513.035845	490200.667652	40.846439
3512.904742	490056.797150	40.851444
3512.662557	489908.340188	40.856448
3512.438913	489771.262956	40.861453
3512.155724	489622.304572	40.866458
3512.097336	489490.914330	40.871463
3511.675235	489360.293558	40.876468
3511.477634	489232.365752	40.881472
3511.136342	489111.747683	40.886477
3511.327826	488974.947445	40.891482
3511.157605	488868.820278	40.896487
3510.891694	488748.490403	40.901492
3510.952913	488623.448669	40.906496
3510.646473	488524.730205	40.911501
3510.718858	488405.605188	40.916506
3510.446228	488293.824756	40.921511
3510.218738	488193.572911	40.926516
3510.179391	488083.572928	40.931520
3510.073643	487985.778558	40.936525
3509.703542	487877.503597	40.941530
3509.853437	487775.009024	40.946535
3509.545328	487694.806503	40.951540
3509.805014	487593.304163	40.956544
3509.219408	487501.661327	40.961549
3509.130225	487407.150071	40.966554
3509.014644	487315.122380	40.971559
3508.826254	487226.092256	40.976564
3508.919576	487134.938813	40.981568
3508.851890	487062.333533	40.986573
3508.844472	486978.331666	40.991578
3508.613318	486895.379691	40.996583
3508.257653	486817.104234	41.001588
3508.635092	486735.515127	41.006592
3508.579828	486663.007279	41.011597
3508.528477	486586.854862	41.016602
3508.436875	486499.272073	41.021607
3508.050751	486433.550342	41.026612
3507.923261	486363.482675	41.031616
3507.708050	486291.607875	41.036621
3507.914029	486222.545441	41.041626
3507.907414	486152.658720	41.046631
3507.603257	486093.551211	41.051636
3507.649391	486021.377645	41.056640
3507.594672	485952.611699	41.061645
3507.134035	485893.125374	41.066650
3507.187554	485827.376911	41.071655
3507.078575	485773.953676	41.076660
3507.222735	485718.310909	41.081664
3506.884094	485662.851619	41.086669
3506.807347	485612.458884	41.091674
3507.123070	485549.346855	41.096679
3506.684503	485503.722184	41.101684
3506.861050	485446.959638	41.106688
3506.724876	485399.511754	41.111693
3506.503906	485348.434362	41.116698
3506.709840	485296.727228	41.121703
3506.686966	485250.170563	41.126708
3506.839331	485190.577192	41.131712
3507.069266	485153.390487	41.136717
3506.707299	485102.285848	41.141722
3506.552992	485048.716322	41.146727
3506.262526	485006.708994	41.151732
3506.387295	484956.634246	41.156736
3506.454018	484917.197449	41.161741
3506.439899	484869.119972	41.166746
3506.469466	484824.982535	41.171751
3506.402466	484773.522913	41.176756
3506.427804	484715.569174	41.181760
3506.279654	484683.658965	41.186765
3506.273194	484643.221832	41.191770
3506.525891	484581.331771	41.196775
3505.890643	484551.883228	41.201780
3506.279733	484501.559612	41.206784
3506.041691	484468.196627	41.211789
3505.945807	484431.468929	41.216794
3505.948895	484389.612456	41.221799
3505.801931	484362.104698	41.226804
3505.756143	484311.449900	41.231808
3505.855855	484272.917052	41.236813
3505.655649	484241.267994	41.241818
3505.605765	484206.607080	41.246823
3505.332064	484176.387602	41.251828
3505.215519	484144.217960	41.256832
3505.245604	484117.236329	41.261837
3505.430330	484084.610236	41.266842
3505.470376	484050.692853	41.271847
3505.436606	484021.950529	41.276852
3505.568905	483987.865435	41.281856
3505.491294	483962.268509	41.286861
3505.259327	483938.621202	41.291866
3505.811011	483902.895328	41.296871
3505.178949	483881.998764	41.301876
3505.731924	483846.272555	41.306880
3505.408016	483817.427600	41.311885
3505.499120	483789.979531	41.316890
3505.643000	483746.174180	41.321895
3505.455674	483721.759756	41.326900
3505.411789	483680.618222	41.331904
3505.305825	483669.602516	41.336909
3505.143968	483633.997936	41.341914
3505.619004	483597.626553	41.346919
3505.027247	483578.291787	41.351924
3505.253926	483542.772525	41.356928
3505.310410	483525.047902	41.361933
3505.204498	483498.948995	41.366938
3505.535116	483467.410376	41.371943
3505.195544	483444.033855	41.376948
3505.298363	483406.662730	41.381952
3504.815050	483379.919484	41.386957
3504.726526	483360.093635	41.391962
3504.993479	483340.207067	41.396967
3504.911411	483312.231065	41.401972
3505.162958	483289.917553	41.406976
3505.019579	483267.418370	41.411981
3505.175717	483235.048674	41.416986
3505.055220	483207.888912	41.421991
3504.841635	483185.097921	41.426996
3505.203091	483162.613637	41.432000
3504.771070	483144.921431	41.437005
3504.729101	483125.340448	41.442010
3505.203042	483095.193931	41.447015
3504.791824	483080.231349	41.452020
3504.501649	483055.732339	41.457024
3505.111768	483036.495457	41.462029
3505.350846	483019.700852	41.467034
3505.152403	482993.212076	41.472039
3505.072344	482970.347395	41.477044
3504.922806	482938.586129	41.482048
3505.211075	482915.759719	41.487053
3504.892389	482889.443168	41.492058
3505.251265	482854.557971	41.497063
3504.764582	482841.075945	41.502068
3504.575583	482828.656638	41.507072
3504.825872	482803.356368	41.512077
3504.727678	482791.984476	41.517082
3504.967688	482771.494478	41.522087
3504.654196	482755.249523	41.527092
3504.648181	482727.512697	41.532096
3504.818323	482714.373972	41.537101
3504.818266	482699.138397	41.542106
3505.286749	482667.473589	41.547111
3504.916170	482650.630884	41.552116
3505.173216	482619.660113	41.557120
3504.855703	482596.784880	41.562125
3504.696203	482578.488789	41.567130
3504.907179	482557.952886	41.572135
3505.099160	482543.038708	41.577140
3505.190606	482510.830594	41.582144
3505.154452	482488.312119	41.587149
3504.888295	482457.430402	41.592154
3505.160590	482441.844399	41.597159
3504.922876	482424.624472	41.602164
3505.293884	482388.319004	41.607168
3505.532754	482355.528645	41.612173
3505.130106	482324.973710	41.617178
3504.808686	482296.277714	41.622183
3504.801595	482277.347876	41.627188
3504.997592	482243.299184	41.632192
3504.855573	482223.633059	41.637197
3504.727678	482210.291763	41.642202
3504.807591	482182.185091	41.647207
3504.798391	482164.166621	41.652212
3504.789767	482146.907309	41.657216
3504.940858	482125.773716	41.662221
3504.841347	482104.328559	41.667226
3505.051462	482080.856388	41.672231
3504.872023	482073.851097	41.677236
3504.850500	482038.624313	41.682240
3504.755151	482019.354942	41.687245
3504.540736	481991.298227	41.692250
3504.825073	481966.598384	41.697255
3504.640761	481948.710835	41.702260
3504.797004	481927.272414	41.707264
3504.927035	481919.454938	41.712269
3504.674949	481893.024306	41.717274
3504.725568	481872.768093	41.722279
3504.665793	481856.681472	41.727284
3504.583330	481831.588502	41.732288
3504.633641	481816.039858	41.737293
3504.470159	481793.339771	41.742298
3504.663275	481770.831863	41.747303
3504.311171	481756.009931	41.752308
3504.501911	481743.626267	41.757312
3504.566109	481729.543140	41.762317
3504.405849	481714.030363	41.767322
3504.632160	481696.679882	41.772327
3504.589206	481675.983848	41.777332
3504.448583	481661.378825	41.782336
3504.662339	481644.131676	41.787341
3504.451614	481634.296851	41.792346
3504.586854	481613.367839	41.797351
3504.362401	481606.066332	41.802356
3504.668944	481593.713412	41.807360
3504.554500	481571.409628	41.812365
3504.098273	481550.277815	41.817370
3504.191927	481540.492206	41.822375
3504.376423	481539.853302	41.827380
3504.382181	481509.935918	41.832384
3504.553643	481500.339482	41.837389
3504.611134	481483.371961	41.842394
3504.523882	481470.428134	41.847399
3504.337859	481456.438138	41.852404
3504.387443	481434.814860	41.857408
3504.607646	481431.284499	41.862413
3504.411864	481403.375541	41.867418
3504.820129	481391.511317	41.872423
3504.444992	481370.162963	41.877428
3504.548643	481361.539821	41.882432
3504.727490	481340.754906	41.887437
3504.363511	481328.921259	41.892442
3504.447263	481298.585240	41.897447
3504.400239	481291.557033	41.902452
3504.719155	481267.305910	41.907456
3504.630534	481247.629593	41.912461
3504.714982	481237.440425	41.917466
3504.676164	481217.654331	41.922471
3504.341623	481195.792628	41.927476
3504.358885	481178.781067	41.932480
3504.692185	481161.766149	41.937485
3504.249979	481150.705057	41.942490
3504.685006	481130.584853	41.947495
3504.632705	481108.067397	41.952500
3504.880427	481094.154920	41.957504
3504.542635	481073.306048	41.962509
3504.065472	481064.326345	41.967514
3504.618646	481036.440797	41.972519
3504.186140	481032.211864	41.977524
3504.486142	481013.785091	41.982528
3504.858339	480998.180778	41.987533
3504.595273	480983.494866	41.992538
3504.760362	480964.635486	41.997543
3504.596650	480947.502742	42.002548
3504.681490	480923.999828	42.007552
3504.742322	480899.032950	42.012557
3504.363249	480897.022220	42.017562
3504.568027	480862.716300	42.022567
3504.454263	480846.233016	42.027572
3504.799256	480837.922768	42.032576
3504.948881	480812.485011	42.037581
3504.399583	480793.089345	42.042586
3504.440280	480773.187939	42.047591
3504.337779	480756.601406	42.052596
3504.167274	480737.039755	42.057600
3504.372636	480730.879434	42.062605
3504.461539	480714.918270	42.067610
3504.887612	480690.749319	42.072615
3504.395456	480676.760363	42.077620
3504.608733	480659.259240	42.082624
3504.809482	480634.318727	42.087629
3504.531401	480621.508117	42.092634
3504.692542	480592.322012	42.097639
3504.223753	480587.289205	42.102644
3504.485212	480560.718298	42.107648
3505.031296	480547.817533	42.112653
3504.838105	480530.335066	42.117658
3504.898039	480509.012644	42.122663
3504.808487	480490.095001	42.127668
3504.755508	480461.755212	42.132672
3504.828040	480447.112805	42.137677
3504.856135	480429.997440	42.142682
3504.794049	480409.910691	42.147687
3504.412825	480387.347250	42.152692
3504.294254	480374.559850	42.157696
3504.328204	480347.268127	42.162701
3504.163965	480338.437120	42.167706
3504.485344	480323.499005	42.172711
3504.230023	480310.127428	42.177716
3504.288867	480282.628863	42.182720
3504.335754	480283.683989	42.187725
3503.994972	480264.758382	42.192730
3504.116176	480248.133182	42.197735
3504.512236	480244.319445	42.202740
3504.444563	480225.195292	42.207744
3504.719072	480216.036191	42.212749
3504.140410	480185.355789	42.217754
3504.436598	480173.358031	42.222759
3504.218236	480161.397501	42.227764
3504.326454	480144.875671	42.232768
3504.409767	480130.534909	42.237773
3504.413699	480116.106443	42.242778
3504.658094	480107.559917	42.247783
3504.553059	480082.417733	42.252788
3504.598999	480058.160970	42.257792
3504.433772	480028.320941	42.262797
3504.245387	480030.631236	42.267802
3504.400012	480017.189444	42.272807
3504.639169	480006.466921	42.277812
3504.437893	479975.468601	42.282816
3504.461618	479963.669101	42.287821
3504.335856	479948.402029	42.292826
3504.371847	479926.171767	42.297831
3504.095102	479928.952783	42.302836
3504.585545	479917.174810	42.307840
3504.539665	479890.149149	42.312845
3504.208466	479883.776409	42.317850
3504.691503	479852.559783	42.322855
3504.365730	479855.906054	42.327860
3504.048537	479833.533484	42.332864
3504.375726	479816.315843	42.337869
3504.152585	479811.595246	42.342874
3504.053258	479776.174813	42.347879
3504.179988	479769.116343	42.352884
3504.437011	479767.857495	42.357888
3504.513616	479750.631953	42.362893
3504.214451	479741.064316	42.367898
3504.181570	479720.111186	42.372903
3504.084846	479704.231449	42.377908
3504.312149	479701.357666	42.382912
3504.148198	479685.894393	42.387917
3504.119853	479662.307910	42.392922
3504.140887	479649.040531	42.397927
3503.926303	479651.254097	42.402932
3504.148700	479637.547324	42.407936
3504.339722	479619.188363	42.412941
3504.143985	479621.550591	42.417946
3504.258533	479595.762731	42.422951
3504.164011	479580.135636	42.427956
3503.985989	479574.901018	42.432960
3504.198942	479564.739589	42.437965
3504.291364	479556.168127	42.442970
3504.234286	479537.952698	42.447975
3503.829198	479532.959341	42.452980
3503.699617	479522.501996	42.457984
3504.179692	479504.903574	42.462989
3503.857848	479510.780522	42.467994
3504.206063	479483.231330	42.472999
3504.006146	479486.708056	42.478004
3503.939048	479477.151279	42.483008
3504.091786	479463.304392	42.488013
3504.029622	479454.101141	42.493018
3503.899347	479446.327041	42.498023
3503.887341	479441.367792	42.503028
3503.835121	479433.732235	42.508032
3504.153528	479411.554370	42.513037
3503.573365	479414.792280	42.518042
3504.004128	479412.541849	42.523047
3504.240976	479405.970694	42.528052
3504.086503	479383.974790	42.533056
3504.263507	479369.566802	42.538061
3504.026083	479369.202371	42.543066
3504.043748	479342.772554	42.548071
3503.976837	479349.567921	42.553076
3504.211012	479341.174658	42.558080
3504.291616	479319.847304	42.563085
3503.800778	479304.844530	42.568090
3504.190426	479301.284823	42.573095
3504.013822	479300.099985	42.578100
3504.225516	479286.951664	42.583104
3504.333314	479277.263666	42.588109
3504.254575	479273.277667	42.593114
3504.604814	479248.208464	42.598119
3504.189806	479245.849295	42.603124
3504.026744	479219.905796	42.608128
3504.311194	479204.163040	42.613133
3504.137971	479205.357066	42.618138
3504.325066	479164.570741	42.623143
3504.193639	479164.086953	42.628148
3504.234049	479153.752249	42.633152
3504.495455	479133.456964	42.638157
3504.470561	479129.107352	42.643162
3504.571435	479102.511097	42.648167
3504.735433	479083.346179	42.653172
3504.496704	479065.060037	42.658176
3504.717261	479048.923041	42.663181
3504.484730	479038.533621	42.668186
3504.612547	479012.540158	42.673191
3504.344684	478997.296547	42.678196
3504.075820	478980.635533	42.683200
3504.123085	478962.199199	42.688205
3503.909958	478956.008478	42.693210
3504.190589	478933.330206	42.698215
3503.711778	478932.399454	42.703220
3503.900476	478934.848010	42.708224
3504.072757	478912.593232	42.713229
3503.867866	478908.274300	42.718234
3503.884991	478895.057664	42.723239
3503.978195	478894.434258	42.728244
3503.995113	478876.964941	42.733248
3504.005015	478858.382999	42.738253
3503.999407	478863.953020	42.743258
3504.130458	478857.197222	42.748263
3504.126299	478835.782517	42.753268
3503.782659	478830.322824	42.758272
3503.965687	478825.380732	42.763277
3503.925621	478818.249117	42.768282
3503.747384	478796.054046	42.773287
3503.915960	478792.785128	42.778292
3503.963442	478788.372448	42.783296
3503.824640	478783.080275	42.788301
3503.405715	478773.937595	42.793306
3503.893251	478748.945516	42.798311
3503.731761	478757.478600	42.803316
3503.733901	478763.705490	42.808321
3503.999849	478748.269266	42.813325
3503.732061	478760.313818	42.818330
3503.987373	478748.271472	42.823335
3504.184197	478734.821524	42.828340
3504.030001	478728.063756	42.833345
3504.282454	478723.616062	42.838349
3503.727549	478709.788173	42.843354
3504.459206	478699.487065	42.848359
3504.560175	478682.205720	42.853364
3504.090878	478676.969948	42.858369
3503.927530	478657.657963	42.863373
3503.881212	478654.780109	42.868378
3504.285479	478623.524192	42.873383
3504.015769	478630.000059	42.878388
3504.076411	478620.977929	42.883393
3504.175402	478602.127372	42.888397
3504.005671	478586.613518	42.893402
3504.199572	478583.137724	42.898407
3503.932695	478566.729131	42.903412
3503.999310	478558.769145	42.908417
3504.087021	478548.527277	42.913421
3503.934363	478553.464333	42.918426
3504.290190	478521.558343	42.923431
3504.096664	478511.111332	42.928436
3504.261869	478509.361793	42.933441
3504.210948	478486.385177	42.938445
3504.182428	478476.112485	42.943450
3504.080886	478468.839344	42.948455
3504.055542	478444.946994	42.953460
3503.764346	478429.504374	42.958465
3504.254135	478430.129583	42.963469
3504.312283	478419.993947	42.968474
3504.595704	478410.376757	42.973479
3504.369574	478395.834316	42.978484
3504.084680	478370.517951	42.983489
3504.495610	478361.132107	42.988493
3503.951541	478349.479135	42.993498
3503.878592	478329.543818	42.998503
3504.117561	478325.300845	43.003508
3503.716514	478320.711493	43.008513
3503.923130	478306.449492	43.013517
3503.811870	478295.633907	43.018522
3504.106598	478280.951809	43.023527
3503.874419	478284.383642	43.028532
3504.125386	478284.796490	43.033537
3504.247075	478256.018390	43.038541
3503.849007	478257.352127	43.043546
3504.010556	478252.008515	43.048551
3504.097645	478234.881003	43.053556
3504.011662	478217.732397	43.058561
3504.272104	478206.397627	43.063565
3504.061650	478202.028847	43.068570
3503.603443	478181.298451	43.073575
3503.646106	478176.683928	43.078580
3503.705528	478177.990184	43.083585
3504.031789	478174.896749	43.088589
3503.887728	478165.504310	43.093594
3504.005146	478144.827473	43.098599
3504.249733	478137.292580	43.103604
3503.697742	478132.425176	43.108609
3504.104779	478131.545640	43.113613
3503.933789	478127.727028	43.118618
3503.863863	478120.498979	43.123623
3503.986292	478123.870293	43.128628
3503.640427	478111.018844	43.133633
3504.326177	478088.726013	43.138637
3504.431655	478082.227444	43.143642
3504.047847	478072.065818	43.148647
3503.901524	478050.117535	43.153652
3503.828223	478050.940165	43.158657
3504.110934	478040.765975	43.163661
3503.934280	478048.137494	43.168666
3504.228584	478021.050962	43.173671
3504.381650	478002.139921	43.178676
3504.273826	478001.449551	43.183681
3504.240324	477970.672303	43.188685
3504.031599	477970.859870	43.193690
3504.468514	477961.570645	43.198695
3504.292531	477939.222253	43.203700
3504.110219	477931.355127	43.208705
3504.214274	477910.376525	43.213709
3504.267162	477896.140453	43.218714
3504.109632	477893.129577	43.223719
3503.894217	477864.965352	43.228724
3503.636379	477855.085878	43.233729
3504.307175	477838.162108	43.238733
3503.952912	477848.146182	43.243738
3503.994805	477836.544718	43.248743
3503.885570	477819.399708	43.253748
3503.659605	477822.223001	43.258753
3504.060277	477810.762781	43.263757
3503.763071	477806.712501	43.268762
3504.122243	477786.044609	43.273767
3504.150213	477767.812881	43.278772
3503.977648	477767.032296	43.283777
3504.721088	477755.513514	43.288781
3504.276523	477746.729106	43.293786
3504.458808	477727.255855	43.298791
3504.545785	477712.254359	43.303796
3504.160680	477697.535981	43.308801
3504.197374	477674.239596	43.313805
3503.990440	477668.452423	43.318810
3504.168871	477650.903720	43.323815
3504.126318	477630.253615	43.328820
3503.773034	477631.579748	43.333825
3504.105768	477611.827530	43.338829
3504.064640	477610.872602	43.343834
3503.968003	477597.471924	43.348839
3504.005972	477585.617815	43.353844
3503.932537	477586.643013	43.358849
3503.967418	477573.270492	43.363853
3503.855889	477554.707954	43.368858
3503.955396	477549.425361	43.373863
3504.237465	477541.529405	43.378868
3503.833793	477541.243951	43.383873
3503.840037	477513.851434	43.388877
3503.976092	477520.714090	43.393882
3503.589855	477512.932234	43.398887
3503.893270	477510.855214	43.403892
3503.861900	477495.114278	43.408897
3504.122408	477472.589520	43.413901
3503.778968	477481.508688	43.418906
3503.960138	477479.705694	43.423911
3503.738937	477463.895882	43.428916
3503.427894	477449.822865	43.433921
3504.098025	477447.278170	43.438925
3504.060897	477453.309688	43.443930
3503.705352	477445.016248	43.448935
3504.131955	477439.930930	43.453940
3503.863321	477418.357190	43.458945
3503.970564	477401.681139	43.463949
3504.153594	477401.953714	43.468954
3503.746889	477385.061614	43.473959
3503.772007	477373.108298	43.478964
3503.738174	477370.886321	43.483969
3504.012055	477366.586534	43.488973
3503.994896	477367.804662	43.493978
3503.882663	477345.090234	43.498983
3503.761804	477333.161817	43.503988
3503.823693	477329.100747	43.508993
3503.834011	477330.111658	43.513997
3503.539589	477325.757004	43.519002
3503.708476	477306.032433	43.524007
3503.803293	477295.788648	43.529012
3503.671159	477288.874682	43.534017
3503.923772	477293.641614	43.539021
3503.870415	477296.536778	43.544026
3503.911334	477275.973284	43.549031
3504.049368	477261.570283	43.554036
3503.894873	477252.331051	43.559041
3503.855641	477252.742843	43.564045
3504.036921	477260.559883	43.569050
3503.849261	477235.681023	43.574055
3503.742502	477220.003355	43.579060
3503.604504	477227.520501	43.584065
3503.752592	477221.368774	43.589069
3504.043152	477219.850869	43.594074
3503.956890	477193.992630	43.599079
3503.690474	477184.063623	43.604084
3503.541601	477184.899195	43.609089
3504.188752	477169.548444	43.614093
3503.682685	477171.103227	43.619098
3504.047619	477144.965348	43.624103
3504.306391	477133.225141	43.629108
3504.112156	477145.055669	43.634113
3504.166046	477121.148055	43.639117
3503.849321	477101.658078	43.644122
3503.872209	477099.932706	43.649127
3504.062040	477095.444679	43.654132
3503.741645	477091.955154	43.659137
3504.013420	477062.795120	43.664141
3503.854729	477074.265196	43.669146
3504.031907	477064.159116	43.674151
3504.188327	477052.233804	43.679156
3503.903640	477042.915431	43.684161
3504.124837	477030.371453	43.689165
3503.994015	477031.254582	43.694170
3504.159576	476999.935382	43.699175
3504.249998	477001.894655	43.704180
3503.752810	477003.042873	43.709185
3503.865260	476973.909902	43.714189
3503.818834	476961.411573	43.719194
3504.018199	476952.263666	43.724199
3504.195500	476957.954937	43.729204
3503.821970	476946.575739	43.734209
3503.750870	476933.625909	43.739213
3504.008150	476930.341513	43.744218
3504.158697	476923.075344	43.749223
3504.137073	476920.294264	43.754228
3504.183158	476902.666176	43.759233
3504.416288	476883.132712	43.764237
3503.986895	476868.978189	43.769242
3503.817950	476855.538681	43.774247
3503.884974	476842.717101	43.779252
3503.966155	476853.133696	43.784257
3503.971514	476838.499851	43.789261
3503.895568	476829.955857	43.794266
3503.646759	476819.770479	43.799271
3503.934647	476810.556753	43.804276
3503.573791	476815.529827	43.809281
3504.003856	476799.000638	43.814285
3504.139571	476784.850825	43.819290
3503.824237	476788.043968	43.824295
3503.888911	476777.805041	43.829300
3503.639851	476776.480506	43.834305
3504.029526	476753.629010	43.839309
3503.720100	476752.112248	43.844314
3503.702573	476739.862000	43.849319
3504.014593	476733.226418	43.854324
3503.811495	476739.894111	43.859329
3504.182409	476716.438171	43.864333
3503.665816	476700.019900	43.869338
3503.698663	476700.166230	43.874343
3504.175103	476703.072293	43.879348
3503.832149	476682.877479	43.884353
3503.675731	476662.853326	43.889357
3503.762104	476660.509470	43.894362
3503.885794	476663.273236	43.899367
3504.131302	476665.104798	43.904372
3503.599467	476649.600489	43.909377
3504.026990	476628.767721	43.914381
3503.560119	476634.214648	43.919386
3503.616999	476631.217586	43.924391
3503.887891	476631.120735	43.929396
3503.763756	476630.028028	43.934401
3503.980833	476599.914557	43.939405
3503.498348	476596.401979	43.944410
3503.821303	476594.726592	43.949415
3504.133333	476594.926520	43.954420
3503.739379	476587.094951	43.959425
3503.918580	476562.506971	43.964429
3503.858874	476555.124655	43.969434
3503.953822	476553.488195	43.974439
3504.120829	476543.788637	43.979444
3503.998256	476530.543507	43.984449
3503.874877	476519.171964	43.989453
3503.783121	476509.465937	43.994458
3503.565885	476515.376615	43.999463
3503.849716	476503.176020	44.004468
3503.672536	476481.990632	44.009473
3503.806296	476476.347443	44.014477
3503.889553	476477.092777	44.019482
3503.814478	476475.384073	44.024487
3504.146807	476470.922197	44.029492
3503.718661	476447.703621	44.034497
3503.788339	476437.058575	44.039501
3503.803843	476440.650996	44.044506
3503.928755	476424.274844	44.049511
3504.161082	476422.918721	44.054516
3503.898572	476410.659450	44.059521
3504.005132	476394.691479	44.064525
3503.742281	476398.280803	44.069530
3503.935175	476391.108461	44.074535
3503.930490	476372.121404	44.079540
3503.623284	476370.502961	44.084545
3503.921069	476359.667018	44.089549
3503.871387	476362.865509	44.094554
3503.517375	476361.710767	44.099559
3503.735011	476337.926076	44.104564
3503.650841	476325.535027	44.109569
3503.772547	476319.235600	44.114573
3503.673034	476318.999456	44.119578
3503.929709	476314.347922	44.124583
3504.396014	476308.799804	44.129588
3503.784092	476294.929176	44.134593
3503.624907	476280.728059	44.139597
3503.829679	476278.718380	44.144602
3503.678898	476280.161934	44.149607
3503.941432	476270.547190	44.154612
3503.704668	476254.182008	44.159617
3504.066502	476242.524904	44.164621
3503.658022	476240.721203	44.169626
3503.512825	476238.923181	44.174631
3503.913176	476239.361207	44.179636
3503.510812	476217.201267	44.184641
3503.837093	476199.068946	44.189645
3503.282467	476198.201622	44.194650
3503.521186	476208.034700	44.199655
3504.264416	476194.540223	44.204660
3503.604786	476199.463207	44.209665
3503.851591	476194.762693	44.214669
3503.759477	476178.423379	44.219674
3503.511099	476171.174393	44.224679
3503.737093	476167.996475	44.229684
3503.469755	476168.599145	44.234689
3503.833807	476165.650827	44.239693
3503.986461	476160.409396	44.244698
3503.545382	476153.851562	44.249703
3504.161744	476135.568377	44.254708
3503.525493	476141.601356	44.259713
3503.835803	476127.117414	44.264717
3503.573234	476133.542305	44.269722
3503.758242	476132.447417	44.274727
3503.862956	476117.644127	44.279732
3503.730678	476112.907050	44.284737
3504.008600	476100.200847	44.289741
3503.786959	476097.453796	44.294746
3503.692343	476095.343312	44.299751
3504.007877	476079.795102	44.304756
3503.618527	476075.101910	44.309761
3503.826286	476060.736697	44.314765
3503.895038	476055.408291	44.319770
3504.162641	476054.096754	44.324775
3504.370426	476029.908264	44.329780
3503.770792	476030.365136	44.334785
3503.715954	476023.437493	44.339789
3503.856934	476015.007985	44.344794
3503.628620	475992.362335	44.349799
3503.907766	475982.693969	44.354804
3503.656680	475985.420561	44.359809
3503.722264	475972.497348	44.364813
3503.882233	475984.875768	44.369818
3503.707988	475971.639058	44.374823
3503.860688	475947.409230	44.379828
3503.626030	475941.879420	44.384833
3503.905553	475938.489780	44.389837
3503.723731	475940.647559	44.394842
3503.670623	475943.492259	44.399847
3503.891443	475910.642698	44.404852
3503.863090	475903.052223	44.409857
3503.899880	475903.096614	44.414861
3503.841077	475905.435935	44.419866
3503.725341	475898.468007	44.424871
3503.782353	475876.026673	44.429876
3503.567408	475878.139480	44.434881
3503.566923	475868.771980	44.439885
3503.774378	475866.609891	44.444890
3503.780472	475878.913385	44.449895
3504.095993	475871.213545	44.454900
3503.654334	475845.312816	44.459905
3503.928239	475831.189309	44.464909
3503.496679	475836.630440	44.469914
3503.799577	475835.009046	44.474919
3503.798140	475829.692560	44.479924
3503.726713	475832.894855	44.484929
3503.927727	475819.290145	44.489933
3503.964801	475810.422561	44.494938
3503.479656	475806.049472	44.499943
3503.722633	475801.602692	44.504948
3503.784780	475801.389574	44.509953
3503.682442	475791.735611	44.514957
3503.563178	475776.413295	44.519962
3503.856536	475757.931709	44.524967
3504.334387	475754.457535	44.529972
3503.797385	475755.916441	44.534977
3503.645534	475747.891264	44.539981
3503.821650	475735.151556	44.544986
3503.632520	475735.335797	44.549991
3503.851936	475729.728390	44.554996
3503.506912	475729.635432	44.560001
3503.665270	475728.798251	44.565005
3503.734343	475730.811942	44.570010
3503.438313	475710.304227	44.575015
3504.228356	475683.939777	44.580020
3503.984173	475686.969051	44.585025
3503.619947	475682.372740	44.590029
3503.743163	475692.377726	44.595034
3503.970659	475678.768389	44.600039
3504.144629	475659.496910	44.605044
3503.625829	475658.167714	44.610049
3503.769925	475654.801146	44.615053
3503.786517	475653.481805	44.620058
3503.707508	475639.469048	44.625063
3503.974663	475618.611885	44.630068
3503.709947	475615.568296	44.635073
3503.973146	475616.688033	44.640077
3503.975799	475614.307702	44.645082
3503.855450	475603.238893	44.650087
3504.193858	475576.191858	44.655092
3503.712387	475586.148241	44.660097
3503.535579	475580.709718	44.665101
3503.619334	475581.353730	44.670106
3503.515803	475563.395448	44.675111
3503.974341	475540.581326	44.680116
3503.973150	475546.961791	44.685121
3503.913810	475547.832784	44.690125
3503.912865	475537.857554	44.695130
3503.653726	475518.862428	44.700135
3503.957943	475509.695901	44.705140
3503.947052	475504.026478	44.710145
3503.793102	475500.812047	44.715149
3503.930347	475496.737705	44.720154
3503.485558	475473.622011	44.725159
3503.667156	475466.603150	44.730164
3503.561238	475463.026052	44.735169
3503.700293	475460.774322	44.740173
3503.859431	475456.797507	44.745178
3503.425224	475467.556075	44.750183
3503.885072	475455.476644	44.755188
3504.070878	475442.735081	44.760193
3503.872022	475429.603456	44.765197
3503.712047	475428.668707	44.770202
3503.513587	475432.551043	44.775207
3503.345762	475428.832599	44.780212
3503.494558	475437.263608	44.785217
3503.767135	475432.001494	44.790221
3503.736480	475405.067862	44.795226
3503.883604	475393.851982	44.800231
3504.059731	475385.011088	44.805236
3503.912406	475398.505753	44.810241
3503.953600	475379.155378	44.815245
3504.150434	475355.575519	44.820250
3503.774674	475363.235297	44.825255
3503.784707	475350.979418	44.830260
3503.761171	475349.464358	44.835265
3503.471317	475334.930361	44.840269
3503.847521	475321.396645	44.845274
3503.559930	475310.609403	44.850279
3503.772162	475307.079226	44.855284
3503.359702	475314.897202	44.860289
3503.761586	475310.726995	44.865293
3504.070582	475311.281921	44.870298
3503.837538	475296.130545	44.875303
3503.655646	475273.931821	44.880308
3503.827052	475270.611157	44.885313
3503.702286	475272.759271	44.890317
3503.820816	475274.207556	44.895322
3503.663743	475253.219867	44.900327
3503.922221	475237.680692	44.905332
3503.709178	475245.717835	44.910337
3503.694887	475240.960386	44.915341
3503.767314	475235.934942	44.920346
3503.330811	475240.060514	44.925351
3503.833200	475229.087698	44.930356
3503.607160	475217.023952	44.935361
3503.653514	475198.989085	44.940365
3503.921766	475194.082105	44.945370
3503.629723	475202.436582	44.950375
3503.817060	475193.897508	44.955380
3503.538551	475201.642023	44.960385
3503.773813	475185.397840	44.965389
3503.784975	475158.709898	44.970394
3503.771893	475167.776324	44.975399
3503.726985	475159.175615	44.980404
3503.760199	475161.701868	44.985409
3503.694598	475157.054435	44.990413
3503.648532	475137.161690	44.995418
3503.537581	475130.445843	45.000423
3503.867870	475129.072901	45.005428
3503.695354	475131.482373	45.010433
3503.835298	475124.622408	45.015437
3504.295383	475128.493638	45.020442
3503.753226	475119.825902	45.025447
3504.245122	475090.827710	45.030452
3504.238109	475090.373204	45.035457
3504.078014	475081.792127	45.040461
3504.058549	475061.388379	45.045466
3503.615501	475054.881124	45.050471
3504.187000	475049.770412	45.055476
3503.834387	475030.841381	45.060481
3503.596604	475013.411867	45.065485
3503.560415	475006.278104	45.070490
3503.372477	475006.614061	45.075495
3503.590563	475004.652610	45.080500
3503.500824	475006.896050	45.085505
3503.504392	475012.263124	45.090509
3503.758626	475011.308264	45.095514
3503.342736	475008.341026	45.100519
3503.760768	475001.230979	45.105524
3503.648680	474988.084224	45.110529
