Tue Jun 08 16:51:51 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.494819	99.618491	0.000000
-1.591655	78.033415	0.005005
-2.259386	52.935845	0.010010
-4.602833	8.912398	0.015014
-8.669513	-2.054706	0.020019
-13.974571	9.347879	0.025024
-18.877794	-3.039612	0.030029
-23.450780	1.825026	0.035034
-27.567827	0.154459	0.040038
-30.887883	6.258375	0.045043
-34.654102	6.635007	0.050048
-38.121473	0.472973	0.055053
-42.063162	5.413711	0.060058
-45.879147	-2.094883	0.065062
-49.592263	-8.224239	0.070067
-53.704338	0.464662	0.075072
-57.060599	-1.978126	0.080077
-60.906586	5.192500	0.085082
-64.395129	2.872655	0.090086
-67.980682	2.367344	0.095091
-72.262773	7.839338	0.100096
-75.680675	3.250053	0.105101
-79.873441	9.367872	0.110106
-83.551180	4.091755	0.115110
-87.033938	5.530136	0.120115
-90.852837	7.494284	0.125120
-94.562653	-3.406830	0.130125
-98.673603	4.601045	0.135130
-102.285132	-2.365889	0.140134
-105.928933	3.289945	0.145139
-109.886145	8.937955	0.150144
-113.246617	-1.705310	0.155149
-117.144524	0.530547	0.160154
-121.232361	-0.747077	0.165158
-124.668718	3.387913	0.170163
-128.678469	-2.296193	0.175168
-132.180698	3.889158	0.180173
-135.665211	0.576779	0.185178
-139.509299	-4.854298	0.190182
-143.635214	-10.486099	0.195187
-147.327506	-4.679431	0.200192
-151.230044	-10.504257	0.205197
-155.657190	2.228462	0.210202
-159.264488	2.517946	0.215206
-162.628724	2.909818	0.220211
-166.779861	6.996906	0.225216
-170.191570	6.470545	0.230221
-173.839160	12.760194	0.235226
-177.516923	3.302234	0.240230
-181.183128	4.216003	0.245235
-185.094988	14.031516	0.250240
-188.710672	9.800294	0.255245
-192.367419	12.069061	0.260250
-196.453238	7.321678	0.265254
-199.948062	3.153024	0.270259
-203.744962	8.858873	0.275264
-207.517725	-3.055211	0.280269
-211.570858	4.168424	0.285274
-215.448884	7.179712	0.290278
-218.572320	5.868608	0.295283
-222.389333	8.874964	0.300288
-226.495109	5.491590	0.305293
-230.056118	3.669401	0.310298
-233.588495	0.049150	0.315302
-237.695172	-1.870482	0.320307
-241.892922	6.766563	0.325312
-245.380539	9.067543	0.330317
-248.980669	10.994300	0.335322
-253.010016	4.430711	0.340326
-256.217339	0.203320	0.345331
-260.276824	2.253079	0.350336
-263.838688	8.878195	0.355341
-267.942166	2.920581	0.360346
-271.416866	3.375687	0.365350
-275.216219	-7.385564	0.370355
-279.404308	1.434576	0.375360
-282.686138	-0.426376	0.380365
-286.458479	3.759253	0.385370
-290.502495	8.677486	0.390374
-294.243095	-1.800165	0.395379
-298.360853	12.143860	0.400384
-301.826992	1.227192	0.405389
-305.394723	6.287146	0.410394
-309.043448	2.821508	0.415398
-312.642087	6.484375	0.420403
-316.532736	9.222408	0.425408
-320.615056	4.418102	0.430413
-324.293105	6.355520	0.435418
-328.278719	1.962891	0.440422
-331.633309	-4.236396	0.445427
-335.434944	8.077760	0.450432
-338.850750	13.241144	0.455437
-343.006915	6.075758	0.460442
-346.956705	12.793529	0.465446
-350.450827	-5.508785	0.470451
-354.249525	3.005432	0.475456
-358.214505	4.456479	0.480461
-361.838051	5.712787	0.485466
-365.612026	14.133178	0.490470
-369.324117	6.050916	0.495475
-373.348742	9.178266	0.500480
-376.938486	4.019538	0.505485
-380.710868	8.314979	0.510490
-384.617577	9.435947	0.515494
-387.960843	3.099769	0.520499
-391.864053	9.693147	0.525504
-395.362944	8.658139	0.530509
-399.528266	14.006982	0.535514
-403.045582	10.540983	0.540518
-406.890373	3.085423	0.545523
-411.235415	5.871487	0.550528
-414.781159	-1.621944	0.555533
-418.320608	3.448635	0.560538
-422.072865	3.210609	0.565542
-425.567407	-3.767821	0.570547
-429.749460	-0.593680	0.575552
-433.230541	-0.641394	0.580557
-437.020246	-0.018444	0.585562
-440.702786	5.620211	0.590566
-444.611133	-1.699285	0.595571
-448.620432	6.140663	0.600576
-451.823152	5.436966	0.605581
-455.746946	-0.057905	0.610586
-459.471582	4.052578	0.615590
-463.430602	2.512400	0.620595
-467.399798	11.438033	0.625600
-471.179727	-0.930057	0.630605
-474.774279	4.729052	0.635610
-478.485292	-8.922591	0.640614
-481.923562	-3.483698	0.645619
-486.130455	1.901163	0.650624
-489.748946	0.052737	0.655629
-493.377325	-7.076736	0.660634
-497.617700	4.893236	0.665638
-500.659738	-1.207971	0.670643
-504.922797	0.512225	0.675648
-508.998003	3.422993	0.680653
-512.334215	5.495714	0.685658
-516.265402	9.557610	0.690662
-519.732669	10.445416	0.695667
-523.853009	10.969260	0.700672
-527.448865	1.233515	0.705677
-530.953487	6.856712	0.710682
-535.340668	5.828580	0.715686
-538.324349	3.105545	0.720691
-542.526855	6.883646	0.725696
-545.831147	12.241580	0.730701
-549.613811	10.246122	0.735706
-553.660026	1.784423	0.740710
-557.504370	-1.355748	0.745715
-561.708939	-0.395476	0.750720
-565.142501	-1.694562	0.755725
-568.545435	0.368333	0.760730
-572.522554	2.521466	0.765734
-576.321143	3.299995	0.770739
-580.293673	-0.578758	0.775744
-584.070729	-4.142128	0.780749
-587.833766	2.378805	0.785754
-591.639009	11.865700	0.790758
-594.686603	0.581449	0.795763
-598.339494	12.451887	0.800768
-602.465046	3.481654	0.805773
-606.612951	3.073669	0.810778
-610.523354	10.878231	0.815782
-613.947673	6.029191	0.820787
-617.831597	16.621762	0.825792
-621.379926	12.773665	0.830797
-624.864698	7.258481	0.835802
-628.822296	10.854516	0.840806
-632.342637	4.102909	0.845811
-636.812602	8.818633	0.850816
-640.085179	13.218766	0.855821
-644.306783	9.458201	0.860826
-647.812624	8.603390	0.865830
-651.298237	-2.740635	0.870835
-655.076071	8.166885	0.875840
-659.409808	1.492128	0.880845
-662.965927	9.857201	0.885850
-666.783218	10.643359	0.890854
-669.993988	7.244969	0.895859
-673.493656	7.413381	0.900864
-677.428125	6.053908	0.905869
-681.750576	11.488776	0.910874
-685.860300	17.344212	0.915878
-689.376968	5.611234	0.920883
-693.357954	11.054613	0.925888
-697.045146	7.282120	0.930893
-700.781025	3.610348	0.935898
-703.946929	5.127445	0.940902
-707.409267	-0.228896	0.945907
-711.357380	13.959079	0.950912
-715.406009	5.021548	0.955917
-719.253959	4.179328	0.960922
-722.965041	9.501416	0.965926
-726.456583	3.207545	0.970931
-730.019280	5.295614	0.975936
-734.312254	4.742135	0.980941
-738.169079	5.618422	0.985946
-741.737158	7.661244	0.990950
-745.326821	5.002097	0.995955
-749.535469	8.937352	1.000960
-753.283766	0.777198	1.005965
-756.621082	2.812002	1.010970
-760.641767	1.567658	1.015974
-764.497625	-4.120140	1.020979
-768.181861	2.460430	1.025984
-771.517775	2.197427	1.030989
-775.587018	1.637561	1.035994
-779.550839	0.465574	1.040998
-783.044789	3.788758	1.046003
-787.214006	6.039783	1.051008
-790.895720	-5.047445	1.056013
-794.617898	1.748457	1.061018
-798.535224	0.765860	1.066022
-802.231139	-3.357906	1.071027
-805.993951	1.821954	1.076032
-809.255878	4.107126	1.081037
-813.385570	1.841889	1.086042
-816.986775	7.934602	1.091046
-820.670009	-5.549378	1.096051
-824.358682	12.217538	1.101056
-828.026788	11.662678	1.106061
-832.081257	3.250438	1.111066
-836.236626	9.937983	1.116070
-839.363601	0.943823	1.121075
-843.832555	3.796568	1.126080
-846.855917	-1.796042	1.131085
-850.798157	-0.942886	1.136090
-854.807131	2.338505	1.141094
-858.418644	-1.256189	1.146099
-862.262653	8.162573	1.151104
-866.075957	-2.111008	1.156109
-869.594738	-1.570503	1.161114
-873.149348	3.169495	1.166118
-876.850373	0.779032	1.171123
-881.355892	6.261693	1.176128
-884.602539	8.335104	1.181133
-888.591242	2.817055	1.186138
-892.406280	9.133623	1.191142
-895.695125	-5.217260	1.196147
-899.750400	5.085226	1.201152
-903.767765	2.258472	1.206157
-907.322906	-0.913655	1.211162
-910.992779	8.809568	1.216166
-914.629261	-0.166929	1.221171
-918.484633	10.691738	1.226176
-922.512817	8.760863	1.231181
-926.051522	0.050201	1.236186
-930.016774	-1.339672	1.241190
-933.509459	-0.757809	1.246195
-937.321073	2.605424	1.251200
-941.380213	9.220494	1.256205
-945.355035	8.288951	1.261210
-948.672433	15.329280	1.266214
-952.293167	8.863984	1.271219
-956.369147	2.500530	1.276224
-959.867694	1.391718	1.281229
-963.597665	3.303050	1.286234
-967.679433	10.903264	1.291238
-971.028886	11.633053	1.296243
-975.225760	12.919610	1.301248
-978.618703	0.077074	1.306253
-982.318159	1.816223	1.311258
-986.497071	-0.807072	1.316262
-990.015918	4.428546	1.321267
-993.728187	2.796369	1.326272
-997.407991	-3.760967	1.331277
-1001.263138	1.166111	1.336282
-1005.130669	1.502150	1.341286
-1008.911880	3.896357	1.346291
-1012.800768	4.169364	1.351296
-1016.453738	-3.339851	1.356301
-1020.161562	0.325737	1.361306
-1024.317378	7.047470	1.366310
-1027.685874	5.712719	1.371315
-1031.589609	6.628107	1.376320
-1034.769933	-3.425982	1.381325
-1038.659137	-3.317093	1.386330
-1042.746609	6.907364	1.391334
-1046.560333	2.131865	1.396339
-1050.482056	14.171931	1.401344
-1054.381138	6.333587	1.406349
-1057.432692	-2.001160	1.411354
-1061.660927	0.693248	1.416358
-1065.101873	-2.671625	1.421363
-1068.814715	3.308224	1.426368
-1072.972952	3.854488	1.431373
-1076.618098	-1.700258	1.436378
-1080.601778	6.628016	1.441382
-1084.060481	1.587533	1.446387
-1087.703321	6.247725	1.451392
-1091.587070	5.738013	1.456397
-1095.147468	0.925773	1.461402
-1099.536474	5.976180	1.466406
-1102.862058	-5.324642	1.471411
-1106.811775	4.879767	1.476416
-1110.487324	-1.356906	1.481421
-1113.881117	2.832289	1.486426
-1117.778836	15.245229	1.491430
-1122.211642	7.646218	1.496435
-1125.773261	4.443420	1.501440
-1129.252003	7.762290	1.506445
-1132.519341	-0.128009	1.511450
-1136.554188	16.444985	1.516454
-1140.174461	9.965573	1.521459
-1144.521739	9.165274	1.526464
-1148.048972	8.854109	1.531469
-1151.689741	-1.703791	1.536474
-1155.603806	6.730609	1.541478
-1159.271963	2.722784	1.546483
-1163.146150	10.961676	1.551488
-1167.027593	4.962103	1.556493
-1170.725399	3.456274	1.561498
-1174.609574	5.997374	1.566502
-1178.210341	-0.191689	1.571507
-1181.803430	7.481095	1.576512
-1185.378887	1.878562	1.581517
-1189.319563	11.918083	1.586522
-1193.477505	5.958520	1.591526
-1196.680597	1.646673	1.596531
-1200.786972	4.096492	1.601536
-1204.265227	1.845681	1.606541
-1208.247328	-6.137310	1.611546
-1212.291291	4.929219	1.616550
-1215.494530	0.144559	1.621555
-1219.455709	-3.286352	1.626560
-1223.036826	-0.307429	1.631565
-1226.906103	1.873163	1.636570
-1230.961390	14.642434	1.641574
-1234.353592	12.033871	1.646579
-1238.902949	11.867929	1.651584
-1242.243813	3.376191	1.656589
-1245.852684	-5.979695	1.661594
-1249.523096	6.071832	1.666598
-1252.965609	3.894259	1.671603
-1257.346676	6.940340	1.676608
-1260.914224	6.177549	1.681613
-1264.589131	-0.428926	1.686618
-1268.429103	-0.238685	1.691622
-1272.150726	-7.750469	1.696627
-1275.712663	1.552681	1.701632
-1280.092472	-5.871314	1.706637
-1283.034420	-0.714818	1.711642
-1287.366141	5.509253	1.716646
-1290.816090	-8.251926	1.721651
-1294.983271	4.739485	1.726656
-1298.710718	-0.297674	1.731661
-1302.156693	0.890229	1.736666
-1306.098266	0.481036	1.741670
-1309.410026	-4.342928	1.746675
-1313.207125	-0.933712	1.751680
-1317.273821	-1.470601	1.756685
-1321.055831	-1.945079	1.761690
-1325.260952	5.403500	1.766694
-1328.962269	1.770574	1.771699
-1332.424095	5.788085	1.776704
-1336.202065	6.390860	1.781709
-1339.636299	-0.743946	1.786714
-1343.543113	5.244973	1.791718
-1346.857153	1.572777	1.796723
-1351.290932	4.120815	1.801728
-1355.119646	7.522870	1.806733
-1358.794048	-5.109129	1.811738
-1362.563426	2.113325	1.816742
-1365.863740	-2.116558	1.821747
-1369.659140	2.657298	1.826752
-1373.678766	-1.445074	1.831757
-1377.555734	-5.836396	1.836762
-1381.358221	-0.036667	1.841766
-1384.887272	-2.662248	1.846771
-1389.162960	0.137332	1.851776
-1392.698449	-0.387716	1.856781
-1395.749755	2.269440	1.861786
-1399.926140	12.770773	1.866790
-1403.485747	1.963145	1.871795
-1407.989182	9.833926	1.876800
-1411.413048	3.592982	1.881805
-1414.998528	1.659955	1.886810
-1419.109334	1.915410	1.891814
-1422.327582	0.520831	1.896819
-1426.307429	2.448253	1.901824
-1430.244736	6.568440	1.906829
-1433.709938	11.123012	1.911834
-1437.650100	11.297464	1.916838
-1441.383692	8.291842	1.921843
-1445.185341	6.901984	1.926848
-1449.097924	7.513382	1.931853
-1452.629961	9.163785	1.936858
-1456.676660	20.772532	1.941862
-1460.044976	1.290485	1.946867
-1463.980835	2.900939	1.951872
-1467.855253	14.770595	1.956877
-1471.118155	10.040598	1.961882
-1475.312519	5.201045	1.966886
-1479.112277	-1.935174	1.971891
-1482.314504	5.897645	1.976896
-1486.356930	-1.114385	1.981901
-1489.929848	2.645254	1.986906
-1494.240366	4.584158	1.991910
-1497.724929	1.346349	1.996915
-1502.130133	4.251112	2.006912
-1503.393688	2.470502	2.016909
-1500.171738	4.628161	2.026906
-1497.033880	7.531799	2.036902
-1495.290789	2.348046	2.046899
-1493.446205	3.778038	2.056896
-1491.723423	-0.050615	2.066893
-1489.850944	0.378269	2.076890
-1487.809217	3.339021	2.086886
-1486.027863	-1.348993	2.096883
-1483.546903	3.662515	2.106880
-1481.664587	9.617874	2.116877
-1480.656219	6.998778	2.126874
-1478.107903	8.656452	2.136870
-1476.248493	5.675368	2.146867
-1474.395267	13.048596	2.156864
-1472.594927	10.567322	2.166861
-1470.668078	7.568331	2.176858
-1468.735068	7.315369	2.186854
-1467.141973	6.400341	2.196851
-1464.983935	6.014268	2.206848
-1463.322367	5.696887	2.216845
-1461.213909	-1.273120	2.226842
-1459.022103	0.554098	2.236838
-1457.196643	0.533820	2.246835
-1455.705936	1.819115	2.256832
-1453.586855	0.146622	2.266829
-1451.582187	1.319913	2.276826
-1449.920174	-0.092658	2.286822
-1448.364233	-5.294433	2.296819
-1446.360726	-1.627183	2.306816
-1444.036452	1.743888	2.316813
-1442.236354	0.468052	2.326810
-1440.640306	-3.249098	2.336806
-1438.687840	0.228135	2.346803
-1436.838647	4.867632	2.356800
-1434.453132	1.261867	2.366797
-1432.518901	-4.927697	2.376794
-1431.140982	1.148716	2.386790
-1429.363391	3.758480	2.396787
-1427.445864	-6.513866	2.406784
-1425.881586	-3.722022	2.416781
-1423.507040	-6.945705	2.426778
-1421.370668	-4.360818	2.436774
-1419.907177	-4.135523	2.446771
-1418.026882	2.225696	2.456768
-1415.860124	-0.215348	2.466765
-1414.099228	2.901180	2.476762
-1412.459223	1.183352	2.486758
-1410.588248	-1.032593	2.496755
-1408.179556	2.065532	2.506752
-1406.654584	-1.255651	2.516749
-1404.960746	-0.073996	2.526746
-1402.796348	1.332322	2.536742
-1400.797763	0.010947	2.546739
-1398.959135	2.300001	2.556736
-1397.539643	3.227638	2.566733
-1395.530515	4.108132	2.576730
-1393.376560	-4.155271	2.586726
-1391.328727	6.660419	2.596723
-1389.725647	5.746865	2.606720
-1387.923508	2.628244	2.616717
-1385.928260	-3.501437	2.626714
-1384.035290	3.927450	2.636710
-1381.787225	-0.488169	2.646707
-1380.681807	1.769548	2.656704
-1378.961345	2.359362	2.666701
-1376.674508	-4.238136	2.676698
-1374.600364	0.023266	2.686694
-1372.615246	3.785403	2.696691
-1370.974330	1.969422	2.706688
-1369.254240	6.452495	2.716685
-1367.078250	8.475737	2.726682
-1365.016945	4.469233	2.736678
-1363.420364	0.166715	2.746675
-1361.687890	6.944612	2.756672
-1359.520526	5.700575	2.766669
-1357.466778	4.093099	2.776666
-1356.125445	6.324924	2.786662
-1354.182575	1.491839	2.796659
-1352.337147	0.957569	2.806656
-1350.409146	-1.893759	2.816653
-1348.435960	-3.705152	2.826650
-1346.512547	2.686638	2.836646
-1344.575769	-4.475145	2.846643
-1342.802686	3.260882	2.856640
-1340.845867	2.916944	2.866637
-1338.968300	-4.204236	2.876634
-1337.171287	-3.761530	2.886630
-1335.167737	2.918045	2.896627
-1333.406595	-0.913581	2.906624
-1331.615236	-3.865921	2.916621
-1329.594095	-5.014084	2.926618
-1327.512690	-0.671700	2.936614
-1325.791469	2.492784	2.946611
-1324.000728	-2.246972	2.956608
-1321.980551	1.700054	2.966605
-1320.559072	-3.466730	2.976602
-1318.592021	-6.209350	2.986598
-1316.451409	-5.056181	2.996595
-1314.553394	0.742038	3.006592
-1312.755961	0.966133	3.016589
-1310.996202	-5.790575	3.026586
-1308.815160	-5.773060	3.036582
-1307.227609	0.015254	3.046579
-1305.427610	4.407961	3.056576
-1303.574306	2.313658	3.066573
-1301.291381	2.645258	3.076570
-1299.297342	-1.597852	3.086566
-1297.468088	0.172371	3.096563
-1296.049574	-3.028527	3.106560
-1294.070780	-0.257632	3.116557
-1292.098560	-1.134562	3.126554
-1290.162308	3.336714	3.136550
-1288.158974	-1.453375	3.146547
-1286.569135	2.133643	3.156544
-1284.769580	-2.285914	3.166541
-1282.520906	-1.060784	3.176538
-1280.785449	4.436560	3.186534
-1278.997405	-1.800160	3.196531
-1277.032996	5.312995	3.206528
-1275.277413	0.401846	3.216525
-1273.165754	-5.109125	3.226522
-1271.477159	1.408004	3.236518
-1269.573224	0.635686	3.246515
-1267.819177	1.031658	3.256512
-1265.720119	2.066315	3.266509
-1263.942213	3.193279	3.276506
-1261.966247	-6.287170	3.286502
-1260.404602	-2.753001	3.296499
-1258.434942	-2.613396	3.306496
-1256.369411	-3.279485	3.316493
-1254.149305	-3.235848	3.326490
-1252.632365	-7.075299	3.336486
-1250.634052	1.534627	3.346483
-1249.119388	1.194346	3.356480
-1247.273666	-2.388961	3.366477
-1245.186639	4.270400	3.376474
-1243.045499	1.987576	3.386470
-1241.451756	-0.295690	3.396467
-1239.642553	2.703544	3.406464
-1237.352979	1.328713	3.416461
-1235.760497	-0.862647	3.426458
-1234.005656	-2.695376	3.436454
-1232.215149	-2.667265	3.446451
-1229.948374	0.504347	3.456448
-1228.388244	-2.713738	3.466445
-1226.434230	2.681678	3.476442
-1224.128188	-0.183538	3.486438
-1222.549692	-0.350606	3.496435
-1220.733499	4.445240	3.506432
-1219.182282	4.708498	3.516429
-1216.897723	-0.053583	3.526426
-1215.232974	3.176769	3.536422
-1213.193659	2.119994	3.546419
-1211.198205	1.521685	3.556416
-1209.734425	-1.798409	3.566413
-1207.677302	-2.108134	3.576410
-1205.703024	1.543710	3.586406
-1203.942661	2.638144	3.596403
-1202.140965	3.683589	3.606400
-1200.226281	5.020659	3.616397
-1198.202993	0.278163	3.626394
-1196.293358	-1.776367	3.636390
-1194.166748	2.751980	3.646387
-1192.744033	-0.347250	3.656384
-1190.885239	-1.159601	3.666381
-1188.623905	0.029023	3.676378
-1187.094344	-6.116639	3.686374
-1185.024919	-6.843830	3.696371
-1183.454161	-3.276021	3.706368
-1181.250000	-1.992605	3.716365
-1179.499048	-3.697387	3.726362
-1177.752915	-4.738971	3.736358
-1175.778587	-0.604571	3.746355
-1173.887171	-2.914034	3.756352
-1171.857892	-0.669865	3.766349
-1170.235736	-3.648020	3.776346
-1168.122116	1.716066	3.786342
-1165.880374	-5.667562	3.796339
-1164.518063	-0.071704	3.806336
-1162.559099	0.911973	3.816333
-1160.344074	3.320670	3.826330
-1159.116077	3.838244	3.836326
-1157.511311	5.172435	3.846323
-1155.252536	10.317953	3.856320
-1153.155949	1.135760	3.866317
-1151.288299	1.889698	3.876314
-1149.008222	5.064211	3.886310
-1147.308106	4.690539	3.896307
-1145.628321	4.973639	3.906304
-1143.969144	11.733800	3.916301
-1142.281512	6.851359	3.926298
-1140.083302	1.176193	3.936294
-1138.050934	5.740120	3.946291
-1136.040212	6.293234	3.956288
-1134.293561	8.040567	3.966285
-1132.370366	1.838390	3.976282
-1130.917134	7.011587	3.986278
-1129.028986	6.007683	3.996275
-1127.178720	3.985904	4.006272
-1124.990104	1.086758	4.016269
-1122.981405	7.495245	4.026266
-1121.250588	2.951996	4.036262
-1119.616431	1.307999	4.046259
-1117.841696	5.246691	4.056256
-1115.507142	8.877426	4.066253
-1113.565892	4.249829	4.076250
-1112.018985	6.259110	4.086246
-1109.994414	12.690965	4.096243
-1108.373927	6.198127	4.106240
-1106.436785	7.607266	4.116237
-1104.134071	-0.630183	4.126234
-1102.340590	5.346552	4.136230
-1100.916324	10.341754	4.146227
-1098.826534	2.996494	4.156224
-1097.160766	1.775484	4.166221
-1094.748148	-6.936900	4.176218
-1093.031937	4.121263	4.186214
-1091.314492	6.028551	4.196211
-1089.267297	6.537485	4.206208
-1087.664617	4.781527	4.216205
-1085.523199	5.260847	4.226202
-1083.555021	8.993240	4.236198
-1082.040365	3.429540	4.246195
-1079.995336	1.679440	4.256192
-1078.152884	2.181247	4.266189
-1076.196988	-3.936808	4.276186
-1074.455141	1.623954	4.286182
-1071.935577	-2.106204	4.296179
-1070.648234	-3.733712	4.306176
-1069.139994	-5.431160	4.316173
-1066.921167	-3.019113	4.326170
-1065.048255	-4.587893	4.336166
-1063.235005	-5.023639	4.346163
-1061.140618	1.107352	4.356160
-1059.526525	-0.357310	4.366157
-1057.502807	1.059909	4.376154
-1055.433532	4.040658	4.386150
-1053.941308	10.935442	4.396147
-1052.146467	7.120265	4.406144
-1049.898634	-0.691977	4.416141
-1048.058137	-3.379949	4.426138
-1046.207019	-1.152948	4.436134
-1044.595948	-5.122710	4.446131
-1042.202133	-10.216072	4.456128
-1040.596487	-6.222627	4.466125
-1038.737611	-10.217939	4.476122
-1036.634579	-1.128700	4.486118
-1034.893846	-8.485925	4.496115
-1033.005710	0.177818	4.506112
-1031.376974	-1.432808	4.516109
-1029.750932	-1.799249	4.526106
-1027.590362	3.565945	4.536102
-1025.557515	-0.294826	4.546099
-1023.532012	-3.161965	4.556096
-1021.858028	-1.033379	4.566093
-1019.974278	-2.020276	4.576090
-1017.981134	-10.425454	4.586086
-1016.084161	-2.453254	4.596083
-1014.458309	-0.390305	4.606080
-1012.404807	3.166623	4.616077
-1010.564253	1.039457	4.626074
-1008.555163	-0.515924	4.636070
-1006.934632	-1.402296	4.646067
-1005.179697	-4.044734	4.656064
-1003.312518	0.341324	4.666061
-1000.957313	-3.502457	4.676058
-999.383732	-4.028634	4.686054
-997.449963	-4.426948	4.696051
-995.632286	0.390091	4.706048
-993.711873	-3.863961	4.716045
-991.618221	-2.563053	4.726042
-989.988343	-6.862073	4.736038
-988.045239	-1.839320	4.746035
-986.048998	-4.805358	4.756032
-984.591914	-4.736500	4.766029
-982.145736	-0.071619	4.776026
-980.245202	-2.260842	4.786022
-978.951165	-5.612981	4.796019
-977.010112	0.493400	4.806016
-975.129864	4.648798	4.816013
-973.031268	1.687324	4.826010
-971.146012	-3.264157	4.836006
-969.028150	-3.543883	4.846003
-967.115707	-3.193948	4.856000
-965.624768	-3.923290	4.865997
-964.082266	-3.264418	4.875994
-961.795078	-3.987785	4.885990
-959.710310	-7.359476	4.895987
-958.096841	-4.117841	4.905984
-956.186773	-5.061804	4.915981
-954.463792	-7.110271	4.925978
-952.365228	-6.438569	4.935974
-950.204595	-3.734684	4.945971
-948.579374	-0.029505	4.955968
-947.102967	-1.696944	4.965965
-945.076417	-4.345282	4.975962
-943.135865	-6.404221	4.985958
-941.039435	-9.592552	4.995955
-939.526170	-5.941660	5.005952
-937.133089	-3.434966	5.015949
-935.333223	-8.131485	5.025946
-933.838974	-10.571060	5.035942
-931.870282	-5.767666	5.045939
-929.575761	-3.236143	5.055936
-928.032320	-6.342976	5.065933
-926.161959	-5.743930	5.075930
-924.397443	0.049346	5.085926
-922.436410	-3.405818	5.095923
-920.542842	0.930301	5.105920
-918.663306	3.978866	5.115917
-916.712679	0.173357	5.125914
-914.565374	1.209394	5.135910
-913.185382	-0.854873	5.145907
-911.271615	3.259233	5.155904
-909.487451	1.157202	5.165901
-907.298886	5.666773	5.175898
-905.054394	2.777111	5.185894
-903.558790	0.616330	5.195891
-901.935323	1.962428	5.205888
-900.318846	7.243251	5.215885
-897.958076	-2.129234	5.225882
-895.918202	-2.722771	5.235878
-894.508078	1.013427	5.245875
-892.249226	-4.914694	5.255872
-890.328394	-7.631805	5.265869
-888.400491	-5.758585	5.275866
-887.082291	-3.255073	5.285862
-884.913713	-3.635943	5.295859
-882.902508	-6.035799	5.305856
-881.125646	-4.554383	5.315853
-879.198344	-4.469379	5.325850
-877.174909	-3.341318	5.335846
-875.263928	-7.405583	5.345843
-873.731188	-3.380582	5.355840
-871.804197	-4.281174	5.365837
-869.913716	-6.142971	5.375834
-867.926339	-3.020416	5.385830
-866.161621	-2.936348	5.395827
-864.378280	1.732911	5.405824
-862.042769	1.510727	5.415821
-860.299749	-2.021204	5.425818
-858.578972	-4.279903	5.435814
-856.771125	-2.887581	5.445811
-854.746179	-7.125927	5.455808
-853.105873	-3.507478	5.465805
-851.155566	-3.727955	5.475802
-849.222412	-3.696899	5.485798
-847.467383	-1.352931	5.495795
-845.281800	1.939938	5.505792
-843.535631	0.590612	5.515789
-841.984847	5.097058	5.525786
-839.843831	-2.571474	5.535782
-837.808351	-2.085307	5.545779
-835.977495	3.299045	5.555776
-834.363253	8.188627	5.565773
-832.386833	-1.024192	5.575770
-830.465791	-2.034799	5.585766
-828.276505	-0.505589	5.595763
-826.605747	5.433063	5.605760
-824.618360	8.704635	5.615757
-823.067958	8.654381	5.625754
-821.318531	6.228741	5.635750
-819.453842	6.143514	5.645747
-817.497232	7.804357	5.655744
-815.263224	9.629026	5.665741
-813.235835	9.472402	5.675738
-811.478917	10.497247	5.685734
-809.664520	5.940946	5.695731
-808.023055	5.945020	5.705728
-806.189887	8.653022	5.715725
-804.122755	4.787251	5.725722
-802.310771	0.190267	5.735718
-800.694673	-2.636540	5.745715
-798.713750	2.951293	5.755712
-796.635676	1.111472	5.765709
-794.832686	1.992858	5.775706
-792.781573	1.288757	5.785702
-790.745365	-4.484911	5.795699
-788.773889	-5.725869	5.805696
-787.419870	2.936412	5.815693
-785.731161	2.366050	5.825690
-783.545916	-0.530773	5.835686
-781.812855	4.974726	5.845683
-779.637099	12.077962	5.855680
-777.715625	8.490531	5.865677
-775.919761	2.021050	5.875674
-774.122405	0.005335	5.885670
-772.374921	3.866263	5.895667
-770.533255	3.219462	5.905664
-768.770582	3.543419	5.915661
-766.469583	3.250143	5.925658
-764.712875	2.809603	5.935654
-763.074231	0.451611	5.945651
-761.031241	-4.213064	5.955648
-758.731578	-1.361813	5.965645
-757.203178	1.989357	5.975642
-755.397968	5.259821	5.985638
-753.457871	8.908671	5.995635
-751.926622	1.967678	6.005632
-749.745024	5.918518	6.015629
-747.623273	2.206620	6.025626
-746.086992	3.963348	6.035622
-744.105570	0.567991	6.045619
-742.424150	2.484375	6.055616
-740.248325	1.364475	6.065613
-738.608259	6.456755	6.075610
-736.848570	-1.549405	6.085606
-734.462897	-3.997260	6.095603
-732.875159	1.816962	6.105600
-731.108951	4.724609	6.115597
-729.401855	3.925052	6.125594
-727.148554	-1.275645	6.135590
-725.355148	1.277180	6.145587
-723.492625	3.904300	6.155584
-721.299814	2.587841	6.165581
-719.625975	4.245487	6.175578
-717.920239	-2.592255	6.185574
-716.290554	-4.679555	6.195571
-714.248551	3.863105	6.205568
-712.041557	2.262431	6.215565
-710.152301	-5.447415	6.225562
-708.624519	3.986169	6.235558
-706.725277	4.134558	6.245555
-704.147435	0.366537	6.255552
-702.809097	1.052638	6.265549
-701.271342	0.257650	6.275546
-699.139441	-8.964016	6.285542
-697.035923	-6.033620	6.295539
-695.646752	-4.885545	6.305536
-693.483431	-1.723936	6.315533
-691.370767	-0.756141	6.325530
-689.845130	-0.864541	6.335526
-687.851792	-0.899467	6.345523
-685.864106	-5.073648	6.355520
-684.137630	-7.130911	6.365517
-682.326775	-4.182295	6.375514
-680.306191	-5.545849	6.385510
-678.252305	-1.903451	6.395507
-676.573372	0.667855	6.405504
-674.535449	-1.693417	6.415501
-673.015728	-2.475420	6.425498
-670.659471	-3.224321	6.435494
-669.282447	0.102668	6.445491
-667.307610	0.765312	6.455488
-665.080411	-0.228996	6.465485
-663.336678	2.161650	6.475482
-661.666226	0.929723	6.485478
-659.778156	1.627416	6.495475
-658.344391	1.950160	6.505472
-655.991811	6.136897	6.515469
-653.841772	-1.322856	6.525466
-652.230548	0.676352	6.535462
-650.087137	-2.401744	6.545459
-648.407907	0.473439	6.555456
-646.534278	7.989820	6.565453
-644.828233	-0.395994	6.575450
-642.812800	2.603295	6.585446
-640.616265	-0.809962	6.595443
-639.034023	5.473569	6.605440
-637.522689	5.470397	6.615437
-635.457610	-0.342153	6.625434
-633.523915	-3.318254	6.635430
-631.432148	-6.159442	6.645427
-629.354133	-4.055368	6.655424
-627.834581	0.831974	6.665421
-626.089167	0.956998	6.675418
-624.046859	-2.956998	6.685414
-622.117967	-0.365329	6.695411
-620.168615	-1.015923	6.705408
-618.269074	-4.230793	6.715405
-616.543644	-2.351157	6.725402
-614.703576	3.353027	6.735398
-612.598327	-0.751981	6.745395
-611.072856	2.730958	6.755392
-609.421008	-2.967989	6.765389
-607.110920	-0.894636	6.775386
-605.020835	0.915714	6.785382
-603.359136	-7.507134	6.795379
-601.673072	-4.701081	6.805376
-599.690917	-2.742185	6.815373
-597.498436	0.540544	6.825370
-596.062701	-6.715991	6.835366
-593.791527	-4.355749	6.845363
-591.763108	-5.103683	6.855360
-590.045050	-2.150564	6.865357
-588.767646	-2.386274	6.875354
-586.671486	0.133237	6.885350
-584.799282	-3.783961	6.895347
-583.144805	-3.823533	6.905344
-580.952647	0.282090	6.915341
-578.850445	-4.928181	6.925338
-577.033562	-6.165046	6.935334
-575.223282	-5.972485	6.945331
-573.373188	-2.010119	6.955328
-571.604495	0.373912	6.965325
-569.413268	0.386498	6.975322
-567.658766	0.750275	6.985318
-565.942661	-4.112351	6.995315
-563.880482	-0.348012	7.005312
-562.271391	-2.066549	7.015309
-560.206820	1.967707	7.025306
-558.229981	0.307401	7.035302
-556.527642	0.512563	7.045299
-555.059716	-1.105870	7.055296
-552.637677	1.451408	7.065293
-550.690191	-2.139208	7.075290
-548.882005	-4.711570	7.085286
-547.142841	-7.873994	7.095283
-545.583734	-2.472520	7.105280
-543.186210	5.242131	7.115277
-541.260159	1.143398	7.125274
-539.500824	-0.580360	7.135270
-537.715610	-3.867270	7.145267
-535.803720	0.196357	7.155264
-534.123511	-2.061585	7.165261
-532.198938	-0.253628	7.175258
-530.047867	-5.238297	7.185254
-528.498400	-2.200105	7.195251
-526.316775	2.706472	7.205248
-524.667061	-0.704994	7.215245
-523.084050	-4.416836	7.225242
-520.517997	-3.178962	7.235238
-518.461835	-3.465274	7.245235
-517.006131	-2.313932	7.255232
-515.829181	3.202922	7.265229
-513.529756	0.465271	7.275226
-511.386210	-5.503757	7.285222
-509.604663	-8.833500	7.295219
-507.675154	-2.273567	7.305216
-505.703627	0.603298	7.315213
-504.160400	1.963317	7.325210
-501.775870	1.580759	7.335206
-500.000744	0.802814	7.345203
-498.421948	-6.367978	7.355200
-496.677620	4.177825	7.365197
-494.572399	1.439119	7.375194
-492.296557	-2.429918	7.385190
-490.738313	-3.223211	7.395187
-489.313747	-0.126030	7.405184
-487.273568	2.388908	7.415181
-485.114700	0.507307	7.425178
-483.131008	-1.564372	7.435174
-481.349184	1.207122	7.445171
-479.335921	1.600444	7.455168
-477.720783	-1.974225	7.465165
-475.953186	-6.261532	7.475162
-474.071038	-8.034394	7.485158
-471.958463	-0.429689	7.495155
-470.339394	-8.255925	7.505152
-468.223708	-3.060171	7.515149
-466.111034	-6.335258	7.525146
-464.515385	-5.701923	7.535142
-462.603625	-5.577708	7.545139
-460.403826	1.180910	7.555136
-458.811238	2.708346	7.565133
-457.281418	1.123589	7.575130
-455.211704	2.228894	7.585126
-453.499238	-3.326667	7.595123
-451.152517	-3.369154	7.605120
-449.712531	-0.790355	7.615117
-447.635471	0.173788	7.625114
-445.911233	2.099939	7.635110
-443.741430	1.373661	7.645107
-442.163866	1.665878	7.655104
-440.124961	-0.982384	7.665101
-437.861637	-1.339372	7.675098
-436.436856	-5.851615	7.685094
-434.476443	-3.668777	7.695091
-432.742611	-5.225292	7.705088
-430.866976	0.104935	7.715085
-428.815136	-2.791363	7.725082
-427.050908	-0.545224	7.735078
-424.804263	-4.391040	7.745075
-423.662043	3.381347	7.755072
-421.541139	-1.613515	7.765069
-419.597240	3.844913	7.775066
-417.497354	7.803233	7.785062
-415.885702	3.404374	7.795059
-413.714221	1.688211	7.805056
-411.666613	2.655448	7.815053
-410.128163	3.967314	7.825050
-408.540083	9.229112	7.835046
-406.214070	8.026698	7.845043
-403.933409	6.033736	7.855040
-403.053539	8.229248	7.865037
-400.796909	0.913743	7.875034
-398.918212	-2.313668	7.885030
-397.032459	-2.161250	7.895027
-395.375215	4.750157	7.905024
-393.255173	9.265838	7.915021
-391.250070	7.689282	7.925018
-389.659622	1.341721	7.935014
-387.547462	-0.277306	7.945011
-385.733574	2.697797	7.955008
-383.849038	1.412252	7.965005
-382.126150	3.197570	7.975002
-379.695241	-1.290833	7.984998
-378.350416	4.089376	7.994995
-376.336544	-0.607692	8.004992
-374.385248	1.466079	8.014989
-372.724395	5.487483	8.024986
-370.607126	-0.355650	8.034982
-368.860014	1.635771	8.044979
-366.853178	0.432404	8.054976
-365.190161	10.543265	8.064973
-363.261788	6.697927	8.074970
-361.475666	2.040329	8.084966
-359.582775	-0.000309	8.094963
-357.377361	-1.268562	8.104960
-355.830070	2.091773	8.114957
-353.764968	3.486027	8.124954
-351.527966	2.027794	8.134950
-349.937856	2.192214	8.144947
-348.554404	2.394851	8.154944
-346.572624	1.544763	8.164941
-344.755280	-4.187628	8.174938
-342.484841	-3.140414	8.184934
-340.567439	1.418352	8.194931
-338.789993	1.018686	8.204928
-336.911296	6.192326	8.214925
-335.047706	3.964650	8.224922
-333.137778	8.486764	8.234918
-331.213747	0.929559	8.244915
-329.324793	6.014497	8.254912
-327.476582	5.830339	8.264909
-325.818391	5.338104	8.274906
-323.776365	4.912030	8.284902
-321.800776	-0.794540	8.294899
-319.996114	1.286623	8.304896
-318.368906	-5.778602	8.314893
-316.234875	-0.538488	8.324890
-314.734453	-0.283186	8.334886
-312.661576	-4.151312	8.344883
-310.335950	-0.820131	8.354880
-308.859764	-0.795425	8.364877
-306.939259	1.245322	8.374874
-305.046128	-0.220301	8.384870
-303.163749	-2.282035	8.394867
-301.160284	0.269327	8.404864
-299.537191	-4.114462	8.414861
-297.600553	1.101029	8.424858
-295.554335	0.276270	8.434854
-293.839562	-4.689977	8.444851
-291.813666	2.037703	8.454848
-289.979901	-0.851957	8.464845
-288.412137	0.855670	8.474842
-286.541249	-2.029290	8.484838
-284.030006	0.635358	8.494835
-282.324945	-1.248935	8.504832
-280.806541	6.705592	8.514829
-278.961576	6.506993	8.524826
-276.619337	6.454696	8.534822
-275.044223	5.199346	8.544819
-273.227177	8.443097	8.554816
-271.336354	8.180911	8.564813
-269.280343	5.777585	8.574810
-267.414274	1.259650	8.584807
-265.606024	-3.758982	8.594803
-263.700254	-2.586736	8.604800
-261.983273	-9.763379	8.614797
-260.472265	-4.052781	8.624794
-258.105659	-1.672367	8.634791
-255.791786	-2.692406	8.644787
-254.282144	-3.448828	8.654784
-252.744136	0.739528	8.664781
-250.546804	-1.471055	8.674778
-248.608999	-3.866744	8.684775
-247.039430	-5.901678	8.694771
-245.132138	-1.923676	8.704768
-243.229941	1.502693	8.714765
-241.154716	-2.980757	8.724762
-239.438936	0.636068	8.734759
-237.552746	0.307109	8.744755
-235.451147	-5.702826	8.754752
-233.234028	-0.500235	8.764749
-231.906671	-7.101801	8.774746
-230.077270	-9.408936	8.784743
-228.074675	-11.876590	8.794739
-226.340254	-1.166127	8.804736
-224.321844	-8.681776	8.814733
-222.458330	-7.612530	8.824730
-220.560208	-7.842354	8.834727
-218.485645	-1.314266	8.844723
-216.743501	-6.625460	8.854720
-215.016072	-7.503797	8.864717
-213.065052	-4.382592	8.874714
-211.160903	-4.318618	8.884711
-209.766475	-4.307917	8.894707
-207.383228	-2.094738	8.904704
-205.732151	-5.014687	8.914701
-204.059338	-3.468903	8.924698
-201.675894	-3.346825	8.934695
-199.793748	-4.569441	8.944691
-197.648080	0.355337	8.954688
-196.392708	-1.852547	8.964685
-194.362662	-0.896820	8.974682
-192.656475	-8.852136	8.984679
-190.597761	-3.983186	8.994675
-188.752842	-7.075093	9.004672
-186.752409	-4.558726	9.014669
-185.057071	-1.710619	9.024666
-182.733927	-7.259374	9.034663
-181.313193	-0.423109	9.044659
-179.337132	-2.698071	9.054656
-177.834188	-1.845988	9.064653
-175.955660	-6.125341	9.074650
-173.787309	-8.588597	9.084647
-171.333482	-4.544230	9.094643
-169.729211	-0.868732	9.104640
-168.058682	-5.860153	9.114637
-166.341922	-6.427585	9.124634
-164.471760	-2.629719	9.134631
-162.278742	-3.578397	9.144627
-160.605692	0.822777	9.154624
-158.766900	6.234940	9.164621
-156.959454	4.212198	9.174618
-154.595713	3.887533	9.184615
-152.771894	-4.342069	9.194611
-151.444939	-3.618672	9.204608
-149.588226	-7.631852	9.214605
-147.584760	-14.434710	9.224602
-145.298443	-2.704749	9.234599
-143.778423	2.775524	9.244595
-141.914326	-2.070844	9.254592
-139.464710	-1.804762	9.264589
-138.210990	-5.643788	9.274586
-136.279697	-4.833532	9.284583
-134.452360	-4.989133	9.294579
-132.215002	0.020341	9.304576
-130.391783	4.891374	9.314573
-128.717030	8.473785	9.324570
-126.726537	1.889334	9.334567
-125.098257	-1.401341	9.344563
-123.070225	1.037604	9.354560
-121.409759	-0.789187	9.364557
-119.468868	-2.401250	9.374554
-117.306320	0.879752	9.384551
-115.333594	2.561867	9.394547
-113.561489	-2.418107	9.404544
-111.911456	0.518818	9.414541
-109.910218	8.637628	9.424538
-108.037537	0.623745	9.434535
-106.309779	-2.570952	9.444531
-104.025318	0.039024	9.454528
-102.211786	-0.723220	9.464525
-100.371652	-2.766563	9.474522
-98.562635	3.690143	9.484519
-96.952305	-6.512886	9.494515
-95.029537	1.540737	9.504512
-93.038502	7.523992	9.514509
-91.361455	-2.353757	9.524506
-89.137352	-2.922003	9.534503
-87.766993	1.207823	9.544499
-85.429814	4.562047	9.554496
-83.221743	5.386519	9.564493
-81.958981	2.867943	9.574490
-79.848390	6.321493	9.584487
-77.891050	1.931437	9.594483
-76.007991	4.946193	9.604480
-74.327140	4.265993	9.614477
-72.611662	10.609915	9.624474
-70.253234	4.787202	9.634471
-68.768881	-0.518867	9.644467
-66.955802	1.898472	9.654464
-64.977123	7.285902	9.664461
-63.055899	4.486456	9.674458
-61.036525	2.634896	9.684455
-59.127294	0.810525	9.694451
-57.393990	4.679334	9.704448
-55.544168	1.169289	9.714445
-53.723067	1.239667	9.724442
-51.580212	5.265500	9.734439
-49.607726	4.642010	9.744435
-48.111198	0.987037	9.754432
-46.391210	4.421424	9.764429
-44.036731	8.014971	9.774426
-42.422394	3.399189	9.784423
-40.734901	8.192362	9.794419
-38.658872	10.118431	9.804416
-36.596338	7.268680	9.814413
-35.010292	0.538617	9.824410
-32.865384	4.372429	9.834407
-31.053028	3.675229	9.844403
-29.298746	2.738608	9.854400
-27.283421	6.355934	9.864397
-25.320844	-0.567923	9.874394
-23.621865	1.472599	9.884391
-21.552399	-6.165158	9.894387
-19.730332	0.992036	9.904384
-18.280201	-0.079366	9.914381
-15.969684	-10.510718	9.924378
-13.967498	-9.771452	9.934375
-12.554671	-5.736621	9.944371
-10.428768	-3.055540	9.954368
-8.430378	-7.017475	9.964365
-6.942952	-4.324140	9.974362
-5.388726	16.470788	9.984359
-4.384842	47.590637	9.994355
-2.941281	94.733095	10.004352
-1.284435	161.273948	10.014349
0.000000	225.211316	10.019354
0.508360	253.237721	10.024359
1.248091	282.712979	10.029363
1.391556	318.354949	10.034368
1.733120	344.846647	10.039373
2.495178	366.374557	10.044378
2.557592	384.912869	10.049383
2.869848	386.177727	10.054387
3.349988	411.617934	10.059392
3.625438	415.945808	10.064397
3.746772	417.724566	10.069402
3.783060	427.294661	10.074407
4.026047	422.354180	10.079411
3.905093	434.751377	10.084416
3.915964	431.085768	10.089421
3.996007	423.233751	10.094426
3.842005	425.330102	10.099431
3.846110	416.264717	10.104435
3.570516	422.751849	10.109440
3.874927	438.781344	10.114445
3.899130	441.108052	10.119450
3.976272	451.708085	10.124455
3.835889	440.515447	10.129459
3.811711	454.498628	10.134464
4.029785	445.139971	10.139469
4.198644	445.185265	10.144474
4.187707	452.840794	10.149479
4.452087	452.861027	10.154483
4.163582	450.479059	10.159488
4.327822	457.524317	10.164493
4.409230	470.923380	10.169498
4.339658	493.312448	10.174503
4.677048	489.721888	10.179507
4.725199	495.374362	10.184512
5.069429	482.059870	10.189517
4.828089	473.698482	10.194522
4.950226	477.135725	10.199527
5.345195	467.123461	10.204531
5.087876	474.667304	10.209536
4.811463	472.170370	10.214541
5.138123	469.505695	10.219546
4.956371	471.161171	10.224551
5.394157	471.021414	10.229555
4.997726	474.681379	10.234560
5.013831	476.181357	10.239565
4.663818	479.468249	10.244570
4.394720	484.097132	10.249575
5.113474	482.133748	10.254579
4.895824	504.000348	10.259584
5.048758	502.622246	10.264589
5.208265	511.089335	10.269594
5.067415	515.298755	10.274599
5.651186	513.101941	10.279603
5.542643	522.023927	10.284608
5.706060	523.290239	10.289613
5.438447	520.555350	10.294618
4.962028	521.469544	10.299623
5.492722	520.471915	10.304627
5.415348	518.265703	10.309632
5.475712	525.218279	10.314637
5.812573	538.723990	10.319642
5.970460	548.370412	10.324647
6.394350	550.761233	10.329651
5.903151	538.926859	10.334656
6.450564	538.796725	10.339661
5.830972	539.417716	10.344666
5.544316	539.022448	10.349671
5.816578	543.394719	10.354675
5.952694	556.958154	10.359680
6.021850	568.159219	10.364685
6.267897	564.975868	10.369690
6.029413	576.562438	10.374695
6.304207	572.945883	10.379699
6.441304	572.245861	10.384704
6.667155	571.234579	10.389709
6.923953	571.567943	10.394714
6.501648	573.537033	10.399719
6.803227	569.589451	10.404723
6.651948	571.068797	10.409728
6.643772	574.860367	10.414733
6.974110	569.183704	10.419738
7.046145	578.261069	10.424743
6.792230	564.031865	10.429747
6.714405	561.547838	10.434752
7.024772	564.729808	10.439757
6.805231	558.472850	10.444762
6.383072	576.192927	10.449767
6.314497	568.639073	10.454771
6.460052	580.678464	10.459776
6.704862	580.968096	10.464781
6.967031	585.303426	10.469786
6.716684	600.486002	10.474791
7.136806	606.993656	10.479795
6.836363	616.304244	10.484800
6.764572	622.886378	10.489805
7.125548	623.496740	10.494810
6.952458	629.593763	10.499815
7.305180	624.502170	10.504819
7.146747	634.905490	10.509824
7.422815	645.333789	10.514829
7.684769	650.955187	10.519834
7.776245	651.978063	10.524839
7.773729	644.318112	10.529843
7.610744	642.770356	10.534848
7.501692	650.864370	10.539853
7.693976	652.158505	10.544858
7.759298	663.420689	10.549863
7.650667	659.697756	10.554867
7.677581	664.307121	10.559872
7.793868	664.473138	10.564877
8.042378	660.117013	10.569882
7.881742	663.634358	10.574887
8.004707	660.711296	10.579891
8.102750	669.352821	10.584896
8.093413	671.069542	10.589901
8.757977	663.711640	10.594906
8.294043	669.012254	10.599911
8.136671	663.430626	10.604915
8.087533	675.619522	10.609920
8.294077	676.072423	10.614925
8.005374	676.855758	10.619930
7.873240	675.520202	10.624935
8.635900	683.722922	10.629939
8.591554	702.067554	10.634944
9.287282	695.729792	10.639949
9.238766	679.503081	10.644954
8.738586	685.096092	10.649959
8.864867	664.051406	10.654963
8.839421	671.009287	10.659968
8.790811	670.898849	10.664973
8.529245	670.493354	10.669978
8.567829	679.142711	10.674983
8.897590	675.305135	10.679987
8.880487	687.511047	10.684992
9.145272	697.790135	10.689997
9.197791	690.438085	10.695002
8.956517	695.063838	10.700007
9.599707	695.179381	10.705011
9.280487	686.294798	10.710016
9.297752	676.455711	10.715021
8.986534	684.515329	10.720026
9.271609	703.024526	10.725031
9.752736	706.554212	10.730035
9.091489	702.548660	10.735040
9.030969	716.010557	10.740045
9.260236	722.925183	10.745050
8.851390	727.172715	10.750055
9.338906	721.338393	10.755059
9.199436	725.367637	10.760064
9.518510	721.112682	10.765069
9.966913	735.892170	10.770074
9.909935	745.264114	10.775079
9.818985	731.679429	10.780083
9.677345	743.148073	10.785088
9.981995	744.459265	10.790093
10.028724	742.684494	10.795098
9.957340	748.329134	10.800103
10.080971	746.315393	10.805107
10.128455	749.786022	10.810112
10.071362	751.347524	10.815117
9.882602	745.403757	10.820122
10.139745	758.959643	10.825127
10.036712	758.890903	10.830131
10.171930	754.653647	10.835136
10.443333	749.797005	10.840141
10.500181	747.066837	10.845146
10.528145	754.239014	10.850151
10.504371	753.232627	10.855155
10.161091	755.883700	10.860160
10.082149	752.535776	10.865165
10.283741	748.675159	10.870170
9.979509	761.162853	10.875175
10.568346	770.802627	10.880179
10.575110	779.749199	10.885184
11.221309	779.467525	10.890189
11.521771	763.488780	10.895194
11.377354	764.467638	10.900199
11.185804	749.972575	10.905203
11.190693	744.509541	10.910208
11.189357	740.812401	10.915213
11.049184	748.777990	10.920218
10.830017	744.821757	10.925223
11.173935	745.096768	10.930227
10.886484	741.099745	10.935232
10.929101	749.070308	10.940237
11.434101	754.449156	10.945242
11.601505	769.808553	10.950247
11.526588	756.208467	10.955251
11.277758	754.389240	10.960256
11.332599	747.032818	10.965261
11.379990	756.715682	10.970266
11.321194	768.523421	10.975271
11.637405	761.585193	10.980275
11.615621	779.604739	10.985280
11.612030	784.115557	10.990285
11.958865	779.972667	10.995290
11.540693	782.048834	11.000295
11.754749	781.030089	11.005299
11.774666	780.909479	11.010304
11.967733	786.774838	11.015309
11.846618	787.905619	11.020314
11.615768	798.774613	11.025319
12.201983	782.368309	11.030323
12.237631	787.163315	11.035328
12.385643	784.626321	11.040333
12.313240	781.910809	11.045338
12.091131	790.715449	11.050343
12.628398	787.779353	11.055347
12.535003	795.785891	11.060352
11.938269	790.171394	11.065357
12.378355	782.102336	11.070362
11.993208	792.916862	11.075367
12.278511	794.157956	11.080371
12.130161	797.262313	11.085376
11.929332	796.186415	11.090381
12.463005	795.500886	11.095386
12.498118	803.342898	11.100391
12.567524	808.738030	11.105395
12.555822	814.678377	11.110400
12.808967	815.449733	11.115405
12.767639	818.996788	11.120410
12.818943	822.113101	11.125415
13.058764	818.155914	11.130419
12.914616	821.280871	11.135424
12.946155	817.927016	11.140429
13.002935	814.980536	11.145434
12.925619	821.305944	11.150439
12.730429	806.891582	11.155443
12.690713	813.747766	11.160448
12.742464	819.061852	11.165453
13.048599	826.755172	11.170458
12.532225	844.728150	11.175463
13.004804	840.458291	11.180467
13.300059	850.582259	11.185472
13.348502	844.295816	11.190477
13.924936	834.412071	11.195482
13.613381	851.277459	11.200487
13.669679	845.548606	11.205491
13.480993	844.278783	11.210496
13.221282	853.830814	11.215501
14.128890	841.469404	11.220506
13.810750	854.893488	11.225511
14.079105	853.705562	11.230515
14.109496	851.772135	11.235520
13.985355	855.248925	11.240525
14.148909	842.903378	11.245530
14.066867	848.083312	11.250535
13.819141	849.056993	11.255539
14.109082	847.748527	11.260544
13.871262	849.686019	11.265549
14.093338	847.699990	11.270554
13.979782	855.584887	11.275559
13.958928	848.555994	11.280563
14.136151	848.084340	11.285568
14.431927	854.866045	11.290573
14.528384	853.458913	11.295578
14.262669	858.048247	11.300583
13.953142	852.992368	11.305587
14.125570	858.187883	11.310592
14.157315	864.104221	11.315597
14.675920	876.676712	11.320602
14.443455	877.847117	11.325607
14.978804	885.496824	11.330611
14.840727	883.574910	11.335616
14.591297	881.378014	11.340621
14.941387	879.022670	11.345626
14.379976	886.957528	11.350631
14.919661	883.565876	11.355635
15.103667	880.484677	11.360640
15.100442	885.398087	11.365645
15.224837	872.009643	11.370650
14.847787	881.407732	11.375655
15.202609	882.745071	11.380659
15.433737	881.741155	11.385664
15.070710	884.587078	11.390669
15.298288	876.503488	11.395674
15.148559	890.638453	11.400679
15.289220	881.353992	11.405683
15.445874	885.854733	11.410688
14.936212	886.938457	11.415693
15.326785	883.941049	11.420698
15.168247	885.865742	11.425703
15.236047	886.669275	11.430707
15.214256	882.337724	11.435712
15.166300	893.372395	11.440717
15.710993	896.131763	11.445722
15.533371	904.290955	11.450727
16.164596	911.072406	11.455731
16.097632	914.168358	11.460736
15.808002	901.321791	11.465741
16.101157	886.202713	11.470746
15.930288	892.435244	11.475751
15.884517	881.949214	11.480755
15.803053	895.835640	11.485760
15.727046	910.078375	11.490765
16.159779	911.888272	11.495770
15.976364	916.045097	11.500775
16.255127	920.816224	11.505779
16.212958	915.094754	11.510784
15.852732	924.236173	11.515789
16.567116	914.274647	11.520794
16.524098	923.896934	11.525799
16.683182	910.021726	11.530803
16.500848	915.415454	11.535808
16.458173	919.724989	11.540813
16.704189	908.944573	11.545818
16.337945	919.855022	11.550823
16.486699	920.992831	11.555827
16.957440	916.010777	11.560832
16.168262	913.165509	11.565837
16.906553	910.110451	11.570842
16.629632	917.298267	11.575847
16.683455	915.639495	11.580851
16.702293	925.780118	11.585856
16.601332	924.163278	11.590861
16.765291	919.193165	11.595866
16.732882	925.199077	11.600871
16.883254	936.664769	11.605875
17.046023	942.124071	11.610880
16.791888	939.384822	11.615885
16.970112	942.192427	11.620890
16.832504	945.945885	11.625895
17.287427	945.445956	11.630899
17.360567	943.910578	11.635904
17.785175	943.661766	11.640909
17.601045	937.717920	11.645914
17.254071	939.873478	11.650919
17.315946	943.265894	11.655923
17.695350	931.324580	11.660928
17.342411	946.351399	11.665933
17.437979	941.500767	11.670938
17.729432	945.258817	11.675943
17.659955	934.590896	11.680947
17.626370	941.421217	11.685952
17.915897	950.970714	11.690957
17.951159	939.102214	11.695962
17.396562	952.670738	11.700967
18.182652	962.177735	11.705971
18.211873	969.364400	11.710976
18.035155	965.607672	11.715981
18.075563	962.233714	11.720986
18.351852	961.813754	11.725991
18.245052	953.706930	11.730995
18.319048	948.959072	11.736000
18.136554	947.563839	11.741005
18.475907	948.388315	11.746010
18.263925	951.740452	11.751015
18.406758	950.031284	11.756019
18.313629	952.199372	11.761024
18.609374	967.664459	11.766029
18.936552	957.227327	11.771034
18.572900	941.841077	11.776039
18.345482	938.231994	11.781043
18.657016	946.066947	11.786048
18.854390	961.072451	11.791053
18.502434	959.591405	11.796058
18.474278	971.931275	11.801063
18.839904	965.854871	11.806067
18.964058	967.529395	11.811072
19.057379	966.405814	11.816077
19.329711	964.316813	11.821082
19.122475	969.420359	11.826087
19.118631	949.077329	11.831091
19.053055	949.748999	11.836096
18.912917	961.806091	11.841101
18.953406	956.712664	11.846106
19.091611	965.530229	11.851111
19.169987	963.409747	11.856115
19.366371	962.985725	11.861120
19.086228	961.631311	11.866125
19.275704	958.255478	11.871130
18.936308	971.926068	11.876135
19.340553	964.840026	11.881139
19.242911	960.107778	11.886144
19.058859	972.572667	11.891149
19.507830	971.834550	11.896154
19.392643	997.200159	11.901159
19.882621	992.155574	11.906163
19.730320	989.095700	11.911168
19.489878	1003.300398	11.916173
20.216155	999.941860	11.921178
19.873763	1001.535724	11.926183
19.719525	988.314163	11.931187
20.048293	985.055756	11.936192
20.172672	987.349581	11.941197
20.133045	983.206979	11.946202
20.265904	1001.085399	11.951207
20.354814	994.505381	11.956211
20.340165	994.366222	11.961216
20.079851	996.189563	11.966221
20.323660	996.429640	11.971226
20.407920	991.783430	11.976231
20.059615	989.239526	11.981235
20.257229	996.216939	11.986240
20.251272	998.561533	11.991245
20.482836	994.672033	11.996250
20.286557	995.631376	12.001255
20.116233	990.808160	12.006259
20.383373	991.795808	12.011264
20.243643	998.441065	12.016269
20.424296	1009.714120	12.021274
20.774689	1015.862063	12.026279
20.816274	1019.010476	12.031283
21.022328	1019.591367	12.036288
20.808986	1014.136445	12.041293
20.801119	995.416401	12.046298
20.738459	993.585752	12.051303
20.876928	993.062318	12.056307
21.181045	994.570990	12.061312
20.813628	993.826795	12.066317
20.892521	993.800282	12.071322
20.817728	993.101440	12.076327
20.738237	987.063057	12.081331
20.872939	990.328919	12.086336
20.795653	992.770215	12.091341
20.961004	988.572730	12.096346
20.840402	1000.418873	12.101351
20.545050	993.032772	12.106355
20.832915	988.498494	12.111360
20.565419	996.729590	12.116365
20.740360	986.947746	12.121370
20.673534	990.790919	12.126375
20.724036	985.221297	12.131379
21.039459	989.406296	12.136384
20.688057	990.593549	12.141389
20.928184	983.954055	12.146394
20.635948	970.888405	12.151399
20.575161	966.859565	12.156403
20.634403	969.452315	12.161408
20.594498	975.314665	12.166413
20.733419	978.577827	12.171418
20.660698	979.213619	12.176423
20.972292	981.852314	12.181427
20.672572	972.779487	12.186432
20.667609	972.978928	12.191437
20.621036	965.623211	12.196442
20.274038	979.945236	12.201447
20.275201	977.572335	12.206451
20.790663	998.771174	12.211456
20.656234	1003.133174	12.216461
20.900801	999.030656	12.221466
20.840923	1006.402746	12.226471
20.768779	1005.844764	12.231475
20.974368	1002.656421	12.236480
20.351334	994.675192	12.241485
21.149344	988.378198	12.246490
20.559797	980.131895	12.251495
20.198497	980.664009	12.256499
20.665118	988.008975	12.261504
20.667485	996.591298	12.266509
20.805733	996.082506	12.271514
21.107594	1006.440311	12.276519
20.940773	995.029966	12.281523
21.230382	984.339523	12.286528
20.710194	982.496533	12.291533
21.028365	973.254213	12.296538
20.815427	985.716170	12.301543
20.985888	981.763335	12.306547
20.698374	976.239434	12.311552
20.872061	980.496495	12.316557
20.568036	980.821421	12.321562
20.407293	980.968625	12.326567
20.747902	976.702410	12.331571
20.788849	972.832967	12.336576
20.235815	978.589483	12.341581
21.150085	978.872498	12.346586
21.021855	977.676771	12.351591
21.054325	976.747963	12.356595
21.201675	967.559014	12.361600
20.534301	957.753451	12.366605
20.633472	949.045268	12.371610
20.434232	956.406096	12.376615
20.875188	970.693276	12.381619
21.058355	964.740128	12.386624
20.620607	956.830176	12.391629
20.496722	949.370486	12.396634
20.427234	946.385237	12.401639
20.609593	965.296434	12.406643
21.090346	971.357273	12.411648
20.705384	970.361879	12.416653
20.610700	951.243488	12.421658
20.380174	950.741874	12.426663
20.511659	967.507347	12.431667
20.763860	970.046487	12.436672
20.500015	982.011912	12.441677
20.766729	983.006738	12.446682
20.523009	981.410422	12.451687
20.494066	973.539710	12.456691
20.734765	985.199159	12.461696
20.714023	991.098491	12.466701
20.902804	980.472707	12.471706
20.873255	978.629277	12.476711
21.014750	980.868851	12.481715
21.072264	967.549817	12.486720
20.661252	961.938939	12.491725
20.433322	955.585758	12.496730
20.610936	955.809158	12.501735
20.566360	952.137539	12.506739
20.484980	956.628192	12.511744
20.553929	975.500425	12.516749
20.656572	980.380319	12.521754
20.922438	983.937898	12.526759
20.914690	980.052724	12.531763
20.766145	965.231931	12.536768
20.563739	967.485862	12.541773
20.315310	970.469650	12.546778
20.899042	984.067237	12.551783
20.803551	979.908556	12.556787
20.782805	971.436445	12.561792
20.626977	971.804251	12.566797
21.121020	963.479537	12.571802
20.748590	954.358794	12.576807
20.481475	961.055480	12.581811
20.757670	962.061706	12.586816
20.520703	964.609717	12.591821
20.561708	958.414896	12.596826
20.561853	960.139103	12.601831
20.664184	970.283597	12.606835
20.756127	977.318592	12.611840
20.756781	984.662135	12.616845
21.021264	974.343503	12.621850
20.531310	976.527922	12.626855
20.457399	967.146780	12.631859
20.802631	966.099216	12.636864
20.663093	971.175366	12.641869
20.495918	964.775055	12.646874
20.596043	976.345311	12.651879
21.020806	988.332411	12.656883
20.986859	975.901807	12.661888
20.754879	965.463041	12.666893
20.575772	968.835597	12.671898
20.688668	972.236641	12.676903
20.475298	970.337888	12.681907
20.632629	969.985692	12.686912
20.610153	966.053704	12.691917
20.727746	964.892409	12.696922
20.657758	967.776524	12.701927
20.673562	965.262564	12.706931
21.044634	959.887063	12.711936
20.890011	975.679242	12.716941
21.350246	968.104788	12.721946
20.968530	970.815774	12.726951
20.748316	978.008500	12.731955
20.837526	961.392359	12.736960
20.741170	973.559190	12.741965
20.704238	970.763352	12.746970
20.732018	970.550209	12.751975
20.869838	980.272971	12.756979
21.078132	971.389357	12.761984
20.827577	974.079434	12.766989
21.132945	966.344826	12.771994
21.230433	951.561993	12.776999
20.747130	951.017273	12.782003
20.949279	944.734830	12.787008
20.690050	947.148893	12.792013
21.137350	943.838594	12.797018
21.017288	952.629776	12.802023
20.619549	950.867241	12.807027
21.240187	939.535078	12.812032
20.880113	953.542351	12.817037
20.920444	935.590948	12.822042
20.171856	923.929091	12.827047
20.697307	933.823781	12.832051
20.806110	953.009281	12.837056
20.652809	945.714899	12.842061
20.670169	940.843730	12.847066
20.528974	944.917140	12.852071
20.950746	955.365272	12.857075
21.265079	943.952599	12.862080
20.472868	936.407769	12.867085
20.428117	917.985454	12.872090
20.676398	918.476601	12.877095
20.443350	930.740650	12.882099
20.679954	938.063058	12.887104
20.892749	949.194771	12.892109
20.789911	939.876236	12.897114
20.483114	926.830882	12.902119
20.605405	941.553587	12.907123
20.787667	946.874156	12.912128
20.782875	944.578859	12.917133
20.696725	924.350630	12.922138
20.686614	921.169681	12.927143
20.278724	925.525258	12.932147
20.495220	936.478697	12.937152
20.643388	946.815841	12.942157
20.763057	951.774121	12.947162
20.642262	957.203101	12.952167
20.623856	960.839810	12.957171
20.731751	953.927741	12.962176
20.676996	962.483918	12.967181
20.548725	961.988850	12.972186
20.679479	954.624050	12.977191
20.865350	960.227028	12.982195
20.950149	958.919779	12.987200
20.344903	968.711122	12.992205
20.941959	953.813818	12.997210
20.939118	954.952753	13.002215
20.809111	959.323851	13.007219
20.753953	935.585068	13.012224
20.480973	941.264343	13.017229
20.795964	948.021086	13.022234
21.049389	942.955890	13.027239
20.400136	935.085765	13.032243
20.497082	925.275490	13.037248
20.145087	942.057910	13.042253
20.675626	951.911476	13.047258
20.830932	956.225760	13.052263
20.799933	960.093968	13.057267
20.751036	959.454240	13.062272
20.859400	958.539656	13.067277
20.936607	966.817423	13.072282
20.858113	952.559758	13.077287
20.745797	947.697794	13.082291
21.070120	933.607131	13.087296
20.405400	936.712025	13.092301
20.574139	937.923776	13.097306
20.786573	936.822800	13.102311
20.207323	932.466025	13.107315
20.908729	942.514892	13.112320
20.960968	947.093158	13.117325
21.038084	940.173346	13.122330
20.800692	931.545772	13.127335
20.465537	930.797628	13.132339
20.801583	928.654287	13.137344
20.849409	933.528960	13.142349
20.988712	933.338538	13.147354
20.696132	937.405930	13.152359
20.896793	931.782160	13.157363
21.025857	936.562379	13.162368
20.743464	938.933440	13.167373
20.656726	936.208121	13.172378
20.492079	933.644580	13.177383
20.236094	936.896102	13.182387
20.442147	933.642562	13.187392
20.173745	937.817912	13.192397
20.520302	927.413793	13.197402
20.555320	937.957433	13.202407
20.370659	942.398686	13.207411
20.871315	950.569106	13.212416
20.994538	946.948454	13.217421
20.446525	942.860659	13.222426
20.816008	933.501014	13.227431
20.465486	947.730851	13.232435
20.748529	936.444337	13.237440
20.397704	950.176471	13.242445
20.562523	966.271498	13.247450
20.792069	975.662744	13.252455
21.007741	980.519706	13.257459
20.876071	957.381766	13.262464
20.191695	950.976586	13.267469
20.715297	951.852761	13.272474
20.716666	973.766940	13.277479
20.799517	971.255694	13.282483
20.818355	965.743612	13.287488
20.474520	960.896471	13.292493
20.571538	969.506760	13.297498
20.727657	970.671336	13.302503
20.600873	973.674925	13.307507
20.849307	964.351016	13.312512
20.805082	974.522219	13.317517
20.710741	968.621783	13.322522
20.614691	959.559438	13.327527
20.428662	974.698192	13.332531
20.872084	973.428531	13.337536
20.747488	985.256006	13.342541
20.899934	969.303218	13.347546
20.858271	952.911628	13.352551
20.520697	943.689389	13.357555
20.675425	933.545522	13.362560
20.535734	942.366905	13.367565
20.849504	951.931194	13.372570
20.803815	941.958261	13.377575
20.448765	947.715162	13.382579
20.658069	938.259031	13.387584
20.590979	951.767258	13.392589
20.647936	956.223535	13.397594
21.123238	966.073160	13.402599
20.574417	961.291954	13.407603
20.730676	948.826391	13.412608
20.651758	952.781759	13.417613
20.688463	943.519427	13.422618
20.523160	949.936551	13.427623
20.504007	950.551314	13.432627
20.636970	961.243965	13.437632
20.852066	972.722665	13.442637
20.875973	963.364227	13.447642
20.718937	951.824343	13.452647
20.611297	956.809362	13.457651
20.572471	948.256680	13.462656
20.606823	956.935338	13.467661
20.820829	965.592276	13.472666
20.734497	951.390429	13.477671
20.673951	949.233374	13.482675
20.566137	948.411514	13.487680
20.415834	960.533110	13.492685
20.481625	967.898635	13.497690
21.108250	974.010252	13.502695
20.627721	979.165790	13.507699
20.882706	977.168577	13.512704
20.651462	984.143331	13.517709
21.109081	966.474422	13.522714
20.527129	958.861558	13.527719
20.787142	960.746470	13.532723
20.647653	951.691183	13.537728
20.753375	952.225326	13.542733
20.595387	955.225578	13.547738
20.648356	942.724441	13.552743
20.740924	954.562027	13.557747
20.699867	956.099878	13.562752
20.948901	956.089982	13.567757
20.858038	953.225237	13.572762
20.799387	947.237769	13.577767
20.628245	958.348870	13.582771
20.916728	948.724422	13.587776
20.482805	961.854637	13.592781
20.645161	959.318314	13.597786
20.959553	955.801460	13.602791
20.882792	955.529664	13.607795
20.957822	951.772802	13.612800
20.914976	963.368351	13.617805
20.741211	954.813144	13.622810
20.715021	953.631897	13.627815
20.643200	958.653801	13.632819
20.905957	949.032580	13.637824
20.867079	958.450891	13.642829
20.758112	955.222149	13.647834
21.253188	952.681279	13.652839
20.428606	945.626332	13.657843
20.599605	936.384794	13.662848
20.361612	953.265705	13.667853
20.765125	954.002209	13.672858
21.271501	952.550048	13.677863
20.565795	942.040549	13.682867
20.625097	927.610861	13.687872
20.332373	934.774159	13.692877
20.285413	940.144290	13.697882
20.648492	951.349314	13.702887
20.559007	952.467579	13.707891
20.660061	954.003169	13.712896
20.501649	964.356179	13.717901
20.387348	961.542425	13.722906
20.443516	959.527987	13.727911
20.197468	971.364433	13.732915
20.725357	960.633151	13.737920
20.630524	967.298723	13.742925
20.444844	965.615879	13.747930
20.665513	964.816249	13.752935
20.533352	960.312943	13.757939
20.513262	955.000564	13.762944
20.451330	974.430493	13.767949
20.977364	980.248705	13.772954
21.055492	981.060341	13.777959
20.548100	975.485325	13.782963
20.800801	969.918539	13.787968
20.586858	970.805909	13.792973
20.530115	965.442575	13.797978
20.458090	965.981537	13.802983
20.666811	980.091045	13.807987
20.804193	988.242059	13.812992
20.534706	998.532426	13.817997
20.779169	993.947563	13.823002
21.084479	990.134630	13.828007
20.525480	981.606380	13.833011
20.586750	960.362443	13.838016
20.445338	974.985921	13.843021
20.769432	990.951034	13.848026
20.934078	996.447139	13.853031
21.092104	995.681932	13.858035
21.116700	981.124726	13.863040
20.770175	975.561995	13.868045
