Fri Mar 05 17:50:46 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-2.306076	92.166746	0.000000
-2.665676	82.358470	0.005005
-3.319006	57.962227	0.010010
-5.113075	25.996905	0.015014
-8.079339	-23.876095	0.020019
-13.346130	-37.498549	0.025024
-18.950796	-31.814859	0.030029
-23.513923	-29.989097	0.035034
-28.063276	-29.034459	0.040038
-31.771503	-37.324420	0.045043
-35.394575	-34.894778	0.050048
-38.940723	-30.286924	0.055053
-42.426152	-42.187504	0.060058
-46.051616	-33.231769	0.065062
-50.075074	-28.801656	0.070067
-53.452930	-38.986240	0.075072
-57.520660	-33.837819	0.080077
-61.151973	-38.873998	0.085082
-65.021491	-39.762465	0.090086
-69.001259	-30.280222	0.095091
-72.597553	-40.980306	0.100096
-76.451836	-24.938756	0.105101
-79.849034	-34.453139	0.110106
-84.017165	-31.569023	0.115110
-87.879869	-29.443284	0.120115
-91.547987	-33.040038	0.125120
-95.428168	-27.566647	0.130125
-98.647874	-38.588559	0.135130
-102.412429	-38.847136	0.140134
-106.349754	-29.038856	0.145139
-109.804427	-28.108905	0.150144
-113.966907	-28.680882	0.155149
-117.877092	-26.153266	0.160154
-121.708814	-20.121415	0.165158
-125.280371	-22.962365	0.170163
-128.627369	-43.716189	0.175168
-132.736447	-25.569592	0.180173
-136.690583	-28.450408	0.185178
-140.540542	-33.475234	0.190182
-144.682177	-29.633262	0.195187
-148.441338	-33.649079	0.200192
-152.072449	-27.876286	0.205197
-155.689170	-28.946877	0.210202
-159.542182	-22.351732	0.215206
-163.164967	-20.101725	0.220211
-166.404927	-32.531741	0.225216
-170.575403	-28.212019	0.230221
-174.150711	-36.980294	0.235226
-177.920047	-24.331697	0.240230
-181.924658	-23.993579	0.245235
-185.010487	-33.592186	0.250240
-189.239517	-26.052285	0.255245
-192.994817	-27.862404	0.260250
-196.671190	-35.587879	0.265254
-200.677672	-30.335453	0.270259
-204.448123	-32.144712	0.275264
-208.179959	-21.981122	0.280269
-212.159964	-30.418239	0.285274
-215.814393	-33.588036	0.290278
-219.465808	-41.173945	0.295283
-222.642048	-34.599982	0.300288
-226.548278	-25.881466	0.305293
-230.426613	-33.350718	0.310298
-234.655564	-29.934647	0.315302
-238.626798	-28.269185	0.320307
-241.983409	-42.500336	0.325312
-245.964486	-20.658551	0.330317
-249.184111	-36.199983	0.335322
-253.260123	-30.521621	0.340326
-257.140822	-34.472131	0.345331
-260.483136	-31.430932	0.350336
-264.536309	-32.707672	0.355341
-268.361501	-29.010623	0.360346
-272.254717	-26.897070	0.365350
-275.896631	-30.516644	0.370355
-279.311376	-27.996887	0.375360
-283.421554	-16.020731	0.380365
-287.040609	-25.456814	0.385370
-290.704954	-30.235043	0.390374
-294.771902	-27.748356	0.395379
-298.389810	-29.826254	0.400384
-302.226487	-29.454816	0.405389
-305.694993	-29.525359	0.410394
-309.491148	-23.662909	0.415398
-313.683928	-31.824599	0.420403
-317.217808	-27.311351	0.425408
-321.052141	-25.975125	0.430413
-324.871415	-27.566657	0.435418
-328.618561	-32.274835	0.440422
-331.986179	-26.400337	0.445427
-335.763702	-31.616184	0.450432
-339.858766	-20.195886	0.455437
-343.165662	-28.251360	0.460442
-347.330993	-23.405437	0.465446
-351.410403	-25.307070	0.470451
-354.914909	-25.586268	0.475456
-358.888901	-25.429369	0.480461
-362.160000	-26.624216	0.485466
-366.137485	-19.616205	0.490470
-369.808291	-28.567631	0.495475
-373.350069	-29.553660	0.500480
-377.704933	-23.198188	0.505485
-381.218554	-30.797959	0.510490
-384.950057	-33.400078	0.515494
-388.943561	-24.500215	0.520499
-392.396408	-30.098982	0.525504
-396.248237	-26.085232	0.530509
-399.774885	-27.988304	0.535514
-403.700178	-25.678601	0.540518
-407.407258	-26.141426	0.545523
-410.899616	-35.206434	0.550528
-415.340071	-26.648340	0.555533
-418.952571	-29.502805	0.560538
-422.720380	-27.226104	0.565542
-426.405786	-25.240108	0.570547
-430.111577	-32.858003	0.575552
-433.651318	-25.878785	0.580557
-437.400126	-36.981298	0.585562
-441.267773	-27.965830	0.590566
-445.478804	-26.821575	0.595571
-448.677660	-32.041330	0.600576
-452.722321	-26.474883	0.605581
-456.303398	-39.692110	0.610586
-460.071772	-31.261769	0.615590
-464.009385	-28.522631	0.620595
-467.660633	-28.536946	0.625600
-471.619536	-27.674192	0.630605
-475.257027	-29.747113	0.635610
-478.924801	-22.720574	0.640614
-482.925927	-25.090238	0.645619
-486.029272	-33.305744	0.650624
-490.250040	-26.339112	0.655629
-493.934030	-24.892577	0.660634
-497.963476	-27.984693	0.665638
-501.423178	-31.213531	0.670643
-505.336825	-33.385807	0.675648
-509.157389	-36.093356	0.680653
-512.730905	-39.989995	0.685658
-516.286986	-34.462057	0.690662
-520.346409	-26.797297	0.695667
-524.377877	-42.839438	0.700672
-527.935108	-31.403825	0.705677
-531.804298	-29.598057	0.710682
-535.432347	-34.861104	0.715686
-539.471011	-36.839883	0.720691
-542.828640	-28.181701	0.725696
-546.370321	-26.021354	0.730701
-550.045389	-34.500275	0.735706
-554.019952	-35.716534	0.740710
-557.994599	-37.856899	0.745715
-561.490636	-48.868678	0.750720
-565.836414	-34.643490	0.755725
-569.303319	-29.194376	0.760730
-573.151183	-35.723282	0.765734
-576.964140	-33.456475	0.770739
-580.098260	-23.687462	0.775744
-584.133159	-21.924525	0.780749
-588.009730	-34.741085	0.785754
-591.870465	-33.244087	0.790758
-595.724938	-29.992874	0.795763
-599.235992	-21.658623	0.800768
-603.093709	-20.546878	0.805773
-607.080767	-31.166330	0.810778
-610.968457	-29.803772	0.815782
-614.781004	-28.965739	0.820787
-617.931986	-42.716626	0.825792
-621.897235	-29.124587	0.830797
-625.369477	-31.808745	0.835802
-629.599459	-33.671645	0.840806
-633.238690	-22.839391	0.845811
-636.640878	-36.523312	0.850816
-640.688193	-31.776178	0.855821
-644.304176	-23.734194	0.860826
-648.143917	-33.107616	0.865830
-652.326556	-28.130675	0.870835
-656.128159	-32.227203	0.875840
-659.957602	-29.631191	0.880845
-663.221384	-34.354552	0.885850
-666.758286	-28.398937	0.890854
-670.979036	-26.254487	0.895859
-674.465106	-35.531403	0.900864
-678.289881	-26.907212	0.905869
-682.016228	-35.712046	0.910874
-685.790261	-27.422392	0.915878
-689.688464	-26.281960	0.920883
-693.429250	-27.470683	0.925888
-697.175412	-19.122381	0.930893
-700.880535	-35.919692	0.935898
-704.455811	-26.827534	0.940902
-708.563514	-34.357090	0.945907
-712.291963	-27.613838	0.950912
-716.055685	-31.173830	0.955917
-719.791883	-30.803585	0.960922
-723.724805	-28.373867	0.965926
-727.316243	-33.180398	0.970931
-730.979728	-33.126117	0.975936
-734.643011	-36.910293	0.980941
-738.123952	-26.822304	0.985946
-742.428451	-36.849862	0.990950
-745.965161	-32.874884	0.995955
-749.724133	-43.398052	1.000960
-753.434300	-30.641390	1.005965
-757.235588	-32.012736	1.010970
-761.311534	-40.923992	1.015974
-765.093026	-35.086848	1.020979
-768.714315	-40.858398	1.025984
-772.531089	-34.063093	1.030989
-776.037389	-40.539006	1.035994
-779.731572	-42.277527	1.040998
-783.722038	-38.381363	1.046003
-787.338920	-32.852778	1.051008
-791.408374	-35.441232	1.056013
-794.908376	-35.953895	1.061018
-798.599878	-29.892954	1.066022
-802.402848	-30.415529	1.071027
-806.147242	-38.461883	1.076032
-810.289364	-24.626809	1.081037
-813.726586	-26.161916	1.086042
-817.481337	-26.622786	1.091046
-821.212101	-33.791328	1.096051
-824.824383	-34.891568	1.101056
-829.193416	-23.863527	1.106061
-832.914371	-33.108956	1.111066
-836.299767	-23.860877	1.116070
-839.831621	-27.090290	1.121075
-843.503571	-34.003260	1.126080
-847.748190	-21.460650	1.131085
-851.394382	-33.914586	1.136090
-855.429718	-31.159188	1.141094
-859.134244	-18.739168	1.146099
-862.432290	-29.099289	1.151104
-866.217697	-31.321423	1.156109
-869.942953	-34.904659	1.161114
-873.799462	-29.722424	1.166118
-877.800997	-30.489108	1.171123
-881.574917	-27.346513	1.176128
-885.384256	-36.653416	1.181133
-888.824550	-29.312551	1.186138
-892.655720	-28.540482	1.191142
-896.451202	-22.760821	1.196147
-900.332035	-33.538653	1.201152
-904.273605	-26.975509	1.206157
-907.647503	-28.668840	1.211162
-911.732067	-26.001672	1.216166
-915.619049	-23.090112	1.221171
-918.813316	-29.000666	1.226176
-922.934365	-18.379550	1.231181
-926.819454	-22.738259	1.236186
-929.906555	-26.188462	1.241190
-934.173662	-21.948182	1.246195
-937.764934	-29.287074	1.251200
-941.617629	-28.073078	1.256205
-945.498735	-25.353226	1.261210
-949.335888	-28.940520	1.266214
-953.218489	-22.378839	1.271219
-956.433207	-32.704828	1.276224
-960.351164	-36.042630	1.281229
-964.039905	-39.350843	1.286234
-967.894308	-33.143747	1.291238
-971.682040	-25.974294	1.296243
-975.479739	-32.972598	1.301248
-979.213947	-26.841475	1.306253
-983.008217	-30.115437	1.311258
-986.736333	-27.981397	1.316262
-990.868922	-29.733056	1.321267
-994.201398	-28.237880	1.326272
-998.213144	-25.094915	1.331277
-1001.695120	-27.344852	1.336282
-1005.633521	-36.878497	1.341286
-1009.136393	-32.918007	1.346291
-1012.903153	-37.309680	1.351296
-1017.168664	-28.909383	1.356301
-1020.916263	-33.778786	1.361306
-1024.672492	-30.312356	1.366310
-1028.376055	-41.497574	1.371315
-1031.693506	-39.239905	1.376320
-1035.412498	-27.969323	1.381325
-1039.389738	-32.268940	1.386330
-1043.309175	-30.794937	1.391334
-1046.956187	-25.106600	1.396339
-1050.544291	-30.062968	1.401344
-1054.470684	-29.795815	1.406349
-1058.158749	-33.751345	1.411354
-1062.090738	-32.009578	1.416358
-1066.239083	-20.958073	1.421363
-1069.567215	-31.690755	1.426368
-1073.542851	-30.702101	1.431373
-1076.677007	-38.456879	1.436378
-1080.621887	-34.715751	1.441382
-1084.472121	-28.356955	1.446387
-1088.534563	-37.306831	1.451392
-1092.408034	-24.795586	1.456397
-1095.931550	-31.343155	1.461402
-1099.284287	-28.143008	1.466406
-1103.440997	-25.895279	1.471411
-1106.799010	-26.658064	1.476416
-1111.067863	-21.993765	1.481421
-1114.584423	-23.607200	1.486426
-1118.269050	-20.371278	1.491430
-1122.333530	-22.171445	1.496435
-1125.649454	-33.281317	1.501440
-1129.851366	-26.190445	1.506445
-1133.524984	-26.723711	1.511450
-1137.493009	-30.611458	1.516454
-1141.235210	-18.777166	1.521459
-1144.432182	-32.985919	1.526464
-1148.111231	-32.010683	1.531469
-1152.176239	-34.036222	1.536474
-1156.030625	-34.081625	1.541478
-1160.296248	-28.169564	1.546483
-1163.973450	-31.758430	1.551488
-1167.562494	-26.689485	1.556493
-1170.739428	-32.301242	1.561498
-1174.248001	-33.753431	1.566502
-1178.834302	-23.558943	1.571507
-1182.659661	-24.741231	1.576512
-1186.637147	-27.920883	1.581517
-1190.220735	-31.387487	1.586522
-1193.582437	-30.486612	1.591526
-1197.016917	-36.728922	1.596531
-1200.426953	-35.790340	1.601536
-1204.716218	-22.442028	1.606541
-1209.208563	-26.856051	1.611546
-1212.004145	-29.614480	1.616550
-1216.578274	-27.257968	1.621555
-1220.148606	-26.284245	1.626560
-1224.001643	-27.739587	1.631565
-1227.382737	-26.723593	1.636570
-1231.101139	-29.861045	1.641574
-1235.336338	-29.558364	1.646579
-1238.768223	-38.041936	1.651584
-1242.945888	-27.832296	1.656589
-1246.370092	-26.837762	1.661594
-1249.709972	-32.297170	1.666598
-1253.802552	-29.296961	1.671603
-1257.545775	-42.622518	1.676608
-1261.158722	-32.876972	1.681613
-1265.270138	-35.052583	1.686618
-1268.640217	-31.945619	1.691622
-1272.748153	-37.807211	1.696627
-1276.310575	-45.229011	1.701632
-1280.476610	-32.436478	1.706637
-1284.262943	-34.325028	1.711642
-1287.389454	-32.427150	1.716646
-1291.339770	-30.258643	1.721651
-1295.130989	-36.494169	1.726656
-1298.938851	-32.023959	1.731661
-1302.769747	-35.302563	1.736666
-1306.604904	-30.728621	1.741670
-1310.389051	-29.865621	1.746675
-1313.685808	-32.073763	1.751680
-1317.661487	-22.055599	1.756685
-1321.696892	-30.227974	1.761690
-1325.124262	-32.259070	1.766694
-1329.131068	-21.023196	1.771699
-1332.883744	-32.587188	1.776704
-1336.653540	-21.714101	1.781709
-1340.515074	-23.338202	1.786714
-1344.224158	-30.730116	1.791718
-1347.671750	-25.667773	1.796723
-1351.355377	-32.179054	1.801728
-1355.493118	-19.431917	1.806733
-1359.267668	-23.583642	1.811738
-1362.953540	-29.854842	1.816742
-1366.946494	-28.031052	1.821747
-1370.199548	-25.769020	1.826752
-1374.090704	-22.550103	1.831757
-1378.061508	-26.861194	1.836762
-1381.808014	-29.697424	1.841766
-1385.608433	-19.148950	1.846771
-1389.045580	-30.668738	1.851776
-1392.879677	-21.338610	1.856781
-1396.518883	-22.269639	1.861786
-1400.518735	-32.855629	1.866790
-1404.392640	-28.702690	1.871795
-1407.901005	-39.122913	1.876800
-1411.777347	-29.716609	1.881805
-1415.445966	-31.715253	1.886810
-1419.042457	-35.272469	1.891814
-1423.392487	-32.467295	1.896819
-1427.032068	-40.065737	1.901824
-1430.565812	-29.421123	1.906829
-1434.318503	-32.770374	1.911834
-1438.107149	-31.583162	1.916838
-1442.128692	-28.098823	1.921843
-1445.470369	-37.750870	1.926848
-1449.548984	-24.429561	1.931853
-1453.513065	-26.809778	1.936858
-1456.852801	-26.728921	1.941862
-1460.645677	-29.114460	1.946867
-1464.330713	-29.765222	1.951872
-1468.062369	-28.043023	1.956877
-1471.943792	-28.939877	1.961882
-1475.910463	-31.225019	1.966886
-1479.790909	-27.130835	1.971891
-1483.077088	-36.290227	1.976896
-1486.844448	-27.282887	1.981901
-1490.437843	-28.809319	1.986906
-1494.456572	-34.413544	1.991910
-1498.582900	-27.050276	1.996915
-1502.348210	-32.696711	2.006912
-1503.113624	-29.748740	2.016909
-1500.564494	-23.093492	2.026906
-1497.785896	-26.451183	2.036902
-1495.460253	-35.736576	2.046899
-1493.963367	-28.355429	2.056896
-1492.252436	-28.450435	2.066893
-1489.951540	-31.891098	2.076890
-1487.806393	-29.257627	2.086886
-1486.227958	-35.205333	2.096883
-1484.397499	-31.531427	2.106880
-1482.178906	-26.269603	2.116877
-1480.214514	-22.366075	2.126874
-1478.647880	-26.194435	2.136870
-1476.588218	-30.764926	2.146867
-1474.849241	-28.958543	2.156864
-1472.968275	-26.936465	2.166861
-1471.102962	-30.515791	2.176858
-1469.061877	-33.670084	2.186854
-1467.238301	-30.205070	2.196851
-1465.266851	-29.305941	2.206848
-1463.413714	-25.278790	2.216845
-1461.561657	-28.139115	2.226842
-1459.721268	-27.961130	2.236838
-1457.754176	-30.070893	2.246835
-1455.816977	-25.997194	2.256832
-1454.115535	-32.962512	2.266829
-1452.106109	-28.117186	2.276826
-1450.396805	-26.119709	2.286822
-1448.545536	-28.724098	2.296819
-1446.235486	-33.830463	2.306816
-1444.611009	-34.121601	2.316813
-1442.691323	-25.235415	2.326810
-1440.676779	-22.975739	2.336806
-1438.966492	-24.684354	2.346803
-1437.079462	-27.378148	2.356800
-1435.209590	-19.939825	2.366797
-1433.162300	-23.061925	2.376794
-1431.431549	-23.805876	2.386790
-1429.968708	-19.995690	2.396787
-1427.808373	-29.055603	2.406784
-1425.475437	-27.884302	2.416781
-1423.813547	-25.716576	2.426778
-1422.010279	-23.547798	2.436774
-1419.966805	-25.462909	2.446771
-1418.250365	-27.507244	2.456768
-1416.431719	-26.488867	2.466765
-1414.479573	-28.199869	2.476762
-1412.730922	-25.082827	2.486758
-1410.583867	-22.149573	2.496755
-1408.871787	-21.069916	2.506752
-1407.257594	-24.643728	2.516749
-1405.178964	-24.388574	2.526746
-1403.168010	-28.035378	2.536742
-1401.741133	-20.655583	2.546739
-1399.195119	-27.018682	2.556736
-1397.401613	-24.221453	2.566733
-1395.775987	-33.882603	2.576730
-1394.041255	-25.203614	2.586726
-1391.696873	-22.079292	2.596723
-1389.991337	-24.167653	2.606720
-1388.361831	-24.876416	2.616717
-1386.290164	-23.399552	2.626714
-1384.419243	-22.545840	2.636710
-1382.550854	-22.711764	2.646707