3503.551621	474979.239144	45.115533
3503.467330	474973.227623	45.120538
3503.235452	474985.015326	45.125543
3503.550405	474983.391801	45.130548
3503.787174	474981.173966	45.135553
3503.332173	474976.795530	45.140557
3503.447294	474980.472502	45.145562
3503.230327	474983.041499	45.150567
3503.776655	474982.796337	45.155572
3503.620990	474984.139548	45.160577
3503.338551	474964.894637	45.165581
3503.556778	474950.324221	45.170586
3503.255537	474945.868884	45.175591
3503.364215	474932.886947	45.180596
3503.597586	474933.859905	45.185601
3503.441871	474940.823986	45.190605
3503.419633	474943.866121	45.195610
3503.720644	474941.839866	45.200615
3504.011023	474928.523071	45.205620
3503.721071	474944.473063	45.210625
3503.715271	474943.157494	45.215629
3503.971185	474924.327001	45.220634
3503.870612	474910.368010	45.225639
3503.862449	474919.484357	45.230644
3503.793313	474907.798724	45.235649
3503.807121	474906.783635	45.240653
3503.965251	474874.651874	45.245658
3503.654679	474876.831760	45.250663
3503.961973	474865.284379	45.255668
3503.768870	474870.836991	45.260673
3503.675296	474863.561055	45.265677
3503.913050	474846.151463	45.270682
3503.523479	474839.837554	45.275687
3503.672873	474833.988640	45.280692
3503.771411	474841.263816	45.285697
3503.584613	474839.219565	45.290701
3503.475234	474841.213186	45.295706
3503.535900	474853.356130	45.300711
3503.835394	474822.314188	45.305716
3503.960692	474807.962082	45.310721
3503.669494	474807.859926	45.315725
3503.923933	474791.915956	45.320730
3503.878569	474793.139070	45.325735
3503.737536	474773.616621	45.330740
3503.771379	474759.533287	45.335745
3503.758197	474757.661938	45.340749
3503.636255	474749.985691	45.345754
3503.499094	474753.300675	45.350759
3504.102611	474752.843191	45.355764
3503.518401	474730.915064	45.360769
3503.587096	474718.496832	45.365773
3503.769365	474712.743545	45.370778
3503.887165	474719.863562	45.375783
3503.926079	474716.362867	45.380788
3503.704315	474720.654443	45.385793
3503.942861	474698.130042	45.390797
3504.113770	474683.820691	45.395802
3503.763025	474687.830464	45.400807
3503.846702	474673.586638	45.405812
3503.528354	474663.411937	45.410817
3503.474099	474644.836677	45.415821
3503.698377	474640.342173	45.420826
3503.604330	474637.370558	45.425831
3503.744909	474629.548157	45.430836
3504.050958	474635.218166	45.435841
3504.368850	474629.796170	45.440845
3504.414762	474610.798660	45.445850
3504.100780	474607.054365	45.450855
3504.235954	474589.155655	45.455860
3503.769272	474568.878365	45.460865
3503.311329	474563.740740	45.465869
3503.615238	474561.562032	45.470874
3503.510795	474566.188087	45.475879
3503.797561	474556.061922	45.480884
3503.737519	474557.996509	45.485889
3503.789453	474548.467470	45.490893
3504.383110	474532.617275	45.495898
3503.652875	474524.487765	45.500903
3503.844491	474528.708801	45.505908
3503.621971	474507.073126	45.510913
3503.752484	474495.910178	45.515917
3504.058793	474488.464536	45.520922
3503.997718	474494.247914	45.525927
3503.795742	474490.737669	45.530932
3503.620229	474468.334329	45.535937
3504.016937	474457.328464	45.540941
3504.234860	474452.024765	45.545946
3503.917845	474451.572536	45.550951
3503.919166	474436.532355	45.555956
3504.075108	474421.415122	45.560961
3503.710625	474412.969912	45.565965
3503.862245	474411.576786	45.570970
3503.711674	474419.552980	45.575975
3503.674074	474393.682496	45.580980
3504.012472	474393.067714	45.585985
3503.941669	474386.192821	45.590989
3504.037584	474374.934428	45.595994
3503.795878	474371.279024	45.600999
3504.109178	474349.652954	45.606004
3503.708346	474340.504958	45.611009
3503.933676	474334.744201	45.616013
3504.212530	474329.430064	45.621018
3504.083388	474318.311345	45.626023
3504.226619	474293.422645	45.631028
3504.109631	474290.961293	45.636033
3504.039315	474268.995510	45.641037
3504.357275	474257.597852	45.646042
3503.945555	474260.706603	45.651047
3503.938380	474231.792285	45.656052
3503.868376	474221.423014	45.661057
3503.786139	474215.562817	45.666061
3503.968903	474215.582288	45.671066
3503.754000	474205.237750	45.676071
3503.808686	474181.427466	45.681076
3503.645496	474183.734187	45.686081
3503.579417	474178.833387	45.691085
3504.036742	474173.184889	45.696090
3503.814097	474180.768368	45.701095
3503.643120	474158.667721	45.706100
3503.607424	474143.937467	45.711105
3503.538641	474145.417824	45.716109
3503.562377	474137.513886	45.721114
3503.634756	474143.325227	45.726119
3504.002548	474137.641365	45.731124
3503.868232	474135.993199	45.736129
3503.729461	474115.001093	45.741133
3503.901770	474099.222474	45.746138
3503.776514	474100.155431	45.751143
3503.857807	474102.572339	45.756148
3503.785052	474092.456669	45.761153
3503.717284	474079.352341	45.766157
3503.361616	474064.727299	45.771162
3503.287088	474063.170200	45.776167
3503.637383	474061.489921	45.781172
3503.482686	474064.301614	45.786177
3503.548432	474068.746811	45.791181
3503.679392	474060.166202	45.796186
3503.730792	474062.537578	45.801191
3503.832094	474061.710067	45.806196
3503.857521	474039.828946	45.811201
3503.775787	474027.334656	45.816205
3503.509958	474016.846785	45.821210
3503.497737	474025.913623	45.826215
3503.715493	474020.863035	45.831220
3503.432893	474020.455559	45.836225
3503.356974	474024.266624	45.841229
3503.615235	474022.753979	45.846234
3503.717986	474028.864015	45.851239
3503.660184	473997.071448	45.856244
3503.800025	473985.146986	45.861249
3503.802136	473984.893459	45.866253
3504.004367	473983.795505	45.871258
3503.774000	473983.834878	45.876263
3503.685271	473963.998798	45.881268
3503.826556	473954.454198	45.886273
3503.621885	473953.071234	45.891277
3503.629443	473947.499466	45.896282
3503.468507	473938.563513	45.901287
3503.882163	473940.366640	45.906292
3504.026493	473936.645234	45.911297
3503.713140	473919.227591	45.916301
3503.538159	473915.915192	45.921306
3503.507208	473922.048092	45.926311
3503.800115	473917.946826	45.931316
3503.680467	473911.687790	45.936321
3503.459385	473910.054419	45.941325
3503.767054	473907.723070	45.946330
3503.720818	473888.740554	45.951335
3503.739510	473879.672620	45.956340
3503.633107	473874.221570	45.961345
3503.642623	473876.448199	45.966349
3503.161696	473870.909174	45.971354
3503.432582	473876.686703	45.976359
3503.570916	473875.852861	45.981364
3503.940667	473883.183386	45.986369
3503.752132	473861.591795	45.991373
3503.990759	473842.206102	45.996378
3503.958645	473840.641742	46.001383
3503.961376	473839.122073	46.006388
3504.217046	473838.926531	46.011393
3503.912367	473813.911103	46.016397
3503.983659	473796.579592	46.021402
3503.842913	473798.477397	46.026407
3503.920942	473781.701778	46.031412
3504.082181	473758.885589	46.036417
3503.733269	473766.642721	46.041421
3504.100325	473762.072986	46.046426
3504.199383	473746.053367	46.051431
3503.568549	473722.359547	46.056436
3503.625613	473724.628717	46.061441
3503.622897	473717.336816	46.066445
3503.582513	473713.950756	46.071450
3503.539942	473721.706241	46.076455
3503.183430	473715.538226	46.081460
3503.672692	473719.556699	46.086465
3503.585554	473705.138731	46.091469
3503.742089	473682.272609	46.096474
3503.474789	473676.950258	46.101479
3503.317228	473676.926558	46.106484
3503.615581	473670.444142	46.111489
3503.333695	473678.088583	46.116493
3503.562417	473680.885507	46.121498
3503.362808	473683.249150	46.126503
3503.195487	473675.833414	46.131508
3503.342548	473683.303327	46.136513
3503.406349	473677.975083	46.141517
3503.547250	473679.774166	46.146522
3503.499618	473683.783039	46.151527
3503.576005	473681.237944	46.156532
3503.582502	473684.123454	46.161537
3503.650503	473682.541986	46.166541
3503.540536	473647.263443	46.171546
3503.232927	473652.785327	46.176551
3503.376537	473647.544731	46.181556
3503.574400	473651.106557	46.186561
3503.605712	473644.771013	46.191565
3503.593565	473644.266706	46.196570
3503.856361	473645.994338	46.201575
3503.604960	473648.873247	46.206580
3503.660848	473648.357324	46.211585
3503.216268	473649.395469	46.216589
3503.956037	473634.937536	46.221594
3503.432221	473625.556974	46.226599
3503.545478	473619.663208	46.231604
3503.775574	473611.571884	46.236609
3503.792830	473609.897790	46.241613
3503.946630	473606.833048	46.246618
3503.566625	473615.709675	46.251623
3503.703572	473592.188442	46.256628
3503.728034	473579.270581	46.261633
3503.436226	473576.180637	46.266637
3503.854049	473570.690629	46.271642
3503.438170	473571.622593	46.276647
3503.517785	473572.014173	46.281652
3503.783172	473564.271298	46.286657
3503.874627	473570.535340	46.291661
3503.809626	473543.452940	46.296666
3503.866988	473540.050158	46.301671
3503.776646	473529.835900	46.306676
3503.700850	473532.482274	46.311681
3503.673090	473531.170355	46.316685
3504.056774	473512.823037	46.321690
3503.836699	473509.011841	46.326695
3503.854071	473496.398987	46.331700
3503.960409	473498.052063	46.336705
3503.684278	473493.389517	46.341709
3503.713785	473459.454145	46.346714
3503.598409	473448.028699	46.351719
3503.622444	473464.787267	46.356724
3503.586189	473449.600776	46.361729
3503.811951	473457.209269	46.366733
3503.856262	473454.011269	46.371738
3503.530383	473443.178830	46.376743
3503.814748	473419.075141	46.381748
3503.815309	473414.973040	46.386753
3503.512826	473418.924199	46.391757
3503.402790	473411.802431	46.396762
3503.639791	473412.167142	46.401767
3503.834139	473413.551985	46.406772
3503.780029	473406.825806	46.411777
3503.756181	473396.650764	46.416781
3504.011539	473376.704662	46.421786
3504.082084	473381.706273	46.426791
3503.944492	473376.868114	46.431796
3504.113692	473354.708425	46.436801
3503.774108	473337.244072	46.441805
3503.660319	473337.111611	46.446810
3503.486869	473332.785990	46.451815
3503.470054	473334.460109	46.456820
3503.794820	473333.948909	46.461825
3503.675313	473340.198408	46.466829
3503.484924	473315.871792	46.471834
3503.430201	473312.032322	46.476839
3503.468440	473304.986481	46.481844
3503.925792	473302.882714	46.486849
3503.557294	473304.110457	46.491853
3503.590333	473297.116144	46.496858
3503.455875	473308.077989	46.501863
3504.123531	473307.964025	46.506868
3504.320069	473284.179015	46.511873
3503.859927	473272.913615	46.516877
3503.891633	473256.196075	46.521882
3503.759954	473262.295749	46.526887
3503.870807	473243.083180	46.531892
3504.153779	473233.159517	46.536897
3503.968919	473231.114756	46.541901
3504.054266	473223.149266	46.546906
3503.555391	473208.598644	46.551911
3503.346923	473196.986367	46.556916
3503.869677	473186.464663	46.561921
3503.591037	473191.475304	46.566925
3503.500072	473177.310795	46.571930
3503.681397	473171.354621	46.576935
3503.624341	473180.834673	46.581940
3503.731797	473172.966673	46.586945
3503.465444	473167.188225	46.591949
3503.670489	473144.211874	46.596954
3503.354162	473145.329433	46.601959
3503.682009	473152.869976	46.606964
3503.757537	473152.603901	46.611969
3503.246522	473154.818210	46.616973
3503.821093	473153.200843	46.621978
3503.258601	473155.778444	46.626983
3503.184869	473159.538669	46.631988
3503.886621	473154.405205	46.636993
3503.536060	473158.465915	46.641997
3503.461849	473123.484134	46.647002
3503.314754	473118.039810	46.652007
3503.271749	473107.209517	46.657012
3503.550699	473107.617715	46.662017
3503.241479	473113.950326	46.667021
3503.569365	473106.753666	46.672026
3503.668501	473118.992463	46.677031
3503.690420	473107.644652	46.682036
3503.696587	473110.378377	46.687041
3503.324553	473121.532828	46.692045
3503.712319	473112.654717	46.697050
3503.623748	473121.937606	46.702055
3503.638157	473120.010738	46.707060
3503.806141	473085.342033	46.712065
3504.080813	473075.926138	46.717069
3504.169104	473073.936006	46.722074
3503.985372	473074.423207	46.727079
3503.827486	473051.407426	46.732084
3504.093060	473040.119257	46.737089
3503.713353	473027.016806	46.742093
3503.701413	473019.675564	46.747098
3503.526827	473033.379176	46.752103
3503.333724	473011.534160	46.757108
3503.618972	472989.354221	46.762113
3503.296996	472987.940570	46.767117
3503.699909	472993.949050	46.772122
3503.708661	472993.745019	46.777127
3503.351170	472996.236994	46.782132
3503.565576	472983.539505	46.787137
3503.042192	472996.340470	46.792141
3503.679829	472997.345792	46.797146
3503.498162	472998.946803	46.802151
3503.504120	472995.147550	46.807156
3503.543759	472997.723645	46.812161
3503.762199	472997.179948	46.817165
3503.899926	472970.517891	46.822170
3503.756973	472959.451360	46.827175
3503.378109	472957.794201	46.832180
3503.919910	472947.117179	46.837185
3503.280509	472957.608367	46.842189
3503.478577	472957.270722	46.847194
3503.719154	472960.369594	46.852199
3503.270927	472959.433292	46.857204
3503.880401	472959.076043	46.862209
3503.567458	472934.516637	46.867213
3503.462091	472922.278858	46.872218
3503.494034	472926.730100	46.877223
3503.785061	472923.844390	46.882228
3504.018715	472918.841434	46.887233
3503.565919	472922.869007	46.892237
3503.432160	472914.181140	46.897242
3503.616266	472897.487900	46.902247
3503.548573	472882.964686	46.907252
3503.617864	472876.166601	46.912257
3503.644658	472872.110545	46.917261
3504.038406	472871.131759	46.922266
3504.034684	472863.080036	46.927271
3503.849599	472860.073036	46.932276
3504.173003	472841.076980	46.937281
3503.881563	472837.429764	46.942285
3504.085884	472832.836946	46.947290
3503.648982	472821.263439	46.952295
3503.621221	472814.735124	46.957300
3503.587653	472790.583622	46.962305
3503.716096	472784.838932	46.967309
3503.732172	472792.128991	46.972314
3503.671822	472795.836360	46.977319
3503.484362	472791.209140	46.982324
3503.775661	472776.168748	46.987329
3503.460578	472768.879169	46.992333
3503.505014	472758.641474	46.997338
3503.569110	472756.452863	47.002343
3503.384900	472756.686932	47.007348
3503.610848	472760.750577	47.012353
3503.327672	472757.304510	47.017357
3503.360429	472758.565062	47.022362
3503.624440	472753.556879	47.027367
3503.427546	472753.438603	47.032372
3503.693776	472743.112385	47.037377
3503.330042	472753.759193	47.042381
3503.886221	472756.196479	47.047386
3503.932949	472734.006321	47.052391
3503.799656	472727.546639	47.057396
3503.810045	472716.707003	47.062401
3503.666067	472716.326469	47.067405
3503.960351	472711.768906	47.072410
3504.006739	472693.680955	47.077415
3503.704466	472684.920466	47.082420
3504.237582	472680.879204	47.087425
3503.945813	472682.296462	47.092429
3503.759002	472652.549407	47.097434
3503.841162	472648.433205	47.102439
3503.636578	472643.656938	47.107444
3503.794978	472635.577435	47.112449
3503.935951	472644.770722	47.117453
3503.991122	472625.769603	47.122458
3503.882887	472608.416997	47.127463
3503.913526	472606.689884	47.132468
3503.973228	472602.678795	47.137473
3503.857932	472594.392784	47.142477
3504.300242	472565.500419	47.147482
3503.984011	472556.033224	47.152487
3504.092445	472561.686969	47.157492
3504.370742	472536.013187	47.162497
3504.427325	472524.659103	47.167501
3503.860152	472509.866370	47.172506
3504.054402	472489.220726	47.177511
3503.952452	472486.807210	47.182516
3504.122442	472479.434691	47.187521
3503.666076	472463.103649	47.192525
3503.826900	472445.806241	47.197530
3504.156196	472441.040053	47.202535
3504.075847	472440.800585	47.207540
3504.063026	472425.659904	47.212545
3504.038808	472405.608568	47.217549
3504.205950	472397.983277	47.222554
3504.082559	472397.396641	47.227559
3503.943722	472379.441304	47.232564
3503.906737	472361.772431	47.237569
3503.594633	472365.624163	47.242573
3503.678331	472359.177947	47.247578
3503.573210	472360.917877	47.252583
3503.216129	472345.177524	47.257588
3503.383323	472326.055682	47.262593
3503.701769	472326.963609	47.267597
3503.168065	472326.700258	47.272602
3503.191886	472321.277163	47.277607
3503.077031	472325.044577	47.282612
3503.426496	472323.313644	47.287617
3502.887742	472336.573492	47.292621
3503.405802	472359.579377	47.297626
3503.692025	472356.795692	47.302631
3503.492205	472334.039413	47.307636
3503.680259	472310.710421	47.312641
3503.435323	472312.930038	47.317645
3503.586242	472317.816920	47.322650
3503.324089	472318.722693	47.327655
3503.345691	472321.555189	47.332660
3503.670156	472310.408462	47.337665
3503.921853	472317.861057	47.342669
3503.361457	472319.222919	47.347674
3503.760012	472314.546164	47.352679
3503.647624	472304.790808	47.357684
3503.707578	472283.762704	47.362689
3503.592146	472281.554046	47.367693
3503.539972	472272.548076	47.372698
3503.530740	472277.411668	47.377703
3503.523883	472275.741572	47.382708
3504.034736	472272.159835	47.387713
3503.992010	472278.193995	47.392717
3503.689085	472248.567415	47.397722
3503.582506	472231.315467	47.402727
3503.255109	472244.640582	47.407732
3503.618962	472235.462267	47.412737
3503.412097	472235.446981	47.417741
3503.373587	472234.440680	47.422746
3503.190435	472237.966545	47.427751
3503.239955	472241.553972	47.432756
3503.441901	472232.403300	47.437761
3503.420119	472236.711943	47.442765
3503.618208	472230.144859	47.447770
3503.826100	472223.728037	47.452775
3503.275491	472230.811202	47.457780
3503.504382	472235.634146	47.462785
3503.305936	472210.142612	47.467789
3503.098765	472200.808553	47.472794
3503.118536	472213.264079	47.477799
3503.291506	472222.249527	47.482804
3503.669297	472222.286349	47.487809
3503.276303	472218.555059	47.492813
3503.371322	472213.221067	47.497818
3503.495333	472198.208776	47.502823
3503.126034	472203.589680	47.507828
3503.503997	472199.777392	47.512833
3503.359588	472210.488350	47.517837
3503.354113	472204.766348	47.522842
3503.630393	472208.568292	47.527847
3502.983426	472208.020404	47.532852
3503.806841	472204.790450	47.537857
3503.548630	472208.531720	47.542861
3503.448603	472208.751421	47.547866
3503.705803	472209.821749	47.552871
3503.205874	472211.223940	47.557876
3503.499277	472207.020925	47.562881
3503.334029	472215.709607	47.567885
3503.415022	472212.707714	47.572890
3503.299906	472213.284512	47.577895
3503.343763	472211.099293	47.582900
3503.727584	472208.197629	47.587905
3503.501890	472213.554011	47.592909
3503.257305	472193.388138	47.597914
3503.374059	472184.150697	47.602919
3503.476903	472180.334736	47.607924
3503.787638	472174.660024	47.612929
3503.295649	472182.948699	47.617933
3503.270759	472172.722521	47.622938
3503.610585	472176.462975	47.627943
3503.426187	472175.025768	47.632948
3503.712588	472164.797079	47.637953
3503.589001	472172.009936	47.642957
3503.587882	472171.756936	47.647962
3503.675822	472167.690287	47.652967
3503.557946	472169.837579	47.657972
3503.746754	472147.976987	47.662977
3503.399859	472140.287425	47.667981
3503.205342	472130.697940	47.672986
3503.538422	472135.199244	47.677991
3503.311380	472141.619442	47.682996
3503.571722	472132.711980	47.688001
3503.556128	472135.145688	47.693005
3503.265995	472134.739452	47.698010
3503.412563	472138.715495	47.703015
3503.176924	472137.287035	47.708020
3503.617092	472130.881166	47.713025
3503.562925	472136.309574	47.718029
3503.775584	472130.499658	47.723034
3503.899314	472128.959189	47.728039
3503.384032	472111.219810	47.733044
3503.734443	472092.724845	47.738049
3503.391476	472092.783444	47.743053
3503.492880	472094.082966	47.748058
3503.971338	472090.658665	47.753063
3503.778133	472091.147507	47.758068
3503.832520	472095.189946	47.763073
3503.468213	472082.894539	47.768077
3503.679634	472070.804695	47.773082
3503.681056	472066.702151	47.778087
3503.263397	472069.356458	47.783092
3503.850851	472067.787450	47.788097
3503.809118	472060.248333	47.793101
3503.472398	472067.801500	47.798106
3503.890564	472070.920844	47.803111
3503.780045	472058.987256	47.808116
3503.892001	472038.101936	47.813121
3503.686864	472034.490471	47.818125
3503.940147	472031.712363	47.823130
3503.927981	472023.408489	47.828135
3503.720829	472018.936378	47.833140
3503.857166	471997.641679	47.838145
3503.651041	471995.853644	47.843149
3503.300346	471986.746569	47.848154
3504.276809	471988.757671	47.853159
3503.725018	471988.497402	47.858164
3503.997840	471953.504821	47.863169
3503.580858	471950.891795	47.868173
3503.532114	471949.735287	47.873178
3503.740722	471945.496046	47.878183
3503.440303	471945.344794	47.883188
3503.774096	471941.590643	47.888193
3503.577191	471951.601661	47.893197
3503.569098	471924.405902	47.898202
3503.526441	471916.309773	47.903207
3503.395776	471921.852597	47.908212
3503.917142	471904.948947	47.913217
3503.845631	471913.824349	47.918221
3503.832199	471914.940905	47.923226
3503.691423	471902.860444	47.928231
3503.492206	471876.254362	47.933236
3503.916120	471865.444917	47.938241
3503.678606	471872.727988	47.943245
3503.656884	471867.160598	47.948250
3503.869576	471861.299947	47.953255
3503.476397	471866.330498	47.958260
3503.519278	471855.839342	47.963265
3503.289290	471842.913080	47.968269
3503.362060	471836.063377	47.973274
3503.504071	471826.720155	47.978279
3503.569087	471825.746802	47.983284
3503.706479	471821.772928	47.988289
3503.541886	471826.207343	47.993293
3503.426852	471824.049210	47.998298
3503.961776	471821.830743	48.003303
3503.636938	471830.952027	48.008308
3503.872757	471823.973185	48.013313
3503.731401	471803.637325	48.018317
3503.464900	471792.540551	48.023322
3503.509376	471794.964046	48.028327
3503.393099	471790.121835	48.033332
3503.485874	471788.839858	48.038337
3503.405671	471786.422539	48.043341
3503.689749	471798.630622	48.048346
3503.333322	471789.727017	48.053351
3503.459405	471790.819759	48.058356
3503.726996	471779.733075	48.063361
3503.443206	471790.265484	48.068365
3503.298119	471789.935767	48.073370
3504.072507	471782.054599	48.078375
3503.264778	471765.124531	48.083380
3503.537027	471764.267730	48.088385
3503.610039	471763.900772	48.093389
3503.530454	471755.000528	48.098394
3503.798724	471763.108925	48.103399
3503.434820	471766.513800	48.108404
3503.549793	471764.215092	48.113409
3503.665750	471763.688861	48.118413
3503.618633	471750.933899	48.123418
3503.914084	471723.078253	48.128423
3503.789617	471714.337594	48.133428
3503.738815	471708.471240	48.138433
3503.401135	471721.393304	48.143437
3503.674908	471726.056775	48.148442
3503.802501	471710.182481	48.153447
3503.658556	471696.380426	48.158452
3503.905279	471674.509393	48.163457
3503.944153	471677.592274	48.168461
3504.006171	471673.985769	48.173466
3504.056452	471669.570912	48.178471
3503.865999	471650.560098	48.183476
3503.968928	471629.979749	48.188481
3503.857676	471629.593604	48.193485
3503.715994	471632.909911	48.198490
3503.500078	471612.687870	48.203495
3503.253653	471601.182375	48.208500
3503.611637	471590.130793	48.213505
3503.662415	471601.923014	48.218509
3503.688894	471598.018678	48.223514
3503.819178	471591.766835	48.228519
3503.809514	471591.413990	48.233524
3503.755792	471580.837881	48.238529
3503.596096	471567.089067	48.243533
3503.470433	471561.792572	48.248538
3503.626185	471556.093491	48.253543
3503.379802	471556.591426	48.258548
3503.376884	471547.323459	48.263553
3503.509166	471544.565941	48.268557
3503.283191	471550.023854	48.273562
3503.495056	471557.483553	48.278567
3503.650923	471551.936394	48.283572
3503.652734	471541.046894	48.288577
3503.539069	471550.841322	48.293581
3503.430332	471545.339342	48.298586
3503.900223	471545.107203	48.303591
3503.348850	471520.080173	48.308596
3503.596785	471511.377127	48.313601
3503.823116	471509.312612	48.318605
3503.358298	471516.229452	48.323610
3503.795316	471504.809791	48.328615
3503.743046	471511.605543	48.333620
3504.118864	471506.476642	48.338625
3503.756962	471488.254653	48.343629
3503.855340	471483.375710	48.348634
3504.217956	471459.762617	48.353639
3503.973634	471459.095303	48.358644
3504.080418	471433.651891	48.363649
3504.104731	471431.723157	48.368653
3503.883411	471434.040140	48.373658
3503.773505	471422.156690	48.378663
3503.669538	471408.448892	48.383668
3503.677483	471393.810311	48.388673
3503.596767	471385.973692	48.393677
3503.753372	471389.745590	48.398682
3503.663976	471390.166076	48.403687
3503.275050	471401.476374	48.408692
3503.582529	471394.535785	48.413697
3503.270102	471370.176827	48.418701
3503.126313	471379.621951	48.423706
3503.328134	471385.665290	48.428711
3503.200359	471395.310264	48.433716
3503.356417	471385.559240	48.438721
3503.430091	471395.929536	48.443725
3503.587055	471395.244349	48.448730
3503.605352	471358.724033	48.453735
3503.630005	471360.847081	48.458740
3503.805653	471348.813529	48.463745
3504.104253	471350.433969	48.468749
3503.510415	471347.344573	48.473754
3503.474783	471352.415506	48.478759
3503.289975	471355.840521	48.483764
3503.407974	471346.349216	48.488769
3503.326717	471342.919057	48.493773
3503.583887	471351.536010	48.498778
3503.523895	471318.169165	48.503783
3503.346792	471315.464441	48.508788
3503.521124	471315.536008	48.513793
3503.615837	471314.253668	48.518797
3503.617484	471314.050832	48.523802
3503.659174	471319.716349	48.528807
3503.467666	471313.721952	48.533812
3503.518483	471313.713313	48.538817
3503.686178	471313.076938	48.543821
3503.438755	471315.803578	48.548826
3503.562164	471293.547973	48.553831
3503.525496	471289.097225	48.558836
3503.626478	471280.925647	48.563841
3503.449850	471279.132506	48.568845
3503.103235	471288.308419	48.573850
3503.563576	471281.341687	48.578855
3503.454747	471285.766708	48.583860
3503.662227	471278.995097	48.588865
3503.663333	471283.198754	48.593869
3503.350156	471292.267659	48.598874
3504.164229	471275.465410	48.603879
3503.670935	471275.296436	48.608884
3503.771348	471251.677204	48.613889
3503.844560	471242.851923	48.618893
3503.752969	471239.423509	48.623898
3503.730625	471238.059855	48.628903
3503.532735	471244.019545	48.633908
3503.747991	471230.358406	48.638913
3503.802860	471201.378154	48.643917
3503.629472	471200.546773	48.648922
3504.010029	471197.696163	48.653927
3503.560177	471197.266528	48.658932
3503.599673	471196.145555	48.663937
3503.503709	471192.819176	48.668941
3503.739863	471174.241521	48.673946
3503.540040	471152.142238	48.678951
3503.782057	471160.559272	48.683956
3503.549911	471159.383381	48.688961
3503.683827	471157.739797	48.693965
3503.310251	471158.512704	48.698970
3503.605007	471154.866360	48.703975
3503.315220	471154.915879	48.708980
3503.215263	471157.313469	48.713985
3503.619500	471144.025189	48.718989
3503.531217	471154.828462	48.723994
3503.895446	471140.837930	48.728999
3503.756406	471131.998190	48.734004
3503.534720	471123.780343	48.739009
3503.548100	471116.889870	48.744013
3503.244100	471117.600249	48.749018
3503.416282	471117.013751	48.754023
3503.708418	471114.076929	48.759028
3503.606203	471117.285290	48.764033
3503.583861	471112.984000	48.769037
3503.602087	471109.840704	48.774042
3503.827281	471087.972666	48.779047
3503.578721	471084.267133	48.784052
3503.676443	471070.271406	48.789057
3503.681220	471075.436811	48.794061
3503.460059	471081.755067	48.799066
3503.807001	471075.364761	48.804071
3503.576371	471078.088567	48.809076
3503.390114	471061.203690	48.814081
3503.643466	471041.356745	48.819085
3503.134387	471039.012559	48.824090
3503.542626	471032.054633	48.829095
3503.267154	471036.508167	48.834100
3503.284140	471044.051996	48.839105
3503.573588	471038.988366	48.844109
3503.248893	471038.436058	48.849114
3503.742471	471034.603796	48.854119
3503.591566	471037.871133	48.859124
3503.342442	471034.368282	48.864129
3503.465063	471038.095405	48.869133
3503.402194	471039.423050	48.874138
3503.541091	471038.386392	48.879143
3503.354229	471044.597506	48.884148
3503.740689	471045.848428	48.889153
3503.919893	471034.624452	48.894157
3503.872886	471017.462514	48.899162
3503.549935	471002.525587	48.904167
3503.808262	471006.128246	48.909172
3503.557044	470995.686827	48.914177
3503.896631	470992.286042	48.919181
3503.870515	470993.050276	48.924186
3503.605958	470970.202096	48.929191
3503.495756	470963.332668	48.934196
3503.541629	470970.162507	48.939201
3503.594729	470962.454809	48.944205
3503.890710	470967.064029	48.949210
3503.743938	470966.025496	48.954215
3503.600577	470956.882517	48.959220
3503.862587	470935.008016	48.964225
3503.706954	470925.867117	48.969229
3503.641099	470930.740727	48.974234
3503.992245	470911.130193	48.979239
3504.069853	470917.498788	48.984244
3503.715900	470891.474873	48.989249
3503.873449	470884.357101	48.994253
3503.713988	470878.407742	48.999258
3503.668068	470870.362369	49.004263
3503.506016	470887.256317	49.009268
3503.510353	470875.150417	49.014273
3503.549570	470857.163219	49.019277
3503.668767	470849.444190	49.024282
3503.810223	470844.203180	49.029287
3503.627352	470842.411062	49.034292
3503.513985	470833.161602	49.039297
3503.711223	470827.556517	49.044301
3503.192417	470842.232193	49.049306
3503.409053	470838.548478	49.054311
3503.691712	470833.334005	49.059316
3503.807432	470830.883108	49.064321
3504.001554	470820.213601	49.069325
3503.843881	470817.100291	49.074330
3503.939360	470804.219039	49.079335
3503.906763	470803.059703	49.084340
3503.852977	470789.646783	49.089345
3503.922636	470774.136139	49.094349
3503.825774	470776.735848	49.099354
3503.886560	470763.252697	49.104359
3503.911381	470773.277130	49.109364
3503.686352	470745.660861	49.114369
3503.960216	470729.963364	49.119373
3503.503277	470732.118064	49.124378
3503.915331	470721.664540	49.129383
3503.997711	470722.106359	49.134388
3503.849805	470700.605478	49.139393
3504.194772	470686.769849	49.144397
3503.795105	470685.977082	49.149402
3504.001150	470675.508058	49.154407
3503.774886	470654.982853	49.159412
3503.634439	470645.991175	49.164417
3503.981691	470651.199518	49.169421
3504.016005	470649.775498	49.174426
3504.377641	470631.884983	49.179431
3503.890156	470619.001846	49.184436
3503.815104	470611.062636	49.189441
3504.034289	470602.212131	49.194445
3503.980797	470586.722361	49.199450
3504.120291	470563.905997	49.204455
3503.787841	470572.168134	49.209460
3503.665731	470565.401895	49.214465
3503.605330	470558.422515	49.219469
3503.419210	470535.459114	49.224474
3503.518816	470516.650877	49.229479
3503.334398	470521.443535	49.234484
3503.323259	470532.132692	49.239489
3503.728178	470518.134752	49.244493
3503.482466	470522.836575	49.249498
3503.448454	470509.470730	49.254503
3503.350253	470519.972157	49.259508
3503.261922	470514.213139	49.264513
3503.696624	470515.759762	49.269517
3503.647741	470518.401965	49.274522
3503.572483	470506.208117	49.279527
3503.728346	470517.628522	49.284532
3503.798142	470509.411285	49.289537
3503.768472	470490.118591	49.294541
3503.590259	470482.247593	49.299546
3503.487367	470482.569102	49.304551
3503.632587	470484.671661	49.309556
3503.367825	470473.877712	49.314561
3503.893037	470469.736034	49.319565
3503.493149	470472.539477	49.324570
3503.595681	470460.061990	49.329575
3503.805929	470455.619535	49.334580
3503.489302	470443.821414	49.339585
3503.580382	470432.713429	49.344589
3503.265740	470432.260686	49.349594
3503.542639	470431.858889	49.354599
3503.599340	470436.306495	49.359604
3503.527989	470438.091486	49.364609
3503.765991	470433.998840	49.369613
3503.492358	470438.604151	49.374618
3503.469209	470428.022173	49.379623