20.304421	975.903994	13.873050
20.750257	963.628373	13.878055
20.670121	973.261791	13.883059
20.757301	961.957130	13.888064
20.998517	968.680741	13.893069
20.895597	977.695969	13.898074
21.140794	964.970805	13.903079
20.759044	978.277219	13.908083
20.790690	969.331131	13.913088
20.677891	970.631418	13.918093
20.906650	972.589979	13.923098
21.183099	964.906513	13.928103
20.959851	971.584630	13.933107
20.550857	951.735794	13.938112
20.632089	941.135976	13.943117
20.685443	939.231363	13.948122
20.845055	938.937987	13.953127
20.736773	946.173086	13.958131
20.831643	933.758718	13.963136
20.898856	945.996560	13.968141
20.469659	941.423400	13.973146
20.409647	935.581826	13.978151
20.732368	946.918503	13.983155
20.407269	938.602802	13.988160
20.675366	942.613142	13.993165
20.596471	965.063301	13.998170
20.757926	966.130252	14.003175
20.858138	973.733427	14.008179
20.651323	956.793445	14.013184
20.743894	957.764049	14.018189
20.639919	950.588328	14.023207
20.874730	943.127173	14.028224
20.412091	945.010584	14.033242
20.697045	958.442925	14.038259
20.751911	956.916926	14.043277
20.798499	969.525131	14.048295
20.830830	969.641289	14.053312
20.926553	973.763763	14.058330
21.218511	963.840281	14.063347
21.032078	952.868049	14.068365
20.761113	951.438470	14.073383
21.007513	942.349636	14.078400
20.770819	947.307887	14.083418
20.712240	942.728708	14.088435
20.773894	951.311625	14.093453
20.596876	966.224844	14.098471
21.003740	970.840068	14.103488
21.023501	978.210814	14.108506
20.984724	972.308461	14.113523
20.738168	985.835500	14.118541
20.613306	982.585870	14.123559
20.950546	974.473239	14.128576
20.852558	984.995480	14.133594
21.174008	968.943315	14.138611
20.840599	971.946770	14.143629
20.668012	981.102183	14.148647
20.916115	969.434529	14.153664
20.857344	988.726595	14.158682
21.048704	999.303573	14.163699
21.238091	1010.002557	14.168717
21.198701	1015.543183	14.173735
21.110914	1009.970501	14.178752
20.986323	1015.552114	14.183770
21.008346	1019.176573	14.188787
21.412894	1015.831441	14.193805
21.274789	1021.493725	14.198823
21.316134	1010.501691	14.203840
21.201284	1014.706740	14.208858
21.306348	1010.093184	14.213875
21.411022	1022.641864	14.218893
21.387004	1018.593387	14.223911
21.500708	1011.087212	14.228928
21.349393	1021.468611	14.233946
21.360853	1014.013431	14.238963
21.689388	1008.259126	14.243981
21.286107	1018.028562	14.248999
21.624957	1017.355895	14.254016
21.546997	1017.606719	14.259034
21.364096	1016.258892	14.264051
21.346072	1012.370424	14.269069
21.211457	1014.657867	14.274087
21.180687	1006.819355	14.279104
21.614757	1028.210184	14.284122
21.880659	1032.275148	14.289139
22.033906	1037.188618	14.294157
22.017830	1039.590002	14.299175
22.410883	1019.569333	14.304192
21.781665	1022.103796	14.309210
21.848154	1019.537934	14.314227
21.727971	1007.286109	14.319245
21.559419	1021.160064	14.324263
22.071257	1012.669816	14.329280
21.847606	1025.267310	14.334298
21.934898	1018.903925	14.339315
21.771080	1013.815175	14.344333
21.498739	1016.697925	14.349351
21.694000	1012.442945	14.354368
21.307442	1018.223816	14.359386
21.695136	1017.155348	14.364403
21.988074	1022.955947	14.369421
21.722050	1031.243886	14.374439
21.928934	1030.727712	14.379456
21.983896	1040.846970	14.384474
21.782174	1040.611104	14.389491
22.088691	1048.142968	14.394509
22.022129	1045.781422	14.399527
22.168980	1040.311029	14.404544
22.052707	1035.200339	14.409562
21.788427	1040.526759	14.414579
21.763981	1043.500484	14.419597
21.779359	1044.447952	14.424615
22.303656	1040.980308	14.429632
21.924751	1041.855998	14.434650
22.036754	1037.563314	14.439667
22.130799	1032.439008	14.444685
22.099345	1039.021266	14.449703
22.043778	1033.065072	14.454720
22.051616	1049.897595	14.459738
22.380623	1061.274300	14.464755
22.746380	1069.548432	14.469773
22.654256	1063.853630	14.474791
22.792856	1039.658553	14.479808
22.484221	1037.941704	14.484826
22.344024	1036.258578	14.489843
22.341062	1033.765255	14.494861
22.173139	1040.313033	14.499879
22.584218	1034.087448	14.504896
22.384254	1036.604618	14.509914
22.516531	1041.425222	14.514931
22.380272	1038.235806	14.519949
22.012518	1052.167566	14.524967
22.790038	1063.665024	14.529984
22.461659	1070.195835	14.535002
22.584657	1075.055444	14.540019
22.790800	1066.104552	14.545037
22.853422	1078.001385	14.550055
23.088260	1060.624511	14.555072
22.752943	1049.945079	14.560090
22.191779	1043.049120	14.565107
22.950921	1047.340170	14.570125
22.547231	1061.548985	14.575143
22.587190	1067.313836	14.580160
22.839812	1066.965816	14.585178
22.605549	1071.422867	14.590195
22.815190	1065.138099	14.595213
22.712376	1071.498337	14.600231
22.976254	1064.611315	14.605248
22.842403	1073.386493	14.610266
22.909008	1069.370106	14.615283
23.148940	1065.307467	14.620301
23.049790	1069.302344	14.625319
22.978032	1061.430277	14.630336
22.917043	1060.821045	14.635354
22.845581	1070.661977	14.640371
22.974774	1067.092767	14.645389
22.651511	1064.915792	14.650407
22.756236	1068.465054	14.655424
22.869826	1066.868342	14.660442
22.986386	1068.100059	14.665459
23.045639	1062.795475	14.670477
22.891486	1070.784707	14.675495
22.977659	1068.347360	14.680512
22.767570	1073.777894	14.685530
22.953704	1069.332718	14.690547
23.030334	1066.696600	14.695565
23.050969	1078.798284	14.700583
23.285780	1081.220443	14.705600
23.439550	1089.167520	14.710618
23.201257	1091.443615	14.715635
23.763875	1091.739344	14.720653
23.554839	1083.143900	14.725671
23.989991	1074.226973	14.730688
24.131455	1066.405360	14.735706
23.605455	1063.582389	14.740723
23.583894	1055.493043	14.745741
23.222728	1062.625576	14.750759
23.613941	1056.868381	14.755776
23.301761	1056.697914	14.760794
23.362769	1063.711210	14.765811
23.621365	1068.972007	14.770829
23.328767	1064.623481	14.775847
23.560088	1063.410549	14.780864
23.510126	1062.983298	14.785882
23.322960	1065.863264	14.790899
23.428948	1050.293658	14.795917
23.174447	1066.929036	14.800935
23.228076	1065.685149	14.805952
23.669052	1073.753066	14.810970
23.897471	1096.376577	14.815987
24.059283	1083.218014	14.821005
23.645302	1079.874617	14.826023
23.324166	1075.746350	14.831040
23.516186	1086.921348	14.836058
23.548371	1093.949837	14.841075
23.723818	1084.668347	14.846093
24.029649	1093.882360	14.851111
23.992608	1087.258748	14.856128
23.979875	1094.472510	14.861146
23.975231	1098.990600	14.866163
23.992858	1092.706457	14.871181
24.136223	1092.520094	14.876199
23.961849	1096.093985	14.881216
24.073984	1092.878900	14.886234
23.906676	1100.084519	14.891251
23.940513	1086.128545	14.896269
23.751590	1095.813241	14.901287
24.030859	1094.607048	14.906304
23.903547	1087.738659	14.911322
23.991994	1093.328265	14.916339
24.227010	1086.837549	14.921357
23.846240	1086.707583	14.926375
23.693172	1094.963590	14.931392
23.900838	1096.771463	14.936410
24.266067	1099.795719	14.941427
24.864087	1086.289508	14.946445
24.342076	1096.538044	14.951463
24.111441	1090.077554	14.956480
24.169456	1093.978163	14.961498
24.162824	1096.409435	14.966515
24.293732	1088.649074	14.971533
24.242037	1090.527402	14.976551
23.945828	1087.506749	14.981568
24.726413	1099.152538	14.986586
24.349065	1106.263454	14.991603
24.382922	1112.670753	14.996621
24.414104	1125.044700	15.001639
24.485589	1126.381007	15.006656
24.767505	1120.209819	15.011674
24.615515	1128.106183	15.016691
24.522222	1104.425209	15.021709
24.369512	1106.083046	15.026727
24.739247	1115.665276	15.031744
24.896801	1113.100322	15.036762
24.626113	1106.462034	15.041779
24.507328	1096.230518	15.046797
24.683442	1109.519435	15.051815
24.435561	1121.859331	15.056832
24.670240	1121.297835	15.061850
24.454373	1126.555743	15.066867
24.522750	1124.954965	15.071885
24.793597	1123.764388	15.076903
24.407018	1128.610588	15.081920
24.895286	1115.694079	15.086938
24.892177	1117.567623	15.091955
24.717226	1112.772503	15.096973
24.728752	1123.699713	15.101991
24.772308	1129.432866	15.107008
25.057999	1118.499263	15.112026
24.887053	1123.567564	15.117043
24.973163	1122.184629	15.122061
24.977126	1120.989413	15.127079
24.682690	1126.113930	15.132096
25.021145	1123.821523	15.137114
24.462912	1138.921536	15.142131
25.108019	1138.834986	15.147149
25.193992	1151.680699	15.152167
25.343239	1149.912498	15.157184
25.608254	1142.902403	15.162202
25.259070	1137.930046	15.167219
25.261952	1136.779112	15.172237
25.394914	1125.271646	15.177255
25.485904	1114.582073	15.182272
25.327899	1113.107518	15.187290
25.307808	1116.173825	15.192307
25.788918	1111.878076	15.197325
25.741948	1115.200190	15.202343
25.457269	1117.648033	15.207360
25.869029	1110.720281	15.212378
25.323191	1123.925497	15.217395
25.344758	1111.672122	15.222413
25.446980	1116.467585	15.227431
25.131861	1116.921289	15.232448
25.222811	1116.171035	15.237466
25.080086	1125.323775	15.242483
25.136259	1116.401324	15.247501
25.424142	1127.001606	15.252519
25.182496	1137.541493	15.257536
25.795314	1142.087596	15.262554
25.807235	1144.131021	15.267571
25.413237	1143.644634	15.272589
25.861806	1142.447602	15.277607
25.571270	1142.616362	15.282624
25.936641	1143.199474	15.287642
25.791762	1147.330961	15.292659
25.537596	1141.466655	15.297677
26.019796	1136.476173	15.302695
25.808669	1147.614029	15.307712
25.907927	1147.660835	15.312730
25.602937	1141.688305	15.317747
25.831288	1151.990914	15.322765
25.822742	1143.619348	15.327783
25.795962	1153.952709	15.332800
25.942913	1141.006110	15.337818
25.643785	1139.534881	15.342835
25.928765	1137.964686	15.347853
25.957107	1139.346584	15.352871
25.839054	1144.256994	15.357888
25.805793	1139.554116	15.362906
26.099813	1142.770918	15.367923
26.134427	1146.438526	15.372941
26.030917	1137.918273	15.377959
25.928703	1153.881915	15.382976
26.066401	1156.550282	15.387994
26.063615	1167.492576	15.393011
26.170118	1173.450404	15.398029
26.562601	1169.284805	15.403047
26.266996	1182.230613	15.408064
26.757672	1167.268215	15.413082
26.608350	1162.195830	15.418099
26.216666	1147.683970	15.423117
26.465419	1145.877448	15.428135
26.333209	1148.975189	15.433152
26.017109	1148.044706	15.438170
26.365782	1148.119226	15.443187
26.336953	1163.149361	15.448205
26.587254	1167.283181	15.453223
26.616972	1172.952182	15.458240
26.850486	1167.149539	15.463258
26.363410	1148.993517	15.468275
26.157395	1153.024062	15.473293
26.725955	1164.407412	15.478311
26.565749	1175.190073	15.483328
26.608717	1171.299770	15.488346
26.285182	1173.347954	15.493363
26.386860	1171.639092	15.498381
26.496230	1167.835837	15.503399
26.676336	1170.618598	15.508416
26.746555	1175.149467	15.513434
27.097533	1174.919631	15.518451
26.654216	1164.390930	15.523469
27.202953	1165.978511	15.528487
26.842107	1174.526896	15.533504
26.928082	1168.570007	15.538522
27.145762	1172.100320	15.543539
26.660609	1179.708529	15.548557
27.072919	1171.633324	15.553575
27.183772	1186.935225	15.558592
27.055274	1173.253875	15.563610
27.057237	1176.045918	15.568627
26.827766	1175.782129	15.573645
27.042219	1174.323636	15.578663
26.994394	1180.214612	15.583680
27.011742	1173.397767	15.588698
27.302492	1170.737913	15.593715
27.239595	1176.841331	15.598733
27.256824	1167.337293	15.603751
27.313572	1179.850612	15.608768
27.230976	1175.331393	15.613786
27.274163	1174.932659	15.618803
26.958968	1174.858384	15.623821
27.453876	1174.517644	15.628839
27.110111	1177.261082	15.633856
27.187201	1176.799050	15.638874
27.161818	1177.048736	15.643891
26.897946	1176.647133	15.648909
27.653533	1186.356967	15.653927
27.431426	1206.163564	15.658944
27.633233	1200.286024	15.663962
28.232699	1191.935786	15.668979
27.417039	1177.066243	15.673997
27.739880	1160.836464	15.679015
27.414355	1167.808591	15.684032
27.614171	1170.364333	15.689050
27.750659	1179.008960	15.694067
27.894239	1178.820590	15.699085
28.193027	1161.435003	15.704103
27.868542	1163.325068	15.709120
28.045313	1168.612528	15.714138
28.307641	1169.185354	15.719155
27.888987	1171.951474	15.724173
28.334915	1163.612221	15.729191
27.952165	1147.986146	15.734208
27.433456	1129.635161	15.739226
27.687534	1144.938451	15.744243
27.558882	1167.180341	15.749261
27.706347	1159.831704	15.754279
27.752806	1169.133149	15.759296
27.940359	1163.503360	15.764314
27.938705	1167.950873	15.769331
27.779953	1169.199485	15.774349
27.947092	1162.632573	15.779367
27.666913	1169.091770	15.784384
27.743821	1160.939025	15.789402
27.876936	1174.057404	15.794419
27.745774	1189.905959	15.799437
28.152210	1198.064121	15.804455
27.841227	1199.254184	15.809472
27.988493	1197.304413	15.814490
28.642085	1189.799295	15.819507
28.657951	1186.822761	15.824525
28.421852	1195.004072	15.829543
28.662417	1192.224069	15.834560
28.545870	1189.751377	15.839578
28.547766	1177.667478	15.844595
28.468408	1173.020529	15.849613
28.398409	1164.391357	15.854631
28.331339	1168.849693	15.859648
28.140340	1179.123424	15.864666
28.642655	1191.784392	15.869683
28.215555	1192.049800	15.874701
28.321487	1194.412178	15.879719
28.685478	1191.998445	15.884736
28.753319	1201.726986	15.889754
28.785964	1192.445505	15.894771
28.597559	1199.426422	15.899789
28.904333	1187.149287	15.904807
28.983815	1191.668336	15.909824
28.746774	1194.903754	15.914842
28.841776	1191.840811	15.919859
28.619843	1202.138760	15.924877
28.697052	1193.531975	15.929895
28.781828	1190.028230	15.934912
28.478706	1189.184109	15.939930
29.177344	1193.097749	15.944947
28.698813	1195.443791	15.949965
28.671073	1187.474343	15.954983
28.642976	1202.033093	15.960000
28.606628	1195.952273	15.965018
29.013535	1197.026337	15.970035
29.033770	1198.582872	15.975053
28.539616	1197.832137	15.980071
29.208742	1207.265842	15.985088
29.227321	1224.076631	15.990106
29.370032	1213.417103	15.995123
29.101479	1208.311203	16.000141
28.880201	1212.200274	16.005159
28.851094	1220.004743	16.010176
29.010411	1235.168844	16.015194
29.400051	1220.663124	16.020211
29.406974	1229.641830	16.025229
29.591540	1229.495649	16.030247
29.610537	1227.828911	16.035264
29.840804	1225.039250	16.040282
29.641751	1213.098447	16.045299
29.146809	1211.628105	16.050317
29.373839	1217.248330	16.055335
29.643704	1224.250301	16.060352
29.513300	1221.421289	16.065370
29.275830	1215.426523	16.070387
29.437119	1230.472162	16.075405
29.600162	1233.620094	16.080423
29.835140	1226.561564	16.085440
29.334263	1224.522114	16.090458
29.915183	1222.611777	16.095475
29.539604	1223.201450	16.100493
29.759775	1228.061377	16.105511
30.337734	1220.125082	16.110528
29.729048	1222.417059	16.115546
29.558478	1221.173013	16.120563
29.664007	1221.281741	16.125581
29.347062	1218.753238	16.130599
29.134313	1219.916222	16.135616
29.722427	1226.862054	16.140634
29.793632	1215.560795	16.145651
29.805546	1227.812920	16.150669
30.106505	1241.238825	16.155687
30.373664	1241.826182	16.160704
30.025489	1230.210957	16.165722
29.963962	1219.577780	16.170739
29.864956	1230.678359	16.175757
29.818942	1245.935161	16.180775
29.867786	1249.394431	16.185792
29.755451	1252.966384	16.190810
30.284721	1248.693052	16.195827
30.280114	1256.659495	16.200845
30.211827	1258.499345	16.205863
30.436832	1255.399138	16.210880
30.139035	1261.460179	16.215898
30.625822	1250.175050	16.220915
30.610681	1252.114458	16.225933
30.292807	1253.221446	16.230951
30.736348	1250.738549	16.235968
30.245096	1249.091178	16.240986
30.364272	1251.146938	16.246003
30.160307	1251.107533	16.251021
30.287644	1252.907936	16.256039
30.464538	1250.366024	16.261056
29.894413	1257.008838	16.266074
30.300786	1260.809206	16.271091
30.348216	1278.520694	16.276109
30.505425	1279.993118	16.281127
30.984506	1271.144145	16.286144
30.801967	1274.650573	16.291162
30.758020	1268.610795	16.296179
30.866181	1280.664555	16.301197
30.987211	1280.548953	16.306215
31.009318	1267.159442	16.311232
30.810718	1285.440330	16.316250
30.942235	1278.040431	16.321267
30.709350	1281.666920	16.326285
30.958231	1274.576849	16.331303
31.497061	1276.857930	16.336320
31.295952	1279.500149	16.341338
31.727600	1266.679451	16.346355
31.138167	1249.352739	16.351373
31.140647	1254.547267	16.356391
31.154433	1244.523651	16.361408
30.777817	1251.142341	16.366426
30.954660	1249.634380	16.371443
31.198543	1257.448367	16.376461
31.557147	1264.797376	16.381479
31.378957	1248.647110	16.386496
31.132283	1247.353506	16.391514
31.162896	1243.701937	16.396531
31.197917	1252.490784	16.401549
31.395795	1270.736751	16.406567
31.563949	1275.065803	16.411584
31.620537	1281.451162	16.416602
31.275866	1270.258965	16.421619
31.398802	1281.914885	16.426637
31.399005	1283.549278	16.431655
31.659692	1280.561068	16.436672
31.395144	1286.909356	16.441690
31.578369	1278.600516	16.446707
31.617772	1282.982356	16.451725
31.363122	1287.717001	16.456743
31.560461	1276.824422	16.461760
31.545294	1282.308623	16.466778
31.618814	1284.071009	16.471795
31.804501	1280.956276	16.476813
31.874740	1279.405561	16.481831
31.906892	1270.554469	16.486848
32.032879	1273.444961	16.491866
31.626494	1277.046467	16.496883
31.738454	1279.520826	16.501901
31.322325	1282.907844	16.506919
31.804297	1278.287466	16.511936
31.613720	1289.508521	16.516954
31.924380	1307.043009	16.521971
31.722763	1309.180158	16.526989
31.831352	1318.993132	16.532007
31.748335	1310.327920	16.537024
31.835658	1309.342826	16.542042
32.199154	1305.140031	16.547059
32.120627	1309.110172	16.552077
31.975903	1306.943499	16.557095
32.139821	1305.262931	16.562112
32.029594	1315.198465	16.567130
32.119467	1324.052364	16.572147
32.431815	1328.833915	16.577165
32.523374	1326.528688	16.582183
32.787374	1325.216031	16.587200
32.393772	1335.576575	16.592218
32.755926	1326.080238	16.597235
32.810287	1307.160275	16.602253
32.134682	1308.218749	16.607271
32.886600	1296.436123	16.612288
32.549130	1300.141970	16.617306
33.057936	1288.010054	16.622323
32.625615	1294.574921	16.627341
32.825434	1302.234661	16.632359
32.806875	1293.737555	16.637376
32.787658	1297.071486	16.642394
32.540085	1298.091221	16.647411
32.943603	1298.260285	16.652429
32.979458	1301.325698	16.657447
33.299326	1303.000963	16.662464
33.140306	1296.999409	16.667482
33.184800	1295.898026	16.672499
32.957372	1292.526140	16.677517
32.695398	1306.760884	16.682535
32.958971	1297.173976	16.687552
32.889736	1308.733326	16.692570
33.064951	1310.014854	16.697587
33.215204	1305.140292	16.702605
32.867773	1299.716756	16.707623
33.118759	1300.277752	16.712640
33.065809	1304.691181	16.717658
33.295882	1302.840596	16.722675
33.374113	1298.104774	16.727693
33.082905	1300.228934	16.732711
33.153941	1303.844662	16.737728
32.965211	1301.749319	16.742746
32.975217	1322.309641	16.747763
33.446616	1325.112572	16.752781
33.070498	1338.296743	16.757799
33.275731	1330.744010	16.762816
33.209928	1329.773750	16.767834
32.853892	1335.158525	16.772851
33.170739	1332.806796	16.777869
33.487807	1350.515446	16.782887
33.517013	1352.819343	16.787904
33.737074	1361.678504	16.792922
34.013423	1352.493739	16.797939
33.871203	1340.475372	16.802957
33.409707	1344.715137	16.807975
33.693500	1346.876556	16.812992
33.570782	1354.067165	16.818010
34.128688	1357.731332	16.823027
33.906671	1350.938124	16.828045
33.943461	1357.685208	16.833063
33.881732	1358.828609	16.838080
33.982291	1351.174512	16.843098
33.834741	1361.253495	16.848115
33.920554	1356.184042	16.853133
33.690614	1363.308780	16.858151
33.976027	1364.608824	16.863168
34.235987	1364.004400	16.868186
33.769446	1360.271492	16.873203
34.129446	1358.185613	16.878221
33.616106	1370.230636	16.883239
33.924839	1362.329011	16.888256
33.973498	1364.159060	16.893274
33.987616	1368.609438	16.898291
34.455066	1378.993262	16.903309
34.543199	1392.395940	16.908327
34.707889	1382.540081	16.913344
34.546282	1365.159181	16.918362
34.348601	1353.998419	16.923379
34.475802	1349.316396	16.928397
34.850378	1356.697359	16.933415
34.662238	1354.024298	16.938432
34.337104	1360.383791	16.943450
33.982543	1369.265092	16.948467
34.652046	1372.105332	16.953485
34.363386	1388.210246	16.958503
34.615404	1381.475133	16.963520
34.618246	1385.485283	16.968538
34.570238	1390.058140	16.973555
34.786263	1379.221347	16.978573
34.716905	1390.329556	16.983591
34.938010	1381.357021	16.988608
35.148133	1381.057231	16.993626
34.479374	1386.069223	16.998643
34.787464	1383.286272	17.003661
34.818577	1383.977496	17.008679
34.907062	1388.244248	17.013696
35.085785	1378.795078	17.018714
34.687533	1381.853038	17.023731
35.181901	1396.386571	17.028749
34.956817	1410.809983	17.033767
35.349643	1409.660289	17.038784
35.576491	1406.329006	17.043802
35.380290	1393.878474	17.048819
35.385173	1379.818530	17.053837
35.182943	1380.327300	17.058855
35.036281	1381.093497	17.063872
35.288369	1386.999278	17.068890
35.450752	1403.265479	17.073907
35.512484	1400.903144	17.078925
35.369808	1409.332747	17.083943
35.322903	1405.860588	17.088960
35.863085	1402.926413	17.093978
35.727302	1407.602521	17.098995
35.697857	1393.290947	17.104013
35.370307	1392.791189	17.109031
35.797036	1396.999557	17.114048
35.701776	1400.508374	17.119066
35.462549	1409.590415	17.124083
35.647893	1398.396237	17.129101
35.557010	1409.931418	17.134119
35.585656	1408.943385	17.139136
35.652664	1405.598165	17.144154
35.662934	1408.550652	17.149171
35.870335	1403.452463	17.154189
35.784003	1408.730779	17.159207
35.747401	1413.547773	17.164224
36.199701	1407.694536	17.169242
35.368866	1413.208778	17.174259
36.389555	1419.972648	17.179277
36.223646	1419.942860	17.184295
35.957557	1408.220507	17.189312
36.301885	1416.182722	17.194330
36.297826	1420.451175	17.199347
36.291878	1421.526349	17.204365
36.325363	1412.886779	17.209383
36.073436	1417.947010	17.214400
36.297594	1431.119293	17.219418
36.468534	1441.432332	17.224435
36.942379	1434.487494	17.229453
36.494701	1423.515227	17.234471
36.136243	1412.482392	17.239488
36.240905	1419.645859	17.244506
36.141447	1437.481540	17.249523
36.164228	1438.686448	17.254541
36.462567	1434.111291	17.259559
36.118716	1444.604334	17.264576
36.123838	1439.105341	17.269594
36.251589	1450.801510	17.274611
36.630542	1446.138112	17.279629
36.446873	1458.039269	17.284647
36.460894	1462.318808	17.289664
36.583201	1459.638176	17.294682
36.531407	1461.660673	17.299699
36.868909	1456.704349	17.304717
36.770291	1463.388073	17.309735
37.047667	1478.786131	17.314752
37.205044	1479.057249	17.319770
37.184561	1468.693662	17.324787
37.035364	1460.867351	17.329805
37.147281	1460.864345	17.334823
36.880396	1470.421681	17.339840
37.443341	1478.258642	17.344858
36.909404	1486.121843	17.349875
37.271114	1481.136950	17.354893
37.497308	1479.118489	17.359911
37.508838	1482.073924	17.364928
37.839286	1469.962998	17.369946
37.553606	1451.907932	17.374963
37.416073	1443.935914	17.379981
37.726313	1450.651512	17.384999
37.712401	1446.585048	17.390016
37.807706	1443.388526	17.395034
37.640308	1451.668045	17.400051
37.660027	1442.215781	17.405069
37.493088	1441.194344	17.410087
37.437746	1441.582647	17.415104
37.635646	1434.629997	17.420122
37.228612	1441.425257	17.425139
37.549644	1445.809256	17.430157
37.758729	1455.691314	17.435175
37.712736	1476.649667	17.440192
37.939188	1472.010045	17.445210
38.320740	1477.755461	17.450227
38.265701	1470.671736	17.455245
38.208877	1461.513713	17.460263
37.606042	1456.170922	17.465280
37.859760	1450.054051	17.470298
37.865210	1461.266425	17.475315
38.130080	1468.527261	17.480333
38.128598	1471.121898	17.485351
38.068715	1476.794166	17.490368
38.373902	1470.772409	17.495386
38.325684	1479.166955	17.500403
38.331957	1472.560165	17.505421
38.253005	1469.841196	17.510439
38.048995	1470.174273	17.515456
38.312546	1462.863077	17.520474
38.429004	1472.233418	17.525491
38.295250	1474.150273	17.530509
38.303718	1471.547429	17.535527
38.214078	1479.604162	17.540544
38.349154	1470.644751	17.545562
38.582889	1486.202282	17.550579
38.396193	1499.499794	17.555597
39.307305	1496.404359	17.560615
39.213139	1491.877581	17.565632
39.079083	1479.274973	17.570650
38.874811	1460.881497	17.575667
38.739262	1468.705522	17.580685
38.515805	1468.865538	17.585703
38.396504	1466.731889	17.590720
38.818100	1485.739828	17.595738
38.641801	1497.624002	17.600755
38.698148	1497.050546	17.605773
38.968705	1488.685278	17.610791
39.040075	1498.173612	17.615808
39.113983	1496.804942	17.620826
38.991658	1503.074597	17.625843
38.873340	1501.999145	17.630861
39.297395	1496.252304	17.635879
39.027044	1499.263551	17.640896
39.286173	1493.874547	17.645914
39.128606	1494.585920	17.650931
39.010817	1502.906178	17.655949
39.278545	1520.181706	17.660967
39.196499	1526.610622	17.665984
39.655279	1520.832224	17.671002
39.617187	1524.401747	17.676019
39.509130	1524.350227	17.681037
39.704780	1521.767650	17.686055
39.579988	1527.313650	17.691072
39.940869	1523.592397	17.696090
40.162330	1524.926256	17.701107
40.109007	1518.110352	17.706125
39.833075	1503.443654	17.711143
39.813528	1504.090021	17.716160
39.932201	1485.566730	17.721178
39.772294	1492.372796	17.726195
39.803593	1484.814374	17.731213
40.135524	1486.715961	17.736231
39.782078	1486.242296	17.741248
39.972638	1501.251285	17.746266
40.339950	1508.183129	17.751283
40.190427	1508.178486	17.756301
39.823065	1503.293781	17.761319
40.130611	1517.284205	17.766336
40.376908	1514.450403	17.771354
40.246415	1521.622735	17.776371
40.382126	1521.262859	17.781389
40.130635	1512.268116	17.786407
40.091732	1512.922921	17.791424
40.158443	1515.448781	17.796442
40.346764	1520.465457	17.801459
40.131848	1515.329785	17.806477
40.189227	1512.237005	17.811495
40.255152	1506.073168	17.816512
40.316453	1511.377393	17.821530
40.640001	1527.575931	17.826547
40.465663	1540.629210	17.831565
41.009837	1532.309142	17.836583
40.954831	1536.966715	17.841600
41.081887	1528.369705	17.846618
41.031520	1516.435857	17.851635
40.942418	1512.522439	17.856653
40.782313	1502.735185	17.861671
40.762229	1514.710711	17.866688
40.945748	1519.356519	17.871706
40.901504	1532.247315	17.876723
40.993960	1530.819945	17.881741
41.407010	1532.832051	17.886759
41.370220	1541.757008	17.891776
41.470516	1530.045768	17.896794
41.332929	1519.920357	17.901811
41.145231	1510.511882	17.906829
41.659695	1501.000350	17.911847
41.093732	1504.465865	17.916864
41.236828	1491.325917	17.921882
41.335891	1500.921720	17.926899
41.099926	1510.467479	17.931917
41.438261	1516.691626	17.936935
41.404846	1532.295401	17.941952
41.364151	1535.345635	17.946970
41.283256	1539.072908	17.951987
41.426763	1538.375047	17.957005
41.298604	1540.416947	17.962023
41.170013	1542.156922	17.967040
41.185390	1538.009422	17.972058
41.199354	1557.036150	17.977075
41.314156	1565.732747	17.982093
41.374279	1569.635476	17.987111
41.810910	1571.293115	17.992128
41.987311	1560.911855	17.997146
42.033927	1560.423145	18.002163
41.993774	1563.927275	18.007181
42.303030	1563.222257	18.012199
42.397673	1568.363288	18.017216
42.394415	1569.505735	18.022234
42.457074	1560.325594	18.027251
42.097560	1566.487893	18.032269
42.041189	1558.551907	18.037287
42.153479	1558.943760	18.042304
42.295889	1557.998029	18.047322
42.523246	1556.457361	18.052339
42.397329	1563.069029	18.057357
42.614468	1556.932795	18.062375
42.469625	1557.480949	18.067392
42.505858	1559.339532	18.072410
42.489920	1556.428623	18.077427
42.267260	1559.836077	18.082445
42.766144	1559.595055	18.087463
42.985516	1563.142493	18.092480
42.696314	1553.915190	18.097498
42.697152	1556.500781	18.102515
42.397803	1564.241508	18.107533
42.662476	1553.965209	18.112551
42.677184	1572.184661	18.117568
42.788321	1580.698017	18.122586
43.176169	1580.107490	18.127603
42.966593	1596.832983	18.132621
43.001002	1589.662994	18.137639
43.193029	1590.345145	18.142656
42.824201	1594.045411	18.147674
43.314406	1585.923171	18.152691
43.105423	1587.726940	18.157709
43.248598	1588.173347	18.162727
43.555198	1587.671954	18.167744
43.427552	1580.648664	18.172762
43.695205	1581.156808	18.177779
43.612262	1593.403435	18.182797
43.579263	1572.363656	18.187815
43.525551	1565.178468	18.192832
43.203673	1575.502067	18.197850
43.246468	1567.418352	18.202867
43.004123	1578.341371	18.207885
43.326647	1574.746380	18.212903
43.279527	1584.661816	18.217920
42.957688	1587.597648	18.222938
43.135296	1589.731240	18.227955
43.661187	1612.312375	18.232973
43.908762	1608.186075	18.237991
43.875495	1611.135827	18.243008
43.812743	1613.185422	18.248026
44.006588	1610.159393	18.253043
43.931966	1611.390858	18.258061
44.206562	1597.875088	18.263079
44.098834	1611.343428	18.268096
44.093608	1612.599613	18.273114
44.287861	1607.042541	18.278131
44.243518	1614.981329	18.283149
44.397097	1611.456245	18.288167
44.473589	1601.395663	18.293184
44.090397	1610.920657	18.298202
44.092461	1611.647191	18.303219
44.354881	1605.745719	18.308237
44.170285	1607.566178	18.313255
44.529016	1607.755526	18.318272
44.097194	1611.925306	18.323290
44.580309	1609.771432	18.328307
44.538299	1631.703428	18.333325
44.473354	1632.615091	18.338343
44.675400	1632.460398	18.343360
44.456566	1634.846632	18.348378
44.745836	1636.705153	18.353395
44.726388	1641.343273	18.358413
44.568926	1633.919909	18.363431
44.709756	1638.556929	18.368448
44.806044	1636.745781	18.373466
44.939093	1638.831895	18.378483
44.760562	1645.166367	18.383501
44.683696	1637.687446	18.388519
44.824094	1650.947513	18.393536
45.132159	1660.022489	18.398554
45.036088	1655.509771	18.403571
45.098132	1660.010684	18.408589
45.733136	1661.010633	18.413607
45.296954	1659.034446	18.418624
45.299611	1663.643584	18.423642
45.623863	1656.799502	18.428659
45.637110	1654.925021	18.433677
45.596553	1659.038756	18.438695
45.873257	1654.125476	18.443712
45.794853	1656.306907	18.448730
45.877886	1650.996078	18.453747
45.953443	1654.462277	18.458765
45.876742	1638.128441	18.463783
45.874939	1624.318268	18.468800
45.603461	1626.791093	18.473818
46.146375	1619.448859	18.478835
45.853907	1622.811596	18.483853
45.948016	1621.115008	18.488871
45.822113	1611.765963	18.493888
45.762113	1626.855438	18.498906
45.928033	1647.338270	18.503923
46.048476	1646.855012	18.508941
45.959788	1646.451708	18.513959
46.117438	1656.838830	18.518976
45.689735	1660.818132	18.523994
45.821102	1654.617817	18.529011
45.920372	1646.377906	18.534029
45.740299	1656.639446	18.539047
46.017187	1670.887655	18.544064
46.292232	1683.149361	18.549082
46.178933	1685.615550	18.554099
46.401635	1685.400616	18.559117
46.327505	1681.741703	18.564135
46.491569	1685.916436	18.569152
46.313524	1680.357807	18.574170
46.827403	1694.383496	18.579187
46.567545	1699.963738	18.584205
46.683903	1710.131572	18.589223
46.926149	1704.525681	18.594240
47.065595	1710.627296	18.599258
46.970666	1714.898021	18.604275
47.262728	1709.982878	18.609293
46.708539	1708.329314	18.614311
47.177766	1711.611876	18.619328
47.032039	1712.219249	18.624346
47.361525	1704.143404	18.629363
47.422617	1706.582059	18.634381
47.216457	1707.925464	18.639399
47.808763	1703.517176	18.644416
47.733032	1706.746698	18.649434
46.869445	1677.342334	18.654451
46.986335	1677.462506	18.659469
47.398863	1696.859308	18.664487
47.618686	1700.370870	18.669504
47.648424	1711.434361	18.674522
47.402793	1705.017529	18.679539
47.326510	1701.751937	18.684557
47.357603	1713.312497	18.689575
47.548182	1703.448061	18.694592
47.264530	1714.482205	18.699610
47.724728	1701.808638	18.704627
47.399694	1704.154421	18.709645
47.708315	1725.461410	18.714663
48.016113	1725.707530	18.719680
48.053303	1735.679087	18.724698
48.311485	1725.372290	18.729715
48.399255	1719.578287	18.734733
48.296485	1727.443283	18.739751
48.447546	1717.540726	18.744768
48.090103	1697.599828	18.749786
48.164115	1697.990372	18.754803
48.170650	1695.767786	18.759821
48.086725	1715.554486	18.764839
48.234547	1716.615130	18.769856
48.069540	1722.848878	18.774874
48.789702	1717.539826	18.779891
48.428441	1720.273756	18.784909
48.154002	1723.083362	18.789927
48.777510	1714.748810	18.794944
48.551419	1706.450465	18.799962
48.466693	1707.691545	18.804979
48.665646	1713.186041	18.809997
48.474422	1723.448355	18.815015
48.722436	1711.656529	18.820032
48.870498	1728.925244	18.825050
49.094297	1735.977476	18.830067
49.198364	1740.868102	18.835085
49.344375	1732.561857	18.840103
49.368059	1711.686602	18.845120
49.085529	1716.554122	18.850138
48.917005	1710.268965	18.855155
48.894386	1720.985889	18.860173
48.971223	1732.714624	18.865191
49.345520	1727.820026	18.870208
49.286784	1735.892854	18.875226
49.079415	1732.052420	18.880243
49.428278	1734.779969	18.885261
49.021808	1733.664524	18.890279
49.327284	1733.288925	18.895296
49.299917	1740.364534	18.900314
49.413757	1746.701681	18.905331
49.713372	1755.208019	18.910349
49.594117	1763.508191	18.915367
49.798334	1756.887425	18.920384
49.777184	1760.916748	18.925402
49.878106	1761.011702	18.930419
50.169395	1769.067848	18.935437
49.881456	1761.095862	18.940455
50.210651	1759.204605	18.945472
50.253037	1763.535670	18.950490
49.954674	1759.563962	18.955507
50.095306	1762.915867	18.960525
49.879348	1764.757470	18.965543
49.991650	1768.006741	18.970560
50.283106	1771.029604	18.975578
50.138750	1767.962306	18.980595
50.128925	1766.625293	18.985613
50.203252	1768.772286	18.990631
50.726796	1771.996332	18.995648
50.729341	1782.831832	19.000666
50.525548	1767.833581	19.005683
51.032240	1760.260851	19.010701
50.710255	1770.088869	19.015719
50.620994	1764.494119	19.020736
50.756073	1760.643789	19.025754
50.503091	1765.675569	19.030771
50.774953	1770.660285	19.035789
50.973828	1796.037834	19.040807
51.375134	1791.977660	19.045824
50.906546	1778.843513	19.050842
50.974693	1765.814621	19.055859
51.179419	1777.227729	19.060877
51.247064	1778.663976	19.065895
51.176244	1770.306688	19.070912
51.255790	1776.656421	19.075930
51.247966	1788.223315	19.080947
51.386518	1782.935210	19.085965
51.280274	1791.598563	19.090983
51.528320	1790.282305	19.096000
51.743943	1792.835441	19.101018
51.258906	1788.687833	19.106035
51.233868	1785.540224	19.111053
51.280264	1793.675382	19.116071
51.230336	1785.533821	19.121088
51.332176	1790.931990	19.126106
51.277938	1790.277865	19.131123
51.903238	1797.729059	19.136141
51.634405	1806.060018	19.141159
51.738457	1809.063439	19.146176
51.835407	1814.542779	19.151194
52.036628	1816.607386	19.156211
52.235889	1809.532669	19.161229
51.908898	1813.554985	19.166247
52.076312	1813.937788	19.171264
52.552293	1809.878194	19.176282
52.432524	1816.722799	19.181299
52.603159	1803.621574	19.186317
52.111660	1807.349221	19.191335
52.309762	1806.172248	19.196352
52.453732	1804.150520	19.201370
52.161511	1807.758952	19.206387
52.557660	1804.823806	19.211405
52.319946	1811.577201	19.216423
52.298862	1819.330588	19.221440
52.785476	1824.020992	19.226458
52.407721	1839.622291	19.231475
52.621047	1830.678001	19.236493
52.607006	1840.827721	19.241511
52.694404	1840.699771	19.246528
53.105658	1837.508850	19.251546
52.801999	1844.741337	19.256563
52.854263	1835.061969	19.261581
52.839600	1844.879081	19.266599
53.264707	1856.075308	19.271616
53.513052	1854.309726	19.276634
53.139875	1851.815958	19.281651
53.099297	1851.179176	19.286669
52.979636	1867.104014	19.291687
53.106631	1874.867084	19.296704
53.101046	1867.104540	19.301722
53.256816	1875.251307	19.306739
53.775089	1868.949135	19.311757
53.336017	1868.132612	19.316775
53.136216	1870.028157	19.321792
53.598637	1870.902968	19.326810
53.456903	1890.310776	19.331827
53.733083	1891.310444	19.336845
54.207231	1902.465221	19.341863
53.868584	1893.227294	19.346880
54.212208	1899.765295	19.351898
54.001674	1889.874224	19.356915
54.124963	1885.406912	19.361933
54.067956	1897.869042	19.366951
54.115256	1898.579564	19.371968
54.411902	1885.782690	19.376986
54.229861	1893.594816	19.382003
54.644043	1895.532753	19.387021
54.629257	1894.062312	19.392039
54.226897	1900.404942	19.397056
54.387079	1884.658265	19.402074
54.412177	1892.236821	19.407091
54.511991	1884.135292	19.412109
55.088268	1893.854269	19.417127
55.188373	1891.687669	19.422144
54.738808	1884.773377	19.427162
54.603138	1888.936554	19.432179
54.972548	1887.002557	19.437197
54.479277	1888.943300	19.442215
54.671449	1885.281207	19.447232
54.841728	1882.921059	19.452250
54.760849	1890.440215	19.457267
55.102833	1884.484836	19.462285
54.809709	1885.310817	19.467303
54.955715	1907.935069	19.472320
55.458325	1903.700392	19.477338
55.257745	1909.640276	19.482355
55.615420	1908.916706	19.487373
55.166654	1912.263776	19.492391
55.371901	1904.728878	19.497408
55.761604	1908.066069	19.502426
55.276256	1911.063854	19.507443
55.582769	1906.904141	19.512461
56.075058	1909.066907	19.517479
55.951853	1910.277587	19.522496
56.229609	1911.445905	19.527514
55.765240	1908.471638	19.532531
55.666171	1897.655040	19.537549
55.443525	1901.970945	19.542567
55.828356	1901.534094	19.547584
56.005577	1895.350235	19.552602
55.651074	1898.657122	19.557619
56.289214	1893.373101	19.562637
56.244842	1901.989683	19.567655
55.945165	1907.323644	19.572672
56.205964	1915.060644	19.577690
56.248419	1937.455025	19.582707
56.601554	1932.457286	19.587725
56.721686	1927.356171	19.592743
56.284302	1928.434080	19.597760
56.453344	1925.719369	19.602778
56.283776	1928.333843	19.607795
56.768394	1924.911402	19.612813
56.870343	1923.139413	19.617831
56.417265	1926.002125	19.622848
56.465147	1922.008418	19.627866
56.403850	1919.934455	19.632883
56.285007	1932.384770	19.637901
56.556771	1943.587269	19.642919
56.811397	1960.997439	19.647936
56.990748	1955.093542	19.652954
56.546531	1962.060381	19.657971
57.260004	1949.730248	19.662989
56.872439	1959.143983	19.668007
57.182296	1980.518834	19.673024
57.240672	1984.210522	19.678042
57.108974	1992.869688	19.683059
57.532866	1985.207097	19.688077
57.911007	1977.065676	19.693095
57.867491	1984.066988	19.698112
58.308979	1972.056733	19.703130
57.809712	1979.878796	19.708147
58.014342	1979.976840	19.713165
58.072842	1971.368897	19.718183
57.930193	1976.223146	19.723200
58.234385	1968.256634	19.728218
57.878124	1963.702991	19.733235
58.189560	1974.400615	19.738253
58.405204	1971.835801	19.743271
58.334548	1962.905867	19.748288
58.398906	1947.016087	19.753306
58.366593	1946.283777	19.758323
58.077847	1940.468802	19.763341
58.894826	1955.222388	19.768359
58.114275	1962.465029	19.773376
58.495218	1963.466034	19.778394
58.856576	1969.601367	19.783411
58.624725	1977.020448	19.788429
58.378179	1973.878097	19.793447
58.078820	1976.493569	19.798464
58.345083	1970.538540	19.803482
58.310895	1974.241765	19.808499
58.478952	1973.021106	19.813517
58.668305	1990.212943	19.818535
58.959651	2003.941983	19.823552
59.087403	2002.916840	19.828570
58.705210	2002.909561	19.833587
59.081341	1999.411991	19.838605
59.154339	1992.104476	19.843623
59.022471	2008.350489	19.848640
59.518749	1998.429125	19.853658
59.138985	1995.378516	19.858675
59.075383	1991.696069	19.863693
59.359298	1992.781436	19.868711
59.197615	2013.405967	19.873728
59.721896	2011.733630	19.878746
59.803355	2026.665755	19.883763
59.862881	2031.483390	19.888781
59.782791	2023.779216	19.893799
59.650067	2026.661442	19.898816
59.886545	2017.391774	19.903834
60.005827	2029.519021	19.908851
60.216966	2024.859419	19.913869
60.268874	2015.403651	19.918887
59.789421	2028.892768	19.923904
60.050242	2018.756608	19.928922
60.292779	2020.707453	19.933939
59.953794	2024.392464	19.938957
59.983486	2021.187386	19.943975
60.023594	2022.598058	19.948992
59.942202	2017.503902	19.954010
60.165642	2039.783137	19.959027
60.356007	2049.706190	19.964045
60.345835	2041.882526	19.969063
60.360001	2044.990391	19.974080
60.864882	2038.613273	19.979098
60.863464	2042.703861	19.984115
60.882312	2045.729023	19.989133
61.096540	2043.403054	19.994151
60.893445	2039.438171	19.999168
61.127709	2046.913610	20.004186
61.193663	2040.399117	20.009203
60.858310	2040.173938	20.014221
61.110520	2050.735293	20.019239
61.120837	2067.962242	20.024256
61.507500	2063.176853	20.029274
61.400053	2069.511121	20.034291
61.705368	2076.106559	20.039309
61.650686	2076.438064	20.044327
61.594057	2080.357001	20.049344
61.709325	2066.056618	20.054362
62.016840	2060.396886	20.059379
61.558184	2062.767205	20.064397
62.035107	2064.970429	20.069415
61.689995	2064.548470	20.074432
61.942620	2065.241123	20.079450
61.532939	2065.756736	20.084467
61.803749	2063.119448	20.089485
62.008072	2062.415470	20.094503
61.809681	2069.809564	20.099520
62.268829	2066.117014	20.104538
62.215208	2064.522094	20.109555
61.857079	2068.523038	20.114573
62.121032	2081.693381	20.119591
62.274006	2089.309566	20.124608
62.100554	2089.831929	20.129626
62.358888	2093.031819	20.134643
61.975121	2100.179325	20.139661
62.417248	2099.009714	20.144679
62.632120	2112.602727	20.149696
63.183223	2120.666488	20.154714
62.620976	2122.854549	20.159731
62.873858	2125.710057	20.164749
63.347262	2116.358367	20.169767
62.951918	2115.863905	20.174784
63.087887	2108.448676	20.179802
63.671983	2110.509894	20.184819
63.588967	2110.104817	20.189837
63.522300	2093.533318	20.194855
63.167398	2084.671342	20.199872
63.395577	2092.128946	20.204890
63.521349	2102.393466	20.209907
63.449767	2106.020050	20.214925
63.682901	2099.275269	20.219943
63.647496	2108.645254	20.224960
63.585460	2110.237642	20.229978
63.621266	2100.319953	20.234995
63.527141	2104.314625	20.240013
63.529293	2100.446839	20.245031
63.444644	2109.527589	20.250048
63.515117	2104.454619	20.255066
63.799808	2111.070933	20.260083
64.063831	2138.483425	20.265101
64.033593	2135.243318	20.270119
64.341470	2147.209564	20.275136
64.040125	2142.617708	20.280154
64.609713	2132.243080	20.285171
64.463855	2124.100070	20.290189
64.894664	2121.922417	20.295207
64.912620	2131.081664	20.300224
64.759465	2126.664435	20.305242
64.992655	2123.345303	20.310259
64.941792	2124.262455	20.315277
65.201923	2121.239140	20.320295
65.182760	2117.475412	20.325312
65.011342	2120.967915	20.330330
65.160104	2115.525958	20.335347
65.000840	2117.815424	20.340365
65.095020	2117.940280	20.345383
64.781882	2112.728323	20.350400
64.851144	2110.129520	20.355418
65.453849	2107.909403	20.360435
65.354368	2114.599853	20.365453
65.675272	2104.917967	20.370471
65.544379	2111.392510	20.375488
65.793695	2116.470586	20.380506
65.579676	2109.606767	20.385523
65.663650	2117.547042	20.390541
65.639471	2110.544361	20.395559
66.137104	2117.404918	20.400576
66.121831	2116.669679	20.405594
66.167995	2106.995914	20.410611
65.750921	2113.597879	20.415629
65.952983	2115.052457	20.420647
65.982555	2115.854230	20.425664
65.995642	2116.136317	20.430682
66.378690	2115.569040	20.435699
65.857042	2125.392923	20.440717
66.516902	2132.838356	20.445735
66.563481	2143.890211	20.450752
66.475976	2148.051892	20.455770
66.426835	2139.348516	20.460787
66.130675	2149.844877	20.465805
66.595802	2147.628261	20.470823
66.411965	2145.393361	20.475840
66.700397	2141.566654	20.480858
66.424891	2149.455176	20.485875
66.209714	2153.906501	20.490893
66.608441	2156.039669	20.495911
66.736498	2165.396626	20.500928
66.353294	2160.520333	20.505946
66.801313	2174.028934	20.510963
66.758989	2192.925123	20.515981
67.130358	2193.800996	20.520999
66.989756	2192.991164	20.526016
67.167141	2200.282306	20.531034
67.507501	2205.749978	20.536051
67.328123	2212.057260	20.541069
67.584317	2222.017175	20.546087
67.431108	2227.877393	20.551104
67.373099	2222.729154	20.556122
67.585663	2224.529235	20.561139
67.512090	2225.430993	20.566157
67.665634	2240.158810	20.571175
68.053082	2246.956413	20.576192
68.447998	2250.407368	20.581210
68.491258	2236.208953	20.586227
68.717438	2242.879850	20.591245
68.924705	2227.846907	20.596263
68.539192	2214.987559	20.601280
68.242468	2207.846101	20.606298
68.855345	2195.969308	20.611315
68.449954	2202.072780	20.616333
68.859058	2200.284325	20.621351
68.635802	2193.704376	20.626368
68.462992	2209.181128	20.631386
68.760945	2212.927479	20.636403
69.348653	2232.494158	20.641421
69.500137	2230.266333	20.646439
69.074589	2216.865736	20.651456
68.811403	2208.948338	20.656474
69.150966	2220.092556	20.661491
68.890902	2225.294618	20.666509
68.716091	2230.735645	20.671527
69.160597	2233.956803	20.676544
68.762417	2234.233800	20.681562
69.115188	2231.420205	20.686579
69.167557	2245.812567	20.691597
69.013920	2254.552027	20.696615
69.470435	2259.021708	20.701632
69.423638	2259.833825	20.706650
69.589513	2258.112265	20.711667
69.351662	2266.313334	20.716685
69.795823	2279.940816	20.721703
70.190638	2284.826654	20.726720
70.159045	2288.418468	20.731738
70.496277	2281.743176	20.736755
69.840406	2287.095806	20.741773
70.047989	2295.490641	20.746791
70.307653	2287.131543	20.751808
70.121615	2297.149212	20.756826
70.529800	2281.460420	20.761843
70.289030	2281.332421	20.766861
70.263421	2286.058810	20.771879
70.977405	2294.078592	20.776896
70.441231	2316.008461	20.781914
70.967091	2312.314655	20.786931
71.409455	2313.372094	20.791949
71.543112	2310.107001	20.796967
71.506243	2294.600025	20.801984
71.077134	2283.400309	20.807002
71.404661	2277.724468	20.812019
71.276826	2279.560077	20.817037
71.013124	2281.025222	20.822055
71.379287	2279.922961	20.827072
71.312562	2308.058302	20.832090
71.682743	2300.229938	20.837107
71.582206	2308.197219	20.842125
71.394238	2307.113570	20.847143
71.510173	2306.793688	20.852160
71.348604	2316.709522	20.857178
71.504438	2300.879695	20.862195
71.493140	2320.258585	20.867213
71.390692	2327.934034	20.872231
71.965673	2332.692922	20.877248
71.777859	2341.255585	20.882266
72.156869	2335.351966	20.887283
71.829109	2336.656419	20.892301
71.890810	2352.848339	20.897319
72.109498	2362.910852	20.902336
71.800113	2366.973996	20.907354
72.256304	2367.165944	20.912371
72.457910	2377.291247	20.917389
72.452905	2390.003554	20.922407
72.691811	2396.846377	20.927424
72.898889	2406.012344	20.932442
72.919918	2395.535498	20.937459
73.743887	2382.917541	20.942477
73.576723	2367.838405	20.947495
74.191326	2353.056817	20.952512
73.597569	2350.337750	20.957530
73.877473	2347.020801	20.962547
73.851159	2341.976554	20.967565
73.586039	2329.965893	20.972583
74.020224	2316.650919	20.977600
73.837649	2312.491081	20.982618
73.793894	2318.892494	20.987635
73.696317	2318.546216	20.992653
73.503841	2314.725920	20.997671
73.846012	2313.964829	21.002688
73.667631	2314.606566	21.007706
73.812487	2320.193636	21.012723
74.073064	2331.497955	21.017741
74.040338	2344.774117	21.022759
74.654867	2340.627242	21.027776
74.083836	2348.416112	21.032794
73.937634	2348.114396	21.037811
73.993816	2348.125278	21.042829
73.840825	2351.097665	21.047847
73.963369	2344.273299	21.052864
74.346905	2361.163709	21.057882
74.177372	2374.536591	21.062899
74.490257	2376.072996	21.067917
74.054609	2378.593770	21.072935
74.217431	2389.473877	21.077952
74.491571	2403.815762	21.082970
74.715776	2405.524092	21.087987
74.810701	2403.891070	21.093005
74.675481	2412.129745	21.098023
75.512719	2414.162963	21.103040
75.423928	2428.872653	21.108058
75.519790	2436.978009	21.113075
75.202755	2435.090364	21.118093
75.228601	2435.485247	21.123111
75.691066	2425.865917	21.128128
75.934327	2430.261169	21.133146
75.811950	2426.369763	21.138163
75.687048	2428.537223	21.143181
75.848613	2430.487039	21.148199
75.967439	2432.804870	21.153216
76.039282	2432.676038	21.158234
75.804887	2428.295883	21.163251
76.237876	2422.538908	21.168269
75.960512	2430.987031	21.173287
76.052398	2440.016837	21.178304
76.490247	2456.222341	21.183322
76.488311	2455.042210	21.188339
76.685081	2447.003308	21.193357
76.452268	2457.436249	21.198375
76.471756	2449.933332	21.203392
76.428685	2448.920909	21.208410
76.491559	2460.150536	21.213427
76.873126	2456.127837	21.218445
76.923023	2475.862628	21.223463
77.087825	2475.141389	21.228480
76.966824	2485.421299	21.233498
77.454093	2481.260767	21.238515
77.259789	2476.696531	21.243533
77.433226	2481.061241	21.248551
77.571747	2475.215339	21.253568
77.497807	2476.984242	21.258586
77.228127	2480.800412	21.263603
77.586097	2476.512418	21.268621
77.350063	2482.898823	21.273639
77.391186	2480.866290	21.278656
77.471480	2493.435690	21.283674
77.267750	2508.891262	21.288691
77.497556	2505.623821	21.293709
77.528086	2517.090567	21.298727
77.668030	2525.983816	21.303744
78.023584	2536.514396	21.308762
78.111940	2546.749790	21.313779
78.373876	2542.935011	21.318797
78.254198	2548.659657	21.323815
78.238507	2538.037017	21.328832
78.861663	2554.949558	21.333850
78.759183	2551.509116	21.338867
79.026170	2545.462394	21.343885
78.642002	2548.698109	21.348903
79.242565	2557.129666	21.353920
79.178369	2561.668232	21.358938
79.217953	2564.517076	21.363955
79.181977	2563.592421	21.368973
79.089424	2571.886867	21.373991
79.104530	2560.822639	21.379008
79.264243	2565.902442	21.384026
79.471438	2560.879519	21.389043
79.195069	2558.885657	21.394061
79.025302	2563.043832	21.399079
79.504737	2576.817521	21.404096
79.568537	2586.965798	21.409114
79.592488	2594.694522	21.414131
79.733339	2585.320029	21.419149
79.989104	2592.772750	21.424167
79.765622	2586.830575	21.429184
79.895786	2599.387572	21.434202
79.763523	2615.571278	21.439219
79.999344	2614.671687	21.444237
80.130251	2620.047047	21.449255
80.819708	2619.710737	21.454272
80.891094	2614.858349	21.459290
80.873624	2616.812895	21.464307
81.143087	2612.439234	21.469325
80.896637	2618.343146	21.474343
81.030002	2612.982411	21.479360
80.600159	2616.244084	21.484378
80.642601	2617.632359	21.489395
81.045959	2608.657017	21.494413
80.714480	2624.176343	21.499431
80.765236	2631.138155	21.504448
80.975773	2637.948147	21.509466
80.967409	2654.794233	21.514483
81.255747	2647.642047	21.519501
81.280424	2647.896956	21.524519
81.406533	2657.673904	21.529536
81.548075	2664.150008	21.534554
81.506451	2674.968496	21.539571
81.809400	2673.730566	21.544589
81.921271	2670.654205	21.549607
83.124723	2641.608328	21.554624
83.354339	2638.959895	21.559642
82.978646	2629.658970	21.564659
83.263174	2619.995212	21.569677
83.044311	2617.249626	21.574695
83.253230	2611.533360	21.579712
83.121504	2593.749051	21.584730
82.774885	2586.616759	21.589747
83.170972	2565.078389	21.594765
82.600737	2571.935580	21.599783
82.628175	2575.975683	21.604800
82.790258	2573.325451	21.609818
82.955975	2577.601733	21.614835
83.055682	2591.362571	21.619853
83.222611	2605.597018	21.624871
83.355985	2599.906309	21.629888
83.539038	2603.098342	21.634906
83.163834	2611.862599	21.639923
83.261206	2610.354354	21.644941
82.881712	2617.968762	21.649959
83.086160	2611.058573	21.654976
83.471861	2622.787395	21.659994
83.452283	2636.542734	21.665011
83.499810	2642.979032	21.670029
83.496038	2637.248819	21.675047
83.418595	2651.653571	21.680064
83.391900	2657.065414	21.685082
84.000844	2671.314707	21.690099
84.031137	2668.479143	21.695117
84.247396	2669.813997	21.700135
84.644448	2689.532855	21.705152
85.045997	2678.849613	21.710170
84.579046	2669.465080	21.715187
84.865695	2658.824389	21.720205
84.842022	2665.713923	21.725223
84.674294	2675.062437	21.730240
84.847498	2682.022968	21.735258
84.762142	2681.321769	21.740275
85.023174	2682.398511	21.745293
84.781906	2683.311718	21.750311
84.924730	2683.387289	21.755328
85.276171	2686.466204	21.760346
85.249491	2700.144063	21.765363
85.103258	2700.510964	21.770381
85.318112	2717.045572	21.775399
85.590814	2713.832162	21.780416
85.687839	2716.676699	21.785434
85.669442	2724.178848	21.790451
85.955049	2714.164393	21.795469
86.074802	2722.420158	21.800487
85.641802	2720.244430	21.805504
86.026255	2724.629735	21.810522
85.837862	2734.364570	21.815539
86.139637	2749.580931	21.820557
85.973198	2747.091736	21.825575
85.958706	2745.808205	21.830592
86.410372	2757.058807	21.835610
86.460576	2774.742376	21.840627
86.816099	2775.785599	21.845645
86.844095	2771.649390	21.850663
86.504117	2781.222020	21.855680
86.850851	2771.993254	21.860698
86.957726	2780.634791	21.865715
86.747258	2767.392157	21.870733
86.908567	2786.640438	21.875751
87.142082	2791.801381	21.880768
87.394413	2787.897622	21.885786
87.279794	2806.667943	21.890803
87.470779	2800.397890	21.895821
87.290834	2801.157257	21.900839
87.588815	2816.068766	21.905856
87.632848	2823.975296	21.910874
87.746176	2833.679729	21.915891
88.096910	2819.987229	21.920909
87.719595	2830.660190	21.925927
87.851733	2823.340968	21.930944
88.522264	2825.906855	21.935962
88.652476	2847.646036	21.940979
88.427362	2845.752818	21.945997
89.059359	2847.734656	21.951015
88.561879	2839.959485	21.956032
88.668866	2835.682922	21.961050
88.992347	2844.797689	21.966067
88.920345	2852.868247	21.971085
89.252911	2848.855426	21.976103
89.136725	2851.508152	21.981120
89.411981	2848.258837	21.986138
89.113707	2850.422213	21.991155
89.152507	2845.537538	21.996173
89.291421	2840.066306	22.001191
89.402516	2848.055856	22.006208
89.870219	2841.716295	22.011226
89.450695	2848.754891	22.016243
89.490772	2845.441153	22.021261
89.902510	2862.055567	22.026279
90.014302	2871.538986	22.031296
90.188354	2869.891564	22.036314
90.180387	2885.817187	22.041331
90.198337	2884.472167	22.046349
90.450263	2882.464083	22.051367
90.228382	2883.000680	22.056384
90.438800	2881.401362	22.061402
90.167254	2881.318798	22.066419
90.169215	2879.652837	22.071437
90.614802	2879.729269	22.076455
90.721199	2880.811272	22.081472
90.489683	2877.775628	22.086490
90.907901	2893.499823	22.091507
90.660203	2908.286821	22.096525
91.321496	2895.539626	22.101543
91.580014	2890.560565	22.106560
92.182652	2883.168529	22.111578
92.364494	2875.140632	22.116595
92.050133	2856.720281	22.121613
91.626317	2845.388519	22.126631
91.998244	2835.301697	22.131648
91.900296	2832.951954	22.136666
91.744100	2841.711080	22.141683
91.554347	2834.370646	22.146701
91.882271	2836.761371	22.151719
91.627841	2854.095608	22.156736
92.112971	2861.846993	22.161754
91.797653	2866.874451	22.166771
92.250771	2869.255531	22.171789
92.568233	2861.040580	22.176807
92.397104	2870.747338	22.181824
92.397697	2887.093621	22.186842
92.936690	2894.208112	22.191859
93.047353	2898.074157	22.196877
93.440910	2898.254803	22.201895
93.090728	2910.516378	22.206912
93.241558	2901.340811	22.211930
93.365945	2906.409456	22.216947
92.999015	2893.040754	22.221965
93.314020	2895.244691	22.226983
93.031169	2902.720597	22.232000
93.130515	2897.591624	22.237018
93.478832	2905.749235	22.242035
93.233558	2915.264757	22.247053
93.434232	2915.365852	22.252071
93.422577	2918.389718	22.257088
93.387025	2924.786821	22.262106
93.925578	2945.326785	22.267123
93.790469	2944.130071	22.272141
94.285347	2936.164246	22.277159
94.187615	2937.948304	22.282176
94.244872	2932.517028	22.287194
94.559590	2957.793123	22.292211
94.802477	2951.638546	22.297229
95.511912	2944.715666	22.302247
95.614757	2939.070234	22.307264
95.282054	2926.435146	22.312282
95.474223	2926.674733	22.317299
95.185218	2919.558400	22.322317
95.502858	2915.226012	22.327335
95.287084	2917.976153	22.332352
95.510779	2920.180785	22.337370
95.601007	2919.943267	22.342387
95.160010	2917.732653	22.347405
95.372696	2915.257975	22.352423
95.222349	2933.321840	22.357440
94.902797	2945.393903	22.362458
95.484328	2941.627407	22.367475
95.325423	2953.211218	22.372493
95.806698	2970.327310	22.377511
95.942817	2984.081463	22.382528
95.737826	2978.143843	22.387546
96.261913	2986.820287	22.392563
95.989238	3002.459850	22.397581
96.977149	2997.606152	22.402599
96.786020	2999.036079	22.407616
96.956916	2995.166708	22.412634
96.927972	2995.377261	22.417651
97.159231	2999.194305	22.422669
97.181411	2997.496513	22.427687
97.099034	2999.603993	22.432704
97.057422	2999.242592	22.437722
97.127850	2996.809616	22.442739
96.909251	3006.704946	22.447757
97.639687	3018.663999	22.452775
97.557984	3025.169075	22.457792
97.357291	3035.349598	22.462810
97.817260	3031.518078	22.467827
97.572560	3028.358656	22.472845
97.733156	3026.707224	22.477863
98.126547	3048.516548	22.482880
98.386793	3050.498354	22.487898
98.166605	3052.278217	22.492915
97.992838	3057.047563	22.497933
98.565610	3053.179373	22.502951
98.343803	3062.194800	22.507968
98.496333	3055.869809	22.512986
98.539635	3064.251482	22.518003
98.937951	3073.501615	22.523021
99.090215	3076.825821	22.528039
99.406013	3069.875865	22.533056
99.849424	3064.678402	22.538074
99.748389	3069.551053	22.543091
99.934392	3058.736759	22.548109
99.911941	3042.094853	22.553127
99.646961	3030.444328	22.558144
99.273847	3025.787727	22.563162
99.798169	3040.182601	22.568179
99.796722	3057.706807	22.573197
100.347792	3065.688770	22.578215
100.006247	3063.566617	22.583232
99.846714	3067.806651	22.588250
100.194388	3065.482858	22.593267
100.075493	3073.186691	22.598285
100.395492	3055.730006	22.603303
100.311308	3056.109904	22.608320
100.193951	3059.889072	22.613338
100.602281	3065.446992	22.618355
100.412052	3083.041393	22.623373
101.023940	3082.722316	22.628391
100.993671	3089.401314	22.633408
100.839645	3091.035166	22.638426
101.063630	3082.610097	22.643443
100.846417	3093.905523	22.648461
101.074971	3103.742369	22.653479
100.881861	3118.686380	22.658496
100.969045	3116.689972	22.663514
100.787993	3124.204446	22.668531
100.859605	3149.309098	22.673549
101.433533	3144.341253	22.678567
101.352294	3155.241682	22.683584
102.032241	3164.665679	22.688602
102.334165	3167.268042	22.693619
102.278944	3171.584728	22.698637
102.363062	3167.540389	22.703655
102.658512	3170.706970	22.708672
102.574904	3173.082456	22.713690
102.871480	3165.298575	22.718707
102.888433	3166.741673	22.723725
103.042130	3167.580106	22.728743
102.676655	3173.016341	22.733760
102.813200	3186.134247	22.738778
103.343054	3189.295299	22.743795
103.274054	3193.128426	22.748813
103.559437	3190.828683	22.753831
103.731633	3192.971302	22.758848
103.485524	3196.714296	22.763866
103.659943	3191.981891	22.768883
103.535236	3197.648567	22.773901
103.595897	3196.308799	22.778919
103.838408	3213.696059	22.783936
103.989215	3228.799370	22.788954
104.079834	3219.051143	22.793971
104.102718	3223.939614	22.798989
104.247149	3224.793028	22.804007
104.360818	3223.159859	22.809024
104.386738	3244.808786	22.814042
105.054256	3240.564391	22.819059
104.472456	3249.210054	22.824077
104.872726	3246.274731	22.829095
105.074501	3256.843975	22.834112
105.119722	3252.437702	22.839130
105.066573	3244.685386	22.844147
105.060592	3255.372153	22.849165
105.250017	3269.988467	22.854183
105.216592	3277.940794	22.859200
105.533405	3280.947797	22.864218
105.619069	3283.809349	22.869235
105.461371	3278.247841	22.874253
105.720862	3282.347577	22.879271
106.023583	3278.969819	22.884288
105.804958	3288.250239	22.889306
106.509019	3293.365332	22.894323
106.186285	3306.719591	22.899341
106.375589	3305.898820	22.904359
106.435430	3296.875659	22.909376
106.461562	3302.902422	22.914394
106.506612	3291.422223	22.919411
106.246084	3304.893401	22.924429
106.393409	3322.404998	22.929447
106.701214	3329.500256	22.934464
106.844786	3338.672933	22.939482
107.088748	3322.945894	22.944499
106.817020	3346.051013	22.949517
107.538453	3356.094921	22.954535
107.548725	3356.501162	22.959552
107.708997	3362.688455	22.964570
107.586210	3358.746482	22.969587
107.626780	3357.881113	22.974605
107.294674	3375.548205	22.979623
108.062407	3389.089684	22.984640
107.988079	3393.022220	22.989658
108.120781	3385.827865	22.994675
108.210939	3396.227321	22.999693
108.391542	3407.957242	23.004711
108.802642	3403.292884	23.009728
108.480992	3414.996292	23.014746
108.811753	3408.995014	23.019763
108.179375	3414.870087	23.024781
108.562233	3428.765834	23.029799
108.987734	3438.945587	23.034816
108.590566	3449.022234	23.039834
109.398505	3438.000248	23.044851
109.994273	3428.361398	23.049869
110.276196	3433.872602	23.054887
110.301515	3421.682934	23.059904
110.054630	3424.675555	23.064922
110.270628	3419.123964	23.069939
110.529695	3425.789730	23.074957
110.327026	3424.275353	23.079975
110.462767	3418.218509	23.084992
110.265173	3421.131010	23.090010
110.549070	3412.493876	23.095027
110.957627	3413.602873	23.100045
110.837996	3408.063145	23.105063
111.113443	3408.722417	23.110080
111.104088	3415.275106	23.115098
111.352846	3406.317155	23.120115
111.095482	3413.388844	23.125133
111.015989	3422.594298	23.130151
111.469994	3409.362430	23.135168
111.334620	3433.413806	23.140186
111.524327	3442.193510	23.145203
111.772994	3437.519972	23.150221
111.533126	3445.180932	23.155239
111.961762	3435.957429	23.160256
111.462929	3445.113500	23.165274
111.887505	3445.228982	23.170291
111.486615	3453.282987	23.175309
111.836484	3458.510049	23.180327
112.275512	3460.641614	23.185344
112.288773	3469.910740	23.190362
112.182947	3471.189833	23.195379
112.338221	3486.231982	23.200397
112.159211	3504.981095	23.205415
112.463296	3506.570319	23.210432
112.748263	3514.170477	23.215450
113.030967	3527.751124	23.220467
113.059300	3531.719650	23.225485
113.339959	3535.327524	23.230503
113.492038	3532.256705	23.235520
113.490599	3537.336887	23.240538
113.075443	3533.522175	23.245555
113.291718	3548.918576	23.250573
113.293972	3567.851698	23.255591
113.740623	3568.959690	23.260608
113.608993	3585.742059	23.265626
113.681403	3604.865607	23.270643
114.052597	3604.888645	23.275661
113.925552	3610.897681	23.280679
114.347863	3621.149770	23.285696
114.392644	3625.703038	23.290714
114.930529	3620.578984	23.295731
115.093323	3619.129524	23.300749
114.914672	3624.896173	23.305767
115.220423	3641.503595	23.310784
115.189082	3654.267907	23.315802
115.530952	3646.120824	23.320819
115.613175	3649.420932	23.325837
115.778436	3650.611823	23.330855
115.602933	3639.811064	23.335872
115.501065	3647.205099	23.340890
115.638209	3650.187057	23.345907
116.042441	3660.738405	23.350925
116.230210	3667.043180	23.355943
116.443070	3666.258520	23.360960
116.444629	3671.895843	23.365978
116.550797	3667.611321	23.370995