-1380.509438	-29.126699	2.656704
-1378.958927	-22.597243	2.666701
-1376.914237	-26.539964	2.676698
-1374.904011	-21.066244	2.686694
-1373.121102	-24.960740	2.696691
-1371.210226	-25.585054	2.706688
-1369.508232	-31.689844	2.716685
-1367.464578	-21.590222	2.726682
-1365.540294	-26.484753	2.736678
-1363.926862	-23.183388	2.746675
-1361.798099	-20.681387	2.756672
-1360.101899	-28.839542	2.766669
-1358.274330	-22.946551	2.776666
-1356.472091	-21.492849	2.786662
-1354.466167	-27.382587	2.796659
-1352.397449	-23.058258	2.806656
-1350.631904	-22.212914	2.816653
-1348.707752	-22.851967	2.826650
-1347.007074	-19.163485	2.836646
-1345.242430	-15.616297	2.846643
-1343.054664	-16.318070	2.856640
-1341.097231	-20.674709	2.866637
-1339.448832	-22.125441	2.876634
-1337.468889	-23.763458	2.886630
-1335.646387	-21.951388	2.896627
-1333.708852	-27.831742	2.906624
-1331.927722	-25.716193	2.916621
-1329.996248	-28.450176	2.926618
-1327.984180	-19.753938	2.936614
-1326.388078	-20.098874	2.946611
-1324.132176	-21.893161	2.956608
-1322.362833	-20.088362	2.966605
-1320.857173	-30.275028	2.976602
-1318.581181	-24.390619	2.986598
-1316.766330	-30.178687	2.996595
-1314.982979	-22.497453	3.006592
-1312.806054	-28.043459	3.016589
-1311.532948	-29.910964	3.026586
-1309.577358	-27.074869	3.036582
-1307.513653	-21.407532	3.046579
-1305.556950	-23.837626	3.056576
-1303.520794	-25.333026	3.066573
-1301.872812	-21.746606	3.076570
-1299.964180	-21.040972	3.086566
-1297.984932	-24.381023	3.096563
-1296.403203	-17.084360	3.106560
-1294.394177	-23.806689	3.116557
-1292.209654	-21.960944	3.126554
-1290.402356	-23.092848	3.136550
-1288.789750	-22.009811	3.146547
-1286.894711	-17.566039	3.156544
-1284.885486	-23.140448	3.166541
-1282.985483	-23.680841	3.176538
-1281.274231	-21.217738	3.186534
-1279.158677	-19.905701	3.196531
-1277.209281	-19.190782	3.206528
-1275.599604	-25.670754	3.216525
-1273.696168	-20.178270	3.226522
-1271.721721	-18.082557	3.236518
-1269.870086	-16.113248	3.246515
-1267.846577	-17.196839	3.256512
-1266.179132	-22.801801	3.266509
-1264.440615	-23.324231	3.276506
-1262.646100	-15.527098	3.286502
-1260.652350	-24.041509	3.296499
-1258.810468	-19.306562	3.306496
-1256.833164	-22.420469	3.316493
-1254.691102	-21.448983	3.326490
-1252.786287	-18.802877	3.336486
-1251.318842	-27.458852	3.346483
-1249.019715	-27.799394	3.356480
-1247.395344	-24.149153	3.366477
-1245.525374	-24.918404	3.376474
-1243.552516	-27.115759	3.386470
-1241.927960	-27.316763	3.396467
-1239.998181	-26.664992	3.406464
-1237.853691	-20.370225	3.416461
-1236.279456	-22.659318	3.426458
-1234.419358	-19.259166	3.436454
-1232.446613	-23.478425	3.446451
-1230.379571	-27.119850	3.456448
-1228.523783	-24.414561	3.466445
-1226.870238	-24.125962	3.476442
-1224.840941	-23.149825	3.486438
-1222.801334	-23.038269	3.496435
-1221.199977	-20.789649	3.506432
-1219.231651	-19.234515	3.516429
-1217.292732	-23.335449	3.526426
-1215.423044	-23.018268	3.536422
-1213.651827	-25.466766	3.546419
-1211.702654	-24.139887	3.556416
-1209.971348	-31.012715	3.566413
-1208.233869	-22.686918	3.576410
-1206.086198	-28.990024	3.586406
-1204.061200	-21.007084	3.596403
-1202.335721	-20.122055	3.606400
-1200.344125	-19.061703	3.616397
-1198.768605	-21.380188	3.626394
-1196.659795	-20.059102	3.636390
-1194.824608	-20.960121	3.646387
-1192.779177	-22.824821	3.656384
-1191.248764	-25.319250	3.666381
-1189.263948	-21.083978	3.676378
-1187.068831	-25.232198	3.686374
-1185.275887	-28.133381	3.696371
-1183.941640	-22.644488	3.706368
-1181.698010	-33.947883	3.716365
-1180.050417	-28.637815	3.726362
-1177.943090	-31.964310	3.736358
-1176.139997	-29.205546	3.746355
-1174.106063	-29.143568	3.756352
-1172.289074	-24.060341	3.766349
-1170.393372	-30.287575	3.776346
-1168.484534	-26.946486	3.786342
-1166.616961	-26.032058	3.796339
-1164.629935	-30.702776	3.806336
-1162.976688	-27.497639	3.816333
-1161.135017	-27.689112	3.826330
-1159.401701	-28.000622	3.836326
-1157.526922	-30.447488	3.846323
-1155.546511	-24.885109	3.856320
-1153.315805	-29.353215	3.866317
-1151.714695	-32.785812	3.876314
-1149.787642	-25.962730	3.886310
-1147.803336	-24.894850	3.896307
-1146.142594	-24.133639	3.906304
-1144.330833	-26.477251	3.916301
-1142.264485	-28.162088	3.926298
-1140.309104	-23.569943	3.936294
-1138.489870	-26.074228	3.946291
-1136.751542	-22.481611	3.956288
-1134.866381	-22.991088	3.966285
-1132.913893	-27.338873	3.976282
-1131.140055	-27.143664	3.986278
-1129.234646	-26.314210	3.996275
-1127.225202	-28.511006	4.006272
-1125.452484	-27.726640	4.016269
-1123.418012	-29.726901	4.026266
-1121.648147	-22.087557	4.036262
-1120.075386	-15.097234	4.046259
-1117.970584	-20.479948	4.056256
-1115.765721	-21.618475	4.066253
-1113.964131	-28.765391	4.076250
-1112.582405	-20.489184	4.086246
-1110.370835	-14.474242	4.096243
-1108.544011	-16.799712	4.106240
-1106.598414	-21.149534	4.116237
-1104.806121	-25.059548	4.126234
-1102.757442	-18.649052	4.136230
-1101.023470	-23.680312	4.146227
-1099.032209	-24.656752	4.156224
-1097.169754	-26.741585	4.166221
-1095.528894	-23.095448	4.176218
-1093.566612	-25.436258	4.186214
-1091.678699	-19.347419	4.196211
-1089.640512	-20.039240	4.206208
-1087.778848	-24.402464	4.216205
-1086.117102	-25.226706	4.226202
-1084.009203	-23.425348	4.236198
-1082.267352	-20.381171	4.246195
-1080.524774	-20.858323	4.256192
-1078.580496	-28.710175	4.266189
-1076.328506	-30.290432	4.276186
-1074.692660	-28.464088	4.286182
-1072.928803	-20.530044	4.296179
-1071.082759	-21.727981	4.306176
-1069.229836	-24.717624	4.316173
-1067.136172	-29.160574	4.326170
-1065.219910	-24.942650	4.336166
-1063.426331	-20.119282	4.346163
-1061.697111	-20.837452	4.356160
-1059.803942	-19.555961	4.366157
-1057.720463	-19.383380	4.376154
-1056.137075	-27.316446	4.386150
-1054.581275	-27.788968	4.396147
-1052.048969	-27.555532	4.406144
-1050.208640	-20.871652	4.416141
-1048.618182	-24.651443	4.426138
-1046.598074	-25.158748	4.436134
-1044.643688	-27.919853	4.446131
-1042.825004	-28.788113	4.456128
-1040.971442	-22.317931	4.466125
-1038.884901	-25.098590	4.476122
-1037.032583	-25.250613	4.486118
-1035.431088	-27.096283	4.496115
-1033.643069	-27.954895	4.506112
-1031.471502	-25.579435	4.516109
-1029.626990	-23.565368	4.526106
-1027.876194	-24.375389	4.536102
-1026.170939	-26.125537	4.546099
-1024.143566	-21.153205	4.556096
-1021.986965	-32.691245	4.566093
-1020.414408	-34.608069	4.576090
-1018.402431	-29.499056	4.586086
-1016.633698	-24.111125	4.596083
-1014.798298	-22.703512	4.606080
-1012.821857	-29.919376	4.616077
-1010.963774	-25.966849	4.626074
-1009.023924	-25.537559	4.636070
-1007.286503	-26.538067	4.646067
-1005.184826	-20.740720	4.656064
-1003.464825	-34.558502	4.666061
-1001.815975	-28.946117	4.676058
-999.822583	-28.395903	4.686054
-997.707916	-29.818329	4.696051
-995.991039	-22.792540	4.706048
-993.907679	-25.803188	4.716045
-991.868931	-22.567990	4.726042
-990.176159	-23.109744	4.736038
-988.744373	-18.687952	4.746035
-986.421898	-27.694479	4.756032
-984.514176	-27.155816	4.766029
-982.820268	-26.818232	4.776026
-981.112851	-28.494480	4.786022
-978.964555	-26.375787	4.796019
-977.214059	-29.385298	4.806016
-975.228159	-29.193881	4.816013
-973.483722	-29.088592	4.826010
-971.610563	-31.160828	4.836006
-969.488873	-37.619847	4.846003
-967.849388	-25.762491	4.856000
-965.702681	-25.816265	4.865997
-964.214908	-30.893326	4.875994
-962.155561	-25.003904	4.885990
-960.358085	-26.386629	4.895987
-958.286710	-25.117762	4.905984
-956.459527	-24.755679	4.915981
-954.850397	-30.529542	4.925978
-952.652466	-29.258801	4.935974
-951.090188	-26.620040	4.945971
-949.378026	-25.030029	4.955968
-947.051031	-27.544306	4.965965
-945.099191	-25.416275	4.975962
-943.546399	-27.922022	4.985958
-941.677873	-22.324187	4.995955
-939.705439	-20.565775	5.005952
-937.490910	-24.402651	5.015949
-935.837468	-23.253262	5.025946
-934.137852	-23.237097	5.035942
-932.065558	-23.957920	5.045939
-930.388903	-25.933965	5.055936
-928.413392	-23.664433	5.065933
-926.535559	-24.469428	5.075930
-924.666908	-28.521000	5.085926
-922.888600	-20.968106	5.095923
-920.798419	-20.262765	5.105920
-918.826199	-22.617654	5.115917
-917.219147	-27.000044	5.125914
-915.349113	-18.201748	5.135910
-913.382983	-23.491062	5.145907
-911.561920	-21.506310	5.155904
-909.566194	-18.717337	5.165901
-907.650109	-18.089943	5.175898
-905.642464	-27.125013	5.185894
-904.432784	-23.916662	5.195891
-902.108838	-25.514577	5.205888
-900.103649	-22.098658	5.215885
-898.524969	-22.468941	5.225882
-896.573603	-20.983453	5.235878
-894.634565	-19.207032	5.245875
-892.561154	-28.045754	5.255872
-890.674206	-27.134201	5.265869
-888.847066	-28.962163	5.275866
-887.001156	-30.925761	5.285862
-885.359975	-26.208944	5.295859
-883.624767	-28.739080	5.305856
-881.394834	-23.753211	5.315853
-879.516467	-26.802044	5.325850
-877.559798	-24.317868	5.335846
-876.043999	-29.784641	5.345843
-874.012162	-24.351812	5.355840
-871.998732	-24.166287	5.365837
-870.358596	-18.809785	5.375834
-868.318344	-23.532992	5.385830
-866.505308	-29.333082	5.395827
-864.787651	-25.787478	5.405824
-862.700195	-28.151269	5.415821
-860.518367	-27.177881	5.425818
-859.154568	-19.613932	5.435814
-856.915111	-23.509987	5.445811
-855.281184	-23.210093	5.455808
-853.125701	-26.386895	5.465805
-851.617640	-23.390433	5.475802
-849.537452	-21.800757	5.485798
-847.781882	-26.189475	5.495795
-846.062887	-19.381807	5.505792
-844.038239	-20.791287	5.515789
-841.865752	-22.405986	5.525786
-840.040789	-27.281078	5.535782
-838.436317	-27.522805	5.545779
-836.479183	-24.814447	5.555776
-834.544429	-22.576215	5.565773
-832.584419	-26.594953	5.575770
-830.699176	-25.480964	5.585766
-828.948409	-24.670756	5.595763
-827.217465	-26.987002	5.605760
-825.116360	-28.223941	5.615757
-823.363350	-29.469976	5.625754
-821.377568	-31.710106	5.635750
-819.589996	-22.538529	5.645747
-817.953325	-25.692373	5.655744
-815.949452	-25.708967	5.665741
-813.717628	-24.301400	5.675738
-811.963643	-25.563372	5.685734
-810.276838	-27.065670	5.695731
-808.249018	-23.838034	5.705728
-806.627305	-25.020436	5.715725
-804.702126	-24.823906	5.725722
-802.451175	-23.823615	5.735718
-800.842397	-27.434064	5.745715
-799.007672	-29.023158	5.755712
-797.003253	-29.428264	5.765709
-795.026792	-31.700042	5.775706
-793.242847	-31.245653	5.785702
-791.859348	-24.183783	5.795699
-789.633156	-24.690649	5.805696
-787.471372	-23.485030	5.815693
-785.828729	-22.783829	5.825690
-783.916502	-27.099642	5.835686
-781.982024	-30.650025	5.845683
-779.895236	-27.548637	5.855680
-778.344602	-22.594624	5.865677
-776.409607	-25.573479	5.875674
-774.630183	-25.266782	5.885670
-772.660025	-27.319630	5.895667
-770.775295	-27.816115	5.905664
-768.551958	-25.917651	5.915661
-766.998144	-28.038168	5.925658
-765.346451	-32.051787	5.935654
-763.651808	-24.843828	5.945651
-761.212536	-30.104426	5.955648
-759.440497	-26.908502	5.965645
-757.654347	-27.834507	5.975642
-755.742343	-28.733253	5.985638
-753.826024	-20.136432	5.995635
-751.837446	-25.021820	6.005632
-750.081652	-29.007855	6.015629
-748.345400	-23.031855	6.025626
-746.384504	-32.600937	6.035622
-744.842814	-30.719834	6.045619
-742.385605	-33.103139	6.055616
-740.790846	-24.205433	6.065613
-738.957528	-26.086377	6.075610
-737.156896	-26.387807	6.085606
-735.242275	-23.419923	6.095603
-733.380990	-24.493714	6.105600
-731.398390	-23.548368	6.115597
-729.365422	-26.275988	6.125594
-727.436297	-29.116491	6.135590
-725.804004	-28.825720	6.145587
-724.020859	-29.430678	6.155584
-721.869501	-24.329456	6.165581
-720.136543	-25.104820	6.175578
-717.970136	-25.482058	6.185574
-716.336918	-27.646813	6.195571
-714.539744	-27.162899	6.205568
-712.902372	-29.404108	6.215565
-710.789061	-31.604524	6.225562
-708.594621	-26.229108	6.235558
-706.988484	-33.949276	6.245555
-705.320254	-26.193866	6.255552
-703.098197	-28.065847	6.265549
-701.275840	-26.084294	6.275546
-699.694660	-24.162098	6.285542
-697.337633	-28.552082	6.295539
-695.861968	-24.223957	6.305536
-693.838673	-27.467923	6.315533
-691.995560	-27.201342	6.325530
-690.107268	-28.885760	6.335526
-688.132056	-31.760440	6.345523
-686.494869	-30.764600	6.355520
-684.622753	-23.821790	6.365517
-682.469568	-26.669638	6.375514
-680.667449	-26.825994	6.385510
-678.812283	-28.543007	6.395507
-677.044206	-28.742870	6.405504
-675.025153	-33.738859	6.415501
-673.337337	-29.195134	6.425498
-671.035908	-27.416428	6.435494
-669.496033	-23.913323	6.445491
-667.690284	-28.071501	6.455488
-665.702649	-32.026622	6.465485
-663.848361	-27.169998	6.475482
-661.962872	-22.768379	6.485478
-659.952475	-26.611865	6.495475
-658.455299	-25.928387	6.505472
-656.433013	-29.238480	6.515469
-654.254413	-32.965144	6.525466
-652.434333	-26.511386	6.535462
-650.618903	-31.441663	6.545459
-648.850473	-27.911901	6.555456
-647.099044	-26.905864	6.565453
-645.056413	-29.998134	6.575450
-643.049394	-27.104939	6.585446
-640.979261	-24.986075	6.595443
-639.531703	-26.366341	6.605440
-637.606062	-34.254363	6.615437
-635.563823	-31.606802	6.625434
-633.723779	-30.385954	6.635430
-632.224201	-34.122539	6.645427
-630.042433	-32.195194	6.655424
-628.080110	-28.960092	6.665421
-626.367622	-37.493032	6.675418
-624.573487	-36.708549	6.685414
-622.427820	-27.917718	6.695411
-620.609687	-31.395701	6.705408
-618.787155	-36.574995	6.715405
-616.931285	-31.887543	6.725402
-615.171620	-25.479367	6.735398
-613.180160	-27.879717	6.745395
-611.324731	-24.867534	6.755392
-609.283908	-29.311133	6.765389
-607.444812	-24.868897	6.775386
-605.754877	-27.154751	6.785382
-603.854244	-30.895388	6.795379
-601.924287	-24.833370	6.805376
-599.901725	-33.414253	6.815373
-598.073683	-29.268681	6.825370
-596.394321	-30.133293	6.835366
-594.486416	-37.299993	6.845363
-592.502781	-29.838053	6.855360
-590.910848	-28.691225	6.865357
-588.730936	-27.846757	6.875354
-586.778997	-28.890704	6.885350
-584.842873	-30.563733	6.895347
-583.363245	-30.336901	6.905344
-581.360196	-28.633605	6.915341
-579.443741	-29.949786	6.925338
-577.702110	-34.880853	6.935334
-575.599146	-27.987460	6.945331
-573.827722	-26.243998	6.955328
-571.750424	-25.949994	6.965325
-569.891296	-32.590965	6.975322
-567.970740	-33.710413	6.985318
-566.246525	-31.738341	6.995315
-564.723681	-22.757954	7.005312
-562.630983	-27.100850	7.015309
-560.451518	-28.572719	7.025306
-558.580736	-31.687995	7.035302
-556.856271	-31.140239	7.045299
-554.895493	-31.313948	7.055296
-553.299015	-25.280728	7.065293
-551.307631	-29.856917	7.075290
-549.645084	-28.991354	7.085286
-547.515715	-25.700755	7.095283
-545.595765	-32.804606	7.105280
-543.780117	-25.996347	7.115277
-541.737214	-32.020830	7.125274
-539.832725	-27.895317	7.135270
-538.202185	-27.605716	7.145267
-536.298160	-25.164947	7.155264
-534.395070	-24.961511	7.165261
-532.574928	-32.123625	7.175258
-530.506321	-32.472440	7.185254
-528.837704	-29.318241	7.195251
-526.471207	-28.667738	7.205248
-525.026150	-29.297498	7.215245
-523.235265	-33.836901	7.225242
-521.591308	-27.688079	7.235238
-519.254265	-29.044546	7.245235
-517.268275	-29.605955	7.255232
-515.843485	-31.421481	7.265229
-513.606780	-29.722287	7.275226
-511.856019	-29.927157	7.285222
-510.028497	-33.016539	7.295219
