Fri Mar 05 17:43:40 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.044327	91.159708	0.000000
-0.481322	93.667335	0.005005
-1.174999	54.579247	0.010010
-2.399488	4.256086	0.015014
-6.121886	-30.033948	0.020019
-11.533159	-40.164338	0.025024
-16.536550	-37.032428	0.030029
-21.557637	-27.707901	0.035034
-25.984395	-26.994048	0.040038
-29.911456	-34.249701	0.045043
-33.454446	-31.757583	0.050048
-36.721305	-30.634200	0.055053
-40.334956	-26.553786	0.060058
-43.708070	-33.869395	0.065062
-47.990097	-29.993021	0.070067
-51.314606	-31.963986	0.075072
-55.179805	-34.675048	0.080077
-59.101684	-33.710503	0.085082
-62.994873	-33.009159	0.090086
-67.127680	-34.210887	0.095091
-70.965881	-35.325560	0.100096
-74.284190	-22.456203	0.105101
-78.195440	-46.569414	0.110106
-81.584267	-33.526375	0.115110
-85.634738	-31.984587	0.120115
-89.244538	-36.625601	0.125120
-92.860076	-34.881944	0.130125
-97.036526	-29.995694	0.135130
-100.437733	-35.564137	0.140134
-104.423375	-36.732507	0.145139
-108.119172	-30.738589	0.150144
-111.458175	-24.427837	0.155149
-115.726284	-27.246412	0.160154
-119.339189	-38.221745	0.165158
-123.075991	-28.452201	0.170163
-126.790905	-40.627122	0.175168
-130.757042	-33.273232	0.180173
-134.715857	-44.205959	0.185178
-138.444338	-36.554076	0.190182
-142.105234	-45.132535	0.195187
-145.828277	-39.258802	0.200192
-149.116339	-43.563113	0.205197
-153.375067	-32.940666	0.210202
-157.168297	-40.640094	0.215206
-161.258312	-39.542896	0.220211
-165.008414	-33.617504	0.225216
-168.464801	-27.849364	0.230221
-172.389596	-27.182227	0.235226
-175.567889	-29.733037	0.240230
-179.746612	-32.165199	0.245235
-183.418388	-34.796526	0.250240
-187.205575	-31.910391	0.255245
-191.166932	-27.810543	0.260250
-194.450719	-31.957775	0.265254
-198.495339	-24.189113	0.270259
-202.331182	-23.067750	0.275264
-205.900984	-35.557448	0.280269
-209.701346	-38.742245	0.285274
-213.322185	-33.771001	0.290278
-217.307747	-27.415275	0.295283
-221.240103	-22.900520	0.300288
-225.041485	-28.778669	0.305293
-228.878782	-23.049005	0.310298
-232.129424	-33.006454	0.315302
-236.006580	-25.505742	0.320307
-239.504319	-32.831137	0.325312
-243.284625	-31.776923	0.330317
-247.453383	-26.391735	0.335322
-250.958951	-37.349293	0.340326
-255.018132	-33.113877	0.345331
-258.489818	-25.124318	0.350336
-262.527701	-38.075394	0.355341
-266.471227	-37.901873	0.360346
-270.031804	-33.477926	0.365350
-273.852800	-30.810196	0.370355
-277.634392	-34.895200	0.375360
-281.064761	-34.593822	0.380365
-284.979662	-30.304113	0.385370
-288.707966	-28.726676	0.390374
-292.710525	-25.052189	0.395379
-296.465901	-27.531221	0.400384
-299.854303	-33.613944	0.405389
-304.073947	-29.392258	0.410394
-307.634734	-28.007119	0.415398
-311.268957	-28.105258	0.420403
-315.071125	-33.730809	0.425408
-318.677633	-33.786050	0.430413
-322.771272	-30.598464	0.435418
-326.468395	-35.367102	0.440422
-330.326804	-27.495489	0.445427
-334.113500	-26.274527	0.450432
-337.577856	-32.346647	0.455437
-341.373310	-17.536759	0.460442
-344.983065	-33.653286	0.465446
-348.854181	-30.234667	0.470451
-352.691990	-31.719549	0.475456
-356.742438	-35.927087	0.480461
-360.527007	-24.498445	0.485466
-363.804298	-38.170031	0.490470
-367.668855	-25.444924	0.495475
-371.379357	-31.313685	0.500480
-375.074377	-29.817127	0.505485
-379.295249	-22.499446	0.510490
-382.644141	-34.896390	0.515494
-386.640662	-27.415816	0.520499
-390.253643	-29.379674	0.525504
-394.011201	-27.970876	0.530509
-397.993040	-28.718303	0.535514
-401.706725	-32.131104	0.540518
-405.576611	-28.021862	0.545523
-409.363863	-31.225779	0.550528
-412.799247	-36.466594	0.555533
-416.847695	-33.508425	0.560538
-420.352368	-31.553319	0.565542
-424.117380	-23.661781	0.570547
-427.960263	-31.256637	0.575552
-431.834150	-33.386934	0.580557
-435.430779	-27.572378	0.585562
-439.158275	-26.825922	0.590566
-442.822770	-28.205866	0.595571
-446.762982	-32.142260	0.600576
-450.565249	-32.839424	0.605581
-454.596013	-29.150707	0.610586
-458.297822	-32.167909	0.615590
-461.808062	-27.436321	0.620595
-465.405648	-36.073261	0.625600
-469.312007	-35.107377	0.630605
-473.143051	-29.193828	0.635610
-476.575431	-31.522298	0.640614
-480.736954	-29.474821	0.645619
-484.747921	-27.399340	0.650624
-488.062852	-34.425528	0.655629
-492.067220	-33.428184	0.660634
-495.389161	-38.125579	0.665638
-499.304891	-31.394193	0.670643
-503.124295	-39.323838	0.675648
-506.854302	-42.850561	0.680653
-511.109150	-26.576150	0.685658
-514.544518	-33.877964	0.690662
-518.120016	-30.876889	0.695667
-522.232940	-37.960081	0.700672
-525.573423	-37.890337	0.705677
-529.977060	-35.360966	0.710682
-533.297187	-33.980818	0.715686
-536.970422	-32.780814	0.720691
-540.809907	-35.545651	0.725696
-544.366972	-34.873565	0.730701
-548.002544	-29.019510	0.735706
-552.067484	-39.996052	0.740710
-556.123030	-36.839393	0.745715
-559.537181	-37.729269	0.750720
-563.453400	-38.338661	0.755725
-567.292702	-31.614646	0.760730
-571.370417	-34.559004	0.765734
-574.659215	-23.926782	0.770739
-578.392857	-37.184510	0.775744
-582.144386	-29.298047	0.780749
-586.427223	-30.545873	0.785754
-589.662501	-34.299734	0.790758
-593.256351	-32.178740	0.795763
-597.055287	-31.396971	0.800768
-600.582185	-30.007352	0.805773
-604.766667	-34.874312	0.810778
-608.797974	-27.982358	0.815782
-612.391476	-31.701038	0.820787
-616.081843	-34.188366	0.825792
-619.564418	-31.832789	0.830797
-623.580232	-24.454414	0.835802
-627.405172	-35.555900	0.840806
-631.176242	-30.178409	0.845811
-635.237136	-32.287955	0.850816
-638.666476	-29.021462	0.855821
-642.597951	-34.696776	0.860826
-646.102109	-41.391288	0.865830
-649.752235	-26.276172	0.870835
-653.330312	-34.498021	0.875840
-657.108652	-40.208814	0.880845
-661.120261	-32.531424	0.885850
-664.968083	-41.534923	0.890854
-669.135002	-30.678699	0.895859
-672.864829	-29.647646	0.900864
-676.132136	-36.644894	0.905869
-680.323292	-33.792798	0.910874
-683.815575	-39.788959	0.915878
-687.555718	-34.715955	0.920883
-691.722808	-33.504613	0.925888
-695.023399	-34.612718	0.930893
-698.895413	-34.781082	0.935898
-702.053445	-43.626650	0.940902
-706.383405	-35.934588	0.945907
-710.099621	-46.547078	0.950912
-713.742919	-42.699072	0.955917
-717.789740	-26.700430	0.960922
-721.413245	-35.386434	0.965926
-725.259696	-33.937681	0.970931
-728.844560	-37.245961	0.975936
-732.537224	-26.290371	0.980941
-736.960499	-30.986462	0.985946
-740.367208	-34.657520	0.990950
-744.075364	-19.294867	0.995955
-747.630719	-27.379847	1.000960
-750.898773	-34.023619	1.005965
-755.163351	-31.180159	1.010970
-758.663916	-30.095723	1.015974
-762.638315	-23.856030	1.020979
-766.340152	-25.653715	1.025984
-770.543395	-29.367742	1.030989
-774.563684	-23.958082	1.035994
-778.238795	-30.267091	1.040998
-781.798042	-23.678968	1.046003
-785.314492	-27.988454	1.051008
-788.704372	-29.531602	1.056013
-793.012954	-27.791250	1.061018
-796.718498	-34.863362	1.066022
-800.389237	-28.493944	1.071027
-804.316661	-30.342246	1.076032
-807.592406	-28.025764	1.081037
-811.456404	-24.181756	1.086042
-815.056154	-29.387811	1.091046
-819.529652	-29.444063	1.096051
-823.222529	-26.430082	1.101056
-826.786382	-35.410887	1.106061
-830.407853	-30.271475	1.111066
-834.072857	-29.903410	1.116070
-838.181034	-23.957609	1.121075
-841.958576	-28.718873	1.126080
-845.374173	-31.789095	1.131085
-849.592246	-28.643808	1.136090
-853.106253	-31.379733	1.141094
-857.101184	-23.797732	1.146099
-860.500576	-26.367459	1.151104
-863.882096	-31.441161	1.156109
-867.889830	-30.830590	1.161114
-871.640163	-37.606037	1.166118
-875.739928	-31.577152	1.171123
-879.670430	-28.911461	1.176128
-883.239774	-34.506266	1.181133
-887.194786	-21.230532	1.186138
-890.643627	-29.508935	1.191142
-894.065490	-25.992533	1.196147
-898.329319	-26.812307	1.201152
-902.295926	-30.682989	1.206157
-906.138731	-19.180364	1.211162
-909.170751	-26.743189	1.216166
-913.356702	-10.439703	1.221171
-916.946281	-26.690170	1.226176
-920.522967	-28.124408	1.231181
-924.698035	-19.195910	1.236186
-928.458563	-34.852872	1.241190
-931.944492	-27.981359	1.246195
-935.987819	-27.587338	1.251200
-939.653313	-32.863109	1.256205
-943.325001	-27.371713	1.261210
-946.753291	-26.623418	1.266214
-950.679522	-24.661635	1.271219
-954.515416	-31.185926	1.276224
-958.091424	-36.926996	1.281229
-962.254361	-34.742835	1.286234
-966.007593	-31.682714	1.291238
-969.546233	-32.507931	1.296243
-973.305126	-26.647721	1.301248
-977.198761	-33.765153	1.306253
-981.130306	-34.532252	1.311258
-985.119085	-33.845663	1.316262
-988.659525	-26.252549	1.321267
-992.667590	-28.943947	1.326272
-995.890569	-28.439731	1.331277
-999.968605	-22.411743	1.336282
-1003.371627	-28.336531	1.341286
-1007.257834	-29.438853	1.346291
-1010.868342	-27.029131	1.351296
-1014.519680	-27.281153	1.356301
-1018.733448	-20.936528	1.361306
-1022.230061	-35.614423	1.366310
-1026.034215	-28.368599	1.371315
-1029.851067	-27.337259	1.376320
-1033.563564	-29.273165	1.381325
-1037.636694	-28.841086	1.386330
-1041.330141	-30.012028	1.391334
-1045.211587	-26.800385	1.396339
-1048.770660	-26.254957	1.401344
-1052.527882	-34.009104	1.406349
-1056.182354	-20.370372	1.411354
-1059.739438	-33.351147	1.416358
-1063.778102	-26.525083	1.421363
-1067.414205	-25.587250	1.426368
-1070.976829	-24.814133	1.431373
-1075.251679	-26.759374	1.436378
-1078.792088	-28.814199	1.441382
-1082.071594	-29.601845	1.446387
-1085.932541	-26.279870	1.451392
-1089.916048	-33.453694	1.456397
-1094.134890	-31.471676	1.461402
-1097.604259	-37.912420	1.466406
-1101.984794	-28.368062	1.471411
-1105.309320	-28.323705	1.476416
-1108.676056	-36.143374	1.481421
-1112.722376	-29.981498	1.486426
-1116.330341	-26.859220	1.491430
-1120.099002	-28.861698	1.496435
-1123.977582	-31.202985	1.501440
-1127.406684	-36.442147	1.506445
-1131.730802	-36.433387	1.511450
-1134.970860	-32.721795	1.516454
-1138.808426	-30.672957	1.521459
-1142.732612	-25.218137	1.526464
-1146.130634	-34.103525	1.531469
-1150.431833	-31.274001	1.536474
-1154.286970	-36.020749	1.541478
-1157.802497	-27.306983	1.546483
-1161.681415	-32.251771	1.551488
-1164.958940	-35.209560	1.556493
-1169.052502	-30.303203	1.561498
-1172.702845	-38.537880	1.566502
-1176.561296	-34.790371	1.571507
-1180.246949	-31.852692	1.576512
-1184.172663	-36.752105	1.581517
-1188.128151	-29.259460	1.586522
-1191.439411	-38.556059	1.591526
-1195.154176	-38.375014	1.596531
-1198.906561	-35.868187	1.601536
-1202.690187	-35.818042	1.606541
-1206.989937	-29.815735	1.611546
-1210.869382	-41.407378	1.616550
-1214.345408	-38.971557	1.621555
-1218.162538	-32.537088	1.626560
-1221.613142	-36.635652	1.631565
-1225.631290	-31.105738	1.636570
-1229.038976	-26.819977	1.641574
-1232.920498	-37.882958	1.646579
-1236.639748	-35.138516	1.651584
-1240.177993	-42.119961	1.656589
-1244.292025	-28.068374	1.661594
-1248.332634	-30.042891	1.666598
-1252.021380	-27.754326	1.671603
-1255.543607	-29.111603	1.676608
-1258.993162	-39.329008	1.681613
-1263.052014	-31.214136	1.686618
-1266.767472	-38.950944	1.691622
-1270.541997	-37.408733	1.696627
-1274.454525	-29.989058	1.701632
-1277.965737	-33.683588	1.706637
-1281.845144	-31.036448	1.711642
-1285.524522	-40.228254	1.716646
-1289.225550	-40.807791	1.721651
-1293.123534	-35.057295	1.726656
-1297.245823	-36.305852	1.731661
-1301.067429	-24.136590	1.736666
-1304.195226	-37.786494	1.741670
-1307.984427	-30.561549	1.746675
-1311.783004	-33.306417	1.751680
-1315.497021	-31.291258	1.756685
-1319.898886	-21.760441	1.761690
-1323.476594	-40.857774	1.766694
-1327.380748	-29.011162	1.771699
-1330.810215	-32.572035	1.776704
-1334.144430	-33.014666	1.781709
-1338.393531	-38.491264	1.786714
-1342.165992	-31.931283	1.791718
-1345.995452	-32.562712	1.796723
-1349.755235	-29.042031	1.801728
-1353.176727	-37.667863	1.806733
-1356.967409	-22.297443	1.811738
-1360.532482	-32.149261	1.816742
-1364.817200	-32.195261	1.821747
-1368.709057	-29.722608	1.826752
-1372.041257	-38.985614	1.831757
-1375.953364	-33.478733	1.836762
-1379.330309	-33.061306	1.841766
-1383.427270	-35.518584	1.846771
-1387.350926	-32.657601	1.851776
-1390.914045	-29.548393	1.856781
-1394.684594	-28.347247	1.861786
-1398.300195	-37.872357	1.866790
-1402.282817	-41.074897	1.871795
-1406.481894	-39.742048	1.876800
-1409.790744	-29.320016	1.881805
-1413.461173	-30.530317	1.886810
-1416.912771	-32.248744	1.891814
-1420.629601	-40.691562	1.896819
-1424.719586	-35.843690	1.901824
-1428.322402	-43.951502	1.906829
-1432.457193	-29.216605	1.911834
-1436.139670	-36.702936	1.916838
-1440.045546	-33.937754	1.921843
-1443.858844	-30.171807	1.926848
-1447.432926	-39.623055	1.931853
-1451.372065	-38.216624	1.936858
-1454.976697	-39.968837	1.941862
-1458.582678	-38.301918	1.946867
-1462.841447	-32.419258	1.951872
-1465.964235	-42.625571	1.956877
-1469.528840	-36.284758	1.961882
-1473.308245	-39.942345	1.966886
-1477.291509	-30.017797	1.971891
-1481.393059	-24.276974	1.976896
-1485.044266	-29.521023	1.981901
-1489.114839	-28.989211	1.986906
-1492.525724	-38.144811	1.991910
-1496.071786	-35.645317	1.996915
-1499.993625	-33.873930	2.006912
-1501.265708	-32.803672	2.016909
-1498.898934	-34.635691	2.026906
-1495.713178	-36.856233	2.036902
-1493.719003	-35.168975	2.046899
-1491.774485	-32.453725	2.056896
-1489.995892	-26.629678	2.066893
-1488.088005	-27.974504	2.076890
-1485.883374	-29.668436	2.086886
-1484.357382	-34.212757	2.096883
-1482.451787	-31.953915	2.106880
-1480.293579	-34.987302	2.116877
-1478.451681	-35.953643	2.126874
-1476.772661	-27.505121	2.136870
-1474.561121	-33.273990	2.146867
-1472.686727	-33.430763	2.156864
-1470.994950	-34.452011	2.166861
-1469.216833	-39.628820	2.176858
-1467.414416	-36.535518	2.186854
-1464.948029	-36.115998	2.196851
-1463.146838	-28.636010	2.206848
-1461.630581	-41.141695	2.216845
-1459.627453	-38.792658	2.226842
-1457.724956	-41.001891	2.236838
-1455.551481	-44.596666	2.246835
-1453.558056	-40.791805	2.256832
-1452.408641	-40.406148	2.266829
-1450.397793	-36.131949	2.276826
-1448.202197	-37.732816	2.286822
-1446.052570	-40.256356	2.296819
-1444.421183	-41.779514	2.306816
-1442.620776	-37.528458	2.316813
-1441.100884	-28.370717	2.326810
-1439.143466	-30.549255	2.336806
-1436.985222	-32.494672	2.346803
-1434.927586	-39.055209	2.356800
-1433.289476	-38.362508	2.366797
-1431.427391	-44.500137	2.376794
-1429.382246	-34.430135	2.386790
-1427.375899	-41.040877	2.396787
-1425.646015	-41.616596	2.406784
-1423.825859	-40.078265	2.416781
-1421.948266	-37.827521	2.426778
-1420.329232	-38.424964	2.436774
-1418.346426	-40.814398	2.446771
-1416.219849	-41.734686	2.456768
-1414.240042	-41.917761	2.466765
-1412.623488	-38.603599	2.476762
-1410.704395	-38.067977	2.486758
-1408.608590	-40.893931	2.496755
-1407.160527	-39.213906	2.506752
-1405.092509	-43.701262	2.516749
-1403.213199	-38.750673	2.526746
-1401.180098	-38.962797	2.536742
-1399.029952	-34.947702	2.546739
-1397.178544	-35.092838	2.556736
-1396.028532	-39.692179	2.566733
-1394.201386	-32.247869	2.576730
-1392.017459	-32.937306	2.586726
-1389.675215	-37.083273	2.596723
-1388.035238	-37.095076	2.606720
-1386.065727	-39.272347	2.616717
-1384.349334	-34.374610	2.626714
-1382.345910	-36.672574	2.636710
-1380.697591	-38.211031	2.646707
-1378.700509	-49.088308	2.656704
-1376.656620	-39.450703	2.666701
-1374.899904	-35.745249	2.676698
-1373.265819	-35.064493	2.686694
-1371.198266	-40.431255	2.696691
-1369.225774	-40.627332	2.706688
-1367.557075	-44.755458	2.716685
-1365.623703	-41.646720	2.726682
-1363.748111	-32.591654	2.736678
-1361.901172	-33.700822	2.746675
-1359.794924	-40.133284	2.756672
-1358.205524	-34.817287	2.766669
-1356.214278	-36.306406	2.776666
-1354.036068	-45.602071	2.786662
-1352.566222	-39.400058	2.796659
-1350.388539	-38.049955	2.806656
-1348.915362	-38.047663	2.816653
-1346.929581	-43.219728	2.826650
-1344.942759	-35.294074	2.836646
-1343.031740	-42.879528	2.846643
-1341.180038	-39.768749	2.856640
-1339.157738	-40.361209	2.866637
-1337.520415	-38.998814	2.876634
-1335.576432	-43.946275	2.886630
-1333.408490	-37.137540	2.896627
-1331.407616	-42.863083	2.906624
-1330.014371	-45.740729	2.916621
-1327.961914	-45.431656	2.926618
-1326.190202	-40.242716	2.936614
-1324.326242	-45.573692	2.946611
-1322.628633	-43.834078	2.956608
-1320.831295	-42.004631	2.966605
-1318.521932	-38.188634	2.976602
-1316.630037	-41.784006	2.986598
-1314.738106	-44.173019	2.996595
-1312.919842	-43.400115	3.006592
-1311.305709	-38.076990	3.016589
-1309.373046	-41.100964	3.026586
-1307.226071	-42.063892	3.036582
-1305.347092	-40.462245	3.046579
-1303.634029	-38.579821	3.056576
-1301.662385	-41.965305	3.066573
-1299.997912	-44.415800	3.076570
-1298.158597	-36.198062	3.086566
-1296.073568	-38.112683	3.096563
-1294.073885	-38.687273	3.106560
-1292.420814	-41.998078	3.116557
-1290.631167	-35.171386	3.126554
-1288.519247	-41.059937	3.136550
-1286.698880	-42.894294	3.146547
-1285.075696	-43.451254	3.156544
-1282.880998	-42.926474	3.166541
-1281.084953	-38.268780	3.176538
-1278.997322	-40.036954	3.186534
-1277.099969	-42.458385	3.196531
-1275.618046	-43.419063	3.206528
-1273.674055	-39.601390	3.216525
-1271.937586	-40.815969	3.226522
-1269.716890	-37.868398	3.236518
-1267.832825	-40.674553	3.246515
-1265.795524	-39.022418	3.256512
-1264.195796	-37.775536	3.266509
-1262.459360	-38.742198	3.276506
-1260.675827	-37.854743	3.286502
-1258.326463	-44.169702	3.296499
-1256.694395	-41.773734	3.306496
-1254.908106	-42.497306	3.316493
-1252.951556	-41.362785	3.326490
-1251.192431	-41.098283	3.336486
-1249.202708	-36.469978	3.346483
-1247.388971	-34.707835	3.356480
-1245.297269	-35.691862	3.366477
-1243.406646	-34.459936	3.376474
-1241.793764	-40.511756	3.386470
-1239.717519	-36.230459	3.396467
-1237.806639	-37.507662	3.406464
-1236.045486	-36.333962	3.416461
-1234.266266	-31.998812	3.426458
-1232.103879	-32.398851	3.436454
-1230.371396	-32.797992	3.446451
-1228.583574	-35.274493	3.456448
-1226.759097	-35.914151	3.466445
-1225.135525	-37.097998	3.476442
-1223.006262	-34.650507	3.486438
-1221.106353	-39.657146	3.496435
-1219.150889	-31.195804	3.506432
-1217.267581	-37.800903	3.516429
-1215.227034	-34.936560	3.526426
-1213.340342	-31.940223	3.536422
-1211.537335	-31.434807	3.546419
-1209.697779	-32.582149	3.556416
-1207.916184	-36.156631	3.566413
-1206.150807	-34.644096	3.576410
-1204.051330	-34.160849	3.586406
-1201.946052	-36.313900	3.596403
-1200.353689	-31.211424	3.606400
-1198.863649	-32.110192	3.616397
-1196.717966	-35.558178	3.626394
-1194.818278	-35.966677	3.636390
-1192.975512	-39.165656	3.646387
-1191.040031	-37.587166	3.656384
-1188.838630	-41.053533	3.666381
-1187.480980	-32.742836	3.676378
-1185.343302	-34.751051	3.686374
-1183.568941	-39.045966	3.696371
-1181.647409	-38.077892	3.706368
-1179.533734	-45.060886	3.716365
-1177.991463	-36.852359	3.726362
-1176.111761	-38.280845	3.736358
-1173.986211	-37.484361	3.746355
-1172.045667	-38.251498	3.756352
-1170.715681	-36.568219	3.766349
-1168.364419	-38.323209	3.776346
-1166.375214	-39.454984	3.786342
-1164.764587	-40.587769	3.796339
-1162.833843	-43.377625	3.806336
-1161.011396	-39.489877	3.816333
-1159.118153	-32.974922	3.826330
-1157.212321	-38.165626	3.836326
-1155.278652	-47.652536	3.846323
-1153.415208	-36.136815	3.856320
-1151.411760	-41.401554	3.866317
-1150.003393	-37.297543	3.876314
-1148.017649	-37.626610	3.886310
-1145.828886	-33.009526	3.896307
-1144.044451	-33.409019	3.906304
-1142.375411	-37.161244	3.916301
-1140.393548	-38.752894	3.926298
-1138.375116	-33.442209	3.936294
-1136.675891	-32.762230	3.946291
-1134.631064	-36.833527	3.956288
-1132.710484	-35.729464	3.966285
-1131.095947	-40.911443	3.976282
-1129.131530	-41.439196	3.986278
-1126.936459	-44.658167	3.996275
-1125.231528	-45.062296	4.006272
-1123.786031	-38.166197	4.016269
-1121.783077	-40.744932	4.026266
-1119.785230	-36.758887	4.036262
-1117.689401	-37.103960	4.046259
-1115.888625	-32.353723	4.056256
-1114.299793	-39.776937	4.066253
-1112.094957	-34.199192	4.076250
-1110.291606	-28.345630	4.086246
-1108.357708	-34.644519	4.096243
-1106.310853	-32.543749	4.106240
-1104.752840	-32.164855	4.116237
-1102.709098	-26.479219	4.126234
-1100.901647	-25.410719	4.136230
-1099.199003	-31.584185	4.146227
-1097.311224	-30.029563	4.156224
-1095.252406	-39.675407	4.166221
-1093.287235	-38.052633	4.176218
-1091.835600	-38.676758	4.186214
-1089.655411	-35.458832	4.196211
-1087.581431	-39.800027	4.206208
-1085.832595	-42.410717	4.216205
-1084.141504	-36.877088	4.226202
-1082.054253	-37.981841	4.236198
-1080.376319	-38.086344	4.246195
-1078.536631	-34.078121	4.256192
-1076.224399	-44.923479	4.266189
-1074.342199	-38.057722	4.276186
-1073.064980	-34.246907	4.286182
-1071.104588	-35.852434	4.296179
-1069.112102	-39.621607	4.306176
-1067.127886	-39.364546	4.316173
-1065.173995	-45.636594	4.326170
-1063.447745	-41.649692	4.336166
-1061.511388	-42.035526	4.346163
-1059.441851	-40.164142	4.356160
-1058.135193	-45.304723	4.366157
-1055.927872	-37.112473	4.376154
-1053.793034	-39.977519	4.386150
-1052.061383	-37.829444	4.396147
-1050.175347	-35.004977	4.406144
-1048.275403	-43.437951	4.416141
-1046.951478	-36.691308	4.426138
-1045.041688	-31.870023	4.436134
-1042.606538	-37.437417	4.446131
-1040.787562	-41.527777	4.456128
-1039.099797	-38.589482	4.466125
-1037.075188	-38.949934	4.476122
-1035.231470	-36.423437	4.486118
-1033.278065	-38.768374	4.496115
-1031.628106	-40.707920	4.506112
-1029.565537	-40.974959	4.516109
-1027.556395	-42.106648	4.526106
-1025.728018	-35.674363	4.536102
-1024.001996	-40.297763	4.546099
-1022.312615	-39.466120	4.556096
-1020.234278	-43.842691	4.566093
-1018.527819	-41.928993	4.576090
-1016.414270	-39.685645	4.586086
-1014.704558	-35.290251	4.596083
-1012.843945	-38.313519	4.606080
-1010.851944	-36.287579	4.616077
-1008.851994	-37.705162	4.626074
-1007.169759	-34.293831	4.636070
-1005.452319	-36.529954	4.646067
-1003.179983	-37.452649	4.656064
-1001.312563	-37.088429	4.666061
-999.675002	-34.277869	4.676058
-997.605892	-39.996690	4.686054
-996.014699	-37.744001	4.696051
-994.231299	-39.469588	4.706048
-992.003479	-37.415024	4.716045
-990.363005	-46.168056	4.726042
-988.349071	-40.169644	4.736038
-986.430917	-38.119241	4.746035
-984.590687	-42.629818	4.756032
-982.682971	-39.344532	4.766029
-981.026208	-39.592426	4.776026
-978.889619	-33.413870	4.786022
-977.228328	-40.446729	4.796019
-975.224948	-37.697809	4.806016
-972.940510	-39.020323	4.816013
-971.411522	-37.395592	4.826010
-969.594121	-36.323843	4.836006
-967.923097	-34.692610	4.846003
-965.724381	-39.182338	4.856000
-963.979734	-35.333304	4.865997
-962.180067	-37.791763	4.875994
-959.952717	-34.169919	4.885990
-958.385136	-36.989176	4.895987
-956.543899	-39.963512	4.905984
-954.683206	-41.810380	4.915981
-952.839026	-32.046465	4.925978
-950.610482	-39.765303	4.935974
-948.848290	-34.062138	4.945971
-947.080314	-37.084755	4.955968
-945.414936	-35.006530	4.965965
-943.520007	-38.349457	4.975962
-941.426380	-34.586996	4.985958
-939.402451	-41.327274	4.995955
-937.710022	-36.064545	5.005952
-935.682849	-39.070174	5.015949
-934.024142	-36.439798	5.025946
-932.136314	-31.210674	5.035942
-930.095977	-29.571354	5.045939
-928.318119	-31.273901	5.055936
-926.605212	-28.688501	5.065933
-924.410844	-32.840378	5.075930
-922.627334	-30.757339	5.085926
-920.508628	-29.005799	5.095923
-919.235914	-29.457520	5.105920
-917.294643	-36.385891	5.115917
-915.033895	-30.804254	5.125914
-913.526273	-31.211421	5.135910
-911.425303	-28.039078	5.145907
-909.521702	-33.966640	5.155904
-907.548582	-30.219618	5.165901
-905.714993	-35.163308	5.175898
-904.008451	-28.585115	5.185894
-902.154003	-28.364011	5.195891
-899.902860	-38.398891	5.205888
-898.255538	-32.483889	5.215885
-896.349131	-33.804314	5.225882
-894.552309	-26.828423	5.235878
-892.773695	-31.368561	5.245875
-890.797885	-37.418183	5.255872
-888.801102	-37.278248	5.265869
-886.984376	-35.833678	5.275866
-885.239503	-34.350776	5.285862
-883.427498	-31.792240	5.295859
-881.130801	-38.172642	5.305856
-879.455232	-31.872124	5.315853
-877.695130	-32.509115	5.325850
-875.562358	-31.358230	5.335846
-874.112671	-30.131300	5.345843
-871.923631	-32.177446	5.355840
-870.107308	-27.309484	5.365837
-868.130149	-31.199209	5.375834
-866.485520	-31.588773	5.385830
-864.651437	-36.384084	5.395827
-862.723931	-34.650875	5.405824
-860.826662	-33.552333	5.415821
-858.674235	-34.834685	5.425818
-856.947033	-36.574872	5.435814
-855.051910	-35.764943	5.445811
-853.485047	-37.978465	5.455808
-851.398116	-38.945589	5.465805
-849.532033	-38.058379	5.475802
-847.546825	-41.423558	5.485798
-845.787149	-35.851755	5.495795
-843.894871	-34.149216	5.505792
-841.959582	-37.612206	5.515789
-840.067828	-36.252228	5.525786
-838.601981	-34.423094	5.535782
-836.197091	-33.410414	5.545779
-834.456571	-31.615710	5.555776
-832.762464	-34.111676	5.565773
-830.557421	-37.298816	5.575770
-828.750985	-37.357360	5.585766
-827.087410	-36.311439	5.595763
-825.097311	-39.213151	5.605760
-823.349219	-37.647029	5.615757
-821.645789	-36.910646	5.625754
-819.324241	-35.196174	5.635750
-817.396941	-40.675854	5.645747
-815.803584	-39.492379	5.655744
-813.978542	-38.050660	5.665741
-812.130012	-37.886962	5.675738
-810.191029	-36.425556	5.685734
-808.027219	-36.520680	5.695731
-806.181647	-43.984746	5.705728
-804.508517	-32.487228	5.715725
-802.647537	-36.290432	5.725722
-800.648317	-31.625340	5.735718
-798.974468	-34.571224	5.745715
-796.670663	-33.501291	5.755712
-794.907515	-37.017260	5.765709
-793.501349	-35.781744	5.775706
-791.071806	-35.331930	5.785702
-789.519492	-33.895550	5.795699
-787.828875	-38.767352	5.805696
-785.843376	-36.219099	5.815693
-783.702433	-31.647700	5.825690
-782.081190	-35.350989	5.835686
-780.207466	-29.808412	5.845683
-777.964096	-28.476157	5.855680
-776.213419	-33.518613	5.865677
-774.634383	-29.444792	5.875674
-772.678086	-27.640314	5.885670
-770.690862	-34.694348	5.895667
-768.697558	-37.446519	5.905664
-766.808717	-30.022576	5.915661
-764.827317	-36.685655	5.925658
-763.116209	-32.928212	5.935654
-761.472810	-40.418360	5.945651
-759.528620	-39.554614	5.955648
-757.708457	-38.069437	5.965645
-755.728125	-42.900672	5.975642
-753.466687	-37.678998	5.985638
-751.561726	-34.745195	5.995635
-750.006992	-37.471473	6.005632
-748.276442	-42.052774	6.015629
-746.067923	-38.496397	6.025626
-744.582406	-36.664031	6.035622
-742.790974	-39.083905	6.045619
-740.959594	-37.088905	6.055616
-738.747321	-37.804370	6.065613
-736.916691	-37.032988	6.075610
-734.985648	-34.054389	6.085606
-733.417165	-31.586296	6.095603
-731.304327	-35.761290	6.105600
-729.355651	-37.323610	6.115597
-727.499533	-36.999999	6.125594
-725.499066	-33.661416	6.135590
-723.836704	-31.183054	6.145587
-722.045508	-30.356408	6.155584
-719.970371	-33.464266	6.165581
-718.056006	-29.323985	6.175578
-716.284119	-29.738518	6.185574
-714.494986	-39.099382	6.195571
-712.414570	-34.096644	6.205568
-710.713186	-37.812693	6.215565
-708.653980	-36.105138	6.225562
-707.073805	-32.489367	6.235558
-705.060069	-35.295281	6.245555
-703.099784	-36.692059	6.255552
-701.230251	-37.741161	6.265549
-699.489667	-33.250975	6.275546
-697.698137	-32.411732	6.285542
-695.520070	-32.843783	6.295539
-693.602833	-36.174293	6.305536
-692.025882	-33.518042	6.315533
-690.072938	-38.190107	6.325530
-688.133886	-40.147191	6.335526
-686.421903	-33.705492	6.345523
-684.076805	-36.990672	6.355520
-682.678193	-32.259505	6.365517
-680.935221	-34.679487	6.375514
-678.822661	-34.669983	6.385510
-676.654049	-34.993133	6.395507
-674.774550	-30.953039	6.405504
-672.855562	-30.339415	6.415501
-670.988466	-31.928129	6.425498
-669.565935	-27.687114	6.435494
-668.061607	-29.726308	6.445491
-665.850991	-32.148364	6.455488
-663.656783	-29.257544	6.465485
-661.698808	-33.546690	6.475482
-659.844735	-37.214466	6.485478
-657.943615	-38.600175	6.495475
-656.362254	-34.605593	6.505472
-654.516404	-31.824903	6.515469
-652.320056	-36.785314	6.525466
-650.507091	-31.885055	6.535462
-648.861287	-34.704772	6.545459
-646.791427	-35.375292	6.555456
-645.012535	-37.556238	6.565453
-643.236898	-28.640871	6.575450
-641.368110	-24.785360	6.585446
-639.440674	-33.764045	6.595443
-637.248480	-38.166384	6.605440
-635.429449	-37.232009	6.615437
-633.673482	-36.306505	6.625434
-631.894223	-37.543244	6.635430
-630.323235	-32.051652	6.645427
-628.173338	-32.193338	6.655424
-625.862705	-36.802493	6.665421
-624.372144	-36.816732	6.675418
-622.589692	-39.018758	6.685414
-620.394085	-40.803607	6.695411
-618.836356	-38.300558	6.705408
-617.118127	-36.238432	6.715405
-614.899250	-36.364283	6.725402
-613.121529	-27.521857	6.735398
-610.944843	-31.039023	6.745395
-609.244495	-36.049638	6.755392
-607.364294	-34.026012	6.765389
-605.638563	-32.066133	6.775386
-603.806860	-34.940783	6.785382
-601.976182	-30.092263	6.795379
-599.828113	-30.423114	6.805376
-597.873952	-29.911368	6.815373
-596.342471	-33.811788	6.825370
-594.450056	-29.165765	6.835366
-592.304247	-34.462278	6.845363
-590.494885	-30.172476	6.855360
-588.492118	-30.753277	6.865357
-586.688248	-31.547051	6.875354
-584.852855	-33.473283	6.885350
-583.365750	-32.435314	6.895347
-581.377852	-32.388440	6.905344
-579.262226	-25.957445	6.915341
-577.543675	-28.487142	6.925338
-575.285855	-28.949193	6.935334
-573.530875	-32.638974	6.945331
-571.803884	-33.126758	6.955328
-569.829042	-35.100518	6.965325
-568.134307	-33.236717	6.975322
-566.121873	-35.672817	6.985318
-564.629876	-31.908643	6.995315
-562.779168	-36.941666	7.005312
-560.654266	-37.968288	7.015309
-558.286388	-39.177412	7.025306
-556.746455	-34.321890	7.035302
-554.947645	-39.040286	7.045299
-552.840653	-37.262853	7.055296
-551.477872	-33.713305	7.065293
-549.584836	-32.684889	7.075290
-547.222904	-34.388866	7.085286
-545.496753	-26.934002	7.095283
-543.965705	-32.915476	7.105280
-541.944084	-30.301724	7.115277
-539.616856	-34.405005	7.125274
-537.962737	-39.087646	7.135270
-535.909357	-34.160955	7.145267
-534.414914	-28.664960	7.155264
-532.693811	-32.927224	7.165261
-530.576172	-36.918068	7.175258
-528.773885	-29.176917	7.185254
-526.566431	-36.673328	7.195251
-525.159103	-33.955130	7.205248
-523.130948	-32.207711	7.215245
-521.081341	-35.927143	7.225242
-519.387123	-35.988055	7.235238
-517.386681	-37.503207	7.245235
-515.329705	-33.846607	7.255232
-513.676103	-37.273825	7.265229
-511.727884	-41.725511	7.275226
-509.943392	-32.386690	7.285222
-507.902243	-25.427389	7.295219
-506.423608	-32.292621	7.305216
-503.996238	-31.341612	7.315213
-502.286690	-39.566941	7.325210
-500.501578	-33.422577	7.335206
-498.750988	-32.600328	7.345203
-496.863647	-35.265879	7.355200
-494.988550	-34.062440	7.365197
-492.934884	-37.119306	7.375194
-491.215042	-33.726225	7.385190
-489.221580	-30.139986	7.395187
-487.211522	-30.791344	7.405184
-485.409045	-32.235378	7.415181
-483.685713	-36.431645	7.425178
-481.792549	-35.316348	7.435174
-480.060927	-34.821073	7.445171
-477.931009	-29.112300	7.455168
-475.889549	-31.671389	7.465165
-474.247320	-30.601279	7.475162
-472.337980	-32.922939	7.485158
-470.541972	-30.386784	7.495155
-468.904941	-38.518401	7.505152
-466.500227	-38.989597	7.515149
-464.942932	-40.366038	7.525146
-462.813744	-40.537428	7.535142
-460.996599	-35.460832	7.545139
-459.321194	-36.505588	7.555136
-457.245623	-30.164402	7.565133
-455.452024	-33.479721	7.575130
-453.564475	-34.275705	7.585126
-452.020642	-34.658361	7.595123
-449.762820	-30.566382	7.605120
-447.833451	-32.002230	7.615117
-446.056425	-33.330060	7.625114
-444.671701	-31.855632	7.635110
-442.303757	-32.395146	7.645107
-440.424895	-32.013358	7.655104
-438.502923	-30.623138	7.665101
-436.861069	-30.719843	7.675098
-434.775681	-37.478227	7.685094
-432.903873	-36.062624	7.695091
-430.822336	-28.298083	7.705088
-429.354485	-33.448305	7.715085
-427.423472	-33.231158	7.725082
-425.305883	-32.079016	7.735078
-423.467142	-33.143513	7.745075
-422.031616	-32.160366	7.755072
-419.705854	-30.771446	7.765069
-417.912451	-24.408850	7.775066
-416.052302	-25.830462	7.785062
-414.201391	-30.402336	7.795059
-412.290724	-32.165185	7.805056
-410.377674	-32.584662	7.815053
-408.621908	-32.843227	7.825050
-406.505407	-34.487351	7.835046
-404.936577	-27.692552	7.845043
-402.977005	-28.447889	7.855040
-400.972449	-26.099722	7.865037
-398.952733	-31.941233	7.875034
-397.624313	-30.345676	7.885030
-395.624806	-34.957051	7.895027
-393.304125	-27.608045	7.905024
-391.788355	-29.816274	7.915021
-389.793951	-29.015503	7.925018
-387.861716	-22.389244	7.935014
-386.067644	-23.737122	7.945011
-384.462988	-26.638521	7.955008
-382.077938	-28.096543	7.965005
-380.182538	-29.342167	7.975002
-378.430767	-32.753391	7.984998
-376.722241	-30.782698	7.994995
-374.742610	-29.354261	8.004992
-372.947383	-32.178704	8.014989
-370.963509	-34.633770	8.024986
-369.206163	-26.653191	8.034982
-367.459154	-27.538781	8.044979
-365.277894	-28.027887	8.054976
-363.704722	-29.509436	8.064973
-361.862172	-32.565649	8.074970
-359.637455	-27.519298	8.084966
-357.881692	-27.960993	8.094963
-355.958356	-28.009418	8.104960
-354.183427	-27.936248	8.114957
-352.113602	-26.301127	8.124954
-350.537566	-29.423736	8.134950
-348.793907	-29.765592	8.144947
-346.603506	-20.290889	8.154944
-344.839305	-33.250882	8.164941
-342.894812	-30.667276	8.174938
-340.982176	-28.909151	8.184934
-339.073447	-29.787378	8.194931
-337.431413	-30.705138	8.204928
-335.495672	-31.892427	8.214925
-333.218156	-31.220494	8.224922
-331.629535	-34.635641	8.234918
-329.946023	-29.458651	8.244915
-327.878042	-30.586514	8.254912
-326.116149	-27.380029	8.264909
-324.069203	-26.030193	8.274906
-322.335735	-28.822635	8.284902
-320.296558	-24.210860	8.294899
-318.639675	-23.924599	8.304896
-316.465000	-34.082583	8.314893
-314.582506	-30.298468	8.324890
-312.590428	-29.091451	8.334886
-311.324470	-26.126329	8.344883
-309.332320	-28.639513	8.354880
-307.268364	-29.315114	8.364877
-305.347491	-30.642119	8.374874
-303.484380	-35.337444	8.384870
-301.548606	-32.122379	8.394867
-299.994958	-27.429925	8.404864
-298.008652	-26.970434	8.414861
-295.576091	-26.736919	8.424858
-293.800800	-25.962673	8.434854
-292.069849	-32.932804	8.444851
-290.715856	-32.787659	8.454848
-288.712471	-29.725488	8.464845
-286.491185	-27.411817	8.474842
-284.850401	-29.117278	8.484838
-282.902636	-30.131172	8.494835
-280.874117	-31.784830	8.504832
-279.238001	-33.685341	8.514829
-277.188463	-35.144971	8.524826
-275.234587	-28.038887	8.534822
-273.391592	-34.786876	8.544819
-271.717481	-25.284957	8.554816
-269.781616	-22.720439	8.564813
-267.927139	-27.084345	8.574810
-265.813486	-32.004380	8.584807
-264.082385	-27.577079	8.594803
-262.253157	-27.978322	8.604800
-260.446873	-31.683970	8.614797
-258.474097	-29.477458	8.624794
-256.619068	-29.516479	8.634791
-254.774215	-30.079693	8.644787
-252.733662	-27.176588	8.654784
-250.871593	-32.842813	8.664781
-249.096406	-29.759976	8.674778
-246.981779	-25.858109	8.684775
-245.619680	-24.992615	8.694771
-243.598359	-25.925056	8.704768
-241.278924	-27.321938	8.714765
-239.552466	-22.740710	8.724762
-237.906115	-28.298284	8.734759
-236.126853	-28.663110	8.744755
-234.386673	-25.099385	8.754752
-231.871692	-33.606261	8.764749
-230.017449	-40.488652	8.774746
-228.437786	-37.033525	8.784743
-226.614348	-35.283178	8.794739
-224.822940	-42.750830	8.804736
-223.049341	-39.182959	8.814733
-220.964887	-35.648907	8.824730
-218.681585	-35.790988	8.834727
-217.321746	-37.200500	8.844723
-215.554943	-33.017295	8.854720
-213.343644	-32.127826	8.864717
-211.477495	-33.289700	8.874714
-209.598525	-34.161497	8.884711
-207.787276	-34.447718	8.894707
-206.255904	-38.576845	8.904704
-204.270808	-39.039237	8.914701
-202.378994	-40.768912	8.924698
-200.278835	-40.853326	8.934695
-198.099051	-36.094928	8.944691
-196.266985	-35.707059	8.954688
-194.899779	-38.087259	8.964685
-192.808179	-39.779332	8.974682
-190.866737	-31.592712	8.984679
-188.982250	-29.305733	8.994675
-187.572124	-37.566774	9.004672
-185.284205	-40.130213	9.014669
-183.118948	-35.119996	9.024666
-181.429393	-38.647475	9.034663
-179.555638	-35.883489	9.044659
-178.030828	-35.719747	9.054656
-176.240838	-31.423362	9.064653
-173.994009	-31.698536	9.074650
-172.257315	-31.439121	9.084647
-170.108888	-36.273041	9.094643
-168.274265	-34.244945	9.104640
-166.622809	-33.878762	9.114637
-164.970408	-27.532936	9.124634
-162.736054	-25.835476	9.134631
-160.865788	-28.450678	9.144627
-158.979831	-31.425242	9.154624
-157.042183	-37.640330	9.164621
-155.168462	-31.835103	9.174618
-153.194979	-34.441504	9.184615
-151.615906	-36.064393	9.194611
-149.880649	-38.099065	9.204608
-147.920321	-32.953476	9.214605
-145.705259	-28.652257	9.224602
-144.003685	-31.204210	9.234599
-142.325434	-30.373313	9.244595
-140.430198	-33.470930	9.254592
-138.424975	-30.926844	9.264589
-136.217717	-36.703331	9.274586
-134.491863	-40.176568	9.284583
-132.908325	-33.459713	9.294579
-130.989881	-32.141315	9.304576
-129.230983	-28.976835	9.314573
-127.098728	-35.309799	9.324570
-125.062732	-32.325325	9.334567
-123.406148	-41.364642	9.344563
-121.766866	-33.999797	9.354560
-119.622449	-32.736393	9.364557
-117.640923	-30.722221	9.374554
-116.004132	-34.241240	9.384551
-113.775048	-36.829966	9.394547
-112.265444	-33.387265	9.404544
-110.480056	-36.751558	9.414541
-108.187109	-38.742541	9.424538
-106.382264	-30.892491	9.434535
-104.802600	-28.866301	9.444531
-102.756976	-28.869294	9.454528
-101.063891	-31.252486	9.464525
-98.644468	-26.480115	9.474522
-97.175031	-39.449774	9.484519
-95.650056	-30.697650	9.494515
-93.520159	-28.940826	9.504512
-91.468518	-29.178466	9.514509
-89.622730	-31.320736	9.524506
-87.677465	-37.680680	9.534503
-85.829930	-33.773952	9.544499
-83.906175	-29.614104	9.554496
-82.120010	-31.110506	9.564493
-80.257244	-30.468484	9.574490
-78.570820	-29.706744	9.584487
-76.343932	-28.006433	9.594483
-74.471166	-28.851872	9.604480
-72.715273	-28.601764	9.614477
-70.777319	-32.123008	9.624474
-68.977021	-31.374691	9.634471
-67.285921	-25.167602	9.644467
-65.377638	-30.391045	9.654464
-63.110834	-33.434189	9.664461
-61.467228	-27.784815	9.674458
-59.629273	-30.963238	9.684455
-57.872820	-27.567773	9.694451
-56.114863	-27.648001	9.704448
-53.774545	-33.494595	9.714445
-52.256209	-27.462052	9.724442
-49.837597	-26.253379	9.734439
-48.292245	-25.380687	9.744435
-46.573133	-30.431825	9.754432
-44.863574	-33.288160	9.764429
-42.855846	-34.788297	9.774426
-40.895631	-28.279889	9.784423
-38.881165	-23.891301	9.794419
-37.013557	-25.962798	9.804416
-34.972866	-27.975057	9.814413
-33.478064	-26.587422	9.824410
-31.309399	-34.020388	9.834407
-29.525458	-26.141673	9.844403
-28.020818	-19.863753	9.854400
-25.819984	-22.953188	9.864397
-23.897916	-28.450394	9.874394
-22.005604	-29.456814	9.884391
-20.328533	-30.631016	9.894387
-18.322195	-30.690832	9.904384
-16.436573	-31.291949	9.914381
-14.536295	-31.890664	9.924378
-12.664525	-38.515161	9.934375
-10.609029	-29.137031	9.944371
-9.209679	-31.722796	9.954368
-7.451128	-26.791227	9.964365
-5.536807	-13.987744	9.974362
-4.292739	10.643862	9.984359
-2.811328	55.018320	9.994355
-1.462948	112.542350	10.004352
0.000000	155.110513	10.009357
0.303550	190.594160	10.014362
1.132274	220.061292	10.019367
1.485943	247.265499	10.024371
2.376976	265.983112	10.029376
2.233184	274.430474	10.034381
2.385106	287.495587	10.039386
3.137730	299.438238	10.044391
3.163460	319.191280	10.049395
3.403481	323.011884	10.054400
3.615684	327.160222	10.059405
3.231500	330.809136	10.064410
3.645767	322.789815	10.069415
3.211247	314.137857	10.074419
3.503565	306.377708	10.079424
3.526005	320.045435	10.084429
3.460852	333.578902	10.089434
3.444586	327.165878	10.094439
3.394163	330.681127	10.099443
3.708305	331.678024	10.104448
3.820306	332.656696	10.109453
4.058209	344.608939	10.114458
3.988392	339.377780	10.119463
3.904525	343.133348	10.124467
4.083503	334.888181	10.129472
3.702522	327.530323	10.134477
3.474739	335.303522	10.139482
4.051217	339.833759	10.144487
3.773650	356.612014	10.149491
4.097387	355.372691	10.154496
4.104838	346.237030	10.159501
3.989700	353.088618	10.164506
4.025797	354.673949	10.169511
4.153945	357.018933	10.174515
4.301197	353.792282	10.179520
3.834200	361.130532	10.184525
3.952740	362.041927	10.189530
4.297557	374.377715	10.194535
4.409882	385.936832	10.199539
4.576519	390.242277	10.204544
4.544579	392.814665	10.209549
4.683620	397.108743	10.214554
4.994977	394.948811	10.219559
4.722403	396.778936	10.224563
5.104246	402.221815	10.229568
4.934930	392.751594	10.234573
4.602691	389.035250	10.239578
4.663792	388.408712	10.244583
4.898060	403.411618	10.249587
5.102269	395.074078	10.254592
5.025469	402.881582	10.259597
5.114743	407.543171	10.264602
5.480069	403.572047	10.269607
5.302364	411.731565	10.274611
5.389798	404.420388	10.279616
5.197580	398.898050	10.284621
5.182372	397.031496	10.289626
5.253564	395.876609	10.294631
5.049741	404.246883	10.299635
5.349865	409.267531	10.304640
5.313000	409.462497	10.309645
5.438432	409.775089	10.314650
5.338035	406.591080	10.319655
5.257962	415.667071	10.324659
5.373323	414.016249	10.329664
5.337857	413.321528	10.334669
5.112943	419.204992	10.339674
5.771571	427.207466	10.344679
5.306492	441.473498	10.349683
5.817995	444.823448	10.354688
5.767452	454.670670	10.359693
6.135716	452.400721	10.364698
6.006275	453.857914	10.369703
6.140349	452.148905	10.374707
6.244029	448.515991	10.379712
5.872542	457.515478	10.384717
5.879617	460.021726	10.389722
5.872860	455.190505	10.394727
6.089206	455.528024	10.399731
5.967180	451.902722	10.404736
6.284146	454.780619	10.409741
6.241285	457.908311	10.414746
6.555851	453.352293	10.419751
6.249013	464.038397	10.424755
6.694306	470.532550	10.429760
6.449602	467.032475	10.434765
6.569115	481.235267	10.439770
6.963117	478.104859	10.444775
6.599676	477.370977	10.449779
6.694259	481.372528	10.454784
6.753284	485.122689	10.459789
6.667693	485.336467	10.464794
6.965210	484.471928	10.469799
6.875719	499.206428	10.474803
7.354583	491.742881	10.479808
7.293060	493.622940	10.484813
7.090000	479.920453	10.489818
7.110646	470.473503	10.494823
6.751654	470.379202	10.499827
6.817053	476.774666	10.504832
7.307430	497.381156	10.509837
7.259135	493.980645	10.514842
7.146680	496.763027	10.519847
7.172924	499.747232	10.524851
7.435763	497.301688	10.529856
7.579012	497.683986	10.534861
7.218987	504.073196	10.539866
7.367863	500.850984	10.544871
7.391775	501.217620	10.549875
7.350950	503.720477	10.554880
7.281603	502.693662	10.559885
7.412154	505.095062	10.564890
7.635961	503.972599	10.569895
7.353670	520.515234	10.574899
7.592755	529.458382	10.579904
7.973057	538.479945	10.584909
7.820698	541.446911	10.589914
7.805040	536.571347	10.594919
7.961821	539.823345	10.599923
7.755244	540.057998	10.604928
8.029457	533.912389	10.609933
7.737640	541.516124	10.614938
8.175515	532.194990	10.619943
7.592125	549.796589	10.624947
8.145143	550.536187	10.629952
8.403919	562.860625	10.634957
8.628871	568.617198	10.639962
8.538357	547.995394	10.644967
8.457785	555.365154	10.649971
8.312522	538.966050	10.654976
8.487570	550.217227	10.659981
8.764395	561.027945	10.664986
8.798076	553.976022	10.669991
8.610464	554.996190	10.674995
8.783909	546.534149	10.680000
8.794395	551.252510	10.685005
8.236981	554.096411	10.690010
8.859051	562.158413	10.695015
8.636280	569.705415	10.700019
8.773901	567.546359	10.705024
8.651800	572.640716	10.710029
8.637443	583.015307	10.715034
8.775908	572.197940	10.720039
8.836451	582.260938	10.725043
8.885456	582.743433	10.730048
9.184700	586.650863	10.735053
9.161913	607.337782	10.740058
9.504987	602.655735	10.745063
9.033297	599.854207	10.750067
9.344702	598.869166	10.755072
9.254037	615.378190	10.760077
9.210394	613.539800	10.765082
9.732992	611.174242	10.770087
9.526661	618.412692	10.775091
10.015252	604.837909	10.780096
9.926628	607.182813	10.785101
9.626039	604.697798	10.790106
10.011900	600.385851	10.795111
9.570170	602.624634	10.800115
9.767233	591.592886	10.805120
9.728462	593.444095	10.810125
9.757509	613.094496	10.815130
9.967480	613.259557	10.820135
9.553720	619.865563	10.825139
9.650605	613.000666	10.830144
9.920150	616.393981	10.835149
9.752933	627.106824	10.840154
10.074456	610.792473	10.845159
9.872276	621.583435	10.850163
10.184486	620.610881	10.855168
10.327157	623.103415	10.860173
10.004516	613.433559	10.865178
10.758179	620.181395	10.870183
10.353522	624.062324	10.875187
10.301380	625.259602	10.880192
10.622823	627.521756	10.885197
10.504482	630.606326	10.890202
10.560504	633.989543	10.895207
10.686511	638.359895	10.900211
10.927904	638.895291	10.905216
10.629611	629.235735	10.910221
10.618157	640.133496	10.915226
10.831299	637.957653	10.920231
10.725474	645.451345	10.925235
10.792748	653.929922	10.930240
11.103230	646.967858	10.935245
11.009502	648.433567	10.940250
10.968664	647.264988	10.945255
11.143281	648.102797	10.950259
11.199566	647.398162	10.955264
11.291805	634.042701	10.960269
11.153167	648.196937	10.965274
11.379550	646.872186	10.970279
11.092039	656.550743	10.975283
11.479053	644.348422	10.980288
11.452566	644.808263	10.985293
11.319680	649.016467	10.990298
11.571892	649.154289	10.995303
11.201442	655.329165	11.000307
11.629737	644.549103	11.005312
11.427808	650.033144	11.010317
11.696052	652.944085	11.015322
11.730107	644.094178	11.020327
11.307787	642.748304	11.025331
11.458431	645.465095	11.030336
11.600889	651.974513	11.035341
11.431103	656.734277	11.040346
11.501663	659.003333	11.045351
11.305879	682.242872	11.050355
11.795127	681.214478	11.055360
12.309491	680.268030	11.060365
12.144699	688.532095	11.065370
12.281842	684.643028	11.070375
12.224175	684.367399	11.075379
12.161453	685.601065	11.080384
12.170575	681.315276	11.085389
12.294927	677.123872	11.090394
12.335533	676.801815	11.095399
12.205274	695.481015	11.100403
12.531458	685.647695	11.105408
12.439020	686.387739	11.110413
11.910577	693.289638	11.115418
12.510066	688.845023	11.120423
12.423902	693.612753	11.125427
12.672025	683.955113	11.130432
12.521294	690.597263	11.135437
13.041313	708.152382	11.140442
12.719091	683.074200	11.145447
12.554012	696.693335	11.150451
12.907233	702.483913	11.155456
13.306621	704.754938	11.160461
12.899176	699.315703	11.165466
13.098110	691.608884	11.170471
12.894013	694.224555	11.175475
13.131401	706.983863	11.180480
13.004631	708.074768	11.185485
13.030027	716.036466	11.190490
13.383193	712.070354	11.195495
13.001182	714.842150	11.200499
13.289990	709.972377	11.205504
13.371304	709.482175	11.210509
13.398134	714.041848	11.215514
13.522957	714.058051	11.220519
13.467527	709.163540	11.225523
13.654845	710.445645	11.230528
13.478358	703.211898	11.235533
13.492766	709.369571	11.240538
13.770477	711.473119	11.245543
13.294094	716.989920	11.250547
13.813848	711.577063	11.255552
13.985379	704.795632	11.260557
13.696470	717.813951	11.265562
13.771513	714.522248	11.270567
13.793188	712.130118	11.275571
13.946908	707.730575	11.280576
13.794002	713.974867	11.285581
13.497817	713.413187	11.290586
14.211536	710.593681	11.295591
13.998454	708.366739	11.300595
14.072043	725.732863	11.305600
14.421468	731.129784	11.310605
14.210071	736.191128	11.315610
14.616497	735.186980	11.320615
14.457849	727.985860	11.325619
14.226847	709.853603	11.330624
14.092735	724.528422	11.335629
14.568882	742.134738	11.340634
14.660084	736.505559	11.345639
14.360632	747.042444	11.350643
14.641604	742.979019	11.355648
14.414927	744.127655	11.360653
14.414316	748.437803	11.365658
14.814379	737.390915	11.370663
14.577179	752.022273	11.375667
14.382759	747.354152	11.380672
14.526852	746.469123	11.385677
14.536817	745.827858	11.390682
14.793336	752.980723	11.395687
14.941696	771.466546	11.400691
14.985054	776.817674	11.405696
15.011150	782.488555	11.410701
15.104876	781.647831	11.415706
15.450573	774.244021	11.420711
15.500777	774.144380	11.425715
15.694991	772.364235	11.430720
15.824131	767.073590	11.435725
15.455394	762.022432	11.440730
15.358795	750.612373	11.445735
15.284092	749.082511	11.450739
15.028796	748.074297	11.455744
15.410658	758.457575	11.460749
15.577679	769.583246	11.465754
15.675695	767.163159	11.470759
15.665954	768.084001	11.475763
15.790835	766.786469	11.480768
15.827374	767.707027	11.485773
15.702748	770.466168	11.490778
15.900501	765.785170	11.495783
15.892669	767.503721	11.500787
15.904748	771.038283	11.505792
15.986352	767.650897	11.510797
15.738035	778.209613	11.515802
15.911351	776.107918	11.520807
15.797928	779.116033	11.525811
15.702905	766.547328	11.530816
16.181584	774.174962	11.535821
15.691505	777.054689	11.540826
15.925369	782.861971	11.545831
15.764955	794.326918	11.550835
16.200874	796.621309	11.555840
16.483989	801.620362	11.560845
16.385735	806.248117	11.565850
16.565123	799.868339	11.570855
16.523798	811.736182	11.575859
16.668991	806.729207	11.580864
16.889309	805.996824	11.585869
16.775919	812.644114	11.590874
16.907017	805.619114	11.595879
16.743670	806.764750	11.600883
16.588737	801.312012	11.605888
16.559509	801.002668	11.610893
16.584903	810.199291	11.615898
16.733381	800.213659	11.620903
16.685833	819.050941	11.625907
16.897662	818.878997	11.630912
17.662119	821.636705	11.635917
17.118122	815.165697	11.640922
17.184293	805.637144	11.645927
17.153928	800.898681	11.650931
17.203969	804.737887	11.655936
17.308390	822.140213	11.660941
17.348302	816.720265	11.665946
17.565734	819.133883	11.670951
17.339449	828.291804	11.675955
17.392158	819.475877	11.680960
17.562448	823.193396	11.685965
17.329496	825.229374	11.690970
17.646005	822.691631	11.695975
17.276663	821.010828	11.700979
17.471695	820.456748	11.705984
17.573793	821.694103	11.710989
17.388892	827.200728	11.715994
17.645106	815.141353	11.720999
17.359193	826.068046	11.726003
17.781000	817.767318	11.731008
17.797068	830.022664	11.736013
17.598880	851.968839	11.741018
18.029948	855.472869	11.746023
18.096587	845.235304	11.751027
18.155529	855.271148	11.756032
18.264404	848.703091	11.761037
17.867888	864.817223	11.766042
18.504718	856.739247	11.771047
18.418200	857.115620	11.776051
18.578607	857.355617	11.781056
18.690385	859.922513	11.786061
18.225387	859.233195	11.791066
18.192698	861.705638	11.796071
18.188953	854.771514	11.801075
18.339414	856.548415	11.806080
18.390268	859.154993	11.811085
18.342911	860.478485	11.816090
18.735856	861.466006	11.821095
18.471014	867.529500	11.826099
18.880387	867.001163	11.831104
19.201493	869.807514	11.836109
18.892295	855.727321	11.841114
19.053911	855.366247	11.846119
18.742250	856.090797	11.851123
18.925033	858.106207	11.856128
18.964463	865.719573	11.861133
18.765901	875.928190	11.866138
19.152749	873.853143	11.871143
19.032780	880.624527	11.876147
19.075693	882.961901	11.881152
19.455167	876.067581	11.886157
19.159057	880.294787	11.891162
19.349306	883.299438	11.896167
19.113074	889.070554	11.901171
18.945144	876.241330	11.906176
19.212512	882.963554	11.911181
18.935248	883.241028	11.916186
19.484134	885.394401	11.921191
19.527393	908.121462	11.926195
20.065398	909.542427	11.931200
20.138254	897.268564	11.936205
20.074089	896.992390	11.941210
20.245129	874.973663	11.946215
19.907953	879.905292	11.951219
19.938903	881.914957	11.956224
20.181084	873.901493	11.961229
19.787391	877.118350	11.966234
20.021869	868.472907	11.971239
19.923294	880.965799	11.976243
19.938135	872.935763	11.981248
20.190535	874.043483	11.986253
19.865707	879.951741	11.991258
20.215804	870.821030	11.996263
20.069088	892.281191	12.001267
20.394932	892.833883	12.006272
20.746968	906.604150	12.011277
20.138471	895.729043	12.016282
20.641410	876.468586	12.021287
20.316108	875.711249	12.026291
20.169566	883.373211	12.031296
20.446605	875.446448	12.036301
20.183851	878.340404	12.041306
20.245044	878.817022	12.046311
20.279857	892.196278	12.051315
20.652336	898.367892	12.056320
20.888297	887.477965	12.061325
20.328430	887.806820	12.066330
20.778871	874.274147	12.071335
20.587956	883.964258	12.076339
20.741012	881.813734	12.081344
20.483266	873.428163	12.086349
20.710725	876.648462	12.091354
20.685639	870.063123	12.096359
20.425444	872.769782	12.101363
20.445185	864.697174	12.106368
20.506291	845.621569	12.111373
20.243271	846.457432	12.116378
20.329929	845.257462	12.121383
20.000565	845.735652	12.126387
20.427604	860.276159	12.131392
20.409474	865.294893	12.136397
20.221824	855.276882	12.141402
20.337274	847.360135	12.146407
20.158283	857.439450	12.151411
20.302958	872.905822	12.156416
20.255958	868.766138	12.161421
20.179621	883.241070	12.166426
20.436213	876.768513	12.171431
20.284136	878.054298	12.176435
20.086536	884.341275	12.181440
20.372492	885.048577	12.186445
20.474459	880.337872	12.191450
20.413637	877.456561	12.196455
20.545914	883.413352	12.201459
20.454589	883.688769	12.206464
20.783159	878.883569	12.211469
20.406730	873.162536	12.216474
20.413450	854.062474	12.221479
20.302516	861.905633	12.226483
20.168545	849.290235	12.231488
20.502077	855.419940	12.236493
20.093992	853.374691	12.241498
20.087830	858.714822	12.246503
20.418815	878.542953	12.251507
20.588773	876.618416	12.256512
20.661469	869.508073	12.261517
20.381378	865.452092	12.266522
20.558625	852.483459	12.271527
20.688025	856.648312	12.276531
20.628420	855.614398	12.281536
20.719284	850.502521	12.286541
20.511634	857.252394	12.291546
20.606010	846.821151	12.296551
20.491667	851.216497	12.301555
20.628495	847.817918	12.306560
20.731438	851.470485	12.311565
20.452446	839.597388	12.316570
20.113364	821.582375	12.321575
20.163144	830.738848	12.326579
20.059584	842.171898	12.331584
20.299575	854.699875	12.336589
20.435074	852.084543	12.341594
20.425006	844.888843	12.346599
20.428410	860.338306	12.351603
20.303242	851.609871	12.356608
20.596560	849.775272	12.361613
19.850493	846.808487	12.366618
20.044060	844.788717	12.371623
20.541763	854.375285	12.376627
20.149895	857.285098	12.381632
20.523841	857.541505	12.386637
20.471765	863.552925	12.391642
20.484427	857.594781	12.396647
20.525631	857.601453	12.401651
20.450313	853.309368	12.406656
20.322822	840.718177	12.411661
20.203230	841.994046	12.416666
20.050771	845.089622	12.421671
20.464980	856.926640	12.426675
20.098641	855.603358	12.431680
20.061906	853.133779	12.436685
20.275154	854.512697	12.441690
20.553156	859.889516	12.446695
20.350924	865.812123	12.451699
20.514045	868.094837	12.456704
20.927362	859.141726	12.461709
20.673011	855.453052	12.466714
20.089292	839.021816	12.471719
20.184142	845.094170	12.476723
20.130589	854.574677	12.481728
20.486123	858.123086	12.486733
20.498680	867.086803	12.491738
20.618569	848.754889	12.496743
19.991728	834.916997	12.501747
19.932244	843.541284	12.506752
20.466975	852.386223	12.511757
20.277999	859.139428	12.516762
20.459363	858.384868	12.521767
20.392502	869.574730	12.526771
20.524863	870.483954	12.531776
20.736843	863.942027	12.536781
20.283224	848.460743	12.541786
20.487391	831.610510	12.546791
20.599801	836.913585	12.551795
20.225417	839.167683	12.556800
20.447604	830.692973	12.561805
19.947666	838.643112	12.566810
20.278443	834.181384	12.571815
20.338543	831.392771	12.576819
20.295767	828.234175	12.581824
20.195249	828.907699	12.586829
19.946631	850.981777	12.591834
20.469390	847.210165	12.596839
20.399832	866.176400	12.601843
20.596510	870.516625	12.606848
20.688515	861.215751	12.611853
20.640956	844.389881	12.616858
20.545717	837.063463	12.621863
20.490664	843.893870	12.626867
20.468434	839.131228	12.631872
20.526097	831.424000	12.636877
20.206400	838.167290	12.641882
20.115500	830.418308	12.646887
20.411418	844.327578	12.651891
20.600196	847.105352	12.656896
20.387139	836.211377	12.661901
20.524919	835.061608	12.666906
20.756443	833.354361	12.671911
20.282743	844.608304	12.676915
20.435485	835.550885	12.681920
20.631571	832.175189	12.686925
20.532139	842.274134	12.691930
20.559122	835.531469	12.696935
20.406299	836.718011	12.701939
20.465461	826.737932	12.706944
20.497203	821.397352	12.711949
20.187971	820.896100	12.716954
20.259252	803.627869	12.721959
20.005642	816.042133	12.726963
20.411062	817.820947	12.731968
20.381679	822.665615	12.736973
20.389666	832.402822	12.741978
20.358683	826.138596	12.746983
20.122333	844.387798	12.751987
20.212888	837.284874	12.756992
20.562575	839.850884	12.761997
20.317247	838.484646	12.767002
20.317895	842.118830	12.772007
20.136196	845.226955	12.777011
20.153587	835.793692	12.782016
20.370162	835.821284	12.787021
20.071868	844.583806	12.792026
20.256880	837.073905	12.797031
20.562793	841.989692	12.802035
20.422200	843.099372	12.807040
20.529476	827.885077	12.812045
20.442931	836.911895	12.817050
20.623368	836.333332	12.822055
20.640895	845.147995	12.827059
20.167652	834.794676	12.832064
20.510456	817.032069	12.837069
20.366306	827.222512	12.842074
20.545833	815.719470	12.847079
20.439638	822.532001	12.852083
20.425236	810.830425	12.857088
20.307903	816.065258	12.862093
20.305806	821.397630	12.867098
20.716196	814.417187	12.872103
20.498472	820.437661	12.877107
20.459662	817.420375	12.882112
20.636557	811.137193	12.887117
20.187882	821.381722	12.892122
20.374610	822.342990	12.897127
20.474552	820.700102	12.902131
20.252004	820.497292	12.907136
20.514025	816.872151	12.912141
20.327409	826.199592	12.917146
20.349550	821.873046	12.922151
20.129252	823.182324	12.927155
20.198301	828.979638	12.932160
20.131021	829.731448	12.937165
19.905945	827.209115	12.942170
20.252385	819.930544	12.947175
19.978044	831.768541	12.952179
20.475258	842.096420	12.957184
20.448880	831.315404	12.962189
20.170630	829.392967	12.967194
20.784078	827.232895	12.972199
20.295559	827.721486	12.977203
20.129246	828.433892	12.982208
20.337705	819.843095	12.987213
20.233887	829.206222	12.992218
20.182043	827.485030	12.997223
20.452152	834.979578	13.002227
20.192771	833.992511	13.007232
20.594669	841.108827	13.012237
20.453518	845.524218	13.017242
20.345810	827.562979	13.022247
20.413591	832.821126	13.027251
20.104496	834.573541	13.032256
20.233870	821.554218	13.037261
20.171469	829.676652	13.042266
20.725863	837.026502	13.047271
20.411095	839.991831	13.052275
20.076564	833.533929	13.057280
20.341426	828.064693	13.062285
20.226280	839.827627	13.067290
20.443988	846.751739	13.072295
20.524327	848.975106	13.077299
20.411255	847.753370	13.082304
20.478271	833.255979	13.087309
20.327208	844.077591	13.092314
20.471154	831.124540	13.097319
20.072754	837.780236	13.102323
20.395857	828.953507	13.107328
20.597696	831.625106	13.112333
20.291195	840.519835	13.117338
20.565230	826.073019	13.122343
20.128639	830.310000	13.127347
20.395321	838.075570	13.132352
20.437612	827.823764	13.137357
20.263503	832.964358	13.142362
20.387570	832.908135	13.147367
20.200235	832.252598	13.152371
20.258098	835.314627	13.157376
20.287393	833.679851	13.162381
20.096383	838.593673	13.167386
20.383716	839.676105	13.172391
20.371805	831.581753	13.177395
20.360179	837.817758	13.182400
20.497273	834.016188	13.187405
20.156642	833.108319	13.192410
19.991594	834.364626	13.197415
20.215890	849.759133	13.202419
20.424372	850.977157	13.207424
20.510735	855.146508	13.212429
20.401567	866.462975	13.217434
20.751312	859.100271	13.222439
20.566662	846.995268	13.227443
20.411869	846.243856	13.232448
20.515270	834.439885	13.237453
20.574509	829.265244	13.242458
20.473372	830.875670	13.247463
20.273504	843.058224	13.252467
20.348981	839.116656	13.257472
20.722075	833.283979	13.262477
20.317811	846.363392	13.267482
20.478382	831.594801	13.272487
20.461645	834.502343	13.277491
20.120258	833.511796	13.282496
20.610886	837.825631	13.287501
20.291188	848.260939	13.292506
20.276355	833.521899	13.297511
19.845886	833.405084	13.302515
20.226639	840.571298	13.307520
20.191061	836.349369	13.312525
20.205539	839.941919	13.317530
20.221995	833.156774	13.322535
20.577613	848.880453	13.327539
20.271447	841.273042	13.332544
20.165701	838.794759	13.337549
20.232703	837.851839	13.342554
20.061497	834.903767	13.347559
20.018775	837.813877	13.352563
20.425432	850.021926	13.357568
20.828702	857.522058	13.362573
20.500099	855.613169	13.367578
20.499806	844.677368	13.372583
20.653864	841.008722	13.377587
20.292681	831.872409	13.382592
20.553274	836.562011	13.387597
20.160996	847.474931	13.392602
20.703457	831.076995	13.397607
20.558914	838.170855	13.402611
20.564473	838.052312	13.407616
20.511439	839.364090	13.412621
20.315633	840.472324	13.417626
20.266046	840.252179	13.422631
20.672272	844.501410	13.427635
20.206812	840.809348	13.432640
20.588268	845.680758	13.437645
20.572938	848.918483	13.442650
20.678586	847.243139	13.447655
20.818521	836.676891	13.452659
20.403186	819.779596	13.457664
20.525440	802.784749	13.462669
19.992542	810.233090	13.467674
20.232362	805.796917	13.472679
20.321645	808.002292	13.477683
20.179214	804.514209	13.482688
20.496379	808.376262	13.487693
20.211533	816.446638	13.492698
20.502680	808.058723	13.497703
20.396867	804.451249	13.502707
20.327149	810.127960	13.507712
20.583501	802.788854	13.512717
20.105866	806.470924	13.517722
20.331107	804.442165	13.522727
20.377752	806.046366	13.527731
20.615568	804.648808	13.532736
20.697635	806.714183	13.537741
20.367174	815.002378	13.542746
20.321410	805.299271	13.547751
20.336791	809.984604	13.552755
20.219490	805.329397	13.557760
20.369506	799.171945	13.562765
20.270913	811.690804	13.567770
20.103716	817.431167	13.572775
20.150054	817.040378	13.577779
20.099992	812.618896	13.582784
20.249841	816.556527	13.587789
20.286061	817.963676	13.592794
20.313104	825.893630	13.597799
20.481748	835.800777	13.602803
20.153993	828.918343	13.607808