3503.545658	470404.507273	49.384628
3503.330569	470390.209899	49.389633
3503.722783	470390.244268	49.394637
3503.395302	470387.717038	49.399642
3503.748798	470389.986648	49.404647
3503.770272	470386.488122	49.409652
3503.496827	470392.764884	49.414657
3504.003510	470385.384708	49.419661
3503.826993	470376.247108	49.424666
3504.154467	470352.385377	49.429671
3504.020125	470347.191322	49.434676
3503.887740	470346.859409	49.439681
3503.910759	470321.124893	49.444685
3503.610826	470322.847623	49.449690
3503.720051	470310.014338	49.454695
3503.905677	470312.869781	49.459700
3503.480701	470312.587827	49.464705
3503.629294	470310.232551	49.469709
3503.239741	470299.662414	49.474714
3503.305936	470292.661320	49.479719
3503.555409	470294.999355	49.484724
3503.345836	470280.498352	49.489729
3503.104003	470265.952196	49.494733
3503.201096	470284.220663	49.499738
3503.267548	470297.378601	49.504743
3503.381312	470308.654368	49.509748
3503.440575	470297.804991	49.514753
3503.774842	470270.497733	49.519757
3503.370229	470274.264381	49.524762
3503.411587	470266.406451	49.529767
3503.580180	470273.215587	49.534772
3503.268487	470269.925881	49.539777
3503.389693	470274.818369	49.544781
3503.301698	470281.924570	49.549786
3503.519598	470271.757204	49.554791
3503.765325	470277.489497	49.559796
3503.410206	470277.043661	49.564801
3503.522200	470271.756873	49.569805
3503.201260	470277.585924	49.574810
3503.272812	470269.317632	49.579815
3503.321075	470275.134294	49.584820
3503.229045	470275.960462	49.589825
3502.980499	470270.279376	49.594829
3503.149252	470275.214397	49.599834
3503.299785	470266.983269	49.604839
3503.099717	470271.677361	49.609844
3503.195268	470271.407829	49.614849
3503.347014	470265.253184	49.619853
3503.518614	470270.440975	49.624858
3503.321024	470270.728006	49.629863
3503.352908	470273.964264	49.634868
3503.515724	470274.848219	49.639873
3503.270711	470270.989966	49.644877
3503.148174	470279.874850	49.649882
3503.718753	470269.292706	49.654887
3503.796929	470266.645543	49.659892
3503.368467	470267.731761	49.664897
3503.566139	470261.467971	49.669901
3503.423623	470257.896120	49.674906
3503.432877	470232.467740	49.679911
3503.560104	470235.738375	49.684916
3503.615474	470230.461244	49.689921
3503.601875	470223.676354	49.694925
3503.455658	470221.472708	49.699930
3503.691393	470222.445517	49.704935
3504.051383	470229.880453	49.709940
3503.140672	470227.756694	49.714945
3503.565045	470230.925941	49.719949
3503.552263	470223.229192	49.724954
3503.596481	470205.493776	49.729959
3503.831646	470196.893608	49.734964
3503.820890	470191.019942	49.739969
3503.726068	470190.529659	49.744973
3503.707545	470187.291181	49.749978
3503.743447	470186.069459	49.754983
3503.675445	470179.192540	49.759988
3503.576141	470166.901277	49.764993
3503.714754	470160.748841	49.769997
3503.911294	470155.548886	49.775002
3504.146375	470152.621659	49.780007
3503.992073	470139.833256	49.785012
3503.924215	470125.561194	49.790017
3504.282767	470121.802457	49.795021
3503.989179	470120.434385	49.800026
3503.573145	470093.558894	49.805031
3503.720477	470080.718947	49.810036
3503.595065	470085.805549	49.815041
3504.032165	470071.649831	49.820045
3503.446899	470072.864137	49.825050
3503.623453	470075.113347	49.830055
3503.583161	470067.674489	49.835060
3503.408768	470052.711440	49.840065
3503.619418	470036.568298	49.845069
3503.227368	470038.914602	49.850074
3503.297904	470028.924223	49.855079
3503.698843	470032.046854	49.860084
3503.495981	470033.145215	49.865089
3503.434820	470034.168729	49.870093
3503.410906	470032.248088	49.875098
3503.257254	470035.110853	49.880103
3503.826464	470023.667729	49.885108
3503.627404	470031.400808	49.890113
3503.749685	470022.921140	49.895117
3503.780390	470029.247392	49.900122
3503.708754	470007.327485	49.905127
3503.529456	470000.773415	49.910132
3503.317961	469994.731357	49.915137
3503.718730	469995.827954	49.920141
3503.585570	470003.195229	49.925146
3503.553871	469996.109438	49.930151
3503.577362	469990.533772	49.935156
3503.712241	469999.172227	49.940161
3503.785510	469981.127730	49.945165
3503.528486	469967.090455	49.950170
3503.444887	469956.771794	49.955175
3503.644969	469949.139890	49.960180
3503.502547	469957.167239	49.965185
3503.329753	469943.368824	49.970189
3503.490216	469949.774250	49.975194
3503.640830	469944.683384	49.980199
3503.640222	469947.570682	49.985204
3503.841495	469948.245478	49.990209
3503.910228	469929.897796	49.995213
3503.497380	469915.481874	50.000218
3503.447562	469903.232642	50.005223
3503.487559	469901.351726	50.010228
3503.298800	469909.133748	50.015233
3503.207958	469907.832345	50.020237
3503.178070	469915.941801	50.025242
3503.310127	469904.066729	50.030247
3503.134023	469911.593329	50.035252
3503.010143	469904.573895	50.040257
3503.428537	469896.904693	50.045261
3503.337763	469908.874100	50.050266
3503.021640	469909.687895	50.055271
3503.465971	469907.079464	50.060276
3503.315190	469914.399131	50.065281
3503.119898	469907.290588	50.070285
3503.317193	469905.838682	50.075290
3502.993148	469907.565566	50.080295
3503.354806	469902.033437	50.085300
3503.350112	469909.480117	50.090305
3503.391349	469899.849237	50.095309
3503.375116	469912.059173	50.100314
3503.643033	469901.781765	50.105319
3503.560385	469898.503535	50.110324
3503.245301	469900.026282	50.115329
3503.567469	469903.770208	50.120333
3503.604501	469907.360214	50.125338
3503.533075	469910.563522	50.130343
3503.589995	469914.352737	50.135348
3503.274488	469922.713567	50.140353
3503.665963	469908.210954	50.145357
3503.314599	469914.146615	50.150362
3503.326187	469905.077971	50.155367
3503.375121	469906.943777	50.160372
3503.380964	469911.146931	50.165377
3503.494145	469906.670269	50.170381
3503.318614	469901.584429	50.175386
3503.420562	469876.291698	50.180391
3503.458231	469867.826409	50.185396
3503.356494	469874.225979	50.190401
3503.718168	469860.842764	50.195405
3503.369381	469878.529279	50.200410
3503.414718	469872.797893	50.205415
3503.604021	469870.081048	50.210420
3503.365975	469875.237591	50.215425
3503.431180	469872.997804	50.220429
3503.619376	469880.766124	50.225434
3503.595259	469876.870072	50.230439
3503.549555	469876.979218	50.235444
3503.381558	469882.984882	50.240449
3503.911137	469874.182342	50.245453
3503.748513	469854.759745	50.250458
3503.666443	469851.582713	50.255463
3503.949902	469842.872835	50.260468
3503.826039	469846.591629	50.265473
3503.869422	469835.339481	50.270477
3503.629410	469823.578542	50.275482
3503.564588	469794.920481	50.280487
3503.502416	469790.625691	50.285492
3503.236274	469794.318137	50.290497
3503.814349	469787.381410	50.295501
3503.542529	469796.089401	50.300506
3503.557421	469793.756892	50.305511
3503.495845	469792.146570	50.310516
3503.614337	469796.583776	50.315521
3503.773875	469783.842849	50.320525
3503.751673	469767.587280	50.325530
3503.817017	469756.331336	50.330535
3504.348628	469759.127787	50.335540
3503.600477	469760.876447	50.340545
3503.583311	469738.946928	50.345549
3503.635148	469718.474524	50.350554
3503.619075	469715.438157	50.355559
3503.762046	469708.879610	50.360564
3503.523866	469722.393879	50.365569
3503.332396	469710.472623	50.370573
3503.140861	469717.242147	50.375578
3503.001985	469716.961983	50.380583
3503.218018	469714.189899	50.385588
3503.232229	469709.628785	50.390593
3503.398456	469710.562838	50.395597
3503.298638	469717.316701	50.400602
3503.138180	469717.445442	50.405607
3503.511999	469711.100741	50.410612
3503.261683	469718.538784	50.415617
3503.728524	469702.047698	50.420621
3503.685197	469714.211736	50.425626
3503.453938	469717.239758	50.430631
3503.518487	469705.882614	50.435636
3503.588384	469710.885315	50.440641
3503.640720	469708.900969	50.445645
3503.683007	469700.941341	50.450650
3503.448481	469688.368941	50.455655
3503.944817	469688.182924	50.460660
3503.296839	469685.912933	50.465665
3503.335479	469681.195684	50.470669
3503.408473	469678.245408	50.475674
3503.678431	469675.312153	50.480679
3503.834223	469676.399946	50.485684
3503.465897	469685.529688	50.490689
3503.671987	469673.034000	50.495693
3503.671411	469657.281170	50.500698
3503.532957	469644.945600	50.505703
3503.477600	469642.067887	50.510708
3503.242179	469637.701339	50.515713
3503.243408	469635.523101	50.520717
3503.701061	469647.956208	50.525722
3503.613694	469639.106944	50.530727
3503.795926	469628.185534	50.535732
3503.828860	469603.410751	50.540737
3503.684749	469560.177866	50.545741
3503.786401	469526.526989	50.550746
3503.437976	469464.080623	50.555751
3503.420549	469395.904361	50.560756
3503.463355	469325.184892	50.565761
3503.056787	469232.760779	50.570765
3502.949578	469143.729573	50.575770
3502.682422	469040.997953	50.580775
3502.943208	468932.907556	50.585780
3502.658783	468826.986490	50.590785
3502.378215	468694.672828	50.595789
3502.273508	468557.819873	50.600794
3501.867485	468418.585898	50.605799
3501.308392	468273.500910	50.610804
3500.791809	468121.416930	50.615809
3500.685496	467963.841369	50.620813
3500.406457	467802.798629	50.625818
3500.214065	467628.872599	50.630823
3499.882824	467458.210841	50.635828
3499.115452	467279.719234	50.640833
3499.070513	467083.625094	50.645837
3498.851619	466895.714912	50.650842
3498.477514	466700.635604	50.655847
3498.460490	466488.015290	50.660852
3498.036604	466277.691209	50.665857
3497.767084	466067.338473	50.670861
3497.102344	465841.649455	50.675866
3496.506302	465618.529898	50.680871
3496.341654	465386.923888	50.685876
3495.726543	465155.848005	50.690881
3495.152547	464910.424099	50.695885
3494.853848	464679.389834	50.700890
3494.325234	464439.576123	50.705895
3493.579453	464191.892473	50.710900
3493.213176	463940.948802	50.715905
3492.767539	463693.815576	50.720909
3491.774127	463434.206836	50.725914
3491.533707	463177.506250	50.730919
3491.061652	462914.964083	50.735924
3490.617364	462664.169337	50.740929
3490.064551	462384.405693	50.745933
3489.414924	462126.747778	50.750938
3489.010569	461856.224311	50.755943
3488.934082	461568.361366	50.760948
3488.008145	461296.905801	50.765953
3487.714163	461012.771128	50.770957
3486.959517	460735.856347	50.775962
3486.107169	460447.501436	50.780967
3486.067659	460157.432533	50.785972
3485.160201	459871.055073	50.790977
3484.476432	459577.438880	50.795981
3484.065560	459277.031358	50.800986
3483.437809	458985.626784	50.805991
3483.199797	458689.438057	50.810996
3482.390415	458401.248891	50.816001
3481.470375	458098.427178	50.821005
3481.125792	457794.134176	50.826010
3480.623188	457495.438812	50.831015
3480.202611	457183.344173	50.836020
3479.389258	456875.113202	50.841025
3478.746965	456566.645567	50.846029
3478.279018	456261.438130	50.851034
3477.485508	455940.771126	50.856039
3477.043103	455626.223145	50.861044
3476.409003	455309.928887	50.866049
3475.742670	454998.450810	50.871053
3474.794988	454684.430760	50.876058
3474.200759	454364.161095	50.881063
3473.676676	454046.206306	50.886068
3472.824343	453729.924826	50.891073
3472.260235	453409.685783	50.896077
3471.491862	453094.039195	50.901082
3471.017431	452785.333612	50.906087
3470.640475	452470.472462	50.911092
3469.951351	452149.880301	50.916097
3469.241269	451817.676840	50.921101
3468.657632	451497.056555	50.926106
3467.783652	451176.125996	50.931111
3467.344034	450845.026876	50.936116
3466.407474	450530.231819	50.941121
3465.763487	450199.005229	50.946125
3465.196003	449877.089685	50.951130
3464.473322	449557.173139	50.956135
3463.835185	449235.361204	50.961140
3462.971603	448915.357522	50.966145
3462.468276	448585.602582	50.971149
3461.819873	448266.972073	50.976154
3461.160264	447944.129930	50.981159
3460.820253	447614.433348	50.986164
3459.928133	447278.030870	50.991169
3459.272657	446942.748982	50.996173
3458.670104	446623.477401	51.001178
3457.646757	446293.217755	51.006183
3457.346083	445965.568061	51.011188
3456.155415	445642.984499	51.016193
3455.324935	445320.841708	51.021197
3454.907529	445004.100726	51.026202
3453.865362	444684.469548	51.031207
3453.600066	444351.819046	51.036212
3452.750523	444039.347103	51.041217
3452.140180	443718.562806	51.046221
3451.597242	443399.993855	51.051226
3450.581317	443083.681914	51.056231
3450.088802	442747.089441	51.061236
3449.204864	442441.447523	51.066241
3448.858773	442119.072845	51.071245
3448.409651	441784.892727	51.076250
3447.619263	441471.207132	51.081255
3446.959478	441145.168886	51.086260
3446.348468	440826.421787	51.091265
3445.322975	440494.349394	51.096269
3444.544112	440177.904193	51.101274
3443.919814	439854.529232	51.106279
3443.524829	439528.016008	51.111284
3442.581020	439222.846779	51.116289
3442.156874	438892.270918	51.121293
3441.600594	438568.561200	51.126298
3440.717104	438240.489110	51.131303
3440.096211	437925.354508	51.136308
3439.103149	437599.320944	51.141313
3438.534725	437276.101870	51.146317
3437.788192	436965.186001	51.151322
3437.003373	436643.821169	51.156327
3436.535379	436312.555111	51.161332
3435.799761	436005.987307	51.166337
3435.092731	435684.798459	51.171341
3434.396927	435371.061448	51.176346
3434.091372	435052.230437	51.181351
3432.877432	434734.260405	51.186356
3432.093155	434420.271670	51.191361
3431.728146	434100.574910	51.196365
3431.171232	433792.576728	51.201370
3430.265407	433474.333548	51.206375
3429.438555	433148.917870	51.211380
3428.946231	432843.483729	51.216385
3428.440111	432524.397982	51.221389
3427.731435	432210.010840	51.226394
3426.740635	431893.739300	51.231399
3426.263817	431568.089281	51.236404
3425.345532	431262.909941	51.241409
3424.483198	430952.185654	51.246413
3424.083295	430640.414046	51.251418
3423.086327	430330.922386	51.256423
3422.755196	430012.431906	51.261428
3421.925754	429707.318504	51.266433
3421.221161	429395.277809	51.271437
3420.884513	429077.333805	51.276442
3419.884878	428766.705408	51.281447
3419.312856	428463.105170	51.286452
3418.772967	428150.918338	51.291457
3418.040463	427839.470823	51.296461
3417.821018	427524.886356	51.301466
3416.631028	427209.651381	51.306471
3416.104453	426887.091673	51.311476
3415.518993	426581.388654	51.316481
3414.633282	426270.657324	51.321485
3414.304977	425950.538171	51.326490
3413.350771	425637.983054	51.331495
3412.875198	425322.601160	51.336500
3412.254384	425010.183972	51.341505
3411.360430	424689.484733	51.346509
3410.677682	424382.907393	51.351514
3409.992548	424085.818933	51.356519
3409.349325	423753.592406	51.361524
3408.821869	423452.306773	51.366529
3407.812097	423135.667742	51.371533
3407.387620	422821.462838	51.376538
3406.344452	422506.547311	51.381543
3405.769506	422200.634742	51.386548
3405.137160	421897.926403	51.391553
3404.309499	421583.774461	51.396557
3403.859358	421266.101870	51.401562
3402.739887	420963.185990	51.406567
3402.602676	420655.427957	51.411572
3401.831595	420353.688935	51.416577
3400.847738	420047.413305	51.421581
3400.407736	419737.867879	51.426586
3399.702125	419432.781028	51.431591
3398.884826	419125.475567	51.436596
3398.274939	418823.995085	51.441601
3397.620170	418527.291273	51.446605
3396.845037	418216.743377	51.451610
3396.076528	417904.641901	51.456615
3396.032229	417599.546713	51.461620
3394.885995	417292.630392	51.466625
3394.194148	416984.337959	51.471629
3393.697835	416676.389201	51.476634
3392.669438	416378.048270	51.481639
3392.287806	416064.207748	51.486644
3391.405462	415776.980521	51.491649
3390.696495	415467.606259	51.496653
3390.126876	415156.351002	51.501658
3389.260968	414871.294303	51.506663
3388.436402	414565.001066	51.511668
3387.845882	414267.830225	51.516673
3386.996355	413967.754840	51.521677
3386.750085	413655.486722	51.526682
3385.621701	413368.579255	51.531687
3385.508450	413059.125073	51.536692
3384.293280	412762.932318	51.541697
3383.786016	412461.866917	51.546701
3383.301418	412158.077148	51.551706
3382.330901	411874.173348	51.556711
3381.870475	411572.226325	51.561716
3381.258343	411277.869008	51.566721
3380.438765	410984.305633	51.571725
3379.708296	410685.771910	51.576730
3379.038725	410391.770003	51.581735
3378.563830	410093.516059	51.586740
3377.911884	409798.564940	51.591745
3377.371597	409502.931195	51.596749
3377.195695	409197.175298	51.601754
3376.042470	408902.731562	51.606759
3375.510793	408590.807488	51.611764
3374.743913	408295.833947	51.616769
3374.201279	407986.342749	51.621773
3373.656761	407684.111841	51.626778
3372.527214	407385.939417	51.631783
3371.639606	407076.750634	51.636788
3371.350030	406785.031479	51.641793
3370.594646	406479.521363	51.646797
3370.441398	406180.203774	51.651802
3369.006356	405888.543599	51.656807
3368.358891	405581.506428	51.661812
3367.662740	405282.576470	51.666817
3367.210726	404988.021062	51.671821
3366.126863	404690.776417	51.676826
3365.375283	404399.593214	51.681831
3364.926888	404102.665478	51.686836
3364.035047	403813.659056	51.691841
3363.590583	403521.372696	51.696845
3363.100017	403216.822376	51.701850
3362.214876	402927.297524	51.706855
3361.764427	402632.361065	51.711860
3361.005644	402344.637484	51.716865
3360.110482	402048.322879	51.721869
3359.705967	401744.249791	51.726874
3359.007083	401477.235461	51.731879
3358.381790	401163.896385	51.736884
3357.727977	400881.068016	51.741889
3356.978184	400588.396635	51.746893
3356.466616	400285.570826	51.751898
3355.520222	399989.700536	51.756903
3354.917378	399704.616130	51.761908
3354.425226	399406.274175	51.766913
3353.681141	399114.272520	51.771917
3353.410556	398817.487065	51.776922
3352.565012	398525.420500	51.781927
3351.993554	398212.192066	51.786932
3351.367845	397917.464983	51.791937
3350.290079	397618.188161	51.796941
3349.774682	397321.047954	51.801946
3348.926821	397037.579452	51.806951
3348.279327	396729.124343	51.811956
3347.528310	396442.305168	51.816961
3346.729852	396160.903051	51.821965
3346.080316	395862.729110	51.826970
3345.838215	395578.050390	51.831975
3345.298283	395282.926179	51.836980
3344.655298	394985.428201	51.841985
3343.703486	394685.845621	51.846989
3343.126845	394383.959928	51.851994
3342.154155	394095.173725	51.856999
3341.983858	393797.837127	51.862004
3341.118075	393495.661425	51.867009
3339.881755	393202.642710	51.872013
3339.081731	392910.817109	51.877018
3338.615304	392631.763976	51.882023
3337.751624	392347.287367	51.887028
3337.655122	392055.612786	51.892033
3336.726749	391761.485499	51.897037
3336.047602	391472.420477	51.902042
3335.205604	391184.930610	51.907047
3334.515951	390895.506094	51.912052
3334.148609	390611.665272	51.917057
3333.479486	390321.443992	51.922061
3332.637400	390028.250787	51.927066
3331.508032	389741.253751	51.932071
3331.147347	389463.144404	51.937076
3330.421440	389172.972725	51.942081
3329.530071	388891.111400	51.947085
3329.159024	388598.738948	51.952090
3328.656333	388323.871100	51.957095
3327.748824	388036.184886	51.962100
3327.141044	387755.535467	51.967105
3326.540882	387470.027986	51.972109
3326.073627	387180.581271	51.977114
3325.533953	386894.981939	51.982119
3324.628793	386610.611527	51.987124
3324.006400	386324.436554	51.992129
3323.084090	386042.122584	51.997133
3322.587807	385748.626448	52.002138
3322.171952	385460.654620	52.007143
3321.227958	385171.143702	52.012148
3320.794636	384893.031344	52.017153
3319.969765	384608.578313	52.022157
3319.517495	384311.782531	52.027162
3318.512100	384033.887447	52.032167
3317.995408	383740.071202	52.037172
3317.522187	383453.692315	52.042177
3316.135874	383168.534384	52.047181
3315.922371	382889.680745	52.052186
3315.206416	382612.257698	52.057191
3314.324263	382321.642824	52.062196
3313.477084	382030.333050	52.067201
3313.497549	381754.683317	52.072205
3313.117510	381467.228710	52.077210
3311.842114	381185.923560	52.082215
3311.423550	380898.699304	52.087220
3310.919735	380605.945476	52.092225
3310.324073	380324.821878	52.097229
3309.812868	380027.310532	52.102234
3308.732479	379735.460894	52.107239
3307.829133	379442.332806	52.112244
3307.227645	379162.242571	52.117249
3306.493286	378870.758380	52.122253
3305.631198	378577.361396	52.127258
3304.824051	378309.526995	52.132263
3304.351760	378025.896908	52.137268
3303.655791	377742.073823	52.142273
3303.136143	377461.472325	52.147277
3302.442619	377176.398341	52.152282
3301.591718	376903.551903	52.157287
3301.103811	376621.616005	52.162292
3300.501838	376336.773545	52.167297
3299.372518	376053.213680	52.172301
3299.166156	375774.680299	52.177306
3298.294247	375500.961780	52.182311
3297.618965	375208.647734	52.187316
3297.288784	374934.501653	52.192321
3296.507272	374654.455660	52.197325
3295.990184	374370.675614	52.202330
3295.371322	374085.893615	52.207335
3294.481802	373802.579323	52.212340
3293.775531	373523.375792	52.217345
3292.643244	373239.513588	52.222349
3292.293002	372962.889042	52.227354
3291.554730	372685.286109	52.232359
3290.972334	372411.570020	52.237364
3290.458348	372128.178016	52.242369
3289.468264	371847.128033	52.247373
3288.993706	371565.402945	52.252378
3288.265026	371295.771505	52.257383
3287.682757	371007.067904	52.262388
3287.181585	370729.688815	52.267393
3286.535715	370452.510279	52.272397
3286.097668	370161.410422	52.277402
3284.866411	369884.454611	52.282407
3284.141636	369606.011600	52.287412
3283.873146	369318.257932	52.292417
3283.210751	369047.581105	52.297421
3282.215057	368764.041266	52.302426
3281.606252	368476.669615	52.307431
3281.069742	368205.481857	52.312436
3280.435103	367924.365888	52.317441
3279.656928	367648.053069	52.322445
3279.020091	367372.070047	52.327450
3278.337517	367096.016476	52.332455
3277.666531	366801.598162	52.337460
3277.146590	366527.318115	52.342465
3276.520106	366255.699030	52.347469
3276.208775	365968.892747	52.352474
3275.020938	365692.075796	52.357479
3274.594041	365393.433936	52.362484
3273.711810	365117.043725	52.367489
3272.833197	364850.976118	52.372493
3272.794188	364557.703737	52.377498
3271.722392	364282.280753	52.382503
3271.215400	363987.608822	52.387508
3270.323855	363712.176339	52.392513
3269.504170	363432.253448	52.397517
3269.099126	363160.294446	52.402522
3268.251545	362886.501623	52.407527
3267.962708	362598.546871	52.412532
3267.238795	362324.321986	52.417537
3266.253578	362046.426484	52.422541
3266.023401	361764.534098	52.427546
3264.765129	361488.893963	52.432551
3264.472948	361202.277379	52.437556
3263.775011	360924.223036	52.442561
3262.780404	360641.054192	52.447565
3262.735979	360363.011413	52.452570
3261.403083	360087.806523	52.457575
3260.959528	359813.185424	52.462580
3260.581834	359527.842962	52.467585
3259.809907	359259.022449	52.472589
3259.185338	358969.495869	52.477594
3258.319352	358696.821420	52.482599
3257.760603	358416.182074	52.487604
3256.396505	358132.804041	52.492609
3255.873828	357872.096590	52.497613
3255.265494	357583.727281	52.502618
3254.689906	357317.225778	52.507623
3254.326448	357042.750025	52.512628
3253.729154	356767.625558	52.517633
3252.554622	356496.184455	52.522637
3252.127821	356228.632918	52.527642
3251.499065	355952.999588	52.532647
3250.878623	355680.568124	52.537652
3250.123867	355415.941751	52.542657
3249.414314	355140.469405	52.547661
3248.930030	354858.597224	52.552666
3248.370155	354595.687548	52.557671
3247.332310	354312.430793	52.562676
3247.296709	354029.357068	52.567681
3246.080720	353766.274407	52.572685
3245.683731	353481.757823	52.577690
3245.511605	353206.587939	52.582695
3244.163091	352934.135681	52.587700
3243.512986	352654.770049	52.592705
3242.733508	352386.312823	52.597709
3242.435088	352099.811267	52.602714
3241.379978	351828.293955	52.607719
3241.095202	351554.175656	52.612724
3240.773272	351277.416167	52.617729
3239.654202	350998.145253	52.622733
3239.431072	350717.243947	52.627738
3238.672571	350441.952908	52.632743
3238.197110	350161.599921	52.637748
3237.485070	349880.395103	52.642753
3236.937588	349588.373283	52.647757
3236.190431	349309.104328	52.652762
3234.902145	349023.845494	52.657767
3234.725473	348735.087519	52.662772
3233.949043	348460.143286	52.667777
3232.960657	348175.056733	52.672781
3232.279848	347900.626990	52.677786
3231.714435	347620.832954	52.682791
3230.733232	347350.445598	52.687796
3230.007267	347070.217586	52.692801
3229.338072	346804.913081	52.697805
3228.956358	346521.442510	52.702810
3228.046873	346257.193559	52.707815
3227.815784	345980.258213	52.712820
3226.942311	345705.898925	52.717825
3226.195541	345434.925793	52.722829
3225.670836	345152.590663	52.727834
3225.080291	344890.900054	52.732839
3223.855074	344614.100830	52.737844
3223.547000	344329.942588	52.742849
3222.692760	344059.208743	52.747853
3222.433068	343780.865643	52.752858
3221.490997	343519.176468	52.757863
3220.889031	343245.519579	52.762868
3220.740049	342978.831973	52.767873
3219.793797	342701.032317	52.772877
3218.974895	342417.000640	52.777882
3218.144138	342137.753024	52.782887
3217.733495	341857.643202	52.787892
3217.252464	341597.747636	52.792897
3216.629033	341319.045080	52.797901
3215.594452	341038.222785	52.802906
3215.013920	340768.110456	52.807911
3214.107003	340491.003758	52.812916
3213.459950	340211.001097	52.817921
3213.153802	339945.952061	52.822925
3212.390296	339669.045218	52.827930
3211.593563	339386.493293	52.832935
3210.970506	339124.522131	52.837940
3210.541352	338842.387797	52.842945
3209.581089	338570.139772	52.847949
3209.412342	338283.300938	52.852954
3208.379580	338020.808650	52.857959
3207.889241	337741.706798	52.862964
3207.243718	337459.601614	52.867969
3206.232646	337184.453689	52.872973
3206.094113	336914.677464	52.877978
3204.909651	336639.708890	52.882983
3204.734361	336360.520163	52.887988
3204.135873	336076.516088	52.892993
3203.090282	335800.806725	52.897997
3202.700198	335513.073888	52.903002
3201.801819	335246.599776	52.908007
3201.161544	334967.661072	52.913012
3200.505963	334688.316301	52.918017
3200.107870	334412.896149	52.923021
3199.564267	334129.915469	52.928026
3198.611600	333855.885049	52.933031
3198.029197	333577.667106	52.938036
3197.273351	333299.222831	52.943041
3196.032566	333019.867384	52.948045
3195.784339	332739.730129	52.953050
3194.758874	332461.785645	52.958055
3193.811076	332197.518765	52.963060
3193.804048	331920.746397	52.968065
3192.766338	331667.563258	52.973069
3192.038404	331378.287752	52.978074
3191.482581	331103.462875	52.983079
3191.132362	330842.955873	52.988084
3190.278706	330563.852496	52.993089
3189.136845	330301.365712	52.998093
3189.023045	330025.416451	53.003098
3188.346384	329764.603811	53.008103
3187.343851	329492.036058	53.013108
3186.874466	329216.805282	53.018113
3185.899145	328950.873160	53.023117
3185.523674	328675.598245	53.028122
3184.674167	328415.979664	53.033127
3184.316956	328149.174631	53.038132
3183.814657	327870.939573	53.043137
3182.656341	327607.755829	53.048141
3182.340284	327328.570039	53.053146
3181.381316	327059.393828	53.058151
3180.679112	326797.146584	53.063156
3180.332467	326527.048819	53.068161
3179.467449	326265.106975	53.073165
3179.066369	325996.772322	53.078170
3178.326602	325722.130974	53.083175
3177.210612	325459.006652	53.088180
3176.867247	325182.004278	53.093185
3175.842899	324925.047145	53.098189
3175.337586	324660.058675	53.103194
3175.012397	324387.911183	53.108199
3173.987582	324121.430939	53.113204
3173.361605	323849.205128	53.118209
3172.911888	323584.456981	53.123213
3172.293909	323309.885604	53.128218
3171.907091	323046.346187	53.133223
3170.943852	322767.809560	53.138228
3170.649251	322498.321137	53.143233
3169.856796	322225.149280	53.148237
3169.023099	321957.354247	53.153242
3168.338565	321682.761560	53.158247
3167.514564	321414.122534	53.163252
3166.685069	321143.726890	53.168257
3165.910216	320877.444519	53.173261
3165.303087	320614.314308	53.178266
3164.829411	320350.931116	53.183271
3163.942373	320085.733735	53.188276
3163.836587	319813.986961	53.193281
3162.791598	319548.101589	53.198285
3162.685467	319280.298290	53.203290
3161.543016	319007.019673	53.208295
3160.910271	318743.682571	53.213300
3160.614473	318473.286385	53.218305
3159.842943	318192.100490	53.223309
3158.871934	317921.079153	53.228314
3157.812126	317654.272217	53.233319
3157.717631	317392.772505	53.238324
3157.421830	317118.654147	53.243329
3156.622068	316855.541764	53.248333
3155.788839	316570.082849	53.253338
3155.699865	316300.711766	53.258343
3154.695436	316021.796816	53.263348
3154.214917	315742.002062	53.268353
3153.662840	315470.237477	53.273357
3152.842241	315189.429374	53.278362
3151.574162	314914.297249	53.283367
3150.919814	314643.743419	53.288372
3150.429595	314363.537468	53.293377
3149.463222	314101.868714	53.298381
3149.286040	313830.950226	53.303386
3148.369214	313548.242677	53.308391
3147.566996	313282.265919	53.313396
3147.119289	313023.254102	53.318401
3146.639322	312745.764099	53.323405
3145.969011	312467.058088	53.328410
3145.040750	312207.081660	53.333415
3144.363761	311931.022441	53.338420
3144.208838	311656.171404	53.343425
3143.023804	311383.710237	53.348429
3142.442333	311101.241446	53.353434
3141.738659	310837.326636	53.358439
3140.979739	310557.712066	53.363444
3140.528756	310305.819853	53.368449
3139.643373	310034.626495	53.373453
3139.149134	309758.146183	53.378458
3138.189132	309487.600120	53.383463
3137.301163	309229.134096	53.388468
3136.798895	308959.628216	53.393473
3135.917996	308696.321881	53.398477
3135.601214	308425.458569	53.403482
3134.907147	308160.387256	53.408487
3134.161596	307885.470835	53.413492
3133.700858	307626.111839	53.418497
3132.676256	307355.238493	53.423501
3132.402353	307091.823149	53.428506
3131.565620	306822.978204	53.433511
3131.092543	306568.990047	53.438516
3130.516054	306295.006824	53.443521
3129.498894	306022.982048	53.448525
3128.971992	305752.782177	53.453530
3128.541246	305487.708072	53.458535
3127.273795	305220.917419	53.463540
3126.852215	304961.976142	53.468545
3126.358047	304696.859455	53.473549
3125.656854	304423.629767	53.478554
3124.869580	304168.414936	53.483559
3123.665088	303901.940380	53.488564
3123.511986	303633.019338	53.493569
3122.887141	303379.811333	53.498573
3122.396240	303116.929825	53.503578
3121.617710	302847.196595	53.508583
3120.892985	302572.080951	53.513588
3120.255656	302309.502134	53.518593
3119.451976	302052.679857	53.523597
3118.844603	301782.303083	53.528602
3118.069224	301521.655185	53.533607
3117.916925	301264.388389	53.538612
3117.427696	300984.364436	53.543617
3116.486712	300716.154844	53.548621
3115.789929	300444.949144	53.553626
3115.173341	300179.941748	53.558631
3114.383521	299920.386675	53.563636
3113.650747	299652.163924	53.568641
3113.229073	299389.539940	53.573645
3112.300018	299109.483674	53.578650
3111.686078	298843.580907	53.583655
3110.259427	298587.084666	53.588660
3110.240628	298327.164399	53.593665
3109.441065	298069.566624	53.598669
3108.686517	297800.705887	53.603674
3108.294599	297536.620435	53.608679
3107.696789	297275.752337	53.613684
3107.007775	297008.304200	53.618689
3106.222876	296754.545455	53.623693
3105.760190	296482.855847	53.628698
3105.152258	296220.102485	53.633703
3104.470851	295967.826447	53.638708
3103.858501	295682.333695	53.643713