-508.309545	-26.859157	7.305216
-506.239370	-29.011453	7.315213
-504.062899	-33.173457	7.325210
-502.262066	-27.708131	7.335206
-500.466622	-30.064451	7.345203
-498.635407	-31.115888	7.355200
-497.106705	-29.834154	7.365197
-494.881009	-29.467463	7.375194
-492.996180	-32.747574	7.385190
-491.247244	-29.778289	7.395187
-489.533177	-30.643633	7.405184
-487.364492	-28.759857	7.415181
-485.640427	-32.371147	7.425178
-483.719264	-30.103609	7.435174
-481.819279	-26.522092	7.445171
-479.822497	-27.797336	7.455168
-477.973076	-25.185159	7.465165
-476.224578	-31.115202	7.475162
-474.501023	-27.571822	7.485158
-472.533757	-20.944039	7.495155
-470.665881	-25.181477	7.505152
-468.720189	-22.766255	7.515149
-467.098227	-24.186904	7.525146
-464.692649	-29.304460	7.535142
-462.901221	-28.508368	7.545139
-461.050508	-27.497520	7.555136
-459.454626	-28.716620	7.565133
-457.223464	-27.048067	7.575130
-455.635106	-26.661668	7.585126
-453.715704	-26.001275	7.595123
-451.752498	-23.852534	7.605120
-450.038439	-27.637476	7.615117
-447.990999	-28.497604	7.625114
-446.305317	-24.971839	7.635110
-444.216950	-33.499952	7.645107
-442.847196	-24.730305	7.655104
-440.537205	-29.865733	7.665101
-438.301396	-33.525551	7.675098
-436.442285	-32.391282	7.685094
-435.178940	-26.284251	7.695091
-432.870874	-28.302359	7.705088
-431.090529	-27.330780	7.715085
-429.408610	-30.112628	7.725082
-427.250391	-31.854157	7.735078
-425.668081	-31.629413	7.745075
-423.371090	-32.650954	7.755072
-421.757711	-31.332164	7.765069
-420.082268	-27.823693	7.775066
-418.234926	-29.439780	7.785062
-416.272723	-32.381643	7.795059
-414.428844	-28.669526	7.805056
-412.095571	-27.636216	7.815053
-410.585668	-19.803181	7.825050
-408.409245	-27.697927	7.835046
-406.960459	-28.340844	7.845043
-405.231900	-24.856634	7.855040
-403.091649	-24.684646	7.865037
-400.833961	-23.542934	7.875034
-398.909559	-30.497382	7.885030
-397.466640	-29.497165	7.895027
-395.891037	-25.977471	7.905024
-393.505064	-27.821656	7.915021
-391.472208	-26.242963	7.925018
-389.779600	-28.429617	7.935014
-388.322037	-23.561527	7.945011
-386.295547	-25.788857	7.955008
-384.184156	-25.841203	7.965005
-382.393931	-27.754476	7.975002
-380.419202	-24.205335	7.984998
-378.491282	-27.413289	7.994995
-376.926474	-26.937811	8.004992
-374.895627	-30.569585	8.014989
-373.071348	-28.373333	8.024986
-370.930699	-23.090054	8.034982
-369.091984	-26.646936	8.044979
-367.498748	-32.064198	8.054976
-365.527661	-27.598625	8.064973
-363.543439	-30.654495	8.074970
-361.601718	-34.662049	8.084966
-360.305362	-30.612987	8.094963
-358.057641	-33.016147	8.104960
-356.022257	-35.687000	8.114957
-354.268452	-29.970875	8.124954
-352.464065	-26.824011	8.134950
-350.201516	-29.283220	8.144947
-348.601814	-31.819769	8.154944
-346.791271	-34.181546	8.164941
-345.048904	-30.696338	8.174938
-342.993271	-29.195454	8.184934
-341.063198	-28.678786	8.194931
-339.066128	-32.140920	8.204928
-337.353980	-23.441654	8.214925
-335.477106	-28.583636	8.224922
-333.671082	-28.767197	8.234918
-331.710360	-33.759920	8.244915
-330.013778	-24.780254	8.254912
-327.960346	-31.936838	8.264909
-325.880342	-32.407303	8.274906
-324.092896	-22.759995	8.284902
-322.340378	-29.270084	8.294899
-320.524561	-20.574721	8.304896
-318.715906	-21.971388	8.314893
-316.812761	-18.387078	8.324890
-314.671201	-30.400615	8.334886
-312.806961	-28.264382	8.344883
-311.143633	-30.252087	8.354880
-309.319798	-28.537319	8.364877
-307.316080	-25.310129	8.374874
-305.918111	-23.833707	8.384870
-303.620065	-34.451083	8.394867
-301.409192	-33.898678	8.404864
-300.026574	-20.179142	8.414861
-298.009152	-26.396748	8.424858
-296.172076	-28.424811	8.434854
-293.829340	-31.199942	8.444851
-292.249437	-21.238409	8.454848
-290.510022	-22.080816	8.464845
-288.539317	-26.432435	8.474842
-286.681179	-25.610541	8.484838
-284.833342	-28.894066	8.494835
-282.800455	-29.803839	8.504832
-281.088330	-26.151114	8.514829
-279.463495	-22.309179	8.524826
-277.535633	-31.874234	8.534822
-275.126569	-32.180853	8.544819
-273.564395	-30.826944	8.554816
-271.761207	-29.156222	8.564813
-269.714240	-23.936847	8.574810
-267.875465	-27.953163	8.584807
-266.017672	-29.880295	8.594803
-264.218522	-34.286620	8.604800
-262.006199	-32.480658	8.614797
-260.483168	-29.621991	8.624794
-258.584554	-30.270299	8.634791
-256.452973	-33.172753	8.644787
-254.582506	-34.306066	8.654784
-252.924868	-25.348545	8.664781
-251.374511	-30.395716	8.674778
-249.425881	-33.774253	8.684775
-247.242042	-31.663715	8.694771
-245.129021	-32.106221	8.704768
-243.603968	-34.491834	8.714765
-241.877552	-33.211490	8.724762
-239.637335	-32.358958	8.734759
-238.051902	-32.276702	8.744755
-236.023181	-34.447419	8.754752
-234.138962	-26.348723	8.764749
-232.222849	-25.776053	8.774746
-230.375280	-26.288291	8.784743
-228.485647	-34.917157	8.794739
-226.389015	-32.314234	8.804736
-224.414833	-38.041694	8.814733
-222.777188	-34.045443	8.824730
-221.093792	-31.404986	8.834727
-219.434855	-32.435035	8.844723
-217.093031	-35.509964	8.854720
-215.569484	-30.194373	8.864717
-213.721474	-28.557603	8.874714
-211.392548	-34.174292	8.884711
-209.439253	-31.393733	8.894707
-207.811429	-33.239906	8.904704
-206.136370	-30.037551	8.914701
-204.161838	-30.906365	8.924698
-202.304357	-35.970939	8.934695
-200.300285	-35.805460	8.944691
-198.673503	-35.906629	8.954688
-196.634290	-35.783073	8.964685
-194.951369	-33.164628	8.974682
-192.793324	-38.814032	8.984679
-190.982337	-36.201811	8.994675
-189.196635	-33.541339	9.004672
-187.363522	-33.495418	9.014669
-185.274024	-30.232862	9.024666
-183.316271	-37.339324	9.034663
-181.447025	-36.321743	9.044659
-179.980756	-32.566547	9.054656
-178.366323	-32.117807	9.064653
-175.899539	-31.937722	9.074650
-173.723911	-30.406890	9.084647
-172.155591	-32.876737	9.094643
-170.580267	-24.926072	9.104640
-168.813418	-24.182682	9.114637
-166.711983	-26.213359	9.124634
-164.760597	-33.151416	9.134631
-162.725644	-31.975515	9.144627
-160.889151	-25.385013	9.154624
-158.858862	-30.646090	9.164621
-157.396813	-27.539188	9.174618
-155.320737	-32.894415	9.184615
-153.423489	-27.993695	9.194611
-151.536463	-32.281326	9.204608
-149.955777	-29.618111	9.214605
-147.923230	-29.401866	9.224602
-145.922443	-24.271331	9.234599
-143.757072	-28.713904	9.244595
-142.396413	-31.163230	9.254592
-140.651499	-31.229522	9.264589
-138.765380	-30.165649	9.274586
-136.522433	-35.796973	9.284583
-134.634092	-31.832765	9.294579
-132.824575	-33.227854	9.304576
-131.094060	-31.066981	9.314573
-129.002782	-32.889152	9.324570
-127.047504	-37.484512	9.334567
-125.419986	-33.657111	9.344563
-123.659941	-35.306419	9.354560
-121.481975	-34.807022	9.364557
-119.635195	-31.827804	9.374554
-117.845877	-33.216501	9.384551
-116.025633	-30.747811	9.394547
-114.058183	-38.668972	9.404544
-112.245052	-31.526780	9.414541
-110.444794	-34.510464	9.424538
-108.428164	-36.473874	9.434535
-106.510498	-36.788769	9.444531
-104.649942	-30.884205	9.454528
-102.863909	-30.705964	9.464525
-101.116396	-30.229454	9.474522
-98.985379	-33.456966	9.484519
-97.001264	-26.694164	9.494515
-95.337018	-28.516074	9.504512
-93.626115	-28.057403	9.514509
-91.509700	-28.764016	9.524506
-89.796737	-28.880441	9.534503
-87.598356	-27.578962	9.544499
-86.068064	-32.738103	9.554496
-84.246797	-32.409145	9.564493
-82.056861	-30.539440	9.574490
-80.154694	-30.297601	9.584487
-78.585381	-28.922596	9.594483
-76.567662	-29.345014	9.604480
-74.699912	-25.061662	9.614477
-72.810289	-24.822552	9.624474
-70.786524	-24.383776	9.634471
-69.083172	-25.616611	9.644467
-67.341238	-23.448038	9.654464
-65.300177	-29.306058	9.664461
-63.444420	-31.347983	9.674458
-61.518763	-29.203979	9.684455
-59.555399	-29.739298	9.694451
-57.857526	-37.296869	9.704448
-56.096889	-28.620906	9.714445
-54.098074	-28.337619	9.724442
-52.053466	-30.613359	9.734439
-50.217654	-25.658538	9.744435
-48.432725	-26.430661	9.754432
-46.415574	-22.840631	9.764429
-44.462232	-26.410828	9.774426
-42.984914	-29.725075	9.784423
-41.073903	-29.685153	9.794419
-38.972807	-27.583329	9.804416
-37.014870	-26.205550	9.814413
-35.279404	-30.309436	9.824410
-33.365876	-35.774432	9.834407
-31.588703	-31.880831	9.844403
-29.868852	-28.919190	9.854400
-27.905318	-29.020275	9.864397
-25.813039	-23.144712	9.874394
-24.126953	-24.575299	9.884391
-21.983672	-26.618846	9.894387
-20.251274	-25.784583	9.904384
-18.412358	-26.118428	9.914381
-16.559397	-25.428138	9.924378
-14.553152	-31.192138	9.934375
-12.875398	-31.538169	9.944371
-10.914393	-33.620529	9.954368
-8.796488	-29.064378	9.964365
-7.939862	-12.360028	9.974362
-6.092620	14.530630	9.984359
-4.748021	52.731692	9.994355
-3.090686	99.588280	10.004352
-1.709157	162.295381	10.014349
0.000000	209.725351	10.019354
0.706575	235.233605	10.024359
1.347072	259.547577	10.029363
2.078143	281.314398	10.034368
2.435274	302.521114	10.039373
2.590996	315.053061	10.044378
2.670738	322.853351	10.049383
2.991257	314.280087	10.054387
2.625693	328.325583	10.059392
3.150261	325.665273	10.064397
3.270421	329.065439	10.069402
3.041548	337.405427	10.074407
3.440280	326.476173	10.079411
3.154637	333.103068	10.084416
3.507960	325.488148	10.089421
3.531367	338.331398	10.094426
3.186194	341.249089	10.099431
3.723497	341.537421	10.104435
3.596686	343.511897	10.109440
3.677142	345.287721	10.114445
3.709940	345.137673	10.119450
3.782268	345.638953	10.124455
3.931551	341.980294	10.129459
3.606325	350.507558	10.134464
3.829611	347.165121	10.139469
3.600465	352.210685	10.144474
3.618279	354.994781	10.149479
4.229184	366.093165	10.154483
3.912323	359.473011	10.159488
4.030225	352.703083	10.164493
4.210804	362.173187	10.169498
4.264210	370.337273	10.174503
4.382518	370.365986	10.179507
4.045065	368.997575	10.184512
4.436723	357.670430	10.189517
4.472402	360.568380	10.194522
4.214291	361.310037	10.199527
4.434350	365.329833	10.204531
4.163371	367.035551	10.209536
4.449849	365.561312	10.214541
4.365325	371.421234	10.219546
4.216692	379.273751	10.224551
4.902738	385.261522	10.229555
4.523524	400.211344	10.234560
4.644616	398.493803	10.239565
4.505123	401.146870	10.244570
4.977019	405.400917	10.249575
5.167931	401.070081	10.254579
5.156440	413.040538	10.259584
5.309585	384.999826	10.264589
5.035474	384.651132	10.269594
4.864228	384.136210	10.274599
5.166152	377.795843	10.279603
4.729463	384.686567	10.284608
5.302545	374.019648	10.289613
5.070044	382.292426	10.294618
5.026934	391.509626	10.299623
5.155612	382.623123	10.304627
5.411760	404.864880	10.309632
5.262840	403.266106	10.314637
5.328125	408.878204	10.319642
5.539351	413.309460	10.324647
5.678445	417.679677	10.329651
5.263000	409.677943	10.334656
5.354163	412.532358	10.339661
5.462703	425.508773	10.344666
5.499329	423.883555	10.349671
6.058083	420.722577	10.354675
6.051509	424.005776	10.359680
5.871940	421.889879	10.364685
5.902886	423.310884	10.369690
5.795731	428.860602	10.374695
5.933310	429.348324	10.379699
5.773600	436.063995	10.384704
5.715400	426.133290	10.389709
5.842624	428.717009	10.394714
6.073640	427.259495	10.399719
6.218018	437.216428	10.404723
6.164414	436.384673	10.409728
6.150165	434.616170	10.414733
6.020027	442.861616	10.419738
6.046723	442.072250	10.424743
6.272854	427.011720	10.429747
6.122419	436.354885	10.434752
6.318720	439.924295	10.439757
6.000197	438.904544	10.444762
5.970822	449.551569	10.449767
6.720715	461.372235	10.454771
6.859403	468.212226	10.459776
6.909266	469.390504	10.464781
6.859154	462.648901	10.469786
6.526744	454.867304	10.474791
7.042042	463.803079	10.479795
6.605137	460.509146	10.484800
6.730402	466.062810	10.489805
7.234271	471.928276	10.494810
6.899559	470.103644	10.499815
6.770442	463.210627	10.504819
7.108962	474.330462	10.509824
7.285982	476.843164	10.514829
7.267103	482.706853	10.519834
7.276812	483.561929	10.524839
7.591238	476.822103	10.529843
6.826645	470.205499	10.534848
7.287381	473.464637	10.539853
7.232095	480.740882	10.544858
7.278740	480.617011	10.549863
7.300117	481.091727	10.554867
7.279885	486.534555	10.559872
7.392835	482.329680	10.564877
7.424213	489.891750	10.569882
7.721268	489.701128	10.574887
7.801597	483.025449	10.579891
7.456833	491.486519	10.584896
7.431109	486.097300	10.589901
7.916186	492.020970	10.594906
7.595621	492.853026	10.599911
7.936263	481.609622	10.604915
7.742982	491.615719	10.609920
7.974389	491.422951	10.614925
7.948247	492.846761	10.619930
7.545460	500.254143	10.624935
8.057177	506.589918	10.629939
8.196907	515.560396	10.634944
8.263640	515.892250	10.639949
8.187010	514.113186	10.644954
8.197171	527.256783	10.649959
8.138057	521.178962	10.654963
8.012014	538.045697	10.659968
8.380392	529.262808	10.664973
8.497293	524.633057	10.669978
8.321506	532.226616	10.674983
8.317823	524.334196	10.679987
8.338243	531.200967	10.684992
8.295997	527.986006	10.689997
8.480976	527.090957	10.695002
8.440153	529.751965	10.700007
8.807034	527.563085	10.705011
8.493961	536.810821	10.710016
8.525583	552.654133	10.715021
9.007951	562.688139	10.720026
8.826781	568.550939	10.725031
9.101969	561.339476	10.730035
8.895897	565.392602	10.735040
8.997214	570.164739	10.740045
9.204878	563.937106	10.745050
9.416082	570.882284	10.750055
9.404308	562.891777	10.755059
9.223264	572.889670	10.760064
9.202851	566.248946	10.765069
9.660067	573.000331	10.770074
9.246455	570.853928	10.775079
9.640625	569.950744	10.780083
9.564548	566.714360	10.785088
9.554749	573.649054	10.790093
9.548522	564.050614	10.795098
9.484037	567.962876	10.800103
9.864493	566.834779	10.805107
9.254397	576.951576	10.810112
9.665503	566.453868	10.815117
9.469891	573.809317	10.820122
9.591104	583.035124	10.825127
9.877558	574.200615	10.830131
9.576474	572.077268	10.835136
9.714633	577.870212	10.840141
9.858848	577.576223	10.845146
10.041306	578.649775	10.850151
10.044406	577.160786	10.855155
9.697376	582.250465	10.860160
9.991375	577.431586	10.865165
9.700706	581.767891	10.870170
9.909557	598.458267	10.875175
10.508515	600.515727	10.880179
10.170882	597.543424	10.885184
10.310323	604.484293	10.890189
10.001173	608.400894	10.895194
10.375502	599.877234	10.900199
10.648114	599.042327	10.905203
10.260592	611.112352	10.910208
10.404155	604.393413	10.915213
10.694420	603.379056	10.920218
10.474488	608.658224	10.925223
10.690881	604.654452	10.930227
10.315964	610.600216	10.935232
10.630496	619.773132	10.940237
10.983976	636.044633	10.945242
10.925429	640.227226	10.950247
11.334459	637.206789	10.955251
10.892911	627.952156	10.960256
11.106060	630.717765	10.965261
11.338811	634.059040	10.970266
10.688090	630.961612	10.975271
10.703286	630.298660	10.980275
10.909361	640.075566	10.985280
10.838988	638.081003	10.990285
11.166427	639.438968	10.995290
11.139571	644.414516	11.000295
11.499869	631.821025	11.005299
10.987939	648.887434	11.010304
11.130470	645.585410	11.015309
11.494895	651.454267	11.020314
11.616222	666.071400	11.025319
12.157040	658.612499	11.030323
11.551622	657.918425	11.035328
11.417521	643.741527	11.040333
11.471949	664.572818	11.045338
11.626926	672.071899	11.050343
11.851209	667.854732	11.055347
11.937213	666.175876	11.060352
12.358849	663.829996	11.065357
12.294586	658.755971	11.070362
12.285821	648.059435	11.075367
12.527764	643.036719	11.080371
12.133473	642.494279	11.085376