20.334802	832.696484	13.612813
20.200551	846.341595	13.617818
20.612088	838.853128	13.622823
20.743325	832.854002	13.627827
20.535121	813.378225	13.632832
20.553058	806.808131	13.637837
20.079215	809.667137	13.642842
20.196509	805.107779	13.647847
20.186469	811.402661	13.652851
20.536642	815.692366	13.657856
20.440356	802.570266	13.662861
20.131955	814.344289	13.667866
20.515354	802.738559	13.672871
20.380791	813.164817	13.677875
20.674487	815.679034	13.682880
20.476780	811.055575	13.687885
20.037297	814.752854	13.692890
20.335079	812.306418	13.697895
20.326889	813.336625	13.702899
20.481778	814.559251	13.707904
20.681364	804.652205	13.712909
20.086320	816.449867	13.717914
20.618309	809.767819	13.722919
20.256341	811.663507	13.727923
20.298931	810.799395	13.732928
20.502833	804.194122	13.737933
19.956212	812.750992	13.742938
20.165021	813.472961	13.747943
20.504332	813.306706	13.752947
19.923724	819.227347	13.757952
20.079173	812.218963	13.762957
19.773119	822.897317	13.767962
20.401016	833.291877	13.772967
20.647680	838.172954	13.777971
20.518325	845.629496	13.782976
20.754840	837.590145	13.787981
20.276272	832.842724	13.792986
20.196636	817.869584	13.797991
20.360999	823.191178	13.802995
19.962636	816.257716	13.808000
20.227642	830.253912	13.813005
20.281678	845.265522	13.818010
20.616836	851.392600	13.823015
20.665283	850.266540	13.828019
20.552314	834.125329	13.833024
20.559280	824.495020	13.838029
20.059035	832.908874	13.843034
20.471568	816.529311	13.848039
20.217285	817.660275	13.853043
20.127919	823.580635	13.858048
20.230321	820.670936	13.863053
20.206315	833.362439	13.868058
20.521675	841.189640	13.873063
20.321358	841.749759	13.878067
20.433739	836.024114	13.883072
20.681991	817.584236	13.888077
20.141824	824.972237	13.893082
20.272855	821.744916	13.898087
20.517512	827.205108	13.903091
20.342997	824.349827	13.908096
20.513162	818.420988	13.913101
20.171073	832.024323	13.918106
20.353198	822.737488	13.923111
20.291535	829.741635	13.928115
20.142547	821.425489	13.933120
20.323224	815.562790	13.938125
20.382012	825.834416	13.943130
20.475724	826.249858	13.948135
20.267322	826.758434	13.953139
19.985748	824.950868	13.958144
20.377110	830.805596	13.963149
20.572311	847.226708	13.968154
20.719220	842.087758	13.973159
20.486467	827.819551	13.978163
20.309452	828.751306	13.983168
20.597368	822.798953	13.988173
20.169035	834.208094	13.993178
20.302736	820.784342	13.998183
20.372102	819.949078	14.003187
20.028525	828.427837	14.008192
20.395828	823.833158	14.013210
20.322715	823.854882	14.018227
20.649901	818.654617	14.023245
20.173765	821.893868	14.028263
20.162086	813.506312	14.033280
20.844330	816.406645	14.038298
20.493480	828.612159	14.043315
20.567063	822.340956	14.048333
20.524125	828.183787	14.053351
20.620659	826.406373	14.058368
20.404468	813.742756	14.063386
20.456594	825.257122	14.068403
20.540931	822.327010	14.073421
20.503368	820.025910	14.078439
20.362658	826.752677	14.083456
20.789774	818.624694	14.088474
20.627435	823.762948	14.093491
20.556794	818.813331	14.098509
20.480564	829.695342	14.103527
20.506326	840.660199	14.108544
20.918284	850.591300	14.113562
20.901858	854.304671	14.118579
21.029087	842.834501	14.123597
20.609659	833.776548	14.128615
20.400914	833.147411	14.133632
20.949097	841.604820	14.138650
20.564352	854.853213	14.143667
20.613031	851.957098	14.148685
20.476873	862.831388	14.153703
20.396410	870.309154	14.158720
20.637568	862.924989	14.163738
20.454405	860.346645	14.168755
20.572472	850.486413	14.173773
20.580411	868.822477	14.178791
20.532968	874.128048	14.183808
21.340328	877.668350	14.188826
21.042498	886.845910	14.193843
21.377937	872.823988	14.198861
21.228707	877.733646	14.203879
21.154391	863.626070	14.208896
21.125022	863.634525	14.213914
21.008229	864.801345	14.218931
21.057854	864.153021	14.223949
20.987016	865.637355	14.228967
20.717953	869.269897	14.233984
21.190314	874.808753	14.239002
21.260007	881.795369	14.244019
21.282102	888.500130	14.249037
21.714750	889.175035	14.254055
21.242246	881.996711	14.259072
21.191798	873.447769	14.264090
21.166717	874.322313	14.269107
21.380446	876.593426	14.274125
21.425985	872.318994	14.279143
21.160151	871.057925	14.284160
21.333704	876.528032	14.289178
21.464074	877.478460	14.294195
21.094576	876.212689	14.299213
21.484188	872.146085	14.304231
21.202603	888.615474	14.309248
21.479053	879.299421	14.314266
21.410081	886.545691	14.319283
21.407563	883.912576	14.324301
21.468386	877.342138	14.329319
20.979262	889.210306	14.334336
21.385155	883.790603	14.339354
21.481199	882.757332	14.344371
21.441253	879.158017	14.349389
21.806907	885.622357	14.354407
21.647912	879.556545	14.359424
21.440056	881.258584	14.364442
21.669230	889.579704	14.369459
21.786273	881.272256	14.374477
21.800174	877.076804	14.379495
21.375173	885.049995	14.384512
21.966394	881.073148	14.389530
21.845547	878.564303	14.394547
21.662820	880.230872	14.399565
21.943603	890.121571	14.404583
21.840233	894.264903	14.409600
21.890684	881.321162	14.414618
21.770869	885.839151	14.419635
21.658360	882.967164	14.424653
21.880408	882.452581	14.429671
21.531873	883.782211	14.434688
21.747788	887.651238	14.439706
21.941226	878.944627	14.444723
21.922918	883.055511	14.449741
21.994924	885.310689	14.454759
21.864633	892.201785	14.459776
22.102992	878.019156	14.464794
21.853733	886.002072	14.469811
21.691624	888.335490	14.474829
22.095486	893.359867	14.479847
21.895895	907.079806	14.484864
22.296469	904.814210	14.489882
22.073839	911.720043	14.494899
22.050227	909.139840	14.499917
22.476051	916.477889	14.504935
22.281431	909.166350	14.509952
22.363789	901.872776	14.514970
22.128368	896.251747	14.519987
22.079858	890.902157	14.525005
22.356469	892.389282	14.530023
22.083927	906.197937	14.535040
22.333110	914.883984	14.540058
22.714948	916.466805	14.545075
22.489629	904.127836	14.550093
22.280179	888.608701	14.555111
22.311468	885.064880	14.560128
22.303278	887.343073	14.565146
21.927314	893.415232	14.570163
22.284201	913.165752	14.575181
22.404776	915.461167	14.580199
22.237859	928.760618	14.585216
22.547407	920.839315	14.590234
22.469030	922.701613	14.595251
22.480683	925.592515	14.600269
22.603803	928.940714	14.605287
22.296650	928.924257	14.610304
22.925502	920.704265	14.615322
22.675477	923.711624	14.620339
22.820527	922.057028	14.625357
22.963081	918.048693	14.630375
22.827751	926.436622	14.635392
22.535416	918.693904	14.640410
23.063592	925.575167	14.645427
22.663190	915.903767	14.650445
22.630830	910.626316	14.655463
22.648343	921.819861	14.660480
22.906374	919.555762	14.665498
22.565776	919.898585	14.670515
22.531168	924.163098	14.675533
22.896333	908.059130	14.680551
22.656792	917.268312	14.685568
22.513283	914.734760	14.690586
22.719817	910.730381	14.695603
22.766430	922.011311	14.700621
22.786290	911.240935	14.705639
22.558147	920.360995	14.710656
22.807220	914.488858	14.715674
22.799999	917.753233	14.720691
22.829247	936.937028	14.725709
23.093880	935.714050	14.730727
23.185156	945.588606	14.735744
23.114884	943.759127	14.740762
23.529295	947.531228	14.745779
23.142581	941.662952	14.750797
22.888788	925.833871	14.755815
23.052153	933.243678	14.760832
23.135052	941.084766	14.765850
23.505435	947.756029	14.770867
23.268496	954.248866	14.775885
23.688552	939.653362	14.780903
23.330699	930.549347	14.785920
23.199006	921.155998	14.790938
23.169181	921.854327	14.795955
23.204959	934.825714	14.800973
23.207512	939.233748	14.805991
23.175530	946.881581	14.811008
23.350109	947.119428	14.816026
23.462944	939.054876	14.821043
23.386573	950.147795	14.826061
23.684321	947.838815	14.831079
23.325543	952.407521	14.836096
23.483135	952.613470	14.841114
23.332614	949.657080	14.846131
23.687471	954.082864	14.851149
23.810255	953.033526	14.856167
23.481324	957.785459	14.861184
23.239876	957.611438	14.866202
23.252829	949.944286	14.871219
23.267606	955.465703	14.876237
23.469624	946.034844	14.881255
23.459854	959.297461	14.886272
23.366769	951.536318	14.891290
23.730204	954.009306	14.896307
23.560927	972.107911	14.901325
24.029192	972.825120	14.906343
23.992399	973.036116	14.911360
23.922030	960.308999	14.916378
24.057117	955.345401	14.921395
23.311695	955.476713	14.926413
24.140880	964.018371	14.931431
23.719740	955.085677	14.936448
23.693250	955.638751	14.941466
24.056069	959.047046	14.946483
24.229445	975.834885	14.951501
24.518120	957.823879	14.956519
24.215831	954.111436	14.961536
24.073137	949.112703	14.966554
23.967499	946.872780	14.971571
24.005774	959.742325	14.976589
23.870827	945.459501	14.981607
23.942283	954.686748	14.986624
23.980910	951.070164	14.991642
23.940145	958.525913	14.996659
23.852794	971.529555	15.001677
24.190222	975.367427	15.006695
24.256821	988.272594	15.011712
24.630070	984.469705	15.016730
24.692627	975.274226	15.021747
24.388818	964.046535	15.026765
24.364078	955.813571	15.031783
24.187713	952.744893	15.036800
24.319172	948.370214	15.041818
24.007478	950.318495	15.046835
24.063636	974.134755	15.051853
24.670383	971.196015	15.056871
24.515859	984.120715	15.061888
24.419830	985.727061	15.066906
24.429360	990.609862	15.071923
24.565146	988.268503	15.076941
24.609356	987.236414	15.081959
24.325365	998.751039	15.086976
24.420677	987.785306	15.091994
24.742885	985.235668	15.097011
24.564871	990.799645	15.102029
24.597944	980.872653	15.107047
24.744322	985.799696	15.112064
24.319191	984.136927	15.117082
24.792756	978.054346	15.122099
24.931948	984.051457	15.127117
24.787724	980.143116	15.132135
24.879313	973.592898	15.137152
24.931509	981.322495	15.142170
24.898344	985.854224	15.147187
24.464394	990.190313	15.152205
24.657159	982.510197	15.157223
24.578464	986.078583	15.162240
24.733804	984.788871	15.167258
24.749595	983.865926	15.172275
24.376111	988.624975	15.177293
24.701797	986.939201	15.182311
24.672065	991.177786	15.187328
24.794196	1004.619191	15.192346
24.736417	1003.493250	15.197363
25.092124	1012.772730	15.202381
24.887866	1007.786155	15.207399
24.930039	1020.886379	15.212416
24.800181	1012.390922	15.217434
24.922974	1011.328993	15.222451
25.091141	1013.922016	15.227469
24.960259	1014.341511	15.232487
25.135687	1004.705632	15.237504
24.909968	1011.375252	15.242522
25.349761	1007.379264	15.247539
24.750944	1018.531177	15.252557
25.044114	1021.937224	15.257575
25.450432	1035.528397	15.262592
25.018220	1051.952777	15.267610
25.260269	1038.323139	15.272627
25.328018	1044.578647	15.277645
25.548961	1033.475646	15.282663
25.598252	1034.564078	15.287680
25.579247	1039.729100	15.292698
25.528950	1037.085487	15.297715
25.714942	1039.669379	15.302733
25.699809	1034.059569	15.307751
25.441687	1037.054871	15.312768
25.291107	1045.228998	15.317786
25.330395	1039.383979	15.322803
25.591440	1050.969027	15.327821
25.367547	1036.461974	15.332839
25.338920	1031.662107	15.337856
25.458466	1034.294351	15.342874
25.558725	1041.606521	15.347891
25.432057	1038.093361	15.352909
25.373157	1037.439528	15.357927
25.987662	1050.980993	15.362944
26.044310	1061.783779	15.367962
26.003492	1044.776949	15.372979
25.564043	1046.394028	15.377997
25.610275	1045.981417	15.383015
26.098991	1052.538682	15.388032
26.045788	1064.114082	15.393050
26.170951	1053.327593	15.398067
25.880414	1050.211820	15.403085
26.022818	1034.163692	15.408103
26.114000	1033.139052	15.413120
25.939280	1036.164312	15.418138
26.029107	1032.284699	15.423155
26.106908	1034.354135	15.428173
26.008161	1029.033743	15.433191
26.133474	1029.063934	15.438208
25.988615	1026.115278	15.443226
26.306682	1024.935682	15.448243
26.239074	1037.475314	15.453261
26.229293	1045.844861	15.458279
26.297992	1031.026864	15.463296
25.987442	1030.008093	15.468314
26.445277	1036.724441	15.473331
26.691544	1047.386856	15.478349
26.371601	1033.599091	15.483367
26.193727	1024.223266	15.488384
26.287789	1022.516226	15.493402
26.424999	1024.156953	15.498419
26.334492	1027.212827	15.503437
26.225374	1040.059545	15.508455
26.348055	1042.851747	15.513472
26.336916	1053.279140	15.518490
26.640456	1049.569154	15.523507
26.452706	1057.609210	15.528525
26.721238	1050.490373	15.533543
26.553474	1054.019495	15.538560
26.616026	1052.196348	15.543578
26.770703	1049.461049	15.548595
26.582332	1057.215684	15.553613
26.638029	1055.960736	15.558631
26.834232	1051.666941	15.563648
26.686862	1063.565689	15.568666
27.003796	1054.288689	15.573683
27.022849	1054.559995	15.578701
27.037019	1046.275940	15.583719
26.874185	1053.379166	15.588736
26.789822	1059.397806	15.593754
27.107642	1051.232855	15.598771
26.831366	1048.594605	15.603789
27.259921	1039.546003	15.608807
27.001673	1030.455140	15.613824
26.963896	1027.246359	15.618842
26.912689	1023.526102	15.623859
26.880502	1026.575034	15.628877
26.874232	1050.487898	15.633895
27.358780	1046.187443	15.638912
26.942088	1051.359265	15.643930
27.116612	1046.779477	15.648947
26.866918	1048.044591	15.653965
27.071817	1050.210169	15.658983
26.910963	1045.723985	15.664000
26.817584	1051.903730	15.669018
26.908265	1054.093818	15.674035
27.128660	1046.279480	15.679053
26.877564	1042.304793	15.684071
27.281575	1043.448342	15.689088
26.859092	1048.805140	15.694106
27.132241	1064.144853	15.699123
27.383539	1078.231151	15.704141
27.605007	1071.247232	15.709159
27.883745	1071.986023	15.714176
27.436753	1066.613401	15.719194
27.232156	1062.135762	15.724211
27.465906	1067.221154	15.729229
27.658729	1082.778202	15.734247
27.704926	1068.920209	15.739264
27.587688	1079.341733	15.744282
27.757930	1065.297208	15.749299
27.838969	1063.688987	15.754317
27.694839	1055.950874	15.759335
27.789164	1045.258189	15.764352
27.678788	1048.963784	15.769370
27.540568	1042.089159	15.774387
27.823779	1052.003965	15.779405
27.979132	1061.746465	15.784423
27.618278	1053.489970	15.789440
28.078372	1066.609315	15.794458
27.973784	1056.636583	15.799475
27.622560	1048.516202	15.804493
27.455684	1067.877750	15.809511
28.046080	1066.422684	15.814528
27.870971	1074.942891	15.819546
27.910580	1075.974665	15.824563
28.217189	1078.664390	15.829581
27.927236	1079.563886	15.834599
27.979979	1079.105402	15.839616
27.965246	1087.615769	15.844634
28.195345	1083.510052	15.849651
27.835918	1075.544342	15.854669
27.852275	1079.900665	15.859687
28.444198	1063.861039	15.864704
27.831538	1080.013766	15.869722
27.988495	1077.507773	15.874739
28.145309	1077.673733	15.879757
28.163958	1090.828898	15.884775
28.291164	1072.042003	15.889792
28.171024	1078.269288	15.894810
28.439727	1086.850859	15.899827
28.626127	1104.777278	15.904845
28.333698	1100.837483	15.909863
28.534686	1085.616065	15.914880
28.077211	1080.169601	15.919898
28.514597	1095.791483	15.924915
28.786075	1101.397076	15.929933
28.829746	1093.821696	15.934951
28.762982	1084.216528	15.939968
28.580153	1079.887217	15.944986
28.248893	1078.331380	15.950003
28.762747	1087.315111	15.955021
28.640379	1103.053020	15.960039
29.048606	1092.907233	15.965056
28.894111	1088.600144	15.970074
28.680175	1074.950383	15.975091
28.612893	1075.948866	15.980109
28.723825	1076.911060	15.985127
28.966689	1070.647361	15.990144
28.853385	1081.242874	15.995162
28.854878	1074.986206	16.000179
28.886765	1071.764732	16.005197
29.148212	1093.797574	16.010215
28.818061	1072.150552	16.015232
28.992732	1074.714233	16.020250
28.989466	1090.395378	16.025267
29.084815	1085.514370	16.030285
29.085657	1094.970058	16.035303
28.834402	1092.458378	16.040320
28.938100	1105.608644	16.045338
28.919273	1101.913092	16.050355
29.089111	1095.847443	16.055373
28.781393	1104.025428	16.060391
29.026137	1099.821410	16.065408
28.890919	1096.986825	16.070426
28.856769	1095.646310	16.075443
29.171475	1103.251517	16.080461
29.330040	1121.629947	16.085479
29.334099	1115.166775	16.090496
29.271955	1136.605527	16.095514
29.481018	1127.559629	16.100531
29.652560	1129.957068	16.105549
29.253194	1133.410670	16.110567
29.685700	1128.206871	16.115584
29.745845	1132.487795	16.120602
29.506757	1122.582876	16.125619
29.799840	1116.319800	16.130637
29.481414	1110.039419	16.135655
29.751550	1102.954122	16.140672
29.865891	1107.343592	16.145690
29.590079	1100.310762	16.150707
29.722281	1097.272282	16.155725
29.500371	1111.656680	16.160743
29.503478	1118.908874	16.165760
29.742628	1126.865150	16.170778
29.787872	1127.951089	16.175795
29.993506	1136.374425	16.180813
29.903934	1125.736968	16.185831
30.160919	1128.762612	16.190848
29.897810	1127.026004	16.195866
29.698873	1133.601740	16.200883
29.957125	1118.751063	16.205901
29.764277	1122.237009	16.210919
30.241951	1128.368183	16.215936
30.167085	1129.811498	16.220954
29.680267	1124.636340	16.225971
29.956855	1131.093759	16.230989
30.012366	1127.669505	16.236007
30.251134	1126.387712	16.241024
30.227679	1134.613191	16.246042
29.778898	1134.394365	16.251059
30.182504	1118.983285	16.256077
30.114405	1129.808377	16.261095
29.891135	1131.526274	16.266112
29.980922	1131.392235	16.271130
29.909490	1143.587268	16.276147
30.185888	1150.333394	16.281165
30.094171	1166.263122	16.286183
30.552071	1147.132360	16.291200
30.369819	1159.105180	16.296218
30.468940	1157.103145	16.301235
30.684617	1153.992347	16.306253
29.977532	1159.794149	16.311271
30.257751	1154.614629	16.316288
30.237476	1156.794899	16.321306
30.443548	1175.600001	16.326323
30.861813	1184.616343	16.331341
30.931900	1191.016269	16.336359
31.001849	1164.489179	16.341376
31.080308	1155.748041	16.346394
30.536441	1151.099529	16.351411
30.806052	1144.813441	16.356429
31.070312	1139.273867	16.361447
31.231489	1141.424409	16.366464
30.845258	1138.468605	16.371482
30.905978	1141.879506	16.376499
31.177961	1138.136776	16.381517
31.098619	1142.678277	16.386535
31.190013	1133.975991	16.391552
31.190334	1139.311795	16.396570
30.837321	1149.841763	16.401587
31.261353	1139.076761	16.406605
30.929064	1146.432801	16.411623
31.251699	1145.714966	16.416640
31.271793	1139.500925	16.421658
31.129696	1145.856803	16.426675
31.418873	1129.562565	16.431693
31.247719	1138.219040	16.436711
31.411808	1133.504815	16.441728
31.262537	1136.004548	16.446746
31.537373	1148.802710	16.451763
31.434691	1132.255556	16.456781
31.318912	1139.234908	16.461799
31.172523	1138.595024	16.466816
31.484228	1142.166467	16.471834
31.227979	1141.076888	16.476851
31.263493	1142.180111	16.481869
31.009293	1151.486165	16.486887
31.424788	1158.567208	16.491904
31.829914	1169.087180	16.496922
31.322649	1171.564573	16.501939
31.706183	1173.074003	16.506957
31.818472	1169.528992	16.511975
31.824655	1170.893314	16.516992
31.819039	1174.179514	16.522010
31.845752	1165.300323	16.527027
32.339913	1158.735369	16.532045
31.939006	1164.511937	16.537063
31.783789	1150.247088	16.542080
31.965786	1156.444309	16.547098
31.522810	1165.829247	16.552115
32.154211	1156.270779	16.557133
31.896399	1164.911988	16.562151
32.218724	1159.758000	16.567168
32.291275	1158.744189	16.572186
32.375991	1154.023738	16.577203
32.020151	1132.014186	16.582221
31.928344	1132.125413	16.587239
32.059553	1140.412750	16.592256
32.356274	1148.281986	16.597274
32.050663	1161.847603	16.602291
32.104116	1156.632672	16.607309
32.191877	1155.889372	16.612327
32.241567	1161.285741	16.617344
32.293688	1156.863876	16.622362
32.282284	1159.101724	16.627379
32.354768	1154.507501	16.632397
32.382565	1155.030687	16.637415
31.947776	1158.143858	16.642432
32.174052	1157.386331	16.647450
32.162545	1159.781507	16.652467
32.247479	1154.730667	16.657485
32.583713	1160.413263	16.662503
32.566807	1180.805820	16.667520
32.673933	1187.540419	16.672538
32.663217	1187.508930	16.677555
32.751285	1183.846648	16.682573
32.868055	1191.923158	16.687591
32.696653	1176.406299	16.692608
32.852585	1179.146031	16.697626
32.871448	1182.160897	16.702643
32.896800	1183.934321	16.707661
33.014749	1181.632745	16.712679
32.589240	1189.091769	16.717696
32.925116	1178.135505	16.722714
32.880127	1180.942678	16.727731
32.954927	1178.975980	16.732749
32.798693	1190.794444	16.737767
32.776019	1190.473048	16.742784
33.166973	1183.200906	16.747802
32.793501	1190.359030	16.752819
33.077532	1183.093716	16.757837
33.035722	1188.448843	16.762855
33.000675	1182.330100	16.767872
33.018117	1188.725050	16.772890
32.974239	1186.167694	16.777907
33.189484	1192.309288	16.782925
33.203467	1207.626776	16.787943
33.454863	1214.220393	16.792960
33.456878	1210.854205	16.797978
33.320509	1213.437629	16.802995
33.565185	1211.805653	16.808013
33.506558	1211.958782	16.813031
33.475868	1221.328340	16.818048
33.741033	1207.060101	16.823066
33.542656	1215.232508	16.828083
33.822710	1202.951117	16.833101
33.386628	1189.607256	16.838119
33.536628	1201.335199	16.843136
33.621061	1208.091518	16.848154
33.498069	1208.814946	16.853171
33.497933	1208.707833	16.858189
33.549364	1216.375539	16.863207
33.487383	1201.975426	16.868224
33.672447	1208.438825	16.873242
33.645447	1206.080134	16.878259
33.969947	1214.819634	16.883277
33.799171	1213.080088	16.888295
33.478743	1224.544069	16.893312
33.757977	1220.869380	16.898330
34.020806	1239.596296	16.903347
34.365862	1233.146331	16.908365
33.979139	1240.739203	16.913383
34.313927	1240.027291	16.918400
34.215049	1241.031611	16.923418
34.231050	1243.474327	16.928435
34.213221	1237.038976	16.933453
34.071826	1234.963597	16.938471
33.825748	1243.000471	16.943488
33.985448	1236.350390	16.948506
34.079724	1236.783534	16.953523
33.943243	1234.626355	16.958541
34.104323	1239.385175	16.963559
34.232553	1252.191079	16.968576
34.635637	1256.000465	16.973594
34.526516	1267.614049	16.978611
34.515004	1274.926071	16.983629
34.986268	1278.524015	16.988647
34.740126	1264.566159	16.993664
34.462399	1245.691028	16.998682
34.455619	1254.423609	17.003699
34.535518	1265.594884	17.008717
34.830157	1269.263469	17.013735
34.636875	1278.305041	17.018752
34.956060	1270.555058	17.023770
34.469503	1273.548298	17.028787
34.839350	1265.127162	17.033805
34.932380	1256.404878	17.038823
35.004409	1262.319215	17.043840
34.745890	1267.112717	17.048858
34.549645	1268.370110	17.053875
34.469366	1269.420232	17.058893
35.034251	1264.940938	17.063911
34.652242	1262.933820	17.068928
34.758766	1268.128456	17.073946
34.873824	1286.164797	17.078963
35.109141	1288.898968	17.083981
35.398836	1282.879411	17.088999
35.181474	1287.904685	17.094016
35.494358	1282.339999	17.099034
35.316769	1287.238584	17.104051
35.522798	1287.712899	17.109069
35.440148	1284.991810	17.114087
35.351890	1290.766544	17.119104
35.673080	1284.891411	17.124122
35.446149	1289.686174	17.129139
35.345731	1285.658284	17.134157
35.603665	1288.490315	17.139175
35.415075	1292.874669	17.144192
35.685839	1284.857102	17.149210
35.493040	1289.482816	17.154227
35.587689	1286.897842	17.159245
35.843169	1282.401031	17.164263
35.406365	1288.549912	17.169280
35.811838	1281.383166	17.174298
35.697951	1276.898859	17.179315
35.761320	1282.435460	17.184333
35.814722	1282.208902	17.189351
35.291739	1290.069727	17.194368
35.686647	1289.090230	17.199386
35.915538	1301.563923	17.204403
36.039456	1309.860385	17.209421
35.873822	1322.416682	17.214439
35.945081	1315.998550	17.219456
36.316063	1315.683586	17.224474
36.058587	1316.438692	17.229491
36.130743	1323.388945	17.234509
36.068758	1312.673801	17.239527
35.835520	1324.569152	17.244544
35.813382	1318.525376	17.249562
36.160638	1319.795200	17.254579
36.140535	1314.350468	17.259597
36.275364	1313.477734	17.264615
36.237242	1321.834655	17.269632
36.371120	1323.631689	17.274650
36.574668	1340.140626	17.279667
36.527647	1343.571117	17.284685
36.777039	1338.484545	17.289703
36.492015	1341.705224	17.294720
36.626925	1339.483509	17.299738
36.750780	1336.830943	17.304755
36.762401	1329.955880	17.309773
36.764696	1339.665558	17.314791
36.712559	1342.255234	17.319808
37.147921	1335.217413	17.324826
36.768003	1315.306059	17.329843
36.681662	1310.810269	17.334861
37.029620	1312.246732	17.339879
37.005762	1325.990950	17.344896
36.760020	1305.284227	17.349914
37.105139	1322.067887	17.354931
36.926351	1327.552671	17.359949
37.252507	1332.567572	17.364967
37.127380	1326.702252	17.369984
36.975218	1313.935958	17.375002
37.026905	1329.809958	17.380019
37.026246	1331.721265	17.385037
37.675482	1339.365272	17.390055
37.173040	1339.409061	17.395072
37.284133	1338.912159	17.400090
37.295454	1342.309748	17.405107
37.274430	1341.940891	17.410125
37.238776	1334.285223	17.415143
37.224044	1329.292692	17.420160
37.542447	1325.193276	17.425178
37.486591	1333.417741	17.430195
37.585422	1331.862500	17.435213
37.798074	1327.218338	17.440231
37.619259	1338.878489	17.445248
37.425579	1327.651829	17.450266
37.687792	1331.369650	17.455283
37.457287	1331.756274	17.460301
37.738349	1325.324341	17.465319
37.586764	1338.682285	17.470336
37.600083	1332.916801	17.475354
37.557405	1333.447301	17.480371
37.576189	1336.583343	17.485389
37.823008	1342.761654	17.490407
37.579513	1359.147627	17.495424
37.783410	1365.313128	17.500442
38.085905	1359.546348	17.505459
38.255445	1361.312529	17.510477
38.312056	1356.227594	17.515495
38.176639	1364.723548	17.520512
38.321632	1364.410017	17.525530
38.126183	1360.770884	17.530547
38.052705	1368.695350	17.535565
38.145352	1358.101026	17.540583
38.001892	1360.374911	17.545600
38.026271	1362.397855	17.550618
38.312145	1365.858635	17.555635
38.353391	1361.961512	17.560653
38.730236	1362.593431	17.565671
38.392694	1368.059501	17.570688
38.444068	1359.862937	17.575706
38.403953	1357.738351	17.580723
38.268396	1360.310659	17.585741
38.443640	1369.389473	17.590759
38.534699	1398.020973	17.595776
38.836346	1391.087041	17.600794
39.084745	1388.738672	17.605811
38.887876	1392.158463	17.610829
38.896506	1379.997298	17.615847
38.749164	1378.333437	17.620864
38.839101	1379.209331	17.625882
38.634580	1390.542476	17.630899
38.520056	1389.473535	17.635917
38.776636	1379.638837	17.640935
38.844237	1379.992862	17.645952
38.763100	1378.656669	17.650970
38.794091	1389.070504	17.655987
38.822758	1387.050571	17.661005
39.385939	1376.591991	17.666023
38.560557	1398.326687	17.671040
38.807679	1411.413454	17.676058
39.643784	1413.308519	17.681075
39.424414	1418.909929	17.686093
39.607069	1410.626326	17.691111
39.356596	1411.807430	17.696128
39.340341	1412.804090	17.701146
39.446790	1407.072491	17.706163
39.426719	1412.623236	17.711181
39.816707	1410.527582	17.716199
39.495033	1415.266704	17.721216
39.442389	1413.715161	17.726234
39.708094	1407.239234	17.731251
39.765409	1418.269499	17.736269
39.850309	1412.052085	17.741287
39.882274	1408.717257	17.746304
39.827591	1412.708240	17.751322
39.940679	1406.736464	17.756339
40.025235	1414.539789	17.761357
40.259919	1404.747894	17.766375
40.140008	1413.066784	17.771392
40.086426	1410.481046	17.776410
40.093132	1400.006586	17.781427
39.601107	1403.889551	17.786445
39.866181	1413.098009	17.791463
40.048622	1417.413786	17.796480
40.050695	1421.324141	17.801498
39.860561	1407.173943	17.806515
40.114923	1415.430783	17.811533
40.345464	1415.598363	17.816551
39.997783	1419.238857	17.821568
39.740511	1411.081262	17.826586
40.218309	1421.993341	17.831603
40.100573	1436.834963	17.836621
40.485102	1438.104359	17.841639
40.575782	1441.538869	17.846656
40.325657	1440.961923	17.851674
40.694724	1442.340760	17.856691
40.678689	1445.457995	17.861709
40.692370	1437.916323	17.866727
40.474083	1445.555588	17.871744
40.302152	1444.325899	17.876762
40.156581	1438.749321	17.881779
40.313965	1451.575135	17.886797
40.763654	1464.576156	17.891815
40.771843	1473.948328	17.896832
40.480029	1478.851822	17.901850
40.988352	1481.563727	17.906867
40.862091	1484.774848	17.911885
41.141857	1470.498519	17.916903
40.812849	1475.299396	17.921920
40.740154	1468.534464	17.926938
41.233774	1471.433558	17.931955
41.232626	1474.086705	17.936973
41.475799	1477.209801	17.941991
41.344430	1479.568299	17.947008
40.662315	1476.902666	17.952026
40.898322	1477.380859	17.957043
41.156124	1496.383423	17.962061
41.626539	1497.624969	17.967079
41.537162	1500.179711	17.972096
41.398728	1496.060290	17.977114
41.811803	1489.677237	17.982131
41.500823	1501.523777	17.987149
41.705836	1493.736039	17.992167
41.593387	1493.200060	17.997184
41.769167	1494.112611	18.002202
41.863725	1490.444498	18.007219
41.568607	1501.578228	18.012237
41.805657	1495.568554	18.017255
41.928116	1501.175260	18.022272
41.473717	1488.539604	18.027290
41.707566	1491.062459	18.032307
41.773140	1496.946458	18.037325
41.702648	1495.433936	18.042343
41.550852	1498.058412	18.047360
41.985453	1509.381748	18.052378
42.078810	1518.579903	18.057395
41.921022	1530.282474	18.062413
41.756301	1531.626105	18.067431
42.037647	1535.824675	18.072448
41.867089	1528.829123	18.077466
42.371921	1517.201452	18.082483
42.455365	1525.464376	18.087501
42.214566	1519.343696	18.092519
42.531777	1525.659523	18.097536
42.315474	1520.470179	18.102554
42.778940	1518.745857	18.107571
42.606364	1524.625373	18.112589
42.804265	1521.478005	18.117607
42.618242	1521.956648	18.122624
42.588464	1522.577914	18.127642
42.644647	1514.461513	18.132659
42.646958	1532.737957	18.137677
43.170711	1537.859856	18.142695
43.430320	1520.994121	18.147712
43.410591	1513.753493	18.152730
43.371564	1506.294917	18.157747
43.253736	1505.316164	18.162765
43.131278	1506.444608	18.167783
43.175480	1507.890209	18.172800
43.068610	1511.172968	18.177818
43.048984	1508.685626	18.182835
42.760906	1512.829486	18.187853
42.887334	1502.604868	18.192871
42.987473	1506.439040	18.197888
43.080006	1504.614202	18.202906
43.365084	1506.844147	18.207923
42.966726	1507.478574	18.212941
43.193796	1505.548115	18.217959
43.488457	1519.034059	18.222976
43.406804	1530.748872	18.227994
43.533118	1526.834992	18.233011
43.775849	1529.405991	18.238029
43.748159	1521.953465	18.243047
43.700695	1527.278154	18.248064
43.559785	1535.497421	18.253082
43.810038	1531.581864	18.258099
43.640263	1541.807585	18.263117
43.999757	1531.931201	18.268135
44.163705	1529.908551	18.273152
44.114767	1536.239515	18.278170
44.124901	1529.163231	18.283187
43.835458	1532.917957	18.288205
43.930685	1536.831579	18.293223
44.136786	1533.535810	18.298240
43.962969	1537.610326	18.303258
44.224925	1528.237967	18.308275
44.137778	1539.684654	18.313293
44.314671	1535.233336	18.318311
44.182570	1522.740534	18.323328
43.926080	1529.342144	18.328346
44.195809	1529.056697	18.333363
44.184714	1525.917490	18.338381
43.836951	1532.119916	18.343399
44.302700	1536.763385	18.348416
44.372467	1549.796758	18.353434
44.717994	1557.402796	18.358451
44.318056	1561.651820	18.363469
44.339985	1562.478792	18.368487
44.998820	1569.137378	18.373504
44.524646	1574.173029	18.378522
44.663351	1578.488750	18.383539
44.575845	1561.023106	18.388557
44.366708	1565.835572	18.393575
44.637828	1564.671290	18.398592
44.545922	1566.145682	18.403610
44.917879	1570.528030	18.408627
45.121431	1585.826695	18.413645
44.967046	1592.368787	18.418663
45.236591	1586.228040	18.423680
45.181621	1589.425455	18.428698
45.331062	1589.747556	18.433715
45.027672	1587.628742	18.438733
45.196268	1588.385915	18.443751
45.052082	1585.610084	18.448768
45.003982	1586.988608	18.453786
45.185790	1587.366114	18.458803
45.295823	1578.666097	18.463821
45.481818	1578.836850	18.468839
45.831031	1573.498303	18.473856
45.576934	1582.606395	18.478874
45.451217	1572.712977	18.483891
45.404148	1586.029307	18.488909
45.224047	1581.211729	18.493927
45.709778	1602.228704	18.498944
45.669489	1616.318766	18.503962
45.783376	1611.599809	18.508979
45.422204	1613.564716	18.513997
45.693741	1626.501479	18.519015
46.106171	1613.751853	18.524032
45.797010	1615.463838	18.529050
45.874347	1621.937523	18.534067
45.861105	1620.822522	18.539085
45.714786	1624.960324	18.544103
46.281149	1620.771726	18.549120
45.983472	1643.131335	18.554138
46.556565	1650.840354	18.559155
46.396688	1647.290653	18.564173
46.067149	1650.420174	18.569191
46.312683	1647.524757	18.574208
46.045364	1649.661121	18.579226
46.210373	1647.263870	18.584243
45.893481	1650.870407	18.589261
46.239151	1644.766263	18.594279
46.488202	1646.360909	18.599296
46.339702	1670.985736	18.604314
46.745403	1675.800078	18.609331
46.833651	1675.560877	18.614349
46.630990	1681.602572	18.619367
46.911302	1668.973079	18.624384
46.962065	1681.345720	18.629402
46.726788	1680.345571	18.634419
46.885800	1673.534151	18.639437
46.696464	1674.114010	18.644455
47.120088	1675.094022	18.649472
46.728936	1678.293157	18.654490
47.265168	1680.487795	18.659507
47.453965	1666.598626	18.664525
47.041856	1674.546586	18.669543
47.402448	1670.384499	18.674560
47.062300	1680.992240	18.679578
47.267505	1669.244692	18.684595
47.349939	1679.044071	18.689613
47.218520	1688.833513	18.694631
47.576785	1689.425150	18.699648
47.311301	1696.142324	18.704666
47.505588	1691.118694	18.709683
47.658548	1692.250423	18.714701
47.327712	1702.250234	18.719719
47.710159	1690.751282	18.724736
47.690739	1690.405758	18.729754
47.955671	1686.354100	18.734771
48.110176	1697.420204	18.739789
48.261470	1692.487595	18.744807
48.278035	1686.714374	18.749824
47.866040	1696.940290	18.754842
47.987728	1691.449993	18.759859
48.121105	1686.660257	18.764877
47.901468	1696.326907	18.769895
48.135259	1685.454194	18.774912
48.019859	1685.699760	18.779930
47.973666	1686.643006	18.784947
48.166866	1691.858580	18.789965
47.931352	1699.805135	18.794983
47.982138	1698.642160	18.800000
48.096501	1721.433299	18.805018
48.540940	1725.249589	18.810035
48.893817	1722.965524	18.815053
48.630509	1725.153174	18.820071
48.470597	1714.287381	18.825088
48.912082	1716.444434	18.830106
48.837896	1714.385797	18.835123
49.001223	1716.997812	18.840141
48.739100	1719.846009	18.845159
49.054049	1717.339882	18.850176
49.033333	1720.184189	18.855194
48.856441	1722.771017	18.860211
48.793231	1721.265962	18.865229
49.169930	1716.029171	18.870247
49.221268	1717.711204	18.875264
48.863375	1719.604808	18.880282
48.986477	1715.655207	18.885299
49.373646	1720.330934	18.890317
49.289874	1714.385708	18.895335
49.415663	1711.274972	18.900352
49.439410	1714.259279	18.905370
48.982459	1701.767003	18.910387
49.321324	1710.894662	18.915405
49.080993	1733.501692	18.920423
49.529753	1738.140857	18.925440
49.758693	1749.351662	18.930458
49.556086	1741.802637	18.935475
49.958720	1742.686105	18.940493
49.498850	1741.978199	18.945511
49.830421	1735.158109	18.950528
49.653264	1746.736514	18.955546
49.603867	1746.394983	18.960563
49.747067	1743.909163	18.965581
49.774066	1745.647783	18.970599
49.835478	1739.431617	18.975616
49.933458	1748.998879	18.980634
49.949249	1767.719465	18.985651
50.108172	1777.006438	18.990669
50.134644	1775.861493	18.995687
50.644391	1770.338382	19.000704
50.726021	1773.993873	19.005722
50.611878	1757.602008	19.010739
50.644594	1754.362160	19.015757
50.631048	1737.750547	19.020775
50.639726	1735.335738	19.025792
50.548578	1731.972488	19.030810
50.402226	1727.560079	19.035827
50.871123	1733.608749	19.040845
50.812724	1727.267749	19.045863
50.867443	1725.056406	19.050880
50.833029	1720.423992	19.055898
50.822523	1720.072326	19.060915
51.165104	1719.895607	19.065933
50.930900	1723.395369	19.070951
50.871278	1721.362726	19.075968
50.952379	1729.502645	19.080986
51.102780	1745.565869	19.086003
51.282689	1747.605752	19.091021
51.156149	1754.907256	19.096039
51.424219	1752.248135	19.101056
51.414880	1756.265804	19.106074
50.976847	1751.921929	19.111091
51.568420	1751.304338	19.116109
51.342731	1754.175048	19.121127
51.497818	1750.865343	19.126144
51.468509	1747.090279	19.131162
51.307337	1755.312113	19.136179
51.468765	1748.530164	19.141197
51.286875	1756.230646	19.146215
51.547775	1752.161521	19.151232
51.605326	1749.342473	19.156250
51.393257	1749.988101	19.161267
51.972108	1751.465661	19.166285
51.827360	1770.396703	19.171303
51.850829	1775.028981	19.176320
51.920931	1785.106492	19.181338
51.884565	1780.977005	19.186355
52.009648	1780.168727	19.191373
51.826828	1784.365883	19.196391
52.169290	1785.601906	19.201408
51.924013	1780.099305	19.206426
51.687710	1788.003557	19.211443
52.101105	1788.551010	19.216461
52.278129	1804.783103	19.221479
52.615084	1802.089390	19.226496
52.564681	1809.408670	19.231514
52.372337	1802.259927	19.236531
52.770063	1803.229135	19.241549
52.432416	1807.571338	19.246567
52.586201	1793.961368	19.251584
52.891658	1797.261025	19.256602
52.709228	1800.865817	19.261619
52.813574	1799.564504	19.266637
52.632825	1803.076998	19.271655
52.722552	1801.833078	19.276672
52.949804	1810.699359	19.281690
52.840219	1831.587429	19.286707
52.896557	1831.834712	19.291725
53.018600	1835.633228	19.296743
53.204330	1836.221710	19.301760
53.548832	1827.006688	19.306778
53.338876	1830.582841	19.311795
53.337458	1832.418822	19.316813
53.354014	1829.114673	19.321831
53.212682	1836.731642	19.326848
53.407088	1826.630465	19.331866
53.481837	1828.440139	19.336883
53.582631	1825.157168	19.341901
53.331183	1833.910237	19.346919
53.305784	1829.119818	19.351936
53.242804	1835.855889	19.356954
53.377160	1855.367874	19.361971
53.815282	1850.371378	19.366989
53.831472	1854.986750	19.372007
53.786826	1852.354672	19.377024
53.980567	1859.218143	19.382042
53.570228	1858.315906	19.387059
53.843499	1866.197928	19.392077
54.019483	1884.009765	19.397095
54.047619	1891.392074	19.402112
54.253323	1882.586160	19.407130
54.159572	1889.300418	19.412147
54.359225	1885.981215	19.417165
54.323407	1893.294277	19.422183
54.482874	1883.353594	19.427200
54.795254	1881.079110	19.432218
54.508689	1882.891352	19.437235
54.769861	1878.420984	19.442253
54.588395	1884.243853	19.447271
54.621615	1880.240894	19.452288
54.904386	1877.414221	19.457306
54.626580	1884.366279	19.462323
54.986880	1892.954174	19.467341
54.941207	1902.925161	19.472359
55.220841	1903.625314	19.477376
55.209803	1907.761285	19.482394
55.429273	1912.469325	19.487411
55.506880	1892.767389	19.492429
55.040969	1883.997789	19.497447
55.046326	1895.207393	19.502464
55.319943	1895.204498	19.507482
55.278829	1903.177581	19.512499
55.624825	1903.981207	19.517517
55.705399	1910.470237	19.522535
55.736964	1910.203103	19.527552
56.109756	1899.868124	19.532570
55.479826	1884.296992	19.537587
55.726299	1887.370883	19.542605
55.489255	1898.844116	19.547623
55.441415	1902.278015	19.552640
55.743904	1900.264684	19.557658
55.848707	1905.639954	19.562675
55.799111	1900.686612	19.567693
56.275805	1903.542874	19.572711
55.756730	1907.810209	19.577728
55.947666	1902.971893	19.582746
55.506900	1900.290496	19.587763
55.840344	1898.020516	19.592781
56.013097	1920.731862	19.597799
55.729299	1926.940770	19.602816
56.071613	1932.097254	19.607834
55.939923	1928.782901	19.612851
56.134108	1923.932261	19.617869
56.203092	1936.935428	19.622887
56.458595	1943.515352	19.627904
56.563376	1955.061544	19.632922
56.443703	1964.225520	19.637939
56.696866	1953.484029	19.642957
56.608045	1961.318444	19.647975
56.579191	1961.761022	19.652992
56.665552	1954.573263	19.658010
56.969116	1976.713211	19.663027
57.366243	1971.247317	19.668045
57.398788	1978.087783	19.673063
57.188672	1965.939776	19.678080
57.425993	1952.199133	19.683098
56.848078	1963.368872	19.688115
57.609173	1966.167992	19.693133
57.965163	1973.934622	19.698151
57.640594	1963.350548	19.703168
57.766197	1955.624786	19.708186
57.450006	1951.988240	19.713203
57.313930	1950.407469	19.718221
57.498535	1951.483043	19.723239
57.833459	1967.845098	19.728256
57.939453	1967.736000	19.733274
57.719811	1977.383957	19.738291
58.110329	1974.570759	19.743309
58.258128	1972.494776	19.748327
58.004495	1959.995809	19.753344
58.187681	1946.038836	19.758362
57.727194	1958.494819	19.763379
58.275881	1961.529183	19.768397
57.909857	1963.428833	19.773415
58.272789	1975.407407	19.778432
58.515406	1973.285624	19.783450
58.241585	1971.733897	19.788467
58.417207	1970.465253	19.793485
58.625589	1967.430963	19.798503
58.416449	1970.987354	19.803520
58.296580	1968.170601	19.808538
58.318481	1972.725317	19.813555
58.237602	1964.842121	19.818573
58.401664	1976.178292	19.823591
58.419708	1998.853864	19.828608
58.738056	2004.737873	19.833626
58.816838	2004.124967	19.838643
58.887950	2005.313038	19.843661
58.776155	1996.399582	19.848679
58.931404	2003.904838	19.853696
59.103457	2005.588892	19.858714
58.942249	2005.259680	19.863731
59.360553	2010.679386	19.868749
59.065226	1998.746312	19.873767
59.135725	2009.456346	19.878784
59.347889	2016.652835	19.883802
59.247032	2027.991178	19.888819
59.545217	2025.147073	19.893837
59.562413	2028.240255	19.898855
59.515936	2025.923080	19.903872
59.622819	2029.380317	19.908890
59.645103	2030.900260	19.913907
59.820198	2032.887462	19.918925
59.975067	2026.240154	19.923943
59.676338	2028.052779	19.928960
59.947207	2017.499564	19.933978
59.709754	2030.807331	19.938995
59.936577	2041.571906	19.944013
60.082479	2049.737854	19.949031
59.955138	2060.695794	19.954048
60.320887	2065.960287	19.959066
60.607629	2066.955867	19.964083
60.394494	2055.692416	19.969101
60.560217	2059.605949	19.974119
60.223622	2064.778718	19.979136
60.552213	2051.466287	19.984154
60.463587	2055.318909	19.989171
60.372641	2054.094342	19.994189
60.760363	2054.302940	19.999207
60.118479	2061.717460	20.004224
60.324968	2071.377754	20.009242
60.363040	2077.210525	20.014259
60.391599	2077.815431	20.019277
60.506131	2095.461913	20.024295
60.834778	2105.389075	20.029312
61.230667	2101.816704	20.034330
61.043399	2107.824654	20.039347
61.013894	2108.025063	20.044365
60.905639	2101.110546	20.049383
60.870397	2113.686056	20.054400
61.293064	2123.552613	20.059418
61.358426	2127.317767	20.064435
61.444382	2128.113321	20.069453
61.693840	2135.274817	20.074471
61.737261	2144.051053	20.079488
61.657881	2131.438409	20.084506
61.931736	2134.780156	20.089523
61.882391	2125.760695	20.094541
62.182948	2124.242422	20.099559
62.229953	2132.498916	20.104576
62.136139	2127.025519	20.109594
62.046885	2122.007630	20.114611
62.025753	2127.934817	20.119629
62.429721	2118.264121	20.124647
62.131460	2130.406477	20.129664
62.548502	2126.706443	20.134682
62.217596	2128.161583	20.139699
62.299559	2133.781284	20.144717
62.736752	2121.644762	20.149735
62.364430	2118.337276	20.154752
62.424808	2117.379617	20.159770
62.557860	2120.470861	20.164787
62.859471	2117.357171	20.169805
62.798802	2121.812617	20.174823
62.823728	2141.427390	20.179840
63.204463	2146.094843	20.184858
63.150289	2159.121782	20.189875
62.909576	2158.947622	20.194893
63.193830	2151.445813	20.199911
63.016107	2149.125164	20.204928
63.019975	2153.999032	20.209946
62.909587	2153.996022	20.214963
63.327429	2144.176786	20.219981
63.689470	2142.799736	20.224999
63.439379	2144.557422	20.230016
63.744132	2142.825306	20.235034
63.569411	2145.775277	20.240051
63.695146	2145.224099	20.245069
63.604888	2138.042391	20.250087
63.465417	2135.456849	20.255104
63.877333	2137.075135	20.260122
63.870655	2154.246239	20.265139
63.937885	2156.410343	20.270157
64.179200	2157.504422	20.275175
64.143928	2166.441892	20.280192
63.897155	2159.488081	20.285210
64.392232	2159.090387	20.290227
64.166065	2162.650326	20.295245
64.272203	2159.876940	20.300263
64.458503	2162.081839	20.305280
64.409214	2160.341680	20.310298
64.344662	2157.175464	20.315315
64.368253	2154.261854	20.320333
64.711045	2157.502938	20.325351
64.484524	2164.056001	20.330368
64.613361	2158.804307	20.335386
64.950392	2174.459092	20.340403
64.563634	2194.241850	20.345421
65.004595	2187.456811	20.350439
64.844396	2195.405780	20.355456
64.719688	2190.091462	20.360474
64.741245	2202.535279	20.365491
64.810368	2189.557510	20.370509
65.227255	2188.560298	20.375527
65.024882	2199.031593	20.380544
65.341821	2205.848050	20.385562
65.270683	2216.344052	20.390579
65.015500	2220.901343	20.395597
65.449516	2219.731488	20.400615
65.549327	2222.861879	20.405632
65.586696	2223.625070	20.410650
65.348518	2222.057404	20.415667
65.602300	2218.996945	20.420685
65.982338	2234.554476	20.425703
65.900577	2255.006072	20.430720
66.021887	2258.706487	20.435738
66.057780	2253.113243	20.440755
66.330734	2256.606192	20.445773
66.193821	2248.912702	20.450791
66.347655	2259.803138	20.455808
66.033190	2257.203004	20.460826
66.326592	2264.085385	20.465843
66.187792	2256.796514	20.470861
66.228982	2246.859501	20.475879
66.278153	2250.608390	20.480896
66.358047	2263.048461	20.485914
66.671759	2277.215645	20.490931
66.505779	2282.872584	20.495949
66.667399	2279.512162	20.500967
66.831718	2288.020633	20.505984
66.905056	2279.705990	20.511002
66.811009	2285.627563	20.516019
66.646815	2289.806946	20.521037
67.048184	2295.146078	20.526055
67.270055	2317.117076	20.531072
67.177623	2310.771024	20.536090
67.675677	2305.879666	20.541107
67.593871	2310.440014	20.546125
67.806617	2310.637978	20.551143
67.516199	2310.879212	20.556160
67.384971	2311.756609	20.561178
67.599422	2306.915198	20.566195
67.665817	2307.894019	20.571213
67.681004	2296.846475	20.576231
67.397790	2313.178490	20.581248
67.718103	2309.981543	20.586266
67.839856	2315.469109	20.591283
68.011417	2326.510946	20.596301
68.245834	2328.248023	20.601319
68.290316	2332.965228	20.606336
68.308503	2334.559011	20.611354
68.699037	2332.997264	20.616371
68.523918	2332.857478	20.621389
68.726356	2336.400237	20.626407
68.445067	2338.763901	20.631424
68.371988	2333.784265	20.636442
68.651000	2334.243047	20.641459
68.697840	2329.249794	20.646477
68.739536	2328.369044	20.651495
68.816745	2328.921365	20.656512
68.676486	2326.294223	20.661530
68.944824	2323.285698	20.666547
68.585230	2332.582560	20.671565
68.946449	2336.155848	20.676583
69.060058	2352.757366	20.681600
69.203882	2356.724029	20.686618
69.396115	2358.544926	20.691635
69.125354	2363.369051	20.696653
69.119639	2359.438247	20.701671
69.062138	2356.635071	20.706688
69.288068	2352.819146	20.711706
69.507215	2360.510266	20.716723
69.637161	2378.138900	20.721741
69.800759	2375.470371	20.726759
70.095782	2379.910076	20.731776
69.723149	2373.356960	20.736794
70.285337	2379.338324	20.741811
70.166091	2378.015981	20.746829
70.205848	2387.438768	20.751847
70.096414	2388.436194	20.756864
70.001340	2382.407543	20.761882
70.157500	2378.733318	20.766899
69.949231	2384.622802	20.771917
70.195414	2384.496852	20.776935
70.222735	2401.713955	20.781952
70.126394	2407.424339	20.786970
70.570441	2409.496924	20.791987
70.525390	2408.696080	20.797005
70.700594	2406.858734	20.802023
70.721830	2412.426083	20.807040
70.678414	2423.879858	20.812058
71.188483	2429.040447	20.817075
71.094921	2441.589355	20.822093
71.208482	2425.121883	20.827111
71.275931	2425.732401	20.832128
71.211841	2430.454366	20.837146
71.884303	2433.865556	20.842163
71.643862	2434.481123	20.847181
71.785446	2432.024552	20.852199
71.725844	2432.402037	20.857216
71.780403	2431.674195	20.862234
71.994219	2427.807480	20.867251
71.583862	2430.526844	20.872269
71.703870	2423.933688	20.877287
71.967913	2428.670187	20.882304
71.947501	2423.682908	20.887322
72.224571	2423.414371	20.892339
71.993648	2429.249275	20.897357
71.951066	2412.431496	20.902375
72.067349	2423.759115	20.907392
72.236618	2413.729981	20.912410
72.245767	2420.424139	20.917427
72.365129	2449.184555	20.922445
72.390906	2446.644188	20.927463
72.549913	2448.480621	20.932480
72.388377	2448.622641	20.937498
72.627570	2449.273422	20.942515
72.700172	2456.808611	20.947533
72.580398	2439.096913	20.952551
72.922662	2440.716903	20.957568
72.911486	2437.693933	20.962586
73.363479	2441.244906	20.967603
72.849822	2458.069289	20.972621
73.095017	2458.220390	20.977639
73.784911	2457.331445	20.982656
73.440303	2454.950831	20.987674
74.007463	2452.195119	20.992691
73.853983	2449.949219	20.997709
73.895975	2435.117540	21.002727
73.920395	2426.040505	21.007744
73.859343	2428.612129	21.012762
74.127960	2423.970499	21.017779
74.054833	2425.195766	21.022797
73.915660	2425.825075	21.027815
74.115079	2421.679044	21.032832
73.877015	2427.279884	21.037850
74.110857	2420.084111	21.042867
74.120027	2441.478793	21.047885
74.474321	2437.153094	21.052903
74.348504	2439.643012	21.057920
74.127450	2442.797087	21.062938
74.509760	2434.079888	21.067955
74.276333	2442.477248	21.072973
74.434387	2437.168878	21.077991
74.534928	2436.748354	21.083008
74.456831	2447.959105	21.088026
74.870059	2466.057912	21.093043
74.978906	2467.785926	21.098061
75.152268	2469.974844	21.103079
75.024100	2468.660208	21.108096
74.983695	2466.957140	21.113114
75.372024	2462.628366	21.118131
75.321881	2469.541245	21.123149
75.266546	2469.588452	21.128167
75.379701	2463.561959	21.133184
75.120687	2472.666664	21.138202
75.346484	2478.891292	21.143219
75.484609	2498.869223	21.148237
75.604824	2501.787963	21.153255
76.090375	2506.069102	21.158272
76.094306	2503.484224	21.163290
76.002383	2498.812750	21.168307
76.025248	2504.368075	21.173325
76.019325	2504.435721	21.178343
76.261963	2494.966713	21.183360
76.237126	2501.593171	21.188378
76.489894	2496.419923	21.193395
76.335437	2501.787201	21.198413
76.140203	2497.733976	21.203431
76.331833	2511.532261	21.208448
76.308028	2523.961559	21.213466
76.679956	2516.254432	21.218483
76.426230	2523.481417	21.223501
76.522688	2524.339823	21.228519
76.932123	2527.325722	21.233536
76.920655	2524.744869	21.238554
76.968266	2523.499739	21.243571
76.892050	2534.313792	21.248589
77.070420	2542.424494	21.253607
77.442821	2540.141129	21.258624
76.992666	2554.027640	21.263642
77.450530	2548.704457	21.268659
77.283974	2553.987153	21.273677
77.568036	2557.873297	21.278695
77.904769	2548.250802	21.283712
77.746576	2545.772793	21.288730
77.583755	2547.850141	21.293747
77.414835	2555.486827	21.298765
77.689183	2567.954360	21.303783
77.983710	2575.628067	21.308800
77.908827	2585.649802	21.313818
78.091556	2571.198300	21.318835
78.297828	2586.142023	21.323853
78.168406	2580.583669	21.328871
78.319242	2584.991366	21.333888
78.172825	2600.272176	21.338906
78.267191	2601.846761	21.343923
78.626960	2603.976081	21.348941
78.751712	2608.618430	21.353959
79.140614	2605.895839	21.358976
78.787917	2603.472437	21.363994
78.787786	2609.496373	21.369011
79.081935	2607.926371	21.374029
79.092664	2608.544369	21.379047
79.293006	2605.467181	21.384064
79.260808	2603.603887	21.389082
79.415641	2625.283185	21.394099
79.549165	2624.003894	21.399117
79.645244	2626.666917	21.404135
79.871972	2625.353883	21.409152
79.762101	2635.595197	21.414170
79.935373	2625.654957	21.419187
80.048024	2621.625757	21.424205
79.848440	2624.153429	21.429223
80.250026	2624.315778	21.434240
80.005214	2625.392233	21.439258
80.115741	2617.216211	21.444275
80.169679	2621.117043	21.449293
80.080846	2621.581005	21.454311
80.339327	2612.672629	21.459328
79.961508	2620.071271	21.464346
80.202355	2621.919849	21.469363
80.384936	2621.203048	21.474381
80.343319	2643.431309	21.479399
80.327490	2641.319968	21.484416
80.200901	2649.881335	21.489434
80.541604	2642.847767	21.494451
80.664550	2649.002340	21.499469
80.629032	2666.901568	21.504487
81.060059	2669.112358	21.509504
80.881960	2685.738746	21.514522
81.516599	2681.465814	21.519539
81.394572	2683.112675	21.524557
81.008963	2686.349681	21.529575
81.335502	2678.681961	21.534592
81.450788	2690.304937	21.539610
81.621317	2701.711439	21.544627
81.899806	2706.690373	21.549645
81.798454	2712.614856	21.554663
82.199220	2701.751738	21.559680
81.884225	2708.487492	21.564698
81.958349	2703.905897	21.569715
82.095846	2701.519944	21.574733
82.213938	2701.526909	21.579751
82.352154	2704.191094	21.584768
82.176803	2701.918749	21.589786
82.200509	2697.609507	21.594803
82.573981	2706.003059	21.599821
82.230518	2723.949890	21.604839
82.713335	2716.453104	21.609856
82.483355	2729.425200	21.614874
82.366623	2729.187206	21.619891
83.068858	2724.407897	21.624909
82.814943	2724.536330	21.629927
83.158971	2735.802701	21.634944
83.211920	2748.572367	21.639962
83.307322	2755.949106	21.644979
83.499639	2756.446115	21.649997
83.346886	2766.586588	21.655015
83.711456	2751.641003	21.660032
83.507618	2763.062414	21.665050
83.016139	2752.360423	21.670067
83.385421	2753.602486	21.675085
83.538486	2760.779663	21.680103
83.632359	2782.752108	21.685120
84.048567	2789.014943	21.690138
84.333103	2776.246165	21.695155
84.272087	2777.529316	21.700173
84.292740	2781.528323	21.705191
84.552562	2768.144401	21.710208
84.788130	2779.233014	21.715226
84.868165	2777.974039	21.720243
85.178199	2762.179694	21.725261
85.101447	2766.432585	21.730279
84.905899	2768.973010	21.735296
84.923206	2771.904282	21.740314
85.362777	2762.419431	21.745331
85.008985	2767.767461	21.750349
84.939046	2772.747702	21.755367
84.991221	2760.908049	21.760384
85.080508	2766.503227	21.765402
85.112660	2769.039594	21.770419
85.306045	2760.557646	21.775437
85.149197	2762.165229	21.780455
85.014107	2766.411690	21.785472
85.081975	2782.360207	21.790490
85.438778	2795.151471	21.795507
85.473062	2787.091349	21.800525
85.440611	2796.659646	21.805543
85.977572	2806.591043	21.810560
85.832655	2828.181564	21.815578
85.804843	2836.857872	21.820595
86.105206	2827.124571	21.825613
86.098075	2835.161180	21.830631
86.014109	2836.838174	21.835648
85.737957	2842.412991	21.840666
85.877067	2858.461935	21.845683
86.441844	2850.806481	21.850701
86.217853	2860.833301	21.855719
86.442457	2873.806192	21.860736
86.600817	2886.472637	21.865754
86.450106	2893.513458	21.870771
86.646356	2886.830844	21.875789
86.608948	2905.137363	21.880807
87.086722	2920.037346	21.885824
86.766340	2916.502700	21.890842
87.094920	2929.090905	21.895859
87.408491	2921.449513	21.900877
87.409782	2952.330903	21.905895
87.747137	2944.260912	21.910912
87.635584	2943.534362	21.915930
87.752196	2947.020159	21.920947
88.032536	2945.530991	21.925965
88.072192	2944.066044	21.930983
88.573150	2933.670574	21.936000
88.480140	2944.138331	21.941018
88.558959	2932.446903	21.946035
88.783870	2928.999936	21.951053
88.479580	2929.314973	21.956071
88.532834	2924.436921	21.961088
88.676229	2927.859444	21.966106
88.516644	2943.430626	21.971123
88.713697	2931.853289	21.976141
88.554135	2933.883757	21.981159
88.894115	2947.622611	21.986176
89.057368	2960.247434	21.991194
89.034417	2961.559143	21.996211
89.408537	2953.041183	22.001229
88.926739	2959.558213	22.006247
89.215357	2962.721589	22.011264
89.339260	2960.072659	22.016282
89.140918	2961.925237	22.021299
89.542423	2973.304559	22.026317
89.609302	2983.388131	22.031335
89.520852	2978.350940	22.036352
89.937745	2981.150095	22.041370
89.584066	2987.535787	22.046387
89.880017	2978.361619	22.051405
89.772740	2984.660818	22.056423
89.958430	2996.442729	22.061440
90.243091	3004.374687	22.066458
90.092329	3009.030419	22.071475
90.471004	3012.033126	22.076493
90.608745	3000.697258	22.081511
90.893419	3009.840673	22.086528
90.840344	3016.275988	22.091546
90.791977	3015.579477	22.096563
91.164497	3005.809380	22.101581
91.002271	3005.732821	22.106599
91.364346	3025.295016	22.111616
91.580281	3023.176555	22.116634
91.489300	3019.515623	22.121651
91.448960	3015.251114	22.126669
91.519661	3029.368890	22.131687
91.610148	3033.152298	22.136704
91.487710	3025.585888	22.141722
91.606315	3035.879153	22.146739
91.850269	3029.370588	22.151757
91.425442	3034.274563	22.156775
91.701169	3032.420325	22.161792
91.359691	3038.730147	22.166810
91.467608	3061.533845	22.171827
91.877364	3050.599813	22.176845
91.949934	3076.620326	22.181863
92.131740	3089.379967	22.186880
92.106043	3088.712092	22.191898
92.133090	3096.531781	22.196915
92.919400	3101.961657	22.201933
92.670641	3124.945050	22.206951
92.654151	3123.832024	22.211968
93.005562	3126.409583	22.216986
92.967599	3119.769720	22.222003
93.342409	3115.133755	22.227021
93.437050	3115.081528	22.232039
93.475205	3103.615928	22.237056
93.350722	3108.966846	22.242074
93.658302	3107.970491	22.247091
94.128035	3115.450559	22.252109
93.968274	3116.544164	22.257127
94.074438	3108.856298	22.262144
94.366005	3097.745198	22.267162
94.228809	3095.345560	22.272179
94.035454	3100.681498	22.277197
94.245079	3109.358651	22.282215
94.448474	3127.476008	22.287232
94.688450	3122.092182	22.292250
94.474929	3134.652943	22.297267
94.888711	3123.772496	22.302285
94.703030	3132.213766	22.307303
94.426800	3135.422412	22.312320
94.552565	3123.821679	22.317338
94.476741	3131.571257	22.322355
94.361804	3128.597731	22.327373
94.688134	3134.802677	22.332391
94.916820	3142.841970	22.337408
95.075568	3142.658373	22.342426
94.891807	3170.291689	22.347443
95.568583	3148.937277	22.352461
95.369267	3155.936413	22.357479
95.282924	3178.396029	22.362496
95.803055	3178.283032	22.367514
95.893899	3172.935556	22.372531
95.914942	3175.119764	22.377549
95.841112	3181.075446	22.382567
95.920934	3176.466835	22.387584
96.269683	3180.633900	22.392602
96.044881	3185.725508	22.397619
96.684246	3190.367796	22.402637
96.327060	3202.038986	22.407655
96.442666	3213.200552	22.412672
96.435603	3206.399174	22.417690
96.553065	3217.204085	22.422707
96.865365	3215.206325	22.427725
96.637040	3217.040903	22.432743
96.994657	3234.787665	22.437760
97.117576	3236.097378	22.442778
97.056798	3243.149984	22.447795
97.462227	3233.887400	22.452813
97.407503	3235.450428	22.457831
97.283940	3240.629752	22.462848
97.448102	3238.387357	22.467866
97.550889	3256.693985	22.472883
97.744587	3263.728049	22.477901
97.661971	3267.030930	22.482919
97.712188	3266.760012	22.487936
98.038205	3255.035202	22.492954
97.746016	3266.450637	22.497971
98.303805	3280.513009	22.502989
98.313345	3291.531066	22.508007
98.560435	3290.112461	22.513024
98.764176	3289.298642	22.518042
98.690231	3297.881884	22.523059
98.786792	3292.470519	22.528077
98.802130	3289.793216	22.533095
99.153485	3287.568950	22.538112
99.143949	3286.970076	22.543130
99.176524	3313.429271	22.548147
99.428155	3317.413619	22.553165
99.918108	3309.023308	22.558183
99.807109	3314.809542	22.563200
99.973038	3319.717742	22.568218
99.565601	3303.145137	22.573235
100.001572	3313.924503	22.578253
100.180029	3315.813800	22.583271
100.154553	3307.441173	22.588288
100.174164	3298.288846	22.593306
99.788955	3309.430437	22.598323
99.578305	3302.894335	22.603341
99.737923	3307.540788	22.608359
99.825133	3310.159724	22.613376
100.199845	3311.842297	22.618394
100.371781	3342.030194	22.623411
100.379639	3334.723691	22.628429
100.451039	3340.423422	22.633447
100.493150	3359.802656	22.638464
101.032034	3350.954538	22.643482
100.807360	3363.208894	22.648499
100.853606	3355.449426	22.653517
100.988206	3361.167407	22.658535
100.827923	3388.826496	22.663552
101.429980	3392.319952	22.668570
101.264877	3401.493641	22.673587
101.628720	3392.637223	22.678605
101.548563	3398.351704	22.683623
101.566070	3416.945896	22.688640
102.130923	3419.102425	22.693658
101.916541	3425.582521	22.698675
101.931609	3424.541536	22.703693
102.298542	3415.918256	22.708711
102.249153	3429.042320	22.713728
102.719589	3428.137192	22.718746
102.476657	3448.402959	22.723763
102.800843	3452.976802	22.728781
102.972710	3458.717987	22.733799
102.550732	3460.477270	22.738816
103.062218	3450.178097	22.743834
102.785682	3456.278709	22.748851
103.045488	3458.937805	22.753869
103.605508	3463.515739	22.758887
103.582678	3481.830879	22.763904
103.566045	3480.933401	22.768922
103.844262	3482.713984	22.773939
103.729680	3473.049574	22.778957
103.972971	3478.631481	22.783975
103.794641	3482.056661	22.788992
104.169331	3477.649529	22.794010
103.859440	3477.800265	22.799027
103.980780	3480.283986	22.804045
104.189478	3494.075756	22.809063
104.004570	3514.833481	22.814080
104.320997	3509.067582	22.819098
104.535195	3508.385821	22.824115
104.302535	3510.627841	22.829133
104.321701	3530.392501	22.834151
104.032390	3539.882663	22.839168
104.753095	3542.908038	22.844186
104.995663	3552.044347	22.849203
105.322943	3561.765038	22.854221
105.693623	3557.301094	22.859239
105.358701	3569.585788	22.864256
105.752073	3563.894921	22.869274
105.793871	3565.332456	22.874291
105.904370	3564.597999	22.879309
105.889873	3564.148589	22.884327
105.553873	3570.696916	22.889344
105.952126	3558.839984	22.894362
105.913382	3568.113204	22.899379
105.825536	3581.788712	22.904397
106.331966	3588.993339	22.909415
106.307464	3595.105740	22.914432
106.695990	3584.483084	22.919450
106.258749	3590.930347	22.924467
106.578623	3592.229927	22.929485
106.589019	3593.357009	22.934503
106.498863	3621.584356	22.939520
106.814157	3618.771840	22.944538
106.859057	3627.790245	22.949555
107.028315	3642.403458	22.954573
107.026116	3647.878250	22.959591
107.239418	3655.930506	22.964608
107.628975	3663.396895	22.969626
107.546000	3659.868263	22.974643
107.680609	3677.863531	22.979661
107.802269	3688.463578	22.984679
107.604582	3694.192981	22.989696
107.948063	3689.199955	22.994714
108.064206	3683.601237	22.999731
107.739543	3698.751122	23.004749
108.211061	3706.062072	23.009767
108.102325	3713.320011	23.014784
108.535122	3706.850266	23.019802
108.251520	3733.463690	23.024819
108.491891	3734.887672	23.029837
108.954330	3732.627535	23.034855
108.861690	3736.373457	23.039872
109.246572	3755.842521	23.044890
109.348984	3767.364560	23.049907
109.076339	3770.005558	23.054925
109.643755	3762.190306	23.059943
109.321155	3761.929265	23.064960
109.772018	3753.880072	23.069978
109.857804	3769.719026	23.074995
109.950822	3784.423994	23.080013
110.261138	3787.938895	23.085031
110.130463	3791.597278	23.090048
110.667260	3787.200395	23.095066
110.403272	3784.088441	23.100083
110.473738	3789.985172	23.105101
110.871621	3786.079314	23.110119
110.511402	3785.096572	23.115136
110.859768	3772.713254	23.120154
110.867514	3783.996297	23.125171
111.068622	3800.709015	23.130189
111.582831	3805.981943	23.135207
111.372092	3811.832264	23.140224
111.432897	3804.122161	23.145242
111.472683	3806.156361	23.150259
111.476574	3807.315178	23.155277
111.370537	3798.202243	23.160295
111.553551	3799.351378	23.165312
111.578002	3797.603985	23.170330
111.726987	3815.928331	23.175347
112.033467	3828.945656	23.180365
112.228115	3830.888296	23.185383
112.106027	3833.812899	23.190400