116.830140	3669.715160	23.376013
116.729759	3677.725635	23.381031
116.945886	3667.528743	23.386048
116.828058	3676.466049	23.391066
116.895547	3697.628831	23.396083
117.266544	3706.888748	23.401101
117.216664	3707.888126	23.406119
117.277535	3703.367207	23.411136
117.248370	3701.993177	23.416154
117.828844	3706.323105	23.421171
117.837412	3699.747669	23.426189
117.711429	3710.200138	23.431207
118.209347	3716.228089	23.436224
117.880067	3720.974676	23.441242
118.119803	3720.282279	23.446259
118.212172	3716.819202	23.451277
118.286967	3715.115464	23.456295
118.160606	3712.431796	23.461312
118.050202	3721.278857	23.466330
118.596667	3733.142410	23.471347
118.940978	3741.393294	23.476365
118.673078	3745.280343	23.481383
119.092249	3744.685561	23.486400
119.172698	3763.430668	23.491418
119.248861	3768.262130	23.496435
119.706179	3766.625125	23.501453
119.703788	3773.146840	23.506471
119.611928	3773.663536	23.511488
119.584949	3775.991599	23.516506
119.715111	3770.427823	23.521523
120.294470	3783.156065	23.526541
119.977646	3795.485062	23.531559
120.516958	3791.094747	23.536576
120.594169	3794.659588	23.541594
120.198583	3798.151902	23.546611
120.469624	3792.758502	23.551629
120.532599	3798.442836	23.556647
120.496727	3805.954796	23.561664
120.831074	3814.961155	23.566682
120.824416	3818.064672	23.571699
121.068564	3821.853718	23.576717
121.109708	3844.355400	23.581735
121.359361	3849.049244	23.586752
121.249493	3845.604270	23.591770
121.399660	3852.137669	23.596787
121.876137	3862.929586	23.601805
121.874880	3873.790809	23.606823
122.416847	3872.720529	23.611840
122.456360	3881.114313	23.616858
122.292939	3872.721372	23.621875
123.013923	3865.054990	23.626893
123.343891	3866.355492	23.631911
123.037642	3872.858456	23.636928
123.101256	3865.778115	23.641946
123.014028	3876.810811	23.646963
123.165761	3865.670262	23.651981
123.197466	3869.632781	23.656999
123.456855	3868.827534	23.662016
123.506705	3866.023844	23.667034
122.861646	3870.621410	23.672051
123.226902	3884.138595	23.677069
123.363426	3901.142324	23.682087
123.438741	3897.059141	23.687104
123.880084	3913.585324	23.692122
124.011354	3929.623599	23.697139
123.688132	3927.723438	23.702157
123.573903	3928.651163	23.707175
123.619726	3938.644300	23.712192
124.171397	3955.083091	23.717210
124.159508	3963.560553	23.722227
124.739508	3973.746461	23.727245
124.624544	3978.656435	23.732263
124.891302	3982.950436	23.737280
125.503267	3978.506659	23.742298
125.630807	3969.907841	23.747315
125.959318	3963.540506	23.752333
125.693816	3972.385942	23.757351
125.912671	3960.940831	23.762368
125.896522	3966.626976	23.767386
125.685043	3976.201924	23.772403
126.357126	3990.358903	23.777421
126.150594	3999.451792	23.782439
126.135603	3998.280083	23.787456
126.528017	3995.530272	23.792474
126.351868	3997.168796	23.797491
126.647153	4001.288577	23.802509
126.526348	4012.495670	23.807527
126.833228	4022.005410	23.812544
126.928306	4023.054780	23.817562
126.835321	4033.241896	23.822579
127.128097	4029.686899	23.827597
127.295418	4050.730652	23.832615
127.591373	4054.795200	23.837632
127.868479	4051.709148	23.842650
127.691983	4051.956824	23.847667
127.819595	4051.541971	23.852685
127.844462	4074.794997	23.857703
128.063120	4078.001708	23.862720
128.365692	4082.565260	23.867738
128.484787	4090.589513	23.872755
128.832526	4067.852345	23.877773
128.541959	4069.709756	23.882791
128.654710	4085.752940	23.887808
129.027072	4099.999993	23.892826
128.963130	4115.922278	23.897843
129.410578	4110.467025	23.902861
129.186652	4109.879303	23.907879
129.420729	4108.857852	23.912896
129.799516	4108.589752	23.917914
129.575778	4117.281614	23.922931
130.173413	4116.719236	23.927949
129.839910	4129.740511	23.932967
130.259028	4129.269382	23.937984
130.773480	4123.057558	23.943002
130.848018	4117.606373	23.948019
131.231107	4109.550439	23.953037
131.117710	4121.325781	23.958055
131.340683	4105.246350	23.963072
131.822942	4095.843151	23.968090
131.361687	4087.512180	23.973107
131.468035	4074.359049	23.978125
131.547336	4081.779724	23.983143
131.330337	4076.749495	23.988160
131.429966	4065.167226	23.993178
131.464307	4091.924294	23.998195
131.931305	4092.250682	24.003213
131.762567	4094.768492	24.008231
131.676940	4096.673471	24.013248
131.617288	4090.789274	24.018266
131.404446	4118.360618	24.023283
131.746561	4121.690307	24.028301
131.750087	4139.335367	24.033319
131.858902	4160.390084	24.038336
132.466029	4159.806387	24.043354
132.152502	4175.397403	24.048371
132.200146	4187.418488	24.053389
132.421111	4198.936514	24.058407
132.414781	4210.788869	24.063424
132.949295	4213.729592	24.068442
132.915194	4246.614484	24.073459
133.210972	4250.962655	24.078477
133.594984	4261.923497	24.083495
133.986479	4273.027198	24.088512
134.233107	4281.378601	24.093530
134.415903	4280.582526	24.098547
134.558353	4281.925450	24.103565
134.697900	4277.464915	24.108583
134.435576	4280.517838	24.113600
134.897250	4270.430474	24.118618
134.331259	4281.113124	24.123635
134.866398	4293.639069	24.128653
135.252502	4304.942984	24.133671
135.203640	4302.797262	24.138688
135.931747	4299.409376	24.143706
135.675587	4307.787915	24.148723
135.334137	4301.903902	24.153741
135.285401	4322.206889	24.158759
134.996048	4331.454361	24.163776
135.243759	4342.312606	24.168794
135.582896	4365.152242	24.173811
136.174151	4366.956968	24.178829
137.128530	4382.338706	24.183847
136.652507	4382.011574	24.188864
136.526014	4386.200611	24.193882
136.728303	4395.733234	24.198899
137.113442	4387.142013	24.203917
137.097126	4386.064230	24.208935
137.019625	4391.596433	24.213952
137.367714	4399.602853	24.218970
137.611008	4412.375830	24.223987
137.631397	4425.836033	24.229005
137.895196	4415.194144	24.234023
137.718687	4421.186762	24.239040
137.962223	4418.925525	24.244058
138.110714	4438.862473	24.249075
138.666635	4434.587281	24.254093
139.025790	4427.426095	24.259111
138.964684	4421.189167	24.264128
139.106666	4415.275796	24.269146
139.506259	4423.059166	24.274163
139.092570	4416.284876	24.279181
139.713390	4410.621010	24.284199
139.665695	4422.009615	24.289216
139.651650	4420.680188	24.294234
139.656963	4418.399143	24.299251
140.025408	4413.428330	24.304269
139.556380	4411.100219	24.309287
139.804044	4419.808312	24.314304
140.103959	4409.296494	24.319322
140.334363	4437.780090	24.324339
140.244405	4441.455648	24.329357
140.756737	4446.793028	24.334375
140.362989	4451.255522	24.339392
140.807901	4440.759784	24.344410
140.418260	4452.392122	24.349427
140.716140	4465.374745	24.354445
141.331127	4474.296355	24.359463
140.866262	4473.946042	24.364480
141.169593	4486.322062	24.369498
141.440591	4503.047408	24.374515
141.652233	4507.026499	24.379533
141.879596	4501.534805	24.384551
141.775217	4515.581992	24.389568
141.956545	4527.225985	24.394586
142.149373	4531.331965	24.399603
142.234849	4534.824670	24.404621
142.480094	4546.565626	24.409639
142.264910	4569.376138	24.414656
142.349996	4562.938451	24.419674
142.599666	4570.845262	24.424691
142.823126	4589.765317	24.429709
143.015375	4589.966326	24.434727
142.718478	4596.594790	24.439744
142.851013	4617.117546	24.444762
143.234546	4631.070953	24.449779
143.470655	4642.306309	24.454797
143.996847	4649.619923	24.459815
143.879990	4654.188595	24.464832
144.267681	4662.164732	24.469850
144.440592	4672.216886	24.474867
144.350070	4685.035495	24.479885
144.841540	4676.081692	24.484903
144.700569	4683.704240	24.489920
144.787035	4693.671196	24.494938
145.293591	4701.404074	24.499955
145.428082	4705.573661	24.504973
146.395589	4686.477736	24.509991
146.679947	4692.221320	24.515008
146.694115	4687.047298	24.520026
147.090103	4667.155401	24.525043
146.961046	4659.593408	24.530061
147.108727	4655.258970	24.535079
147.011048	4658.831146	24.540096
146.645893	4640.355975	24.545114
146.717354	4640.533584	24.550131
146.761320	4647.931441	24.555149
147.127417	4645.584576	24.560167
146.876594	4655.098941	24.565184
146.880131	4651.364977	24.570202
146.986750	4644.830624	24.575219
146.352372	4662.765204	24.580237
147.017352	4682.391017	24.585255
146.541468	4702.856719	24.590272
146.831455	4708.682047	24.595290
147.598405	4724.327032	24.600307
148.034168	4735.695208	24.605325
147.795862	4739.635708	24.610343
147.869762	4757.804202	24.615360
148.188525	4769.779253	24.620378
148.404843	4778.485829	24.625395
148.489623	4798.345935	24.630413
148.881727	4801.564807	24.635431
148.909126	4807.915649	24.640448
149.332197	4823.530679	24.645466
149.509206	4828.976871	24.650483
149.497808	4835.751827	24.655501
149.670387	4832.921414	24.660519
149.830119	4838.077567	24.665536
149.860221	4855.638529	24.670554
150.217328	4855.445026	24.675571
150.034893	4878.368515	24.680589
150.260815	4870.613243	24.685607
149.944848	4880.285412	24.690624
150.277373	4896.608379	24.695642
150.684293	4903.535345	24.700659
150.646449	4923.912849	24.705677
151.113233	4920.819320	24.710695
151.993916	4930.637673	24.715712
151.893651	4929.512020	24.720730
152.015525	4925.700207	24.725747
152.063483	4945.547120	24.730765
152.522415	4948.296941	24.735783
152.567013	4957.609614	24.740800
152.391326	4952.446784	24.745818
152.552764	4963.950369	24.750835
152.779903	4954.994466	24.755853
153.085550	4946.038499	24.760871
153.051045	4952.745790	24.765888
153.261070	4943.252499	24.770906
153.218267	4944.992708	24.775923
153.286815	4962.024985	24.780941
153.889520	4961.245112	24.785959
154.029879	4965.463383	24.790976
153.849466	4968.416540	24.795994
154.345879	4954.566478	24.801011
153.945568	4966.054516	24.806029
154.154738	4964.874240	24.811047
153.942610	4968.681134	24.816064
153.923857	4976.078081	24.821082
154.342420	4983.235444	24.826099
154.037516	4996.224168	24.831117
154.608027	5009.466901	24.836135
154.632722	5022.466883	24.841152
154.379846	5030.292303	24.846170
155.060494	5047.913667	24.851187
154.994699	5061.209599	24.856205
155.158016	5074.016513	24.861223
155.316714	5087.123540	24.866240
155.724912	5099.149672	24.871258
156.174689	5103.348808	24.876275
155.914348	5122.161822	24.881293
156.255776	5118.636842	24.886311
156.667885	5137.495281	24.891328
157.231218	5137.709877	24.896346
157.596530	5134.356447	24.901363
157.112182	5142.407491	24.906381
157.685418	5129.214408	24.911399
157.805533	5129.986243	24.916416
157.738590	5125.247380	24.921434
158.448829	5119.104007	24.926451
158.518707	5120.412973	24.931469
158.290141	5125.200208	24.936487
158.318884	5138.127126	24.941504
158.408823	5158.789426	24.946522
158.658947	5152.652452	24.951539
158.359567	5162.680334	24.956557
158.573499	5159.715961	24.961575
158.840798	5181.450613	24.966592
158.674380	5181.687912	24.971610
159.438687	5189.303594	24.976627
159.152214	5208.158210	24.981645
159.283460	5207.374867	24.986663
159.923984	5211.515340	24.991680
159.792466	5216.915310	24.996698
160.179737	5221.118891	25.001715
160.111742	5239.020824	25.006733
160.334326	5229.965514	25.011751
160.400383	5240.253743	25.016768
160.557296	5259.901208	25.021786
161.134802	5259.391086	25.026803
160.968088	5266.770998	25.031821
161.153041	5266.896078	25.036839
161.377103	5277.289572	25.041856
161.550215	5292.805349	25.046874
161.925138	5301.693757	25.051891
161.994297	5300.266500	25.056909
161.706982	5308.270460	25.061927
161.674227	5304.988384	25.066944
161.845075	5329.675416	25.071962
162.480616	5337.554272	25.076979
162.489793	5335.160583	25.081997
162.344219	5346.227144	25.087015
163.001470	5354.699342	25.092032
163.195217	5364.786172	25.097050
163.131309	5358.316205	25.102067
163.165282	5358.854701	25.107085
163.681133	5371.406869	25.112103
163.981467	5383.287086	25.117120
163.774482	5382.153701	25.122138
164.019517	5377.996934	25.127155
164.054489	5393.927176	25.132173
164.031106	5399.087334	25.137191
164.602357	5400.417499	25.142208
164.308562	5408.027995	25.147226
164.769233	5414.893199	25.152243
164.746333	5436.225035	25.157261
164.988758	5432.198668	25.162279
165.250276	5442.298348	25.167296
165.176607	5455.399828	25.172314
165.763968	5455.289728	25.177331
165.946540	5455.523129	25.182349
166.109877	5465.446674	25.187367
166.276261	5468.839072	25.192384
166.043314	5489.177492	25.197402
166.505047	5488.062583	25.202419
166.469868	5501.208702	25.207437
166.513398	5509.593209	25.212455
166.963782	5513.555260	25.217472
166.758483	5520.386590	25.222490
167.346372	5533.518085	25.227507
166.991969	5547.479075	25.232525
167.326878	5543.339941	25.237543
167.542415	5558.371371	25.242560
167.423644	5576.661263	25.247578
167.700389	5583.788074	25.252595
167.626245	5614.511023	25.257613
167.994178	5615.512940	25.262631
168.207393	5630.236062	25.267648
168.309236	5643.078393	25.272666
169.181382	5655.765843	25.277683
169.174671	5664.688370	25.282701
169.513688	5664.217546	25.287719
169.643511	5660.660194	25.292736
169.416345	5668.565801	25.297754
170.044264	5676.555624	25.302771
169.975791	5693.581454	25.307789
169.951919	5693.262634	25.312807
170.473265	5690.025701	25.317824
170.416696	5705.122031	25.322842
170.746310	5719.381815	25.327859
171.083723	5725.812213	25.332877
171.116898	5715.125497	25.337895
171.329393	5722.175951	25.342912
171.472685	5723.886707	25.347930
172.050034	5705.013205	25.352947
171.999209	5706.462640	25.357965
172.152593	5701.973342	25.362983
172.549941	5701.956467	25.368000
172.342495	5713.784556	25.373018
172.627703	5714.640760	25.378035
172.636091	5727.157322	25.383053
172.879363	5723.938119	25.388071
173.217175	5723.710109	25.393088
172.989852	5731.049425	25.398106
173.340017	5728.052931	25.403123
173.041167	5732.774413	25.408141
173.323759	5751.310780	25.413159
173.779940	5752.098292	25.418176
173.780499	5760.690371	25.423194
174.007011	5769.790380	25.428211
174.315901	5781.493774	25.433229
174.526049	5773.925876	25.438247
174.923721	5780.922558	25.443264
174.990225	5776.030655	25.448282
175.082342	5765.661481	25.453299
175.167471	5783.103760	25.458317
175.340199	5798.904455	25.463335
175.648002	5798.863546	25.468352
175.803852	5800.369720	25.473370
175.905939	5792.118503	25.478387
176.312509	5799.194012	25.483405
176.278834	5816.915057	25.488423
176.799075	5809.483032	25.493440
176.732187	5815.173811	25.498458
177.019187	5810.613529	25.503475
176.852053	5816.214366	25.508493
176.917914	5812.139402	25.513511
177.033755	5814.305435	25.518528
177.060591	5834.752576	25.523546
177.403363	5840.418038	25.528563
177.479115	5849.265092	25.533581
177.930868	5859.170952	25.538599
178.325022	5866.885866	25.543616
178.081977	5871.085032	25.548634
178.439393	5874.180892	25.553651
178.289943	5891.100298	25.558669
178.394005	5911.913183	25.563687
178.673624	5908.972860	25.568704
178.582830	5927.281990	25.573722
179.054153	5938.000600	25.578739
179.266607	5942.736897	25.583757
179.296113	5958.661552	25.588775
179.445480	5962.980159	25.593792
179.474344	5990.243134	25.598810
179.842790	5993.058281	25.603827
179.856441	5996.963774	25.608845
180.099791	6021.549655	25.613863
180.580909	6018.552715	25.618880
180.977124	6022.197285	25.623898
180.813206	6032.964988	25.628915
181.048863	6043.215999	25.633933
181.436815	6048.536653	25.638951
181.089384	6046.627773	25.643968
181.457312	6057.888014	25.648986
181.643564	6069.636275	25.654003
181.845218	6068.253981	25.659021
182.082957	6100.709349	25.664039
182.469929	6102.894324	25.669056
182.431131	6112.588254	25.674074
182.405958	6114.557942	25.679092
182.688115	6132.820706	25.684109
183.341461	6120.700905	25.689127
184.425009	6110.633394	25.694144
184.954509	6102.446598	25.699162
185.241025	6090.508646	25.704180
185.437824	6077.350957	25.709197
185.409511	6068.607577	25.714215
185.552802	6055.346436	25.719232
185.309303	6055.114094	25.724250
185.157486	6055.516681	25.729268
185.316889	6054.045531	25.734285
185.189426	6065.871198	25.739303
185.610193	6054.658580	25.744320
185.430312	6052.129411	25.749338
185.552149	6042.827817	25.754356
185.776483	6055.252481	25.759373
185.557151	6079.324622	25.764391
186.019312	6080.991785	25.769408
186.095145	6095.621523	25.774426
185.869720	6115.050436	25.779444
186.412851	6112.532017	25.784461
186.147651	6133.695217	25.789479
186.646923	6140.216196	25.794496
186.992850	6151.499180	25.799514
187.125561	6185.689148	25.804532
187.323768	6185.234573	25.809549
187.021402	6206.728778	25.814567
187.669946	6219.611771	25.819584
187.662342	6232.597799	25.824602
187.764624	6247.983287	25.829620
187.996989	6252.711537	25.834637
188.207943	6272.496719	25.839655
188.470687	6272.981064	25.844672
189.078309	6286.792756	25.849690
189.714358	6287.681015	25.854708
189.703945	6284.508338	25.859725
189.999207	6290.112000	25.864743
190.181418	6289.497107	25.869760
190.407274	6297.712137	25.874778
190.426783	6308.532869	25.879796
190.371311	6305.849996	25.884813
190.699472	6319.819902	25.889831
190.634959	6320.309933	25.894848
190.630660	6325.258374	25.899866
190.612307	6343.206603	25.904884
191.073909	6349.091347	25.909901
190.318296	6366.736675	25.914919
190.941508	6383.572992	25.919936
191.494095	6400.881464	25.924954
191.983409	6414.701732	25.929972
192.028370	6413.115466	25.934989
191.893029	6438.464041	25.940007
192.180709	6442.960728	25.945024
192.641824	6459.636647	25.950042
192.943715	6475.459198	25.955060
193.253080	6471.664505	25.960077
193.137263	6483.220657	25.965095
193.483812	6497.727948	25.970112
193.517611	6502.527334	25.975130
193.291137	6520.820229	25.980148
193.763853	6527.738209	25.985165
193.881032	6539.697954	25.990183
194.316743	6559.306324	25.995200
194.762484	6568.663035	26.000218
194.829935	6584.677127	26.005236
195.505889	6571.708664	26.010253
195.393219	6593.485175	26.015271
195.735352	6586.141618	26.020288
195.873766	6590.968787	26.025306
196.370166	6594.710539	26.030324
196.169565	6586.235092	26.035341
196.051667	6603.812326	26.040359
196.369545	6621.258951	26.045376
196.299823	6630.593775	26.050394
196.628706	6659.278741	26.055412
196.949487	6660.048552	26.060429
197.188024	6674.424063	26.065447
197.463077	6685.785746	26.070464
197.566260	6683.707378	26.075482
197.941874	6698.213021	26.080500
198.256087	6700.644511	26.085517
198.420149	6725.308877	26.090535
198.442846	6721.412020	26.095552
198.320257	6716.905939	26.100570
198.493842	6732.563257	26.105588
198.728459	6735.178549	26.110605
198.923637	6762.141776	26.115623
198.453907	6775.775422	26.120640
199.059912	6784.119325	26.125658
198.833649	6806.387455	26.130676
199.506639	6816.434808	26.135693
199.514517	6842.169099	26.140711
199.746129	6856.196201	26.145728
200.289654	6871.651599	26.150746
200.425490	6894.427322	26.155764
200.684480	6907.966100	26.160781
200.805792	6913.830611	26.165799
201.107323	6931.975960	26.170816
201.497478	6932.915864	26.175834
201.475177	6930.688033	26.180852
202.155871	6941.838570	26.185869
202.025844	6951.628210	26.190887
202.956398	6951.372632	26.195904
203.092235	6949.109813	26.200922
203.400540	6952.850809	26.205940
203.748152	6943.133448	26.210957
203.698435	6947.992973	26.215975
203.446787	6942.202073	26.220992
203.950890	6940.686724	26.226010
203.985365	6954.513744	26.231028
204.138045	6964.852046	26.236045
204.041050	6975.471842	26.241063
204.354940	6980.484105	26.246080
204.758876	6982.244851	26.251098
204.826110	7003.699614	26.256116
205.155027	6999.981010	26.261133
205.159372	7003.794603	26.266151
205.052458	7015.245629	26.271168
205.367495	7024.105097	26.276186
205.247161	7041.535919	26.281204
205.669504	7057.360458	26.286221
205.564727	7063.180277	26.291239
205.811813	7087.111749	26.296256
205.929226	7099.368857	26.301274
205.926387	7116.938747	26.306292
206.395684	7136.430997	26.311309
206.902610	7156.490310	26.316327
206.927902	7170.675158	26.321344
207.215675	7173.316861	26.326362
207.414492	7191.592761	26.331380
207.564432	7206.406966	26.336397
207.892514	7212.574882	26.341415
208.166732	7231.769827	26.346432
208.933568	7237.337105	26.351450
208.937504	7250.862387	26.356468
209.410876	7255.898606	26.361485
209.561445	7271.198026	26.366503
209.667633	7280.528284	26.371520
210.368592	7273.628653	26.376538
210.205683	7270.543366	26.381556
210.378006	7276.171603	26.386573
210.019724	7279.923742	26.391591
210.265084	7293.082329	26.396608
210.393185	7301.751057	26.401626
210.670900	7333.678215	26.406644
210.884207	7339.258485	26.411661
211.177432	7350.875916	26.416679
210.549596	7359.171656	26.421696
211.502858	7387.906094	26.426714
211.522415	7399.935997	26.431732
212.108502	7411.415829	26.436749
212.206528	7424.981062	26.441767
212.179795	7433.773299	26.446784
212.702481	7444.178470	26.451802
212.439796	7458.917899	26.456820
212.742593	7463.853440	26.461837
213.018337	7483.938613	26.466855
213.035595	7496.102116	26.471872
213.591240	7509.530683	26.476890
213.384685	7526.315077	26.481908
213.993474	7544.561283	26.486925
214.377992	7540.049973	26.491943
215.046521	7535.420656	26.496960
215.788811	7542.336990	26.501978
215.616963	7540.984722	26.506996
215.854267	7549.931859	26.512013
216.265615	7552.151463	26.517031
215.973321	7560.063649	26.522048
216.427525	7556.208427	26.527066
216.660187	7560.388723	26.532084
216.535859	7557.060433	26.537101
216.557282	7559.404385	26.542119
216.450395	7582.608705	26.547136
217.074756	7583.339920	26.552154
217.317860	7601.368425	26.557172
217.469261	7621.640519	26.562189
217.569813	7622.131443	26.567207
217.543728	7633.130259	26.572224
217.972749	7643.830492	26.577242
218.000971	7660.598416	26.582260
218.382564	7673.772566	26.587277
218.172734	7688.490541	26.592295
218.229244	7713.920111	26.597312
218.507673	7723.252615	26.602330
218.954553	7734.334288	26.607348
219.683381	7739.024362	26.612365
220.070942	7757.518285	26.617383
220.674567	7749.011505	26.622400
221.123827	7751.232518	26.627418
221.466389	7752.570589	26.632436
221.912252	7753.081105	26.637453
222.014378	7753.266101	26.642471
221.872521	7745.863178	26.647488
222.368793	7744.813109	26.652506
222.515259	7744.015221	26.657524
222.408128	7745.410680	26.662541
222.484694	7744.922558	26.667559
222.837255	7741.004361	26.672576
222.936813	7741.571087	26.677594
222.654166	7754.788262	26.682612
222.797397	7768.941607	26.687629
222.737074	7782.365698	26.692647
222.543221	7807.164771	26.697664
222.970427	7809.309218	26.702682
223.252546	7827.579444	26.707700
223.285663	7850.330806	26.712717
223.854342	7857.942725	26.717735
223.838274	7882.955656	26.722752
224.216214	7898.972987	26.727770
224.610264	7913.554568	26.732788
224.666847	7939.037266	26.737805
224.861040	7934.203174	26.742823
225.048631	7965.534920	26.747840
225.643700	7974.645494	26.752858
225.822934	7986.576777	26.757876
226.045136	8003.274782	26.762893
226.281984	8004.960297	26.767911
226.467612	8025.390898	26.772928
226.573258	8033.803897	26.777946
226.743238	8046.996509	26.782964
226.925450	8061.754766	26.787981
227.605421	8068.738736	26.792999
227.648305	8088.976451	26.798016
227.830530	8091.593072	26.803034
228.546977	8103.934191	26.808052
228.390313	8112.577329	26.813069
228.534095	8112.345529	26.818087
228.744296	8133.353457	26.823104
229.025839	8134.167099	26.828122
229.404800	8151.687646	26.833140
229.314518	8157.060263	26.838157
229.701541	8163.802213	26.843175
229.413878	8177.423164	26.848192
230.157908	8197.595191	26.853210
230.726840	8198.636886	26.858228
230.602934	8220.177246	26.863245
231.286915	8218.395397	26.868263
231.417316	8223.924800	26.873280
232.090398	8238.820455	26.878298
232.118896	8245.284347	26.883316
232.281325	8247.910689	26.888333
232.679586	8242.582231	26.893351
232.230410	8257.634030	26.898368
232.785137	8261.385882	26.903386
233.096189	8273.970729	26.908404
232.947980	8287.823121	26.913421
233.207192	8295.203107	26.918439
233.389152	8311.950085	26.923456
233.469884	8313.451258	26.928474
233.833144	8331.006993	26.933492
233.646555	8351.802757	26.938509
234.394110	8370.649288	26.943527
234.425651	8384.149522	26.948544
234.670511	8396.526797	26.953562
234.942604	8400.665103	26.958580
234.994836	8422.857008	26.963597
235.762018	8439.574712	26.968615
236.079538	8450.664876	26.973632
236.454993	8468.257275	26.978650
236.091371	8468.529991	26.983668
236.186630	8485.832460	26.988685
236.560822	8499.118067	26.993703
236.572180	8511.770227	26.998720
237.004999	8524.448634	27.003738
237.688037	8528.284125	27.008756
237.332542	8537.456327	27.013773
237.721803	8552.003072	27.018791
237.967478	8565.068112	27.023808
238.315556	8575.650490	27.028826
238.458375	8580.240369	27.033844
238.612557	8599.520555	27.038861
239.171714	8603.292213	27.043879
239.075270	8620.704894	27.048896
239.181743	8628.198663	27.053914
239.689825	8645.706284	27.058932
239.657776	8652.655780	27.063949
240.134797	8659.796127	27.068967
240.252036	8678.418596	27.073984
240.607814	8690.423348	27.079002
241.135273	8696.445793	27.084020
241.206434	8702.882860	27.089037
241.696748	8716.051839	27.094055
242.026254	8739.151512	27.099072
242.250402	8744.479883	27.104090
242.313769	8735.765028	27.109108
242.284346	8758.359796	27.114125
242.609491	8765.253630	27.119143
242.609468	8778.560281	27.124160
242.734730	8786.784383	27.129178
243.161679	8810.615904	27.134196
243.219429	8820.461942	27.139213
243.523060	8829.804165	27.144231
244.361189	8845.978341	27.149248
244.543411	8850.541847	27.154266
244.887302	8859.513204	27.159284
244.828612	8878.428411	27.164301
245.344768	8876.869860	27.169319
245.610666	8893.931589	27.174336
245.752622	8912.123867	27.179354
245.939395	8909.315523	27.184372
245.926162	8931.628072	27.189389
246.314481	8929.287825	27.194407
246.513062	8957.090064	27.199424
247.005314	8964.156243	27.204442
247.411768	8960.505053	27.209460
247.716289	8980.317724	27.214477
247.663386	8993.335809	27.219495
247.826155	8995.630531	27.224512
247.995349	9004.145021	27.229530
248.376052	9020.369417	27.234548
248.584801	9033.408865	27.239565
248.828542	9035.070462	27.244583
248.638496	9052.464199	27.249600
248.799962	9054.820606	27.254618
249.064231	9074.996401	27.259636
249.592744	9093.982964	27.264653
249.896288	9112.888356	27.269671
250.424372	9119.125940	27.274688
250.293654	9127.674569	27.279706
250.923971	9144.941972	27.284724
251.107214	9138.716467	27.289741
251.642410	9142.003104	27.294759
251.751458	9162.199312	27.299776
251.588823	9163.902215	27.304794
252.201863	9162.363274	27.309812
252.336477	9178.765522	27.314829
252.545500	9195.385087	27.319847
252.633451	9201.280579	27.324864
252.868850	9211.602213	27.329882
253.325964	9224.711122	27.334900
253.389811	9233.142944	27.339917
253.800824	9245.106341	27.344935
253.954301	9258.138113	27.349952
254.095812	9267.602923	27.354970
254.169007	9287.400471	27.359988
254.322870	9299.370168	27.365005
254.388905	9316.135699	27.370023
255.556913	9307.395072	27.375040
256.821398	9307.731455	27.380058
257.295018	9303.665290	27.385076
257.550694	9293.325684	27.390093
257.776659	9279.181066	27.395111
257.756539	9273.956288	27.400128
257.434523	9274.938050	27.405146
257.858603	9276.051924	27.410164
258.015804	9274.832192	27.415181
258.131218	9272.945212	27.420199
257.947270	9279.648413	27.425216
257.777176	9301.898545	27.430234
258.437970	9305.899556	27.435252
258.653680	9324.525590	27.440269
258.770841	9342.171098	27.445287
258.904594	9349.834647	27.450304
258.720981	9373.100392	27.455322
259.268823	9386.461758	27.460340
259.827968	9399.132599	27.465357
259.991416	9407.277989	27.470375
260.479857	9420.019268	27.475392
260.734455	9434.136870	27.480410
261.745385	9452.048451	27.485428
261.687661	9465.664950	27.490445
261.717797	9473.962435	27.495463
262.026360	9471.416754	27.500480
261.987278	9486.943033	27.505498
261.947352	9495.291931	27.510516
262.188975	9512.957262	27.515533
262.363697	9526.360638	27.520551
262.546723	9543.300170	27.525568
262.410085	9571.015956	27.530586
262.425526	9582.911893	27.535604
262.576222	9614.051473	27.540621
262.742294	9649.657346	27.545639
263.442225	9665.394340	27.550656
263.731238	9699.174997	27.555674
263.904346	9716.303926	27.560692
263.953683	9738.910989	27.565709
264.639270	9766.336479	27.570727
264.750613	9779.560259	27.575744
265.229040	9802.230956	27.580762
265.663332	9811.836572	27.585780
265.902538	9831.417238	27.590797
266.426976	9847.086793	27.595815
266.748885	9852.096226	27.600832
267.039684	9876.001510	27.605850
267.331853	9888.097637	27.610868
267.599075	9900.815759	27.615885
268.121556	9903.182900	27.620903
268.494043	9901.292755	27.625920
268.412164	9931.079812	27.630938
269.220321	9934.778386	27.635956
269.328187	9944.499911	27.640973
269.011488	9950.635220	27.645991
269.677315	9962.557053	27.651008
269.701230	9970.390999	27.656026
269.985936	9991.568220	27.661044
270.126207	10008.198832	27.666061
270.325956	10023.588565	27.671079
270.462767	10031.579680	27.676096
270.570838	10053.277331	27.681114
270.715410	10080.306011	27.686132
271.198599	10106.320181	27.691149
271.529212	10131.823192	27.696167
271.905994	10142.586054	27.701184
272.008913	10168.900298	27.706202
272.502284	10189.225741	27.711220
273.012020	10203.747816	27.716237
273.185779	10224.214754	27.721255
273.651675	10220.753229	27.726272
274.174905	10229.035921	27.731290
274.590417	10244.154085	27.736308
274.861361	10253.483829	27.741325
274.792066	10257.180020	27.746343
275.322512	10276.077826	27.751360
275.110166	10281.259331	27.756378
275.221500	10299.775162	27.761396
275.916011	10316.624683	27.766413
275.930380	10330.785819	27.771431
276.229386	10343.716306	27.776448
276.284276	10359.353380	27.781466
276.507362	10374.340761	27.786484
276.630263	10395.755830	27.791501
277.139065	10429.265539	27.796519
277.266991	10442.269552	27.801536
277.882219	10463.729546	27.806554
277.678171	10479.950055	27.811572
278.144783	10498.879548	27.816589
278.257207	10512.236112	27.821607
278.841098	10524.214954	27.826624
278.638171	10554.692061	27.831642
279.604338	10566.873308	27.836660
280.028031	10574.883281	27.841677
280.579783	10578.917490	27.846695
281.308303	10585.124447	27.851712
281.423363	10590.979555	27.856730
281.592059	10585.301238	27.861748
282.116640	10587.586179	27.866765
282.018342	10592.456703	27.871783
282.416354	10583.374630	27.876800
282.376814	10595.759793	27.881818
282.825627	10613.592524	27.886836
283.124664	10608.624632	27.891853
282.700094	10618.266052	27.896871
282.760422	10637.156609	27.901888
283.071952	10654.429847	27.906906
283.172149	10673.231668	27.911924
283.495554	10696.130324	27.916941
283.414357	10719.610519	27.921959
284.105069	10738.120522	27.926976
284.492763	10771.328642	27.931994
284.511340	10781.190468	27.937012
284.960557	10801.133431	27.942029
284.936913	10833.476111	27.947047
285.665774	10851.481727	27.952064
285.598967	10870.711098	27.957082
286.519578	10898.200660	27.962100
286.889034	10916.921943	27.967117
286.935278	10930.824420	27.972135
287.220912	10949.845343	27.977152
287.135480	10978.621630	27.982170
288.166366	10990.163326	27.987188
288.632794	11002.236724	27.992205
288.455590	11013.192823	27.997223
289.006986	11029.777655	28.002240
289.138961	11046.078237	28.007258
289.791065	11065.033332	28.012276
290.045676	11076.489091	28.017293
289.995674	11091.798148	28.022311
290.585421	11105.658049	28.027328
290.836504	11109.215999	28.032346
291.327837	11139.420767	28.037364
291.667971	11133.805855	28.042381
291.723758	11151.922441	28.047399
291.960951	11165.836517	28.052416
292.056388	11173.348329	28.057434
291.976938	11196.248975	28.062452
292.032757	11206.498654	28.067469
292.458011	11239.321497	28.072487
292.870039	11248.936515	28.077504
292.992403	11264.324930	28.082522
293.729711	11287.142448	28.087540
294.539538	11300.945885	28.092557
294.491486	11321.915546	28.097575
294.824189	11332.357387	28.102592
295.340854	11329.145385	28.107610
295.705805	11334.136873	28.112628
296.162641	11337.476800	28.117645
295.938013	11340.162899	28.122663
295.846217	11346.020639	28.127680
296.764414	11361.934635	28.132698
296.551313	11375.560453	28.137716
297.201933	11386.436379	28.142733
296.867947	11411.662905	28.147751
297.352988	11429.085308	28.152768
297.566502	11440.746936	28.157786
297.518876	11467.134787	28.162804
298.167557	11481.273307	28.167821
297.849781	11510.024164	28.172839
298.391354	11524.623919	28.177856
298.902336	11559.245054	28.182874
299.133262	11574.211711	28.187892
300.350371	11574.220626	28.192909
300.806473	11586.669731	28.197927
301.086142	11598.009671	28.202944
301.448328	11601.305991	28.207962
301.157921	11607.092276	28.212980
301.588451	11627.011092	28.217997
302.013337	11633.458039	28.223015
302.470049	11645.788889	28.228032
302.448335	11665.791567	28.233050
302.612929	11675.138784	28.238068
303.524126	11685.596748	28.243085
303.849165	11700.178617	28.248103
303.947957	11698.467564	28.253120
304.084827	11708.169415	28.258138
304.028879	11725.618669	28.263156
304.493202	11744.939274	28.268173
304.799956	11759.458139	28.273191
305.171613	11789.911567	28.278208
305.450552	11806.837023	28.283226
305.234974	11830.423798	28.288244
305.983522	11827.996194	28.293261
306.190133	11867.210536	28.298279
306.429147	11880.472456	28.303296
306.540724	11895.942115	28.308314
306.789867	11921.307454	28.313332
307.149177	11945.100028	28.318349
307.891673	11974.996959	28.323367
307.692290	11983.937091	28.328384
307.886055	12005.911065	28.333402
308.544667	12034.909984	28.338420
309.085354	12047.874480	28.343437
309.005199	12063.216408	28.348455
309.178767	12082.916630	28.353472
309.875137	12091.742696	28.358490
310.237046	12118.151238	28.363508
310.372331	12127.708618	28.368525
311.141170	12144.685996	28.373543
311.291748	12151.821600	28.378560
311.360261	12179.716269	28.383578
310.946320	12192.776729	28.388596
311.856017	12217.228700	28.393613
311.926902	12237.859221	28.398631
312.250953	12261.146093	28.403648
312.531849	12284.541261	28.408666
312.820482	12302.918660	28.413684
313.067638	12327.640377	28.418701
313.141870	12353.732968	28.423719
313.616141	12378.132152	28.428736
314.395336	12396.201781	28.433754
315.439163	12401.003174	28.438772
315.938785	12403.760742	28.443789
315.921472	12407.357100	28.448807
316.074245	12431.923364	28.453824
316.816151	12433.726889	28.458842
317.018780	12441.649596	28.463860
317.048141	12455.928210	28.468877
317.195221	12476.991991	28.473895
317.736979	12473.373582	28.478912
317.988049	12485.472388	28.483930
318.251846	12495.048934	28.488948
318.223132	12510.811147	28.493965
318.626568	12534.822392	28.498983
319.027136	12555.198226	28.504000
319.320591	12563.732692	28.509018
318.961098	12590.352321	28.514036
319.953657	12610.469158	28.519053
319.863476	12627.906328	28.524071
320.494933	12650.080385	28.529088
320.598384	12673.567988	28.534106
320.772131	12687.910318	28.539124
321.326826	12716.102404	28.544141
321.637877	12744.430861	28.549159
321.626682	12769.563172	28.554176
321.948065	12799.634658	28.559194
322.100886	12828.286680	28.564212
322.686914	12850.512926	28.569229
323.265975	12876.434719	28.574247
323.390306	12893.348397	28.579264
323.780763	12910.865826	28.584282
324.193756	12934.463086	28.589300
324.748683	12951.788459	28.594317
325.054710	12973.853243	28.599335
325.116659	12998.774782	28.604352
325.599967	13018.153533	28.609370
326.037668	13042.629325	28.614388
326.443584	13046.791603	28.619405
326.689826	13069.738342	28.624423
326.688335	13090.382339	28.629440
327.194747	13103.813773	28.634458
327.244351	13130.680956	28.639476
327.900705	13149.335145	28.644493
327.983813	13175.719101	28.649511
327.894748	13198.802293	28.654528
328.711382	13222.341822	28.659546
328.792777	13247.492093	28.664564
329.441907	13263.053742	28.669581
329.541667	13286.238664	28.674599
329.733198	13310.202253	28.679616
330.147637	13319.819662	28.684634
330.620689	13353.804892	28.689652
330.833699	13375.395984	28.694669
331.190823	13404.977008	28.699687
331.686022	13427.437111	28.704704
331.994986	13441.719097	28.709722
332.266774	13465.081261	28.714740
332.616781	13483.422672	28.719757
332.878187	13504.479211	28.724775
333.128348	13528.847594	28.729792
333.815651	13541.030030	28.734810
334.054333	13558.210076	28.739828
335.247557	13559.361095	28.744845
335.220326	13567.287491	28.749863
335.724854	13578.345968	28.754880
336.044415	13594.780861	28.759898
336.594391	13610.251081	28.764916
336.656679	13610.883513	28.769933
336.959523	13627.587672	28.774951
336.989850	13639.931640	28.779968
337.672824	13659.975166	28.784986
337.560391	13676.156339	28.790004
337.286609	13700.556456	28.795021
338.138133	13715.839546	28.800039
338.993276	13739.374797	28.805056
338.987158	13759.369473	28.810074
339.352719	13775.237125	28.815092
339.648490	13781.276766	28.820109
340.590770	13790.764584	28.825127
341.196898	13794.290648	28.830144
342.570801	13793.139469	28.835162
343.004216	13790.656850	28.840180
343.790527	13759.684510	28.845197
344.183613	13742.963473	28.850215
343.720255	13740.423348	28.855232
344.036204	13737.292576	28.860250
344.099920	13736.723736	28.865268
344.342597	13729.354624	28.870285
344.556141	13727.177642	28.875303
344.524741	13727.690586	28.880320
344.941442	13736.171444	28.885338
345.087337	13736.721777	28.890356
344.363120	13759.227406	28.895373
345.210414	13771.874359	28.900391
345.065310	13791.894471	28.905408
345.289153	13819.770036	28.910426
345.363062	13848.454700	28.915444
345.902582	13877.100595	28.920461
346.457813	13899.823737	28.925479
346.686352	13927.132831	28.930496
346.679221	13950.737359	28.935514
346.937871	13981.272550	28.940532
347.146761	14008.660804	28.945549
347.609420	14026.699804	28.950567
347.897681	14060.103454	28.955584
348.079273	14089.424201	28.960602
348.514787	14117.147352	28.965620
348.797752	14155.225522	28.970637
349.220345	14173.156487	28.975655
349.152646	14211.264936	28.980672
349.813367	14246.742463	28.985690
350.394265	14275.935210	28.990708
351.111905	14304.043783	28.995725
351.575432	14327.170980	29.000743
351.767063	14359.326096	29.005760
352.213849	14374.775320	29.010778
352.575933	14406.813047	29.015796
353.211648	14426.400626	29.020813
353.605293	14438.080807	29.025831
354.040348	14465.883436	29.030848
354.151965	14480.387720	29.035866
354.507188	14497.283968	29.040884
355.133598	14519.007470	29.045901
355.821865	14518.374124	29.050919
356.576419	14537.684543	29.055936
356.948889	14544.581404	29.060954
357.247572	14561.104383	29.065972
357.369278	14571.180944	29.070989
357.952630	14570.833538	29.076007
357.995057	14609.392174	29.081024
357.948970	14614.753031	29.086042
358.562797	14634.008869	29.091060
358.578828	14653.014103	29.096077
359.080514	14679.822096	29.101095
359.248557	14700.316107	29.106112
359.773799	14721.289580	29.111130
360.578696	14739.544978	29.116148
360.561660	14753.891858	29.121165
360.753773	14763.143122	29.126183
361.208416	14799.453168	29.131200
361.525602	14815.892842	29.136218
361.604534	14842.089453	29.141236
362.358631	14871.710691	29.146253
361.995505	14878.475252	29.151271
362.210982	14924.173830	29.156288
362.690510	14951.044383	29.161306
363.097429	14976.174604	29.166324
363.218631	15016.716254	29.171341
363.849472	15026.828787	29.176359
364.267834	15064.959935	29.181376
364.918544	15091.114119	29.186394
365.448957	15115.298106	29.191412
365.719005	15139.627633	29.196429
365.777490	15152.265824	29.201447
366.224477	15176.249822	29.206464
366.549499	15211.645092	29.211482
367.207386	15226.139955	29.216500
367.533769	15255.485244	29.221517
368.172203	15262.259588	29.226535
368.832156	15278.265818	29.231552
369.044028	15285.854139	29.236570
369.479769	15301.824731	29.241588
369.622129	15323.250784	29.246605
369.900366	15341.570312	29.251623
370.296444	15360.801267	29.256640
370.237933	15384.022565	29.261658
370.783279	15409.876896	29.266676
370.688552	15426.660474	29.271693
371.161948	15448.012616	29.276711
371.721438	15483.415573	29.281728
372.081794	15511.912161	29.286746
372.347970	15543.563413	29.291764
372.748330	15559.349582	29.296781
373.619917	15567.504370	29.301799
373.748939	15595.894150	29.306816
374.119820	15617.391762	29.311834
374.576038	15640.198904	29.316852
375.062845	15671.904017	29.321869
375.616883	15690.679519	29.326887
375.582953	15715.613707	29.331904
375.742874	15734.070596	29.336922
376.528871	15752.342969	29.341940
377.022330	15774.138201	29.346957
377.501411	15793.451591	29.351975
377.949822	15814.050261	29.356992
378.239061	15825.460847	29.362010
379.102928	15852.063648	29.367028
379.720943	15867.970447	29.372045
380.198554	15863.496892	29.377063
380.174864	15891.596500	29.382080
380.525488	15900.539067	29.387098
380.899057	15917.509290	29.392116
380.887917	15942.879720	29.397133
381.386679	15955.542382	29.402151
381.191606	15978.898260	29.407168
381.828339	15999.029808	29.412186
382.033425	16019.002051	29.417204
382.106555	16050.813464	29.422221
382.580383	16074.277112	29.427239
382.583045	16109.710627	29.432256
382.885929	16134.791075	29.437274
383.545407	16160.388985	29.442292
383.752902	16203.379488	29.447309
384.466285	16227.782815	29.452327
384.866834	16261.531083	29.457344
384.975257	16294.000575	29.462362
385.447746	16323.338479	29.467380
385.707991	16365.128597	29.472397
386.335283	16388.093466	29.477415
386.580403	16416.396964	29.482432
386.882948	16453.977338	29.487450
387.443570	16472.739988	29.492468
387.536887	16504.947641	29.497485
388.227175	16520.458036	29.502503
388.813041	16546.966142	29.507520
389.746385	16568.663387	29.512538
390.158688	16579.993498	29.517556
390.299693	16601.905395	29.522573
390.611647	16617.736099	29.527591
390.960607	16635.141640	29.532608
391.406215	16658.128561	29.537626
391.986021	16675.152496	29.542644
391.890587	16708.001394	29.547661
392.833932	16730.542111	29.552679
393.068862	16743.800768	29.557696
393.594101	16759.517811	29.562714
393.700477	16791.268187	29.567732
394.067156	16816.488493	29.572749
394.300138	16835.416477	29.577767
395.020016	16845.738729	29.582784
395.534548	16865.072516	29.587802
396.496399	16887.391148	29.592820
396.877449	16909.689533	29.597837
396.932137	16923.627148	29.602855
396.932316	16936.480051	29.607872
397.107424	16965.974098	29.612890
397.613319	16986.427220	29.617908
397.908257	17013.052139	29.622925
398.409847	17046.418941	29.627943
398.806691	17067.950242	29.632960
398.436915	17102.874278	29.637978
399.260762	17126.243168	29.642996
399.503508	17152.744830	29.648013
399.987712	17186.274116	29.653031
400.331475	17222.285284	29.658048
400.769833	17255.977063	29.663066
401.018117	17278.881996	29.668084
401.415164	17324.387366	29.673101
402.271057	17343.617491	29.678119
402.773022	17376.439420	29.683136
403.295527	17406.726023	29.688154
403.529837	17426.696521	29.693172
403.889704	17449.018175	29.698189
404.388017	17481.472033	29.703207
404.473976	17515.104911	29.708224
404.863941	17555.065936	29.713242
405.501348	17573.679514	29.718260
405.987227	17612.523827	29.723277
406.923606	17625.620412	29.728295
407.457253	17643.998029	29.733312
407.996001	17671.575429	29.738330
408.098296	17673.115551	29.743348
408.778893	17688.907747	29.748365
409.172559	17706.510120	29.753383
409.776210	17714.330378	29.758400
409.787107	17728.350265	29.763418
410.254098	17736.105668	29.768436
410.279880	17767.179608	29.773453
410.364296	17777.125768	29.778471
410.837472	17805.854467	29.783488
411.727824	17810.158818	29.788506
412.711868	17817.042109	29.793524
412.905856	17832.968282	29.798541
413.186996	17848.922102	29.803559
414.119690	17853.769425	29.808576
414.120889	17875.137816	29.813594
414.426284	17881.333393	29.818612
414.669288	17899.655471	29.823629
414.918298	17910.793757	29.828647
415.512780	17927.267820	29.833664
415.430933	17949.896018	29.838682
415.986564	17976.208206	29.843700
415.776811	18003.384700	29.848717
416.198901	18030.008368	29.853735
416.616140	18060.150233	29.858752
417.117468	18094.324801	29.863770
417.812248	18121.584540	29.868788
418.063174	18154.901919	29.873805
418.263422	18189.303276	29.878823
418.998610	18206.292693	29.883840
419.107045	18247.090331	29.888858
419.619427	18265.964173	29.893876
420.302758	18299.407965	29.898893
420.815434	18334.293697	29.903911
421.306698	18362.974531	29.908928
421.198004	18397.049297	29.913946
422.107797	18416.220976	29.918964
422.414261	18454.358563	29.923981
422.935576	18488.621953	29.928999
423.190580	18513.058310	29.934016
423.541743	18551.030796	29.939034
423.710323	18584.074617	29.944052
424.217665	18611.247451	29.949069
425.029434	18634.585844	29.954087
425.887161	18656.335039	29.959104
426.289209	18683.819288	29.964122
427.109130	18701.210918	29.969140
427.507517	18727.377804	29.974157
427.898539	18742.027114	29.979175
428.339922	18749.051092	29.984192
428.115802	18769.544785	29.989210
428.511892	18793.925841	29.994228
429.239971	18828.783571	29.999245
429.301263	18847.588743	30.004263
429.624818	18881.413832	30.009280
429.637287	18915.257612	30.014298
429.876819	18949.256476	30.019316
430.510652	18987.009652	30.024333
430.902947	19012.517407	30.029351
432.237029	19031.142511	30.034368
432.750841	19061.649601	30.039386
433.196590	19064.792799	30.044404
433.669392	19087.962873	30.049421
433.807677	19117.091767	30.054439
434.329367	19126.886537	30.059456
434.422237	19160.619278	30.064474
434.590934	19179.128921	30.069492
435.258621	19205.706061	30.074509
435.127835	19238.422489	30.079527
435.902102	19266.914470	30.084544
436.248385	19293.638274	30.089562
436.658953	19324.704336	30.094580
437.118869	19341.218621	30.099597
437.731995	19370.936676	30.104615
438.619844	19388.836114	30.109632
438.881398	19419.678770	30.114650
439.473574	19451.759295	30.119668
439.773101	19468.195551	30.124685
440.175356	19495.578605	30.129703
440.356439	19516.256038	30.134720
440.832990	19548.791732	30.139738
441.157200	19586.931997	30.144756
441.689567	19615.565356	30.149773
441.911999	19661.125903	30.154791
442.237105	19679.703895	30.159808
442.433408	19720.611450	30.164826
442.972125	19760.394559	30.169844
443.583158	19802.741748	30.174861
443.803373	19841.283554	30.179879
444.621703	19874.157067	30.184896
444.776679	19916.669413	30.189914
445.324342	19952.812323	30.194932
445.895279	19990.114962	30.199949
446.101788	20023.713272	30.204967
446.601000	20055.963822	30.209984
447.208046	20092.073202	30.215002
447.984109	20141.893601	30.220020
448.835118	20163.940760	30.225037
448.690767	20195.953394	30.230055
451.423938	20171.232825	30.235072
452.657311	20157.560670	30.240090
453.128588	20163.479540	30.245108
453.629151	20155.059026	30.250125
453.670577	20147.590721	30.255143
453.924609	20141.467230	30.260160
454.103661	20141.444471	30.265178
454.100666	20142.657555	30.270196
454.148338	20153.361956	30.275213
454.498172	20175.083478	30.280231
454.716956	20186.266297	30.285248
455.235743	20213.818184	30.290266
455.188173	20245.188351	30.295284
455.268703	20270.324130	30.300301
455.351753	20302.184470	30.305319
455.724827	20328.474863	30.310336
455.788421	20368.728712	30.315354
456.045678	20398.298272	30.320372
456.300231	20434.681656	30.325389
456.976583	20482.131310	30.330407
457.234489	20525.576778	30.335424
457.392785	20569.627573	30.340442
458.047123	20615.774205	30.345460
458.397271	20663.871569	30.350477
458.624408	20720.074484	30.355495
459.439631	20761.763090	30.360512
459.716337	20804.526440	30.365530
460.426241	20853.239150	30.370548
461.651140	20889.569186	30.375565
462.376282	20917.763320	30.380583
463.283700	20938.964529	30.385600
464.390154	20960.212079	30.390618
464.701809	20985.020749	30.395636
465.673559	20996.472440	30.400653
465.918024	21017.971843	30.405671
466.372363	21016.542672	30.410688
466.670422	21040.551140	30.415706
466.817550	21069.908947	30.420724
467.503166	21080.704876	30.425741
467.741409	21102.528706	30.430759
468.053327	21122.157574	30.435776
468.745105	21153.817437	30.440794
468.611951	21186.574294	30.445812
468.929467	21204.912427	30.450829
469.176221	21247.074933	30.455847
470.094158	21278.275251	30.460864
470.729937	21310.124764	30.465882
470.613693	21349.050911	30.470900
471.169666	21375.773611	30.475917
471.487164	21416.672374	30.480935
471.734490	21447.909074	30.485952
472.252395	21481.672945	30.490970
472.213340	21526.657286	30.495988
472.606168	21569.248126	30.501005
473.263981	21613.739559	30.506023
473.942356	21649.447390	30.511040
474.733795	21699.012699	30.516058
475.209470	21737.825687	30.521076
476.106934	21765.908127	30.526093
477.022169	21796.151098	30.531111
477.695965	21819.807706	30.536128
477.591644	21854.882129	30.541146
477.797686	21888.613516	30.546164
478.436117	21919.208484	30.551181
478.788620	21957.098499	30.556199
479.919731	21985.242190	30.561216
480.311509	22016.830490	30.566234
480.584568	22059.427310	30.571252
480.880566	22076.372901	30.576269
481.246875	22113.005651	30.581287
481.775874	22141.829938	30.586304
482.217383	22167.256745	30.591322
482.761753	22201.395977	30.596340
483.450548	22221.535545	30.601357
483.662266	22249.556519	30.606375
483.868235	22288.844333	30.611392
484.174026	22321.318414	30.616410
484.401657	22361.337548	30.621428
485.208014	22386.301614	30.626445
485.674874	22433.565530	30.631463
485.940101	22474.143043	30.636480
486.776808	22511.449839	30.641498
486.788559	22557.104710	30.646516
487.694573	22580.639004	30.651533
489.126774	22593.337558	30.656551
490.163598	22617.455053	30.661568
490.409238	22631.000369	30.666586
490.495403	22669.678790	30.671604
490.931783	22677.028556	30.676621
491.384634	22703.044016	30.681639
492.357070	22725.677703	30.686656
492.910075	22740.555045	30.691674
493.171646	22769.593381	30.696692
493.609089	22797.712198	30.701709
493.699092	22824.666834	30.706727
493.924335	22857.461676	30.711744
494.455438	22890.513267	30.716762
494.616284	22929.006004	30.721780
495.475368	22965.552990	30.726797
496.137773	23005.306734	30.731815
496.643542	23041.122755	30.736832
496.971636	23068.443851	30.741850
497.331257	23107.117404	30.746868
498.133746	23135.322466	30.751885
498.707803	23160.674421	30.756903
499.230992	23186.246455	30.761920
500.144632	23208.237963	30.766938
500.681046	23234.391310	30.771956
501.211653	23249.213007	30.776973
501.867783	23278.856422	30.781991
501.938901	23297.043472	30.787008
502.648107	23329.522886	30.792026
502.622100	23374.867839	30.797044
502.595984	23402.962994	30.802061
503.638379	23438.262087	30.807079
503.362819	23479.344683	30.812096
504.135401	23512.163693	30.817114
504.242272	23564.703069	30.822132
504.835778	23608.078375	30.827149
505.167891	23655.381368	30.832167
505.179269	23707.360327	30.837184
505.792137	23746.812016	30.842202
506.197538	23808.672086	30.847220
506.534246	23860.523215	30.852237
507.421034	23918.147097	30.857255
507.717873	23961.700298	30.862272
508.546291	24009.341889	30.867290
509.100691	24052.709245	30.872308
509.948674	24083.343153	30.877325
511.282544	24102.144252	30.882343
511.993844	24129.596939	30.887360
512.939852	24140.525267	30.892378
513.402190	24178.947063	30.897396
513.988348	24188.763694	30.902413
514.236797	24219.361786	30.907431
514.640409	24241.779526	30.912448
515.337633	24254.945936	30.917466
515.482816	24288.283993	30.922484
515.603290	24318.790635	30.927501
516.245042	24347.296505	30.932519
516.242210	24390.927374	30.937536
516.368126	24424.694826	30.942554
516.861693	24468.549957	30.947572
517.508132	24513.773219	30.952589
518.151735	24554.669333	30.957607
518.099552	24610.910799	30.962624
519.567695	24636.670058	30.967642
520.402587	24677.312882	30.972660
521.083529	24701.282962	30.977677
521.889065	24735.278397	30.982695
522.156008	24764.722942	30.987712
522.955133	24783.029707	30.992730
523.174961	24818.980442	30.997748
523.868023	24845.860147	31.002765
524.445446	24870.885996	31.007783
524.820357	24906.785106	31.012800
525.640987	24926.249159	31.017818
525.913284	24961.333202	31.022836
526.153828	24994.350303	31.027853
526.775541	25026.753286	31.032871
527.229622	25068.957481	31.037888
527.501781	25100.900016	31.042906
528.026093	25147.606371	31.047924
528.505239	25181.084503	31.052941
529.011289	25219.668313	31.057959
529.141290	25268.357314	31.062976
529.727701	25310.000009	31.067994
530.840169	25348.707324	31.073012
531.568622	25374.272678	31.078029
532.599697	25387.212415	31.083047
533.807450	25413.266666	31.088064
534.020874	25421.387662	31.093082
534.895883	25444.350787	31.098100
536.006969	25444.132059	31.103117
536.739235	25469.867246	31.108135
536.670534	25478.096546	31.113152
537.110247	25480.103218	31.118170
537.303448	25505.126423	31.123188
537.379153	25524.381260	31.128205
537.594946	25549.056816	31.133223
537.956864	25584.073139	31.138240
538.222678	25601.844406	31.143258
538.672252	25646.132773	31.148276
538.656066	25682.191985	31.153293
539.392935	25708.803703	31.158311
539.515099	25754.041181	31.163328
540.510616	25792.482467	31.168346
540.787267	25833.955525	31.173364
541.414073	25880.305603	31.178381
541.954841	25905.184659	31.183399
542.522276	25958.548297	31.188416
542.637598	26010.800280	31.193434
543.176586	26057.881974	31.198452
543.512110	26098.386573	31.203469
544.295138	26145.076526	31.208487
544.655790	26207.766742	31.213504
545.493501	26253.125822	31.218522
546.066968	26302.164461	31.223540
546.339771	26355.876339	31.228557
547.312948	26400.900283	31.233575
547.413715	26459.547476	31.238592
547.798088	26503.890211	31.243610
548.612200	26562.175768	31.248628
548.972334	26615.756760	31.253645
549.918621	26662.868101	31.258663
550.375493	26721.243792	31.263680
550.982962	26759.230025	31.268698
551.827754	26812.611855	31.273716
552.631764	26868.332203	31.278733
553.578237	26889.619292	31.283751
554.133704	26925.696702	31.288768
555.232526	26950.487950	31.293786
556.086414	26980.851526	31.298804
556.494391	27015.197182	31.303821
557.249478	27032.870308	31.308839
557.441213	27066.388702	31.313856
557.926112	27094.960681	31.318874
558.642310	27126.651037	31.323892
558.925898	27158.623790	31.328909
559.509578	27192.422301	31.333927
559.868454	27230.685613	31.338944
560.574896	27266.302496	31.343962
560.823298	27306.676555	31.348980
561.400426	27335.867249	31.353997
561.910570	27370.164550	31.359015
562.639339	27411.926707	31.364032
563.250495	27436.884233	31.369050
564.322756	27470.202058	31.374068
564.524438	27508.164805	31.379085
565.235948	27537.730327	31.384103
565.509735	27575.620923	31.389120
566.009854	27606.106148	31.394138
566.809146	27645.903904	31.399156
566.647281	27694.728566	31.404173
567.649136	27725.099639	31.409191
568.147555	27767.602506	31.414208
568.053888	27798.773464	31.419226
568.697620	27830.032670	31.424244
568.901281	27879.710149	31.429261
569.546830	27928.043768	31.434279
569.952918	27974.576052	31.439296
570.375676	28026.383863	31.444314
570.412855	28079.100269	31.449332
570.877022	28142.502182	31.454349
571.782061	28189.482741	31.459367
572.307667	28249.000176	31.464384
572.785375	28308.040146	31.469402
573.547647	28358.102832	31.474420
574.287090	28423.099207	31.479437
575.088579	28463.788168	31.484455
575.625637	28521.957361	31.489472
576.583847	28566.907432	31.494490
577.087587	28611.941795	31.499508
577.762918	28668.595434	31.504525
578.708732	28709.326494	31.509543
579.701700	28744.004405	31.514560
580.444534	28786.641395	31.519578
580.800176	28821.406569	31.524596
580.869827	28872.889297	31.529613
581.631331	28898.116576	31.534631
582.494259	28943.449932	31.539648
582.641920	28983.687353	31.544666
583.075807	29038.190729	31.549684
583.341493	29091.599856	31.554701
583.984809	29131.096419	31.559719
584.787868	29198.097755	31.564736
585.139572	29244.759462	31.569754
585.977040	29283.775066	31.574772
586.362830	29349.138355	31.579789
587.059271	29386.815302	31.584807
587.834712	29438.932853	31.589824
588.317145	29485.610661	31.594842
589.301099	29527.321515	31.599860
589.459073	29580.400344	31.604877
590.417177	29616.843426	31.609895
591.274961	29664.927747	31.614912
591.818053	29710.362050	31.619930
592.821623	29750.681755	31.624948
592.780136	29798.380960	31.629965
593.869976	29837.177857	31.634983
594.192575	29886.881637	31.640000
594.730603	29920.819440	31.645018
595.807296	29953.974005	31.650036
596.000246	29994.840188	31.655053
597.439013	30023.158853	31.660071
598.009594	30049.998159	31.665088
598.740429	30077.529467	31.670106
599.590403	30098.502545	31.675124
600.013678	30132.703377	31.680141
600.341843	30163.121530	31.685159
600.617336	30187.651402	31.690176
600.925567	30230.208580	31.695194
601.748692	30252.066786	31.700212
602.197907	30283.108101	31.705229
603.374756	30294.732846	31.710247
604.115702	30304.741001	31.715264
604.313695	30345.017074	31.720282
604.900754	30361.315060	31.725300
605.718188	30402.220341	31.730317
606.210457	30432.159620	31.735335
606.736043	30464.384064	31.740352
607.156259	30502.129654	31.745370
607.619895	30527.492346	31.750388
608.097876	30560.381447	31.755405
608.482922	30590.342520	31.760423
609.086891	30628.050585	31.765440
609.469000	30678.614137	31.770458
609.690346	30718.694576	31.775476
609.847446	30777.769341	31.780493
610.372801	30832.426663	31.785511
610.876631	30894.118247	31.790528
611.436000	30962.960339	31.795546
612.044254	31019.137601	31.800564
612.631075	31086.845800	31.805581
613.392983	31149.103067	31.810599
614.192214	31207.100497	31.815616
614.301448	31277.469316	31.820634
615.592032	31322.685025	31.825652
616.062833	31381.840582	31.830669
616.527945	31441.303401	31.835687
617.545789	31503.401305	31.840704
618.683515	31550.483491	31.845722
619.386787	31592.095840	31.850740
619.711397	31650.349588	31.855757
620.640480	31691.538498	31.860775
621.789652	31723.232383	31.865792
622.172696	31760.434779	31.870810
623.007422	31811.731849	31.875828
623.253782	31858.715114	31.880845
624.136251	31893.648515	31.885863
625.209567	31928.217943	31.890880
626.307713	31949.961710	31.895898
627.193010	31981.114312	31.900916
627.642178	32012.016653	31.905933
627.910151	32049.289857	31.910951
629.037818	32069.507674	31.915968
629.009920	32103.171084	31.920986
630.216195	32129.986681	31.926004
630.646333	32166.386621	31.931021
631.251141	32186.959230	31.936039
632.005633	32220.769678	31.941056
632.201341	32258.008363	31.946074
632.521460	32285.048595	31.951092
632.980293	32326.755032	31.956109
633.080292	32370.523782	31.961127
633.945711	32411.542234	31.966144
634.026814	32458.356576	31.971162
634.466470	32504.658338	31.976180
634.984432	32554.651681	31.981197
635.377984	32610.684554	31.986215
636.041745	32657.421685	31.991232
636.723923	32716.397131	31.996250
638.598168	32732.151731	32.001268
639.404694	32772.572033	32.006285
640.220576	32808.736781	32.011303
640.488881	32856.097606	32.016320
640.802603	32891.095688	32.021338
641.080243	32924.152869	32.026356
642.116620	32975.358778	32.031373
642.432636	33020.799420	32.036391
643.490814	33072.569926	32.041408
643.794684	33125.703757	32.046426
644.534116	33173.625348	32.051444
645.191213	33220.601783	32.056461
645.349906	33267.411255	32.061479
646.098367	33318.456025	32.066496
646.495857	33380.559439	32.071514
646.732563	33437.912538	32.076532
647.573970	33510.945074	32.081549
648.075945	33568.754938	32.086567
648.663363	33632.568768	32.091584
649.086249	33704.821682	32.096602
649.852933	33759.310908	32.101620
650.420545	33833.950717	32.106637
651.296358	33905.423054	32.111655
652.398207	33957.327496	32.116672
653.223174	34026.688181	32.121690
653.880945	34079.574836	32.126708
654.474363	34136.730182	32.131725
655.214988	34195.555294	32.136743
656.180280	34241.689426	32.141760
656.304425	34308.876798	32.146778
657.399234	34369.099908	32.151796
657.975169	34428.774580	32.156813
658.368604	34486.994184	32.161831
659.442288	34542.780846	32.166848
659.637985	34600.883200	32.171866
660.570625	34658.944705	32.176884
662.002542	34720.894459	32.181901
662.167280	34772.649336	32.186919
662.850658	34820.862659	32.191936
663.739358	34876.113932	32.196954
664.190252	34924.550419	32.201972
664.716929	34977.803033	32.206989
665.270763	35037.735996	32.212007
666.349718	35089.445626	32.217024
666.420394	35144.733705	32.222042
666.649132	35213.408878	32.227060
667.693620	35277.368000	32.232077
668.382095	35335.170507	32.237095
668.733948	35382.858215	32.242112
669.775306	35442.623779	32.247130
670.957251	35473.810542	32.252148
672.233364	35506.928657	32.257165
672.691369	35557.903275	32.262183
673.858971	35589.420951	32.267200
674.049673	35630.328773	32.272218
674.659206	35655.825241	32.277236
675.484260	35695.961713	32.282253
675.762214	35746.232283	32.287271
676.330127	35784.254072	32.292288
677.195093	35837.189282	32.297306
677.183686	35883.453898	32.302324
677.709136	35931.915024	32.307341
678.049923	36000.561353	32.312359
678.837905	36052.743380	32.317376
679.260513	36126.669423	32.322394
679.886095	36190.103814	32.327412
680.608302	36263.259425	32.332429
681.121979	36332.455011	32.337447
682.019949	36385.973262	32.342464
682.651161	36458.008925	32.347482
683.322207	36533.680611	32.352500
684.141862	36590.861756	32.357517
684.541188	36671.132200	32.362535
685.452504	36734.371181	32.367552
686.242785	36815.601148	32.372570
686.827862	36884.941267	32.377588
687.814467	36941.302622	32.382605
688.357765	37014.766515	32.387623
689.282804	37076.921637	32.392640
690.444738	37143.442961	32.397658
691.053842	37197.679117	32.402676
692.280541	37244.956679	32.407693
692.470301	37308.286536	32.412711
693.448908	37356.822179	32.417728
694.293907	37420.475787	32.422746
695.293057	37473.897827	32.427764
696.239062	37514.746773	32.432781
697.061949	37558.653592	32.437799
697.377988	37603.755328	32.442816
697.933612	37651.395123	32.447834
698.677063	37699.530029	32.452852
699.459472	37742.235220	32.457869