12.227227	636.486652	11.090381
12.354770	634.271272	11.095386
12.058501	639.673023	11.100391
12.358662	629.230816	11.105395
12.079460	640.282136	11.110400
12.487928	635.645271	11.115405
12.207908	630.637211	11.120410
12.027878	648.977802	11.125415
12.366155	646.892824	11.130419
12.119190	670.885377	11.135424
12.354061	667.927409	11.140429
12.720480	670.778976	11.145434
12.350866	675.476438	11.150439
12.924436	670.297518	11.155443
12.796091	672.728062	11.160448
12.881253	674.179083	11.165453
12.782514	679.945194	11.170458
12.574814	678.424367	11.175463
13.117425	671.961110	11.180467
12.653285	674.068289	11.185472
12.646422	669.757091	11.190477
13.080251	678.596387	11.195482
12.815135	674.482512	11.200487
12.926666	671.814688	11.205491
12.840514	682.605781	11.210496
12.960935	680.061916	11.215501
13.147382	700.429038	11.220506
12.982141	713.042488	11.225511
13.357102	704.808064	11.230515
13.339816	707.639619	11.235520
13.542305	704.320133	11.240525
13.484946	706.702299	11.245530
13.620216	711.317665	11.250535
13.786198	699.672982	11.255539
13.877463	709.178850	11.260544
13.703918	702.244704	11.265549
13.729838	703.250973	11.270554
13.622418	700.543155	11.275559
14.026964	701.856496	11.280563
13.580699	709.003600	11.285568
13.865876	697.173523	11.290573
13.774722	698.859269	11.295578
13.792920	704.152533	11.300583
14.167200	703.748512	11.305587
13.757683	705.880101	11.310592
14.001411	711.749310	11.315597
13.913732	711.877907	11.320602
14.041553	712.333287	11.325607
13.967593	709.592531	11.330611
14.000531	717.265656	11.335616
14.391093	719.378454	11.340621
14.566307	720.934188	11.345626
14.095857	730.740206	11.350631
14.310562	723.124323	11.355635
14.082707	733.602922	11.360640
14.367694	734.418836	11.365645
14.557078	738.601340	11.370650
14.716463	741.897567	11.375655
14.887347	738.276368	11.380659
14.504621	749.856841	11.385664
15.012692	741.985978	11.390669
14.987816	738.399158	11.395674
14.703152	746.596087	11.400679
14.838683	736.607457	11.405683
15.026089	736.991039	11.410688
14.792322	729.857519	11.415693
15.005837	733.314649	11.420698
14.807648	739.620242	11.425703
15.275134	733.310092	11.430707
14.897699	749.848127	11.435712
15.129927	737.309670	11.440717
14.968546	742.217602	11.445722
14.680477	735.803225	11.450727
15.395234	753.356981	11.455731
15.187258	767.694760	11.460736
15.516376	769.613919	11.465741
15.333544	777.365650	11.470746
15.576170	777.493609	11.475751
15.672150	776.149861	11.480755
15.459876	784.023786	11.485760
15.689310	783.133461	11.490765
15.907487	769.643856	11.495770
15.582844	778.480387	11.500775
16.029910	769.131241	11.505779
15.506191	774.376913	11.510784
15.965692	770.900501	11.515789
15.929970	772.626305	11.520794
15.579390	775.657705	11.525799
15.831593	768.691105	11.530803
15.937058	783.250955	11.535808
15.873446	777.186361	11.540813
15.921356	775.768271	11.545818
15.602292	781.095643	11.550823
16.000165	771.520930	11.555827
15.908952	781.943860	11.560832
15.979021	798.233937	11.565837
16.187474	805.038516	11.570842
16.432166	803.275191	11.575847
16.824692	797.479278	11.580851
16.718706	806.806916	11.585856
16.640391	804.483982	11.590861
16.905288	804.855206	11.595866
16.595968	797.886683	11.600871
16.742900	782.364498	11.605875
16.593931	793.177520	11.610880
16.785976	788.390606	11.615885
17.125458	794.384150	11.620890
16.674620	778.786197	11.625895
16.752782	772.930038	11.630899
16.823909	802.446351	11.635904
16.866087	798.591752	11.640909
16.965311	804.071633	11.645914
16.774310	806.279569	11.650919
17.041392	805.194773	11.655923
16.860033	808.240194	11.660928
16.659415	808.954565	11.665933
16.980373	801.616613	11.670938
16.570209	807.804643	11.675943
17.057020	811.767035	11.680947
17.379060	826.889322	11.685952
17.249002	841.176893	11.690957
17.625243	839.670155	11.695962
17.736370	835.768275	11.700967
17.984408	826.467397	11.705971
17.552087	815.556781	11.710976
17.167796	813.434840	11.715981
17.726829	819.805790	11.720986
17.509457	831.693512	11.725991
17.923979	832.119727	11.730995
17.798811	840.233704	11.736000
17.878541	838.797127	11.741005
18.156172	835.942703	11.746010
17.714838	829.420253	11.751015
18.055288	834.567538	11.756019
17.958182	837.235213	11.761024
17.852899	836.846172	11.766029
18.077773	837.928750	11.771034
17.796159	854.471334	11.776039
18.045908	841.341730	11.781043
18.045858	835.975097	11.786048
18.009242	838.436773	11.791053
18.434552	839.201925	11.796058
18.131979	843.013449	11.801063
18.408059	842.508381	11.806067
18.255972	843.215013	11.811072
18.116794	835.484399	11.816077
18.295235	846.985694	11.821082
18.192101	863.730079	11.826087
18.625713	861.185909	11.831091
18.555581	863.762545	11.836096
18.321955	877.413746	11.841101
18.708152	865.770080	11.846106
18.487240	868.806050	11.851111
18.707250	863.666897	11.856115
18.653267	875.140624	11.861120
18.726659	864.773059	11.866125
18.690788	861.161151	11.871130
18.681766	874.332567	11.876135
19.201442	884.736990	11.881139
18.981965	901.044977	11.886144
19.022439	907.187983	11.891149
19.298510	904.847148	11.896154
19.218953	905.020187	11.901159
19.667946	895.241677	11.906163
19.557343	905.383119	11.911168
19.359025	893.339023	11.916173
19.196882	885.181492	11.921178
19.373143	893.810452	11.926183
19.411545	890.118085	11.931187
19.195220	907.210192	11.936192
19.478517	910.603401	11.941197
19.751423	901.938031	11.946202
19.790933	907.069469	11.951207
19.889618	898.541500	11.956211
19.446623	905.031305	11.961216
19.566235	908.663533	11.966221
19.699262	904.947396	11.971226
19.556934	909.401288	11.976231
19.469989	904.086340	11.981235
19.567656	905.133225	11.986240
19.598919	923.996395	11.991245
19.717555	927.872448	11.996250
19.904447	933.369148	12.001255
20.261009	923.382200	12.006259
20.349393	925.519570	12.011264
20.487388	929.723731	12.016269
20.742724	929.143902	12.021274
20.625019	933.361249	12.026279
20.791284	929.333842	12.031283
20.382758	910.161549	12.036288
20.360741	908.421039	12.041293
20.455145	902.672635	12.046298
20.494032	907.513194	12.051303
20.552808	905.080848	12.056307
20.081325	907.771186	12.061312
20.324655	901.285383	12.066317
20.589648	898.431386	12.071322
20.660729	896.508853	12.076327
20.669809	897.081749	12.081331
20.602461	899.763614	12.086336
20.248722	887.174184	12.091341
20.287019	878.697651	12.096346
19.868387	877.312171	12.101351
20.176884	882.686944	12.106355
20.100092	908.328431	12.111360
20.051544	903.534906	12.116365
20.184682	905.829944	12.121370
20.030871	907.290717	12.126375
20.424942	913.381270	12.131379
20.147347	919.502466	12.136384
20.338514	913.580913	12.141389
20.408127	909.557888	12.146394
20.229675	913.751798	12.151399
20.742111	910.419893	12.156403
20.430698	918.966573	12.161408
20.503927	901.431783	12.166413
20.383056	881.406951	12.171418
20.014903	880.771223	12.176423
20.122463	871.771873	12.181427
20.681576	881.748126	12.186432
20.549814	888.110215	12.191437
20.319655	880.438248	12.196442
19.908213	882.986528	12.201447
20.328474	874.728224	12.206451
20.230349	876.467148	12.211456
20.234118	883.232651	12.216461
20.329670	884.394213	12.221466
19.957546	884.215694	12.226471
20.089256	883.112268	12.231475
20.148220	890.279810	12.236480
20.349556	897.991622	12.241485
20.175176	902.195920	12.246490
20.368937	904.082276	12.251495
20.582323	887.357078	12.256499
20.439585	890.576936	12.261504
20.431969	886.171167	12.266509
20.479664	882.609799	12.271514
20.319190	884.279811	12.276519
20.241228	883.891143	12.281523
20.071884	882.317651	12.286528
20.150118	880.061208	12.291533
20.146279	887.233246	12.296538
20.042519	888.858728	12.301543
20.276524	879.818703	12.306547
20.076590	885.050620	12.311552
20.377482	888.973295	12.316557
20.256572	875.803421	12.321562
20.213415	881.996029	12.326567
20.244601	876.261662	12.331571
20.058135	890.126938	12.336576
20.271015	890.850273	12.341581
20.385013	882.600597	12.346586
19.921002	896.832668	12.351591
20.563546	908.916069	12.356595
20.297507	898.145255	12.361600
20.187783	894.595585	12.366605
20.536724	891.212483	12.371610
20.422097	881.498645	12.376615
20.687284	884.530422	12.381619
20.381075	887.046936	12.386624
20.487815	879.290480	12.391629
20.710792	890.048192	12.396634
20.372035	889.359673	12.401639
20.733971	882.353437	12.406643
20.638280	889.671816	12.411648
20.423537	883.975094	12.416653
20.240580	870.281267	12.421658
20.269332	865.763249	12.426663
20.543905	863.223154	12.431667
20.046660	870.963576	12.436672
20.178515	864.698228	12.441677
20.082258	858.663252	12.446682
20.179936	873.904961	12.451687
20.546151	880.803484	12.456691
20.304225	877.367955	12.461696
20.156446	875.250863	12.466701
20.242617	873.325926	12.471706
20.247507	870.360440	12.476711
20.201067	869.786953	12.481715
20.048690	870.313053	12.486720
20.257688	889.274787	12.491725
20.485075	893.969358	12.496730
20.114316	889.868328	12.501735
20.176757	878.174567	12.506739
20.301758	893.415881	12.511744
20.550315	886.423784	12.516749
20.260841	879.649984	12.521754
20.019568	886.964770	12.526759
20.183865	882.828081	12.531763
20.179174	895.615586	12.536768
20.190585	905.014457	12.541773
20.633587	907.404378	12.546778
19.868350	902.893128	12.551783
20.553843	896.858829	12.556787
20.507542	891.131295	12.561792
20.525769	880.315942	12.566797
20.503877	877.149702	12.571802
20.452954	883.987013	12.576807
20.588289	873.684475	12.581811
20.426717	876.400291	12.586816
20.231720	872.299620	12.591821
20.557850	871.348131	12.596826
20.384570	878.210476	12.601831
20.529945	879.882962	12.606835
20.337590	881.045496	12.611840
20.207228	882.197355	12.616845
20.261940	877.889680	12.621850
20.307538	878.741420	12.626855
20.277764	867.127826	12.631859
20.499809	887.329456	12.636864
20.367026	883.499586	12.641869
20.471215	866.014311	12.646874
20.022937	855.791466	12.651879
20.125648	855.992209	12.656883
20.454560	874.304741	12.661888
20.377582	869.335182	12.666893
20.348846	856.149047	12.671898
19.966745	843.283452	12.676903
20.290373	859.715312	12.681907
20.236713	869.462830	12.686912
20.230965	865.315417	12.691917
20.474781	876.011442	12.696922
20.081660	872.427335	12.701927
20.316415	856.689193	12.706931
20.135375	858.626650	12.711936
20.233659	871.713921	12.716941
20.631320	876.690443	12.721946
20.241634	864.810947	12.726951
20.637801	858.458497	12.731955
20.158038	857.012588	12.736960
20.138334	851.148350	12.741965
20.310096	843.734027	12.746970
20.291394	849.327361	12.751975
20.362001	849.976394	12.756979
20.448634	857.238865	12.761984
20.309540	856.173114	12.766989
20.133461	840.708696	12.771994
20.121774	846.177895	12.776999
20.289156	849.106192	12.782003
20.075835	853.614762	12.787008
19.854671	848.999401	12.792013
20.199941	859.207674	12.797018
20.120440	871.655394	12.802023
20.348838	876.669952	12.807027
20.328010	883.631787	12.812032
20.292157	886.789648	12.817037
20.436125	876.382430	12.822042
19.877513	873.301796	12.827047
20.042583	869.847090	12.832051
19.984896	888.168468	12.837056
19.995288	887.370639	12.842061
20.511159	890.571401	12.847066
20.350124	892.473341	12.852071
20.333217	894.730013	12.857075
20.376149	897.766488	12.862080
20.419523	896.427178	12.867085
20.474474	896.700201	12.872090
20.384683	891.989748	12.877095
20.328796	880.396869	12.882099
20.027227	871.559767	12.887104
20.200396	887.345382	12.892109
20.634843	884.780573	12.897114
20.411678	886.902178	12.902119
20.208708	865.222660	12.907123
20.119835	864.064523	12.912128
19.822705	862.095057	12.917133
20.530958	867.915472	12.922138
20.001193	892.801196	12.927143
20.624973	888.826208	12.932147
20.362366	874.709797	12.937152
20.002741	871.041493	12.942157
20.111034	868.963202	12.947162
20.232165	880.798550	12.952167
20.449917	889.586487	12.957171
20.609673	891.713257	12.962176
20.310442	868.210168	12.967181
20.332852	857.236454	12.972186
20.228074	863.494082	12.977191
20.418200	851.116012	12.982195
20.462153	854.460641	12.987200
20.221916	857.116453	12.992205
20.510081	853.135075	12.997210
20.425073	858.479553	13.002215
20.285522	848.839105	13.007219
20.371251	866.736995	13.012224
20.249022	855.567132	13.017229
20.474046	857.662195	13.022234
20.455556	858.609320	13.027239
20.449129	849.311953	13.032243
20.341266	859.008968	13.037248
20.488686	853.256071	13.042253
20.526673	856.989622	13.047258
20.582298	861.184034	13.052263
20.134827	852.209349	13.057267
20.091134	843.149765	13.062272
20.351339	854.963699	13.067277
20.490365	847.718615	13.072282
20.078700	844.426874	13.077287
20.387147	836.902435	13.082291
20.323068	837.721987	13.087296
20.041135	831.262429	13.092301
20.016273	835.068296	13.097306
20.363108	847.848581	13.102311
20.709678	848.675971	13.107315
20.162038	837.003849	13.112320
20.176436	834.461097	13.117325
20.337427	833.479962	13.122330
20.031670	834.696066	13.127335
20.320698	848.560374	13.132339
20.308144	852.871324	13.137344
20.305731	850.467671	13.142349
20.460611	838.356246	13.147354
20.397355	836.691714	13.152359
20.203457	837.722803	13.157363
20.001717	849.399867	13.162368
19.993237	838.268651	13.167373
20.838989	845.837435	13.172378
20.121999	843.605323	13.177383
20.030161	845.085381	13.182387
20.473813	842.783277	13.187392
20.147754	840.156830	13.192397
20.274840	838.028233	13.197402
20.169768	841.023641	13.202407
20.209603	832.070602	13.207411
20.129306	840.779880	13.212416
20.127703	858.775276	13.217421
20.531544	859.328576	13.222426
20.281904	860.784915	13.227431
20.286792	846.700779	13.232435
20.570864	839.653361	13.237440
20.238014	838.049966	13.242445
20.260251	837.840879	13.247450
19.940310	838.305385	13.252455
20.426570	835.703143	13.257459
20.216053	836.580748	13.262464
19.856312	846.064014	13.267469
20.373077	851.613736	13.272474
20.171628	870.264770	13.277479
20.386314	870.722072	13.282483
20.559779	866.288215	13.287488
20.370742	846.977696	13.292493
20.365813	843.442867	13.297498
20.124096	847.105900	13.302503
20.190247	839.059442	13.307507
20.299258	842.690189	13.312512
20.111792	848.185849	13.317517
20.641191	845.100436	13.322522
20.154010	843.154977	13.327527
20.180148	843.833971	13.332531
20.161264	847.231992	13.337536
20.107765	843.760897	13.342541
20.230757	841.037593	13.347546
19.992987	852.931740	13.352551
20.400380	861.079069	13.357555
20.373069	869.829591	13.362560
20.004267	859.057848	13.367565
20.007153	862.836428	13.372570
20.152375	877.715706	13.377575
20.415083	874.614471	13.382579
20.624346	869.696249	13.387584
20.342666	863.471627	13.392589
20.162379	854.383355	13.397594
20.065276	860.750944	13.402599
20.068523	866.454336	13.407603
20.230821	879.557427	13.412608
20.184283	874.190309	13.417613
20.469033	874.764970	13.422618
20.504090	876.140417	13.427623
20.701264	875.946009	13.432627
20.209976	860.450624	13.437632
20.052138	860.600664	13.442637
20.019103	848.367011	13.447642
20.114102	863.341815	13.452647
20.531315	877.618623	13.457651
20.154350	872.418550	13.462656
20.288502	880.589757	13.467661
20.635721	867.457200	13.472666
20.320576	855.091901	13.477671
20.493548	849.550205	13.482675
20.272003	856.633149	13.487680
20.117061	862.280549	13.492685
20.089392	859.835975	13.497690
19.857570	861.482669	13.502695
20.348253	855.885565	13.507699
20.152469	868.423588	13.512704
20.232653	886.073989	13.517709
20.300014	878.666050	13.522714