3103.159099	295415.366995	53.648717
3102.358033	295154.095359	53.653722
3101.642014	294895.889647	53.658727
3101.044126	294625.593347	53.663732
3099.867155	294354.504063	53.668737
3099.377826	294111.510522	53.673741
3099.107450	293836.878383	53.678746
3098.291059	293569.748838	53.683751
3097.439542	293321.366142	53.688756
3097.183987	293053.401088	53.693761
3095.963903	292789.292465	53.698765
3095.699895	292523.568435	53.703770
3094.843750	292266.933814	53.708775
3094.049324	292012.758108	53.713780
3093.666666	291735.211631	53.718785
3092.561093	291484.372822	53.723789
3091.939114	291217.790223	53.728794
3091.617930	290959.991821	53.733799
3090.772857	290704.676028	53.738804
3090.208280	290439.940793	53.743809
3089.543113	290178.634429	53.748813
3088.858466	289918.222098	53.753818
3088.561647	289658.328648	53.758823
3087.621623	289395.972588	53.763828
3087.150698	289125.336142	53.768833
3086.299954	288872.640389	53.773837
3085.751831	288619.765108	53.778842
3085.178393	288348.813472	53.783847
3084.499339	288073.295591	53.788852
3083.696869	287813.841254	53.793857
3083.362041	287550.894176	53.798861
3082.817406	287274.052925	53.803866
3081.873429	287008.967897	53.808871
3081.040338	286751.044631	53.813876
3080.492287	286485.738145	53.818881
3079.775135	286219.517810	53.823885
3079.047579	285962.237130	53.828890
3078.424109	285689.888055	53.833895
3077.954111	285432.867987	53.838900
3077.071977	285158.703089	53.843905
3076.428960	284898.910396	53.848909
3075.807022	284636.134144	53.853914
3074.912511	284371.799640	53.858919
3074.084610	284122.019734	53.863924
3073.418950	283851.507940	53.868929
3073.067962	283597.647540	53.873933
3072.070719	283333.685272	53.878938
3071.720980	283068.669686	53.883943
3071.337569	282813.693020	53.888948
3070.413972	282543.222979	53.893953
3069.691946	282290.493395	53.898957
3068.834740	282020.927900	53.903962
3068.600790	281759.379197	53.908967
3067.654485	281497.977239	53.913972
3067.007392	281223.943399	53.918977
3066.632496	280978.206634	53.923981
3065.792547	280704.153955	53.928986
3065.153573	280446.619667	53.933991
3064.467944	280187.412178	53.938996
3063.470855	279913.232282	53.944001
3062.940519	279658.123047	53.949005
3062.732963	279403.442165	53.954010
3062.077217	279134.754461	53.959015
3060.957577	278877.325466	53.964020
3060.808806	278606.436641	53.969025
3060.194927	278346.857701	53.974029
3059.170814	278079.199130	53.979034
3058.629448	277814.488256	53.984039
3057.649418	277547.865549	53.989044
3057.572414	277281.266471	53.994049
3056.447092	277020.958183	53.999053
3056.049219	276755.941232	54.004058
3055.322341	276484.995410	54.009063
3054.678348	276222.464643	54.014068
3053.982237	275951.258196	54.019073
3053.199102	275693.207266	54.024077
3052.466647	275432.524258	54.029082
3052.180079	275164.583035	54.034087
3051.359662	274907.912765	54.039092
3050.671452	274631.431624	54.044097
3049.889966	274359.855784	54.049101
3049.464593	274100.443054	54.054106
3048.534570	273840.759711	54.059111
3047.735828	273571.121414	54.064116
3047.582496	273311.737747	54.069121
3046.821470	273048.866732	54.074125
3045.744958	272774.741828	54.079130
3045.282910	272506.369149	54.084135
3044.029091	272244.651120	54.089140
3044.008952	271987.535407	54.094145
3043.217471	271728.564763	54.099149
3042.768846	271464.747408	54.104154
3042.164388	271204.852953	54.109159
3040.701680	270932.371115	54.114164
3040.762509	270675.342214	54.119169
3039.759986	270409.020814	54.124173
3039.409104	270147.528560	54.129178
3038.928736	269878.825394	54.134183
3038.292547	269623.137119	54.139188
3037.658798	269356.115104	54.144193
3037.020138	269087.922192	54.149197
3036.323488	268809.067995	54.154202
3035.450688	268545.422432	54.159207
3034.626841	268278.177349	54.164212
3033.823107	268011.845466	54.169217
3033.347969	267751.187500	54.174221
3032.272776	267493.764407	54.179226
3031.608386	267220.862916	54.184231
3031.234904	266972.844552	54.189236
3030.457260	266704.571730	54.194241
3029.649238	266452.094004	54.199245
3029.009898	266196.862242	54.204250
3028.633889	265931.550981	54.209255
3027.616594	265674.906345	54.214260
3026.952767	265399.889725	54.219265
3026.371689	265137.694654	54.224269
3025.509824	264879.367607	54.229274
3025.119854	264615.229507	54.234279
3024.216278	264355.406706	54.239284
3023.657202	264096.314429	54.244289
3022.787558	263841.833864	54.249293
3022.307799	263592.634858	54.254298
3021.928558	263325.590946	54.259303
3020.713071	263079.930143	54.264308
3020.491990	262824.599764	54.269313
3019.801823	262571.667024	54.274317
3019.313347	262319.438306	54.279322
3018.341275	262053.233738	54.284327
3017.646157	261792.864888	54.289332
3017.293102	261531.851744	54.294337
3016.828655	261274.932447	54.299341
3015.825104	261008.656509	54.304346
3015.336108	260750.900810	54.309351
3014.586498	260496.551364	54.314356
3013.979605	260225.928799	54.319361
3013.374558	259971.860149	54.324365
3012.305619	259711.707411	54.329370
3012.143883	259443.224346	54.334375
3011.184386	259192.348688	54.339380
3010.647773	258929.226957	54.344385
3009.996940	258684.894741	54.349389
3009.110718	258421.858139	54.354394
3008.685222	258156.043164	54.359399
3008.190519	257892.837740	54.364404
3007.456894	257631.888846	54.369409
3006.880842	257366.124996	54.374413
3006.067049	257107.660183	54.379418
3005.118421	256839.897046	54.384423
3004.571231	256594.630125	54.389428
3004.244123	256325.258172	54.394433
3003.578505	256066.640696	54.399437
3002.782266	255806.644796	54.404442
3002.064459	255540.472211	54.409447
3001.406630	255275.435464	54.414452
3000.545647	255020.900869	54.419457
3000.230974	254752.214530	54.424461
2999.221693	254496.763007	54.429466
2998.513911	254226.972366	54.434471
2997.995266	253985.317236	54.439476
2997.451629	253714.072418	54.444481
2996.791341	253471.168165	54.449485
2995.737440	253201.436848	54.454490
2995.198264	252945.879805	54.459495
2994.382022	252692.051056	54.464500
2994.025404	252426.479438	54.469505
2993.120040	252170.832343	54.474509
2992.259396	251909.039863	54.479514
2991.704398	251657.000461	54.484519
2991.302646	251407.812847	54.489524
2990.337348	251144.663214	54.494529
2989.917422	250891.811469	54.499533
2988.931165	250638.165193	54.504538
2988.991999	250378.584326	54.509543
2987.954785	250134.701214	54.514548
2987.345013	249865.557274	54.519553
2986.523522	249609.030833	54.524557
2986.226262	249357.101051	54.529562
2985.082429	249097.140796	54.534567
2984.207933	248835.937652	54.539572
2984.036113	248579.249751	54.544577
2982.994436	248330.809416	54.549581
2982.519007	248077.739162	54.554586
2981.978204	247813.525253	54.559591
2981.000723	247572.027092	54.564596
2980.408891	247308.586231	54.569601
2980.102398	247062.873368	54.574605
2979.479588	246798.266587	54.579610
2978.830772	246537.637405	54.584615
2978.160118	246287.020986	54.589620
2977.499740	246020.027154	54.594625
2976.845869	245762.684697	54.599629
2976.471598	245509.649637	54.604634
2975.956259	245237.614422	54.609639
2974.843693	244974.620640	54.614644
2973.759582	244714.194434	54.619649
2973.223209	244462.996026	54.624653
2972.586482	244199.539519	54.629658
2972.249826	243930.327192	54.634663
2970.960907	243687.382146	54.639668
2970.258691	243427.604803	54.644673
2970.066443	243181.926007	54.649677
2969.158633	242929.748095	54.654682
2968.420182	242681.820013	54.659687
2967.715385	242416.874064	54.664692
2966.864468	242172.454687	54.669697
2966.787878	241915.042127	54.674701
2966.039883	241667.294829	54.679706
2965.629636	241400.567724	54.684711
2964.935772	241152.073092	54.689716
2964.093043	240879.511959	54.694721
2963.493013	240631.383800	54.699725
2962.550108	240384.995312	54.704730
2962.244989	240121.842454	54.709735
2961.413548	239866.496398	54.714740
2960.674704	239601.355353	54.719745
2960.196570	239352.851105	54.724749
2959.094653	239090.981538	54.729754
2958.885896	238842.890212	54.734759
2958.109970	238591.381594	54.739764
2957.197160	238325.940650	54.744769
2956.637558	238069.098489	54.749773
2955.628879	237820.712027	54.754778
2954.998168	237569.892832	54.759783
2954.543711	237319.349419	54.764788
2954.029999	237069.860574	54.769793
2953.323137	236810.931320	54.774797
2952.694239	236565.995880	54.779802
2952.078668	236297.297842	54.784807
2951.437323	236054.657168	54.789812
2950.605986	235800.232643	54.794817
2949.895124	235539.268363	54.799821
2949.484368	235294.042550	54.804826
2948.941199	235038.194581	54.809831
2948.466680	234781.036427	54.814836
2947.717863	234512.923896	54.819841
2947.156135	234257.258433	54.824845
2945.819840	234001.139944	54.829850
2945.253088	233741.401411	54.834855
2944.199118	233489.131794	54.839860
2943.976929	233238.859599	54.844865
2943.738857	232987.953814	54.849869
2942.995887	232737.185596	54.854874
2942.243319	232474.806722	54.859879
2941.370166	232227.932387	54.864884
2940.918593	231964.815286	54.869889
2940.015277	231707.760361	54.874893
2939.320905	231455.050324	54.879898
2938.522806	231198.156486	54.884903
2937.975009	230951.508606	54.889908
2937.487303	230704.163256	54.894913
2936.846022	230447.727690	54.899917
2935.798611	230205.444642	54.904922
2935.302965	229939.919130	54.909927
2934.792839	229689.676106	54.914932
2934.106863	229436.636829	54.919937
2933.579524	229189.733604	54.924941
2932.598335	228940.743745	54.929946
2932.131892	228684.612338	54.934951
2931.336146	228436.406551	54.939956
2930.662228	228181.049987	54.944961
2930.473687	227919.168139	54.949965
2929.883660	227660.360311	54.954970
2929.098880	227413.758756	54.959975
2928.269815	227157.411924	54.964980
2927.556262	226886.581464	54.969985
2927.136984	226637.983463	54.974989
2925.935522	226380.963215	54.979994
2925.718058	226126.525570	54.984999
2925.222178	225870.684463	54.990004
2924.186937	225622.448240	54.995009
2923.739519	225353.790862	55.000013
2922.909790	225106.462709	55.005018
2922.465684	224843.357208	55.010023
2921.716116	224601.313053	55.015028
2921.253200	224327.720249	55.020033
2920.686586	224068.762597	55.025037
2919.029616	223816.536252	55.030042
2919.173163	223551.448625	55.035047
2918.205935	223306.974075	55.040052
2917.726277	223052.434547	55.045057
2917.049670	222793.141857	55.050061
2916.257773	222544.284431	55.055066
2915.106566	222285.837867	55.060071
2914.733126	222033.981582	55.065076
2914.046832	221782.892295	55.070081
2913.541034	221532.893135	55.075085
2912.435955	221286.307271	55.080090
2912.080570	221027.905745	55.085095
2910.994383	220790.892267	55.090100
2910.622640	220539.573682	55.095105
2910.037129	220290.965910	55.100109
2909.357609	220047.034665	55.105114
2908.932492	219792.442012	55.110119
2907.891339	219541.494689	55.115124
2907.360855	219298.558179	55.120129
2906.510675	219047.935846	55.125133
2905.850530	218799.369644	55.130138
2905.456367	218551.344228	55.135143
2904.810814	218303.260488	55.140148
2903.673401	218045.992639	55.145153
2903.387154	217803.094160	55.150157
2902.629010	217557.806925	55.155162
2902.318182	217305.696036	55.160167
2901.357839	217065.435331	55.165172
2900.877123	216807.243491	55.170177
2900.304979	216562.334241	55.175181
2899.288403	216314.700579	55.180186
2898.710433	216055.075864	55.185191
2897.994548	215810.778642	55.190196
2897.247829	215571.783577	55.195201
2896.893160	215324.395734	55.200205
2896.264262	215071.937344	55.205210
2895.518121	214823.471824	55.210215
2895.122824	214583.069579	55.215220
2894.560046	214318.812617	55.220225
2894.202697	214058.442506	55.225229
2893.154434	213826.403584	55.230234
2892.631296	213557.329536	55.235239
2891.744698	213309.401173	55.240244
2890.975134	213044.648365	55.245249
2890.340320	212793.240932	55.250253
2889.579968	212543.943524	55.255258
2889.426764	212285.682241	55.260263
2888.695229	212028.793605	55.265268
2887.993013	211772.970080	55.270273
2887.437584	211520.534078	55.275277
2886.742956	211266.543936	55.280282
2886.271556	210996.119029	55.285287
2885.221966	210742.954874	55.290292
2884.568754	210488.119629	55.295297
2883.640607	210229.971183	55.300301
2882.169404	209970.795989	55.305306
2882.357848	209729.466431	55.310311
2881.192222	209487.783315	55.315316
2880.747676	209232.254074	55.320321
2880.439200	208985.129966	55.325325
2878.896502	208744.022594	55.330330
2878.464386	208493.712943	55.335335
2878.074629	208256.865605	55.340340
2877.360019	208003.181186	55.345345
2876.680730	207759.332076	55.350349
2876.004743	207516.819797	55.355354
2875.679857	207263.720273	55.360359
2874.629734	207027.893112	55.365364
2874.625575	206788.297967	55.370369
2874.282728	206532.695904	55.375373
2873.286883	206281.890920	55.380378
2872.716549	206021.606452	55.385383
2872.149438	205765.701414	55.390388
2871.208031	205516.569874	55.395393
2870.671440	205259.260936	55.400397
2869.732203	205003.447389	55.405402
2869.246937	204754.787678	55.410407
2868.249854	204504.128515	55.415412
2867.692807	204248.761305	55.420417
2867.093786	203994.140431	55.425421
2866.197556	203752.135430	55.430426
2865.412031	203494.747527	55.435431
2864.571126	203240.234121	55.440436
2864.202578	203005.919116	55.445441
2863.294455	202762.799064	55.450445
2862.784623	202515.996544	55.455450
2862.150795	202258.281387	55.460455
2861.360607	202021.151890	55.465460
2860.623033	201783.403143	55.470465
2860.038761	201532.148559	55.475469
2859.437519	201289.069952	55.480474
2858.923406	201041.471091	55.485479
2858.174692	200801.296112	55.490484
2857.632725	200555.307536	55.495489
2857.005100	200319.415918	55.500493
2855.953276	200068.360811	55.505498
2855.780628	199817.741875	55.510503
2854.757353	199578.661647	55.515508
2854.133354	199339.895858	55.520513
2853.814469	199085.765816	55.525517
2852.666426	198842.496103	55.530522
2852.018910	198598.454336	55.535527
2851.390066	198348.860467	55.540532
2850.813081	198114.240373	55.545537
2850.230750	197868.560727	55.550541
2849.295290	197626.569966	55.555546
2849.119658	197381.306236	55.560551
2848.268575	197147.894556	55.565556
2847.442823	196902.743629	55.570561
2846.946321	196653.387829	55.575565
2846.371721	196413.885375	55.580570
2845.574850	196159.096758	55.585575
2844.717925	195920.280717	55.590580
2844.613995	195668.048495	55.595585
2843.901401	195428.000352	55.600589
2843.118200	195183.052048	55.605594
2842.560337	194929.423716	55.610599
2842.305251	194683.750600	55.615604
2841.444799	194432.937885	55.620609
2840.942946	194172.404281	55.625613
2840.220328	193934.908882	55.630618
2839.452514	193671.228008	55.635623
2838.834657	193420.352273	55.640628
2838.198854	193170.689721	55.645633
2837.516686	192914.150338	55.650637
2836.549532	192662.509944	55.655642
2836.016665	192413.112763	55.660647
2835.374954	192162.195118	55.665652
2834.375632	191916.774252	55.670657
2833.945370	191660.018695	55.675661
2833.153577	191414.704324	55.680666
2832.603161	191166.587816	55.685671
2831.981249	190917.848144	55.690676
2831.146879	190670.163961	55.695681
2830.397844	190411.724374	55.700685
2829.230437	190177.959070	55.705690
2829.202686	189924.170975	55.710695
2828.439709	189686.062106	55.715700
2827.278374	189443.122324	55.720705
2826.994534	189198.048143	55.725709
2826.475838	188958.907671	55.730714
2825.895119	188714.535260	55.735719
2825.099110	188470.162453	55.740724
2824.493263	188226.203583	55.745729
2823.894612	187982.549924	55.750733
2822.988539	187740.642450	55.755738
2822.420765	187489.184071	55.760743
2821.952372	187242.864051	55.765748
2820.614351	187007.765766	55.770753
2820.292200	186753.061469	55.775757
2819.652164	186511.419022	55.780762
2819.186857	186274.240131	55.785767
2818.238160	186027.472807	55.790772
2817.929221	185792.865336	55.795777
2817.207934	185553.226071	55.800781
2816.830664	185301.197357	55.805786
2816.071739	185052.352873	55.810791
2815.628414	184804.944489	55.815796
2814.677068	184562.879839	55.820801
2814.051952	184307.118258	55.825805
2813.539990	184058.834046	55.830810
2812.812119	183807.291838	55.835815
2812.044783	183552.232463	55.840820
2811.398899	183306.201483	55.845825
2811.011086	183049.883330	55.850829
2809.697346	182808.193608	55.855834
2809.063409	182552.034351	55.860839
2808.556890	182305.602233	55.865844
2807.548870	182067.821141	55.870849
2807.400748	181816.405230	55.875853
2806.439100	181576.887700	55.880858
2806.152736	181333.132836	55.885863
2805.342345	181089.468622	55.890868
2804.632476	180848.549686	55.895873
2804.165559	180589.711558	55.900877
2802.878148	180349.300762	55.905882
2802.432504	180113.926257	55.910887
2801.930194	179858.075360	55.915892
2801.142547	179619.440285	55.920897
2800.700097	179370.796501	55.925901
2799.791264	179143.216684	55.930906
2799.037408	178895.773584	55.935911
2798.466462	178648.643957	55.940916
2797.948043	178407.487064	55.945921
2797.342646	178154.283322	55.950925
2796.389774	177926.092825	55.955930
2795.843375	177675.718885	55.960935
2795.516286	177438.033002	55.965940
2794.198480	177195.745927	55.970945
2793.653964	176955.032884	55.975949
2793.183794	176716.776752	55.980954
2792.021785	176468.333457	55.985959
2791.479682	176230.473614	55.990964
2790.538024	176008.244579	55.995969
2790.203997	175760.477583	56.000973
2789.382286	175533.140577	56.005978
2788.944619	175296.310638	56.010983
2788.050760	175058.987212	56.015988
2787.620765	174820.605916	56.020993
2787.317926	174585.499442	56.025997
2786.379474	174351.800507	56.031002
2785.723364	174107.506652	56.036007
2784.853388	173865.846132	56.041012
2784.131402	173639.887582	56.046017
2783.698279	173393.930564	56.051021
2782.836011	173172.591250	56.056026
2782.298642	172933.626698	56.061031
2781.843953	172699.254957	56.066036
2780.555461	172467.126148	56.071041
2780.369823	172221.667117	56.076045
2779.532189	171993.064138	56.081050
2779.266098	171757.341540	56.086055
2778.474867	171525.806589	56.091060
2777.671148	171283.333329	56.096065
2777.067347	171046.043432	56.101069
2776.237591	170817.711890	56.106074
2775.771294	170583.594177	56.111079
2775.137422	170343.348572	56.116084
2774.594164	170110.925718	56.121089
2773.872528	169864.883396	56.126093
2772.817017	169635.985472	56.131098
2772.557031	169394.612136	56.136103
2771.931757	169150.452707	56.141108
2771.154725	168921.332580	56.146113
2770.712513	168672.666189	56.151117
2769.794232	168439.908629	56.156122
2768.883962	168202.163883	56.161127
2768.582332	167970.015731	56.166132
2767.762369	167732.932232	56.171137
2767.460037	167495.685162	56.176141
2766.204036	167257.381029	56.181146
2765.708017	167025.996016	56.186151
2765.395715	166795.585780	56.191156
2764.439869	166557.475725	56.196161
2764.207054	166306.941774	56.201165
2763.547656	166079.329600	56.206170
2763.002419	165831.968404	56.211175
2762.096932	165587.049000	56.216180
2760.757095	165354.277504	56.221185
2760.609612	165111.775378	56.226189
2759.719347	164880.659582	56.231194
2759.170377	164638.330419	56.236199
2758.358116	164410.765593	56.241204
2757.557946	164182.093165	56.246209
2757.178898	163942.486463	56.251213
2756.595685	163715.865571	56.256218
2755.888191	163470.300714	56.261223
2754.872039	163232.129716	56.266228
2754.281254	163012.128424	56.271233
2753.740683	162777.885565	56.276237
2753.281184	162541.556705	56.281242
2752.331448	162302.921514	56.286247
2751.899948	162068.485766	56.291252
2750.724861	161837.956244	56.296257
2750.713571	161601.734006	56.301261
2749.632153	161365.785001	56.306266
2749.040984	161132.933481	56.311271
2748.471134	160906.248697	56.316276
2747.144351	160681.322615	56.321281
2747.128359	160448.821723	56.326285
2746.394042	160225.475798	56.331290
2746.025229	159989.895981	56.336295
2745.555592	159747.389881	56.341300
2744.505611	159523.592843	56.346305
2744.261271	159282.322861	56.351309
2743.386874	159050.536042	56.356314
2742.620956	158811.812732	56.361319
2742.021290	158578.417123	56.366324
2741.216596	158338.736502	56.371329
2740.935080	158102.363814	56.376333
2740.274120	157875.354840	56.381338
2739.972885	157627.642981	56.386343
2739.057390	157389.525780	56.391348
2737.968762	157149.226502	56.396353
2737.546805	156907.390209	56.401357
2736.848426	156677.061981	56.406362
2735.758209	156437.085126	56.411367
2735.531493	156192.676012	56.416372
2734.474816	155960.479887	56.421377
2734.002243	155721.520912	56.426381
2733.572985	155497.423470	56.431386
2733.079919	155261.446770	56.436391
2732.917001	155023.914304	56.441396
2731.696621	154777.877631	56.446401
2731.123850	154529.938571	56.451405
2729.961216	154292.009011	56.456410
2729.198761	154056.759500	56.461415
2728.312481	153823.656389	56.466420
2727.819273	153589.063102	56.471425
2727.097133	153347.108766	56.476429
2726.580273	153115.256591	56.481434
2725.719871	152888.080886	56.486439
2725.289998	152666.097854	56.491444
2724.366980	152440.830311	56.496449
2724.220191	152201.442586	56.501453
2723.232624	151966.244042	56.506458
2722.530512	151733.414352	56.511463
2722.041998	151497.586519	56.516468
2721.269698	151271.320786	56.521473
2720.684582	151028.530801	56.526477
2719.911086	150803.603268	56.531482
2719.102540	150568.344472	56.536487
2718.718175	150332.938320	56.541492
2717.595335	150101.398453	56.546497
2717.188948	149881.194953	56.551501
2716.621265	149648.367612	56.556506
2716.048292	149421.125002	56.561511
2715.579406	149189.834956	56.566516
2714.690719	148959.381032	56.571521
2714.277564	148715.698946	56.576525
2713.359799	148488.266545	56.581530
2712.510364	148259.857438	56.586535
2712.157536	148022.133234	56.591540
2711.242722	147793.496541	56.596545
2710.654872	147562.224104	56.601549
2709.945751	147329.409822	56.606554
2709.356937	147095.711785	56.611559
2708.657929	146867.056601	56.616564
2707.878975	146645.638747	56.621569
2707.921335	146405.428697	56.626573
2707.463412	146173.964681	56.631578
2706.098425	145940.508317	56.636583
2705.772585	145696.970907	56.641588
2704.845858	145465.845771	56.646593
2704.097470	145217.132542	56.651597
2703.160311	144991.771966	56.656602
2702.786548	144761.802808	56.661607
2702.096458	144536.237531	56.666612
2701.375024	144301.384763	56.671617
2701.412532	144072.265113	56.676621
2700.692669	143832.443807	56.681626
2699.899012	143592.166283	56.686631
2699.292177	143356.321077	56.691636
2698.118205	143111.318553	56.696641
2697.659825	142879.468732	56.701645
2696.912648	142648.941158	56.706650
2696.194941	142409.459547	56.711655
2695.470614	142177.418176	56.716660
2694.262377	141949.338675	56.721665
2693.672485	141717.226477	56.726669
2693.287395	141493.598793	56.731674
2692.308887	141272.273360	56.736679
2691.698690	141038.656197	56.741684
2691.126508	140824.180147	56.746689
2690.692541	140590.586689	56.751693
2690.252414	140360.975015	56.756698
2689.691658	140134.550987	56.761703
2689.136293	139895.745181	56.766708
2688.462825	139676.742268	56.771713
2687.474287	139431.085225	56.776717
2687.465311	139198.598005	56.781722
2686.211463	138966.083582	56.786727
2685.517096	138725.720513	56.791732
2684.130847	138492.520012	56.796737
2684.080719	138267.559080	56.801741
2683.327553	138040.546001	56.806746
2682.673268	137819.288811	56.811751
2682.655024	137578.627512	56.816756
2681.377415	137351.683214	56.821761
2680.892396	137120.715133	56.826765
2680.020993	136897.517979	56.831770
2679.512209	136667.688380	56.836775
2678.942902	136446.832345	56.841780
2678.301823	136209.655749	56.846785
2677.722992	135973.715894	56.851789
2677.223578	135748.034857	56.856794
2676.773443	135513.550739	56.861799
2675.716750	135278.180464	56.866804
2674.786807	135045.917094	56.871809
2674.450656	134805.012078	56.876813
2673.804748	134588.490351	56.881818
2673.395318	134348.478204	56.886823
2672.692012	134111.060157	56.891828
2672.027376	133872.480532	56.896833
2671.411023	133630.500666	56.901837
2670.706854	133404.463734	56.906842
2669.543682	133163.584875	56.911847
2669.005969	132924.774320	56.916852
2667.919516	132701.171660	56.921857
2667.387827	132472.061213	56.926861
2666.858744	132246.142125	56.931866
2665.938922	132017.940055	56.936871
2665.824922	131782.573327	56.941876
2664.722254	131561.192738	56.946881
2664.309517	131328.511263	56.951885
2663.643930	131101.009322	56.956890
2662.668279	130872.761282	56.961895
2662.175496	130644.101875	56.966900
2661.311094	130420.540473	56.971905
2660.778437	130188.561283	56.976909
2660.131840	129967.672849	56.981914
2659.163335	129739.990810	56.986919
2658.687678	129516.140489	56.991924
2658.039307	129301.687653	56.996929
2657.579492	129063.006608	57.001933
2656.685076	128846.362152	57.006938
2656.359428	128624.665618	57.011943
2655.673996	128393.882037	57.016948
2654.667276	128168.517983	57.021953
2654.129495	127945.400992	57.026957
2653.592158	127716.668482	57.031962
2652.745320	127492.933981	57.036967
2652.248813	127254.654067	57.041972
2651.422761	127034.147107	57.046977
2651.091311	126807.965714	57.051981
2650.345836	126591.972074	57.056986
2649.359535	126365.003566	57.061991
2648.700928	126135.477310	57.066996
2647.868935	125917.762190	57.072001
2647.549441	125700.647190	57.077005
2646.986719	125470.766348	57.082010
2646.359220	125253.160713	57.087015
2645.859106	125021.277476	57.092020
2644.975228	124797.301792	57.097025
2644.656451	124562.976672	57.102029
2643.878279	124336.978575	57.107034
2642.959371	124106.901928	57.112039
2642.489152	123885.047733	57.117044
2641.758998	123660.024824	57.122049
2641.091032	123426.898945	57.127053
2640.515549	123194.991552	57.132058
2639.713850	122978.727852	57.137063
2639.259476	122748.861567	57.142068
2638.471240	122525.915356	57.147073
2637.950159	122282.468531	57.152077
2637.225489	122065.473935	57.157082
2636.393270	121836.047631	57.162087
2636.089191	121608.197238	57.167092
2634.951513	121385.814692	57.172097
2634.659539	121153.658483	57.177101
2634.148143	120923.294916	57.182106
2633.137093	120684.544108	57.187111
2632.812639	120460.415851	57.192116
2631.952393	120228.414773	57.197121
2631.225245	119991.386987	57.202125
2630.701959	119766.573749	57.207130
2630.261598	119532.473544	57.212135
2629.414408	119303.094641	57.217140
2627.974532	119084.935344	57.222145
2627.486981	118853.351381	57.227149
2627.028713	118625.969383	57.232154
2626.174365	118410.141531	57.237159
2625.579375	118183.408834	57.242164
2624.700312	117960.448749	57.247169
2624.129128	117739.089255	57.252173
2623.160951	117515.436367	57.257178
2622.522165	117304.407299	57.262183
2622.134440	117084.329899	57.267188
2621.467281	116870.895112	57.272193
2620.799674	116653.117357	57.277197
2620.255339	116426.211797	57.282202
2619.336896	116215.378174	57.287207
2619.091609	115992.655106	57.292212
2617.712704	115782.970419	57.297217
2617.268183	115559.382825	57.302221
2616.718581	115343.805092	57.307226
2615.943688	115128.737490	57.312231
2615.500606	114909.384757	57.317236
2614.674364	114695.269187	57.322241
2614.322689	114476.717113	57.327245
2613.357897	114251.932975	57.332250
2612.762269	114034.772445	57.337255
2612.314464	113820.243080	57.342260
2611.239341	113614.040883	57.347265
2610.487552	113387.931534	57.352269
2610.299330	113171.609804	57.357274
2609.744383	112957.041766	57.362279
2609.412619	112736.962727	57.367284
2608.696700	112526.731383	57.372289
2608.103061	112288.511768	57.377293
2607.352621	112076.359043	57.382298
2606.649929	111841.400740	57.387303
2606.057419	111618.834734	57.392308
2604.944071	111401.795641	57.397313
2604.375489	111181.413629	57.402317
2603.858289	110955.093207	57.407322
2603.221960	110732.948178	57.412327
2602.824691	110504.489865	57.417332
2601.915918	110296.695984	57.422337
2600.857585	110059.501950	57.427341
2600.044476	109841.839472	57.432346
2599.491297	109629.608142	57.437351
2599.121686	109417.550267	57.442356
2598.180225	109193.412289	57.447361
2597.496755	108972.534058	57.452365
2597.000235	108755.943638	57.457370
2596.065096	108540.407795	57.462375
2595.802647	108321.647208	57.467380
2594.362607	108106.277289	57.472385
2594.159837	107893.161286	57.477389
2593.605464	107677.427457	57.482394
2592.817891	107469.456427	57.487399
2592.377876	107253.452419	57.492404
2591.338990	107038.136662	57.497409
2591.221209	106826.690769	57.502413
2590.545351	106606.655815	57.507418
2589.551414	106393.458227	57.512423
2589.213619	106166.803738	57.517428
2588.470781	105953.427014	57.522433
2587.587016	105724.990164	57.527437
2586.855493	105513.938828	57.532442
2585.976475	105312.450843	57.537447
2585.525860	105093.253232	57.542452
2584.453250	104881.693755	57.547457
2583.980413	104668.128714	57.552461
2583.127656	104466.274366	57.557466
2582.695043	104263.994184	57.562471
2582.214673	104043.857926	57.567476
2581.820238	103833.993913	57.572481
2580.854165	103615.798087	57.577485
2580.617982	103412.500393	57.582490
2579.758008	103195.432663	57.587495
2579.422552	102969.008050	57.592500
2578.030559	102763.525836	57.597505
2577.885822	102554.695838	57.602509
2577.665533	102335.189572	57.607514
2576.816695	102117.570142	57.612519
2576.163931	101889.812391	57.617524
2575.293471	101665.737764	57.622529
2574.385816	101448.260910	57.627533
2573.818427	101238.117014	57.632538
2572.673822	101012.171345	57.637543
2572.459979	100800.180358	57.642548
2571.570572	100593.258063	57.647553
2570.932759	100377.578597	57.652557
2570.435997	100166.625077	57.657562
2569.467412	99951.627795	57.662567
2568.739889	99732.236468	57.667572
2568.315561	99521.129821	57.672577
2567.493409	99319.658954	57.677581
2567.086353	99109.866701	57.682586
2566.317358	98905.673170	57.687591
2565.757387	98672.430708	57.692596
2565.156604	98469.500446	57.697601
2564.331672	98262.382684	57.702605
2563.608327	98045.943899	57.707610
2562.708418	97846.268814	57.712615
2562.707222	97630.395612	57.717620
2562.299302	97414.562028	57.722625
2561.379065	97206.878818	57.727629
2560.925194	96993.405129	57.732634
2559.997389	96770.214310	57.737639
2559.803986	96542.209436	57.742644
2558.889055	96328.458375	57.747649
2558.005680	96110.019680	57.752653
2557.524968	95890.308129	57.757658
2556.821581	95675.295134	57.762663
2555.931219	95440.882098	57.767668
2554.867525	95234.071035	57.772673
2554.149918	95028.306832	57.777677
2554.252696	94818.456473	57.782682
2552.950752	94602.444322	57.787687
2552.723970	94385.488656	57.792692
2552.142457	94171.851244	57.797697
2551.615106	93961.005164	57.802701
2551.097090	93738.126597	57.807706
2549.918949	93518.301206	57.812711
2549.437673	93296.251680	57.817716
2548.744023	93084.057981	57.822721
2548.022929	92870.741180	57.827725
2547.691248	92646.203258	57.832730
2546.539179	92434.245801	57.837735
2546.114549	92213.344928	57.842740
2545.025775	92003.157222	57.847745
2544.409608	91793.537795	57.852749
2544.054879	91575.492668	57.857754
2542.994718	91364.683641	57.862759
2542.871414	91146.571031	57.867764
2541.832550	90945.242419	57.872769
2541.246660	90735.557051	57.877773
2540.290521	90510.606008	57.882778
2539.363703	90317.576041	57.887783
2538.999948	90096.131775	57.892788
2538.504182	89893.672002	57.897793
2537.544713	89684.249903	57.902797
2537.366822	89470.660421	57.907802
2536.337280	89269.693056	57.912807
2535.597439	89045.987627	57.917812