699.900682	37798.623206	32.462887
700.357093	37847.498987	32.467904
701.075459	37911.902037	32.472922
702.088651	37959.148577	32.477940
702.662683	38004.519617	32.482957
703.239418	38062.596140	32.487975
704.487205	38115.977462	32.492992
704.685155	38174.763203	32.498010
705.419425	38235.736436	32.503028
705.836494	38279.133659	32.508045
706.319227	38346.388121	32.513063
706.752107	38398.309377	32.518080
707.589914	38456.648630	32.523098
707.939044	38512.760999	32.528116
709.798063	38530.897281	32.533133
711.776000	38556.393842	32.538151
712.810835	38579.109843	32.543168
713.546873	38606.422882	32.548186
714.556005	38625.860248	32.553204
715.395374	38643.975593	32.558221
716.444162	38645.904734	32.563239
716.807827	38668.344373	32.568256
717.445284	38665.214124	32.573274
718.057555	38705.368418	32.578292
718.554920	38708.111786	32.583309
718.566893	38744.078852	32.588327
719.333886	38767.087204	32.593344
719.962512	38802.951906	32.598362
720.067826	38848.370602	32.603380
720.910758	38887.529250	32.608397
720.944572	38940.483246	32.613415
721.434399	38980.100346	32.618432
721.957107	39032.140595	32.623450
722.833630	39094.819134	32.628468
723.516209	39154.238445	32.633485
723.700860	39214.813442	32.638503
724.670111	39277.331498	32.643520
725.687044	39350.654151	32.648538
725.657031	39414.076258	32.653556
726.855694	39481.186969	32.658573
727.173604	39550.267222	32.663591
727.507801	39619.951085	32.668608
728.301934	39695.346376	32.673626
728.724703	39772.759786	32.678644
730.080556	39848.949760	32.683661
730.926185	39933.865136	32.688679
731.360835	40009.449568	32.693696
732.183820	40075.401850	32.698714
732.885961	40152.446967	32.703732
733.767756	40225.632068	32.708749
734.230144	40310.245436	32.713767
734.512550	40387.221357	32.718784
735.623490	40467.496952	32.723802
736.221680	40554.695968	32.728820
737.443372	40632.320237	32.733837
737.596687	40713.840688	32.738855
738.724141	40786.891204	32.743872
739.609358	40870.143396	32.748890
739.980191	40939.248163	32.753908
740.885593	41018.970948	32.758925
741.818110	41112.824431	32.763943
742.745232	41180.297220	32.768960
743.819688	41250.652863	32.773978
744.760009	41309.504507	32.778996
746.165137	41367.411618	32.784013
746.722937	41427.377381	32.789031
747.012738	41479.104456	32.794048
748.407631	41533.985979	32.799066
748.637208	41596.313352	32.804084
749.324255	41646.094231	32.809101
750.173678	41694.376105	32.814119
751.062912	41749.395398	32.819136
751.851574	41806.699070	32.824154
752.346327	41861.723120	32.829172
753.394078	41912.787966	32.834189
753.717917	41978.734617	32.839207
754.432753	42043.095811	32.844224
755.353075	42089.936259	32.849242
755.799236	42159.389425	32.854260
756.627645	42218.117864	32.859277
757.035017	42293.059479	32.864295
757.947095	42356.254440	32.869312
758.974187	42411.949868	32.874330
759.512940	42496.844239	32.879348
760.183649	42563.289246	32.884365
760.431156	42634.647436	32.889383
761.181454	42709.020455	32.894400
762.236303	42778.384277	32.899418
762.548028	42863.675995	32.904436
763.596330	42950.496489	32.909453
764.199460	43025.416966	32.914471
764.451932	43103.987980	32.919488
765.630559	43195.498398	32.924506
766.507628	43274.844107	32.929524
767.509194	43347.853572	32.934541
768.480430	43430.338274	32.939559
769.228788	43500.186700	32.944576
770.221350	43584.945093	32.949594
771.237399	43656.052359	32.954612
771.872285	43716.514305	32.959629
772.883243	43785.428339	32.964647
773.749642	43860.035478	32.969664
774.679630	43923.608409	32.974682
775.058763	43995.157613	32.979700
775.901942	44064.950838	32.984717
776.520049	44136.459642	32.989735
776.916264	44217.344251	32.994752
778.121742	44286.719408	32.999770
778.674362	44367.353664	33.004788
779.151279	44445.692872	33.009805
780.039294	44513.850644	33.014823
780.931127	44597.519282	33.019840
781.650733	44675.969448	33.024858
782.045945	44753.913405	33.029876
783.321210	44827.090128	33.034893
784.139186	44915.771734	33.039911
784.694919	45001.647088	33.044928
785.988609	45063.904709	33.049946
787.054322	45140.270132	33.054964
787.822239	45202.706690	33.059981
788.663136	45264.859370	33.064999
789.988562	45316.855385	33.070016
791.583129	45356.764137	33.075034
792.097927	45401.459082	33.080052
793.098669	45432.425293	33.085069
793.785371	45471.176076	33.090087
793.931500	45518.552410	33.095104
794.957254	45558.859029	33.100122
795.756188	45612.774517	33.105140
796.247672	45665.602778	33.110157
797.136482	45723.415961	33.115175
797.495267	45785.864513	33.120192
798.027444	45849.878380	33.125210
798.487797	45910.187738	33.130228
799.012641	45972.510557	33.135245
799.560079	46045.425045	33.140263
800.130628	46134.069444	33.145280
801.149246	46208.618692	33.150298
801.748063	46298.623312	33.155316
802.522301	46374.642535	33.160333
803.064202	46463.009134	33.165351
803.877290	46564.376045	33.170368
804.690896	46644.315189	33.175386
805.115357	46736.947753	33.180404
806.247724	46835.137961	33.185421
806.979624	46921.073895	33.190439
807.897174	47016.756305	33.195456
809.101142	47088.933827	33.200474
810.112323	47178.682457	33.205492
811.843013	47243.806381	33.210509
813.646500	47309.120189	33.215527
814.443359	47371.287274	33.220544
815.671931	47418.107070	33.225562
816.391132	47481.885915	33.230580
817.572882	47517.062969	33.235597
818.402323	47564.311535	33.240615
818.653005	47619.811005	33.245632
819.564971	47661.139592	33.250650
820.510996	47726.437461	33.255668
821.063357	47771.036764	33.260685
821.786951	47827.235945	33.265703
822.177514	47886.931805	33.270720
822.638943	47943.640512	33.275738
823.198850	48013.799922	33.280756
823.913383	48092.549244	33.285773
824.351535	48166.122195	33.290791
824.852649	48250.925515	33.295808
826.190926	48329.850072	33.300826
826.656495	48410.241509	33.305844
827.728859	48499.998461	33.310861
828.512152	48571.138665	33.315879
829.498347	48641.776920	33.320896
830.542661	48714.502731	33.325914
831.448786	48801.769067	33.330932
831.624254	48876.160394	33.335949
832.735122	48948.294514	33.340967
834.412408	49002.157532	33.345984
836.012929	49049.230295	33.351002
836.809338	49098.639269	33.356020
837.915722	49151.684502	33.361037
838.583714	49190.414427	33.366055
838.671425	49243.918662	33.371072
839.476297	49297.015936	33.376090
839.830632	49362.357514	33.381108
840.087995	49438.531068	33.386125
840.706170	49509.526120	33.391143
841.152653	49588.163195	33.396160
842.351876	49663.266618	33.401178
842.862931	49751.192409	33.406196
843.208183	49831.749333	33.411213
844.161009	49920.421484	33.416231
845.089293	50019.705237	33.421248
845.674325	50120.292830	33.426266
846.611030	50220.763852	33.431284
847.142753	50318.228110	33.436301
848.471667	50408.259516	33.441319
848.951524	50512.904079	33.446336
849.711348	50603.754066	33.451354
851.132385	50693.865778	33.456372
852.021581	50794.474245	33.461389
853.129200	50881.835447	33.466407
853.964333	50973.103860	33.471424
854.698286	51064.118363	33.476442
855.690166	51154.413107	33.481460
856.621487	51249.362256	33.486477
857.633015	51335.686865	33.491495
858.300686	51433.638828	33.496512
859.079350	51529.000871	33.501530
859.964891	51624.648334	33.506548
860.781682	51725.987919	33.511565
862.058563	51812.401858	33.516583
862.651291	51911.518922	33.521600
863.059955	52009.606572	33.526618
863.866728	52103.570292	33.531636
864.687740	52211.198186	33.536653
866.020302	52307.296817	33.541671
866.647189	52407.528848	33.546688
867.578538	52504.297387	33.551706
868.666969	52597.520218	33.556724
869.469402	52705.792142	33.561741
870.745518	52793.632144	33.566759
872.195435	52879.509351	33.571776
873.547281	52954.814101	33.576794
875.010764	53028.981659	33.581812
876.044426	53092.039476	33.586829
877.490349	53153.131350	33.591847
877.644561	53222.026816	33.596864
878.516609	53283.988237	33.601882
879.648500	53341.103277	33.606900
879.882944	53414.800382	33.611917
880.551141	53475.590476	33.616935
881.409735	53549.471839	33.621952
882.172497	53605.203907	33.626970
883.155160	53677.377432	33.631988
883.907555	53745.306617	33.637005
884.297395	53819.155533	33.642023
884.893052	53900.513992	33.647040
885.594632	53974.499656	33.652058
886.685760	54041.240790	33.657076
887.693217	54125.859621	33.662093
888.556366	54193.859836	33.667111
889.795772	54282.136100	33.672128
890.878103	54360.007250	33.677146
891.951240	54422.190546	33.682164
893.031475	54478.433075	33.687181
894.230935	54539.034340	33.692199
894.654516	54611.774616	33.697216
895.581950	54687.019631	33.702234
896.408324	54753.625254	33.707252
897.111886	54843.423869	33.712269
897.963363	54923.099761	33.717287
898.649978	55008.636685	33.722304
899.382774	55079.783863	33.727322
900.607558	55155.586353	33.732340
901.417628	55238.765055	33.737357
902.723425	55314.055063	33.742375
903.718874	55381.783913	33.747392
904.774546	55463.670296	33.752410
905.417349	55544.995803	33.757428
906.115137	55627.588709	33.762445
907.367999	55702.251004	33.767463
907.814322	55784.799156	33.772480
908.342605	55871.630746	33.777498
909.085470	55953.060840	33.782516
909.582591	56057.801279	33.787533
910.791407	56138.533027	33.792551
911.585324	56243.703881	33.797568
912.482555	56338.272487	33.802586
913.824045	56415.525881	33.807604
914.875413	56507.079766	33.812621
916.318303	56584.986317	33.817639
917.404079	56669.924812	33.822656
918.410833	56739.406838	33.827674
919.707850	56817.156004	33.832692
920.207611	56900.331548	33.837709
921.322233	56969.637904	33.842727
922.427128	57059.782174	33.847744
923.139879	57139.844541	33.852762
923.760445	57219.095126	33.857780
924.504337	57305.327203	33.862797
925.446558	57381.982795	33.867815
926.125790	57473.604807	33.872832
926.945185	57562.081225	33.877850
927.779984	57657.020625	33.882868
928.020613	57756.233365	33.887885
928.654219	57849.078313	33.892903
929.675687	57938.987997	33.897920
930.420549	58033.407366	33.902938
930.932366	58125.604518	33.907956
931.780955	58222.591894	33.912973
933.072007	58325.887243	33.917991
933.557432	58432.613869	33.923008
934.482076	58541.111320	33.928026
935.637986	58644.298711	33.933044
936.209275	58756.314965	33.938061
937.392381	58860.288821	33.943079
939.102623	58955.577351	33.948096
941.182127	59028.751540	33.953114
942.668840	59098.936874	33.958132
943.893055	59178.666888	33.963149
944.995033	59245.113764	33.968167
946.185367	59305.629841	33.973184
947.313834	59363.047054	33.978202
948.021895	59424.594137	33.983220
949.158509	59499.005970	33.988237
949.838808	59568.180704	33.993255
950.656265	59641.838695	33.998272
950.765764	59714.847089	34.003290
951.934905	59792.718065	34.008308
952.244177	59878.359195	34.013325
953.142768	59966.415356	34.018343
953.826203	60046.247692	34.023360
954.509399	60155.288090	34.028378
955.475415	60247.113660	34.033396
956.304417	60359.562303	34.038413
957.050715	60457.930461	34.043431
957.826478	60563.733596	34.048448
958.900775	60680.598138	34.053466
959.916520	60786.367644	34.058484
960.353637	60904.575141	34.063501
961.982688	61012.528939	34.068519
962.790562	61124.517636	34.073536
963.571344	61246.315429	34.078554
964.415868	61347.812549	34.083572
965.255204	61474.001087	34.088589
966.094045	61583.641861	34.093607
967.491060	61695.703438	34.098624
968.668520	61821.248329	34.103642
969.804667	61920.631305	34.108660
970.912428	62036.113459	34.113677
972.109103	62131.302431	34.118695
973.529921	62224.045047	34.123712
974.577080	62331.877834	34.128730
975.696691	62424.489612	34.133748
976.383692	62521.986453	34.138765
977.178138	62622.708234	34.143783
978.724714	62708.458975	34.148800
979.062172	62809.493812	34.153818
980.249978	62900.907604	34.158836
980.892581	63010.899290	34.163853
982.012067	63111.782710	34.168871
982.908883	63205.675150	34.173888
983.821810	63296.638349	34.178906
985.075765	63380.507563	34.183924
985.896724	63470.772927	34.188941
986.394067	63566.600292	34.193959
987.824591	63665.663059	34.198976
988.297272	63763.290919	34.203994
989.691428	63862.834982	34.209012
990.266616	63962.051949	34.214029
991.362546	64062.988259	34.219047
992.322025	64161.862205	34.224064
993.170552	64265.225204	34.229082
993.994934	64377.133781	34.234100
995.156015	64480.684553	34.239117
995.739770	64599.646588	34.244135
996.874086	64703.702483	34.249152
997.447624	64814.436196	34.254170
998.260155	64940.169850	34.259188
999.624357	65064.558002	34.264205
1001.250255	65175.979544	34.269223
1003.093348	65274.878122	34.274240
1003.813886	65379.608831	34.279258
1005.704295	65462.795759	34.284276
1006.764338	65541.339239	34.289293
1007.811265	65638.163064	34.294311
1009.329146	65706.614216	34.299328
1011.694081	65749.700676	34.304346
1013.645094	65817.331984	34.309364
1014.631863	65871.054993	34.314381
1015.335522	65926.988879	34.319399
1016.648011	65974.074756	34.324416
1017.130236	66039.189075	34.329434
1018.025727	66090.753357	34.334452
1019.078972	66147.019957	34.339469
1019.592799	66206.660446	34.344487
1020.551144	66255.818147	34.349504
1020.721915	66331.703339	34.354522
1021.764453	66409.829446	34.359540
1022.222873	66509.432482	34.364557
1022.714477	66598.351425	34.369575
1023.675772	66687.550702	34.374592
1023.896576	66800.397444	34.379610
1024.804041	66900.159358	34.384628
1025.404854	67006.195809	34.389645
1026.233758	67136.681775	34.394663
1027.254147	67247.781667	34.399680
1027.887643	67369.393704	34.404698
1029.451359	67488.103022	34.409716
1031.411794	67587.226282	34.414733
1032.779927	67691.263176	34.419751
1033.796286	67796.031047	34.424768
1034.749414	67900.272807	34.429786
1036.042044	68001.971994	34.434804
1037.209229	68099.304952	34.439821
1038.319639	68176.553349	34.444839
1039.711230	68248.986267	34.449856
1040.532947	68329.642214	34.454874
1041.892426	68403.706197	34.459892
1042.548428	68492.996928	34.464909
1043.542008	68580.111957	34.469927
1044.360038	68659.252213	34.474944
1045.039632	68755.855957	34.479962
1045.772386	68840.531673	34.484980
1046.967968	68930.459008	34.489997
1047.574217	69037.130613	34.495015
1048.708906	69150.004000	34.500032
1049.512502	69265.483000	34.505050
1050.261115	69373.295398	34.510068
1051.516258	69491.986473	34.515085
1051.855755	69611.840425	34.520103
1052.738014	69724.791667	34.525120
1053.377721	69859.923821	34.530138
1054.765584	69988.143486	34.535156
1055.503135	70126.144113	34.540173
1056.212840	70273.395614	34.545191
1057.737787	70404.616998	34.550208
1058.594134	70533.632843	34.555226
1059.699747	70675.052012	34.560244
1060.686735	70819.217993	34.565261
1061.930922	70954.316707	34.570279
1063.573168	71087.065167	34.575296
1064.437302	71232.311021	34.580314
1065.921633	71357.132625	34.585332
1067.367521	71492.762986	34.590349
1067.874977	71632.045770	34.595367
1068.765359	71752.791127	34.600384
1070.350060	71877.838847	34.605402
1071.158687	72013.929395	34.610420
1073.077907	72132.261923	34.615437
1074.963121	72243.707476	34.620455
1076.265856	72349.997850	34.625472
1077.538934	72465.723380	34.630490
1078.611993	72564.717914	34.635508
1079.473959	72671.369917	34.640525
1080.407681	72784.195427	34.645543
1081.266245	72887.357987	34.650560
1082.442038	73005.752969	34.655578
1083.197760	73115.309283	34.660596
1084.291380	73228.027477	34.665613
1085.146817	73356.003959	34.670631
1086.322400	73466.343948	34.675648
1087.993914	73576.137877	34.680666
1089.592270	73670.923790	34.685684
1091.552985	73770.575006	34.690701
1092.780904	73868.638146	34.695719
1093.784686	73961.705597	34.700736
1094.689425	74049.300493	34.705754
1095.566708	74145.628664	34.710772
1096.610087	74226.515209	34.715789
1097.841166	74322.334511	34.720807
1099.197061	74395.831337	34.725824
1100.426121	74457.054531	34.730842
1101.273522	74533.358585	34.735860
1102.828412	74605.917576	34.740877
1103.506897	74681.504721	34.745895
1104.569432	74755.495721	34.750912
1105.367757	74836.831257	34.755930
1105.929960	74920.231527	34.760948
1107.054162	75014.193594	34.765965
1107.576483	75119.543054	34.770983
1108.689481	75212.457915	34.776000
1109.413008	75317.666337	34.781018
1110.063096	75431.110549	34.786036
1111.311061	75535.743170	34.791053
1112.206993	75658.083953	34.796071
1113.301887	75785.616013	34.801088
1114.412143	75909.369965	34.806106
1115.047286	76040.119549	34.811124
1116.483873	76154.040007	34.816141
1117.506648	76271.245205	34.821159
1118.985853	76399.695409	34.826176
1120.033502	76520.857384	34.831194
1120.889197	76661.497512	34.836212
1122.138341	76778.268099	34.841229
1122.870419	76917.450817	34.846247
1123.897899	77043.951544	34.851264
1125.292377	77196.053365	34.856282
1126.417267	77324.069802	34.861300
1127.559954	77456.891482	34.866317
1128.643837	77586.516844	34.871335
1130.200445	77709.483170	34.876352
1132.777934	77820.186689	34.881370
1133.769694	77944.769212	34.886388
1134.887653	78049.454808	34.891405
1136.015367	78160.705541	34.896423
1136.972036	78276.895061	34.901440
1138.133852	78385.901670	34.906458
1139.238590	78517.002764	34.911476
1139.896022	78635.959229	34.916493
1140.892207	78755.269515	34.921511
1141.835223	78886.337171	34.926528
1143.073044	79011.452787	34.931546
1143.908404	79147.734173	34.936564
1145.085502	79288.285022	34.941581
1146.253332	79416.824702	34.946599
1147.604874	79546.301582	34.951616
1148.848342	79675.443426	34.956634
1149.668572	79810.396505	34.961652
1151.071890	79930.687104	34.966669
1151.842783	80077.689408	34.971687
1153.074518	80205.570965	34.976704
1154.155884	80355.001884	34.981722
1154.963359	80495.528551	34.986740
1156.288034	80627.407608	34.991757
1157.701927	80761.284026	34.996775
1159.334472	80878.636427	35.001792
1160.833708	80987.762208	35.006810
1161.834013	81103.281701	35.011828
1162.969373	81199.152974	35.016845
1163.970325	81327.510521	35.021863
1164.775605	81443.368798	35.026880
1166.001025	81562.363453	35.031898
1167.192841	81688.330407	35.036916
1169.262307	81793.332141	35.041933
1170.440575	81895.582853	35.046951
1171.356882	82016.537194	35.051968
1172.888673	82126.162632	35.056986
1173.695641	82240.575731	35.062004
1175.218694	82352.082876	35.067021
1175.989159	82472.248373	35.072039
1176.640632	82599.597210	35.077056
1177.653280	82721.759881	35.082074
1178.435539	82862.900042	35.087092
1179.645428	82991.148798	35.092109
1180.794488	83139.377654	35.097127
1181.510964	83277.292009	35.102144
1183.160143	83410.403198	35.107162
1184.326812	83545.147973	35.112180
1185.745645	83675.693218	35.117197
1187.326784	83817.056727	35.122215
1188.594658	83950.052781	35.127232
1190.270450	84081.220693	35.132250
1190.647478	84219.591036	35.137268
1191.472933	84352.589190	35.142285
1192.356415	84510.553502	35.147303
1193.368419	84663.694132	35.152320
1195.080710	84803.819895	35.157338
1195.802145	84961.764361	35.162356
1197.364076	85109.118725	35.167373
1198.577377	85258.818063	35.172391
1199.940834	85404.544022	35.177408
1201.382346	85548.359133	35.182426
1202.674344	85689.346790	35.187444
1203.870758	85828.832925	35.192461
1204.835606	85982.933077	35.197479
1205.756673	86137.105008	35.202496
1207.251761	86289.768492	35.207514
1208.212021	86435.209126	35.212532
1209.380703	86593.189173	35.217549
1210.670490	86747.017172	35.222567
1212.274747	86905.487942	35.227584
1213.376352	87042.947072	35.232602
1214.743240	87192.739919	35.237620
1216.142185	87346.856870	35.242637
1217.404711	87489.277833	35.247655
1218.833113	87615.729732	35.252672
1220.298318	87752.877566	35.257690
1221.569388	87897.489177	35.262708
1223.446609	88013.506459	35.267725
1224.696525	88141.580178	35.272743
1226.049535	88263.441155	35.277760
1227.311809	88373.787376	35.282778
1228.370557	88474.511297	35.287796
1229.881140	88574.253276	35.292813
1230.832542	88686.388235	35.297831
1231.851680	88800.942388	35.302848
1232.962208	88916.183944	35.307866
1234.117866	89035.120720	35.312884
1235.117603	89152.059525	35.317901
1236.526236	89281.903233	35.322919
1237.417442	89404.494603	35.327936
1238.912763	89524.521191	35.332954
1240.098639	89649.740533	35.337972
1241.134585	89780.891217	35.342989
1242.236832	89907.335062	35.348007
1243.262386	90034.109152	35.353024
1244.805043	90168.206849	35.358042
1245.444475	90315.143656	35.363060
1246.830729	90448.459536	35.368077
1248.189205	90589.211485	35.373095
1249.383557	90743.106708	35.378112
1250.620077	90878.469633	35.383130
1251.758145	91021.768242	35.388148
1253.172973	91164.602571	35.393165
1254.005010	91316.639288	35.398183
1254.999954	91464.629820	35.403200
1256.338289	91606.713957	35.408218
1257.110457	91776.853642	35.413236
1258.712093	91932.553863	35.418253
1260.346300	92086.040441	35.423271
1261.278787	92257.858698	35.428288
1262.963548	92403.812574	35.433306
1264.048456	92560.858527	35.438324
1265.029962	92735.893594	35.443341
1266.207711	92899.894969	35.448359
1266.978341	93061.289568	35.453376
1268.374595	93227.180008	35.458394
1269.501413	93410.601175	35.463412
1270.957181	93585.561069	35.468429
1272.448169	93750.843775	35.473447
1273.517410	93929.081621	35.478464
1275.331205	94079.435417	35.483482
1277.275086	94244.466636	35.488500
1279.077705	94396.406821	35.493517
1281.165854	94539.499937	35.498535
1282.357341	94688.172468	35.503552
1283.707356	94813.959771	35.508570
1284.291851	94961.636352	35.513588
1285.485551	95098.966862	35.518605
1286.911154	95242.557253	35.523623
1288.366906	95400.931393	35.528640
1289.734058	95531.897738	35.533658
1291.165892	95668.513238	35.538676
1292.115320	95804.439724	35.543693
1293.504453	95954.250772	35.548711
1294.433050	96091.176287	35.553728
1295.692842	96221.848072	35.558746
1297.315970	96344.779131	35.563764
1299.029995	96473.310640	35.568781
1300.431947	96580.428423	35.573799
1301.771291	96701.985370	35.578816
1303.712153	96811.227680	35.583834
1305.342723	96918.991501	35.588852
1307.169234	97015.782403	35.593869
1308.480051	97117.625416	35.598887
1309.640089	97225.793969	35.603904
1310.829493	97326.892559	35.608922
1311.475948	97442.595209	35.613940
1313.164014	97547.338295	35.618957
1314.791297	97646.014381	35.623975
1315.240183	97770.856441	35.628992
1316.626909	97887.447377	35.634010
1317.293981	98010.005704	35.639028
1318.408950	98133.007111	35.644045
1319.849490	98263.886415	35.649063
1320.800270	98411.761044	35.654080
1321.651434	98552.891745	35.659098
1322.565105	98705.624204	35.664116
1323.349648	98859.069798	35.669133
1324.509070	99020.125820	35.674151
1325.335807	99197.093781	35.679168
1326.632535	99376.154217	35.684186
1327.931858	99550.656739	35.689204
1328.750658	99725.147721	35.694221
1330.238337	99916.753777	35.699239
1331.707935	100104.704636	35.704256
1332.985476	100280.640453	35.709274
1334.680294	100473.380219	35.714292
1335.742909	100660.239731	35.719309
1337.473955	100836.196671	35.724327
1338.500362	101034.424442	35.729344
1340.307991	101221.103477	35.734362
1341.814054	101398.597078	35.739380
1343.222334	101576.678511	35.744397
1345.016615	101754.112534	35.749415
1346.177363	101932.200770	35.754432
1347.568467	102108.503108	35.759450
1348.404302	102287.143282	35.764468
1350.176969	102460.077257	35.769485
1352.266401	102620.863462	35.774503
1353.685212	102803.612011	35.779520
1355.283323	102973.134452	35.784538
1356.948277	103135.604891	35.789556
1358.247693	103306.421759	35.794573
1359.175541	103464.916961	35.799591
1360.503017	103635.490520	35.804608
1361.962339	103796.404424	35.809626
1363.694742	103965.606291	35.814644
1364.300488	104137.636471	35.819661
1366.399091	104280.953094	35.824679
1367.503117	104438.740035	35.829696
1368.992224	104592.611676	35.834714
1370.532262	104739.370083	35.839732
1371.414783	104888.673653	35.844749
1372.800946	105030.241741	35.849767
1374.132368	105188.830143	35.854784
1375.456937	105334.767432	35.859802
1376.482445	105498.134407	35.864820
1377.602889	105668.984427	35.869837
1379.117396	105829.255203	35.874855
1380.217315	105994.449054	35.879872
1381.668243	106169.083550	35.884890
1383.449078	106336.556884	35.889908
1384.495934	106498.583657	35.894925
1386.026717	106666.342503	35.899943
1387.301818	106841.201450	35.904960
1388.949002	107014.807175	35.909978
1390.931807	107184.987212	35.914996
1391.820756	107349.554133	35.920013
1393.109869	107511.368175	35.925031
1394.442823	107702.841776	35.930048
1395.658026	107862.935184	35.935066
1397.585033	108040.996397	35.940084
1398.697938	108216.195981	35.945101
1400.229588	108384.700010	35.950119
1401.493681	108571.035902	35.955136
1402.852164	108753.341315	35.960154
1404.075579	108931.617437	35.965172
1405.164499	109124.675557	35.970189
1406.836131	109292.451827	35.975207
1407.992221	109489.884054	35.980224
1409.526143	109680.551701	35.985242
1411.090245	109871.304178	35.990260
1412.291775	110062.196039	35.995277
1413.926455	110254.585937	36.000295
1415.608248	110451.935071	36.005312
1416.910592	110627.345627	36.010330
1418.517853	110819.820157	36.015348
1419.889137	111009.308632	36.020365
1421.533893	111198.042151	36.025383
1423.016820	111373.869914	36.030400
1424.938203	111544.733601	36.035418
1427.383958	111715.850647	36.040436
1429.295443	111877.647179	36.045453
1430.810739	112023.904267	36.050471
1432.459297	112170.050629	36.055488
1434.315413	112300.135806	36.060506
1436.114854	112431.802264	36.065524
1437.126959	112582.354555	36.070541
1438.823464	112728.584308	36.075559
1440.021127	112871.593495	36.080576
1441.113921	113025.390373	36.085594
1442.430215	113167.253178	36.090612
1443.520268	113318.277501	36.095629
1444.823424	113459.548554	36.100647
1445.956969	113610.871069	36.105664
1447.005003	113750.312123	36.110682
1448.706546	113895.014020	36.115700
1449.507691	114034.486056	36.120717
1450.720579	114190.549292	36.125735
1452.085012	114343.001832	36.130752
1453.194913	114506.686443	36.135770
1454.771085	114678.489791	36.140788
1455.897776	114839.905480	36.145805
1457.337952	115013.343241	36.150823
1458.405502	115194.004602	36.155840
1459.562610	115371.370120	36.160858
1461.587007	115539.858292	36.165876
1462.479094	115736.910788	36.170893
1463.964886	115919.836535	36.175911
1465.778273	116114.212466	36.180928
1466.957579	116303.591860	36.185946
1468.502961	116478.262208	36.190964
1469.714083	116689.382066	36.195981
1471.443932	116882.738442	36.200999
1473.071509	117070.436903	36.206016
1474.625138	117262.799603	36.211034
1475.917096	117452.813467	36.216052
1477.120269	117658.429679	36.221069
1478.521458	117866.205633	36.226087
1480.270048	118074.392462	36.231104
1481.401968	118286.196386	36.236122
1482.999105	118487.024442	36.241140
1484.327650	118699.950842	36.246157
1485.568545	118914.376411	36.251175
1487.203549	119128.381275	36.256192
1488.777523	119344.907234	36.261210
1490.532197	119559.845165	36.266228
1492.028064	119776.260931	36.271245
1493.260970	119995.815368	36.276263
1494.896062	120212.463942	36.281280
1496.250921	120425.144820	36.286298
1497.536028	120640.006196	36.291316
1499.067662	120873.747500	36.296333
1501.198073	121069.255261	36.301351
1503.110677	121282.150951	36.306368
1505.388122	121479.334419	36.311386
1507.641387	121655.168997	36.316404
1509.753238	121835.363064	36.321421
1511.249496	122006.576780	36.326439
1513.397509	122177.870033	36.331456
1514.964705	122361.785060	36.336474
1516.753619	122528.908821	36.341492
1517.753778	122704.000791	36.346509
1518.571656	122871.089843	36.351527
1520.258316	123038.145201	36.356544
1521.599828	123222.433601	36.361562
1523.255694	123398.051057	36.366580
1524.764444	123565.646722	36.371597
1526.657293	123741.301650	36.376615
1528.185241	123887.616063	36.381632
1529.078011	124049.603775	36.386650
1530.405944	124209.844874	36.391668
1531.774357	124376.379022	36.396685
1533.075873	124552.203180	36.401703
1534.302966	124712.261372	36.406720
1535.522239	124902.068867	36.411738
1537.025896	125080.092172	36.416756
1538.341080	125270.607978	36.421773
1539.756579	125446.823332	36.426791
1541.227053	125628.518487	36.431808
1542.878954	125832.123942	36.436826
1544.563184	126009.766807	36.441844
1546.989378	126183.785401	36.446861
1549.305560	126353.374826	36.451879
1550.766680	126521.920033	36.456896
1552.162976	126705.129862	36.461914
1554.107107	126865.165213	36.466932
1555.483768	127042.030035	36.471949
1556.823542	127216.912118	36.476967
1558.413105	127395.136805	36.481984
1559.228703	127585.638204	36.487002
1560.890690	127772.319963	36.492020
1561.970771	127964.857214	36.497037
1563.111625	128159.641545	36.502055
1564.946852	128358.085684	36.507072
1566.278556	128570.890439	36.512090
1567.750807	128765.127425	36.517108
1568.986314	128979.954212	36.522125
1570.361564	129204.709416	36.527143
1572.036288	129407.776405	36.532160
1573.616271	129620.494998	36.537178
1575.732815	129830.930152	36.542196
1577.736347	130041.601533	36.547213
1579.375300	130255.442479	36.552231
1581.470174	130443.422271	36.557248
1583.131967	130649.896735	36.562266
1584.695131	130848.301518	36.567284
1586.258388	131042.207169	36.572301
1587.232722	131259.058871	36.577319
1589.022018	131454.386181	36.582336
1590.466201	131666.127374	36.587354
1592.120976	131873.650392	36.592372
1593.578983	132087.331597	36.597389
1595.345969	132302.457276	36.602407
1597.169605	132511.197859	36.607424
1598.248418	132732.389914	36.612442
1599.904677	132942.176102	36.617460
1601.333105	133161.739190	36.622477
1602.611113	133384.207371	36.627495
1604.030853	133601.733738	36.632512
1605.124521	133826.835440	36.637530
1607.187401	134049.896458	36.642548
1608.661462	134278.841022	36.647565
1610.491498	134511.098695	36.652583
1611.825124	134726.948295	36.657600
1613.304244	134943.027969	36.662618
1614.855452	135150.082229	36.667636
1616.276962	135369.242740	36.672653
1617.562982	135590.101466	36.677671
1619.245705	135809.169443	36.682688
1620.962616	136039.124196	36.687706
1622.678192	136259.546133	36.692724
1624.653605	136483.855571	36.697741
1626.440325	136699.221931	36.702759
1628.617396	136909.400451	36.707776
1630.500499	137132.677612	36.712794
1632.195407	137334.179852	36.717812
1634.025632	137549.962594	36.722829
1635.658636	137750.438173	36.727847
1637.486618	137960.429338	36.732864
1639.282250	138176.310720	36.737882
1641.182977	138375.450825	36.742900
1642.710013	138585.725556	36.747917
1644.015770	138803.305050	36.752935
1646.408355	138997.406740	36.757952
1647.981134	139199.752381	36.762970
1649.715408	139400.943040	36.767988
1651.491466	139597.359947	36.773005
1653.199706	139800.586222	36.778023
1655.203255	139973.875485	36.783040
1657.443405	140159.590009	36.788058
1659.386638	140349.604303	36.793076
1660.797697	140539.710690	36.798093
1662.433268	140732.835734	36.803111
1664.118645	140909.214767	36.808128
1665.453737	141099.679573	36.813146
1667.079039	141302.624447	36.818164
1668.458328	141490.788575	36.823181
1669.570938	141701.749054	36.828199
1670.953816	141907.237047	36.833216
1672.577153	142123.185088	36.838234
1674.754456	142313.271401	36.843252
1676.721120	142515.860489	36.848269
1678.364572	142718.417263	36.853287
1680.239673	142922.901178	36.858304
1681.986177	143128.790554	36.863322
1683.332742	143340.747937	36.868340
1684.733471	143531.848655	36.873357
1686.211725	143755.351631	36.878375
1687.649816	143968.577916	36.883392
1688.804526	144197.135626	36.888410
1690.341604	144425.959091	36.893428
1692.039811	144650.381126	36.898445
1693.541046	144884.375215	36.903463
1695.687152	145115.546482	36.908480
1696.972618	145348.223476	36.913498
1698.299391	145589.747184	36.918516
1700.195113	145818.835110	36.923533
1701.585101	146055.011759	36.928551
1703.641926	146257.783973	36.933568
1706.010050	146481.367056	36.938586
1707.724666	146689.476198	36.943604
1709.635944	146906.392799	36.948621
1710.677306	147119.882930	36.953639
1712.430824	147326.910956	36.958656
1714.179446	147540.903968	36.963674
1715.854447	147749.457066	36.968692
1717.805672	147955.795245	36.973709
1719.287680	148187.454537	36.978727
1720.981141	148408.577276	36.983744
1722.479120	148633.831508	36.988762
1723.994974	148863.333002	36.993780
1725.627381	149101.111009	36.998797
1726.981346	149334.815965	37.003815
1728.573143	149566.807420	37.008832
1730.728142	149807.303559	37.013850
1732.396553	150047.301013	37.018868
1734.246049	150282.626664	37.023885
1735.571488	150529.065864	37.028903
1736.899948	150779.920211	37.033920
1739.185259	151036.929232	37.038938
1741.070318	151292.283385	37.043956
1742.866737	151539.688602	37.048973
1744.698743	151799.228349	37.053991
1746.632000	152036.998511	37.059008
1748.617960	152288.282924	37.064026
1750.091006	152554.180706	37.069044
1752.028924	152800.123691	37.074061
1753.762974	153052.306005	37.079079
1755.942474	153305.530008	37.084096
1757.490889	153555.730407	37.089114
1758.846412	153812.536287	37.094132
1760.866016	154061.504936	37.099149
1762.226147	154326.368466	37.104167
1763.792448	154582.813461	37.109184
1765.716133	154856.781001	37.114202
1767.066133	155126.002693	37.119220
1768.897901	155382.610379	37.124237
1770.513862	155663.575123	37.129255
1772.325156	155941.222789	37.134272
1773.837580	156223.782190	37.139290
1775.613510	156495.819872	37.144308
1777.736180	156766.391905	37.149325
1779.462813	157061.213279	37.154343
1781.752182	157334.678383	37.159360
1783.517501	157608.552128	37.164378
1785.535176	157879.771131	37.169396
1787.928957	158138.418710	37.174413
1789.751831	158403.128265	37.179431
1791.777129	158657.744380	37.184448
1794.066100	158904.755671	37.189466
1795.458219	159166.410174	37.194484
1797.288277	159414.517943	37.199501
1799.293347	159677.123797	37.204519
1801.180593	159911.218343	37.209536
1802.868520	160139.715226	37.214554
1804.446265	160370.376328	37.219572
1806.410568	160592.637054	37.224589
1807.898624	160839.593771	37.229607
1809.240532	161073.369377	37.234624
1810.718915	161314.938381	37.239642
1812.417194	161567.128646	37.244660
1814.395334	161807.320816	37.249677
1816.214792	162069.262751	37.254695
1817.942007	162321.680884	37.259712
1820.024140	162563.305896	37.264730
1821.483650	162825.098310	37.269748
1823.445662	163073.915379	37.274765
1825.471688	163332.657650	37.279783
1827.475626	163581.470451	37.284800
1829.252114	163835.195841	37.289818
1830.815905	164099.071624	37.294836
1833.060153	164359.736634	37.299853
1834.545500	164626.052469	37.304871
1836.324577	164875.596246	37.309888
1838.628483	165140.239843	37.314906
1839.974610	165409.286863	37.319924
1842.360565	165665.177085	37.324941
1844.185919	165936.797246	37.329959
1845.794274	166205.360095	37.334976
1847.506249	166474.135223	37.339994
1849.458326	166748.847402	37.345012
1851.064151	167016.514596	37.350029
1853.423014	167290.805184	37.355047
1855.305175	167565.204351	37.360064
1857.307494	167836.513802	37.365082
1858.971580	168115.559799	37.370100
1861.001514	168381.588967	37.375117
1862.784496	168648.232947	37.380135
1864.411707	168921.922465	37.385152
1866.031661	169197.975122	37.390170
1867.561807	169479.514067	37.395188
1869.636780	169762.205116	37.400205
1871.657604	170050.668357	37.405223
1873.521749	170338.538363	37.410240
1875.639649	170619.082622	37.415258
1877.672539	170907.599809	37.420276
1879.399580	171188.468107	37.425293
1881.324750	171461.575782	37.430311
1883.349672	171750.759342	37.435328
1885.454275	172022.532421	37.440346
1887.219018	172309.086172	37.445364
1889.004411	172585.269880	37.450381
1891.090328	172861.987530	37.455399
1893.427108	173150.250488	37.460416
1895.461939	173425.063782	37.465434
1897.430167	173707.314180	37.470452
1899.957866	173974.152525	37.475469
1901.725749	174224.458985	37.480487
1903.665983	174470.993367	37.485504
1905.668269	174707.276613	37.490522
1907.316975	174946.134325	37.495540
1909.190341	175175.347471	37.500557
1911.325655	175412.093580	37.505575
1913.508405	175639.111103	37.510592
1915.600042	175855.382905	37.515610
1917.099314	176092.647150	37.520628
1919.010914	176328.242846	37.525645
1920.692131	176573.651584	37.530663
1922.519323	176805.722979	37.535680
1924.698402	177042.583482	37.540698
1925.993365	177300.664678	37.545716
1927.962450	177553.174369	37.550733
1929.984877	177805.942707	37.555751
1931.400366	178074.693765	37.560768
1932.898185	178333.570417	37.565786
1934.544430	178612.374967	37.570804
1936.091066	178882.833901	37.575821
1938.028754	179170.095338	37.580839
1939.773380	179458.635217	37.585856
1941.333807	179750.850898	37.590874
1942.927756	180058.623412	37.595892
1944.594095	180364.849531	37.600909
1946.343652	180682.118434	37.605927
1947.846443	181004.026177	37.610944
1950.068125	181327.780261	37.615962
1951.989216	181655.954037	37.620980
1953.908779	181972.516045	37.625997
1955.740967	182308.692809	37.631015
1957.674389	182650.490045	37.636032
1960.027139	182974.663063	37.641050
1962.320328	183312.264906	37.646068
1964.279468	183641.256418	37.651085
1966.427187	183976.005796	37.656103
1968.099382	184292.458402	37.661120
1970.634607	184680.851686	37.666138
1972.937169	185028.934441	37.671156
1974.657770	185349.091218	37.676173
1977.094118	185673.379776	37.681191
1979.437247	185982.212347	37.686208
1982.102843	186285.621908	37.691226
1984.008266	186598.150401	37.696244
1986.292096	186896.347774	37.701261
1988.755190	187205.153656	37.706279
1990.395924	187519.268342	37.711296
1992.519752	187812.800912	37.716314
1994.987387	188115.441410	37.721332
1996.928234	188412.791148	37.726349
1999.091242	188696.470580	37.731367
2001.083791	188985.093269	37.736384
2003.065951	189292.278523	37.741402
2004.741667	189591.113930	37.746420
2007.030685	189880.096419	37.751437
2008.857061	190157.835723	37.756455
2010.615574	190434.470755	37.761472
2012.851109	190692.072076	37.766490
2014.193666	190969.885106	37.771508
2016.092172	191243.757731	37.776525
2018.255567	191531.004865	37.781543
2020.168227	191807.048389	37.786560
2022.395644	192076.107769	37.791578
2024.265523	192361.377690	37.796596
2026.270928	192655.766277	37.801613
2028.488617	192931.711769	37.806631
2029.990482	193221.174456	37.811648
2032.197978	193511.838086	37.816666
2033.807364	193799.545719	37.821684
2035.754907	194096.604163	37.826701
2037.823772	194398.721440	37.831719
2039.491637	194714.632663	37.836736
2041.406937	195014.531918	37.841754
2044.038146	195322.727373	37.846772
2046.236546	195627.113367	37.851789
2048.375647	195929.022507	37.856807
2050.171267	196241.161177	37.861824
2052.291894	196547.557914	37.866842
2054.600079	196868.994150	37.871860
2056.460922	197171.451579	37.876877
2058.616694	197478.354342	37.881895
2060.900347	197800.129251	37.886912
2062.882231	198114.263331	37.891930
2064.997730	198436.717463	37.896948
2066.504026	198751.430908	37.901965
2069.074855	199065.455847	37.906983
2071.122939	199391.226961	37.912000
2073.613394	199699.072569	37.917018
2076.070201	200009.731207	37.922036
2077.988417	200323.403531	37.927053
2080.139898	200631.818976	37.932071
2082.516798	200946.634440	37.937088
2084.299010	201251.268541	37.942106
2086.761181	201567.240199	37.947124
2088.595188	201874.089971	37.952141
2091.070730	202173.936839	37.957159
2092.831924	202498.348858	37.962176
2095.188090	202811.398214	37.967194
2096.814644	203126.414727	37.972212
2098.800495	203444.558094	37.977229
2100.782026	203757.510352	37.982247
2102.527668	204091.784889	37.987264
2104.469460	204420.211938	37.992282
2106.664725	204756.901126	37.997300
2108.374975	205091.744690	38.002317
2110.408203	205427.270897	38.007335
2111.849744	205781.907964	38.012352
2113.906008	206132.657585	38.017370
2116.079531	206488.378869	38.022388
2118.304447	206835.255302	38.027405
2120.837549	207179.820298	38.032423
2122.964788	207504.291979	38.037440
2125.100158	207814.351442	38.042458
2127.644772	208125.345212	38.047476
2129.557774	208445.844652	38.052493
2132.351590	208747.579376	38.057511
2134.591829	209055.657291	38.062528
2136.202700	209365.596283	38.067546
2138.395591	209683.335118	38.072564
2140.659834	209999.793098	38.077581
2142.626211	210317.928539	38.082599
2144.704151	210652.477659	38.087616
2146.604955	210975.807596	38.092634
2148.676435	211310.868236	38.097652
2150.470597	211642.345795	38.102669
2152.562113	211985.938874	38.107687
2154.556315	212337.067426	38.112704
2156.934764	212679.623560	38.117722
2158.800551	213022.471807	38.122740
2160.563226	213380.780544	38.127757
2163.085992	213725.144450	38.132775
2164.905531	214092.792429	38.137792
2167.434589	214446.250194	38.142810
2169.587351	214812.269293	38.147828
2171.748906	215179.659750	38.152845
2173.964017	215544.147060	38.157863
2175.781722	215907.916329	38.162880
2177.796351	216280.974360	38.167898
2179.846710	216653.926068	38.172916
2181.901432	217041.050655	38.177933
2184.524462	217420.815577	38.182951
2186.731862	217810.990151	38.187968
2188.706289	218196.761262	38.192986
2191.200019	218584.324483	38.198004
2193.262612	218978.160134	38.203021
2195.679543	219353.954233	38.208039
2198.188782	219748.376676	38.213056
2200.497614	220118.985096	38.218074
2202.605631	220502.303253	38.223092
2204.723021	220893.418672	38.228109
2207.709447	221266.454930	38.233127
2209.507264	221661.386716	38.238144
2211.918176	222044.912245	38.243162
2213.776272	222415.503584	38.248180
2215.931551	222813.781658	38.253197
2218.497408	223195.328634	38.258215
2220.698969	223585.981425	38.263232
2222.783493	223982.802239	38.268250
2224.885342	224367.302377	38.273268
2227.027814	224752.050743	38.278285
2229.705261	225134.727588	38.283303
2231.868712	225532.352561	38.288320
2235.075313	225903.155509	38.293338
2238.058244	226262.186594	38.298356
2240.779856	226614.964028	38.303373
2243.625888	226960.939188	38.308391
2245.905498	227278.690499	38.313408
2248.367625	227582.898230	38.318426
2250.381092	227891.450642	38.323444
2252.808228	228203.971705	38.328461
2254.851565	228491.894964	38.333479
2257.031786	228814.670669	38.338496
2258.950024	229124.207243	38.343514
2261.108055	229432.814435	38.348532
2262.625115	229761.598606	38.353549
2264.647862	230085.115225	38.358567
2266.551983	230421.353339	38.363584
2268.552861	230761.690619	38.368602
2271.041110	231099.201980	38.373620
2272.887033	231456.560632	38.378637
2274.632663	231810.558854	38.383655
2277.293560	232179.819960	38.388672
2279.243713	232538.687234	38.393690
2281.740932	232894.438964	38.398708
2283.666990	233281.177312	38.403725
2285.734654	233642.922580	38.408743
2288.059283	234025.911200	38.413760
2289.929127	234406.616040	38.418778
2292.779095	234785.121959	38.423796
2295.338052	235170.409874	38.428813
2297.627689	235556.405068	38.433831
2299.964575	235942.011930	38.438848
2302.653264	236324.333358	38.443866
2305.176590	236688.343575	38.448884
2307.482535	237071.900352	38.453901
2309.695364	237446.862463	38.458919
2311.478359	237847.224621	38.463936
2313.353230	238243.126437	38.468954
2316.609473	238632.239024	38.473972
2319.452317	239020.254460	38.478989
2322.107256	239400.834409	38.484007
2323.957594	239791.865877	38.489024
2326.262857	240170.423852	38.494042
2328.859233	240547.510104	38.499060
2331.012822	240933.944512	38.504077
2333.713325	241316.221598	38.509095
2336.090845	241697.716175	38.514112
2338.212160	242078.924859	38.519130
2340.788668	242460.970734	38.524148
2343.167741	242856.514260	38.529165
2345.519004	243239.158530	38.534183
2348.038483	243629.115899	38.539200
2350.234757	244015.750454	38.544218
2352.552871	244390.298346	38.549236
2354.559173	244782.529490	38.554253
2356.728240	245171.430895	38.559271
2359.115455	245563.496189	38.564288
2361.156905	245966.671257	38.569306
2363.755837	246359.107641	38.574324
2365.442696	246771.844847	38.579341
2367.985824	247156.924712	38.584359
2370.385819	247524.399752	38.589376
2372.732338	247905.169992	38.594394
2375.564332	248269.243995	38.599412
2378.405864	248630.090463	38.604429
2380.548273	248995.502241	38.609447
2383.328192	249358.214175	38.614464
2385.083697	249727.071198	38.619482
2387.511168	250095.813577	38.624500
2389.673222	250476.820438	38.629517
2391.841521	250849.138594	38.634535
2394.515298	251226.883011	38.639552
2396.433039	251612.657244	38.644570
2398.340085	251998.027041	38.649588
2400.681174	252404.153393	38.654605
2403.093934	252800.081001	38.659623
2405.371544	253210.054415	38.664640
2407.551669	253619.257141	38.669658
2410.086888	254034.013396	38.674676
2412.242773	254461.460000	38.679693
2414.662993	254874.889759	38.684711
2417.134847	255300.250275	38.689728
2419.169912	255739.504868	38.694746
2421.827463	256157.339803	38.699764
2424.434954	256599.773628	38.704781
2426.817850	257035.132955	38.709799
2429.079938	257475.872999	38.714816
2431.745311	257908.059396	38.719834
2434.943040	258343.787393	38.724852
2437.077827	258782.161133	38.729869
2439.252049	259221.290132	38.734887
2442.367731	259651.112929	38.739904
2444.613217	260090.686751	38.744922
2447.342139	260518.974979	38.749940
2450.217366	260955.214617	38.754957
2452.599456	261386.508536	38.759975
2455.610379	261813.554040	38.764992
2458.152054	262249.799250	38.770010
2460.687167	262667.272435	38.775028
2463.048036	263093.539217	38.780045
2465.518702	263517.195834	38.785063
2468.106593	263940.171637	38.790080
2470.482344	264366.536587	38.795098
2472.956389	264790.267886	38.800116
2475.358048	265215.408369	38.805133
2477.722818	265649.852266	38.810151
2480.716296	266081.266943	38.815168
2483.166676	266511.351469	38.820186
2485.608943	266934.628965	38.825204
2488.582792	267344.351633	38.830221
2492.024107	267755.238697	38.835239
2495.404109	268150.716286	38.840256
2497.962935	268543.209266	38.845274
2500.881064	268910.440859	38.850292
2503.221678	269288.287493	38.855309
2506.062982	269653.854813	38.860327
2508.382819	269991.821948	38.865344
2510.773540	270338.388088	38.870362
2512.909941	270684.082806	38.875380
2515.031994	271038.543455	38.880397
2517.254499	271394.967893	38.885415
2519.593665	271743.116119	38.890432
2521.419581	272107.405993	38.895450
2523.272928	272481.597629	38.900468
2525.422796	272868.769471	38.905485
2527.395244	273269.916942	38.910503
2529.764050	273669.700494	38.915520
2532.050376	274085.983556	38.920538
2534.344322	274502.823429	38.925556
2535.942635	274928.875428	38.930573
2538.275253	275364.199893	38.935591
2540.836533	275812.515674	38.940608
2543.315474	276265.797985	38.945626
2545.970988	276706.602168	38.950644
2548.407098	277172.743204	38.955661
2550.739207	277621.018028	38.960679
2554.188728	278074.486010	38.965696
2556.339089	278531.451798	38.970714
2559.087139	278992.048357	38.975732
2561.900195	279451.362569	38.980749
2564.076063	279925.415801	38.985767
2567.270594	280383.417728	38.990784
2569.707750	280859.328870	38.995802
2572.577768	281326.782251	39.000820
2575.172390	281794.687807	39.005837
2578.213989	282261.169359	39.010855
2581.193173	282725.805938	39.015872
2583.926764	283183.497834	39.020890
2586.502560	283636.211356	39.025908
2589.444041	284085.812919	39.030925
2592.028600	284549.495374	39.035943
2594.900143	284988.082202	39.040960
2597.349152	285447.593846	39.045978
2599.884590	285903.710957	39.050996
2602.468593	286352.807750	39.056013
2605.108692	286815.838308	39.061031
2607.773473	287269.210950	39.066048
2610.376976	287728.282178	39.071066
2613.719807	288169.648553	39.076084
2617.231746	288601.662707	39.081101
2620.328089	289039.512226	39.086119
2623.309280	289453.046828	39.091136
2625.939194	289890.617498	39.096154
2628.250262	290302.739808	39.101172
2631.402669	290722.641607	39.106189
2633.659848	291150.670391	39.111207
2636.070786	291576.233006	39.116224
2638.375018	292003.310873	39.121242
2640.734056	292429.615819	39.126260
2643.182787	292865.733316	39.131277
2645.381343	293294.322970	39.136295
2648.243954	293702.122738	39.141312
2651.070346	294100.301021	39.146330
2653.399345	294497.800896	39.151348
2656.156866	294894.616504	39.156365
2658.339058	295305.066408	39.161383
2660.891432	295717.940506	39.166400
2663.205834	296138.752541	39.171418
2665.694837	296561.006126	39.176436
2667.976613	296988.144436	39.181453
2670.161081	297429.393498	39.186471
2672.433538	297870.752570	39.191488
2675.401466	298329.185151	39.196506
2677.761708	298786.576546	39.201524
2679.831666	299259.253945	39.206541
2681.941117	299744.011454	39.211559
2684.857623	300224.945949	39.216576
2687.234641	300720.116412	39.221594
2689.548483	301219.764909	39.226612
2692.326444	301725.477420	39.231629
2694.925867	302240.004903	39.236647
2698.122563	302751.049612	39.241664
2700.903905	303262.721079	39.246682
2703.624652	303765.257238	39.251700
2706.731137	304267.546792	39.256717
2709.673946	304784.946618	39.261735
2712.759087	305282.357811	39.266752
2715.172551	305799.232383	39.271770
2717.976059	306306.285191	39.276788
2721.289293	306805.654541	39.281805
2723.615726	307320.858333	39.286823
2726.945590	307830.833735	39.291840
2729.633520	308340.560049	39.296858
2732.313067	308861.762939	39.301876
2735.216997	309364.487543	39.306893
2737.952020	309885.826465	39.311911
2740.823454	310388.397580	39.316928
2743.982606	310905.289255	39.321946
2747.222074	311400.502653	39.326964
2750.892594	311890.306416	39.331981
2753.366344	312385.263192	39.336999
2755.988415	312878.388348	39.342016
2758.617828	313369.528230	39.347034
2761.131745	313877.342341	39.352052
2764.201791	314364.997437	39.357069
2766.836359	314869.431981	39.362087
2769.914123	315356.901143	39.367104
2772.699436	315844.442255	39.372122
2775.708922	316334.633184	39.377140
2778.946305	316822.496378	39.382157
2781.202697	317312.681999	39.387175
2784.029957	317802.411019	39.392192
2786.711868	318296.046170	39.397210
2789.173102	318791.086478	39.402228
2792.152089	319287.151789	39.407245
2794.556422	319773.942299	39.412263
2797.252728	320236.812038	39.417280
2799.871129	320705.049142	39.422298
2802.365446	321170.536468	39.427316
2805.054320	321634.666839	39.432333
2807.548205	322109.846320	39.437351
2810.655251	322576.843478	39.442368
2813.639275	323048.402858	39.447386
2815.930797	323521.625701	39.452404
2819.001232	324000.602057	39.457421
2821.929835	324484.118092	39.462439
2825.224149	324955.533495	39.467456
2828.597711	325434.319697	39.472474
2831.284025	325916.621500	39.477492
2833.795204	326386.813764	39.482509
2836.901980	326879.140283	39.487527
2839.347589	327361.649019	39.492544
2842.103686	327839.607085	39.497562
2844.993061	328332.821523	39.502580
2847.779142	328822.698248	39.507597
2850.778937	329321.495757	39.512615
2853.664015	329818.709080	39.517632
2856.700662	330321.959412	39.522650
2859.094107	330832.778592	39.527668
2862.257509	331341.506756	39.532685
2864.752104	331848.770546	39.537703
2867.336652	332365.000660	39.542720
2870.307537	332879.814403	39.547738
2873.017338	333406.547945	39.552756
2876.161953	333934.445821	39.557773
2878.882743	334459.110860	39.562791
2882.090837	334972.848352	39.567808
2885.176704	335499.115924	39.572826
2887.715694	336028.009946	39.577844
2890.604034	336557.625719	39.582861
2893.486710	337104.979759	39.587879
2896.211113	337637.277527	39.592896
2899.608481	338171.916797	39.597914
2902.293344	338706.748236	39.602932
2905.222940	339242.344330	39.607949
2908.276748	339795.350648	39.612967
2911.194387	340332.053721	39.617984
2914.205144	340872.339099	39.623002
2917.100768	341422.790475	39.628020
2920.126168	341959.380953	39.633037
2922.548520	342505.890620	39.638055
2925.463882	343066.877897	39.643072
2928.752067	343608.556981	39.648090
2931.602941	344171.623235	39.653108
2934.894365	344717.019690	39.658125
2937.875877	345263.731607	39.663143
2940.727691	345809.418667	39.668160
2943.596664	346356.263680	39.673178
2946.000033	346915.083896	39.678196
2948.922785	347462.794590	39.683213
2951.707119	348019.759577	39.688231
2954.606015	348556.599485	39.693248
2957.695371	349068.252079	39.698266
2961.120938	349574.994405	39.703284
2964.400972	350087.516110	39.708301
2967.469185	350595.982478	39.713319
2970.514117	351104.142357	39.718336
2973.889870	351604.728673	39.723354
2976.316620	352125.771192	39.728372
2979.317699	352625.394582	39.733389
2982.030450	353145.868262	39.738407
2984.657881	353678.123621	39.743424
2987.806003	354198.763646	39.748442
2990.701055	354732.228568	39.753460
2993.717880	355259.170349	39.758477
2996.157457	355803.584300	39.763495
2998.862975	356351.523103	39.768512
3001.610433	356898.102679	39.773530
3004.530885	357468.240964	39.778548
3007.283453	358036.750753	39.783565
3009.960931	358609.958944	39.788583
3013.189139	359187.301705	39.793600
3016.787298	359760.361426	39.798618
3019.646484	360343.966060	39.803636
3022.356734	360932.077851	39.808653
3025.503745	361518.000545	39.813671
3028.081687	362107.233432	39.818688
3031.410995	362702.442720	39.823706
3034.325274	363307.936927	39.828724
3037.504638	363906.527035	39.833741
3040.798956	364521.804949	39.838759
3043.029366	365130.430960	39.843776
3046.408701	365738.089846	39.848794
3049.209603	366361.209326	39.853812
3052.879891	366976.458754	39.858829
3056.115763	367587.510821	39.863847
3059.086637	368215.693670	39.868864
3062.480588	368823.476798	39.873882
3065.471001	369447.551423	39.878900
3068.553769	370069.849418	39.883917
3072.059653	370683.897527	39.888935
3075.163347	371304.217548	39.893952
3078.625531	371919.317024	39.898970
3081.872248	372535.685300	39.903988
3085.198279	373141.504387	39.909005
3088.981583	373739.804203	39.914023
3092.186486	374329.798310	39.919040
3095.502631	374922.045719	39.924058
3098.640879	375524.152719	39.929076
3101.615464	376116.158910	39.934093
3105.109091	376694.727630	39.939111
3108.763307	377282.920423	39.944128
3111.805139	377846.357183	39.949146
3115.203836	378423.695290	39.954164
3118.633405	378979.033911	39.959181
3122.023422	379521.057975	39.964199
3124.990466	380042.886083	39.969216
3128.702938	380552.103709	39.974234
3131.981981	381051.930022	39.979252
3134.873891	381540.836232	39.984269
3137.953223	382046.918666	39.989287
3140.696933	382561.062364	39.994304
3143.680453	383068.032579	39.999322
3146.629717	383576.673957	40.004340
3149.566471	384093.802549	40.009357
3152.536890	384606.429651	40.014375
3155.529670	385132.658618	40.019392
3158.391425	385659.788513	40.024410
3161.442276	386206.955291	40.029428
3164.135973	386743.120684	40.034445
3167.266259	387287.466448	40.039463
3169.872317	387855.112529	40.044480
3172.651689	388410.550990	40.049498
3175.414945	388998.276496	40.054516
3178.230089	389580.025055	40.059533
3181.571677	390175.436456	40.064551
3184.102258	390783.623009	40.069568
3187.414260	391377.621792	40.074586
3190.824123	391997.166510	40.079604
3193.796574	392610.183270	40.084621
3197.302357	393227.481077	40.089639
3200.096832	393849.272191	40.094656
3203.650630	394467.423068	40.099674
3206.811048	395091.685286	40.104692
3210.160495	395731.969421	40.109709
3213.873213	396354.209653	40.114727
3216.706414	396982.085988	40.119744
3220.627176	397611.663553	40.124762
3223.707455	398247.452709	40.129780
3227.265307	398877.317942	40.134797
3230.689780	399511.119713	40.139815
3233.705995	400152.528142	40.144832
3237.232515	400783.116663	40.149850
3240.217149	401417.356275	40.154868
3243.300874	402052.578118	40.159885
3246.188062	402696.762983	40.164903
3249.414077	403347.842519	40.169920
3252.984354	403984.457289	40.174938
3256.038194	404635.789217	40.179956
3259.225040	405301.700940	40.184973
3262.673686	405961.826266	40.189991
3265.544116	406626.112960	40.195008
3268.704507	407277.186211	40.200026
3272.359703	407945.308970	40.205044
3275.856153	408605.564147	40.210061
3279.314737	409267.759930	40.215079
3282.652389	409918.865291	40.220096
3286.122063	410571.147903	40.225114
3289.733205	411212.904067	40.230132
3293.305348	411866.276852	40.235149
3296.976662	412491.350760	40.240167
3299.789282	413098.650106	40.245184
3303.115562	413704.454548	40.250202
3306.178212	414303.983665	40.255220
3309.440915	414899.260652	40.260237
3312.740106	415499.303938	40.265255
3315.582926	416101.411658	40.270272
3318.904675	416707.601701	40.275290
3322.210125	417321.858008	40.280308
3325.782021	417927.494942	40.285325
3329.153757	418532.037313	40.290343
3332.450405	419153.618945	40.295360
3335.728818	419769.136632	40.300378
3339.301905	420393.577255	40.305396
3342.172682	421020.198225	40.310413
3345.939636	421643.612012	40.315431
3348.977284	422268.805494	40.320448
3352.467079	422892.336123	40.325466
3356.330070	423523.685815	40.330484
3359.357226	424168.984270	40.335501
3362.591106	424803.749731	40.340519
3365.412176	425450.112371	40.345536
3368.641720	426101.551864	40.350554
3371.766976	426760.939728	40.355572
3375.098314	427421.033513	40.360589
3379.004263	428082.883864	40.365607
3382.097793	428753.763865	40.370624
3385.391640	429426.463492	40.375642
3388.983262	430104.003005	40.380660
3392.248365	430773.176097	40.385677
3395.754945	431451.399592	40.390695
3398.985874	432136.483268	40.395712
3402.517334	432813.650251	40.400730
3406.355818	433499.095762	40.405748
3409.831673	434180.786910	40.410765
3413.801681	434859.691036	40.415783
3417.032294	435546.798250	40.420800
3420.246640	436221.590234	40.425818
3423.895112	436913.695653	40.430836
3426.732961	437608.043453	40.435853
3430.358366	438307.042291	40.440871
3433.718426	439006.317495	40.445888
3437.063350	439703.599934	40.450906
3440.510323	440414.807449	40.455924
3443.615688	441119.220075	40.460941
3447.185151	441823.581417	40.465959
3450.701430	442548.165564	40.470976
3454.084680	443260.455067	40.475994
3457.585778	443975.432771	40.481012
3460.608628	444702.305592	40.486029
3464.482040	445418.284726	40.491047
3468.040881	446143.044432	40.496064
3471.487012	446857.227345	40.501082
3474.571596	447582.373105	40.506100
3477.690027	448310.320588	40.511117
3481.488316	449020.382661	40.516122
3484.219494	449714.362193	40.521127
3487.451432	450339.684323	40.526132
3490.766655	450911.636591	40.531136
3493.800768	451434.493601	40.536141
3496.676103	451895.715700	40.541146
3499.275458	452318.292790	40.546151
3501.470349	452681.970690	40.551156
3503.855365	452984.927334	40.556160
3506.155291	453253.472305	40.561165
3507.917519	453444.492712	40.566170
3509.954714	453607.988304	40.571175
3511.529196	453729.029694	40.576180
3512.984025	453800.157818	40.581184
3514.195760	453846.639566	40.586189
3515.324124	453851.820434	40.591194
3516.175453	453837.785141	40.596199
3517.017924	453794.450555	40.601204
3518.078022	453712.298108	40.606208
3518.598316	453622.582729	40.611213
3519.255140	453506.685475	40.616218
3519.555129	453372.446403	40.621223
3519.497449	453225.695204	40.626228
3520.019954	453064.142277	40.631232
3519.457872	452904.446228	40.636237
3519.849285	452731.810730	40.641242
3520.426147	452547.583320	40.646247
3520.148815	452355.642084	40.651252
3520.331170	452153.075501	40.656256
3520.487633	451944.731785	40.661261
3520.380244	451742.514846	40.666266
3520.525940	451532.546474	40.671271
3520.274801	451315.596502	40.676276
3520.487093	451085.281714	40.681280
3520.036603	450857.612577	40.686285
3519.553157	450630.960602	40.691290
3519.610483	450408.776986	40.696295
3519.011037	450190.252306	40.701300
3519.014557	449964.473290	40.706304
3518.434667	449754.154569	40.711309
3518.266037	449535.803009	40.716314
3517.802119	449327.843289	40.721319
3517.798923	449123.656411	40.726324
3517.597917	448916.205477	40.731328
3517.444904	448722.789821	40.736333
3517.656679	448509.889586	40.741338
3517.151548	448312.524487	40.746343
3516.735358	448108.246165	40.751348
3516.665628	447902.791138	40.756352
3516.220402	447719.354907	40.761357
3516.305874	447527.256705	40.766362
3515.910557	447334.731764	40.771367
3515.493858	447150.474391	40.776372
3515.346387	446962.366197	40.781376
3515.023209	446783.819910	40.786381
3514.557688	446613.207327	40.791386
3514.295113	446449.810435	40.796391
3514.087240	446278.542644	40.801396
3513.880297	446114.018025	40.806400
3513.583235	445962.439196	40.811405
3513.498809	445798.499776	40.816410
3513.277489	445646.956491	40.821415
3512.783780	445497.537897	40.826420
3512.999840	445346.627795	40.831424
3512.560095	445207.087166	40.836429
3512.197005	445064.895384	40.841434
3512.101696	444937.668536	40.846439
3511.752285	444795.624780	40.851444
3512.237590	444663.327084	40.856448
3511.602091	444540.906665	40.861453
3511.804365	444403.381258	40.866458
3511.289831	444278.352171	40.871463
3511.346515	444153.681275	40.876468
3511.235000	444031.117775	40.881472
3510.561447	443917.119326	40.886477
3510.807920	443793.174703	40.891482
3510.304321	443689.086667	40.896487
3510.321924	443583.844057	40.901492
3510.654862	443469.772831	40.906496
3510.192921	443371.052291	40.911501
3509.867669	443254.049202	40.916506
3509.556527	443157.736443	40.921511
3509.254766	443062.537478	40.926516
3509.792330	442960.296935	40.931520
3509.202943	442868.798034	40.936525
3509.215694	442773.189061	40.941530
3508.669124	442691.826085	40.946535
3508.617941	442606.016272	40.951540
3508.816734	442523.003787	40.956544
3508.571319	442444.834578	40.961549
3508.665511	442357.578785	40.966554
3508.399030	442270.891438	40.971559
3508.272735	442197.468784	40.976564
3508.545902	442115.253588	40.981568
3507.878120	442049.277501	40.986573
3507.915060	441968.217962	40.991578
3507.828240	441901.837900	40.996583
3507.545921	441835.237408	41.001588
3507.729126	441764.753056	41.006592
3507.420197	441707.489612	41.011597
3507.509681	441642.042384	41.016602
3507.575104	441572.287639	41.021607
3507.542186	441514.570781	41.026612
3507.745760	441448.444097	41.031616
3507.264767	441383.499288	41.036621
3507.429896	441319.204812	41.041626
3507.206789	441262.026996	41.046631
3507.195186	441201.363714	41.051636
3507.392522	441130.012608	41.056640