20.236076	884.215356	13.527719
20.177126	883.441992	13.532723
20.099908	883.162026	13.537728
20.296777	894.549232	13.542733
20.625022	882.979458	13.547738
20.299258	878.670961	13.552743
20.087858	870.382508	13.557747
20.192244	876.695888	13.562752
20.357661	881.365642	13.567757
20.329903	880.908247	13.572762
20.251969	881.095221	13.577767
20.405716	863.902485	13.582771
20.152392	867.852043	13.587776
20.213244	862.273027	13.592781
20.270093	865.231575	13.597786
20.086263	871.397725	13.602791
20.577573	875.355475	13.607795
20.302194	866.998373	13.612800
20.291730	864.435137	13.617805
20.098110	863.808634	13.622810
19.717142	879.504412	13.627815
20.414782	884.101894	13.632819
20.493223	894.506520	13.637824
20.563289	886.090367	13.642829
20.770841	872.642578	13.647834
20.341268	867.444589	13.652839
20.182757	863.670084	13.657843
20.191805	870.470225	13.662848
20.014662	867.122147	13.667853
20.257145	869.949363	13.672858
20.126321	873.037204	13.677863
20.254761	868.238329	13.682867
20.258173	866.276915	13.687872
20.027442	869.978417	13.692877
20.230131	872.547814	13.697882
20.205943	885.218559	13.702887
20.491059	880.912773	13.707891
20.364285	876.628526	13.712896
20.015080	874.474168	13.717901
20.236502	860.399640	13.722906
20.304331	873.289900	13.727911
20.611068	875.152713	13.732915
20.547597	874.433693	13.737920
20.053518	871.200827	13.742925
20.457779	873.589824	13.747930
20.379102	871.812619	13.752935
20.164967	868.904936	13.757939
20.116711	872.318688	13.762944
20.366490	878.921147	13.767949
20.292492	862.640037	13.772954
20.344992	878.983475	13.777959
20.268766	869.167316	13.782963
20.481952	873.751382	13.787968
20.186473	875.459487	13.792973
20.705569	865.740785	13.797978
20.255849	875.002643	13.802983
20.111154	876.247471	13.807987
20.281561	870.884391	13.812992
20.445699	878.728295	13.817997
20.798894	872.605066	13.823002
20.230063	868.944107	13.828007
20.644852	873.917896	13.833011
20.425476	867.827640	13.838016
20.355651	870.557209	13.843021
20.299295	852.878337	13.848026
20.101781	867.420358	13.853031
20.361082	862.685778	13.858035
20.041408	851.623112	13.863040
19.903706	869.458072	13.868045
20.249741	874.799255	13.873050
20.173112	881.658803	13.878055
20.573318	874.127595	13.883059
20.384425	876.841460	13.888064
20.261936	882.747858	13.893069
20.627261	875.547888	13.898074
19.949563	865.686515	13.903079
20.220787	860.802572	13.908083
20.108457	865.528450	13.913088
20.185925	877.407033	13.918093
20.374559	871.614436	13.923098
20.356318	878.981963	13.928103
20.170391	866.699345	13.933107
20.238842	880.501084	13.938112
20.092787	873.301458	13.943117
20.483924	873.331606	13.948122
20.210397	880.705156	13.953127
20.081902	873.468032	13.958131
20.466236	878.861462	13.963136
20.527944	873.222375	13.968141
20.470340	859.905997	13.973146
19.936940	862.497383	13.978151
20.351514	858.528172	13.983155
20.191269	862.941537	13.988160
20.128904	873.522375	13.993165
20.426201	872.387019	13.998170
20.448423	878.998174	14.003175
20.106124	865.761108	14.008179
20.094596	860.485403	14.013184
20.257472	865.296710	14.018189
20.448002	871.757280	14.023207
20.094953	878.027582	14.028224
20.361847	876.833782	14.033242
20.500130	870.824020	14.038259
20.185387	875.754230	14.043277
20.670266	870.920132	14.048295
20.343873	852.825278	14.053312
20.316891	853.162564	14.058330
20.532313	849.838358	14.063347
20.282250	847.979796	14.068365
20.517439	847.986604	14.073383
20.303890	857.365097	14.078400
20.496199	870.570694	14.083418
20.670136	870.938857	14.088435
20.374049	863.625070	14.093453
20.464685	853.387366	14.098471
20.471561	873.915393	14.103488
20.514709	876.464274	14.108506
20.263730	874.761591	14.113523
20.291959	885.124050	14.118541
20.575211	880.101089	14.123559
20.527578	887.075407	14.128576
20.531351	886.421458	14.133594
20.565249	882.031324	14.138611
20.261325	886.592494	14.143629
20.466956	884.544049	14.148647
20.523038	887.217503	14.153664
20.428298	884.214906	14.158682
20.740312	894.777511	14.163699
20.699713	908.351426	14.168717
20.813271	910.222877	14.173735
20.568289	925.318344	14.178752
20.898060	917.605031	14.183770
21.087950	917.221856	14.188787
20.984768	928.242410	14.193805
21.121309	915.012386	14.198823
21.083749	907.957804	14.203840
20.855534	895.182396	14.208858
20.943338	894.165817	14.213875
20.973033	892.446680	14.218893
21.044296	884.445053	14.223911
20.820233	892.495981	14.228928
21.114979	893.478047	14.233946
20.920433	892.552122	14.238963
20.793032	902.056909	14.243981
21.453545	913.380379	14.248999
21.037666	917.468609	14.254016
21.013671	915.744661	14.259034
20.968935	917.098642	14.264051
20.659227	921.792885	14.269069
20.997525	920.882648	14.274087
21.019077	931.500260	14.279104
21.153926	930.695621	14.284122
21.360569	925.883861	14.289139
20.936162	931.799036	14.294157
21.225612	924.782741	14.299175
21.373747	924.801074	14.304192
21.132613	921.737658	14.309210
21.375359	923.855145	14.314227
21.278359	916.880828	14.319245
21.616263	921.500094	14.324263
21.048547	928.842902	14.329280
21.247612	923.186810	14.334298
21.299949	924.138326	14.339315
21.343164	919.190605	14.344333
21.253673	923.026208	14.349351
21.173033	928.243153	14.354368
21.112845	929.587801	14.359386
21.793419	943.798665	14.364403
21.343838	966.900070	14.369421
21.684231	954.190443	14.374439
21.707594	957.133409	14.379456
21.622522	949.342308	14.384474
21.693000	927.739756	14.389491
21.385162	941.925789	14.394509
21.774111	946.858620	14.399527
21.719350	948.608264	14.404544
21.562279	943.902489	14.409562
21.880651	947.301793	14.414579
21.656230	943.567138	14.419597
21.753552	937.990193	14.424615
21.609546	946.770099	14.429632
21.696080	952.608506	14.434650
21.935564	958.437466	14.439667
22.031419	957.550165	14.444685
21.470315	941.314290	14.449703
21.495055	948.333725	14.454720
21.767250	960.067610	14.459738
21.465684	962.283718	14.464755
21.367715	972.801654	14.469773
21.893625	957.574570	14.474791
21.974677	963.092157	14.479808
21.738562	968.447179	14.484826
21.853927	965.116096	14.489843
21.610039	972.387612	14.494861
21.646813	969.803703	14.499879
21.840714	978.134883	14.504896
21.838710	991.163932	14.509914
22.301603	994.998756	14.514931
22.148550	1001.459806	14.519949
22.525078	989.469587	14.524967
22.402638	993.921614	14.529984
22.052806	989.147464	14.535002
22.358862	971.764883	14.540019
22.231362	966.627287	14.545037
22.193917	969.258255	14.550055
22.174009	967.506121	14.555072
22.309203	972.343361	14.560090
22.112022	961.847092	14.565107
21.853034	989.532044	14.570125
22.386163	988.021264	14.575143
22.525322	995.479460	14.580160
22.238816	993.365556	14.585178
22.655085	990.187831	14.590195
22.649162	998.061659	14.595213
22.415554	971.266740	14.600231
22.444248	975.993547	14.605248
22.108046	972.755724	14.610266
22.484802	978.908880	14.615283
22.080435	996.364328	14.620301
22.518272	998.718138	14.625319
22.654967	996.351107	14.630336
22.514219	998.960016	14.635354
22.477535	996.740195	14.640371
22.558443	1000.012210	14.645389
22.630599	995.588411	14.650407
22.542334	1001.263586	14.655424
22.502751	994.807852	14.660442
22.664593	993.781816	14.665459
22.496099	997.754315	14.670477
22.384880	999.996700	14.675495
22.463109	997.464379	14.680512
22.445897	990.395500	14.685530
22.795087	996.406761	14.690547
22.495744	997.717983	14.695565
22.537592	996.073978	14.700583
22.759425	1008.927335	14.705600
22.812986	1017.886568	14.710618
23.242625	1006.781389	14.715635
22.963046	1002.796741	14.720653
23.186328	992.500028	14.725671
23.213818	976.866332	14.730688
22.651781	987.920789	14.735706
23.070012	983.005259	14.740723
22.938766	984.776545	14.745741
23.038115	983.525299	14.750759
23.190613	983.100107	14.755776
23.033702	981.848047	14.760794
23.186569	975.932662	14.765811
23.217819	981.717762	14.770829
23.151092	981.876550	14.775847
23.661899	983.379467	14.780864
23.336960	985.257156	14.785882
23.563100	979.875950	14.790899
23.541953	988.628420	14.795917
23.454045	986.981515	14.800935
23.475820	985.553082	14.805952
23.172003	975.767550	14.810970
23.294816	973.479820	14.815987
22.990607	979.696755	14.821005
23.058074	987.309534	14.826023
23.389551	986.880965	14.831040
23.221283	989.275600	14.836058
23.304002	983.640402	14.841075
23.163275	984.983743	14.846093
23.000500	986.451730	14.851111
23.337822	983.330646	14.856128
23.119976	996.748075	14.861146
23.459204	986.425007	14.866163
23.156748	986.903766	14.871181
22.991167	987.692619	14.876199
23.361767	1001.944329	14.881216
23.522917	1014.911194	14.886234
23.858038	1007.114393	14.891251
23.695779	1015.196432	14.896269
23.851346	1016.284867	14.901287
23.702926	994.153957	14.906304
23.392817	1000.063513	14.911322
23.641977	1006.027023	14.916339
23.661046	1019.176224	14.921357
23.739888	1022.496554	14.926375
23.708365	1022.317014	14.931392
23.619617	1025.025393	14.936410
23.744650	1024.920775	14.941427
23.614872	1022.615906	14.946445
23.565639	1020.304483	14.951463
23.697592	1026.356698	14.956480
23.778380	1019.332739	14.961498
24.095045	1014.847125	14.966515
24.123869	1021.843921	14.971533
24.095679	1014.767342	14.976551
24.194058	1013.755360	14.981568
24.041928	1023.746328	14.986586
23.850050	1018.154128	14.991603
23.777633	1022.618636	14.996621
23.926919	1022.131032	15.001639
24.013492	1010.655829	15.006656
24.020161	1013.009981	15.011674
23.926316	1019.742396	15.016691
24.157785	1018.613226	15.021709
23.622811	1020.091815	15.026727
24.453639	1021.140977	15.031744
23.829685	1026.776542	15.036762
24.223546	1019.962210	15.041779
24.131905	1019.040314	15.046797
24.220617	1022.814484	15.051815
24.420238	1027.415726	15.056832
24.127728	1039.322332	15.061850
24.744422	1033.859150	15.066867
24.198449	1031.659989	15.071885
24.241426	1022.760620	15.076903
24.694052	1027.370274	15.081920
24.115247	1033.006504	15.086938
24.350478	1042.203419	15.091955
24.598875	1046.860598	15.096973
24.236176	1059.723069	15.101991
24.372586	1052.860118	15.107008
24.263275	1060.221117	15.112026
24.580522	1052.390175	15.117043
24.601790	1052.346941	15.122061
24.352676	1052.121878	15.127079
24.684463	1047.530018	15.132096
24.611694	1053.143750	15.137114
24.578511	1047.468022	15.142131
24.687751	1052.188298	15.147149
24.562741	1052.518413	15.152167
24.781304	1049.376144	15.157184
24.683556	1055.856713	15.162202
24.834381	1054.888276	15.167219
24.607570	1051.069026	15.172237
24.598266	1059.134559	15.177255
24.439205	1049.427355	15.182272
24.516107	1051.988974	15.187290
24.576700	1044.132901	15.192307
24.916137	1058.150524	15.197325
25.217868	1066.435453	15.202343
25.038857	1053.672509	15.207360
24.738684	1056.850367	15.212378
24.846811	1053.396143	15.217395
25.189485	1064.975718	15.222413
24.867835	1065.563726	15.227431
25.153668	1066.503966	15.232448
25.181402	1070.221017	15.237466
25.024937	1065.207562	15.242483
25.268070	1061.200877	15.247501
24.901625	1070.493776	15.252519
25.242939	1072.423307	15.257536
25.191615	1081.290764	15.262554
25.048090	1080.708280	15.267571
25.039820	1091.520325	15.272589
24.793887	1087.090600	15.277607
24.958937	1082.441161	15.282624
25.060659	1089.308379	15.287642
25.033909	1086.212307	15.292659
25.357303	1085.711089	15.297677
25.181695	1089.978919	15.302695
25.454008	1079.356556	15.307712
25.588173	1077.745011	15.312730
25.237635	1082.657401	15.317747
25.492112	1084.883159	15.322765
25.294276	1092.014460	15.327783
25.622313	1078.932294	15.332800
25.641131	1085.681377	15.337818
25.556053	1085.908378	15.342835
25.684321	1081.522010	15.347853
25.275013	1089.192796	15.352871
25.679377	1073.251120	15.357888
25.576018	1080.837708	15.362906
25.834896	1080.095082	15.367923
25.946811	1084.460992	15.372941
25.625062	1086.428638	15.377959
25.797378	1075.703456	15.382976
25.709014	1080.292442	15.387994
25.822758	1087.434610	15.393011
25.936301	1070.844791	15.398029
25.993471	1068.790898	15.403047
26.363565	1068.412800	15.408064
26.337511	1069.807862	15.413082
26.349279	1073.680839	15.418099
26.385922	1071.913380	15.423117
26.290332	1070.192968	15.428135
26.077710	1062.745424	15.433152
26.266375	1042.040977	15.438170
25.958413	1042.224871	15.443187
26.135921	1034.109469	15.448205
25.857941	1038.788464	15.453223
25.767686	1036.997988	15.458240
25.772796	1053.423091	15.463258
25.888199	1063.597943	15.468275
26.431871	1057.230061	15.473293
26.168870	1070.646108	15.478311
25.972283	1068.486388	15.483328
26.203378	1066.081479	15.488346
25.958320	1067.719123	15.493363
26.359485	1064.638179	15.498381
25.969907	1069.531622	15.503399
26.425666	1072.484302	15.508416
26.074085	1067.263640	15.513434
26.306708	1061.926204	15.518451
26.296378	1058.604137	15.523469
26.216890	1071.315262	15.528487
26.513190	1069.958659	15.533504
25.957613	1069.974395	15.538522
25.933853	1072.209134	15.543539
26.430428	1078.649193	15.548557
26.600891	1100.314766	15.553575
26.857367	1098.900801	15.558592
26.592982	1098.386359	15.563610
26.846466	1099.655823	15.568627
26.872324	1072.935743	15.573645
26.656443	1076.587039	15.578663
26.820244	1063.972340	15.583680
26.700011	1061.994723	15.588698
26.400323	1066.280764	15.593715
26.711099	1075.041696	15.598733
26.645470	1088.941474	15.603751
26.910272	1089.085926	15.608768
27.032141	1094.396481	15.613786
26.710483	1085.129703	15.618803
27.166565	1088.828778	15.623821
26.451690	1084.904097	15.628839
26.529194	1087.788115	15.633856
26.775548	1091.847850	15.638874
26.860470	1095.204195	15.643891
27.270901	1088.565738	15.648909
26.986297	1098.964087	15.653927
27.292789	1093.878355	15.658944
27.171853	1097.277759	15.663962
27.030487	1102.666483	15.668979
27.355443	1096.106154	15.673997
27.064908	1094.535603	15.679015
27.139678	1084.922435	15.684032
27.266805	1090.279343	15.689050
27.034363	1096.835686	15.694067
27.094974	1095.116314	15.699085
27.082855	1103.131193	15.704103
27.461999	1092.127605	15.709120
27.560440	1094.722764	15.714138
27.275133	1097.556893	15.719155
27.384081	1082.384386	15.724173
27.267219	1091.321294	15.729191
27.140784	1096.273454	15.734208
27.262402	1092.719536	15.739226
27.067238	1099.495677	15.744243
27.408732	1092.532353	15.749261
27.115541	1096.833884	15.754279
27.320481	1100.162435	15.759296
27.411493	1092.442279	15.764314
27.324295	1096.495437	15.769331
27.468890	1112.365859	15.774349
27.422823	1123.128897	15.779367
27.727302	1132.804065	15.784384
27.862932	1126.510674	15.789402
27.651889	1122.831258	15.794419
27.633350	1124.549975	15.799437
27.715706	1128.712174	15.804455
27.954640	1123.063019	15.809472
27.815640	1124.863874	15.814490
27.914195	1136.531997	15.819507
27.978488	1126.153576	15.824525
28.002036	1129.434769	15.829543
27.958339	1131.675843	15.834560
27.897210	1133.210221	15.839578
27.739525	1130.656513	15.844595
27.715805	1124.817214	15.849613
27.751325	1129.682202	15.854631
27.795410	1123.419145	15.859648
27.855237	1125.352679	15.864666
27.790201	1131.574005	15.869683
28.102120	1130.595601	15.874701
28.104117	1128.934341	15.879719
27.870248	1120.392118	15.884736
27.857775	1133.876023	15.889754
27.791693	1145.380063	15.894771
28.293634	1148.630579	15.899789
28.273558	1161.307137	15.904807
28.191821	1162.631646	15.909824
28.306193	1157.732274	15.914842
28.268984	1171.713332	15.919859
28.425505	1163.968532	15.924877
28.408535	1169.472728	15.929895