2534.938992	88846.933669	57.922817
2534.245326	88646.548570	57.927821
2534.095833	88429.486347	57.932826
2532.951001	88229.016878	57.937831
2532.067353	88048.604972	57.942836
2531.575342	87771.781521	57.947841
2531.334469	87561.100241	57.952845
2530.672804	87349.693317	57.957850
2529.776031	87143.328022	57.962855
2529.257508	86923.220941	57.967860
2528.537109	86729.353259	57.972865
2527.706600	86514.981626	57.977869
2527.105612	86302.666338	57.982874
2526.677474	86102.016038	57.987879
2525.772099	85887.250476	57.992884
2525.063182	85683.549350	57.997889
2524.378857	85482.459577	58.002893
2524.117699	85268.020897	58.007898
2523.313911	85062.146268	58.012903
2522.595543	84842.562092	58.017908
2522.043220	84639.115986	58.022913
2521.091883	84434.642354	58.027917
2520.828667	84228.359052	58.032922
2519.655800	84016.162059	58.037927
2519.577412	83806.139746	58.042932
2518.681126	83606.681809	58.047937
2518.330939	83394.679670	58.052941
2517.255478	83181.991467	58.057946
2516.561244	82972.399096	58.062951
2516.091001	82759.357537	58.067956
2515.123604	82560.808774	58.072961
2514.826851	82353.748465	58.077965
2514.258607	82137.690888	58.082970
2513.403988	81923.200310	58.087975
2513.022959	81722.547665	58.092980
2512.309829	81512.534009	58.097985
2511.070817	81299.307432	58.102989
2511.095461	81084.541104	58.107994
2510.346688	80871.995823	58.112999
2509.612782	80655.726691	58.118004
2508.767416	80455.132727	58.123009
2507.949315	80248.478511	58.128013
2507.580399	80034.766041	58.133018
2506.823695	79829.405357	58.138023
2506.244401	79614.508639	58.143028
2505.513949	79401.466431	58.148033
2504.388273	79207.812955	58.153037
2504.264078	78984.668904	58.158042
2503.526615	78778.134689	58.163047
2502.973143	78556.057631	58.168052
2502.089543	78357.473748	58.173057
2501.377181	78142.740497	58.178061
2500.837804	77930.998555	58.183066
2500.268867	77726.537991	58.188071
2499.563217	77514.612737	58.193076
2498.785172	77301.148071	58.198081
2498.157249	77106.679079	58.203085
2497.820368	76889.198231	58.208090
2497.082076	76690.293394	58.213095
2496.276145	76467.011649	58.218100
2495.419941	76261.414896	58.223105
2494.600919	76050.689662	58.228109
2494.377964	75845.077244	58.233114
2493.283940	75639.488805	58.238119
2492.995034	75424.195412	58.243124
2492.534294	75229.219473	58.248129
2491.511917	75013.364229	58.253133
2490.814966	74798.374921	58.258138
2489.800838	74594.424835	58.263143
2488.996565	74386.274626	58.268148
2488.473462	74184.711050	58.273153
2487.635752	73998.719535	58.278157
2487.248166	73788.201913	58.283162
2486.468654	73581.037878	58.288167
2485.911530	73374.896683	58.293172
2485.188285	73183.509089	58.298177
2484.659386	72975.845008	58.303181
2484.066378	72781.395095	58.308186
2483.137785	72584.093935	58.313191
2482.549656	72365.413092	58.318196
2481.643233	72166.856463	58.323201
2480.989962	71976.329714	58.328205
2480.549890	71772.707009	58.333210
2479.565325	71573.814053	58.338215
2478.894122	71375.154645	58.343220
2478.153163	71174.778097	58.348225
2477.470946	70982.204396	58.353229
2476.929389	70785.100550	58.358234
2476.214274	70587.381478	58.363239
2475.901524	70394.515228	58.368244
2475.187046	70191.626233	58.373249
2474.520133	70003.591617	58.378253
2474.066133	69804.097916	58.383258
2473.246256	69611.147817	58.388263
2472.890699	69403.285204	58.393268
2471.575059	69203.652727	58.398273
2470.792289	69002.048146	58.403277
2470.696012	68814.452495	58.408282
2469.661619	68620.045471	58.413287
2469.280828	68421.921346	58.418292
2468.607640	68223.836358	58.423297
2467.899479	68028.447030	58.428301
2467.414907	67820.716840	58.433306
2466.536869	67630.171649	58.438311
2465.873164	67429.081286	58.443316
2465.200827	67236.780197	58.448321
2464.441620	67042.378473	58.453325
2464.353364	66844.668990	58.458330
2463.434107	66642.089375	58.463335
2462.602059	66443.864214	58.468340
2461.921027	66248.562599	58.473345
2461.300229	66056.770453	58.478349
2460.495875	65850.540333	58.483354
2459.699130	65668.264370	58.488359
2459.191661	65471.463350	58.493364
2458.631622	65279.883358	58.498369
2457.840331	65081.423110	58.503373
2457.704900	64882.389897	58.508378
2456.202905	64687.597995	58.513383
2456.059460	64490.750216	58.518388
2455.580535	64294.703200	58.523393
2454.509272	64101.332553	58.528397
2453.996569	63891.921680	58.533402
2453.267939	63701.665156	58.538407
2452.649613	63502.138135	58.543412
2452.183706	63311.979666	58.548417
2451.141963	63112.230876	58.553421
2450.907572	62912.187519	58.558426
2449.832691	62719.413334	58.563431
2449.233728	62509.606424	58.568436
2448.730842	62326.415627	58.573441
2447.954792	62146.498939	58.578445
2447.444674	61933.697680	58.583450
2446.649746	61748.945857	58.588455
2446.372722	61536.089809	58.593460
2445.217457	61354.856948	58.598465
2444.843392	61164.803796	58.603469
2444.407903	60958.647522	58.608474
2443.386602	60764.862060	58.613479
2443.223991	60561.616178	58.618484
2441.888429	60364.073327	58.623489
2441.466160	60176.857462	58.628493
2440.750230	59969.485310	58.633498
2440.172185	59784.656955	58.638503
2439.561978	59579.159030	58.643508
2439.057483	59387.775842	58.648513
2438.295175	59195.057141	58.653517
2437.951495	58991.635965	58.658522
2436.903830	58790.168416	58.663527
2436.099395	58585.334653	58.668532
2435.908636	58391.068440	58.673537
2434.869980	58197.595348	58.678541
2434.430438	58000.308629	58.683546
2433.442466	57797.516418	58.688551
2433.084018	57599.243956	58.693556
2432.703774	57405.330019	58.698561
2431.290811	57213.457287	58.703565
2430.803668	57006.684385	58.708570
2430.158025	56819.151023	58.713575
2429.592309	56623.812697	58.718580
2429.440310	56421.613611	58.723585
2428.438314	56237.694589	58.728589
2427.956191	56032.483042	58.733594
2427.304108	55832.136671	58.738599
2426.523758	55624.908543	58.743604
2425.786128	55437.175689	58.748609
2425.034950	55233.861904	58.753613
2424.590089	55023.066501	58.758618
2423.458293	54834.234656	58.763623
2422.645712	54635.549496	58.768628
2421.990110	54436.687429	58.773633
2421.287126	54242.897147	58.778637
2420.550193	54043.381388	58.783642
2419.925132	53862.150103	58.788647
2419.011554	53672.062969	58.793652
2418.583302	53484.396921	58.798657
2417.708428	53298.677758	58.803661
2417.390135	53107.898772	58.808666
2416.865350	52920.913360	58.813671
2416.157370	52729.146762	58.818676
2415.683269	52532.825529	58.823681
2414.498341	52349.055962	58.828685
2413.793661	52151.175328	58.833690
2413.194358	51967.562557	58.838695
2412.392467	51774.877462	58.843700
2412.091200	51593.383534	58.848705
2411.068994	51422.459556	58.853709
2410.791171	51220.835138	58.858714
2410.233150	51033.075197	58.863719
2409.378909	50837.469248	58.868724
2409.009378	50650.029111	58.873729
2408.083290	50468.722078	58.878733
2407.613649	50268.685697	58.883738
2406.670586	50092.870101	58.888743
2405.909179	49894.122515	58.893748
2405.210226	49705.607694	58.898753
2404.233071	49530.056342	58.903757
2404.124986	49334.179517	58.908762
2403.495615	49149.230261	58.913767
2402.507339	48963.020458	58.918772
2401.877894	48780.867728	58.923777
2401.099537	48597.317190	58.928781
2400.236104	48420.420104	58.933786
2399.566384	48239.229323	58.938791
2398.749135	48055.684233	58.943796
2398.431996	47878.135053	58.948801
2398.137888	47697.752739	58.953805
2397.566119	47515.440560	58.958810
2396.558113	47337.327360	58.963815
2396.178758	47146.129322	58.968820
2395.532478	46957.144604	58.973825
2394.713586	46777.987844	58.978829
2394.018100	46581.716865	58.983834
2393.307021	46415.067723	58.988839
2392.372603	46227.026006	58.993844
2391.936900	46036.864996	58.998849
2391.006713	45862.909377	59.003853
2390.386805	45683.390039	59.008858
2389.536333	45501.283940	59.013863
2388.793699	45320.304093	59.018868
2388.567994	45155.488906	59.023873
2387.641186	44982.601354	59.028877
2387.140055	44802.462115	59.033882
2386.358670	44626.459757	59.038887
2386.013025	44445.762259	59.043892
2385.214912	44263.541897	59.048897
2384.327537	44090.766516	59.053901
2383.700804	43910.543233	59.058906
2382.924398	43734.231709	59.063911
2382.534792	43558.954215	59.068916
2381.776967	43379.109805	59.073921
2381.152280	43212.967763	59.078925
2380.374971	43036.830677	59.083930
2379.482386	42854.589379	59.088935
2378.937363	42683.848156	59.093940
2378.158027	42504.566577	59.098945
2377.467193	42338.453046	59.103949
2376.515929	42177.307946	59.108954
2376.398438	42003.919860	59.113959
2375.630926	41832.812884	59.118964
2375.187074	41654.843208	59.123969
2374.376848	41484.269016	59.128973
2373.738059	41304.249977	59.133978
2373.116163	41139.439417	59.138983
2372.265644	40965.739950	59.143988
2371.995698	40788.840813	59.148993
2371.084907	40616.455845	59.153997
2371.284375	40446.433828	59.159002
2370.394170	40264.074861	59.164007
2369.549188	40085.653787	59.169012
2368.393302	39908.885995	59.174017
2367.609243	39736.202640	59.179021
2366.904226	39552.641551	59.184026
2366.461917	39385.008346	59.189031
2365.400581	39211.937333	59.194036
2365.183399	39043.917395	59.199041
2364.195355	38872.166334	59.204045
2363.638793	38704.432221	59.209050
2362.432751	38529.987085	59.214055
2362.086604	38370.230476	59.219060
2361.521863	38204.622787	59.224065
2360.747054	38037.732761	59.229069
2360.347040	37868.052083	59.234074
2359.852403	37714.982159	59.239079
2358.980795	37541.707636	59.244084
2358.280749	37372.212587	59.249089
2357.370560	37210.056014	59.254093
2356.913248	37037.440123	59.259098
2356.148520	36880.002282	59.264103
2355.630116	36717.963451	59.269108
2355.058312	36552.495270	59.274113
2354.065618	36386.113209	59.279117
2353.383729	36215.530810	59.284122
2352.801967	36056.423208	59.289127
2351.937722	35887.435157	59.294132
2351.393760	35716.713582	59.299137
2350.577187	35572.959960	59.304141
2350.049356	35406.377601	59.309146
2349.366051	35243.636413	59.314151
2348.931815	35083.936158	59.319156
2348.080316	34918.090782	59.324161
2347.270340	34769.712995	59.329165
2346.921014	34599.864109	59.334170
2346.427041	34447.644143	59.339175
2345.388974	34280.330326	59.344180
2344.638397	34114.332655	59.349185
2343.942416	33964.201677	59.354189
2343.434009	33802.060523	59.359194
2342.583641	33644.424841	59.364199
2341.592976	33495.332180	59.369204
2341.311452	33342.803582	59.374209
2340.236926	33191.531932	59.379213
2340.038680	33028.566343	59.384218
2338.909716	32884.602722	59.389223
2338.229282	32732.242422	59.394228
2337.950908	32576.248946	59.399233
2337.111678	32432.460876	59.404237
2336.188495	32280.642643	59.409242
2335.588791	32134.990458	59.414247
2335.217844	31979.173025	59.419252
2334.195021	31827.891363	59.424257
2333.122170	31683.870835	59.429261
2332.611380	31541.669406	59.434266
2331.908469	31406.819584	59.439271
2330.945194	31267.722200	59.444276
2330.445323	31129.786809	59.449281
2329.596031	31008.834452	59.454285
2328.680807	30869.225779	59.459290
2327.849934	30733.570899	59.464295
2327.018395	30605.569800	59.469300
2326.512369	30476.251710	59.474305
2325.724658	30351.209174	59.479309
2325.327181	30225.275118	59.484314
2324.157888	30108.591035	59.489319
2323.624710	29983.849213	59.494324
2323.171880	29868.148239	59.499329
2322.209047	29751.934183	59.504333
2321.452136	29631.646040	59.509338
2320.990402	29511.238645	59.514343
2320.011036	29388.209604	59.519348
2319.468580	29273.179487	59.524353
2318.836542	29159.304221	59.529357
2318.431804	29044.966942	59.534362
2317.641708	28934.365674	59.539367
2316.990808	28815.741477	59.544372
2316.370748	28703.559430	59.549377
2315.515727	28593.914036	59.554381
2314.698845	28472.938641	59.559386
2314.054701	28360.848299	59.564391
2313.573400	28249.164173	59.569396
2312.702578	28137.588484	59.574401
2311.948997	28032.718190	59.579405
2311.335681	27919.170365	59.584410
2310.495354	27817.567828	59.589415
2309.696019	27707.026455	59.594420
2309.271575	27605.834807	59.599425
2308.643325	27497.372068	59.604429
2307.954645	27389.439061	59.609434
2307.421066	27282.144417	59.614439
2306.746768	27180.589924	59.619444
2306.295616	27065.501680	59.624449
2305.493270	26965.137450	59.629453
2304.886712	26850.048731	59.634458
2304.315154	26741.894098	59.639463
2303.213531	26640.001481	59.644468
2302.798570	26533.775994	59.649473
2302.174430	26439.112184	59.654477
2301.448991	26323.642420	59.659482
2300.902019	26230.041895	59.664487
2300.128783	26122.592928	59.669492
2299.280684	26017.886861	59.674497
2298.620565	25914.806539	59.679501
2298.191955	25800.719024	59.684506
2297.448518	25705.345854	59.689511
2296.398521	25605.974268	59.694516
2296.333087	25502.683999	59.699521
2295.456105	25402.528119	59.704525
2294.889862	25290.823633	59.709530
2294.005078	25201.530611	59.714535
2293.370537	25094.279333	59.719540
2292.670669	24994.259975	59.724545
2292.333580	24903.676223	59.729549
2291.529981	24791.889035	59.734554
2291.153936	24695.525645	59.739559
2290.359629	24583.260677	59.744564
2289.474988	24479.145705	59.749569
2288.622537	24396.331165	59.754573
2287.888610	24297.055341	59.759578
2287.046945	24201.634502	59.764583
2286.273641	24109.035993	59.769588
2285.757884	24016.118813	59.774593
2284.851061	23938.125727	59.779597
2284.012489	23851.311055	59.784602
2283.317227	23769.294850	59.789607
2282.262979	23684.513323	59.794612
2281.786622	23604.977661	59.799617
2281.077258	23515.862571	59.804621
2280.131376	23441.021716	59.809626
2279.489631	23370.297017	59.814631
2278.823789	23292.196078	59.819636
2278.229399	23222.504263	59.824641
2277.124685	23149.389952	59.829645
2276.544642	23070.712473	59.834650
2275.972830	22996.919512	59.839655
2275.020906	22933.582747	59.844660
2274.765525	22865.655815	59.849665
2273.860266	22806.175694	59.854669
2273.389762	22737.226739	59.859674
2272.572312	22672.985706	59.864679
2271.976819	22602.936113	59.869684
2271.800611	22528.846678	59.874689
2270.753714	22461.556312	59.879693
2269.981959	22393.346428	59.884698
2269.572721	22327.617113	59.889703
2269.143889	22255.415538	59.894708
2268.514868	22183.276960	59.899713
2267.847440	22120.470040	59.904718
2267.329455	22036.563040	59.909722
2266.287141	21973.817607	59.914727
2265.154200	21911.271297	59.919732
2264.835111	21841.079531	59.924737
2263.776232	21780.440348	59.929742
2263.376931	21707.850276	59.934746
2262.596482	21661.481176	59.939751
2262.256565	21591.466322	59.944756
2261.474243	21527.799054	59.949761
2260.724294	21462.898091	59.954766
2260.233628	21392.764385	59.959770
2259.393589	21335.018848	59.964775
2258.412432	21273.887572	59.969780
2258.316058	21203.565483	59.974785
2257.263226	21153.766315	59.979790
2257.001575	21085.880716	59.984794
2256.598551	21027.775340	59.989799
2255.768277	20953.319243	59.994804
2255.040551	20880.874222	59.999809
2253.649908	20830.883990	60.004814
2253.223384	20768.799677	60.009818
2252.562770	20719.869010	60.014823
2251.660155	20667.930362	60.019828
2251.655464	20601.436603	60.024833
2250.793651	20542.812194	60.029838
2250.203987	20479.299282	60.034842
2249.850462	20421.208065	60.039847
2249.103455	20366.489887	60.044852
2248.460846	20291.150941	60.049857
2247.680771	20237.241901	60.054862
2247.151909	20169.712335	60.059866
2246.907213	20108.438759	60.064871
2245.995650	20043.004921	60.069876
2245.387103	19978.120224	60.074881
2244.475341	19911.785865	60.079886
2243.753161	19848.444992	60.084890
2242.965951	19779.818244	60.089895
2242.327892	19732.971631	60.094900
2241.639823	19668.556986	60.099905
2240.840141	19616.009588	60.104910
2240.389828	19563.288790	60.109914
2239.856097	19496.418761	60.114919
2239.041261	19439.465750	60.119924
2238.358903	19381.220930	60.124929
2237.788064	19314.125596	60.129934
2237.073159	19258.409640	60.134938
2236.488931	19199.838837	60.139943
2235.913364	19143.557237	60.144948
2235.249196	19076.455098	60.149953
2234.412806	19026.593562	60.154958
2233.894238	18965.007395	60.159962
2233.003073	18901.167852	60.164967
2232.145809	18847.119958	60.169972
2232.010201	18787.623445	60.174977
2231.417542	18729.074687	60.179982
2230.744962	18675.270800	60.184986
2229.943148	18601.485651	60.189991
2229.159247	18549.580634	60.194996
2228.587846	18480.231507	60.200001
2227.714114	18435.962617	60.205006
2227.306239	18373.792220	60.210010
2226.617803	18302.303079	60.215015
2225.868559	18257.561302	60.220020
2225.480153	18199.060069	60.225025
2224.495907	18145.417081	60.230030
2223.954198	18084.767506	60.235034
2223.672447	18026.275505	60.240039
2222.766203	17974.729861	60.245044
2222.334172	17906.312381	60.250049
2221.574299	17847.131431	60.255054
2220.961962	17778.176289	60.260058
2220.545796	17722.125078	60.265063
2219.356556	17661.149947	60.270068
2219.094738	17594.587113	60.275073
2218.173744	17541.205522	60.280078
2217.466272	17482.198666	60.285082
2216.972216	17412.387093	60.290087
2216.298889	17348.803859	60.295092
2215.755927	17292.077161	60.300097
2215.004937	17237.597426	60.305102
2214.215617	17175.650014	60.310106
2213.729140	17103.428097	60.315111
2212.777151	17051.033306	60.320116
2212.274288	16990.058617	60.325121
2211.898025	16930.720468	60.330126
2210.846431	16862.334180	60.335130
2210.309134	16806.028579	60.340135
2209.514856	16754.415389	60.345140
2208.820866	16683.488859	60.350145
2207.944661	16629.008816	60.355150
2207.142603	16565.788802	60.360154
2206.775948	16518.839937	60.365159
2205.749710	16468.250366	60.370164
2205.464439	16414.897993	60.375169
2204.716967	16363.850140	60.380174
2203.721927	16306.646197	60.385178
2203.579006	16256.857641	60.390183
2202.736269	16194.126454	60.395188
2202.612482	16130.956456	60.400193
2201.656973	16079.420345	60.405198
2200.677385	16016.340248	60.410202
2200.234437	15956.468554	60.415207
2199.426506	15900.827081	60.420212
2198.978352	15834.171946	60.425217
2198.189861	15790.368035	60.430222
2197.503638	15734.067817	60.435226
2197.041591	15673.388076	60.440231
2196.028557	15616.507246	60.445236
2195.682516	15558.175525	60.450241
2194.758871	15509.083766	60.455246
2194.118834	15458.192581	60.460250
2193.866938	15390.693339	60.465255
2192.902860	15346.555562	60.470260
2192.310755	15280.102688	60.475265
2191.569743	15228.736401	60.480270
2191.240367	15173.715621	60.485274
2190.362358	15113.655868	60.490279
2189.416911	15054.943260	60.495284
2189.106600	14997.647264	60.500289
2188.468261	14946.724171	60.505294
2187.931266	14888.049761	60.510298
2187.497805	14828.371728	60.515303
2186.798229	14771.143089	60.520308
2186.334180	14697.410660	60.525313
2185.469722	14641.157277	60.530318
2184.599682	14569.271120	60.535322
2184.060109	14513.915527	60.540327
2183.514465	14464.161706	60.545332
2182.918164	14396.192852	60.550337
2182.364597	14335.971394	60.555342
2181.242182	14268.959036	60.560346
2180.679499	14210.914046	60.565351
2179.572873	14158.322535	60.570356
2178.802447	14089.589851	60.575361
2178.553813	14036.392134	60.580366
2177.670859	13983.641247	60.585370
2177.130461	13928.802915	60.590375
2176.230791	13875.475285	60.595380
2175.865329	13812.473956	60.600385
2175.525991	13754.605703	60.605390
2174.566929	13690.895706	60.610394
2173.873477	13625.076774	60.615399
2173.550622	13584.003945	60.620404
2172.662037	13521.551455	60.625409
2171.986793	13477.155952	60.630414
2171.411138	13416.821530	60.635418
2170.634019	13348.421760	60.640423
2169.761984	13301.546316	60.645428
2169.181608	13244.615459	60.650433
2168.659810	13183.507876	60.655438
2167.768793	13126.881802	60.660442
2167.413892	13061.855767	60.665447
2166.417432	13022.375411	60.670452
2166.158618	12953.422493	60.675457
2165.506329	12903.999749	60.680462
2164.657882	12847.662843	60.685466
2164.292689	12786.476227	60.690471
2163.620080	12731.146213	60.695476
2163.159409	12661.614373	60.700481
2162.287505	12604.937846	60.705486
2161.798788	12542.736710	60.710490
2161.265865	12487.322003	60.715495
2160.283732	12420.490698	60.720500
2159.590071	12348.530345	60.725505
2158.807182	12296.960725	60.730510
2158.223978	12242.514555	60.735514
2157.736803	12175.893489	60.740519
2156.910990	12116.488307	60.745524
2156.265009	12052.712160	60.750529
2155.307440	11999.154039	60.755534
2154.532197	11926.127157	60.760538
2154.267543	11884.810034	60.765543
2153.428511	11829.048577	60.770548
2153.166104	11761.450632	60.775553
2151.875330	11702.308182	60.780558
2151.174790	11658.369078	60.785562
2150.790066	11593.191221	60.790567
2149.681690	11553.205831	60.795572
2149.023106	11488.963195	60.800577
2148.364428	11442.935065	60.805582
2147.738289	11389.203760	60.810586
2147.347641	11334.994697	60.815591
2146.741096	11289.092384	60.820596
2146.019730	11232.518108	60.825601
2145.290729	11181.897100	60.830606
2144.716595	11123.602707	60.835610
2144.688771	11057.280505	60.840615
2143.474382	11002.511931	60.845620
2143.045667	10946.939265	60.850625
2142.342505	10898.014749	60.855630
2141.498262	10841.951049	60.860634
2140.867081	10764.814252	60.865639
2140.180213	10724.036779	60.870644
2139.618197	10667.577824	60.875649
2138.867969	10617.714246	60.880654
2138.085446	10565.616024	60.885658
2137.647968	10508.468016	60.890663
2136.801749	10452.363340	60.895668
2136.325218	10391.094133	60.900673
2135.879913	10337.648188	60.905678
2134.799067	10287.745796	60.910682
2134.417884	10217.141175	60.915687
2133.414991	10170.077501	60.920692
2133.100857	10120.681178	60.925697
2132.437078	10062.105743	60.930702
2131.510250	10001.987751	60.935706
2131.141424	9938.580075	60.940711
2130.431527	9886.354701	60.945716
2129.623270	9829.169809	60.950721
2128.904925	9768.533592	60.955726
2128.094944	9726.541090	60.960730
2127.709494	9662.265268	60.965735
2126.815835	9618.740707	60.970740
2126.452809	9558.121915	60.975745
2125.874039	9502.383954	60.980750
2125.084887	9452.296804	60.985754
2124.721816	9390.095681	60.990759
2123.665530	9332.067119	60.995764
2123.123746	9275.554252	61.000769
2122.441881	9220.313573	61.005774
2121.703928	9154.997365	61.010778
2121.310788	9101.143728	61.015783
2120.465992	9044.219043	61.020788
2119.680235	8987.693620	61.025793
2118.937269	8931.690294	61.030798
2118.411066	8884.531452	61.035802
2117.729660	8829.998178	61.040807
2117.246646	8778.677524	61.045812
2116.438104	8719.311822	61.050817
2115.935042	8658.078980	61.055822
2114.915512	8608.177608	61.060826
2114.219009	8553.504095	61.065831
2113.555341	8503.845486	61.070836
2112.904095	8452.587028	61.075841
2112.588889	8396.147484	61.080846
2112.190905	8341.826455	61.085850
2111.534493	8271.609126	61.090855
2110.736370	8222.081801	61.095860
2110.074579	8161.154440	61.100865
2109.069891	8098.598075	61.105870
2108.084982	8048.435820	61.110874
2108.026607	7991.851084	61.115879
2107.262805	7941.671089	61.120884
2106.871298	7888.347247	61.125889
2106.117088	7827.037305	61.130894
2105.237063	7768.604321	61.135898
2104.748561	7709.165489	61.140903
2103.828251	7668.983790	61.145908
2103.117799	7603.711024	61.150913
2102.468371	7544.748939	61.155918
2101.568766	7481.498556	61.160922
2101.207212	7436.761036	61.165927
2100.533143	7390.332420	61.170932
2099.816968	7324.213520	61.175937
2099.120119	7277.271808	61.180942
2098.426624	7228.849584	61.185946
2098.284910	7164.903745	61.190951
2097.206380	7118.400564	61.195956
2096.518245	7063.283667	61.200961
2095.859287	7015.445362	61.205966
2095.445042	6964.527840	61.210970
2094.331611	6905.386052	61.215975
2093.861562	6853.802377	61.220980
2093.424952	6799.076165	61.225985
2092.750912	6748.447806	61.230990
2091.760870	6696.224621	61.235994
2091.569539	6644.792177	61.240999
2090.942765	6591.256999	61.246004
2090.215022	6528.059962	61.251009
2089.297745	6482.472446	61.256014
2088.761842	6423.484012	61.261018
2087.989997	6369.863034	61.266023
2086.992381	6314.368078	61.271028
2086.683826	6261.669623	61.276033
2086.172736	6202.758313	61.281038
2085.359270	6144.131125	61.286042
2084.636493	6092.559962	61.291047
2083.911212	6048.385280	61.296052
2083.339721	6000.430806	61.301057
2082.646880	5943.640389	61.306062
2081.854599	5891.247019	61.311066
2081.463713	5830.771022	61.316071
2080.713819	5787.500771	61.321076
2080.052102	5728.218956	61.326081
2079.702852	5678.044648	61.331086
2078.608053	5627.194881	61.336090
2078.095799	5562.529894	61.341095
2077.337007	5503.753561	61.346100
2076.883599	5450.180712	61.351105
2076.223275	5397.539750	61.356110
2075.550928	5351.401059	61.361114
2074.914158	5292.818643	61.366119
2073.990972	5245.762099	61.371124
2073.475233	5194.441144	61.376129
2073.391173	5130.901054	61.381134
2072.158669	5077.397968	61.386138
2071.457118	5011.167689	61.391143
2070.793960	4958.730824	61.396148
2070.402813	4897.722217	61.401153
2069.712285	4845.225655	61.406158
2068.846638	4801.922610	61.411162
2067.739483	4735.597026	61.416167
2066.954095	4694.117325	61.421172
2066.189926	4640.128927	61.426177
2065.694662	4590.103844	61.431182
2064.943528	4539.163246	61.436186
2064.702178	4492.539546	61.441191
2063.840276	4451.822954	61.446196
2063.260488	4401.352554	61.451201
2062.847517	4360.185901	61.456206
2062.091509	4306.750790	61.461210
2061.509548	4242.896693	61.466215
2060.567829	4206.415842	61.471220
2060.331617	4155.250213	61.476225
2059.647049	4105.826792	61.481230
2058.834387	4046.882662	61.486234
2058.362045	4003.370813	61.491239
2057.270584	3950.215383	61.496244
2056.906841	3898.217226	61.501249
2056.027393	3840.632398	61.506254
2055.115855	3796.223423	61.511258
2055.274991	3739.491772	61.516263
2054.140885	3696.337957	61.521268
2053.917709	3640.404824	61.526273
2052.962305	3584.826915	61.531278
2052.285328	3525.218775	61.536282
2051.749034	3473.005171	61.541287
2050.925881	3428.499994	61.546292
2050.133327	3378.523276	61.551297
2049.490817	3320.947190	61.556302
2048.589248	3279.142073	61.561306
2048.588411	3220.126120	61.566311
2047.695838	3176.836873	61.571316
2046.938314	3132.244716	61.576321
2046.427692	3079.397929	61.581326
2045.649618	3026.137528	61.586330
2045.160505	2967.573988	61.591335
2044.373270	2921.253584	61.596340
2043.786955	2864.455187	61.601345
2042.853329	2817.919307	61.606350
2041.998787	2768.683117	61.611354
2041.510713	2709.490278	61.616359
2040.803821	2665.565865	61.621364
2040.146551	2623.137212	61.626369
2039.850826	2570.245110	61.631374
2039.059766	2519.718957	61.636378
2038.328124	2462.935814	61.641383
2037.618640	2425.585593	61.646388
2036.871916	2369.302789	61.651393
2036.354365	2319.893507	61.656398
2035.423694	2277.667306	61.661402
2035.045973	2230.946487	61.666407
2034.357326	2185.738861	61.671412
2033.708394	2135.863904	61.676417
2032.953080	2080.989777	61.681422
2031.994812	2029.343446	61.686426
2031.794846	1980.851247	61.691431
2030.606686	1930.315176	61.696436
2030.240553	1882.495173	61.701441
2029.755941	1841.215893	61.706446
2028.916192	1796.850027	61.711450
2028.328451	1742.740314	61.716455
2027.516900	1701.004139	61.721460
2026.741349	1651.224229	61.726465
2026.487193	1603.714360	61.731470
2025.685664	1558.804972	61.736474
2024.855623	1502.527293	61.741479
2024.235220	1462.117016	61.746484
2023.702616	1417.114268	61.751489
2022.813085	1368.705993	61.756494
2022.079779	1324.568795	61.761498
2021.683935	1275.360677	61.766503
2020.918359	1227.734951	61.771508
2020.157934	1183.761084	61.776513
2019.825441	1140.062305	61.781518
2018.838433	1089.922844	61.786522
2017.889608	1046.103568	61.791527
2017.219076	1011.704716	61.796532
2016.669724	963.655566	61.801537
2016.044830	914.119866	61.806542
2015.635508	870.733801	61.811546
2015.285085	832.887802	61.816551
2014.180591	787.134033	61.821556
2013.416344	751.176786	61.826561
2012.616412	705.939973	61.831566
2012.043404	668.632182	61.836570
2011.458143	616.953161	61.841575
2010.812463	572.241791	61.846580
2010.247104	532.986199	61.851585
2009.966821	496.507417	61.856590
2008.966629	463.199571	61.861594
2008.334053	406.443258	61.866599
2007.634003	373.972398	61.871604
2007.191089	329.572031	61.876609
2006.560786	276.734638	61.881614
2005.209884	255.745004	61.886618
2004.594929	204.219663	61.891623
2003.874709	172.887500	61.896628
2002.900519	145.795519	61.901633
2002.393516	101.949506	61.906638
2001.094817	74.148194	61.911642
2000.652810	48.797238	61.916647
2000.092437	25.483580	61.921652
1998.870972	4.557802	61.926657
1998.115453	-9.161179	61.931662
1995.199948	53.946952	61.936666
1993.993783	53.870307	61.941671
1993.669936	67.303553	61.946676
1993.149402	62.477596	61.951681
1993.410253	64.832113	61.956686
1993.288605	63.700776	61.961690
1992.517114	59.697714	61.966695
1991.769222	64.490476	61.971700
1991.552026	72.069170	61.976705
1991.467425	62.788443	61.981710
1990.341818	73.421349	61.986714
1989.510023	70.543682	61.991719
1989.109835	67.049049	61.996724
1987.891053	76.900565	62.001729
1987.102663	75.678424	62.006734
1986.074842	77.763148	62.011738
1985.609292	69.037826	62.016743
1985.218877	71.163110	62.021748
1984.514723	71.741874	62.026753
1983.996505	74.429786	62.031758
1983.542624	75.534132	62.036762
1983.455896	64.656735	62.041767
1982.319825	76.780708	62.046772
1981.651549	77.555036	62.051777
1981.716165	72.103607	62.056782
1979.767136	78.443893	62.061786
1979.724316	69.572445	62.066791
1979.206387	81.717779	62.071796
1978.240607	73.562349	62.076801
1977.488192	71.262394	62.081806
1976.719187	66.440261	62.086810
1976.065718	78.854294	62.091815
1975.343546	82.737572	62.096820
1975.032991	75.433960	62.101825
1975.074614	72.835547	62.106830
1973.604522	87.393667	62.111834
1973.271540	73.611022	62.116839
1972.600485	72.971153	62.121844
1972.047433	74.377452	62.126849
1971.472726	73.725048	62.131854
1970.062618	80.103798	62.136858
1969.923687	76.310274	62.141863
1968.880251	75.789763	62.146868
1968.291708	77.095954	62.151873
1967.930769	68.838639	62.156878
1966.848061	76.332512	62.161882
1966.339871	77.388915	62.166887
1965.580649	72.554846	62.171892
1964.814255	76.188726	62.176897
1965.098074	65.244785	62.181902
1964.180632	76.596787	62.186906
1963.411930	65.405024	62.191911
1962.606378	68.397869	62.196916
1961.452329	72.298583	62.201921
1961.655113	61.675203	62.206926
1960.586203	79.207969	62.211930
1960.488424	73.068696	62.216935
1959.262113	65.458743	62.221940
1958.175072	73.243869	62.226945
1958.352823	76.094553	62.231950
1957.845290	77.634376	62.236954
1956.457802	67.796966	62.241959
1956.120390	77.076938	62.246964
1955.217464	77.424853	62.251969
1954.625138	67.318394	62.256974
1954.325527	84.430627	62.261978
1953.862129	71.456974	62.266983
1952.858284	73.987581	62.271988
1952.005509	76.504582	62.276993
1951.613378	71.142343	62.281998
1950.568471	75.601467	62.287002
1950.031247	77.341755	62.292007
1949.179042	70.243700	62.297012
1948.399834	81.504956	62.302017
1948.708422	71.424762	62.307022
1947.440703	85.731563	62.312026
1946.672341	76.835030	62.317031
1946.045354	65.474956	62.322036
1945.495195	77.194371	62.327041
1945.636970	65.814093	62.332046
1944.270478	85.392288	62.337050
1943.653210	75.883357	62.342055
1942.909421	68.925038	62.347060
1942.187652	73.423220	62.352065
1941.698699	69.217101	62.357070
1940.718196	73.475743	62.362074
1940.167162	81.738363	62.367079
1939.482485	71.116018	62.372084
1938.811137	74.186561	62.377089
1938.493929	77.078105	62.382094