3507.120926	441071.625205	41.061645
3507.035252	441014.271104	41.066650
3507.067920	440956.643027	41.071655
3506.672755	440904.819691	41.076660
3506.872383	440850.865698	41.081664
3506.375725	440805.095657	41.086669
3506.734071	440745.128814	41.091674
3506.623487	440698.125963	41.096679
3506.292402	440650.957761	41.101684
3506.442871	440592.243393	41.106688
3506.563311	440555.548681	41.111693
3506.489004	440499.560874	41.116698
3506.299815	440450.998435	41.121703
3506.102326	440407.509847	41.126708
3506.086822	440371.345295	41.131712
3505.919365	440330.945681	41.136717
3506.138505	440282.972583	41.141722
3506.040899	440243.372493	41.146727
3506.061347	440213.390087	41.151732
3506.574092	440156.235927	41.156736
3506.214500	440117.694865	41.161741
3506.278348	440069.240558	41.166746
3506.332763	440024.642952	41.171751
3506.252339	439983.466947	41.176756
3506.239208	439930.663012	41.181760
3506.305280	439895.143195	41.186765
3506.113208	439842.471056	41.191770
3506.181696	439804.921614	41.196775
3506.063039	439766.237344	41.201780
3506.215021	439713.709059	41.206784
3506.068042	439676.196189	41.211789
3505.869532	439625.452261	41.216794
3505.539504	439592.992497	41.221799
3505.453604	439560.440273	41.226804
3505.569060	439516.947223	41.231808
3505.339019	439496.695555	41.236813
3505.459785	439456.245128	41.241818
3505.563832	439424.167546	41.246823
3505.435232	439389.136706	41.251828
3505.540079	439351.935382	41.256832
3505.506681	439331.142708	41.261837
3505.553152	439288.472635	41.266842
3505.527107	439258.496873	41.271847
3505.601532	439222.061446	41.276852
3505.374839	439183.039508	41.281856
3505.409538	439156.249113	41.286861
3505.477228	439128.387758	41.291866
3505.361734	439098.934338	41.296871
3505.176294	439065.891100	41.301876
3505.369021	439025.326144	41.306880
3504.985449	439013.013903	41.311885
3505.033293	438979.677061	41.316890
3505.086604	438948.165471	41.321895
3505.038393	438935.795925	41.326900
3505.232253	438903.296426	41.331904
3505.137844	438879.723659	41.336909
3505.007183	438848.141882	41.341914
3505.122071	438814.641158	41.346919
3504.572313	438795.204376	41.351924
3504.662360	438769.012813	41.356928
3504.827998	438742.098103	41.361933
3504.873631	438730.371899	41.366938
3504.601260	438700.234527	41.371943
3504.710143	438686.265410	41.376948
3504.956638	438658.474394	41.381952
3504.739083	438647.351109	41.386957
3504.820491	438620.552093	41.391962
3505.208875	438598.875043	41.396967
3504.720746	438581.608920	41.401972
3504.974827	438555.693475	41.406976
3504.707115	438531.541175	41.411981
3504.870605	438506.249897	41.416986
3504.893930	438477.127058	41.421991
3504.683325	438457.429150	41.426996
3504.665791	438429.885851	41.432000
3504.745687	438417.443413	41.437005
3504.700026	438398.275318	41.442010
3504.963053	438374.133685	41.447015
3504.694312	438350.235014	41.452020
3504.752961	438333.788479	41.457024
3504.639315	438314.581190	41.462029
3504.614988	438294.394760	41.467034
3504.755680	438273.317719	41.472039
3504.551830	438256.104263	41.477044
3504.808610	438221.208701	41.482048
3504.509395	438209.896218	41.487053
3504.518632	438187.116708	41.492058
3504.537996	438163.016451	41.497063
3504.224546	438157.946227	41.502068
3504.055094	438128.399274	41.507072
3504.383899	438127.531480	41.512077
3504.491141	438106.916570	41.517082
3504.720670	438089.831910	41.522087
3504.675760	438069.851713	41.527092
3504.527406	438055.621740	41.532096
3504.528316	438032.742032	41.537101
3504.546489	438006.206730	41.542106
3504.856362	438001.740271	41.547111
3504.561624	437989.513756	41.552116
3504.519963	437955.480432	41.557120
3504.576440	437950.803575	41.562125
3504.624949	437923.958609	41.567130
3504.722042	437901.113074	41.572135
3504.464304	437885.329005	41.577140
3504.819887	437868.019727	41.582144
3504.793159	437845.601128	41.587149
3504.612370	437822.143454	41.592154
3504.542572	437811.501835	41.597159
3504.707507	437787.934362	41.602164
3504.719031	437771.799848	41.607168
3504.488208	437756.974989	41.612173
3504.330686	437737.723964	41.617178
3504.347625	437712.406080	41.622183
3504.423470	437701.536614	41.627188
3504.435343	437678.350282	41.632192
3504.349909	437668.573702	41.637197
3504.442898	437649.990070	41.642202
3504.501226	437632.071854	41.647207
3504.373169	437609.264466	41.652212
3504.854366	437593.049627	41.657216
3504.539602	437573.013600	41.662221
3504.793850	437558.257980	41.667226
3504.951983	437531.951876	41.672231
3504.683860	437518.858115	41.677236
3504.482414	437485.612339	41.682240
3504.640058	437471.786334	41.687245
3504.342614	437456.160937	41.692250
3504.817846	437435.939164	41.697255
3504.511232	437426.707566	41.702260
3504.578167	437398.032464	41.707264
3504.698525	437383.959110	41.712269
3504.406468	437365.390257	41.717274
3504.572603	437345.221180	41.722279
3504.517486	437324.075216	41.727284
3504.676638	437303.399970	41.732288
3504.313965	437282.255748	41.737293
3504.278373	437271.963159	41.742298
3503.959195	437248.832909	41.747303
3503.984767	437243.045064	41.752308
3504.165659	437220.083062	41.757312
3504.091264	437213.145427	41.762317
3504.025356	437205.090222	41.767322
3504.194962	437199.227039	41.772327
3503.811584	437174.890090	41.777332
3503.974053	437166.795876	41.782336
3504.030166	437168.866378	41.787341
3504.137351	437149.315985	41.792346
3504.384074	437137.808274	41.797351
3503.976639	437124.484405	41.802356
3504.167212	437104.463138	41.807360
3503.951342	437103.180981	41.812365
3504.204642	437088.881810	41.817370
3504.157843	437076.003663	41.822375
3504.207695	437076.147390	41.827380
3504.435382	437045.871667	41.832384
3504.235900	437040.629528	41.837389
3504.213410	437025.159814	41.842394
3504.504992	437006.338808	41.847399
3504.178634	436991.479021	41.852404
3504.811155	436958.597396	41.857408
3504.348549	436949.950302	41.862413
3504.302124	436929.005414	41.867418
3504.363155	436915.144830	41.872423
3504.189613	436908.426964	41.877428
3504.163006	436890.066058	41.882432
3504.027013	436872.434082	41.887437
3504.167532	436872.815996	41.892442
3504.578503	436866.150512	41.897447
3504.424359	436835.584569	41.902452
3504.575440	436831.703062	41.907456
3504.336321	436805.971275	41.912461
3504.372732	436791.911884	41.917466
3504.487763	436768.301129	41.922471
3504.087876	436764.412220	41.927476
3504.743882	436744.209694	41.932480
3504.400821	436722.046919	41.937485
3504.172952	436704.379766	41.942490
3504.525515	436685.446612	41.947495
3504.124724	436678.361608	41.952500
3504.343792	436651.688933	41.957504
3504.296809	436659.307085	41.962509
3504.255183	436634.353123	41.967514
3504.682772	436617.182790	41.972519
3504.209366	436606.964652	41.977524
3504.744724	436576.838701	41.982528
3504.619270	436560.523768	41.987533
3504.664784	436547.020746	41.992538
3504.616408	436521.205329	41.997543
3504.411159	436505.462058	42.002548
3504.300663	436481.483637	42.007552
3504.183961	436472.777295	42.012557
3504.140033	436452.288146	42.017562
3504.310713	436426.536686	42.022567
3504.030039	436434.093349	42.027572
3504.217708	436412.600665	42.032576
3504.332761	436401.673140	42.037581
3504.504818	436386.880053	42.042586
3504.360509	436360.979363	42.047591
3504.150820	436356.854969	42.052596
3504.190079	436329.350126	42.057600
3504.327134	436327.804722	42.062605
3503.895499	436304.844906	42.067610
3504.202849	436291.804370	42.072615
3504.275430	436294.683897	42.077620
3504.302229	436266.166410	42.082624
3504.320846	436262.764037	42.087629
3504.784971	436235.237269	42.092634
3504.754546	436220.377176	42.097639
3504.385322	436198.725702	42.102644
3504.402749	436181.472869	42.107648
3503.993948	436165.003091	42.112653
3504.050856	436151.193476	42.117658
3504.496454	436132.497649	42.122663
3504.480575	436118.751178	42.127668
3504.526233	436106.008894	42.132672
3504.488840	436077.248453	42.137677
3504.685712	436065.292091	42.142682
3504.728984	436043.772976	42.147687
3504.249639	436026.249700	42.152692
3504.678577	436005.730140	42.157696
3504.283675	435999.506417	42.162701
3504.387065	435967.119582	42.167706
3504.687561	435958.595483	42.172711
3504.230688	435938.328584	42.177716
3504.555528	435918.029661	42.182720
3504.314535	435895.138346	42.187725
3504.186368	435885.216079	42.192730
3504.425466	435877.108319	42.197735
3504.248651	435845.022832	42.202740
3503.860510	435829.208846	42.207744
3503.937504	435810.727899	42.212749
3503.761725	435799.900479	42.217754
3503.962746	435797.633816	42.222759
3503.853277	435791.665713	42.227764
3504.074305	435768.543173	42.232768
3503.792059	435771.635561	42.237773
3503.926052	435769.836963	42.242778
3504.125565	435747.682058	42.247783
3504.011561	435743.693420	42.252788
3503.871183	435732.707715	42.257792
3504.081943	435727.750373	42.262797
3504.001356	435716.500771	42.267802
3504.236817	435716.511342	42.272807
3503.948246	435690.380835	42.277812
3504.033036	435676.718378	42.282816
3503.727638	435682.605219	42.287821
3503.985396	435667.746292	42.292826
3503.995524	435650.139146	42.297831
3503.630135	435654.311207	42.302836
3503.675476	435650.853443	42.307840
3503.975531	435641.365313	42.312845
3504.140789	435627.739823	42.317850
3504.176852	435616.165836	42.322855
3504.051967	435601.270728	42.327860
3503.965226	435580.432944	42.332864
3503.773159	435577.979697	42.337869
3503.791327	435565.799903	42.342874
3503.954324	435546.796692	42.347879
3503.768599	435551.039567	42.352884
3503.969488	435532.993867	42.357888
3504.004046	435543.591924	42.362893
3503.858331	435522.104583	42.367898
3504.024920	435507.768482	42.372903
3503.883430	435517.381881	42.377908
3503.853054	435493.642413	42.382912
3503.611009	435481.151849	42.387917
3503.847278	435477.001882	42.392922
3503.936328	435476.124194	42.397927
3504.030645	435468.243955	42.402932
3504.094414	435444.691307	42.407936
3503.727633	435449.015852	42.412941
3503.689755	435441.208913	42.417946
3503.960501	435414.170798	42.422951
3503.678027	435407.826240	42.427956
3503.783002	435393.906483	42.432960
3503.936614	435403.469541	42.437965
3503.839334	435390.446841	42.442970
3503.906115	435373.743069	42.447975
3503.705263	435368.297826	42.452980
3503.821777	435370.155234	42.457984
3503.707775	435359.317055	42.462989
3503.635659	435346.645190	42.467994
3503.870857	435341.835802	42.472999
3504.116387	435339.307810	42.478004
3504.100411	435331.902988	42.483008
3503.695248	435318.729870	42.488013
3503.885971	435311.847855	42.493018
3504.161895	435301.095279	42.498023
3503.834206	435285.321326	42.503028
3504.247821	435267.797200	42.508032
3503.938220	435266.683151	42.513037
3503.786375	435239.158876	42.518042
3504.067421	435229.775295	42.523047
3504.074337	435230.078576	42.528052
3504.146170	435210.938439	42.533056
3504.511637	435197.887351	42.538061
3504.545455	435189.712923	42.543066
3504.567265	435168.754751	42.548071
3504.406702	435160.309079	42.553076
3504.162918	435127.625163	42.558080
3504.080508	435121.094152	42.563085
3503.838621	435105.102473	42.568090
3503.813258	435091.052573	42.573095
3503.938411	435093.517377	42.578100
3504.055502	435080.153470	42.583104
3504.125942	435070.298409	42.588109
3503.942008	435056.174088	42.593114
3503.992444	435046.626857	42.598119
3503.795798	435029.917075	42.603124
3504.122549	435012.914960	42.608128
3504.217233	435013.609159	42.613133
3503.849212	434995.355747	42.618138
3504.138081	434976.076878	42.623143
3503.912817	434982.508331	42.628148
3504.172183	434956.080467	42.633152
3503.975295	434954.084614	42.638157
3504.110470	434951.473946	42.643162
3504.366770	434925.452472	42.648167
3504.344798	434914.090988	42.653172
3504.228854	434894.779696	42.658176
3504.250789	434872.654258	42.663181
3503.693148	434875.286411	42.668186
3504.132612	434852.835971	42.673191
3503.661871	434836.629490	42.678196
3504.087883	434828.692393	42.683200
3504.094020	434826.915553	42.688205
3503.835943	434803.823099	42.693210
3504.103156	434790.940770	42.698215
3503.830697	434796.162620	42.703220
3503.727732	434772.840697	42.708224
3503.989104	434763.916926	42.713229
3503.886159	434762.412398	42.718234
3504.119477	434751.971267	42.723239
3504.044957	434733.160147	42.728244
3504.228783	434729.881550	42.733248
3504.055822	434716.414741	42.738253
3504.084424	434697.230814	42.743258
3504.547656	434685.076031	42.748263
3504.438878	434666.321443	42.753268
3504.064826	434646.445151	42.758272
3503.987742	434627.279212	42.763277
3503.717410	434613.626014	42.768282
3503.903033	434611.209648	42.773287
3503.648598	434612.927503	42.778292
3503.990595	434609.672619	42.783296
3504.052277	434595.150903	42.788301
3503.828897	434584.381768	42.793306
3504.079267	434578.757812	42.798311
3503.969044	434565.127985	42.803316
3503.949889	434555.693908	42.808321
3504.063151	434556.283472	42.813325
3504.012610	434532.444965	42.818330
3504.094406	434516.143909	42.823335
3504.202736	434520.945630	42.828340
3504.456625	434498.577268	42.833345
3503.941286	434479.181603	42.838349
3504.090550	434463.376378	42.843354
3504.123486	434442.517115	42.848359
3504.270557	434436.555590	42.853364
3504.159976	434419.881402	42.858369
3504.590418	434403.926647	42.863373
3504.099525	434390.209498	42.868378
3504.291280	434367.090531	42.873383
3504.096885	434359.360684	42.878388
3504.323261	434338.569775	42.883393
3504.091100	434317.299010	42.888397
3503.735742	434321.926252	42.893402
3503.664381	434297.025531	42.898407
3503.485824	434292.692485	42.903412
3503.756140	434280.976341	42.908417
3503.832959	434279.390347	42.913421
3503.305310	434285.822888	42.918426
3503.898681	434278.009243	42.923431
3504.066684	434269.354919	42.928436
3504.044046	434258.348396	42.933441
3503.984224	434246.942302	42.938445
3503.915469	434227.876084	42.943450
3504.064585	434205.119409	42.948455
3503.855657	434207.996530	42.953460
3503.659991	434199.911670	42.958465
3503.909823	434177.492947	42.963469
3503.778156	434173.202611	42.968474
3504.179082	434174.250462	42.973479
3503.797107	434168.988075	42.978484
3503.973379	434143.892685	42.983489
3504.038680	434139.213534	42.988493
3503.742911	434128.558023	42.993498
3503.956418	434110.306083	42.998503
3503.686411	434099.747639	43.003508
3503.588097	434096.770825	43.008513
3503.812224	434102.212478	43.013517
3504.038850	434096.693937	43.018522
3504.163060	434074.499522	43.023527
3503.944844	434072.862411	43.028532
3503.698832	434053.014477	43.033537
3504.224584	434033.846584	43.038541
3503.579771	434031.927132	43.043546
3504.007775	434027.490466	43.048551
3503.918985	434019.539512	43.053556
3503.808700	434009.917811	43.058561
3503.933332	434008.932512	43.063565
3503.544265	434002.352061	43.068570
3503.857842	433986.721409	43.073575
3504.102707	433977.698671	43.078580
3504.527493	433969.660008	43.083585
3504.271313	433941.086440	43.088589
3504.048493	433926.206956	43.093594
3504.123000	433908.232290	43.098599
3504.004483	433896.734563	43.103604
3504.067240	433889.062128	43.108609
3504.126266	433884.434736	43.113613
3503.828012	433860.587084	43.118618
3504.147984	433846.680411	43.123623
3504.108288	433845.215762	43.128628
3504.129125	433814.971048	43.133633
3503.851785	433806.392591	43.138637
3503.878021	433807.098515	43.143642
3504.204426	433794.205519	43.148647
3503.619226	433773.704893	43.153652
3504.001278	433763.237916	43.158657
3504.188899	433770.512536	43.163661
3503.671340	433742.744456	43.168666
3503.788938	433727.958938	43.173671
3503.496486	433732.169633	43.178676
3503.769144	433730.600902	43.183681
3503.606296	433722.358047	43.188685
3503.284139	433711.250182	43.193690
3503.789752	433697.159499	43.198695
3504.391900	433689.090454	43.203700
3503.726155	433687.580469	43.208705
3503.575895	433665.483264	43.213709
3503.349702	433658.976383	43.218714
3503.994740	433652.117777	43.223719
3503.355546	433662.882493	43.228724
3503.966662	433651.006355	43.233729
3503.668313	433653.391407	43.238733
3503.897509	433636.151224	43.243738
3504.222952	433625.693850	43.248743
3504.039415	433623.035970	43.253748
3503.846712	433603.939654	43.258753
3503.739859	433584.879404	43.263757
3503.617761	433591.851780	43.268762
3503.804427	433584.919198	43.273767
3503.643110	433575.661213	43.278772
3503.909870	433554.659733	43.283777
3503.929232	433553.387944	43.288781
3503.487577	433560.617858	43.293786
3503.609743	433546.085147	43.298791
3503.572608	433534.218156	43.303796
3503.436000	433508.718826	43.308801
3503.476354	433514.445704	43.313805
3503.450252	433515.211314	43.318810
3503.614141	433507.572224	43.323815
3503.445823	433513.486956	43.328820
3503.373970	433512.484445	43.333825
3503.955609	433512.334429	43.338829
3503.741279	433504.810660	43.343834
3503.772056	433491.460562	43.348839
3503.440170	433484.007599	43.353844
3503.827377	433474.858877	43.358849
3504.162209	433468.763559	43.363853
3503.641065	433455.558421	43.368858
3503.980825	433439.060328	43.373863
3503.918863	433441.658744	43.378868
3503.664879	433438.454719	43.383873
3503.797740	433426.304939	43.388877
3503.660780	433414.708637	43.393882
3503.884065	433412.945350	43.398887
3503.877958	433407.872313	43.403892
3504.089853	433390.431935	43.408897
3503.629232	433374.222682	43.413901
3503.497382	433379.014914	43.418906
3503.867647	433372.710555	43.423911
3503.654726	433376.095874	43.428916
3503.878479	433356.014898	43.433921
3503.985513	433334.736043	43.438925
3503.701762	433337.829013	43.443930
3503.889357	433326.227990	43.448935
3503.869213	433311.770172	43.453940
3504.110930	433305.234037	43.458945
3503.887730	433308.215190	43.463949
3503.705106	433285.260539	43.468954
3504.183192	433270.159466	43.473959
3503.723227	433274.804778	43.478964
3503.728213	433265.315306	43.483969
3503.872882	433239.513941	43.488973
3503.477866	433233.796889	43.493978
3503.636597	433229.406049	43.498983
3503.794734	433233.742862	43.503988
3503.782810	433229.330420	43.508993
3503.976289	433219.250585	43.513997
3503.665993	433211.692364	43.519002
3503.913476	433193.484635	43.524007
3503.875454	433194.049325	43.529012
3503.676929	433180.839683	43.534017
3503.754781	433158.449329	43.539021
3503.400716	433167.643337	43.544026
3503.614253	433163.040159	43.549031
3503.789963	433168.794754	43.554036
3504.304416	433155.006681	43.559041
3504.319215	433132.931519	43.564045
3503.985141	433127.812937	43.569050
3504.237314	433100.217096	43.574055
3504.210636	433084.897638	43.579060
3504.121186	433078.925405	43.584065
3504.023851	433060.116803	43.589069
3504.041933	433052.959137	43.594074
3504.206633	433032.025348	43.599079
3503.670182	433026.687588	43.604084
3503.520620	433006.467083	43.609089
3503.868924	433007.676202	43.614093
3503.436749	433015.868766	43.619098
3503.731094	432992.527927	43.624103
3503.659377	432979.905422	43.629108
3503.573882	432976.418852	43.634113
3503.728284	432975.326942	43.639117
3503.743151	432975.324442	43.644122
3503.992842	432960.617361	43.649127
3503.905837	432950.940496	43.654132
3503.758857	432937.569686	43.659137
3503.985973	432939.459151	43.664141
3503.426596	432915.705842	43.669146
3503.627389	432899.434060	43.674151
3503.466831	432897.178109	43.679156
3503.535580	432896.405275	43.684161
3503.534489	432900.363402	43.689165
3503.566850	432907.766292	43.694170
3503.825471	432896.812575	43.699175
3503.699160	432878.211741	43.704180
3503.895605	432861.027311	43.709185
3503.730617	432862.222597	43.714189
3503.606577	432869.855175	43.719194
3503.769945	432858.765476	43.724199
3503.919138	432839.153463	43.729204
3503.797415	432838.057952	43.734209
3504.198770	432836.822384	43.739213
3503.711950	432828.025616	43.744218
3504.301913	432799.610600	43.749223
3503.876709	432798.871361	43.754228
3503.919823	432785.417262	43.759233
3503.949035	432762.375175	43.764237
3503.853628	432764.776407	43.769242
3504.043352	432754.189585	43.774247
3503.607076	432728.486843	43.779252
3503.608790	432720.367756	43.784257
3503.641704	432718.129496	43.789261
3503.410105	432721.771813	43.794266
3503.713280	432715.377246	43.799271
3503.589632	432721.436781	43.804276
3503.553674	432711.700357	43.809281
3503.838165	432690.898033	43.814285
3503.776141	432688.371524	43.819290
3503.919150	432685.302577	43.824295
3503.723428	432675.999360	43.829300
3503.291347	432654.050786	43.834305
3503.696037	432642.869035	43.839309
3503.431048	432641.341292	43.844314
3503.825797	432637.721925	43.849319
3503.613076	432645.369720	43.854324
3503.677629	432632.368556	43.859329
3503.807004	432614.738709	43.864333
3503.241679	432607.173090	43.869338
3503.793435	432606.317773	43.874343
3503.712030	432605.113881	43.879348
3503.715149	432601.713608	43.884353
3503.777415	432588.915782	43.889357
3503.595025	432577.022356	43.894362
3504.255818	432566.507242	43.899367
3503.663020	432565.999584	43.904372
3503.524288	432567.850061	43.909377
3503.768291	432554.260039	43.914381
3503.558024	432543.842904	43.919386
3503.972657	432540.423100	43.924391
3503.875471	432543.890265	43.929396
3503.669772	432529.159179	43.934401
3503.757788	432507.020172	43.939405
3503.365058	432510.233347	43.944410
3503.667903	432501.403104	43.949415
3503.786890	432500.164990	43.954420
3503.610093	432499.687785	43.959425
3503.872335	432467.268862	43.964429
3503.603176	432463.255398	43.969434
3503.318777	432460.157915	43.974439
3503.356582	432465.834746	43.979444
3503.509488	432458.856847	43.984449
3503.875106	432456.003576	43.989453
3503.704302	432457.859538	43.994458
3503.465087	432430.651260	43.999463
3503.368128	432423.665271	44.004468
3503.185114	432422.174258	44.009473
3503.618342	432422.861475	44.014477
3503.595505	432427.483059	44.019482
3503.512470	432422.879631	44.024487
3503.503650	432419.633600	44.029492
3503.698840	432430.763851	44.034497
3503.601498	432406.423689	44.039501
3503.538151	432399.381210	44.044506
3503.629685	432389.521395	44.049511
3503.728135	432397.877290	44.054516
3503.082022	432395.653455	44.059521
3503.475048	432392.034345	44.064525
3503.815429	432391.874777	44.069530
3503.361746	432378.200807	44.074535
3503.446134	432367.428819	44.079540
3503.437932	432359.006838	44.084545
3503.891255	432358.269807	44.089549
3503.380767	432361.858313	44.094554
3503.772629	432347.938462	44.099559
3503.773776	432353.723068	44.104564
3503.723024	432340.639940	44.109569
3503.350839	432319.898665	44.114573
3503.512242	432321.241222	44.119578
3503.499246	432320.736044	44.124583
3503.551843	432319.001820	44.129588
3503.591833	432326.911031	44.134593
3503.683924	432324.358166	44.139597
3503.550123	432308.954997	44.144602
3503.564914	432281.347965	44.149607
3503.585544	432281.090763	44.154612
3503.296464	432290.629229	44.159617
3503.818227	432279.782519	44.164621
3503.592851	432283.779048	44.169626
3503.345334	432270.780222	44.174631
3503.662417	432266.463648	44.179636
3503.520122	432264.255261	44.184641
3503.941948	432262.001294	44.189645
3503.526570	432264.964650	44.194650
3503.859529	432261.051314	44.199655
3503.764505	432243.307268	44.204660
3503.640569	432239.370455	44.209665
3504.129156	432227.920461	44.214669
3504.188469	432222.531529	44.219674
3504.318191	432198.507584	44.224679
3504.227970	432195.985835	44.229684
3504.066300	432185.306521	44.234689
3504.097605	432150.287903	44.239693
3503.804317	432155.767625	44.244698
3504.401130	432141.102239	44.249703
3504.041638	432123.301770	44.254708
3504.086867	432105.990367	44.259713
3504.173433	432089.636030	44.264717
3503.986232	432070.030058	44.269722
3504.132389	432066.757516	44.274727
3503.661855	432050.244555	44.279732
3503.697459	432038.059906	44.284737
3504.251523	432029.795520	44.289741
3503.976801	432023.448693	44.294746
3503.951125	432002.698710	44.299751
3503.972542	431990.161249	44.304756
3503.817414	431988.158003	44.309761
3503.768037	431968.426923	44.314765
3503.573904	431959.326122	44.319770
3503.521225	431947.207244	44.324775
3503.389847	431955.196588	44.329780
3503.191948	431953.758831	44.334785
3503.651842	431953.172899	44.339789
3503.350187	431963.830023	44.344794
3503.212657	431959.946228	44.349799
3503.470209	431956.806883	44.354804
3503.617542	431948.814894	44.359809
3503.663724	431928.103319	44.364813
3503.332653	431920.395985	44.369818
3503.838147	431913.002506	44.374823
3503.845163	431915.437083	44.379828
3503.763499	431915.603299	44.384833
3504.137118	431883.671986	44.389837
3503.875923	431879.657059	44.394842
3503.773675	431869.271920	44.399847
3503.953800	431871.270986	44.404852
3503.611520	431850.219714	44.409857
3503.857340	431839.419916	44.414861
3503.759178	431842.735118	44.419866
3503.692507	431835.185589	44.424871
3503.998267	431819.656293	44.429876
3503.240733	431805.272694	44.434881
3503.633378	431792.773228	44.439885
3503.444938	431799.503749	44.444890
3503.575117	431800.547200	44.449895
3503.739844	431802.396667	44.454900
3503.688831	431786.776035	44.459905
3503.632093	431766.132633	44.464909
3503.675019	431777.745901	44.469914
3503.485300	431771.739704	44.474919
3503.586030	431765.227209	44.479924
3503.262825	431766.145097	44.484929
3503.555440	431770.205501	44.489933
3503.607451	431755.988111	44.494938
3503.124624	431732.017529	44.499943
3503.528270	431738.393245	44.504948
3503.638780	431739.237078	44.509953
3503.595734	431729.805919	44.514957
3503.493705	431740.936508	44.519962
3503.974996	431737.606696	44.524967
3504.055967	431712.118969	44.529972
3503.715095	431701.977478	44.534977
3503.826689	431693.027350	44.539981
3503.877276	431694.338121	44.544986
3503.761114	431684.817938	44.549991
3503.759736	431667.361930	44.554996
3503.699991	431659.100729	44.560001
3503.952912	431657.433741	44.565005
3503.724415	431651.484879	44.570010
3503.739264	431627.378466	44.575015
3503.861590	431624.668127	44.580020
3503.598050	431624.205714	44.585025
3503.935027	431621.052762	44.590029
3503.648785	431607.704959	44.595034
3503.573828	431585.643642	44.600039
3503.308878	431585.688922	44.605044
3503.157103	431584.801462	44.610049
3503.651895	431582.534972	44.615053
3503.468535	431585.154326	44.620058
3503.761946	431584.749049	44.625063
3503.987834	431575.779359	44.630068
3503.360820	431559.292765	44.635073
3503.587925	431542.609574	44.640077
3503.746511	431542.024336	44.645082
3503.668728	431539.246665	44.650087
3503.766305	431535.880852	44.655092
3503.810654	431521.207918	44.660097
3503.898975	431504.802123	44.665101
3503.745616	431507.619345	44.670106
3503.807798	431503.752117	44.675111
3503.555318	431483.598595	44.680116
3503.274128	431470.097613	44.685121
3503.570058	431453.808570	44.690125
3504.093600	431459.504200	44.695130
3503.885584	431455.784592	44.700135
3503.673788	431441.815035	44.705140
3503.707418	431428.057292	44.710145
3503.981014	431418.216721	44.715149
3503.506720	431428.599095	44.720154
3503.523481	431423.115752	44.725159
3503.703442	431411.667309	44.730164
3503.325235	431394.833640	44.735169
3504.138168	431386.626315	44.740173
3503.686378	431383.455776	44.745178
3503.770599	431385.978717	44.750183
3503.809011	431374.757407	44.755188
3503.378470	431364.174368	44.760193
3503.849976	431349.580626	44.765197
3503.660632	431353.114450	44.770202
3503.350725	431356.059911	44.775207
3503.575033	431350.135147	44.780212
3503.536183	431352.932834	44.785217
3503.525775	431334.158728	44.790221
3503.536186	431323.297395	44.795226
3503.757956	431313.719359	44.800231
3503.407994	431317.026885	44.805236
3503.435230	431312.302914	44.810241
3503.340753	431312.319085	44.815245
3503.189028	431320.159884	44.820250
3503.528401	431313.048310	44.825255
3503.494040	431309.045297	44.830260
3503.522796	431289.300297	44.835265
3503.456715	431278.249021	44.840269
3503.498180	431277.074824	44.845274
3503.396629	431275.417589	44.850279
3503.215476	431275.347068	44.855284
3503.309737	431277.005627	44.860289
3503.568524	431268.080947	44.865293
3503.484558	431274.996765	44.870298
3503.487350	431277.635113	44.875303
3503.359047	431275.424241	44.880308
3503.409660	431266.585853	44.885313
3503.481111	431247.696208	44.890317
3503.315987	431245.187144	44.895322
3503.438707	431231.769294	44.900327
3503.621312	431240.770936	44.905332
3503.604207	431240.621658	44.910337
3503.564235	431238.598684	44.915341
3503.185889	431244.803587	44.920346
3503.513226	431239.622391	44.925351
3503.524562	431240.077209	44.930356
3503.521831	431222.062890	44.935361
3503.658741	431217.472412	44.940365
3503.437941	431214.211661	44.945370
3503.555574	431210.131933	44.950375
3503.495670	431207.655645	44.955380
3503.215688	431220.694472	44.960385
3503.704895	431212.542363	44.965389
3503.514261	431211.509286	44.970394
3503.430775	431196.502753	44.975399
3503.470494	431178.734883	44.980404
3503.395085	431170.729913	44.985409
3503.563006	431174.913207	44.990413
3503.194966	431186.698436	44.995418
3503.629435	431174.090005	45.000423
3503.382505	431169.006850	45.005428
3503.319099	431169.880400	45.010433
3503.584396	431175.873927	45.015437
3503.669129	431178.599787	45.020442
3503.445302	431152.859013	45.025447
3503.516564	431143.712575	45.030452
3503.532967	431139.751612	45.035457
3503.660614	431127.347784	45.040461
3503.396798	431141.652549	45.045466
3503.619515	431131.617561	45.050471
3503.798034	431129.202046	45.055476
3503.293670	431117.971799	45.060481
3503.645462	431104.108791	45.065485
3503.654732	431101.823666	45.070490
3503.668777	431094.260112	45.075495
3503.478252	431098.606117	45.080500
3503.443539	431106.224023	45.085505
3503.514564	431088.958202	45.090509
3503.671571	431091.418000	45.095514
3503.418387	431076.897081	45.100519
3503.568540	431077.023721	45.105524
3503.057607	431074.116968	45.110529
3503.396292	431063.808418	45.115533
3503.408936	431070.758546	45.120538
3503.350814	431077.974488	45.125543
3503.435962	431067.354006	45.130548
3503.204869	431080.993519	45.135553
3503.511316	431066.377037	45.140557
3503.656778	431078.176133	45.145562
3503.537348	431056.324892	45.150567
3503.599146	431041.953154	45.155572
3503.689548	431041.633279	45.160577
3503.668889	431025.347247	45.165581
3503.662060	431037.020128	45.170586
3503.524798	431032.730160	45.175591
3503.597887	431007.445991	45.180596
3503.332006	431003.685443	45.185601
3503.637098	430995.361711	45.190605
3503.432448	431002.196723	45.195610
3503.651553	430992.416024	45.200615
3503.786872	431001.324340	45.205620
3503.643225	430993.990666	45.210625
3503.764792	430966.668314	45.215629
3503.659039	430958.008748	45.220634
3503.366115	430963.590180	45.225639
3503.538756	430958.993549	45.230644
3503.747132	430949.163917	45.235649
3503.847178	430947.928955	45.240653
3503.644901	430931.927602	45.245658
3503.514281	430920.836428	45.250663
3503.716585	430919.228778	45.255668
3503.283223	430927.270038	45.260673
3503.525539	430924.386890	45.265677
3503.473947	430923.989765	45.270682
3503.462624	430912.472244	45.275687
3503.543556	430892.261278	45.280692
3503.784498	430893.742578	45.285697
3504.011917	430886.041030	45.290701
3503.664444	430881.989914	45.295706
3503.671955	430875.848314	45.300711
3503.859451	430857.547498	45.305716
3503.761752	430850.053692	45.310721
3503.694987	430852.754712	45.315725
3503.547784	430856.027682	45.320730
3503.762268	430848.683558	45.325735
3503.631977	430822.418978	45.330740
3503.800976	430822.034933	45.335745
3503.918917	430812.271431	45.340749
3504.011630	430810.733233	45.345754
3503.813071	430793.665465	45.350759
3503.755542	430781.394565	45.355764
3503.302342	430778.731652	45.360769
3503.492312	430772.660363	45.365773
3503.449133	430776.473799	45.370778
3503.668238	430766.693005	45.375783
3503.833613	430746.365999	45.380788
3503.670915	430738.223544	45.385793
3503.752034	430735.012667	45.390797
3503.725049	430745.268219	45.395802
3503.541587	430721.955933	45.400807
3503.539184	430713.227881	45.405812
3503.398534	430699.397970	45.410817
3503.420335	430701.931644	45.415821
3503.302587	430702.966731	45.420826
3503.500732	430695.270119	45.425831
3503.651552	430688.190551	45.430836
3503.373939	430694.378398	45.435841
3503.374963	430694.479757	45.440845
3503.137918	430698.224813	45.445850
3503.035963	430704.027435	45.450855
3503.709704	430690.515187	45.455860
3503.573608	430691.959384	45.460865
3503.556783	430667.908131	45.465869
3503.607204	430660.338225	45.470874
3503.690580	430658.598622	45.475879
3503.884819	430661.711823	45.480884
3503.988259	430662.506156	45.485889
3504.122751	430636.145407	45.490893
3504.077569	430635.493447	45.495898
3503.924851	430619.077437	45.500903
3503.975637	430591.715985	45.505908
3503.513174	430583.523166	45.510913
3503.681752	430581.819756	45.515917
3503.602089	430580.260228	45.520922
3503.532889	430570.021106	45.525927
3503.462597	430548.719220	45.530932
3503.446591	430552.122072	45.535937
3503.362033	430538.739216	45.540941
3503.526337	430546.120333	45.545946
3503.230188	430544.851505	45.550951
3503.575021	430544.792664	45.555956
3503.431412	430541.315648	45.560961
3503.620280	430540.826711	45.565965
3503.541463	430538.962550	45.570970
3503.394975	430517.673646	45.575975
3503.463030	430501.321352	45.580980
3503.004588	430502.363874	45.585985
3503.285032	430490.948569	45.590989
3503.580437	430502.519364	45.595994
3503.525012	430509.887264	45.600999
3503.601138	430501.196471	45.606004
3503.396486	430499.556784	45.611009
3503.593983	430500.994781	45.616013
3503.699672	430497.728929	45.621018
3503.596078	430483.841815	45.626023
3503.602269	430474.807721	45.631028
3503.639272	430474.852189	45.636033
3503.849764	430476.490959	45.641037
3503.504834	430480.000733	45.646042
3503.267862	430463.091524	45.651047
3503.650674	430443.640585	45.656052
3503.721520	430434.798426	45.661057
3503.486820	430432.707136	45.666061
3503.466769	430432.456860	45.671066
3503.734607	430432.969391	45.676071
3503.778632	430428.242374	45.681076
3503.334959	430416.037216	45.686081
3503.542078	430403.873172	45.691085
3503.836435	430400.727335	45.696090
3503.663937	430394.717840	45.701095
3503.990397	430396.083075	45.706100
3503.941783	430387.261296	45.711105
3503.856066	430365.200658	45.716109
3504.183966	430366.667145	45.721114
3504.041385	430362.936187	45.726119
3503.969647	430331.434025	45.731124
3503.718612	430330.614213	45.736129
3503.878646	430318.052181	45.741133
3504.026224	430308.384904	45.746138
3504.079457	430288.076648	45.751143
3503.969608	430284.644577	45.756148
3503.615964	430269.074598	45.761153
3503.499860	430258.488111	45.766157
3503.393562	430249.676129	45.771162
3502.982973	430243.757997	45.776167
3503.166308	430239.260896	45.781172
3503.094368	430243.282322	45.786177
3503.374761	430240.747825	45.791181
3503.432000	430244.696445	45.796186
3503.249064	430241.784329	45.801191
3503.725645	430236.780422	45.806196
3503.522172	430245.746877	45.811201
3503.549801	430237.165763	45.816205
3503.510839	430248.286297	45.821210
3503.413656	430229.576865	45.826215
3503.618044	430215.028025	45.831220
3503.385420	430216.640979	45.836225
3503.501299	430208.044786	45.841229
3503.181989	430208.606829	45.846234
3503.353706	430203.451978	45.851239
3503.541565	430202.861710	45.856244
3503.364185	430205.226455	45.861249
3503.197641	430202.260786	45.866253
3503.144285	430203.234152	45.871258
3503.202696	430205.406391	45.876263
3503.473544	430197.443460	45.881268
3503.253091	430203.114194	45.886273
3503.639187	430204.773747	45.891277
3503.725495	430202.830617	45.896282
3503.393538	430174.620561	45.901287
3503.736594	430164.209371	45.906292
3503.303264	430163.725170	45.911297
3503.568604	430166.065073	45.916301
3503.657520	430173.865167	45.921306
3503.490679	430170.696552	45.926311
3503.819676	430164.956606	45.931316
3503.506097	430147.705010	45.936321
3503.611185	430143.069006	45.941325
3503.524557	430140.647916	45.946330
3503.358877	430143.873391	45.951335
3503.471491	430131.420852	45.956340
3503.424041	430135.184373	45.961345
3503.410619	430136.303168	45.966349
3503.528022	430118.876465	45.971354
3503.208984	430105.330403	45.976359
3503.586090	430098.110521	45.981364
3503.411185	430097.379199	45.986369
3503.784640	430095.691520	45.991373
3503.504364	430101.676985	45.996378
3503.771545	430090.466743	46.001383
3503.722116	430088.749774	46.006388
3503.412219	430075.049889	46.011393
3503.571982	430056.702433	46.016397
3503.713693	430056.576778	46.021402
3503.112865	430059.115338	46.026407
3503.807166	430054.886194	46.031412
3503.358610	430055.622555	46.036417
3503.700864	430054.904423	46.041421
3503.548368	430037.828236	46.046426
3503.085840	430027.453041	46.051431
3503.374199	430020.349786	46.056436
3503.199896	430020.988571	46.061441
3503.267205	430020.114391	46.066445
3503.632618	430022.132729	46.071450
3503.177135	430028.148129	46.076455
3503.313101	430027.921958	46.081460
3503.596981	430026.300318	46.086465
3503.661774	430027.608757	46.091469
3503.723636	430022.269630	46.096474
3503.437361	430013.539038	46.101479
3503.650795	429998.328787	46.106484
3503.247514	429993.728809	46.111489
3503.312283	429978.442432	46.116493
3503.218837	429984.396025	46.121498
3502.943675	429990.786635	46.126503
3503.319485	429981.942981	46.131508
3503.211077	429989.370840	46.136513
3503.364984	429990.004332	46.141517
3503.564860	429983.271416	46.146522
3503.265425	429996.111252	46.151527
3503.634992	429991.836047	46.156532
3503.721007	429993.597603	46.161537
3503.245637	429980.179660	46.166541
3503.355636	429963.210843	46.171546
3503.131560	429961.980424	46.176551
3503.825925	429962.217142	46.181556
3503.357981	429956.460976	46.186561
3503.621825	429955.197994	46.191565
3503.752979	429954.109915	46.196570
3503.275036	429956.982744	46.201575
3503.407337	429957.416932	46.206580
3503.609893	429961.949772	46.211585
3503.735542	429944.420033	46.216589
3503.673399	429931.641987	46.221594
3503.740009	429931.173913	46.226599
3503.730120	429920.416890	46.231604
3503.874901	429923.792380	46.236609
3504.091288	429903.455931	46.241613
3504.082330	429883.462436	46.246618
3503.847485	429887.460989	46.251623
3504.324365	429875.808848	46.256628
3504.058298	429855.047247	46.261633
3503.917086	429836.852508	46.266637
3503.980850	429823.088672	46.271642
3503.628735	429815.637975	46.276647
3503.896111	429807.066516	46.281652
3503.549854	429804.435977	46.286657
3503.620940	429792.294843	46.291661
3503.573400	429777.281257	46.296666
3503.766284	429769.077748	46.301671
3504.303382	429764.012660	46.306676
3503.671630	429768.079005	46.311681
3503.727556	429746.298093	46.316685
3503.837378	429728.618647	46.321690
3503.416602	429736.505917	46.326695
3504.044575	429727.771359	46.331700
3503.657044	429727.025581	46.336705
3503.897908	429699.275383	46.341709
3503.912359	429695.010012	46.346714
3503.744712	429686.868035	46.351719
3503.679128	429677.998136	46.356724
3503.132945	429664.592102	46.361729
3503.597090	429655.276498	46.366733
3503.592860	429645.076626	46.371738
3503.647975	429647.350978	46.376743
3503.768697	429646.416914	46.381748
3503.450326	429645.557826	46.386753
3503.472081	429640.986701	46.391757
3503.626330	429635.885458	46.396762
3503.341771	429619.339008	46.401767
3503.361980	429604.719740	46.406772
3503.419093	429612.119456	46.411777
3503.350537	429606.447256	46.416781
3503.400919	429604.154964	46.421786
3503.157101	429610.337326	46.426791
3503.647989	429598.327409	46.431796
3503.513413	429604.643368	46.436801
3503.547669	429608.849768	46.441805
3503.715455	429613.236365	46.446810
3503.514169	429586.931768	46.451815
3503.606319	429578.745392	46.456820
3503.411749	429581.722129	46.461825
3503.543268	429578.451739	46.466829
3503.695571	429583.145483	46.471834
3503.725241	429582.886708	46.476839
3503.682583	429559.498469	46.481844
3503.540382	429536.279453	46.486849
3503.588615	429537.895246	46.491853
3503.709786	429536.605853	46.496858
3503.589562	429536.829420	46.501863
3503.661242	429522.810307	46.506868
3503.617230	429514.190412	46.511873
3503.756416	429495.389283	46.516877
3503.828670	429495.173986	46.521882
3503.343180	429495.459921	46.526887
3503.435041	429492.602288	46.531892
3503.479694	429501.272911	46.536897
3503.243511	429489.691584	46.541901
3503.464629	429478.488916	46.546906
3503.131964	429456.571087	46.551911
3503.044320	429448.516865	46.556916
3503.068647	429462.874956	46.561921
3503.190677	429470.720380	46.566925
3503.403647	429468.603313	46.571930
3503.197642	429466.405535	46.576935
3503.502639	429450.722547	46.581940
3503.152281	429458.547136	46.586945
3503.284751	429454.160069	46.591949
3502.914556	429451.279828	46.596954
3502.824020	429453.477570	46.601959
3503.194044	429452.094931	46.606964
3503.067634	429471.147741	46.611969
3503.055210	429491.297567	46.616973
3503.349543	429497.641818	46.621978
3503.264247	429492.226198	46.626983
3503.264347	429476.443038	46.631988
3503.148239	429468.799682	46.636993
3503.425408	429452.563199	46.641997
3503.686347	429454.396427	46.647002
3503.284924	429460.351990	46.652007
3503.844618	429451.375240	46.657012
3503.321884	429459.178512	46.662017
3503.459514	429457.734055	46.667021
3503.373269	429459.626565	46.672026
3503.204665	429466.303620	46.677031
3503.416758	429455.406981	46.682036
3503.281952	429463.702261	46.687041
3503.369904	429465.463526	46.692045
3503.681070	429452.824475	46.697050
3503.184389	429437.785863	46.702055
3503.287829	429423.253769	46.707060
3503.702799	429427.141445	46.712065
3503.575040	429429.650044	46.717069
3503.430206	429430.639062	46.722074
3503.742636	429430.433504	46.727079
3503.680319	429420.852451	46.732084
3503.383273	429400.400236	46.737089
3503.859814	429385.347662	46.742093
3503.545911	429382.610051	46.747098
3502.945206	429395.400156	46.752103
3503.572699	429388.695554	46.757108
3503.481038	429392.923493	46.762113
3503.259764	429393.316564	46.767117
3503.230090	429393.626170	46.772122
3503.297062	429397.827021	46.777127
3503.549936	429384.487387	46.782132
3503.397993	429388.421120	46.787137
3503.278645	429371.338786	46.792141
3503.506962	429360.642333	46.797146
3503.694686	429362.538820	46.802151
3503.834542	429355.765222	46.807156
3503.357533	429357.876712	46.812161
3503.163874	429354.255815	46.817165
3503.520603	429346.277932	46.822170
3503.744399	429355.476270	46.827175
3503.576263	429335.357237	46.832180
3503.688132	429318.489135	46.837185
3503.495429	429317.659325	46.842189
3504.047444	429312.490094	46.847194
3503.939893	429318.294014	46.852199
3503.933824	429299.466780	46.857204
3504.084812	429289.849252	46.862209
3503.880010	429279.632719	46.867213
3503.747601	429270.926327	46.872218
3503.461533	429250.472106	46.877223
3503.525447	429243.000939	46.882228
3503.518041	429250.005783	46.887233
3503.780978	429241.637877	46.892237
3503.842372	429232.441627	46.897242
3503.457641	429229.411589	46.902247
3503.371848	429206.487116	46.907252
3503.466001	429202.766301	46.912257
3503.374575	429204.355213	46.917261
3503.377488	429204.202504	46.922266
3503.577711	429201.833837	46.927271
3503.364644	429205.118282	46.932276
3503.353887	429206.439668	46.937281
3503.302922	429206.397659	46.942285
3503.542811	429204.580474	46.947290
3503.135933	429207.390508	46.952295
3503.165195	429208.400558	46.957300
3503.482700	429207.026873	46.962305
3503.387047	429194.152646	46.967309
3503.549508	429173.672522	46.972314
3503.176774	429167.138645	46.977319
3503.254188	429156.823120	46.982324
3503.192224	429166.273328	46.987329
3503.370328	429168.069973	46.992333
3503.731474	429154.051965	46.997338
3503.352976	429163.099468	47.002343
3503.209886	429169.924502	47.007348
3503.438291	429167.246517	47.012353
3503.538029	429154.085152	47.017357
3503.311303	429168.283288	47.022362
3503.260941	429169.611438	47.027367
3503.402429	429159.386474	47.032372
3503.398356	429165.578766	47.037377
3503.627254	429137.373195	47.042381
3503.304679	429136.362552	47.047386
3503.718052	429136.799513	47.052391
3503.912694	429132.452522	47.057396
3503.509725	429128.359823	47.062401
3503.474081	429125.320916	47.067405
3503.510887	429114.251047	47.072410
3503.122009	429096.960782	47.077415
3503.212897	429084.815901	47.082420
3503.566758	429086.075036	47.087425
3503.420405	429082.192265	47.092429
3503.641757	429088.244586	47.097434
3503.183687	429094.920422	47.102439
3503.487926	429087.560422	47.107444
3503.433060	429095.385426	47.112449
3503.343984	429095.045420	47.117453
3503.419191	429089.703802	47.122458
3503.299423	429097.387636	47.127463
3503.420430	429089.500666	47.132468
3503.275856	429069.225130	47.137473
3503.174529	429057.772815	47.142477
3503.355792	429053.478844	47.147482
3503.347790	429053.886255	47.152487
3503.399948	429046.620036	47.157492
3503.117127	429056.463255	47.162497
3503.456611	429051.787012	47.167501
3503.708060	429053.977148	47.172506
3503.616997	429057.951291	47.177511
3503.825179	429056.241010	47.182516
3503.401713	429056.465608	47.187521
3503.254535	429045.680876	47.192525
3503.546682	429023.706706	47.197530
3503.438142	429026.770325	47.202535
3503.222373	429015.236029	47.207540
3503.276320	429020.910944	47.212545
3503.387083	429021.044323	47.217549
3503.035903	429015.115733	47.222554
3502.865525	429022.199224	47.227559
3503.297864	429017.050363	47.232564
3503.329507	429022.932090	47.237569
3503.606308	429020.296576	47.242573
3503.603605	429020.500079	47.247578
3503.464586	429025.395930	47.252583
3503.991111	429023.631290	47.257588
3503.765627	429011.489642	47.262593
3503.592473	428996.040247	47.267597
3503.564126	428989.447518	47.272602
3503.552993	428994.270788	47.277607
3503.878788	428978.380931	47.282612
3503.716812	428977.951870	47.287617
3503.580750	428964.018647	47.292621
3503.642478	428945.839316	47.297626
3503.578328	428940.013949	47.302631
3503.617899	428939.753477	47.307636
3503.718316	428939.584117	47.312641
3503.473374	428932.470094	47.317645
3503.662344	428909.650669	47.322650
3503.594400	428908.596539	47.327655
3503.760546	428897.859740	47.332660
3503.610871	428901.945420	47.337665
3503.518199	428897.596693	47.342669
3503.262804	428895.559548	47.347674
3503.468879	428898.670965	47.352679
3503.507207	428883.337639	47.357684
3503.616045	428875.300423	47.362689
3503.555202	428863.485843	47.367693
3503.618740	428853.324807	47.372698
3503.238745	428863.336951	47.377703
3503.727455	428854.625851	47.382708
3503.568905	428865.310700	47.387713
3503.388091	428842.554351	47.392717
3503.710086	428832.095418	47.397722
3503.408059	428833.212803	47.402727
3503.587697	428824.858974	47.407732
3503.791119	428837.207569	47.412737
3503.753159	428825.287560	47.417741
3503.531693	428818.474001	47.422746
3503.339176	428803.992060	47.427751
3503.549030	428780.509178	47.432756
3503.611314	428784.964696	47.437761
3503.518898	428788.380852	47.442765
3503.769099	428789.200941	47.447770
3503.408689	428790.734307	47.452775
3503.616124	428789.176388	47.457780
3503.463547	428774.180096	47.462785
3503.285456	428763.603518	47.467789
3503.711257	428745.209613	47.472794
3503.386066	428757.293251	47.477799
3503.472081	428743.727989	47.482804
3503.439899	428747.184616	47.487809
3503.183581	428744.589350	47.492813
3503.504762	428747.427376	47.497818
3503.203101	428757.121682	47.502823
3503.532671	428749.858755	47.507828
3503.893860	428749.797121	47.512833
3503.619848	428735.532058	47.517837
3503.858773	428714.632468	47.522842
3503.783658	428715.964871	47.527847
3503.905400	428711.528747	47.532852
3503.473654	428698.863890	47.537857
3503.419468	428691.311210	47.542861
3503.623422	428675.137445	47.547866
3503.732798	428687.806686	47.552871
3503.671329	428677.920677	47.557876
3503.845912	428681.139003	47.562881
3503.306184	428663.823425	47.567885
3503.599847	428642.812922	47.572890
3503.458456	428646.085206	47.577895
3503.503858	428632.425311	47.582900
3503.813679	428635.519049	47.587905
3503.783557	428629.332534	47.592909
3503.775218	428621.772004	47.597914
3503.566578	428604.653607	47.602919
3503.731261	428592.546625	47.607924
3503.481398	428596.801719	47.612929
3503.610095	428589.979055	47.617933
3503.678869	428585.907214	47.622938
3503.284569	428578.463324	47.627943
3503.277593	428557.098065	47.632948
3503.233036	428550.609484	47.637953
3503.385567	428555.607905	47.642957
3503.597427	428553.541698	47.647962
3503.319200	428558.055401	47.652967
3503.432968	428554.940156	47.657972
3503.338190	428555.413144	47.662977
3503.616252	428556.736003	47.667981
3503.591884	428549.330442	47.672986
3503.385818	428561.901357	47.677991
3503.583180	428545.931636	47.682996
3503.668955	428533.381330	47.688001
3503.442512	428521.391847	47.693005
3503.532367	428523.203610	47.698010
3503.341371	428524.352803	47.703015
3503.531101	428517.012178	47.708020
3503.664007	428525.008317	47.713025
3503.588112	428526.543871	47.718029
3503.817742	428497.880642	47.723034
3503.530641	428491.382707	47.728039
3503.209332	428485.195122	47.733044
3503.358481	428479.992997	47.738049
3503.025765	428484.566770	47.743053
3503.140316	428482.872435	47.748058
3503.025483	428481.775539	47.753063
3503.191785	428476.671988	47.758068
3503.084593	428480.953494	47.763073
3503.328780	428484.362970	47.768077
3503.082817	428485.318542	47.773082
3502.756874	428489.738902	47.778087
3503.568782	428484.372859	47.783092
3503.446546	428481.450158	47.788097
3503.394593	428476.383873	47.793101
3503.874425	428483.407254	47.798106
3503.480435	428491.797883	47.803111
3503.529440	428485.394811	47.808116
3503.584206	428459.501999	47.813121
3503.170909	428450.843264	47.818125
3502.934165	428445.656270	47.823130
3503.180831	428445.309679	47.828135
3503.158023	428450.541070	47.833140
3502.887383	428454.647481	47.838145
3503.072057	428471.922413	47.843149
3503.320477	428476.092448	47.848154
3503.146001	428492.971921	47.853159
3503.224547	428486.157791	47.858164
3503.110451	428486.228064	47.863169
3502.753328	428488.978934	47.868173
3503.336620	428487.610578	47.873178
3503.679241	428497.093475	47.878183
3503.404456	428480.087786	47.883188
3503.515427	428461.645914	47.888193
3503.613900	428453.661076	47.893197
3503.687241	428449.842192	47.898202
3503.498127	428458.248602	47.903207
3503.120121	428457.095138	47.908212
3503.435532	428452.372137	47.913217
3503.388271	428461.718613	47.918221
3503.218664	428454.591581	47.923226
3503.198797	428460.583748	47.928231
3503.270565	428454.582798	47.933236
3503.349386	428455.178402	47.938241
3503.129454	428453.541179	47.943245
3503.319703	428449.651580	47.948250
3503.145783	428452.320421	47.953255
3503.301292	428451.177362	47.958260
3503.330275	428432.394203	47.963265
3503.003589	428427.831586	47.968269
3503.184436	428436.885363	47.973274
3503.238825	428449.716377	47.978279
3503.248368	428433.321882	47.983284
3503.637822	428426.302390	47.988289
3503.399713	428426.444591	47.993293
3503.560445	428413.475406	47.998298
3503.470165	428421.154424	48.003303
3503.460536	428422.069645	48.008308
3503.278219	428418.548170	48.013313
3503.245997	428427.283067	48.018317
3503.484930	428420.390779	48.023322
3503.608374	428418.593418	48.028327
3503.618597	428412.907478	48.033332
3503.498128	428391.003174	48.038337
3503.393540	428390.361294	48.043341
3503.609229	428378.905270	48.048346
3503.710293	428389.495252	48.053351
3503.738448	428385.988586	48.058356
3503.782821	428385.625784	48.063361
3503.753717	428367.461516	48.068365
3503.517689	428353.037479	48.073370
3503.268177	428352.521848	48.078375
3503.449990	428347.720134	48.083380
3503.608656	428347.337815	48.088385
3503.434731	428350.666447	48.093389
3503.937536	428330.381238	48.098394
3503.281549	428317.043933	48.103399
3503.319093	428311.048789	48.108404
3503.804556	428313.452799	48.113409
3503.192397	428312.948336	48.118413
3503.358580	428303.784583	48.123418
3503.543268	428312.888504	48.128423
3503.689968	428307.483749	48.133428
3503.775198	428307.824501	48.138433
3503.784866	428292.546438	48.143437
3504.034033	428268.193544	48.148442
3503.995192	428271.955893	48.153447
3504.008878	428268.197918	48.158452
3503.808559	428243.363472	48.163457
3503.898423	428235.380030	48.168461
3503.736847	428225.866192	48.173466
3503.978053	428218.465933	48.178471
3503.672490	428199.181434	48.183476
3503.541227	428198.848618	48.188481
3503.734070	428193.638969	48.193485
3503.406061	428195.319097	48.198490
3503.279846	428190.925215	48.203495
3503.321378	428189.649348	48.208500
3503.556523	428169.257447	48.213505
3503.555246	428156.214279	48.218509
3503.380408	428144.621814	48.223514
3503.217752	428146.527475	48.228519
3503.155776	428151.105836	48.233524
3503.118519	428153.446859	48.238529
3503.250831	428150.277642	48.243533
3503.471892	428137.856284	48.248538
3503.566504	428145.503822	48.253543
3502.942676	428142.463714	48.258548
3503.254668	428145.201877	48.263553
3503.452620	428149.532845	48.268557
3503.663534	428143.355798	48.273562
3503.301375	428157.323903	48.278567
3503.266365	428149.412507	48.283572
3503.644580	428152.900652	48.288577
3503.255328	428128.352109	48.293581
3503.611881	428115.095561	48.298586
3503.336807	428118.746012	48.303591
3503.313193	428119.003847	48.308596
3503.578344	428108.909571	48.313601
3503.422104	428105.332843	48.318605
3503.391887	428111.682135	48.323610
3503.298882	428116.316553	48.328615
3503.509367	428105.571824	48.333620
3503.701134	428100.362338	48.338625
3503.341028	428096.871172	48.343629
3503.557633	428080.441076	48.348634
3503.421056	428080.007660	48.353639
3503.419148	428078.028666	48.358644
3504.021654	428080.158951	48.363649
3504.031231	428076.756916	48.368653
3503.841462	428055.828438	48.373658
3503.479542	428044.978408	48.378663
3503.692955	428043.165656	48.383668
3503.954783	428032.564386	48.388673
3503.768197	428035.184683	48.393677
3503.833000	428004.518885	48.398682
3503.887406	427997.759489	48.403687
3503.793289	427996.253009	48.408692
3503.854810	427994.364683	48.413697
3503.716255	427973.122869	48.418701
3503.639098	427959.940290	48.423706
3503.567414	427958.683743	48.428711
3503.535388	427954.730511	48.433716
3503.429745	427949.165750	48.438721
3503.144813	427964.491115	48.443725
3502.970596	427958.481288	48.448730
3502.952433	427960.260785	48.453735
3503.190028	427963.874475	48.458740
3503.329169	427961.769881	48.463745
3503.160270	427955.200861	48.468749
3503.217437	427957.627286	48.473754
3503.017571	427967.000015	48.478759
3503.490303	427960.321438	48.483764
3503.666801	427957.702934	48.488769
3503.201307	427959.000530	48.493773
3503.465206	427945.911967	48.498778
3502.962601	427933.005031	48.503783
3503.127065	427916.989750	48.508788
3503.696840	427927.296895	48.513793
3503.361418	427930.754667	48.518797
3503.495223	427922.712863	48.523802
3503.577144	427935.894728	48.528807
3503.451179	427924.598328	48.533812
3503.190075	427922.409813	48.538817
3503.125533	427928.917274	48.543821
3503.006372	427928.836154	48.548826
3503.203782	427936.922984	48.553831
3503.075060	427920.348729	48.558836
3503.183822	427922.208064	48.563841
3503.238568	427927.324822	48.568845
3503.475428	427925.203539	48.573850
3503.261938	427925.544550	48.578855
3503.291289	427934.573634	48.583860
3503.554134	427925.037958	48.588865
3503.291787	427931.579194	48.593869
3503.273163	427928.841744	48.598874
3503.300739	427935.993265	48.603879
3503.101064	427933.337483	48.608884
3503.760734	427929.722918	48.613889
3503.362427	427909.438956	48.618893
3503.500778	427885.053837	48.623898
3503.430510	427882.629720	48.628903
3503.428357	427884.609502	48.633908
3503.600191	427883.514383	48.638913
3503.153891	427886.382055	48.643917
3503.691270	427885.123013	48.648922
3503.313399	427883.766483	48.653927
3503.108943	427887.049639	48.658932
3503.029553	427886.707962	48.663937
3502.858915	427888.970279	48.668941
3503.346607	427872.341491	48.673946
3503.423727	427881.057920	48.678951
3503.404470	427880.908987	48.683956
3503.464710	427888.460971	48.688961
3503.525606	427868.606096	48.693965
3503.340213	427853.767082	48.698970
3503.315215	427859.709524	48.703975
3503.249498	427851.041972	48.708980
3503.338604	427857.573971	48.713985
3503.344119	427859.349433	48.718989
3503.415845	427850.150880	48.723994
3503.348037	427855.085567	48.728999
3503.310867	427856.969824	48.734004
3503.347195	427856.405374	48.739009
3503.447656	427852.581763	48.744013
3503.888985	427851.745146	48.749018
3503.611208	427829.816429	48.754023
3503.443438	427822.841153	48.759028
3503.622177	427812.913766	48.764033
3503.348414	427816.208766	48.769037
3503.599440	427808.603689	48.774042
3503.203001	427819.075862	48.779047
3503.376715	427816.762338	48.784052
3503.629060	427812.049979	48.789057
3503.247374	427818.104089	48.794061
3503.150332	427811.573513	48.799066
3503.262807	427823.785909	48.804071
3503.211466	427808.010416	48.809076
3503.325607	427803.676927	48.814081
3503.365603	427791.032538	48.819085
3503.218625	427784.510481	48.824090
3503.190976	427777.511265	48.829095
3503.027433	427776.524161	48.834100
3503.265933	427776.483476	48.839105
3503.289088	427775.007711	48.844109
3503.291002	427773.434066	48.849114
3503.171982	427778.682034	48.854119
3503.150189	427778.787301	48.859124
3503.338954	427780.734493	48.864129
3503.031346	427784.441304	48.869133
3502.946561	427770.752388	48.874138
3503.048130	427784.489270	48.879143
3502.846428	427791.426217	48.884148
3503.023019	427806.926645	48.889153
3503.140382	427818.579922	48.894157
3503.106228	427813.611962	48.899162
3503.409685	427819.498331	48.904167
3503.119242	427825.892132	48.909172
3503.433120	427824.468236	48.914177
3503.008957	427829.666790	48.919181
3503.192288	427816.693419	48.924186
3503.527312	427827.903498	48.929191
3503.179763	427812.889133	48.934196
3503.477157	427801.875660	48.939201
3503.311799	427802.005441	48.944205
3503.589389	427784.803426	48.949210
3503.479764	427786.903075	48.954215
3503.653726	427786.822657	48.959220
3503.996658	427783.769688	48.964225
3503.825598	427784.712497	48.969229
3503.543638	427757.709083	48.974234
3503.489634	427752.490733	48.979239
3503.414339	427751.488559	48.984244
3503.673910	427747.891530	48.989249
3503.583259	427749.937188	48.994253
3503.779373	427747.924354	48.999258
3503.779843	427731.581675	49.004263
3503.493287	427716.759849	49.009268
3503.761532	427709.151800	49.014273
3503.137020	427706.822301	49.019277
3503.374823	427702.619940	49.024282
3503.419849	427710.073071	49.029287
3503.320847	427710.749811	49.034292
3503.356482	427709.931708	49.039297
3503.125987	427712.559538	49.044301
3503.385475	427702.567563	49.049306
3503.566249	427712.382934	49.054311
3503.213591	427683.259856	49.059316
3503.466679	427672.203135	49.064321
3503.207404	427664.634392	49.069325
3503.287798	427665.128241	49.074330
3503.325292	427668.014839	49.079335
3503.151141	427672.663199	49.084340
3503.246482	427662.902251	49.089345
3503.337674	427669.535452	49.094349
3503.331424	427665.983801	49.099354
3503.401700	427671.047209	49.104359
3503.476872	427668.039945	49.109364
3503.577575	427669.393139	49.114369
3503.502457	427679.861261	49.119373
3503.500447	427682.602341	49.124378
3503.597747	427676.393819	49.129383
3503.843154	427654.477114	49.134388
3503.861894	427641.430244	49.139393
3503.675495	427643.441507	49.144397
3503.706611	427638.056336	49.149402
3503.705247	427625.469674	49.154407
3503.457048	427609.270879	49.159412
3503.595490	427599.096514	49.164417
3503.578140	427602.906053	49.169421
3503.441118	427589.124444	49.174426
3503.692487	427597.303685	49.179431
3503.713739	427593.493557	49.184436
3503.446244	427567.401026	49.189441
3503.145153	427565.473074	49.194445
3503.467609	427544.202911	49.199450
3503.222836	427549.878433	49.204455
3503.259792	427555.861126	49.209460
3503.511911	427554.752284	49.214465
3503.335332	427556.558861	49.219469
3503.509623	427545.870814	49.224474
3503.595050	427555.042729	49.229479
3503.375483	427548.939033	49.234484
3503.469869	427560.190328	49.239489
3503.271646	427562.508140	49.244493
3503.585820	427537.483596	49.249498
3503.357342	427531.838203	49.254503
3503.376837	427521.887131	49.259508
3503.563050	427517.592038	49.264513
3503.510958	427515.672320	49.269517
3503.094971	427514.677554	49.274522
3503.192817	427519.381009	49.279527
3503.217494	427515.925562	49.284532
3503.316274	427517.583617	49.289537
3503.182042	427526.640788	49.294541
3503.311132	427518.244375	49.299546
3503.273470	427530.330296	49.304551
3503.110927	427526.196263	49.309556
3503.517307	427518.310796	49.314561
3503.053333	427526.764469	49.319565
3503.334681	427522.453132	49.324570
3503.240863	427529.625504	49.329575
3503.126853	427526.955049	49.334580
3503.526996	427520.694776	49.339585
3503.206500	427518.820888	49.344589
3503.400590	427514.981235	49.349594
3503.249109	427514.956386	49.354599
3503.221553	427502.272623	49.359604
3503.424546	427497.010334	49.364609
3503.361215	427490.270897	49.369613
3503.254737	427492.167018	49.374618
3503.389461	427496.102870	49.379623
3503.467933	427496.901575	49.384628
3503.529526	427491.967953	49.389633
3503.219333	427502.527047	49.394637
3503.360776	427495.955662	49.399642
3503.257040	427496.633217	49.404647
3503.045284	427491.086467	49.409652
3503.516741	427490.904497	49.414657
3503.574355	427499.827412	49.419661
3503.692448	427491.788146	49.424666
3503.564780	427482.420481	49.429671
3503.514569	427466.238535	49.434676
3503.676313	427457.278230	49.439681
3503.327717	427464.392616	49.444685
3503.494986	427453.908742	49.449690
3503.363705	427451.647261	49.454695
3503.464232	427450.006002	49.459700
3503.472895	427460.053883	49.464705
3503.500084	427455.075374	49.469709
3503.690715	427442.455832	49.474714
3503.388731	427422.967072	49.479719
3503.486644	427414.525191	49.484724
3503.344875	427408.915718	49.489729
3503.060234	427416.628248	49.494733
3503.264250	427409.487859	49.499738