28.830384	1162.183504	15.934912
28.797000	1154.960598	15.939930
28.285108	1163.350183	15.944947
28.802254	1155.892382	15.949965
28.612492	1153.865277	15.954983
28.498491	1144.906708	15.960000
28.529640	1137.904766	15.965018
28.446864	1146.966840	15.970035
28.597396	1143.981701	15.975053
28.659814	1153.700997	15.980071
28.777811	1157.484690	15.985088
28.807306	1155.454862	15.990106
28.430485	1164.429344	15.995123
28.684419	1155.160384	16.000141
28.693904	1163.725591	16.005159
28.603611	1149.662383	16.010176
28.738156	1155.492428	16.015194
28.678472	1161.616167	16.020211
28.902754	1155.364469	16.025229
28.792441	1154.992989	16.030247
28.776192	1156.322784	16.035264
28.965117	1143.858174	16.040282
28.896453	1156.192458	16.045299
29.098381	1151.760498	16.050317
28.739308	1157.264982	16.055335
28.684151	1155.297423	16.060352
29.110143	1157.755402	16.065370
28.877305	1155.046139	16.070387
28.803628	1154.635780	16.075405
28.899384	1171.779633	16.080423
29.255025	1179.751630	16.085440
29.371907	1186.458377	16.090458
29.308721	1191.724546	16.095475
29.638619	1187.546676	16.100493
29.345043	1192.424060	16.105511
29.247506	1185.638475	16.110528
29.620824	1182.237099	16.115546
29.598430	1180.552193	16.120563
29.403769	1163.139915	16.125581
29.362888	1162.346775	16.130599
29.041877	1151.474478	16.135616
29.384045	1165.068599	16.140634
29.306310	1189.297969	16.145651
29.539869	1186.865118	16.150669
29.876426	1180.611234	16.155687
29.755458	1189.602343	16.160704
29.753121	1190.810364	16.165722
29.682502	1189.465079	16.170739
29.858106	1203.347727	16.175757
29.439712	1190.869037	16.180775
29.788369	1181.074473	16.185792
29.867149	1185.109836	16.190810
29.693098	1185.778919	16.195827
29.803094	1170.868865	16.200845
29.881208	1177.146822	16.205863
29.865653	1184.205834	16.210880
30.274036	1180.684027	16.215898
29.828706	1189.908566	16.220915
30.064847	1188.495476	16.225933
29.978522	1192.457281	16.230951
29.798352	1186.370759	16.235968
30.181943	1184.665147	16.240986
29.844102	1188.811794	16.246003
30.121906	1181.592728	16.251021
30.297606	1189.168686	16.256039
29.974174	1196.136800	16.261056
29.966591	1186.185893	16.266074
30.402505	1190.257111	16.271091
30.312550	1181.844491	16.276109
30.507771	1190.043440	16.281127
30.609646	1191.753186	16.286144
30.402381	1178.027951	16.291162
30.439354	1182.541919	16.296179
30.141007	1166.294557	16.301197
30.385613	1178.560016	16.306215
30.105526	1180.255172	16.311232
30.535623	1182.663734	16.316250
30.430018	1189.332817	16.321267
30.517689	1180.515104	16.326285
30.278038	1183.194093	16.331303
30.068920	1180.905785	16.336320
30.434580	1185.412164	16.341338
30.423307	1178.586867	16.346355
30.627407	1178.264346	16.351373
30.745946	1179.379937	16.356391
30.685168	1183.461941	16.361408
30.539499	1186.734741	16.366426
30.348741	1187.445817	16.371443
30.343489	1183.824017	16.376461
30.482976	1189.565193	16.381479
30.745092	1197.488405	16.386496
30.732531	1193.231439	16.391514
30.513825	1201.155045	16.396531
30.534305	1200.457515	16.401549
30.975529	1194.637633	16.406567
30.843440	1206.302483	16.411584
31.179454	1197.793598	16.416602
31.117139	1205.437416	16.421619
31.181364	1198.245328	16.426637
31.339843	1201.097576	16.431655
30.879648	1197.708793	16.436672
31.273329	1191.196453	16.441690
31.160786	1206.529079	16.446707
31.107696	1205.125150	16.451725
31.288782	1193.448314	16.456743
30.885678	1205.872162	16.461760
31.287462	1199.409652	16.466778
31.167433	1202.662635	16.471795
31.291294	1198.180188	16.476813
31.300651	1203.857963	16.481831
31.451527	1212.683810	16.486848
31.664961	1214.861862	16.491866
31.396792	1212.671063	16.496883
31.506488	1204.998207	16.501901
31.847727	1203.983660	16.506919
31.459213	1199.846432	16.511936
31.397871	1195.537467	16.516954
31.545143	1198.113845	16.521971
31.507379	1209.236655	16.526989
31.732891	1207.907062	16.532007
31.706018	1219.170511	16.537024
32.142165	1212.420924	16.542042
31.860282	1213.133164	16.547059
31.632746	1198.685143	16.552077
32.000353	1184.840683	16.557095
31.617296	1193.389073	16.562112
31.769118	1190.919705	16.567130
32.115831	1201.336205	16.572147
32.065643	1199.850011	16.577165
32.006902	1185.437221	16.582183
31.514502	1203.105170	16.587200
31.911395	1209.602875	16.592218
31.943595	1228.129488	16.597235
31.908243	1225.119707	16.602253
32.340619	1214.839043	16.607271
32.068771	1223.151834	16.612288
32.293589	1216.711249	16.617306
31.926444	1221.490258	16.622323
32.300420	1222.650061	16.627341
32.058384	1220.924671	16.632359
31.766867	1217.129069	16.637376
32.568244	1220.344429	16.642394
32.262079	1221.482927	16.647411
32.024992	1219.655282	16.652429
32.536303	1214.278848	16.657447
32.269054	1218.089393	16.662464
32.326238	1217.250719	16.667482
32.430413	1226.571694	16.672499
32.399238	1223.398429	16.677517
32.725505	1218.568280	16.682535
32.457791	1222.466209	16.687552
32.476685	1218.008363	16.692570
32.453124	1224.253003	16.697587
32.891876	1240.061703	16.702605
32.970679	1228.040905	16.707623
32.516161	1219.124802	16.712640
32.568218	1228.520162	16.717658
32.520605	1239.774350	16.722675
32.588832	1248.091908	16.727693
32.804594	1247.976752	16.732711
32.583946	1250.210672	16.737728
32.670810	1238.918513	16.742746
32.735899	1246.442139	16.747763
32.562214	1245.934462	16.752781
32.938860	1244.900106	16.757799
32.560409	1247.699566	16.762816
32.755304	1257.630625	16.767834
33.118991	1271.301643	16.772851
33.050621	1274.557415	16.777869
33.481883	1270.283125	16.782887
33.287344	1281.648088	16.787904
33.552453	1277.032182	16.792922
33.196073	1266.111954	16.797939
33.144164	1275.244694	16.802957
33.562976	1267.646781	16.807975
33.417638	1260.551012	16.812992
33.288216	1242.285033	16.818010
33.131386	1253.836669	16.823027
33.311131	1264.533119	16.828045
33.628767	1269.087299	16.833063
33.412711	1274.838809	16.838080
33.892627	1272.043372	16.843098
33.846918	1266.235053	16.848115
33.233850	1252.233101	16.853133
33.624788	1260.363906	16.858151
33.554869	1269.666268	16.863168
33.859190	1274.671704	16.868186
33.984732	1266.412654	16.873203
33.874687	1257.001108	16.878221
33.614659	1248.633667	16.883239
33.649610	1253.745770	16.888256
33.904891	1257.242520	16.893274
33.777856	1271.723314	16.898291
33.657121	1280.358912	16.903309
33.980124	1277.396579	16.908327
33.741859	1279.815797	16.913344
33.894670	1273.385886	16.918362
33.961176	1276.915895	16.923379
34.053437	1275.322811	16.928397
34.370973	1267.086626	16.933415
33.985944	1280.462548	16.938432
34.218670	1271.907169	16.943450
34.242288	1262.757465	16.948467
34.129297	1273.217448	16.953485
34.442556	1275.776805	16.958503
34.376691	1280.783865	16.963520
34.153452	1270.297821	16.968538
34.341648	1270.658216	16.973555
34.475275	1280.967964	16.978573
34.504850	1274.504221	16.983591
33.860630	1283.659073	16.988608
34.301938	1278.960004	16.993626
34.289040	1270.280982	16.998643
34.386194	1278.532591	17.003661
34.316803	1274.705479	17.008679
34.410246	1276.868856	17.013696
34.229486	1285.228507	17.018714
34.506726	1288.739067	17.023731
34.478177	1298.226771	17.028749
34.858872	1294.762841	17.033767
34.651063	1299.726475	17.038784
34.695884	1298.514576	17.043802
34.732207	1296.002259	17.048819
34.654237	1303.324559	17.053837
35.043148	1294.193657	17.058855
35.166407	1294.326866	17.063872
34.952343	1295.208416	17.068890
35.025356	1298.741326	17.073907
35.014665	1299.662018	17.078925
35.193259	1296.698329	17.083943
34.902391	1301.153716	17.088960
34.678051	1294.798894	17.093978
34.945185	1294.515871	17.098995
34.855284	1297.727101	17.104013
35.046328	1290.691718	17.109031
35.278092	1290.991678	17.114048
35.371110	1280.857122	17.119066
35.521049	1288.026652	17.124083
35.239859	1292.610276	17.129101
35.368030	1278.521538	17.134119
35.513967	1288.056131	17.139136
34.945449	1279.889682	17.144154
35.534018	1275.814473	17.149171
35.529245	1291.805662	17.154189
35.492110	1282.251901	17.159207
35.526358	1287.197375	17.164224
35.571244	1292.667370	17.169242
36.037826	1289.747419	17.174259
35.459841	1303.317743	17.179277
35.633262	1290.317469	17.184295
35.685221	1303.561576	17.189312
35.927496	1306.430370	17.194330
35.866123	1300.931297	17.199347
35.543241	1305.815753	17.204365
35.669828	1319.397995	17.209383
35.979314	1322.131008	17.214400
35.870793	1323.352043	17.219418
36.158661	1321.858327	17.224435
35.838462	1325.756787	17.229453
35.921250	1316.328606	17.234471
35.990832	1317.664390	17.239488
35.328695	1316.974260	17.244506
36.088739	1323.058567	17.249523
35.970121	1321.703620	17.254541
35.896451	1321.893409	17.259559
36.129138	1313.401724	17.264576
36.033319	1320.647435	17.269594
36.448653	1322.644641	17.274611
36.213744	1342.779277	17.279629
36.721635	1337.060400	17.284647
36.450979	1332.459923	17.289664
36.328807	1327.857790	17.294682
36.597529	1326.405669	17.299699
36.069354	1326.140945	17.304717
36.485680	1333.415099	17.309735
36.682700	1353.694808	17.314752
36.613583	1349.451536	17.319770
36.887338	1336.675908	17.324787
36.503591	1353.648684	17.329805
36.847349	1345.137693	17.334823
37.267966	1347.147431	17.339840
36.841556	1329.522572	17.344858
36.768144	1324.390379	17.349875
36.660594	1318.591903	17.354893
36.625205	1323.032506	17.359911
37.085666	1330.624473	17.364928
37.167329	1334.612223	17.369946
36.760723	1323.347577	17.374963
36.772388	1321.831055	17.379981
36.880400	1334.589588	17.384999
36.793485	1340.671337	17.390016
36.441083	1349.597988	17.395034
36.868604	1345.460351	17.400051
36.929159	1351.228339	17.405069
37.012358	1334.398436	17.410087
36.897287	1341.843872	17.415104
36.943568	1360.609885	17.420122
37.164912	1360.677896	17.425139
37.431112	1371.061739	17.430157
37.598037	1365.442853	17.435175
37.648617	1367.834108	17.440192
37.617789	1372.760887	17.445210
37.995182	1361.986270	17.450227
37.773614	1353.889507	17.455245
37.662066	1340.585399	17.460263
37.602758	1343.669055	17.465280
37.462038	1341.281716	17.470298
37.749501	1337.324520	17.475315
37.474569	1340.433913	17.480333
37.570068	1332.705048	17.485351
37.793896	1348.117104	17.490368
37.900608	1360.382687	17.495386
38.075220	1358.526330	17.500403
38.254014	1356.497832	17.505421
37.845534	1346.834142	17.510439
37.891597	1336.345213	17.515456
37.799397	1343.037399	17.520474
38.198126	1344.315183	17.525491
37.870289	1346.219334	17.530509
38.155806	1363.086951	17.535527
38.526328	1373.819914	17.540544
38.005219	1360.371096	17.545562
38.209306	1355.769618	17.550579
38.157655	1363.893201	17.555597
38.554511	1361.846442	17.560615
38.217491	1362.253638	17.565632
38.065884	1376.976787	17.570650
38.492520	1366.791321	17.575667
38.069118	1376.039222	17.580685
38.128020	1381.846814	17.585703
38.388825	1371.437664	17.590720
38.226457	1380.275818	17.595738
38.258234	1374.790964	17.600755
38.305499	1381.588349	17.605773
38.484063	1376.211441	17.610791
38.425075	1376.343041	17.615808
38.227504	1381.196523	17.620826
38.571183	1383.906003	17.625843
38.542553	1403.994452	17.630861
38.603268	1397.809642	17.635879
38.834837	1400.264851	17.640896
38.741784	1407.014622	17.645914
38.731463	1404.909306	17.650931
38.732296	1401.312439	17.655949
38.881376	1397.461461	17.660967
38.750777	1405.010087	17.665984
38.799454	1404.120059	17.671002
38.961525	1391.064872	17.676019
38.826956	1405.244169	17.681037
39.106296	1412.365591	17.686055
39.213372	1417.300281	17.691072
39.166943	1423.059404	17.696090
39.458742	1418.085238	17.701107
39.446841	1425.770685	17.706125
39.424592	1419.547971	17.711143
39.856893	1424.824080	17.716160
39.590723	1410.334029	17.721178
39.855638	1390.620598	17.726195
39.754816	1392.498773	17.731213
39.311498	1393.700060	17.736231
39.629870	1389.146417	17.741248
39.130339	1389.842249	17.746266
39.612407	1395.527295	17.751283
39.789871	1404.146082	17.756301
39.721878	1419.154836	17.761319
39.863032	1411.905539	17.766336
39.551608	1414.823336	17.771354
40.040878	1407.748986	17.776371
39.983920	1418.366103	17.781389
39.769381	1420.571543	17.786407
40.131138	1418.701848	17.791424
39.759015	1415.582919	17.796442
39.617470	1417.525012	17.801459
39.837597	1416.976543	17.806477
39.475481	1419.653082	17.811495
39.686447	1416.961082	17.816512
39.916878	1425.456594	17.821530
40.085199	1431.286083	17.826547
39.941596	1446.208602	17.831565
40.289313	1454.517098	17.836583
40.596413	1446.704870	17.841600
40.524529	1455.280866	17.846618
40.732711	1450.643309	17.851635
40.647157	1437.400254	17.856653
40.271621	1421.575509	17.861671
40.520096	1418.142077	17.866688
40.166769	1441.401138	17.871706
40.708695	1434.679416	17.876723
40.782856	1440.792149	17.881741
40.716786	1444.872711	17.886759
41.217344	1441.042749	17.891776
40.810809	1432.734750	17.896794
40.628008	1418.901557	17.901811
40.652141	1418.835842	17.906829
40.801982	1436.641545	17.911847
41.223641	1439.556481	17.916864
40.865532	1429.375786	17.921882
40.755950	1424.184828	17.926899
41.052025	1438.009159	17.931917
41.182707	1442.929867	17.936935
41.117274	1438.031548	17.941952
41.326522	1428.082862	17.946970
41.059126	1419.145442	17.951987
41.067758	1421.608682	17.957005
40.835121	1438.287659	17.962023
40.995500	1434.579600	17.967040
40.965629	1443.603530	17.972058
41.136207	1446.015774	17.977075
41.602449	1435.009051	17.982093
41.111894	1444.900112	17.987111
41.289583	1429.142080	17.992128
41.141229	1440.781395	17.997146
41.249056	1440.881671	18.002163
41.385132	1453.039607	18.007181
41.588578	1464.210664	18.012199
41.825555	1461.560915	18.017216
41.838479	1474.161690	18.022234
42.111237	1467.843135	18.027251
42.109358	1448.015648	18.032269
41.603196	1442.102144	18.037287
41.732227	1437.813084	18.042304
41.697467	1445.615454	18.047322
41.958104	1454.578899	18.052339
42.003837	1463.083440	18.057357
41.916264	1471.390579	18.062375
42.219662	1466.109355	18.067392
41.896966	1470.071964	18.072410
41.847054	1463.848137	18.077427
42.285596	1469.540941	18.082445
41.856244	1474.225336	18.087463
42.170438	1466.147676	18.092480
42.053296	1473.027172	18.097498
41.985241	1466.553745	18.102515
41.867198	1466.167757	18.107533
41.863116	1485.428069	18.112551
42.591630	1487.561768	18.117568
42.531372	1501.327364	18.122586
42.593944	1497.878728	18.127603
43.000158	1495.850124	18.132621
42.636050	1495.984767	18.137639
43.093347	1497.304353	18.142656
42.691864	1487.497081	18.147674
42.473485	1478.871944	18.152691
42.724408	1485.912985	18.157709
42.745205	1494.600076	18.162727
43.013676	1495.395238	18.167744
42.785053	1500.441704	18.172762
42.683582	1497.751538	18.177779
42.944756	1489.879753	18.182797
42.775175	1493.612651	18.187815
42.967787	1479.902798	18.192832
43.079310	1486.115780	18.197850
43.205553	1487.902693	18.202867
43.519326	1484.782116	18.207885
43.018290	1489.588070	18.212903
43.233512	1476.755584	18.217920
43.264940	1480.428889	18.222938
43.156309	1483.039840	18.227955
43.314461	1483.942267	18.232973
43.527272	1487.708565	18.237991
43.521909	1487.336855	18.243008
43.310263	1478.369269	18.248026
43.352515	1481.054477	18.253043
43.306590	1485.430738	18.258061
42.943549	1482.714647	18.263079
43.553178	1490.544839	18.268096
43.846597	1510.250921	18.273114
43.638480	1513.812203	18.278131
43.997864	1506.307810	18.283149
43.757263	1512.240307	18.288167
43.725905	1508.723273	18.293184
43.925035	1513.493863	18.298202