112.460618	3834.108639	23.195418
112.482358	3829.101574	23.200435
112.503136	3845.198787	23.205453
112.756323	3856.688987	23.210471
112.795983	3863.826573	23.215488
112.727987	3862.157637	23.220506
112.608783	3860.711637	23.225523
112.492640	3875.502757	23.230541
112.939818	3890.246550	23.235559
113.173323	3899.631548	23.240576
113.081956	3897.759430	23.245594
113.548719	3914.761122	23.250611
113.511436	3926.729597	23.255629
113.851901	3927.557046	23.260647
114.010600	3926.256324	23.265664
114.190786	3921.872210	23.270682
114.438183	3932.315497	23.275699
114.332566	3952.033750	23.280717
114.466935	3951.984627	23.285735
114.218024	3955.490401	23.290752
114.764041	3956.798012	23.295770
115.448857	3946.749354	23.300787
115.075174	3951.411819	23.305805
115.049751	3940.496962	23.310823
114.867248	3955.134321	23.315840
115.107272	3959.558109	23.320858
115.092483	3964.460727	23.325875
115.293590	3982.413509	23.330893
115.646172	3975.943065	23.335911
115.396184	3977.392552	23.340928
115.873591	3970.910860	23.345946
116.007175	3992.929132	23.350963
115.750383	4007.144123	23.355981
115.824643	4009.751875	23.360999
115.999927	4009.114060	23.366016
116.171978	4008.463387	23.371034
116.358256	4023.098653	23.376051
116.365403	4036.517914	23.381069
116.789855	4024.314213	23.386087
116.554854	4034.981609	23.391104
116.623315	4037.779889	23.396122
116.966360	4051.904784	23.401139
116.847339	4058.771175	23.406157
117.423584	4043.770867	23.411175
117.537281	4059.082517	23.416192
117.728422	4045.475524	23.421210
117.780683	4048.259868	23.426227
117.899349	4044.991650	23.431245
117.991354	4037.907395	23.436263
118.328555	4035.102323	23.441280
118.251636	4044.492856	23.446298
118.195427	4031.099968	23.451315
118.090447	4042.480641	23.456333
118.368053	4055.059851	23.461351
118.301011	4069.133719	23.466368
118.198357	4063.480059	23.471386
118.525290	4068.866338	23.476403
118.222261	4084.356962	23.481421
118.719594	4095.594433	23.486439
118.945083	4103.632405	23.491456
119.103899	4102.162504	23.496474
119.170927	4105.907448	23.501491
119.031703	4121.276799	23.506509
119.331812	4124.324525	23.511527
119.606521	4122.876266	23.516544
119.511309	4132.963658	23.521562
119.900874	4146.616275	23.526579
119.479041	4164.037658	23.531597
120.073986	4162.475395	23.536615
120.250677	4163.398992	23.541632
119.957778	4168.446723	23.546650
120.281264	4182.747155	23.551667
120.545121	4192.831617	23.556685
120.901435	4191.780222	23.561703
120.597818	4195.871443	23.566720
120.782109	4213.527447	23.571738
121.158530	4226.223217	23.576755
120.954449	4237.926665	23.581773
121.511420	4225.137587	23.586791
121.380624	4225.277863	23.591808
121.043222	4232.662205	23.596826
121.597991	4246.544258	23.601843
121.595480	4252.492147	23.606861
121.946252	4256.158056	23.611879
121.789608	4262.302032	23.616896
121.991748	4279.936388	23.621914
122.245829	4275.364160	23.626931
122.122019	4287.023379	23.631949
122.601219	4279.090542	23.636967
122.524934	4293.657801	23.641984
122.616113	4300.111584	23.647002
123.006631	4313.562015	23.652019
123.185931	4311.767842	23.657037
123.098161	4311.803704	23.662055
123.690787	4315.009378	23.667072
123.419912	4317.378767	23.672090
123.696749	4306.579083	23.677107
123.367829	4313.384653	23.682125
123.824806	4320.708459	23.687143
123.772603	4339.312569	23.692160
123.927970	4335.711155	23.697178
124.439296	4334.377773	23.702195
123.951295	4339.045211	23.707213
124.448817	4331.608213	23.712231
124.451233	4339.917116	23.717248
124.405619	4333.801101	23.722266
124.716342	4346.577470	23.727283
124.728609	4363.294190	23.732301
124.954410	4358.593489	23.737319
125.215949	4363.608738	23.742336
125.014854	4374.462934	23.747354
125.248626	4355.230015	23.752371
125.095942	4376.246578	23.757389
125.640676	4388.165895	23.762407
126.023989	4392.898182	23.767424
125.732960	4395.092995	23.772442
125.854014	4384.532873	23.777459
125.857614	4388.591682	23.782477
125.757879	4406.753444	23.787495
126.077158	4415.168426	23.792512
125.895829	4426.774774	23.797530
126.136352	4435.388782	23.802547
126.452168	4450.279963	23.807565
126.881937	4450.946873	23.812583
127.030667	4451.265227	23.817600
127.426067	4457.339355	23.822618
127.437151	4446.374245	23.827635
127.431203	4452.618575	23.832653
127.759765	4467.853119	23.837671
127.824421	4471.513567	23.842688
127.941130	4478.592748	23.847706
128.031598	4478.760684	23.852723
128.047863	4480.824691	23.857741
127.884105	4478.086041	23.862759
128.269949	4469.168045	23.867776
128.168867	4472.174391	23.872794
128.488750	4487.051587	23.877811
128.244369	4502.075413	23.882829
128.230159	4508.555533	23.887847
128.347802	4505.623315	23.892864
128.332456	4531.018436	23.897882
128.840358	4534.900893	23.902899
128.857682	4540.272200	23.907917
129.060182	4554.921143	23.912935
129.323091	4561.557719	23.917952
129.307345	4578.962042	23.922970
129.559153	4565.573841	23.927987
129.497640	4584.772162	23.933005
129.648675	4591.428950	23.938023
130.006858	4585.126500	23.943040
129.888742	4593.061393	23.948058
130.246355	4608.504658	23.953075
130.201070	4628.906529	23.958093
130.417871	4621.891786	23.963111
130.508668	4630.161585	23.968128
130.623932	4636.976725	23.973146
130.618360	4641.422572	23.978163
130.583296	4657.391894	23.983181
130.539046	4660.259403	23.988199
130.646581	4670.188954	23.993216
130.842740	4690.766408	23.998234
131.154807	4691.704645	24.003251
131.982013	4693.263313	24.008269
132.773920	4678.303510	24.013287
133.286967	4669.503580	24.018304
133.188985	4656.754838	24.023322
133.435529	4637.842082	24.028339
133.263888	4645.809139	24.033357
133.200108	4631.595548	24.038375
133.433350	4604.589336	24.043392
133.078706	4602.433393	24.048410
133.187740	4594.127489	24.053427
133.076105	4600.836391	24.058445
133.235279	4619.731290	24.063463
133.857535	4611.274312	24.068480
133.876809	4630.887802	24.073498
134.013984	4627.846235	24.078515
133.985015	4625.982169	24.083533
133.952431	4627.139786	24.088551
134.089457	4628.007585	24.093568
134.252565	4631.118175	24.098586
134.237236	4624.554271	24.103603
134.493906	4629.606580	24.108621
134.364557	4625.077288	24.113639
134.528172	4636.018284	24.118656
134.533141	4657.654457	24.123674
134.565093	4653.145855	24.128691
134.726539	4662.460223	24.133709
134.480229	4684.074346	24.138727
134.910311	4680.622587	24.143744
134.733188	4701.806367	24.148762
135.106691	4716.529697	24.153779
135.336195	4723.441528	24.158797
135.508987	4735.218239	24.163815
135.873274	4744.256423	24.168832
135.699827	4753.727310	24.173850
135.920278	4744.880366	24.178867
136.344443	4762.684456	24.183885
136.289446	4772.005867	24.188903
136.547002	4773.265930	24.193920
136.588149	4781.846631	24.198938
136.827134	4790.364322	24.203955
136.884038	4795.952850	24.208973
137.047607	4800.825733	24.213991
137.259710	4797.260794	24.219008
137.329027	4809.835311	24.224026
137.218457	4819.837503	24.229043
137.448700	4828.092259	24.234061
137.361572	4834.510193	24.239079
137.764445	4837.908314	24.244096
137.947312	4854.076768	24.249114
138.271471	4863.742963	24.254131
137.972918	4872.384174	24.259149
138.252861	4869.207287	24.264167
138.513504	4870.706828	24.269184
138.378659	4883.097601	24.274202
138.635282	4891.918588	24.279219
138.573341	4892.108471	24.284237
138.720360	4914.691658	24.289255
139.112795	4924.085802	24.294272
139.207212	4931.794231	24.299290
139.712495	4937.253887	24.304307
139.751117	4950.890040	24.309325
139.955828	4964.674386	24.314343
139.770017	4958.478186	24.319360
140.051091	4968.331489	24.324378
140.179248	4958.082958	24.329395
140.248452	4980.656624	24.334413
140.273602	4997.511264	24.339431
140.689746	4990.642373	24.344448
140.785280	4986.833982	24.349466
140.850829	5003.892255	24.354483
141.061823	5004.472916	24.359501
141.175112	5011.839281	24.364519
141.721720	5008.742584	24.369536
141.451902	5006.997122	24.374554
141.589243	5015.999276	24.379571
141.962668	5029.643488	24.384589
142.137231	5041.207733	24.389607
142.154447	5032.005934	24.394624
142.247883	5043.661006	24.399642
142.114532	5036.586243	24.404659
142.130635	5054.865654	24.409677
142.197912	5072.990590	24.414695
142.538157	5066.898506	24.419712
142.208124	5093.743645	24.424730
142.814331	5096.157414	24.429747
143.445518	5101.262680	24.434765
143.448120	5105.605083	24.439783
143.632945	5124.961520	24.444800
143.688732	5123.649568	24.449818
143.779807	5116.772654	24.454835
144.006582	5119.246139	24.459853
144.135514	5125.024720	24.464871
144.461169	5115.251274	24.469888
144.524134	5132.542992	24.474906
144.526017	5142.889387	24.479923
144.772136	5138.164746	24.484941
144.816608	5147.854480	24.489959
144.947962	5147.507650	24.494976
144.953822	5153.057245	24.499994
145.465650	5158.460868	24.505011
145.613548	5169.898861	24.510029
145.220038	5186.045494	24.515047
145.678092	5177.116351	24.520064
145.539089	5185.969909	24.525082
145.301172	5180.096634	24.530099
145.639568	5190.330400	24.535117
145.616638	5214.934048	24.540135
146.375000	5218.989187	24.545152
146.255416	5219.299986	24.550170
146.628817	5230.546290	24.555187
146.626508	5239.872969	24.560205
146.216652	5247.617119	24.565223
146.762216	5263.329295	24.570240
146.903292	5274.052486	24.575258
146.844307	5273.441745	24.580275
147.196729	5291.909368	24.585293
147.146661	5306.040713	24.590311
147.580716	5301.548842	24.595328
147.545112	5323.245169	24.600346
147.767606	5337.127735	24.605363
147.750100	5340.000553	24.610381
147.872473	5355.724439	24.615399
148.504769	5369.012977	24.620416
148.363352	5379.062950	24.625434
148.420674	5377.883697	24.630451
148.535558	5392.670181	24.635469
148.664048	5399.127151	24.640487
149.252576	5405.035555	24.645504
149.417198	5420.622168	24.650522
149.961857	5424.215762	24.655539
150.106280	5426.187870	24.660557
149.920307	5427.584798	24.665575
150.034387	5420.254033	24.670592
150.134714	5422.704457	24.675610
150.067459	5434.623855	24.680627
150.956497	5443.408071	24.685645
150.790579	5458.638294	24.690663
150.942967	5458.369144	24.695680
151.070894	5457.083426	24.700698
150.868551	5459.943250	24.705715
151.223419	5455.068204	24.710733
151.053090	5473.296030	24.715751
151.336632	5470.851734	24.720768
151.401590	5482.671411	24.725786
151.295757	5487.936811	24.730803
151.571594	5495.937620	24.735821
151.895068	5506.695629	24.740839
152.292951	5511.581745	24.745856
152.085327	5531.038265	24.750874
152.262581	5528.719483	24.755891
152.614461	5523.464083	24.760909
152.810682	5550.144313	24.765927
153.331805	5546.425283	24.770944
153.455728	5548.753947	24.775962
153.501473	5558.977193	24.780979
153.838484	5546.773603	24.785997
153.983352	5545.620506	24.791015
154.258270	5539.053195	24.796032
154.335247	5542.493215	24.801050
154.690374	5538.468626	24.806067
154.844383	5527.152622	24.811085
154.501440	5542.801406	24.816103
154.811894	5536.445586	24.821120
154.746443	5537.028646	24.826138
154.860014	5530.474474	24.831155
154.900278	5526.891913	24.836173
154.623401	5532.115362	24.841191
155.039571	5541.244902	24.846208
155.324617	5552.504753	24.851226
155.352189	5557.095868	24.856243
155.675864	5556.507505	24.861261
155.611526	5589.798309	24.866279
155.647871	5592.154318	24.871296
155.623460	5595.660871	24.876314
155.643118	5607.330511	24.881331
156.125991	5617.360576	24.886349
156.248556	5634.034395	24.891367
156.466985	5638.130893	24.896384
156.511730	5656.013079	24.901402
156.503119	5672.433261	24.906419
157.009635	5672.442824	24.911437
156.904543	5688.861884	24.916455
157.500784	5708.938720	24.921472
157.326688	5709.523372	24.926490
157.824928	5714.705917	24.931507
158.299167	5714.490880	24.936525
158.896156	5728.529691	24.941543
158.402951	5739.656481	24.946560
158.922400	5728.680970	24.951578
158.957627	5733.960160	24.956595
159.348968	5729.137434	24.961613
158.929005	5727.565315	24.966631
159.248267	5721.390551	24.971648
159.451139	5723.267618	24.976666
159.443624	5715.915968	24.981683
159.479654	5743.319982	24.986701
159.540764	5756.064201	24.991719
159.755244	5752.638709	24.996736
159.981742	5761.716012	25.001754
160.055855	5780.557504	25.006771
160.131161	5777.935495	25.011789
160.393014	5785.041732	25.016807
160.410392	5807.537585	25.021824
160.995712	5802.417967	25.026842
160.767070	5822.988406	25.031859
161.222646	5815.440132	25.036877
161.223200	5840.087493	25.041895
161.614622	5840.065052	25.046912
161.418871	5847.654205	25.051930
161.512310	5847.042742	25.056947
161.909249	5863.233246	25.061965
162.094853	5872.852957	25.066983
162.172677	5881.160144	25.072000
162.431583	5880.452273	25.077018
162.364675	5877.094433	25.082035
162.564310	5890.025973	25.087053
162.665532	5898.508046	25.092071
163.067853	5907.778502	25.097088
163.078884	5893.208722	25.102106
162.861457	5927.494044	25.107123
163.402776	5923.949524	25.112141
163.363680	5931.277699	25.117159
163.382599	5957.581721	25.122176
163.886910	5964.658830	25.127194
163.822598	5972.109067	25.132211
164.388889	5984.789463	25.137229
164.560581	6001.979883	25.142247
164.772864	5995.752823	25.147264
165.219167	5994.904915	25.152282
164.920106	5991.938917	25.157299
165.093741	6000.044419	25.162317
165.068644	6010.730119	25.167335
165.136758	6011.638890	25.172352
165.541412	6022.299357	25.177370
165.650500	6037.295129	25.182387
165.712756	6050.765654	25.187405
165.675831	6057.259513	25.192423
166.051232	6074.161822	25.197440
166.350883	6082.986106	25.202458
166.070915	6090.398397	25.207475
166.629316	6108.905016	25.212493
166.611605	6119.458217	25.217511
166.662895	6132.344379	25.222528
166.943293	6145.772343	25.227546
166.947749	6147.308143	25.232563
167.307543	6174.349750	25.237581
167.428974	6181.702024	25.242599
167.452061	6188.180078	25.247616
168.087705	6201.458609	25.252634
168.277154	6216.323725	25.257651
168.513425	6213.074052	25.262669
168.915852	6233.269840	25.267687
168.982863	6241.995187	25.272704
169.301592	6245.265428	25.277722
169.030738	6249.917712	25.282739
169.350730	6240.218397	25.287757
169.349750	6253.676370	25.292775
169.840326	6260.714897	25.297792
170.040237	6259.732368	25.302810
169.931736	6262.875592	25.307827
170.307927	6263.857221	25.312845
170.745992	6270.606702	25.317863
170.734248	6285.630644	25.322880
170.780846	6289.658726	25.327898
170.877610	6284.019632	25.332915
171.525401	6280.148044	25.337933
171.270237	6283.133682	25.342951
171.260921	6283.422200	25.347968
171.698824	6286.736397	25.352986
171.675686	6287.082197	25.358003
171.589163	6303.607557	25.363021
171.928701	6313.445358	25.368039
172.023285	6312.339562	25.373056
171.978194	6322.604569	25.378074
172.324493	6340.629130	25.383091
172.608245	6348.994234	25.388109
172.481714	6362.250433	25.393127
172.528510	6364.750464	25.398144
172.763682	6366.864812	25.403162
172.643566	6388.829530	25.408179
173.020095	6401.597978	25.413197
173.490239	6407.672020	25.418215
173.540942	6431.281604	25.423232
174.166670	6438.744416	25.428250
174.009518	6443.107958	25.433267
174.228074	6444.601000	25.438285
174.324417	6460.489150	25.443303
174.491157	6461.862199	25.448320
174.905812	6467.244822	25.453338
174.699572	6488.237502	25.458355
174.784340	6498.322197	25.463373
175.096075	6512.212097	25.468391
175.381034	6531.043744	25.473408
175.440415	6529.220432	25.478426
175.700055	6545.871060	25.483443
175.824996	6556.518281	25.488461
176.068504	6560.755032	25.493479
175.925144	6574.933142	25.498496
176.382739	6587.750988	25.503514
176.481314	6601.489258	25.508531
176.752928	6617.200918	25.513549
177.196389	6628.095626	25.518567
177.132247	6635.278637	25.523584
177.283424	6643.034775	25.528602
177.396834	6666.242094	25.533619
177.525846	6664.581559	25.538637
177.659759	6682.523941	25.543655
177.593167	6693.418968	25.548672
178.474040	6697.664305	25.553690
178.425074	6726.084560	25.558707
178.424830	6733.513160	25.563725
178.787238	6734.530855	25.568743
179.227373	6744.330086	25.573760
179.685910	6753.281303	25.578778
179.827131	6750.326791	25.583795
179.999951	6752.327599	25.588813
179.789809	6754.648338	25.593831
179.765381	6770.460863	25.598848
180.396335	6776.195464	25.603866
180.299352	6781.533086	25.608883
180.509061	6781.701714	25.613901
180.814917	6787.321334	25.618919
180.644805	6790.421771	25.623936
181.084131	6803.913909	25.628954
180.934142	6817.070386	25.633971
181.219034	6816.365414	25.638989
181.448060	6831.501812	25.644007
181.505953	6844.223870	25.649024
181.755460	6839.387996	25.654042
182.098874	6849.538708	25.659059
182.208747	6859.681021	25.664077
182.388899	6857.949363	25.669095
182.409099	6871.263667	25.674112
182.551625	6881.080535	25.679130
182.720252	6896.810483	25.684148
182.899257	6900.504449	25.689165
183.174547	6909.439337	25.694183
183.189193	6934.855032	25.699200
183.668936	6927.670605	25.704218
183.752058	6950.088459	25.709236
183.795798	6955.997008	25.714253
183.949684	6954.747157	25.719271
184.531313	6981.185173	25.724288
184.757856	6980.433629	25.729306
184.914641	6990.765270	25.734324
184.710243	6989.286901	25.739341
184.913427	7005.497741	25.744359
184.863188	7019.870735	25.749376
185.166549	7023.141240	25.754394
185.529910	7047.316502	25.759412
185.472372	7061.690699	25.764429
185.846899	7061.577321	25.769447
185.972606	7082.137853	25.774464
186.578052	7089.706132	25.779482
186.465670	7108.537332	25.784500
186.430725	7109.567256	25.789517
187.189711	7110.587066	25.794535
187.392336	7133.794267	25.799552
187.373605	7128.687100	25.804570
187.601672	7139.149905	25.809588
188.083766	7139.487571	25.814605
188.030954	7150.383881	25.819623
188.159855	7158.737934	25.824640
188.702136	7157.582737	25.829658
188.678815	7168.031345	25.834676
188.728181	7174.019345	25.839693
189.219705	7173.591448	25.844711
189.251491	7190.242140	25.849728
189.641532	7182.612354	25.854746
189.691086	7190.773699	25.859764
189.620112	7193.554676	25.864781
189.937276	7204.191389	25.869799
189.950994	7218.727491	25.874816
190.708960	7207.808094	25.879834
191.106786	7194.533539	25.884852
191.140414	7191.191635	25.889869
191.403038	7188.626861	25.894887
191.507335	7196.172009	25.899904
191.754696	7193.386193	25.904922
191.773494	7184.253630	25.909940
191.699366	7194.268916	25.914957
192.239782	7175.073964	25.919975
192.249110	7177.831121	25.924992
191.872244	7202.955592	25.930010
192.360066	7211.840257	25.935028
192.456971	7214.611786	25.940045
192.886578	7209.717181	25.945063
192.577606	7225.355224	25.950080
192.736591	7236.054947	25.955098
193.183835	7237.614696	25.960116
193.220668	7247.849967	25.965133
193.799384	7262.792565	25.970151
193.591598	7279.942666	25.975168
193.715459	7273.822026	25.980186
193.881490	7289.823099	25.985204
193.997847	7299.988285	25.990221
194.304692	7295.556635	25.995239
194.126746	7320.330508	26.000256
194.460508	7329.181967	26.005274
194.880321	7345.279954	26.010292
194.899455	7362.672139	26.015309
195.329951	7381.017790	26.020327
195.201522	7389.746245	26.025344
195.916851	7405.381313	26.030362
195.903137	7420.932751	26.035380
195.805097	7427.854396	26.040397
196.122130	7442.397445	26.045415
196.482166	7460.601375	26.050432
196.468266	7467.833827	26.055450
196.960410	7478.797338	26.060468
196.854216	7498.073033	26.065485
197.295713	7509.591535	26.070503
197.338614	7522.922080	26.075520
197.559935	7526.429651	26.080538
197.766988	7550.328086	26.085556
198.026769	7561.920844	26.090573
198.610807	7574.978280	26.095591
198.491488	7588.331597	26.100608
198.728601	7588.805909	26.105626
199.126962	7605.478102	26.110644
199.089218	7614.429482	26.115661
199.657309	7609.874648	26.120679
199.645983	7623.037661	26.125696
199.951228	7635.795325	26.130714
200.349992	7640.803985	26.135732
199.922243	7659.428049	26.140749
200.464604	7663.142578	26.145767
200.381903	7683.682473	26.150784
200.750012	7684.756775	26.155802
200.831374	7692.657578	26.160820
200.691551	7713.726374	26.165837
201.012869	7718.110010	26.170855
200.993984	7739.039558	26.175872
201.217483	7742.944223	26.180890
201.537362	7764.256929	26.185908
201.632989	7786.180650	26.190925
201.919580	7789.115628	26.195943
202.037041	7803.764422	26.200960
202.171354	7826.060146	26.205978
202.465972	7838.953846	26.210996
202.481276	7849.861840	26.216013
202.882536	7874.450255	26.221031
203.019987	7889.534653	26.226048
203.481284	7899.350163	26.231066
203.855071	7907.809997	26.236084
203.694218	7923.872516	26.241101
204.083234	7932.608506	26.246119
204.692208	7946.022309	26.251136
204.951616	7955.744528	26.256154
205.444863	7962.630784	26.261172
205.445847	7966.973098	26.266189
205.818837	7964.359911	26.271207
206.069143	7962.070035	26.276224
206.260677	7964.034975	26.281242
206.428297	7965.365926	26.286260
206.519961	7976.096192	26.291277
206.986985	7973.567165	26.296295
207.190399	7975.967743	26.301312
207.120002	7975.401595	26.306330
207.591239	7968.949872	26.311348
207.688596	7996.863685	26.316365
207.848135	7992.008342	26.321383
207.811217	7994.789547	26.326400
208.297589	7991.217120	26.331418
208.278579	7993.899858	26.336436
208.134805	8006.198246	26.341453
208.074119	8014.267838	26.346471
208.538439	8026.903686	26.351488
208.371535	8050.897555	26.356506
208.865181	8054.740744	26.361524
209.006572	8077.384717	26.366541
209.406208	8082.344207	26.371559
209.315633	8101.289644	26.376576
209.969690	8115.253561	26.381594
210.410146	8118.586659	26.386612
210.475042	8129.324056	26.391629
210.550710	8147.089802	26.396647
210.504968	8157.094122	26.401664
210.824062	8177.175601	26.406682
210.907107	8180.077791	26.411700
211.303172	8192.914705	26.416717
211.747720	8206.032314	26.421735
211.752549	8224.212354	26.426752
211.722802	8214.896856	26.431770
212.093569	8237.802362	26.436788
212.189407	8256.962622	26.441805
212.247138	8253.977058	26.446823
212.284466	8264.700847	26.451840
212.301296	8279.446416	26.456858
212.634526	8291.634764	26.461876
212.644774	8311.435929	26.466893
213.012087	8337.120038	26.471911
213.203245	8348.272643	26.476928
213.527385	8368.093096	26.481946
213.563613	8373.111402	26.486964
213.968626	8400.670014	26.491981
214.382388	8414.973526	26.496999
214.929468	8433.753595	26.502016
215.022865	8435.723226	26.507034
215.441971	8461.599964	26.512052
215.545207	8474.470817	26.517069
215.408901	8479.128697	26.522087
215.561818	8503.984772	26.527104
215.439720	8519.068291	26.532122
216.375913	8534.524543	26.537140
216.145512	8545.330166	26.542157
216.734254	8562.447220	26.547175
217.283047	8570.043789	26.552192
216.995152	8578.241977	26.557210
217.404107	8593.698922	26.562228
217.743962	8602.016220	26.567245
218.762511	8602.098040	26.572263
219.024622	8604.081326	26.577280
219.315135	8617.110137	26.582298
219.968044	8602.166255	26.587316
219.675522	8591.555768	26.592333
219.768546	8578.118075	26.597351
220.052464	8588.852759	26.602368
220.244468	8602.427668	26.607386
220.140346	8601.329381	26.612404
220.240265	8603.255892	26.617421
220.703793	8601.181790	26.622439
220.737153	8598.258671	26.627456
220.873988	8610.620239	26.632474
221.000010	8619.700357	26.637492
220.967660	8631.532534	26.642509
220.882117	8635.469780	26.647527
221.036026	8645.313538	26.652544
221.127504	8668.632521	26.657562
221.090532	8686.239402	26.662580
221.480181	8712.532851	26.667597
221.663190	8731.136030	26.672615
222.026388	8748.348275	26.677632
221.946546	8768.226180	26.682650
222.303794	8789.538720	26.687668
222.611377	8804.984500	26.692685
222.696423	8838.050964	26.697703
222.716895	8854.654943	26.702720
223.379269	8877.016397	26.707738
223.842831	8897.032135	26.712756
223.735753	8915.159236	26.717773
223.881565	8926.214833	26.722791
224.278886	8939.668784	26.727808
224.501432	8958.600013	26.732826
224.866862	8965.067194	26.737844
225.015204	8978.437707	26.742861
225.196569	9001.999826	26.747879
225.776202	9008.399828	26.752896
225.893098	9020.254164	26.757914
225.938455	9032.340267	26.762932
226.032312	9054.519137	26.767949
226.189922	9069.827766	26.772967
226.377338	9094.056031	26.777984
226.689501	9112.410870	26.783002
226.952690	9127.535100	26.788020
226.967822	9149.774272	26.793037
227.456929	9170.437534	26.798055
227.716303	9183.969963	26.803072
227.907812	9209.376273	26.808090
228.183283	9219.415484	26.813108
228.660377	9236.163911	26.818125
229.110772	9241.744111	26.823143
229.624201	9250.152151	26.828160
229.661072	9268.952429	26.833178
230.031450	9266.716410	26.838196
230.005725	9274.653218	26.843213
230.358041	9272.746285	26.848231
230.698041	9288.270030	26.853248
230.810035	9282.975629	26.858266
231.277474	9284.868434	26.863284
231.231486	9312.444738	26.868301
231.612318	9320.188483	26.873319
232.022944	9313.519990	26.878336
231.783562	9319.455716	26.883354
232.436434	9324.328037	26.888372
232.574459	9337.366436	26.893389
232.565697	9346.643191	26.898407
232.901451	9353.860557	26.903424
232.815593	9368.095882	26.908442
233.208972	9367.898438	26.913460
233.433975	9391.734776	26.918477
233.631758	9400.273884	26.923495
233.591582	9405.522713	26.928512
233.817785	9426.313232	26.933530
234.350498	9436.260035	26.938548
234.461964	9447.748832	26.943565
234.542519	9469.198130	26.948583
235.402959	9468.121525	26.953600
235.323702	9490.789816	26.958618
235.989653	9498.000263	26.963636
235.862478	9504.770893	26.968653
236.004578	9512.868381	26.973671
236.451803	9518.373246	26.978688
236.101079	9534.430364	26.983706
236.819467	9539.635843	26.988724
237.164683	9550.971375	26.993741
237.072892	9558.212920	26.998759
237.445704	9559.697830	27.003776
237.410820	9574.135748	27.008794
237.568282	9586.002559	27.013812
237.772995	9592.655789	27.018829
237.836345	9608.216094	27.023847
238.058322	9623.129786	27.028864
237.854208	9649.364089	27.033882
238.087980	9667.303969	27.038900
238.324187	9688.928669	27.043917
238.624036	9721.069178	27.048935
239.056258	9734.571207	27.053952
239.304419	9766.359993	27.058970
239.486911	9766.119820	27.063988
239.892558	9787.930542	27.069005
240.009408	9807.250374	27.074023
240.747499	9812.138001	27.079040
240.791397	9841.195099	27.084058
241.346676	9852.643367	27.089076
241.822670	9874.821952	27.094093
241.702782	9888.981735	27.099111
242.242692	9879.469729	27.104128
242.030954	9906.182235	27.109146
242.262138	9910.846512	27.114164
242.783617	9930.492368	27.119181
242.845145	9950.048258	27.124199
243.179278	9953.616337	27.129216
243.487616	9976.600954	27.134234
243.619845	9983.688939	27.139252
244.111314	10000.871550	27.144269
244.669300	10014.387824	27.149287
245.032755	10012.872935	27.154304
245.038577	10019.721367	27.159322
245.288557	10025.416447	27.164340
245.348607	10037.379812	27.169357
245.568407	10040.861069	27.174375
246.098080	10056.717410	27.179392
246.221562	10065.997926	27.184410
246.288028	10071.928872	27.189428
246.165197	10084.396006	27.194445
245.877736	10096.757170	27.199463
246.575844	10116.792243	27.204480
246.554645	10137.537000	27.209498
246.847900	10153.884461	27.214516
247.168729	10177.626096	27.219533
247.100436	10203.343875	27.224551
247.814638	10226.048135	27.229568
248.155229	10256.731202	27.234586
248.264215	10275.685731	27.239604
248.528812	10288.747672	27.244621
248.752480	10304.815969	27.249639
249.480040	10322.048284	27.254656
249.588133	10334.981737	27.259674
249.515139	10333.398654	27.264692
249.767470	10351.526462	27.269709
250.010579	10366.417058	27.274727
250.444172	10384.048506	27.279744
250.799043	10401.709837	27.284762
250.970667	10401.981004	27.289780
251.270417	10422.026856	27.294797
251.652798	10441.038364	27.299815
251.708873	10449.194537	27.304832
251.983202	10467.191475	27.309850
252.399139	10468.555877	27.314868
252.344868	10487.777534	27.319885
252.371498	10506.125674	27.324903
252.737947	10519.778006	27.329920
253.018199	10534.949730	27.334938
253.132514	10553.213903	27.339956
253.601858	10565.865660	27.344973
253.491298	10590.464946	27.349991
254.106393	10603.570461	27.355008
254.472372	10626.546880	27.360026
254.951225	10632.175409	27.365044
255.130831	10649.866345	27.370061
254.675308	10673.421421	27.375079
255.287701	10685.711843	27.380096
255.650536	10701.164343	27.385114
255.694641	10731.149100	27.390132
256.146075	10740.218179	27.395149
256.357823	10762.074794	27.400167
256.341603	10777.733990	27.405184
256.866136	10802.676690	27.410202
256.827274	10809.614063	27.415220
257.439939	10822.736882	27.420237
257.622740	10857.721498	27.425255
258.280101	10867.059082	27.430272
258.541180	10885.483454	27.435290
258.196754	10895.596424	27.440308
258.931999	10918.479797	27.445325
259.125486	10931.130378	27.450343
259.377976	10942.899089	27.455360
259.782901	10963.444825	27.460378
260.057720	10969.662075	27.465396
260.327390	10987.369549	27.470413
260.583467	11008.461497	27.475431
260.853156	11010.159176	27.480448
261.027140	11022.856822	27.485466
261.239154	11036.947457	27.490484
261.583377	11048.660504	27.495501
261.508385	11072.224609	27.500519
261.683625	11085.480544	27.505536
261.730643	11113.514408	27.510554
262.204739	11138.687661	27.515572
262.684373	11149.323717	27.520589
262.773265	11175.385463	27.525607
262.972663	11182.777551	27.530624
263.273037	11198.234416	27.535642
263.352310	11222.887900	27.540660
263.779853	11236.230867	27.545677
264.067913	11256.823178	27.550695
264.200974	11271.290253	27.555712
264.338838	11288.314638	27.560730
264.636553	11315.182187	27.565748
265.416099	11328.784363	27.570765
265.439180	11346.370207	27.575783
266.222726	11347.770749	27.580800
266.019297	11358.151400	27.585818
266.410298	11374.007818	27.590836
267.137160	11389.993719	27.595853
267.036786	11391.766563	27.600871
267.495726	11395.670867	27.605888
267.606271	11418.439692	27.610906
267.612397	11432.206167	27.615924
268.226101	11451.212183	27.620941
268.066383	11459.293691	27.625959
268.818263	11473.042087	27.630976
268.943213	11486.281792	27.635994
268.706557	11501.508738	27.641012
269.423319	11514.373535	27.646029
269.077726	11537.279194	27.651047
269.524889	11550.432768	27.656064
270.128981	11576.638396	27.661082
270.037856	11586.525887	27.666100
270.535512	11599.411119	27.671117
270.606938	11626.126774	27.676135
270.835052	11647.815190	27.681152
271.519157	11672.064057	27.686170
271.397809	11688.397796	27.691188
271.787150	11706.793868	27.696205
272.167466	11725.342135	27.701223
272.429237	11758.746726	27.706240
272.349205	11772.726974	27.711258
272.472295	11798.626323	27.716276
273.701872	11805.458990	27.721293
273.814763	11812.386407	27.726311
274.677784	11822.552725	27.731328
275.403508	11830.497434	27.736346
275.505431	11828.224736	27.741364
275.755571	11825.161362	27.746381
276.308332	11824.673239	27.751399
275.962704	11825.472391	27.756416
276.347726	11831.990824	27.761434
276.543155	11846.658670	27.766452
276.844897	11840.417514	27.771469
276.715874	11857.306989	27.776487
276.622221	11857.493347	27.781504
277.349989	11877.112798	27.786522
277.158052	11892.187584	27.791540
277.259436	11907.947072	27.796557
277.711161	11933.905455	27.801575
278.004570	11955.051608	27.806592
278.240662	11963.443592	27.811610
278.110799	11988.981360	27.816628
278.659292	11993.746447	27.821645
278.692256	12019.724296	27.826663
278.804467	12042.444792	27.831680
278.963243	12064.698802	27.836698
279.176449	12096.704084	27.841716
279.447520	12109.892509	27.846733
279.567526	12146.624366	27.851751
279.824491	12176.269095	27.856768
279.877305	12206.602897	27.861786
280.378419	12229.062046	27.866804
281.242757	12247.138462	27.871821
281.514650	12276.303799	27.876839
281.788020	12300.773125	27.881856
282.443429	12315.716619	27.886874
282.646751	12339.343803	27.891892
282.739868	12345.504094	27.896909
283.592792	12350.156228	27.901927
284.170531	12349.993829	27.906944
284.703870	12367.920160	27.911962
284.699262	12377.050811	27.916980
285.445281	12370.317405	27.921997
285.375511	12369.967651	27.927015
285.448957	12373.963568	27.932032
285.887373	12390.620521	27.937050
285.927799	12397.920370	27.942068
286.158937	12404.003586	27.947085
286.185263	12428.977897	27.952103
286.604390	12445.351952	27.957120
286.750325	12460.025622	27.962138
286.737336	12478.164907	27.967156
287.395131	12494.450894	27.972173
287.621896	12505.935640	27.977191
287.929910	12527.121587	27.982208
288.246366	12536.748533	27.987226
288.387231	12562.795713	27.992244
288.686073	12572.058868	27.997261
288.777556	12605.294710	28.002279
288.910909	12615.671144	28.007296
289.334540	12633.843258	28.012314
289.365738	12666.194497	28.017332
289.957417	12685.529988	28.022349
290.221947	12712.353935	28.027367
290.741568	12735.118962	28.032384
291.035292	12749.685325	28.037402
291.270193	12759.920316	28.042420
291.589246	12782.841755	28.047437
291.758958	12800.848495	28.052455
291.843109	12815.684279	28.057472
292.640319	12834.749279	28.062490
292.522824	12866.123844	28.067508
293.117155	12876.545062	28.072525
293.374750	12881.913923	28.077543
293.753660	12903.921832	28.082560
294.236586	12909.753074	28.087578
294.771101	12928.421601	28.092596
294.825956	12923.702405	28.097613
294.948039	12946.245164	28.102631
295.258417	12957.729718	28.107648
295.634665	12954.265322	28.112666
295.674836	12987.780350	28.117684
295.670746	12999.816095	28.122701
295.834804	13012.871025	28.127719
296.036257	13031.987042	28.132736
296.505894	13054.275511	28.137754
296.631037	13090.632841	28.142772
296.874635	13100.003029	28.147789
297.086825	13133.597329	28.152807
297.241992	13167.507009	28.157824
297.648065	13179.121124	28.162842
298.182646	13210.010581	28.167860
298.503313	13237.892563	28.172877
299.086861	13261.004986	28.177895
299.062149	13275.999279	28.182912
299.418342	13298.020232	28.187930
299.547193	13329.993232	28.192948
300.242041	13344.350012	28.197965
300.913317	13361.224298	28.202983
300.871665	13380.978855	28.208000
301.739795	13402.130574	28.213018
302.002816	13409.143229	28.218036
302.242692	13426.630376	28.223053
302.559978	13426.444936	28.228071
302.704563	13444.423377	28.233088
303.095470	13444.607310	28.238106
303.483511	13461.434647	28.243124
303.619441	13477.770030	28.248141
303.966735	13500.994271	28.253159
304.301989	13517.865508	28.258176
304.715559	13520.614598	28.263194
304.667857	13538.467437	28.268212
305.020137	13549.222310	28.273229
305.581346	13569.331315	28.278247
305.626610	13582.838632	28.283264
306.003577	13602.929024	28.288282
306.005333	13630.702942	28.293300
306.278757	13644.105856	28.298317
306.431758	13673.936954	28.303335
306.390852	13697.478618	28.308352
307.093416	13721.110836	28.313370
307.294855	13746.425742	28.318388
307.554784	13760.601502	28.323405
307.934596	13784.997596	28.328423
308.156773	13815.788888	28.333440
308.745664	13846.863652	28.338458
308.682528	13881.948036	28.343476
308.912185	13902.638748	28.348493
309.261452	13930.276051	28.353511
308.965457	13957.820711	28.358528
309.614595	13991.089632	28.363546
309.752984	14012.317958	28.368564
310.215549	14041.711934	28.373581
311.086977	14069.034034	28.378599
311.147880	14100.666787	28.383616
311.531657	14110.464180	28.388634
311.937358	14133.780742	28.393652
312.377388	14153.053603	28.398669
312.876428	14172.705393	28.403687
312.978728	14192.044429	28.408704
313.211783	14216.207858	28.413722
313.445554	14252.818001	28.418740
313.606514	14266.913268	28.423757
314.139042	14291.180437	28.428775
314.288285	14310.732177	28.433792
314.293864	14332.717012	28.438810
314.652386	14372.184179	28.443828
315.044503	14397.649363	28.448845
315.465750	14428.179787	28.453863
315.762838	14454.957514	28.458880
316.348261	14475.351694	28.463898
316.474788	14504.726602	28.468916
317.263267	14526.187900	28.473933
317.508405	14543.126293	28.478951
317.587729	14561.614782	28.483968
318.219716	14577.889502	28.488986
318.162164	14605.740468	28.494004
318.497296	14625.314746	28.499021
319.140212	14643.486487	28.504039
319.493173	14666.802128	28.509056
319.822736	14684.980459	28.514074
320.153838	14702.058747	28.519092
320.137653	14720.121185	28.524109
321.242149	14744.965331	28.529127
321.575061	14761.766080	28.534144
321.927351	14775.038734	28.539162
322.143491	14801.487697	28.544180
322.205897	14802.564228	28.549197
322.375854	14812.886327	28.554215
322.502270	14833.831030	28.559232
323.498784	14861.180767	28.564250
323.801542	14878.167524	28.569268
324.005706	14884.636780	28.574285
324.642288	14902.607213	28.579303
325.091647	14920.114271	28.584320
325.247028	14920.545971	28.589338
325.297112	14930.454444	28.594356
325.372876	14942.044406	28.599373
325.929817	14958.919101	28.604391
325.917281	14989.903181	28.609408
326.363336	14997.661497	28.614426
326.884533	15021.957217	28.619444
327.039275	15050.422994	28.624461
327.338232	15054.731852	28.629479
327.397842	15083.418333	28.634496
327.861967	15092.099082	28.639514
327.977253	15122.533604	28.644532
328.162437	15136.859439	28.649549
328.802612	15156.797833	28.654567
328.746923	15176.900881	28.659584
329.143738	15195.316703	28.664602
329.504616	15215.290629	28.669620
329.741943	15241.641907	28.674637
330.147079	15263.445808	28.679655
330.343515	15300.090570	28.684672
330.774374	15314.906289	28.689690
330.919835	15345.140600	28.694708
331.067693	15370.513565	28.699725
331.586074	15395.416353	28.704743
331.702726	15429.938174	28.709760
332.218920	15452.008468	28.714778
332.826567	15485.590261	28.719796
332.953862	15516.290347	28.724813
333.407713	15543.028059	28.729831
333.320617	15572.580467	28.734848
334.106094	15596.290352	28.739866
334.626655	15615.449277	28.744884
335.124011	15652.548246	28.749901
335.794043	15649.444964	28.754919
335.774599	15677.365306	28.759936
335.935598	15690.218495	28.764954
336.459105	15715.996880	28.769972
336.320087	15747.946637	28.774989
336.880342	15770.946103	28.780007
337.494705	15794.386742	28.785024
338.286823	15803.151244	28.790042
338.463777	15826.280177	28.795060
338.811300	15843.156545	28.800077
339.305362	15853.288139	28.805095
339.112065	15878.903100	28.810112
339.622225	15888.017871	28.815130
339.796648	15917.443836	28.820148
340.046014	15939.118020	28.825165
340.395554	15957.865096	28.830183
340.639386	15989.156161	28.835200
341.233281	16011.651652	28.840218
341.562848	16015.149079	28.845236
341.251203	16052.768058	28.850253
341.846189	16077.306226	28.855271
342.122077	16108.008215	28.860288
342.189299	16139.939298	28.865306
342.508908	16162.219879	28.870324
342.967032	16191.148234	28.875341
343.813724	16223.076328	28.880359
343.955860	16248.533727	28.885376
344.368022	16260.993059	28.890394
345.248451	16292.259270	28.895412
345.330826	16319.686621	28.900429
346.044255	16337.029991	28.905447
345.920077	16360.016383	28.910464
346.322398	16377.554250	28.915482
346.705906	16400.223984	28.920500
346.857370	16415.243350	28.925517
347.220453	16431.953718	28.930535
347.184241	16460.675148	28.935552
347.455458	16480.020152	28.940570
348.283105	16506.403723	28.945588
348.360413	16527.979975	28.950605
348.687903	16556.798342	28.955623
348.866334	16581.402511	28.960640
348.985261	16611.277793	28.965658
349.198592	16634.675748	28.970676
349.956089	16673.862795	28.975693
350.842102	16699.187827	28.980711
350.657710	16726.050752	28.985728
350.967672	16751.907810	28.990746
351.147224	16772.360271	28.995764
351.440317	16809.014660	29.000781
351.949562	16834.356649	29.005799
352.048431	16868.789041	29.010816
352.328304	16900.872641	29.015834
352.913782	16934.976068	29.020852
353.327490	16963.592874	29.025869
354.174285	16991.782063	29.030887
354.354952	17017.933392	29.035904
354.704764	17042.482636	29.040922
355.655541	17063.238168	29.045940
355.602041	17094.774907	29.050957
356.283211	17103.257449	29.055975
356.746795	17136.294534	29.060992
356.897858	17160.552805	29.066010
357.045496	17169.084576	29.071028
357.409477	17199.244771	29.076045
357.976544	17216.987259	29.081063
358.591498	17254.455976	29.086080
358.568662	17266.598824	29.091098
359.528637	17274.692151	29.096116
359.616131	17294.382017	29.101133
360.075898	17309.843279	29.106151
360.172214	17338.313715	29.111168
360.539719	17356.997617	29.116186
360.924929	17375.925966	29.121204
360.868404	17397.279081	29.126221
361.528385	17418.221983	29.131239
361.388718	17454.812604	29.136256
361.942914	17481.010704	29.141274
362.489992	17502.001238	29.146292
362.585018	17542.272835	29.151309
363.057326	17559.667029	29.156327
363.252566	17587.136311	29.161344
363.422964	17622.716479	29.166362
363.660029	17645.875556	29.171380
363.899606	17686.146144	29.176397
364.627734	17717.060758	29.181415
365.089658	17753.891266	29.186432
365.254329	17782.157126	29.191450
365.742151	17798.208914	29.196468
365.772973	17829.947096	29.201485
366.356305	17848.942093	29.206503
366.448647	17883.442340	29.211520
366.759751	17917.475108	29.216538
367.183946	17948.731146	29.221556
367.732468	17970.029972	29.226573
368.325317	17995.536529	29.231591
368.644139	18031.417616	29.236608
368.837090	18064.831707	29.241626
369.309599	18084.417516	29.246644
369.354300	18125.891220	29.251661
369.799091	18164.099521	29.256679
370.768716	18186.000872	29.261696
370.709270	18220.389034	29.266714
371.040764	18244.463145	29.271732
371.477647	18278.666041	29.276749
372.293891	18304.110340	29.281767
372.555214	18331.147933	29.286784
372.777983	18368.611745	29.291802
373.458828	18385.109794	29.296820
373.415873	18414.199311	29.301837
373.866714	18435.878934	29.306855
374.426204	18460.293061	29.311872
374.297644	18499.726309	29.316890
374.842195	18520.936357	29.321908
375.077957	18559.641177	29.326925
375.517383	18592.472982	29.331943
375.781180	18633.001625	29.336960
375.955521	18663.865800	29.341978
376.947475	18688.925613	29.346996
377.195637	18730.997693	29.352013
377.809645	18752.816340	29.357031
378.484153	18786.340691	29.362048
378.624557	18815.717515	29.367066
379.239837	18847.927289	29.372084
379.239217	18876.859328	29.377101
379.797464	18900.732949	29.382119
380.110983	18927.467163	29.387136
379.547218	18955.633871	29.392154
380.627165	18987.699018	29.397172
381.197505	19028.944492	29.402189
381.750778	19054.215362	29.407207
382.064581	19081.758155	29.412224
382.168020	19109.310497	29.417242
382.533246	19141.391803	29.422260
382.816799	19171.699749	29.427277
383.468026	19213.467926	29.432295
384.135193	19250.778383	29.437312
384.221375	19273.715460	29.442330
384.549462	19303.008166	29.447348
384.320971	19335.088790	29.452365
384.551393	19370.838592	29.457383
385.361639	19410.422610	29.462400
385.378259	19450.154842	29.467418
386.279754	19481.938768	29.472436
386.697123	19518.717537	29.477453
387.299615	19529.751332	29.482471
387.606833	19564.832158	29.487488
387.933647	19589.913566	29.492506
388.666238	19608.126974	29.497524
388.950189	19632.931773	29.502541
389.279766	19662.446602	29.507559
389.674953	19683.624542	29.512576
389.783682	19710.556922	29.517594
390.497800	19738.315080	29.522612
390.835104	19768.436847	29.527629
391.190562	19796.896455	29.532647
391.586928	19811.373296	29.537664
392.067815	19850.395846	29.542682
392.682786	19865.944388	29.547700
392.675143	19896.906535	29.552717
393.231825	19922.011701	29.557735
393.622922	19949.404309	29.562752
393.968501	19984.231492	29.567770
394.602848	19997.512118	29.572788
394.651894	20036.116451	29.577805
395.090720	20056.426372	29.582823
395.508145	20085.782304	29.587840
395.857853	20121.745560	29.592858
396.541441	20140.431263	29.597876
396.776486	20166.749700	29.602893
396.853374	20201.323271	29.607911
397.192645	20230.953394	29.612928
397.672789	20263.750713	29.617946
398.159998	20295.691692	29.622964
398.593424	20325.434574	29.627981
398.925730	20357.008156	29.632999
399.594068	20387.748577	29.638016
399.427878	20426.320430	29.643034
400.092966	20453.372563	29.648052
400.584262	20496.367524	29.653069
400.662247	20532.975926	29.658087
401.209419	20563.929738	29.663104
401.287017	20593.740061	29.668122
402.345205	20624.596033	29.673140
403.050603	20663.213096	29.678157
403.260475	20685.846636	29.683175
403.739365	20715.657044	29.688192
403.716046	20748.217412	29.693210
404.471234	20775.409321	29.698228
404.794006	20801.760522	29.703245
405.019605	20830.109591	29.708263
405.633695	20854.474652	29.713280
405.884783	20895.899158	29.718298
406.509354	20919.160032	29.723316
406.949537	20955.941680	29.728333
407.155343	20979.823040	29.733351
407.728335	21011.085504	29.738368
407.868413	21036.087923	29.743386
408.572612	21051.954217	29.748404
409.006544	21074.831423	29.753421
409.608366	21107.966320	29.758439
409.705515	21114.318384	29.763456
410.009636	21148.025337	29.768474
410.452398	21163.686093	29.773492
410.361829	21189.824203	29.778509
410.736018	21230.610134	29.783527
411.636143	21245.052141	29.788544
411.485264	21287.484479	29.793562
412.036276	21320.077382	29.798580
412.550733	21346.517094	29.803597
412.945281	21381.084379	29.808615
413.189378	21419.585408	29.813632
413.462043	21446.807315	29.818650
414.139082	21476.792372	29.823668
414.172245	21523.476696	29.828685
414.540585	21565.756954	29.833703
415.520518	21598.413626	29.838720
415.852484	21633.035540	29.843738
416.276991	21673.924864	29.848756
416.847430	21704.195917	29.853773
416.980976	21742.805923	29.858791
417.499223	21774.611846	29.863808
417.772673	21815.431087	29.868826
418.770568	21839.373426	29.873844
419.417256	21868.612664	29.878861
419.700856	21897.751491	29.883879
420.212057	21915.631096	29.888896
420.642384	21950.187624	29.893914
420.893239	21978.476444	29.898932
421.573067	21993.217313	29.903949
421.613520	22023.938096	29.908967
422.107356	22058.293345	29.913984
422.630291	22097.799949	29.919002
423.016475	22124.162157	29.924020
423.606918	22156.177886	29.929037
423.783090	22191.765507	29.934055
424.040196	22216.747207	29.939072
424.426483	22256.501246	29.944090
424.633588	22293.230986	29.949108
424.983440	22327.874412	29.954125
425.325074	22363.891321	29.959143
425.774404	22404.151600	29.964160
425.999682	22450.280309	29.969178
426.404115	22487.172036	29.974196
426.885069	22525.071684	29.979213
427.066355	22566.458907	29.984231
428.068614	22596.213111	29.989248
428.350034	22655.769527	29.994266
428.398554	22693.969261	29.999284
429.168316	22735.006385	30.004301
429.540857	22774.686718	30.009319
429.794929	22822.748819	30.014336
430.186492	22863.156521	30.019354
430.942117	22897.316706	30.024372
431.441431	22919.735610	30.029389
431.938607	22957.707748	30.034407
432.733716	22986.227514	30.039424
432.858059	23022.807499	30.044442
433.297636	23055.727354	30.049460
433.992471	23090.920853	30.054477
434.062911	23113.149208	30.059495
434.731058	23151.852332	30.064512
434.825496	23186.965254	30.069530
435.306308	23218.975389	30.074548
435.734859	23251.379888	30.079565
436.010445	23290.258533	30.084583
436.860520	23322.944186	30.089600
437.166431	23356.506671	30.094618
437.718203	23383.199056	30.099636
438.102206	23415.400668	30.104653
438.827178	23444.370400	30.109671
439.285551	23477.160524	30.114688
439.677088	23512.729391	30.119706
440.487658	23525.283864	30.124724
441.306329	23545.270726	30.129741
441.653764	23573.799854	30.134759
442.055464	23586.593602	30.139776
442.505192	23615.264052	30.144794
442.822738	23633.682955	30.149812
443.520488	23655.920832	30.154829
443.709318	23687.152108	30.159847
444.113983	23702.850598	30.164864
444.154600	23740.727193	30.169882
444.290352	23771.120285	30.174900
444.786783	23800.450832	30.179917
444.664876	23845.725129	30.184935
445.259815	23882.165942	30.189952
445.750078	23933.159572	30.194970
446.065704	23976.660664	30.199988
446.339617	24018.111735	30.205005
446.563809	24072.104581	30.210023
446.926744	24109.184707	30.215040
447.420238	24170.067910	30.220058
448.161890	24215.708257	30.225076
448.904535	24243.844767	30.230093
449.395760	24286.016574	30.235111
450.419306	24315.801339	30.240128
450.818577	24353.248851	30.245146
451.053227	24391.411964	30.250164
451.780655	24427.854972	30.255181
451.901976	24466.585387	30.260199
452.743122	24503.112859	30.265216
453.009750	24539.619293	30.270234
453.026432	24565.746637	30.275252
453.980284	24597.744838	30.280269
454.261363	24636.985107	30.285287
454.827001	24679.721170	30.290304
455.355799	24708.096600	30.295322
455.709442	24745.750818	30.300340
455.972354	24771.889689	30.305357
456.372276	24803.454254	30.310375
456.822520	24833.885916	30.315392
457.225626	24863.093058	30.320410
457.412717	24898.224123	30.325428
457.924457	24927.835539	30.330445
458.611148	24978.040996	30.335463
458.811076	25013.426298	30.340480
459.315184	25053.378090	30.345498
459.689556	25091.657686	30.350516
459.978819	25124.674293	30.355533
460.298513	25180.540058	30.360551
460.984753	25216.673944	30.365568
461.715998	25247.422438	30.370586
461.685444	25297.101099	30.375604
462.460911	25332.271731	30.380621
462.762637	25390.746355	30.385639
463.223687	25428.236955	30.390656
463.946487	25473.032272	30.395674
464.138659	25509.101356	30.400692
464.888840	25553.054302	30.405709
465.295077	25602.186118	30.410727
465.633221	25638.741168	30.415744
466.313765	25677.391716	30.420762
466.516389	25723.490931	30.425780
467.275098	25760.701693	30.430797
467.868519	25803.303968	30.435815
468.264216	25838.867098	30.440832
468.889352	25880.216605	30.445850
469.387479	25925.600456	30.450868
469.852584	25954.523965	30.455885
470.182230	26005.204700	30.460903
470.979401	26038.357350	30.465920
471.878208	26061.604135	30.470938
472.102250	26098.664503	30.475956
472.622781	26128.594235	30.480973
472.951744	26150.766708	30.485991
473.250524	26189.116895	30.491008
473.975096	26225.159495	30.496026
474.203548	26266.626762	30.501044
474.595180	26310.844527	30.506061
474.934041	26353.740924	30.511079
475.563550	26393.442865	30.516096
476.132740	26439.569245	30.521114
476.184340	26481.764854	30.526132
476.797616	26520.210694	30.531149
477.039328	26563.762868	30.536167
477.618686	26605.576915	30.541184
477.997095	26640.289733	30.546202
478.231042	26689.453096	30.551220
478.690365	26732.113855	30.556237
479.062869	26788.094172	30.561255
479.689175	26832.680949	30.566272
479.953023	26890.733710	30.571290
479.955399	26934.854463	30.576308
481.179154	26994.188627	30.581325
481.104520	27042.921611	30.586343
481.734619	27087.935522	30.591360
482.541660	27137.037314	30.596378
482.801918	27182.064705	30.601396
483.230514	27234.361318	30.606413
483.274127	27287.434840	30.611431
484.010774	27331.135573	30.616448
484.559278	27385.265139	30.621466
484.752750	27434.196110	30.626484
485.444836	27492.468031	30.631501
485.956814	27547.760607	30.636519
486.352098	27592.662047	30.641536
487.100902	27649.992610	30.646554
487.321201	27706.317084	30.651572
488.268453	27757.335127	30.656589
488.251769	27810.632701	30.661607
489.234050	27867.704646	30.666624
489.704036	27912.747930	30.671642
489.941372	27966.667410	30.676660
490.533794	28009.720055	30.681677
491.036909	28073.547579	30.686695
491.701874	28127.396320	30.691712
492.410874	28171.188821	30.696730
492.420655	28227.495054	30.701748
492.605405	28290.895074	30.706765
493.548420	28345.932597	30.711783
493.999821	28398.221445	30.716800
494.714946	28448.764893	30.721818
495.057076	28508.968387	30.726836
496.014293	28554.832532	30.731853
496.193075	28614.967882	30.736871
496.869828	28659.620986	30.741888
497.850179	28704.942902	30.746906
497.936926	28759.188420	30.751924
498.562261	28801.700524	30.756941
498.573527	28865.615802	30.761959
498.910944	28908.342673	30.766976
499.628670	28952.525148	30.771994
500.084919	29013.517639	30.777012
500.875449	29060.722540	30.782029
501.241609	29117.802459	30.787047
502.053778	29167.952871	30.792064
502.772013	29213.855366	30.797082
503.414031	29259.459661	30.802100
504.168024	29304.162116	30.807117
504.335185	29343.740047	30.812135
504.834281	29385.416440	30.817152
505.687119	29423.254184	30.822170
505.820754	29466.826618	30.827188
506.094198	29517.825131	30.832205
506.762141	29559.897445	30.837223
507.622180	29594.235683	30.842240
508.888791	29611.226572	30.847258
509.606648	29644.211698	30.852276
510.325852	29652.990484	30.857293
510.253542	29682.172519	30.862311
510.664677	29700.716620	30.867328
511.175270	29722.548262	30.872346
511.438622	29760.524816	30.877364
511.861770	29783.046587	30.882381
512.259303	29818.511763	30.887399
512.285164	29851.698943	30.892416
512.685700	29883.847785	30.897434
513.141089	29925.278774	30.902452
513.222260	29978.139143	30.907469
514.016207	30017.830058	30.912487
514.618973	30065.097718	30.917504
515.802730	30106.714176	30.922522
516.234624	30148.035994	30.927540
516.952191	30185.220918	30.932557
517.556290	30218.171737	30.937575
518.194384	30246.431513	30.942592
519.004126	30277.020246	30.947610
519.244858	30309.874672	30.952628
519.918397	30342.343430	30.957645
520.421292	30370.968545	30.962663
520.544310	30407.247856	30.967680
521.476678	30436.852784	30.972698
521.285750	30481.905984	30.977716
521.866437	30518.330144	30.982733
522.730044	30549.883267	30.987751
522.931606	30592.819005	30.992768
523.447714	30640.864970	30.997786
523.502705	30680.432473	31.002804
524.049895	30717.116165	31.007821
524.283590	30768.039786	31.012839
524.988357	30822.225215	31.017856
525.850616	30866.941493	31.022874
526.097462	30918.887978	31.027892
526.545849	30980.859952	31.032909
527.030339	31021.396971	31.037927
527.201155	31067.809542	31.042944
527.870969	31118.308569	31.047962
528.007991	31183.894612	31.052980
529.129751	31224.775109	31.057997
529.368451	31279.219113	31.063015
529.646931	31343.618462	31.068032
530.539236	31395.835622	31.073050
530.942854	31456.672201	31.078068
531.701263	31514.651579	31.083085
532.325248	31566.863156	31.088103
533.062130	31616.813966	31.093120
533.243303	31674.655720	31.098138
533.934713	31715.892856	31.103156
534.775503	31767.358084	31.108173
535.520245	31816.512252	31.113191
535.801923	31874.855703	31.118208
536.085766	31915.136852	31.123226
536.458915	31969.186570	31.128244
536.646836	32015.580165	31.133261
537.416214	32060.691204	31.138279
537.621216	32120.633447	31.143296
538.460833	32173.915983	31.148314
538.896143	32224.971189	31.153332
539.737957	32268.777141	31.158349
540.358396	32325.192456	31.163367
540.520756	32379.521411	31.168384
541.301348	32421.231601	31.173402
541.580482	32474.826634	31.178420
541.898080	32536.680258	31.183437
542.707430	32595.205444	31.188455
543.239635	32654.725496	31.193472
543.955689	32712.923898	31.198490
544.392994	32768.379963	31.203508
544.814453	32820.739677	31.208525
545.325341	32878.071253	31.213543
545.423128	32939.069181	31.218560
546.153391	32994.241313	31.223578
546.763127	33061.996335	31.228596
546.984061	33127.400156	31.233613
547.590051	33199.604815	31.238631
548.616320	33253.590953	31.243648
550.140450	33299.977096	31.248666
550.442603	33354.463528	31.253684
550.947598	33396.116028	31.258701
551.873877	33456.241422	31.263719
551.896883	33518.421487	31.268736
552.417583	33557.235956	31.273754
552.950353	33606.107612	31.278772
553.462058	33659.789232	31.283789
554.033967	33713.444096	31.288807
554.175984	33777.680731	31.293824
555.279583	33836.578028	31.298842
555.436854	33893.723504	31.303860
555.873474	33952.747935	31.308877
556.319310	34011.365961	31.313895
556.694276	34077.549810	31.318912
558.236342	34121.556539	31.323930
559.043220	34170.438219	31.328948
559.841849	34228.127463	31.333965
560.474208	34267.873259	31.338983
560.517583	34317.682543	31.344000
561.173640	34362.193610	31.349018
561.684061	34400.622293	31.354036
562.310637	34456.537817	31.359053
563.237715	34500.794841	31.364071
563.626786	34554.268705	31.369088
564.128012	34589.391809	31.374106
565.149422	34629.998756	31.379124
566.022896	34669.240465	31.384141
567.120148	34696.012729	31.389159
567.264957	34732.632248	31.394176
567.693512	34759.575749	31.399194
568.304711	34785.843835	31.404212
568.494575	34818.284912	31.409229
569.415154	34841.647166	31.414247
569.568045	34880.814953	31.419264
570.366980	34909.799638	31.424282
571.031469	34934.218089	31.429300
571.348724	34969.603043	31.434317
571.830518	35007.102801	31.439335
572.114675	35051.969750	31.444352
572.659866	35087.082170	31.449370
572.746701	35142.535737	31.454388
573.105243	35194.247624	31.459405
573.990891	35234.846136	31.464423
573.778850	35289.605230	31.469440
574.028001	35346.848242	31.474458
574.877798	35406.035874	31.479476
575.047017	35474.703281	31.484493
575.841021	35553.115662	31.489511
575.854950	35617.975706	31.494528
577.028358	35676.155763	31.499546
577.492571	35757.582469	31.504564
577.650677	35830.770072	31.509581
578.640407	35893.662672	31.514599
579.331990	35965.838850	31.519616
580.106507	36034.382187	31.524634
581.332591	36097.854374	31.529652
581.793631	36148.371973	31.534669
582.630598	36199.966616	31.539687
583.083476	36257.927614	31.544704
583.805464	36307.492829	31.549722
584.390806	36361.966023	31.554740
584.772537	36422.969262	31.559757
585.274808	36473.895935	31.564775
585.514497	36535.655355	31.569792
586.334484	36598.224448	31.574810
586.867507	36662.963275	31.579828
587.529615	36728.102769	31.584845
588.303653	36785.125178	31.589863
588.784755	36843.496790	31.594880
589.707554	36898.236470	31.599898
589.958201	36955.732255	31.604916
590.578121	37023.187921	31.609933
591.464016	37079.627468	31.614951
591.792628	37134.867762	31.619968
592.211512	37196.317247	31.624986
593.187333	37259.507286	31.630004
593.372238	37324.177945	31.635021
594.076474	37381.010082	31.640039
594.791324	37434.709271	31.645056
595.622273	37498.639125	31.650074
596.243823	37553.808908	31.655092
596.566644	37612.296679	31.660109
597.530620	37655.890753	31.665127
597.688907	37726.387088	31.670144
598.428029	37788.952972	31.675162
599.078082	37835.473574	31.680180
599.541694	37892.676876	31.685197
599.919924	37945.502556	31.690215
600.080898	38002.071663	31.695232
600.790705	38057.919676	31.700250
601.072397	38119.574114	31.705268
601.542120	38194.032658	31.710285
602.166925	38257.261823	31.715303
602.852421	38333.320219	31.720320
603.591566	38398.365570	31.725338
604.755433	38446.130578	31.730356
605.838646	38497.771872	31.735373
606.802926	38537.315640	31.740391
607.403050	38599.148176	31.745408
608.210373	38634.284588	31.750426
608.947011	38676.671766	31.755444
609.356131	38725.887060	31.760461
610.476324	38765.937943	31.765479
610.912084	38813.630710	31.770496
611.226962	38849.697507	31.775514
612.020665	38898.109342	31.780532
612.079859	38951.736403	31.785549
612.715978	39001.603876	31.790567
612.921423	39056.780152	31.795584
613.749585	39117.105422	31.800602
614.381517	39173.329041	31.805620
614.754432	39234.280721	31.810637
615.484978	39292.737729	31.815655
616.073431	39351.977649	31.820672
616.192272	39424.958360	31.825690
616.802009	39475.995207	31.830708
617.451157	39540.064198	31.835725
618.222955	39607.548521	31.840743
618.547734	39681.658177	31.845760
619.015347	39745.860927	31.850778
620.067639	39816.799142	31.855796
620.420697	39892.453803	31.860813
621.046166	39960.372838	31.865831
621.268375	40023.461347	31.870848
622.236262	40092.862379	31.875866
622.963445	40166.963675	31.880884
623.232015	40233.789406	31.885901
624.292044	40304.157529	31.890919
624.599476	40392.863675	31.895936
625.480073	40460.788224	31.900954
626.180245	40525.294350	31.905972
626.465166	40604.962394	31.910989
627.060351	40672.579970	31.916007
627.562672	40748.977936	31.921024
628.537631	40825.001336	31.926042
629.242028	40891.763382	31.931060
629.774847	40974.368036	31.936077
630.503064	41035.260081	31.941095
631.194600	41109.197641	31.946112
631.753729	41174.763242	31.951130
632.602576	41249.565843	31.956148
632.805172	41309.116845	31.961165
633.497596	41367.549154	31.966183
633.846920	41437.211833	31.971200
634.249910	41512.493472	31.976218
635.482949	41582.277825	31.981236
635.726338	41655.245020	31.986253
636.643895	41720.929113	31.991271
637.739140	41786.206643	31.996288
638.545662	41845.669641	32.001306
639.387579	41897.752351	32.006324
640.067806	41951.293041	32.011341
640.769260	41998.572261	32.016359
641.378044	42054.326392	32.021376
641.816430	42109.928036	32.026394
642.335646	42168.838564	32.031412
643.145555	42241.711720	32.036429
643.752052	42294.782592	32.041447
644.011088	42370.582982	32.046464
644.765116	42425.791549	32.051482
645.662010	42493.907640	32.056500
645.769991	42561.206433	32.061517
646.327550	42624.323618	32.066535
646.969531	42704.427133	32.071552
647.500309	42771.750902	32.076570
648.315769	42845.515287	32.081588
649.081037	42923.196441	32.086605
649.785715	42987.250499	32.091623
650.581290	43049.854999	32.096640
650.855948	43124.208254	32.101658
651.795053	43190.714691	32.106676
652.194816	43268.515526	32.111693
653.227133	43326.376677	32.116711
654.134639	43393.923634	32.121728
654.854620	43453.951690	32.126746
655.775357	43517.503264	32.131764
656.129246	43593.303353	32.136781
656.798580	43653.008922	32.141799
657.535888	43718.256100	32.146816
658.053485	43792.674481	32.151834
658.495320	43854.243528	32.156852
659.254771	43920.487978	32.161869
660.308937	43966.299945	32.166887
661.216307	44022.416668	32.171904
662.043501	44077.309680	32.176922
662.852654	44133.029127	32.181940
663.291087	44197.931348	32.186957
663.916335	44249.260629	32.191975
664.515570	44307.326504	32.196992
664.662332	44375.717693	32.202010
665.455522	44440.233076	32.207028
666.282955	44505.907373	32.212045
666.560619	44577.616305	32.217063
667.382228	44644.109150	32.222080
667.663055	44710.413879	32.227098
668.647641	44776.038932	32.232116
668.680632	44850.314985	32.237133
669.531141	44902.026764	32.242151
670.185802	44977.911171	32.247168
670.343207	45052.389115	32.252186
671.125777	45114.551957	32.257204
671.819966	45197.778849	32.262221
672.315381	45260.883934	32.267239
673.019712	45344.788224	32.272256
673.757787	45415.190531	32.277274
674.642402	45484.351962	32.282292
674.953528	45557.813752	32.287309
675.565053	45639.279632	32.292327
676.684758	45701.327779	32.297344
677.227959	45784.568874	32.302362