1938.101669	79.888150	62.387098
1937.395577	76.742683	62.392103
1936.859123	70.994233	62.397108
1935.608318	87.696061	62.402113
1935.044778	72.214130	62.407118
1934.035281	77.670180	62.412122
1933.683241	74.625189	62.417127
1933.442346	65.212134	62.422132
1932.233342	74.046370	62.427137
1931.617187	64.527390	62.432142
1930.867173	71.617391	62.437146
1930.118893	75.801178	62.442151
1929.939987	75.231060	62.447156
1929.439188	76.578294	62.452161
1928.800766	68.503845	62.457166
1927.617160	71.594527	62.462170
1927.209708	73.365508	62.467175
1926.932874	73.090025	62.472180
1925.846563	69.882903	62.477185
1925.414563	64.606039	62.482190
1925.026855	74.540373	62.487194
1923.655717	76.064528	62.492199
1922.565985	63.921559	62.497204
1922.388002	80.474185	62.502209
1922.434475	71.013939	62.507214
1921.029322	72.147616	62.512218
1920.660163	79.869144	62.517223
1919.981715	74.524708	62.522228
1919.283036	77.410069	62.527233
1918.845032	67.870085	62.532238
1918.180578	73.649589	62.537242
1917.440833	73.456853	62.542247
1917.206758	76.511009	62.547252
1915.718382	79.441081	62.552257
1915.086358	75.349830	62.557262
1914.117442	74.144770	62.562266
1913.845403	73.729133	62.567271
1913.421860	68.115312	62.572276
1912.422434	71.540786	62.577281
1912.171620	76.744681	62.582286
1911.453484	80.845554	62.587290
1910.848634	77.284894	62.592295
1910.460193	73.035136	62.597300
1909.541220	78.973443	62.602305
1909.331805	72.200803	62.607310
1907.671805	77.451185	62.612314
1906.666266	72.917413	62.617319
1906.714237	66.753212	62.622324
1906.645153	76.976047	62.627329
1905.440805	72.926661	62.632334
1904.157338	77.649622	62.637338
1903.581839	75.446511	62.642343
1903.407731	77.239150	62.647348
1902.483648	79.366138	62.652353
1902.315434	80.151236	62.657358
1901.746632	74.506215	62.662362
1901.125823	75.364401	62.667367
1900.823546	72.881269	62.672372
1899.585603	72.709824	62.677377
1898.972872	77.747884	62.682382
1897.627644	74.282709	62.687386
1897.125790	70.590357	62.692391
1897.098485	73.485197	62.697396
1896.306114	75.301113	62.702401
1895.757391	69.868571	62.707406
1895.151354	74.261304	62.712410
1894.715020	70.423145	62.717415
1894.429669	67.403064	62.722420
1892.864980	78.852384	62.727425
1892.203143	71.997681	62.732430
1891.750573	70.262993	62.737434
1891.168178	64.433601	62.742439
1890.751580	62.010292	62.747444
1889.385183	72.304683	62.752449
1888.465646	61.439919	62.757454
1888.061486	66.189278	62.762458
1887.346958	74.624333	62.767463
1886.595363	62.443265	62.772468
1886.624618	69.305609	62.777473
1885.682088	71.776003	62.782478
1885.024769	74.987829	62.787482
1884.278372	72.695148	62.792487
1884.106021	64.677941	62.797492
1883.666545	73.300401	62.802497
1882.902938	62.933936	62.807502
1881.604520	69.373719	62.812506
1880.848439	78.267444	62.817511
1880.465251	71.010219	62.822516
1879.310061	65.891034	62.827521
1879.425274	68.447294	62.832526
1878.703027	76.786176	62.837530
1877.954022	65.536989	62.842535
1876.611593	64.724246	62.847540
1875.602117	64.629767	62.852545
1876.116660	68.319624	62.857550
1875.335880	69.753445	62.862554
1874.439499	64.604983	62.867559
1874.176931	64.649943	62.872564
1873.492767	64.563751	62.877569
1872.990769	60.817354	62.882574
1871.522844	67.149960	62.887578
1870.679007	67.446334	62.892583
1870.363915	63.046672	62.897588
1869.539619	78.033890	62.902593
1869.462180	69.747823	62.907598
1869.142894	70.655078	62.912602
1868.369215	68.372595	62.917607
1867.265856	68.285101	62.922612
1866.100278	72.301483	62.927617
1865.408151	82.006073	62.932622
1864.930551	76.307167	62.937626
1864.742562	76.298316	62.942631
1864.167820	70.073294	62.947636
1863.288358	71.977532	62.952641
1862.971627	73.293674	62.957646
1862.318124	66.952661	62.962650
1861.300714	66.305358	62.967655
1860.291044	68.043592	62.972660
1859.623292	74.597707	62.977665
1859.297175	69.955995	62.982670
1858.529994	66.331148	62.987674
1857.964281	64.847916	62.992679
1857.975343	64.193197	62.997684
1857.118939	69.838184	63.002689
1856.149780	66.922863	63.007694
1855.075376	75.580536	63.012698
1854.374860	68.344057	63.017703
1854.034349	64.823047	63.022708
1852.968870	76.502342	63.027713
1852.950034	67.713643	63.032718
1852.595292	73.006762	63.037722
1851.798726	62.432007	63.042727
1850.711867	62.536684	63.047732
1849.790742	71.257337	63.052737
1849.360227	70.036356	63.057742
1848.900692	73.965889	63.062746
1848.633227	68.541680	63.067751
1847.944795	71.928165	63.072756
1846.968783	77.997417	63.077761
1846.226337	71.032968	63.082766
1845.738875	70.001722	63.087770
1845.111515	71.741651	63.092775
1843.888981	63.767949	63.097780
1842.772544	74.528374	63.102785
1842.295027	67.985946	63.107790
1841.820067	65.017258	63.112794
1841.787299	74.375360	63.117799
1841.165426	67.105693	63.122804
1840.253975	78.037486	63.127809
1839.986585	68.060582	63.132814
1839.317767	67.786252	63.137818
1837.863626	72.581844	63.142823
1837.455015	55.678909	63.147828
1836.776685	73.493380	63.152833
1836.067740	67.776435	63.157838
1835.624907	68.967712	63.162842
1834.649950	78.427415	63.167847
1834.514859	71.355502	63.172852
1833.840390	68.323848	63.177857
1832.683664	66.226113	63.182862
1831.987834	65.892857	63.187866
1831.269664	73.948423	63.192871
1830.800988	65.859953	63.197876
1830.288277	73.731559	63.202881
1829.955915	73.759253	63.207886
1829.694697	72.157613	63.212890
1828.423976	73.525274	63.217895
1827.852549	67.435870	63.222900
1827.141763	75.123087	63.227905
1826.711675	67.677326	63.232910
1825.458376	67.696412	63.237914
1824.530642	70.291382	63.242919
1824.216159	70.078003	63.247924
1823.421502	75.179165	63.252929
1823.262525	75.076936	63.257934
1822.974563	73.298302	63.262938
1821.968509	79.641500	63.267943
1821.056793	68.444244	63.272948
1819.876956	72.311107	63.277953
1819.608439	66.155274	63.282958
1819.198836	69.198016	63.287962
1818.885422	76.437131	63.292967
1818.267604	65.331297	63.297972
1817.161641	71.361602	63.302977
1816.430146	61.726995	63.307982
1815.509755	64.137560	63.312986
1814.924225	69.995929	63.317991
1814.269309	63.170455	63.322996
1813.854432	62.845181	63.328001
1813.594343	67.556077	63.333006
1812.799172	67.635327	63.338010
1811.878806	69.250138	63.343015
1811.370438	67.048580	63.348020
1810.917015	65.239840	63.353025
1809.937527	69.722131	63.358030
1808.936383	71.034593	63.363034
1808.050431	68.950927	63.368039
1807.615161	61.780783	63.373044
1806.910169	69.299646	63.378049
1806.713466	66.486237	63.383054
1806.289207	65.695222	63.388058
1805.818294	66.277519	63.393063
1804.854202	66.657634	63.398068
1804.006104	68.131402	63.403073
1803.332333	68.954846	63.408078
1802.726694	61.505184	63.413082
1801.273310	63.213957	63.418087
1800.823678	61.831655	63.423092
1800.320545	71.635344	63.428097
1799.899036	60.870122	63.433102
1799.568699	58.739549	63.438106
1798.827471	67.228512	63.443111
1798.616816	62.147468	63.448116
1797.559539	72.231490	63.453121
1796.738164	65.401343	63.458126
1796.218063	67.062927	63.463130
1795.417374	71.663437	63.468135
1794.944851	63.735888	63.473140
1793.402876	75.106340	63.478145
1792.915787	64.388257	63.483150
1791.918735	65.108734	63.488154
1791.695999	72.716392	63.493159
1791.834893	63.009440	63.498164
1791.240206	74.524110	63.503169
1790.504311	70.021990	63.508174
1789.402385	68.977865	63.513178
1788.610738	71.562977	63.518183
1788.189337	72.374425	63.523188
1787.122906	76.611477	63.528193
1786.870523	71.923211	63.533198
1786.432696	70.298111	63.538202
1785.503083	65.387055	63.543207
1784.514535	63.491072	63.548212
1783.726914	72.190072	63.553217
1783.327437	67.292908	63.558222
1782.808169	65.007566	63.563226
1782.437676	73.097589	63.568231
1781.889923	67.906073	63.573236
1780.713035	80.516238	63.578241
1780.418198	70.174976	63.583246
1779.753853	68.143393	63.588250
1779.000488	74.589010	63.593255
1778.145955	64.594954	63.598260
1777.153990	69.225430	63.603265
1776.723068	68.589103	63.608270
1776.133530	69.876141	63.613274
1775.432883	66.496493	63.618279
1775.411927	61.491935	63.623284
1774.515774	68.353936	63.628289
1773.696470	66.813452	63.633294
1772.973611	65.093842	63.638298
1772.246162	69.487620	63.643303
1772.013847	69.699900	63.648308
1770.655940	71.667859	63.653313
1770.062892	68.903323	63.658318
1769.501088	69.648800	63.663322
1768.692048	74.291003	63.668327
1768.441408	66.860730	63.673332
1767.674509	78.715512	63.678337
1767.138583	79.630633	63.683342
1766.501395	71.055108	63.688346
1765.388045	73.360942	63.693351
1765.315232	69.826107	63.698356
1764.723179	75.159833	63.703361
1763.411486	70.031933	63.708366
1762.688703	70.841270	63.713370
1762.069559	78.654120	63.718375
1761.473100	68.253557	63.723380
1761.025757	72.001016	63.728385
1760.668721	66.122824	63.733390
1760.476814	69.670662	63.738394
1758.949862	68.358233	63.743399
1758.228752	70.026584	63.748404
1757.850509	78.580545	63.753409
1757.314611	63.162230	63.758414
1756.096389	64.704467	63.763418
1754.789055	65.692375	63.768423
1755.143737	68.611844	63.773428
1754.669188	75.548940	63.778433
1754.054765	75.703845	63.783438
1753.657223	69.688511	63.788442
1752.588758	70.375033	63.793447
1751.664803	67.056493	63.798452
1750.880401	76.072694	63.803457
1750.464983	74.747302	63.808462
1749.968026	72.942069	63.813466
1749.151419	62.640758	63.818471
1748.317186	61.749775	63.823476
1747.737032	67.833006	63.828481
1747.012686	61.181655	63.833486
1746.663487	71.704232	63.838490
1746.036043	71.685322	63.843495
1745.665036	68.848850	63.848500
1744.108958	72.550380	63.853505
1743.683032	70.108550	63.858510
1743.310801	65.665787	63.863514
1742.508721	69.860769	63.868519
1742.447811	64.921467	63.873524
1741.162973	72.101022	63.878529
1740.459137	71.862301	63.883534
1739.864347	74.951340	63.888538
1739.507079	70.133007	63.893543
1738.947256	67.313845	63.898548
1737.262636	82.113951	63.903553
1736.931307	71.154496	63.908558
1736.461908	65.841823	63.913562
1735.733289	71.985985	63.918567
1736.119569	65.529048	63.923572
1734.810114	71.621026	63.928577
1733.822776	70.867160	63.933582
1733.037270	69.452340	63.938586
1732.488982	72.617103	63.943591
1732.247381	71.670503	63.948596
1731.639520	80.509664	63.953601
1730.781658	65.976537	63.958606
1730.141623	65.396127	63.963610
1729.204541	71.351760	63.968615
1729.303316	60.597783	63.973620
1727.793636	68.314734	63.978625
1727.110148	63.417232	63.983630
1726.566862	61.308104	63.988634
1725.866954	69.580801	63.993639
1725.407023	56.701353	63.998644
1724.959922	70.722089	64.003649
1724.132393	66.394339	64.008654
1723.607783	64.009660	64.013658
1722.785181	66.481265	64.018663
1722.405622	65.624980	64.023668
1721.447805	73.598408	64.028673
1720.158909	70.495865	64.033678
1719.631616	63.986845	64.038682
1719.246469	65.962826	64.043687
1719.097634	62.789935	64.048692
1718.447122	67.217918	64.053697
1718.201711	68.685276	64.058702
1717.105408	63.251733	64.063706
1715.943816	69.284072	64.068711
1715.566345	56.252759	64.073716
1714.992195	60.352690	64.078721
1713.841041	63.212079	64.083726
1713.261194	59.619545	64.088730
1712.533899	59.843109	64.093735
1712.071802	57.274455	64.098740
1711.801815	69.660355	64.103745
1711.372549	65.537998	64.108750
1710.814810	60.337154	64.113754
1709.603656	69.000872	64.118759
1709.314171	55.487160	64.123764
1707.922876	66.690527	64.128769
1707.129044	70.216240	64.133774
1706.635865	61.474782	64.138778
1705.967880	67.865924	64.143783
1705.902992	59.496816	64.148788
1705.415136	65.196377	64.153793
1704.383685	72.972021	64.158798
1703.588533	65.557568	64.163802
1703.045675	64.117021	64.168807
1702.482084	60.705250	64.173812
1701.515595	65.321113	64.178817
1700.717814	64.107733	64.183822
1700.052217	65.280300	64.188826
1699.261635	65.889677	64.193831
1699.240208	55.909002	64.198836
1698.835363	66.382281	64.203841
1697.712562	68.109904	64.208846
1696.503171	65.765438	64.213850
1695.983730	75.286933	64.218855
1695.677438	61.969900	64.223860
1695.485492	62.011468	64.228865
1694.707398	68.607759	64.233870
1693.869292	62.148378	64.238874
1692.910891	69.256290	64.243879
1692.476065	67.439249	64.248884
1691.969471	68.276728	64.253889
1690.852683	71.763765	64.258894
1690.132672	64.817224	64.263898
1689.494555	73.381705	64.268903
1689.168136	66.708847	64.273908
1688.698751	70.454161	64.278913
1688.288475	69.919303	64.283918
1687.338594	61.662955	64.288922
1686.323235	68.920344	64.293927
1685.920900	70.231012	64.298932
1684.721445	73.675357	64.303937
1683.688331	67.860369	64.308942
1683.641709	67.672211	64.313946
1682.562660	71.913412	64.318951
1682.295512	71.049735	64.323956
1681.860827	62.564706	64.328961
1681.722235	66.779571	64.333966
1681.070421	59.007457	64.338970
1679.407425	74.388835	64.343975
1679.153755	67.665637	64.348980
1678.683555	64.379985	64.353985
1677.753264	71.594400	64.358990
1677.602308	63.058451	64.363994
1676.638311	69.139873	64.368999
1675.975706	58.594347	64.374004
1675.126170	64.908800	64.379009
1674.485743	61.771090	64.384014
1674.492336	56.511574	64.389018
1672.893602	68.351995	64.394023
1672.513038	63.049788	64.399028
1671.882292	62.271621	64.404033
1671.416269	66.030174	64.409038
1671.513642	60.824198	64.414042
1670.158915	62.978338	64.419047
1669.439947	67.476853	64.424052
1668.154361	70.964359	64.429057
1667.346837	67.056335	64.434062
1667.089214	58.769552	64.439066
1666.413289	68.096385	64.444071
1666.125726	67.481322	64.449076
1665.597210	62.257721	64.454081
1664.917439	68.593650	64.459086
1664.158803	60.659827	64.464090
1663.023012	58.890509	64.469095
1662.677213	62.343108	64.474100
1662.064883	64.715188	64.479105
1661.457745	61.361794	64.484110
1660.489473	59.979842	64.489114
1659.643716	70.875137	64.494119
1659.382580	64.501756	64.499124
1659.102485	65.084962	64.504129
1658.422785	72.114398	64.509134
1657.503497	71.076546	64.514138
1656.275715	75.677926	64.519143
1656.074082	67.158543	64.524148
1655.822053	70.375239	64.529153
1654.965555	78.268972	64.534158
1654.220663	64.449925	64.539162
1653.153251	76.518362	64.544167
1652.862417	64.000363	64.549172
1652.175283	70.717665	64.554177
1651.166109	75.713456	64.559182
1650.878311	70.048023	64.564186
1649.850986	69.539820	64.569191
1649.505695	61.457506	64.574196
1649.255156	70.734438	64.579201
1648.346075	68.733704	64.584206
1647.695936	59.654795	64.589210
1646.626669	75.560202	64.594215
1646.327149	71.380124	64.599220
1645.327883	70.482666	64.604225
1644.495299	65.232948	64.609230
1643.883818	65.767081	64.614234
1643.391785	74.417875	64.619239
1643.010392	66.110433	64.624244
1642.826418	62.178597	64.629249
1641.803970	69.024331	64.634254
1641.163182	58.469554	64.639258
1640.118255	60.972506	64.644263
1639.596645	62.653702	64.649268
1638.550552	63.309183	64.654273
1637.999269	63.521583	64.659278
1637.575284	60.350391	64.664282
1636.661796	63.906456	64.669287
1636.798463	57.142125	64.674292
1635.672537	62.934302	64.679297
1634.541569	69.967942	64.684302
1634.539725	55.967279	64.689306
1633.524427	66.921979	64.694311
1633.195860	66.881539	64.699316
1632.728208	72.733561	64.704321
1631.358960	64.113226	64.709326
1630.957557	63.512121	64.714330
1630.245400	66.267981	64.719335
1630.049402	63.444202	64.724340
1628.711161	75.750426	64.729345
1627.879381	74.760759	64.734350
1627.765059	65.763436	64.739354
1626.655181	69.171542	64.744359
1626.903310	63.040996	64.749364
1626.208551	67.071579	64.754369
1624.829643	64.677593	64.759374
1624.663914	53.847718	64.764378
1624.147530	72.264823	64.769383
1622.945653	62.461300	64.774388
1622.183979	63.994511	64.779393
1621.205990	66.286285	64.784398
1621.125808	64.695519	64.789402
1620.946578	60.461310	64.794407
1620.269924	62.284693	64.799412
1619.357360	57.680219	64.804417
1618.375829	58.066115	64.809422
1618.068396	53.009942	64.814426
1616.797443	53.861006	64.819431
1616.024644	52.579816	64.824436
1615.758335	60.064266	64.829441
1615.089014	63.985106	64.834446
1614.892372	59.502442	64.839450
1613.878096	66.736761	64.844455
1612.891350	60.519536	64.849460
1612.340656	56.652042	64.854465
1611.642848	54.827125	64.859470
1611.830138	55.969393	64.864474
1610.629321	71.485621	64.869479
1609.963273	56.450792	64.874484
1609.130020	54.196708	64.879489
1608.558763	64.736750	64.884494
1608.021394	62.018760	64.889498
1606.564901	61.177849	64.894503
1606.251869	55.930408	64.899508
1605.555960	57.107384	64.904513
1605.138354	69.131715	64.909518
1605.016238	54.797578	64.914522
1604.358496	65.295582	64.919527
1603.365765	65.444199	64.924532
1602.582010	60.982675	64.929537
1602.146828	60.152892	64.934542
1601.258708	59.797710	64.939546
1600.144905	62.789275	64.944551
1599.836320	61.742047	64.949556
1599.358130	67.288781	64.954561
1598.960909	59.490086	64.959566
1598.491079	55.799009	64.964570
1597.074108	66.723380	64.969575
1596.742908	61.464048	64.974580
1596.172279	62.325915	64.979585
1595.154241	68.164766	64.984590
1594.570184	65.279513	64.989594
1593.947975	67.694736	64.994599
1593.218100	62.498108	64.999604
1592.999698	64.544238	65.004609
1591.783595	68.308407	65.009614
1591.128303	65.171675	65.014618
1590.201153	67.939861	65.019623
1589.720952	65.287874	65.024628
1589.637295	60.117620	65.029633
1588.721790	72.051120	65.034638
1588.936438	64.467824	65.039642
1587.404635	67.348175	65.044647
1586.942382	63.304503	65.049652
1586.401012	62.596310	65.054657
1585.048655	75.257438	65.059662
1584.318145	67.811819	65.064666
1583.762375	59.193987	65.069671
1583.323643	62.523157	65.074676
1583.111571	57.898276	65.079681
1582.411189	66.791555	65.084686
1581.840619	54.738273	65.089690
1580.727714	61.063072	65.094695
1580.318698	58.544950	65.099700
1579.389046	59.989684	65.104705
1578.267866	58.647339	65.109710
1577.823871	54.335690	65.114714
1577.189406	63.398861	65.119719
1576.919211	63.035030	65.124724
1576.649820	61.455333	65.129729
1575.927599	63.624002	65.134734
1575.338061	64.464241	65.139738
1574.275803	60.516942	65.144743
1573.647381	57.341275	65.149748
1572.714677	56.733215	65.154753
1571.717089	73.046333	65.159758
1571.447197	57.448345	65.164762
1570.912221	68.478339	65.169767
1570.295527	60.686422	65.174772
1569.917539	51.244790	65.179777
1568.920320	63.316210	65.184782
1568.566442	63.967308	65.189786
1567.757634	66.143299	65.194791
1566.945335	65.717123	65.199796
1566.614524	59.669874	65.204801
1565.975950	72.358833	65.209806
1565.151365	56.996299	65.214810
1563.752238	66.420855	65.219815
1563.248889	62.523554	65.224820
1562.964353	52.573322	65.229825
1562.453431	60.275679	65.234830
1562.280916	51.032555	65.239834
1561.126616	60.102985	65.244839
1560.556597	64.280769	65.249844
1559.806019	60.477490	65.254849
1558.434250	67.675504	65.259854
1557.577500	63.871054	65.264858
1557.381886	67.675697	65.269863
1556.629800	60.941113	65.274868
1556.270769	64.037182	65.279873
1555.682176	68.941662	65.284878
1555.351367	60.466509	65.289882
1554.745203	65.969623	65.294887
1553.688647	66.459551	65.299892
1552.916320	62.614998	65.304897
1552.501502	58.469665	65.309902
1552.004099	63.016712	65.314906
1550.770260	66.391970	65.319911
1550.176732	55.957017	65.324916
1549.913666	58.954559	65.329921
1549.480649	58.984499	65.334926
1548.810741	52.562681	65.339930
1547.396627	58.857329	65.344935
1546.876976	53.099760	65.349940
1547.084218	55.778006	65.354945
1545.945792	57.502017	65.359950
1545.030914	54.031584	65.364954
1544.150470	60.923282	65.369959
1543.664965	60.288818	65.374964
1543.966526	62.228591	65.379969
1542.573017	66.409954	65.384974
1541.811894	55.573445	65.389978
1541.098153	62.870802	65.394983
1540.613558	56.760671	65.399988
1540.234722	64.372138	65.404993
1538.773672	62.560234	65.409998
1538.195853	53.642651	65.415002
1537.618273	58.386173	65.420007
1536.890042	60.188789	65.425012
1536.894009	60.113152	65.430017
1536.131000	62.967326	65.435022
1535.999182	54.868232	65.440026
1535.007493	57.712994	65.445031
1533.588913	61.391833	65.450036
1532.935002	57.287424	65.455041
1532.049478	64.914562	65.460046
1531.829512	55.504307	65.465050
1531.203262	60.943757	65.470055
1531.034641	54.549429	65.475060
1530.231519	53.963408	65.480065
1529.242796	61.346115	65.485070
1528.918926	57.619408	65.490074
1528.333340	67.971651	65.495079
1526.921941	62.459465	65.500084
1526.739977	60.578244	65.505089
1525.423048	65.953943	65.510094
1525.355701	55.857600	65.515098
1524.854636	63.850758	65.520103
1524.113305	57.702075	65.525108
1523.115848	54.118286	65.530113
1522.558589	67.864190	65.535118
1522.447560	52.614404	65.540122
1521.885521	52.859445	65.545127
1520.693814	63.607515	65.550132
1520.423524	58.360267	65.555137
1519.396266	65.196970	65.560142
1518.575011	61.830905	65.565146
1517.702319	56.767679	65.570151
1517.011345	65.604878	65.575156
1516.805024	57.460514	65.580161
1516.244411	58.311991	65.585166
1515.886252	61.296996	65.590170
1515.045573	61.283034	65.595175
1514.503404	65.253169	65.600180
1513.841757	67.095311	65.605185
1512.118919	73.062305	65.610190
1511.759409	59.214448	65.615194
1511.272912	68.593727	65.620199
1510.635116	72.058811	65.625204
1510.428500	64.090933	65.630209
1509.838006	67.750804	65.635214
1508.818202	57.341453	65.640218
1508.537713	59.962262	65.645223
1507.332005	62.650643	65.650228
1506.581027	59.588720	65.655233
1505.693653	64.172123	65.660238
1505.271016	62.653000	65.665242
1505.103538	67.133319	65.670247
1504.230894	61.935882	65.675252
1504.099728	60.578835	65.680257
1502.845752	62.454468	65.685262
1502.203877	58.811401	65.690266
1501.647190	63.208343	65.695271
1500.888649	62.941915	65.700276
1499.882646	63.961200	65.705281
1499.171413	66.379039	65.710286
1498.957751	61.414980	65.715290
1498.354269	62.858372	65.720295
1497.952255	60.206831	65.725300
1496.821802	50.399029	65.730305
1496.101238	55.333991	65.735310
1495.768128	61.466915	65.740314
1495.049664	60.407354	65.745319
1494.686388	60.293131	65.750324
1493.512684	61.433090	65.755329
1492.800610	69.150540	65.760334
1492.311950	56.509340	65.765338
1491.976845	60.601922	65.770343
1490.532938	63.372917	65.775348
1490.280775	55.579807	65.780353
1489.471378	61.997926	65.785358
1489.341944	50.461635	65.790362
1488.732038	58.989314	65.795367
1487.073772	60.597455	65.800372
1486.635948	57.910204	65.805377
1486.025593	68.420626	65.810382
1486.084343	63.833868	65.815386
1485.844932	65.728078	65.820391
1484.465271	64.667221	65.825396
1483.681557	62.216006	65.830401
1482.788430	71.859482	65.835406
1482.845160	64.694779	65.840410
1481.558830	66.398727	65.845415
1480.485394	65.283878	65.850420
1480.244968	61.274880	65.855425
1479.835404	68.472418	65.860430
1479.291494	67.547973	65.865434
1478.567368	65.380229	65.870439
1477.488511	62.638102	65.875444
1476.859347	56.506545	65.880449
1476.260908	69.873465	65.885454
1476.468410	57.858337	65.890458
1475.365106	57.985249	65.895463
1474.189445	59.904322	65.900468
1473.923263	57.681879	65.905473
1473.568962	60.505181	65.910478
1472.828128	58.757514	65.915482
1471.986792	59.157728	65.920487
1471.161504	70.204651	65.925492
1470.809403	59.555110	65.930497
1469.300850	65.248209	65.935502
1468.987055	57.937731	65.940506
1468.521437	64.647914	65.945511
1468.139224	62.097192	65.950516
1467.461447	56.177631	65.955521
1466.318494	67.897051	65.960526
1465.570095	60.984629	65.965530
1465.331892	65.599414	65.970535
1464.797572	64.386765	65.975540
1464.050468	51.978487	65.980545
1462.609649	56.852797	65.985550
1462.277186	60.930717	65.990554
1462.131815	53.922186	65.995559
1461.454235	68.435881	66.000564
1461.174605	58.430351	66.005569
1459.668026	61.415754	66.010574
1459.453209	57.669599	66.015578
1459.084816	58.047677	66.020583
1458.223993	72.044084	66.025588
1457.493426	57.656232	66.030593
1456.529560	61.561189	66.035598
1456.391443	63.944088	66.040602
1455.138199	69.481393	66.045607
1453.895978	75.484947	66.050612
1453.665476	65.071552	66.055617
1452.997041	66.582511	66.060622
1452.729875	66.945631	66.065626
1452.562585	63.199629	66.070631
1451.411610	66.920706	66.075636
1450.680401	64.821280	66.080641
1450.244239	60.072934	66.085646
1449.730651	58.360186	66.090650
1448.384169	61.324109	66.095655
1447.909035	66.991108	66.100660
1447.431139	61.945579	66.105665
1447.120028	63.752594	66.110670
1446.444781	60.643774	66.115674
1445.132217	66.129657	66.120679
1444.596980	69.537325	66.125684
1444.305977	59.006403	66.130689
1443.154460	58.555026	66.135694
1442.633649	59.199576	66.140698
1442.103618	56.744024	66.145703
1440.968625	62.040837	66.150708
1440.839400	59.987180	66.155713
1440.613598	64.705627	66.160718
1439.774706	56.717705	66.165722
1438.853586	63.242186	66.170727
1438.205110	67.451170	66.175732
1438.259965	64.396580	66.180737
1436.831866	61.904891	66.185742
1436.253424	61.236218	66.190746
1436.007472	62.430138	66.195751
1434.373445	69.923317	66.200756
1433.811530	67.659133	66.205761
1433.471456	66.035100	66.210766
1433.332015	68.840968	66.215770
1432.433007	62.525092	66.220775
1431.110836	66.536384	66.225780
1430.858792	54.747153	66.230785
1430.154026	66.259340	66.235790
1429.128667	62.981516	66.240794
1428.894278	62.373156	66.245799
1428.475136	60.905545	66.250804
1427.594136	57.537884	66.255809
1427.003187	58.149444	66.260814
1426.096394	52.485399	66.265818
1426.079627	59.704508	66.270823
1424.816655	70.477029	66.275828
1424.331944	59.182730	66.280833
1423.770877	66.552246	66.285838
1423.252273	60.153496	66.290842
1421.896169	56.094702	66.295847
1421.391986	53.219092	66.300852
1421.096582	53.198252	66.305857
1420.501623	65.232009	66.310862
1420.075641	53.383348	66.315866
1418.665655	57.728208	66.320871
1417.976297	64.807857	66.325876
1418.081274	58.913389	66.330881
1417.399360	62.607861	66.335886
1416.330892	57.041356	66.340890
1415.506493	55.046700	66.345895
1414.986413	66.622796	66.350900
1414.781993	61.537960	66.355905
1413.427851	68.451551	66.360910
1412.627262	59.951446	66.365914
1412.220154	60.275368	66.370919
1411.851836	65.195832	66.375924
1411.729304	56.496772	66.380929
1410.446090	65.562451	66.385934
1409.755649	69.338118	66.390938
1409.395864	57.231033	66.395943
1407.953572	60.085846	66.400948
1406.975336	58.951165	66.405953
1407.027621	60.904388	66.410958
1406.580395	58.185600	66.415962
1406.146820	52.175701	66.420967
1405.306850	61.525487	66.425972
1404.671204	56.220405	66.430977
1403.578998	55.818486	66.435982
1403.227316	64.140529	66.440986
1402.805450	61.255961	66.445991
1401.489246	63.721712	66.450996
1401.262758	59.971243	66.456001
1400.424549	55.657234	66.461006
1400.035697	51.471164	66.466010
1399.559135	57.560357	66.471015
1397.967913	53.190126	66.476020
1397.538574	46.992411	66.481025
1397.408649	50.396220	66.486030
1396.707761	55.666094	66.491034
1396.415112	55.396902	66.496039
1394.987771	60.472595	66.501044
1395.160494	38.701719	66.506049
1394.430988	47.816284	66.511054
1393.432771	56.618449	66.516058
1392.620860	47.615453	66.521063
1391.813719	59.730129	66.526068
1391.251784	50.211076	66.531073
1390.132500	60.448235	66.536078
1389.568641	61.581319	66.541082
1388.757623	57.048721	66.546087
1387.936799	56.832838	66.551092
1388.114157	51.619106	66.556097
1387.649093	54.503605	66.561102
1386.607637	56.823648	66.566106
1386.205587	48.206390	66.571111
1385.217283	59.284766	66.576116
1384.863525	51.566297	66.581121
1384.729678	52.793920	66.586126
1383.303636	57.734399	66.591130
1382.674243	54.343414	66.596135
1381.962490	56.116782	66.601140
1381.192227	50.022425	66.606145
1380.327958	56.756640	66.611150
1379.585181	52.498928	66.616154
1379.190292	54.308840	66.621159
1378.555900	51.189092	66.626164
1378.613070	49.349046	66.631169
1378.019610	53.204027	66.636174
1377.038841	59.857138	66.641178
1376.648125	53.499662	66.646183
1375.238372	56.799284	66.651188
1374.771192	48.208570	66.656193
1374.037052	52.232889	66.661198
1373.726165	56.388033	66.666202
1372.712497	49.489863	66.671207
1371.994525	61.147984	66.676212
1371.355982	49.545713	66.681217
1371.289537	53.151408	66.686222
1370.125650	48.564754	66.691226
1369.319039	48.517354	66.696231
1368.501644	52.820779	66.701236
1368.529303	51.979679	66.706241
1367.676164	63.274908	66.711246
1366.452218	51.678116	66.716250
1366.214900	43.234759	66.721255
1365.325546	56.852769	66.726260
1365.128555	46.636943	66.731265
1364.220648	56.739239	66.736270
1363.304181	52.127994	66.741274
1363.021960	47.571195	66.746279
1362.156292	60.342041	66.751284
1362.003263	53.229442	66.756289
1360.800680	52.869716	66.761294
1359.816856	56.969936	66.766298
1359.711036	41.679433	66.771303
1359.116184	54.499830	66.776308
1358.259559	47.720432	66.781313
1357.427763	54.520533	66.786318
1356.950691	56.481875	66.791322
1356.549751	43.305862	66.796327
1355.587430	52.207272	66.801332
1354.903541	44.040879	66.806337
1354.172732	44.992161	66.811342
1353.526134	53.337447	66.816346
1353.193294	54.346518	66.821351
1352.311508	52.650235	66.826356
1351.493630	42.025992	66.831361
1350.840616	52.058996	66.836366
1350.381580	51.187139	66.841370
1349.655470	42.309987	66.846375
1348.785089	56.602871	66.851380
1348.157313	46.840904	66.856385
1347.479458	49.134628	66.861390
1347.040543	59.080856	66.866394
1346.710270	48.733908	66.871399
1345.314568	59.108386	66.876404
1344.592690	51.817264	66.881409
1344.264513	59.710960	66.886414
1343.942202	59.360800	66.891418
1343.520084	49.665067	66.896423
1342.253330	54.406586	66.901428
1341.962937	53.188114	66.906433
1341.506740	47.244860	66.911438
1340.312890	51.729568	66.916442
1339.926974	43.294286	66.921447
1339.045003	49.784440	66.926452
1338.710571	44.232820	66.931457
1337.691390	59.108913	66.936462
1337.072505	56.861602	66.941466
1336.533224	54.327125	66.946471
1335.741117	59.817084	66.951476
1335.352811	58.557745	66.956481
1334.076428	56.003014	66.961486
1333.241494	49.297667	66.966490
1333.100548	46.047668	66.971495
1332.711270	52.144811	66.976500
1332.353525	54.731089	66.981505
1331.235777	56.916579	66.986510
1330.176649	58.985066	66.991514
1330.040052	50.518152	66.996519
1329.253979	65.016468	67.001524
1328.632338	53.869971	67.006529
1327.448381	52.269236	67.011534
1326.831472	44.827922	67.016538
1326.808992	51.136600	67.021543
1325.808961	53.597581	67.026548
1325.224291	47.053066	67.031553
1324.631616	50.226637	67.036558
1323.989086	49.752097	67.041562
1323.642967	46.740896	67.046567
1322.263188	53.540078	67.051572
1321.556494	53.402952	67.056577
1321.069928	48.647863	67.061582
1320.602216	57.176069	67.066586
1320.461731	44.793850	67.071591
1319.225498	51.983304	67.076596
1318.610550	52.076381	67.081601
1318.177748	50.613095	67.086606
1317.608143	54.276506	67.091610
1316.739625	46.343032	67.096615
1315.912753	48.870286	67.101620
1315.405962	42.272183	67.106625
1314.811933	35.797563	67.111630
1313.634055	46.448152	67.116634
1313.234261	44.401352	67.121639
1312.460343	45.903543	67.126644
1312.198196	45.174817	67.131649
1311.823193	39.127280	67.136654
1310.486044	35.310006	67.141658
1309.988542	42.260891	67.146663
1309.361651	54.221161	67.151668
1309.074843	47.490664	67.156673
1307.904153	42.802174	67.161678
1307.173357	50.460070	67.166682
1307.123927	45.140306	67.171687
1306.188116	48.152370	67.176692
1305.295404	49.603061	67.181697