43.793996	1514.303977	18.303219
44.122790	1513.699631	18.308237
43.482826	1520.037202	18.313255
43.722299	1517.925067	18.318272
43.709689	1518.053991	18.323290
43.880692	1513.047932	18.328307
44.189710	1523.298416	18.333325
43.688650	1533.683612	18.338343
44.264020	1537.948999	18.343360
44.247146	1545.155487	18.348378
44.546703	1539.537406	18.353395
44.532147	1533.369263	18.358413
44.331658	1544.479739	18.363431
44.527017	1527.843316	18.368448
44.553238	1536.325054	18.373466
44.554615	1536.836387	18.378483
44.671906	1533.080115	18.383501
44.814975	1540.811699	18.388519
44.856751	1531.273505	18.393536
44.812015	1534.463425	18.398554
44.634986	1534.067964	18.403571
44.990311	1536.416936	18.408589
45.124058	1533.000202	18.413607
45.185283	1530.361954	18.418624
45.272988	1531.983543	18.423642
44.771684	1532.870016	18.428659
45.230017	1532.015327	18.433677
45.056759	1541.315466	18.438695
45.385691	1539.889118	18.443712
45.445411	1533.982859	18.448730
45.256529	1518.259598	18.453747
45.382499	1512.449757	18.458765
45.096478	1515.076420	18.463783
45.493862	1517.807251	18.468800
45.124956	1517.188328	18.473818
44.854992	1528.773956	18.478835
45.357638	1531.049875	18.483853
45.530680	1534.667572	18.488871
45.123466	1539.697699	18.493888
45.183364	1541.534529	18.498906
45.032793	1536.186459	18.503923
45.468078	1540.665328	18.508941
45.298677	1560.147964	18.513959
45.375366	1564.900344	18.518976
45.568285	1564.906818	18.523994
45.295661	1569.427022	18.529011
45.336658	1573.396153	18.534029
45.797587	1572.309006	18.539047
45.803662	1578.646607	18.544064
46.387622	1575.458536	18.549082
46.488329	1575.257900	18.554099
46.647730	1561.944986	18.559117
46.316136	1562.115346	18.564135
46.142602	1561.968675	18.569152
46.543421	1552.718514	18.574170
46.462573	1552.063873	18.579187
46.415484	1550.188576	18.584205
46.286567	1554.561575	18.589223
46.255926	1554.887662	18.594240
46.574910	1555.592967	18.599258
46.632171	1550.948773	18.604275
46.530647	1541.554561	18.609293
46.569029	1546.405861	18.614311
46.772272	1550.499347	18.619328
46.690121	1541.956275	18.624346
46.596184	1553.736451	18.629363
46.587962	1543.517963	18.634381
46.558631	1553.571512	18.639399
46.384412	1551.996515	18.644416
46.835439	1562.834766	18.649434
46.623290	1573.730814	18.654451
47.173527	1566.782744	18.659469
47.170577	1570.766749	18.664487
47.099447	1574.497337	18.669504
47.319249	1575.076877	18.674522
47.059098	1574.870081	18.679539
47.550424	1564.103889	18.684557
47.145964	1566.800579	18.689575
47.156365	1567.199564	18.694592
47.239848	1572.754752	18.699610
47.369565	1568.666124	18.704627
47.561566	1566.987095	18.709645
47.510707	1571.440467	18.714663
47.231409	1565.106875	18.719680
47.480592	1569.251247	18.724698
47.493358	1566.066178	18.729715
47.539607	1578.107186	18.734733
47.262864	1573.451755	18.739751
47.361501	1564.058642	18.744768
47.720602	1579.189011	18.749786
47.502031	1597.964534	18.754803
47.932039	1593.808341	18.759821
47.663132	1597.002563	18.764839
47.639423	1601.619157	18.769856
48.034272	1594.024112	18.774874
47.625318	1605.377114	18.779891
48.077052	1605.288036	18.784909
47.784347	1606.323731	18.789927
47.723352	1608.257722	18.794944
48.169187	1616.490883	18.799962
48.152263	1634.250272	18.804979
48.305725	1628.090689	18.809997
48.327443	1630.451980	18.815015
48.198023	1631.268134	18.820032
48.568772	1632.452085	18.825050
48.365160	1635.340145	18.830067
48.223035	1635.064969	18.835085
48.287287	1629.692042	18.840103
48.343835	1632.909091	18.845120
48.452246	1638.914189	18.850138
48.488408	1648.977809	18.855155
48.805589	1661.054334	18.860173
48.838881	1656.973980	18.865191
48.752540	1664.640749	18.870208
49.091917	1656.649426	18.875226
48.980007	1660.521833	18.880243
49.033632	1655.840430	18.885261
49.097650	1662.533803	18.890279
48.989683	1657.351157	18.895296
48.907764	1652.152559	18.900314
48.380944	1655.927527	18.905331
48.729733	1651.549869	18.910349
49.120991	1663.577611	18.915367
49.432226	1687.130659	18.920384
50.067532	1682.605825	18.925402
49.950725	1684.035084	18.930419
49.958791	1673.178343	18.935437
50.053337	1649.028627	18.940455
49.680763	1653.331966	18.945472
49.736611	1646.515409	18.950490
49.436372	1657.727618	18.955507
49.496135	1648.059839	18.960525
49.703296	1652.387919	18.965543
49.476848	1657.820307	18.970560
49.788300	1660.702524	18.975578
49.904433	1675.967708	18.980595
49.968545	1677.588357	18.985613
49.805660	1682.257849	18.990631
49.888298	1685.398383	18.995648
50.010537	1676.617334	19.000666
49.760577	1691.782817	19.005683
50.103930	1686.399966	19.010701
49.993631	1685.365372	19.015719
49.898660	1688.846510	19.020736
50.370273	1680.224477	19.025754
49.896117	1684.949120	19.030771
49.902720	1687.404862	19.035789
50.062432	1709.379041	19.040807
50.235668	1721.343279	19.045824
50.347929	1700.557268	19.050842
50.089963	1719.222027	19.055859
50.316236	1707.539148	19.060877
50.693252	1731.906125	19.065895
50.671078	1736.045841	19.070912
50.890172	1737.706279	19.075930
50.924118	1741.883455	19.080947
50.793700	1730.646809	19.085965
50.796050	1737.079464	19.090983
50.754693	1745.010474	19.096000
50.595830	1730.641430	19.101018
50.496559	1746.184885	19.106035
50.877212	1738.535396	19.111053
51.360328	1755.023494	19.116071
51.316891	1768.571918	19.121088
51.652514	1759.494851	19.126106
51.314154	1749.556198	19.131123
51.610139	1752.456632	19.136141
51.319014	1739.372730	19.141159
51.293319	1752.546251	19.146176
51.762552	1750.002570	19.151194
51.366949	1770.082403	19.156211
51.461381	1765.216686	19.161229
51.922139	1755.788507	19.166247
51.539446	1761.238772	19.171264
51.925353	1762.277158	19.176282
52.116308	1759.110824	19.181299
52.372215	1757.394838	19.186317
52.189799	1759.598351	19.191335
52.026232	1758.517186	19.196352
52.473140	1757.131785	19.201370
52.147576	1745.678473	19.206387
52.153812	1738.827310	19.211405
52.371543	1727.144204	19.216423
52.086056	1727.091684	19.221440
52.709228	1736.655076	19.226458
52.422900	1728.628999	19.231475
51.973549	1724.732579	19.236493
52.277558	1735.819374	19.241511
52.284569	1752.450261	19.246528
52.507222	1756.735786	19.251546
52.628597	1764.062706	19.256563
52.681611	1759.074595	19.261581
52.732821	1748.807155	19.266599
52.531856	1764.320440	19.271616
52.730513	1764.278804	19.276634
52.816767	1758.243154	19.281651
52.689890	1758.899231	19.286669
52.633627	1757.358887	19.291687
52.738153	1762.475018	19.296704
52.669209	1756.107007	19.301722
52.858092	1762.861532	19.306739
53.048451	1784.640581	19.311757
53.400379	1784.154459	19.316775
53.247198	1783.979367	19.321792
53.413973	1786.012350	19.326810
53.139768	1785.505738	19.331827
53.506642	1782.101322	19.336845
53.597467	1784.551514	19.341863
53.477357	1795.295393	19.346880
53.374823	1781.259484	19.351898
53.385755	1784.553063	19.356915
53.269964	1785.054773	19.361933
53.743831	1784.131521	19.366951
53.328829	1784.896478	19.371968
53.564880	1787.994475	19.376986
53.537923	1791.366465	19.382003
53.607208	1805.493186	19.387021
53.908291	1813.005424	19.392039
53.744213	1823.791733	19.397056
53.968959	1817.512937	19.402074
53.802269	1824.858300	19.407091
53.755429	1825.684892	19.412109
54.204429	1820.521122	19.417127
54.254116	1823.041596	19.422144
54.390048	1821.259784	19.427162
54.069119	1815.722466	19.432179
54.045041	1820.279406	19.437197
54.378856	1831.214426	19.442215
54.586492	1840.996760	19.447232
54.961995	1831.920368	19.452250
54.794356	1840.087098	19.457267
54.967795	1843.738632	19.462285
55.106760	1842.909692	19.467303
54.670666	1828.775909	19.472320
54.880849	1826.071374	19.477338
55.034043	1824.642352	19.482355
54.964078	1830.915890	19.487373
55.244866	1831.579320	19.492391
55.034217	1831.553407	19.497408
55.164192	1829.550724	19.502426
55.473142	1830.080661	19.507443
55.027427	1827.439829	19.512461
55.219552	1818.807228	19.517479
55.200083	1833.642697	19.522496
55.340477	1826.333535	19.527514
55.379700	1841.626890	19.532531
55.446416	1844.854164	19.537549
55.255602	1835.117674	19.542567
55.220503	1833.565294	19.547584
55.396503	1836.419594	19.552602
55.358975	1834.230456	19.557619
55.060383	1840.462588	19.562637
55.451024	1848.521407	19.567655
55.352704	1861.386463	19.572672
55.582181	1865.203691	19.577690
55.473257	1869.476843	19.582707
55.609513	1871.521785	19.587725
55.874586	1867.022906	19.592743
56.098999	1879.746834	19.597760
56.041730	1886.509997	19.602778
56.126545	1893.137232	19.607795
55.970497	1899.767487	19.612813
56.267984	1889.310431	19.617831
56.139984	1898.443897	19.622848
56.254810	1897.204265	19.627866
56.184014	1901.653050	19.632883
56.077645	1900.822331	19.637901
56.345595	1890.732607	19.642919
56.143083	1903.034592	19.647936
56.742808	1916.712626	19.652954
56.828950	1913.315196	19.657971
56.971954	1928.562200	19.662989
57.310158	1927.926448	19.668007
57.011972	1920.590434	19.673024
57.131519	1914.665041	19.678042
57.473269	1919.752046	19.683059
57.025250	1900.866653	19.688077
57.198464	1888.834974	19.693095
57.005517	1905.751212	19.698112
57.264100	1908.009484	19.703130
57.151230	1905.929890	19.708147
57.187815	1907.959269	19.713165
57.428620	1905.713932	19.718183
57.586257	1914.202462	19.723200
57.457183	1912.016114	19.728218
57.627982	1906.110082	19.733235
57.240526	1905.807952	19.738253
57.875214	1901.040878	19.743271
57.466629	1912.406643	19.748288
57.745839	1910.536682	19.753306
57.832390	1910.837006	19.758323
57.341540	1911.842180	19.763341
57.531077	1922.546994	19.768359
57.902494	1926.454872	19.773376
58.104579	1936.027345	19.778394
58.310486	1934.876229	19.783411
58.615203	1936.282335	19.788429
58.410250	1925.152605	19.793447
58.421219	1934.554187	19.798464
58.423454	1930.066530	19.803482
59.158341	1918.978059	19.808499
59.149609	1902.748183	19.813517
58.966732	1880.978536	19.818535
59.147916	1879.068364	19.823552
59.163087	1877.172870	19.828570
59.331094	1876.116689	19.833587
58.917716	1864.532552	19.838605
58.853101	1839.887961	19.843623
58.641248	1847.843072	19.848640
58.792948	1841.286448	19.853658
59.064676	1850.139819	19.858675
58.916392	1870.893006	19.863693
59.243913	1870.421000	19.868711
59.326811	1878.722420	19.873728
58.988079	1879.798510	19.878746
59.018121	1865.850713	19.883763
58.970153	1881.329495	19.888781
59.195485	1881.571501	19.893799
59.124416	1880.267912	19.898816
58.908273	1887.324645	19.903834
59.078837	1879.312142	19.908851
59.015694	1894.973490	19.913869
59.355315	1902.061157	19.918887
59.551669	1906.756021	19.923904
59.392341	1916.500179	19.928922
59.661701	1911.066119	19.933939
59.322234	1918.185797	19.938957
59.597478	1919.863261	19.943975
59.734915	1947.250035	19.948992
59.795826	1942.014395	19.954010
60.043137	1944.712609	19.959027
59.517736	1950.588443	19.964045
59.647354	1946.051362	19.969063
59.999018	1947.840138	19.974080
60.247779	1964.370570	19.979098
60.404375	1970.741759	19.984115
60.308460	1973.793627	19.989133
60.631504	1967.781483	19.994151
60.457972	1975.618067	19.999168
60.320387	1977.691751	20.004186
60.799760	1965.995832	20.009203
60.695635	1966.690766	20.014221
60.718923	1964.826216	20.019239
60.694446	1967.521371	20.024256
60.802492	1958.681848	20.029274
61.007135	1964.384622	20.034291
60.576683	1971.879889	20.039309
61.232179	1980.612353	20.044327
61.269049	1983.444822	20.049344
61.009630	1987.019904	20.054362
61.444455	1986.725861	20.059379
61.326343	1996.281792	20.064397
61.330860	1987.719917	20.069415
61.319081	1997.682871	20.074432
61.290218	1987.295884	20.079450
61.314989	1984.418734	20.084467
61.538826	1982.000678	20.089485
61.568468	1977.906658	20.094503
61.645833	1986.580300	20.099520
61.592772	1986.964247	20.104538
61.714393	1983.450232	20.109555
61.950704	1983.092669	20.114573
62.004172	1978.656608	20.119591
62.184282	1974.063483	20.124608
62.116921	1981.935054	20.129626
62.158413	1981.463039	20.134643
61.944460	1991.359907	20.139661
62.432852	1997.446929	20.144679
62.311690	1998.061987	20.149696
62.374808	2010.444409	20.154714
62.419438	2002.135708	20.159731
62.018090	2017.313871	20.164749
62.423369	2005.690307	20.169767
62.623560	2007.660570	20.174784
62.604260	2003.127555	20.179802
62.493014	2001.047688	20.184819
62.471934	2016.472768	20.189837
62.667075	2003.285905	20.194855
62.669555	2017.536757	20.199872
62.863247	2036.753669	20.204890
63.000274	2040.105856	20.209907
63.155951	2040.477753	20.214925
63.224498	2036.620574	20.219943
63.378638	2038.705165	20.224960
63.235888	2040.586176	20.229978
63.326968	2037.111629	20.234995
63.324096	2032.345509	20.240013
63.483302	2032.303086	20.245031
63.718868	2029.380509	20.250048
63.485607	2033.387999	20.255066
63.866417	2029.869607	20.260083
63.515357	2035.427412	20.265101
63.588412	2033.370850	20.270119
63.908767	2030.210567	20.275136
63.611572	2034.298262	20.280154
63.884623	2028.216192	20.285171
63.948729	2036.019628	20.290189
63.615647	2050.711041	20.295207
63.741836	2062.471465	20.300224
63.574339	2061.158853	20.305242
63.907620	2053.209980	20.310259
63.773144	2061.049033	20.315277
64.213336	2084.693072	20.320295
64.717472	2083.583269	20.325312
64.477866	2083.023144	20.330330
64.818144	2093.449968	20.335347
64.786874	2094.723247	20.340365
64.868878	2086.506864	20.345383
65.109675	2088.609106	20.350400
64.646097	2095.723491	20.355418
64.906018	2083.029657	20.360435
64.910849	2094.951052	20.365453
64.702026	2090.904471	20.370471
64.868921	2089.693490	20.375488
64.589628	2098.094488	20.380506
65.045809	2084.570940	20.385523
65.152066	2081.528959	20.390541
64.936536	2086.409134	20.395559
65.268723	2095.536194	20.400576
65.378956	2114.211956	20.405594
66.062067	2110.730288	20.410611
65.886783	2110.114280	20.415629
66.046861	2092.109417	20.420647
65.685145	2081.128852	20.425664
65.617163	2083.774330	20.430682
65.894904	2074.290970	20.435699
66.087616	2091.916797	20.440717
65.937824	2086.584918	20.445735
66.394319	2082.455831	20.450752
65.851257	2086.694450	20.455770
66.314461	2085.345753	20.460787
66.202816	2093.729452	20.465805
65.998212	2095.614827	20.470823
66.201739	2098.088790	20.475840
66.084487	2102.021160	20.480858
66.345986	2101.734306	20.485875
66.324366	2105.031576	20.490893
66.367496	2103.313301	20.495911
66.434175	2101.055588	20.500928
66.317194	2105.809926	20.505946
66.572316	2109.638862	20.510963
66.647248	2134.333153	20.515981
66.709590	2130.016770	20.520999
67.245734	2121.112809	20.526016
67.011207	2139.359819	20.531034
67.293431	2126.787462	20.536051
67.331196	2131.964713	20.541069
67.056876	2138.373234	20.546087
67.393038	2125.454031	20.551104
67.155727	2131.273765	20.556122
67.200345	2124.835565	20.561139
67.106818	2128.576946	20.566157
67.236348	2126.648235	20.571175
67.438873	2145.439111	20.576192
67.538821	2156.892297	20.581210
67.908973	2153.510087	20.586227
67.991807	2162.533006	20.591245
67.689267	2162.992928	20.596263
67.997066	2156.676358	20.601280
67.738030	2167.050144	20.606298
67.742249	2156.474479	20.611315
67.828404	2161.699087	20.616333
67.904487	2163.688378	20.621351
68.381120	2177.144801	20.626368
68.054929	2191.860426	20.631386
68.621135	2183.654869	20.636403
68.735379	2187.627432	20.641421
68.654788	2187.796309	20.646439
68.875468	2188.330899	20.651456
68.612522	2183.665989	20.656474
68.811770	2183.379622	20.661491