678.404435	45846.965018	32.307380
679.413362	45919.629418	32.312397
680.595645	45969.556238	32.317415
681.998491	46006.638429	32.322432
682.855707	46054.493874	32.327450
683.628172	46093.850476	32.332468
684.504805	46139.440855	32.337485
685.130610	46188.242181	32.342503
685.570414	46230.223476	32.347520
686.011855	46285.762227	32.352538
686.550680	46335.609541	32.357556
687.081073	46384.666394	32.362573
687.312480	46446.978504	32.367591
688.063174	46508.261605	32.372608
688.363953	46578.337491	32.377626
688.915558	46639.674832	32.382644
689.406991	46719.407389	32.387661
690.191032	46781.377122	32.392679
690.991367	46851.355625	32.397696
691.141498	46937.523398	32.402714
692.102678	47012.992317	32.407732
692.318960	47093.303609	32.412749
692.790051	47177.973178	32.417767
693.422704	47255.940794	32.422784
693.904595	47342.758198	32.427802
694.890317	47430.420329	32.432820
695.015364	47524.997627	32.437837
696.041858	47616.898146	32.442855
696.921525	47700.586951	32.447872
697.392000	47798.556398	32.452890
698.326046	47880.672315	32.457908
698.969228	47973.572870	32.462925
699.357863	48059.853274	32.467943
700.224350	48151.829372	32.472960
700.705539	48247.773780	32.477978
701.798341	48339.828418	32.482996
702.437063	48437.048834	32.488013
703.296357	48535.023548	32.493031
703.943389	48614.730391	32.498048
704.557346	48714.947729	32.503066
705.116298	48793.028497	32.508084
705.872366	48866.079761	32.513101
706.506118	48954.209368	32.518119
707.145727	49042.723463	32.523136
708.114352	49125.615910	32.528154
708.836577	49206.790270	32.533172
709.772173	49290.395609	32.538189
710.527783	49374.055239	32.543207
711.251555	49437.485994	32.548224
711.807562	49522.544513	32.553242
713.032305	49598.676721	32.558260
713.767482	49666.442440	32.563277
714.634360	49746.264503	32.568295
715.522085	49827.207057	32.573312
716.050835	49898.073921	32.578330
717.047881	49962.687478	32.583348
718.065891	50047.987369	32.588365
718.439763	50110.466359	32.593383
719.591046	50161.659653	32.598400
720.565263	50238.696013	32.603418
721.137128	50299.178055	32.608436
721.949466	50367.325471	32.613453
722.817809	50433.911542	32.618471
723.420848	50495.916727	32.623488
723.700606	50565.907509	32.628506
724.424203	50634.041663	32.633524
724.696691	50713.202087	32.638541
725.082558	50787.771862	32.643559
725.948808	50855.095161	32.648576
726.782392	50938.607669	32.653594
727.750008	51026.350326	32.658612
728.536073	51094.886559	32.663629
729.647576	51170.708947	32.668647
730.776774	51233.926878	32.673664
731.173442	51309.437586	32.678682
732.124210	51367.230780	32.683700
732.834571	51443.156048	32.688717
733.225272	51501.805753	32.693735
734.201611	51575.792447	32.698752
734.702541	51650.066584	32.703770
735.201066	51716.264958	32.708788
736.024189	51798.448091	32.713805
736.305873	51873.591262	32.718823
737.008504	51955.096785	32.723840
737.260685	52056.435061	32.728858
738.213537	52145.697317	32.733876
738.757427	52224.013184	32.738893
739.134007	52328.151650	32.743911
740.029587	52398.701686	32.748928
741.067748	52501.274503	32.753946
741.758927	52592.771045	32.758964
742.613438	52689.168977	32.763981
743.509819	52773.352261	32.768999
744.475695	52855.296529	32.774016
744.818492	52947.096507	32.779034
746.119556	53008.052315	32.784052
747.175330	53075.997618	32.789069
747.667414	53152.652887	32.794087
748.645147	53227.173225	32.799104
748.974962	53302.254681	32.804122
750.013576	53372.788897	32.809140
750.675449	53450.144360	32.814157
751.293902	53517.393926	32.819175
752.013661	53584.807531	32.824192
752.377368	53672.113095	32.829210
753.346839	53740.077778	32.834228
753.927328	53823.523945	32.839245
754.506874	53914.574598	32.844263
755.352340	53995.195357	32.849280
756.308009	54077.320366	32.854298
757.019342	54162.483334	32.859316
758.043324	54240.478945	32.864333
758.327243	54327.134314	32.869351
759.475280	54406.641814	32.874368
759.957073	54499.585942	32.879386
760.304311	54581.645928	32.884404
761.287630	54667.604451	32.889421
761.846349	54768.050424	32.894439
762.901269	54849.837975	32.899456
763.659559	54953.400365	32.904474
764.051420	55051.181821	32.909492
764.545760	55149.831358	32.914509
765.781750	55240.578932	32.919527
767.031201	55318.357004	32.924544
768.016012	55410.161864	32.929562
769.117534	55485.606112	32.934580
770.046519	55570.681006	32.939597
770.736420	55658.199814	32.944615
771.646068	55735.560229	32.949632
772.285747	55814.633891	32.954650
772.704918	55893.301039	32.959668
773.695980	55975.087989	32.964685
774.244399	56064.692662	32.969703
774.996090	56149.356494	32.974720
775.650518	56235.119006	32.979738
776.411306	56321.442697	32.984756
777.267366	56396.121590	32.989773
777.589059	56492.280280	32.994791
778.557885	56589.302486	32.999808
779.230073	56681.517025	33.004826
779.984906	56780.601062	33.009844
781.088760	56887.860341	33.014861
781.450319	56976.097476	33.019879
782.358455	57065.747615	33.024896
782.567751	57169.896031	33.029914
783.456919	57262.375689	33.034932
784.770950	57363.558518	33.039949
784.912992	57472.707507	33.044967
785.838551	57565.628035	33.049984
786.171361	57673.993294	33.055002
786.964224	57774.165796	33.060020
787.976389	57864.895611	33.065037
788.561176	57962.462868	33.070055
790.470610	58023.313277	33.075072
791.865978	58110.014722	33.080090
792.720484	58182.276342	33.085108
794.015651	58242.439100	33.090125
794.598494	58319.540308	33.095143
795.285831	58391.409436	33.100160
796.082430	58461.319740	33.105178
796.830331	58524.775133	33.110196
797.518936	58602.766815	33.115213
798.027479	58677.033463	33.120231
798.889529	58751.512512	33.125248
799.531727	58828.227501	33.130266
799.967808	58920.935921	33.135284
800.880651	58991.937937	33.140301
801.393932	59093.617573	33.145319
802.104197	59178.958555	33.150336
802.914558	59267.596097	33.155354
803.330919	59367.360324	33.160372
804.425291	59463.382972	33.165389
804.820900	59577.931530	33.170407
805.696201	59672.534538	33.175424
806.242640	59764.137086	33.180442
807.320275	59864.569133	33.185460
808.427950	59962.717216	33.190477
809.013531	60063.560182	33.195495
810.080146	60176.404730	33.200512
810.914405	60267.193483	33.205530
811.656832	60370.567598	33.210548
812.504572	60466.877773	33.215565
813.205594	60579.290341	33.220583
814.259948	60673.727802	33.225600
814.982693	60776.703104	33.230618
815.552661	60876.558254	33.235636
816.993899	60973.218631	33.240653
817.969046	61055.592502	33.245671
819.639068	61143.994719	33.250688
820.424830	61227.482577	33.255706
821.185630	61312.989411	33.260724
821.898267	61394.917097	33.265741
822.263813	61485.344234	33.270759
823.459853	61566.507335	33.275776
823.821052	61664.764150	33.280794
824.090448	61762.578203	33.285812
825.339126	61853.542316	33.290829
825.828178	61952.585520	33.295847
826.583654	62055.474162	33.300864
827.200496	62160.959094	33.305882
827.911782	62254.868539	33.310900
829.137022	62351.150345	33.315917
829.461743	62463.952954	33.320935
830.359168	62567.298625	33.325952
831.197675	62671.007926	33.330970
831.508066	62786.391622	33.335988
832.703651	62881.967135	33.341005
833.358876	62983.067223	33.346023
833.940627	63088.054441	33.351040
834.953048	63191.347303	33.356058
835.805516	63286.303631	33.361076
837.392795	63363.976188	33.366093
840.621405	63408.796416	33.371111
842.997484	63428.882494	33.376128
844.493175	63479.341112	33.381146
844.793155	63522.868638	33.386164
845.416840	63553.289132	33.391181
845.951771	63594.682448	33.396199
846.593138	63637.843253	33.401216
847.381506	63684.918946	33.406234
848.108253	63738.292411	33.411252
848.294092	63783.095633	33.416269
848.531251	63849.568356	33.421287
848.703697	63912.195488	33.426304
849.685683	63987.677255	33.431322
850.370696	64067.252224	33.436340
851.331916	64137.163681	33.441357
851.890083	64223.056941	33.446375
852.107388	64307.270962	33.451392
853.086532	64407.480639	33.456410
853.323128	64498.290006	33.461428
854.210396	64596.295032	33.466445
854.790789	64701.029188	33.471463
855.655367	64800.081102	33.476480
856.738681	64909.868618	33.481498
857.185416	65021.356189	33.486516
858.257478	65126.598713	33.491533
858.739300	65241.751996	33.496551
859.523755	65359.725636	33.501568
860.542388	65469.368716	33.506586
861.140108	65588.043054	33.511604
862.349957	65690.237786	33.516621
863.136446	65809.489869	33.521639
864.261787	65926.114591	33.526656
865.107902	66043.981529	33.531674
866.019469	66159.040309	33.536692
867.321850	66252.666829	33.541709
868.281819	66362.355901	33.546727
868.856513	66461.626725	33.551744
869.956488	66567.352768	33.556762
870.453748	66678.342799	33.561780
871.641527	66785.704859	33.566797
872.222112	66900.782811	33.571815
872.578649	67013.761834	33.576832
873.604591	67125.472592	33.581850
874.484422	67252.274288	33.586868
875.336961	67366.079819	33.591885
876.101870	67481.719399	33.596903
876.933209	67607.899378	33.601920
877.841345	67721.502295	33.606938
878.304127	67833.515211	33.611956
879.499074	67941.874378	33.616973
880.563115	68057.722479	33.621991
881.288222	68165.772277	33.627008
882.241589	68276.989450	33.632026
883.288758	68389.405345	33.637044
884.683491	68492.877400	33.642061
885.834028	68596.344637	33.647079
886.687275	68700.554696	33.652096
887.840357	68789.693581	33.657114
888.873331	68893.421178	33.662132
890.039547	68983.076926	33.667149
890.887314	69075.866948	33.672167
891.168640	69169.461482	33.677184
892.356764	69264.257916	33.682202
893.099837	69363.112350	33.687220
893.833994	69464.982451	33.692237
894.729332	69562.341532	33.697255
895.611848	69676.048320	33.702272
896.558177	69777.715687	33.707290
897.061419	69889.089445	33.712308
897.924038	69993.431238	33.717325
898.711174	70108.362494	33.722343
899.319213	70228.390259	33.727360
900.380450	70339.488218	33.732378
900.988412	70463.352700	33.737396
902.037248	70575.964074	33.742413
902.819651	70703.669220	33.747431
903.722585	70823.603125	33.752448
904.726064	70953.694719	33.757466
905.405731	71077.071416	33.762484
906.387487	71204.880763	33.767501
907.156300	71325.420364	33.772519
908.016367	71455.986701	33.777536
908.911508	71582.845491	33.782554
909.526848	71724.023903	33.787572
910.744663	71847.635698	33.792589
911.722961	71981.371395	33.797607
912.765697	72117.581095	33.802624
913.851112	72230.537260	33.807642
914.546403	72369.868691	33.812660
915.757458	72487.115918	33.817677
916.568474	72613.628148	33.822695
917.611489	72748.862647	33.827712
919.172421	72871.137080	33.832730
919.498111	72992.168015	33.837748
920.957298	73108.602140	33.842765
922.090621	73229.411214	33.847783
922.805750	73350.502414	33.852800
923.993397	73458.235772	33.857818
925.036870	73561.979806	33.862836
926.256985	73663.806750	33.867853
927.372133	73777.626369	33.872871
928.370096	73881.777426	33.877888
929.196244	73979.314494	33.882906
930.121334	74078.346676	33.887924
931.196435	74160.204011	33.892941
932.003690	74245.611702	33.897959
932.873301	74333.569303	33.902976
934.367235	74409.338361	33.907994
934.983515	74496.161515	33.913012
936.168177	74582.641820	33.918029
937.103972	74671.095945	33.923047
937.855582	74764.243786	33.928064
938.698564	74852.441722	33.933082
939.237332	74959.098229	33.938100
939.853098	75060.333208	33.943117
940.767358	75153.033527	33.948135
941.414709	75268.225260	33.953152
942.119055	75378.643295	33.958170
943.056153	75494.858297	33.963188
943.902528	75613.199305	33.968205
944.716380	75732.620597	33.973223
945.259563	75855.498537	33.978240
946.570252	75969.963020	33.983258
947.637030	76092.462039	33.988276
949.075982	76209.163784	33.993293
950.286736	76315.650984	33.998311
950.924596	76427.380957	34.003328
952.093643	76537.756638	34.008346
952.884282	76651.644059	34.013364
954.236228	76761.201801	34.018381
955.261189	76871.140820	34.023399
955.892318	76998.056758	34.028416
956.512636	77112.308833	34.033434
957.385853	77236.482542	34.038452
957.889729	77360.911705	34.043469
958.933098	77489.364219	34.048487
959.319160	77625.424783	34.053504
960.554651	77761.344787	34.058522
961.088652	77911.232458	34.063540
962.127262	78050.030050	34.068557
963.025193	78186.891491	34.073575
963.837506	78326.156769	34.078592
964.693033	78458.058521	34.083610
966.222709	78617.482957	34.088628
967.046851	78756.167727	34.093645
968.209992	78889.331756	34.098663
969.139045	79042.161000	34.103680
970.753959	79180.697533	34.108698
971.613414	79315.998616	34.113716
973.138841	79430.068995	34.118733
974.672849	79542.912311	34.123751
975.172119	79670.731720	34.128768
976.120063	79786.368806	34.133786
977.251921	79908.956101	34.138804
978.402725	80034.379432	34.143821
979.245931	80157.911763	34.148839
980.125416	80276.558851	34.153856
980.846415	80399.195438	34.158874
981.890503	80523.778970	34.163892
982.664549	80633.442930	34.168909
983.675028	80745.914599	34.173927
984.702850	80858.706521	34.178944
985.789556	80966.369093	34.183962
986.660751	81084.668087	34.188980
987.160101	81201.939558	34.193997
988.369902	81327.146350	34.199015
989.064413	81457.847386	34.204032
990.000388	81578.187152	34.209050
990.940388	81707.276538	34.214068
991.683497	81844.123504	34.219085
992.876835	81974.558748	34.224103
993.984139	82111.716201	34.229120
994.701880	82236.949812	34.234138
995.872213	82374.465635	34.239156
996.741128	82514.881614	34.244173
997.532038	82647.370222	34.249191
998.377616	82808.326468	34.254208
999.452856	82931.079585	34.259226
1000.513855	83080.990182	34.264244
1001.820117	83215.442498	34.269261
1003.026047	83351.068638	34.274279
1003.813218	83496.707522	34.279296
1004.932748	83641.466287	34.284314
1006.048804	83778.519388	34.289332
1007.097456	83907.655554	34.294349
1008.265298	84039.858996	34.299367
1009.743598	84176.566207	34.304384
1010.981309	84298.169655	34.309402
1012.029921	84434.852043	34.314420
1012.724702	84562.891423	34.319437
1014.086296	84682.346582	34.324455
1015.273126	84815.563487	34.329472
1016.361607	84943.220062	34.334490
1017.099018	85075.966314	34.339508
1018.115059	85210.755656	34.344525
1019.077967	85330.834295	34.349543
1019.863210	85468.431462	34.354560
1020.676201	85602.952070	34.359578
1021.571655	85737.454084	34.364596
1022.111239	85879.961794	34.369613
1023.080415	86020.277511	34.374631
1023.913594	86174.337277	34.379648
1025.204802	86317.145667	34.384666
1027.188607	86437.776333	34.389684
1029.286352	86558.357939	34.394701
1030.916874	86667.044309	34.399719
1032.047790	86780.098001	34.404736
1033.049902	86896.606427	34.409754
1034.403363	86994.715074	34.414772
1034.766613	87110.725545	34.419789
1036.266947	87194.748176	34.424807
1036.606300	87317.289486	34.429824
1037.466399	87418.956526	34.434842
1038.230859	87529.479747	34.439860
1039.139769	87651.217780	34.444877
1040.102200	87753.104092	34.449895
1040.137213	87877.872350	34.454912
1041.285925	87996.873931	34.459930
1042.249629	88122.216790	34.464948
1042.713739	88263.576021	34.469965
1043.676742	88388.142689	34.474983
1044.520468	88538.201957	34.480000
1045.652887	88672.058506	34.485018
1046.954275	88799.179196	34.490036
1048.165189	88937.843816	34.495053
1049.020073	89077.229980	34.500071
1049.656163	89220.933294	34.505088
1051.294866	89365.882053	34.510106
1052.429603	89514.263786	34.515124
1052.922050	89660.383402	34.520141
1054.185584	89806.627996	34.525159
1055.524622	89966.534859	34.530176
1056.242526	90114.993288	34.535194
1057.275410	90255.705753	34.540212
1058.010665	90413.770302	34.545229
1059.079578	90563.630571	34.550247
1060.204375	90723.475832	34.555264
1060.996980	90884.987874	34.560282
1062.090001	91044.138481	34.565300
1062.616740	91215.074739	34.570317
1064.220969	91382.836671	34.575335
1065.038388	91549.479029	34.580352
1066.479443	91713.986842	34.585370
1067.598970	91876.358594	34.590388
1068.682645	92039.249561	34.595405
1070.010172	92195.815874	34.600423
1071.284474	92362.524507	34.605440
1072.500932	92523.481416	34.610458
1073.930893	92662.248529	34.615476
1074.835614	92832.207342	34.620493
1076.098548	92985.905207	34.625511
1076.571593	93148.597812	34.630528
1077.691021	93306.318291	34.635546
1078.685033	93467.861383	34.640564
1079.446043	93634.756055	34.645581
1080.951319	93796.884379	34.650599
1081.898104	93953.308532	34.655616
1082.948289	94127.549086	34.660634
1084.501366	94281.045248	34.665652
1084.677440	94463.138342	34.670669
1086.188763	94631.673307	34.675687
1087.948443	94785.886494	34.680704
1089.314233	94941.112253	34.685722
1090.684361	95075.558035	34.690740
1091.343871	95234.257155	34.695757
1092.869609	95381.078726	34.700775
1094.259936	95536.336311	34.705792
1095.202517	95683.828257	34.710810
1096.357619	95810.044532	34.715828
1096.897345	95952.902057	34.720845
1097.996490	96090.294317	34.725863
1099.025774	96228.362766	34.730880
1100.029191	96367.271225	34.735898
1101.089138	96507.171088	34.740916
1102.111105	96656.984789	34.745933
1103.351709	96788.032505	34.750951
1104.145025	96955.737379	34.755968
1105.255402	97104.059595	34.760986
1106.207996	97250.750342	34.766004
1106.958487	97409.734884	34.771021
1108.596935	97555.021584	34.776039
1109.679400	97707.951540	34.781056
1110.838181	97869.031701	34.786074
1111.796989	98019.370514	34.791092
1112.633202	98184.673451	34.796109
1113.936212	98338.913802	34.801127
1115.782737	98486.545848	34.806144
1118.774957	98580.996970	34.811162
1121.045842	98692.879732	34.816180
1122.355794	98802.695126	34.821197
1123.186750	98919.141880	34.826215
1124.200620	99017.148786	34.831232
1125.017510	99127.075772	34.836250
1126.304061	99239.611235	34.841268
1126.640084	99368.267790	34.846285
1127.670772	99480.446512	34.851303
1128.416681	99611.310647	34.856320
1129.029543	99746.954673	34.861338
1130.072654	99871.907778	34.866356
1131.054122	100017.858654	34.871373
1132.091458	100157.778037	34.876391
1132.764867	100311.264863	34.881408
1133.781106	100455.321104	34.886426
1134.903340	100613.952260	34.891444
1135.478406	100777.208255	34.896461
1136.547929	100938.361980	34.901479
1137.466074	101097.402200	34.906496
1138.211135	101274.213429	34.911514
1139.550882	101444.395035	34.916532
1140.239003	101628.273246	34.921549
1141.538806	101810.113033	34.926567
1142.983870	101980.477946	34.931584
1144.366540	102159.984993	34.936602
1145.800957	102321.773616	34.941620
1146.345924	102507.820281	34.946637
1148.255775	102672.908471	34.951655
1149.824321	102835.198186	34.956672
1150.999012	103001.247198	34.961690
1152.591348	103160.972533	34.966708
1153.700419	103311.346948	34.971725
1155.016766	103473.915297	34.976743
1155.742194	103624.321065	34.981760
1156.714917	103788.806696	34.986778
1158.099618	103930.813293	34.991796
1159.036378	104086.054807	34.996813
1160.316654	104225.985112	35.001831
1161.808287	104362.041316	35.006848
1162.914303	104507.272513	35.011866
1163.780875	104638.291027	35.016884
1164.884065	104797.117923	35.021901
1165.907802	104943.858382	35.026919
1166.987145	105096.748587	35.031936
1168.309082	105249.215150	35.036954
1169.269997	105397.082214	35.041972
1170.167900	105561.186939	35.046989
1171.669308	105714.811394	35.052007
1172.708045	105881.016034	35.057024
1173.492924	106043.053532	35.062042
1175.109034	106193.833838	35.067060
1175.964958	106364.032743	35.072077
1177.059930	106532.391093	35.077095
1178.366164	106698.913267	35.082112
1179.512780	106867.689787	35.087130
1180.767515	107031.171853	35.092148
1181.899686	107203.915011	35.097165
1183.569719	107368.516868	35.102183
1184.883677	107529.018178	35.107200
1186.028660	107700.984352	35.112218
1186.927481	107855.230916	35.117236
1188.360213	108020.349623	35.122253
1189.359755	108183.626859	35.127271
1190.824608	108349.040169	35.132288
1191.780908	108526.472809	35.137306
1193.246376	108689.141345	35.142324
1193.745921	108876.890278	35.147341
1194.588888	109064.459454	35.152359
1195.814154	109246.209309	35.157376
1196.950104	109422.119751	35.162394
1198.084012	109608.570783	35.167412
1199.003045	109810.362808	35.172429
1200.601677	109991.862593	35.177447
1202.994277	110149.500449	35.182464
1204.044231	110339.388496	35.187482
1205.442686	110504.117948	35.192500
1206.733661	110676.278024	35.197517
1207.817295	110841.199037	35.202535
1209.368312	110995.931355	35.207552
1210.280271	111168.326025	35.212570
1211.939701	111327.917382	35.217588
1212.958714	111497.923505	35.222605
1214.265161	111665.346658	35.227623
1215.446681	111833.797318	35.232640
1216.796904	111997.487197	35.237658
1218.130235	112160.782023	35.242676
1219.093700	112323.991121	35.247693
1219.918182	112492.167476	35.252711
1221.481808	112667.051739	35.257728
1222.164624	112834.980706	35.262746
1223.183042	113005.408673	35.267764
1224.292421	113166.238746	35.272781
1225.417629	113336.550691	35.277799
1226.791049	113493.757717	35.282816
1228.041645	113650.649721	35.287834
1229.449713	113812.392384	35.292852
1230.564429	113977.614038	35.297869
1231.729371	114145.418120	35.302887
1233.418457	114300.167923	35.307904
1234.127658	114459.202243	35.312922
1235.434342	114635.293263	35.317940
1236.769946	114806.613628	35.322957
1237.989754	114975.623717	35.327975
1239.025452	115147.335937	35.332992
1240.137777	115324.374316	35.338010
1242.178891	115480.518866	35.343028
1243.799814	115655.756604	35.348045
1245.110662	115805.257455	35.353063
1246.223416	115962.527565	35.358080
1247.192561	116134.212690	35.363098
1248.792249	116291.546703	35.368116
1250.839211	116447.101087	35.373133
1252.316602	116594.041160	35.378151
1253.705282	116749.657708	35.383168
1255.021500	116909.769470	35.388186
1256.167719	117052.408693	35.393204
1257.315855	117199.594520	35.398221
1258.210563	117363.391476	35.403239
1259.742559	117510.752329	35.408256
1260.720296	117671.448164	35.413274
1261.276094	117833.320135	35.418292
1262.108721	118008.825877	35.423309
1263.116529	118187.806488	35.428327
1264.652753	118364.792092	35.433344
1265.259843	118554.926137	35.438362
1266.634507	118740.063899	35.443380
1267.500189	118935.560825	35.448397
1268.295880	119128.689468	35.453415
1270.044316	119323.162474	35.458432
1270.929903	119536.251469	35.463450
1272.274837	119737.415189	35.468468
1273.142868	119952.346712	35.473485
1274.450063	120156.204541	35.478503
1275.796107	120370.620232	35.483520
1276.871414	120596.225841	35.488538
1278.481308	120802.522884	35.493556
1279.732648	121000.012948	35.498573
1280.887758	121231.791881	35.503591
1282.302944	121439.467360	35.508608
1283.567966	121657.807299	35.513626
1284.872627	121868.784055	35.518644
1285.879780	122086.864536	35.523661
1287.254682	122317.250114	35.528679
1288.828871	122525.808072	35.533696
1289.748027	122747.758361	35.538714
1291.175149	122949.908703	35.543732
1292.288168	123155.783681	35.548749
1293.417482	123363.012936	35.553767
1295.369584	123564.286490	35.558784
1296.791617	123761.237890	35.563802
1298.226910	123962.913237	35.568820
1299.660902	124162.246975	35.573837
1300.477922	124358.120908	35.578855
1302.194798	124548.457169	35.583872
1303.532950	124750.533842	35.588890
1304.920219	124948.246771	35.593908
1306.508128	125144.434534	35.598925
1307.958339	125342.279666	35.603943
1309.134725	125534.824177	35.608960
1310.625960	125741.836788	35.613978
1311.619917	125943.077649	35.618996
1312.858041	126141.304310	35.624013
1313.832627	126344.654016	35.629031
1315.571207	126548.884547	35.634048
1316.698944	126769.390502	35.639066
1317.924732	126963.457351	35.644084
1319.430989	127167.716742	35.649101
1320.488585	127393.521406	35.654119
1322.005031	127602.228905	35.659136
1323.737786	127817.326432	35.664154
1324.508308	128021.316357	35.669172
1325.980217	128234.976384	35.674189
1327.081545	128456.602161	35.679207
1329.561233	128644.729970	35.684224
1330.480266	128853.744539	35.689242
1331.915960	129061.018934	35.694260
1333.821416	129269.449095	35.699277
1335.136725	129466.395086	35.704295
1337.016435	129664.937755	35.709312
1338.131360	129856.204549	35.714330
1339.531794	130053.812608	35.719348
1340.922740	130241.021978	35.724365
1342.429657	130438.527130	35.729383
1344.180762	130633.093522	35.734400
1345.102332	130826.665496	35.739418
1346.532170	131020.145345	35.744436
1347.785548	131221.864621	35.749453
1348.709586	131414.223914	35.754471
1350.087101	131615.748883	35.759488
1351.113132	131816.038790	35.764506
1352.380355	132025.997149	35.769524
1353.710063	132226.862521	35.774541
1355.255103	132425.756516	35.779559
1356.675932	132634.313865	35.784576
1357.453363	132846.788828	35.789594
1358.398372	133055.855663	35.794612
1360.179035	133279.159850	35.799629
1361.337833	133483.659688	35.804647
1362.978843	133705.329495	35.809664
1364.202170	133925.572202	35.814682
1365.341426	134131.841014	35.819700
1366.734697	134332.736343	35.824717
1367.689722	134537.909586	35.829735
1369.646513	134743.837416	35.834752
1370.949870	134935.323686	35.839770
1372.117212	135142.545577	35.844788
1373.553206	135348.281677	35.849805
1375.276729	135556.191089	35.854823
1376.445077	135758.855364	35.859840
1377.929961	135968.731752	35.864858
1379.520999	136174.068862	35.869876
1380.860717	136371.400561	35.874893
1382.299384	136578.830266	35.879911
1383.876606	136779.763879	35.884928
1385.170932	136990.754988	35.889946
1386.666528	137201.931050	35.894964
1388.496580	137400.661718	35.899981
1389.567014	137605.521260	35.904999
1390.747431	137804.383215	35.910016
1392.843966	138012.491465	35.915034
1394.172077	138216.477865	35.920052
1395.473445	138426.895110	35.925069
1396.457478	138630.660212	35.930087
1397.936013	138836.274439	35.935104
1398.867100	139056.411897	35.940122
1399.784499	139277.452951	35.945140
1401.610670	139501.595617	35.950157
1402.610785	139727.594819	35.955175
1403.883219	139955.326747	35.960192
1405.070864	140199.904571	35.965210
1406.538304	140429.320033	35.970228
1408.114273	140658.694637	35.975245
1409.624379	140899.196553	35.980263
1411.411836	141129.504330	35.985280
1413.081302	141359.363651	35.990298
1413.927676	141590.813041	35.995316
1415.837976	141813.121644	36.000333
1417.713021	142030.583135	36.005351
1419.921270	142231.427555	36.010368
1421.544064	142449.058841	36.015386
1423.363736	142650.677528	36.020404
1425.593370	142848.429946	36.025421
1426.714198	143046.321794	36.030439
1428.636629	143230.702754	36.035456
1429.711559	143424.358195	36.040474
1431.202098	143619.241671	36.045492
1432.394742	143813.869498	36.050509
1433.741477	144010.172548	36.055527
1434.921010	144202.371230	36.060544
1435.957640	144411.959178	36.065562
1437.262855	144615.396242	36.070580
1438.933096	144819.816029	36.075597
1439.904099	145036.453557	36.080615
1441.444546	145231.605354	36.085632
1442.552968	145449.770341	36.090650
1443.705272	145642.413154	36.095668
1445.071075	145841.665462	36.100685
1446.107298	146052.012292	36.105703
1447.530911	146246.859354	36.110720
1448.895063	146464.813244	36.115738
1450.421147	146668.874953	36.120756
1451.969716	146875.507718	36.125773
1453.070750	147097.576889	36.130791
1455.230771	147289.321670	36.135808
1457.053300	147501.036311	36.140826
1458.166738	147716.794818	36.145844
1459.435846	147930.641189	36.150861
1460.425485	148147.854746	36.155879
1461.910596	148372.647977	36.160896
1463.241638	148603.171962	36.165914
1464.531966	148825.907570	36.170932
1465.769177	149059.023187	36.175949
1467.352429	149300.908970	36.180967
1468.429047	149541.583944	36.185984
1470.360126	149777.789203	36.191002
1471.493788	150023.301509	36.196020
1473.180219	150257.292480	36.201037
1474.714330	150508.006076	36.206055
1476.155807	150733.405736	36.211072
1477.843675	150989.524745	36.216090
1479.501047	151227.343341	36.221108
1481.003540	151470.234197	36.226125
1482.425713	151718.172895	36.231143
1483.702132	151964.792692	36.236160
1485.183134	152215.502336	36.241178
1486.597895	152469.165833	36.246196
1488.095862	152720.916232	36.251213
1489.440370	152984.877248	36.256231
1490.716413	153228.463530	36.261248
1492.478906	153491.626752	36.266266
1493.876140	153750.260227	36.271284
1495.745285	153997.764451	36.276301
1496.666308	154268.535471	36.281319
1498.085621	154529.796019	36.286336
1500.130998	154776.669331	36.291354
1501.608628	155056.398685	36.296372
1503.396369	155296.457040	36.301389
1504.996695	155552.979844	36.306407
1506.764234	155801.996883	36.311424
1508.534142	156062.363922	36.316442
1510.125603	156306.974610	36.321460
1512.317880	156548.854120	36.326477
1514.392990	156773.394706	36.331495
1516.470069	156992.521949	36.336512
1518.398642	157213.842518	36.341530
1519.731716	157422.413788	36.346548
1521.309192	157628.221168	36.351565
1523.131385	157839.494277	36.356583
1525.135475	158023.539698	36.361600
1526.972359	158205.190630	36.366618
1528.582719	158395.463402	36.371636
1530.683469	158559.219673	36.376653
1531.618735	158728.145458	36.381671
1533.118283	158908.217782	36.386688
1534.438591	159071.808756	36.391706
1535.318592	159258.702250	36.396724
1536.914681	159433.511935	36.401741
1538.216886	159617.144597	36.406759
1539.690749	159803.350613	36.411776
1541.012142	159992.726811	36.416794
1542.183284	160186.870750	36.421812
1543.568127	160383.847826	36.426829
1545.017834	160595.577070	36.431847
1546.116387	160805.385006	36.436864
1548.001194	161005.557964	36.441882
1549.198264	161222.619335	36.446900
1550.368510	161441.220787	36.451917
1551.851833	161669.209228	36.456935
1552.978593	161900.337488	36.461952
1554.175331	162126.674941	36.466970
1555.333803	162368.162460	36.471988
1556.919273	162614.732776	36.477005
1557.810887	162875.581216	36.482023
1559.544908	163138.694701	36.487040
1560.786685	163395.635754	36.492058
1561.959782	163680.275797	36.497076
1563.688058	163939.768696	36.502093
1565.122347	164214.364676	36.507111
1566.568629	164497.521789	36.512128
1568.482519	164771.500359	36.517146
1569.766433	165072.190269	36.522164
1571.301613	165348.059615	36.527181
1572.976125	165646.371078	36.532199
1574.400966	165932.358210	36.537216
1576.299317	166204.612136	36.542234
1578.468873	166498.894482	36.547252
1580.377922	166768.081342	36.552269
1582.249037	167044.480555	36.557287
1584.332610	167317.030180	36.562304
1586.521656	167558.400425	36.567322
1588.089885	167820.558534	36.572340
1590.518516	168071.711457	36.577357
1592.784160	168322.042073	36.582375
1593.968784	168561.777025	36.587392
1595.658257	168797.539176	36.592410
1596.957640	169032.400705	36.597428
1598.679501	169277.547161	36.602445
1599.986904	169523.915298	36.607463
1601.387148	169769.407691	36.612480
1603.780352	170003.200761	36.617498
1605.125103	170258.916316	36.622516
1606.382903	170499.171701	36.627533
1607.699353	170738.797678	36.632551
1609.027754	170995.751084	36.637568
1610.571974	171243.804936	36.642586
1611.905844	171483.204341	36.647604
1612.985768	171725.322134	36.652621
1614.433763	171974.499475	36.657639
1615.660603	172236.969860	36.662656
1617.393445	172488.883308	36.667674
1618.241902	172759.345717	36.672692
1619.655021	173021.702869	36.677709
1621.505374	173303.173297	36.682727
1622.674331	173585.121800	36.687744
1624.518408	173846.971875	36.692762
1626.035335	174136.696235	36.697780
1627.709982	174431.040762	36.702797
1629.138246	174714.123056	36.707815
1630.745308	175006.554152	36.712832
1632.918202	175291.082607	36.717850
1634.097777	175593.785698	36.722868
1635.672989	175884.870637	36.727885
1637.307773	176187.632654	36.732903
1638.744817	176492.394743	36.737920
1640.589219	176791.423315	36.742938
1642.150231	177097.324650	36.747956
1643.908772	177404.110323	36.752973
1645.675946	177706.557841	36.757991
1647.340680	178021.952155	36.763008
1649.171595	178311.173720	36.768026
1651.040852	178633.695798	36.773044
1652.813078	178933.004780	36.778061
1654.292191	179237.094905	36.783079
1656.733283	179539.765651	36.788096
1658.982006	179834.424991	36.793114
1660.515036	180129.656764	36.798132
1662.724566	180412.336189	36.803149
1664.703691	180693.023953	36.808167
1666.326331	180969.443472	36.813184
1668.911799	181232.731773	36.818202
1670.289146	181509.219037	36.823220
1672.601009	181767.021891	36.828237
1674.631070	182021.749642	36.833255
1676.750955	182274.066468	36.838272
1678.718613	182519.645873	36.843290
1680.206551	182766.736637	36.848308
1682.003525	183003.730207	36.853325
1683.901600	183246.710798	36.858343
1685.123560	183489.749314	36.863360
1687.033178	183737.070335	36.868378
1688.257043	183997.165263	36.873396
1689.823710	184250.723124	36.878413
1691.236375	184515.105352	36.883431
1692.376627	184773.898348	36.888448
1693.681206	185029.900450	36.893466
1695.884696	185293.438340	36.898484
1697.413761	185543.202560	36.903501
1699.104494	185811.012371	36.908519
1700.550656	186077.035271	36.913536
1702.277185	186332.952267	36.918554
1703.737011	186593.874719	36.923572
1705.110630	186844.317841	36.928589
1707.246614	187091.088094	36.933607
1708.288740	187345.241229	36.938624
1710.086348	187599.326549	36.943642
1711.476118	187866.447280	36.948660
1712.943165	188129.661372	36.953677
1714.592420	188405.944329	36.958695
1715.699275	188687.099266	36.963712
1717.568570	188949.010388	36.968730
1719.217493	189240.818595	36.973748
1720.655611	189538.690058	36.978765
1722.252227	189823.390719	36.983783
1723.514234	190131.357472	36.988800
1724.971912	190436.363547	36.993818
1726.464041	190754.488416	36.998836
1727.832924	191072.837983	37.003853
1729.859293	191402.989415	37.008871
1731.261814	191725.779739	37.013888
1733.294842	192052.774386	37.018906
1735.171066	192381.725162	37.023924
1737.099540	192708.042706	37.028941
1739.370104	193026.020557	37.033959
1741.721274	193342.578871	37.038976
1743.735954	193643.543855	37.043994
1745.689830	193955.841263	37.049012
1747.906282	194266.499747	37.054029
1749.794024	194570.269883	37.059047
1751.158141	194890.053302	37.064064
1752.981667	195187.960943	37.069082
1754.932039	195502.070623	37.074100
1756.228713	195812.186431	37.079117
1758.211712	196124.213192	37.084135
1759.705288	196437.081060	37.089152
1761.277976	196756.995193	37.094170
1762.882163	197080.219001	37.099188
1764.486020	197398.380524	37.104205
1766.631713	197730.330948	37.109223
1768.116691	198063.860686	37.114240
1770.267944	198375.670969	37.119258
1772.465874	198691.461203	37.124276
1774.146781	199014.379926	37.129293
1775.846005	199336.333003	37.134311
1778.018310	199653.783009	37.139328
1779.985309	199969.465031	37.144346
1781.683953	200287.450861	37.149364
1783.504699	200605.850716	37.154381
1785.454575	200922.734090	37.159399
1787.271103	201237.660269	37.164416
1789.452852	201529.923154	37.169434
1791.518170	201842.503035	37.174452
1792.784179	202143.114518	37.179469
1794.895337	202448.543977	37.184487
1796.609460	202759.585280	37.189504
1798.271485	203056.901833	37.194522
1800.244329	203332.514819	37.199540
1801.956806	203622.527314	37.204557
1803.614911	203897.901011	37.209575
1805.415799	204180.336644	37.214592
1807.168478	204458.706486	37.219610
1808.840244	204753.313680	37.224628
1810.175001	205051.479466	37.229645
1811.822836	205337.613625	37.234663
1813.543713	205645.648084	37.239680
1815.019684	205947.718540	37.244698
1816.469006	206267.795581	37.249716
1818.005580	206592.595563	37.254733
1820.133038	206911.349710	37.259751
1821.633432	207240.018094	37.264768
1823.339332	207563.501549	37.269786
1825.548355	207883.276127	37.274804
1827.417806	208228.496124	37.279821
1828.980540	208543.133712	37.284839
1831.110904	208883.923486	37.289856
1833.184525	209214.288735	37.294874
1834.946516	209544.527457	37.299892
1836.800124	209881.621507	37.304909
1838.671376	210222.523152	37.309927
1840.205854	210563.403905	37.314944
1842.290682	210898.816243	37.319962
1844.219751	211238.761968	37.324980
1845.818295	211575.422999	37.329997
1847.758261	211914.507237	37.335015
1849.683614	212262.088998	37.340032
1851.737469	212602.986909	37.345050
1853.554577	212954.715638	37.350068
1855.120677	213301.521958	37.355085
1857.195758	213652.108877	37.360103
1859.026013	214000.857465	37.365120
1861.023609	214350.685855	37.370138
1863.408603	214696.848841	37.375156
1865.274227	215040.709114	37.380173
1867.454307	215386.235202	37.385191
1869.340496	215725.804271	37.390208
1871.255425	216061.713859	37.395226
1873.376711	216406.225931	37.400244
1875.369731	216732.857890	37.405261
1877.764248	217060.671905	37.410279
1879.516085	217400.486217	37.415296
1881.956608	217713.504296	37.420314
1884.288096	218024.953943	37.425332
1886.440766	218350.907715	37.430349
1888.276393	218651.125852	37.435367
1890.033882	218967.673206	37.440384
1892.109096	219268.566874	37.445402
1894.035939	219577.027364	37.450420
1895.774922	219885.011060	37.455437
1897.735843	220227.230452	37.460455
1899.494800	220550.488401	37.465472
1900.912565	220849.042186	37.470490
1902.856966	221148.554745	37.475508
1904.435915	221441.434955	37.480525
1905.885505	221740.431566	37.485543
1907.822445	222040.164628	37.490560
1909.282540	222344.482132	37.495578
1911.110050	222655.675382	37.500596
1912.551993	222976.974861	37.505613
1914.190430	223290.765528	37.510631
1915.469748	223623.762579	37.515648
1917.012818	223973.137374	37.520666
1918.785955	224313.347425	37.525684
1920.321092	224677.925809	37.530701
1921.962012	225032.965566	37.535719
1923.199488	225405.213161	37.540736
1925.242790	225773.410843	37.545754
1926.948705	226157.129974	37.550772
1929.032770	226542.136840	37.555789
1930.901263	226927.484408	37.560807
1932.687187	227335.221177	37.565824
1934.357479	227730.737004	37.570842
1937.096879	228119.532595	37.575860
1939.015753	228524.663329	37.580877
1941.416074	228922.252783	37.585895
1943.111620	229329.530550	37.590912
1945.336514	229718.363937	37.595930
1947.330608	230118.740602	37.600948
1949.325758	230516.325114	37.605965
1951.616666	230909.343624	37.610983
1953.726408	231306.583141	37.616000
1955.904763	231707.064351	37.621018
1957.724499	232095.946507	37.626036
1959.386823	232515.942349	37.631053
1961.167520	232907.373746	37.636071
1963.349269	233317.258350	37.641088
1965.512674	233718.867705	37.646106
1967.864840	234115.496024	37.651124
1969.678660	234521.735752	37.656141
1972.036490	234918.010714	37.661159
1974.434250	235319.893970	37.666176
1976.373273	235717.889343	37.671194
1978.539537	236100.585425	37.676212
1980.442630	236496.430509	37.681229
1982.883613	236894.147429	37.686247
1984.793242	237283.314390	37.691264
1986.474092	237667.134382	37.696282
1988.901920	238053.199318	37.701300
1990.965370	238448.721179	37.706317
1992.842796	238833.301339	37.711335
1994.945327	239225.797144	37.716352
1996.774029	239616.381943	37.721370
1998.901585	239997.243312	37.726388
2000.880070	240383.438119	37.731405
2002.762840	240762.664371	37.736423
2004.605381	241161.760994	37.741440
2006.334629	241543.122222	37.746458
2008.701486	241915.010797	37.751476
2010.638797	242285.952610	37.756493
2013.030690	242642.472208	37.761511
2014.773908	242989.773768	37.766528
2016.643488	243370.635595	37.771546
2018.835483	243725.462640	37.776564
2020.912061	244083.839620	37.781581
2023.555022	244427.979536	37.786599
2025.685455	244786.527634	37.791616
2027.551254	245142.222955	37.796634
2030.030810	245491.090589	37.801652
2032.140972	245849.365218	37.806669
2034.037289	246193.881942	37.811687
2036.071732	246547.318733	37.816704
2038.049191	246909.859004	37.821722
2040.017028	247257.110192	37.826740
2041.848902	247626.533601	37.831757
2043.813532	247993.701531	37.836775
2045.659200	248359.771544	37.841792
2047.614458	248728.771584	37.846810
2049.577851	249097.339363	37.851828
2051.288822	249483.119441	37.856845
2053.279341	249866.163513	37.861863
2055.446720	250246.233819	37.866880
2057.520719	250639.427057	37.871898
2059.584030	251023.935492	37.876916
2061.531928	251420.655940	37.881933
2063.760768	251803.844322	37.886951
2065.711073	252210.117224	37.891968
2067.451646	252610.022995	37.896986
2069.614034	253001.175216	37.902004
2071.543294	253410.807114	37.907021
2073.235489	253819.308977	37.912039
2075.413693	254240.283256	37.917056
2077.183894	254659.748187	37.922074
2079.583947	255075.786358	37.927092
2081.371170	255493.878531	37.932109
2083.501540	255906.506375	37.937127
2085.642273	256346.517147	37.942144
2087.538198	256763.425956	37.947162
2090.393975	257181.453388	37.952180
2092.268007	257607.334248	37.957197
2094.879128	258028.932911	37.962215
2097.306309	258446.827271	37.967232
2099.808443	258855.997302	37.972250
2102.195710	259259.064133	37.977268
2104.520061	259656.502131	37.982285
2107.187367	260047.637214	37.987303
2109.341313	260430.877771	37.992320
2112.000139	260815.689935	37.997338
2114.420040	261190.887388	38.002356
2116.465276	261569.396292	38.007373
2118.725037	261937.888262	38.012391
2121.105681	262297.927684	38.017408
2122.899325	262669.237908	38.022426
2124.762870	263005.786102	38.027444
2126.837461	263356.933292	38.032461
2128.544148	263694.218282	38.037479
2130.632136	264042.010778	38.042496
2132.353330	264402.309278	38.047514
2134.556270	264751.938581	38.052532
2136.455320	265118.560272	38.057549
2138.401446	265477.528443	38.062567
2140.523765	265846.554019	38.067584
2141.878568	266217.632246	38.072602
2144.074034	266591.956050	38.077620
2145.746775	266990.419899	38.082637
2147.770578	267375.415430	38.087655
2150.014889	267771.350461	38.092672
2151.474157	268178.968747	38.097690
2153.937545	268573.726378	38.102708
2155.997760	268987.372036	38.107725
2157.990577	269402.120948	38.112743
2160.040488	269822.754591	38.117760
2161.949303	270245.722510	38.122778
2164.641396	270668.642600	38.127796
2166.681271	271098.423583	38.132813
2169.026654	271513.981168	38.137831
2171.161263	271942.604241	38.142848
2173.304727	272389.694292	38.147866
2175.315882	272817.676650	38.152884
2177.599502	273249.705817	38.157901
2180.192496	273686.665041	38.162919
2182.667465	274106.597318	38.167936
2184.621381	274544.801079	38.172954
2187.132044	274973.822117	38.177972
2189.631564	275417.934520	38.182989
2191.603519	275839.597706	38.188007
2193.755851	276273.832309	38.193024
2196.344490	276707.946827	38.198042
2198.590368	277136.628456	38.203060
2201.077815	277570.072890	38.208077
2203.477293	277994.589137	38.213095
2206.547017	278404.112571	38.218112
2208.870923	278829.707405	38.223130
2211.290790	279219.823762	38.228148
2213.374885	279638.165467	38.233165
2215.455760	280050.207433	38.238183
2217.781679	280454.919559	38.243200
2219.666839	280875.248134	38.248218
2221.637780	281286.747891	38.253236
2223.696820	281704.635006	38.258253
2225.851157	282121.134920	38.263271
2228.174742	282545.304837	38.268288
2230.161864	282964.345492	38.273306
2232.618585	283393.548787	38.278324
2234.700796	283814.707455	38.283341
2237.211432	284243.520324	38.288359
2239.356302	284672.873399	38.293376
2240.970737	285100.023834	38.298394
2243.394795	285499.152899	38.303412
2245.432239	285901.035543	38.308429
2247.220352	286310.527344	38.313447
2249.375513	286728.318021	38.318464
2251.109724	287150.899848	38.323482
2252.939696	287572.653038	38.328500
2254.900715	288016.917181	38.333517
2256.875976	288458.384096	38.338535
2259.363967	288894.764702	38.343552
2261.344635	289341.894200	38.348570
2264.004070	289789.016956	38.353588
2266.621174	290229.185347	38.358605
2268.471687	290692.006608	38.363623
2270.653435	291139.431366	38.368640
2272.443115	291609.601873	38.373658
2275.005879	292068.700430	38.378676
2277.501259	292531.314281	38.383693
2280.143574	292991.820892	38.388711
2282.990481	293450.922375	38.393728
2284.974618	293911.531369	38.398746
2287.180624	294383.255718	38.403764
2289.845783	294848.200026	38.408781
2291.801480	295330.224282	38.413799
2294.069635	295799.166593	38.418816
2296.507945	296280.172080	38.423834
2298.898342	296742.665974	38.428852
2301.250964	297216.874900	38.433869
2303.596160	297693.039673	38.438887
2306.262984	298167.272439	38.443904
2308.091575	298654.312155	38.448922
2310.321170	299137.197245	38.453940
2312.688300	299631.007125	38.458957
2314.725386	300115.875738	38.463975
2317.138932	300602.588281	38.468992
2319.228591	301103.499097	38.474010
2321.815464	301597.598157	38.479028
2324.047461	302095.993808	38.484045
2326.206215	302593.611950	38.489063
2329.098573	303084.253861	38.494080
2331.413369	303590.480081	38.499098
2333.691079	304084.873639	38.504116
2336.475840	304587.008411	38.509133
2338.800222	305082.686369	38.514151
2341.492539	305575.129106	38.519168
2343.740893	306071.196397	38.524186
2346.353240	306558.771219	38.529204
2348.843313	307050.503756	38.534221
2351.308599	307528.014296	38.539239
2354.201726	308010.306541	38.544256
2356.593757	308488.383730	38.549274
2358.958666	308971.390840	38.554292
2361.778502	309430.041874	38.559309
2364.163336	309898.640440	38.564327
2366.568719	310368.046614	38.569344
2368.870539	310834.470143	38.574362
2370.807313	311278.522132	38.579380
2373.516549	311711.452109	38.584397
2375.512509	312152.189305	38.589415
2377.876686	312590.021667	38.594432
2380.399232	313024.830078	38.599450
2382.325431	313459.578822	38.604468
2385.178685	313902.814320	38.609485
2387.523658	314335.664321	38.614503
2390.240910	314771.399686	38.619520
2392.713990	315205.927355	38.624538
2394.945397	315648.568029	38.629556
2397.149424	316087.756932	38.634573
2398.970262	316540.059092	38.639591
2401.104675	316995.458756	38.644608
2403.524519	317455.992127	38.649626
2405.701906	317923.292017	38.654644
2408.038055	318397.015340	38.659661
2410.015442	318878.056704	38.664679
2412.285459	319347.722059	38.669696
2414.445868	319851.002528	38.674714
2416.903041	320337.293462	38.679732
2419.058407	320832.721569	38.684749
2421.164603	321347.075082	38.689767
2423.277593	321858.072146	38.694784
2425.591897	322384.195807	38.699802
2427.586123	322903.967123	38.704820
2430.258800	323436.782780	38.709837
2432.403857	323979.481385	38.714855
2434.534115	324525.911897	38.719872
2436.961163	325073.510680	38.724890
2439.450332	325634.606140	38.729908
2442.136980	326186.067023	38.734925
2444.321502	326755.608560	38.739943
2447.358748	327314.395827	38.744960
2449.873931	327880.194460	38.749978
2452.581562	328430.874184	38.754996
2455.651966	328976.642123	38.760013
2458.491049	329523.458483	38.765031
2461.014898	330060.239437	38.770048
2463.584228	330611.991437	38.775066
2466.020078	331158.453177	38.780084
2468.871936	331697.556998	38.785101
2471.357507	332238.898566	38.790119
2474.196966	332778.224652	38.795136
2476.787604	333318.779447	38.800154
2479.292618	333855.941004	38.805172
2481.759802	334388.584536	38.810189
2484.371900	334933.160546	38.815207
2486.653169	335457.445762	38.820224
2489.481744	335996.316462	38.825242
2492.057004	336533.800992	38.830260
2494.852446	337053.015378	38.835277
2497.449738	337587.948620	38.840295
2500.051892	338113.101218	38.845312
2502.613465	338624.138794	38.850330
2504.996789	339098.816142	38.855348
2508.045740	339572.825861	38.860365
2510.480734	340053.835330	38.865383
2512.927704	340529.913557	38.870400
2515.268276	341002.120358	38.875418
2517.456486	341483.157763	38.880436
2520.461201	341957.105358	38.885453
2522.542528	342439.446939	38.890471
2525.238221	342915.695548	38.895488
2527.436745	343412.050676	38.900506
2529.200192	343906.972648	38.905524
2532.120240	344402.037241	38.910541
2534.406370	344902.884942	38.915559
2536.923189	345405.291175	38.920576
2539.868107	345906.762010	38.925594
2543.212080	346381.889417	38.930612
2546.422070	346868.052028	38.935629
2548.348924	347357.383970	38.940647
2551.514842	347847.327693	38.945664
2553.812946	348341.872567	38.950682
2556.014903	348843.866363	38.955700
2558.727167	349336.838876	38.960717
2560.700718	349837.717340	38.965735
2563.128235	350341.108551	38.970752
2565.621293	350860.426540	38.975770
2567.684527	351387.702267	38.980788
2570.084629	351912.203212	38.985805
2572.217159	352444.762780	38.990823
2574.347666	352988.587792	38.995840
2576.714295	353534.603471	39.000858
2579.173757	354098.392551	39.005876
2581.355512	354665.544615	39.010893
2583.656413	355248.155106	39.015911
2585.935585	355832.462941	39.020928
2588.538533	356424.530444	39.025946
2591.062422	357015.664269	39.030964
2593.486878	357608.558099	39.035981
2595.901005	358217.182908	39.040999
2598.846200	358824.396145	39.046016
2601.387901	359438.975336	39.051034
2603.520416	360051.352585	39.056052
2606.528529	360653.684970	39.061069
2609.357960	361274.565276	39.066087
2612.151482	361893.615716	39.071104
2615.050122	362507.514670	39.076122
2617.747722	363139.380157	39.081140
2620.775886	363749.460582	39.086157
2623.007162	364373.058728	39.091175
2625.884876	364979.009816	39.096192
2628.727082	365603.179379	39.101210
2631.224492	366215.137679	39.106228
2634.237552	366830.482472	39.111245
2637.017855	367446.692952	39.116263
2639.568416	368053.541998	39.121280
2642.085637	368657.139760	39.126298
2644.654908	369242.704341	39.131316
2647.451283	369815.537454	39.136333
2650.106707	370394.119871	39.141351
2653.121464	370967.562613	39.146368
2655.539160	371529.521577	39.151386
2658.390142	372105.816605	39.156404
2660.961557	372672.404593	39.161421
2663.704979	373250.908237	39.166439
2666.067349	373823.755268	39.171456
2669.311247	374394.501006	39.176474
2671.577654	374978.257080	39.181492
2674.700033	375548.574501	39.186509
2677.492916	376120.280686	39.191527
2679.674476	376710.697660	39.196544
2682.417079	377294.877379	39.201562
2684.838808	377883.615144	39.206580
2687.554151	378476.711906	39.211597
2690.467608	379066.039014	39.216615
2693.189933	379650.009253	39.221632
2696.489934	380244.635416	39.226650
2699.264711	380841.441102	39.231668
2702.210321	381425.095318	39.236685
2704.764235	382011.542266	39.241703
2707.522275	382622.731242	39.246720
2709.892370	383211.573110	39.251738
2712.547565	383810.862109	39.256756
2715.369225	384404.889756	39.261773
2718.209193	385006.996474	39.266791
2720.599958	385609.976138	39.271808
2723.565880	386216.938450	39.276826
2726.345323	386833.355563	39.281844
2729.100373	387430.438996	39.286861
2731.921057	388049.745596	39.291879
2734.144396	388667.462123	39.296896
2737.030623	389284.783975	39.301914
2739.504676	389914.460796	39.306932
2742.204241	390536.558321	39.311949
2744.806487	391171.467448	39.316967
2747.441320	391801.592075	39.321984
2750.336272	392432.526284	39.327002
2753.059371	393077.018111	39.332020
2756.001947	393722.502776	39.337037
2758.702873	394365.071881	39.342055
2761.190297	395014.078187	39.347072
2764.217968	395653.173077	39.352090
2767.047209	396297.815039	39.357108
2769.665617	396940.449389	39.362125
2772.379145	397598.269872	39.367143
2775.294656	398243.519601	39.372160
2778.356329	398886.197988	39.377178
2781.026097	399544.189222	39.382196
2784.572837	400181.846436	39.387213
2787.304434	400817.845366	39.392231
2790.374216	401454.361285	39.397248
2793.486960	402069.789744	39.402266
2796.175695	402672.622733	39.407284
2799.541469	403259.137370	39.412301
2802.556423	403838.141988	39.417319
2805.157493	404407.340025	39.422336
2808.508935	404982.721100	39.427354
2811.009617	405553.739309	39.432372
2814.052914	406121.593816	39.437389
2817.639225	406679.465849	39.442407
2820.357653	407231.254783	39.447424
2823.283889	407777.424314	39.452442
2826.439998	408344.763478	39.457460
2828.921793	408897.320091	39.462477
2831.752927	409449.938018	39.467495
2834.237503	410014.133102	39.472512
2837.371469	410572.816141	39.477530
2839.497457	411146.804643	39.482548
2842.344857	411723.455749	39.487565
2845.085448	412284.551230	39.492583
2847.981886	412868.015104	39.497600
2851.186370	413445.843113	39.502618
2853.495682	414031.606908	39.507636
2856.249437	414612.042731	39.512653
2859.128658	415205.700696	39.517671
2861.489865	415810.933265	39.522688
2864.346064	416397.018649	39.527706
2867.184589	417010.614034	39.532724
2869.883416	417617.680725	39.537741
2872.857039	418235.054513	39.542759
2875.253617	418859.271458	39.547776
2878.253392	419480.515884	39.552794
2880.845766	420115.645096	39.557812
2884.008569	420743.549940	39.562829
2886.335753	421388.573297	39.567847
2889.187650	422036.057402	39.572864
2892.371170	422679.344178	39.577882
2894.914308	423345.644653	39.582900
2897.970505	423993.227422	39.587917
2900.652935	424645.059158	39.592935
2903.655273	425312.986571	39.597952
2906.533854	425974.026734	39.602970
2909.327472	426652.846445	39.607988
2912.323553	427329.970329	39.613005
2915.958212	427983.444445	39.618023
2919.105031	428665.246963	39.623040
2922.035373	429322.497381	39.628058
2924.812898	429988.620238	39.633076
2927.632753	430663.507915	39.638093
2930.864335	431324.054003	39.643111
2933.220230	431996.093130	39.648128
2936.202417	432677.639175	39.653146
2939.504106	433349.062650	39.658164
2942.431814	434021.135400	39.663181
2945.677544	434685.973544	39.668199
2948.492353	435371.171106	39.673216
2951.599355	436023.005479	39.678234
2953.827941	436672.049972	39.683252
2956.608202	437306.329656	39.688269
2959.838082	437934.267972	39.693287
2962.405435	438577.486806	39.698304
2965.731946	439213.682055	39.703322
2968.553211	439862.852964	39.708340
2971.339433	440481.732671	39.713357
2974.676572	441136.104745	39.718375
2977.273549	441792.702856	39.723392
2980.612732	442441.722994	39.728410
2983.471662	443094.649466	39.733428
2986.023676	443746.847325	39.738445
2989.352155	444411.206747	39.743463
2992.277195	445077.940222	39.748480
2995.329075	445735.320137	39.753498
2998.200232	446404.809059	39.758516
3001.246251	447073.188225	39.763533
3004.137532	447754.480732	39.768551
3006.971600	448432.775958	39.773568
3010.357759	449114.254096	39.778586
3013.001907	449804.231647	39.783604
3015.922348	450503.963815	39.788621
3019.041706	451195.697156	39.793639
3021.483167	451915.504271	39.798656
3024.498599	452615.460496	39.803674
3027.234696	453348.131442	39.808692
3030.226905	454067.175891	39.813709
3032.965542	454800.608943	39.818727
3036.062830	455542.816606	39.823744
3039.221326	456278.462465	39.828762
3042.006923	457024.616900	39.833780
3044.742503	457775.054843	39.838797
3047.636820	458535.712949	39.843815
3050.544959	459311.975874	39.848832
3053.618175	460078.825674	39.853850
3056.324121	460860.782328	39.858868
3059.267669	461645.303756	39.863885
3063.055507	462424.098619	39.868903
3065.831640	463213.142174	39.873920
3069.672574	463984.688994	39.878938
3072.976540	464767.724038	39.883956
3076.153461	465545.490105	39.888973
3079.775770	466304.494222	39.893991
3083.584803	467079.827736	39.899008
3087.319419	467835.521951	39.904026
3090.528902	468590.311028	39.909044
3094.162345	469336.257109	39.914061
3097.606902	470072.598334	39.919079
3100.414056	470819.076735	39.924096
3103.660589	471540.277595	39.929114
3107.325042	472280.701748	39.934132
3110.051782	473014.270018	39.939149
3113.914448	473729.936576	39.944167
3116.762877	474454.080163	39.949184
3119.898204	475158.435884	39.954202
3123.100504	475844.405452	39.959220
3125.931467	476514.284279	39.964237
3128.715521	477188.090947	39.969255
3131.318836	477867.463694	39.974272
3134.505828	478549.450347	39.979290
3137.142031	479229.478792	39.984308
3140.098569	479918.935172	39.989325
3143.390034	480612.711435	39.994343
3146.349805	481320.767664	39.999360
3148.769109	482025.598715	40.004378
3151.585579	482746.057972	40.009396
3154.264528	483475.709308	40.014413
3157.246327	484206.144176	40.019431
3160.058108	484961.691528	40.024448
3163.204529	485713.265486	40.029466
3166.003760	486476.738323	40.034484
3168.682823	487255.154543	40.039501
3171.823127	488038.366412	40.044519
3174.694445	488838.815475	40.049536
3177.581877	489646.401360	40.054554
3181.098306	490468.754891	40.059572
3183.838415	491275.333869	40.064589
3187.459878	492084.718560	40.069607
3190.750750	492921.041157	40.074624
3194.227847	493731.285651	40.079642
3197.830140	494556.373258	40.084660
3201.030175	495388.658496	40.089677
3204.288238	496215.543600	40.094695
3207.549802	497044.814332	40.099712
3211.165105	497874.092069	40.104730
3214.396467	498715.460020	40.109748
3217.407465	499552.481222	40.114765
3220.948562	500381.452825	40.119783
3223.977883	501229.348263	40.124800
3227.133820	502057.242407	40.129818
3230.391885	502903.506996	40.134836
3233.694904	503738.416701	40.139853
3237.382680	504596.898885	40.144871
3240.967329	505438.194311	40.149888
3244.209775	506282.935189	40.154906
3247.669614	507127.449125	40.159924
3251.046146	507956.795198	40.164941
3254.584357	508786.681294	40.169959
3258.333152	509632.994644	40.174976
3261.306053	510464.099853	40.179994
3264.452549	511297.811199	40.185012
3267.768192	512140.889613	40.190029
3270.951620	512964.220540	40.195047
3274.423542	513815.565393	40.200064
3277.546054	514653.453234	40.205082
3280.842357	515482.998875	40.210100
3283.916854	516334.126961	40.215117
3287.366774	517158.369305	40.220135
3290.703192	517998.677525	40.225152
3294.357326	518822.804459	40.230170
3297.941104	519613.364700	40.235188
3301.352609	520399.526716	40.240205
3304.902180	521164.197966	40.245223
3307.915413	521944.246826	40.250240
3311.512939	522710.199089	40.255258
3314.639778	523473.214737	40.260276
3317.522715	524260.987237	40.265293
3321.021851	525037.986317	40.270311
3323.791999	525815.617441	40.275328
3326.762957	526613.896980	40.280346
3329.924985	527411.098094	40.285364
3332.451706	528226.152088	40.290381
3336.070377	529039.277740	40.295399
3339.140257	529854.363286	40.300416
3342.313608	530692.219476	40.305434
3345.930968	531526.685007	40.310452
3348.969010	532372.787238	40.315469
3352.478322	533215.140946	40.320487
3355.445619	534074.262290	40.325504
3358.580693	534934.921482	40.330522
3362.008252	535801.481374	40.335540
3364.998359	536677.431401	40.340557
3368.156442	537566.603201	40.345575
3370.924723	538459.663172	40.350592
3374.096664	539366.508140	40.355610
3378.076638	540276.494973	40.360628
3381.107730	541187.986891	40.365645
3384.703711	542113.384069	40.370663
3388.256496	543039.536439	40.375680
3391.597791	543961.334352	40.380698
3395.296935	544895.303539	40.385716
3398.452783	545831.363762	40.390733
3402.047812	546757.780351	40.395751
3405.752611	547703.854091	40.400768
3409.011487	548645.507543	40.405786
3412.257552	549597.269372	40.410804
3415.331889	550544.818617	40.415821
3418.728030	551505.691996	40.420839
3422.467037	552458.093559	40.425856
3425.855922	553428.400988	40.430874
3429.466113	554379.789491	40.435892
3433.124354	555350.527568	40.440909
3436.547949	556312.834788	40.445927
3439.888714	557293.702783	40.450944
3443.645863	558246.770569	40.455962
3447.767393	559209.926790	40.460980
3451.291386	560169.489949	40.465997
3455.204220	561102.723597	40.471015
3459.361295	562056.122300	40.476032
3463.294744	562976.805447	40.481050
3467.371066	563909.321426	40.486068
3470.959078	564826.365672	40.491085
3474.529282	565738.424489	40.496103
3478.350448	566651.036353	40.501120
3482.008443	567524.535072	40.506125
3486.150227	568353.037514	40.511130
3489.263149	569128.791748	40.516135
3492.770041	569844.829831	40.521140
3496.006845	570477.383145	40.526144
3498.950884	571055.085039	40.531149
3501.559439	571547.216296	40.536154
3503.799801	571971.071972	40.541159
3506.510642	572355.141284	40.546164
3508.858228	572664.698001	40.551168
3510.764038	572923.890233	40.556173
3512.781024	573113.893631	40.561178
3514.506297	573262.481402	40.566183
3515.977505	573363.150588	40.571188
3517.773664	573399.338152	40.576192
3518.645375	573421.868979	40.581197
3519.883909	573371.449181	40.586202
3520.830698	573315.634762	40.591207
3522.076155	573209.246136	40.596212
3522.198837	573084.394907	40.601216
3522.860503	572930.994476	40.606221
3523.906289	572741.007935	40.611226
3524.350813	572548.796315	40.616231
3524.887061	572313.039943	40.621236
3525.333367	572074.522731	40.626240
3525.692133	571812.537575	40.631245
3525.650305	571528.039451	40.636250
3525.652279	571241.009213	40.641255
3526.199418	570937.562185	40.646260
3526.231884	570635.298122	40.651264
3526.626903	570310.799870	40.656269
3526.834196	569975.590853	40.661274
3526.654378	569645.473592	40.666279
3526.320223	569302.724662	40.671284
3526.532269	568951.465309	40.676288
3526.419861	568603.271696	40.681293
3526.465516	568248.795261	40.686298
3526.151015	567907.872506	40.691303
3526.214910	567532.712283	40.696308
3526.027317	567181.520663	40.701312
3525.886739	566815.343871	40.706317
3525.617947	566439.298910	40.711322
3525.594779	566093.042973	40.716327
3525.280213	565732.005655	40.721332
3525.351815	565367.923896	40.726336
3525.066381	565006.358799	40.731341
3524.982477	564639.005858	40.736346
3524.768456	564293.742783	40.741351
3524.413571	563926.816911	40.746356
3524.338740	563563.416232	40.751360
3523.596800	563224.914537	40.756365
3523.663314	562871.707112	40.761370
3523.078464	562530.289971	40.766375
3523.124569	562177.673044	40.771380
3523.001154	561843.022709	40.776384
3522.897150	561499.184966	40.781389
3522.606087	561161.973344	40.786394
3522.382485	560831.247267	40.791399
3522.334700	560489.442976	40.796404
3522.047979	560162.089326	40.801408
3521.450212	559841.534122	40.806413
3521.658697	559518.423695	40.811418
3521.202741	559211.144164	40.816423
3521.179740	558884.878784	40.821428
3520.675652	558572.802160	40.826432
3520.514840	558264.497092	40.831437
3520.293185	557947.268437	40.836442
3519.977541	557666.913992	40.841447
3520.032272	557342.315266	40.846452
3519.637197	557059.086550	40.851456
3519.136368	556768.000835	40.856461
3519.092440	556475.979490	40.861466
3518.477034	556208.101435	40.866471
3518.463032	555906.127303	40.871476
3518.371167	555648.193327	40.876480
3518.063074	555379.797103	40.881485
3518.234617	555100.020999	40.886490
3517.566353	554836.412991	40.891495
3517.376391	554584.931936	40.896500
3517.313894	554327.372929	40.901504
3516.832524	554060.543016	40.906509
3516.555586	553811.937491	40.911514
3516.327927	553567.658338	40.916519
3516.130197	553331.744705	40.921524