1304.670420	53.467786	67.186702
1304.176497	52.688349	67.191706
1304.062836	49.895892	67.196711
1302.622448	53.562729	67.201716
1301.747135	48.875379	67.206721
1300.940617	48.267873	67.211726
1300.415268	45.229334	67.216730
1300.500877	47.014618	67.221735
1299.773523	55.457412	67.226740
1298.948525	47.620302	67.231745
1298.344836	47.979071	67.236750
1297.368190	55.964439	67.241754
1296.914561	51.615402	67.246759
1295.752916	54.504692	67.251764
1295.134719	54.250978	67.256769
1294.843982	53.509779	67.261774
1294.231732	54.872197	67.266778
1293.965621	47.879226	67.271783
1292.576447	53.890592	67.276788
1291.939477	55.304608	67.281793
1291.119575	51.869678	67.286798
1290.756714	46.642650	67.291802
1291.054656	50.565281	67.296807
1289.298401	57.045655	67.301812
1288.862917	48.891613	67.306817
1288.699164	45.090156	67.311822
1287.835224	42.424569	67.316826
1286.553644	48.581321	67.321831
1286.274020	51.136858	67.326836
1285.797756	44.516954	67.331841
1285.519133	50.708043	67.336846
1284.313471	52.575453	67.341850
1284.112629	45.677488	67.346855
1282.878107	51.700271	67.351860
1281.707748	49.022805	67.356865
1281.319817	41.660715	67.361870
1280.396626	54.159185	67.366874
1280.497387	41.258858	67.371879
1280.013809	50.733146	67.376884
1279.407841	51.182697	67.381889
1278.467212	46.750074	67.386894
1277.316763	49.833229	67.391898
1277.309069	40.183796	67.396903
1276.374696	54.126865	67.401908
1275.445357	49.266806	67.406913
1275.090774	43.049996	67.411918
1274.462118	47.972793	67.416922
1273.733324	46.367170	67.421927
1272.579267	52.065934	67.426932
1272.214725	40.513885	67.431937
1271.811039	41.769154	67.436942
1271.163677	49.143967	67.441946
1270.877101	46.420981	67.446951
1269.333414	51.490173	67.451956
1269.086108	47.921694	67.456961
1268.928380	47.570598	67.461966
1268.065712	49.880184	67.466970
1267.403743	39.584518	67.471975
1266.239145	46.755004	67.476980
1266.206019	48.206160	67.481985
1264.965335	45.971768	67.486990
1263.579814	45.663516	67.491994
1263.627789	51.828688	67.496999
1262.915200	48.585381	67.502004
1262.680214	47.200728	67.507009
1262.429040	44.276693	67.512014
1261.436002	58.729520	67.517018
1260.761044	44.980736	67.522023
1259.779634	52.850481	67.527028
1258.821285	50.807345	67.532033
1258.226718	46.399159	67.537038
1257.298500	51.810589	67.542042
1257.526065	46.596160	67.547047
1257.023014	52.764491	67.552052
1255.922057	38.588938	67.557057
1255.195647	38.795442	67.562062
1254.455113	46.168444	67.567066
1253.961133	42.547468	67.572071
1253.041768	38.599870	67.577076
1252.610371	50.131953	67.582081
1252.193347	39.001766	67.587086
1251.605773	48.407415	67.592090
1250.734803	47.012048	67.597095
1249.652478	48.104048	67.602100
1249.142234	46.542324	67.607105
1249.084734	46.959157	67.612110
1247.688182	55.667307	67.617114
1247.067004	42.003264	67.622119
1246.509066	44.017140	67.627124
1246.134129	45.561157	67.632129
1245.806985	37.439104	67.637134
1244.253135	50.512494	67.642138
1243.726252	51.499137	67.647143
1243.023355	52.031600	67.652148
1242.649055	42.486774	67.657153
1242.248217	43.790897	67.662158
1241.177682	52.034304	67.667162
1240.566518	46.237986	67.672167
1239.937598	45.951380	67.677172
1239.547501	46.112543	67.682177
1238.877130	41.710630	67.687182
1237.958984	51.157879	67.692186
1237.586682	37.635959	67.697191
1237.308121	50.280627	67.702196
1236.109511	43.482842	67.707201
1235.331215	38.289058	67.712206
1234.662967	47.988767	67.717210
1234.212722	44.385962	67.722215
1232.891667	46.986784	67.727220
1232.610740	43.922591	67.732225
1232.466450	38.301330	67.737230
1231.610850	45.210902	67.742234
1231.230418	45.475010	67.747239
1230.305889	44.463797	67.752244
1229.588975	49.906154	67.757249
1228.874737	49.125369	67.762254
1227.656142	51.219204	67.767258
1227.375057	39.800104	67.772263
1226.475360	46.961162	67.777268
1226.063986	44.496771	67.782273
1225.607162	46.390712	67.787278
1225.240666	46.714800	67.792282
1224.112443	48.250824	67.797287
1223.300912	52.875349	67.802292
1222.807591	49.110587	67.807297
1222.474870	51.595484	67.812302
1221.046818	45.689966	67.817306
1221.072045	40.456500	67.822311
1220.877110	42.737026	67.827316
1220.022781	44.344571	67.832321
1218.940091	39.919314	67.837326
1217.865426	49.160874	67.842330
1217.402537	43.547584	67.847335
1217.210663	40.952856	67.852340
1216.167096	46.927956	67.857345
1215.478542	43.747645	67.862350
1214.626702	44.519943	67.867354
1214.789400	43.086150	67.872359
1213.583663	45.386984	67.877364
1212.468997	47.565654	67.882369
1212.276304	45.417094	67.887374
1211.600544	48.612398	67.892378
1211.451603	40.815870	67.897383
1210.254798	51.011450	67.902388
1209.406458	44.828665	67.907393
1208.748641	46.268363	67.912398
1208.459206	52.050798	67.917402
1208.134561	39.444358	67.922407
1206.780082	49.872975	67.927412
1206.066459	46.209484	67.932417
1205.869332	44.274435	67.937422
1205.296744	50.585324	67.942426
1204.361721	48.626622	67.947431
1203.496266	51.289569	67.952436
1203.216795	45.043726	67.957441
1202.454097	39.195209	67.962446
1201.160362	50.218525	67.967450
1200.888600	50.071288	67.972455
1200.343962	50.408116	67.977460
1199.798587	53.633990	67.982465
1199.727178	49.976983	67.987470
1198.116555	47.863577	67.992474
1197.782914	49.719456	67.997479
1197.168033	48.093553	68.002484
1196.526177	51.392785	68.007489
1195.487662	49.091035	68.012494
1194.362789	46.641449	68.017498
1194.591198	45.337713	68.022503
1194.026448	49.395805	68.027508
1193.681769	48.608195	68.032513
1193.282459	40.285358	68.037518
1192.388781	38.987043	68.042522
1191.526314	35.038797	68.047527
1189.994108	44.017269	68.052532
1189.595581	48.513059	68.057537
1189.382681	44.850676	68.062542
1188.536499	54.206666	68.067546
1187.842122	43.447249	68.072551
1187.095633	52.141994	68.077556
1186.338489	49.402091	68.082561
1186.066029	41.099376	68.087566
1184.821608	55.585771	68.092570
1184.335349	45.707248	68.097575
1183.638452	54.954394	68.102580
1183.204836	40.907354	68.107585
1182.660379	35.984579	68.112590
1181.793292	45.783461	68.117594
1181.098223	47.771484	68.122599
1180.328616	48.755484	68.127604
1179.844663	47.704764	68.132609
1179.482563	46.737779	68.137614
1178.695044	52.999422	68.142618
1177.911593	42.168029	68.147623
1177.278174	45.735802	68.152628
1176.801802	48.328581	68.157633
1176.127181	43.890698	68.162638
1175.000965	51.862610	68.167642
1174.611446	42.680777	68.172647
1174.134013	41.664861	68.177652
1173.647019	47.096668	68.182657
1172.593800	42.268504	68.187662
1171.936818	52.619542	68.192666
1171.159178	47.180143	68.197671
1171.056266	52.356727	68.202676
1170.070153	44.134760	68.207681
1169.441985	41.477378	68.212686
1168.875083	46.343821	68.217690
1168.259551	35.724064	68.222695
1166.916565	47.530246	68.227700
1166.352227	46.434083	68.232705
1166.038262	34.087523	68.237710
1165.021934	49.094170	68.242714
1164.922832	42.391552	68.247719
1164.163839	45.168899	68.252724
1163.328705	45.121679	68.257729
1162.889026	45.002012	68.262734
1162.326014	45.936431	68.267738
1161.414564	45.027591	68.272743
1160.535605	44.666183	68.277748
1159.850355	44.044646	68.282753
1159.376107	37.298903	68.287758
1159.111365	44.703331	68.292762
1158.455280	44.603351	68.297767
1157.446033	38.011972	68.302772
1156.775482	54.534330	68.307777
1156.371366	44.695825	68.312782
1154.999024	46.682587	68.317786
1154.434827	43.903733	68.322791
1154.038484	47.299870	68.327796
1153.808585	44.937828	68.332801
1153.602700	46.150158	68.337806
1152.046456	47.742118	68.342810
1151.509881	38.340354	68.347815
1150.752663	48.163451	68.352820
1150.369208	43.221006	68.357825
1149.870996	42.191282	68.362830
1148.975900	45.062195	68.367834
1148.852953	37.276619	68.372839
1147.635215	40.508680	68.377844
1146.877048	36.760072	68.382849
1146.651588	44.007782	68.387854
1145.509255	45.809119	68.392858
1144.761990	35.525327	68.397863
1144.065093	41.227141	68.402868
1143.339085	51.886823	68.407873
1143.439260	45.235342	68.412878
1142.246938	52.060090	68.417882
1141.271145	46.534635	68.422887
1140.601044	50.085405	68.427892
1140.416316	43.864793	68.432897
1140.250877	45.240714	68.437902
1138.901296	57.469592	68.442906
1138.299349	49.015676	68.447911
1137.987849	38.476885	68.452916
1136.667485	53.894787	68.457921
1136.228662	42.287987	68.462926
1135.631077	50.875136	68.467930
1135.211992	55.188540	68.472935
1134.532576	52.146011	68.477940
1133.366561	50.876577	68.482945
1132.905586	48.245042	68.487950
1132.072856	49.280513	68.492954
1131.932806	52.796573	68.497959
1131.481411	49.885913	68.502964
1130.287634	57.589944	68.507969
1129.704753	43.686888	68.512974
1129.285027	50.521048	68.517978
1128.421948	45.793750	68.522983
1127.260433	50.308092	68.527988
1126.740583	51.211835	68.532993
1126.729119	43.112712	68.537998
1126.072843	56.024935	68.543002
1125.301766	54.693798	68.548007
1124.707772	58.456527	68.553012
1123.879056	48.967426	68.558017
1123.345060	42.218891	68.563022
1121.744309	46.133087	68.568026
1121.163059	40.814802	68.573031
1121.026492	43.005602	68.578036
1120.407614	46.470633	68.583041
1120.426844	45.484144	68.588046
1119.386424	46.099285	68.593050
1118.968790	39.992369	68.598055
1117.980566	45.860512	68.603060
1116.964296	50.421033	68.608065
1116.228835	38.511765	68.613070
1115.388972	47.017643	68.618074
1115.233557	53.015142	68.623079
1115.138798	52.716423	68.628084
1113.983374	48.616655	68.633089
1113.257097	48.373183	68.638094
1112.152935	51.746454	68.643098
1111.892438	49.206112	68.648103
1111.461135	51.779337	68.653108
1110.354250	45.711106	68.658113
1109.553096	41.504891	68.663118
1108.695809	52.745180	68.668122
1108.370224	47.793224	68.673127
1107.902775	49.041661	68.678132
1107.563379	49.102184	68.683137
1106.993362	49.261799	68.688142
1105.764547	50.017355	68.693146
1105.343673	50.236295	68.698151
1105.047286	49.522918	68.703156
1103.756705	46.546761	68.708161
1103.294462	54.956799	68.713166
1102.643486	50.242526	68.718170
1102.227623	41.752811	68.723175
1101.743039	51.867498	68.728180
1101.025396	59.597366	68.733185
1100.421362	50.485036	68.738190
1098.959274	53.833948	68.743194
1098.315878	47.624777	68.748199
1098.072824	49.792763	68.753204
1097.076228	49.873855	68.758209
1097.202235	45.517560	68.763214
1095.867293	56.875564	68.768218
1095.368199	53.797033	68.773223
1094.943379	46.448392	68.778228
1093.964087	50.477219	68.783233
1093.373106	45.494532	68.788238
1092.406962	51.718090	68.793242
1091.791367	46.502394	68.798247
1091.743589	48.661808	68.803252
1091.100988	48.924638	68.808257
1090.403065	44.923763	68.813262
1089.676703	46.805451	68.818266
1088.650634	48.213096	68.823271
1087.465619	42.032338	68.828276
1086.507594	56.417204	68.833281
1086.494930	49.097454	68.838286
1085.967975	57.008603	68.843290
1085.839853	51.829030	68.848295
1085.454026	47.239084	68.853300
1084.658287	45.768502	68.858305
1083.911155	37.766152	68.863310
1083.035698	47.468191	68.868314
1082.230204	46.007174	68.873319
1081.511713	37.781643	68.878324
1080.661839	54.146820	68.883329
1080.358408	44.158465	68.888334
1079.110496	44.876246	68.893338
1078.576845	44.803071	68.898343
1078.244499	43.830605	68.903348
1077.564691	56.421613	68.908353
1077.291982	47.387546	68.913358
1076.066443	48.153600	68.918362
1075.388425	48.720901	68.923367
1074.957391	47.084452	68.928372
1074.570250	49.181591	68.933377
1073.883408	37.894763	68.938382
1072.783037	48.029243	68.943386
1072.489219	41.898368	68.948391
1071.795335	39.122393	68.953396
1070.241889	53.714607	68.958401
1069.726078	47.304394	68.963406
1069.147305	48.700180	68.968410
1069.033356	41.995377	68.973415
1068.684544	36.024308	68.978420
1068.045859	49.524794	68.983425
1067.307942	52.257495	68.988430
1066.614590	55.376490	68.993434
1065.818014	54.176828	68.998439
1064.737106	45.425234	69.003444
1063.925896	47.607623	69.008449
1063.628253	44.161067	69.013454
1063.402161	45.291207	69.018458
1062.410867	48.964878	69.023463
1061.516486	49.812376	69.028468
1060.800029	46.748179	69.033473
1060.751145	41.354528	69.038478
1060.094178	45.714983	69.043482
1058.604045	45.050515	69.048487
1057.958129	37.581071	69.053492
1057.492917	42.470761	69.058497
1057.485241	44.311087	69.063502
1056.646619	40.345760	69.068506
1055.941816	45.449365	69.073511
1055.664732	39.883226	69.078516
1054.398794	48.971649	69.083521
1053.795423	43.918069	69.088526
1052.641297	52.359751	69.093530
1052.232290	52.144846	69.098535
1051.903524	53.618604	69.103540
1051.337283	59.416077	69.108545
1050.387727	44.950210	69.113550
1049.513144	54.622897	69.118554
1049.154665	49.858150	69.123559
1048.869942	48.007185	69.128564
1047.812892	45.047893	69.133569
1047.408973	42.363180	69.138574
1046.657937	43.487695	69.143578
1045.383732	51.700086	69.148583
1044.975106	48.041234	69.153588
1044.489154	48.812082	69.158593
1043.948964	36.306929	69.163598
1043.117372	49.107465	69.168602
1042.843066	41.691614	69.173607
1042.339637	37.533897	69.178612
1041.413330	41.912058	69.183617
1040.773370	37.566155	69.188622
1039.316993	48.513535	69.193626
1038.876003	51.568791	69.198631
1038.484175	51.727897	69.203636
1037.758053	45.051750	69.208641
1037.452199	42.221567	69.213646
1036.993295	46.233125	69.218650
1035.658261	45.237778	69.223655
1035.554259	44.626451	69.228660
1034.654170	45.490720	69.233665
1034.233243	35.518552	69.238670
1033.088522	48.543228	69.243674
1032.170950	49.321286	69.248679
1032.223212	46.799228	69.253684
1031.583204	45.067131	69.258689
1030.760350	43.669882	69.263694
1030.059844	46.275792	69.268698
1029.552223	42.981244	69.273703
1028.966297	39.263553	69.278708
1027.425887	46.159375	69.283713
1027.300979	42.766132	69.288718
1026.628572	48.291273	69.293722
1026.206556	58.157235	69.298727
1025.492413	47.547682	69.303732
1024.294256	46.093133	69.308737
1023.897835	40.486649	69.313742
1023.249196	41.996240	69.318746
1023.004798	39.526566	69.323751
1022.209938	35.864392	69.328756
1020.989822	44.257774	69.333761
1020.779175	35.162177	69.338766
1020.613115	46.725776	69.343770
1019.588216	49.538417	69.348775
1019.092860	42.649871	69.353780
1018.326982	45.717346	69.358785
1017.767928	38.780108	69.363790
1016.657752	41.319211	69.368794
1015.951535	51.054639	69.373799
1015.534548	43.377848	69.378804
1014.436845	49.051609	69.383809
1013.701294	47.011421	69.388814
1012.870970	46.213447	69.393818
1012.728138	40.588403	69.398823
1012.249172	47.939915	69.403828
1011.750856	46.853385	69.408833
1011.581962	39.265550	69.413838
1010.629826	41.809166	69.418842
1009.869781	51.196596	69.423847
1008.835572	42.823844	69.428852
1008.051135	43.550687	69.433857
1007.790293	39.036054	69.438862
1007.076359	41.718866	69.443866
1005.993530	42.450234	69.448871
1005.534896	37.821062	69.453876
1004.752186	46.396103	69.458881
1004.491799	36.058572	69.463886
1003.402421	47.859632	69.468890
1002.196105	45.660871	69.473895
1001.983912	36.534358	69.478900
1001.413429	48.115905	69.483905
1001.159023	42.058810	69.488910
1000.359442	42.486686	69.493914
999.894049	44.426319	69.498919
999.249008	44.312232	69.503924
998.372611	45.947668	69.508929
998.170929	44.840732	69.513934
996.686159	50.738671	69.518938
995.964230	52.108063	69.523943
995.563852	48.255972	69.528948
995.066523	49.762548	69.533953
994.221373	40.233672	69.538958
993.378337	49.837804	69.543962
993.142992	52.029734	69.548967
992.543937	46.539660	69.553972
991.807721	52.552548	69.558977
990.982713	50.603469	69.563982
990.415606	42.987127	69.568986
989.571263	46.406708	69.573991
989.602913	41.841195	69.578996
988.316789	47.286717	69.584001
987.476117	49.175759	69.589006
987.042285	39.493160	69.594010
986.243781	56.217414	69.599015
985.822437	47.216316	69.604020
984.797545	47.432532	69.609025
984.793516	54.676265	69.614030
983.831697	54.759713	69.619034
983.058315	59.146037	69.624039
982.436496	50.125985	69.629044
981.907700	58.882536	69.634049
981.463442	56.503535	69.639054
980.589343	51.738290	69.644058
979.605932	54.852105	69.649063
978.961548	49.679252	69.654068
978.342977	56.642596	69.659073
978.064486	49.378249	69.664078
977.283046	53.642801	69.669082
976.442670	56.768829	69.674087
975.947956	52.788825	69.679092
975.353681	57.653656	69.684097
974.370343	53.633790	69.689102
973.456086	47.602473	69.694106
973.323545	57.116506	69.699111
972.998541	57.369562	69.704116
971.467149	51.017250	69.709121
970.830572	47.714796	69.714126
970.441134	47.774031	69.719130
969.729317	51.012639	69.724135
969.528151	48.370178	69.729140
968.662464	59.702702	69.734145
967.918921	47.573023	69.739150
966.914912	48.271165	69.744154
966.555990	53.829856	69.749159
966.292308	46.645471	69.754164
965.085481	65.361922	69.759169
964.559173	54.363784	69.764174
963.879044	48.338553	69.769178
963.435767	57.231237	69.774183
962.939068	51.012362	69.779188
961.998135	51.755752	69.784193
961.149186	56.738406	69.789198
961.024587	58.088786	69.794202
959.979268	62.166444	69.799207
959.182865	52.118067	69.804212
958.441527	60.159090	69.809217
957.910260	52.207814	69.814222
957.693907	55.329991	69.819226
956.376208	51.304635	69.824231
955.938242	46.557066	69.829236
955.601808	55.823797	69.834241
955.121650	57.664916	69.839246
954.032923	56.731217	69.844250
953.212814	65.618185	69.849255
953.039561	52.032229	69.854260
951.742631	47.429799	69.859265
950.980829	53.919150	69.864270
950.061305	50.590558	69.869274
949.699202	63.430299	69.874279
949.574454	42.210560	69.879284
948.933208	48.029958	69.884289
948.487069	45.574316	69.889294
948.020001	57.806802	69.894298
947.287369	59.473280	69.899303
946.407686	47.204697	69.904308
945.159430	60.155943	69.909313
944.800300	45.539653	69.914318
944.507827	50.066233	69.919322
943.315093	50.383831	69.924327
942.652599	50.527331	69.929332
941.830452	56.317719	69.934337
941.446519	46.528294	69.939342
941.039141	47.368190	69.944346
939.729725	52.021180	69.949351
939.372536	47.971448	69.954356
938.439163	58.972954	69.959361
938.485924	50.291537	69.964366
937.971000	56.376656	69.969370
936.917351	57.542753	69.974375
936.130859	45.325314	69.979380
935.253681	49.583768	69.984385
935.057658	44.669246	69.989390
934.168170	47.350953	69.994394
933.021117	50.511354	69.999399
933.077082	41.693768	70.004404
932.193790	59.092112	70.009409
932.004899	51.407842	70.014414
930.814025	46.627790	70.019418
930.173437	50.428117	70.024423
930.234392	47.540251	70.029428
929.071502	53.695691	70.034433
928.213413	49.480317	70.039438
927.801544	46.892498	70.044442
926.875293	53.940513	70.049447
926.531625	50.964061	70.054452
924.905600	49.857936	70.059457
924.344277	49.058112	70.064462
924.226918	49.755184	70.069466
923.717019	48.931949	70.074471
923.667842	51.831689	70.079476
922.293470	47.182535	70.084481
921.611005	45.746262	70.089486
921.340243	45.217971	70.094490
920.272049	52.834607	70.099495
919.892434	44.282666	70.104500
918.864181	46.800258	70.109505
918.773342	47.467921	70.114510
918.114725	43.964395	70.119514
916.773910	51.325768	70.124519
916.511780	41.421942	70.129524
916.062178	55.579610	70.134529
914.896964	44.523954	70.139534
914.367649	40.238855	70.144538
913.237105	51.982244	70.149543
913.257518	38.250249	70.154548
912.734176	51.418760	70.159553
911.927611	53.882991	70.164558
911.372606	48.070800	70.169562
910.479654	56.181210	70.174567
909.784611	54.603416	70.179572
908.770716	52.316857	70.184577
908.153997	54.596608	70.189582
908.088812	51.249190	70.194586
907.333931	55.724715	70.199591
906.475722	47.035286	70.204596
905.606502	66.114286	70.209601
905.067792	47.684640	70.214606
904.780086	54.080164	70.219610
903.821950	55.829084	70.224615
902.835172	50.402275	70.229620
901.853891	56.084536	70.234625
901.781013	50.908543	70.239630
901.580926	45.143717	70.244634
901.097839	52.447785	70.249639
900.387523	43.880256	70.254644
899.282793	48.761865	70.259649
898.284708	47.820944	70.264654
897.594545	40.206357	70.269658
897.124173	43.194419	70.274663
896.635503	43.081588	70.279668
895.859196	46.697148	70.284673
895.526092	50.928732	70.289678
894.760201	44.390473	70.294682
893.691617	46.098315	70.299687
893.284996	44.032993	70.304692
892.634044	49.612098	70.309697
891.658101	50.022438	70.314702
891.307417	46.061198	70.319706
890.464225	56.963975	70.324711
890.232257	47.342730	70.329716
889.389244	51.881111	70.334721
888.639311	53.316495	70.339726
887.742516	41.573861	70.344730
887.808440	55.219305	70.349735
886.904186	48.684221	70.354740
885.588956	48.465873	70.359745
884.978762	47.888360	70.364750
884.960006	46.456826	70.369754
884.202620	52.148105	70.374759
883.434065	46.350787	70.379764
882.398526	45.940465	70.384769
882.070921	46.373566	70.389774
881.982627	44.499234	70.394778
880.631820	57.301086	70.399783
879.979246	40.523101	70.404788
879.029874	47.502056	70.409793
878.755351	46.668904	70.414798
878.680948	48.795377	70.419802
877.391576	56.213076	70.424807
877.089702	50.104522	70.429812
876.426157	49.810474	70.434817
875.814830	50.194679	70.439822
875.352012	42.147232	70.444826
874.041602	55.789220	70.449831
873.195744	41.476174	70.454836
872.058926	48.033711	70.459841
871.820367	51.806627	70.464846
871.609473	44.810176	70.469850
871.137011	41.919735	70.474855
870.292763	40.119626	70.479860
869.390073	47.245314	70.484865
868.554375	46.310925	70.489870
868.376732	39.028929	70.494874
867.433679	46.961615	70.499879
866.792959	38.789521	70.504884
866.214614	38.215239	70.509889
865.808639	33.821791	70.514894
865.143088	41.768913	70.519898
863.857714	54.034983	70.524903
863.468109	38.330977	70.529908
862.959781	47.756214	70.534913
862.265955	50.399681	70.539918
861.367464	47.693128	70.544922
860.484570	47.530201	70.549927
860.127113	44.614537	70.554932
859.450558	53.694009	70.559937
859.058071	50.399498	70.564942
858.708490	40.049241	70.569946
857.475461	50.933926	70.574951
857.050029	47.637955	70.579956
856.367188	46.194257	70.584961
855.544269	44.290633	70.589966
854.653239	43.496770	70.594970
854.388728	43.284367	70.599975
854.079473	41.998508	70.604980
853.189357	42.239032	70.609985
852.172456	44.520627	70.614990
851.731138	44.926632	70.619994
850.766903	49.291582	70.624999
850.692054	51.950600	70.630004
849.352716	46.293293	70.635009
848.719638	46.869110	70.640014
848.654109	42.792720	70.645018
848.167241	46.413574	70.650023
846.979240	49.380096	70.655028
845.945464	46.625276	70.660033
845.430640	49.916203	70.665038
845.273884	38.311677	70.670042
844.634820	45.892313	70.675047
843.886218	43.352316	70.680052
843.094874	46.990589	70.685057
842.430571	48.360392	70.690062
842.007762	36.650660	70.695066
840.798571	48.672378	70.700071
840.835164	45.250298	70.705076
840.013031	49.009102	70.710081
838.993086	55.377296	70.715086
837.960881	42.126778	70.720090
837.551241	47.559559	70.725095
837.211451	49.887796	70.730100
836.882858	47.131391	70.735105
835.853040	54.680680	70.740110
835.233015	50.640062	70.745114
834.510467	54.593376	70.750119
833.986517	48.970078	70.755124
833.052728	54.541193	70.760129
832.402924	52.940269	70.765134
831.965586	48.515486	70.770138
830.885166	63.921536	70.775143
830.817505	47.837533	70.780148
829.858007	44.878163	70.785153
829.168365	51.813426	70.790158
829.430292	47.565689	70.795162
827.935351	56.420237	70.800167
827.199537	48.417584	70.805172
826.498067	54.992133	70.810177
825.993010	46.138819	70.815182
825.206354	43.597843	70.820186
824.178755	50.777300	70.825191
823.902985	39.606034	70.830196
823.646996	51.269491	70.835201
822.687331	41.399511	70.840206
821.610287	34.442890	70.845210
820.998130	41.348693	70.850215
820.704038	42.537459	70.855220
820.512836	48.492527	70.860225
819.454596	51.904564	70.865230
818.872968	49.641082	70.870234
817.937256	53.112258	70.875239
817.173452	45.532800	70.880244
816.319026	55.696627	70.885249
815.662315	52.457644	70.890254
815.513428	46.146062	70.895258
814.832348	52.550944	70.900263
814.160936	48.804905	70.905268
813.242660	58.476412	70.910273
812.429552	54.854901	70.915278
812.176973	49.499709	70.920282
811.536017	56.116390	70.925287
810.333352	49.740198	70.930292
809.909795	45.542781	70.935297
809.013089	53.057035	70.940302
808.930537	44.625927	70.945306
808.557945	52.444327	70.950311
807.899149	45.186337	70.955316
806.932465	48.491908	70.960321
805.952010	44.263183	70.965326
805.020910	46.146823	70.970330
804.185530	46.641254	70.975335
803.829834	52.143739	70.980340
803.416047	48.734075	70.985345
802.983506	49.188709	70.990350
802.768863	44.789727	70.995354
801.276204	46.359454	71.000359
800.780308	40.747148	71.005364
800.163323	44.166096	71.010369
799.832080	41.678949	71.015374
798.753836	33.383279	71.020378
797.797452	49.401584	71.025383
797.690181	42.002941	71.030388
797.446905	40.398699	71.035393
795.889125	47.147561	71.040398
795.435964	46.134632	71.045402
795.025317	50.996043	71.050407
794.656397	51.850676	71.055412
793.620844	44.714856	71.060417
792.370374	50.619679	71.065422
792.191369	36.374396	71.070426
791.602259	52.645167	71.075431
790.983239	46.839622	71.080436
790.306576	39.634828	71.085441
789.456131	41.237038	71.090446
788.902873	44.921765	71.095450
788.327064	48.437471	71.100455
787.464540	34.817668	71.105460
787.138322	43.367810	71.110465
786.566661	46.705185	71.115470
785.725711	44.698486	71.120474
784.534628	46.878491	71.125479
784.106679	44.778152	71.130484
783.890751	39.955076	71.135489
783.073877	38.878146	71.140494
781.995275	36.256146	71.145498
781.290059	47.495659	71.150503
781.317842	42.802141	71.155508
780.956771	45.287964	71.160513
779.875849	49.249386	71.165518
779.103185	38.660587	71.170522
778.284890	51.002566	71.175527
777.542292	37.711542	71.180532
776.648168	33.701708	71.185537
775.911239	40.073526	71.190542
775.919627	39.412562	71.195546
775.303724	46.940684	71.200551
774.838787	46.521450	71.205556
774.082857	44.627681	71.210561
773.472380	48.596537	71.215566
772.450388	42.926339	71.220570
771.118170	41.670470	71.225575
770.563075	43.734426	71.230580
770.161468	40.121378	71.235585
769.496234	38.667573	71.240590
769.590329	37.952061	71.245594
768.708841	48.553918	71.250599
767.908937	43.373014	71.255604
767.218135	40.238559	71.260609
766.562411	43.164439	71.265614
766.160552	33.529696	71.270618
765.323659	39.323807	71.275623
764.866515	43.984773	71.280628
764.070094	34.676157	71.285633
762.756707	51.675697	71.290638
762.530652	46.513719	71.295642
761.962754	50.528174	71.300647
761.167140	45.311801	71.305652
760.285417	47.508286	71.310657
759.626556	48.649813	71.315662
759.479723	42.989953	71.320666
758.818490	44.842369	71.325671
757.524313	47.555142	71.330676
756.739796	48.818452	71.335681
756.287089	43.421372	71.340686
755.953923	39.160719	71.345690
755.348437	47.215183	71.350695
754.710549	39.710483	71.355700
753.615249	44.525768	71.360705
753.112523	47.704503	71.365710
752.664160	40.392717	71.370714
752.082310	42.492440	71.375719
750.714418	41.938961	71.380724
750.378977	34.083655	71.385729
749.887641	39.109272	71.390734
749.892502	32.080222	71.395738
748.444610	47.522767	71.400743
747.776530	41.040415	71.405748
747.234613	44.266913	71.410753
746.531293	42.575704	71.415758
746.435012	30.767431	71.420762
745.382032	38.759612	71.425767
744.619958	37.867105	71.430772
744.039172	38.234647	71.435777
743.433146	43.799354	71.440782
742.636939	41.054386	71.445786
741.816539	40.638816	71.450791
741.106695	41.967884	71.455796
740.917767	40.915221	71.460801
740.115411	42.851022	71.465806
739.782466	37.662364	71.470810
739.060169	42.792676	71.475815
738.468488	37.557558	71.480820
737.332369	35.552491	71.485825
736.452583	37.082371	71.490830
736.547681	39.633724	71.495834
735.502531	42.749866	71.500839
734.614818	38.819464	71.505844
734.281035	37.160867	71.510849
733.576140	38.417249	71.515854
732.955772	37.212722	71.520858
731.590497	32.120790	71.525863
731.391852	39.871096	71.530868
730.989682	36.126711	71.535873
730.477499	48.919508	71.540878
729.640033	39.959752	71.545882
728.475468	43.925643	71.550887
728.062391	41.798291	71.555892
727.905998	49.060208	71.560897
726.459374	50.023291	71.565902
725.785191	37.677740	71.570906
725.163929	43.965410	71.575911
724.768360	46.602795	71.580916
724.149129	41.317928	71.585921
723.649568	40.951601	71.590926
722.904466	29.886024	71.595930
722.101541	43.556337	71.600935
721.662284	35.883021	71.605940
721.299104	41.910569	71.610945
720.095707	41.758761	71.615950
719.648738	37.276045	71.620954
718.951846	41.734942	71.625959
718.394558	43.362726	71.630964
717.663453	40.798046	71.635969
716.467625	45.737131	71.640974
716.116593	40.272512	71.645978
715.756368	48.736118	71.650983
715.029080	43.774482	71.655988
714.223631	41.594357	71.660993
713.438301	41.657097	71.665998
713.240851	36.240374	71.671002
712.590988	48.718488	71.676007
711.561726	48.831306	71.681012
710.901098	42.502018	71.686017
710.027143	43.899860	71.691022
709.958761	38.774427	71.696026
708.862800	50.468888	71.701031
707.860861	48.192565	71.706036
707.544502	46.356126	71.711041
707.231487	56.456417	71.716046
706.864438	42.567815	71.721050
705.931153	44.872609	71.726055
705.262113	55.331901	71.731060
704.794633	48.303246	71.736065
703.148794	55.156031	71.741070
702.569271	41.149499	71.746074
701.676429	45.244097	71.751079
701.452942	48.663927	71.756084
701.442922	42.528293	71.761089
700.682016	49.297757	71.766094
699.724826	44.568919	71.771098
698.960429	46.855833	71.776103
698.799165	50.631297	71.781108
698.286879	46.239898	71.786113
697.225265	47.863301	71.791118
696.330681	42.449964	71.796122
696.271840	49.341110	71.801127
695.052803	44.599505	71.806132
694.675750	42.700838	71.811137
694.052457	42.770555	71.816142
693.235947	35.365152	71.821146
692.091564	41.355625	71.826151
691.606106	44.140245	71.831156
691.322716	33.933807	71.836161
690.572807	45.599768	71.841166
690.108807	31.593191	71.846170
689.066196	46.198988	71.851175
688.091757	46.050592	71.856180
688.205136	45.721357	71.861185
686.942862	45.793973	71.866190
686.116830	44.847304	71.871194
685.617741	56.600953	71.876199
684.996661	43.424520	71.881204
684.946277	35.421709	71.886209
684.145291	44.331064	71.891214
683.300326	47.072283	71.896218
682.604157	46.645702	71.901223
682.041090	45.176775	71.906228
681.624172	37.168869	71.911233
680.434396	49.028605	71.916238
679.952764	43.177442	71.921242
679.262934	38.297023	71.926247
678.610439	41.161573	71.931252
677.563692	37.922338	71.936257
676.763773	44.143914	71.941262
676.605885	30.004377	71.946266
676.184743	40.765379	71.951271
675.574396	43.129318	71.956276
674.530800	42.199006	71.961281
673.691290	49.414938	71.966286
673.083356	48.136056	71.971290
672.991071	35.793850	71.976295
672.419424	47.372039	71.981300
671.636920	50.014143	71.986305
671.263551	46.779534	71.991310
670.327166	38.514857	71.996314
669.032671	45.429815	72.001319
668.089124	50.281087	72.006324
668.219894	44.427630	72.011329
667.550518	45.350326	72.016334
666.340925	34.463019	72.021338
665.913822	37.774845	72.026343
665.457365	43.871662	72.031348
665.196384	41.150267	72.036353
664.155700	51.136420	72.041358
663.298898	48.707355	72.046362
662.755376	50.752762	72.051367
661.958181	46.855811	72.056372
661.964225	43.165040	72.061377
660.721393	49.025556	72.066382