3503.572945	427414.612121	49.504743
3503.524520	427415.940038	49.509748
3503.706037	427410.935169	49.514753
3502.986829	427411.870081	49.519757
3503.243094	427409.694685	49.524762
3503.194809	427420.919653	49.529767
3503.364409	427417.337937	49.534772
3503.503392	427405.691525	49.539777
3503.368527	427393.533570	49.544781
3503.367399	427378.307514	49.549786
3503.585059	427377.559828	49.554791
3503.476742	427375.395927	49.559796
3503.866958	427374.720285	49.564801
3503.796370	427370.824294	49.569805
3503.819777	427362.445872	49.574810
3503.455327	427351.189920	49.579815
3503.597618	427344.313823	49.584820
3503.561600	427334.016871	49.589825
3503.504071	427339.355945	49.594829
3503.988148	427334.400906	49.599834
3503.859328	427313.410610	49.604839
3503.380297	427305.219468	49.609844
3503.501206	427288.348374	49.614849
3503.329470	427297.818072	49.619853
3503.357524	427294.463525	49.624858
3503.392275	427290.092744	49.629863
3503.342055	427294.466245	49.634868
3503.824215	427286.872290	49.639873
3503.539153	427280.221408	49.644877
3503.647654	427253.455276	49.649882
3503.610595	427251.583723	49.654887
3503.443324	427252.982698	49.659892
3503.704274	427257.404582	49.664897
3503.311770	427264.526524	49.669901
3503.513218	427255.407100	49.674906
3503.442880	427238.416363	49.679911
3503.159887	427227.653989	49.684916
3503.863104	427214.794539	49.689921
3503.366886	427224.167408	49.694925
3503.552885	427217.588339	49.699930
3503.547548	427213.630426	49.704935
3503.555113	427217.841810	49.709940
3503.291694	427215.247586	49.714945
3503.454903	427213.849381	49.719949
3503.544025	427207.642134	49.724954
3503.541062	427187.696085	49.729959
3503.267653	427179.368279	49.734964
3503.285434	427174.949620	49.739969
3503.081302	427183.612819	49.744973
3503.267983	427178.607019	49.749978
3503.618516	427183.927206	49.754983
3503.214013	427183.793295	49.759988
3503.237484	427182.165176	49.764993
3503.145532	427185.530727	49.769997
3503.313076	427182.456875	49.775002
3503.414012	427185.738736	49.780007
3503.098687	427183.204126	49.785012
3503.547560	427176.478651	49.790017
3503.342615	427185.395762	49.795021
3503.399632	427179.244744	49.800026
3503.255230	427177.949816	49.805031
3503.346282	427187.729970	49.810036
3503.419427	427183.555633	49.815041
3503.291836	427162.006691	49.820045
3502.930189	427141.614301	49.825050
3502.823031	427161.173232	49.830055
3502.847185	427184.922368	49.835060
3503.412553	427171.578885	49.840065
3503.206708	427181.206718	49.845069
3503.388453	427187.266290	49.850074
3503.558798	427190.384035	49.855079
3503.299472	427165.609289	49.860084
3503.641639	427158.495991	49.865089
3503.508682	427148.012491	49.870093
3503.711570	427141.278253	49.875098
3503.450860	427145.992251	49.880103
3503.303075	427149.824134	49.885108
3503.427750	427140.616265	49.890113
3503.492660	427143.701265	49.895117
3503.245372	427133.947848	49.900122
3503.290113	427122.266634	49.905127
3503.135663	427118.587941	49.910132
3503.627121	427098.861925	49.915137
3503.451828	427101.328130	49.920141
3503.441029	427099.452082	49.925146
3503.643644	427102.259799	49.930151
3503.781229	427093.709521	49.935156
3503.686930	427094.436231	49.940161
3503.637009	427092.160823	49.945165
3503.770651	427075.236649	49.950170
3503.700459	427062.915217	49.955175
3503.319459	427055.214798	49.960180
3503.596776	427060.598270	49.965185
3503.380898	427065.862933	49.970189
3503.716558	427063.064889	49.975194
3503.585633	427055.372526	49.980199
3503.034385	427031.713340	49.985204
3503.467977	427022.706454	49.990209
3503.176374	427024.989507	49.995213
3503.286704	427016.646876	50.000218
3503.191336	427022.906073	50.005223
3503.022536	427033.796516	50.010228
3503.678969	427033.126164	50.015233
3503.256076	427030.203864	50.020237
3503.601071	427032.175198	50.025242
3503.465918	427025.346382	50.030247
3503.215486	427032.748665	50.035252
3503.168341	427026.919924	50.040257
3503.248527	427032.946122	50.045261
3503.006947	427021.719789	50.050266
3503.169780	427026.107714	50.055271
3503.210457	427034.932187	50.060276
3503.556948	427027.462826	50.065281
3503.159541	427034.839449	50.070285
3503.568148	427030.100254	50.075290
3503.513747	427024.831057	50.080295
3503.273108	427005.331478	50.085300
3503.305096	426983.298331	50.090305
3503.178785	426991.440760	50.095309
3503.304258	426983.958369	50.100314
3503.266763	426985.030668	50.105319
3503.105810	426989.575398	50.110324
3503.197805	426984.230439	50.115329
3503.223010	426989.758485	50.120333
3503.329736	426987.202544	50.125338
3503.550890	426992.900151	50.130343
3503.583805	426996.853470	50.135348
3503.596000	426991.116097	50.140353
3503.467055	426995.097054	50.145357
3503.518459	426995.494357	50.150362
3503.376515	426995.366368	50.155367
3502.935218	426993.919104	50.160372
3503.392815	426985.060370	50.165377
3503.400093	426990.033171	50.170381
3503.418478	426969.372721	50.175386
3503.434666	426952.367005	50.180391
3503.591205	426944.117969	50.185396
3503.773536	426947.335210	50.190401
3503.549045	426959.453322	50.195405
3503.490567	426948.297199	50.200410
3503.127153	426957.647496	50.205415
3503.336748	426957.053439	50.210420
3503.506557	426945.655315	50.215425
3503.611577	426928.076106	50.220429
3503.467902	426916.223942	50.225434
3503.420357	426906.436326	50.230439
3503.241750	426909.359915	50.235444
3503.559406	426907.427768	50.240449
3503.319013	426916.249521	50.245453
3503.600091	426906.152016	50.250458
3503.365476	426915.023539	50.255463
3503.377501	426914.107929	50.260468
3503.582839	426916.052364	50.265473
3503.372164	426888.325214	50.270477
3503.226129	426882.005769	50.275482
3503.880441	426875.092864	50.280487
3503.463443	426880.848708	50.285492
3503.700650	426870.048103	50.290497
3503.671164	426878.224794	50.295501
3503.358997	426871.882958	50.300506
3503.525191	426869.875159	50.305511
3503.455551	426854.761978	50.310516
3503.487571	426837.245922	50.315521
3503.637852	426835.545370	50.320525
3503.284578	426833.118713	50.325530
3503.643140	426827.575936	50.330535
3503.522962	426832.621288	50.335540
3503.700541	426842.386810	50.340545
3503.452581	426827.456326	50.345549
3503.518811	426807.345877	50.350554
3503.368849	426801.433125	50.355559
3503.236116	426804.957960	50.360564
3503.484767	426789.536611	50.365569
3503.064120	426793.973454	50.370573
3503.264607	426798.050459	50.375578
3503.306899	426786.166477	50.380583
3503.351436	426792.401846	50.385588
3503.592905	426796.015054	50.390593
3503.379084	426798.487869	50.395597
3503.546371	426792.216411	50.400602
3503.548305	426788.003409	50.405607
3503.236891	426778.565329	50.410612
3503.481694	426755.277498	50.415617
3503.505204	426752.938764	50.420621
3503.345351	426756.468237	50.425626
3503.581767	426751.758389	50.430631
3503.381901	426761.131592	50.435636
3503.503122	426755.527814	50.440641
3503.442704	426761.984134	50.445645
3503.650315	426758.852630	50.450650
3503.445542	426745.335878	50.455655
3503.206264	426729.642515	50.460660
3503.394191	426719.814616	50.465665
3503.265541	426717.806393	50.470669
3503.754499	426715.235913	50.475674
3503.574572	426717.550682	50.480679
3503.741205	426718.791161	50.485684
3503.720118	426713.262428	50.490689
3503.699761	426701.084566	50.495693
3503.572320	426677.352662	50.500698
3503.866892	426678.114496	50.505703
3503.254319	426680.198608	50.510708
3503.255285	426670.605635	50.515713
3503.499639	426669.193544	50.520717
3503.931661	426674.956734	50.525722
3504.116695	426651.577496	50.530727
3503.850191	426625.940564	50.535732
3504.103102	426592.652274	50.540737
3503.206408	426560.879890	50.545741
3503.205904	426507.535348	50.550746
3503.066720	426452.031846	50.555751
3502.900700	426391.863208	50.560756
3502.914217	426323.796499	50.565761
3502.575780	426258.784337	50.570765
3502.628782	426178.173564	50.575770
3502.412850	426080.807857	50.580775
3501.978101	425975.205680	50.585780
3502.294234	425852.318776	50.590785
3502.196805	425739.095084	50.595789
3501.428568	425608.575386	50.600794
3501.403860	425480.059870	50.605799
3501.064368	425337.740311	50.610804
3500.794106	425188.352595	50.615809
3500.290180	425041.491053	50.620813
3500.213741	424884.403704	50.625818
3500.002113	424723.785219	50.630823
3499.683157	424551.661408	50.635828
3499.265092	424367.319970	50.640833
3498.743643	424196.801787	50.645837
3498.347934	424001.743164	50.650842
3498.307980	423809.921746	50.655847
3497.784148	423618.892105	50.660852
3497.240684	423412.940090	50.665857
3496.876691	423207.006448	50.670861
3496.475295	422999.706836	50.675866
3496.257454	422782.322849	50.680871
3495.978228	422562.409186	50.685876
3495.647142	422328.795871	50.690881
3494.374107	422110.520022	50.695885
3494.217595	421878.801691	50.700890
3493.862525	421643.713731	50.705895
3492.995698	421405.055694	50.710900
3492.809866	421148.967393	50.715905
3492.309159	420920.979447	50.720909
3491.923801	420669.514729	50.725914
3491.566623	420418.068026	50.730919
3490.960762	420157.040433	50.735924
3490.505226	419894.207477	50.740929
3489.792777	419626.440101	50.745933
3489.507287	419368.116508	50.750938
3488.879428	419104.568458	50.755943
3487.892276	418839.276566	50.760948
3487.927516	418564.515889	50.765953
3487.284532	418291.619686	50.770957
3486.675550	418011.225579	50.775962
3485.857701	417734.951343	50.780967
3485.232667	417459.326612	50.785972
3485.159638	417173.855727	50.790977
3484.556477	416890.528571	50.795981
3483.458084	416611.903477	50.800986
3483.163206	416311.100828	50.805991
3482.119684	416031.190559	50.810996
3481.986762	415733.120808	50.816001
3481.146549	415448.066193	50.821005
3480.582129	415153.998727	50.826010
3480.016372	414858.049249	50.831015
3479.310527	414563.415183	50.836020
3478.550725	414258.275234	50.841025
3477.894380	413973.096657	50.846029
3477.225607	413683.930631	50.851034
3476.777447	413377.406706	50.856039
3475.874154	413091.803524	50.861044
3475.385828	412783.222696	50.866049
3474.926373	412497.410229	50.871053
3474.173011	412191.356089	50.876058
3473.390465	411892.362582	50.881063
3472.754637	411597.657452	50.886068
3472.515453	411296.634471	50.891073
3471.961935	410996.220378	50.896077
3471.202499	410683.750421	50.901082
3470.648838	410369.870322	50.906087
3469.785868	410064.317986	50.911092
3469.204199	409749.851230	50.916097
3468.853166	409445.855019	50.921101
3468.066398	409129.511289	50.926106
3467.776522	408817.294671	50.931111
3466.713042	408500.330430	50.936116
3466.139145	408180.307439	50.941121
3465.526673	407875.703071	50.946125
3464.569897	407555.204669	50.951130
3464.011554	407241.948862	50.956135
3463.464088	406936.992600	50.961140
3462.942729	406606.503473	50.966145
3462.072591	406291.029464	50.971149
3461.249989	405974.934103	50.976154
3460.712256	405656.881508	50.981159
3459.785145	405352.124657	50.986164
3459.485328	405027.953705	50.991169
3459.164277	404719.657387	50.996173
3457.981096	404397.052200	51.001178
3457.224834	404077.951773	51.006183
3456.552502	403760.128750	51.011188
3455.866573	403449.873864	51.016193
3455.117726	403137.162327	51.021197
3454.590043	402822.834604	51.026202
3453.943140	402503.341721	51.031207
3452.745036	402197.224578	51.036212
3452.592879	401879.824644	51.041217
3451.708643	401570.827380	51.046221
3451.056311	401250.457408	51.051226
3450.390786	400942.584413	51.056231
3449.470154	400630.407618	51.061236
3449.133349	400318.000655	51.066241
3448.364489	400007.315283	51.071245
3447.426505	399690.812391	51.076250
3446.923564	399376.213242	51.081255
3445.965471	399078.785821	51.086260
3445.597310	398766.316338	51.091265
3444.818337	398461.535218	51.096269
3444.446717	398150.075816	51.101274
3443.762711	397833.102474	51.106279
3442.877444	397525.763570	51.111284
3442.117337	397214.589041	51.116289
3441.793192	396902.269631	51.121293
3440.877437	396588.015315	51.126298
3440.221148	396273.408404	51.131303
3439.389493	395969.295973	51.136308
3438.659912	395653.297463	51.141313
3438.373517	395349.314137	51.146317
3437.543726	395034.901368	51.151322
3436.754110	394720.249695	51.156327
3435.793232	394416.727616	51.161332
3435.741532	394100.698280	51.166337
3434.930505	393793.409052	51.171341
3434.268161	393486.396164	51.176346
3433.585168	393168.304863	51.181351
3432.457587	392867.412615	51.186356
3431.808184	392547.657287	51.191361
3430.871365	392242.940001	51.196365
3430.299003	391933.253045	51.201370
3429.977589	391633.481284	51.206375
3429.413571	391339.516396	51.211380
3428.727350	391026.358174	51.216385
3428.121433	390720.272971	51.221389
3427.724980	390408.075358	51.226394
3427.140597	390089.578892	51.231399
3426.180523	389772.566373	51.236404
3425.321085	389463.436865	51.241409
3424.969306	389157.877072	51.246413
3424.168620	388840.243172	51.251418
3423.207067	388536.585698	51.256423
3422.446186	388223.513141	51.261428
3422.005611	387910.738517	51.266433
3421.156479	387606.569833	51.271437
3420.270051	387297.321554	51.276442
3419.772990	386996.492378	51.281447
3419.143934	386693.598779	51.286452
3418.720392	386390.235084	51.291457
3418.106386	386083.774824	51.296461
3417.245981	385769.677972	51.301466
3416.526829	385454.054299	51.306471
3415.426375	385150.412999	51.311476
3415.255097	384842.238404	51.316481
3414.334845	384538.026709	51.321485
3413.288735	384225.725447	51.326490
3412.758060	383928.456600	51.331495
3412.365627	383624.273137	51.336500
3411.685698	383323.567329	51.341505
3410.919796	383020.331550	51.346509
3410.228048	382714.080858	51.351514
3409.553104	382413.009832	51.356519
3408.883631	382112.290936	51.361524
3408.125952	381800.857367	51.366529
3407.472263	381502.468703	51.371533
3406.453705	381203.580381	51.376538
3406.048813	380895.662103	51.381543
3405.315289	380604.523574	51.386548
3404.328461	380307.604432	51.391553
3404.033164	380017.275581	51.396557
3403.296049	379710.902758	51.401562
3402.858076	379415.000373	51.406567
3401.940271	379118.948495	51.411572
3401.515281	378809.412629	51.416577
3400.914931	378502.929034	51.421581
3400.006341	378210.045235	51.426586
3399.583382	377908.686581	51.431591
3398.527204	377618.339623	51.436596
3397.950804	377316.976443	51.441601
3397.211833	377024.714336	51.446605
3396.713525	376713.875091	51.451610
3395.854332	376422.441857	51.456615
3395.399635	376133.352292	51.461620
3394.505226	375828.979352	51.466625
3393.746519	375531.622998	51.471629
3392.897391	375240.610155	51.476634
3392.703681	374941.906408	51.481639
3391.906457	374644.599795	51.486644
3391.334347	374349.006499	51.491649
3390.474202	374056.790563	51.496653
3389.709079	373761.860845	51.501658
3389.481599	373459.921043	51.506663
3388.612116	373176.496561	51.511668
3388.163921	372859.028648	51.516673
3387.805354	372564.121082	51.521677
3386.598079	372270.373036	51.526682
3386.075231	371962.902375	51.531687
3385.228247	371664.485519	51.536692
3384.352284	371368.766371	51.541697
3383.336959	371065.745484	51.546701
3382.972105	370777.943744	51.551706
3382.161269	370478.875068	51.556711
3381.641691	370189.289639	51.561716
3380.947057	369900.214902	51.566721
3380.130677	369606.632381	51.571725
3379.552531	369316.363357	51.576730
3379.177132	369017.843879	51.581735
3378.307575	368729.425357	51.586740
3377.532322	368433.181676	51.591745
3376.640784	368142.244761	51.596749
3376.413449	367852.845021	51.601754
3375.965508	367559.996787	51.606759
3374.975601	367269.552902	51.611764
3374.865751	366975.319913	51.616769
3373.762288	366677.261690	51.621773
3372.931180	366374.627903	51.626778
3372.443259	366078.519625	51.631783
3371.597023	365790.023197	51.636788
3370.910794	365486.670808	51.641793
3370.633518	365205.524051	51.646797
3369.905379	364911.761810	51.651802
3369.356216	364614.635141	51.656807
3368.264903	364330.492751	51.661812
3367.816126	364024.951736	51.666817
3367.219956	363732.276802	51.671821
3366.535139	363437.249522	51.676826
3365.839126	363131.336631	51.681831
3365.115808	362836.667346	51.686836
3364.527019	362543.905747	51.691841
3363.969609	362247.423285	51.696845
3363.230211	361952.699109	51.701850
3363.031730	361646.842045	51.706855
3361.659289	361347.134613	51.711860
3361.000578	361049.414018	51.716865
3360.366924	360749.245171	51.721869
3359.435341	360466.064324	51.726874
3358.956783	360161.235395	51.731879
3357.755495	359872.983947	51.736884
3357.165870	359587.245750	51.741889
3356.715870	359301.710563	51.746893
3356.253222	359013.352142	51.751898
3355.694542	358724.066912	51.756903
3354.717098	358432.078594	51.761908
3354.029912	358136.350346	51.766913
3353.105345	357852.055895	51.771917
3352.713062	357570.797210	51.776922
3352.184797	357275.035495	51.781927
3351.465423	356994.057589	51.786932
3350.873750	356695.835111	51.791937
3350.099334	356415.523969	51.796941
3349.287920	356123.846742	51.801946
3348.698963	355825.108697	51.806951
3347.938905	355548.146916	51.811956
3347.373524	355264.841440	51.816961
3346.943497	354967.672621	51.821965
3345.715951	354690.377920	51.826970
3345.552128	354392.828826	51.831975
3344.851077	354104.832502	51.836980
3343.825910	353813.938655	51.841985
3343.229693	353535.688985	51.846989
3342.480673	353252.477513	51.851994
3342.171263	352952.882503	51.856999
3341.332974	352679.527425	51.862004
3340.560773	352389.598130	51.867009
3340.314700	352106.751017	51.872013
3339.265678	351815.084308	51.877018
3338.830381	351524.811763	51.882023
3337.879612	351241.621367	51.887028
3337.494637	350950.191539	51.892033
3336.880209	350669.941921	51.897037
3335.984540	350383.581856	51.902042
3335.424532	350083.755199	51.907047
3334.127399	349810.104077	51.912052
3333.945217	349523.311217	51.917057
3333.746273	349235.857869	51.922061
3332.722968	348957.422554	51.927066
3332.309723	348664.557579	51.932071
3331.131363	348372.711806	51.937076
3330.690616	348075.598836	51.942081
3329.992753	347789.417092	51.947085
3329.280565	347502.472690	51.952090
3328.795240	347217.217805	51.957095
3327.818725	346939.601499	51.962100
3327.389111	346641.764736	51.967105
3326.849577	346354.300124	51.972109
3325.616930	346069.216517	51.977114
3325.029998	345784.529714	51.982119
3324.437851	345512.309372	51.987124
3324.234020	345218.292168	51.992129
3323.299419	344933.405025	51.997133
3322.290764	344653.414025	52.002138
3322.045746	344367.744081	52.007143
3321.211854	344089.068369	52.012148
3320.464072	343803.531717	52.017153
3319.965771	343511.614997	52.022157
3319.091402	343236.477925	52.027162
3318.490900	342939.995047	52.032167
3317.662841	342665.381077	52.037172
3316.877885	342383.277251	52.042177
3316.469912	342106.781691	52.047181
3315.707545	341828.894659	52.052186
3315.157389	341545.880631	52.057191
3314.152368	341259.176636	52.062196
3313.400699	340979.756113	52.067201
3312.735144	340717.724428	52.072205
3312.132348	340444.306123	52.077210
3311.821695	340158.469424	52.082215
3311.091323	339889.141223	52.087220
3310.485951	339596.353767	52.092225
3309.628732	339317.476124	52.097229
3309.090546	339036.074057	52.102234
3308.422545	338752.707683	52.107239
3307.427084	338475.859233	52.112244
3307.130977	338194.385605	52.117249
3306.415929	337915.068647	52.122253
3305.743429	337634.470480	52.127258
3304.990543	337347.039003	52.132263
3304.238022	337081.694700	52.137268
3303.709448	336801.398149	52.142273
3303.176099	336518.734181	52.147277
3302.075385	336239.244808	52.152282
3301.857606	335962.377005	52.157287
3300.968479	335687.480128	52.162292
3300.433928	335403.563237	52.167297
3299.956937	335123.783143	52.172301
3299.102119	334843.328048	52.177306
3298.278896	334545.458761	52.182311
3297.694409	334280.071328	52.187316
3297.445958	334001.009670	52.192321
3297.019293	333719.406560	52.197325
3295.584921	333438.839353	52.202330
3295.155746	333145.094070	52.207335
3295.102673	332865.534971	52.212340
3293.997483	332571.113039	52.217345
3292.951099	332290.015427	52.222349
3292.461664	332007.319648	52.227354
3292.111195	331718.897723	52.232359
3290.797441	331443.542314	52.237364
3290.479522	331157.097010	52.242369
3290.000826	330875.080691	52.247373
3288.875358	330597.932750	52.252378
3288.411658	330315.834652	52.257383
3287.604097	330036.186277	52.262388
3286.880384	329750.795583	52.267393
3286.608506	329475.201495	52.272397
3285.832079	329200.659393	52.277402
3285.376295	328914.404221	52.282407
3284.582075	328640.295110	52.287412
3283.751104	328354.635677	52.292417
3283.216918	328070.451257	52.297421
3282.516861	327793.216804	52.302426
3281.939537	327502.928359	52.307431
3281.069131	327230.810792	52.312436
3280.494755	326940.137222	52.317441
3279.464827	326663.411830	52.322445
3278.834262	326387.227785	52.327450
3278.340564	326110.433639	52.332455
3277.515044	325839.370937	52.337460
3277.086763	325555.614271	52.342465
3276.392848	325269.127184	52.347469
3275.462813	325003.245564	52.352474
3274.798610	324725.964995	52.357479
3274.106894	324443.164358	52.362484
3273.403111	324168.560630	52.367489
3273.065530	323898.805743	52.372493
3272.329216	323621.405141	52.377498
3272.009931	323338.586643	52.382503
3271.083270	323067.477794	52.387508
3270.194778	322786.408507	52.392513
3269.709492	322512.065463	52.397517
3268.661977	322239.649975	52.402522
3268.508481	321961.073246	52.407527
3267.788136	321680.682969	52.412532
3267.005811	321399.462006	52.417537
3266.293390	321120.264266	52.422541
3266.052301	320844.344894	52.427546
3265.017949	320552.191966	52.432551
3264.261399	320279.641942	52.437556
3263.659300	320004.238800	52.442561
3263.088345	319730.814711	52.447565
3262.378929	319452.958337	52.452570
3261.553755	319173.389540	52.457575
3260.891580	318907.639818	52.462580
3260.194314	318621.810074	52.467585
3259.741755	318347.596282	52.472589
3258.544221	318077.148862	52.477594
3258.389831	317795.728608	52.482599
3257.498335	317529.274277	52.487604
3256.973409	317256.799403	52.492609
3256.408136	316964.397621	52.497613
3255.222435	316698.041165	52.502618
3254.722848	316421.536403	52.507623
3254.147706	316158.917566	52.512628
3253.457094	315879.668415	52.517633
3252.875002	315611.473538	52.522637
3251.979926	315338.290509	52.527642
3251.838652	315058.180492	52.532647
3250.914077	314789.175385	52.537652
3250.320449	314501.528572	52.542657
3249.773390	314231.387626	52.547661
3248.678549	313965.157904	52.552666
3248.383730	313682.497400	52.557671
3247.605912	313408.955914	52.562676
3246.912851	313133.311336	52.567681
3246.293746	312863.788531	52.572685
3245.399453	312589.652838	52.577690
3245.165074	312309.675233	52.582695
3244.279127	312040.322255	52.587700
3243.592958	311759.146790	52.592705
3243.078912	311480.537656	52.597709
3242.271319	311202.843221	52.602714
3241.781124	310920.332711	52.607719
3241.111178	310643.732891	52.612724
3240.324693	310372.651146	52.617729
3239.931742	310093.532465	52.622733
3238.783663	309823.452520	52.627738
3238.559038	309535.723251	52.632743
3237.748397	309274.570930	52.637748
3237.067992	308989.437974	52.642753
3236.463466	308713.201918	52.647757
3235.434710	308443.198624	52.652762
3235.181914	308163.336184	52.657767
3234.588818	307894.045857	52.662772
3233.720754	307608.125236	52.667777
3233.156724	307325.079582	52.672781
3232.196333	307058.624341	52.677786
3231.935448	306775.244919	52.682791
3231.105156	306501.127523	52.687796
3230.095885	306218.103141	52.692801
3229.514613	305939.562127	52.697805
3228.942591	305673.214264	52.702810
3228.185624	305401.626761	52.707815
3227.311578	305137.365638	52.712820
3227.091166	304859.574131	52.717825
3226.350541	304579.680922	52.722829
3225.761024	304316.590766	52.727834
3225.043758	304033.865597	52.732839
3224.292894	303762.831955	52.737844
3223.734076	303478.957611	52.742849
3223.018506	303200.354169	52.747853
3222.142122	302937.410670	52.752858
3221.518540	302658.102337	52.757863
3220.880959	302391.220803	52.762868
3220.069289	302112.757658	52.767873
3219.518839	301840.970948	52.772877
3218.551761	301575.034432	52.777882
3218.082604	301297.910674	52.782887
3217.552728	301031.745122	52.787892
3216.687845	300761.358389	52.792897
3215.910854	300497.601481	52.797901
3215.317395	300223.474803	52.802906
3214.569418	299946.852944	52.807911
3214.264655	299689.022209	52.812916
3213.518342	299418.025709	52.817921
3212.928008	299147.969374	52.822925
3212.271380	298880.724490	52.827930
3211.238460	298609.341800	52.832935
3210.949215	298339.893807	52.837940
3209.995327	298071.806280	52.842945
3209.490163	297796.893709	52.847949
3208.666503	297530.361169	52.852954
3208.221573	297260.529421	52.857959
3207.614313	296992.889039	52.862964
3207.133371	296716.441580	52.867969
3206.581440	296440.158276	52.872973
3205.753006	296176.169308	52.877978
3205.420402	295899.541530	52.882983
3204.727870	295619.715176	52.887988
3203.604659	295346.913177	52.892993
3202.867657	295069.715695	52.897997
3201.953605	294798.149733	52.903002
3201.417640	294523.259146	52.908007
3200.559235	294262.911817	52.913012
3199.935553	293992.872980	52.918017
3199.554842	293715.127342	52.923021
3198.723827	293453.652996	52.928026
3198.214186	293182.344957	52.933031
3197.496465	292913.083465	52.938036
3196.617086	292643.874405	52.943041
3196.060953	292369.312939	52.948045
3195.299852	292105.429884	52.953050
3194.963255	291831.975523	52.958055
3194.134623	291569.375995	52.963060
3193.608142	291313.039444	52.968065
3193.287808	291022.111812	52.973069
3192.434042	290763.767351	52.978074
3191.780577	290478.879465	52.983079
3190.993441	290205.345515	52.988084
3190.274573	289927.470286	52.993089
3189.882785	289667.211114	52.998093
3189.105768	289399.352283	53.003098
3188.218749	289121.631290	53.008103
3187.361429	288853.428498	53.013108
3186.925970	288582.555649	53.018113
3186.543623	288301.665389	53.023117
3185.819699	288036.697625	53.028122
3184.980662	287755.298492	53.033127
3184.372933	287482.364625	53.038132
3183.300664	287214.475273	53.043137
3182.649568	286942.668178	53.048141
3181.727764	286671.186894	53.053146
3181.414379	286410.627665	53.058151
3180.972156	286147.110490	53.063156
3180.002358	285875.151985	53.068161
3179.500728	285607.289331	53.073165
3178.566065	285341.333662	53.078170
3177.865990	285074.140538	53.083175
3177.601120	284813.468193	53.088180
3177.136541	284540.733262	53.093185
3176.291835	284275.982618	53.098189
3175.751319	283998.242890	53.103194
3174.721336	283726.749001	53.108199
3173.889477	283469.889157	53.113204
3173.143943	283201.656308	53.118209
3172.665093	282933.326505	53.123213
3171.898571	282675.919387	53.128218
3171.278993	282400.864200	53.133223
3170.417010	282140.060055	53.138228
3170.052883	281878.508320	53.143233
3169.571178	281613.385509	53.148237
3168.979200	281351.031462	53.153242
3168.188294	281080.332562	53.158247
3167.626688	280816.546369	53.163252
3167.008308	280550.935881	53.168257
3166.012368	280279.048333	53.173261
3165.363321	280022.661116	53.178266
3164.740791	279746.761645	53.183271
3164.186808	279479.585061	53.188276
3163.501090	279212.074049	53.193281
3162.945853	278946.806882	53.198285
3162.129838	278683.137342	53.203290
3161.458709	278410.784001	53.208295
3161.046474	278143.759520	53.213300
3160.081469	277875.173748	53.218305
3159.867033	277610.228475	53.223309
3159.052991	277347.830084	53.228314
3158.184443	277074.973768	53.233319
3157.565369	276812.439497	53.238324
3157.011287	276533.263869	53.243329
3156.421049	276256.004060	53.248333
3155.456279	276002.568582	53.253338
3154.706873	275734.350593	53.258343
3153.994520	275460.752385	53.263348
3153.463348	275203.498231	53.268353
3152.867304	274929.370147	53.273357
3151.976768	274669.069769	53.278362
3151.618259	274402.031272	53.283367
3150.929137	274133.928382	53.288372
3150.097417	273874.814017	53.293377
3150.164217	273600.545651	53.298381
3148.830107	273333.061380	53.303386
3148.503529	273056.210997	53.308391
3147.676669	272786.016346	53.313396
3146.747250	272512.298958	53.318401
3146.551435	272250.909528	53.323405
3145.605621	271989.520619	53.328410
3145.109590	271712.264787	53.333415
3144.220870	271445.390088	53.338420
3143.375468	271184.136053	53.343425
3143.319823	270906.549506	53.348429
3142.352016	270640.782657	53.353434
3141.434839	270366.628078	53.358439
3140.793789	270106.942617	53.363444
3139.983282	269844.739117	53.368449
3139.350853	269586.477929	53.373453
3138.959207	269323.030926	53.378458
3138.360435	269046.477758	53.383463
3137.638768	268789.249882	53.388468
3137.103253	268520.147511	53.393473
3136.772028	268246.655044	53.398477
3135.608212	267981.428813	53.403482
3134.983746	267708.699124	53.408487
3133.997998	267452.152075	53.413492
3133.392404	267179.953598	53.418497
3133.043752	266917.108674	53.423501
3132.210062	266653.022104	53.428506
3131.580074	266385.105850	53.433511
3130.678421	266119.426072	53.438516
3129.896708	265862.486603	53.443521
3129.508993	265599.316440	53.448525
3128.379789	265340.780617	53.453530
3128.228337	265075.023001	53.458535
3127.642265	264815.579136	53.463540
3126.981858	264548.736651	53.468545
3126.371324	264275.620381	53.473549
3125.582489	264014.224247	53.478554
3125.254472	263735.278204	53.483559
3124.522678	263475.782177	53.488564
3123.644295	263213.789742	53.493569
3123.021597	262940.751318	53.498573
3122.333125	262681.502238	53.503578
3121.535530	262412.924916	53.508583
3121.061699	262145.616524	53.513588
3120.271465	261879.559086	53.518593
3119.800601	261612.479211	53.523597
3119.125911	261356.283484	53.528602
3118.419006	261082.061756	53.533607
3117.790223	260818.446808	53.538612
3116.921169	260544.991200	53.543617
3116.460368	260277.323449	53.548621
3115.938497	260010.302770	53.553626
3115.168831	259738.663692	53.558631
3114.466860	259480.256433	53.563636
3113.910100	259212.604847	53.568641
3113.162141	258938.669773	53.573645
3112.468854	258672.977004	53.578650
3111.709923	258401.692415	53.583655
3111.170522	258130.039205	53.588660
3110.455757	257866.820424	53.593665
3109.821571	257592.101708	53.598669
3108.406147	257330.352396	53.603674
3108.149926	257059.312903	53.608679
3107.383289	256798.929892	53.613684
3107.080759	256541.141753	53.618689
3106.476091	256271.002226	53.623693
3105.568435	256019.073277	53.628698
3105.198189	255747.620310	53.633703
3104.602763	255485.119688	53.638708
3103.687719	255214.320126	53.643713
3103.366683	254942.145703	53.648717
3102.368382	254680.910983	53.653722
3101.580447	254413.986424	53.658727
3101.084416	254150.195556	53.663732
3100.012740	253883.727041	53.668737
3099.681866	253617.208424	53.673741
3099.002560	253366.870720	53.678746
3098.410724	253090.846236	53.683751
3097.820273	252825.900220	53.688756
3096.929645	252557.694692	53.693761
3096.390138	252296.713136	53.698765
3095.336197	252037.092940	53.703770
3094.928604	251775.936187	53.708775
3094.024957	251517.079982	53.713780
3093.314750	251234.581895	53.718785
3092.799001	250969.012434	53.723789
3092.064938	250716.978444	53.728794
3091.321291	250453.943981	53.733799
3091.008771	250193.968540	53.738804
3089.941910	249937.076367	53.743809
3089.383801	249669.044262	53.748813
3088.917475	249421.625696	53.753818
3088.038582	249151.993212	53.758823
3087.353070	248887.090338	53.763828
3086.775664	248637.908343	53.768833
3086.103428	248376.314299	53.773837
3085.393940	248119.463797	53.778842
3084.855219	247862.737067	53.783847
3084.141853	247604.130219	53.788852
3083.315982	247350.305238	53.793857
3082.754526	247083.650346	53.798861
3081.851228	246830.246382	53.803866
3081.340152	246577.998024	53.808871
3080.771392	246323.238359	53.813876
3079.731178	246055.035979	53.818881
3079.734436	245796.638905	53.823885
3078.525634	245544.714152	53.828890
3078.285607	245287.148494	53.833895
3077.484815	245031.639837	53.838900
3076.872982	244777.296069	53.843905
3076.422210	244513.705655	53.848909
3075.541340	244256.301173	53.853914
3074.698830	243994.764574	53.858919
3073.806297	243737.489832	53.863924
3073.176801	243480.832520	53.868929
3072.772975	243219.298017	53.873933
3072.236417	242974.340356	53.878938
3071.394176	242706.412425	53.883943
3070.894426	242457.883441	53.888948
3070.255947	242205.430903	53.893953
3069.718927	241934.038895	53.898957
3068.577956	241675.560477	53.903962
3068.143341	241424.932944	53.908967
3067.607606	241179.085331	53.913972
3066.969367	240914.587843	53.918977
3066.561497	240654.176985	53.923981
3065.804668	240404.191224	53.928986
3064.814076	240136.418511	53.933991
3064.393358	239870.611582	53.938996
3063.826772	239621.459997	53.944001
3063.346364	239349.526221	53.949005
3062.502609	239084.632852	53.954010
3061.917308	238827.921534	53.959015
3061.346787	238568.330187	53.964020
3060.306065	238301.943341	53.969025
3059.712125	238031.838687	53.974029
3059.232664	237781.095252	53.979034
3058.414838	237516.785043	53.984039
3057.845969	237247.237358	53.989044
3057.098844	237000.997293	53.994049
3056.593624	236732.076070	53.999053
3055.987726	236461.746252	54.004058
3055.139817	236196.067646	54.009063
3054.174066	235931.097130	54.014068
3053.545363	235684.609229	54.019073
3053.289279	235421.886571	54.024077
3052.501582	235162.056437	54.029082
3051.783374	234900.661316	54.034087
3051.438036	234632.887119	54.039092
3050.322047	234378.895088	54.044097
3049.563920	234108.263509	54.049101
3048.945893	233857.828854	54.054106
3048.186932	233596.926414	54.059111
3047.704947	233328.948285	54.064116
3046.486618	233079.534079	54.069121
3046.654843	232817.353868	54.074125
3045.996138	232564.203100	54.079130
3045.005008	232293.410396	54.084135
3044.330463	232034.685999	54.089140
3043.450195	231782.389183	54.094145
3043.047579	231515.775532	54.099149
3042.305019	231259.661529	54.104154
3041.580551	231003.290180	54.109159
3040.872145	230745.668660	54.114164
3040.332868	230492.857216	54.119169
3039.743742	230233.815523	54.124173
3038.708633	229977.549851	54.129178
3038.064040	229718.034648	54.134183
3037.501736	229463.395279	54.139188
3036.612265	229214.058200	54.144193
3036.417290	228956.020911	54.149197
3035.596713	228698.702132	54.154202
3034.744998	228443.706505	54.159207
3034.134642	228194.603592	54.164212
3033.553984	227944.069961	54.169217
3032.901287	227679.644874	54.174221
3032.265388	227431.871867	54.179226
3031.716514	227179.195058	54.184231
3031.274106	226914.098851	54.189236
3030.434981	226669.978017	54.194241
3029.860451	226401.085567	54.199245
3029.000357	226136.087698	54.204250
3028.473810	225878.698404	54.209255
3027.604577	225622.361299	54.214260
3026.923650	225376.051251	54.219265
3026.548668	225110.896158	54.224269
3025.754714	224856.406644	54.229274
3025.080333	224612.872616	54.234279
3024.565475	224342.675469	54.239284
3023.626663	224083.552162	54.244289
3023.023903	223825.950795	54.249293
3022.264030	223570.566774	54.254298
3021.445379	223312.417667	54.259303
3020.892169	223049.156283	54.264308
3020.164786	222811.364382	54.269313
3019.898103	222549.888580	54.274317
3019.033347	222299.694451	54.279322
3018.235405	222042.053810	54.284327
3017.827356	221783.328541	54.289332
3016.838434	221530.152456	54.294337
3016.811558	221271.032160	54.299341
3015.469829	221025.353027	54.304346
3015.068183	220757.589147	54.309351
3014.139305	220503.182780	54.314356
3013.337855	220248.627894	54.319361
3013.158825	219992.031978	54.324365
3012.313722	219743.495204	54.329370
3011.441606	219486.000313	54.334375
3011.151713	219237.624458	54.339380
3010.485015	218977.854846	54.344385
3009.988058	218721.265284	54.349389
3008.572384	218468.270890	54.354394
3008.504084	218223.500803	54.359399
3007.533933	217962.792411	54.364404
3006.737991	217708.242521	54.369409
3006.407886	217452.722439	54.374413
3005.879636	217201.641994	54.379418
3005.340950	216947.202788	54.384423
3004.869480	216684.044304	54.389428
3003.816563	216416.657105	54.394433
3003.394801	216167.088786	54.399437
3002.276087	215917.665623	54.404442
3001.755377	215648.203413	54.409447
3001.362854	215386.358895	54.414452
3000.468463	215138.350740	54.419457
2999.973208	214887.372261	54.424461
2999.205576	214635.829857	54.429466
2998.360391	214376.178776	54.434471
2997.590787	214117.075654	54.439476
2996.828725	213869.302751	54.444481
2996.375615	213609.255741	54.449485
2995.469231	213370.369717	54.454490
2994.903929	213110.827028	54.459495
2994.816074	212855.251974	54.464500
2993.746965	212599.030483	54.469505
2993.044439	212341.524888	54.474509
2992.517362	212087.783874	54.479514
2991.535846	211836.998404	54.484519
2991.336713	211583.635609	54.489524
2990.412187	211325.814337	54.494529
2989.953278	211064.680609	54.499533
2989.174249	210815.060077	54.504538
2988.230001	210559.357695	54.509543
2988.000541	210306.130997	54.514548
2987.044284	210054.174968	54.519553
2986.612253	209803.199472	54.524557
2985.702929	209555.870827	54.529562
2985.122855	209303.343467	54.534567
2984.510013	209045.220994	54.539572
2983.730350	208793.849520	54.544577
2983.714092	208535.117431	54.549581
2982.418763	208269.832069	54.554586
2981.838993	208015.729888	54.559591
2981.253984	207765.346640	54.564596
2980.356237	207512.395126	54.569601
2979.875917	207257.603548	54.574605
2979.147273	207000.792882	54.579610
2978.525169	206741.800676	54.584615
2977.670836	206483.867382	54.589620
2976.910514	206246.312525	54.594625
2976.279719	205989.131876	54.599629
2975.731824	205748.525152	54.604634
2975.271719	205490.756808	54.609639
2974.793062	205221.942844	54.614644
2974.178485	204980.827896	54.619649
2973.698693	204716.827755	54.624653
2972.493200	204464.078386	54.629658
2971.843735	204209.223520	54.634663
2971.476744	203958.254723	54.639668
2970.676634	203706.138687	54.644673
2970.051333	203430.609168	54.649677
2969.308193	203182.851394	54.654682
2968.553523	202931.608482	54.659687
2968.064325	202682.383229	54.664692
2967.536476	202425.107615	54.669697
2966.647886	202154.363085	54.674701
2966.111618	201904.817480	54.679706
2965.000609	201643.214346	54.684711
2964.425910	201376.034154	54.689716
2963.640139	201153.761764	54.694721
2963.468504	200892.789998	54.699725
2962.796551	200641.375180	54.704730
2961.795834	200384.760255	54.709735
2961.374581	200129.625640	54.714740
2960.223705	199883.157802	54.719745
2959.750304	199625.971766	54.724749
2958.719980	199375.908214	54.729754
2958.409559	199126.702662	54.734759
2957.932031	198867.496163	54.739764
2956.827675	198624.346970	54.744769
2956.510581	198371.288376	54.749773
2955.639464	198124.384249	54.754778
2955.075989	197881.043386	54.759783
2954.473050	197622.932129	54.764788
2953.836164	197378.243606	54.769793
2953.257527	197119.060874	54.774797
2952.581233	196870.893258	54.779802
2951.908951	196625.589768	54.784807
2951.366871	196371.304092	54.789812
2950.745132	196128.221239	54.794817
2950.123609	195871.494436	54.799821
2949.394079	195612.063214	54.804826
2948.435757	195369.346094	54.809831
2947.768738	195107.653250	54.814836
2946.862576	194856.426653	54.819841
2946.383559	194606.209916	54.824845
2945.681710	194369.040277	54.829850
2945.094052	194114.325515	54.834855
2944.810400	193861.825378	54.839860
2943.727678	193618.550483	54.844865
2943.343577	193364.898474	54.849869
2942.419805	193113.108838	54.854874
2941.932332	192862.900250	54.859879
2941.469122	192619.141442	54.864884
2940.760455	192368.463475	54.869889
2940.310101	192107.509359	54.874893
2939.173949	191858.497402	54.879898
2938.239571	191610.151966	54.884903
2937.732648	191350.776132	54.889908
2936.858285	191105.731579	54.894913
2936.416945	190858.921262	54.899917
2935.821162	190608.625578	54.904922
2935.069580	190370.550240	54.909927
2934.751791	190115.398152	54.914932
2933.691839	189859.673944	54.919937
2933.345507	189613.501465	54.924941
2932.641420	189370.572872	54.929946
2931.578171	189116.621407	54.934951
2931.116974	188872.800598	54.939956
2930.315771	188637.502257	54.944961
2930.133665	188380.488875	54.949965
2929.147250	188137.664401	54.954970
2928.562699	187889.897911	54.959975
2928.096232	187631.014611	54.964980
2927.259542	187388.600324	54.969985
2926.789737	187132.672356	54.974989
2926.050612	186888.309020	54.979994
2925.582215	186635.615516	54.984999
2925.008620	186376.959669	54.990004
2924.136335	186131.820492	54.995009
2923.202332	185872.999402	55.000013
2922.936986	185621.446439	55.005018
2921.848776	185375.545618	55.010023
2921.126405	185119.160641	55.015028
2920.520634	184877.290068	55.020033
2920.311708	184628.137060	55.025037
2919.129361	184374.493774	55.030042
2918.725152	184125.452702	55.035047
2918.261048	183874.259572	55.040052
2917.266408	183631.035486	55.045057
2916.710767	183377.722290	55.050061
2916.392819	183122.575309	55.055066
2915.219630	182870.375273	55.060071
2914.897397	182615.880363	55.065076
2914.205395	182381.110716	55.070081
2913.678525	182126.780288	55.075085
2913.127925	181867.479467	55.080090
2912.320245	181612.766748	55.085095
2911.618697	181352.527045	55.090100
2910.697683	181114.277080	55.095105
2910.074446	180853.148357	55.100109
2909.404209	180613.050782	55.105114
2908.745977	180357.529487	55.110119
2908.066805	180103.858111	55.115124
2907.310760	179857.199780	55.120129
2906.670919	179607.774169	55.125133
2905.983842	179370.968075	55.130138
2905.240678	179117.643193	55.135143
2904.599113	178867.597859	55.140148
2903.695187	178619.609037	55.145153
2903.221310	178374.220063	55.150157
2902.936239	178123.404794	55.155162
2902.458948	177887.740210	55.160167
2901.767639	177628.636793	55.165172
2900.963843	177371.233507	55.170177
2900.419041	177123.050503	55.175181
2899.736217	176871.571272	55.180186
2898.711188	176621.984025	55.185191
2898.288298	176360.436284	55.190196
2897.876993	176117.554011	55.195201
2896.761231	175856.216332	55.200205
2896.451768	175612.504748	55.205210
2895.830595	175357.943304	55.210215
2894.961855	175105.779346	55.215220
2894.432500	174852.260851	55.220225
2893.525010	174591.428563	55.225229
2892.818455	174351.277243	55.230234
2892.000876	174097.302904	55.235239
2891.449599	173841.617598	55.240244
2890.721792	173600.392067	55.245249
2889.983870	173356.637513	55.250253
2889.291594	173111.769451	55.255258
2888.236272	172860.132314	55.260263
2887.728136	172616.405804	55.265268
2886.916847	172381.205863	55.270273
2886.433897	172135.378166	55.275277
2885.963936	171892.119528	55.280282
2884.907774	171648.453375	55.285287
2884.329038	171406.653463	55.290292
2884.009983	171172.660314	55.295297
2883.284573	170931.765735	55.300301
2882.506825	170684.761753	55.305306
2882.086325	170438.524974	55.310311
2881.547311	170192.907682	55.315316
2880.625592	169953.120308	55.320321
2879.822017	169701.265927	55.325325
2879.127706	169462.001982	55.330330
2878.452601	169228.880799	55.335335
2878.192100	168972.611992	55.340340
2877.177871	168735.327482	55.345345
2876.813247	168484.676864	55.350349
2876.032548	168238.793093	55.355354
2875.444962	167995.689162	55.360359
2874.789138	167751.084283	55.365364
2873.910822	167511.531086	55.370369
2873.255562	167261.700096	55.375373
2872.702790	167025.134295	55.380378
2871.980839	166792.249709	55.385383
2871.377329	166540.340226	55.390388
2870.629234	166300.313180	55.395393
2869.995923	166054.110679	55.400397
2869.579686	165813.177190	55.405402
2868.604038	165570.305198	55.410407
2868.320060	165317.012232	55.415412
2867.193009	165076.560362	55.420417
2866.452649	164831.833072	55.425421
2865.972145	164597.366652	55.430426
2865.100371	164359.355619	55.435431
2864.511558	164106.986658	55.440436
2863.666434	163874.723467	55.445441
2863.185352	163632.057429	55.450445
2862.612658	163397.982040	55.455450
2862.171914	163165.157404	55.460455
2861.547156	162918.563805	55.465460
2860.654220	162681.163357	55.470465
2860.295681	162444.919474	55.475469
2859.518860	162195.099580	55.480474
2858.839628	161953.939583	55.485479
2857.777126	161710.785782	55.490484
2857.286799	161477.291813	55.495489
2856.667811	161234.332042	55.500493
2856.018645	160995.538200	55.505498
2855.226877	160756.388470	55.510503
2854.927767	160501.078195	55.515508
2854.108676	160274.439313	55.520513
2853.435259	160027.272823	55.525517
2852.698422	159783.336647	55.530522
2851.726949	159547.315296	55.535527
2851.244407	159295.083600	55.540532
2850.299739	159075.773531	55.545537
2849.446503	158821.522078	55.550541
2849.050229	158595.913853	55.555546
2848.580814	158362.611606	55.560551
2847.698466	158119.040707	55.565556
2847.187260	157889.322299	55.570561
2846.931292	157656.674376	55.575565
2846.535834	157413.609502	55.580570
2845.574610	157176.251687	55.585575
2845.109047	156932.425803	55.590580
2843.985497	156690.532565	55.595585
2843.163353	156441.021774	55.600589
2842.829398	156200.573602	55.605594
2842.060800	155969.625395	55.610599
2841.229643	155725.347769	55.615604
2841.245258	155491.152314	55.620609
2840.844152	155243.688164	55.625613
2840.062777	154994.128460	55.630618
2838.906612	154746.681943	55.635623
2838.476557	154498.286214	55.640628
2837.776966	154260.061431	55.645633
2837.231897	154012.883851	55.650637
2836.554343	153771.313479	55.655642
2835.536601	153522.782637	55.660647
2835.436800	153276.779874	55.665652
2834.503149	153030.882989	55.670657
2833.305192	152782.705545	55.675661
2833.084541	152535.240147	55.680666
2832.035999	152296.565440	55.685671
2831.406526	152053.776555	55.690676
2830.961845	151814.111412	55.695681
2830.386051	151570.515198	55.700685
2829.688909	151323.291525	55.705690
2828.872298	151096.703678	55.710695
2828.404600	150837.871667	55.715700
2827.430223	150607.168029	55.720705
2826.888776	150358.143615	55.725709
2826.054306	150114.651669	55.730714
2825.451635	149883.405642	55.735719
2824.490853	149644.147388	55.740724
2824.073891	149408.625274	55.745729
2823.323323	149169.842727	55.750733
2823.074108	148921.540721	55.755738
2821.778069	148696.485950	55.760743
2821.627478	148455.240217	55.765748
2820.872976	148217.570640	55.770753
2820.023592	147982.449206	55.775757
2819.686873	147746.949175	55.780762
2818.861417	147500.420768	55.785767
2818.300981	147266.754886	55.790772
2817.193368	147025.071568	55.795777
2816.605926	146791.756600	55.800781
2816.313328	146551.590072	55.805786
2815.982975	146321.234921	55.810791
2815.129249	146074.886108	55.815796
2814.037358	145840.099401	55.820801
2813.495094	145598.735676	55.825805
2812.591810	145361.923559	55.830810
2812.148729	145130.819527	55.835815
2811.855372	144894.096927	55.840820
2810.739339	144653.727517	55.845825
2810.096547	144408.396466	55.850829
2809.732453	144179.039571	55.855834
2808.823211	143948.696575	55.860839
2808.425591	143693.856307	55.865844
2807.657517	143460.962168	55.870849
2807.114165	143224.700052	55.875853
2806.345139	142978.815441	55.880858
2805.563005	142737.054054	55.885863
2804.865844	142495.584912	55.890868
2804.192813	142265.441196	55.895873
2803.809439	142029.617328	55.900877
2803.182575	141786.500922	55.905882
2802.448689	141544.052859	55.910887
2801.614601	141299.246183	55.915892
2800.735525	141071.484688	55.920897
2800.321224	140822.325205	55.925901
2799.431760	140590.029991	55.930906
2799.014639	140353.752695	55.935911
2799.187799	140116.893023	55.940916
2798.080209	139879.796169	55.945921
2797.309045	139631.227373	55.950925
2796.909991	139378.299877	55.955930
2795.622261	139152.387779	55.960935
2795.450455	138900.518212	55.965940
2794.046232	138660.759905	55.970945
2793.392022	138422.959910	55.975949
2793.086537	138190.250412	55.980954
2792.164314	137950.211286	55.985959
2791.969098	137707.532608	55.990964
2791.066844	137467.760401	55.995969
2790.148657	137230.878196	56.000973
2789.329967	136993.370468	56.005978
2788.688615	136756.088325	56.010983
2787.829604	136522.722079	56.015988
2787.187710	136291.303332	56.020993
2786.771101	136068.275351	56.025997
2786.562371	135834.891697	56.031002
2785.666564	135602.122819	56.036007
2784.967006	135360.233523	56.041012
2784.198712	135128.857073	56.046017
2783.308206	134891.325563	56.051021
2782.765810	134665.951430	56.056026
2782.340471	134431.508709	56.061031
2781.973281	134194.973140	56.066036
2780.710189	133961.960684	56.071041
2780.057554	133725.286583	56.076045
2779.705153	133489.884751	56.081050
2778.493018	133248.339894	56.086055
2777.998077	133028.014792	56.091060
2777.272188	132793.304564	56.096065
2777.027462	132565.974610	56.101069
2776.030556	132327.615389	56.106074
2775.414840	132118.451002	56.111079
2775.140710	131874.175833	56.116084
2774.264575	131634.924047	56.121089
2773.425836	131405.225285	56.126093
2772.971262	131168.395977	56.131098
2772.362414	130947.062186	56.136103
2771.676522	130702.103629	56.141108
2770.951418	130474.209487	56.146113
2770.239836	130244.332011	56.151117
2769.771358	130014.147737	56.156122
2769.062136	129776.647738	56.161127
2769.010232	129547.653805	56.166132
2767.990527	129312.612294	56.171137
2767.098015	129068.387779	56.176141
2766.811681	128827.225986	56.181146
2765.799785	128594.170983	56.186151
2764.753144	128347.728928	56.191156
2764.333942	128122.099495	56.196161
2763.935434	127886.212569	56.201165
2762.993366	127646.531603	56.206170
2762.079166	127426.456244	56.211175
2761.664698	127184.096180	56.216180
2760.820280	126952.092138	56.221185
2760.078813	126716.793609	56.226189
2759.578376	126482.357900	56.231194
2758.553036	126256.934391	56.236199
2758.362672	126034.927911	56.241204
2757.454189	125805.751686	56.246209
2757.026973	125566.506949	56.251213
2756.239357	125337.237282	56.256218
2755.469991	125113.582743	56.261223
2755.102392	124874.396696	56.266228
2754.413005	124651.100339	56.271233
2753.644612	124410.575917	56.276237
2752.893839	124177.432982	56.281242
2752.321584	123959.051848	56.286247
2751.810542	123721.589263	56.291252
2751.052204	123497.004308	56.296257
2749.936278	123254.146836	56.301261
2749.629349	123036.311439	56.306266
2748.848327	122813.018734	56.311271
2748.433644	122570.733001	56.316276
2747.626423	122344.474997	56.321281
2747.193287	122121.394751	56.326285
2746.392964	121887.617102	56.331290
2745.771951	121654.572959	56.336295
2745.155656	121423.956581	56.341300
2744.514279	121189.000979	56.346305
2743.659315	120959.026119	56.351309
2743.563667	120723.027991	56.356314
2742.631895	120491.977190	56.361319
2741.788023	120256.085216	56.366324
2741.226819	120030.285388	56.371329
2740.358687	119793.524579	56.376333
2739.550100	119561.786582	56.381338
2739.009751	119345.936251	56.386343
2738.442749	119108.011434	56.391348
2737.850615	118878.642960	56.396353
2737.378906	118648.518830	56.401357
2736.939942	118407.884439	56.406362
2736.228612	118186.672479	56.411367
2735.518927	117941.235170	56.416372
2734.387004	117709.668625	56.421377
2734.084058	117471.915176	56.426381
2733.535160	117233.202097	56.431386
2732.914560	117007.740476	56.436391
2732.162913	116762.802981	56.441396
2731.470521	116540.355301	56.446401
2730.783912	116297.468581	56.451405
2730.116862	116066.483532	56.456410
2728.961942	115827.974504	56.461415
2728.321342	115596.023255	56.466420
2727.425062	115359.862074	56.471425
2726.794832	115138.329180	56.476429
2726.282535	114905.853451	56.481434
2725.638113	114685.393512	56.486439
2725.215686	114459.676570	56.491444
2724.652389	114232.296056	56.496449
2723.611594	114007.653762	56.501453
2722.890573	113774.308337	56.506458
2722.308731	113548.600448	56.511463
2721.516739	113313.136975	56.516468
2720.687527	113097.090421	56.521473
2720.282545	112875.790646	56.526477
2719.909955	112637.695332	56.531482
2719.089131	112414.793609	56.536487
2718.594877	112188.446518	56.541492
2717.474323	111961.115967	56.546497
2716.732213	111738.523688	56.551501
2716.340870	111515.720809	56.556506
2715.673573	111283.441004	56.561511
2715.218375	111055.038800	56.566516
2714.158235	110840.674795	56.571521
2713.477004	110614.601001	56.576525
2713.091540	110382.420240	56.581530
2711.884510	110171.337890	56.586535
2711.494901	109947.391494	56.591540
2710.887742	109727.357724	56.596545
2710.238625	109506.342250	56.601549
2709.801676	109280.491593	56.606554
2708.977271	109054.353405	56.611559
2708.190162	108823.130692	56.616564
2707.795859	108599.018240	56.621569
2707.286089	108375.651243	56.626573
2706.440838	108156.140621	56.631578
2705.579432	107933.866006	56.636583
2705.488665	107702.406738	56.641588
2704.678925	107474.526554	56.646593
2703.528599	107259.062902	56.651597
2703.174261	107035.083442	56.656602
2702.413488	106813.969096	56.661607
2702.292717	106568.936579	56.666612
2701.240089	106347.723535	56.671617
2700.812042	106122.303850	56.676621
2699.966997	105895.408084	56.681626
2699.149231	105676.090602	56.686631
2698.885834	105436.070580	56.691636
2698.186825	105205.104875	56.696641
2697.247310	104976.937780	56.701645
2696.786842	104745.274960	56.706650
2695.496604	104527.076179	56.711655
2695.138698	104296.783801	56.716660
2694.260099	104074.962951	56.721665
2693.589406	103865.196618	56.726669
2693.227898	103628.612580	56.731674
2692.713496	103417.223176	56.736679
2691.875618	103185.384489	56.741684
2691.054327	102960.211059	56.746689
2690.102991	102739.162957	56.751693
2689.470849	102511.320020	56.756698
2689.301712	102300.439208	56.761703
2688.732175	102079.598020	56.766708
2687.650880	101855.024443	56.771713
2687.204937	101632.388351	56.776717
2686.523921	101407.585137	56.781722
2685.867943	101180.773545	56.786727
2685.393922	100960.712642	56.791732
2684.542121	100734.065366	56.796737
2683.837996	100506.264873	56.801741
2683.147924	100282.640944	56.806746
2682.491097	100062.656971	56.811751
2681.788782	99841.781241	56.816756
2681.164947	99622.823719	56.821761
2680.421200	99409.188932	56.826765
2679.855523	99164.561343	56.831770
2679.208727	98955.027062	56.836775
2678.062060	98732.878374	56.841780
2677.899545	98517.348921	56.846785
2676.770089	98294.439379	56.851789
2676.604341	98072.135097	56.856794
2675.719018	97860.524131	56.861799
2675.003569	97639.656862	56.866804
2674.098243	97422.124543	56.871809
2673.881211	97213.394283	56.876813
2673.216158	96982.432013	56.881818
2672.303477	96769.736722	56.886823
2671.597970	96546.078168	56.891828
2671.245224	96319.194139	56.896833
2670.044560	96100.390755	56.901837
2670.121601	95886.061226	56.906842
2669.412442	95683.279514	56.911847
2668.778811	95444.392358	56.916852
2668.033158	95230.589826	56.921857
2667.546336	95008.544973	56.926861
2666.325417	94776.777617	56.931866
2665.875535	94565.176900	56.936871
2665.048545	94342.396426	56.941876
2664.395195	94123.770566	56.946881
2663.635748	93906.745007	56.951885
2663.392396	93684.822601	56.956890
2662.441792	93472.770946	56.961895
2661.781486	93247.839414	56.966900
2661.051283	93027.472069	56.971905
2660.243485	92812.304718	56.976909
2659.663518	92601.225232	56.981914
2658.837444	92382.872674	56.986919
2658.476051	92164.125324	56.991924
2657.729836	91950.776236	56.996929
2657.146379	91744.273719	57.001933
2656.519972	91520.234190	57.006938
2656.098560	91304.227078	57.011943
2655.479243	91078.940258	57.016948
2655.093843	90861.560227	57.021953
2654.170080	90642.573540	57.026957
2653.361348	90411.455608	57.031962
2652.485257	90195.574076	57.036967
2651.936258	89974.435337	57.041972
2651.291228	89760.167969	57.046977
2650.775882	89543.906947	57.051981
2650.282039	89316.958845	57.056986
2649.856731	89097.240967	57.061991
2649.166185	88872.342066	57.066996
2648.435261	88643.689557	57.072001
2647.398949	88425.053018	57.077005
2647.068646	88198.899617	57.082010
2646.353455	87968.315627	57.087015
2645.202799	87742.490741	57.092020
2644.445976	87525.305637	57.097025
2643.896511	87308.575598	57.102029
2643.726876	87090.558084	57.107034
2642.729844	86875.044162	57.112039
2641.991291	86597.933690	57.117044
2641.479253	86378.261850	57.122049
2640.609185	86166.666177	57.127053
2640.282923	85934.017818	57.132058
2639.448330	85717.972716	57.137063
2638.648460	85500.883199	57.142068
2637.937629	85284.922397	57.147073
2637.187582	85067.828337	57.152077
2636.846948	84845.622793	57.157082
2635.980647	84632.904602	57.162087
2635.326008	84408.270020	57.167092
2634.656935	84188.080739	57.172097
2634.086290	83975.945991	57.177101
2633.707970	83750.299866	57.182106
2632.617385	83545.889386	57.187111
2632.147044	83318.708948	57.192116
2631.349754	83097.695439	57.197121
2630.468353	82882.052305	57.202125
2629.659200	82664.356232	57.207130
2629.185313	82466.072700	57.212135
2628.659687	82238.455511	57.217140
2628.216896	82017.867402	57.222145
2627.644469	81809.044804	57.227149
2627.184168	81588.324224	57.232154
2626.568673	81371.323946	57.237159
2625.834519	81144.596772	57.242164
2625.117719	80919.790773	57.247169
2624.450484	80704.518204	57.252173
2623.545816	80472.562185	57.257178
2622.520074	80256.676406	57.262183
2622.058654	80033.142027	57.267188
2621.139573	79807.810633	57.272193
2620.011470	79607.221565	57.277197
2619.700952	79388.665642	57.282202
2618.891017	79185.222492	57.287207
2618.484250	78983.951114	57.292212
2618.052899	78767.647979	57.297217
2617.318390	78561.146831	57.302221
2616.784980	78331.863571	57.307226
2615.777468	78125.799922	57.312231
2615.298651	77909.696987	57.317236
2614.836805	77698.685884	57.322241
2614.148234	77489.802022	57.327245
2613.299850	77267.584940	57.332250
2612.751447	77054.317891	57.337255
2611.972402	76845.068606	57.342260
2611.648590	76633.479440	57.347265
2610.595360	76418.040702	57.352269
2610.369564	76199.545437	57.357274
2609.671698	75982.654972	57.362279
2608.699617	75763.511509	57.367284
2607.986925	75550.293161	57.372289
2607.035556	75343.795134	57.377293
2606.585451	75126.388673	57.382298
2605.582581	74928.153373	57.387303
2605.167212	74701.727820	57.392308
2604.870734	74489.279166	57.397313
2603.746995	74289.491271	57.402317
2603.425739	74068.959635	57.407322
2602.702167	73867.001920	57.412327
2602.092907	73645.109694	57.417332
2601.720073	73436.520427	57.422337
2600.501471	73229.998964	57.427341
2600.169431	73009.207079	57.432346
2599.197170	72804.784315	57.437351
2598.747120	72594.713468	57.442356
2597.928482	72385.766505	57.447361
2597.243113	72179.702694	57.452365
2596.633924	71957.580172	57.457370
2595.971517	71751.909562	57.462375
2595.275436	71537.940841	57.467380
2594.760268	71331.817870	57.472385
2594.172279	71132.296744	57.477389
2593.560150	70905.493675	57.482394
2592.481388	70706.256886	57.487399
2592.125202	70491.859920	57.492404
2591.516881	70275.511086	57.497409
2590.377597	70076.258720	57.502413
2589.842394	69858.785725	57.507418
2589.530199	69649.873494	57.512423
2588.528957	69447.820162	57.517428
2588.186199	69238.137350	57.522433
2587.227662	69036.873017	57.527437
2586.845149	68813.685156	57.532442
2585.915118	68607.899888	57.537447
2585.523996	68403.273325	57.542452
2585.011727	68189.902130	57.547457
2584.244787	67987.030036	57.552461
2583.807474	67769.092281	57.557466
2582.770425	67551.500152	57.562471
2582.168238	67346.590115	57.567476
2581.667338	67133.759979	57.572481
2581.006610	66930.036663	57.577485
2580.478856	66709.767080	57.582490
2579.512934	66498.544110	57.587495
2578.263170	66281.020322	57.592500
2577.980283	66068.512194	57.597505
2576.982898	65880.107390	57.602509
2576.539625	65665.000185	57.607514
2576.037762	65455.204176	57.612519
2575.390183	65253.966710	57.617524
2575.272209	65059.175509	57.622529
2574.131945	64857.880256	57.627533
2573.469094	64627.773947	57.632538
2572.785525	64421.689125	57.637543
2572.476741	64208.494244	57.642548
2571.570255	64008.751685	57.647553
2570.996626	63802.058367	57.652557
2570.615362	63584.597713	57.657562
2569.963193	63364.669486	57.662567
2569.279843	63153.095807	57.667572
2568.526488	62942.905192	57.672577
2567.520406	62735.288635	57.677581
2566.768362	62513.725968	57.682586
2565.902855	62308.833823	57.687591
2565.125827	62103.180745	57.692596
2564.812269	61894.902825	57.697601
2564.049488	61699.841164	57.702605
2563.550958	61487.422623	57.707610
2562.646911	61281.076955	57.712615
2561.838191	61071.776597	57.717620
2561.228014	60872.070504	57.722625
2560.593630	60673.720276	57.727629
2560.055398	60460.140384	57.732634
2559.116292	60264.247909	57.737639
2558.333669	60061.866936	57.742644
2557.827926	59859.275867	57.747649
2556.790754	59681.218497	57.752653
2556.664702	59462.331673	57.757658
2555.882043	59265.129301	57.762663
2555.107869	59062.047045	57.767668
2554.725134	58861.478845	57.772673
2553.608266	58670.035861	57.777677
2553.416221	58466.638232	57.782682
2552.567945	58260.154973	57.787687
2552.039643	58063.909184	57.792692
2551.754349	57852.239471	57.797697
2550.706982	57654.616370	57.802701
2549.833390	57450.623085	57.807706
2549.311399	57248.073378	57.812711
2548.825444	57054.852372	57.817716
2548.386604	56849.390576	57.822721
2547.301092	56649.889370	57.827725
2547.038000	56444.217909	57.832730
2546.091756	56248.986161	57.837735
2545.580907	56043.190078	57.842740
2545.020535	55844.943880	57.847745
2544.048334	55635.264776	57.852749
2543.564859	55422.437965	57.857754
2542.534841	55230.379134	57.862759
2542.067982	55022.279911	57.867764
2541.971249	54818.554239	57.872769
2540.557266	54625.857299	57.877773
2540.240894	54411.903998	57.882778
2539.458097	54224.291483	57.887783
2538.823964	54014.945323	57.892788
2538.525350	53808.686121	57.897793
2537.650700	53602.039747	57.902797
2536.919775	53398.075903	57.907802
2535.995675	53199.614042	57.912807
2534.983285	52997.051731	57.917812
2534.453084	52794.801803	57.922817
2533.900791	52608.286357	57.927821
2533.190064	52405.748203	57.932826
2532.500168	52216.453806	57.937831
2531.847867	52015.486931	57.942836
2531.583657	51816.995803	57.947841
2530.434436	51620.653248	57.952845
2529.984998	51433.295201	57.957850
2529.278237	51241.143679	57.962855
2528.729868	51031.219006	57.967860
2528.252458	50829.385582	57.972865