3515.891251	553100.777713	40.926528
3515.780893	552856.972394	40.931533
3515.678763	552625.976136	40.936538
3515.458971	552400.746237	40.941543
3515.257529	552170.464673	40.946548
3515.116878	551947.283713	40.951552
3514.583305	551736.825322	40.956557
3514.682798	551530.199269	40.961562
3514.540202	551318.815258	40.966567
3514.247815	551103.112599	40.971572
3514.357379	550900.815172	40.976576
3514.032066	550700.248739	40.981581
3514.060456	550488.876023	40.986586
3513.617394	550301.795023	40.991591
3513.439411	550105.486072	40.996596
3513.326222	549915.269915	41.001600
3513.023624	549724.526129	41.006605
3513.467779	549539.111670	41.011610
3512.631363	549352.787057	41.016615
3512.510511	549165.337711	41.021620
3512.361762	548989.194179	41.026624
3512.312341	548821.157533	41.031629
3512.349591	548652.600605	41.036634
3511.850003	548484.833083	41.041639
3511.753497	548323.055821	41.046644
3511.939832	548152.299525	41.051648
3511.451680	548001.329925	41.056653
3511.805908	547834.631201	41.061658
3511.501718	547676.008580	41.066663
3511.518334	547515.970889	41.071668
3511.191128	547360.628943	41.076672
3511.032900	547210.860771	41.081677
3511.347608	547059.805045	41.086682
3511.143169	546910.545811	41.091687
3510.787981	546759.693807	41.096692
3510.676454	546610.568253	41.101696
3510.515464	546478.256228	41.106701
3510.664161	546343.673277	41.111706
3510.397880	546205.974875	41.116711
3510.222166	546061.850732	41.121716
3509.915216	545925.115127	41.126720
3510.029904	545794.671402	41.131725
3510.038048	545657.580671	41.136730
3509.819512	545546.115497	41.141735
3509.787772	545411.956355	41.146740
3509.656020	545279.578467	41.151744
3509.743227	545159.178234	41.156749
3509.773652	545026.873405	41.161754
3509.344054	544903.473662	41.166759
3509.413205	544793.370712	41.171764
3509.383101	544672.530756	41.176768
3509.023735	544560.878493	41.181773
3509.224698	544430.510050	41.186778
3509.113806	544315.182170	41.191783
3509.040467	544199.191218	41.196788
3508.951368	544088.754683	41.201792
3508.780629	543983.226852	41.206797
3509.161886	543871.603792	41.211802
3508.593337	543755.283786	41.216807
3508.516604	543645.700185	41.221812
3508.699947	543545.817728	41.226816
3508.239655	543447.449830	41.231821
3508.500533	543338.769778	41.236826
3508.434707	543241.095416	41.241831
3508.250676	543134.856898	41.246836
3508.312249	543047.611219	41.251840
3508.069277	542937.796258	41.256845
3508.213998	542832.614281	41.261850
3508.097722	542751.352151	41.266855
3508.222896	542650.513673	41.271860
3507.790773	542553.700458	41.276864
3507.668624	542468.701790	41.281869
3507.783723	542369.226120	41.286874
3507.772286	542290.873109	41.291879
3507.545965	542196.902778	41.296884
3507.388663	542106.404552	41.301888
3507.278581	542025.238466	41.306893
3507.316803	541939.252182	41.311898
3507.270439	541867.061951	41.316903
3507.188764	541780.134434	41.321908
3507.514919	541705.865029	41.326912
3507.198294	541626.143094	41.331917
3507.251858	541530.811642	41.336922
3507.074543	541464.951285	41.341927
3506.981660	541378.578590	41.346932
3506.709586	541307.178674	41.351936
3506.651861	541231.351917	41.356941
3506.769954	541157.668070	41.361946
3506.837664	541102.824749	41.366951
3506.700941	541015.901500	41.371956
3506.525162	540948.978330	41.376960
3506.326015	540885.239497	41.381965
3506.572351	540817.542155	41.386970
3506.345215	540759.563224	41.391975
3506.252214	540689.798291	41.396980
3506.424659	540615.901230	41.401984
3506.041045	540558.703634	41.406989
3506.444803	540501.431875	41.411994
3506.338493	540435.404304	41.416999
3506.576943	540373.967297	41.422004
3506.433511	540302.895727	41.427008
3505.997870	540250.603009	41.432013
3506.009234	540178.143067	41.437018
3505.742638	540129.408249	41.442023
3505.522296	540071.880036	41.447028
3505.689120	540021.662543	41.452032
3505.785157	539964.336389	41.457037
3505.557352	539920.644185	41.462042
3505.373981	539866.492466	41.467047
3505.601158	539810.760828	41.472052
3505.747184	539767.413056	41.477056
3505.471764	539717.516918	41.482061
3505.699241	539661.330226	41.487066
3505.589533	539621.304641	41.492071
3505.157388	539575.724907	41.497076
3505.878692	539521.933931	41.502080
3505.702219	539478.181837	41.507085
3505.810814	539413.832686	41.512090
3505.293267	539383.919637	41.517095
3505.710201	539323.106595	41.522100
3505.944467	539264.847006	41.527104
3505.672873	539222.422114	41.532109
3505.702732	539162.376554	41.537114
3505.567427	539111.850308	41.542119
3505.465809	539069.044643	41.547124
3505.487834	539018.341728	41.552128
3505.306875	538974.437392	41.557133
3505.204233	538921.178481	41.562138
3504.912236	538873.655567	41.567143
3505.286344	538834.763385	41.572148
3505.422881	538793.787728	41.577152
3505.159085	538757.874556	41.582157
3505.254929	538708.421393	41.587162
3505.159319	538667.886072	41.592167
3505.352503	538618.164738	41.597172
3505.169030	538579.966008	41.602176
3504.987111	538545.099867	41.607181
3505.298253	538494.198009	41.612186
3505.122788	538457.765174	41.617191
3505.059170	538409.194724	41.622196
3505.302490	538368.807036	41.627200
3505.018203	538322.240665	41.632205
3505.120590	538276.774536	41.637210
3505.156624	538245.913247	41.642215
3504.959353	538201.453750	41.647220
3505.175212	538158.443838	41.652224
3504.962300	538126.308644	41.657229
3505.381412	538079.882864	41.662234
3505.288514	538054.192612	41.667239
3505.081485	538011.249117	41.672244
3505.321232	537966.164356	41.677248
3504.731686	537925.301107	41.682253
3504.897306	537892.701587	41.687258
3504.837351	537859.430630	41.692263
3504.839134	537821.705725	41.697268
3505.029538	537779.355281	41.702272
3504.956351	537738.965440	41.707277
3504.988893	537697.599248	41.712282
3505.029603	537672.291249	41.717287
3505.091168	537623.597500	41.722292
3504.973668	537573.265323	41.727296
3504.292199	537545.950157	41.732301
3504.546964	537509.699564	41.737306
3504.565053	537483.283774	41.742311
3504.457088	537449.463981	41.747316
3504.500950	537422.538986	41.752320
3504.240115	537392.884446	41.757325
3504.777339	537357.043375	41.762330
3504.425441	537333.311948	41.767335
3504.363559	537310.544710	41.772340
3504.667589	537279.891622	41.777344
3504.450067	537261.694192	41.782349
3504.958782	537225.453292	41.787354
3504.715762	537192.815850	41.792359
3504.880393	537152.235357	41.797364
3504.678668	537133.479737	41.802368
3504.474443	537087.553477	41.807373
3504.680781	537049.491308	41.812378
3504.390686	537017.416473	41.817383
3503.944319	536992.133819	41.822388
3504.692908	536968.379412	41.827392
3504.359096	536947.573767	41.832397
3504.478092	536919.272394	41.837402
3504.401342	536888.072648	41.842407
3504.360173	536852.877354	41.847412
3504.633731	536833.642214	41.852416
3504.419087	536799.080268	41.857421
3504.719480	536766.356031	41.862426
3504.515236	536744.469029	41.867431
3504.565402	536714.309473	41.872436
3504.635985	536679.752684	41.877440
3504.325642	536653.084331	41.882445
3504.418247	536623.069403	41.887450
3504.172078	536594.572614	41.892455
3504.336447	536560.707809	41.897460
3504.056141	536551.711457	41.902464
3504.172705	536529.621929	41.907469
3504.473632	536498.614226	41.912474
3504.696843	536474.790569	41.917479
3504.497382	536443.760826	41.922484
3504.305378	536412.174275	41.927488
3504.019977	536388.784409	41.932493
3504.416548	536370.185825	41.937498
3504.060469	536352.160725	41.942503
3504.024275	536324.589865	41.947508
3503.922238	536296.322271	41.952512
3503.777710	536293.264062	41.957517
3504.029457	536259.687820	41.962522
3504.173402	536249.816135	41.967527
3504.306562	536222.167819	41.972532
3504.716560	536199.021307	41.977536
3504.392603	536167.707638	41.982541
3504.448691	536135.525731	41.987546
3504.419224	536114.822371	41.992551
3504.199779	536082.481871	41.997556
3504.385136	536053.461309	42.002560
3504.112184	536037.746031	42.007565
3504.074974	536011.083898	42.012570
3504.157341	535988.998995	42.017575
3504.046843	535953.964111	42.022580
3504.170020	535944.600587	42.027584
3504.186728	535922.172412	42.032589
3504.421946	535891.527419	42.037594
3503.993020	535877.099320	42.042599
3504.203619	535853.428214	42.047604
3504.502098	535829.288612	42.052608
3504.007930	535813.254510	42.057613
3504.403411	535785.563948	42.062618
3504.473653	535768.581960	42.067623
3504.481928	535729.234599	42.072628
3504.394760	535710.661159	42.077632
3504.488535	535683.927247	42.082637
3504.596231	535637.997842	42.087642
3504.317023	535621.020411	42.092647
3504.304031	535586.726907	42.097652
3504.550446	535561.231376	42.102656
3504.106957	535545.492035	42.107661
3504.309210	535510.457218	42.112666
3504.326268	535488.129371	42.117671
3504.228287	535460.667740	42.122676
3504.393712	535437.205169	42.127680
3504.100770	535407.551848	42.132685
3504.300742	535381.659285	42.137690
3504.043155	535366.041907	42.142695
3504.064752	535345.683005	42.147700
3504.246624	535318.783005	42.152704
3503.627123	535291.100435	42.157709
3504.246541	535270.343893	42.162714
3504.257095	535251.552414	42.167719
3504.173647	535230.502823	42.172724
3504.444502	535209.043638	42.177728
3504.213585	535183.976490	42.182733
3504.341888	535149.154577	42.187738
3504.429729	535131.411451	42.192743
3504.133268	535101.404523	42.197748
3504.398983	535076.359731	42.202752
3504.294203	535064.253625	42.207757
3504.087826	535039.283383	42.212762
3504.493084	535014.468989	42.217767
3504.208135	534989.763638	42.222772
3504.185001	534951.884059	42.227776
3504.111719	534946.389799	42.232781
3504.349454	534910.034725	42.237786
3504.173126	534898.293373	42.242791
3503.937736	534863.578804	42.247796
3504.651839	534840.887298	42.252800
3504.216239	534817.619793	42.257805
3503.994868	534797.046007	42.262810
3504.307724	534770.073836	42.267815
3504.032404	534749.104421	42.272820
3504.153520	534719.485355	42.277824
3503.988820	534708.449182	42.282829
3504.061342	534677.271854	42.287834
3504.082945	534669.539983	42.292839
3504.076781	534643.224150	42.297844
3504.232182	534622.944168	42.302848
3504.273015	534605.662472	42.307853
3504.339949	534577.263983	42.312858
3504.036616	534545.034524	42.317863
3504.123123	534526.785790	42.322868
3504.389422	534504.013026	42.327872
3504.254066	534493.376159	42.332877
3504.145418	534446.063041	42.337882
3503.921246	534428.469442	42.342887
3503.765435	534409.652715	42.347892
3504.234347	534379.371878	42.352896
3503.737970	534376.166840	42.357901
3503.938972	534342.392381	42.362906
3504.120253	534337.867928	42.367911
3503.860780	534313.106950	42.372916
3503.980089	534309.602542	42.377920
3503.818171	534286.139439	42.382925
3503.920539	534262.179914	42.387930
3503.812976	534253.660039	42.392935
3503.905652	534228.590705	42.397940
3503.944568	534214.844797	42.402944
3503.988370	534198.117821	42.407949
3504.006959	534163.361533	42.412954
3503.847500	534154.496211	42.417959
3503.932955	534135.944101	42.422964
3504.125841	534117.627557	42.427968
3503.676185	534103.655685	42.432973
3503.962649	534072.443322	42.437978
3503.564829	534070.283431	42.442983
3503.741732	534048.382857	42.447988
3503.819931	534030.084335	42.452992
3503.534296	534030.432401	42.457997
3503.994952	534006.971507	42.463002
3503.654275	533985.203157	42.468007
3503.895671	533969.202414	42.473012
3504.032292	533955.895462	42.478016
3503.896616	533937.529603	42.483021
3503.922522	533927.068916	42.488026
3504.000835	533902.910578	42.493031
3503.674590	533886.443805	42.498036
3503.920956	533865.441251	42.503040
3503.973300	533850.935182	42.508045
3503.654074	533824.465372	42.513050
3503.836502	533811.252084	42.518055
3503.714905	533790.509641	42.523060
3503.892449	533785.328927	42.528064
3503.540015	533770.634182	42.533069
3503.849536	533748.712224	42.538074
3503.792153	533745.033554	42.543079
3503.708671	533717.718066	42.548084
3503.788707	533701.692034	42.553088
3503.798131	533692.193576	42.558093
3503.977351	533664.886991	42.563098
3503.773716	533648.400586	42.568103
3503.944184	533636.249856	42.573108
3504.100603	533616.321998	42.578112
3504.079147	533598.644898	42.583117
3504.349551	533577.234032	42.588122
3503.998473	533576.279051	42.593127
3504.113701	533547.365882	42.598132
3504.086404	533523.375189	42.603136
3503.862614	533495.727875	42.608141
3504.064141	533480.743241	42.613146
3503.792147	533469.268496	42.618151
3503.741063	533445.938146	42.623156
3503.950329	533425.547048	42.628160
3503.856515	533423.995724	42.633165
3504.062624	533393.855525	42.638170
3504.056298	533375.367524	42.643175
3503.871929	533355.594221	42.648180
3504.109489	533339.088274	42.653184
3504.082592	533314.491001	42.658189
3504.125477	533295.995127	42.663194
3503.762145	533268.116878	42.668199
3503.781375	533247.553515	42.673204
3503.906586	533236.369436	42.678208
3503.765193	533227.298660	42.683213
3504.045390	533209.371375	42.688218
3503.636021	533189.330320	42.693223
3503.701441	533167.648186	42.698228
3503.608228	533167.713274	42.703232
3503.691984	533151.736602	42.708237
3503.984221	533123.148283	42.713242
3503.942114	533107.696625	42.718247
3503.936892	533095.118586	42.723252
3504.036052	533053.274702	42.728256
3503.773938	533053.366484	42.733261
3503.877660	533034.304996	42.738266
3503.642467	533025.198408	42.743271
3503.806325	533001.580833	42.748276
3503.773971	532969.456808	42.753280
3503.481116	532973.796903	42.758285
3503.886775	532959.739333	42.763290
3503.720158	532945.923746	42.768295
3503.683274	532932.037127	42.773300
3504.122396	532915.296804	42.778304
3503.964554	532900.823064	42.783309
3503.827723	532865.886354	42.788314
3503.949031	532858.087301	42.793319
3503.678237	532838.478550	42.798324
3503.879980	532820.007520	42.803329
3503.761354	532801.081921	42.808333
3503.683364	532778.714658	42.813338
3503.716431	532782.043455	42.818343
3503.569792	532748.067870	42.823348
3503.967075	532726.484225	42.828353
3503.744528	532718.436338	42.833357
3503.708777	532702.831718	42.838362
3503.779286	532682.916238	42.843367
3503.670289	532671.516176	42.848372
3503.951919	532651.415735	42.853377
3503.796147	532640.124079	42.858381
3504.130392	532622.440167	42.863386
3503.861151	532609.953980	42.868391
3503.778995	532600.216733	42.873396
3504.093136	532574.452980	42.878401
3503.652806	532550.778651	42.883405
3503.616309	532548.308844	42.888410
3503.865058	532521.797557	42.893415
3503.607343	532505.116405	42.898420
3503.584608	532498.855503	42.903425
3503.479013	532484.827786	42.908429
3503.956979	532450.298164	42.913434
3503.865184	532448.847461	42.918439
3504.070381	532430.830093	42.923444
3504.018762	532401.991678	42.928449
3503.926131	532396.752164	42.933453
3504.059344	532369.652648	42.938458
3504.001523	532352.737663	42.943463
3503.949271	532323.596086	42.948468
3503.945749	532308.440650	42.953473
3503.788009	532298.866719	42.958477
3504.023461	532266.597876	42.963482
3503.976872	532261.098441	42.968487
3503.502032	532246.118473	42.973492
3503.805312	532218.486619	42.978497
3503.556226	532212.109815	42.983501
3503.507927	532182.664230	42.988506
3503.568347	532172.348463	42.993511
3503.398749	532170.000671	42.998516
3503.588317	532157.340568	43.003521
3503.816518	532144.270188	43.008525
3503.887312	532125.819029	43.013530
3503.737498	532121.295740	43.018535
3503.514532	532105.669588	43.023540
3504.061682	532088.254543	43.028545
3503.683347	532081.847591	43.033549
3503.416640	532057.942989	43.038554
3503.668330	532048.455756	43.043559
3503.742842	532023.739370	43.048564
3503.794557	532020.295649	43.053569
3503.467898	532001.300913	43.058573
3503.653343	531981.618973	43.063578
3503.679500	531973.935557	43.068583
3503.486295	531962.497762	43.073588
3503.686435	531938.872839	43.078593
3503.340548	531935.744542	43.083597
3503.458422	531933.149198	43.088602
3503.584882	531918.174922	43.093607
3503.423488	531902.134668	43.098612
3503.858189	531890.193417	43.103617
3503.406296	531900.469879	43.108621
3503.727371	531861.669481	43.113626
3503.661131	531856.880302	43.118631
3503.563679	531848.205941	43.123636
3503.715128	531832.015131	43.128641
3503.356042	531815.399779	43.133645
3503.431194	531809.931466	43.138650
3503.581711	531802.733522	43.143655
3503.761638	531792.044968	43.148660
3503.802385	531764.150674	43.153665
3503.365902	531762.451254	43.158669
3503.727740	531757.291262	43.163674
3503.615521	531733.715394	43.168679
3503.469457	531717.824091	43.173684
3503.641178	531714.512902	43.178689
3503.582110	531706.438652	43.183693
3503.699174	531674.743029	43.188698
3503.468337	531667.251643	43.193703
3503.623427	531665.761847	43.198708
3503.884573	531646.370648	43.203713
3503.640708	531637.769831	43.208717
3503.365396	531621.848336	43.213722
3503.506256	531616.015918	43.218727
3503.484483	531593.132847	43.223732
3503.793403	531570.854263	43.228737
3503.756457	531569.697939	43.233741
3503.475123	531553.423672	43.238746
3503.264420	531538.805450	43.243751
3503.740976	531533.576732	43.248756
3503.647378	531527.276116	43.253761
3503.386199	531519.637888	43.258765
3503.779224	531488.706626	43.263770
3503.621521	531487.923035	43.268775
3503.641025	531487.161961	43.273780
3503.639534	531456.292985	43.278785
3503.517257	531437.214736	43.283789
3503.665224	531434.513509	43.288794
3503.547487	531423.720180	43.293799
3503.397950	531395.400599	43.298804
3503.709892	531380.548060	43.303809
3503.608144	531401.126614	43.308813
3503.802696	531375.228212	43.313818
3503.665040	531361.760296	43.318823
3503.519414	531357.842393	43.323828
3503.596901	531352.626163	43.328833
3503.565052	531327.319212	43.333837
3503.793885	531304.446633	43.338842
3503.508902	531303.177922	43.343847
3503.553107	531285.841471	43.348852
3503.803377	531270.291256	43.353857
3503.486848	531261.853283	43.358861
3503.683438	531248.029307	43.363866
3503.641465	531228.584451	43.368871
3503.480156	531214.311779	43.373876
3503.698650	531208.365893	43.378881
3503.433549	531193.402283	43.383885
3503.795651	531178.996334	43.388890
3503.557911	531175.648697	43.393895
3503.641884	531161.236165	43.398900
3503.537337	531131.090158	43.403905
3503.259693	531123.757477	43.408909
3503.456838	531124.888195	43.413914
3503.721138	531113.983750	43.418919
3503.574658	531099.354966	43.423924
3503.378784	531083.117224	43.428929
3503.422206	531072.651847	43.433933
3503.804547	531072.439689	43.438938
3503.741590	531054.463113	43.443943
3503.374933	531043.001532	43.448948
3503.832320	531029.540334	43.453953
3503.507952	531024.134887	43.458957
3503.515854	530992.303561	43.463962
3503.867750	530987.043841	43.468967
3503.525000	530984.217996	43.473972
3503.572336	530950.763593	43.478977
3503.697599	530947.712203	43.483981
3503.681801	530929.677506	43.488986
3503.725291	530922.900264	43.493991
3503.683754	530911.639823	43.498996
3503.828778	530880.544458	43.504001
3503.560778	530880.081412	43.509005
3503.569830	530845.874974	43.514010
3503.411512	530851.710117	43.519015
3503.590052	530837.433913	43.524020
3503.523013	530837.646445	43.529025
3503.424958	530817.249979	43.534029
3503.554822	530800.909939	43.539034
3503.511103	530797.379983	43.544039
3503.593143	530790.950262	43.549044
3503.593087	530754.117794	43.554049
3503.504012	530752.969648	43.559053
3503.316832	530746.936129	43.564058
3503.371585	530750.261934	43.569063
3503.418142	530735.046530	43.574068
3503.600419	530721.426449	43.579073
3502.967213	530711.370914	43.584077
3503.277904	530706.622859	43.589082
3503.381432	530705.545319	43.594087
3503.389306	530692.710647	43.599092
3503.579771	530669.843204	43.604097
3503.144372	530660.817395	43.609101
3503.448892	530656.575548	43.614106
3503.455617	530652.431289	43.619111
3503.635496	530652.554275	43.624116
3503.814804	530638.378818	43.629121
3503.495206	530625.747420	43.634125
3503.585087	530622.600510	43.639130
3503.707342	530595.044920	43.644135
3503.578295	530583.697023	43.649140
3503.742207	530571.999667	43.654145
3503.536781	530580.974911	43.659149
3503.653095	530545.992988	43.664154
3503.435623	530545.420896	43.669159
3503.629077	530531.293632	43.674164
3503.612780	530521.595202	43.679169
3503.481896	530496.605709	43.684173
3503.516329	530494.073840	43.689178
3503.498697	530483.870345	43.694183
3503.137800	530482.007258	43.699188
3503.401814	530464.584632	43.704193
3503.546724	530448.191320	43.709197
3503.374493	530447.308922	43.714202
3503.373862	530444.833112	43.719207
3503.424507	530435.427202	43.724212
3503.581326	530412.362600	43.729217
3503.473333	530405.760652	43.734221
3503.523894	530392.060051	43.739226
3503.484379	530388.478813	43.744231
3503.274178	530378.154106	43.749236
3503.509385	530363.312732	43.754241
3503.490403	530355.787231	43.759245
3503.825666	530346.033131	43.764250
3503.750267	530336.798660	43.769255
3503.317249	530305.844036	43.774260
3503.134643	530308.045351	43.779265
3503.283293	530307.465912	43.784269
3503.359763	530304.422109	43.789274
3503.368889	530297.902658	43.794279
3503.394943	530273.949051	43.799284
3503.417730	530261.263246	43.804289
3503.499889	530259.077479	43.809293
3503.649539	530251.929486	43.814298
3503.486412	530237.252000	43.819303
3503.415235	530231.098895	43.824308
3503.744539	530209.522520	43.829313
3503.448983	530211.640647	43.834317
3503.410764	530187.141277	43.839322
3503.489633	530172.880221	43.844327
3503.441177	530172.736139	43.849332
3503.652381	530163.304691	43.854337
3503.354002	530147.587442	43.859341
3503.404260	530122.972935	43.864346
3503.274034	530126.681793	43.869351
3503.713504	530115.092125	43.874356
3503.802966	530103.103027	43.879361
3503.539019	530093.342419	43.884365
3503.537734	530078.588678	43.889370
3503.683616	530079.677049	43.894375
3503.624129	530056.444003	43.899380
3503.806255	530041.155973	43.904385
3503.531582	530033.114933	43.909389
3503.531798	530014.824018	43.914394
3503.567446	530000.973852	43.919399
3503.546481	529997.086431	43.924404
3503.562995	529982.531895	43.929409
3503.218878	529975.461814	43.934413
3503.536807	529961.011202	43.939418
3503.617727	529936.694720	43.944423
3503.541346	529937.161375	43.949428
3503.486634	529933.228745	43.954433
3503.453187	529915.397778	43.959437
3503.834457	529906.697206	43.964442
3503.693704	529906.769818	43.969447
3503.491574	529884.215915	43.974452
3503.878896	529858.132958	43.979457
3503.587143	529859.543147	43.984461
3503.532731	529856.418888	43.989466
3503.633366	529823.711565	43.994471
3503.598754	529815.228253	43.999476
3503.632017	529803.096225	44.004481
3503.233904	529801.390519	44.009485
3503.404903	529778.322745	44.014490
3503.378232	529774.234060	44.019495
3503.139025	529769.319994	44.024500
3503.556193	529766.879102	44.029505
3503.188725	529768.654959	44.034509
3503.398942	529753.766431	44.039514
3503.336821	529735.788209	44.044519
3503.172311	529722.575764	44.049524
3503.517415	529716.861945	44.054529
3503.698829	529720.976396	44.059533
3503.411026	529703.134859	44.064538
3503.270669	529684.916304	44.069543
3503.060888	529682.170261	44.074548
3503.366123	529668.630891	44.079553
3503.233996	529677.746649	44.084557
3503.237984	529671.429861	44.089562
3503.247629	529666.021681	44.094567
3503.046752	529645.993637	44.099572
3503.436609	529627.438578	44.104577
3502.862911	529627.680671	44.109581
3503.247334	529627.468171	44.114586
3503.261018	529638.683089	44.119591
3503.182953	529637.280480	44.124596
3503.380492	529617.593657	44.129601
3503.377611	529625.476343	44.134605
3503.296456	529604.115593	44.139610
3503.219805	529588.564852	44.144615
3502.969673	529588.199998	44.149620
3503.403921	529577.570798	44.154625
3503.425410	529578.224109	44.159629
3503.568837	529565.973431	44.164634
3503.429832	529551.392546	44.169639
3503.624671	529544.641317	44.174644
3503.647443	529535.138217	44.179649
3503.269633	529541.210649	44.184653
3503.395110	529527.093225	44.189658
3503.595884	529499.978060	44.194663
3503.541236	529482.048895	44.199668
3503.621760	529482.339180	44.204673
3503.397163	529467.923331	44.209677
3503.717427	529449.934876	44.214682
3503.409160	529448.568632	44.219687
3503.666756	529446.557141	44.224692
3503.766439	529409.604695	44.229697
3503.621163	529401.997640	44.234701
3503.677383	529403.100229	44.239706
3503.699035	529385.815770	44.244711
3503.663436	529360.506234	44.249716
3503.680886	529350.852276	44.254721
3503.679454	529349.589117	44.259725
3503.744525	529316.431599	44.264730
3503.863299	529314.997851	44.269735
3503.625124	529300.937699	44.274740
3503.788399	529275.040773	44.279745
3503.736772	529267.065146	44.284749
3503.428468	529248.064159	44.289754
3503.462265	529233.859904	44.294759
3503.444383	529214.560329	44.299764
3503.768021	529220.522024	44.304769
3503.437134	529220.574159	44.309773
3503.444139	529193.893326	44.314778
3503.504442	529179.331126	44.319783
3503.289726	529187.853866	44.324788
3503.657950	529179.963429	44.329793
3503.264925	529171.182707	44.334797
3503.395988	529144.179006	44.339802
3503.566890	529141.473762	44.344807
3503.357343	529140.900363	44.349812
3503.468576	529135.728594	44.354817
3503.033848	529124.427951	44.359821
3503.408289	529093.848617	44.364826
3503.348373	529092.746269	44.369831
3503.212140	529084.076504	44.374836
3503.702572	529086.879036	44.379841
3503.392186	529080.510636	44.384845
3503.291030	529053.442421	44.389850
3503.496982	529063.970472	44.394855
3503.333305	529045.704331	44.399860
3503.572651	529044.807334	44.404865
3503.492200	529038.806817	44.409869
3503.753443	529009.154749	44.414874
3503.573907	529013.023252	44.419879
3503.495172	528999.998763	44.424884
3503.476157	528987.470127	44.429889
3503.087183	528961.811557	44.434893
3503.417724	528959.839007	44.439898
3503.395774	528954.283984	44.444903
3503.170164	528953.409935	44.449908
3503.472729	528940.123014	44.454913
3503.191216	528920.965805	44.459917
3503.606413	528905.084003	44.464922
3503.343202	528898.000647	44.469927
3503.363139	528896.582482	44.474932
3503.473139	528900.860027	44.479937
3503.368614	528881.422146	44.484941
3503.592760	528862.488133	44.489946
3503.077915	528867.066563	44.494951
3502.997330	528857.478327	44.499956
3503.295726	528851.771579	44.504961
3503.422793	528866.203087	44.509965
3503.509402	528847.796099	44.514970
3503.403542	528821.536719	44.519975
3503.322074	528825.288706	44.524980
3503.745713	528815.570225	44.529985
3503.691151	528808.251729	44.534989
3503.401981	528787.428054	44.539994
3503.197554	528773.412626	44.544999
3503.094067	528773.883599	44.550004
3503.455350	528761.345210	44.555009
3503.164333	528761.643698	44.560013
3503.231729	528764.765802	44.565018
3503.270961	528729.690959	44.570023
3503.451286	528718.393880	44.575028
3503.294852	528714.426490	44.580033
3503.268818	528722.010101	44.585037
3503.353545	528720.985930	44.590042
3503.406892	528703.695713	44.595047
3503.347625	528690.870017	44.600052
3503.811383	528685.440261	44.605057
3503.320088	528674.552483	44.610061
3503.518681	528669.063567	44.615066
3503.309398	528647.873363	44.620071
3503.230780	528634.040052	44.625076
3503.800331	528630.058966	44.630081
3503.553000	528625.449012	44.635085
3503.751690	528599.595912	44.640090
3503.593520	528593.203256	44.645095
3503.338884	528589.554544	44.650100
3503.566451	528576.178107	44.655105
3503.484013	528557.393245	44.660109
3503.321356	528547.059818	44.665114
3503.330482	528538.013057	44.670119
3502.966318	528537.312477	44.675124
3503.390372	528522.540587	44.680129
3503.244334	528535.044826	44.685133
3503.390210	528508.340885	44.690138
3503.531034	528496.241383	44.695143
3503.549003	528494.014985	44.700148
3503.655865	528485.357002	44.705153
3503.487371	528485.130812	44.710157
3503.282794	528470.710884	44.715162
3503.415011	528459.016968	44.720167
3503.438936	528464.824192	44.725172
3503.716613	528455.128558	44.730177
3503.340218	528431.892666	44.735181
3503.149803	528415.600767	44.740186
3503.230677	528417.255382	44.745191
3502.849048	528415.850107	44.750196
3503.317926	528410.874237	44.755201
3503.275592	528407.141397	44.760205
3503.212175	528417.661921	44.765210
3503.262553	528402.342592	44.770215
3502.853112	528372.946924	44.775220
3503.327926	528356.448764	44.780225
3503.012555	528358.267073	44.785229
3503.505773	528366.324644	44.790234
3503.596487	528353.070712	44.795239
3503.258580	528360.602723	44.800244
3503.505079	528343.180521	44.805249
3503.383124	528333.093182	44.810253
3503.242670	528318.814578	44.815258
3503.632530	528321.734209	44.820263
3503.689965	528308.990823	44.825268
3503.869522	528286.222707	44.830273
3503.223663	528289.659761	44.835277
3503.243298	528278.589894	44.840282
3503.904343	528266.761725	44.845287
3503.378402	528252.139725	44.850292
3503.608686	528231.485880	44.855297
3503.570990	528229.571439	44.860301
3503.292716	528216.881035	44.865306
3503.269247	528202.887033	44.870311
3503.314470	528185.900730	44.875316
3503.733037	528172.493766	44.880321
3503.222430	528183.287253	44.885325
3503.424858	528170.722970	44.890330
3503.583164	528157.407659	44.895335
3503.092939	528149.955581	44.900340
3503.186037	528128.666356	44.905345
3503.327649	528143.803687	44.910349
3503.102104	528123.878671	44.915354
3503.134403	528129.634161	44.920359
3502.740531	528132.879824	44.925364
3503.430318	528133.730773	44.930369
3503.068103	528110.492166	44.935373
3503.284542	528096.914951	44.940378
3503.292234	528088.777754	44.945383
3502.996981	528090.441315	44.950388
3503.356498	528095.740838	44.955393
3503.431866	528086.784416	44.960397
3503.313264	528070.986142	44.965402
3503.531489	528062.916724	44.970407
3503.154379	528047.715147	44.975412
3503.609545	528042.033865	44.980417
3502.920048	528042.092143	44.985421
3503.447543	528034.226499	44.990426
3503.488149	528041.294572	44.995431
3503.302303	528007.971828	45.000436
3503.142550	528002.084516	45.005441
3503.158783	527997.432723	45.010445
3503.358409	527991.640209	45.015450
3503.108431	528006.839561	45.020455
3502.999355	527996.194105	45.025460
3503.326107	527986.692562	45.030465
3503.214565	527994.946971	45.035469
3503.335485	527956.774966	45.040474
3503.487120	527954.830568	45.045479
3503.229132	527951.839172	45.050484
3503.293607	527943.591859	45.055489
3502.998071	527952.633371	45.060493
3503.282989	527950.920576	45.065498
3503.227324	527925.056039	45.070503
3503.146088	527914.557729	45.075508
3503.620354	527908.368044	45.080513
3503.498217	527904.243428	45.085517
3503.413813	527902.336329	45.090522
3503.439620	527886.969851	45.095527
3503.277915	527874.563950	45.100532
3503.527033	527862.648984	45.105537
3503.271748	527861.880629	45.110541
3503.215502	527862.798966	45.115546
3503.446355	527853.918906	45.120551
3503.442987	527837.900052	45.125556
3503.629150	527815.231283	45.130561
3503.556824	527821.559294	45.135565
3503.069971	527820.372731	45.140570
3503.368049	527811.987362	45.145575
3503.075695	527786.513744	45.150580
3503.482984	527773.765168	45.155585
3503.078353	527776.254592	45.160589
3503.338581	527768.986932	45.165594
3503.261352	527778.954188	45.170599
3503.159850	527773.259721	45.175604
3503.684507	527754.529559	45.180609
3503.427519	527748.758589	45.185613
3503.192234	527737.273824	45.190618
3503.563859	527731.807772	45.195623
3503.301102	527738.570186	45.200628
3503.447580	527722.325396	45.205633
3503.463313	527709.588118	45.210637
3503.487401	527691.139130	45.215642
3503.467421	527690.181976	45.220647
3503.418048	527697.112821	45.225652
3503.678157	527656.542982	45.230657
3503.371210	527657.602021	45.235661
3503.642648	527644.723209	45.240666
3503.752797	527646.878623	45.245671
3503.046767	527615.759712	45.250676
3503.394086	527597.208996	45.255681
3503.580603	527610.015149	45.260685
3503.785834	527600.785255	45.265690
3503.430993	527584.063673	45.270695
3503.316963	527572.711229	45.275700
3503.764138	527568.395479	45.280705
3503.568738	527566.606951	45.285709
3503.688059	527543.493545	45.290714
3503.993993	527522.574146	45.295719
3503.763343	527505.327505	45.300724
3503.732468	527487.392316	45.305729
3503.472743	527470.605046	45.310733
3503.974133	527463.753948	45.315738
3504.055171	527441.151794	45.320743
3503.473482	527423.808938	45.325748
3503.696395	527414.323465	45.330753
3503.320570	527399.070525	45.335757
3503.092823	527373.636566	45.340762
3503.296370	527373.907449	45.345767
3503.013228	527371.122058	45.350772
3502.985956	527360.362175	45.355777
3503.155424	527367.410183	45.360781
3503.203702	527364.117594	45.365786
3503.471572	527374.333776	45.370791
3503.059384	527371.215033	45.375796
3503.392823	527335.787389	45.380801
3503.397780	527330.530756	45.385805
3503.171837	527322.581697	45.390810
3503.078093	527324.718844	45.395815
3502.943829	527315.592975	45.400820
3503.432956	527319.103533	45.405825
3503.255072	527321.102371	45.410829
3503.466458	527312.022943	45.415834
3503.295795	527291.077493	45.420839
3503.169523	527298.273344	45.425844
3503.098963	527281.708655	45.430849
3503.040183	527291.521695	45.435853
3503.258107	527275.063013	45.440858
3503.121143	527287.718408	45.445863
3503.115674	527281.200016	45.450868
3503.381256	527257.608258	45.455873
3503.162435	527245.817320	45.460877
3503.542366	527226.502981	45.465882
3503.613498	527226.491578	45.470887
3503.371325	527234.918635	45.475892
3503.427208	527218.839254	45.480897
3503.432882	527205.547267	45.485901
3503.474269	527186.791744	45.490906
3503.567821	527194.508795	45.495911
3503.217820	527180.565496	45.500916
3503.455026	527152.581437	45.505921
3503.051879	527145.873160	45.510925
3503.104695	527144.550715	45.515930
3503.262684	527136.136595	45.520935
3503.328112	527144.767765	45.525940
3503.428952	527135.756244	45.530945
3503.212367	527128.159360	45.535949
3503.271053	527115.414816	45.540954
3503.552150	527106.223182	45.545959
3503.333613	527100.951259	45.550964
3503.397587	527092.198221	45.555969
3503.119617	527095.476311	45.560973
3502.965153	527089.789968	45.565978
3503.218941	527078.379038	45.570983
3502.783450	527063.185740	45.575988
3502.755996	527059.652375	45.580993
3503.050454	527058.645487	45.585997
3503.067238	527048.737547	45.591002
3502.958982	527058.962841	45.596007
3502.822567	527052.465051	45.601012
3503.166834	527048.013816	45.606017
3503.006816	527052.637756	45.611021
3502.907466	527049.368433	45.616026
3503.271617	527041.325971	45.621031
3502.870725	527048.262119	45.626036
3503.375048	527047.070453	45.631041
3503.058293	527046.564454	45.636045
3503.328981	527044.297911	45.641050
3503.588326	527049.108256	45.646055
3503.569261	527023.388072	45.651060
3503.789704	527010.061978	45.656065
3503.517221	527011.974733	45.661069
3503.428346	526992.835276	45.666074
3503.376869	526968.838369	45.671079
3503.561082	526969.971437	45.676084
3503.538998	526951.983717	45.681089
3503.256675	526963.752683	45.686093
3503.226683	526937.528721	45.691098
3503.661646	526926.442806	45.696103
3503.312146	526923.111919	45.701108
3503.427215	526915.917348	45.706113
3503.289633	526918.768993	45.711117
3503.209632	526901.346274	45.716122
3503.660658	526877.926791	45.721127
3503.406774	526876.299037	45.726132
3503.330043	526864.030526	45.731137
3503.478676	526878.005608	45.736141
3503.340308	526857.408239	45.741146
3503.561185	526838.371252	45.746151
3503.176004	526837.926597	45.751156
3503.182629	526826.352401	45.756161
3503.208055	526832.412672	45.761165
3503.142818	526831.159395	45.766170
3503.214350	526828.014631	45.771175
3503.311869	526801.921904	45.776180
3503.394160	526794.479773	45.781185
3503.141327	526783.047626	45.786189
3503.352930	526784.378528	45.791194
3503.581365	526784.847637	45.796199
3503.015828	526773.363830	45.801204
3503.508506	526759.489128	45.806209
3503.156587	526740.239328	45.811213
3502.978804	526747.140345	45.816218
3503.318367	526738.444631	45.821223
3503.424346	526748.181430	45.826228
3503.422747	526738.326739	45.831233
3503.426452	526715.382013	45.836237
3503.236422	526691.558197	45.841242
3503.369958	526698.713258	45.846247
3503.323453	526682.346292	45.851252
3503.383459	526684.661375	45.856257
3503.313402	526686.289488	45.861261
3503.039200	526663.641296	45.866266
3503.478699	526654.525442	45.871271
3503.415397	526646.550339	45.876276
3503.541643	526647.692592	45.881281
3503.328312	526644.643350	45.886285
3503.625972	526632.467103	45.891290
3503.671714	526614.063980	45.896295
3503.186914	526609.137200	45.901300
3503.789655	526602.876170	45.906305
3503.736978	526580.698228	45.911309
3503.306807	526561.864881	45.916314
3503.560129	526549.897729	45.921319
3503.361194	526555.993564	45.926324
3503.116119	526557.447199	45.931329
3503.115903	526529.701720	45.936333
3503.366138	526504.089749	45.941338
3503.594506	526507.186859	45.946343
3503.103334	526506.860021	45.951348
3503.193332	526500.376759	45.956353
3503.274906	526506.023974	45.961357
3503.411444	526497.259141	45.966362
3503.457302	526474.256867	45.971367
3503.690974	526471.844480	45.976372
3503.729660	526453.391748	45.981377
3503.365565	526462.697632	45.986381
3503.210715	526425.374141	45.991386
3503.571581	526427.995481	45.996391
3503.285769	526411.564981	46.001396
3503.128737	526414.824096	46.006401
3503.267343	526410.506266	46.011405
3503.605773	526409.846158	46.016410
3503.503903	526383.228334	46.021415
3503.201227	526371.500537	46.026420
3503.506645	526381.054425	46.031425
3503.165954	526377.014490	46.036429
3503.162920	526361.752171	46.041434
3503.215117	526336.727154	46.046439
3503.220692	526338.747658	46.051444
3503.075954	526334.120818	46.056449
3503.181748	526334.659863	46.061453
3503.097462	526330.680470	46.066458
3503.309948	526322.459462	46.071463
3503.114984	526325.067588	46.076468
3502.959503	526325.344694	46.081473
3502.846293	526338.654092	46.086477
3503.020846	526334.835947	46.091482
3503.159953	526331.023403	46.096487
3502.904552	526320.955872	46.101492
3503.149015	526299.033808	46.106497
3503.200296	526298.772849	46.111501
3503.313046	526293.195605	46.116506
3503.259153	526291.182411	46.121511
3503.308782	526278.893477	46.126516
3503.650898	526278.333859	46.131521
3503.505209	526280.833126	46.136525
3503.063079	526258.008742	46.141530
3503.448264	526252.843276	46.146535
3503.129692	526241.825440	46.151540
3502.885885	526246.412317	46.156545
3502.775827	526241.678891	46.161549
3503.192356	526240.197810	46.166554
3503.381589	526239.409658	46.171559
3502.959863	526250.746331	46.176564
3503.409252	526222.221713	46.181569
3502.789237	526216.204323	46.186573
3503.007928	526199.845487	46.191578
3503.446660	526193.155367	46.196583
3503.044166	526193.673671	46.201588
3503.374304	526187.253407	46.206593
3503.305781	526187.820006	46.211597
3503.088080	526186.338079	46.216602
3503.030684	526184.578121	46.221607
3503.267609	526201.875425	46.226612
3503.456524	526160.504397	46.231617
3503.312986	526151.530942	46.236621
3503.227465	526144.367726	46.241626
3503.295561	526147.692394	46.246631
3503.029401	526152.030133	46.251636
3503.149508	526143.520399	46.256641
3503.241390	526141.130372	46.261645
3503.178505	526120.520119	46.266650
3503.146080	526108.092404	46.271655
3503.356932	526109.928876	46.276660
3503.718781	526100.319585	46.281665
3503.257869	526100.897664	46.286669
3502.959499	526105.392125	46.291674
3503.079855	526085.763654	46.296679
3502.998704	526073.242534	46.301684
3503.170472	526067.959120	46.306689
3503.389448	526060.646664	46.311693
3503.290982	526050.352001	46.316698
3503.318576	526061.971571	46.321703
3502.821568	526065.436107	46.326708
3503.300217	526063.338719	46.331713
3502.931152	526047.325316	46.336717
3503.379342	526054.734175	46.341722
3503.610611	526031.954657	46.346727
3503.323282	526012.137830	46.351732
3503.389308	526005.961393	46.356737
3503.568734	526014.979478	46.361741
3503.568503	525999.261512	46.366746
3503.534142	525975.866879	46.371751
3503.473693	525973.046044	46.376756
3503.900298	525957.563817	46.381761
3503.665498	525942.186106	46.386765
3503.707453	525926.360322	46.391770
3503.718249	525919.838801	46.396775
3503.493691	525907.896156	46.401780
3503.367951	525886.486894	46.406785
3503.435513	525880.512327	46.411789
3503.713840	525872.988244	46.416794
3503.811077	525863.117391	46.421799
3503.692977	525847.822226	46.426804
3503.778120	525824.054703	46.431809
3503.435010	525820.520410	46.436813
3503.517000	525792.053091	46.441818
3504.177091	525784.822413	46.446823
3503.364541	525772.315570	46.451828
3503.538627	525737.617125	46.456833
3503.338357	525743.208074	46.461837
3503.528374	525735.546262	46.466842
3503.764932	525728.129794	46.471847
3503.237046	525715.830619	46.476852
3503.633390	525694.389127	46.481857
3503.278421	525689.239378	46.486861
3503.189280	525684.401399	46.491866
3503.402301	525695.587605	46.496871
3503.459887	525679.455861	46.501876
3503.650771	525650.263509	46.506881
3503.579296	525658.462254	46.511885
3503.406149	525644.439114	46.516890
3503.417962	525620.581795	46.521895
3503.176023	525607.175985	46.526900
3503.965808	525586.025953	46.531905
3503.501927	525591.102667	46.536909
3503.438809	525577.163159	46.541914
3503.604272	525573.851680	46.546919
3503.286934	525560.963158	46.551924
3503.609166	525562.731550	46.556929
3503.591454	525557.073586	46.561933
3503.440076	525538.498211	46.566938
3503.511623	525513.216138	46.571943
3503.212152	525520.642329	46.576948
3503.488076	525506.649176	46.581953
3503.602795	525494.298810	46.586957
3503.647653	525472.811490	46.591962
3503.481563	525472.736496	46.596967
3503.414609	525467.136824	46.601972
3503.728399	525436.206249	46.606977
3503.285703	525423.084720	46.611981
3503.338986	525413.473244	46.616986
3503.647989	525415.698618	46.621991
3503.358943	525405.433659	46.626996
3503.581021	525383.311711	46.632001
3503.397716	525378.993937	46.637005
3503.427895	525370.902338	46.642010
3503.161402	525371.955129	46.647015
3503.012761	525375.769088	46.652020
3503.247766	525358.699230	46.657025
3503.150035	525339.710811	46.662029
3503.266522	525338.580321	46.667034
3503.395737	525320.061429	46.672039
3503.191464	525326.663993	46.677044
3503.644191	525327.198784	46.682049
3503.532765	525314.429144	46.687053
3503.567998	525287.939450	46.692058
3503.354367	525282.817772	46.697063
3503.170829	525285.171550	46.702068
3503.451674	525273.199094	46.707073
3503.284150	525256.344371	46.712077
3503.046582	525245.161416	46.717082
3503.570836	525237.143289	46.722087
3503.234617	525238.965241	46.727092
3503.474443	525234.176217	46.732097
3503.363534	525228.836119	46.737101
3503.312310	525207.616338	46.742106
3503.382490	525197.041760	46.747111
3503.240054	525188.926807	46.752116
3503.402281	525175.355673	46.757121
3503.166231	525190.302796	46.762125
3503.008866	525187.749850	46.767130
3503.244688	525180.181618	46.772135
3503.135014	525160.335655	46.777140
3503.318241	525142.111275	46.782145
3503.337461	525134.829967	46.787149
3503.475367	525132.836856	46.792154
3503.792043	525136.071905	46.797159
3503.367647	525112.282769	46.802164
3503.342162	525100.712396	46.807169
3503.394660	525092.920384	46.812173
3503.505175	525084.411602	46.817178
3503.693274	525077.760632	46.822183
3503.122620	525060.767244	46.827188
3503.227680	525056.100553	46.832193
3503.325868	525054.265337	46.837197
3503.522907	525040.385331	46.842202
3503.629936	525042.844849	46.847207
3503.107573	525027.865504	46.852212
3503.465601	524999.403690	46.857217
3503.450541	525000.467310	46.862221
3503.574284	524992.765075	46.867226
3503.675175	524985.571877	46.872231
3503.375587	524955.899804	46.877236
3503.687725	524948.319401	46.882241
3503.285366	524949.899123	46.887245
3503.183932	524945.366121	46.892250
3503.539475	524933.937580	46.897255
3503.450184	524917.322850	46.902260
3503.681453	524902.123193	46.907265
3503.445754	524894.427175	46.912269
3503.251357	524889.858307	46.917274
3503.508648	524859.238807	46.922279
3503.312016	524858.056684	46.927284
3503.685907	524845.361597	46.932289
3503.395094	524856.729107	46.937293
3503.733772	524839.895029	46.942298
3503.626116	524825.203754	46.947303
3503.605635	524828.795413	46.952308
3503.516495	524806.266964	46.957313
3503.184463	524787.213833	46.962317
3503.170922	524772.709810	46.967322
3503.213879	524768.002306	46.972327
3503.486016	524765.431956	46.977332
3503.335824	524765.910425	46.982337
3503.022575	524777.786972	46.987341
3503.246821	524763.750796	46.992346
3503.190776	524732.776227	46.997351
3503.227945	524732.416387	47.002356
3503.361446	524724.459762	47.007361
3503.294492	524721.387015	47.012365
3503.118694	524723.385845	47.017370
3503.316501	524720.978866	47.022375
3503.235785	524719.171888	47.027380
3503.138922	524695.077646	47.032385
3502.980156	524684.538914	47.037389
3503.064198	524668.755778	47.042394
3503.182286	524671.516869	47.047399
3502.995446	524681.402297	47.052404
3503.183177	524680.361589	47.057409
3503.077406	524677.345512	47.062413
3502.774651	524675.219814	47.067418
3503.286109	524665.737653	47.072423
3503.299507	524678.017544	47.077428
3503.317676	524667.905732	47.082433
3503.133188	524649.587277	47.087437
3503.055809	524635.143763	47.092442
3503.706604	524626.195541	47.097447
3503.228864	524642.798781	47.102452
3503.567675	524625.762281	47.107457
3503.754472	524624.873350	47.112461
3503.398470	524602.336246	47.117466
3503.570071	524593.514286	47.122471
3503.516662	524585.081691	47.127476
3503.424319	524568.669259	47.132481
3503.259815	524556.716111	47.137485
3503.179099	524546.063863	47.142490
3503.340374	524530.773828	47.147495
3503.154502	524548.038658	47.152500
3503.387972	524543.402067	47.157505
3503.259632	524551.206012	47.162509
3503.074894	524521.262260	47.167514
3503.301859	524507.528696	47.172519
3502.982088	524490.747773	47.177524
3503.304134	524480.789994	47.182529
3502.891284	524495.108628	47.187533
3503.097681	524490.425756	47.192538
3503.222041	524477.365461	47.197543
3502.934698	524493.584951	47.202548
3503.291023	524479.072752	47.207553
3503.247589	524483.325194	47.212557
3503.237851	524469.376285	47.217562
3503.349051	524441.508483	47.222567
3503.213988	524438.648625	47.227572
3503.270557	524431.007282	47.232577
3503.174078	524433.499058	47.237581
3503.102586	524442.355509	47.242586
3503.881642	524427.978631	47.247591
3503.402234	524414.255538	47.252596
3503.382220	524393.130835	47.257601
3503.399155	524397.525394	47.262605
3503.411269	524390.901953	47.267610
3503.562369	524384.711447	47.272615
3503.282566	524362.970681	47.277620
3503.632119	524347.347445	47.282625
3503.621764	524342.547153	47.287629
3503.459979	524330.896676	47.292634
3503.546607	524304.245599	47.297639
3503.296012	524299.533807	47.302644
3503.172743	524299.654219	47.307649
3503.135748	524301.732254	47.312653
3503.428770	524301.635238	47.317658
3503.398064	524279.652810	47.322663
3502.957007	524267.844245	47.327668
3503.301705	524246.307892	47.332673
3503.167944	524257.903729	47.337677
3502.987243	524252.169972	47.342682
3503.184799	524243.192082	47.347687
3503.210224	524246.726071	47.352692
3503.006953	524246.758036	47.357697
3503.061336	524256.959417	47.362701
3503.232286	524238.382136	47.367706
3503.457600	524222.727870	47.372711
3502.947784	524210.222494	47.377716
3503.216117	524214.678461	47.382721
3502.903002	524211.189613	47.387725
3502.941606	524208.656084	47.392730
3503.284369	524209.006114	47.397735
3503.238016	524210.731822	47.402740
3503.023352	524208.440502	47.407745
3503.017934	524215.113184	47.412749
3503.450391	524217.925761	47.417754
3503.408843	524182.044940	47.422759
3503.101117	524171.023957	47.427764
3503.108810	524167.939307	47.432769
3502.855914	524174.297301	47.437773
3502.966462	524161.946569	47.442778
3503.277131	524154.062753	47.447783
3502.943949	524163.921081	47.452788
3503.018050	524156.883383	47.457793
3502.732175	524163.297139	47.462797
3502.780970	524173.752183	47.467802
3503.291777	524167.150925	47.472807
3502.936493	524166.903643	47.477812
3503.339125	524155.517654	47.482817
3503.299044	524156.585284	47.487821
3503.174574	524135.780025	47.492826
3503.285824	524117.313130	47.497831
3503.130377	524126.385207	47.502836
3503.456610	524111.978524	47.507841
3503.303299	524119.078985	47.512845
3503.304587	524106.745479	47.517850
3503.536956	524099.986017	47.522855
3503.263209	524086.129046	47.527860
3503.382331	524073.423072	47.532865
3503.365020	524074.739838	47.537869
3503.132074	524082.459451	47.542874
3503.200085	524075.169951	47.547879
3503.051295	524062.152489	47.552884
3503.371174	524031.470975	47.557889
3503.214459	524037.409454	47.562893
3503.336801	524038.148147	47.567898
3503.416956	524026.358119	47.572903
3503.132749	524036.562607	47.577908
3503.272106	524027.947616	47.582913
3503.484742	524003.702330	47.587917
3503.415069	523995.271996	47.592922
3503.421078	523985.262768	47.597927
3503.184179	523988.231720	47.602932
3503.268788	523977.906789	47.607937
3503.379270	523975.766232	47.612941
3503.223941	523949.910999	47.617946
3502.981004	523941.811297	47.622951
3503.244583	523935.147926	47.627956
3503.277281	523933.980034	47.632961
3503.383024	523941.545094	47.637965
3503.241190	523937.574199	47.642970
3503.591560	523931.453118	47.647975
3503.345537	523910.970056	47.652980
3503.371763	523901.917961	47.657985
3503.175432	523896.489826	47.662989
3503.271668	523903.298211	47.667994
3503.466805	523894.825972	47.672999
3503.161114	523881.984800	47.678004
3503.208609	523850.183423	47.683009
3503.495725	523851.452094	47.688013
3503.552894	523846.691528	47.693018
3503.487859	523843.871042	47.698023
3503.076694	523841.105260	47.703028
3503.445881	523820.373212	47.708033
3503.306799	523814.127255	47.713037
3503.240196	523799.782380	47.718042
3503.700244	523788.589244	47.723047
3503.068606	523795.765446	47.728052
3503.193400	523787.102081	47.733057
3503.143961	523777.708047	47.738061
3503.211490	523762.937566	47.743066
3503.483126	523756.070661	47.748071
3502.940332	523756.257380	47.753076
3503.194720	523747.725153	47.758081
3503.249520	523751.608436	47.763085
3502.919775	523752.469139	47.768090
3503.284173	523745.941396	47.773095
3503.201606	523741.253430	47.778100
3503.201360	523714.817294	47.783105
3503.326287	523716.061062	47.788109
3503.463442	523705.727652	47.793114
3503.550453	523709.454214	47.798119
3502.985056	523712.930056	47.803124
3503.424152	523701.891813	47.808129
3503.260049	523685.540367	47.813133
3502.996011	523674.663779	47.818138
3503.473373	523654.925363	47.823143
3503.307985	523661.370822	47.828148
3503.397515	523646.748399	47.833153
3503.479939	523656.794087	47.838157
3503.412286	523632.036523	47.843162
3503.384349	523615.966768	47.848167
3503.485523	523605.184055	47.853172
3503.396917	523610.909738	47.858177
3503.559160	523599.207519	47.863181
3503.278357	523585.300684	47.868186
3503.552530	523556.900119	47.873191
3503.317782	523561.031400	47.878196
3503.222554	523558.468372	47.883201
3503.446016	523555.096766	47.888205
3503.218108	523541.282627	47.893210
3503.479052	523524.712198	47.898215
3503.163921	523511.012914	47.903220
3503.098751	523513.449336	47.908225
3503.041656	523512.497796	47.913229
3503.167917	523523.092663	47.918234
3503.442989	523507.227648	47.923239
3503.114746	523505.813486	47.928244
3503.071781	523471.447731	47.933249
3503.047864	523475.191879	47.938253
3503.032572	523463.972549	47.943258
3502.986586	523462.614869	47.948263
3503.051928	523469.478868	47.953268
3503.500165	523462.280641	47.958273
3503.220662	523460.302746	47.963277
3503.114058	523464.868728	47.968282
3503.427730	523452.434802	47.973287
3503.398108	523447.131810	47.978292
3503.156639	523436.807520	47.983297
3503.173475	523424.925965	47.988301
3503.405393	523425.799011	47.993306
3503.113864	523416.139741	47.998311
3502.974782	523426.321677	48.003316
3503.218227	523417.942649	48.008321
3502.804644	523413.155260	48.013325
3502.962932	523418.184868	48.018330
3503.218921	523414.808092	48.023335
3503.073819	523386.726232	48.028340
3503.193491	523381.399623	48.033345
3503.397920	523373.380574	48.038349
3503.249163	523371.685292	48.043354
3503.598048	523365.918068	48.048359
3503.418998	523374.741557	48.053364
3503.379119	523351.495611	48.058369
3503.594257	523337.358536	48.063373
3503.115000	523349.312919	48.068378
3503.522052	523340.705802	48.073383
3503.419401	523339.913095	48.078388
3503.737395	523308.927216	48.083393
3503.544184	523294.349159	48.088397
3503.339546	523292.662701	48.093402
3503.716722	523283.200955	48.098407
3503.310880	523264.157679	48.103412
3503.058569	523252.571276	48.108417
3503.296626	523241.615041	48.113421
3503.566260	523240.308557	48.118426
3503.292746	523242.525205	48.123431
3503.485516	523225.004824	48.128436
3503.149951	523204.989951	48.133441
3503.208054	523201.341114	48.138445
3503.156997	523198.821597	48.143450
3503.316721	523183.985466	48.148455
3502.934465	523194.913660	48.153460
3503.316494	523192.628986	48.158465
3503.757892	523185.684460	48.163469
3503.353567	523172.555018	48.168474
3503.449204	523147.417062	48.173479
3503.144864	523148.324329	48.178484
3503.316414	523145.264134	48.183489
3503.306442	523150.623711	48.188493
3503.227730	523123.036386	48.193498
3503.458782	523103.740616	48.198503
3503.290558	523106.901070	48.203508
3503.340555	523095.317324	48.208513
3503.352235	523103.251486	48.213517
3502.898735	523105.243855	48.218522
3503.148752	523090.696661	48.223527
3503.258500	523073.239786	48.228532
3503.508252	523052.778374	48.233537
3503.063692	523061.441801	48.238541
3503.037841	523054.217223	48.243546
3503.201968	523040.290146	48.248551
3503.286042	523052.256813	48.253556
3503.120805	523055.315707	48.258561
3502.943924	523050.743544	48.263565
3502.853501	523047.219245	48.268570
3503.055276	523047.642136	48.273575
3503.074696	523043.847730	48.278580
3503.140875	523017.854894	48.283585
3503.159845	523010.319918	48.288589
3503.183852	523011.579692	48.293594
3503.515206	522996.362420	48.298599
3502.990795	523001.550605	48.303604
3503.077856	522998.250990	48.308609
3502.980776	523005.444152	48.313613
3502.915141	522995.951125	48.318618
3503.151979	523001.372842	48.323623
3503.206529	523003.739871	48.328628
3503.060376	522984.200279	48.333633
3502.869835	522971.896222	48.338637
3502.895144	522959.810788	48.343642
3503.083075	522947.093051	48.348647
3502.916453	522950.354381	48.353652
3503.056892	522955.892448	48.358657
3503.191660	522957.387467	48.363661
3502.963186	522952.014641	48.368666
3502.871428	522959.358631	48.373671
3502.642603	522958.939692	48.378676
3503.137662	522948.397584	48.383681
3503.038847	522955.692141	48.388685
3502.787920	522955.276695	48.393690
3503.137088	522952.238942	48.398695
3502.549742	522953.595342	48.403700
3502.889351	522950.508549	48.408705
3503.259251	522960.913632	48.413709
3502.935263	522946.103182	48.418714
3503.098338	522955.883814	48.423719
3502.788061	522948.097549	48.428724
3503.338099	522955.340108	48.433729
3503.228743	522947.016595	48.438733
3502.997566	522954.584818	48.443738
3503.206398	522942.419817	48.448743
3502.975239	522930.374894	48.453748
3503.136981	522911.848090	48.458753
3503.274386	522904.294347	48.463757
3503.214288	522905.365223	48.468762
3503.418265	522912.561395	48.473767
3502.985566	522907.675776	48.478772
3503.238018	522908.393959	48.483777
3502.959735	522901.411406	48.488781
3502.533726	522903.450003	48.493786
3503.069985	522906.296958	48.498791
3503.234613	522895.402644	48.503796
3503.260789	522893.376367	48.508801
3502.989830	522868.346465	48.513805
3503.183366	522861.036578	48.518810
3503.007403	522862.024670	48.523815
3502.709569	522872.029846	48.528820
3502.877649	522859.062430	48.533825
3502.822289	522863.064437	48.538829
3502.948116	522859.152072	48.543834
3503.161669	522845.520313	48.548839
3502.869856	522863.460835	48.553844
3503.295572	522860.057119	48.558849
3502.962007	522871.129485	48.563853
3503.103849	522856.851925	48.568858
3503.120683	522856.343609	48.573863
3502.859030	522862.703501	48.578868
3502.955649	522858.189157	48.583873
3503.288403	522848.430880	48.588877
3502.972605	522848.379531	48.593882
3503.324258	522843.471028	48.598887
3503.346949	522823.348510	48.603892
3503.299547	522803.287595	48.608897
3503.264620	522809.813874	48.613901
3503.081802	522805.394229	48.618906
3503.430202	522803.519214	48.623911
3503.439295	522816.003405	48.628916
3503.684761	522788.768672	48.633921
3503.271863	522775.994110	48.638925
3503.078052	522768.644300	48.643930
3503.200310	522760.031335	48.648935
3503.030569	522763.596495	48.653940
3503.046385	522769.053223	48.658945
3502.816059	522773.436753	48.663949
3502.956882	522768.915398	48.668954
3503.505304	522751.439394	48.673959
3503.223419	522737.279247	48.678964
3503.194015	522719.641783	48.683969
3503.557045	522718.977647	48.688973
3502.979739	522729.128181	48.693978
3503.171874	522712.567795	48.698983
3502.991057	522712.697312	48.703988
3503.026740	522713.955264	48.708993
3503.296039	522718.209295	48.713997
3502.828163	522700.287258	48.719002
3503.303488	522692.477808	48.724007
3503.052279	522675.431402	48.729012
3503.050831	522676.088623	48.734017
3503.681023	522662.340312	48.739021
3502.984365	522669.476733	48.744026
3503.165157	522662.522622	48.749031
3502.918316	522665.392286	48.754036
3503.180075	522668.434317	48.759041
3503.069485	522667.036230	48.764045
3503.025783	522678.012366	48.769050
3503.475822	522652.918729	48.774055
3503.189500	522639.163599	48.779060
3503.289272	522634.294842	48.784065
3503.483392	522619.149455	48.789069
3503.388064	522620.529221	48.794074
3503.371169	522624.373556	48.799079
3503.309840	522599.512307	48.804084
3503.457119	522594.686580	48.809089
3503.407631	522584.735805	48.814093
3503.001238	522591.169230	48.819098
3503.503620	522584.063158	48.824103
3503.543324	522577.333511	48.829108
3503.462277	522558.339169	48.834113
3503.438061	522549.900894	48.839117
3503.236143	522535.879583	48.844122
3503.492082	522534.474107	48.849127
3503.103907	522513.304025	48.854132
3503.238843	522494.326024	48.859137
3503.012038	522486.425242	48.864141
3503.007187	522493.502953	48.869146
3503.275919	522488.506348	48.874151
3502.941420	522500.994534	48.879156
3502.487872	522498.639621	48.884161
3502.599805	522486.085186	48.889165
3502.841479	522498.077907	48.894170
3503.108459	522495.103609	48.899175
3502.761083	522506.886116	48.904180
3502.938072	522491.793869	48.909185
3503.013522	522492.186190	48.914189
3503.066938	522492.480892	48.919194
3503.353837	522475.753635	48.924199
3503.159890	522491.353764	48.929204
3503.083929	522489.293029	48.934209
3503.020912	522494.155699	48.939213
3503.166407	522482.556421	48.944218
3503.288898	522477.380722	48.949223
3502.760921	522466.494481	48.954228
3503.441505	522445.256500	48.959233
3503.357403	522449.212600	48.964237
3503.049762	522447.542331	48.969242
3503.229401	522444.227972	48.974247
3503.222299	522442.712408	48.979252
3503.032908	522438.142047	48.984257
3503.027373	522439.305433	48.989261
3503.057001	522446.579919	48.994266
3503.345301	522432.784347	48.999271
3502.867450	522418.604341	49.004276
3503.067759	522398.503774	49.009281
3503.168964	522404.098783	49.014285
3502.814867	522401.424831	49.019290
3503.084283	522396.023681	49.024295
3503.102686	522391.875426	49.029300
3503.050127	522397.949698	49.034305
3502.921339	522388.112437	49.039309
3502.402986	522393.603164	49.044314
3503.015575	522394.517207	49.049319
3502.708016	522405.990188	49.054324
3502.723951	522392.945343	49.059329
3502.958269	522400.288602	49.064333
3502.510409	522407.638571	49.069338
3503.144234	522399.753380	49.074343
3502.831354	522407.284220	49.079348
3502.708453	522411.903625	49.084353
3502.785940	522399.101811	49.089357
3502.768961	522408.759579	49.094362
3503.176028	522403.286125	49.099367
3503.021499	522406.545653	49.104372
3503.032846	522402.347965	49.109377
3503.299175	522408.574038	49.114381
3502.907213	522400.092704	49.119386
3503.036708	522414.630768	49.124391
3502.665414	522408.319863	49.129396
3503.183874	522403.384865	49.134401
3502.856315	522411.676289	49.139405
3502.819355	522402.330033	49.144410
3503.199415	522403.028071	49.149415
3503.139283	522407.940863	49.154420
3503.093647	522410.475465	49.159425
3503.018371	522402.955102	49.164429
3502.844625	522413.850867	49.169434
3503.590916	522397.303679	49.174439
3503.495623	522379.676257	49.179444
3503.061709	522357.047218	49.184449
3503.621788	522369.293019	49.189453
3503.080850	522350.876629	49.194458
3503.200205	522350.453196	49.199463
3503.359109	522358.971069	49.204468
3503.072172	522327.826163	49.209473
3503.204054	522321.688456	49.214477
3502.931944	522312.935377	49.219482
3503.123009	522320.740470	49.224487
3503.153674	522303.699674	49.229492
3503.150825	522301.425154	49.234497
3503.099884	522308.206922	49.239501
3503.249298	522310.255752	49.244506
3503.542685	522300.756125	49.249511
3503.360116	522300.380408	49.254516
3503.079751	522269.386004	49.259521
3503.170116	522263.608697	49.264525
3503.079892	522264.836032	49.269530
3503.263637	522251.511794	49.274535
3503.483610	522255.318781	49.279540
3503.312686	522246.145262	49.284545
3503.456664	522227.367725	49.289549
3503.159432	522220.034010	49.294554
3503.407296	522218.225370	49.299559
3503.355572	522216.716836	49.304564
3503.110851	522215.744321	49.309569
3503.378799	522217.622774	49.314573
3502.910756	522199.952964	49.319578
3503.443898	522180.355592	49.324583
3503.096490	522174.495786	49.329588
3503.309809	522167.536323	49.334593
3503.225692	522160.775520	49.339597
3503.110246	522166.101541	49.344602
3503.463284	522163.517997	49.349607
3502.970401	522170.218015	49.354612
3502.954594	522142.720178	49.359617
3503.475191	522130.758055	49.364621
3502.970915	522136.398298	49.369626
3502.923096	522125.183180	49.374631
3502.992292	522119.257511	49.379636
3503.122489	522125.151346	49.384641
3503.194687	522126.049709	49.389645
3503.036589	522125.872328	49.394650