660.422914	51.336856	72.071386
659.802537	48.939123	72.076391
658.665005	50.174514	72.081396
658.007560	38.205828	72.086401
657.325131	42.769615	72.091406
657.288942	43.739741	72.096410
656.343871	45.383841	72.101415
655.388375	42.947215	72.106420
655.217271	43.412330	72.111425
653.903667	43.533615	72.116430
652.780976	44.787778	72.121434
652.096847	41.537340	72.126439
652.003324	33.974134	72.131444
651.935259	31.450991	72.136449
651.328272	46.492124	72.141454
650.827645	41.323916	72.146458
649.874940	39.835702	72.151463
649.168649	41.960703	72.156468
648.344564	40.419666	72.161473
647.201341	43.496183	72.166478
646.726165	43.716966	72.171482
646.283562	46.856593	72.176487
645.815620	44.619446	72.181492
645.050581	37.976108	72.186497
643.919138	50.814216	72.191502
643.637973	31.105491	72.196506
643.337292	39.843872	72.201511
642.303136	47.189465	72.206516
641.491141	42.933104	72.211521
641.023897	52.963504	72.216526
640.446939	45.649690	72.221530
639.317597	39.318228	72.226535
638.644011	47.909332	72.231540
638.241761	42.528098	72.236545
637.503517	39.427057	72.241550
637.487144	39.399113	72.246554
636.600287	37.975800	72.251559
635.506596	41.796943	72.256564
635.052387	40.920387	72.261569
634.144414	48.423562	72.266574
633.979734	41.110558	72.271578
632.786097	42.316884	72.276583
632.116688	48.304935	72.281588
631.915678	42.813043	72.286593
631.243059	41.485649	72.291598
630.720720	41.086526	72.296602
629.735245	45.328051	72.301607
628.791803	45.051995	72.306612
628.603398	40.347370	72.311617
627.607848	53.940177	72.316622
626.807106	44.922051	72.321626
626.290737	43.513021	72.326631
625.722459	52.622500	72.331636
625.507633	45.630699	72.336641
624.454604	49.348175	72.341646
623.889667	42.662267	72.346650
623.196259	44.183917	72.351655
622.608606	43.226022	72.356660
621.460818	38.566570	72.361665
620.694236	40.195093	72.366670
620.696312	43.957568	72.371674
620.138338	48.864356	72.376679
618.873470	48.165772	72.381684
618.567917	36.455340	72.386689
617.822424	46.549198	72.391694
617.367275	44.120795	72.396698
616.960805	43.284216	72.401703
615.580693	43.137845	72.406708
615.414756	42.085197	72.411713
614.814851	49.792155	72.416718
614.125107	49.183310	72.421722
612.861392	47.285788	72.426727
612.172450	49.801350	72.431732
612.209674	45.515933	72.436737
611.553306	43.888539	72.441742
610.344350	36.316726	72.446746
610.002211	40.467761	72.451751
609.352816	42.554599	72.456756
609.006676	38.344342	72.461761
607.715091	52.119704	72.466766
606.835061	38.981743	72.471770
606.445147	41.791443	72.476775
606.225991	42.519777	72.481780
605.630882	40.442178	72.486785
604.847733	50.928126	72.491790
603.970386	44.486000	72.496794
603.615300	42.144658	72.501799
602.405595	38.517731	72.506804
601.811630	30.879629	72.511809
601.178384	37.397501	72.516814
600.895999	47.377277	72.521818
599.989600	49.239353	72.526823
598.598509	43.330489	72.531828
598.379749	38.344507	72.536833
597.760295	46.584911	72.541838
597.490943	43.879166	72.546842
597.390845	45.202852	72.551847
596.300133	52.577880	72.556852
595.791736	45.157991	72.561857
595.140566	49.212777	72.566862
593.753847	53.569635	72.571866
593.323424	41.022889	72.576871
592.267834	49.716947	72.581876
591.918358	40.355477	72.586881
591.645388	49.074903	72.591886
590.810803	45.424754	72.596890
590.082470	47.650639	72.601895
589.278046	54.413361	72.606900
589.099123	50.794939	72.611905
588.438803	50.640503	72.616910
587.186983	48.794236	72.621914
586.891749	48.783679	72.626919
586.280333	49.236220	72.631924
585.574370	43.561658	72.636929
584.470315	50.588468	72.641934
583.940166	50.695132	72.646938
583.942106	46.648246	72.651943
583.037508	47.677568	72.656948
582.244573	35.479899	72.661953
581.573483	41.264567	72.666958
581.310522	50.551060	72.671962
580.065168	41.871613	72.676967
578.914411	51.112473	72.681972
578.976795	41.712012	72.686977
578.420901	47.355373	72.691982
577.927250	45.722997	72.696986
576.981646	38.569463	72.701991
575.995941	51.475364	72.706996
575.619994	44.286190	72.712001
575.196697	51.784875	72.717006
573.928659	45.487852	72.722010
573.163443	37.832519	72.727015
572.602560	44.652188	72.732020
572.453206	35.525233	72.737025
571.744545	42.839139	72.742030
571.120836	43.247212	72.747034
570.247344	44.366331	72.752039
569.636409	52.190833	72.757044
569.082836	43.304045	72.762049
568.350319	46.237974	72.767054
567.414545	50.072729	72.772058
567.144037	36.369715	72.777063
566.239781	55.925193	72.782068
566.671011	39.609722	72.787073
565.205466	49.476853	72.792078
564.255025	42.226261	72.797082
563.572823	47.964288	72.802087
562.400083	47.729903	72.807092
561.993480	41.040561	72.812097
561.488492	42.232715	72.817102
561.026429	40.088119	72.822106
561.073602	36.097430	72.827111
560.165652	47.835079	72.832116
559.437675	40.260599	72.837121
558.853675	41.948236	72.842126
557.617119	52.876196	72.847130
557.150082	43.060825	72.852135
556.151761	44.802088	72.857140
555.860496	38.057855	72.862145
555.049387	40.766055	72.867150
554.033657	41.019869	72.872154
553.574555	44.194300	72.877159
552.966369	44.898512	72.882164
552.896427	41.594164	72.887169
551.760594	39.553571	72.892174
551.106658	36.350475	72.897178
550.833155	35.077461	72.902183
549.981741	36.231877	72.907188
548.976900	37.660067	72.912193
548.296876	49.482997	72.917198
547.722696	42.597384	72.922202
547.550818	40.230577	72.927207
547.023940	38.917300	72.932212
546.100875	35.850709	72.937217
545.528264	46.949882	72.942222
544.307624	38.874861	72.947226
543.860642	37.665123	72.952231
542.950781	46.986279	72.957236
542.972374	35.597940	72.962241
541.909840	44.219380	72.967246
540.587492	47.672380	72.972250
540.356400	39.850142	72.977255
539.900656	52.253157	72.982260
539.637775	44.047178	72.987265
538.568939	43.339497	72.992270
537.464582	41.341275	72.997274
536.908045	35.020241	73.002279
536.206424	41.019341	73.007284
536.380145	39.647197	73.012289
535.681718	43.694690	73.017294
534.251596	41.625982	73.022298
534.010095	32.605607	73.027303
533.337656	37.028754	73.032308
533.076922	35.999853	73.037313
532.153069	40.969339	73.042318
531.025654	48.492365	73.047322
530.646590	44.093953	73.052327
530.215701	49.319607	73.057332
529.158844	38.402624	73.062337
528.571509	44.016246	73.067342
527.565813	39.876386	73.072346
527.451815	33.641750	73.077351
526.910080	44.518144	73.082356
526.516209	41.096814	73.087361
525.415272	55.985370	73.092366
524.680763	50.840283	73.097370
524.262236	45.208448	73.102375
523.084086	55.978390	73.107380
522.236762	41.048383	73.112385
522.055547	44.533992	73.117390
521.856038	51.386078	73.122394
520.880448	45.111193	73.127399
519.535197	48.259853	73.132404
519.377044	45.326651	73.137409
518.801105	37.889146	73.142414
518.544410	50.160951	73.147418
517.649204	36.195938	73.152423
516.596235	52.028710	73.157428
516.096641	45.729495	73.162433
515.778067	43.936081	73.167438
514.971000	48.013246	73.172442
514.296258	39.857717	73.177447
513.883182	45.552788	73.182452
512.732693	36.466743	73.187457
512.003182	40.493908	73.192462
511.502578	46.158586	73.197466
511.186964	44.219412	73.202471
510.128094	44.058680	73.207476
509.391474	43.653661	73.212481
508.698325	40.029423	73.217486
508.393885	44.237551	73.222490
508.169000	30.443452	73.227495
506.716274	51.594391	73.232500
506.118170	37.912395	73.237505
505.401627	47.164904	73.242510
505.012455	44.548378	73.247514
504.114753	36.877479	73.252519
503.332692	42.559993	73.257524
503.142520	40.582746	73.262529
502.630321	46.231255	73.267534
501.613718	43.788557	73.272538
500.917480	41.527395	73.277543
499.991192	43.398422	73.282548
499.936439	38.260011	73.287553
498.977421	38.785547	73.292558
498.141901	48.444473	73.297562
497.554400	40.851462	73.302567
497.017005	42.568616	73.307572
496.514183	43.008480	73.312577
495.371175	32.536512	73.317582
494.662599	45.805424	73.322586
494.541939	42.008486	73.327591
493.981977	38.363796	73.332596
493.428121	40.848723	73.337601
492.458498	41.638167	73.342606
491.582164	35.329708	73.347610
490.986459	36.355846	73.352615
489.991805	45.615752	73.357620
489.190564	36.402766	73.362625
488.997199	47.455897	73.367630
488.484034	41.337028	73.372634
488.231494	31.999231	73.377639
486.775447	41.134134	73.382644
486.295236	45.324622	73.387649
486.037631	41.104338	73.392654
485.313502	42.913489	73.397658
484.391132	34.327540	73.402663
483.366437	35.657704	73.407668
483.042448	37.676952	73.412673
482.806157	43.618422	73.417678
481.863709	45.451960	73.422682
481.271630	36.870591	73.427687
480.559317	44.193024	73.432692
479.945363	39.929208	73.437697
479.012889	38.367306	73.442702
478.327530	38.503736	73.447706
478.100040	41.691767	73.452711
477.223585	39.843573	73.457716
476.588230	39.190300	73.462721
475.562576	40.283409	73.467726
474.649896	37.117166	73.472730
474.587114	28.620352	73.477735
474.107101	38.650561	73.482740
473.070200	36.622640	73.487745
472.246931	31.754079	73.492750
471.265345	39.635385	73.497754
471.466429	33.063752	73.502759
471.140231	33.337965	73.507764
470.310060	37.978398	73.512769
469.752843	41.988279	73.517774
468.777568	49.458008	73.522778
467.858069	35.537042	73.527783
467.002116	37.940722	73.532788
466.647153	39.364528	73.537793
466.014278	33.732730	73.542798
464.736324	35.508904	73.547802
464.014723	31.541417	73.552807
463.595386	50.907214	73.557812
463.128304	42.670323	73.562817
463.044013	39.382254	73.567822
462.475862	50.702493	73.572826
461.533961	32.975611	73.577831
460.791168	43.999347	73.582836
460.453278	42.637510	73.587841
459.281537	35.703147	73.592846
458.387912	43.518070	73.597850
458.399861	50.894407	73.602855
457.565633	52.646251	73.607860
456.351523	53.079730	73.612865
455.571120	45.686746	73.617870
454.827094	54.132049	73.622874
454.763082	40.784038	73.627879
454.295600	47.285357	73.632884
453.553144	44.871080	73.637889
452.867876	42.300961	73.642894
452.161830	48.953683	73.647898
451.806006	44.361047	73.652903
450.561079	46.384576	73.657908
449.698382	42.320092	73.662913
449.306240	45.356352	73.667918
448.931850	47.602516	73.672922
448.947317	36.835724	73.677927
447.476177	40.350162	73.682932
446.857925	41.977369	73.687937
446.029769	40.859410	73.692942
444.798017	45.245005	73.697946
444.375825	36.334154	73.702951
443.617337	42.422740	73.707956
443.650646	40.334177	73.712961
443.416293	39.096301	73.717966
441.873467	48.002157	73.722970
441.882339	41.782387	73.727975
441.252628	51.672479	73.732980
440.601594	33.659326	73.737985
439.672780	42.089321	73.742990
438.648601	49.285611	73.747994
438.429839	44.453581	73.752999
437.174018	44.392929	73.758004
436.662564	45.524234	73.763009
436.313202	50.728026	73.768014
435.673565	49.906161	73.773018
435.342933	41.946662	73.778023
433.840030	43.798103	73.783028
433.024760	38.624645	73.788033
432.670779	40.909151	73.793038
432.338283	41.868086	73.798042
432.320745	41.712060	73.803047
431.160964	44.971448	73.808052
430.595196	50.918860	73.813057
429.745990	43.379395	73.818062
428.265261	41.174929	73.823066
427.686734	34.440080	73.828071
427.180717	45.471395	73.833076
426.878732	42.813491	73.838081
426.549199	36.257402	73.843086
425.945138	41.957969	73.848090
425.147276	38.488262	73.853095
424.545016	45.950514	73.858100
424.263205	45.240606	73.863105
422.863488	35.013170	73.868110
421.900743	37.511338	73.873114
421.542366	30.317606	73.878119
421.218755	34.981357	73.883124
420.397061	36.108597	73.888129
419.634341	34.676291	73.893134
418.996220	36.935285	73.898138
418.362576	37.859389	73.903143
417.765613	46.939050	73.908148
416.907159	44.702544	73.913153
416.040432	39.154644	73.918158
415.638281	36.335894	73.923162
415.255783	28.721193	73.928167
414.917853	40.366288	73.933172
414.071221	32.568250	73.938177
413.512300	37.191412	73.943182
412.336028	40.650985	73.948186
411.549810	31.804504	73.953191
410.676676	29.600121	73.958196
410.332053	36.668501	73.963201
410.000575	30.866649	73.968206
409.286645	37.079828	73.973210
408.483128	40.374867	73.978215
407.439762	38.655550	73.983220
407.160156	44.894160	73.988225
406.933995	40.126162	73.993230
405.605105	43.207708	73.998234
405.232408	38.389039	74.003239
404.432650	46.102624	74.008244
404.082466	30.234498	74.013249
403.600799	36.818766	74.018254
402.372048	32.792952	74.023258
401.926310	34.260343	74.028263
401.366575	34.732863	74.033268
400.261933	30.496714	74.038273
399.299354	30.692507	74.043278
398.604327	35.070593	74.048282
398.423232	28.482362	74.053287
398.179086	36.253080	74.058292
397.577788	35.194534	74.063297
396.918369	34.623550	74.068302
395.882012	39.362483	74.073306
395.484943	31.477536	74.078311
394.384995	26.909818	74.083316
393.502990	35.878071	74.088321
393.183211	27.129278	74.093326
392.657050	37.133449	74.098330
392.259076	31.272342	74.103335
391.691364	40.836034	74.108340
390.700534	32.837335	74.113345
390.596398	32.935346	74.118350
389.038593	41.717865	74.123354
388.253773	35.077190	74.128359
387.414126	41.231792	74.133364
386.888032	41.874984	74.138369
387.375259	28.908148	74.143374
386.551255	38.743116	74.148378
385.721370	35.081552	74.153383
385.015115	40.704904	74.158388
383.677997	33.134611	74.163393
383.106977	30.143899	74.168398
381.986390	35.837076	74.173402
382.056276	26.499694	74.178407
381.454899	32.210458	74.183412
381.548448	29.924874	74.188417
380.348572	37.140227	74.193422
379.704926	38.384976	74.198426
378.782533	32.618485	74.203431
377.633261	35.230334	74.208436
377.074204	38.957528	74.213441
376.837622	31.789504	74.218446
376.207085	44.730062	74.223450
376.028851	33.203898	74.228455
374.600244	39.173669	74.233460
373.798540	40.286045	74.238465
373.582018	29.786380	74.243470
372.956231	36.347194	74.248474
372.488078	30.111696	74.253479
371.675749	40.934996	74.258484
371.025589	39.292761	74.263489
370.310515	43.641527	74.268494
369.007967	43.896382	74.273498
368.800481	38.445100	74.278503
368.481803	46.027293	74.283508
367.426969	43.002666	74.288513
366.390109	39.007522	74.293518
365.729754	41.957132	74.298522
365.587710	37.405233	74.303527
364.981099	33.845924	74.308532
364.288016	42.370911	74.313537
363.491355	36.235133	74.318542
362.650868	39.043126	74.323546
362.570310	36.898296	74.328551
361.891022	40.702542	74.333556
361.031817	35.065347	74.338561
360.214315	35.079978	74.343566
359.224653	33.911168	74.348570
359.083959	34.684481	74.353575
358.638420	29.778839	74.358580
357.347593	41.062282	74.363585
357.098016	32.175942	74.368590
356.575925	38.421374	74.373594
355.621354	40.460683	74.378599
354.626045	34.441843	74.383604
354.125518	27.072762	74.388609
353.939102	29.260661	74.393614
352.949643	44.006961	74.398618
352.041157	39.476300	74.403623
351.546038	41.370947	74.408628
351.225683	31.855728	74.413633
350.617669	32.738344	74.418638
349.761351	33.858504	74.423642
349.061380	36.584788	74.428647
348.617879	38.234551	74.433652
347.821418	33.187751	74.438657
347.265590	33.289369	74.443662
346.401669	39.070792	74.448666
345.878852	33.178591	74.453671
344.746248	36.318082	74.458676
343.957219	39.725113	74.463681
343.402407	40.547300	74.468686
343.030881	41.684234	74.473690
342.653002	37.721801	74.478695
342.522963	33.415332	74.483700
341.659339	32.540693	74.488705
341.016397	29.577709	74.493710
339.645502	40.095718	74.498714
338.847834	34.861244	74.503719
338.327221	33.027086	74.508724
337.778139	38.640081	74.513729
337.144220	36.272747	74.518734
336.276711	38.924728	74.523738
335.481140	34.697199	74.528743
334.863980	31.277062	74.533748
334.434736	39.548816	74.538753
334.219044	29.469777	74.543758
332.840084	42.045614	74.548762
332.343358	35.416755	74.553767
332.025842	39.579365	74.558772
331.211908	35.997573	74.563777
330.808283	34.594124	74.568782
329.634170	36.119260	74.573786
329.350990	34.838053	74.578791
328.640592	38.926695	74.583796
327.888119	45.793421	74.588801
326.903978	37.342438	74.593806
326.240910	37.430467	74.598810
326.300062	34.723702	74.603815
325.850799	39.431096	74.608820
324.317504	41.090423	74.613825
324.055891	41.073726	74.618830
323.258566	42.630988	74.623834
322.933205	32.779942	74.628839
321.719979	34.114428	74.633844
320.976592	38.783030	74.638849
321.259397	33.920307	74.643854
320.016605	49.343940	74.648858
319.446177	40.657058	74.653863
318.581620	41.371690	74.658868
318.439093	42.572001	74.663873
317.460895	33.522016	74.668878
315.994419	43.035297	74.673882
315.450652	31.741522	74.678887
315.102172	36.777803	74.683892
314.835828	38.349049	74.688897
314.643254	34.408935	74.693902
313.543103	36.377684	74.698906
313.001893	40.583767	74.703911
311.905651	33.925045	74.708916
310.762561	39.850237	74.713921
310.432623	38.890840	74.718926
309.465780	36.229676	74.723930
309.183651	27.645747	74.728935
309.220377	39.385293	74.733940
308.345103	30.653571	74.738945
307.366443	29.111465	74.743950
306.530233	43.457314	74.748954
306.190732	36.196419	74.753959
306.140187	33.744888	74.758964
304.614055	37.140510	74.763969
304.088194	36.535595	74.768974
303.484675	36.622499	74.773978
303.080936	38.691344	74.778983
302.075353	37.502777	74.783988
301.844366	36.739959	74.788993
301.190566	34.934160	74.793998
299.808459	41.158857	74.799002
299.030648	40.522922	74.804007
298.269651	39.377691	74.809012
297.820012	41.724386	74.814017
297.779219	35.221845	74.819022
297.309991	41.969765	74.824026
296.525984	40.338248	74.829031
295.716644	29.730614	74.834036
294.847794	32.491771	74.839041
293.826940	28.274052	74.844046
293.259578	40.356728	74.849050
292.865250	30.122011	74.854055
292.761441	29.975248	74.859060
291.944312	33.118303	74.864065
291.390468	30.968553	74.869070
290.797711	30.178540	74.874074
289.856949	28.809141	74.879079
289.171120	31.120929	74.884084
288.044131	36.080269	74.889089
286.806285	27.571349	74.894094
286.465077	39.917609	74.899098
285.951230	33.034737	74.904103
285.574045	30.293429	74.909108
285.052379	41.181378	74.914113
284.659856	26.323108	74.919118
283.693695	32.288233	74.924122
283.098997	29.839191	74.929127
282.394355	32.056317	74.934132
281.839325	44.231218	74.939137
281.211486	34.726480	74.944142
279.891027	36.585771	74.949146
279.617728	35.338792	74.954151
279.159144	31.313233	74.959156
278.274015	35.986793	74.964161
277.596577	29.335241	74.969166
276.683195	37.309872	74.974170
275.995594	31.986289	74.979175
275.871484	37.974835	74.984180
275.386249	30.186727	74.989185
274.668079	25.589917	74.994190
273.579290	39.210161	74.999194
273.329663	32.030177	75.004199
272.568261	31.833510	75.009204
271.310929	34.300099	75.014209
271.045054	25.025411	75.019214
270.267111	30.707635	75.024218
270.296852	31.257143	75.029223
269.196965	35.017447	75.034228
268.381758	39.098010	75.039233
268.166607	30.729169	75.044238
267.084252	38.663691	75.049242
266.062500	39.736044	75.054247
265.513076	34.217078	75.059252
264.786974	39.941732	75.064257
264.820813	35.400744	75.069262
264.039065	40.971526	75.074266
262.870916	36.232781	75.079271
262.332424	34.962581	75.084276
261.749786	33.232611	75.089281
261.506111	32.577753	75.094286
260.646638	32.433028	75.099290
259.727226	34.162795	75.104295
259.378803	34.643712	75.109300
258.821761	43.419710	75.114305
257.792841	36.552110	75.119310
257.061951	34.861762	75.124314
256.985055	32.684337	75.129319
256.444409	32.466805	75.134324
254.994915	35.116722	75.139329
254.406571	33.110250	75.144334
253.738965	39.860992	75.149338
253.480228	41.728549	75.154343
252.333869	39.598662	75.159348
251.264366	49.647033	75.164353
251.513570	36.972821	75.169358
250.962099	35.906149	75.174362
250.471290	40.192013	75.179367
249.122866	35.512198	75.184372
248.372304	46.089673	75.189377
248.020641	36.478395	75.194382
247.660022	41.237699	75.199386
246.626287	43.527030	75.204391
245.918975	40.897966	75.209396
245.378081	48.468121	75.214401
245.056832	36.454552	75.219406
244.074452	45.097816	75.224410
243.284986	41.869849	75.229415
242.915547	40.332268	75.234420
241.838736	40.907650	75.239425
240.934919	27.159729	75.244430
240.249120	36.600777	75.249434
239.787995	37.226138	75.254439
239.448200	33.014839	75.259444
238.753612	43.305236	75.264449
238.729730	42.075107	75.269454
237.634749	38.869120	75.274458
236.871556	39.387587	75.279463
236.090113	36.211139	75.284468
234.743493	48.645278	75.289473
234.586319	35.673253	75.294478
234.123977	34.327639	75.299482
233.673782	36.012503	75.304487
232.987076	33.275313	75.309492
231.831755	39.814416	75.314497
231.587637	28.539952	75.319502
231.272055	42.690381	75.324506
230.132069	42.965563	75.329511
229.882743	34.628635	75.334516
228.919020	43.606179	75.339521
228.549236	33.041234	75.344526
227.344121	42.773793	75.349530
226.727447	39.052031	75.354535
226.258813	37.354231	75.359540
225.214210	35.673851	75.364545
224.152303	33.349903	75.369550
223.516277	45.850905	75.374554
223.792357	42.939597	75.379559
223.438969	37.138366	75.384564
222.784729	38.054578	75.389569
221.686063	39.787845	75.394574
220.892451	42.839255	75.399578
220.191280	40.025209	75.404583
219.844665	36.610816	75.409588
218.590409	42.521135	75.414593
218.227330	32.228578	75.419598
217.738597	40.227917	75.424602
217.080566	41.323189	75.429607
216.299825	39.459432	75.434612
215.227221	40.472228	75.439617
214.814780	38.769138	75.444622
214.561581	40.972040	75.449626
212.849073	35.472866	75.454631
212.416680	34.099228	75.459636
212.133766	47.104135	75.464641
211.798954	33.827852	75.469646
210.782251	47.104589	75.474650
210.358273	38.267899	75.479655
210.448338	36.963769	75.484660
209.124020	44.699401	75.489665
208.870674	34.022531	75.494670
207.622749	39.419433	75.499674
206.764782	39.803371	75.504679
206.322493	33.776610	75.509684
205.685775	39.588176	75.514689
205.265029	32.751330	75.519694
204.164474	36.238621	75.524698
203.585452	33.327066	75.529703
203.007701	30.414110	75.534708
202.548875	35.864019	75.539713
201.998210	35.096801	75.544718
200.963043	35.496117	75.549722
200.157348	37.490198	75.554727
200.189219	33.195851	75.559732
199.075875	35.158991	75.564737
198.264441	34.668565	75.569742
197.582646	31.262690	75.574746
197.601818	33.575206	75.579751
196.921503	32.409453	75.584756
195.642720	33.358919	75.589761
195.168191	24.572745	75.594766
194.797048	34.890976	75.599770
193.393068	33.498380	75.604775
193.043647	29.139931	75.609780
192.174014	38.514214	75.614785
191.857010	36.696088	75.619790
191.527894	40.438351	75.624794
190.640850	41.823131	75.629799
189.959650	36.442813	75.634804
189.222752	45.417002	75.639809
188.804792	36.818875	75.644814
187.484998	46.109685	75.649818
186.838366	50.579756	75.654823
187.060652	42.891803	75.659828
185.975693	51.550294	75.664833
185.515654	38.438759	75.669838
184.676762	41.432020	75.674842
184.069373	41.465133	75.679847
183.260366	39.644909	75.684852
182.242589	41.850995	75.689857
181.718664	35.046838	75.694862
181.514697	30.050866	75.699866
180.289930	36.960673	75.704871
179.430149	33.584523	75.709876
178.577403	37.144594	75.714881
178.581548	34.398317	75.719886
177.942691	36.412745	75.724890
177.402031	39.474083	75.729895
177.390899	33.330786	75.734900
176.115893	36.134748	75.739905
175.440597	25.256691	75.744910
174.805721	28.772307	75.749914
173.992209	32.404594	75.754919
173.101871	26.446360	75.759924
172.264890	32.551977	75.764929
172.142347	30.041352	75.769934
171.771434	35.129635	75.774938
170.685104	30.821732	75.779943
169.912845	28.901272	75.784948
169.280570	28.346982	75.789953
168.825134	34.233649	75.794958
167.839455	36.866049	75.799962
167.097563	32.764345	75.804967
166.736553	30.379068	75.809972
166.339827	30.784989	75.814977
165.725538	30.180252	75.819982
164.808542	22.788663	75.824986
164.028456	28.450739	75.829991
163.609411	20.152792	75.834996
162.807134	19.154785	75.840001
162.000720	28.748343	75.845006
161.309443	31.295933	75.850010
160.759688	29.191287	75.855015
160.582524	22.954887	75.860020
159.326941	32.655052	75.865025
158.945557	20.713396	75.870030
158.344565	27.502453	75.875034
157.199089	26.444080	75.880039
156.662808	34.163036	75.885044
155.775628	32.351088	75.890049
155.442979	29.079958	75.895054
155.104288	37.521701	75.900058
154.664981	32.298462	75.905063
153.990047	31.394275	75.910068
153.007181	39.485431	75.915073
152.294931	33.098013	75.920078
151.050596	31.604251	75.925082
150.025758	33.930756	75.930087
150.406670	22.605603	75.935092
149.648287	33.854237	75.940097
149.308006	32.092603	75.945102
148.480130	30.494686	75.950106
147.273299	27.533674	75.955111
147.035623	20.757031	75.960116
146.259494	28.220280	75.965121
145.184379	30.349761	75.970126
144.728067	33.185076	75.975130
143.898494	38.188582	75.980135
144.027496	30.432161	75.985140
143.270674	38.560349	75.990145
142.248795	33.276339	75.995150
141.576561	29.315057	76.000154
140.872353	36.073660	76.005159
140.746958	26.568870	76.010164
139.335103	38.583966	76.015169
138.768294	44.040945	76.020174
138.272263	33.705674	76.025178
137.841041	38.039744	76.030183
137.640332	33.304120	76.035188
136.427035	41.216509	76.040193
136.092913	33.359890	76.045198
135.212692	36.354716	76.050202
133.343224	38.728533	76.055207
133.309280	29.108598	76.060212
132.655973	31.052486	76.065217
132.558458	29.829853	76.070222
132.185485	33.533453	76.075226
130.854002	36.099625	76.080231
130.376807	26.353590	76.085236
130.000491	40.882685	76.090241
129.474347	31.452913	76.095246
128.570319	28.688267	76.100250
127.126745	32.964988	76.105255
127.143939	30.268184	76.110260
126.451666	33.741544	76.115265
126.346934	34.827228	76.120270
125.217500	33.447186	76.125274
124.204147	30.116719	76.130279
124.073988	32.324974	76.135284
122.900555	37.209024	76.140289
122.108732	40.644589	76.145294
122.115295	30.075931	76.150298
121.399039	30.915558	76.155303
120.974446	27.827946	76.160308
119.928038	34.657058	76.165313
118.998490	29.716807	76.170318
118.907359	25.226067	76.175322
117.615526	31.172449	76.180327
116.754149	26.859941	76.185332
116.283349	31.462095	76.190337
116.002863	38.305940	76.195342
115.637936	30.512631	76.200346
114.354304	36.537340	76.205351
114.122048	29.772003	76.210356
113.259709	30.781139	76.215361
112.629690	31.443362	76.220366
112.153672	31.500932	76.225370
111.084532	36.730237	76.230375
111.029369	36.251476	76.235380
109.858074	38.033137	76.240385
108.526709	35.571086	76.245390
108.302430	37.190388	76.250394
107.763085	37.953900	76.255399
107.987666	30.153860	76.260404
106.942169	28.371039	76.265409
106.074637	31.228703	76.270414
105.289984	33.188798	76.275418
104.616955	33.531970	76.280423
104.034745	27.656708	76.285428
103.142173	36.829681	76.290433
102.449220	26.776455	76.295438
102.007825	30.359164	76.300442
101.448533	35.802223	76.305447
101.168592	33.867233	76.310452
100.179635	39.181077	76.315457
99.175609	32.175056	76.320462
98.529741	33.914398	76.325466
97.340220	33.715375	76.330471
97.539047	31.032822	76.335476
96.356412	39.268358	76.340481
96.053764	37.547246	76.345486
95.807849	35.852722	76.350490
94.892044	42.893513	76.355495
94.220132	36.492086	76.360500
93.258485	32.453730	76.365505
92.738809	35.772775	76.370510
91.876018	30.918578	76.375514
91.077693	34.834438	76.380519
90.858675	34.909523	76.385524
90.133984	32.746069	76.390529
89.677414	37.314209	76.395534
88.963240	30.731360	76.400538
88.207662	39.260365	76.405543
87.765848	32.346234	76.410548
86.794210	34.872037	76.415553
85.513084	38.389128	76.420558
85.073584	37.887057	76.425562
84.614351	38.520002	76.430567
84.141055	36.809992	76.435572
83.896556	40.988114	76.440577
83.144824	36.691943	76.445582
82.411306	30.053600	76.450586
81.566017	39.672386	76.455591
81.017135	33.281447	76.460596
80.450233	42.369381	76.465601
79.781681	35.120334	76.470606
79.270411	29.279884	76.475610
78.133265	42.937647	76.480615
77.919135	31.796215	76.485620
77.247892	33.753053	76.490625
75.832879	35.368496	76.495630
75.577047	28.608390	76.500634
74.724291	36.486997	76.505639
74.518010	31.678524	76.510644
73.735832	31.708463	76.515649
72.605951	40.485974	76.520654
72.255557	26.156550	76.525658
71.184835	37.998704	76.530663
71.332937	28.071268	76.535668
70.442892	32.395196	76.540673
69.489152	22.334198	76.545678
69.162492	26.705601	76.550682
68.421956	25.360338	76.555687
67.667992	25.510170	76.560692
66.343020	34.317179	76.565697
65.739294	29.922222	76.570702
65.435061	23.973652	76.575706
65.050800	36.373064	76.580711
64.867917	30.966937	76.585716
63.958341	38.409265	76.590721
63.003978	29.986811	76.595726
62.671900	25.008476	76.600730
61.748091	35.498822	76.605735
60.951430	30.715789	76.610740
60.152413	34.622298	76.615745
59.801204	33.393430	76.620750
59.458428	30.251933	76.625754
58.430497	38.420690	76.630759
57.683332	28.654645	76.635764
56.748928	31.270773	76.640769
56.117811	28.801566	76.645774
56.192421	27.622840	76.650778
55.001729	25.494294	76.655783
54.531964	31.021867	76.660788
54.024603	34.715751	76.665793
52.893501	31.481274	76.670798
52.052663	30.422403	76.675802
51.657010	37.758461	76.680807
51.266955	26.066583	76.685812
50.953846	24.978016	76.690817
50.023445	38.202463	76.695822
49.237064	28.155007	76.700826
48.555505	34.727772	76.705831
47.985559	26.861871	76.710836
47.072436	32.146536	76.715841
46.413405	30.164845	76.720846
46.073163	32.173480	76.725850
45.163226	40.316483	76.730855
44.621755	32.142955	76.735860
43.691966	27.555635	76.740865
43.213609	37.522797	76.745870
42.945320	31.498596	76.750874
41.251494	38.025860	76.755879
41.085588	30.582096	76.760884
40.475228	35.417774	76.765889
39.498447	36.238928	76.770894
39.687389	21.589690	76.775898
38.740497	30.815002	76.780903
38.064527	20.996896	76.785908
37.553404	27.588590	76.790913
36.776468	30.798995	76.795918
35.852852	28.106803	76.800922
35.195600	34.999063	76.805927
34.930806	25.936976	76.810932
34.146335	34.191087	76.815937
33.032423	37.384672	76.820942
32.899516	32.997802	76.825946
32.029463	36.093921	76.830951
31.683423	35.108889	76.835956
30.406417	30.459141	76.840961
29.912715	39.447292	76.845966
29.428372	25.950790	76.850970
28.718018	30.901105	76.855975
28.363775	33.088971	76.860980
27.685410	35.269258	76.865985
26.678065	32.668393	76.870990
25.937810	32.137769	76.875994
24.767877	38.816773	76.880999
24.346396	34.257951	76.886004
23.816016	28.872730	76.891009
23.615746	31.668099	76.896014
23.505476	24.943829	76.901018
22.483870	35.361742	76.906023
21.732947	30.253924	76.911028
21.064126	37.504987	76.916033
19.646150	38.887286	76.921038
19.250421	35.588699	76.926042
19.002637	39.771726	76.931047
18.341299	33.782949	76.936052
17.045626	38.398264	76.941057
16.189563	42.147995	76.946062
16.088700	33.000960	76.951066
15.536294	44.413223	76.956071
15.192651	35.695420	76.961076
14.320225	37.732943	76.966081
13.105165	38.784814	76.971086
12.857524	37.013228	76.976090
12.235348	40.415772	76.981095
11.633366	43.577239	76.986100
10.558802	38.494126	76.991105
10.249275	42.956143	76.996110
10.014351	39.174489	77.001114
8.823413	40.786659	77.006119
7.732448	29.271808	77.011124
7.323287	47.964399	77.016129
6.351487	45.362573	77.021134
6.471893	31.949470	77.026139
6.032680	39.632449	77.031143
5.360173	30.835653	77.036148
4.651808	39.954159	77.041153
3.511466	35.885285	77.046158