2527.540485	50640.445814	57.977869
2526.954318	50440.737838	57.982874
2526.074689	50250.253371	57.987879
2525.635372	50045.558643	57.992884
2525.110835	49836.326739	57.997889
2524.071697	49641.441930	58.002893
2523.471092	49435.280116	58.007898
2522.804340	49247.448119	58.012903
2522.109824	49039.393849	58.017908
2521.489011	48834.134864	58.022913
2520.742506	48651.559911	58.027917
2520.268759	48452.727071	58.032922
2519.569558	48253.250835	58.037927
2518.461780	48055.664091	58.042932
2517.963175	47860.891569	58.047937
2517.469513	47662.925199	58.052941
2517.051152	47463.222278	58.057946
2516.428969	47278.707501	58.062951
2515.213604	47069.607707	58.067956
2515.028911	46870.744894	58.072961
2514.202846	46672.931009	58.077965
2513.405578	46476.608717	58.082970
2512.904285	46279.702739	58.087975
2511.923031	46086.189522	58.092980
2511.592115	45883.382008	58.097985
2510.680050	45690.674665	58.102989
2509.696839	45487.675745	58.107994
2509.034471	45314.283936	58.112999
2508.457116	45118.359067	58.118004
2507.900142	44926.713177	58.123009
2506.883820	44748.397387	58.128013
2506.435685	44543.724549	58.133018
2505.991518	44364.953619	58.138023
2505.220892	44179.933727	58.143028
2504.936548	43981.352277	58.148033
2503.684080	43799.540006	58.153037
2503.455488	43602.589723	58.158042
2502.628089	43409.979650	58.163047
2501.864287	43224.125831	58.168052
2501.334090	43029.775155	58.173057
2500.656685	42837.354211	58.178061
2499.982297	42640.366705	58.183066
2499.288383	42457.338567	58.188071
2498.663215	42270.587239	58.193076
2498.540965	42074.356467	58.198081
2497.476426	41888.934432	58.203085
2497.063182	41691.788758	58.208090
2496.223324	41502.077739	58.213095
2495.540778	41309.711292	58.218100
2494.878271	41110.230795	58.223105
2493.935766	40921.533970	58.228109
2493.451471	40730.981810	58.233114
2492.989265	40543.735533	58.238119
2492.283638	40350.809984	58.243124
2491.547155	40157.018108	58.248129
2490.849480	39972.302520	58.253133
2490.561952	39767.343985	58.258138
2489.515024	39580.599835	58.263143
2489.118347	39380.259977	58.268148
2488.407936	39184.005023	58.273153
2487.666986	38991.020499	58.278157
2487.233967	38794.975443	58.283162
2486.672818	38610.117144	58.288167
2485.377674	38415.701533	58.293172
2484.993474	38218.831361	58.298177
2483.693790	38025.404917	58.303181
2482.952345	37838.879312	58.308186
2482.260689	37656.448646	58.313191
2481.775108	37476.658775	58.318196
2481.625123	37283.537271	58.323201
2480.703981	37104.072359	58.328205
2480.065367	36909.319900	58.333210
2479.238553	36720.003699	58.338215
2478.409142	36533.496892	58.343220
2477.828685	36351.145632	58.348225
2476.908737	36175.819362	58.353229
2476.390155	35988.321943	58.358234
2475.509950	35814.985977	58.363239
2474.699334	35629.108588	58.368244
2474.278479	35449.928792	58.373249
2473.554184	35281.061540	58.378253
2473.162844	35089.884094	58.383258
2472.676649	34914.074946	58.388263
2471.810725	34737.924227	58.393268
2471.597446	34559.021488	58.398273
2470.384279	34373.488390	58.403277
2469.877556	34188.712894	58.408282
2469.427911	33999.407948	58.413287
2468.436730	33833.542458	58.418292
2468.058265	33636.730167	58.423297
2467.436559	33471.760385	58.428301
2466.565368	33277.564333	58.433306
2466.000956	33096.246000	58.438311
2465.210070	32905.903461	58.443316
2464.563097	32730.082912	58.448321
2463.741161	32553.518839	58.453325
2463.320370	32374.217613	58.458330
2462.528241	32186.996143	58.463335
2461.481295	32013.544771	58.468340
2461.321108	31828.889247	58.473345
2460.288211	31660.320593	58.478349
2459.631149	31486.946867	58.483354
2459.026836	31309.608039	58.488359
2458.124007	31142.698779	58.493364
2457.724137	30967.112696	58.498369
2456.743948	30782.690424	58.503373
2456.391092	30614.986592	58.508378
2455.575541	30444.285334	58.513383
2454.745588	30268.934674	58.518388
2454.402126	30096.805224	58.523393
2453.490228	29934.935579	58.528397
2452.958013	29752.285355	58.533402
2452.083525	29585.003087	58.538407
2451.342675	29414.431817	58.543412
2451.033980	29244.294433	58.548417
2450.129785	29074.105495	58.553421
2449.703592	28893.584375	58.558426
2449.007045	28736.310375	58.563431
2448.072700	28562.595037	58.568436
2447.324985	28392.173983	58.573441
2446.647507	28232.339055	58.578445
2445.996438	28060.753301	58.583450
2445.081038	27892.206678	58.588455
2444.240191	27734.425404	58.593460
2443.757442	27568.698931	58.598465
2442.655078	27423.794343	58.603469
2442.430003	27265.848738	58.608474
2441.758212	27115.163944	58.613479
2440.292008	26960.469704	58.618484
2439.849250	26810.358814	58.623489
2438.861971	26659.855231	58.628493
2437.947688	26516.643419	58.633498
2437.179694	26389.901761	58.638503
2436.811062	26258.168300	58.643508
2436.134568	26111.085874	58.648513
2435.082776	25966.959583	58.653517
2434.292570	25831.227836	58.658522
2434.265463	25691.049627	58.663527
2433.045239	25554.239186	58.668532
2432.480535	25420.856720	58.673537
2431.462579	25305.004005	58.678541
2430.985464	25172.180902	58.683546
2429.916689	25043.232902	58.688551
2429.204821	24916.116032	58.693556
2428.756844	24782.873470	58.698561
2428.025133	24667.776184	58.703565
2427.602929	24540.906649	58.708570
2426.994640	24408.747472	58.713575
2426.219345	24278.822061	58.718580
2425.356496	24156.078579	58.723585
2424.729170	24044.275455	58.728589
2424.073730	23917.918395	58.733594
2423.299263	23796.395673	58.738599
2422.432661	23674.342481	58.743604
2422.083856	23562.902790	58.748609
2421.286325	23446.145718	58.753613
2420.673428	23320.035581	58.758618
2420.135236	23198.365997	58.763623
2419.448290	23078.408156	58.768628
2418.898181	22967.436792	58.773633
2418.036272	22850.210956	58.778637
2417.588934	22729.654879	58.783642
2416.763031	22617.385861	58.788647
2416.039661	22497.106283	58.793652
2415.814578	22372.928898	58.798657
2415.132877	22257.519781	58.803661
2414.338037	22133.906363	58.808666
2413.496532	22010.899434	58.813671
2412.868308	21900.289820	58.818676
2412.169543	21786.309686	58.823681
2411.735744	21666.071802	58.828685
2410.953189	21544.512637	58.833690
2410.261178	21424.360125	58.838695
2409.918080	21312.333302	58.843700
2409.685578	21182.333747	58.848705
2408.223344	21067.491383	58.853709
2407.582170	20947.395192	58.858714
2406.868479	20834.453129	58.863719
2406.289623	20717.648803	58.868724
2405.949127	20601.209225	58.873729
2405.155265	20486.790835	58.878733
2404.572885	20360.197725	58.883738
2403.986468	20242.640725	58.888743
2402.849866	20129.239750	58.893748
2402.583855	20008.910563	58.898753
2401.836299	19894.456627	58.903757
2401.003334	19770.838404	58.908762
2400.557535	19658.310457	58.913767
2399.793799	19540.298597	58.918772
2399.551960	19426.580190	58.923777
2398.574651	19312.926649	58.928781
2398.234582	19189.070319	58.933786
2397.530424	19063.288593	58.938791
2396.982192	18950.324453	58.943796
2396.142861	18820.851381	58.948801
2395.148879	18703.352616	58.953805
2394.624487	18588.276596	58.958810
2394.037937	18466.446718	58.963815
2393.321275	18354.055956	58.968820
2392.726383	18232.975263	58.973825
2392.083408	18119.754688	58.978829
2391.876684	17995.753115	58.983834
2390.963658	17877.936461	58.988839
2390.435588	17758.177053	58.993844
2389.814515	17630.242189	58.998849
2389.207073	17509.905399	59.003853
2388.500333	17389.638608	59.008858
2387.670607	17260.169572	59.013863
2386.857099	17135.192252	59.018868
2386.422263	17012.272195	59.023873
2385.437227	16896.126403	59.028877
2385.017738	16767.199531	59.033882
2384.398529	16646.834594	59.038887
2383.502804	16545.445740	59.043892
2383.183860	16419.504125	59.048897
2382.370590	16303.268280	59.053901
2381.924976	16171.608354	59.058906
2381.087196	16046.870900	59.063911
2380.128123	15928.911462	59.068916
2379.727367	15789.351045	59.073921
2379.015225	15685.105498	59.078925
2378.108724	15568.688421	59.083930
2377.693431	15450.351759	59.088935
2376.459843	15342.796525	59.093940
2376.218580	15217.508135	59.098945
2375.915558	15104.455278	59.103949
2374.882210	14983.509407	59.108954
2374.140442	14860.897884	59.113959
2373.308208	14744.979583	59.118964
2373.247123	14620.657322	59.123969
2371.805665	14516.441089	59.128973
2371.331055	14401.412218	59.133978
2371.216349	14283.557124	59.138983
2370.280792	14181.854468	59.143988
2369.519186	14050.082053	59.148993
2368.688969	13939.157905	59.153997
2367.854182	13824.480652	59.159002
2367.440009	13711.857671	59.164007
2366.636295	13596.321789	59.169012
2366.211814	13485.565181	59.174017
2365.487208	13379.582238	59.179021
2364.706951	13261.377330	59.184026
2363.865437	13151.827258	59.189031
2363.288343	13048.550169	59.194036
2362.714197	12926.565867	59.199041
2361.933957	12820.333730	59.204045
2361.287706	12710.497223	59.209050
2361.177068	12597.177360	59.214055
2360.010978	12492.102018	59.219060
2359.849672	12384.583365	59.224065
2359.098420	12269.815743	59.229069
2358.242751	12148.498421	59.234074
2357.829718	12030.468677	59.239079
2356.821114	11920.282277	59.244084
2356.073247	11798.304452	59.249089
2355.110026	11700.862674	59.254093
2354.466841	11585.695836	59.259098
2354.341841	11482.818972	59.264103
2353.457973	11370.764753	59.269108
2352.893012	11255.962897	59.274113
2352.153612	11154.525081	59.279117
2351.469387	11041.677433	59.284122
2351.093180	10936.663446	59.289127
2350.253261	10825.779356	59.294132
2349.691140	10706.854061	59.299137
2348.818944	10599.895258	59.304141
2348.155624	10484.283026	59.309146
2347.943619	10377.136962	59.314151
2346.679671	10272.961560	59.319156
2346.521026	10156.097823	59.324161
2345.699086	10048.355169	59.329165
2345.047599	9937.655026	59.334170
2344.229504	9819.727892	59.339175
2343.325377	9721.788605	59.344180
2342.813695	9609.501174	59.349185
2341.976610	9499.812083	59.354189
2340.971450	9401.230066	59.359194
2340.550270	9290.926237	59.364199
2339.696516	9197.207456	59.369204
2339.309229	9101.259379	59.374209
2338.186130	8992.703194	59.379213
2337.298686	8895.996683	59.384218
2336.674741	8789.822506	59.389223
2335.814868	8706.538678	59.394228
2335.304727	8611.293800	59.399233
2334.784246	8524.679678	59.404237
2334.298100	8424.721861	59.409242
2333.474711	8336.424442	59.414247
2332.363312	8252.681251	59.419252
2331.671129	8161.328555	59.424257
2330.787449	8086.241086	59.429261
2330.246710	8003.641655	59.434266
2329.355253	7921.740012	59.439271
2328.284887	7848.119118	59.444276
2327.896619	7772.393940	59.449281
2326.850173	7696.285658	59.454285
2326.096146	7630.788669	59.459290
2325.418395	7561.545459	59.464295
2324.311839	7494.817172	59.469300
2323.672511	7424.812923	59.474305
2322.866707	7369.096550	59.479309
2322.184906	7304.714011	59.484314
2321.925477	7248.772730	59.489319
2320.902207	7199.336694	59.494324
2320.681895	7132.595793	59.499329
2319.590990	7078.285255	59.504333
2318.852627	7020.495632	59.509338
2318.232857	6967.735025	59.514343
2317.310645	6916.590075	59.519348
2317.180779	6856.747811	59.524353
2316.450321	6801.074233	59.529357
2315.688185	6750.443438	59.534362
2315.131551	6691.114672	59.539367
2314.610365	6633.904538	59.544372
2313.779278	6576.837634	59.549377
2313.227998	6525.749760	59.554381
2312.764426	6469.358033	59.559386
2312.181077	6410.232316	59.564391
2311.214228	6354.603874	59.569396
2310.573202	6287.571987	59.574401
2309.895087	6237.825604	59.579405
2309.135967	6187.280580	59.584410
2308.891064	6123.723650	59.589415
2307.443868	6075.129634	59.594420
2307.316778	6018.983638	59.599425
2306.634380	5961.750564	59.604429
2305.676327	5906.554955	59.609434
2305.321251	5854.484839	59.614439
2304.643371	5815.739869	59.619444
2304.273009	5753.301217	59.624449
2303.439103	5710.209694	59.629453
2302.739099	5654.961354	59.634458
2302.155186	5589.625265	59.639463
2301.300063	5545.324023	59.644468
2300.966080	5487.360237	59.649473
2300.440319	5430.312349	59.654477
2299.476048	5364.528125	59.659482
2298.514617	5316.776528	59.664487
2297.802963	5266.468747	59.669492
2297.335289	5209.320903	59.674497
2297.020117	5155.792413	59.679501
2296.225887	5115.009523	59.684506
2295.693696	5044.955521	59.689511
2294.740126	4996.205377	59.694516
2294.459745	4944.656130	59.699521
2293.297359	4887.835925	59.704525
2292.849087	4837.794017	59.709530
2292.314828	4775.461455	59.714535
2291.552937	4734.450535	59.719540
2291.284928	4676.581866	59.724545
2290.157288	4623.855056	59.729549
2289.619076	4565.542614	59.734554
2289.306263	4510.241517	59.739559
2288.324578	4459.774788	59.744564
2287.842895	4404.236822	59.749569
2287.335983	4353.397070	59.754573
2286.441064	4295.086607	59.759578
2285.928558	4242.213237	59.764583
2284.957248	4188.673864	59.769588
2284.466440	4132.901515	59.774593
2283.793357	4077.712491	59.779597
2283.042054	4027.795236	59.784602
2282.386859	3968.848014	59.789607
2281.615598	3924.226636	59.794612
2281.084779	3866.887538	59.799617
2280.181520	3813.336220	59.804621
2279.276849	3765.043439	59.809626
2279.067759	3716.619223	59.814631
2278.576170	3667.638614	59.819636
2277.966887	3610.294913	59.824641
2277.015017	3566.721668	59.829645
2276.569321	3513.086805	59.834650
2276.129493	3463.666849	59.839655
2275.731066	3411.253672	59.844660
2275.084454	3358.151145	59.849665
2274.071135	3291.070017	59.854669
2273.512425	3233.077091	59.859674
2272.736561	3181.294574	59.864679
2271.826592	3136.842849	59.869684
2271.172767	3069.375086	59.874689
2270.541565	3019.683674	59.879693
2269.356234	2973.324480	59.884698
2269.399551	2919.000820	59.889703
2268.353731	2866.595935	59.894708
2267.859627	2814.961465	59.899713
2267.400177	2774.924050	59.904718
2266.522323	2722.945716	59.909722
2266.265519	2669.881493	59.914727
2265.394649	2618.007325	59.919732
2265.002300	2564.311295	59.924737
2264.219199	2511.136269	59.929742
2262.854973	2454.309601	59.934746
2262.529432	2400.055542	59.939751
2261.747662	2353.738125	59.944756
2261.135724	2296.910498	59.949761
2260.472673	2262.088666	59.954766
2259.862642	2208.686890	59.959770
2259.375677	2156.183280	59.964775
2258.358295	2110.361650	59.969780
2257.784333	2062.415470	59.974785
2257.688756	2012.618273	59.979790
2256.744691	1963.414789	59.984794
2256.431699	1901.125210	59.989799
2255.704610	1854.010384	59.994804
2255.116007	1797.204656	59.999809
2254.239452	1754.756923	60.004814
2253.916157	1697.205877	60.009818
2253.169417	1633.378542	60.014823
2252.190302	1593.807631	60.019828
2251.437213	1535.041400	60.024833
2250.931211	1484.811169	60.029838
2249.870949	1432.905807	60.034842
2249.212338	1382.727266	60.039847
2248.214283	1335.290851	60.044852
2248.162180	1288.782719	60.049857
2247.222372	1244.369883	60.054862
2246.509568	1191.522059	60.059866
2245.876035	1143.682037	60.064871
2244.699456	1103.767576	60.069876
2244.420550	1063.502331	60.074881
2243.847096	1019.225253	60.079886
2242.953175	974.588624	60.084890
2242.695070	924.202535	60.089895
2241.806847	882.909443	60.094900
2241.042311	836.422646	60.099905
2240.739367	798.945105	60.104910
2239.526588	757.000479	60.109914
2239.209070	715.528917	60.114919
2238.835382	684.358608	60.119924
2238.094026	628.527847	60.124929
2237.373604	581.983343	60.129934
2236.759648	540.722018	60.134938
2236.122132	488.781843	60.139943
2235.241708	459.256643	60.144948
2234.722013	405.465841	60.149953
2233.828612	359.060926	60.154958
2232.951077	321.295173	60.159962
2232.648394	276.611538	60.164967
2231.925126	245.089007	60.169972
2231.149926	196.832841	60.174977
2230.803687	158.711370	60.179982
2229.514320	124.512974	60.184986
2229.165828	77.841243	60.189991
2227.843885	43.974635	60.194996
2227.400252	16.122213	60.200001
2226.667487	-16.585869	60.205006
2225.746557	-37.915170	60.210010
2222.920259	-17.774865	60.215015
2218.803255	58.368252	60.220020
2219.303982	54.271914	60.225025
2220.507151	51.951680	60.230030
2220.325456	54.120197	60.235034
2220.875370	49.613229	60.240039
2220.646944	64.648515	60.245044
2219.462719	59.255138	60.250049
2218.466443	64.931895	60.255054
2217.616207	69.163873	60.260058
2216.868960	57.124078	60.265063
2216.042835	65.305837	60.270068
2214.879963	63.505098	60.275073
2214.952203	64.933904	60.280078
2214.272867	68.028677	60.285082
2213.431560	70.524730	60.290087
2213.236865	72.631134	60.295092
2212.764705	68.285928	60.300097
2212.353646	63.706074	60.305102
2211.298797	74.095148	60.310106
2210.719034	65.538529	60.315111
2209.810225	65.221512	60.320116
2209.195368	71.841157	60.325121
2208.062344	72.911243	60.330126
2207.574800	73.338463	60.335130
2207.331271	65.921132	60.340135
2206.855147	65.421176	60.345140
2205.813249	74.993729	60.350145
2205.193516	74.426758	60.355150
2204.189974	81.686803	60.360154
2204.275956	69.483188	60.365159
2203.628050	79.876089	60.370164
2203.261566	70.370796	60.375169
2202.143386	67.802187	60.380174
2201.100536	78.897340	60.385178
2201.264269	67.457634	60.390183
2200.455155	72.568332	60.395188
2199.938959	69.705332	60.400193
2198.967037	63.745147	60.405198
2197.984605	68.946273	60.410202
2197.613554	69.650794	60.415207
2196.586816	80.303080	60.420212
2195.934989	70.319242	60.425217
2195.169662	67.736866	60.430222
2194.246546	78.256961	60.435226
2194.442450	63.301908	60.440231
2193.965425	64.299278	60.445236
2192.722913	66.829213	60.450241
2192.174778	70.714277	60.455246
2191.718915	69.772323	60.460250
2191.024598	69.621513	60.465255
2190.565769	63.960799	60.470260
2190.043954	71.310553	60.475265
2189.504183	67.587151	60.480270
2188.084254	71.855776	60.485274
2187.566708	68.666575	60.490279
2187.105472	79.197280	60.495284
2186.784818	74.681303	60.500289
2186.069224	76.518389	60.505294
2184.785283	78.880946	60.510298
2184.339085	75.126934	60.515303
2183.819289	80.858786	60.520308
2183.617388	80.589420	60.525313
2182.838808	69.868612	60.530318
2181.401425	75.031106	60.535322
2181.131600	67.733138	60.540327
2180.424031	71.510871	60.545332
2180.054778	73.748967	60.550337
2179.053879	77.129256	60.555342
2178.059580	76.255706	60.560346
2178.001708	68.124945	60.565351
2177.212190	67.222688	60.570356
2176.714358	66.505799	60.575361
2176.250093	73.865448	60.580366
2175.048596	67.665068	60.585370
2174.801492	64.718947	60.590375
2173.754739	69.710428	60.595380
2173.033325	69.083091	60.600385
2172.729683	63.930290	60.605390
2172.248847	72.523507	60.610394
2171.428430	75.549260	60.615399
2170.270302	77.937274	60.620404
2169.947023	66.369294	60.625409
2169.455624	74.931162	60.630414
2168.586514	77.096860	60.635418
2167.994802	67.771009	60.640423
2167.450652	71.749337	60.645428
2166.421893	74.033124	60.650433
2166.115274	63.868289	60.655438
2165.443640	74.884165	60.660442
2164.696375	71.842408	60.665447
2163.691709	65.737443	60.670452
2163.562991	72.357628	60.675457
2162.711932	77.486952	60.680462
2161.954233	80.207125	60.685466
2161.679660	69.596693	60.690471
2161.045584	74.738641	60.695476
2160.114714	75.153269	60.700481
2159.506376	74.689349	60.705486
2158.605958	78.042983	60.710490
2158.373806	67.631736	60.715495
2157.433646	77.373993	60.720500
2156.912630	73.306743	60.725505
2156.663233	70.273387	60.730510
2156.301959	72.659717	60.735514
2155.368193	69.696831	60.740519
2154.041985	66.420556	60.745524
2153.182145	72.837377	60.750529
2152.471427	71.482719	60.755534
2152.354007	77.809275	60.760538
2151.824806	75.293885	60.765543
2150.811743	72.760990	60.770548
2149.852164	80.174962	60.775553
2149.297422	76.478596	60.780558
2148.993927	74.637072	60.785562
2148.599147	73.130883	60.790567
2147.677611	70.207353	60.795572
2147.514966	77.083199	60.800577
2147.135421	61.145831	60.805582
2146.018192	69.006742	60.810586
2144.660284	63.990442	60.815591
2143.924545	71.780976	60.820596
2143.879201	66.993719	60.825601
2143.218294	66.322487	60.830606
2141.873029	77.543573	60.835610
2141.561535	70.220763	60.840615
2140.907754	71.617431	60.845620
2140.209318	69.628729	60.850625
2139.635107	59.587032	60.855630
2138.982631	72.392839	60.860634
2138.412944	65.564567	60.865639
2137.783507	71.758043	60.870644
2137.559487	73.961828	60.875649
2136.894929	64.751072	60.880654
2136.377524	73.849864	60.885658
2135.584844	70.287745	60.890663
2134.292012	71.212686	60.895668
2133.415612	70.124383	60.900673
2133.055686	63.867315	60.905678
2132.255885	77.015677	60.910682
2131.946470	62.770321	60.915687
2131.055343	58.027466	60.920692
2130.333102	69.775119	60.925697
2130.433723	62.137499	60.930702
2129.395369	66.016019	60.935706
2129.312302	68.322401	60.940711
2128.034986	70.211356	60.945716
2127.336290	65.538609	60.950721
2126.582550	66.076098	60.955726
2125.783237	79.173855	60.960730
2125.481078	62.354477	60.965735
2124.815621	70.737702	60.970740
2123.895169	70.109284	60.975745
2123.698730	65.502601	60.980750
2122.239502	72.655465	60.985754
2121.626536	64.602284	60.990759
2121.200537	65.590933	60.995764
2120.812999	72.072233	61.000769
2120.163027	66.070817	61.005774
2119.344788	71.880553	61.010778
2118.917650	66.319424	61.015783
2118.371497	60.336963	61.020788
2117.723546	65.185639	61.025793
2116.716321	63.787757	61.030798
2115.211621	69.367549	61.035802
2115.641763	65.403665	61.040807
2114.331855	64.893963	61.045812
2113.415202	63.518089	61.050817
2114.291557	60.457581	61.055822
2113.313270	70.520948	61.060826
2112.677697	64.481546	61.065831
2111.722257	61.396857	61.070836
2110.208463	66.351391	61.075841
2109.710218	57.683752	61.080846
2109.558855	61.292940	61.085850
2108.695567	55.464982	61.090855
2108.050394	65.651759	61.095860
2107.355698	66.226123	61.100865
2107.234727	53.327304	61.105870
2106.245588	64.978505	61.110874
2106.113825	59.381860	61.115879
2105.000725	66.206720	61.120884
2103.876189	67.217746	61.125889
2103.238814	63.755382	61.130894
2102.625083	77.848455	61.135898
2102.184263	68.631014	61.140903
2101.439324	68.552818	61.145908
2101.077975	62.892418	61.150913
2100.984076	67.851191	61.155918
2100.149381	70.196924	61.160922
2099.304180	69.962200	61.165927
2098.120912	59.729435	61.170932
2097.312850	70.105120	61.175937
2097.306810	62.655474	61.180942
2096.653913	72.079399	61.185946
2095.883286	64.896705	61.190951
2094.744011	69.615877	61.195956
2093.921860	65.887105	61.200961
2093.733764	70.870279	61.205966
2092.751193	71.467437	61.210970
2092.400759	61.818113	61.215975
2091.694380	73.717787	61.220980
2091.531903	73.260506	61.225985
2090.750142	67.283215	61.230990
2089.396773	70.004625	61.235994
2088.971515	67.436729	61.240999
2088.207083	71.400241	61.246004
2087.782985	66.433439	61.251009
2087.456089	65.861393	61.256014
2086.828603	68.994675	61.261018
2086.292504	69.781115	61.266023
2085.194255	63.435610	61.271028
2084.493653	71.936948	61.276033
2083.845849	68.217434	61.281038
2082.909255	68.963434	61.286042
2081.916512	66.615755	61.291047
2081.946308	59.330501	61.296052
2080.837317	65.260623	61.301057
2080.085219	60.384266	61.306062
2079.152031	62.039116	61.311066
2078.999923	63.783779	61.316071
2078.548160	66.708592	61.321076
2078.195542	65.158096	61.326081
2077.992068	66.922202	61.331086
2076.833011	67.622178	61.336090
2076.123307	69.479583	61.341095
2074.757461	68.703550	61.346100
2074.449620	70.198941	61.351105
2074.346934	63.061867	61.356110
2073.711176	69.645620	61.361114
2072.647186	65.034575	61.366119
2071.795571	63.780604	61.371124
2070.912421	74.277684	61.376129
2070.891840	63.773426	61.381134
2069.837326	68.907163	61.386138
2068.930131	64.866905	61.391143
2069.014119	66.870382	61.396148
2068.178973	72.259481	61.401153
2067.144579	67.190631	61.406158
2066.131185	67.154410	61.411162
2065.760854	62.421958	61.416167
2065.293202	63.655355	61.421172
2064.645510	70.452720	61.426177
2064.546901	62.983780	61.431182
2063.498353	73.957945	61.436186
2062.328152	59.223554	61.441191
2061.614061	66.134112	61.446196
2061.035229	73.061798	61.451201
2060.770424	59.639714	61.456206
2059.931374	68.777730	61.461210
2059.793286	66.958446	61.466215
2059.546760	66.178848	61.471220
2058.295496	66.367255	61.476225
2057.498469	65.193156	61.481230
2056.636124	66.385518	61.486234
2056.190886	66.656310	61.491239
2055.716312	60.520307	61.496244
2054.561859	60.778204	61.501249
2053.957299	53.097404	61.506254
2052.870057	61.591453	61.511258
2053.010431	60.291356	61.516263
2052.295511	58.092340	61.521268
2051.691685	66.174509	61.526273
2050.911759	60.723470	61.531278
2049.811996	63.536897	61.536282
2049.619214	56.539970	61.541287
2048.930305	65.945975	61.546292
2048.141422	63.178188	61.551297
2048.004938	57.122904	61.556302
2047.017188	60.502539	61.561306
2045.793604	56.343913	61.566311
2045.203507	69.851909	61.571316
2044.397132	61.136333	61.576321
2044.181337	57.671734	61.581326
2043.897132	57.524211	61.586330
2043.699208	53.056339	61.591335
2042.444692	65.928408	61.596340
2041.615936	70.339092	61.601345
2040.906487	68.681879	61.606350
2040.183461	72.008736	61.611354
2039.592036	64.209244	61.616359
2038.613441	66.891032	61.621364
2038.022821	63.272267	61.626369
2037.325367	60.466740	61.631374
2036.863668	66.016950	61.636378
2036.445749	62.328383	61.641383
2036.146102	64.532869	61.646388
2035.462827	59.864212	61.651393
2034.733230	56.538419	61.656398
2033.372240	71.447298	61.661402
2033.182555	66.165682	61.666407
2032.399471	62.306694	61.671412
2031.809962	58.307231	61.676417
2030.721730	60.560951	61.681422
2029.688700	73.071078	61.686426
2029.192781	66.947411	61.691431
2028.829414	73.768378	61.696436
2028.300248	72.482547	61.701441
2028.149753	70.333427	61.706446
2027.790177	83.529646	61.711450
2026.906794	69.675367	61.716455
2025.896853	70.153672	61.721460
2024.751116	76.612305	61.726465
2024.730098	62.662625	61.731470
2024.116732	63.081384	61.736474
2022.891574	60.852813	61.741479
2022.409105	70.544020	61.746484
2021.731120	73.164128	61.751489
2021.486471	67.577324	61.756494
2020.485075	75.550276	61.761498
2019.624851	66.037503	61.766503
2018.605243	65.190024	61.771508
2018.133148	70.185856	61.776513
2017.786357	64.525345	61.781518
2017.137960	69.814217	61.786522
2016.992014	81.968937	61.791527
2016.417122	79.059159	61.796532
2015.241765	76.953116	61.801537
2014.249194	70.071285	61.806542
2013.790884	75.521451	61.811546
2013.472166	64.674267	61.816551
2012.845506	63.544451	61.821556
2011.410509	68.804067	61.826561
2011.035969	62.782400	61.831566
2010.581304	71.807303	61.836570
2009.905361	68.007355	61.841575
2009.363640	61.859161	61.846580
2009.034123	67.466496	61.851585
2008.206986	61.392781	61.856590
2007.023663	72.466185	61.861594
2006.580450	66.133778	61.866599
2006.225930	70.299141	61.871604
2005.233023	78.033023	61.876609
2004.172118	73.931836	61.881614
2003.369349	70.827368	61.886618
2002.958497	69.713135	61.891623
2002.764378	68.431966	61.896628
2002.168509	70.496870	61.901633
2002.007890	72.189703	61.906638
2001.217672	76.898129	61.911642
2000.329884	64.803484	61.916647
1999.694033	63.593535	61.921652
1998.631970	73.935310	61.926657
1997.760237	64.893044	61.931662
1996.704498	73.503686	61.936666
1996.245543	61.845271	61.941671
1995.810975	57.456170	61.946676
1995.158009	62.030592	61.951681
1994.893340	62.563777	61.956686
1994.439726	62.141697	61.961690
1993.909564	58.922316	61.966695
1993.033178	70.249912	61.971700
1991.860849	62.853732	61.976705
1991.896802	55.205871	61.981710
1991.276429	67.556595	61.986714
1989.969617	63.996009	61.991719
1989.272914	59.015857	61.996724
1988.737695	63.359754	62.001729
1988.502814	57.758654	62.006734
1987.543039	69.082357	62.011738
1986.633715	68.621395	62.016743
1986.080339	66.568035	62.021748
1985.286390	67.694632	62.026753
1984.878874	57.578668	62.031758
1983.924240	66.036623	62.036762
1983.578308	60.504649	62.041767
1983.029606	65.930408	62.046772
1982.383780	61.805593	62.051777
1982.099471	61.010752	62.056782
1981.041770	62.058920	62.061786
1979.588459	60.453177	62.066791
1978.964413	56.799089	62.071796
1978.288677	66.387965	62.076801
1977.989488	62.589494	62.081806
1977.483998	61.719995	62.086810
1977.146731	54.687006	62.091815
1977.089184	61.229479	62.096820
1976.018284	55.337597	62.101825
1975.377610	60.210299	62.106830
1974.271770	69.177257	62.111834
1973.780741	62.281879	62.116839
1972.500784	58.494479	62.121844
1971.749937	64.790436	62.126849
1971.098351	53.827323	62.131854
1970.657680	62.166964	62.136858
1970.101614	56.167673	62.141863
1970.032099	57.265868	62.146868
1969.784976	65.809628	62.151873
1969.268977	55.481711	62.156878
1967.845440	66.289115	62.161882
1967.088810	63.307020	62.166887
1966.160645	69.672390	62.171892
1965.277668	58.692017	62.176897
1964.731204	57.296660	62.181902
1964.111681	69.466064	62.186906
1963.840834	60.975857	62.191911
1963.422583	61.656495	62.196916
1962.587520	66.490614	62.201921
1962.102433	62.913014	62.206926
1961.421738	64.674683	62.211930
1960.815696	69.587646	62.216935
1959.604367	55.754371	62.221940
1958.530828	68.236693	62.226945
1958.141315	55.805789	62.231950
1957.484588	69.944887	62.236954
1957.160191	62.393009	62.241959
1957.212397	62.338725	62.246964
1956.007132	68.250994	62.251969
1954.966902	61.546670	62.256974
1954.586696	64.295046	62.261978
1954.303912	69.551771	62.266983
1953.338206	56.358159	62.271988
1951.694476	65.352004	62.276993
1951.653747	52.055424	62.281998
1950.936317	58.534734	62.287002
1950.730260	60.972279	62.292007
1950.622429	67.188634	62.297012
1949.367970	68.069555	62.302017
1948.289973	57.945537	62.307022
1948.162659	67.442966	62.312026
1947.329596	61.801706	62.317031
1946.221874	61.389295	62.322036
1945.678830	68.703211	62.327041
1945.454360	63.450843	62.332046
1944.764720	65.475742	62.337050
1944.306834	66.345917	62.342055
1943.557455	63.162068	62.347060
1942.373251	70.039772	62.352065
1941.805746	60.863378	62.357070
1941.255412	65.921146	62.362074
1940.650473	63.448739	62.367079
1939.763695	58.396512	62.372084
1938.836628	66.110447	62.377089
1938.129006	63.426670	62.382094
1937.702410	66.031016	62.387098
1937.290232	60.911019	62.392103
1937.232875	61.520842	62.397108
1936.094825	73.716983	62.402113
1935.437774	66.856720	62.407118
1934.557276	64.900379	62.412122
1934.089999	60.822787	62.417127
1933.914026	58.670533	62.422132
1932.502496	65.018730	62.427137
1931.923960	64.680391	62.432142
1931.123520	64.828020	62.437146
1930.740233	67.647973	62.442151
1930.914734	65.323268	62.447156
1929.316835	67.057513	62.452161
1928.685454	55.228888	62.457166
1928.254045	66.814293	62.462170
1927.526687	62.834480	62.467175
1926.786460	53.907105	62.472180
1925.393439	59.734265	62.477185
1925.378381	55.286432	62.482190
1924.775410	64.993118	62.487194
1923.842828	60.673037	62.492199
1923.766789	55.355021	62.497204
1923.032494	65.450471	62.502209
1922.208982	57.242704	62.507214
1921.664082	61.871668	62.512218
1920.918890	67.307756	62.517223
1920.350172	61.297216	62.522228
1918.847875	67.952246	62.527233
1918.609256	55.205814	62.532238
1917.945625	64.924456	62.537242
1917.618730	65.569732	62.542247
1917.494804	59.555730	62.547252
1916.240241	68.656290	62.552257
1915.432615	60.385413	62.557262
1914.675348	63.909183	62.562266
1914.412271	62.482323	62.567271
1913.797875	50.209899	62.572276
1912.553820	63.124792	62.577281
1912.069469	61.646976	62.582286
1911.642666	62.566701	62.587290
1910.845597	64.209737	62.592295
1910.707176	54.508391	62.597300
1908.945030	67.297983	62.602305
1908.508855	65.810345	62.607310
1908.061272	69.939923	62.612314
1907.732459	64.344637	62.617319
1907.410974	66.622727	62.622324
1906.670956	74.878591	62.627329
1905.479885	66.268726	62.632334
1904.407897	68.082737	62.637338
1903.897860	71.327778	62.642343
1903.819947	61.364641	62.647348
1903.328021	69.879625	62.652353
1902.328839	65.734355	62.657358
1901.366323	67.161762	62.662362
1900.867437	64.268999	62.667367
1900.412455	58.992918	62.672372
1899.991741	62.751599	62.677377
1899.303753	62.152923	62.682382
1898.202679	57.181970	62.687386
1897.659428	64.242116	62.692391
1897.343025	59.088768	62.697396
1896.260998	64.420647	62.702401
1895.092594	55.765073	62.707406
1894.532358	63.585589	62.712410
1894.288234	67.746277	62.717415
1893.703523	60.379069	62.722420
1893.114614	63.682205	62.727425
1892.927887	64.313372	62.732430
1892.353089	63.000234	62.737434
1890.784387	66.453230	62.742439
1890.540096	61.561874	62.747444
1889.920562	65.667976	62.752449
1888.870565	60.923143	62.757454
1888.536110	60.886852	62.762458
1887.852907	62.472519	62.767463
1887.544768	64.034282	62.772468
1886.705133	61.836891	62.777473
1885.885977	57.917396	62.782478
1885.254496	62.886027	62.787482
1884.769741	65.391778	62.792487
1884.253364	57.707764	62.797492
1883.003488	65.487983	62.802497
1882.548233	60.888892	62.807502
1881.865758	66.176891	62.812506
1881.367152	64.450870	62.817511
1880.604375	56.926243	62.822516
1879.450916	60.974879	62.827521
1879.437850	55.876213	62.832526
1878.556575	56.656202	62.837530
1877.948212	57.758562	62.842535
1876.924069	55.863516	62.847540
1876.266962	58.391253	62.852545
1875.452274	53.584460	62.857550
1875.642772	54.011755	62.862554
1875.060118	55.785868	62.867559
1873.895441	52.478883	62.872564
1872.968988	63.558478	62.877569
1872.732579	63.830267	62.882574
1872.059442	60.189725	62.887578
1871.612885	59.565143	62.892583
1870.734747	58.291273	62.897588
1869.280103	63.600461	62.902593
1869.061804	56.677390	62.907598
1868.731867	60.826706	62.912602
1868.034855	65.479724	62.917607
1867.881500	60.883061	62.922612
1866.707410	66.701989	62.927617
1866.150975	65.402686	62.932622
1865.601125	53.141333	62.937626
1864.413055	55.265723	62.942631
1863.667400	49.851888	62.947636
1862.886079	56.423445	62.952641
1862.667102	58.470457	62.957646
1862.134186	62.412143	62.962650
1861.833903	63.545872	62.967655
1860.951313	61.915941	62.972660
1860.173247	69.768202	62.977665
1859.740666	67.458940	62.982670
1859.637479	65.688560	62.987674
1857.913329	67.623628	62.992679
1857.737767	54.197373	62.997684
1856.729384	72.507224	63.002689
1855.646920	59.580316	63.007694
1854.930617	63.383649	63.012698
1854.286665	68.432571	63.017703
1854.202955	63.202313	63.022708
1853.192749	79.643494	63.027713
1853.221861	69.030104	63.032718
1852.701769	65.880462	63.037722
1851.341367	73.007393	63.042727
1850.855787	67.487484	63.047732
1850.308541	70.203261	63.052737
1849.824272	69.440271	63.057742
1848.654838	63.204506	63.062746
1848.013287	69.309678	63.067751
1847.796954	58.862229	63.072756
1847.108768	72.100830	63.077761
1845.997242	75.535226	63.082766
1845.119427	68.945239	63.087770
1844.624811	69.777497	63.092775
1844.448122	61.165414	63.097780
1843.869656	77.644039	63.102785
1843.084808	63.037212	63.107790
1842.045005	65.909493	63.112794
1841.517276	64.008863	63.117799
1841.348894	59.983957	63.122804
1840.182024	75.242917	63.127809
1839.385340	61.688462	63.132814
1838.737768	57.861193	63.137818
1838.156433	64.127369	63.142823
1838.033526	61.611189	63.147828
1837.066075	70.374101	63.152833
1836.089119	61.936433	63.157838
1835.360545	57.375033	63.162842
1834.597248	67.927006	63.167847
1835.099702	58.859275	63.172852
1834.001278	75.696054	63.177857
1832.914145	63.875949	63.182862
1832.292395	67.678897	63.187866
1831.937939	63.477020	63.192871
1831.089922	64.433292	63.197876
1829.817599	73.606770	63.202881
1829.455450	62.793103	63.207886
1829.239033	68.140704	63.212890
1828.546446	70.016523	63.217895
1828.406662	59.695710	63.222900
1827.027121	68.296637	63.227905
1826.968878	58.934459	63.232910
1825.522515	60.270194	63.237914
1824.230421	68.354079	63.242919
1823.776679	72.860091	63.247924
1823.827056	70.890157	63.252929
1823.394739	73.436676	63.257934
1822.667648	67.694420	63.262938
1822.080086	69.796206	63.267943
1821.331509	59.621788	63.272948
1820.230586	73.610709	63.277953
1819.752955	66.239006	63.282958
1819.636010	72.963734	63.287962
1818.484904	71.107789	63.292967
1817.805623	65.611948	63.297972
1816.980862	72.680003	63.302977
1816.581423	64.426939	63.307982
1815.597445	65.685145	63.312986
1814.700039	66.933671	63.317991
1814.472232	58.947283	63.322996
1813.913597	66.941205	63.328001
1813.304797	64.251592	63.333006
1813.058959	60.410064	63.338010
1811.535631	52.762170	63.343015
1811.375185	60.251798	63.348020
1810.922252	60.455641	63.353025
1810.548738	59.918431	63.358030
1809.692369	58.510590	63.363034
1808.649242	56.540259	63.368039
1807.734253	53.115969	63.373044
1806.776941	58.681114	63.378049
1806.140249	53.852960	63.383054
1805.867061	62.218809	63.388058
1805.087657	61.921958	63.393063
1805.250920	53.955502	63.398068
1803.963264	64.265231	63.403073
1803.345375	60.490912	63.408078
1802.686386	67.016286	63.413082
1802.182881	65.233878	63.418087
1801.282033	59.857262	63.423092
1800.163586	73.129218	63.428097
1800.045923	57.784207	63.433102
1799.548057	58.200597	63.438106
1798.864508	64.583732	63.443111
1798.073540	58.678737	63.448116
1797.410016	64.096519	63.453121
1796.804072	62.910690	63.458126
1796.245109	56.417738	63.463130
1795.093476	58.644455	63.468135
1794.513947	53.750867	63.473140
1793.813193	59.003316	63.478145
1793.424089	67.478996	63.483150
1792.719357	66.462430	63.488154
1791.278638	61.512513	63.493159
1791.173968	56.401500	63.498164
1790.336944	60.893355	63.503169
1789.783282	59.144398	63.508174
1789.520201	63.324512	63.513178
1789.113341	68.465499	63.518183
1788.795903	53.681624	63.523188
1787.498239	64.768293	63.528193
1786.617386	64.580771	63.533198
1786.367824	57.926335	63.538202
1785.492848	64.694312	63.543207
1784.990470	61.013910	63.548212
1783.972791	65.875740	63.553217
1783.626765	66.208129	63.558222
1783.051041	69.702036	63.563226
1781.918961	70.078922	63.568231
1781.021589	67.996424	63.573236
1780.790352	69.365832	63.578241
1780.132409	65.232070	63.583246
1780.075619	55.669529	63.588250
1778.932128	60.737612	63.593255
1778.183030	53.820508	63.598260
1777.322840	66.277389	63.603265
1777.075594	63.190804	63.608270
1776.091181	59.522226	63.613274
1775.246368	65.594683	63.618279
1774.738649	64.181665	63.623284
1774.212102	61.432198	63.628289
1773.755401	61.473275	63.633294
1772.967481	61.542605	63.638298
1772.052184	62.829723	63.643303
1771.646981	57.168188	63.648308
1771.122008	70.640559	63.653313
1770.353060	59.444557	63.658318
1769.529334	57.081054	63.663322
1768.770741	72.069641	63.668327
1768.359789	63.756979	63.673332
1768.012666	59.041118	63.678337
1767.298159	64.836292	63.683342
1766.418585	62.213147	63.688346
1765.709595	64.197168	63.693351
1764.970511	51.083263	63.698356
1764.221269	61.229033	63.703361
1763.264317	62.438415	63.708366
1762.859743	56.499288	63.713370
1762.677048	61.425873	63.718375
1762.073725	53.761892	63.723380
1761.166362	59.182319	63.728385
1760.387799	60.361179	63.733390
1760.113483	59.810158	63.738394
1758.921413	61.642373	63.743399
1757.971090	59.282376	63.748404
1757.434585	66.410844	63.753409
1757.087468	63.975660	63.758414
1757.005084	57.088949	63.763418
1755.378675	63.530392	63.768423
1755.038043	58.170427	63.773428
1754.541271	62.538151	63.778433
1754.015356	62.912768	63.783438
1753.058550	54.886923	63.788442
1751.921659	59.971248	63.793447
1751.749173	56.322429	63.798452
1751.173569	68.336295	63.803457
1750.868933	57.810817	63.808462
1750.118246	60.152483	63.813466
1749.120310	67.353194	63.818471
1748.764017	60.697683	63.823476
1747.855896	64.159655	63.828481
1746.853478	64.157537	63.833486
1746.208982	63.729064	63.838490
1745.679360	67.134957	63.843495
1745.453382	70.038918	63.848500
1744.942063	59.689325	63.853505
1743.788718	68.267351	63.858510
1743.155625	64.611689	63.863514
1742.324615	68.448871	63.868519
1742.132104	65.858162	63.873524
1741.038426	73.156965	63.878529
1740.340933	70.411883	63.883534
1739.815627	76.799528	63.888538
1738.874801	79.134260	63.893543
1738.944457	62.777910	63.898548
1737.954670	66.899615	63.903553
1737.121520	63.953548	63.908558
1736.898629	60.867142	63.913562
1736.319254	62.152047	63.918567
1735.021865	57.556948	63.923572
1734.564958	55.660002	63.928577
1734.038681	63.444318	63.933582
1733.723546	62.479513	63.938586
1732.456439	62.354539	63.943591
1732.039776	60.301109	63.948596
1731.610838	67.028296	63.953601
1731.095845	61.619224	63.958606
1730.090430	62.345481	63.963610
1728.806118	59.496350	63.968615
1728.245297	61.640144	63.973620
1727.759028	68.632129	63.978625
1727.520892	59.687961	63.983630
1726.926371	64.411080	63.988634
1725.422756	58.672249	63.993639
1725.329149	60.164943	63.998644
1724.796682	65.270583	64.003649
1724.247525	58.933852	64.008654
1723.571510	60.334764	64.013658
1722.429724	63.397401	64.018663
1722.133655	56.417395	64.023668
1721.316316	57.769861	64.028673
1721.010309	60.891188	64.033678
1720.124162	54.333057	64.038682
1718.930328	59.840006	64.043687
1718.783173	57.916900	64.048692
1718.414023	62.647638	64.053697
1717.789159	56.697660	64.058702
1716.786753	50.799656	64.063706
1716.210576	63.866722	64.068711
1715.928344	59.323307	64.073716
1714.505123	55.354058	64.078721
1713.395281	58.767265	64.083726
1713.563014	54.472894	64.088730
1713.096279	60.874983	64.093735
1712.604219	48.882058	64.098740
1711.356389	56.644581	64.103745
1710.751464	56.930490	64.108750
1710.644017	54.363912	64.113754
1709.691424	56.228972	64.118759
1709.082051	54.229834	64.123764
1708.650126	58.710404	64.128769
1707.732019	58.857675	64.133774
1706.790729	54.505190	64.138778
1705.728551	55.239586	64.143783
1705.423416	57.765136	64.148788
1705.166357	58.689775	64.153793
1704.485333	59.320663	64.158798
1703.402810	56.953695	64.163802
1702.502520	65.707098	64.168807
1702.600639	60.514814	64.173812
1701.787253	61.212559	64.178817
1700.119590	64.564124	64.183822
1699.972163	58.037083	64.188826
1699.162823	68.266166	64.193831
1699.258980	56.973861	64.198836
1698.756068	59.948102	64.203841
1697.912159	58.054621	64.208846
1697.154985	60.696994	64.213850
1696.239719	63.159587	64.218855
1695.831833	56.540544	64.223860
1694.752315	68.043034	64.228865
1694.080156	63.121891	64.233870
1693.637538	56.039077	64.238874
1692.712479	66.674783	64.243879
1692.494191	51.818311	64.248884
1691.591647	58.624957	64.253889
1690.824667	58.223370	64.258894
1690.320532	52.605618	64.263898
1690.255051	66.538538	64.268903
1688.808205	54.202571	64.273908
1687.606273	58.300192	64.278913
1687.146188	61.057510	64.283918
1687.010891	54.107628	64.288922
1686.078874	65.217395	64.293927
1685.949569	64.025016	64.298932
1685.539558	60.419608	64.303937
1684.730580	58.382790	64.308942
1684.127249	57.637033	64.313946
1683.449392	59.596000	64.318951
1682.323647	55.624803	64.323956
1681.428077	60.809155	64.328961
1680.750660	60.141993	64.333966
1680.579684	50.498748	64.338970
1679.943337	56.463305	64.343975
1679.538555	56.484059	64.348980
1678.241408	61.508982	64.353985
1677.696703	56.301574	64.358990
1677.506138	49.736923	64.363994
1676.453862	57.415070	64.368999
1675.773095	50.403802	64.374004
1675.065536	55.287968	64.379009
1674.698371	50.009131	64.384014
1674.230338	51.070131	64.389018
1673.193039	58.659274	64.394023
1672.754137	48.684134	64.399028
1672.199664	49.029305	64.404033
1670.751774	47.967831	64.409038
1670.351914	47.738283	64.414042
1669.611156	47.407604	64.419047
1669.474857	42.601607	64.424052
1669.043839	53.629583	64.429057
1668.134003	52.189868	64.434062
1667.475198	48.026675	64.439066
1666.696312	49.453879	64.444071
1665.722067	43.963551	64.449076
1664.877729	55.005022	64.454081
1664.602060	51.967521	64.459086
1664.344866	49.233159	64.464090
1663.623147	55.888081	64.469095
1662.854489	52.445492	64.474100
1662.019748	47.595994	64.479105
1661.368084	51.511828	64.484110
1660.712951	50.690075	64.489114
1659.349928	53.510332	64.494119
1658.930036	47.393853	64.499124
1658.374923	55.543477	64.504129
1658.266611	50.467440	64.509134
1657.865935	51.514941	64.514138
1656.600214	51.723679	64.519143
1655.834339	54.187554	64.524148
1655.539260	51.032987	64.529153
1655.274799	57.194420	64.534158
1654.418874	46.687914	64.539162
1653.326204	53.698404	64.544167
1653.065512	51.291467	64.549172
1651.682505	50.923070	64.554177
1650.821370	55.349990	64.559182
1650.586962	54.316118	64.564186
1649.839641	52.927934	64.569191
1649.630227	56.710856	64.574196
1649.043691	54.675847	64.579201
1647.470648	52.957673	64.584206
1646.877629	48.624944	64.589210
1646.201790	56.442350	64.594215
1646.256521	57.014047	64.599220
1645.867676	66.736986	64.604225
1645.094730	50.760105	64.609230
1644.605917	47.149639	64.614234
1643.604550	65.803262	64.619239
1642.968756	56.936631	64.624244
1641.853988	60.332931	64.629249
1640.955286	61.455002	64.634254
1640.997227	47.748426	64.639258
1640.044589	55.070070	64.644263
1640.104113	53.494871	64.649268
1639.105709	49.317562	64.654273
1638.285001	51.988575	64.659278
1637.839660	51.134082	64.664282
1636.496295	56.228496	64.669287
1635.872941	47.211330	64.674292
1635.457677	48.191069	64.679297
1635.109769	54.120083	64.684302
1634.683656	51.589095	64.689306
1633.495100	54.017941	64.694311
1632.872668	47.529174	64.699316
1632.339113	55.295391	64.704321
1631.683590	55.465631	64.709326
1630.880958	51.715457	64.714330
1629.697790	51.095774	64.719335
1629.565488	55.835714	64.724340
1629.219829	51.361188	64.729345
1628.327632	47.276624	64.734350
1627.349199	46.388628	64.739354
1626.773661	46.337955	64.744359
1626.470438	44.231969	64.749364
1626.078043	49.039310	64.754369
1624.798119	55.468064	64.759374
1624.424820	51.740731	64.764378
1623.366388	52.444504	64.769383
1623.173233	51.707110	64.774388
1622.785330	50.445704	64.779393
1621.793696	54.894960	64.784398
1621.335369	50.445242	64.789402
1620.870124	51.399590	64.794407
1619.692995	44.551038	64.799412
1619.016068	48.123847	64.804417
1618.560499	53.892083	64.809422
1617.535538	50.439288	64.814426
1616.199996	56.401139	64.819431
1615.682509	49.850206	64.824436
1615.962904	48.043009	64.829441
1614.809292	50.904015	64.834446
1614.729666	41.815517	64.839450
1614.192983	52.750658	64.844455
1613.359490	50.301229	64.849460
1612.492594	46.000376	64.854465
1612.043144	58.560245	64.859470
1611.005289	50.320559	64.864474
1610.007985	56.648849	64.869479
1609.567535	54.694629	64.874484
1609.209407	50.271580	64.879489
1608.829052	50.352103	64.884494
1607.843153	42.400359	64.889498
1606.907952	45.727645	64.894503
1606.722890	45.246618	64.899508
1606.183610	50.479734	64.904513
1605.069498	49.356422	64.909518
1604.315238	49.741711	64.914522
1603.756671	58.056130	64.919527
1603.535815	43.351300	64.924532
1602.234941	40.461228	64.929537
1601.220525	53.931287	64.934542
1601.156279	37.304233	64.939546
1600.522403	43.691107	64.944551
1600.334389	38.949228	64.949556
1599.759100	44.494015	64.954561
1598.603242	56.032462	64.959566
1598.336739	45.746797	64.964570
1597.092291	52.713008	64.969575
1595.862097	46.960593	64.974580
1595.757306	49.501593	64.979585
1595.066055	44.412040	64.984590
1594.939849	42.934939	64.989594
1594.352023	49.490374	64.994599
1593.203701	48.292398	64.999604
1592.655654	33.869745	65.004609
1592.047294	44.753202	65.009614
1591.825723	36.594087	65.014618
1590.426855	43.540540	65.019623
1589.576059	40.477927	65.024628
1589.460822	40.397429	65.029633
1588.715162	42.838115	65.034638
1587.949993	42.609910	65.039642
1586.969303	49.986091	65.044647
1586.645529	46.039115	65.049652
1586.416527	37.464056	65.054657
1585.549884	42.123227	65.059662
1584.647049	41.429134	65.064666
1583.816968	43.727171	65.069671
1583.340876	50.746617	65.074676
1583.024064	46.415970	65.079681
1581.937778	51.535079	65.084686
1581.744376	40.561155	65.089690
1580.843120	49.711808	65.094695
1580.146184	37.731090	65.099700
1579.438853	37.151559	65.104705
1578.879485	45.828458	65.109710
1578.222398	45.680832	65.114714
1577.504712	43.075020	65.119719
1576.626273	43.028430	65.124724
1576.333738	41.858070	65.129729
1575.778008	48.703260	65.134734
1574.689290	39.282226	65.139738
1573.869547	50.561844	65.144743
1573.397621	42.082039	65.149748
1573.132080	36.400981	65.154753
1571.953779	44.570414	65.159758
1571.425172	44.304490	65.164762
1570.701126	42.512883	65.169767
1570.095169	41.969686	65.174772
1569.630622	41.220323	65.179777
1568.775413	40.763201	65.184782
1568.073571	40.031950	65.189786
1567.291557	50.472655	65.194791
1566.965238	44.473592	65.199796
1566.632401	40.574352	65.204801
1565.521172	54.750157	65.209806
1564.984486	43.789986	65.214810
1564.043573	50.667941	65.219815
1563.650256	48.093456	65.224820
1562.760638	48.287190	65.229825
1561.797068	45.680437	65.234830
1561.570438	41.014245	65.239834
1561.183393	55.168739	65.244839
1560.254560	39.424224	65.249844
1559.510359	39.071257	65.254849
1558.882065	35.245083	65.259854
1558.680513	38.230908	65.264858
1557.910838	49.494853	65.269863
1556.595177	52.264003	65.274868
1556.328755	42.676587	65.279873
1555.522074	43.878049	65.284878
1555.233572	42.368728	65.289882
1554.457376	45.689336	65.294887
1553.369525	43.326869	65.299892
1552.986478	34.411884	65.304897
1552.699925	50.097251	65.309902
1551.871694	49.128304	65.314906
1550.927815	47.391296	65.319911
1549.910454	47.386643	65.324916
1549.873503	41.442264	65.329921
1549.037877	41.425060	65.334926
1548.098103	39.130012	65.339930
1547.547416	38.869053	65.344935
1547.240764	38.293186	65.349940
1546.733844	42.216622	65.354945
1545.488665	44.905031	65.359950
1545.049034	39.290872	65.364954
1544.235905	33.015939	65.369959
1543.774145	34.791495	65.374964
1543.242343	43.318420	65.379969
1542.372774	47.365499	65.384974
1541.743347	34.551835	65.389978
1541.004698	39.396725	65.394983
1540.691652	32.131912	65.399988
1539.470359	36.273919	65.404993
1538.607113	42.530718	65.409998
1538.143246	38.054334	65.415002
1538.146525	41.289694	65.420007
1537.792778	44.543134	65.425012
1536.633474	35.273529	65.430017
1535.559602	40.654188	65.435022
1535.532646	36.569583	65.440026
1534.771263	34.410182	65.445031
1533.849943	44.748417	65.450036
1533.429514	35.781020	65.455041
1532.556842	46.011461	65.460046
1531.456947	34.345632	65.465050
1530.773282	48.265109	65.470055
1530.208924	41.366577	65.475060
1530.002075	39.214502	65.480065
1529.509536	39.668686	65.485070
1529.284745	34.131046	65.490074
1527.653272	34.030196	65.495079
1527.156954	39.613966	65.500084
1526.823196	38.150681	65.505089
1525.928419	47.120238	65.510094
1525.273882	30.914347	65.515098
1524.568106	39.985360	65.520103
1524.240110	42.847572	65.525108
1523.194718	41.358853	65.530113
1522.096335	45.332205	65.535118
1521.979338	40.733301	65.540122
1521.283499	41.655284	65.545127
1521.135041	39.576896	65.550132
1519.961724	32.812591	65.555137
1518.985781	43.580152	65.560142
1518.609743	41.474796	65.565146
1518.249358	45.298948	65.570151
1517.550154	46.829766	65.575156
1516.888887	42.397430	65.580161
1515.617108	48.929407	65.585166
1515.758834	46.592153	65.590170
1514.447253	47.954636	65.595175
1514.117467	47.998487	65.600180
1513.866150	47.320393	65.605185
1512.250277	44.252955	65.610190
1511.770653	43.093700	65.615194
1511.304330	45.626316	65.620199
1510.608045	46.883886	65.625204
1510.570148	43.070744	65.630209
1509.328122	47.924823	65.635214
1508.710010	47.543968	65.640218
1508.169571	46.476433	65.645223
1507.421111	48.875769	65.650228
1507.281657	45.132900	65.655233
1505.594503	51.124162	65.660238
1505.351327	38.088090	65.665242
1504.868978	48.295149	65.670247
1504.203371	42.293378	65.675252
1503.456467	41.754971	65.680257
1502.221862	46.474367	65.685262
1502.405087	47.894418	65.690266
1501.734743	47.836302	65.695271
1500.603903	46.535887	65.700276
1499.847212	43.289825	65.705281
1499.584556	45.484837	65.710286
1498.773326	37.651643	65.715290
1497.950452	39.572688	65.720295
1497.525089	43.124161	65.725300
1497.047652	38.831279	65.730305
1496.196963	48.516806	65.735310
1495.504544	40.943920	65.740314
1495.452656	41.381501	65.745319
1494.287089	42.418619	65.750324
1493.660870	38.210804	65.755329
1492.873657	42.031829	65.760334
1492.293727	38.974583	65.765338
1491.178660	36.577319	65.770343
1490.655840	38.089792	65.775348
1490.378783	32.486501	65.780353
1489.742277	45.416640	65.785358
1489.233204	39.395976	65.790362
1488.205944	40.982550	65.795367
1487.739003	41.926147	65.800372
1487.285951	45.183165	65.805377
1486.009693	43.676339	65.810382
1485.742847	38.879282	65.815386
1485.193907	44.313386	65.820391
1484.226257	42.436784	65.825396
1483.441654	40.916069	65.830401
1482.704998	40.283547	65.835406
1482.669811	33.541944	65.840410
1481.798953	43.365914	65.845415
1480.872245	43.187872	65.850420
1480.330730	34.816310	65.855425
1479.477860	48.408714	65.860430
1479.374106	40.782048	65.865434
1478.634441	43.123437	65.870439
1477.567447	40.256130	65.875444
1477.185465	31.544256	65.880449
1476.260268	43.930548	65.885454
1475.597948	46.116601	65.890458
1474.590368	46.189232	65.895463
1474.056009	49.071767	65.900468
1473.989294	43.474312	65.905473
1473.427066	40.264836	65.910478
1472.619042	42.169528	65.915482
1471.495299	46.177229	65.920487
1470.663821	43.365529	65.925492
1470.652970	35.752569	65.930497
1470.115863	44.264615	65.935502
1468.956964	45.191656	65.940506
1467.862719	41.341831	65.945511
1467.598059	45.676152	65.950516
1467.670839	40.682420	65.955521
1466.564644	44.722642	65.960526
1465.888903	34.682700	65.965530
1465.288690	34.144453	65.970535
1464.702841	47.923246	65.975540
1464.068129	39.183972	65.980545
1462.596796	51.164826	65.985550
1462.328172	38.728350	65.990554
1462.101379	44.728204	65.995559
1461.538566	50.352176	66.000564
1460.602238	39.622662	66.005569
1459.749887	51.119434	66.010574
1459.311352	41.103227	66.015578
1458.744974	46.426640	66.020583
1457.516433	44.917180	66.025588
1456.991519	42.100378	66.030593
1456.217819	45.256367	66.035598
1456.177121	41.720009	66.040602
1455.702684	37.397805	66.045607
1454.378728	43.758731	66.050612
1453.983252	35.598613	66.055617
1453.407499	44.923678	66.060622
1453.059257	42.986456	66.065626
1451.967567	42.739558	66.070631
1450.921850	48.940369	66.075636
1450.643824	36.524057	66.080641
1449.876514	45.017483	66.085646
1449.045264	46.279215	66.090650
1448.595128	44.861906	66.095655
1448.156732	43.696786	66.100660
1447.851786	44.455167	66.105665
1446.471642	58.254665	66.110670
1446.005134	43.889924	66.115674
1445.594129	49.140562	66.120679
1444.746734	53.074128	66.125684
1444.150894	44.004141	66.130689
1443.239067	42.105362	66.135694
1442.723115	36.401657	66.140698
1441.998272	42.841607	66.145703
1441.254075	50.831765	66.150708
1440.605540	42.712986	66.155713
1439.942173	51.916875	66.160718
1439.848141	38.372155	66.165722
1438.805666	46.127986	66.170727
1438.053001	46.437634	66.175732
1437.707202	43.661619	66.180737
1436.894839	43.284024	66.185742
1435.798439	35.830429	66.190746
1435.247236	40.333393	66.195751
1434.703071	41.582697	66.200756
1434.410180	37.476909	66.205761
1433.349572	43.286737	66.210766
1432.575613	38.856339	66.215770
1432.074800	40.535172	66.220775
1431.668296	36.679345	66.225780
1430.912535	38.021311	66.230785
1429.351295	46.218814	66.235790
1429.095054	45.450783	66.240794
1428.465839	44.838956	66.245799
1428.018605	48.201950	66.250804
1428.143122	42.649525	66.255809
1427.479910	47.663479	66.260814
1426.452130	41.635299	66.265818
1425.855936	40.198786	66.270823
1424.699103	41.405730	66.275828
1424.335600	34.497314	66.280833
1423.835491	50.681037	66.285838
1423.183523	38.198874	66.290842
1422.207293	41.535973	66.295847
1421.435733	39.100454	66.300852
1421.168742	39.501043	66.305857
1420.176239	38.366432	66.310862
1419.374557	46.481685	66.315866
1418.820941	41.432947	66.320871
1418.088304	42.035602	66.325876
1418.016216	36.804185	66.330881
1417.186784	39.962613	66.335886
1415.968897	40.774242	66.340890
1415.607391	48.175107	66.345895
1414.795522	41.082923	66.350900
1414.154085	39.502585	66.355905
1413.317782	50.361908	66.360910
1412.377171	37.729824	66.365914
1412.087359	36.420860	66.370919
1411.503576	40.967690	66.375924
1411.432051	45.431969	66.380929
1410.454280	37.837292	66.385934
1409.629287	41.568878	66.390938
1409.286886	35.014463	66.395943
1408.293265	39.618419	66.400948
1407.776219	42.649566	66.405953
1406.707566	47.925148	66.410958
1406.223913	46.495030	66.415962
1405.954998	31.813871	66.420967
1405.486818	36.969694	66.425972
1404.534012	38.289342	66.430977
1403.478579	42.561662	66.435982
1403.357818	34.610305	66.440986
1402.387895	48.116172	66.445991
1401.154736	40.905062	66.450996
1401.202946	36.068690	66.456001
1400.386826	45.819748	66.461006
1400.329763	39.488845	66.466010
1399.280659	40.005153	66.471015
1398.581203	44.871374	66.476020
1398.092524	38.049120	66.481025
1397.231030	44.846000	66.486030
1396.360755	39.517145	66.491034
1395.651025	38.152173	66.496039
1395.348481	33.877920	66.501044
1394.536211	38.882654	66.506049
1393.773144	39.939707	66.511054
1393.068886	36.578512	66.516058
1392.884158	41.598190	66.521063
1392.003402	42.763805	66.526068
1391.227006	38.434090	66.531073
1390.509716	46.140579	66.536078
1389.923358	39.641740	66.541082
1388.682222	42.071346	66.546087
1387.727148	45.271811	66.551092
1387.405598	39.306691	66.556097
1386.973548	39.216485	66.561102
1386.854543	41.823070	66.566106
1386.530858	38.532908	66.571111
1385.976502	44.740008	66.576116
1385.040551	45.711793	66.581121
1383.794387	43.496066	66.586126
1382.933035	46.238407	66.591130
1382.444697	43.551530	66.596135
1381.640508	49.199061	66.601140
1381.447250	38.587100	66.606145
1380.995523	46.600612	66.611150
1379.839448	35.907557	66.616154
1379.158149	39.618101	66.621159
1378.511195	46.671138	66.626164
1378.294170	38.189185	66.631169
1377.131215	41.811266	66.636174
1376.525931	49.406221	66.641178
1376.110083	43.238965	66.646183
1375.438587	43.949969	66.651188
1374.793698	37.994413	66.656193
1373.669568	49.952161	66.661198
1373.569175	37.973983	66.666202
1373.089139	45.283827	66.671207
1371.893862	40.784647	66.676212
1371.423993	45.574862	66.681217
1370.534601	44.531157	66.686222
1369.881662	47.338477	66.691226
1369.598972	40.977123	66.696231
1368.389292	39.340913	66.701236
1367.909372	38.288298	66.706241
1367.499715	41.443951	66.711246
1366.915494	43.653355	66.716250
1366.048046	37.804973	66.721255
1365.165815	40.197620	66.726260
1364.922306	34.201779	66.731265
1364.251864	40.138633	66.736270
1363.458111	34.122121	66.741274
1362.533393	37.728290	66.746279
1361.686571	33.498659	66.751284
1361.630259	33.453867	66.756289
1360.998823	38.015962	66.761294
1360.519597	43.987976	66.766298
1359.697587	41.534263	66.771303
1358.877982	40.030614	66.776308
1358.555703	36.859418	66.781313
1357.380103	41.324017	66.786318
1356.706322	41.176908	66.791322
1356.378643	38.708441	66.796327
1355.274549	37.141787	66.801332
1354.528157	34.110689	66.806337
1353.546756	44.398435	66.811342
1353.102387	43.380785	66.816346
1353.276974	42.285997	66.821351
1352.423084	39.094494	66.826356
1351.997380	33.300360	66.831361
1351.126678	44.000185	66.836366
1350.447986	39.982945	66.841370
1349.362276	44.577808	66.846375
1348.644359	43.184246	66.851380
1348.187037	41.208867	66.856385
1347.725363	39.228707	66.861390
1347.343485	42.534335	66.866394
1346.011774	36.099547	66.871399
1345.355735	42.452336	66.876404
1345.183581	42.498029	66.881409
1344.320776	41.283209	66.886414
1343.380765	44.550571	66.891418
1342.727471	39.436019	66.896423
1341.909977	49.335730	66.901428
1341.855115	42.274625	66.906433
1341.359352	42.397818	66.911438
1340.417734	44.825502	66.916442
1339.534851	38.418483	66.921447
1338.857212	43.171638	66.926452
1338.804853	39.400847	66.931457
1337.495640	50.074696	66.936462
1336.790834	38.384717	66.941466
1336.646761	39.027148	66.946471
1335.823316	47.525454	66.951476
1334.993621	39.264432	66.956481
1334.251295	51.204191	66.961486
1333.961230	39.928714	66.966490
1333.679247	41.596146	66.971495
1332.388637	37.014225	66.976500
1331.934920	30.767021	66.981505
1331.343625	39.040461	66.986510
1330.397726	39.183084	66.991514
1329.640794	30.954608	66.996519
1328.944791	41.459930	67.001524
1328.497010	31.622961	67.006529
1327.569446	30.399100	67.011534
1326.985623	31.318115	67.016538
1326.490965	35.704042	67.021543
1325.782552	38.960179	67.026548
1325.734543	36.248850	67.031553
1324.533676	32.411002	67.036558
1323.421486	38.500844	67.041562
1323.502381	34.644879	67.046567
1322.353396	37.915650	67.051572
1321.435140	33.339461	67.056577
1320.956230	39.959149	67.061582
1320.418896	36.210201	67.066586
1320.143962	39.540545	67.071591
1318.858932	44.516489	67.076596
1318.048670	35.575999	67.081601
1317.504491	40.765361	67.086606
1317.044917	38.297767	67.091610
1316.949477	30.937317	67.096615
1316.421132	39.094593	67.101620
1315.374902	30.851702	67.106625
1314.797633	40.003745	67.111630
1314.003330	30.404906	67.116634
1313.135022	30.595824	67.121639
1312.253415	32.760226	67.126644
1312.074156	33.561041	67.131649
1311.558007	38.065510	67.136654
1310.640309	38.039897	67.141658
1309.940741	39.736187	67.146663
1309.126137	47.091465	67.151668
1308.993281	33.187517	67.156673
1307.891657	39.987224	67.161678
1306.771432	45.373881	67.166682
1306.479119	35.965799	67.171687
1306.071199	44.908470	67.176692
1305.712245	36.142552	67.181697
1304.969115	39.103072	67.186702
1304.114201	42.558756	67.191706
1303.647651	37.278829	67.196711
1302.375880	42.458547	67.201716
1301.456197	39.477254	67.206721
1301.022370	44.645358	67.211726
1300.728333	36.818012	67.216730
1300.482813	39.234687	67.221735
1299.361340	41.271612	67.226740
1298.615242	37.586035	67.231745
1297.809611	45.422119	67.236750
1297.644066	49.201082	67.241754
1297.460749	40.967959	67.246759
1296.068728	39.909268	67.251764
1295.524153	36.143801	67.256769
1294.810354	43.561555	67.261774
1293.442562	34.062080	67.266778
1293.029710	30.811272	67.271783
1292.313160	42.734770	67.276788
1292.209053	35.333175	67.281793
1291.703865	41.015968	67.286798
1291.283559	33.940068	67.291802