3503.547645	522115.731569	49.399655
3503.110809	522124.697584	49.404660
3503.209399	522099.506981	49.409665
3503.157760	522087.129745	49.414669
3502.972240	522077.958437	49.419674
3503.023788	522072.237749	49.424679
3503.040789	522076.531826	49.429684
3503.245933	522078.167461	49.434689
3502.781542	522075.814197	49.439693
3503.227091	522074.580923	49.444698
3503.566201	522060.878110	49.449703
3503.440846	522073.636883	49.454708
3503.176943	522058.765570	49.459713
3503.072411	522036.185128	49.464717
3502.749942	522027.288196	49.469722
3503.216456	522036.617011	49.474727
3502.835620	522034.654953	49.479732
3502.692153	522028.105684	49.484737
3502.933677	522029.583917	49.489741
3502.853178	522035.662741	49.494746
3503.297060	522021.791679	49.499751
3503.022362	522030.226599	49.504756
3502.881980	522029.743103	49.509761
3503.090961	522024.300830	49.514765
3502.971931	522023.055676	49.519770
3503.092569	522025.109090	49.524775
3502.916756	522036.612062	49.529780
3503.315182	522021.484380	49.534785
3503.179502	522032.829355	49.539789
3502.935835	522011.939090	49.544794
3503.016060	521983.616971	49.549799
3502.900814	521996.222550	49.554804
3502.736814	521979.717702	49.559809
3503.286967	521977.305184	49.564813
3503.092506	521975.364216	49.569818
3503.410947	521973.392738	49.574823
3503.094296	521985.372976	49.579828
3503.161741	521975.150583	49.584833
3503.556898	521973.824161	49.589837
3502.889884	521975.850409	49.594842
3503.557938	521976.755713	49.599847
3503.121055	521967.472412	49.604852
3502.957789	521943.536209	49.609857
3503.351510	521943.119956	49.614861
3503.202103	521945.569927	49.619866
3503.571656	521930.598381	49.624871
3503.158206	521940.774060	49.629876
3503.336529	521928.714226	49.634881
3503.222189	521905.831838	49.639885
3502.850611	521900.582383	49.644890
3503.421118	521878.703876	49.649895
3503.374697	521891.905290	49.654900
3503.107189	521892.604592	49.659905
3503.589103	521889.343453	49.664909
3503.592342	521888.584491	49.669914
3503.660741	521861.123422	49.674919
3503.338736	521869.212032	49.679924
3503.562431	521859.167083	49.684929
3503.344818	521843.024437	49.689933
3502.823048	521825.261604	49.694938
3503.070029	521811.522588	49.699943
3503.098857	521808.636358	49.704948
3502.940508	521818.316821	49.709953
3502.498255	521812.118003	49.714957
3502.626083	521807.699540	49.719962
3502.966275	521803.095854	49.724967
3502.757302	521802.926509	49.729972
3502.714636	521800.961529	49.734977
3503.240766	521817.257347	49.739981
3502.822665	521816.160551	49.744986
3503.080322	521807.727893	49.749991
3503.019540	521806.675729	49.754996
3503.382719	521800.096846	49.760001
3503.187106	521808.114959	49.765005
3502.896129	521807.099176	49.770010
3503.394155	521805.958694	49.775015
3502.999239	521813.957749	49.780020
3503.313042	521813.958546	49.785025
3503.282036	521811.385091	49.790029
3502.930627	521790.107145	49.795034
3502.901475	521768.929899	49.800039
3503.382471	521762.635700	49.805044
3503.324358	521766.385647	49.810049
3502.969177	521764.722819	49.815053
3502.932048	521768.267237	49.820058
3503.514580	521764.181323	49.825063
3503.016592	521777.353093	49.830068
3503.166575	521762.112776	49.835073
3503.220023	521764.884585	49.840077
3502.826680	521736.384114	49.845082
3503.269995	521720.844634	49.850087
3502.915431	521718.878385	49.855092
3503.293673	521711.589342	49.860097
3503.127184	521720.967830	49.865101
3503.166504	521717.978819	49.870106
3503.392317	521710.410548	49.875111
3503.189130	521721.058665	49.880116
3503.135939	521711.664023	49.885121
3503.679039	521700.355219	49.890125
3503.292782	521687.019498	49.895130
3503.290604	521662.248569	49.900135
3502.912586	521669.284511	49.905140
3503.224136	521670.802264	49.910145
3503.514153	521666.408683	49.915149
3503.476759	521662.774593	49.920154
3503.477035	521623.544958	49.925159
3503.065405	521627.805790	49.930164
3503.306095	521628.020357	49.935169
3503.287334	521622.057855	49.940173
3503.122530	521626.987426	49.945178
3503.069756	521618.856500	49.950183
3502.980403	521599.811794	49.955188
3502.776136	521584.930621	49.960193
3502.962814	521584.850403	49.965197
3502.623796	521589.655858	49.970202
3502.895761	521605.031543	49.975207
3502.832609	521618.943572	49.980212
3503.169900	521607.363910	49.985217
3503.370510	521583.015792	49.990221
3503.204556	521580.210859	49.995226
3503.334938	521571.292659	50.000231
3503.024094	521573.212110	50.005236
3503.020361	521575.436898	50.010241
3503.324106	521572.355516	50.015245
3503.001034	521582.062153	50.020250
3503.385981	521573.457596	50.025255
3503.147400	521565.709885	50.030260
3502.594672	521543.047931	50.035265
3503.111565	521531.642045	50.040269
3502.903725	521532.281377	50.045274
3502.771335	521522.848589	50.050279
3502.736140	521533.571386	50.055284
3502.754259	521527.956897	50.060289
3503.077869	521535.842528	50.065293
3502.900122	521532.584468	50.070298
3503.383720	521524.874261	50.075303
3503.060766	521523.661298	50.080308
3502.892627	521527.327582	50.085313
3503.347733	521523.615624	50.090317
3503.346737	521514.111511	50.095322
3503.403405	521516.427869	50.100327
3503.199200	521524.194709	50.105332
3503.117603	521514.248351	50.110337
3503.454729	521489.019102	50.115341
3502.918578	521490.519186	50.120346
3503.471919	521476.327038	50.125351
3503.371219	521480.791536	50.130356
3503.318078	521479.535928	50.135361
3503.076926	521484.528162	50.140365
3503.403991	521478.965936	50.145370
3503.480045	521460.754341	50.150375
3503.041094	521450.813868	50.155380
3503.103503	521434.323236	50.160385
3503.135784	521431.891380	50.165389
3503.222928	521431.624676	50.170394
3503.598217	521428.178081	50.175399
3503.596321	521413.719754	50.180404
3503.202826	521396.188946	50.185409
3503.025579	521398.491736	50.190413
3503.227305	521383.192332	50.195418
3503.352932	521383.374534	50.200423
3503.001687	521388.384197	50.205428
3503.339945	521376.602002	50.210433
3503.284487	521365.589783	50.215437
3503.205124	521357.311266	50.220442
3503.214839	521336.632857	50.225447
3503.351391	521337.318876	50.230452
3503.349159	521338.532372	50.235457
3503.237668	521338.499279	50.240461
3503.167178	521339.521346	50.245466
3503.032888	521312.748590	50.250471
3502.798060	521308.791743	50.255476
3503.283711	521292.284630	50.260481
3503.353258	521282.668124	50.265485
3503.165867	521296.549510	50.270490
3503.469896	521288.614800	50.275495
3503.254984	521289.861914	50.280500
3503.306764	521290.106342	50.285505
3503.076242	521266.988643	50.290509
3502.873261	521245.737079	50.295514
3503.548069	521245.883041	50.300519
3503.115588	521255.202727	50.305524
3503.082697	521249.798422	50.310529
3503.461656	521245.845663	50.315533
3503.074516	521237.009072	50.320538
3503.261144	521235.108893	50.325543
3502.997174	521238.032068	50.330548
3503.395898	521236.351142	50.335553
3503.101741	521201.615832	50.340557
3502.998257	521202.087020	50.345562
3503.164402	521198.370103	50.350567
3503.128907	521208.284285	50.355572
3503.035915	521207.388836	50.360577
3503.485918	521193.718323	50.365581
3503.056806	521205.514688	50.370586
3503.098731	521189.734812	50.375591
3502.975713	521193.899587	50.380596
3502.921221	521189.004224	50.385601
3503.046699	521176.143307	50.390605
3503.035245	521161.635711	50.395610
3502.689258	521149.203171	50.400615
3502.741669	521167.445045	50.405620
3503.131267	521177.696501	50.410625
3503.280533	521161.646858	50.415629
3503.068741	521156.270797	50.420634
3503.064307	521155.765788	50.425639
3503.102643	521156.164008	50.430644
3503.276076	521160.989708	50.435649
3503.269992	521156.036129	50.440653
3503.036898	521154.505606	50.445658
3503.461177	521154.539500	50.450663
3503.021127	521139.947958	50.455668
3502.879997	521121.011983	50.460673
3502.939316	521127.524043	50.465677
3502.791679	521122.238941	50.470682
3502.884863	521114.084695	50.475687
3503.062166	521115.573164	50.480692
3502.936045	521116.856812	50.485697
3502.811761	521115.359643	50.490701
3502.923089	521128.991741	50.495706
3503.498416	521109.285305	50.500711
3503.013875	521115.984435	50.505716
3503.082401	521126.236112	50.510721
3503.136368	521121.273032	50.515725
3502.843623	521124.200774	50.520730
3502.965384	521094.859441	50.525735
3502.760600	521081.393430	50.530740
3503.008485	521044.802687	50.535745
3502.633029	521004.367060	50.540749
3502.472054	520956.111885	50.545754
3503.023002	520881.101188	50.550759
3502.826150	520817.077867	50.555764
3502.654843	520725.092679	50.560769
3502.656650	520619.732683	50.565773
3502.564394	520522.324303	50.570778
3502.476013	520403.882931	50.575783
3502.222614	520269.490570	50.580788
3502.142529	520129.002741	50.585793
3501.957159	519981.249915	50.590797
3501.762298	519837.137502	50.595802
3501.787894	519672.360713	50.600807
3501.526419	519506.616437	50.605812
3501.166886	519319.498866	50.610817
3501.046007	519121.420226	50.615821
3500.694519	518934.752044	50.620826
3500.580018	518727.010334	50.625831
3500.033635	518511.547545	50.630836
3499.644520	518291.556904	50.635841
3499.784670	518073.249429	50.640845
3499.218103	517842.257786	50.645850
3499.330394	517596.036423	50.650855
3499.292982	517352.363382	50.655860
3498.299498	517084.666634	50.660865
3498.420189	516831.403681	50.665869
3497.796662	516563.538898	50.670874
3497.552280	516283.473095	50.675879
3497.428646	516008.086564	50.680884
3497.155222	515713.906514	50.685889
3496.668471	515415.709180	50.690893
3496.149719	515116.095512	50.695898
3496.349202	514804.730845	50.700903
3495.681701	514493.598557	50.705908
3495.313375	514175.180792	50.710913
3495.263894	513834.199696	50.715917
3494.611030	513516.067275	50.720922
3494.456623	513157.184303	50.725927
3493.999021	512807.901298	50.730932
3493.225529	512450.820858	50.735937
3493.143896	512092.864775	50.740941
3492.378303	511748.464452	50.745946
3492.042923	511373.840682	50.750951
3491.761637	511003.803397	50.755956
3491.423192	510619.299231	50.760961
3491.074733	510232.916202	50.765965
3490.476288	509843.123861	50.770970
3490.347544	509446.013956	50.775975
3489.696384	509051.456391	50.780980
3488.994229	508638.785590	50.785985
3488.507474	508221.922114	50.790989
3488.007226	507818.559591	50.795994
3487.825321	507397.782739	50.800999
3487.068420	506989.128754	50.806004
3486.621011	506558.152693	50.811009
3486.203916	506127.363522	50.816013
3485.338632	505695.976680	50.821018
3485.387489	505262.258736	50.826023
3484.628671	504824.963571	50.831028
3484.149965	504372.583427	50.836033
3483.734603	503930.353488	50.841037
3482.955472	503481.540267	50.846042
3482.656096	503016.444824	50.851047
3482.252101	502563.955638	50.856052
3481.679471	502101.055473	50.861057
3481.296666	501629.104047	50.866061
3480.257988	501152.283493	50.871066
3479.808321	500677.432278	50.876071
3478.900419	500204.614886	50.881076
3478.800043	499739.958752	50.886081
3478.451879	499259.131350	50.891085
3477.690295	498782.557944	50.896090
3477.468094	498289.636775	50.901095
3476.850637	497800.611996	50.906100
3475.907509	497309.853537	50.911105
3475.182295	496814.845280	50.916109
3474.512331	496318.245284	50.921114
3474.398471	495823.518350	50.926119
3473.300806	495333.895292	50.931124
3472.738369	494819.668469	50.936129
3472.291532	494312.193820	50.941133
3471.435351	493821.783200	50.946138
3471.102390	493322.415404	50.951143
3470.422641	492814.176621	50.956148
3469.805761	492302.267872	50.961153
3469.291346	491781.010879	50.966157
3468.354884	491282.189722	50.971162
3467.876463	490763.886350	50.976167
3467.086585	490257.721897	50.981172
3466.416560	489733.545378	50.986177
3466.077730	489216.595086	50.991181
3465.135160	488711.932391	50.996186
3464.713528	488189.091634	51.001191
3464.089431	487688.200592	51.006196
3463.537602	487154.866866	51.011201
3462.984015	486634.941865	51.016205
3461.722589	486121.497167	51.021210
3461.388940	485595.480935	51.026215
3460.646295	485070.274744	51.031220
3459.667415	484556.945938	51.036225
3459.383086	484026.319387	51.041229
3458.384613	483514.283018	51.046234
3457.759320	482986.873489	51.051239
3456.974893	482470.722481	51.056244
3456.437359	481946.766670	51.061249
3455.614735	481429.783350	51.066253
3454.782434	480916.740070	51.071258
3454.649925	480392.931806	51.076263
3453.741922	479873.995315	51.081268
3452.870660	479351.188108	51.086273
3452.659843	478819.749222	51.091277
3451.440890	478307.864423	51.096282
3450.597431	477789.065547	51.101287
3450.289205	477281.469901	51.106292
3449.664271	476759.315465	51.111297
3448.911260	476230.426957	51.116301
3448.200749	475722.399096	51.121306
3447.821492	475189.217330	51.126311
3446.983925	474665.977556	51.131316
3446.026424	474143.250027	51.136321
3445.621458	473621.891592	51.141325
3444.705204	473098.572992	51.146330
3444.208703	472579.533965	51.151335
3443.480407	472060.011440	51.156340
3442.949618	471529.798881	51.161345
3442.066418	471015.799901	51.166349
3440.883199	470508.730124	51.171354
3440.545676	469981.843681	51.176359
3439.722700	469471.345437	51.181364
3438.998592	468955.647610	51.186369
3438.465364	468436.763343	51.191373
3437.500914	467923.460852	51.196378
3436.791947	467411.372938	51.201383
3435.856588	466898.851943	51.206388
3435.439374	466392.371936	51.211393
3434.692619	465883.903552	51.216397
3433.803281	465372.402957	51.221402
3433.078326	464865.022194	51.226407
3432.725696	464350.369509	51.231412
3431.838087	463852.067500	51.236417
3431.062175	463342.376442	51.241421
3430.323119	462838.093853	51.246426
3429.643498	462329.631336	51.251431
3428.977273	461834.341039	51.256436
3428.131590	461327.504053	51.261441
3427.439604	460821.391677	51.266445
3426.479919	460328.852126	51.271450
3425.865836	459823.414260	51.276455
3425.417434	459334.626223	51.281460
3424.318268	458836.292630	51.286465
3423.858152	458343.172795	51.291469
3422.878400	457848.906624	51.296474
3422.246228	457357.668777	51.301479
3421.505052	456869.988225	51.306484
3421.072383	456383.922239	51.311489
3420.737813	455891.894651	51.316493
3419.254181	455399.834931	51.321498
3418.890849	454903.427179	51.326503
3418.054283	454418.295427	51.331508
3417.264553	453926.600991	51.336513
3416.808215	453432.255582	51.341517
3416.197622	452948.172650	51.346522
3415.354238	452465.841278	51.351527
3414.479442	451981.880977	51.356532
3413.495776	451483.618819	51.361537
3412.885690	451009.541160	51.366541
3412.083313	450533.302165	51.371546
3411.565737	450047.214766	51.376551
3410.805298	449566.788162	51.381556
3410.118807	449095.524845	51.386561
3409.479513	448622.823573	51.391565
3408.497299	448147.071286	51.396570
3408.143234	447661.973696	51.401575
3407.001745	447191.504975	51.406580
3406.558254	446723.250990	51.411585
3405.845848	446255.334700	51.416589
3405.494605	445786.184700	51.421594
3404.804575	445302.055803	51.426599
3403.833680	444835.116572	51.431604
3403.055422	444365.396888	51.436609
3402.343905	443889.871106	51.441613
3401.517238	443422.830633	51.446618
3400.827674	442958.246562	51.451623
3400.291109	442485.913821	51.456628
3399.426807	442022.912871	51.461633
3398.680326	441561.914892	51.466637
3397.875429	441102.338735	51.471642
3397.101502	440634.982136	51.476647
3396.505786	440177.842867	51.481652
3395.548427	439708.213106	51.486657
3395.026008	439259.319890	51.491661
3394.130690	438801.110821	51.496666
3393.522465	438337.085617	51.501671
3392.691754	437899.030049	51.506676
3391.915722	437448.823989	51.511681
3391.791935	436994.901891	51.516685
3390.685845	436546.229436	51.521690
3390.255470	436090.460792	51.526695
3389.242034	435642.798335	51.531700
3388.328423	435194.731308	51.536705
3387.644362	434752.281519	51.541709
3386.984647	434312.079696	51.546714
3386.470941	433853.237167	51.551719
3385.533267	433410.753278	51.556724
3384.912119	432976.514081	51.561729
3384.403074	432518.205354	51.566733
3383.353421	432088.919140	51.571738
3382.607275	431650.995621	51.576743
3382.088249	431209.727869	51.581748
3381.391026	430775.945959	51.586753
3380.798140	430348.158258	51.591757
3380.006275	429908.866703	51.596762
3379.429660	429462.753753	51.601767
3378.780735	429040.387577	51.606772
3377.899677	428607.538210	51.611777
3377.458577	428157.420168	51.616781
3376.624995	427723.964698	51.621786
3376.007050	427289.401429	51.626791
3375.277873	426846.696631	51.631796
3374.715952	426401.723165	51.636801
3373.778306	425972.649083	51.641805
3373.128300	425541.897239	51.646810
3372.467552	425104.714665	51.651815
3371.674827	424677.577945	51.656820
3370.800745	424246.891594	51.661825
3370.541041	423806.576810	51.666829
3369.368719	423385.473762	51.671834
3368.613474	422958.380217	51.676839
3367.986781	422535.907808	51.681844
3367.355955	422112.134130	51.686849
3367.114291	421693.728080	51.691853
3366.123879	421274.062418	51.696858
3365.516523	420845.667987	51.701863
3364.650031	420413.675470	51.706868
3363.830791	419990.864299	51.711873
3363.284444	419564.701249	51.716877
3362.316045	419142.662884	51.721882
3361.753574	418716.972129	51.726887
3361.199610	418306.160070	51.731892
3360.237317	417878.690803	51.736897
3359.907038	417464.630237	51.741901
3358.776633	417057.828856	51.746906
3358.122434	416633.620117	51.751911
3357.353243	416227.816778	51.756916
3356.422202	415806.688185	51.761921
3356.286352	415404.685535	51.766925
3355.494848	414996.124442	51.771930
3354.862718	414583.314826	51.776935
3353.969092	414178.721797	51.781940
3353.371534	413760.864374	51.786945
3352.750928	413351.440038	51.791949
3351.790086	412947.780628	51.796954
3351.196903	412526.474735	51.801959
3350.717322	412128.622763	51.806964
3349.939022	411724.739822	51.811969
3349.424180	411315.346618	51.816973
3348.616053	410907.467920	51.821978
3347.981821	410504.866901	51.826983
3346.955885	410093.301575	51.831988
3346.328725	409685.682481	51.836993
3345.811085	409289.399439	51.841997
3344.940468	408888.567466	51.847002
3344.495367	408480.801619	51.852007
3343.803785	408073.043843	51.857012
3343.048880	407681.122767	51.862017
3342.127879	407268.358752	51.867021
3341.543794	406866.184122	51.872026
3340.995849	406462.880294	51.877031
3340.176077	406074.659312	51.882036
3339.504401	405678.429894	51.887041
3338.828011	405273.580543	51.892045
3337.861512	404877.463744	51.897050
3337.514826	404478.981920	51.902055
3336.554041	404086.844388	51.907060
3335.815488	403691.693125	51.912065
3335.298992	403301.356303	51.917069
3334.769496	402904.230446	51.922074
3334.373815	402508.730545	51.927079
3333.726479	402116.696842	51.932084
3332.686998	401714.553265	51.937089
3331.925308	401317.927221	51.942093
3331.350098	400925.130348	51.947098
3330.793718	400528.411231	51.952103
3330.091926	400135.040096	51.957108
3329.235701	399741.027693	51.962113
3328.506076	399345.694083	51.967117
3328.009805	398957.588831	51.972122
3327.237061	398553.177546	51.977127
3326.335732	398168.889154	51.982132
3326.050122	397778.880916	51.987137
3325.618047	397376.790812	51.992141
3324.378458	396996.050324	51.997146
3323.773117	396596.011836	52.002151
3323.401513	396210.803402	52.007156
3322.257390	395811.603349	52.012161
3321.842981	395427.562075	52.017165
3321.108877	395035.329973	52.022170
3320.533507	394647.313860	52.027175
3319.693980	394258.419823	52.032180
3319.133277	393870.900956	52.037185
3318.310373	393475.130921	52.042189
3317.503335	393098.218596	52.047194
3317.023030	392701.800669	52.052199
3316.427295	392323.244663	52.057204
3315.789278	391930.554816	52.062209
3315.262791	391546.106130	52.067213
3314.315061	391159.151806	52.072218
3313.907646	390768.370113	52.077223
3313.050843	390386.198338	52.082228
3311.691701	389992.609040	52.087233
3311.356171	389621.585032	52.092237
3310.569294	389240.711938	52.097242
3309.950014	388856.909521	52.102247
3309.388116	388480.137334	52.107252
3308.435045	388095.692943	52.112257
3308.129271	387714.295144	52.117261
3307.156830	387344.085520	52.122266
3306.813174	386962.075444	52.127271
3306.253995	386575.543625	52.132276
3305.200548	386198.825250	52.137281
3304.896176	385809.651196	52.142285
3304.095632	385441.378444	52.147290
3303.144285	385057.562659	52.152295
3302.508556	384686.789550	52.157300
3301.691546	384308.183341	52.162305
3301.309498	383932.047548	52.167309
3300.476943	383561.879197	52.172314
3300.014922	383177.025558	52.177319
3299.333857	382810.030135	52.182324
3298.317673	382433.725207	52.187329
3297.921188	382042.288145	52.192333
3296.814646	381679.952197	52.197338
3296.226739	381302.372941	52.202343
3295.745339	380934.310406	52.207348
3295.100099	380555.334007	52.212353
3294.320125	380180.622533	52.217357
3293.479362	379814.793339	52.222362
3293.086536	379432.357847	52.227367
3292.648988	379072.918051	52.232372
3291.646636	378702.881847	52.237377
3291.025539	378322.684316	52.242381
3290.316678	377961.344154	52.247386
3289.661861	377582.441949	52.252391
3288.883543	377218.537008	52.257396
3288.342227	376848.639327	52.262401
3287.808366	376465.561303	52.267405
3286.861452	376110.600814	52.272410
3286.284117	375731.617813	52.277415
3285.628175	375359.511507	52.282420
3284.566010	375001.405311	52.287425
3284.188722	374623.245087	52.292429
3283.440111	374254.755309	52.297434
3282.756930	373889.278895	52.302439
3282.372852	373513.856680	52.307444
3281.860665	373153.485051	52.312449
3280.992806	372780.345741	52.317453
3279.757439	372416.164586	52.322458
3279.377144	372050.166055	52.327463
3278.746833	371686.595091	52.332468
3278.308349	371333.115326	52.337473
3277.677639	370956.920371	52.342477
3276.799975	370587.349919	52.347482
3276.200055	370220.632423	52.352487
3275.534726	369862.240929	52.357492
3274.888887	369488.197708	52.362497
3274.071703	369129.162634	52.367501
3273.284753	368756.483678	52.372506
3272.892950	368384.018849	52.377511
3272.098169	368018.178308	52.382516
3271.030873	367663.037621	52.387521
3270.763288	367297.183960	52.392525
3269.916712	366934.827985	52.397530
3269.189612	366574.281933	52.402535
3268.891661	366214.733620	52.407540
3267.876621	365846.034856	52.412545
3267.254980	365480.807305	52.417549
3266.495894	365135.978018	52.422554
3265.648303	364768.287014	52.427559
3265.433670	364407.973134	52.432564
3264.041376	364050.514182	52.437569
3264.033105	363684.538961	52.442573
3262.884912	363324.771230	52.447578
3262.530087	362965.078735	52.452583
3261.831804	362608.872686	52.457588
3261.032536	362258.175803	52.462593
3260.850265	361893.613262	52.467597
3259.811608	361543.813950	52.472602
3259.435436	361176.146780	52.477607
3258.867241	360813.875989	52.482612
3258.114822	360452.751134	52.487617
3257.607253	360090.668760	52.492621
3256.622787	359731.305393	52.497626
3255.839707	359358.675671	52.502631
3254.787421	359003.134415	52.507636
3254.054173	358643.901269	52.512641
3253.730921	358292.539853	52.517645
3252.632772	357944.123019	52.522650
3252.265461	357592.712617	52.527655
3251.894602	357245.422644	52.532660
3250.853698	356890.983789	52.537665
3250.391318	356527.315323	52.542669
3249.446437	356176.164292	52.547674
3249.338816	355813.274245	52.552679
3248.491468	355470.678658	52.557684
3247.491519	355104.667303	52.562689
3246.893374	354754.494822	52.567693
3246.184209	354411.819282	52.572698
3245.382527	354058.060528	52.577703
3245.180983	353696.315310	52.582708
3243.975149	353337.882052	52.587713
3243.629573	352988.904508	52.592717
3242.601544	352647.870907	52.597722
3241.990640	352304.478647	52.602727
3241.404277	351954.794216	52.607732
3240.632468	351611.931853	52.612737
3240.355352	351250.639664	52.617741
3239.616626	350917.540304	52.622746
3239.150755	350552.964718	52.627751
3238.131658	350206.034902	52.632756
3237.305899	349856.094548	52.637761
3236.935347	349499.004628	52.642765
3235.736075	349161.666047	52.647770
3235.567998	348808.509889	52.652775
3234.685857	348467.146490	52.657780
3234.066561	348120.801833	52.662785
3233.346296	347775.565388	52.667789
3232.687960	347426.626507	52.672794
3232.252980	347077.701013	52.677799
3231.763936	346730.029042	52.682804
3230.905296	346381.471656	52.687809
3230.305775	346024.115546	52.692813
3229.743811	345685.484244	52.697818
3229.085098	345325.816941	52.702823
3228.127410	344979.277391	52.707828
3227.483749	344633.373311	52.712833
3227.042779	344272.774141	52.717837
3225.965175	343935.919478	52.722842
3225.379981	343582.745741	52.727847
3224.742010	343238.334238	52.732852
3224.080849	342896.927928	52.737857
3223.593908	342535.434495	52.742861
3222.613714	342195.983667	52.747866
3222.044811	341844.629700	52.752871
3221.242096	341504.739629	52.757876
3220.302186	341150.920347	52.762881
3220.107456	340816.173856	52.767885
3219.022898	340488.082690	52.772890
3218.756424	340144.842026	52.777895
3218.194136	339799.889860	52.782900
3217.422573	339452.550651	52.787905
3217.040082	339104.257033	52.792909
3215.716954	338756.466657	52.797914
3215.091500	338407.062127	52.802919
3214.296233	338071.734060	52.807924
3213.621143	337733.279615	52.812929
3213.247820	337388.768052	52.817933
3212.249139	337064.260211	52.822938
3211.645618	336726.400111	52.827943
3211.152481	336391.422818	52.832948
3210.243685	336052.996580	52.837953
3210.112974	335713.299972	52.842957
3208.811707	335370.961103	52.847962
3208.787389	335028.851239	52.852967
3208.195037	334697.419586	52.857972
3207.336759	334347.393781	52.862977
3206.917275	334001.675398	52.867981
3206.025996	333655.673495	52.872986
3205.125392	333307.431065	52.877991
3204.841901	332966.751993	52.882996
3203.822134	332631.482931	52.888001
3203.320957	332284.190489	52.893005
3202.540568	331954.201008	52.898010
3201.813255	331603.656905	52.903015
3200.987110	331267.408770	52.908020
3200.388859	330934.916295	52.913025
3200.071981	330583.742178	52.918029
3199.419774	330254.259199	52.923034
3198.526165	329908.748481	52.928039
3198.106752	329571.817113	52.933044
3197.291830	329227.436388	52.938049
3196.837609	328883.404347	52.943053
3195.944230	328542.622588	52.948058
3195.201231	328199.549617	52.953063
3194.721741	327862.951007	52.958068
3193.734620	327519.964498	52.963073
3193.464441	327178.721584	52.968077
3192.473095	326847.826059	52.973082
3191.704268	326504.240377	52.978087
3191.242018	326165.492992	52.983092
3190.289026	325833.848759	52.988097
3189.681993	325495.248696	52.993101
3188.546072	325161.084570	52.998106
3188.071175	324831.448264	53.003111
3187.641488	324499.461093	53.008116
3186.575357	324176.764522	53.013121
3186.287962	323838.972591	53.018125
3185.634996	323507.016707	53.023130
3185.088090	323169.339471	53.028135
3184.420150	322834.888101	53.033140
3183.654646	322508.420157	53.038145
3182.967743	322171.219351	53.043149
3181.924741	321845.683896	53.048154
3181.840533	321500.543011	53.053159
3181.048101	321182.782053	53.058164
3180.249713	320849.489306	53.063169
3179.618874	320521.872199	53.068173
3178.847823	320191.271565	53.073178
3178.360116	319860.344792	53.078183
3177.563359	319525.875549	53.083188
3177.160919	319206.237987	53.088193
3176.591650	318853.397578	53.093197
3175.585900	318534.515120	53.098202
3175.190132	318194.706860	53.103207
3174.391424	317863.236393	53.108212
3173.639600	317532.546671	53.113217
3173.204978	317188.004868	53.118221
3172.459739	316871.290765	53.123226
3171.764751	316527.577108	53.128231
3171.092488	316188.492874	53.133236
3170.222144	315864.207316	53.138241
3169.947132	315521.620415	53.143245
3168.962207	315199.005888	53.148250
3168.303430	314856.528330	53.153255
3167.651050	314522.629726	53.158260
3166.885375	314201.046761	53.163265
3166.512884	313865.090106	53.168269
3165.519149	313545.170825	53.173274
3165.058014	313209.378842	53.178279
3164.181209	312878.591506	53.183284
3163.140361	312550.731958	53.188289
3162.750552	312218.999743	53.193293
3161.644996	311903.549351	53.198298
3161.271023	311572.398310	53.203303
3160.629528	311250.430203	53.208308
3159.970749	310930.093595	53.213313
3159.405164	310609.639461	53.218317
3158.597613	310285.479439	53.223322
3157.705688	309960.058617	53.228327
3157.205466	309640.100680	53.233332
3156.389794	309321.974281	53.238337
3156.141629	308998.002222	53.243341
3155.235031	308677.214667	53.248346
3154.337346	308353.012557	53.253351
3153.612125	308046.505787	53.258356
3152.915578	307730.571697	53.263361
3152.797690	307411.387580	53.268365
3151.953911	307088.675987	53.273370
3151.309984	306768.605766	53.278375
3150.715851	306452.448480	53.283380
3150.030318	306136.865099	53.288385
3149.774298	305804.049392	53.293389
3148.571205	305485.465000	53.298394
3148.178615	305159.952332	53.303399
3147.646367	304842.635367	53.308404
3146.815218	304514.083715	53.313409
3146.124206	304181.027146	53.318413
3145.076691	303854.749096	53.323418
3144.564848	303526.068139	53.328423
3143.876519	303211.013043	53.333428
3143.076100	302891.365663	53.338433
3142.770557	302559.950429	53.343437
3142.082271	302250.521155	53.348442
3141.232518	301926.932217	53.353447
3140.800434	301594.567096	53.358452
3139.865913	301278.528100	53.363457
3139.484474	300956.339986	53.368461
3138.088416	300647.579619	53.373466
3137.980769	300317.350454	53.378471
3137.250309	300005.758606	53.383476
3136.473453	299689.538608	53.388481
3136.127073	299365.890080	53.393485
3135.353398	299054.939878	53.398490
3134.636518	298739.803592	53.403495
3134.040091	298415.963555	53.408500
3133.411583	298101.066748	53.413505
3132.536750	297779.077674	53.418509
3131.689682	297460.368810	53.423514
3130.885257	297142.543955	53.428519
3130.308854	296834.996499	53.433524
3129.514767	296526.082287	53.438529
3129.188376	296211.236168	53.443533
3128.578667	295894.982728	53.448538
3127.782336	295576.899197	53.453543
3127.284312	295263.963202	53.458548
3126.351252	294951.579411	53.463553
3125.799261	294636.053308	53.468557
3124.841820	294324.742002	53.473562
3124.375715	294005.024710	53.478567
3124.266548	293693.527282	53.483572
3123.177823	293376.530661	53.488577
3122.498755	293051.472021	53.493581
3121.588739	292756.500863	53.498586
3120.929477	292434.188637	53.503591
3120.346952	292112.093010	53.508596
3119.558201	291810.963775	53.513601
3119.247989	291500.004394	53.518605
3118.260740	291196.180758	53.523610
3117.841191	290871.459946	53.528615
3117.364393	290562.970590	53.533620
3116.239032	290254.379736	53.538625
3115.814306	289941.297212	53.543629
3114.982382	289632.608241	53.548634
3114.180899	289313.064863	53.553639
3113.192662	289008.296457	53.558644
3112.691910	288705.920945	53.563649
3112.476943	288394.866315	53.568653
3111.361089	288093.988208	53.573658
3110.902062	287788.217909	53.578663
3110.471486	287479.004637	53.583668
3109.606714	287168.535431	53.588673
3109.275923	286864.271989	53.593677
3108.838045	286554.804282	53.598682
3107.878080	286235.613744	53.603687
3107.281193	285919.676285	53.608692
3106.472704	285608.330790	53.613697
3106.394686	285286.223809	53.618701
3105.175682	284979.323228	53.623706
3104.518825	284657.332765	53.628711
3103.946403	284349.055961	53.633716
3103.367573	284040.423380	53.638721
3102.418504	283727.468641	53.643725
3101.790954	283416.500245	53.648730
3101.052960	283092.840503	53.653735
3100.340344	282788.022953	53.658740
3099.492093	282483.506819	53.663745
3099.265350	282162.668909	53.668749
3098.415948	281871.243233	53.673754
3097.541980	281565.431740	53.678759
3097.185138	281245.326970	53.683764
3096.182826	280937.599859	53.688769
3095.543324	280632.845900	53.693773
3095.121235	280331.673884	53.698778
3094.497902	280015.023391	53.703783
3093.587737	279707.459388	53.708788
3092.652897	279402.675206	53.713793
3092.095571	279091.158465	53.718797
3091.224707	278795.838141	53.723802
3090.559215	278497.785574	53.728807
3090.087245	278201.103047	53.733812
3089.565959	277894.801200	53.738817
3088.949380	277586.858904	53.743821
3087.742079	277299.053608	53.748826
3087.126314	276990.525262	53.753831
3086.826278	276700.869885	53.758836
3086.035901	276407.038832	53.763841
3085.619537	276096.008325	53.768845
3084.704882	275793.486660	53.773850
3083.984229	275496.002465	53.778855
3083.519312	275192.467231	53.783860
3082.606794	274895.548183	53.788865
3081.975718	274592.650444	53.793869
3081.307550	274303.791648	53.798874
3080.762196	273998.791921	53.803879
3080.102840	273706.035066	53.808884
3079.425715	273403.704917	53.813889
3078.940949	273108.882986	53.818893
3078.078178	272809.663929	53.823898
3077.498916	272510.756592	53.828903
3076.730858	272211.548079	53.833908
3075.840405	271910.245102	53.838913
3075.445975	271606.342308	53.843917
3074.482186	271320.510342	53.848922
3073.727724	271024.024997	53.853927
3073.253866	270721.535717	53.858932
3072.251150	270439.963318	53.863937
3071.985781	270133.748287	53.868941
3071.261057	269851.393468	53.873946
3070.704009	269558.544714	53.878951
3070.006052	269260.191730	53.883956
3069.035606	268967.535940	53.888961
3068.626067	268670.843905	53.893965
3067.832269	268381.165641	53.898970
3067.320905	268081.433765	53.903975
3066.856976	267784.725238	53.908980
3066.147231	267495.467012	53.913985
3065.679777	267193.410987	53.918989
3064.867989	266906.486803	53.923994
3064.263944	266604.987536	53.928999
3063.560804	266301.976026	53.934004
3062.979860	266005.134122	53.939009
3062.270496	265693.948669	53.944013
3061.391945	265406.908534	53.949018
3060.804234	265099.575375	53.954023
3060.213435	264813.916285	53.959028
3059.513808	264522.620685	53.964033
3059.017519	264217.744081	53.969037
3058.116594	263929.409581	53.974042
3057.297605	263632.097567	53.979047
3056.739013	263331.026237	53.984052
3055.962895	263038.623228	53.989057
3055.391809	262740.763320	53.994061
3054.375179	262450.971114	53.999066
3053.721806	262156.359152	54.004071
3053.514151	261866.006450	54.009076
3052.467949	261580.778421	54.014081
3052.010191	261284.913810	54.019085
3051.217751	260994.017739	54.024090
3050.737892	260699.557908	54.029095
3050.363358	260401.567135	54.034100
3049.463900	260109.873875	54.039105
3049.016767	259810.519929	54.044109
3048.080562	259526.702612	54.049114
3047.269915	259231.354309	54.054119
3046.830851	258936.151256	54.059124
3045.694229	258646.458068	54.064129
3045.369441	258356.814985	54.069133
3044.676137	258067.434290	54.074138
3043.778276	257773.400268	54.079143
3043.575162	257492.576154	54.084148
3042.903609	257189.134956	54.089153
3042.607462	256890.091531	54.094157
3041.535539	256598.709625	54.099162
3041.143606	256302.610862	54.104167
3040.464808	256003.883809	54.109172
3039.211716	255708.940810	54.114177
3038.924903	255414.023540	54.119181
3038.081291	255116.520730	54.124186
3037.424361	254828.106054	54.129191
3036.846914	254542.582452	54.134196
3035.922737	254249.524904	54.139201
3035.517925	253950.961074	54.144205
3034.607946	253657.800260	54.149210
3033.953723	253370.354950	54.154215
3033.492815	253073.125597	54.159220
3032.578682	252788.803788	54.164225
3032.342671	252496.225652	54.169229
3031.510772	252207.485916	54.174234
3030.531589	251911.028014	54.179239
3029.902199	251620.601795	54.184244
3029.277985	251339.954463	54.189249
3028.635387	251048.792719	54.194253
3028.093024	250754.865185	54.199258
3027.185813	250464.535756	54.204263
3026.596307	250178.511320	54.209268
3025.811150	249897.662576	54.214273
3025.154960	249599.451186	54.219277
3024.253831	249322.594539	54.224282
3023.732612	249044.481303	54.229287
3023.163719	248756.826191	54.234292
3022.325359	248475.478964	54.239297
3022.201765	248179.961705	54.244301
3021.106896	247916.125953	54.249306
3020.764405	247619.498415	54.254311
3020.103649	247327.633061	54.259316
3019.151434	247043.326901	54.264321
3018.757206	246760.308125	54.269325
3018.118152	246464.519232	54.274330
3017.461500	246174.641819	54.279335
3016.612581	245886.094175	54.284340
3015.958405	245605.690823	54.289345
3015.141588	245312.555392	54.294349
3014.666336	245037.217999	54.299354
3014.138616	244747.654120	54.304359
3013.386237	244458.813975	54.309364
3012.326354	244179.852831	54.314369
3012.005369	243894.103328	54.319373
3010.793572	243621.406436	54.324378
3010.390163	243332.233331	54.329383
3009.748121	243055.525735	54.334388
3009.097106	242771.664384	54.339393
3008.674911	242485.806605	54.344397
3007.763037	242212.250274	54.349402
3006.948406	241925.972017	54.354407
3006.613217	241639.134680	54.359412
3005.764264	241363.991382	54.364417
3005.435507	241081.254177	54.369421
3004.314415	240803.328582	54.374426
3003.705934	240519.236372	54.379431
3003.239091	240237.541564	54.384436
3002.270256	239963.566301	54.389441
3001.837266	239679.652009	54.394445
3001.133156	239402.733157	54.399450
3000.566710	239120.394675	54.404455
2999.875679	238841.285126	54.409460
2999.041683	238569.354391	54.414465
2998.360247	238281.383047	54.419469
2997.536358	237999.189918	54.424474
2997.200311	237724.406766	54.429479
2996.621502	237450.146534	54.434484
2995.443874	237172.493176	54.439489
2994.865736	236884.025247	54.444493
2994.086479	236616.012047	54.449498
2993.366874	236343.788513	54.454503
2992.958886	236069.861185	54.459508
2992.260348	235797.177347	54.464513
2991.752374	235522.554259	54.469517
2990.820425	235248.202706	54.474522
2990.000701	234967.340882	54.479527
2989.807492	234695.674837	54.484532
2988.653016	234432.742861	54.489537
2988.066351	234152.228306	54.494541
2987.282475	233888.780720	54.499546
2986.856600	233620.617367	54.504551
2986.247556	233345.099388	54.509556
2985.552054	233074.179218	54.514561
2985.080346	232799.379436	54.519565
2983.964569	232537.006466	54.524570
2983.516701	232267.602551	54.529575
2982.788843	231987.880313	54.534580
2982.226686	231728.146409	54.539585
2982.173127	231446.791230	54.544589
2980.864963	231177.883011	54.549594
2980.154860	230897.702810	54.554599
2979.635848	230626.074054	54.559604
2978.730169	230357.995644	54.564609
2978.624821	230085.946498	54.569613
2977.306775	229822.645443	54.574618
2976.959692	229537.675874	54.579623
2976.334138	229270.294678	54.584628
2975.664445	229004.398053	54.589633
2975.324202	228728.570810	54.594637
2974.770592	228451.556016	54.599642
2973.882644	228176.173639	54.604647
2973.112363	227907.393541	54.609652
2972.187804	227634.055583	54.614657
2971.731690	227353.973385	54.619661
2971.004058	227080.962441	54.624666
2970.204810	226818.377415	54.629671
2969.640480	226541.930489	54.634676
2968.906979	226282.239283	54.639681
2968.441648	226002.315695	54.644685
2967.770116	225738.033327	54.649690
2966.769623	225459.723916	54.654695
2966.387656	225189.324979	54.659700
2965.654034	224929.854371	54.664705
2965.185951	224655.384331	54.669709
2964.398373	224387.763786	54.674714
2963.846771	224109.693368	54.679719
2963.002036	223841.294378	54.684724
2962.180540	223574.789399	54.689729
2961.509634	223293.278043	54.694733
2961.167501	223022.294365	54.699738
2960.430749	222756.937124	54.704743
2959.524217	222486.642928	54.709748
2958.986969	222225.851428	54.714753
2958.620183	221945.709728	54.719757
2957.603974	221692.608337	54.724762
2956.916175	221412.850345	54.729767
2956.456793	221137.843617	54.734772
2955.479786	220886.991832	54.739777
2955.058383	220612.922972	54.744781
2954.484061	220348.617520	54.749786
2953.447591	220081.636545	54.754791
2952.954866	219811.909947	54.759796
2952.319676	219542.397813	54.764801
2951.857512	219269.129510	54.769805
2951.142776	219013.901661	54.774810
2950.333734	218742.510524	54.779815
2949.884718	218466.939073	54.784820
2948.880060	218205.267940	54.789825
2948.618794	217928.777738	54.794829
2947.766782	217662.170889	54.799834
2947.071690	217397.971455	54.804839
2946.420618	217123.035358	54.809844
2945.681463	216860.232354	54.814849
2945.007212	216593.397666	54.819853
2944.172694	216334.277667	54.824858
2943.425146	216068.500338	54.829863
2943.063820	215785.224277	54.834868
2942.283680	215520.434308	54.839873
2941.668930	215267.838812	54.844877
2940.951766	214998.802169	54.849882
2940.434014	214725.610904	54.854887
2940.044467	214463.741658	54.859892
2939.326839	214201.085266	54.864897
2938.864072	213928.206692	54.869901
2938.046648	213651.439529	54.874906
2937.279641	213389.443250	54.879911
2936.628863	213111.022681	54.884916
2935.956827	212857.274178	54.889921
2935.303529	212576.399665	54.894925
2934.325168	212310.304385	54.899930
2933.494164	212039.082842	54.904935
2933.244328	211769.246872	54.909940
2932.259979	211509.112553	54.914945
2931.455280	211237.661058	54.919949
2931.044102	210981.600174	54.924954
2930.417615	210713.584673	54.929959
2930.105396	210448.397035	54.934964
2928.979726	210186.826704	54.939969
2928.451083	209917.042602	54.944973
2927.871734	209646.147631	54.949978
2927.143210	209378.764819	54.954983
2926.997595	209116.369171	54.959988
2925.479319	208843.768069	54.964993
2924.925886	208577.633702	54.969997
2924.546182	208320.445822	54.975002
2923.688987	208048.176273	54.980007
2923.229166	207783.532324	54.985012
2922.583763	207524.773449	54.990017
2921.804290	207253.564202	54.995021
2921.171313	206991.076538	55.000026
2920.245361	206716.176538	55.005031
2919.961836	206456.601278	55.010036
2919.045283	206199.532763	55.015041
2919.064002	205930.163027	55.020045
2917.963287	205673.075018	55.025050
2917.111643	205398.767445	55.030055
2916.869393	205124.441017	55.035060
2915.841937	204861.350609	55.040065
2915.139383	204594.353755	55.045069
2914.265480	204335.581183	55.050074
2913.807463	204065.137292	55.055079
2913.317581	203799.612127	55.060084
2912.182833	203543.900550	55.065089
2911.956517	203275.625325	55.070093
2910.970915	203008.273324	55.075098
2910.302517	202749.284405	55.080103
2909.980792	202491.081700	55.085108
2909.198127	202226.119204	55.090113
2908.219496	201958.300151	55.095117
2907.740864	201700.914899	55.100122
2907.105356	201434.863824	55.105127
2906.512895	201172.726774	55.110132
2905.503408	200922.161149	55.115137
2904.796752	200647.038828	55.120141
2904.057150	200401.103183	55.125146
2903.469279	200145.867590	55.130151
2903.112893	199884.920902	55.135156
2902.008523	199633.625322	55.140161
2901.604106	199362.508279	55.145165
2900.664076	199114.866731	55.150170
2900.150145	198855.095190	55.155175
2899.650398	198604.001310	55.160180
2898.792633	198351.145573	55.165185
2898.518025	198089.494655	55.170189
2897.699503	197819.927026	55.175194
2896.757495	197574.710639	55.180199
2896.343499	197310.604212	55.185204
2895.602866	197056.272674	55.190209
2895.175294	196798.291646	55.195213
2894.127569	196546.759759	55.200218
2893.625474	196289.849181	55.205223
2893.116056	196035.867702	55.210228
2891.976987	195782.636111	55.215233
2891.380665	195523.351988	55.220237
2890.866563	195273.345036	55.225242
2890.070704	195021.691553	55.230247
2889.491810	194771.837255	55.235252
2888.716904	194517.358105	55.240257
2888.289503	194262.939712	55.245261
2887.443802	194007.659952	55.250266
2886.974100	193753.250799	55.255271
2886.784395	193494.981364	55.260276
2885.918791	193246.630479	55.265281
2885.585063	192984.772837	55.270285
2884.237280	192716.129888	55.275290
2883.574285	192457.406311	55.280295
2882.916320	192201.749700	55.285300
2882.079058	191957.001538	55.290305
2881.892226	191699.427975	55.295309
2881.225573	191449.413175	55.300314
2880.533109	191186.362156	55.305319
2880.120175	190923.281007	55.310324
2879.036726	190677.725704	55.315329
2878.655089	190416.245465	55.320333
2877.998070	190156.693269	55.325338
2876.957877	189898.411831	55.330343
2876.568982	189636.631581	55.335348
2875.676595	189388.151683	55.340353
2875.323722	189113.900015	55.345357
2874.756311	188872.547063	55.350362
2873.932132	188608.080474	55.355367
2873.437026	188358.970480	55.360372
2872.742110	188090.923927	55.365377
2871.988253	187823.600688	55.370381
2871.147064	187575.516528	55.375386
2870.572682	187312.722429	55.380391
2870.009943	187055.538530	55.385396
2869.067617	186794.853899	55.390401
2868.669708	186527.939672	55.395405
2867.849123	186284.489985	55.400410
2866.917416	186026.594132	55.405415
2866.606463	185764.275928	55.410420
2865.746617	185511.231389	55.415425
2865.231464	185259.265908	55.420429
2864.431755	185007.474088	55.425434
2863.954929	184753.991418	55.430439
2863.212323	184497.995184	55.435444
2862.323574	184236.642290	55.440449
2861.693397	183980.567561	55.445453
2861.264621	183724.665931	55.450458
2860.438309	183476.792298	55.455463
2859.804784	183214.501683	55.460468
2859.374064	182969.099752	55.465473
2858.999754	182708.590191	55.470477
2857.862284	182457.896482	55.475482
2857.195391	182197.817872	55.480487
2856.837411	181945.248120	55.485492
2855.815621	181692.072556	55.490497
2855.344024	181426.968243	55.495501
2854.675688	181179.782039	55.500506
2853.691698	180924.645913	55.505511
2853.246919	180659.758241	55.510516
2852.047897	180422.009989	55.515521
2851.607973	180160.457360	55.520525
2851.354456	179906.063795	55.525530
2850.671721	179656.865972	55.530535
2849.798356	179405.664540	55.535540
2848.912171	179158.193608	55.540545
2848.623949	178892.325229	55.545549
2848.085371	178647.104533	55.550554
2847.097950	178389.096483	55.555559
2846.701841	178137.203642	55.560564
2845.986425	177886.062445	55.565569
2845.062959	177631.686723	55.570573
2844.355724	177386.385537	55.575578
2843.631513	177130.378613	55.580583
2843.201275	176872.431494	55.585588
2842.396097	176624.797163	55.590593
2842.021369	176373.204023	55.595597
2841.249447	176124.816951	55.600602
2840.512292	175870.244346	55.605607
2839.939017	175615.482003	55.610612
2839.180083	175369.424989	55.615617
2838.298640	175109.258117	55.620621
2837.719702	174870.005642	55.625626
2837.090570	174621.388773	55.630631
2836.561144	174375.593893	55.635636
2835.926542	174128.367224	55.640641
2835.162696	173863.420161	55.645645
2834.638243	173612.617990	55.650650
2833.744344	173363.847227	55.655655
2833.171516	173114.124148	55.660660
2832.610418	172871.128697	55.665665
2831.981704	172615.020295	55.670669
2831.235878	172368.038206	55.675674
2830.315520	172117.320757	55.680679
2829.954990	171870.674979	55.685684
2829.265143	171620.547323	55.690689
2828.960767	171365.451146	55.695693
2828.199839	171115.007270	55.700698
2827.561373	170864.927113	55.705703
2827.011127	170603.655885	55.710708
2825.970783	170346.380971	55.715713
2825.334730	170097.691505	55.720717
2824.608712	169853.430753	55.725722
2824.037319	169598.477330	55.730727
2823.597765	169345.374107	55.735732
2822.304772	169092.878218	55.740737
2821.822708	168840.764224	55.745741
2821.063526	168589.013681	55.750746
2820.338925	168345.792250	55.755751
2820.019417	168090.440071	55.760756
2819.070713	167847.028384	55.765761
2818.558006	167595.525073	55.770765
2817.866924	167348.019191	55.775770
2817.015649	167101.455862	55.780775
2816.501085	166852.157673	55.785780
2815.720261	166606.883453	55.790785
2815.183681	166357.668296	55.795789
2814.389670	166111.038756	55.800794
2813.779858	165864.152769	55.805799
2812.990491	165625.574859	55.810804
2812.400171	165384.334777	55.815809
2812.010594	165133.464110	55.820813
2811.209784	164891.523031	55.825818
2810.445275	164649.221737	55.830823
2809.965270	164394.085234	55.835828
2809.107788	164157.027918	55.840833
2808.604752	163907.912770	55.845837
2807.781423	163661.825380	55.850842
2807.463145	163412.849608	55.855847
2806.422352	163169.737134	55.860852
2805.763141	162920.538962	55.865857
2805.172548	162669.106521	55.870861
2804.743704	162430.059792	55.875866
2803.732554	162189.797242	55.880871
2803.547778	161933.855463	55.885876
2802.822985	161696.144599	55.890881
2802.327717	161444.730950	55.895885
2801.625812	161192.449058	55.900890
2800.429901	160947.100144	55.905895
2799.992501	160705.981011	55.910900
2799.157805	160453.992325	55.915905
2798.527166	160204.274323	55.920909
2797.931159	159986.858574	55.925914
2797.511288	159658.920633	55.930919
2796.846526	159400.644577	55.935924
2796.076040	159156.893357	55.940929
2795.487744	158915.886505	55.945933
2794.871025	158658.930453	55.950938
2794.121582	158415.969243	55.955943
2793.444702	158159.763733	55.960948
2792.586451	157924.082416	55.965953
2792.089405	157661.635330	55.970957
2791.386583	157424.038519	55.975962
2790.637954	157171.093418	55.980967
2790.385174	156927.835043	55.985972
2789.389743	156689.081876	55.990977
2788.669715	156436.773227	55.995981
2788.076055	156185.755792	56.000986
2787.595024	155943.659181	56.005991
2786.920751	155697.387093	56.010996
2786.242467	155456.570960	56.016001
2785.701124	155195.369952	56.021005
2784.787401	154941.501213	56.026010
2784.212364	154704.996114	56.031015
2783.682516	154452.138021	56.036020
2782.830366	154206.082813	56.041025
2782.041103	153950.765318	56.046029
2781.581786	153704.066795	56.051034
2780.627377	153464.185586	56.056039
2780.154165	153216.577596	56.061044
2779.540267	152977.472161	56.066049
2778.821934	152720.195201	56.071053
2777.960392	152475.247272	56.076058
2777.314164	152239.317293	56.081063
2777.056548	151987.133681	56.086068
2776.266150	151744.277151	56.091073
2775.270345	151496.879057	56.096077
2774.859043	151253.444929	56.101082
2774.068969	151001.963241	56.106087
2773.418512	150757.413980	56.111092
2772.464512	150519.536720	56.116097
2771.964147	150276.098482	56.121101
2771.145741	150036.817816	56.126106
2770.689107	149801.205654	56.131111
2769.934201	149554.241552	56.136116
2769.252276	149316.609544	56.141121
2768.502225	149081.138020	56.146125
2767.909342	148838.551275	56.151130
2767.477342	148602.676966	56.156135
2766.817590	148359.723103	56.161140
2765.895579	148112.389718	56.166145
2765.702593	147866.544131	56.171149
2765.005319	147624.593072	56.176154
2763.936943	147379.347395	56.181159
2763.537955	147134.912618	56.186164
2762.649186	146907.561880	56.191169
2762.078549	146658.315813	56.196173
2761.092467	146413.966830	56.201178
2760.401820	146176.461029	56.206183
2760.353416	145930.645529	56.211188
2759.172378	145702.383836	56.216193
2758.742656	145452.451350	56.221197
2758.112854	145220.699970	56.226202
2757.131452	144979.360462	56.231207
2756.447498	144740.542724	56.236212
2755.976420	144508.097917	56.241217
2755.239171	144261.540380	56.246221
2754.926096	144020.064257	56.251226
2754.073776	143784.673454	56.256231
2753.761147	143548.805005	56.261236
2752.660636	143312.249859	56.266241
2751.913507	143069.401195	56.271245
2751.367924	142826.230237	56.276250
2750.514161	142591.814452	56.281255
2750.397233	142350.053373	56.286260
2749.544513	142113.442720	56.291265
2748.813980	141865.568898	56.296269
2748.049986	141626.978357	56.301274
2747.471767	141376.174493	56.306279
2746.898242	141142.741893	56.311284
2745.867459	140909.853647	56.316289
2745.695160	140669.156508	56.321293
2744.835244	140426.562589	56.326298
2744.095595	140195.692111	56.331303
2743.571491	139944.522966	56.336308
2742.645274	139713.291824	56.341313
2742.140012	139469.988664	56.346317
2741.351788	139235.550130	56.351322
2740.553165	139008.090515	56.356327
2740.227103	138765.666759	56.361332
2739.198180	138530.687387	56.366337
2738.790629	138286.222116	56.371341
2738.169932	138055.933633	56.376346
2737.430192	137823.391546	56.381351
2737.102664	137583.836267	56.386356
2736.281659	137350.802535	56.391361
2736.021582	137094.406352	56.396365
2735.108589	136861.441852	56.401370
2734.183251	136618.952601	56.406375
2733.800379	136374.156102	56.411380
2732.996523	136136.517435	56.416385
2732.384434	135890.732192	56.421389
2731.704430	135655.605966	56.426394
2730.884278	135419.462078	56.431399
2730.444131	135174.239990	56.436404
2729.657292	134932.822553	56.441409
2728.955440	134691.292018	56.446413
2728.493314	134449.890657	56.451418
2727.378714	134216.254974	56.456423
2727.258356	133976.632731	56.461428
2726.358908	133737.694836	56.466433
2725.681648	133496.589552	56.471437
2724.858066	133253.794520	56.476442
2724.450527	133010.668858	56.481447
2723.784142	132763.775341	56.486452
2722.771372	132537.822438	56.491457
2722.310516	132294.546139	56.496461
2721.478604	132061.276918	56.501466
2720.994116	131825.579173	56.506471
2720.477230	131571.203108	56.511476
2719.437066	131345.390992	56.516481
2718.993530	131109.781592	56.521485
2718.267229	130865.251190	56.526490
2717.558888	130632.418673	56.531495
2716.846930	130392.526341	56.536500
2715.952399	130161.962740	56.541505
2715.484898	129925.668384	56.546509
2714.907191	129690.079358	56.551514
2714.028534	129471.255236	56.556519
2713.517046	129222.564326	56.561524
2712.798907	128986.431883	56.566529
2712.205528	128759.553575	56.571533
2711.470619	128521.865458	56.576538
2710.906121	128287.632451	56.581543
2710.358499	128047.911943	56.586548
2709.671572	127825.387069	56.591553
2708.941304	127583.832478	56.596557
2708.231256	127346.785501	56.601562
2707.639727	127111.499847	56.606567
2707.126534	126865.446565	56.611572
2706.231277	126641.757677	56.616577
2705.553884	126392.280156	56.621581
2704.960928	126172.357241	56.626586
2704.099302	125925.973855	56.631591
2703.687459	125705.200498	56.636596
2702.883706	125478.433233	56.641601
2702.165996	125222.318086	56.646605
2701.787785	124999.538562	56.651610
2701.055383	124761.933267	56.656615
2700.378066	124524.943587	56.661620
2699.703856	124288.272963	56.666625
2698.675213	124052.841570	56.671629
2698.337565	123820.071129	56.676634
2697.444544	123594.362349	56.681639
2696.928708	123353.027040	56.686644
2696.045225	123131.079456	56.691649
2695.403361	122891.241296	56.696653
2694.968437	122656.566143	56.701658
2693.888188	122435.404691	56.706663
2693.556000	122202.545795	56.711668
2692.965026	121983.494657	56.716673
2692.006702	121741.367787	56.721677
2691.559907	121520.938922	56.726682
2690.775584	121287.461263	56.731687
2690.395863	121060.143406	56.736692
2689.391890	120835.148465	56.741697
2689.033925	120595.578016	56.746701
2688.541179	120355.713656	56.751706
2687.626574	120139.623993	56.756711
2686.924633	119892.407212	56.761716
2686.444311	119670.119903	56.766721
2685.735336	119436.710146	56.771725
2685.034134	119204.075735	56.776730
2684.246233	118964.804084	56.781735
2683.816052	118741.843777	56.786740
2683.048641	118504.160163	56.791745
2682.314338	118273.405652	56.796749
2681.621457	118047.020464	56.801754
2680.850228	117822.046229	56.806759
2680.340499	117582.889198	56.811764
2679.845470	117358.471933	56.816769
2679.420935	117118.207501	56.821773
2678.477715	116880.985559	56.826778
2677.593155	116657.143922	56.831783
2677.271661	116422.608013	56.836788
2676.440364	116196.489465	56.841793
2675.872426	115962.136447	56.846797
2675.156569	115726.095173	56.851802
2674.342814	115498.513720	56.856807
2673.814727	115258.371931	56.861812
2673.055252	115036.378064	56.866817
2672.448478	114800.683504	56.871821
2671.646234	114581.410672	56.876826
2670.860493	114347.805169	56.881831
2670.564178	114103.384934	56.886836
2669.578048	113888.647331	56.891841
2669.006447	113649.244849	56.896845
2668.478776	113426.707873	56.901850
2667.605179	113202.691716	56.906855
2667.345749	112955.090592	56.911860
2666.494846	112731.201969	56.916865
2666.159492	112497.034477	56.921869
2665.396462	112267.969831	56.926874
2664.563743	112038.505792	56.931879
2664.276248	111795.185470	56.936884
2663.268439	111570.107199	56.941889
2662.545845	111328.104275	56.946893
2661.939714	111101.570379	56.951898
2661.270888	110865.294204	56.956903
2660.517787	110636.922014	56.961908
2659.539919	110399.772683	56.966913
2658.885308	110175.850505	56.971917
2658.354285	109945.932774	56.976922
2657.560213	109716.325392	56.981927
2656.994951	109488.124426	56.986932
2656.147915	109266.030548	56.991937
2655.888027	109044.270818	56.996941
2655.210109	108811.797842	57.001946
2654.325608	108590.674219	57.006951
2653.776097	108358.705544	57.011956
2652.791579	108132.354049	57.016961
2652.220221	107908.413951	57.021965
2651.737263	107696.036070	57.026970
2651.067888	107477.629690	57.031975
2650.613578	107229.380639	57.036980
2649.702611	107014.551067	57.041985
2648.966281	106781.592722	57.046989
2648.319297	106551.864852	57.051994
2647.731126	106331.488913	57.056999
2647.253225	106103.959304	57.062004
2646.350950	105887.920106	57.067009
2645.414021	105654.788679	57.072013
2645.188403	105443.868148	57.077018
2644.322220	105209.543333	57.082023
2643.800881	104972.602876	57.087028
2643.158721	104755.682444	57.092033
2642.343680	104529.179214	57.097037
2641.854272	104305.957448	57.102042
2640.962052	104080.397015	57.107047
2640.502593	103848.806338	57.112052
2639.531933	103631.745148	57.117057
2638.776306	103411.206883	57.122061
2638.089957	103189.175122	57.127066
2637.278378	102982.569104	57.132071
2636.722533	102757.837092	57.137076
2636.100013	102537.565010	57.142081
2635.760034	102314.979038	57.147085
2635.321916	102095.614439	57.152090
2634.634179	101881.994644	57.157095
2634.106845	101651.083306	57.162100
2633.049238	101426.018454	57.167105
2632.709568	101189.816541	57.172109
2631.823401	100972.132052	57.177114
2630.905814	100751.276402	57.182119
2630.620296	100518.942301	57.187124
2629.699807	100301.244127	57.192129
2629.092381	100071.337967	57.197133
2628.720243	99851.749219	57.202138
2627.966887	99632.280041	57.207143
2627.599722	99411.432341	57.212148
2626.651724	99178.398313	57.217153
2625.888569	98949.346213	57.222157
2625.278423	98728.613300	57.227162
2624.559411	98508.559422	57.232167
2624.065991	98277.137012	57.237172
2623.401726	98058.791353	57.242177
2622.572440	97835.926095	57.247181
2621.873563	97597.933828	57.252186
2621.018705	97380.601604	57.257191
2620.321277	97148.582271	57.262196
2619.687885	96933.654775	57.267201
2619.158139	96707.150435	57.272205
2618.272515	96490.072565	57.277210
2617.568271	96277.185726	57.282215
2617.238129	96054.854914	57.287220
2616.671170	95834.599675	57.292225
2615.948115	95616.375451	57.297229
2615.517910	95391.434961	57.302234
2614.603120	95164.049334	57.307239
2614.116691	94927.129451	57.312244
2613.238096	94713.885362	57.317249
2612.403180	94495.283789	57.322253
2612.006567	94270.254004	57.327258
2611.062872	94058.497741	57.332263
2610.466671	93826.179254	57.337268
2609.735522	93607.747431	57.342273
2609.319402	93382.824745	57.347277
2608.464610	93163.668533	57.352282
2608.051804	92947.526387	57.357287
2607.460779	92720.558069	57.362292
2606.473175	92502.044510	57.367297
2606.032153	92275.380360	57.372301
2605.400118	92059.788858	57.377306
2604.248544	91846.507524	57.382311
2604.110252	91622.573145	57.387316
2603.483611	91390.050215	57.392321
2602.753430	91170.855828	57.397325
2602.096805	90952.431889	57.402330
2601.577158	90735.852612	57.407335
2601.121056	90494.460252	57.412340
2600.120335	90276.477978	57.417345
2599.595583	90049.469437	57.422349
2598.804194	89826.519084	57.427354
2597.796511	89607.206686	57.432359
2597.149940	89378.613892	57.437364
2596.555924	89165.054564	57.442369
2595.998795	88945.132122	57.447373
2595.067990	88733.494437	57.452378
2594.607550	88517.529987	57.457383
2593.915603	88290.648598	57.462388
2593.150714	88075.250328	57.467393
2592.519352	87855.629603	57.472397
2592.094584	87631.394575	57.477402
2591.078996	87421.647031	57.482407
2590.769665	87200.536408	57.487412
2589.788005	86983.281385	57.492417
2589.240436	86764.603060	57.497421
2588.472830	86555.255719	57.502426
2587.680461	86338.306850	57.507431
2587.521716	86110.317770	57.512436
2586.483091	85894.173142	57.517441
2586.200087	85672.687297	57.522445
2585.587100	85451.617371	57.527450
2584.361046	85244.948216	57.532455
2584.093691	85024.835859	57.537460
2583.476671	84809.269273	57.542465
2582.648147	84586.359723	57.547469
2581.928202	84370.059536	57.552474
2581.416089	84151.630423	57.557479
2580.657441	83928.799082	57.562484
2579.740126	83728.890942	57.567489
2579.274435	83500.940285	57.572493
2578.723569	83280.453501	57.577498
2577.904931	83067.693827	57.582503
2577.257860	82854.471743	57.587508
2576.472390	82645.374734	57.592513
2576.077378	82425.055980	57.597517
2575.217815	82212.286052	57.602522
2574.504253	81996.421070	57.607527
2574.013204	81773.088316	57.612532
2573.345195	81573.452618	57.617537
2572.970323	81350.841164	57.622541
2572.118547	81127.566104	57.627546
2571.419921	80912.292997	57.632551
2570.926171	80697.464976	57.637556
2570.192134	80480.078737	57.642561
2569.511739	80253.496521	57.647565
2569.192553	80033.026086	57.652570
2567.914336	79809.781994	57.657575
2567.767593	79601.913328	57.662580
2566.859367	79384.642178	57.667585
2566.221231	79159.871356	57.672589
2565.447129	78936.810254	57.677594
2564.573113	78726.017357	57.682599
2564.069857	78511.232435	57.687604
2563.071487	78303.999718	57.692609
2562.425864	78082.461064	57.697613
2562.082458	77874.913394	57.702618
2561.266006	77664.052513	57.707623
2560.830349	77440.871558	57.712628
2559.925614	77234.693024	57.717633
2559.584752	77010.772982	57.722637
2558.786222	76806.001358	57.727642
2557.920691	76594.969138	57.732647
2557.433784	76366.117709	57.737652
2556.802448	76169.360716	57.742657
2556.335383	75944.921063	57.747661
2555.818105	75733.899573	57.752666
2554.660572	75521.670129	57.757671
2554.331487	75298.736436	57.762676
2553.410165	75087.069698	57.767681
2552.627647	74867.507405	57.772685
2552.048462	74661.334965	57.777690
2551.447664	74438.409434	57.782695
2551.013309	74220.845485	57.787700
2550.197411	74018.677040	57.792705
2549.631139	73806.745664	57.797709
2548.794917	73582.124560	57.802714
2548.099614	73375.844257	57.807719
2547.448411	73151.629455	57.812724
2546.744269	72945.595717	57.817729
2546.253170	72730.077878	57.822733
2545.834467	72510.141475	57.827738
2544.865548	72305.537383	57.832743
2544.567395	72072.764060	57.837748
2543.834065	71860.860691	57.842753
2543.155980	71646.714532	57.847757
2542.643972	71425.936936	57.852762
2541.674164	71208.940282	57.857767
2541.453572	70989.622714	57.862772
2540.667959	70768.623373	57.867777
2539.513737	70547.235149	57.872781
2539.027043	70342.017337	57.877786
2538.331801	70114.441918	57.882791
2537.954310	69894.147789	57.887796
2536.912980	69681.575338	57.892801
2536.282721	69465.836176	57.897805
2535.716708	69251.755114	57.902810
2534.989507	69039.431173	57.907815
2534.465525	68813.680534	57.912820
2533.928426	68606.556826	57.917825
2533.025993	68390.346855	57.922829
2532.373080	68166.365949	57.927834
2531.688729	67955.567082	57.932839
2530.771122	67738.568636	57.937844
2530.214964	67528.400102	57.942849
2529.464442	67303.228463	57.947853
2529.168571	67101.542072	57.952858
2527.913442	66894.144940	57.957863
2527.402543	66670.557682	57.962868
2526.918271	66468.654366	57.967873
2526.301110	66253.214518	57.972877
2525.776608	66040.853010	57.977882
2525.015897	65837.435753	57.982887
2524.598494	65608.785667	57.987892
2523.610719	65401.719927	57.992897
2522.763954	65189.630990	57.997901
2522.286584	64977.305343	58.002906
2521.301526	64764.274061	58.007911
2521.096777	64563.017594	58.012916
2520.479684	64346.902364	58.017921
2519.460841	64134.969462	58.022925
2518.799643	63926.807088	58.027930
2517.834037	63728.830408	58.032935
2517.741459	63505.473102	58.037940
2517.004528	63304.326836	58.042945
2516.429143	63088.953718	58.047949
2515.730288	62868.970569	58.052954
2514.722813	62659.927020	58.057959
2514.423207	62457.713534	58.062964
2513.781599	62248.736810	58.067969
2512.907449	62035.037610	58.072973
2512.157776	61824.433200	58.077978
2511.291149	61618.148965	58.082983
2510.623197	61410.904715	58.087988
2510.250021	61212.439197	58.092993
2509.539690	61000.511211	58.097997
2509.208348	60783.143718	58.103002
2508.275471	60574.545012	58.108007
2507.761306	60367.968436	58.113012
2507.055836	60171.877469	58.118017
2506.485538	59950.764968	58.123021
2506.052728	59742.457082	58.128026
2505.116580	59535.098649	58.133031
2504.446506	59309.834124	58.138036
2503.840874	59115.346429	58.143041
2503.139319	58903.969268	58.148045
2502.564672	58682.590655	58.153050
2501.854157	58475.407596	58.158055
2501.119114	58262.802155	58.163060
2500.362944	58054.656072	58.168065
2500.083689	57843.606959	58.173069
2499.615524	57630.035832	58.178074
2498.584724	57420.861012	58.183079
2498.297626	57197.903479	58.188084
2497.278894	56988.627158	58.193089
2496.194823	56771.884445	58.198093
2495.849904	56562.012373	58.203098
2495.196556	56361.607501	58.208103
2494.571908	56139.020040	58.213108
2493.787481	55939.938155	58.218113
2493.257212	55727.813501	58.223117
2492.426378	55518.264499	58.228122
2491.699862	55312.258623	58.233127
2491.370695	55091.073797	58.238132
2490.381880	54894.187669	58.243137
2489.694608	54690.745992	58.248141
2489.307240	54475.711047	58.253146
2488.141206	54261.773605	58.258151
2487.783211	54053.599935	58.263156
2487.131153	53854.450018	58.268161
2486.554991	53647.407334	58.273165
2486.215575	53433.013102	58.278170
2485.158254	53229.769730	58.283175
2484.735983	53010.029805	58.288180
2484.090443	52801.033105	58.293185
2483.318476	52589.454569	58.298189
2482.756586	52373.975214	58.303194
2481.640136	52170.189796	58.308199
2480.829723	51951.758258	58.313204
2480.205666	51756.591654	58.318209
2479.752938	51548.588189	58.323213
2478.905792	51342.624068	58.328218
2477.934348	51152.154535	58.333223
2477.912510	50936.964202	58.338228
2477.143830	50745.523918	58.343233
2476.301783	50545.016578	58.348237
2475.509154	50324.124468	58.353242
2474.682111	50129.083566	58.358247
2474.165585	49931.363187	58.363252
2473.540802	49727.340733	58.368257
2472.845380	49522.642079	58.373261
2472.249310	49320.214275	58.378266
2471.365937	49131.656781	58.383271
2471.146217	48922.605836	58.388276
2470.315206	48727.992087	58.393281
2469.506808	48527.932220	58.398285
2469.188386	48331.925447	58.403290
2468.290796	48127.376048	58.408295
2467.688215	47922.956227	58.413300
2466.988932	47730.429916	58.418305
2466.335079	47522.928900	58.423309
2465.679640	47323.472029	58.428314
2464.816004	47117.616034	58.433319
2464.650657	46925.146670	58.438324
2463.748352	46719.658887	58.443329
2462.826063	46521.290918	58.448333
2462.505691	46316.379858	58.453338
2461.660709	46120.493619	58.458343
2461.301622	45919.771921	58.463348
2460.481403	45720.194755	58.468353
2459.881797	45511.965373	58.473357
2459.670301	45309.914524	58.478362
2458.586673	45109.351712	58.483367
2458.089824	44904.488200	58.488372
2457.403040	44696.253829	58.493377
2456.573150	44495.721062	58.498381
2455.880720	44285.411252	58.503386
2455.049433	44092.021992	58.508391
2454.813002	43889.580274	58.513396
2453.531921	43688.347068	58.518401
2453.211681	43488.295377	58.523405
2452.553531	43276.170528	58.528410
2451.535347	43088.002546	58.533415
2451.084312	42877.016752	58.538420
2450.351710	42685.053794	58.543425
2449.881418	42488.851473	58.548429
2449.433846	42284.526371	58.553434
2448.481529	42088.642180	58.558439
2448.105222	41884.664688	58.563444
2447.085318	41679.131357	58.568449
2446.386310	41480.763002	58.573453
2446.193795	41263.785246	58.578458
2444.967898	41078.012142	58.583463
2444.773193	40872.496720	58.588468
2444.078914	40673.874413	58.593473
2443.144005	40477.354303	58.598477
2442.562404	40273.305057	58.603482
2441.773815	40078.613010	58.608487
2441.455766	39868.420708	58.613492
2440.518349	39680.744994	58.618497
2439.795823	39483.642892	58.623501
2439.628189	39280.330319	58.628506
2438.604999	39079.898786	58.633511
2437.868366	38877.898549	58.638516
2437.258059	38686.087203	58.643521
2436.658377	38476.306017	58.648525
2436.220779	38271.989014	58.653530
2435.262986	38077.691186	58.658535
2434.821580	37872.892657	58.663540
2433.792427	37674.675977	58.668545
2432.944531	37478.543273	58.673549
2432.637674	37273.354395	58.678554
2432.139179	37079.949956	58.683559
2431.485474	36872.565127	58.688564
2430.707785	36683.393773	58.693569
2429.798712	36484.836837	58.698573
2429.292685	36280.331751	58.703578
2428.570113	36094.060440	58.708583
2428.183356	35887.887784	58.713588
2427.069110	35685.359434	58.718593
2426.369036	35486.306906	58.723597
2425.955725	35298.471613	58.728602
2425.220438	35106.461346	58.733607
2424.654023	34907.729556	58.738612
2423.724108	34712.035536	58.743617
2422.896821	34509.834634	58.748621
2422.721156	34317.501256	58.753626
2421.627518	34128.901806	58.758631
2421.205507	33927.988684	58.763636
2420.521808	33736.735071	58.768641
2419.749178	33547.530213	58.773645
2419.098746	33342.192393	58.778650
2418.160149	33154.715691	58.783655
2417.485648	32972.088990	58.788660
2417.090845	32783.811159	58.793665
2416.210707	32596.043846	58.798669
2415.777650	32404.392805	58.803674
2415.086026	32215.185491	58.808679
2414.631084	32013.512070	58.813684
2413.880271	31827.619829	58.818689
2413.183629	31642.278920	58.823693
2412.781528	31443.805689	58.828698
2412.060853	31256.083563	58.833703
2411.000741	31051.270411	58.838708
2410.228678	30858.807644	58.843713
2409.605739	30678.874875	58.848717
2409.302539	30490.804500	58.853722
2408.513728	30301.828831	58.858727
2408.121651	30108.225851	58.863732
2407.359554	29917.594380	58.868737
2406.130596	29723.330664	58.873741
2405.941234	29535.539145	58.878746
2405.015816	29345.166161	58.883751
2404.878517	29151.722076	58.888756
2404.238782	28969.750296	58.893761
2403.158081	28769.335995	58.898765
2402.743021	28566.153179	58.903770
2401.727496	28390.929161	58.908775
2401.345527	28186.434446	58.913780
2400.757733	28011.538505	58.918785
2400.023264	27818.554029	58.923789
2399.667228	27619.840029	58.928794
2398.790567	27427.020185	58.933799
2397.916798	27226.072250	58.938804
2397.386267	27039.543643	58.943809
2396.563918	26853.954463	58.948813
2396.056890	26654.356745	58.953818
2395.168335	26462.703483	58.958823
2394.684523	26269.871423	58.963828
2394.217124	26085.342168	58.968833
2393.270287	25894.404698	58.973837
2392.517754	25711.345880	58.978842
2391.947848	25511.299888	58.983847
2391.354238	25322.767996	58.988852
2390.371648	25133.471458	58.993857
2390.006089	24935.475070	58.998861
2389.023694	24749.655824	59.003866
2388.474543	24561.372208	59.008871
2387.903409	24368.853130	59.013876
2387.347505	24187.056745	59.018881
2386.587851	23994.826349	59.023885
2386.013220	23811.376306	59.028890
2385.062655	23625.569758	59.033895
2384.663103	23429.674355	59.038900
2383.471180	23244.754730	59.043905
2382.994567	23062.376498	59.048909
2382.481336	22879.792141	59.053914
2381.747351	22705.039252	59.058919
2381.189441	22515.694430	59.063924
2380.695088	22330.177281	59.068929
2380.113083	22142.931794	59.073933
2379.436529	21954.400550	59.078938
2378.358833	21767.947985	59.083943
2377.715625	21579.594360	59.088948
2377.189195	21402.656061	59.093953
2376.285323	21219.428583	59.098957
2376.079874	21036.726541	59.103962
2375.205656	20859.265920	59.108967
2374.395216	20674.034582	59.113972
2373.929386	20489.777241	59.118977
2373.232458	20307.772687	59.123981
2372.489062	20117.967903	59.128986
2371.985069	19941.488483	59.133991
2371.078298	19752.081154	59.138996
2370.436947	19572.244393	59.144001
2369.754095	19392.098081	59.149005
2369.331882	19210.613724	59.154010
2368.376486	19036.099053	59.159015
2367.660967	18849.155307	59.164020
2367.209675	18674.828805	59.169025
2366.451694	18495.922879	59.174029
2365.664802	18312.026927	59.179034
2364.990915	18133.985362	59.184039
2364.629886	17944.921043	59.189044
2363.563276	17779.428441	59.194049
2363.326001	17594.318918	59.199053
2362.501443	17408.090555	59.204058
2361.845698	17235.750961	59.209063
2361.246924	17047.172147	59.214068
2360.424787	16877.319972	59.219073
2359.695898	16706.336671	59.224077
2359.125876	16523.012731	59.229082
2358.269711	16354.064071	59.234087
2357.825247	16171.958957	59.239092
2356.927895	15982.846970	59.244097
2356.175827	15817.614635	59.249101
2355.882197	15636.592640	59.254106
2354.963740	15481.984526	59.259111
2354.419594	15296.406537	59.264116
2354.111701	15116.358232	59.269121
2353.156353	14931.958424	59.274125
2352.673145	14748.532562	59.279130
2351.776810	14581.715853	59.284135
2351.279315	14402.429910	59.289140
2350.526152	14225.152683	59.294145
2349.579301	14044.816941	59.299149
2349.265297	13867.796797	59.304154
2348.437910	13691.019725	59.309159
2347.761824	13514.599329	59.314164
2347.166334	13349.319342	59.319169
2346.300761	13167.240347	59.324173
2345.515886	12993.021672	59.329178
2344.684563	12832.886226	59.334183
2344.431318	12660.171234	59.339188
2343.551906	12490.959381	59.344193
2342.614225	12326.220072	59.349197
2342.245559	12150.734617	59.354202
2341.320430	12000.148352	59.359207
2340.696736	11815.726632	59.364212
2340.071670	11656.533755	59.369217
2339.222274	11482.556347	59.374221
2338.756595	11310.204860	59.379226
2337.763304	11155.970366	59.384231
2337.698304	10991.442448	59.389236
2336.471541	10836.914419	59.394241
2336.120736	10667.555709	59.399245
2335.467186	10495.889700	59.404250
2334.880108	10333.606880	59.409255
2334.112882	10167.174272	59.414260
2333.202151	10003.629549	59.419265
2332.671081	9848.455820	59.424269
2332.323589	9684.732109	59.429274
2331.070093	9530.137010	59.434279
2330.747747	9363.350343	59.439284
2330.205062	9198.271401	59.444289
2329.235800	9039.640263	59.449293
2328.516214	8870.515749	59.454298
2327.906223	8725.492888	59.459303
2327.321286	8564.407258	59.464308
2326.579255	8406.166092	59.469313
2325.860451	8252.769143	59.474317
2325.245383	8088.566303	59.479322
2324.439223	7939.318976	59.484327
2323.732860	7779.602613	59.489332
2323.067123	7622.137070	59.494337
2322.023754	7482.687090	59.499341
2321.669985	7323.527922	59.504346
2320.726245	7176.373418	59.509351
2320.207066	7030.795921	59.514356
2319.695116	6873.644397	59.519361
2318.554216	6729.405813	59.524365
2318.388745	6571.418358	59.529370
2317.481124	6433.372266	59.534375
2316.895468	6285.970143	59.539380
2316.366555	6135.780542	59.544385
2315.367653	5990.339738	59.549389
2314.730951	5837.114235	59.554394
2313.982701	5701.554997	59.559399
2313.360939	5553.851088	59.564404
2312.448219	5415.458676	59.569409
2311.658136	5276.387078	59.574413
2311.284755	5135.740921	59.579418
2310.489936	5015.114773	59.584423
2309.641504	4876.288078	59.589428
2308.955377	4734.833955	59.594433
2307.918118	4598.821840	59.599437
2307.305632	4468.382513	59.604442
2306.305860	4348.764473	59.609447
2305.895731	4219.424750	59.614452
2304.866347	4100.913723	59.619457
2304.125435	3977.470054	59.624461
2303.361725	3864.186801	59.629466
2302.571913	3751.062359	59.634471
2301.780477	3638.529006	59.639476
2301.299655	3538.154252	59.644481
2299.842358	3431.442356	59.649485
2299.263352	3332.260546	59.654490
2297.920201	3242.112944	59.659495
2297.014016	3152.154496	59.664500
2295.791005	3070.114071	59.669505
2295.058050	3007.236485	59.674509
2293.554283	2934.767946	59.679514
2292.288682	2901.047908	59.684519
2291.129728	2855.833327	59.689524
2290.423597	2816.759504	59.694529
2289.563433	2779.084882	59.699533
2289.320701	2747.001946	59.704538
2288.432298	2708.978656	59.709543
2287.882193	2667.384329	59.714548
2287.498077	2638.173529	59.719553
2286.530914	2609.448020	59.724557
2286.389926	2561.407191	59.729562
2285.766739	2531.761321	59.734567
2285.090014	2490.068491	59.739572
2284.616997	2455.504514	59.744577
2283.654747	2421.866812	59.749581
2283.237517	2377.191445	59.754586
2282.589691	2335.503147	59.759591
2282.024889	2303.082667	59.764596
2281.393049	2265.317950	59.769601
2280.574975	2234.612888	59.774605
2279.999797	2190.415828	59.779610
2279.260243	2165.804954	59.784615
2278.959478	2129.765683	59.789620
2278.288220	2094.849142	59.794625
2277.910534	2051.560450	59.799629
2277.533601	2014.009104	59.804634
2276.636275	1972.113781	59.809639
2276.180357	1924.817408	59.814644
2275.154525	1889.441831	59.819649
2274.461968	1856.186941	59.824653
2274.132691	1798.341117	59.829658
2273.410109	1769.320589	59.834663
2273.132923	1732.590875	59.839668
2272.237109	1685.321674	59.844673
2271.591303	1643.777768	59.849677
2271.033608	1608.163012	59.854682
2270.335780	1559.794241	59.859687
2269.636025	1516.850000	59.864692
2269.007971	1477.187744	59.869697
2267.985887	1434.340611	59.874701
2267.734868	1388.616709	59.879706
2266.962292	1358.495365	59.884711
2266.469600	1314.450321	59.889716
2265.844626	1273.894645	59.894721
2265.136676	1231.525066	59.899725
2264.598556	1188.172898	59.904730
2263.408163	1152.187244	59.909735
2262.706950	1117.132693	59.914740
2262.063095	1074.577550	59.919745
2261.479827	1044.634227	59.924750
2260.991161	1006.397408	59.929754
2260.327029	973.321399	59.934759
2259.577272	938.073892	59.939764
2259.094351	909.273355	59.944769
2258.310318	871.578179	59.949774
2257.826788	824.326812	59.954778
2256.975301	798.197500	59.959783
2256.580691	748.135999	59.964788
2255.985579	712.417390	59.969793
2254.907077	684.556324	59.974798
2254.537553	641.505507	59.979802
2253.834223	606.602351	59.984807
2253.185122	572.059723	59.989812
2252.595133	519.849628	59.994817
2251.593556	497.378338	59.999822
2251.023729	458.389357	60.004826
2250.131517	428.389854	60.009831
2249.646420	399.185356	60.014836
2249.028126	373.007995	60.019841
2247.933579	343.283636	60.024846
2247.510195	307.479644	60.029850
2246.256431	281.465542	60.034855
2245.782208	257.687157	60.039860
2245.425819	236.656325	60.044865
2244.497389	213.451572	60.049870
2244.301561	187.318719	60.054874
2243.635656	172.053987	60.059879
2242.823781	129.169478	60.064884
2241.999291	109.157749	60.069889
2241.224228	85.523568	60.074894
2240.976218	69.700612	60.079898
2239.875983	60.567135	60.084903
2239.284011	32.078183	60.089908
2238.307426	9.387635	60.094913
2236.982591	8.047376	60.099918
2236.445866	-0.369570	60.104922
2235.693161	5.299335	60.109927
2234.041651	17.657190	60.114932
2233.035117	32.272030	60.119937
2232.307053	40.010876	60.124942
2232.323010	31.799577	60.129946
2232.253991	38.577537	60.134951
2231.654515	31.507877	60.139956
2231.010448	36.374185	60.144961
2230.657599	44.414662	60.149966
2230.207461	39.852496	60.154970
2229.122489	45.843802	60.159975
2228.220109	46.459902	60.164980
2227.155865	47.945408	60.169985
2226.704581	53.885086	60.174990
2226.142889	47.728854	60.179994
2225.690729	56.876420	60.184999
2225.148856	58.824728	60.190004
2224.921296	50.186814	60.195009
2223.566081	51.932958	60.200014
2223.308086	55.036381	60.205018
2222.724600	59.421546	60.210023
2221.933721	60.534085	60.215028
2221.168284	51.856906	60.220033
2220.273249	62.043045	60.225038
2220.523252	61.717777	60.230042
2219.741232	66.301608	60.235047
2219.011599	64.016897	60.240052
2218.131237	60.117527	60.245057
2216.995684	66.008051	60.250062
2216.239186	62.574768	60.255066
2215.884601	59.549272	60.260071
2215.526143	59.894577	60.265076
2214.810694	59.274575	60.270081
2213.729306	70.633655	60.275086
2213.306172	57.109474	60.280090
2212.923369	70.600321	60.285095
2212.314103	62.235857	60.290100
2211.799700	70.134808	60.295105
2210.713502	65.066368	60.300110
2209.879987	71.506691	60.305114
2209.115717	67.405967	60.310119
2209.092619	65.244160	60.315124
2208.499381	65.741836	60.320129
2207.710506	70.809340	60.325134
2207.285066	59.556499	60.330138
2206.241095	67.425909	60.335143
2205.595987	70.914044	60.340148
2204.798286	66.255612	60.345153
2203.924270	77.868829	60.350158
2203.855173	67.911000	60.355162
2203.536710	73.944744	60.360167
2202.807408	74.405655	60.365172
2202.217590	62.261038	60.370177
2201.207858	71.427674	60.375182
2200.623191	62.111496	60.380186
2199.709941	71.340104	60.385191
2199.132555	59.125704	60.390196
2198.380029	57.939115	60.395201
2197.349087	63.037134	60.400206
2196.810063	58.328209	60.405210
2195.871709	63.760073	60.410215
2195.892631	58.019234	60.415220
2195.553990	60.906779	60.420225
2194.589186	62.061110	60.425230
2194.512084	54.866000	60.430234
2193.431441	65.322883	60.435239
2192.755561	61.779040	60.440244
2192.119749	62.520033	60.445249
2191.159276	63.394539	60.450254
2190.266751	64.431742	60.455258
2189.610248	69.669075	60.460263
2188.724317	65.728017	60.465268
2188.371923	65.733294	60.470273
2187.488245	71.512906	60.475278
2187.620918	68.288679	60.480282
2187.304069	76.302962	60.485287
2185.978635	65.949892	60.490292
2185.783445	63.973094	60.495297
2184.711018	69.577630	60.500302
2183.822083	61.484641	60.505306
2183.306630	71.750936	60.510311
2182.660764	67.167779	60.515316
2182.566434	61.091961	60.520321
2181.633204	68.271981	60.525326
2181.092238	67.219002	60.530330
2179.964408	70.591322	60.535335
2179.634819	68.566454	60.540340
2179.182987	68.685287	60.545345
2177.815195	72.636610	60.550350
2177.703205	67.082447	60.555354
2177.164866	74.565702	60.560359
2175.940504	62.419253	60.565364
2175.438927	69.196457	60.570369
2174.583733	75.673349	60.575374
2174.234266	62.547525	60.580378
2173.477835	71.845884	60.585383
2172.757257	80.561355	60.590388
2172.475064	70.479629	60.595393
2171.362492	73.327524	60.600398
2171.108366	70.082654	60.605402
2170.449270	73.755955	60.610407
2169.471851	75.530507	60.615412
2168.971830	61.865559	60.620417
2168.245377	72.643180	60.625422
2167.657197	58.230500	60.630426
2167.173928	65.427452	60.635431
2166.228918	58.116130	60.640436
2165.660128	69.942716	60.645441
2164.936606	73.804449	60.650446
2164.476181	58.896804	60.655450
2163.505557	69.804632	60.660455
2163.051651	67.518773	60.665460
2162.561314	65.454752	60.670465
2161.763359	65.287855	60.675470
2161.514020	65.436069	60.680474
2160.851625	67.301003	60.685479
2159.907269	67.808660	60.690484
2158.890214	61.024470	60.695489
2157.676132	69.144827	60.700494
2157.905654	64.703512	60.705498
2157.299553	66.263027	60.710503
2156.736680	66.677043	60.715508
2156.220157	57.466774	60.720513
2154.434160	68.790991	60.725518
2154.452167	62.460793	60.730522
2154.325135	63.482222	60.735527
2153.050656	65.715522	60.740532
2152.073028	69.857285	60.745537
2151.525289	75.484254	60.750542
2151.859991	65.967028	60.755546
2150.477382	64.020919	60.760551
2149.671821	71.106571	60.765556
2148.878908	67.780018	60.770561
2148.829461	72.446350	60.775566
2148.152648	65.010474	60.780570
2146.806799	79.259714	60.785575
2146.258402	75.918022	60.790580
2146.311710	66.074831	60.795585
2145.489399	67.340623	60.800590
2144.430563	69.041361	60.805594
2143.724160	72.111850	60.810599
2143.054844	71.467200	60.815604
2142.669533	69.667237	60.820609
2141.670109	71.957835	60.825614
2141.417984	63.885260	60.830618
2140.755882	71.068010	60.835623
2140.151428	60.870258	60.840628
2139.834092	58.532773	60.845633
2138.733540	67.283296	60.850638
2138.514219	63.861010	60.855642
2137.967424	66.261156	60.860647
2136.748846	72.712126	60.865652
2136.007102	69.420039	60.870657
2135.061369	71.634307	60.875662
2135.018051	62.022509	60.880666
2133.963960	63.522211	60.885671
2133.045718	69.075492	60.890676
2132.662886	61.059931	60.895681
2132.033644	70.983136	60.900686
2131.815227	59.959262	60.905690
2130.924397	66.474932	60.910695
2130.146953	66.725866	60.915700
2129.773027	65.215856	60.920705
2129.069974	71.438366	60.925710
2128.819712	59.952734	60.930714
2127.986177	68.378601	60.935719
2126.309136	65.671764	60.940724
2125.776578	61.559537	60.945729
2125.641823	68.696466	60.950734
2124.948829	66.579446	60.955738
2124.051434	66.865184	60.960743
2123.374911	63.537521	60.965748
2122.536153	55.565919	60.970753
2121.940278	66.214008	60.975758
2121.888818	66.447532	60.980762
2121.236894	77.703805	60.985767
2120.445153	67.841723	60.990772
2119.857901	59.816020	60.995777
2118.956060	66.885412	61.000782
2118.715787	62.152760	61.005786
2118.045528	66.859241	61.010791
2117.006300	62.887337	61.015796
2116.015160	65.384801	61.020801
2115.079484	65.048945	61.025806
2114.684643	63.435016	61.030810
2114.515805	56.027372	61.035815
2113.716284	62.380314	61.040820
2113.561704	66.471925	61.045825
2112.140339	71.337013	61.050830
2111.732952	63.763776	61.055834
2111.227989	71.006759	61.060839
2110.992868	65.357015	61.065844
2110.036247	60.581899	61.070849
2108.956785	63.948147	61.075854
2108.306016	59.802639	61.080858
2107.313897	63.872592	61.085863
2106.531228	59.741705	61.090868
2106.326846	57.490388	61.095873
2105.683307	64.889407	61.100878
2105.463851	58.625281	61.105882
2104.584448	61.809965	61.110887
2103.810619	68.037401	61.115892
2103.425135	59.787286	61.120897
2102.911107	62.697938	61.125902
2102.530233	55.585734	61.130906
2101.122205	52.273219	61.135911
2100.239567	66.642943	61.140916
2099.677281	65.254295	61.145921
2098.782804	69.474351	61.150926
2098.742092	60.928239	61.155930
2098.384795	59.950220	61.160935
2097.664362	69.629259	61.165940
2097.050258	63.087108	61.170945
2095.400927	67.644576	61.175950
2094.853105	62.478147	61.180954
2094.200491	69.340832	61.185959
2093.884265	65.475002	61.190964
2093.430919	62.670215	61.195969
2092.466438	67.481739	61.200974
2091.961792	63.104876	61.205978
2091.402238	65.119097	61.210983
2091.101178	59.512940	61.215988
2090.440656	53.405544	61.220993
2089.446615	73.061916	61.225998
2088.826034	62.024588	61.231002
2087.963945	65.979291	61.236007
2087.235176	65.886599	61.241012
2086.857070	64.632743	61.246017
2086.042889	65.954037	61.251022
2085.639904	66.183413	61.256026
2084.478916	62.844322	61.261031
2083.590966	58.566134	61.266036
2083.414332	62.401030	61.271041
2082.298192	62.945435	61.276046
2082.016150	62.272466	61.281050
2081.460795	61.728029	61.286055
2080.602618	62.318239	61.291060
2080.186390	53.289212	61.296065
2079.592022	61.290754	61.301070
2079.302685	56.067543	61.306074
2078.735261	62.585526	61.311079
2077.590270	56.947699	61.316084
2076.886013	57.258002	61.321089
2076.186668	55.124658	61.326094
2075.349935	63.232475	61.331098
2075.074305	59.109455	61.336103
2074.336355	67.405039	61.341108
2073.273800	58.044882	61.346113
2072.108426	59.003986	61.351118
2072.117080	57.467971	61.356122
2071.409212	61.415553	61.361127
2070.643942	61.809661	61.366132
2070.108181	57.242187	61.371137
2069.635694	68.567763	61.376142
2069.202575	55.835322	61.381146
2068.243103	60.792723	61.386151
2067.960689	60.100890	61.391156
2067.109095	60.827264	61.396161
2065.886967	67.313518	61.401166
2065.123613	58.604523	61.406170
2064.693101	58.175905	61.411175
2064.142940	64.845704	61.416180
2063.800638	63.753339	61.421185
2062.919807	63.862992	61.426190
2062.840901	59.513200	61.431194
2062.281105	60.814633	61.436199
2061.023306	61.472997	61.441204
2060.340770	57.089677	61.446209
2059.153947	62.609899	61.451214
2058.680806	58.748476	61.456218
2058.545337	65.185299	61.461223
2058.006498	57.233942	61.466228
2057.565349	59.218339	61.471233
2056.265000	60.107401	61.476238
2055.520330	48.138819	61.481242
2054.814531	54.692955	61.486247
2054.103881	65.482275	61.491252
2053.717091	51.920840	61.496257
2053.137114	64.499887	61.501262
2052.659786	59.519416	61.506266
2052.118723	62.462753	61.511271
2051.005370	62.270242	61.516276
2050.288690	61.622093	61.521281
2049.371648	64.907391	61.526286
2049.106213	51.654728	61.531290
2048.570182	63.848307	61.536295
2048.087168	67.506306	61.541300
2047.647717	59.472941	61.546305
2046.338027	62.789010	61.551310
2045.347009	61.462104	61.556314
2044.918337	53.964811	61.561319
2044.084403	66.218284	61.566324
2043.955848	65.320675	61.571329
2043.109832	73.415784	61.576334
2042.914119	61.287534	61.581338
2042.510483	68.927633	61.586343
2040.972079	72.399860	61.591348
2040.249337	63.533028	61.596353
2039.493027	69.951677	61.601358
2039.414576	67.428050	61.606362
2038.615603	67.956836	61.611367
2038.213817	69.692124	61.616372
2037.934239	71.032677	61.621377
2036.495965	67.683992	61.626382
2035.710644	57.540214	61.631386
2035.155264	67.913786	61.636391
2034.480967	64.339774	61.641396
2034.220871	64.887127	61.646401
2033.500179	70.443781	61.651406
2032.451836	68.094579	61.656410
2031.297371	66.755768	61.661415
2030.827233	65.970720	61.666420
2030.507987	66.891762	61.671425
2029.695780	69.444444	61.676430
2029.562535	69.430734	61.681434
2029.058230	66.119924	61.686439
2028.224538	65.036157	61.691444
2028.022111	64.984538	61.696449
2026.864028	62.938203	61.701454
2026.094176	60.644163	61.706458
2025.734037	60.497716	61.711463
2024.657964	65.921523	61.716468
2023.737661	61.285768	61.721473
2022.778782	68.920941	61.726478
2022.458653	62.467785	61.731482
2021.778367	72.427493	61.736487
2021.086300	70.281967	61.741492
2020.726469	67.815615	61.746497
2020.057749	69.624810	61.751502
2019.824984	70.618867	61.756506
2019.274456	66.865932	61.761511
2018.491539	65.704720	61.766516
2017.753918	62.077681	61.771521
2016.832024	63.665264	61.776526
2016.450372	63.069617	61.781530
2015.922397	68.231386	61.786535
2014.306260	67.580908	61.791540
2014.022912	60.973673	61.796545
2013.107854	65.345262	61.801550
2012.651255	64.733123	61.806554
2012.197025	69.895806	61.811559
2011.821686	65.995213	61.816564
2011.609887	60.830674	61.821569
2009.975609	67.768741	61.826574
2009.453548	62.131435	61.831578
2008.697390	55.457308	61.836583
2008.214289	66.935968	61.841588
2008.008268	66.131085	61.846593
2006.744963	68.982464	61.851598
2006.081927	54.788324	61.856602
2005.292369	59.428598	61.861607
2004.583764	60.619610	61.866612
2004.465999	59.652477	61.871617
2003.878662	60.586106	61.876622
2003.477923	62.751769	61.881626
2002.214346	66.699250	61.886631
2001.082743	67.906933	61.891636
2000.801144	60.561358	61.896641
2000.354054	57.457533	61.901646
1999.703833	57.590535	61.906650
1999.113385	58.275484	61.911655
1998.487246	63.116920	61.916660
1997.802568	53.688944	61.921665
1996.535827	67.498287	61.926670
1996.069792	68.157182	61.931674
1995.509495	61.871469	61.936679
1995.065519	67.179192	61.941684
1994.707625	66.243863	61.946689
1993.887758	64.482931	61.951694
1992.774089	56.712720	61.956698
1992.319257	60.385176	61.961703
1991.614429	64.683978	61.966708
1991.441788	59.516381	61.971713
1990.635703	64.357993	61.976718
1989.792497	64.920623	61.981722
1988.588250	64.020271	61.986727
1987.746572	69.151405	61.991732
1987.379896	59.709229	61.996737
1986.927566	65.232759	62.001742
1986.493726	60.213859	62.006746
1986.269735	64.218710	62.011751
1985.447450	63.073219	62.016756
1985.179339	56.555042	62.021761
1983.934351	64.402803	62.026766
1983.564296	61.343529	62.031770
1982.743025	54.317022	62.036775
1981.474297	54.488269	62.041780
1980.782373	60.530829	62.046785
1979.751649	65.761360	62.051790
1979.590206	51.760453	62.056794
1979.189984	57.611623	62.061799
1978.378905	60.764999	62.066804
1978.185628	59.432935	62.071809
1977.679568	65.917539	62.076814
1976.676436	61.197172	62.081818
1975.935683	63.888347	62.086823
1974.996505	71.476250	62.091828
1974.744507	54.923835	62.096833
1974.121931	70.124420	62.101838
1973.419140	59.617460	62.106842
1972.360412	64.305198	62.111847
1971.879102	68.883941	62.116852
1971.433579	59.799659	62.121857
1970.488377	67.200848	62.126862
1970.144592	62.449951	62.131866
1969.317936	67.443077	62.136871
1968.029775	61.673475	62.141876
1967.694347	61.116233	62.146881
1967.198475	61.578005	62.151886
1966.871849	61.413630	62.156890
1966.275324	69.013384	62.161895
1965.709033	65.122607	62.166900
1964.762484	54.031406	62.171905
1963.823779	64.133066	62.176910
1963.188512	65.566355	62.181914
1962.846437	60.747375	62.186919
1962.095398	64.780687	62.191924
1961.540847	59.971777	62.196929
1960.170341	66.773380	62.201934
1959.718314	65.726832	62.206938
1959.204444	66.672466	62.211943
1958.738106	64.229338	62.216948
1958.370730	65.944980	62.221953
1957.717938	63.397398	62.226958
1956.855771	62.411222	62.231962
1955.691780	67.062055	62.236967
1955.122953	65.829030	62.241972
1954.920669	61.971947	62.246977
1954.083402	64.457659	62.251982
1953.894039	59.117668	62.256986
1952.996290	62.169682	62.261991
1952.192192	60.581315	62.266996
1951.777084	57.284754	62.272001
1951.158802	56.146319	62.277006
1950.021837	64.211928	62.282010
1949.352698	55.921716	62.287015
1948.734509	55.281618	62.292020
1948.306532	48.416641	62.297025
1947.557716	53.563004	62.302030
1946.944221	58.922872	62.307034
1945.984271	54.600970	62.312039
1945.140436	58.384068	62.317044
1944.607731	48.646544	62.322049
1944.035771	57.839955	62.327054
1943.803707	61.074907	62.332058
1943.276779	53.820332	62.337063
1942.101067	57.059983	62.342068
1941.813685	49.920360	62.347073
1940.693717	59.790581	62.352078
1940.402688	58.805220	62.357082
1939.934598	60.357066	62.362087
1938.701249	66.753681	62.367092
1937.969199	51.562786	62.372097
1937.155126	66.462584	62.377102
1936.601681	53.886489	62.382106
1936.421708	54.938408	62.387111
1935.742435	57.108865	62.392116
1935.691396	56.802971	62.397121
1934.168493	67.828486	62.402126
1933.193617	65.043435	62.407130
1932.702720	63.135680	62.412135
1932.249255	66.270151	62.417140
1931.864676	53.607324	62.422145
1931.470749	56.357002	62.427150
1930.417791	57.757247	62.432154
1929.496811	63.170660	62.437159
1928.870883	66.900250	62.442164
1928.972015	59.960744	62.447169
1927.500580	66.712146	62.452174
1926.386235	59.498776	62.457178
1925.850163	57.464144	62.462183
1925.394328	66.716405	62.467188
1924.881742	58.417119	62.472193
1924.479715	70.972666	62.477198
1923.981792	58.550194	62.482202
1923.710509	53.893462	62.487207
1922.773608	63.535922	62.492212
1921.956841	62.063124	62.497217
1921.369789	62.449486	62.502222
1920.572151	57.578244	62.507226
1919.564783	49.277078	62.512231
1918.437706	64.565633	62.517236
1917.987838	59.822124	62.522241
1917.438461	65.520350	62.527246
1916.947780	59.001243	62.532250
1916.549011	53.557296	62.537255
1916.057442	63.980675	62.542260
1915.834081	64.075899	62.547265
1914.487670	63.092486	62.552270
1913.873978	64.596483	62.557274
1913.310618	62.190845	62.562279
1912.624218	62.851618	62.567284
1912.416701	60.777449	62.572289
1911.090912	60.404240	62.577294
1910.402487	61.653578	62.582298
1910.171506	57.092958	62.587303
1909.019289	64.432402	62.592308
1907.972055	55.538284	62.597313
1907.174123	67.440692	62.602318
1907.170044	55.868720	62.607322
1906.705923	62.796134	62.612327
1906.048960	65.052951	62.617332
1905.982263	55.433857	62.622337
1904.998148	58.829201	62.627342
1904.122668	53.546095	62.632346
1903.742261	59.624378	62.637351
1902.202995	60.403198	62.642356
1901.579629	57.311607	62.647361
1900.634450	68.486713	62.652366
1900.533627	57.568807	62.657370
1899.995364	49.645795	62.662375
1899.356133	60.628814	62.667380
1898.953386	55.049875	62.672385
1898.454244	66.436464	62.677390
1897.637406	60.915375	62.682394
1896.562972	58.437901	62.687399
1895.763137	63.340049	62.692404
1895.718247	57.480356	62.697409
1894.705183	67.428249	62.702414
1893.928568	59.614040	62.707418
1893.520175	64.484011	62.712423
1892.790872	64.814109	62.717428
1892.434038	55.174841	62.722433
1890.873987	67.051575	62.727438
1890.330960	60.165444	62.732442
1889.839704	59.648721	62.737447
1888.977236	65.970706	62.742452
1888.953416	68.721564	62.747457
1888.559231	66.427855	62.752462
1888.031712	58.506290	62.757466
1886.637879	60.553642	62.762471
1885.849580	63.025291	62.767476
1885.559463	64.567817	62.772481
1884.884433	68.155390	62.777486
1884.395676	68.868378	62.782490
1883.509554	59.322599	62.787495
1882.473316	70.840195	62.792500
1882.459673	61.916046	62.797505
1881.590920	64.731652	62.802510
1880.942058	65.487405	62.807514
1879.942470	72.009371	62.812519
1879.277473	68.541167	62.817524
1878.894688	62.107448	62.822529
1878.373479	77.104284	62.827534
1877.653663	65.671171	62.832538
1876.788995	64.212300	62.837543
1875.520953	69.745490	62.842548
1875.368807	63.667842	62.847553
1874.893783	59.833568	62.852558
1874.508861	66.631712	62.857562
1874.064220	61.660286	62.862567
1872.806515	67.155562	62.867572
1871.985539	66.255921	62.872577
1871.466147	67.312842	62.877582
1871.187134	69.531742	62.882586
1870.920887	63.008554	62.887591
1869.434096	68.360418	62.892596
1868.801981	62.529295	62.897601
1868.281075	71.509601	62.902606
1867.809424	61.976878	62.907610
1867.109239	65.771889	62.912615
1865.788014	60.986946	62.917620
1865.153258	60.428351	62.922625
1864.817015	63.339203	62.927630
1864.415825	58.042316	62.932634
1863.852873	60.924502	62.937639
1863.396117	68.123585	62.942644
1862.245532	49.865558	62.947649
1861.272142	56.167307	62.952654
1860.776028	63.784248	62.957658
1860.614022	55.836203	62.962663
1859.922860	64.092857	62.967668
1859.451303	51.342930	62.972673
1858.290478	64.233422	62.977678
1857.516864	59.030360	62.982682
1857.191950	52.283090	62.987687
1856.602878	54.883975	62.992692
1855.632955	55.990349	62.997697
1854.602471	61.585183	63.002702
1854.425755	58.481042	63.007706
1853.963942	61.542726	63.012711
1853.516967	60.826579	63.017716
1852.622562	61.629208	63.022721
1851.650779	68.711354	63.027726
1850.865503	58.790010	63.032730
1850.538859	57.181068	63.037735
1849.949592	71.338670	63.042740
1848.955490	50.548283	63.047745
1848.192001	64.367662	63.052750
1847.470943	63.152524	63.057754
1847.116588	59.904688	63.062759
1846.442562	59.749751	63.067764
1846.501218	52.250832	63.072769
1845.376100	56.704709	63.077774
1844.504742	56.327197	63.082778
1844.513721	57.393279	63.087783
1843.222763	65.038644	63.092788
1842.170843	60.234612	63.097793
1841.525814	59.816435	63.102798
1840.889755	65.758686	63.107802
1840.617464	56.012960	63.112807
1840.085959	55.646150	63.117812
1839.664578	53.620138	63.122817
1838.730271	58.907950	63.127822
1838.063762	58.020067	63.132826
1837.354313	60.487095	63.137831
1836.734383	56.980210	63.142836
1835.810206	55.051378	63.147841
1835.089493	53.407230	63.152846
1834.260062	53.802131	63.157850
1833.896267	45.583339	63.162855
1833.116109	65.454957	63.167860
1832.854752	51.007867	63.172865
1831.902124	61.059725	63.177870
1830.677669	57.872768	63.182874
1830.695361	60.072947	63.187879
1829.856866	62.396453	63.192884
1829.887331	57.086234	63.197889
1828.959626	64.309628	63.202894
1828.116035	61.279833	63.207898
1827.459204	53.907135	63.212903
1826.750623	68.227192	63.217908
1826.221304	49.667104	63.222913
1825.134175	59.131575	63.227918
1824.532601	68.406984	63.232922
1823.837177	57.203431	63.237927
1823.436519	72.468147	63.242932
1823.051067	57.214379	63.247937
1821.652940	62.358209	63.252942
1820.810503	60.138841	63.257946
1820.420415	62.515738	63.262951
1819.691700	65.634001	63.267956
1819.631971	57.988287	63.272961
1819.309786	69.053454	63.277966
1818.766569	65.985429	63.282970
1817.679714	68.887729	63.287975
1816.733113	62.478887	63.292980
1816.397589	61.976877	63.297985
1815.337902	57.399611	63.302990
1814.488735	53.590064	63.307994
1814.089249	59.638266	63.312999
1813.345051	59.464515	63.318004
1813.132532	52.098549	63.323009
1812.481597	54.594140	63.328014
1811.065917	59.690295	63.333018
1810.435885	61.067590	63.338023
1810.010327	66.747749	63.343028
1809.686392	59.306424	63.348033
1809.244836	66.170339	63.353038
1808.401825	58.074950	63.358042
1807.819801	59.648063	63.363047
1806.843828	66.057482	63.368052
1806.548438	55.886471	63.373057
1805.000726	58.576504	63.378062
1804.551437	59.727968	63.383066
1804.061430	59.633715	63.388071
1803.543617	62.409389	63.393076
1803.596992	56.655534	63.398081
1802.337397	62.207912	63.403086
1801.090870	59.817734	63.408090
1800.905045	60.643494	63.413095
1799.949404	62.491991	63.418100
1799.534951	55.132857	63.423105
1799.040453	58.751709	63.428110
1798.788820	63.320812	63.433114
1797.997849	55.614584	63.438119
1797.159729	56.413026	63.443124
1796.502029	53.065125	63.448129
1795.534388	58.183189	63.453134
1794.455065	61.156844	63.458138
1793.950797	55.925229	63.463143
1793.169621	64.577835	63.468148
1793.235330	53.840101	63.473153
1792.737360	59.637420	63.478158
1791.803455	56.052662	63.483162
1791.001687	59.780235	63.488167
1789.980468	64.501507	63.493172
1789.702603	56.496172	63.498177
1789.355349	63.892351	63.503182
1788.782409	61.164968	63.508186
1787.909111	49.292620	63.513191
1786.879385	58.836303	63.518196
1786.580067	48.448292	63.523201
1785.947402	60.209347	63.528206
1784.639843	65.140104	63.533210
1784.175877	54.978520	63.538215
1783.643189	62.952961	63.543220
1783.705414	52.502806	63.548225
1782.739370	63.433651	63.553230
1781.643284	62.041526	63.558234
1780.685543	57.919627	63.563239
1780.070515	57.950893	63.568244
1780.085032	60.589997	63.573249
1779.230258	61.231806	63.578254
1778.880795	58.306502	63.583258
1777.696367	61.208538	63.588263
1776.680271	66.411582	63.593268
1776.744211	53.981947	63.598273
1776.084963	63.091464	63.603278
1775.021247	60.708541	63.608282
1774.195645	57.075051	63.613287
1773.636413	63.577584	63.618292
1772.960619	55.408346	63.623297
1772.968182	56.744328	63.628302
1772.485804	58.960833	63.633306
1771.329305	51.402556	63.638311
1770.520795	64.894760	63.643316
1770.344372	52.157922	63.648321
1769.196858	63.410920	63.653326
1767.988348	58.685409	63.658330
1767.724859	68.214664	63.663335
1766.675605	71.428000	63.668340
1766.570519	59.644987	63.673345
1766.263063	61.030994	63.678350
1765.668486	59.451996	63.683354
1764.758013	53.654073	63.688359
1763.671098	65.367414	63.693364
1763.411359	57.389168	63.698369
1763.029753	55.249614	63.703374
1761.960945	57.614445	63.708378
1761.118704	57.500437	63.713383
1760.288045	67.879900	63.718388
1760.131801	56.362075	63.723393
1759.503810	56.231391	63.728398
1758.687374	50.681907	63.733402
1757.934675	51.365864	63.738407
1757.388980	58.634273	63.743412
1756.755287	55.325151	63.748417
1756.125689	50.797892	63.753422
1755.146875	58.305405	63.758426
1754.323112	56.420585	63.763431
1753.635290	60.385556	63.768436
1753.863864	55.791405	63.773441
1753.102875	60.351506	63.778446
1752.081401	63.998856	63.783450
1751.389023	59.932605	63.788455
1750.442491	69.037287	63.793460
1750.428580	53.068487	63.798465
1749.739500	48.378779	63.803470
1748.485741	55.149313	63.808474
1747.843501	49.275683	63.813479
1747.386946	56.723914	63.818484
1746.986085	48.938410	63.823489
1746.553514	53.692375	63.828494
1745.223482	53.971249	63.833498
1744.766674	43.750197	63.838503
1744.271120	56.730621	63.843508
1743.910258	45.041863	63.848513
1742.689005	50.603943	63.853518
1741.472448	47.199722	63.858522
1741.141507	50.611245	63.863527
1740.721160	59.917807	63.868532
1740.113827	59.140408	63.873537
1739.767465	56.020640	63.878542
1739.376052	51.394055	63.883546
1738.343366	47.262000	63.888551
1737.649488	59.274070	63.893556
1737.281548	50.237465	63.898561
1736.139860	54.307636	63.903566
1735.389069	62.868689	63.908570
1734.822058	57.714866	63.913575
1733.980136	56.736590	63.918580
1733.793025	53.413325	63.923585
1733.426084	62.187825	63.928590
1732.046393	59.408795	63.933594
1731.597960	55.873126	63.938599
1730.887142	58.095953	63.943604
1730.475899	44.934346	63.948609
1729.733205	60.581395	63.953614
1728.896701	66.386755	63.958618
1728.266941	54.195037	63.963623
1727.759170	67.084365	63.968628
1727.396120	52.546212	63.973633
1726.124829	54.411746	63.978638
1725.660794	45.268975	63.983642
1725.089169	52.147240	63.988647
1724.220546	54.339933	63.993652
1723.131872	47.381232	63.998657
1722.382701	45.494040	64.003662
1721.935916	49.472777	64.008666
1721.683765	46.931024	64.013671
1721.074261	60.153491	64.018676
1721.233441	42.282100	64.023681
1720.196742	57.509033	64.028686
1718.707762	50.479858	64.033690
1718.451353	46.301800	64.038695
1717.693476	55.773938	64.043700
1717.314228	51.493955	64.048705
1716.368750	53.113769	64.053710
1715.167081	51.158087	64.058714
1715.038624	46.819349	64.063719
1714.319877	54.329726	64.068724
1714.261394	52.340725	64.073729
1713.144974	50.792577	64.078734
1712.039135	56.268529	64.083738
1711.720340	44.492669	64.088743
1711.021964	53.548477	64.093748
1710.623279	51.965191	64.098753
1709.941961	51.999117	64.103758
1709.060292	49.185162	64.108762
1708.644536	54.168289	64.113767
1707.928033	55.212387	64.118772
1707.544035	55.054004	64.123777
1706.368977	50.881491	64.128782
1705.477378	48.824525	64.133786
1705.088292	43.929480	64.138791
1704.487651	46.942265	64.143796
1704.412157	47.692155	64.148801
1703.119437	51.817867	64.153806
1702.231093	49.842391	64.158810
1702.175103	44.083837	64.163815
1701.358876	55.530254	64.168820
1700.626613	45.635256	64.173825
1699.633892	47.387167	64.178830
1699.071699	53.208888	64.183834
1698.819815	52.816621	64.188839
1698.056313	53.530697	64.193844
1697.313133	50.860341	64.198849
1696.550147	58.278395	64.203854
1695.928189	55.656599	64.208858
1695.774686	53.797815	64.213863
1694.298396	58.443153	64.218868
1693.949913	56.839279	64.223873
1693.303738	61.037361	64.228878
1692.673677	53.901745	64.233882
1692.514087	55.043486	64.238887
1691.044969	57.590204	64.243892
1690.051675	47.233588	64.248897
1689.636983	58.160465	64.253902
1689.156117	59.755383	64.258906
1688.571961	56.574039	64.263911
1688.005838	61.566859	64.268916
1687.682680	50.258502	64.273921
1686.815877	51.906834	64.278926
1685.819422	53.856476	64.283930
1685.684005	45.159870	64.288935
1684.941152	57.037789	64.293940
1684.084179	46.929200	64.298945
1683.355306	52.581844	64.303950
1682.476318	46.578671	64.308954
1682.380054	46.436094	64.313959
1681.384610	56.863818	64.318964
1680.747479	43.086782	64.323969
1680.238069	46.256980	64.328974
1679.549951	48.719080	64.333978
1678.940965	43.989863	64.338983
1677.813189	46.368822	64.343988
1677.384563	56.044153	64.348993
1676.665048	55.040145	64.353998
1676.401326	54.586677	64.359002
1675.789781	53.133407	64.364007
1674.576386	48.916535	64.369012
1674.180719	51.631825	64.374017
1673.921156	43.637805	64.379022
1672.543225	54.009580	64.384026
1671.924898	49.158838	64.389031
1670.961914	52.853697	64.394036
1670.445763	44.498284	64.399041
1670.113694	45.508140	64.404046
1669.875763	48.956937	64.409050
1669.996918	40.676929	64.414055
1668.388072	52.312330	64.419060
1667.804228	46.918337	64.424065
1666.420168	49.232345	64.429070
1665.379043	56.820748	64.434074
1665.198907	51.160767	64.439079
1664.409395	45.484033	64.444084
1664.394995	42.729470	64.449089
1664.243009	52.942792	64.454094
1663.552010	46.813566	64.459098
1662.438536	40.779836	64.464103
1661.437777	48.264047	64.469108
1661.462180	40.882557	64.474113
1660.320404	50.362061	64.479118
1659.263054	53.340161	64.484122
1658.617255	45.375952	64.489127
1657.810035	50.399185	64.494132
1657.873165	46.596183	64.499137
1657.578072	40.186442	64.504142
1656.285842	44.212741	64.509146
1655.780604	39.326696	64.514151
1654.916142	47.681870	64.519156
1654.379401	43.843260	64.524161
1653.243099	46.360786	64.529166
1652.377763	49.215341	64.534170
1652.180501	45.871621	64.539175
1651.296942	55.180796	64.544180
1651.323911	45.775537	64.549185
1650.975648	42.130930	64.554190
1650.074572	47.486060	64.559194
1649.302217	39.598735	64.564199
1648.548853	44.652839	64.569204
1648.087223	36.610496	64.574209
1646.821731	46.945492	64.579214
1646.037091	52.717396	64.584218
1645.811193	43.596749	64.589223
1644.958216	45.223972	64.594228
1644.606423	37.612065	64.599233
1643.721715	48.110518	64.604238
1642.776615	54.254864	64.609242
1642.757709	42.767298	64.614247
1642.039503	56.230977	64.619252
1641.002866	46.706069	64.624257
1639.720625	55.122884	64.629262
1638.993511	51.604694	64.634266
1639.155022	49.367849	64.639271
1638.439205	46.168007	64.644276
1638.456712	46.116176	64.649281
1637.697439	39.668203	64.654286
1636.844917	49.395099	64.659290
1636.467424	40.292228	64.664295
1634.994851	37.745645	64.669300
1634.315353	39.927246	64.674305
1633.718247	43.636539	64.679310
1633.073090	48.570952	64.684314
1633.196287	37.150711	64.689319
1632.088531	44.601460	64.694324
1631.316985	38.748411	64.699329
1630.733753	39.506413	64.704334
1629.933086	50.401554	64.709338
1629.065349	44.037049	64.714343
1628.025929	45.719128	64.719348
1627.784111	50.803949	64.724353
1627.387264	53.634557	64.729358
1626.989711	50.068750	64.734362
1626.323903	37.166829	64.739367
1624.964434	52.626414	64.744372
1624.530196	49.880194	64.749377
1624.141533	54.639815	64.754382
1623.296694	55.336870	64.759386
1622.387178	53.207080	64.764391
1621.533594	59.701196	64.769396
1621.314143	48.963045	64.774401
1620.547387	47.767850	64.779406
1620.421622	58.776573	64.784410
1620.057388	55.793714	64.789415
1618.771462	60.120250	64.794420
1618.518655	51.382370	64.799425
1616.922909	59.606133	64.804430
1616.050205	59.020741	64.809434
1615.564253	52.516735	64.814439
1614.889756	56.596320	64.819444
1614.525492	59.281397	64.824449
1614.647538	51.449126	64.829454
1613.523840	58.377262	64.834458
1612.626522	52.173587	64.839463
1611.798204	55.326646	64.844468
1611.509491	55.578944	64.849473
1611.426721	57.467048	64.854478
1610.059564	62.383694	64.859482
1609.351560	52.546378	64.864487
1608.454549	50.275827	64.869492
1608.409141	54.058344	64.874497
1607.740207	47.271154	64.879502
1606.587145	56.452833	64.884506
1606.534001	50.176559	64.889511
1605.772025	58.040777	64.894516
1604.834222	51.018738	64.899521
1603.685763	47.662120	64.904526
1602.979256	46.184528	64.909530
1602.838821	48.947594	64.914535
1602.309070	53.486764	64.919540
1601.697368	49.021368	64.924545
1600.914343	49.610832	64.929550
1600.087956	50.563599	64.934554
1599.832726	49.903773	64.939559
1598.901577	52.152173	64.944564
1597.583260	44.236475	64.949569
1597.225035	36.594059	64.954574
1596.415429	48.868967	64.959578
1596.142340	44.786623	64.964583
1595.611835	49.884190	64.969588
1595.315747	47.667997	64.974593
1594.931049	52.764480	64.979598
1593.506408	52.919680	64.984602
1593.207052	40.729154	64.989607
1592.067277	46.757773	64.994612
1591.124626	48.463919	64.999617
1590.533329	51.735457	65.004622
1589.820329	53.349923	65.009626
1589.737075	42.922904	65.014631
1589.160785	56.446051	65.019636
1588.850473	48.422257	65.024641
1587.749480	43.657684	65.029646
1586.379483	45.756597	65.034650
1586.428133	47.045043	65.039655
1585.895514	49.799448	65.044660
1585.505531	49.250925	65.049665
1584.387617	50.251588	65.054670
1583.823248	50.722736	65.059674
1583.217891	52.941460	65.064679
1582.196676	53.059384	65.069684
1581.294873	48.975994	65.074689
1581.081219	53.818209	65.079694
1580.540277	57.390851	65.084698
1580.172812	47.013716	65.089703
1578.928403	56.804466	65.094708
1578.302096	50.354309	65.099713
1577.838441	55.684126	65.104718
1576.903223	51.249632	65.109722
1576.069907	52.957338	65.114727
1574.994944	51.213419	65.119732
1574.667615	49.111010	65.124737
1574.268833	46.387555	65.129742
1573.699430	52.057467	65.134746
1573.666243	43.560693	65.139751
1573.235745	46.585898	65.144756
1572.115346	52.120986	65.149761
1571.249401	48.555484	65.154766
1570.467252	50.561011	65.159770
1569.536764	43.389586	65.164775
1568.683174	51.615315	65.169780
1568.332516	45.684377	65.174785
1568.078784	49.686082	65.179790
1567.258463	49.825713	65.184794
1566.632306	47.581536	65.189799
1565.668922	57.315026	65.194804
1565.047026	56.713459	65.199809
1564.805816	51.082118	65.204814
1564.047146	51.786003	65.209818
1563.224569	51.645279	65.214823
1562.546730	55.564547	65.219828
1562.073949	54.269042	65.224833
1561.052458	57.525352	65.229838
1560.289094	49.816410	65.234842
1560.104942	47.336419	65.239847
1559.433596	53.260665	65.244852
1558.843372	51.371924	65.249857
1557.580495	51.476210	65.254862
1557.284642	47.780711	65.259866
1556.758221	45.042844	65.264871
1556.111266	50.739273	65.269876
1555.307706	41.141109	65.274881
1554.350979	44.014944	65.279886
1553.374263	51.056949	65.284890
1553.435937	46.281139	65.289895
1552.854558	50.935759	65.294900
1552.272462	48.594693	65.299905
1551.128351	44.893612	65.304910
1550.511566	49.085472	65.309914
1550.157367	39.879568	65.314919
1549.458252	51.245898	65.319924
1548.538845	49.267528	65.324929
1547.711438	45.385234	65.329934
1546.893101	50.161087	65.334938
1546.973906	42.523046	65.339943
1546.596516	50.427098	65.344948
1545.675890	46.591156	65.349953
1544.716237	39.067965	65.354958
1543.974956	51.532314	65.359962
1543.488647	44.079002	65.364967
1542.145214	46.388195	65.369972
1541.581182	49.090825	65.374977
1541.165574	45.251921	65.379982
1540.696804	48.562350	65.384986
1540.344976	44.511449	65.389991
1539.810247	50.723093	65.394996
1538.838957	52.804415	65.400001
1537.954625	53.771139	65.405006
1537.182586	51.310436	65.410010
1536.875443	42.391965	65.415015
1536.266809	43.658681	65.420020
1535.306119	39.669829	65.425025
1534.780099	49.510459	65.430030
1534.311710	49.786583	65.435034
1533.733334	40.058026	65.440039
1532.733294	46.575429	65.445044
1532.204756	42.828591	65.450049
1532.054143	44.323749	65.455054
1530.799500	55.328894	65.460058
1530.271452	39.033386	65.465063
1529.455878	54.703071	65.470068
1528.984261	39.371637	65.475073
1528.582378	42.784986	65.480078
1527.530311	41.106842	65.485082
1526.490020	37.147990	65.490087
1525.841250	46.426192	65.495092
1525.490339	37.308087	65.500097
1525.059351	43.783961	65.505102
1523.780662	46.533912	65.510106
1523.142785	41.191128	65.515111
1522.468535	44.314999	65.520116
1522.340057	44.630161	65.525121
1522.348661	42.496460	65.530126
1521.501578	46.890509	65.535130
1520.443476	45.727445	65.540135
1519.513978	45.018638	65.545140
1519.058056	42.654379	65.550145
1517.619011	41.532921	65.555150
1516.945443	38.689128	65.560154
1516.989995	38.063684	65.565159
1516.432734	48.073292	65.570164
1515.553673	48.726929	65.575169
1515.399302	44.747166	65.580174
1514.106654	47.633389	65.585178
1513.493753	41.830872	65.590183
1512.966942	43.038857	65.595188
1512.509072	49.255639	65.600193
1512.234925	44.534770	65.605198
1510.990092	47.780849	65.610202
1510.632569	40.032677	65.615207
1510.141153	41.734963	65.620212
1509.162324	45.596404	65.625217
1508.425385	44.298729	65.630222
1507.449808	48.848826	65.635226
1507.071573	41.400431	65.640231
1506.275171	49.989270	65.645236
1505.331974	42.192228	65.650241
1504.858250	38.882993	65.655246
1503.719411	43.323407	65.660250
1503.735953	40.354186	65.665255
1503.298055	49.315016	65.670260
1503.194664	44.606441	65.675265
1501.890890	47.104907	65.680270
1501.179405	48.342239	65.685274
1500.826786	47.503923	65.690279
1499.608147	47.905578	65.695284
1498.717617	45.574110	65.700289
1498.397517	40.870009	65.705294
1497.641106	46.151728	65.710298
1497.777112	40.029927	65.715303
1496.281059	49.745565	65.720308
1495.202974	44.945855	65.725313
1494.926137	44.973914	65.730318
1494.542870	50.175840	65.735322
1494.763813	40.970024	65.740327
1493.248149	42.516507	65.745332
1492.269966	41.843834	65.750337
1491.800067	40.891683	65.755342
1491.155174	47.641265	65.760346
1490.862827	52.527527	65.765351
1489.604104	50.986322	65.770356
1489.013650	44.292364	65.775361
1488.910468	41.769550	65.780366
1488.043603	49.077986	65.785370
1487.045208	34.314436	65.790375
1486.254888	33.857932	65.795380
1485.585053	39.263098	65.800385
1485.131191	43.891155	65.805390
1484.554444	43.195696	65.810394
1484.426879	34.717089	65.815399
1483.516889	48.335843	65.820404
1482.913692	45.443026	65.825409
1482.120250	41.667330	65.830414
1481.289056	45.357078	65.835418
1480.820696	48.965513	65.840423
1479.769519	50.830878	65.845428
1479.578745	48.593235	65.850433
1478.896324	41.406086	65.855438
1477.649677	52.198653	65.860442
1477.242039	36.570050	65.865447
1476.970166	43.430676	65.870452
1476.143936	47.105443	65.875457
1475.290441	40.491141	65.880462
1474.048673	45.804261	65.885466
1473.905330	47.567942	65.890471
1473.289765	44.823759	65.895476
1473.334693	36.768776	65.900481
1472.446816	38.751704	65.905486
1471.230649	48.213128	65.910490
1470.784305	41.519932	65.915495
1470.190880	52.503603	65.920500
1469.353165	39.444547	65.925505
1468.541192	37.748775	65.930510
1467.937556	51.161146	65.935514
1467.446984	36.268016	65.940519
1467.083704	38.653309	65.945524
1466.017373	40.008546	65.950529
1465.612572	46.246862	65.955534
1464.609899	51.263356	65.960538
1464.631626	46.027090	65.965543
1463.181757	45.982931	65.970548
1462.371054	45.526520	65.975553
1462.181089	40.234007	65.980558
1461.459925	48.356708	65.985562
1461.168072	42.637234	65.990567
1460.296904	48.017630	65.995572
1459.423329	47.104404	66.000577
1458.895030	42.791386	66.005582
1458.463108	45.391029	66.010586
1457.535978	40.467994	66.015591
1456.384757	42.486470	66.020596
1456.046999	48.520156	66.025601
1455.830003	38.814625	66.030606
1454.963959	47.048665	66.035610
1454.356025	41.571826	66.040615
1453.508244	42.663663	66.045620
1452.649850	36.841829	66.050625
1452.519483	43.843981	66.055630
1451.436573	38.780115	66.060634
1450.651540	43.049197	66.065639
1450.042918	38.020352	66.070644
1449.369738	42.536602	66.075649
1449.240662	44.479377	66.080654
1448.228764	53.080398	66.085658
1447.709724	33.558429	66.090663
1446.604816	45.096498	66.095668
1446.469271	48.141082	66.100673
1445.914882	42.403407	66.105678
1444.813634	47.796716	66.110682
1443.914023	40.476929	66.115687
1443.137717	37.802459	66.120692
1442.845938	32.650719	66.125697
1442.864828	43.519726	66.130702
1441.948117	46.587525	66.135706
1441.222802	35.669603	66.140711
1440.251949	40.599038	66.145716
1439.683703	48.435650	66.150721
1439.567374	39.158851	66.155726
1438.440339	45.778473	66.160730
1437.965620	37.481206	66.165735
1436.882901	39.756901	66.170740
1436.557980	46.301088	66.175745
1435.838767	37.990636	66.180750
1434.996539	43.890018	66.185754
1434.714969	36.970360	66.190759
1434.026220	45.917441	66.195764
1432.544212	49.669633	66.200769
1431.892545	45.958159	66.205774
1431.158645	52.475879	66.210778
1431.041169	35.624698	66.215783
1430.884850	48.412434	66.220788
1430.054975	36.262111	66.225793
1429.247256	27.222945	66.230798
1428.218926	43.533608	66.235802
1428.197009	39.775670	66.240807
1427.256514	42.353637	66.245812
1426.033956	43.438811	66.250817
1425.918366	36.167904	66.255822
1425.105318	36.481477	66.260826
1424.903120	35.505718	66.265831
1423.359849	45.831325	66.270836
1422.735829	31.992390	66.275841
1422.622083	34.984619	66.280846
1421.776328	47.590174	66.285850
1421.666724	36.227451	66.290855
1420.867668	39.617199	66.295860
1420.085524	32.928501	66.300865
1419.644366	34.783672	66.305870
1418.109713	36.490921	66.310874
1417.247222	37.826396	66.315879
1416.810287	39.512153	66.320884
1416.360316	36.713281	66.325889
1416.028667	40.470316	66.330894
1415.539129	47.283534	66.335898
1415.122089	40.585694	66.340903
1414.239701	45.993118	66.345908
1413.192660	30.533980	66.350913
1413.213355	32.445065	66.355918
1411.648123	43.299323	66.360922
1411.408250	27.965805	66.365927
1410.529218	38.887626	66.370932
1410.165576	38.935799	66.375937
1409.360107	34.118037	66.380942
1408.186810	37.863753	66.385946
1408.046009	29.040313	66.390951
1407.268478	34.735439	66.395956
1406.753542	39.059379	66.400961
1406.189096	35.124305	66.405966
1405.043674	37.070913	66.410970
1404.427549	31.279984	66.415975
1404.133783	39.826799	66.420980
1403.595684	40.733805	66.425985
1402.696944	31.874704	66.430990
1401.554858	40.616280	66.435994
1401.341786	33.173203	66.440999
1400.947186	29.204828	66.446004
1400.356455	30.331524	66.451009
1399.303341	34.796200	66.456014
1398.761586	38.162405	66.461018
1398.465785	36.138595	66.466023
1397.634107	41.925916	66.471028
1396.473330	38.656517	66.476033
1395.948667	27.328236	66.481038
1395.315809	30.174301	66.486042
1394.761185	35.042323	66.491047
1394.686513	37.899024	66.496052
1393.150950	40.152090	66.501057
1392.716239	32.367328	66.506062
1391.837912	34.940156	66.511066
1391.543562	34.467932	66.516071
1391.076185	39.522373	66.521076
1390.143202	39.170581	66.526081
1389.538760	34.421804	66.531086
1388.560037	41.249694	66.536090
1388.493703	35.205792	66.541095
1387.205206	39.774122	66.546100
1386.498645	48.094801	66.551105
1386.442670	43.755615	66.556110
1385.777467	39.749823	66.561114
1384.917683	38.526907	66.566119
1383.786836	45.367941	66.571124
1382.935907	38.202880	66.576129
1382.977599	38.738596	66.581134
1381.966855	45.688281	66.586138
1381.806350	35.070139	66.591143
1381.321697	37.768065	66.596148
1380.240277	37.490336	66.601153
1380.018330	39.816902	66.606158
1379.140723	37.070240	66.611162
1378.073038	30.920561	66.616167
1377.198608	41.395357	66.621172
1376.537814	41.960727	66.626177
1376.352587	36.501883	66.631182
1375.824411	41.796240	66.636186
1375.346422	31.941391	66.641191
1374.242001	33.654399	66.646196
1373.744721	40.610784	66.651201
1373.527849	32.777207	66.656206
1372.221409	46.720789	66.661210
1371.345468	35.930923	66.666215
1370.671994	47.051911	66.671220
1370.239365	43.674668	66.676225
1370.090587	34.570207	66.681230
1368.853310	41.934394	66.686234
1368.219897	38.972290	66.691239
1367.315901	40.284415	66.696244
1366.963771	43.560557	66.701249
1366.482874	44.371741	66.706254
1365.930623	37.116631	66.711258
1365.144090	33.814570	66.716263
1364.592394	40.637671	66.721268
1364.018651	43.592628	66.726273
1363.669184	39.740093	66.731278
1362.112587	40.827928	66.736282
1361.978547	28.045033	66.741287
1361.323956	34.230013	66.746292
1360.070187	38.742370	66.751297
1359.659419	37.082214	66.756302
1358.779066	40.551137	66.761306
1358.616541	31.172882	66.766311
1358.105188	40.276288	66.771316
1357.103650	41.001489	66.776321
1356.276358	39.890120	66.781326
1355.791350	34.560939	66.786330
1355.317244	38.186073	66.791335
1354.327764	43.034913	66.796340
1353.400758	45.178651	66.801345
1353.165364	36.881214	66.806350
1352.506549	44.558758	66.811354
1352.216528	30.818156	66.816359
1351.277565	37.433143	66.821364
1350.354002	51.162900	66.826369
1349.886124	39.167969	66.831374
1349.171683	48.529182	66.836378
1348.603076	36.963452	66.841383
1347.611546	43.126300	66.846388
1347.044294	44.425906	66.851393
1346.946281	39.199221	66.856398
1345.788143	47.474989	66.861402
1345.221639	41.441206	66.866407
1344.409243	38.986983	66.871412
1343.748881	49.069773	66.876417
1343.595909	40.152071	66.881422
1343.096794	45.703604	66.886426
1341.811009	39.337858	66.891431
1341.027692	40.684428	66.896436
1340.298341	36.054874	66.901441
1340.417844	36.698076	66.906446
1339.399340	42.821057	66.911450
1338.614097	39.654426	66.916455
1338.052377	40.702403	66.921460
1337.583483	40.868249	66.926465
1336.829595	33.689360	66.931470
1335.633861	43.150736	66.936474
1335.440237	44.286864	66.941479
1334.949159	42.051240	66.946484
1334.235578	40.284675	66.951489
1333.173539	39.142818	66.956494
1332.140027	48.209382	66.961498
1331.889756	44.494056	66.966503
1331.437525	46.775228	66.971508
1330.937860	53.845550	66.976513
1330.119642	42.947167	66.981518
1329.093910	50.195738	66.986522
1328.923823	44.874848	66.991527
1328.545403	45.893689	66.996532
1327.052232	47.122859	67.001537
1326.684132	39.966226	67.006542
1325.765521	49.541260	67.011546
1325.455506	39.473626	67.016551
1325.165079	48.174467	67.021556
1324.269138	48.259960	67.026561
1323.406129	43.798324	67.031566
1322.752387	54.556621	67.036570
1322.579527	43.511490	67.041575
1321.218418	50.321341	67.046580
1320.300768	49.799969	67.051585
1320.371128	41.651060	67.056590
1319.460341	42.540055	67.061594
1319.222905	36.804074	67.066599
1318.219825	42.768482	67.071604
1317.550657	51.472762	67.076609
1317.260774	47.572912	67.081614
1315.971912	47.470122	67.086618
1314.968707	42.480387	67.091623
1314.716779	40.703518	67.096628
1314.233637	43.322363	67.101633
1314.234232	34.052230	67.106638
1312.968232	39.101171	67.111642
1312.072042	36.576697	67.116647
1311.616334	45.463094	67.121652
1310.849961	37.540254	67.126657
1310.390891	29.790929	67.131662
1309.480762	37.853802	67.136666
1308.603047	27.244036	67.141671
1308.317172	31.583616	67.146676
1307.608087	33.147065	67.151681
1307.052427	25.821553	67.156686
1306.059645	29.357252	67.161690
1305.309343	43.084699	67.166695
1304.726985	42.070034	67.171700
1303.976585	50.989091	67.176705
1303.796674	31.413271	67.181710
1303.474114	41.669452	67.186714
1302.629618	36.055216	67.191719
1301.806155	35.839018	67.196724
1300.675171	42.658024	67.201729
1300.201339	30.623060	67.206734
1299.282111	39.531102	67.211738
1299.028058	39.153413	67.216743
1298.380067	31.432548	67.221748
1297.974745	41.045836	67.226753
1297.589801	35.929432	67.231758
1296.469754	47.961994	67.236762
1295.957770	34.761346	67.241767