1290.202066	34.941523	67.296807
1289.678753	44.764426	67.301812
1289.496534	28.363680	67.306817
1288.000185	41.146160	67.311822
1286.987692	40.283800	67.316826
1286.853215	39.964248	67.321831
1286.549794	42.207295	67.326836
1285.459555	33.737090	67.331841
1284.646972	35.866786	67.336846
1284.126187	37.298011	67.341850
1283.903846	31.739058	67.346855
1282.139898	33.410737	67.351860
1281.638018	27.527820	67.356865
1281.293733	33.537124	67.361870
1280.945024	31.770121	67.366874
1281.158221	41.816257	67.371879
1279.620283	36.468713	67.376884
1278.974491	29.109332	67.381889
1278.329120	37.768194	67.386894
1277.431915	36.232452	67.391898
1276.717551	36.972911	67.396903
1275.932989	39.582126	67.401908
1275.556680	37.094362	67.406913
1275.302475	35.668003	67.411918
1274.592170	37.833872	67.416922
1273.575354	29.881205	67.421927
1272.969647	28.588439	67.426932
1272.788859	29.433725	67.431937
1271.429913	27.461537	67.436942
1270.609025	34.146084	67.441946
1270.399134	36.859012	67.446951
1270.015283	42.999822	67.451956
1269.009829	37.983071	67.456961
1267.892716	37.654518	67.461966
1267.717403	42.841126	67.466970
1267.358439	39.115724	67.471975
1266.480804	38.096868	67.476980
1265.949258	32.343761	67.481985
1264.715447	31.573372	67.486990
1264.294239	35.855943	67.491994
1264.093689	33.757278	67.496999
1262.849906	37.094813	67.502004
1262.506738	34.707950	67.507009
1261.894564	30.803281	67.512014
1260.941082	40.900342	67.517018
1260.655742	29.407773	67.522023
1259.816618	39.504990	67.527028
1259.100827	33.507126	67.532033
1258.294758	39.460102	67.537038
1256.979378	42.028362	67.542042
1256.815469	41.614776	67.547047
1256.157863	40.698376	67.552052
1256.046804	42.335365	67.557057
1255.854766	33.547196	67.562062
1254.555924	41.326806	67.567066
1254.429069	38.102034	67.572071
1253.096935	43.818251	67.577076
1251.959483	43.973552	67.582081
1251.437247	44.851244	67.587086
1250.623812	43.116833	67.592090
1250.693787	41.601818	67.597095
1249.785874	42.827366	67.602100
1249.525805	41.172287	67.607105
1248.595524	43.643042	67.612110
1247.938752	42.795576	67.617114
1247.645402	35.750839	67.622119
1246.144997	34.778215	67.627124
1245.772345	34.486810	67.632129
1245.114288	43.485723	67.637134
1244.727641	44.052061	67.642138
1243.906184	31.596206	67.647143
1242.902340	39.161506	67.652148
1242.479614	36.090410	67.657153
1241.830854	36.892664	67.662158
1241.683959	28.334784	67.667162
1241.131018	35.728550	67.672167
1239.915101	42.850977	67.677172
1239.469695	42.787147	67.682177
1238.428856	46.123496	67.687182
1237.470701	46.278496	67.692186
1237.334434	36.020730	67.697191
1236.619619	48.223000	67.702196
1236.343173	41.009983	67.707201
1235.592158	42.842583	67.712206
1234.561004	42.960348	67.717210
1234.378627	32.358393	67.722215
1233.409990	40.546053	67.727220
1232.354295	33.953924	67.732225
1231.717081	27.853804	67.737230
1231.305287	41.393979	67.742234
1230.776311	46.302471	67.747239
1229.275765	39.003782	67.752244
1228.999010	30.506817	67.757249
1228.606582	32.888648	67.762254
1228.163991	39.298052	67.767258
1228.135213	33.788855	67.772263
1226.718284	40.087193	67.777268
1225.994096	32.054836	67.782273
1225.435137	37.542373	67.787278
1224.665180	44.581347	67.792282
1223.938718	32.366587	67.797287
1222.620634	37.082564	67.802292
1222.879267	30.049508	67.807297
1222.343027	37.559226	67.812302
1221.776814	35.638029	67.817306
1221.090052	36.230488	67.822311
1220.181422	35.715472	67.827316
1219.533551	34.569661	67.832321
1218.471836	36.741624	67.837326
1217.998396	41.358781	67.842330
1217.723077	32.160558	67.847335
1217.585166	35.273244	67.852340
1216.420240	35.341683	67.857345
1215.443725	36.313338	67.862350
1214.917467	34.602000	67.867354
1214.271393	25.696192	67.872359
1213.295927	39.008020	67.877364
1212.481970	34.065861	67.882369
1212.211212	40.808589	67.887374
1211.632040	43.051088	67.892378
1211.342638	24.567648	67.897383
1209.996953	31.199163	67.902388
1209.358686	33.409545	67.907393
1209.064984	29.810734	67.912398
1208.151194	33.507811	67.917402
1207.521785	30.991156	67.922407
1206.611654	38.323717	67.927412
1206.749386	34.474602	67.932417
1205.894148	32.058581	67.937422
1204.908829	31.579985	67.942426
1204.582712	29.261258	67.947431
1203.527406	36.251985	67.952436
1202.481640	34.023312	67.957441
1201.798947	35.961054	67.962446
1201.340337	40.045965	67.967450
1201.281451	34.008271	67.972455
1200.639573	41.173334	67.977460
1199.894840	32.107585	67.982465
1198.985212	36.645877	67.987470
1198.696886	38.275718	67.992474
1197.887666	30.519622	67.997479
1196.737896	39.018545	68.002484
1196.273577	27.731096	68.007489
1195.965662	28.332902	68.012494
1194.495458	34.685758	68.017498
1194.095508	33.784855	68.022503
1193.310451	31.181173	68.027508
1193.209792	24.757894	68.032513
1192.753825	29.454552	68.037518
1192.010185	38.483511	68.042522
1191.258180	37.194094	68.047527
1190.552296	40.887156	68.052532
1189.437149	34.466262	68.057537
1188.525588	30.034214	68.062542
1188.118943	27.880451	68.067546
1187.556440	32.724816	68.072551
1186.851534	40.424457	68.077556
1186.993918	34.652287	68.082561
1186.156216	30.654410	68.087566
1184.796041	40.148909	68.092570
1184.559127	35.635691	68.097575
1184.105661	29.581483	68.102580
1183.084429	32.646470	68.107585
1182.161121	32.151342	68.112590
1181.649491	34.396883	68.117594
1181.267168	27.655929	68.122599
1180.463444	34.688842	68.127604
1179.701380	31.186408	68.132609
1179.081844	28.819637	68.137614
1178.572710	33.566844	68.142618
1178.206450	28.628169	68.147623
1177.181370	38.458035	68.152628
1176.214531	34.743176	68.157633
1176.081708	30.757633	68.162638
1175.472481	33.050673	68.167642
1174.661889	31.875495	68.172647
1173.818508	41.073498	68.177652
1173.380136	36.149536	68.182657
1172.982286	36.561096	68.187662
1171.606043	43.782427	68.192666
1170.958937	24.218729	68.197671
1170.455042	27.898126	68.202676
1170.265894	29.507828	68.207681
1169.199772	30.922704	68.212686
1168.068957	35.742805	68.217690
1167.606134	35.730909	68.222695
1167.392459	34.309064	68.227700
1166.835305	34.444759	68.232705
1166.140469	30.950947	68.237710
1165.536779	31.577740	68.242714
1164.773383	29.548611	68.247719
1164.146170	39.213652	68.252724
1163.087527	38.920899	68.257729
1162.517435	36.650657	68.262734
1161.894958	34.087035	68.267738
1161.821472	34.514896	68.272743
1160.385830	40.137543	68.277748
1159.682004	26.909645	68.282753
1159.336081	34.468088	68.287758
1158.851163	39.347723	68.292762
1158.081017	29.823731	68.297767
1157.175639	34.032899	68.302772
1156.528545	32.862491	68.307777
1156.293496	30.243981	68.312782
1155.255381	35.415296	68.317786
1154.349942	34.996056	68.322791
1153.610115	31.413640	68.327796
1153.246172	36.629777	68.332801
1153.344699	28.373683	68.337806
1152.546926	31.966039	68.342810
1151.563129	26.575767	68.347815
1150.655505	34.882452	68.352820
1150.440704	28.124266	68.357825
1149.514765	35.892935	68.362830
1148.707929	38.612553	68.367834
1148.455660	34.688513	68.372839
1147.347350	33.504714	68.377844
1146.693632	24.095787	68.382849
1145.710288	25.303873	68.387854
1145.198685	32.730034	68.392858
1145.168984	28.401593	68.397863
1144.422174	36.181036	68.402868
1143.543766	33.555849	68.407873
1142.884210	29.717731	68.412878
1142.263858	33.685477	68.417882
1141.854558	28.158946	68.422887
1140.917092	32.078758	68.427892
1140.350227	32.183753	68.432897
1139.578363	25.866326	68.437902
1138.282754	28.342021	68.442906
1138.072261	24.324389	68.447911
1137.697451	28.850057	68.452916
1137.204009	27.685315	68.457921
1136.661343	22.490685	68.462926
1135.397680	25.064325	68.467930
1134.866255	25.351925	68.472935
1134.067611	33.363256	68.477940
1133.535019	30.121917	68.482945
1133.028166	16.417046	68.487950
1131.927148	32.061813	68.492954
1131.659472	21.135032	68.497959
1131.120750	26.065322	68.502964
1130.249153	27.285854	68.507969
1129.487827	24.361167	68.512974
1129.001571	35.248577	68.517978
1128.914335	23.977101	68.522983
1127.389225	27.313495	68.527988
1126.901365	33.727097	68.532993
1126.350419	21.113263	68.537998
1125.822862	22.574870	68.543002
1125.007342	22.379041	68.548007
1124.098850	31.963958	68.553012
1123.483179	24.356312	68.558017
1123.550384	29.375078	68.563022
1122.435988	27.761300	68.568026
1121.488874	15.591863	68.573031
1120.811702	32.461876	68.578036
1120.212269	31.694210	68.583041
1120.248139	30.017283	68.588046
1119.501158	31.784473	68.593050
1118.475297	30.528540	68.598055
1117.773379	31.864881	68.603060
1117.085092	30.394051	68.608065
1116.381204	24.997305	68.613070
1115.363904	29.605750	68.618074
1115.226823	29.811225	68.623079
1114.321222	38.869104	68.628084
1113.247357	34.201984	68.633089
1112.938701	26.658999	68.638094
1112.202318	30.981332	68.643098
1112.125259	17.644161	68.648103
1111.463189	26.635073	68.653108
1110.586888	29.101341	68.658113
1109.632345	27.881354	68.663118
1109.186533	32.785081	68.668122
1108.694878	23.245788	68.673127
1107.489287	21.234364	68.678132
1106.687620	30.154055	68.683137
1106.127411	18.811214	68.688142
1105.903330	29.091260	68.693146
1105.894539	24.354660	68.698151
1104.828785	27.646744	68.703156
1104.210611	25.220544	68.708161
1103.465361	22.297451	68.713166
1102.277136	33.325188	68.718170
1101.624181	18.193977	68.723175
1100.886571	29.187182	68.728180
1100.557799	29.896769	68.733185
1100.318227	20.501014	68.738190
1099.422513	31.088291	68.743194
1098.794943	18.415354	68.748199
1098.187124	26.529396	68.753204
1096.684792	22.995852	68.758209
1096.410914	22.754647	68.763214
1095.615529	37.019664	68.768218
1095.478274	31.967185	68.773223
1094.847116	34.154257	68.778228
1093.998313	35.503122	68.783233
1093.419915	24.378513	68.788238
1092.634382	39.405617	68.793242
1092.127283	38.389657	68.798247
1090.858694	46.014127	68.803252
1090.275938	35.320891	68.808257
1090.108425	28.307129	68.813262
1089.390468	39.168299	68.818266
1089.284447	27.139429	68.823271
1088.059365	32.279220	68.828276
1087.416230	26.857471	68.833281
1087.187547	24.698903	68.838286
1086.303096	32.462840	68.843290
1085.599343	23.110256	68.848295
1084.627567	24.661747	68.853300
1083.867994	38.180940	68.858305
1082.833810	28.876645	68.863310
1082.649647	33.519266	68.868314
1082.544600	31.834893	68.873319
1081.872283	26.625367	68.878324
1080.528332	35.645815	68.883329
1080.036545	25.544871	68.888334
1079.518247	33.676744	68.893338
1078.957954	28.943007	68.898343
1077.957901	26.545494	68.903348
1077.243986	31.356586	68.908353
1077.116607	32.495872	68.913358
1076.391577	37.357419	68.918362
1075.365721	30.125921	68.923367
1074.867237	30.112641	68.928372
1074.066470	39.016396	68.933377
1073.432368	28.584973	68.938382
1072.592785	39.180408	68.943386
1072.013554	23.961975	68.948391
1071.506372	32.802428	68.953396
1071.107590	31.919494	68.958401
1070.263313	27.948424	68.963406
1069.261763	32.232884	68.968410
1068.905933	22.925325	68.973415
1068.412541	25.992703	68.978420
1067.291633	22.718704	68.983425
1066.708862	28.237559	68.988430
1065.872639	31.139051	68.993434
1065.770829	29.063357	68.998439
1065.036922	36.196818	69.003444
1064.505095	37.093933	69.008449
1063.446454	34.886444	69.013454
1062.856154	41.145103	69.018458
1062.546542	32.454852	69.023463
1061.447209	40.176649	69.028468
1060.452633	44.497022	69.033473
1060.198133	29.602300	69.038478
1059.461299	41.287315	69.043482
1059.534383	27.315391	69.048487
1058.381739	30.192125	69.053492
1057.352180	29.211955	69.058497
1057.030437	23.731231	69.063502
1056.710547	30.068310	69.068506
1055.502657	23.238629	69.073511
1054.559335	33.990371	69.078516
1054.038031	29.916633	69.083521
1053.957356	30.858064	69.088526
1053.308926	37.666644	69.093530
1052.368231	25.495334	69.098535
1052.034206	39.602013	69.103540
1051.144958	34.010452	69.108545
1050.503782	31.450049	69.113550
1049.156667	35.421472	69.118554
1048.975815	30.682365	69.123559
1048.546369	34.318630	69.128564
1048.051821	31.991261	69.133569
1047.243368	29.183993	69.138574
1046.364676	36.878665	69.143578
1046.065713	29.049045	69.148583
1044.645346	33.834282	69.153588
1044.155400	22.462843	69.158593
1044.060276	28.754722	69.163598
1043.153460	32.810607	69.168602
1042.758768	23.497077	69.173607
1042.139363	33.469051	69.178612
1041.152156	33.373685	69.183617
1041.007391	27.314003	69.188622
1039.538436	34.922659	69.193626
1039.465013	25.047696	69.198631
1038.549999	34.972798	69.203636
1037.322767	38.357676	69.208641
1036.560955	25.529327	69.213646
1035.899041	34.065904	69.218650
1035.529721	31.803534	69.223655
1035.142961	34.439390	69.228660
1034.680586	33.390516	69.233665
1034.319651	31.281439	69.238670
1032.867319	33.871229	69.243674
1032.391974	33.041670	69.248679
1032.143104	31.131678	69.253684
1031.449789	36.016217	69.258689
1030.687183	39.692958	69.263694
1030.040799	37.425142	69.268698
1029.858554	29.042674	69.273703
1028.477314	37.400083	69.278708
1027.733912	34.170782	69.283713
1027.325935	31.705045	69.288718
1026.344513	32.128923	69.293722
1025.398421	33.654713	69.298727
1024.847329	28.575219	69.303732
1024.626147	33.087213	69.308737
1024.110940	29.871333	69.313742
1023.553686	31.725644	69.318746
1022.882991	33.717401	69.323751
1022.159203	34.865274	69.328756
1021.561747	36.108743	69.333761
1020.517134	30.308153	69.338766
1019.457678	33.993099	69.343770
1018.975767	37.384944	69.348775
1018.862937	33.572820	69.353780
1018.174125	41.354578	69.358785
1017.611110	36.060032	69.363790
1016.414316	38.368054	69.368794
1015.751267	29.780968	69.373799
1015.571104	29.834753	69.378804
1014.705188	36.080220	69.383809
1014.059791	29.673667	69.388814
1013.328189	42.875855	69.393818
1012.965174	41.254606	69.398823
1012.243673	35.946546	69.403828
1011.241334	34.453333	69.408833
1010.746141	23.303445	69.413838
1009.978310	40.493310	69.418842
1009.783210	31.540709	69.423847
1008.408889	36.078084	69.428852
1008.053788	40.955625	69.433857
1008.014896	30.348870	69.438862
1006.764268	38.820883	69.443866
1006.006514	30.808536	69.448871
1005.376220	41.085520	69.453876
1004.796684	36.307723	69.458881
1004.481179	31.964289	69.463886
1003.440402	43.799245	69.468890
1002.674598	34.030221	69.473895
1002.270447	34.689568	69.478900
1001.832561	35.703620	69.483905
1000.616907	30.445454	69.488910
999.873455	31.485782	69.493914
999.734887	38.578082	69.498919
999.112138	26.534697	69.503924
998.357258	27.068592	69.508929
997.935412	26.604458	69.513934
997.306145	37.457151	69.518938
996.292652	32.753673	69.523943
995.501510	41.021876	69.528948
995.071702	38.817234	69.533953
994.344962	34.489360	69.538958
993.075096	37.880364	69.543962
992.408383	31.124197	69.548967
992.054509	35.475373	69.553972
991.686175	33.467035	69.558977
990.859211	28.418213	69.563982
989.604706	38.288572	69.568986
989.003370	30.638629	69.573991
988.570205	25.030951	69.578996
988.073139	35.448922	69.584001
987.875795	23.025209	69.589006
987.753493	31.508846	69.594010
986.954330	24.040409	69.599015
985.597309	31.547016	69.604020
985.210559	28.388085	69.609025
984.216856	17.095830	69.614030
983.291326	31.258795	69.619034
982.495888	26.849933	69.624039
982.291596	35.725749	69.629044
981.688564	40.160253	69.634049
981.638490	33.818321	69.639054
980.226920	36.821515	69.644058
979.550233	30.955953	69.649063
979.570332	35.222166	69.654068
978.305984	39.087069	69.659073
977.460725	29.731111	69.664078
977.043580	29.286304	69.669082
976.477944	27.841857	69.674087
975.501430	33.625901	69.679092
974.728620	27.108159	69.684097
974.508575	28.063985	69.689102
973.956516	36.900286	69.694106
972.997503	39.476657	69.699111
972.457870	30.134277	69.704116
971.690706	26.165417	69.709121
971.213031	27.028794	69.714126
970.754564	28.184127	69.719130
969.956163	25.138326	69.724135
969.095228	25.460270	69.729140
968.544781	33.965918	69.734145
968.367129	19.206872	69.739150
967.376637	24.393739	69.744154
966.637020	23.691547	69.749159
965.758180	25.951442	69.754164
964.738240	26.794404	69.759169
964.289733	29.265979	69.764174
963.484248	34.588919	69.769178
963.479621	34.720401	69.774183
963.004199	33.007888	69.779188
961.913782	38.676057	69.784193
961.758601	33.080374	69.789198
960.735428	35.805885	69.794202
959.283702	41.928277	69.799207
959.230417	39.819015	69.804212
958.251672	33.389434	69.809217
958.304197	29.796481	69.814222
956.835012	37.507820	69.819226
956.222054	31.899359	69.824231
955.755496	30.116255	69.829236
955.131224	36.677165	69.834241
955.018944	30.972300	69.839246
954.198289	37.663943	69.844250
953.196100	37.248284	69.849255
953.243283	31.628998	69.854260
951.929694	41.171609	69.859265
950.969097	33.481759	69.864270
950.515863	40.919640	69.869274
950.161676	33.186328	69.874279
950.014129	35.311906	69.879284
948.228830	37.748361	69.884289
948.185627	27.274978	69.889294
947.632947	31.232729	69.894298
946.688894	28.382392	69.899303
945.947361	31.517143	69.904308
945.168563	36.357912	69.909313
944.730322	27.686160	69.914318
943.417872	32.547274	69.919322
942.892047	31.328499	69.924327
942.176882	34.520310	69.929332
942.013399	36.715324	69.934337
941.622579	27.343519	69.939342
940.932758	31.166082	69.944346
940.672077	28.398830	69.949351
939.526164	28.915235	69.954356
938.502968	31.389715	69.959361
938.566504	26.520349	69.964366
936.950006	36.242723	69.969370
936.428559	36.448903	69.974375
935.944017	27.789424	69.979380
935.318761	37.554785	69.984385
935.535826	29.047892	69.989390
934.310477	30.343646	69.994394
933.770278	31.675602	69.999399
932.890314	30.106978	70.004404
931.529460	39.071931	70.009409
931.165391	28.866647	70.014414
930.864228	25.475578	70.019418
930.609676	32.713649	70.024423
929.734996	28.301002	70.029428
928.594352	31.862508	70.034433
927.907692	31.936336	70.039438
927.466654	38.968336	70.044442
927.301084	34.710146	70.049447
926.528339	32.753313	70.054452
925.312072	39.489821	70.059457
925.044276	35.174143	70.064462
924.227966	26.020074	70.069466
923.261190	26.960117	70.074471
922.763401	21.408910	70.079476
922.194171	32.419466	70.084481
921.645523	31.514451	70.089486
920.654427	34.001594	70.094490
920.021900	29.976529	70.099495
919.426470	32.367488	70.104500
918.827180	41.572254	70.109505
918.601809	33.684655	70.114510
917.893262	36.312474	70.119514
916.720189	36.619996	70.124519
916.328882	35.780003	70.129524
916.003010	32.777222	70.134529
915.010635	30.826825	70.139534
914.184948	40.768218	70.144538
913.322702	31.768454	70.149543
913.253867	26.429948	70.154548
912.388934	42.061142	70.159553
911.648150	26.617805	70.164558
911.201618	36.094808	70.169562
910.713031	32.065617	70.174567
909.802893	29.186586	70.179572
909.131886	30.862639	70.184577
908.577701	27.492013	70.189582
907.397745	38.484416	70.194586
906.588397	40.741499	70.199591
906.226972	39.453915	70.204596
905.864077	43.445084	70.209601
905.547000	35.655292	70.214606
904.550680	39.611272	70.219610
903.732511	44.658121	70.224615
903.063703	36.293477	70.229620
902.250334	44.351955	70.234625
901.672168	35.447214	70.239630
900.749104	34.884996	70.244634
900.252672	37.328077	70.249639
899.986577	31.617194	70.254644
899.294925	37.818223	70.259649
898.071043	41.448070	70.264654
897.672219	37.129968	70.269658
897.041930	40.114629	70.274663
897.120672	34.339948	70.279668
896.265517	32.385000	70.284673
895.687370	31.667793	70.289678
894.075127	37.947947	70.294682
892.996657	27.123758	70.299687
892.791463	38.483258	70.304692
892.203467	37.294083	70.309697
891.906111	36.103284	70.314702
891.302115	40.380469	70.319706
890.889114	37.017240	70.324711
890.546432	32.102586	70.329716
889.516195	40.057295	70.334721
888.912724	26.052071	70.339726
887.846242	40.778762	70.344730
887.265765	35.286321	70.349735
887.001235	28.198414	70.354740
885.598142	35.881081	70.359745
884.835332	31.187983	70.364750
884.149467	37.862467	70.369754
883.484079	43.853750	70.374759
883.338666	41.386081	70.379764
883.069248	35.291317	70.384769
882.253885	37.522198	70.389774
881.537072	31.224213	70.394778
880.773329	32.628407	70.399783
879.692879	23.483673	70.404788
878.899210	37.816684	70.409793
878.468354	30.889493	70.414798
878.398002	44.725619	70.419802
877.403917	38.465649	70.424807
876.717545	39.208473	70.429812
875.672976	36.735740	70.434817
875.678046	30.846978	70.439822
874.569948	33.624152	70.444826
873.258925	30.854447	70.449831
873.042742	27.275154	70.454836
872.574638	35.392119	70.459841
872.549157	34.218304	70.464846
871.799439	32.248459	70.469850
870.868074	41.933630	70.474855
870.315054	33.290232	70.479860
869.530945	34.967110	70.484865
868.565904	33.413465	70.489870
867.733903	40.248367	70.494874
867.062094	41.938773	70.499879
866.811760	31.847037	70.504884
866.428004	43.811431	70.509889
865.717114	42.763695	70.514894
865.154760	45.398060	70.519898
864.576832	42.740409	70.524903
863.729418	37.322901	70.529908
862.695070	47.571998	70.534913
862.105443	34.722886	70.539918
861.150400	38.627989	70.544922
860.345519	39.577023	70.549927
860.028579	40.532873	70.554932
859.159089	48.052318	70.559937
859.338251	36.485784	70.564942
858.535896	37.792391	70.569946
857.114155	40.366332	70.574951
856.938237	41.617745	70.579956
856.550306	36.827680	70.584961
855.914204	34.238019	70.589966
854.749324	42.824047	70.594970
854.357996	39.015031	70.599975
853.688904	41.801091	70.604980
852.598110	44.893052	70.609985
852.073635	36.904727	70.614990
851.736032	34.040926	70.619994
851.028726	27.814737	70.624999
850.039475	35.331402	70.630004
848.989141	41.513745	70.635009
849.004125	36.171540	70.640014
848.375897	41.432951	70.645018
847.864324	36.868132	70.650023
847.386896	29.360408	70.655028
846.364334	36.019936	70.660033
845.772792	34.984918	70.665038
844.615361	32.386270	70.670042
843.837482	34.907955	70.675047
843.570241	34.917060	70.680052
843.139584	41.946495	70.685057
842.633762	35.911570	70.690062
841.721389	39.042046	70.695066
840.831062	36.381464	70.700071
840.197490	29.082054	70.705076
839.960145	34.035342	70.710081
839.121221	26.527964	70.715086
837.850987	40.358430	70.720090
837.494262	38.103395	70.725095
837.530509	33.764857	70.730100
836.598010	36.133433	70.735105
835.404827	33.551963	70.740110
835.130559	31.388588	70.745114
834.429783	38.319036	70.750119
834.064303	36.340221	70.755124
832.491600	41.501713	70.760129
831.851720	35.460938	70.765134
831.851164	36.168398	70.770138
831.186399	44.565748	70.775143
830.727836	35.185827	70.780148
829.744613	39.036555	70.785153
828.939132	36.780233	70.790158
828.899992	34.967351	70.795162
827.489851	39.106718	70.800167
826.941135	33.298603	70.805172
826.315515	37.616599	70.810177
826.095338	34.080228	70.815182
825.705282	37.909876	70.820186
824.482528	35.953173	70.825191
823.967314	29.469100	70.830196
823.180448	45.425589	70.835201
822.436846	41.250232	70.840206
821.814568	39.086471	70.845210
821.191653	49.764018	70.850215
820.911315	37.574788	70.855220
819.537500	50.319390	70.860225
819.031382	34.727728	70.865230
818.675460	33.882867	70.870234
818.080476	41.092019	70.875239
817.608746	33.580559	70.880244
816.134757	35.748617	70.885249
815.936679	36.617797	70.890254
815.283829	37.481985	70.895258
814.338208	42.421998	70.900263
813.747931	31.770774	70.905268
813.012542	37.517882	70.910273
812.680979	38.454530	70.915278
812.326387	31.602308	70.920282
810.966720	38.094994	70.925287
810.340896	42.648276	70.930292
809.499536	41.615793	70.935297
809.658494	40.850491	70.940302
809.512606	36.789058	70.945306
807.890333	34.913029	70.950311
807.418352	35.526777	70.955316
806.626173	46.006354	70.960321
805.632646	42.569294	70.965326
805.040320	35.387947	70.970330
804.814052	45.132733	70.975335
804.527277	39.366589	70.980340
803.618091	38.451114	70.985345
802.788125	30.151994	70.990350
802.034048	40.375583	70.995354
801.165825	36.139872	71.000359
800.467932	46.127671	71.005364
799.860378	44.556223	71.010369
799.721368	35.542334	71.015374
799.200410	42.685917	71.020378
797.978984	47.342802	71.025383
797.515933	30.936190	71.030388
796.650516	37.244749	71.035393
796.109768	37.322021	71.040398
794.949717	29.244830	71.045402
794.422651	36.839033	71.050407
794.429983	27.199725	71.055412
793.717446	35.669198	71.060417
793.035007	38.812397	71.065422
792.076487	36.041936	71.070426
791.435687	42.369256	71.075431
791.315974	31.082467	71.080436
790.119005	36.472090	71.085441
789.178259	40.166742	71.090446
788.940921	33.020902	71.095450
788.170997	42.314502	71.100455
787.677300	32.912978	71.105460
786.564885	36.817025	71.110465
785.807777	42.913626	71.115470
785.575134	44.222517	71.120474
785.012299	36.423923	71.125479
784.284448	30.450725	71.130484
783.309125	35.883693	71.135489
782.881487	40.646172	71.140494
782.694885	41.031838	71.145498
781.307005	39.279079	71.150503
780.709844	26.556015	71.155508
779.850795	38.422616	71.160513
779.773170	28.675894	71.165518
779.072114	30.108046	71.170522
778.318080	35.767567	71.175527
777.669926	30.372787	71.180532
777.150651	39.074405	71.185537
776.374567	39.171072	71.190542
775.707517	40.437541	71.195546
774.658774	40.070550	71.200551
774.507188	34.260335	71.205556
773.299720	41.291002	71.210561
772.742975	25.608172	71.215566
772.224131	32.878486	71.220570
771.376756	36.746213	71.225575
771.566573	31.685889	71.230580
770.436479	39.429179	71.235585
769.812855	31.723892	71.240590
769.220026	42.656396	71.245594
768.407796	36.129662	71.250599
767.476180	42.371019	71.255604
766.827644	51.411740	71.260609
766.177869	42.761644	71.265614
765.930693	44.634308	71.270618
764.604866	43.552987	71.275623
764.363676	37.000667	71.280628
763.342175	38.294305	71.285633
762.970921	31.654142	71.290638
763.106717	39.448991	71.295642
761.356166	34.469224	71.300647
761.036828	36.764354	71.305652
760.542516	37.716648	71.310657
760.130123	31.816909	71.315662
759.176727	24.284164	71.320666
758.259554	39.997722	71.325671
757.866432	34.905421	71.330676
757.010323	47.138214	71.335681
756.295875	38.841417	71.340686
755.771303	42.992514	71.345690
755.003098	32.738076	71.350695
754.743947	29.357984	71.355700
753.549916	41.421305	71.360705
752.761147	36.994768	71.365710
752.512344	37.510688	71.370714
751.988635	43.098787	71.375719
751.646196	37.911756	71.380724
750.331982	47.312414	71.385729
749.655828	40.065704	71.390734
749.622643	40.326018	71.395738
748.974581	37.839468	71.400743
747.761390	30.389514	71.405748
746.877010	30.834717	71.410753
746.602545	33.672784	71.415758
746.164270	38.967579	71.420762
744.910211	37.807659	71.425767
744.557081	31.838958	71.430772
743.506965	35.439859	71.435777
743.474282	41.195669	71.440782
742.929145	39.831813	71.445786
741.759242	40.482629	71.450791
741.250635	28.209770	71.455796
740.751830	36.535272	71.460801
739.921584	33.929548	71.465806
739.152564	29.187416	71.470810
738.430255	41.253609	71.475815
738.564718	30.025123	71.480820
737.374600	41.299535	71.485825
736.391080	34.527037	71.490830
736.138334	34.797728	71.495834
735.417123	37.199200	71.500839
734.747587	33.486013	71.505844
734.058132	41.033043	71.510849
733.738221	30.315789	71.515854
732.731639	38.147655	71.520858
731.805693	33.518453	71.525863
731.663113	30.321275	71.530868
730.950176	34.970006	71.535873
729.767116	27.127685	71.540878
728.838638	31.491254	71.545882
728.235981	39.561013	71.550887
727.702025	36.083927	71.555892
727.161614	37.417913	71.560897
727.000241	35.112452	71.565902
726.436818	32.342609	71.570906
725.441810	40.663911	71.575911
725.001448	31.559167	71.580916
724.326408	37.050039	71.585921
722.909595	30.762274	71.590926
722.565351	24.067365	71.595930
721.818045	37.383944	71.600935
721.723615	33.736045	71.605940
721.097875	32.229695	71.610945
720.102864	32.261644	71.615950
719.829645	25.416813	71.620954
718.863955	35.082612	71.625959
717.934701	34.937123	71.630964
716.986629	37.330095	71.635969
716.279419	39.326170	71.640974
716.408211	38.591690	71.645978
715.763727	37.288276	71.650983
715.072572	28.278206	71.655988
714.049993	44.792541	71.660993
713.679488	38.141203	71.665998
713.119960	31.299631	71.671002
711.898056	44.647392	71.676007
711.618827	31.051638	71.681012
710.916822	41.070533	71.686017
710.499248	32.777364	71.691022
709.291617	36.715103	71.696026
708.272791	40.538005	71.701031
708.526393	32.067887	71.706036
707.952122	39.570713	71.711041
706.938865	34.325724	71.716046
706.204101	39.003064	71.721050
705.254091	37.211235	71.726055
705.353326	27.044645	71.731060
704.464084	35.020217	71.736065
703.571649	29.400475	71.741070
702.717818	32.808687	71.746074
702.237671	33.717904	71.751079
701.887186	33.334329	71.756084
701.237874	38.625808	71.761089
700.375113	35.697261	71.766094
699.838428	31.674366	71.771098
698.369203	35.666001	71.776103
697.864395	35.952640	71.781108
697.079253	37.480124	71.786113
696.848077	28.728342	71.791118
696.462045	29.622620	71.796122
696.140822	29.178378	71.801127
695.522113	24.535630	71.806132
694.502677	29.886567	71.811137
694.151524	36.632398	71.816142
693.054196	34.293083	71.821146
691.979200	31.642067	71.826151
691.575013	38.251730	71.831156
691.462262	29.195863	71.836161
690.781135	31.596788	71.841166
690.371717	23.847722	71.846170
689.385946	34.199815	71.851175
688.069593	21.732610	71.856180
687.185794	27.528439	71.861185
686.919597	31.769871	71.866190
686.652113	27.381539	71.871194
686.014844	38.081668	71.876199
685.284756	27.629287	71.881204
684.398373	28.542972	71.886209
684.064560	31.976171	71.891214
683.242965	33.509113	71.896218
681.979111	35.852380	71.901223
681.496556	29.431812	71.906228
681.322932	27.795911	71.911233
680.742732	22.770409	71.916238
680.029058	30.774321	71.921242
678.992436	28.629860	71.926247
678.675805	28.654146	71.931252
678.204824	37.261443	71.936257
677.222391	27.425812	71.941262
676.318013	23.438286	71.946266
675.593096	29.425173	71.951271
675.176942	28.569723	71.956276
674.324076	35.377034	71.961281
673.654495	27.921602	71.966286
673.186449	34.507470	71.971290
672.777999	30.646942	71.976295
672.168365	34.185023	71.981300
671.032321	35.401992	71.986305
670.385753	27.890122	71.991310
670.153291	20.179819	71.996314
669.313808	34.003998	72.001319
668.804733	31.424577	72.006324
667.580500	35.622522	72.011329
667.001472	28.570367	72.016334
666.906646	25.249363	72.021338
666.236499	44.027384	72.026343
665.590696	25.123201	72.031348
664.416930	36.422447	72.036353
663.962577	35.446050	72.041358
663.563823	28.950738	72.046362
662.622287	29.905847	72.051367
661.752338	24.851835	72.056372
661.354139	34.679346	72.061377
660.897150	34.182582	72.066382
659.891505	36.739365	72.071386
659.047138	31.584658	72.076391
658.730296	29.098219	72.081396
658.406429	33.087443	72.086401
657.473275	36.776077	72.091406
656.548919	25.056806	72.096410
655.872986	33.743817	72.101415
655.699237	27.846234	72.106420
654.472740	31.765902	72.111425
653.790438	34.885014	72.116430
653.752061	31.175415	72.121434
653.080599	41.761018	72.126439
652.087637	33.506833	72.131444
651.420234	42.120944	72.136449
650.860982	33.402875	72.141454
650.813766	29.459937	72.146458
649.467126	39.921622	72.151463
648.745149	27.675079	72.156468
648.359070	35.375781	72.161473
647.277311	38.581093	72.166478
646.534737	31.425916	72.171482
646.077993	36.867948	72.176487
645.916279	25.736397	72.181492
644.809358	25.729512	72.186497
643.930532	29.773948	72.191502
643.361954	23.840992	72.196506
642.746066	35.569628	72.201511
642.485219	41.106381	72.206516
641.457594	32.722357	72.211521
640.603230	28.262483	72.216526
640.516343	24.477123	72.221530
639.995793	35.243302	72.226535
638.690411	26.120208	72.231540
638.158304	34.527990	72.236545
637.719988	36.609051	72.241550
637.192342	38.743308	72.246554
635.930166	38.889727	72.251559
635.513241	36.141768	72.256564
635.080505	42.121234	72.261569
634.442911	39.170701	72.266574
633.215942	34.255223	72.271578
632.374801	45.569724	72.276583
632.070834	34.389124	72.281588
631.792675	41.174159	72.286593
631.261775	38.326919	72.291598
630.488844	37.516810	72.296602
629.482511	41.062471	72.301607
629.379051	35.946611	72.306612
628.456370	34.581538	72.311617
627.284736	29.724472	72.316622
626.789404	24.621285	72.321626
626.380514	33.776854	72.326631
626.121645	31.544152	72.331636
625.113364	34.072974	72.336641
624.270740	26.374060	72.341646
623.773063	35.737067	72.346650
622.907741	34.228755	72.351655
622.466404	33.731286	72.356660
621.530487	36.929772	72.361665
620.837332	42.421784	72.366670
620.775520	35.440880	72.371674
619.604176	46.412507	72.376679
618.870100	36.818925	72.381684
618.158064	28.779501	72.386689
617.761557	37.314437	72.391694
617.776915	29.940207	72.396698
616.292481	40.074607	72.401703
615.624969	26.139638	72.406708
615.062687	37.737521	72.411713
614.350099	38.090554	72.416718
613.556334	28.409712	72.421722
612.912375	31.217146	72.426727
612.462359	25.637279	72.431732
611.979335	34.328344	72.436737
611.271237	40.239731	72.441742
610.248589	25.559609	72.446746
609.931194	36.227827	72.451751
609.618919	35.291431	72.456756
608.671698	33.443097	72.461761
607.515093	38.553884	72.466766
607.352377	31.881173	72.471770
606.425703	32.737437	72.476775
606.081770	28.971251	72.481780
605.160301	33.010369	72.486785
604.272225	28.454048	72.491790
604.092250	29.665900	72.496794
603.566631	34.813832	72.501799
602.571432	32.303499	72.506804
601.895231	34.500314	72.511809
601.436447	33.754011	72.516814
600.568899	25.530065	72.521818
599.775610	36.058386	72.526823
599.275004	29.291211	72.531828
598.857004	28.305435	72.536833
597.649061	28.921357	72.541838
597.173731	34.831939	72.546842
596.395221	33.249552	72.551847
596.201173	27.589911	72.556852
595.749806	33.257981	72.561857
594.469182	35.370079	72.566862
594.146695	26.712111	72.571866
593.509981	39.805284	72.576871
592.536746	35.195270	72.581876
591.908407	28.557342	72.586881
590.898319	38.130900	72.591886
590.991990	33.897395	72.596890
589.941255	40.481267	72.601895
588.676580	39.487014	72.606900
588.149778	31.753336	72.611905
587.680565	35.004883	72.616910
587.712546	33.691762	72.621914
587.092662	34.623747	72.626919
586.479543	29.474829	72.631924
585.607465	33.195243	72.636929
585.013220	39.361845	72.641934
584.398676	27.728846	72.646938
583.091127	26.532745	72.651943
582.494158	31.390157	72.656948
582.180494	39.365409	72.661953
581.441148	40.885064	72.666958
580.679232	32.695913	72.671962
579.882282	39.294326	72.676967
579.479467	36.203715	72.681972
579.210361	39.333350	72.686977
577.965838	40.455250	72.691982
577.311897	37.434112	72.696986
576.813344	40.475175	72.701991
576.379820	35.369691	72.706996
574.827920	33.683781	72.712001
574.305075	34.761367	72.717006
574.504890	33.301866	72.722010
573.785748	36.468350	72.727015
573.114417	36.263698	72.732020
572.339274	32.788885	72.737025
571.763898	32.386225	72.742030
571.325355	35.064922	72.747034
569.874751	49.184076	72.752039
569.234736	37.929626	72.757044
568.870397	39.874866	72.762049
568.421363	36.347335	72.767054
567.720214	37.446394	72.772058
566.195617	44.024231	72.777063
566.016774	39.735187	72.782068
565.751790	35.368542	72.787073
565.139247	24.173733	72.792078
564.498406	24.291074	72.797082
563.378795	39.652898	72.802087
563.145678	32.196121	72.807092
562.838915	27.203519	72.812097
561.405186	31.405014	72.817102
560.872034	33.258791	72.822106
560.517699	37.059436	72.827111
560.086676	34.636381	72.832116
559.328552	34.305296	72.837121
558.188872	38.624558	72.842126
557.710208	35.008164	72.847130
556.425070	38.457143	72.852135
555.771010	31.093808	72.857140
555.476150	35.165296	72.862145
554.902971	36.326504	72.867150
554.813902	27.902477	72.872154
553.698712	37.140779	72.877159
552.922750	35.038917	72.882164
552.763333	34.984566	72.887169
551.501027	34.498307	72.892174
550.968092	24.533992	72.897178
550.063899	35.366694	72.902183
549.551577	32.631539	72.907188
549.279552	32.402679	72.912193
548.287125	36.261345	72.917198
547.932140	38.680611	72.922202
547.021447	44.485017	72.927207
546.571573	39.752972	72.932212
546.157440	39.509780	72.937217
544.545639	49.684181	72.942222
544.620393	37.066291	72.947226
543.694099	42.020793	72.952231
543.467320	40.702671	72.957236
542.268548	42.108828	72.962241
541.435332	40.957770	72.967246
541.127967	37.416230	72.972250
540.490436	36.819764	72.977255
539.576199	35.716534	72.982260
539.076456	32.393869	72.987265
538.602668	35.567654	72.992270
538.201353	28.910179	72.997274
537.575699	38.851659	73.002279
536.712411	44.847274	73.007284
536.604405	39.177629	73.012289
535.435694	40.126691	73.017294
534.053422	41.044062	73.022298
533.609744	41.233406	73.027303
533.256276	43.323619	73.032308
532.372883	43.766717	73.037313
531.514481	44.160931	73.042318
530.955655	35.391501	73.047322
530.294437	40.782527	73.052327
530.005669	33.285161	73.057332
529.558131	34.052631	73.062337
528.536386	42.292886	73.067342
527.923929	30.689935	73.072346
527.546118	32.512361	73.077351
526.780355	33.880639	73.082356
525.564080	37.630832	73.087361
525.093924	43.688550	73.092366
524.914249	34.157883	73.097370
524.151944	32.385244	73.102375
523.222760	35.477205	73.107380
522.725848	37.388325	73.112385
522.028404	38.441759	73.117390
521.468627	32.601650	73.122394
520.251291	39.296573	73.127399
519.771541	35.402888	73.132404
519.676450	29.884184	73.137409
519.103248	35.266048	73.142414
518.325876	36.017409	73.147418
517.207164	35.087370	73.152423
516.920049	37.453957	73.157428
516.181034	34.089010	73.162433
515.233414	36.184327	73.167438
514.779216	35.406459	73.172442
514.192058	36.806893	73.177447
513.034724	34.525666	73.182452
512.436678	35.773240	73.187457
511.777504	39.294563	73.192462
511.548427	40.882309	73.197466
511.076102	44.998024	73.202471
510.112250	40.172488	73.207476
509.333290	33.459339	73.212481
508.645034	40.055317	73.217486
508.423162	38.740698	73.222490
507.195996	35.802402	73.227495
506.560471	33.797661	73.232500
506.383465	29.382397	73.237505
505.649596	36.068289	73.242510
504.564331	28.156395	73.247514
503.508327	37.427981	73.252519
503.149089	37.141836	73.257524
503.211764	37.993975	73.262529
502.505834	43.055187	73.267534
501.798449	36.067291	73.272538
500.493626	40.978905	73.277543
500.118011	36.043103	73.282548
499.752777	37.643522	73.287553
498.754332	40.478162	73.292558
498.296139	35.728210	73.297562
497.166725	33.431151	73.302567
497.126261	31.818624	73.307572
496.667577	25.416892	73.312577
495.320468	31.990380	73.317582
494.698001	30.128263	73.322586
494.552983	38.932321	73.327591
493.698178	38.165868	73.332596
492.651987	30.427269	73.337601
491.831435	33.997166	73.342606
491.831440	30.652422	73.347610
491.301129	29.648799	73.352615
490.477570	36.502815	73.357620
489.610513	30.144219	73.362625
488.848344	32.887455	73.367630
488.560948	34.630842	73.372634
487.403273	39.373569	73.377639
486.538234	30.782141	73.382644
486.492747	33.421120	73.387649
485.884852	37.718740	73.392654
485.015035	31.573762	73.397658
484.052286	39.713128	73.402663
483.304536	34.099829	73.407668
483.557492	33.008564	73.412673
482.310264	41.514817	73.417678
481.566811	26.039711	73.422682
480.920634	31.828792	73.427687
480.310693	32.368717	73.432692
480.106323	28.937028	73.437697
478.825114	33.552117	73.442702
478.765469	29.137665	73.447706
477.992941	34.195290	73.452711
476.851597	29.195720	73.457716
476.287260	25.364299	73.462721
475.688584	35.125904	73.467726
475.205338	25.506357	73.472730
474.173986	26.687273	73.477735
473.507574	26.822428	73.482740
472.812253	29.125160	73.487745
472.258066	28.832164	73.492750
472.204679	23.426705	73.497754
471.151159	22.987580	73.502759
470.221234	29.715752	73.507764
469.451032	22.018286	73.512769
469.426857	32.570331	73.517774
469.189266	27.764427	73.522778
467.880552	28.375940	73.527783
467.278762	25.923349	73.532788
466.261290	21.198591	73.537793
465.196642	27.266605	73.542798
464.701658	27.149768	73.547802
464.390845	30.804413	73.552807
463.776565	34.323573	73.557812
463.579908	30.124429	73.562817
462.617059	26.265780	73.567822
461.779719	29.063740	73.572826
461.087580	31.579466	73.577831
460.565153	34.147026	73.582836
460.580420	33.462388	73.587841
458.900318	35.592846	73.592846
458.676408	31.058527	73.597850
458.086800	37.261048	73.602855
457.448568	33.548074	73.607860
456.655226	30.572950	73.612865
455.605783	27.143982	73.617870
455.637170	30.699331	73.622874
454.229036	34.137044	73.627879
453.248392	33.138364	73.632884
453.062879	30.809032	73.637889
452.528714	37.267299	73.642894
452.309263	31.113900	73.647898
451.817366	34.863126	73.652903
450.841725	41.519013	73.657908
450.566796	34.396236	73.662913
449.300591	31.022571	73.667918
448.583689	34.144872	73.672922
447.878755	37.712725	73.677927
447.554886	33.973511	73.682932
446.673714	27.553009	73.687937
445.518190	38.589042	73.692942
445.285010	33.556608	73.697946
444.797387	31.501270	73.702951
444.226003	40.747050	73.707956
443.392268	29.572017	73.712961
442.361616	30.139044	73.717966
441.996166	34.334334	73.722970
441.623091	32.308311	73.727975
440.735376	29.444488	73.732980
440.128839	21.679117	73.737985
439.641351	30.650006	73.742990
438.941633	28.932574	73.747994
437.890566	31.811371	73.752999
436.854335	42.963930	73.758004
436.555490	25.998003	73.763009
435.900241	28.975142	73.768014
436.001807	37.154346	73.773018
435.073371	36.308555	73.778023
433.672636	39.678300	73.783028
433.443751	34.567767	73.788033
432.950934	43.154338	73.793038
432.309368	37.749416	73.798042
431.557364	34.281718	73.803047
430.755955	36.824463	73.808052
430.295372	35.651803	73.813057
429.470861	33.020293	73.818062
428.762609	30.685418	73.823066
428.189392	27.419173	73.828071
427.903546	32.411163	73.833076
427.236981	25.364586	73.838081
426.243263	40.886808	73.843086
425.661685	33.970128	73.848090
424.755789	30.597484	73.853095
423.819407	34.359334	73.858100
423.291740	25.343030	73.863105
422.866864	35.582844	73.868110
422.532470	34.253174	73.873114
421.953664	35.802967	73.878119
420.643648	26.282486	73.883124
420.407766	26.195457	73.888129
419.907675	31.450726	73.893134
418.800005	32.211340	73.898138
418.038593	34.440937	73.903143
417.445482	32.873780	73.908148
417.277834	32.512970	73.913153
416.308623	32.922246	73.918158
415.672909	30.432847	73.923162
415.013387	31.840167	73.928167
414.619065	32.638787	73.933172
413.765910	33.977061	73.938177
412.642515	37.489138	73.943182
412.233087	32.687425	73.948186
411.946366	34.242028	73.953191
410.794424	36.358564	73.958196
409.952924	34.955941	73.963201
409.160071	43.098174	73.968206
409.089846	36.661852	73.973210
408.660547	43.248590	73.978215
407.854507	35.040203	73.983220
407.109155	26.618144	73.988225
406.491455	30.666807	73.993230
406.184057	22.580591	73.998234
405.388153	32.170745	74.003239
404.124505	30.390893	74.008244
404.278592	28.922253	74.013249
403.065751	36.941076	74.018254
402.380826	37.369921	74.023258
401.804472	28.423538	74.028263
400.843962	35.953095	74.033268
400.317155	35.028614	74.038273
399.357602	42.241452	74.043278
399.005649	31.727106	74.048282
398.437572	39.231645	74.053287
397.770162	34.601636	74.058292
397.574782	37.388268	74.063297
396.263291	34.867455	74.068302
395.858398	29.177263	74.073306
395.464650	32.693370	74.078311
394.269547	35.223069	74.083316
393.481018	33.561125	74.088321
392.680135	39.899326	74.093326
392.602817	35.415673	74.098330
392.109526	34.812665	74.103335
391.295298	35.607465	74.108340
390.765495	32.542192	74.113345
389.782622	36.430823	74.118350
389.338724	39.278597	74.123354
387.916128	39.678348	74.128359
387.359234	36.218666	74.133364
387.162925	30.024995	74.138369
386.658780	36.446148	74.143374
386.510059	32.265241	74.148378
385.568693	42.932631	74.153383
384.393797	46.322893	74.158388
384.299603	30.278682	74.163393
383.523207	35.594332	74.168398
382.741011	33.857099	74.173402
382.493413	30.471903	74.178407
381.295007	42.302743	74.183412
380.401343	31.317986	74.188417
379.375280	35.749644	74.193422
378.869619	36.499062	74.198426
378.610561	38.319698	74.203431
378.060493	36.408087	74.208436
377.909404	34.705976	74.213441
376.622397	37.093545	74.218446
376.141269	32.055852	74.223450
375.607848	31.982714	74.228455
374.420759	38.264350	74.233460
373.984714	26.071509	74.238465
373.425904	29.265006	74.243470
372.997060	30.495044	74.248474
371.963485	32.770106	74.253479
370.966487	30.692739	74.258484
370.827083	34.184204	74.263489
370.372087	40.154860	74.268494
369.326630	37.248616	74.273498
368.347805	36.630144	74.278503
367.854754	40.249714	74.283508
367.992299	35.465573	74.288513
366.637872	33.041728	74.293518
365.976489	32.432007	74.298522
365.175463	32.137120	74.303527
364.627746	34.090116	74.308532
364.530100	27.936773	74.313537
363.200788	36.956025	74.318542
363.048448	30.287879	74.323546
362.247281	35.349635	74.328551
361.528903	41.256885	74.333556
360.754148	26.476349	74.338561
359.602781	35.125259	74.343566
359.214345	36.961358	74.348570
359.050224	37.425286	74.353575
358.602157	36.945969	74.358580
357.732530	35.174781	74.363585
356.658599	37.757927	74.368590
356.274875	34.544473	74.373594
355.578313	31.122154	74.378599
354.250063	28.873815	74.383604
354.093699	26.555283	74.388609
353.674618	36.431759	74.393614
353.336991	33.322504	74.398618
352.346806	29.569217	74.403623
351.483423	29.267652	74.408628
351.051883	26.343825	74.413633
350.350337	29.545209	74.418638
349.297841	30.927525	74.423642
348.965630	39.790497	74.428647
348.221043	34.921505	74.433652
347.800684	36.672687	74.438657
346.771108	38.239748	74.443662
345.932632	34.169954	74.448666
345.615162	32.550435	74.453671
345.143196	37.609060	74.458676
344.692575	37.374508	74.463681
343.690900	33.822916	74.468686
343.237417	35.209142	74.473690
342.555809	35.294423	74.478695
341.043781	25.519668	74.483700
340.481733	25.618404	74.488705
339.838667	32.775424	74.493710
339.463747	26.202663	74.498714
339.644435	26.587759	74.503719
338.939457	44.181281	74.508724
338.247819	34.044878	74.513729
337.494853	34.260014	74.518734
335.930825	35.489625	74.523738
335.562678	35.630914	74.528743
335.028539	37.797887	74.533748
334.941185	27.598972	74.538753
333.572776	38.273637	74.543758
332.753781	35.671199	74.548762
332.277584	38.552141	74.553767
331.589579	43.115725	74.558772
331.372489	32.504072	74.563777
330.627155	34.803551	74.568782
329.939734	39.131392	74.573786
329.411449	33.575243	74.578791
327.713290	43.885273	74.583796
327.671526	38.224423	74.588801
326.823791	38.085170	74.593806
326.377178	30.729749	74.598810
326.101798	35.159457	74.603815
325.263280	45.229396	74.608820
324.467442	35.923565	74.613825
323.795685	44.397921	74.618830
323.384138	34.328378	74.623834
322.432658	38.600431	74.628839
321.400331	38.805032	74.633844
321.002294	36.917106	74.638849
320.817747	41.184021	74.643854
320.109520	40.613122	74.648858
319.563655	35.018938	74.653863
318.706545	31.703873	74.658868
318.130027	30.157175	74.663873
317.053500	38.010160	74.668878
316.447299	34.564071	74.673882
316.110807	34.648228	74.678887
315.135863	43.010744	74.683892
314.269883	33.168290	74.688897
313.450212	35.889433	74.693902
313.005970	34.915683	74.698906
312.965465	32.473091	74.703911
312.368687	39.734280	74.708916
311.437590	30.493477	74.713921
310.532602	35.462910	74.718926
310.240177	38.236178	74.723930
309.429708	34.244875	74.728935
308.340974	38.914246	74.733940
307.836939	25.517759	74.738945
307.283478	33.572784	74.743950
306.800923	38.353375	74.748954
305.781074	36.915424	74.753959
305.174072	44.824509	74.758964
304.501802	38.031547	74.763969
304.081022	30.344092	74.768974
303.820056	30.426357	74.773978
302.875200	35.386047	74.778983
301.899907	41.670867	74.783988
301.666264	36.359070	74.788993
300.631048	40.811652	74.793998
299.599838	33.604192	74.799002
299.323458	32.894547	74.804007
299.057012	40.171351	74.809012
298.434847	33.492164	74.814017
297.285712	35.231690	74.819022
296.831775	32.692603	74.824026
296.409250	29.278190	74.829031
295.315378	31.620045	74.834036
295.057158	21.002824	74.839041
293.806816	32.613244	74.844046
293.414437	35.370488	74.849050
292.232743	27.457032	74.854055
291.670507	39.924847	74.859060
291.558560	33.587261	74.864065
291.306727	37.298903	74.869070
290.389428	36.764633	74.874074
289.522204	36.198098	74.879079
288.404462	33.657926	74.884084
288.271194	28.432738	74.889089
287.704657	38.796694	74.894094
286.665292	39.424455	74.899098
286.173949	29.932246	74.904103
285.364516	32.863597	74.909108
285.239502	30.173798	74.914113
284.263284	40.251945	74.919118
283.527935	40.051203	74.924122
282.899700	37.215960	74.929127
282.464025	44.500063	74.934132
281.649803	32.637303	74.939137
280.678167	29.564099	74.944142
280.239790	39.030620	74.949146
280.028784	37.859802	74.954151
278.561793	44.031943	74.959156
278.070713	35.937357	74.964161
277.398905	38.524222	74.969166
277.123542	34.567911	74.974170
276.128383	39.021525	74.979175
275.161590	40.175629	74.984180
274.868404	29.957135	74.989185
274.556809	35.952947	74.994190
273.906015	36.794353	74.999194
273.318900	28.659394	75.004199
272.137756	37.721552	75.009204
272.123533	27.465903	75.014209
270.822050	36.353700	75.019214
269.917256	30.637507	75.024218
269.992444	27.118449	75.029223
269.026072	36.805328	75.034228
268.350254	28.725835	75.039233
267.269947	35.899388	75.044238
266.910799	37.825204	75.049242
266.597598	26.921769	75.054247
265.835043	41.984405	75.059252
264.832416	33.537797	75.064257
264.133839	39.972941	75.069262
263.283303	36.877798	75.074266
263.404868	34.266122	75.079271
262.497452	37.060730	75.084276
261.588094	32.246445	75.089281
260.894607	32.588757	75.094286
260.763528	33.358056	75.099290
260.301625	29.120322	75.104295
258.856575	31.895379	75.109300
258.620832	35.934242	75.114305
257.868593	37.499964	75.119310
256.693082	30.191340	75.124314
255.936125	30.599397	75.129319
255.398476	37.821244	75.134324
255.066179	21.974974	75.139329
254.671521	30.237630	75.144334
254.194703	35.988228	75.149338
253.262522	38.950098	75.154343
252.585078	38.867716	75.159348
252.448858	31.600805	75.164353
251.287376	35.242593	75.169358
250.488526	31.984658	75.174362
249.964625	33.596895	75.179367
249.105367	32.627187	75.184372
248.196790	29.618966	75.189377
247.478105	34.313727	75.194382
247.303987	32.013242	75.199386
246.662244	32.095652	75.204391
246.151309	34.872035	75.209396
245.317650	33.690718	75.214401
244.603258	38.297118	75.219406
243.917538	38.331412	75.224410
243.201184	28.327555	75.229415
241.999928	29.471331	75.234420
241.535187	29.132639	75.239425
241.249013	37.486039	75.244430
241.137802	39.521321	75.249434
240.386411	29.043897	75.254439
239.222694	33.635348	75.259444
238.511417	38.360418	75.264449
238.287785	34.486817	75.269454
237.452777	38.605901	75.274458
236.712262	33.903592	75.279463
235.876318	34.656353	75.284468
235.327970	31.475079	75.289473
234.332899	28.967182	75.294478
233.561549	32.302116	75.299482
233.456671	31.466769	75.304487
232.745708	33.671955	75.309492
232.399577	31.497266	75.314497
231.219635	34.848163	75.319502
230.420044	34.775670	75.324506
230.214523	25.867992	75.329511
229.674789	32.052108	75.334516
229.009845	27.726033	75.339521
228.191444	34.418937	75.344526
227.557881	33.729078	75.349530
226.560802	28.254885	75.354535
225.219339	37.793317	75.359540
225.259075	32.147715	75.364545
224.999901	34.177177	75.369550
224.040543	31.381731	75.374554
224.081100	34.567629	75.379559
222.856614	32.252995	75.384564
222.517123	33.641795	75.389569
221.112111	39.405457	75.394574
220.040792	39.009700	75.399578
219.764868	31.567806	75.404583
219.184005	33.753456	75.409588
218.970036	24.873279	75.414593
218.928521	26.874509	75.419598
217.522443	28.382588	75.424602
217.102593	25.210869	75.429607
216.274104	30.005764	75.434612
215.308976	27.551945	75.439617
214.389716	36.845123	75.444622
214.066691	28.822003	75.449626
213.759546	22.806027	75.454631
213.220428	35.331053	75.459636
212.101803	19.375654	75.464641
211.415444	32.890194	75.469646
210.909073	33.068606	75.474650
210.668475	21.535414	75.479655
209.071510	32.853181	75.484660
209.076719	30.905223	75.489665
208.497698	29.396072	75.494670
207.688499	28.852368	75.499674
207.074593	30.156375	75.504679
206.621486	32.001990	75.509684
205.696560	22.286119	75.514689
204.521240	35.383196	75.519694
203.768742	30.666766	75.524698
203.705759	38.816918	75.529703
202.947470	41.120610	75.534708
202.632974	34.759335	75.539713
201.834142	40.296338	75.544718
200.820910	35.381065	75.549722
200.407584	31.342235	75.554727
199.411603	35.638907	75.559732
198.852208	23.951166	75.564737
198.376829	32.231608	75.569742
197.943083	28.602041	75.574746
197.877759	24.473167	75.579751
196.446377	34.683417	75.584756
195.804454	35.007822	75.589761
194.617607	32.575041	75.594766
193.713510	27.055315	75.599770
193.157091	27.036664	75.604775
192.661309	28.681978	75.609780
192.435240	27.793202	75.614785
192.133374	32.065225	75.619790
191.355994	28.036701	75.624794
190.504592	25.207365	75.629799
189.771378	35.974076	75.634804
189.475760	24.072580	75.639809
188.395498	24.417261	75.644814
187.611042	25.380663	75.649818
187.122875	28.783104	75.654823
186.511865	30.287129	75.659828
185.886060	28.951780	75.664833
184.936124	33.799075	75.669838
184.167581	29.223549	75.674842
184.058751	32.024159	75.679847
183.355608	34.683901	75.684852
182.654745	25.899034	75.689857
181.682362	24.815320	75.694862
181.501695	30.622908	75.699866
180.432382	30.123008	75.704871
179.494343	29.461272	75.709876
179.105487	32.393169	75.714881
178.561760	26.166322	75.719886
177.847459	34.255237	75.724890
176.957568	22.215633	75.729895
176.440495	28.053652	75.734900
175.536076	29.885457	75.739905
175.213433	30.669044	75.744910
174.561950	33.610438	75.749914
174.055278	20.662043	75.754919
173.402728	34.657465	75.759924
172.803192	26.207312	75.764929
172.045702	27.348055	75.769934
171.051581	29.717833	75.774938
170.657550	25.970549	75.779943
170.147557	38.375329	75.784948
169.493496	28.943800	75.789953
168.504621	25.145734	75.794958
167.852243	30.120431	75.799962
167.554243	27.641466	75.804967
166.635864	33.110153	75.809972
165.608006	28.931165	75.814977
165.348734	24.372151	75.819982
164.803300	36.783794	75.824986
164.296353	25.416258	75.829991
163.371166	30.996237	75.834996
162.940624	28.881811	75.840001
162.475111	33.395426	75.845006
161.094910	38.445555	75.850010
160.373434	19.309413	75.855015
159.837405	36.358860	75.860020
159.539726	34.054695	75.865025
158.803684	23.571115	75.870030
157.900854	31.129492	75.875034
158.029663	24.623949	75.880039
157.068632	29.573800	75.885044
155.954493	32.482804	75.890049
155.320221	26.721847	75.895054
154.709478	35.509410	75.900058
154.223182	24.869734	75.905063
152.974304	35.658140	75.910068
152.201796	31.553793	75.915073
152.047379	21.931627	75.920078
151.536428	35.871199	75.925082
151.153173	22.580753	75.930087
149.897715	28.665739	75.935092
149.246485	30.729652	75.940097
148.829323	30.136909	75.945102
148.072518	34.559155	75.950106
147.617803	26.610329	75.955111
146.559334	32.861666	75.960116
146.140966	23.237778	75.965121
145.874924	29.939413	75.970126
144.987466	28.696290	75.975130
144.042584	24.633733	75.980135
143.341866	34.580194	75.985140
143.469499	31.119642	75.990145
142.444084	26.649735	75.995150
141.338334	27.862421	76.000154
141.168573	29.996154	76.005159
139.996028	34.604532	76.010164
139.202899	28.587803	76.015169
138.387137	41.524970	76.020174
137.523453	35.009185	76.025178
137.496559	27.193847	76.030183
137.175132	33.758935	76.035188
136.796353	27.161999	76.040193
135.885503	35.539990	76.045198
134.836367	30.637207	76.050202
134.833269	25.449320	76.055207
133.797582	20.959864	76.060212
132.940354	22.918576	76.065217
132.547387	32.080091	76.070222
131.476872	40.421118	76.075226
130.683210	30.477908	76.080231
129.837098	31.601089	76.085236
129.434514	39.361065	76.090241
129.123119	31.706595	76.095246
128.281228	34.437890	76.100250
127.435884	29.941458	76.105255
126.738894	37.218650	76.110260
126.511023	28.325869	76.115265
126.143299	23.875051	76.120270
125.130594	34.830194	76.125274
124.532934	31.949082	76.130279
123.922103	35.600700	76.135284
122.732182	31.874608	76.140289
121.883966	28.574641	76.145294
121.574689	31.797219	76.150298
121.343057	23.179409	76.155303
120.786131	36.594005	76.160308
120.158009	29.706682	76.165313
118.999913	23.510176	76.170318
118.476416	37.747932	76.175322
117.824616	22.957847	76.180327
116.808177	37.087886	76.185332
116.262733	27.692220	76.190337
116.051799	32.155878	76.195342
115.164739	41.094625	76.200346
114.206068	32.606188	76.205351
113.546361	39.091124	76.210356
113.132292	34.264986	76.215361
112.762418	33.115887	76.220366
111.498569	35.404822	76.225370
111.092555	28.609678	76.230375
110.278004	35.758220	76.235380
109.989514	39.160381	76.240385
109.363402	25.133998	76.245390
108.113044	32.908662	76.250394
107.701413	27.285980	76.255399
107.104921	34.873552	76.260404
106.797080	36.599936	76.265409
105.805560	31.930425	76.270414
105.006192	43.600134	76.275418
104.732371	32.780759	76.280423
104.297913	32.670162	76.285428
103.937805	35.291629	76.290433
102.743160	25.831619	76.295438
101.665329	28.923081	76.300442
100.852791	31.172538	76.305447
100.177186	31.780605	76.310452
99.786498	33.447776	76.315457
99.342749	30.815395	76.320462
98.579426	34.898919	76.325466
98.434308	37.471688	76.330471
97.145418	42.068052	76.335476
96.571703	34.696173	76.340481
96.145084	26.257442	76.345486
95.143186	41.880548	76.350490
94.444555	38.099839	76.355495
93.806500	32.668333	76.360500
93.614710	33.095963	76.365505
92.522248	28.720453	76.370510
91.425875	39.229321	76.375514
90.933039	37.500162	76.380519
90.361350	38.915753	76.385524
90.514298	35.071150	76.390529
89.870185	31.489504	76.395534
88.543948	34.925509	76.400538
88.338219	31.554476	76.405543
87.367483	40.618878	76.410548
86.656278	41.557897	76.415553
86.035455	37.225466	76.420558
85.135195	38.598712	76.425562
85.194761	32.424360	76.430567
83.937064	29.856136	76.435572
82.740403	30.696422	76.440577
82.343612	41.671103	76.445582
81.911517	44.139531	76.450586
81.839500	36.960702	76.455591
81.329607	34.591881	76.460596
80.270287	35.727152	76.465601
79.622100	31.347314	76.470606
78.760350	35.780061	76.475610
78.284923	29.457843	76.480615
77.329827	40.797434	76.485620
76.775949	27.439154	76.490625
76.457917	30.630473	76.495630
75.541806	38.200614	76.500634
75.011617	31.141388	76.505639
74.597069	40.286477	76.510644
73.363785	37.916950	76.515649
72.619599	27.242563	76.520654
71.756309	38.535231	76.525658
71.894724	32.719177	76.530663
70.908685	36.033314	76.535668
69.798965	17.444921	76.540673
69.566313	25.183254	76.545678
68.619879	32.419537	76.550682
68.737269	27.458873	76.555687
67.962755	39.439693	76.560692
67.109650	33.419447	76.565697
66.304564	26.866403	76.570702
64.977611	41.570307	76.575706
64.346508	40.793608	76.580711
63.775556	48.578507	76.585716
63.241269	39.156855	76.590721
63.192261	30.679438	76.595726
62.452917	38.618720	76.600730
62.119297	37.348550	76.605735
60.825253	36.431318	76.610740
60.386773	39.072935	76.615745
59.768265	35.214949	76.620750
58.691182	34.708910	76.625754
58.465288	32.869257	76.630759
57.643754	35.322749	76.635764
57.339576	30.357393	76.640769
56.788917	26.922352	76.645774
55.505480	22.136733	76.650778
54.993202	26.058412	76.655783
54.068870	26.769915	76.660788
53.267814	26.346413	76.665793
52.904619	26.460034	76.670798
52.350962	31.741872	76.675802
51.987537	12.716484	76.680807
51.036962	21.902545	76.685812
50.102827	24.398236	76.690817
49.853184	29.164167	76.695822
48.938637	33.303227	76.700826
48.754404	22.677310	76.705831
47.666076	20.785800	76.710836
46.793486	26.551367	76.715841
46.544090	15.932679	76.720846
45.963279	19.894921	76.725850
45.158621	18.916288	76.730855
44.271219	25.418553	76.735860
43.806816	22.989838	76.740865
43.748443	20.723993	76.745870
42.505238	27.977608	76.750874
41.764582	23.664551	76.755879
41.201657	29.304795	76.760884
40.329981	28.943136	76.765889
39.406272	20.206384	76.770894
38.794129	28.545797	76.775898
38.650306	31.150315	76.780903
37.716631	20.593293	76.785908
37.380428	31.298648	76.790913
36.508253	29.805839	76.795918
35.507495	28.577823	76.800922
35.240960	21.589450	76.805927
34.956769	28.574832	76.810932
34.023689	17.465908	76.815937
33.401039	28.975847	76.820942
32.746714	39.921265	76.825946
32.291736	22.622633	76.830951
31.094617	24.390181	76.835956
30.568895	32.819378	76.840961
30.063637	25.260529	76.845966
28.820955	26.122928	76.850970
28.530748	16.042125	76.855975
27.768445	27.051044	76.860980
27.530213	27.993050	76.865985
26.778665	23.670417	76.870990
25.636027	28.568142	76.875994
25.235714	10.894257	76.880999
24.625207	17.791909	76.886004
24.056117	22.318156	76.891009
22.895121	16.083895	76.896014
22.242992	23.762710	76.901018
22.008443	16.580580	76.906023
21.608893	24.919461	76.911028
21.159643	22.947593	76.916033
20.227273	19.185665	76.921038
19.600569	29.567432	76.926042
18.898096	21.221406	76.931047
17.872741	14.612994	76.936052
16.974922	22.418797	76.941057
16.922652	23.060122	76.946062
15.916509	25.054648	76.951066
15.005044	26.399434	76.956071
14.316324	25.036217	76.961076
13.882662	32.059859	76.966081
13.537141	23.411859	76.971086
13.151533	23.752336	76.976090
12.434120	12.529082	76.981095
11.528734	10.441228	76.986100
10.735031	19.946161	76.991105
9.879135	14.761620	76.996110
8.847615	21.091243	77.001114
8.854910	23.162648	77.006119
8.335705	18.627300	77.011124
7.688633	17.451141	77.016129
6.785093	15.160090	77.021134
5.813647	22.811161	77.026139
5.876395	12.735368	77.031143
5.018262	14.170872	77.036148
3.997464	25.061097	77.041153
3.405531	14.154201	77.046158