1294.591653	42.718514	67.246772
1293.604258	38.845979	67.251777
1293.355125	38.480125	67.256782
1292.616430	42.175721	67.261786
1292.396209	37.126175	67.266791
1292.096080	33.306814	67.271796
1291.512912	38.568922	67.276801
1290.658787	26.540805	67.281806
1289.668111	45.688926	67.286810
1289.391965	40.933716	67.291815
1288.791276	34.261953	67.296820
1287.624114	36.443892	67.301825
1287.131899	28.113182	67.306830
1286.521786	35.114322	67.311834
1285.935893	42.056419	67.316839
1284.823998	39.392774	67.321844
1284.322418	44.025288	67.326849
1284.266700	39.359621	67.331854
1283.473763	37.763393	67.336858
1282.392577	35.168989	67.341863
1281.884907	40.969484	67.346868
1280.975204	47.425293	67.351873
1280.836629	44.121173	67.356878
1279.662736	46.666908	67.361882
1278.421803	37.799181	67.366887
1278.059313	37.861383	67.371892
1277.704753	40.188538	67.376897
1277.533942	37.302731	67.381902
1276.662586	40.336561	67.386906
1276.234636	37.141533	67.391911
1275.187681	35.541536	67.396916
1274.543671	39.963293	67.401921
1274.481886	37.045959	67.406926
1273.012620	43.904566	67.411930
1272.117182	40.007957	67.416935
1272.022696	43.798265	67.421940
1271.424020	47.228741	67.426945
1271.225924	44.098098	67.431950
1269.882538	41.570618	67.436954
1269.304601	44.633499	67.441959
1268.844676	51.426256	67.446964
1267.440322	52.527792	67.451969
1266.954620	40.646113	67.456974
1266.185203	40.191086	67.461978
1266.018424	39.288562	67.466983
1265.852447	32.825250	67.471988
1265.041085	38.815966	67.476993
1264.367308	35.637946	67.481998
1263.370067	45.764845	67.487002
1262.932609	30.961124	67.492007
1261.595755	32.316873	67.497012
1260.675935	36.916533	67.502017
1260.744186	32.541838	67.507022
1259.910747	41.606573	67.512026
1259.688060	33.543691	67.517031
1259.120930	41.403802	67.522036
1257.976980	36.726649	67.527041
1257.621503	36.795624	67.532046
1256.841489	40.679158	67.537050
1256.225880	38.822918	67.542055
1255.365632	37.021345	67.547060
1254.370305	41.241907	67.552065
1254.279223	36.168681	67.557070
1253.618122	39.935531	67.562074
1252.493176	36.330904	67.567079
1251.596987	33.150403	67.572084
1251.391518	36.887389	67.577089
1250.960456	30.453612	67.582094
1250.417916	38.355547	67.587098
1249.578696	28.958742	67.592103
1248.860953	36.640938	67.597108
1248.111397	42.248073	67.602113
1247.787637	40.235037	67.607118
1246.688586	39.056522	67.612122
1246.025929	32.820427	67.617127
1245.547433	42.415390	67.622132
1244.908760	41.438080	67.627137
1244.703846	38.762714	67.632142
1243.632158	42.716284	67.637146
1242.987860	34.136936	67.642151
1242.769178	33.083385	67.647156
1241.391272	36.098415	67.652161
1240.790987	30.991032	67.657166
1239.931814	39.498434	67.662170
1239.880346	31.525034	67.667175
1238.885044	32.769713	67.672180
1237.601955	38.048497	67.677185
1236.925082	28.589612	67.682190
1236.428421	33.476829	67.687194
1236.237560	36.217955	67.692199
1235.853570	37.985213	67.697204
1235.260002	39.494041	67.702209
1234.548320	33.759360	67.707214
1233.929869	38.840997	67.712218
1233.333946	32.758308	67.717223
1232.393370	43.018137	67.722228
1231.285023	43.072778	67.727233
1230.931531	32.168365	67.732238
1230.165579	46.625332	67.737242
1229.827202	43.236285	67.742247
1228.661170	38.242517	67.747252
1227.908509	41.270106	67.752257
1227.430849	39.138034	67.757262
1227.134305	38.787610	67.762266
1226.833597	37.299223	67.767271
1226.288291	38.981739	67.772276
1225.086392	39.965944	67.777281
1224.591253	30.195874	67.782286
1223.431535	37.424775	67.787290
1222.582841	39.526139	67.792295
1222.005354	38.479178	67.797300
1221.291927	41.074728	67.802305
1221.249644	32.850696	67.807310
1220.461961	41.832466	67.812314
1220.363322	33.349297	67.817319
1219.260312	38.495371	67.822324
1218.390790	41.159899	67.827329
1218.217894	38.441596	67.832334
1216.836418	46.610989	67.837338
1215.977060	40.726319	67.842343
1215.442523	37.947244	67.847348
1214.929030	46.729290	67.852353
1214.817791	45.549840	67.857358
1213.911772	41.495655	67.862362
1213.308423	31.900499	67.867367
1212.499385	39.172995	67.872372
1211.980308	39.055090	67.877377
1211.596175	37.415958	67.882382
1210.214938	41.598546	67.887386
1209.645444	34.724716	67.892391
1209.292185	32.238534	67.897396
1208.417850	49.117733	67.902401
1208.232086	37.987942	67.907406
1206.715461	45.044935	67.912410
1206.475066	37.880639	67.917415
1206.305416	28.402613	67.922420
1205.210076	48.160363	67.927425
1204.727788	34.540263	67.932430
1203.912017	41.541005	67.937434
1203.299889	39.107026	67.942439
1202.674544	34.984560	67.947444
1201.603037	39.772372	67.952449
1201.080136	39.924752	67.957454
1200.402348	39.570298	67.962458
1200.068578	37.377502	67.967463
1199.856437	33.962080	67.972468
1198.631062	35.489379	67.977473
1198.055067	39.157548	67.982478
1197.398331	43.538766	67.987482
1196.661791	36.666269	67.992487
1195.564635	40.051440	67.997492
1194.974181	39.585323	68.002497
1195.001559	39.382100	68.007502
1194.461793	39.064050	68.012506
1193.586709	34.255859	68.017511
1192.589506	29.572753	68.022516
1191.666392	37.987826	68.027521
1191.454027	26.242499	68.032526
1190.637329	36.004791	68.037530
1189.813328	36.362759	68.042535
1189.273417	30.709595	68.047540
1188.322126	35.312705	68.052545
1188.351174	33.819195	68.057550
1187.354204	29.459348	68.062554
1186.684202	27.957149	68.067559
1186.040751	39.590653	68.072564
1185.461930	34.588688	68.077569
1185.256856	36.012091	68.082574
1183.844227	36.033134	68.087578
1183.196928	33.661529	68.092583
1183.013987	30.096379	68.097588
1182.558903	38.665697	68.102593
1181.617683	28.698482	68.107598
1180.417621	36.168794	68.112602
1179.885656	28.457905	68.117607
1179.834807	28.270277	68.122612
1178.831193	37.792623	68.127617
1178.090745	29.545576	68.132622
1177.302151	37.792596	68.137626
1176.889746	37.564688	68.142631
1176.750731	30.742267	68.147636
1175.338551	32.695121	68.152641
1174.797162	29.986537	68.157646
1174.395092	37.066581	68.162650
1173.697176	38.245067	68.167655
1172.526861	37.350746	68.172660
1171.682338	46.008812	68.177665
1171.782042	33.620886	68.182670
1170.947302	40.490603	68.187674
1170.182703	34.776976	68.192679
1169.314117	39.589303	68.197684
1168.650869	42.873940	68.202689
1168.145520	30.889763	68.207694
1167.698081	36.012027	68.212698
1167.195121	37.164242	68.217703
1165.920572	32.981019	68.222708
1165.273786	38.644371	68.227713
1165.413884	30.809259	68.232718
1164.760146	38.323588	68.237722
1163.769661	38.044106	68.242727
1162.940828	33.555021	68.247732
1162.410241	35.027038	68.252737
1161.811746	27.102796	68.257742
1160.838856	28.733470	68.262746
1160.030934	42.837552	68.267751
1159.435881	35.297557	68.272756
1158.485074	42.576844	68.277761
1158.605931	29.143134	68.282766
1157.737234	35.472596	68.287770
1156.678960	30.657283	68.292775
1156.199796	35.516496	68.297780
1155.524310	38.828314	68.302785
1155.641834	35.404626	68.307790
1154.528728	38.010136	68.312794
1154.039186	32.550832	68.317799
1153.498755	33.478760	68.322804
1152.159927	39.411458	68.327809
1151.845121	33.473330	68.332814
1150.941388	32.159709	68.337818
1150.212112	32.644559	68.342823
1149.958295	32.938668	68.347828
1149.066004	37.258002	68.352833
1148.562762	25.912204	68.357838
1147.832031	40.406155	68.362842
1147.438268	31.914737	68.367847
1146.342201	34.235249	68.372852
1145.347469	33.765627	68.377857
1144.860176	29.909821	68.382862
1144.223591	45.077972	68.387866
1143.956425	37.700312	68.392871
1143.222385	30.571959	68.397876
1142.245984	41.439938	68.402881
1141.903719	28.138237	68.407886
1141.335427	32.275148	68.412890
1140.845104	29.309277	68.417895
1139.658051	33.725958	68.422900
1138.976234	38.686795	68.427905
1138.537914	37.576718	68.432910
1138.102459	41.433870	68.437914
1136.958935	35.755287	68.442919
1136.260410	40.621006	68.447924
1135.946996	48.136416	68.452929
1135.489543	31.992276	68.457934
1134.821635	41.341389	68.462938
1133.483558	42.684782	68.467943
1132.960034	39.825122	68.472948
1132.491324	34.550178	68.477953
1132.239416	38.203086	68.482958
1131.397276	39.896559	68.487962
1130.212091	34.781302	68.492967
1129.880572	26.333612	68.497972
1129.136109	33.870260	68.502977
1129.058466	27.788757	68.507982
1128.132806	36.972271	68.512986
1127.120212	31.511004	68.517991
1126.735348	34.435963	68.522996
1125.933527	40.832074	68.528001
1125.080985	31.675574	68.533006
1124.372652	38.466846	68.538010
1124.015095	39.720529	68.543015
1123.689600	28.370122	68.548020
1122.816610	34.709738	68.553025
1122.070942	23.662720	68.558030
1121.019548	37.983733	68.563034
1120.487729	31.640133	68.568039
1120.400562	33.174104	68.573044
1119.611337	30.465525	68.578049
1118.728046	23.922350	68.583054
1117.957084	27.665698	68.588058
1117.387265	31.162577	68.593063
1116.518412	30.672946	68.598068
1115.555397	36.424453	68.603073
1115.283401	25.287904	68.608078
1114.616778	27.872880	68.613082
1114.159811	29.706956	68.618087
1113.841063	24.912821	68.623092
1112.701644	33.163609	68.628097
1112.198173	24.845781	68.633102
1111.749251	33.106598	68.638106
1110.800014	36.017241	68.643111
1109.548723	29.625644	68.648116
1108.519348	39.874394	68.653121
1108.322984	30.129381	68.658126
1108.160237	32.705182	68.663130
1107.762530	30.361713	68.668135
1107.735856	28.310909	68.673140
1106.564173	30.331209	68.678145
1106.255017	29.014503	68.683150
1104.880460	34.575991	68.688154
1103.871860	28.902777	68.693159
1103.465542	27.841235	68.698164
1102.901889	28.905338	68.703169
1102.284746	26.063734	68.708174
1101.470832	34.253290	68.713178
1100.937469	29.122688	68.718183
1100.689983	26.160782	68.723188
1099.143664	35.950830	68.728193
1098.692840	16.151661	68.733198
1097.806364	38.200755	68.738202
1097.637262	31.200193	68.743207
1097.222743	32.672686	68.748212
1096.305323	32.791639	68.753217
1095.690458	25.302133	68.758222
1094.992636	37.475757	68.763226
1094.173776	28.419576	68.768231
1093.943765	27.522392	68.773236
1092.679730	30.129854	68.778241
1092.014303	21.145473	68.783246
1091.506424	36.364114	68.788250
1091.322816	28.411750	68.793255
1090.565032	33.499804	68.798260
1089.519020	36.924191	68.803265
1088.821812	30.852927	68.808270
1088.465405	26.162563	68.813274
1087.575740	26.478966	68.818279
1086.687240	25.038360	68.823284
1085.805107	35.041330	68.828289
1085.796010	30.546470	68.833294
1085.140241	32.401134	68.838298
1084.589421	32.734607	68.843303
1083.652333	28.057757	68.848308
1082.766347	40.827473	68.853313
1082.622061	29.736850	68.858318
1082.095859	43.627390	68.863322
1081.007162	34.320803	68.868327
1080.460368	32.918891	68.873332
1079.793389	36.915385	68.878337
1079.399338	31.636464	68.883342
1078.120552	39.433170	68.888346
1077.422602	40.152768	68.893351
1076.974050	34.381017	68.898356
1076.327636	44.444276	68.903361
1076.165947	26.251850	68.908366
1074.913074	35.750792	68.913370
1073.980792	42.492539	68.918375
1073.744075	30.725875	68.923380
1073.391812	43.995781	68.928385
1072.851152	34.584675	68.933390
1071.618130	36.371884	68.938394
1071.130145	35.197175	68.943399
1070.985310	29.918040	68.948404
1069.604509	30.588556	68.953409
1068.871597	26.070057	68.958414
1068.274402	32.909895	68.963418
1067.510634	34.855864	68.968423
1067.479310	29.323694	68.973428
1066.516622	32.611826	68.978433
1065.797402	25.350253	68.983438
1065.044877	33.219375	68.988442
1064.326744	41.060952	68.993447
1064.138942	25.881680	68.998452
1063.644577	39.992670	69.003457
1062.724868	30.897347	69.008462
1061.820735	34.166704	69.013466
1061.324779	34.582923	69.018471
1060.694575	32.593431	69.023476
1059.678398	37.648475	69.028481
1059.090581	32.818298	69.033486
1058.611368	37.638107	69.038490
1058.095667	36.373187	69.043495
1057.535511	26.837452	69.048500
1056.431403	31.255166	69.053505
1056.030662	25.054748	69.058510
1055.584943	29.973312	69.063514
1054.294099	30.336196	69.068519
1053.949206	30.651111	69.073524
1053.326840	37.912874	69.078529
1053.253212	23.335222	69.083534
1052.060597	37.929467	69.088538
1050.948091	45.838516	69.093543
1050.443279	34.937718	69.098548
1049.965564	23.274061	69.103553
1049.852397	35.133899	69.108558
1048.726655	26.552358	69.113562
1047.796461	22.956278	69.118567
1047.599262	30.107823	69.123572
1046.794575	35.337397	69.128577
1045.526441	27.448751	69.133582
1045.012458	31.712665	69.138586
1044.329430	31.769117	69.143591
1044.216105	30.238330	69.148596
1043.657433	34.656019	69.153601
1043.342767	30.742811	69.158606
1042.117055	31.148960	69.163610
1041.387123	37.210361	69.168615
1041.033093	39.641544	69.173620
1039.882895	29.174601	69.178625
1038.976095	31.750491	69.183630
1038.661751	29.844806	69.188634
1038.020296	37.620569	69.193639
1038.190774	29.433679	69.198644
1036.867146	35.706228	69.203649
1036.002589	30.711913	69.208654
1035.293601	26.782586	69.213658
1034.891005	32.782450	69.218663
1034.609866	24.586979	69.223668
1033.201078	35.981110	69.228673
1033.040155	29.726773	69.233678
1032.322060	30.321847	69.238682
1031.117479	34.806021	69.243687
1031.047288	31.156715	69.248692
1030.237732	29.651528	69.253697
1029.921629	25.483072	69.258702
1029.096797	31.640000	69.263706
1027.843894	26.332134	69.268711
1027.577225	25.983291	69.273716
1026.595990	29.902048	69.278721
1026.354616	23.460230	69.283726
1025.544934	28.386233	69.288730
1024.269346	29.607770	69.293735
1024.101357	27.877511	69.298740
1023.164919	33.372492	69.303745
1023.317601	19.894315	69.308750
1022.746113	29.603434	69.313754
1021.761705	35.904030	69.318759
1021.119501	30.057440	69.323764
1020.320505	28.134239	69.328769
1019.496406	27.689563	69.333774
1018.621336	22.674852	69.338778
1017.865295	30.678590	69.343783
1017.757886	28.892960	69.348788
1017.060308	29.508429	69.353793
1016.954944	30.203158	69.358798
1015.828168	35.370434	69.363802
1015.047705	34.540328	69.368807
1014.551264	26.030587	69.373812
1013.048698	37.904874	69.378817
1012.663298	27.243731	69.383822
1012.156691	31.670488	69.388826
1011.594559	27.892856	69.393831
1011.516785	27.070814	69.398836
1010.522994	29.736251	69.403841
1009.910916	30.379123	69.408846
1009.140509	34.193380	69.413850
1008.720821	41.416598	69.418855
1007.727923	35.942789	69.423860
1006.921185	42.150467	69.428865
1006.420164	30.088381	69.433870
1005.625243	33.895499	69.438874
1005.292336	31.724675	69.443879
1004.433475	27.074840	69.448884
1003.608132	34.234853	69.453889
1003.222585	26.934409	69.458894
1002.562330	26.261811	69.463898
1001.134961	33.457678	69.468903
1000.939140	24.986851	69.473908
1000.219974	33.033615	69.478913
999.978907	31.773903	69.483918
999.670667	33.767272	69.488922
998.436429	30.945021	69.493927
997.608131	32.721493	69.498932
996.881821	39.227054	69.503937
996.804938	33.968655	69.508942
996.181059	39.571623	69.513946
995.048400	45.231884	69.518951
994.564562	39.423184	69.523956
993.779288	33.671908	69.528961
993.684640	34.265579	69.533966
992.068542	37.572534	69.538970
991.189544	35.056487	69.543975
991.120986	34.538924	69.548980
990.262797	45.113733	69.553985
989.804205	33.918580	69.558990
989.687990	35.594378	69.563994
988.994429	29.098343	69.568999
988.450428	24.015200	69.574004
987.558622	36.601345	69.579009
986.151111	36.249502	69.584014
985.402547	35.669811	69.589018
984.873100	40.775182	69.594023
984.472904	32.825753	69.599028
983.933744	35.925097	69.604033
983.880206	26.906479	69.609038
982.680622	26.934742	69.614042
981.961428	32.688500	69.619047
981.845897	35.816642	69.624052
980.239311	31.735237	69.629057
979.555812	24.934816	69.634062
978.869750	33.794801	69.639066
978.350671	34.381881	69.644071
978.204371	20.938661	69.649076
977.745850	36.956896	69.654081
977.206208	27.813759	69.659086
976.048218	32.440361	69.664090
975.564481	33.394000	69.669095
975.061484	25.740069	69.674100
973.252500	31.064793	69.679105
973.094524	25.409272	69.684110
972.527590	35.343193	69.689114
972.017465	32.311121	69.694119
971.711655	26.379485	69.699124
970.765874	42.229234	69.704129
970.100186	32.055844	69.709134
969.863091	37.247172	69.714138
969.004446	33.843175	69.719143
967.980334	30.872382	69.724148
966.878063	41.020803	69.729153
966.344630	36.784426	69.734158
966.240534	36.234671	69.739162
965.578881	32.991730	69.744167
965.698929	26.121811	69.749172
964.090253	34.165026	69.754177
963.530768	30.390139	69.759182
962.797812	29.886824	69.764186
961.842871	34.927427	69.769191
961.152902	28.158003	69.774196
960.657115	36.298552	69.779201
960.154662	27.903329	69.784206
960.021713	31.430079	69.789210
959.204398	36.117607	69.794215
958.521679	27.675369	69.799220
957.940066	32.063605	69.804225
956.804739	28.612169	69.809230
955.770912	26.871442	69.814234
955.034835	34.256974	69.819239
954.847880	28.560331	69.824244
954.540140	32.423993	69.829249
953.799360	28.982324	69.834254
953.037264	30.587418	69.839258
952.660096	34.966780	69.844263
952.200593	24.104546	69.849268
950.685009	35.044170	69.854273
950.084400	27.382121	69.859278
949.833723	29.665973	69.864282
948.887817	35.399039	69.869287
948.233124	35.982471	69.874292
946.930451	32.865190	69.879297
946.956028	24.784944	69.884302
946.665786	30.038346	69.889306
945.663510	33.875320	69.894311
944.638294	23.549407	69.899316
943.986773	32.366052	69.904321
943.499146	25.755261	69.909326
943.251239	22.621547	69.914330
942.547855	27.647358	69.919335
942.043937	32.102085	69.924340
940.992256	34.661636	69.929345
940.462353	23.990390	69.934350
939.995081	27.439443	69.939354
938.828501	28.208414	69.944359
938.396974	23.958987	69.949364
937.785426	38.527043	69.954369
937.186646	27.559233	69.959374
935.955815	36.526414	69.964378
935.328526	34.082304	69.969383
934.734053	25.895708	69.974388
934.416765	30.667687	69.979393
934.200244	29.552318	69.984398
933.421190	28.524885	69.989402
932.598832	20.032337	69.994407
932.087273	18.777826	69.999412
931.168518	31.246835	70.004417
930.171775	28.729046	70.009422
929.493814	28.161793	70.014426
928.745199	26.265300	70.019431
928.771774	30.294974	70.024436
928.033297	36.580121	70.029441
927.302345	29.610638	70.034446
926.238569	34.564487	70.039450
925.737987	32.816193	70.044455
925.470278	29.385993	70.049460
924.421335	34.181354	70.054465
923.363973	28.831390	70.059470
922.661639	29.941255	70.064474
922.222371	35.639444	70.069479
922.552730	30.861906	70.074484
921.853630	36.368040	70.079489
920.905264	28.778685	70.084494
920.241274	29.404606	70.089498
919.318925	29.478673	70.094503
918.466752	25.416043	70.099508
917.270385	34.434518	70.104513
916.849866	32.807535	70.109518
916.787905	34.736489	70.114522
916.156425	31.343675	70.119527
915.395710	26.835960	70.124532
914.607535	31.119871	70.129537
914.149490	32.484193	70.134542
913.700714	25.383077	70.139546
912.366412	29.192468	70.144551
911.838834	24.455257	70.149556
911.215902	36.631182	70.154561
910.995553	34.559162	70.159566
909.865838	28.764954	70.164570
908.801520	31.026890	70.169575
908.584000	33.343318	70.174580
908.138386	35.719699	70.179585
907.683893	28.020218	70.184590
906.733959	35.958638	70.189594
905.754922	31.031480	70.194599
905.730924	23.747646	70.199604
904.669288	31.902547	70.204609
903.997347	31.072555	70.209614
903.215213	31.874985	70.214618
902.569734	41.118058	70.219623
902.170799	28.527225	70.224628
901.368524	40.047259	70.229633
900.759907	32.460619	70.234638
899.922673	36.279231	70.239642
899.327582	37.312108	70.244647
899.206315	28.179692	70.249652
897.801166	41.093570	70.254657
897.263785	32.099915	70.259662
896.913298	32.194956	70.264666
896.194636	32.862701	70.269671
895.813273	38.876549	70.274676
894.442649	38.540967	70.279681
894.020838	39.595158	70.284686
893.591228	36.988707	70.289690
892.867838	38.035695	70.294695
892.186274	26.486533	70.299700
891.181712	28.194888	70.304705
890.959147	28.290073	70.309710
890.277687	35.173314	70.314714
889.599381	32.328883	70.319719
888.655720	28.473221	70.324724
887.686191	34.721026	70.329729
887.633045	30.124372	70.334734
887.095900	34.455079	70.339738
886.368839	29.970404	70.344743
885.528387	27.651700	70.349748
885.014436	40.191931	70.354753
884.706675	33.177193	70.359758
883.191180	42.005186	70.364762
882.314381	40.304157	70.369767
882.201622	36.259489	70.374772
881.195450	40.518177	70.379777
881.117963	37.515050	70.384782
880.774710	32.901482	70.389786
879.480930	39.565190	70.394791
879.506160	31.376186	70.399796
878.671921	38.900367	70.404801
877.382141	39.532845	70.409806
876.844581	40.219086	70.414810
876.120002	41.961742	70.419815
875.698028	34.061539	70.424820
875.065194	36.721623	70.429825
874.140957	32.064894	70.434830
873.317447	35.763051	70.439834
872.599506	41.713767	70.444839
872.541893	35.226954	70.449844
871.916732	45.472951	70.454849
871.269864	30.420400	70.459854
870.561686	32.121020	70.464858
869.549396	36.491077	70.469863
869.384755	27.496463	70.474868
867.911558	33.780275	70.479873
867.418247	30.002767	70.484878
867.110140	30.382819	70.489882
866.496430	30.745271	70.494887
866.112483	33.368901	70.499892
865.036343	42.912345	70.504897
864.891027	34.360954	70.509902
864.009431	33.914442	70.514906
862.504966	36.279565	70.519911
862.265842	32.439524	70.524916
861.748866	41.644805	70.529921
861.438880	24.463267	70.534926
860.786207	33.756374	70.539930
859.597602	36.104347	70.544935
859.290494	26.949473	70.549940
858.557774	36.214319	70.554945
857.789500	32.501076	70.559950
856.625779	33.706468	70.564954
855.803339	38.416919	70.569959
855.696612	25.267059	70.574964
855.322744	36.807231	70.579969
854.898146	32.361165	70.584974
854.027492	34.002489	70.589978
853.116206	37.173698	70.594983
852.897899	34.625094	70.599988
851.947035	35.255687	70.604993
850.769155	27.658736	70.609998
850.132312	33.470384	70.615002
849.494683	33.049706	70.620007
849.396839	28.111643	70.625012
848.773093	26.468130	70.630017
848.041861	28.610841	70.635022
847.000346	27.376036	70.640026
846.493846	30.697299	70.645031
846.131564	24.101280	70.650036
845.552237	31.310489	70.655041
844.585568	27.493203	70.660046
844.108959	29.484997	70.665050
843.381723	29.944376	70.670055
842.960080	26.647503	70.675060
841.687665	30.568512	70.680065
841.022330	30.716825	70.685070
840.729950	25.924850	70.690074
840.188036	29.092469	70.695079
839.174058	27.692427	70.700084
838.318637	28.066547	70.705089
837.558643	25.596277	70.710094
837.512102	26.494548	70.715098
836.942043	22.811271	70.720103
836.199696	15.275909	70.725108
834.968439	21.297286	70.730113
834.485349	20.781049	70.735118
833.900283	26.239084	70.740122
833.832943	26.468849	70.745127
832.572045	20.493703	70.750132
831.788852	24.133410	70.755137
831.338089	26.641515	70.760142
831.180818	22.025168	70.765146
829.908617	27.643037	70.770151
829.547898	25.552366	70.775156
828.807175	24.900508	70.780161
828.224582	19.221124	70.785166
827.261857	21.372299	70.790170
826.689629	25.990887	70.795175
826.089403	27.237497	70.800180
825.558870	29.338808	70.805185
825.168482	23.947392	70.810190
823.965056	27.556213	70.815194
822.881169	29.531123	70.820199
822.748095	21.066111	70.825204
822.388965	27.735623	70.830209
821.776719	28.039503	70.835214
821.013012	18.337544	70.840218
820.206767	24.824318	70.845223
819.907318	19.052558	70.850228
818.457679	28.810007	70.855233
817.836105	27.183503	70.860238
817.634819	23.682820	70.865242
817.063421	32.056201	70.870247
816.500472	26.392616	70.875252
815.345062	29.148507	70.880257
814.748815	25.679148	70.885262
814.530165	29.311009	70.890266
813.494815	35.827948	70.895271
812.567356	26.163091	70.900276
811.992504	31.135356	70.905281
811.653859	26.612538	70.910286
810.938683	30.097916	70.915290
810.358109	28.280375	70.920295
809.235623	31.970942	70.925300
808.779148	32.726296	70.930305
808.199721	31.041043	70.935310
808.110121	29.747780	70.940314
807.070300	30.116568	70.945319
806.347039	24.849107	70.950324
805.669234	36.106481	70.955329
805.002191	24.875182	70.960334
804.105608	29.154298	70.965338
802.984233	31.859043	70.970343
802.826056	29.283527	70.975348
802.006577	30.612354	70.980353
802.079508	27.478052	70.985358
801.647024	30.281312	70.990362
800.247873	34.988953	70.995367
799.993895	22.882888	71.000372
799.387617	31.001612	71.005377
798.543565	26.899886	71.010382
797.752982	20.991829	71.015386
797.220588	35.359627	71.020391
796.644820	26.968237	71.025396
795.575105	33.782403	71.030401
794.962623	27.817608	71.035406
794.542253	29.007210	71.040410
793.496203	31.545420	71.045415
792.697966	26.141656	71.050420
791.885615	30.992449	71.055425
791.356767	25.790245	71.060430
791.114151	25.574801	71.065434
790.195937	33.686409	71.070439
790.223048	23.864884	71.075444
789.731969	30.741493	71.080449
788.473534	21.031559	71.085454
787.888272	27.699220	71.090458
786.987935	22.986684	71.095463
786.493036	17.108840	71.100468
785.505621	28.652051	71.105473
785.188917	28.104606	71.110478
784.613004	28.672385	71.115482
783.674753	26.375594	71.120487
783.022134	24.386593	71.125492
781.953420	24.277417	71.130497
781.967813	28.774247	71.135502
781.764701	26.264236	71.140506
780.655676	24.142873	71.145511
779.850580	20.585339	71.150516
779.109583	19.518780	71.155521
778.655250	22.746588	71.160526
777.903530	18.757913	71.165530
776.906206	27.467194	71.170535
776.446008	28.456547	71.175540
775.636293	26.986167	71.180545
775.420229	30.505648	71.185550
775.057399	21.932130	71.190554
773.800711	25.864858	71.195559
773.199469	20.958052	71.200564
772.784133	22.044348	71.205569
772.017446	20.366836	71.210574
771.570206	24.019316	71.215578
770.991760	26.654993	71.220583
770.444947	21.575511	71.225588
768.854328	26.737867	71.230593
768.371841	23.185755	71.235598
767.970606	21.486341	71.240602
767.615455	27.909205	71.245607
766.693706	22.438378	71.250612
765.645479	24.265701	71.255617
765.101735	19.518487	71.260622
764.777431	24.372022	71.265626
764.335685	33.962745	71.270631
763.307124	15.917875	71.275636
762.404762	26.892434	71.280641
761.937802	19.642859	71.285646
761.661144	22.836078	71.290650
760.502765	33.881362	71.295655
759.667370	18.884115	71.300660
759.269309	16.744205	71.305665
758.801043	22.005453	71.310670
758.375233	22.325403	71.315674
757.297647	26.052999	71.320679
756.708409	19.150915	71.325684
756.157352	31.723863	71.330689
755.548873	27.384367	71.335694
755.192317	22.995306	71.340698
753.925293	31.730184	71.345703
753.519268	24.981868	71.350708
752.572362	29.317900	71.355713
752.121238	23.486714	71.360718
751.293011	28.631796	71.365722
750.335513	37.907215	71.370727
750.326683	16.967012	71.375732
749.690715	22.772226	71.380737
749.401279	23.095700	71.385742
748.523569	20.358756	71.390746
747.334600	24.110395	71.395751
747.065549	18.294384	71.400756
745.586226	25.328322	71.405761
744.909000	27.498734	71.410766
744.359150	19.757709	71.415770
743.975366	22.649422	71.420775
744.084218	15.759217	71.425780
743.402492	21.666339	71.430785
742.336833	20.489042	71.435790
741.520478	17.631941	71.440794
740.884533	24.701936	71.445799
740.594897	18.553294	71.450804
739.215660	27.429048	71.455809
738.568586	24.781553	71.460814
737.966332	20.407956	71.465818
737.432585	26.655817	71.470823
737.411168	20.461321	71.475828
736.320924	29.392000	71.480833
735.482837	21.789909	71.485838
734.987833	16.355243	71.490842
734.143485	26.910544	71.495847
734.144063	21.406441	71.500852
732.873895	22.210920	71.505857
732.299454	14.696178	71.510862
731.911273	19.971489	71.515866
730.901200	28.093004	71.520871
729.910283	22.663167	71.525876
729.082803	26.261065	71.530881
728.607174	24.281750	71.535886
728.583751	24.838857	71.540890
728.284984	30.092052	71.545895
727.268706	13.023014	71.550900
726.682109	19.014346	71.555905
725.768258	23.021830	71.560910
724.942961	27.679149	71.565914
724.108210	31.827016	71.570919
723.680600	22.669281	71.575924
723.246871	31.441825	71.580929
722.848249	26.602126	71.585934
721.987881	16.401484	71.590938
721.065279	30.003462	71.595943
720.451919	23.403287	71.600948
719.494425	28.668311	71.605953
718.348174	29.296943	71.610958
718.014637	20.477490	71.615962
717.643865	24.791196	71.620967
717.440034	23.516125	71.625972
717.153296	29.748320	71.630977
716.313343	35.048253	71.635982
715.585156	19.422069	71.640986
714.272787	24.447111	71.645991
713.359550	17.754328	71.650996
712.609687	28.811860	71.656001
711.945354	20.351019	71.661006
711.931477	18.817036	71.666010
711.201064	26.386226	71.671015
711.138201	20.542124	71.676020
710.052078	19.215127	71.681025
709.101881	16.625364	71.686030
708.863983	13.192030	71.691034
707.936408	25.805999	71.696039
707.293227	18.721697	71.701044
706.342964	22.444811	71.706049
705.669458	22.982411	71.711054
705.678385	17.812890	71.716058
704.531576	26.263703	71.721063
703.741153	20.322539	71.726068
703.426494	21.290310	71.731073
702.741814	21.468549	71.736078
701.899750	33.190503	71.741082
700.885780	28.384122	71.746087
700.814027	22.413696	71.751092
699.901901	28.396938	71.756097
699.568469	23.816539	71.761102
698.489410	20.581789	71.766106
697.450703	23.615630	71.771111
697.347791	19.723965	71.776116
696.757928	28.384167	71.781121
696.002934	32.513035	71.786126
695.180211	26.741026	71.791130
694.231240	17.503878	71.796135
694.190827	12.280711	71.801140
693.535883	21.263523	71.806145
692.980938	19.083945	71.811150
692.205105	22.050702	71.816154
691.613253	22.010727	71.821159
690.670402	14.050005	71.826164
689.783293	19.325908	71.831169
689.119456	17.701437	71.836174
688.686842	16.912251	71.841178
688.276380	29.547977	71.846183
687.687773	11.633392	71.851188
686.772711	16.014837	71.856193
685.567177	17.856198	71.861198
685.579482	13.130865	71.866202
684.789254	18.806102	71.871207
683.779386	11.687152	71.876212
683.082098	17.514757	71.881217
682.156909	26.158961	71.886222
682.115280	26.491874	71.891226
681.478912	21.634844	71.896231
681.343446	15.773920	71.901236
680.046514	20.780748	71.906241
679.468064	27.715437	71.911246
678.963672	21.358137	71.916250
678.396172	26.546884	71.921255
677.683408	21.864453	71.926260
676.922202	19.490629	71.931265
676.381078	17.491790	71.936270
675.563828	12.263000	71.941274
674.486755	25.471666	71.946279
674.169283	20.913963	71.951284
673.715941	23.165445	71.956289
672.862274	23.682852	71.961294
672.158204	23.797952	71.966298
671.301115	27.042595	71.971303
670.932827	25.307987	71.976308
670.561528	23.811992	71.981313
669.854568	27.706124	71.986318
668.845434	14.078647	71.991322
668.030044	24.643544	71.996327
667.951409	22.328203	72.001332
666.479011	28.198806	72.006337
665.903555	30.066014	72.011342
665.564822	16.334943	72.016346
664.863979	27.690621	72.021351
664.833608	21.483362	72.026356
663.762138	24.475123	72.031361
662.792172	29.456709	72.036366
662.418342	28.118820	72.041370
661.561550	27.914447	72.046375
661.251002	19.092924	72.051380
660.020651	23.026241	72.056385
659.212160	22.599701	72.061390
658.891307	11.474203	72.066394
658.163938	27.839605	72.071399
657.908957	15.809436	72.076404
657.067842	22.800145	72.081409
656.051334	23.581619	72.086414
656.162646	14.715004	72.091418
655.579839	19.131867	72.096423
654.673068	11.894007	72.101428
653.941447	21.136629	72.106433
652.883901	16.759858	72.111438
651.911185	19.843136	72.116442
651.184566	21.529402	72.121447
650.693349	13.293346	72.126452
650.259733	21.624303	72.131457
649.854254	18.227122	72.136462
649.609581	10.382339	72.141466
648.441408	24.717325	72.146471
647.720732	16.191361	72.151476
647.118899	16.733333	72.156481
646.674150	21.552437	72.161486
645.881776	15.985364	72.166490
644.712618	10.229121	72.171495
644.463394	16.710820	72.176500
644.083091	19.076838	72.181505
642.972977	20.299022	72.186510
642.670074	14.792787	72.191514
641.165593	20.242711	72.196519
641.258078	17.016985	72.201524
640.554813	26.048506	72.206529
640.187443	16.251970	72.211534
639.316523	18.506870	72.216538
638.353386	28.854017	72.221543
638.058732	23.843232	72.226548
637.302571	20.342616	72.231553
636.491858	25.958049	72.236558
636.072443	17.164908	72.241562
635.379009	18.139383	72.246567
634.787098	19.797895	72.251572
633.703782	12.668586	72.256577
632.998705	15.232986	72.261582
633.015306	7.701434	72.266586
631.774714	22.592031	72.271591
631.276384	11.646196	72.276596
630.606415	17.890529	72.281601
629.707548	20.559912	72.286606
629.579120	18.328200	72.291610
628.441785	20.187114	72.296615
628.019034	13.395763	72.301620
627.050616	21.977474	72.306625
626.723605	19.062990	72.311630
626.091162	11.743609	72.316634
624.947263	21.737899	72.321639
624.770326	16.383504	72.326644
624.115999	19.370356	72.331649
623.351309	22.111418	72.336654
622.612406	17.922050	72.341658
621.789739	18.918686	72.346663
621.418915	13.815953	72.351668
620.846379	18.343156	72.356673
620.079970	24.952953	72.361678
618.876036	12.903595	72.366682
617.935309	24.117697	72.371687
618.168751	13.067948	72.376692
617.869006	21.398090	72.381697
617.129465	25.018288	72.386702
616.196735	21.662497	72.391706
615.273374	25.129033	72.396711
615.002901	24.339271	72.401716
614.091840	18.450471	72.406721
612.622334	18.346844	72.411726
612.738283	19.086770	72.416730
611.983339	21.988718	72.421735
611.621822	13.328299	72.426740
611.051689	16.749621	72.431745
610.159902	20.007692	72.436750
609.735403	14.716380	72.441754
608.821007	27.528558	72.446759
607.625091	20.164865	72.451764
607.169267	17.860708	72.456769
606.668603	13.677563	72.461774
606.324500	23.142348	72.466778
605.645347	26.186778	72.471783
605.373520	15.737913	72.476788
604.348505	19.487159	72.481793
603.287527	20.277313	72.486798
603.031649	19.652393	72.491802
602.010012	23.872635	72.496807
600.863060	19.025977	72.501812
600.700659	19.499556	72.506817
600.002834	27.399487	72.511822
599.899138	18.630196	72.516826
599.249455	23.410976	72.521831
598.661905	18.699170	72.526836
597.789705	23.294603	72.531841
597.027035	23.199848	72.536846
595.759661	8.730405	72.541850
595.020303	27.081627	72.546855
594.652052	24.369267	72.551860
594.391311	18.780628	72.556865
594.038924	19.218228	72.561870
593.247064	16.428246	72.566874
592.075574	20.453148	72.571879
591.810497	17.735398	72.576884
590.992364	20.792502	72.581889
590.154813	21.771017	72.586894
589.226158	16.228824	72.591898
588.411117	23.891945	72.596903
588.500532	20.321337	72.601908
588.289114	21.567583	72.606913
587.269274	20.761544	72.611918
586.559749	14.367552	72.616922
585.739061	18.254582	72.621927
585.432889	16.041719	72.626932
584.261407	17.685307	72.631937
583.444913	22.653514	72.636942
583.259750	22.433671	72.641946
582.404920	27.423755	72.646951
581.382165	23.688058	72.651956
580.694092	24.373097	72.656961
579.981760	16.107618	72.661966
579.726756	19.166506	72.666970
579.329351	24.243020	72.671975
578.632424	16.120174	72.676980
577.585396	17.081590	72.681985
577.063237	19.687839	72.686990
576.731123	17.274095	72.691994
576.094550	16.566301	72.696999
575.291594	18.392485	72.702004
574.632658	18.219712	72.707009
573.785185	14.616961	72.712014
572.829350	15.833527	72.717018
571.790560	16.733707	72.722023
571.451756	18.299878	72.727028
571.101233	20.328409	72.732033
570.543973	20.560510	72.737038
570.534044	20.478348	72.742042
568.920780	22.086643	72.747047
568.512078	13.441634	72.752052
568.192367	18.212444	72.757057
567.280285	13.730541	72.762062
566.091132	16.443023	72.767066
565.304573	13.280028	72.772071
565.130130	15.384599	72.777076
564.851239	15.146568	72.782081
564.259047	18.929399	72.787086
563.280173	14.388746	72.792090
562.340124	14.035234	72.797095
562.189411	14.781356	72.802100
561.581787	13.551689	72.807105
560.455518	21.122452	72.812110
560.045383	10.981072	72.817114
559.220780	24.748830	72.822119
559.008460	16.312253	72.827124
558.023695	25.696145	72.832129
556.773339	23.673094	72.837134
556.702710	19.208568	72.842138
556.022102	22.360478	72.847143
555.021367	21.385822	72.852148
554.266768	14.366631	72.857153
553.167986	26.086919	72.862158
553.333054	25.207292	72.867162
552.767608	26.834797	72.872167
552.686741	24.297456	72.877172
551.324809	22.173902	72.882177
550.541486	20.413953	72.887182
550.223463	17.750375	72.892186
549.518457	24.568038	72.897191
548.273980	24.873330	72.902196
547.990149	25.995489	72.907201
547.291366	25.871649	72.912206
547.260609	22.763327	72.917210
546.143244	26.904215	72.922215
545.173970	20.367095	72.927220
544.680489	13.060301	72.932225
543.968148	13.741331	72.937230
543.878422	15.988535	72.942234
542.564700	18.769757	72.947239
542.061654	16.086763	72.952244
541.480493	14.423934	72.957249
540.649028	27.640830	72.962254
539.598275	16.161661	72.967258
539.097018	20.666486	72.972263
538.611296	15.222508	72.977268
538.192984	18.807329	72.982273
537.899923	16.655466	72.987278
537.589789	16.903409	72.992282
536.274013	29.065141	72.997287
535.907659	24.337043	73.002292
534.437781	19.284800	73.007297
533.742680	22.334940	73.012302
533.200797	16.791092	73.017306
532.866826	22.295920	73.022311
532.553450	21.298526	73.027316
531.583990	20.132808	73.032321
530.750086	23.550428	73.037326
530.236420	12.323202	73.042330
529.678010	14.552015	73.047335
529.030738	20.508889	73.052340
528.356282	17.020529	73.057345
527.313739	19.182948	73.062350
527.086224	21.496258	73.067354
526.226845	25.268038	73.072359
525.384797	13.903876	73.077364
525.045962	21.866491	73.082369
523.939188	21.351883	73.087374
524.074158	17.856026	73.092378
522.970997	21.759682	73.097383
522.083645	16.084777	73.102388
521.633222	23.940582	73.107393
520.835410	24.633656	73.112398
520.549726	16.300239	73.117402
519.455456	21.594997	73.122407
518.916052	22.262680	73.127412
518.131721	16.139261	73.132417
517.974887	20.059345	73.137422
517.217208	18.020919	73.142426
516.147899	22.584692	73.147431
515.592124	17.203919	73.152436
515.368377	21.246631	73.157441
514.190994	26.571980	73.162446
513.447149	12.249442	73.167450
512.772192	20.751324	73.172455
512.332917	19.171561	73.177460
512.162612	20.050124	73.182465
510.972140	24.256290	73.187470
510.172505	12.987886	73.192474
509.636672	23.118757	73.197479
509.423032	14.333876	73.202484
508.269377	14.657838	73.207489
507.473395	17.637317	73.212494
507.427713	12.459160	73.217498
506.489915	22.865383	73.222503
505.765808	18.214782	73.227508
504.924403	15.949989	73.232513
504.152192	17.517395	73.237518
503.657779	20.494571	73.242522
503.218065	24.563802	73.247527
502.421200	15.343521	73.252532
501.592601	13.463062	73.257537
500.736080	25.496452	73.262542
500.794148	13.769709	73.267546
500.041602	18.916995	73.272551
499.271071	13.042133	73.277556
498.364372	18.395333	73.282561
497.725443	21.813444	73.287566
497.578993	21.147449	73.292570
496.359706	21.051342	73.297575
495.758758	13.857880	73.302580
495.435920	16.214763	73.307585
494.670188	25.333535	73.312590
493.850417	18.793125	73.317594
492.943303	14.952312	73.322599
492.463280	22.115788	73.327604
492.227568	19.650429	73.332609
491.177439	30.024091	73.337614
490.669854	28.335359	73.342618
489.927137	31.020917	73.347623
489.451622	27.666464	73.352628
488.970768	23.760901	73.357633
487.529271	28.336665	73.362638
487.354591	24.778164	73.367642
486.643159	33.181783	73.372647
486.239106	22.810778	73.377652
485.102992	25.253061	73.382657
484.242076	29.286887	73.387662
484.092113	22.854254	73.392666
483.610246	21.746505	73.397671
482.704735	16.815713	73.402676
481.763530	20.294597	73.407681
481.087619	26.776464	73.412686
480.486655	22.178797	73.417690
479.973085	24.681190	73.422695
479.244292	21.174691	73.427700
478.593949	25.972949	73.432705
478.081159	24.833856	73.437710
477.679383	22.164706	73.442714
476.784284	33.617599	73.447719
475.821111	24.764455	73.452724
475.054888	26.152712	73.457729
474.473038	25.967686	73.462734
474.395649	16.997093	73.467738
473.848924	29.028450	73.472743
473.028962	22.969071	73.477748
472.173364	23.999388	73.482753
471.379645	31.277502	73.487758
470.227630	20.965731	73.492762
469.556367	29.132706	73.497767
469.172556	17.799650	73.502772
468.833288	25.393314	73.507777
468.095966	27.492940	73.512782
468.090534	24.311198	73.517786
466.796717	33.845286	73.522791
466.083025	21.145454	73.527796
465.582791	30.682432	73.532801
464.463822	28.395634	73.537806
463.557914	29.197414	73.542810
462.863610	31.588248	73.547815
462.778668	24.197463	73.552820
462.469308	27.236634	73.557825
461.860180	30.197400	73.562830
461.274159	24.073946	73.567834
460.508507	24.720913	73.572839
459.856806	28.010175	73.577844
458.895981	19.486268	73.582849
457.922209	20.715197	73.587854
457.603728	17.840385	73.592858
456.948338	30.442593	73.597863
456.515247	24.704805	73.602868
455.483947	27.950459	73.607873
454.637994	26.878642	73.612878
454.525097	24.821095	73.617882
453.484165	27.871156	73.622887
452.488579	15.304558	73.627892
451.969259	26.678659	73.632897
451.246919	30.904894	73.637902
451.110209	19.261226	73.642906
450.512422	31.035781	73.647911
449.616019	18.812943	73.652916
449.093417	16.661390	73.657921
448.093607	29.059838	73.662926
448.004412	21.955176	73.667930
446.979664	22.777472	73.672935
445.999936	28.222754	73.677940
445.627062	22.639387	73.682945
445.012808	26.075658	73.687950
444.674860	21.885551	73.692954
443.470164	18.916954	73.697959
442.979558	18.928720	73.702964
442.589154	26.339712	73.707969
441.831057	23.105988	73.712974
440.891523	14.610242	73.717978
440.130386	23.401847	73.722983
439.556822	18.296756	73.727988
439.569568	19.663424	73.732993
438.357937	26.038253	73.737998
437.894579	20.584427	73.743002
437.162192	21.634551	73.748007
436.229353	19.087869	73.753012
435.093749	22.626127	73.758017
434.230034	27.679174	73.763022
434.484803	20.257926	73.768026
433.695806	23.184272	73.773031
433.454917	16.376609	73.778036
433.190127	24.803696	73.783041
431.921924	28.120220	73.788046
431.664629	17.788933	73.793050
430.487183	26.777763	73.798055
429.247188	31.822951	73.803060
428.362376	25.702954	73.808065
427.866329	26.634998	73.813070
427.871884	21.618999	73.818074
427.527619	24.597499	73.823079
427.064757	27.087091	73.828084
426.118552	22.684801	73.833089
425.194617	27.742715	73.838094
424.889741	21.648600	73.843098
423.472551	22.514507	73.848103
422.855124	24.740130	73.853108
422.229087	22.737533	73.858113
421.785841	23.918221	73.863118
421.487603	11.480245	73.868122
420.802810	26.936829	73.873127
419.759487	25.363434	73.878132
419.146121	22.696467	73.883137
418.463798	22.087471	73.888142
418.249724	17.883942	73.893146
417.250178	22.819856	73.898151
416.473196	27.438022	73.903156
415.970012	17.038678	73.908161
415.330918	33.634488	73.913166
414.702253	23.326098	73.918170
413.579319	27.687135	73.923175
413.383230	19.691140	73.928180
413.141837	19.872949	73.933185
411.708415	17.139517	73.938190
410.976638	16.245076	73.943194
410.165195	21.303992	73.948199
409.820102	8.329413	73.953204
409.751909	13.866020	73.958209
408.996033	28.524917	73.963214
408.005712	26.990393	73.968218
407.188909	24.157138	73.973223
406.661013	29.041564	73.978228
406.376828	27.446572	73.983233
405.160087	32.142696	73.988238
404.739295	26.532276	73.993242
403.792441	29.520056	73.998247
403.658392	29.960742	74.003252
402.881313	26.206482	74.008257
401.690326	36.348718	74.013262
401.446592	20.366355	74.018266
400.900168	24.979329	74.023271
400.298335	19.773092	74.028276
399.441426	19.784881	74.033281
398.484511	28.202397	74.038286
398.689898	22.703528	74.043290
397.267672	30.383017	74.048295
396.415010	23.989817	74.053300
396.173399	24.546995	74.058305
395.442289	30.173465	74.063310
395.419159	19.263952	74.068314
394.127502	24.107640	74.073319
393.476267	19.770334	74.078324
392.911974	23.127688	74.083329
392.011242	31.621415	74.088334
391.504362	10.921521	74.093338
390.600855	23.634233	74.098343
390.092726	20.874809	74.103348
389.836382	21.565229	74.108353
388.686326	19.214034	74.113358
388.410793	18.138086	74.118362
387.823969	26.056642	74.123367
386.961638	20.831989	74.128372
385.935705	34.021557	74.133377
384.788387	33.742141	74.138382
384.823084	20.347479	74.143386
384.459643	24.169595	74.148391
383.794965	24.232764	74.153396
383.026290	20.256390	74.158401
382.012068	28.083771	74.163406
381.748832	21.967259	74.168410
380.889597	30.616810	74.173415
380.193053	23.473307	74.178420
379.331123	25.118128	74.183425
378.405854	26.512832	74.188430
378.258400	22.628290	74.193434
377.894460	23.532985	74.198439
377.044978	26.076305	74.203444
376.378222	19.475288	74.208449
375.468309	26.007080	74.213454
375.356047	23.088381	74.218458
374.420565	23.961140	74.223463
373.767585	23.645539	74.228468
373.222211	14.500362	74.233473
372.624946	21.065916	74.238478
371.469714	19.379482	74.243482
370.369961	28.636667	74.248487
369.583887	26.465611	74.253492
369.550426	33.685687	74.258497
368.981244	27.330908	74.263502
368.767962	22.048571	74.268506
367.619525	27.386716	74.273511
367.019328	28.564036	74.278516
366.388810	21.408441	74.283521
365.964054	28.156255	74.288526
365.408025	10.531525	74.293530
364.228620	19.661044	74.298535
363.911498	16.297152	74.303540
363.473178	22.638674	74.308545
362.525500	29.778914	74.313550
361.563194	28.255716	74.318554
361.003072	30.429642	74.323559
360.363732	18.181655	74.328564
360.135201	16.289207	74.333569
358.619974	26.107787	74.338574
358.136235	18.648096	74.343578
357.636814	17.683526	74.348583
357.286420	20.349181	74.353588
356.764862	22.092741	74.358593
355.921000	23.725228	74.363598
355.006923	13.339341	74.368602
354.612013	14.390905	74.373607
354.007708	19.412097	74.378612
353.308534	9.064512	74.383617
352.301701	13.435454	74.388622
352.095891	9.205387	74.393626
351.454933	17.976280	74.398631
350.203770	20.071085	74.403636
349.630416	28.798093	74.408641
349.140037	21.580747	74.413646
348.843688	16.398389	74.418650
347.895376	24.655266	74.423655
346.995778	23.249821	74.428660
346.373653	19.554472	74.433665
345.974835	24.098199	74.438670
345.449232	22.169509	74.443674
344.649570	21.074584	74.448679
343.657033	23.615480	74.453684
343.313898	12.872097	74.458689
342.589291	21.410307	74.463694
342.377815	10.988160	74.468698
341.267830	16.373802	74.473703
340.726285	21.361341	74.478708
340.253511	14.652151	74.483713
339.017034	23.021187	74.488718
338.324700	8.594326	74.493722
337.819016	19.696587	74.498727
337.477042	20.783876	74.503732
337.349732	20.979052	74.508737
335.796514	23.383787	74.513742
335.112993	12.896510	74.518746
334.304323	30.476601	74.523751
333.860150	23.631958	74.528756
333.606436	25.430614	74.533761
332.881553	19.666814	74.538766
332.205466	20.137112	74.543770
331.084763	29.555352	74.548775
330.799967	25.427762	74.553780
330.407619	16.538922	74.558785
329.097909	31.178856	74.563790
328.742932	24.868805	74.568794
327.810597	28.863595	74.573799
327.528937	24.927902	74.578804
326.724484	25.087483	74.583809
325.682259	22.955687	74.588814
325.357144	19.507915	74.593818
325.048571	25.527554	74.598823
324.507749	24.585359	74.603828
323.384948	21.247364	74.608833
322.343155	30.832814	74.613838
322.558841	19.421605	74.618842
321.922404	17.852799	74.623847
320.849112	18.455790	74.628852
320.148877	18.611380	74.633857
319.452942	31.988081	74.638862
318.596173	17.768784	74.643866
317.703782	25.469530	74.648871
317.060202	19.962451	74.653876
316.778672	13.397840	74.658881
316.246262	23.189125	74.663886
315.952876	18.559836	74.668890
314.816894	20.505409	74.673895
314.154765	23.392646	74.678900
313.847988	15.631940	74.683905
313.046601	28.533412	74.688910
312.341538	18.801816	74.693914
311.406477	20.932998	74.698919
310.818065	19.429085	74.703924
310.394039	14.237119	74.708929
309.440192	18.957618	74.713934
308.470740	7.877230	74.718938
307.722782	18.786282	74.723943
307.556645	19.900746	74.728948
307.401147	23.391671	74.733953
306.334221	33.020558	74.738958
305.935924	18.458526	74.743962
304.844043	20.294568	74.748967
304.607238	21.216858	74.753972
304.131387	20.597066	74.758977
302.955415	35.198353	74.763982
302.784104	28.132024	74.768986
301.640377	23.486865	74.773991
300.683887	15.044352	74.778996
300.048719	24.039848	74.784001
299.555731	29.683585	74.789006
299.116070	23.574703	74.794010
298.802326	23.957298	74.799015
297.760249	28.094173	74.804020
297.352037	22.429732	74.809025
296.634406	26.935964	74.814030
295.581395	24.239748	74.819034
294.423815	25.882829	74.824039
293.992242	21.106825	74.829044
293.671833	20.509572	74.834049
293.032735	24.413480	74.839054
292.845429	16.944411	74.844058
291.876876	29.341073	74.849063
291.123949	26.959748	74.854068
290.735491	23.449533	74.859073
289.479406	37.557369	74.864078
288.963692	25.912627	74.869082
288.413063	22.789399	74.874087
287.772117	29.530674	74.879092
287.401279	27.694031	74.884097
286.433036	33.516025	74.889102
285.793822	21.621299	74.894106
284.915904	26.213007	74.899111
284.405731	25.925134	74.904116
283.969467	18.443703	74.909121
282.786846	28.590952	74.914126
282.435385	18.374058	74.919130
281.771111	24.753181	74.924135
281.410813	22.998441	74.929140
280.908653	20.450990	74.934145
279.375217	28.389546	74.939150
279.304505	21.810261	74.944154
278.853759	28.901286	74.949159
278.018240	23.562011	74.954164
276.971908	23.296514	74.959169
276.517094	27.932757	74.964174
276.547357	29.853322	74.969178
275.223189	26.509596	74.974183
274.475827	19.535090	74.979188
274.079180	19.877282	74.984193
273.615349	22.166770	74.989198
272.416929	14.477224	74.994202
271.657567	17.080333	74.999207
270.943597	26.107320	75.004212
270.993564	24.056945	75.009217
269.930818	24.090548	75.014222
269.285477	22.830695	75.019226
268.494409	22.961352	75.024231
267.799065	19.817039	75.029236
267.320454	19.878970	75.034241
266.539920	27.486205	75.039246
266.161308	16.562405	75.044250
265.250086	10.178600	75.049255
264.333817	18.846726	75.054260
264.399036	15.871362	75.059265
263.186299	18.906299	75.064270
262.746941	14.986293	75.069274
261.997568	21.025728	75.074279
261.510648	22.615545	75.079284
260.984262	18.676292	75.084289
259.642576	22.387827	75.089294
259.280521	14.757376	75.094298
258.822009	17.691021	75.099303
258.133146	23.293439	75.104308
257.708961	25.991369	75.109313
256.605598	21.166327	75.114318
256.124873	18.328447	75.119322
255.409250	20.125037	75.124327
254.957333	21.714007	75.129332
254.024181	19.093328	75.134337
252.940123	24.504839	75.139342
252.953756	19.567991	75.144346
252.362792	21.087657	75.149351
251.372122	25.528606	75.154356
250.166821	16.242641	75.159361
249.603514	30.104434	75.164366
249.953772	21.683896	75.169370
249.316433	14.608283	75.174375
248.291196	17.230122	75.179380
247.564126	8.085565	75.184385
246.599239	22.814068	75.189390
246.396701	16.339384	75.194394
245.303342	21.148378	75.199399
244.486575	24.689514	75.204404
244.183869	20.864429	75.209409
243.738200	24.136668	75.214414
243.183824	22.043847	75.219418
242.103410	22.066085	75.224423
241.346691	20.924923	75.229428
241.102380	18.599744	75.234433
240.370082	28.528564	75.239438
239.734154	18.152012	75.244442
238.489826	27.489059	75.249447
237.966191	19.520073	75.254452
237.687862	21.915622	75.259457
237.295673	29.224409	75.264462
236.313174	15.291715	75.269466
235.372739	14.042639	75.274471
234.649486	25.102320	75.279476
234.785347	13.659686	75.284481
233.683967	24.603014	75.289486
232.766721	12.894568	75.294490
232.446092	19.013906	75.299495
231.723741	17.638601	75.304500
231.336908	19.322861	75.309505
230.189119	22.989310	75.314510
229.718050	21.685919	75.319514
229.093856	24.417312	75.324519
227.818250	23.374638	75.329524
227.235059	20.679259	75.334529
226.362893	19.600663	75.339534
226.231063	20.641850	75.344538
225.927382	17.124444	75.349543
225.490371	20.925185	75.354548
224.576047	17.197600	75.359553
223.553304	24.950692	75.364558
223.352141	18.912627	75.369562
222.452810	17.135009	75.374567
221.786227	29.923543	75.379572
221.030181	16.845777	75.384577
220.318013	14.923202	75.389582
219.767993	10.073056	75.394586
219.525991	20.329012	75.399591
218.478534	19.994330	75.404596
217.847666	13.199984	75.409601
217.304438	21.486945	75.414606
216.349154	14.599227	75.419610
215.441710	11.632253	75.424615
214.789714	14.692946	75.429620
214.745770	13.201617	75.434625
214.111554	20.132649	75.439630
213.214060	15.665915	75.444634
212.620163	16.965273	75.449639
211.699159	19.796026	75.454644
211.347938	16.896509	75.459649
210.200374	16.784380	75.464654
209.844077	12.956806	75.469658
209.101815	16.060277	75.474663
208.555379	13.243923	75.479668
208.180563	14.069945	75.484673
207.150360	24.691261	75.489678
206.680779	8.935788	75.494682
206.281959	20.267040	75.499687
205.421347	21.602611	75.504692
204.546037	15.646787	75.509697
203.154251	19.733783	75.514702
203.205331	14.726312	75.519706
202.634733	15.288642	75.524711
202.184516	15.804973	75.529716
201.459016	14.520070	75.534721
200.605588	18.571710	75.539726
200.037499	19.045327	75.544730
199.057498	17.763148	75.549735
198.470536	24.666150	75.554740
197.793094	12.198793	75.559745
197.134064	21.119257	75.564750
197.198505	18.041510	75.569754
196.136378	14.328037	75.574759
195.177690	21.451154	75.579764
194.823520	23.084479	75.584769
194.010380	20.364263	75.589774
193.124424	19.563856	75.594778
192.246557	20.067936	75.599783
191.598631	23.293575	75.604788
191.492739	18.348976	75.609793
190.895555	22.310881	75.614798
190.476004	20.772194	75.619802
189.377713	17.728416	75.624807
188.526973	26.446047	75.629812
188.392233	19.634118	75.634817
187.611505	28.227044	75.639822
186.707625	12.763171	75.644826
185.951311	13.946496	75.649831
185.778993	23.421757	75.654836
184.695952	28.126626	75.659841
183.515166	25.726810	75.664846
183.002468	16.298928	75.669850
182.622001	19.636478	75.674855
182.147692	28.423416	75.679860
182.284053	14.914803	75.684865
180.805775	27.214550	75.689870
180.422621	24.779042	75.694874
179.817676	19.633294	75.699879
178.280292	19.286846	75.704884
177.911742	18.139017	75.709889
176.884040	19.162176	75.714894
176.953427	15.966941	75.719898
176.837189	19.325447	75.724903
175.617489	20.560573	75.729908
175.220734	21.509952	75.734913
174.039544	24.776456	75.739918
173.390980	22.943107	75.744922
172.493670	26.003496	75.749927
171.820223	16.306341	75.754932
171.731286	20.187221	75.759937
170.783381	30.945250	75.764942
170.419538	17.770283	75.769946
169.464618	15.768149	75.774951
168.994182	19.987406	75.779956
168.195997	9.627293	75.784961
167.877793	17.230227	75.789966
167.290767	15.814443	75.794970
166.281495	18.597779	75.799975
165.538225	14.973841	75.804980
164.899064	19.894965	75.809985
164.087118	18.103438	75.814990
163.400720	14.546130	75.819994
163.226686	11.883313	75.824999
162.569908	15.184488	75.830004
161.548132	17.261737	75.835009
160.366750	28.391319	75.840014
159.884153	15.367760	75.845018
159.795904	12.058881	75.850023
159.271431	18.147642	75.855028
158.889131	14.511889	75.860033
157.553712	17.664209	75.865038
156.936836	17.205709	75.870042
156.721092	14.939067	75.875047
155.602685	26.784040	75.880052
154.780009	10.545537	75.885057
153.896543	19.916547	75.890062
153.703101	9.729694	75.895066
153.434462	14.949729	75.900071
152.452540	13.401359	75.905076
151.570541	19.338957	75.910081
151.077795	24.205201	75.915086
150.865939	9.903675	75.920090
149.579354	9.386366	75.925095
148.797952	11.953597	75.930100
148.423822	13.225816	75.935105
147.798963	18.769164	75.940110
147.292728	8.378283	75.945114
146.344312	16.477530	75.950119
145.513249	11.803106	75.955124
145.069672	13.632048	75.960129
144.424874	22.316853	75.965134
144.083873	21.440616	75.970138
142.941650	19.037828	75.975143
142.314877	21.362779	75.980148
142.167396	19.148335	75.985153
141.356231	25.005256	75.990158
140.568058	19.431397	75.995162
139.792770	22.664738	76.000167
139.459538	22.351838	76.005172
138.499330	16.382769	76.010177
137.539614	28.150404	76.015182
136.851982	26.670240	76.020186
136.472567	26.148651	76.025191
135.999874	25.343877	76.030196
135.628730	15.989639	76.035201
134.331694	21.678013	76.040206
133.702834	16.143415	76.045210
133.429803	21.920842	76.050215
132.378647	19.593430	76.055220
131.761088	14.189501	76.060225
130.956890	19.436581	76.065230
130.586414	20.173610	76.070234
130.067925	19.830322	76.075239
129.438795	19.660801	76.080244
128.868527	21.431095	76.085249
127.905892	26.643514	76.090254
127.552030	20.691314	76.095258
126.699209	25.766369	76.100263
125.592782	32.152944	76.105268
125.163616	15.941597	76.110273
124.480423	21.375975	76.115278
124.208780	17.691043	76.120282
123.785156	11.559152	76.125287
123.104274	22.123216	76.130292
122.484867	14.658415	76.135297
120.892172	19.083431	76.140302
120.086974	14.862229	76.145306
119.704447	11.742206	76.150311
119.128002	19.241233	76.155316
118.968592	12.977323	76.160321
118.462106	26.528851	76.165326
117.733484	19.584534	76.170330
117.025693	20.484164	76.175335
116.414698	15.091810	76.180340
115.507917	15.844966	76.185345
114.493299	28.551805	76.190350
114.094154	27.240123	76.195354
113.748132	21.778707	76.200359
112.136724	27.627612	76.205364
111.851343	16.477668	76.210369
111.078261	27.703019	76.215374
110.787028	21.729797	76.220378
110.420726	23.614236	76.225383
109.482263	24.415026	76.230388
108.604990	18.696107	76.235393
107.910414	25.501161	76.240398
107.510613	21.519685	76.245402
107.108890	27.839631	76.250407
106.225812	21.091842	76.255412
105.253933	24.552092	76.260417
104.818063	23.523824	76.265422
104.613223	19.637423	76.270426
103.347055	15.948644	76.275431
102.127374	21.864405	76.280436
101.844836	19.983751	76.285441
101.585397	31.117741	76.290446
101.374338	26.812842	76.295450
100.460434	31.126482	76.300455
99.434351	28.139043	76.305460
99.020787	17.965217	76.310465
98.261968	21.232214	76.315470
97.405849	29.125945	76.320474
96.561614	21.482525	76.325479
95.701386	24.538604	76.330484
95.956583	19.202106	76.335489
95.183630	31.602324	76.340494
94.503782	26.045902	76.345498
93.761578	21.412521	76.350503
93.055956	25.374391	76.355508
92.652188	18.852967	76.360513
91.075796	26.199203	76.365518
90.579885	25.117430	76.370522
90.196603	22.036958	76.375527
89.753843	24.138604	76.380532
89.521622	17.457357	76.385537
88.335439	24.512702	76.390542
87.636228	17.573170	76.395546
87.348554	16.133326	76.400551
86.164443	16.386644	76.405556
85.191407	16.898052	76.410561
84.480259	20.682600	76.415566
84.004816	21.862170	76.420570
83.794096	24.472466	76.425575
83.190433	25.437506	76.430580
83.019560	18.144054	76.435585
81.727288	23.543098	76.440590
81.098203	21.189406	76.445594
80.615502	25.997286	76.450599
79.612719	31.020574	76.455604
79.022483	20.286694	76.460609
77.924990	28.504362	76.465614
77.652688	22.269495	76.470618
77.430543	16.356230	76.475623
76.093872	21.410680	76.480628
75.615069	17.880222	76.485633
75.162124	21.945311	76.490638
74.698766	25.789701	76.495642
74.137938	20.996511	76.500647
72.769041	26.925043	76.505652
72.559931	13.581925	76.510657
72.246507	20.436594	76.515662
71.468751	19.395041	76.520666
70.480792	22.985605	76.525671
69.861244	22.262614	76.530676
69.609050	20.050681	76.535681
68.409405	15.769392	76.540686
67.818008	19.178441	76.545690
67.276570	21.975523	76.550695
66.279417	29.697779	76.555700
65.495740	16.756960	76.560705
64.706484	29.506727	76.565710
63.779131	20.116619	76.570714
63.591043	18.022203	76.575719
63.314771	20.308625	76.580724
63.119829	21.216375	76.585729
62.280943	20.569366	76.590734
61.305047	20.754797	76.595738
60.774039	17.634808	76.600743
59.911002	30.219716	76.605748
58.920827	20.066887	76.610753
58.025329	20.316772	76.615758
57.548078	21.917700	76.620762
57.187119	23.312416	76.625767
56.798752	33.006645	76.630772
56.854563	19.518770	76.635777
55.355620	29.536769	76.640782
54.582614	18.985018	76.645786
54.275888	24.368837	76.650791
52.827149	30.974040	76.655796
52.347530	16.499182	76.660801
51.704539	25.579548	76.665806
51.536049	20.890960	76.670810
51.077001	24.482343	76.675815
49.831046	26.628505	76.680820
49.309862	17.307678	76.685825
48.324342	23.605608	76.690830
48.134126	23.538006	76.695834
47.923775	29.366949	76.700839
46.919544	20.957401	76.705844
46.347728	14.532179	76.710849
45.538297	21.103237	76.715854
44.551860	12.834367	76.720858
43.728404	22.213183	76.725863
43.023557	25.400624	76.730868
42.892533	14.416901	76.735873
42.157749	21.130603	76.740878
41.176246	14.037405	76.745882
40.748522	14.521791	76.750887
40.089055	16.656428	76.755892
39.665357	13.506715	76.760897
38.981281	22.172569	76.765902
38.111876	10.161691	76.770906
37.269753	19.581333	76.775911
36.476124	18.289999	76.780916
36.180603	25.215937	76.785921
35.483379	30.449139	76.790926
34.837060	29.929131	76.795930
34.537166	21.337870	76.800935
33.708147	20.780765	76.805940
33.091576	19.497466	76.810945
31.651450	33.089091	76.815950
31.195064	30.288381	76.820954
30.859788	23.639346	76.825959
30.299576	25.578377	76.830964
29.933492	22.545637	76.835969
28.622119	26.903765	76.840974
28.160748	24.289940	76.845978
27.886450	22.467909	76.850983
27.006439	27.869042	76.855988
26.125770	18.279112	76.860993
25.486469	34.264677	76.865998
25.050286	19.341331	76.871002
24.401702	27.252446	76.876007
23.533697	25.570837	76.881012
23.106460	20.481954	76.886017
22.428217	26.588954	76.891022
21.173545	27.585295	76.896026
20.656178	21.266517	76.901031
20.036689	23.265468	76.906036
19.800913	18.467762	76.911041
19.190429	22.824501	76.916046
18.556656	23.102047	76.921050
17.468457	17.990844	76.926055
16.941275	16.721679	76.931060
16.855159	11.556316	76.936065
15.558939	18.990376	76.941070
14.832701	15.442623	76.946074
14.424260	20.057310	76.951079
13.772918	24.843209	76.956084
13.337841	11.995060	76.961089
12.081222	22.223595	76.966094
11.612979	21.496988	76.971098
11.030405	20.531562	76.976103
10.199722	23.948824	76.981108
9.269495	15.801897	76.986113
8.533994	16.500964	76.991118
8.076757	23.722365	76.996122
7.762389	23.622527	77.001127
7.385802	24.294313	77.006132
7.291325	17.043883	77.011137
6.000545	27.448192	77.016142
5.315185	17.404478	77.021147
4.722206	18.714778	77.026151
3.311329	24.128045	77.031156
3.100764	15.623476	77.036161