68.866482	2182.610512	20.666509
68.843119	2173.750912	20.671527
68.911650	2181.019608	20.676544
69.006082	2184.185114	20.681562
69.154313	2183.517508	20.686579
68.848160	2177.733842	20.691597
68.652507	2178.999520	20.696615
69.234282	2173.718488	20.701632
68.734765	2174.231063	20.706650
69.113998	2191.618811	20.711667
69.123160	2207.460896	20.716685
69.528062	2208.769245	20.721703
69.823042	2201.537503	20.726720
69.443707	2204.907576	20.731738
69.723407	2209.729264	20.736755
69.925679	2209.797180	20.741773
69.523175	2209.430578	20.746791
69.813162	2200.516269	20.751808
69.657665	2209.986267	20.756826
70.016758	2210.421696	20.761843
69.951102	2215.705145	20.766861
70.170371	2233.175090	20.771879
70.450851	2232.502910	20.776896
70.130688	2246.091189	20.781914
70.386507	2237.161069	20.786931
70.331856	2239.331690	20.791949
70.193817	2243.311464	20.796967
70.084263	2246.055635	20.801984
69.908011	2250.598433	20.807002
70.544323	2259.488306	20.812019
70.447261	2269.815880	20.817037
70.706169	2275.317401	20.822055
70.525416	2267.566024	20.827072
70.562631	2278.511713	20.832090
70.974451	2288.457654	20.837107
71.358810	2293.772411	20.842125
70.992799	2298.526409	20.847143
71.257920	2290.917874	20.852160
71.514025	2295.120348	20.857178
71.493731	2285.925877	20.862195
71.566132	2292.880935	20.867213
71.670046	2286.615705	20.872231
71.999354	2285.949108	20.877248
71.548506	2291.002964	20.882266
71.707978	2293.037971	20.887283
72.164064	2280.309536	20.892301
72.079896	2284.660668	20.897319
72.215880	2283.442802	20.902336
71.870438	2289.703832	20.907354
71.985315	2286.557387	20.912371
71.931898	2280.693255	20.917389
71.933262	2288.620893	20.922407
71.987937	2290.991195	20.927424
72.154846	2308.268991	20.932442
72.352664	2311.392079	20.937459
72.286918	2310.643745	20.942477
72.335961	2312.299907	20.947495
72.343548	2313.265731	20.952512
72.188060	2315.320292	20.957530
72.738872	2326.148711	20.962547
72.928178	2339.703024	20.967565
73.043530	2348.784588	20.972583
73.182022	2343.768487	20.977600
73.196679	2351.284994	20.982618
73.435756	2345.534662	20.987635
73.548243	2344.776781	20.992653
73.400235	2347.210093	20.997671
73.789416	2340.915078	21.002688
73.515982	2329.930472	21.007706
73.668188	2325.714547	21.012723
73.824019	2317.855188	21.017741
73.486547	2318.817045	21.022759
73.735371	2324.192760	21.027776
73.665587	2330.794506	21.032794
73.614985	2337.311386	21.037811
73.925494	2336.156932	21.042829
73.753755	2343.102179	21.047847
73.647131	2332.153898	21.052864
73.628625	2333.197041	21.057882
73.773242	2342.329784	21.062899
74.252150	2342.505403	21.067917
74.086111	2362.392895	21.072935
74.423727	2354.078960	21.077952
74.267067	2354.205692	21.082970
74.264850	2355.229720	21.087987
74.389437	2362.034897	21.093005
74.724070	2376.120639	21.098023
74.979259	2374.939606	21.103040
75.441557	2381.176480	21.108058
75.412048	2374.844387	21.113075
75.478413	2359.505076	21.118093
75.015118	2351.341683	21.123111
75.292144	2339.886195	21.128128
75.356241	2342.164541	21.133146
74.955149	2351.348920	21.138163
75.161941	2359.375989	21.143181
75.330398	2369.382036	21.148199
75.764406	2355.595897	21.153216
75.938570	2361.888153	21.158234
76.164484	2362.524965	21.163251
75.679572	2361.832463	21.168269
75.653114	2369.374415	21.173287
75.687560	2359.854942	21.178304
75.889488	2366.006686	21.183322
75.944855	2370.414254	21.188339
75.975146	2367.807534	21.193357
75.875518	2375.234512	21.198375
76.224713	2382.059728	21.203392
76.505078	2392.677247	21.208410
76.098978	2397.112792	21.213427
76.320137	2392.007189	21.218445
75.892092	2397.634042	21.223463
76.386576	2390.867541	21.228480
76.546439	2393.551468	21.233498
76.124614	2401.466421	21.238515
76.679082	2406.164120	21.243533
76.900047	2421.699700	21.248551
76.954877	2421.988575	21.253568
76.867689	2424.746518	21.258586
77.076649	2424.560861	21.263603
77.281900	2415.816476	21.268621
77.093682	2429.843273	21.273639
77.106288	2421.972088	21.278656
77.164114	2427.585972	21.283674
77.255986	2443.271169	21.288691
77.319670	2448.025911	21.293709
77.227021	2449.810094	21.298727
77.424681	2448.866353	21.303744
77.584768	2445.663892	21.308762
77.490745	2464.942985	21.313779
77.949087	2472.253496	21.318797
78.035268	2482.381297	21.323815
77.799700	2470.734493	21.328832
77.999717	2481.017985	21.333850
78.079303	2480.791602	21.338867
78.349740	2472.548099	21.343885
78.484290	2475.361153	21.348903
78.883985	2467.953682	21.353920
78.778630	2463.092063	21.358938
78.682190	2468.769896	21.363955
79.161107	2457.242789	21.368973
78.831554	2460.982562	21.373991
79.011083	2454.219849	21.379008
79.112577	2459.645070	21.384026
78.903853	2468.978196	21.389043
79.422062	2473.756430	21.394061
79.946228	2485.542618	21.399079
79.596570	2464.868519	21.404096
79.705303	2456.857696	21.409114
79.362890	2458.501573	21.414131
79.521953	2451.303971	21.419149
79.344492	2462.593180	21.424167
79.492984	2468.329495	21.429184
79.704163	2475.269588	21.434202
79.847337	2482.282675	21.439219
79.936577	2484.694694	21.444237
79.881716	2481.629553	21.449255
80.453592	2487.102484	21.454272
80.383959	2483.605477	21.459290
80.368418	2489.403357	21.464307
80.110647	2479.945354	21.469325
80.227079	2483.701326	21.474343
80.168147	2489.269349	21.479360
80.739370	2477.238220	21.484378
80.714944	2483.549613	21.489395
80.727031	2481.397304	21.494413
80.370887	2485.343488	21.499431
80.162963	2487.296306	21.504448
80.640322	2489.236594	21.509466
80.748184	2512.142973	21.514483
80.923000	2516.224749	21.519501
80.934449	2519.970726	21.524519
80.787925	2517.060217	21.529536
80.976376	2514.047517	21.534554
81.076422	2532.765558	21.539571
81.460143	2539.708846	21.544589
81.284863	2542.140246	21.549607
81.201828	2549.699966	21.554624
81.889324	2535.992804	21.559642
81.573517	2547.257729	21.564659
81.635866	2546.022479	21.569677
81.732141	2545.793434	21.574695
81.560428	2557.615925	21.579712
82.067092	2570.038216	21.584730
81.772581	2576.780533	21.589747
81.816028	2571.507336	21.594765
81.927137	2567.915407	21.599783
82.003309	2579.031316	21.604800
82.398650	2591.184255	21.609818
82.051744	2600.858877	21.614835
82.607870	2606.779603	21.619853
82.520061	2608.623604	21.624871
82.434932	2596.542868	21.629888
82.688851	2599.155983	21.634906
83.049554	2618.785186	21.639923
83.292873	2627.595578	21.644941
83.430342	2625.993567	21.649959
83.256989	2623.652124	21.654976
83.589844	2617.652312	21.659994
83.356403	2621.881821	21.665011
83.715718	2618.335255	21.670029
83.872222	2619.339496	21.675047
83.689900	2612.087702	21.680064
84.157644	2613.200422	21.685082
84.120188	2608.423897	21.690099
83.963541	2608.515229	21.695117
83.695776	2601.857606	21.700135
83.748586	2609.527849	21.705152
84.111896	2606.096285	21.710170
84.134063	2615.185010	21.715187
83.922213	2613.827501	21.720205
84.004229	2606.841917	21.725223
84.110195	2614.745184	21.730240
84.489454	2619.828818	21.735258
84.520208	2638.720092	21.740275
84.574606	2635.351945	21.745293
84.666602	2631.126656	21.750311
84.613197	2636.951086	21.755328
84.940694	2632.293347	21.760346
84.633028	2641.077552	21.765363
85.035163	2642.332107	21.770381
84.976050	2642.622638	21.775399
84.775513	2658.652049	21.780416
85.328055	2667.553961	21.785434
85.403116	2669.874662	21.790451
85.613442	2668.872249	21.795469
85.507156	2668.496151	21.800487
85.341483	2669.929363	21.805504
85.941069	2663.665949	21.810522
85.575239	2661.304063	21.815539
85.534644	2657.583697	21.820557
85.828124	2666.240584	21.825575
85.625285	2680.822176	21.830592
86.229659	2687.037313	21.835610
86.093215	2689.810241	21.840627
86.325250	2695.995082	21.845645
86.341610	2688.602221	21.850663
86.532630	2692.806539	21.855680
86.742231	2685.507153	21.860698
86.353875	2695.074383	21.865715
86.625564	2683.108161	21.870733
86.673689	2695.411744	21.875751
86.455387	2711.223784	21.880768
86.930142	2712.210318	21.885786
87.008863	2713.302488	21.890803
87.255655	2713.162714	21.895821
87.408637	2712.109659	21.900839
87.438609	2706.289483	21.905856
87.893647	2703.859615	21.910874
87.699491	2708.981232	21.915891
87.475998	2714.157875	21.920909
87.780259	2710.801782	21.925927
87.450025	2715.542340	21.930944
87.891867	2715.841875	21.935962
87.917042	2727.773128	21.940979
88.014030	2728.934757	21.945997
88.400230	2726.602395	21.951015
88.312251	2736.714094	21.956032
88.516604	2731.202784	21.961050
88.246988	2732.269481	21.966067
88.407801	2727.984418	21.971085
88.479091	2724.922708	21.976103
88.339777	2728.341151	21.981120
88.645157	2723.908744	21.986138
88.398744	2733.598106	21.991155
88.246033	2743.749239	21.996173
88.772556	2750.782346	22.001191
88.710182	2760.944257	22.006208
88.983802	2754.690310	22.011226
88.741202	2770.932652	22.016243
88.910833	2781.653072	22.021261
89.461728	2777.043834	22.026279
89.501178	2789.545541	22.031296
89.486263	2788.226622	22.036314
89.391321	2784.839776	22.041331
89.639628	2783.027344	22.046349
89.699311	2783.370519	22.051367
89.622655	2790.507701	22.056384
90.319813	2795.521035	22.061402
90.369049	2807.377717	22.066419
90.443312	2801.662145	22.071437
90.330826	2792.791210	22.076455
90.359134	2801.827153	22.081472
90.387534	2807.022657	22.086490
90.545257	2813.589912	22.091507
90.682172	2803.588900	22.096525
90.811903	2813.721786	22.101543
90.354474	2813.239630	22.106560
90.819517	2803.064361	22.111578
90.706513	2820.876699	22.116595
90.593070	2815.922641	22.121613
91.117878	2821.252169	22.126631
90.903134	2839.679396	22.131648
91.169294	2833.019906	22.136666
91.240686	2837.820746	22.141683
91.300297	2838.890800	22.146701
91.507373	2829.877630	22.151719
91.285647	2845.933437	22.156736
91.721503	2850.386671	22.161754
91.775598	2862.281168	22.166771
91.912915	2864.622651	22.171789
92.255168	2860.447067	22.176807
92.087767	2866.333819	22.181824
91.927951	2869.978973	22.186842
91.936463	2867.078282	22.191859
92.060801	2868.120710	22.196877
92.731405	2881.938610	22.201895
92.353033	2902.868398	22.206912
92.655427	2894.341875	22.211930
93.196478	2887.405674	22.216947
92.802506	2896.822891	22.221965
92.955481	2881.606887	22.226983
93.189354	2901.674411	22.232000
93.121562	2891.678452	22.237018
92.885311	2892.123101	22.242035
92.989770	2899.853698	22.247053
93.395738	2903.971880	22.252071
93.064399	2928.864458	22.257088
93.415726	2920.810764	22.262106
93.643812	2929.915619	22.267123
93.489185	2926.312488	22.272141
93.799528	2920.544275	22.277159
93.954361	2940.130436	22.282176
94.277332	2942.979612	22.287194
94.127475	2948.795947	22.292211
94.227249	2949.445036	22.297229
94.252007	2942.277266	22.302247
94.332911	2961.033520	22.307264
94.348610	2947.244312	22.312282
94.528701	2944.593148	22.317299
94.550072	2953.040297	22.322317
94.581829	2947.602057	22.327335
94.926378	2951.057454	22.332352
94.627016	2947.843981	22.337370
95.041943	2959.359273	22.342387
95.062157	2967.093114	22.347405
95.514042	2969.478063	22.352423
95.111600	2981.235422	22.357440
95.124712	2973.831923	22.362458
95.044671	2968.827646	22.367475
94.766618	2979.573978	22.372493
95.174098	2990.041863	22.377511
95.447515	3003.846125	22.382528
95.733073	2996.790925	22.387546
95.957781	3007.319436	22.392563
95.961792	2997.673031	22.397581
95.889699	3004.673498	22.402599
95.966275	3021.973623	22.407616
96.390344	3024.577776	22.412634
96.252887	3024.551983	22.417651
96.133818	3037.982269	22.422669
96.422098	3035.437342	22.427687
96.575476	3043.049295	22.432704
96.913121	3048.957060	22.437722
97.210274	3058.253154	22.442739
97.035204	3052.318432	22.447757
97.462915	3055.574941	22.452775
97.213269	3050.405737	22.457792
97.911396	3044.143759	22.462810
97.906355	3046.363227	22.467827
97.724446	3037.223163	22.472845
97.949766	3046.213678	22.477863
97.674176	3035.337441	22.482880
97.695364	3040.362686	22.487898
98.034963	3029.747855	22.492915
97.822045	3047.242068	22.497933
97.837447	3039.451919	22.502951
97.794209	3040.348017	22.507968
97.929681	3039.942795	22.512986
97.974793	3040.785470	22.518003
98.193534	3071.461437	22.523021
98.440983	3060.489973	22.528039
98.410280	3071.374713	22.533056
98.903253	3070.720534	22.538074
98.744718	3069.329306	22.543091
98.560656	3071.467193	22.548109
98.739829	3079.464450	22.553127
98.920915	3095.663972	22.558144
99.172169	3095.579339	22.563162
99.089317	3097.295957	22.568179
99.095295	3102.551781	22.573197
99.370013	3096.515422	22.578215
99.216306	3123.574014	22.583232
99.379907	3137.284207	22.588250
99.596450	3129.977989	22.593267
99.655224	3132.321027	22.598285
99.730954	3131.789236	22.603303
99.670169	3146.937063	22.608320
99.635182	3152.595133	22.613338
99.942642	3154.301435	22.618355
99.862454	3154.447443	22.623373
100.178634	3158.973352	22.628391
100.327371	3173.006910	22.633408
100.579786	3181.034237	22.638426
100.946173	3184.107820	22.643443
100.699133	3192.247053	22.648461
100.784516	3174.624085	22.653479
100.813493	3181.414997	22.658496
100.809323	3179.848101	22.663514
101.430204	3188.903853	22.668531
101.519254	3208.275088	22.673549
101.594511	3206.612922	22.678567
101.822083	3201.100882	22.683584
101.583164	3208.649612	22.688602
102.119560	3203.886010	22.693619
101.657758	3210.587637	22.698637
102.083931	3197.080448	22.703655
102.269658	3201.321157	22.708672
102.291840	3202.992718	22.713690
102.237710	3196.954478	22.718707
102.265251	3207.155852	22.723725
102.210832	3194.773937	22.728743
102.132276	3201.694501	22.733760
102.523906	3215.244897	22.738778
102.732801	3223.234347	22.743795
102.523333	3239.807045	22.748813
102.786804	3234.788019	22.753831
102.842039	3236.945983	22.758848
102.887874	3245.946364	22.763866
103.148237	3251.188422	22.768883
102.617862	3261.265615	22.773901
103.254430	3254.583842	22.778919
103.534526	3263.227487	22.783936
103.194101	3268.551197	22.788954
103.738237	3274.887905	22.793971
103.840906	3290.276497	22.798989
103.861081	3283.272134	22.804007
103.911520	3298.248192	22.809024
103.939745	3295.079950	22.814042
104.157392	3293.512284	22.819059
104.109958	3310.627989	22.824077
104.246756	3321.173892	22.829095
104.188986	3329.283805	22.834112
104.262281	3329.979614	22.839130
104.510949	3327.044470	22.844147
104.672884	3353.155549	22.849165
105.023211	3350.978281	22.854183
105.337472	3349.797982	22.859200
104.927943	3351.898702	22.864218
105.442249	3345.474750	22.869235
105.306766	3356.012176	22.874253
105.242162	3351.659038	22.879271
105.090454	3351.628436	22.884288
105.208094	3361.603934	22.889306
105.704958	3365.574019	22.894323
105.808154	3383.867050	22.899341
105.930194	3371.142174	22.904359
106.126358	3374.379039	22.909376
106.233932	3379.872860	22.914394
106.396641	3374.596877	22.919411
106.212473	3379.962577	22.924429
106.584520	3396.683443	22.929447
106.330199	3402.271956	22.934464
106.492105	3414.863230	22.939482
106.642349	3408.741178	22.944499
106.301658	3408.289156	22.949517
106.896678	3418.949290	22.954535
107.268795	3429.401104	22.959552
107.093200	3438.426686	22.964570
107.292860	3428.350737	22.969587
107.506342	3431.252085	22.974605
107.714829	3430.003686	22.979623
107.730491	3440.321972	22.984640
107.567100	3430.237834	22.989658
108.110768	3420.042526	22.994675
107.991584	3444.114671	22.999693
107.755425	3453.632158	23.004711
108.185483	3467.568430	23.009728
108.129000	3481.126023	23.014746
108.579500	3465.324665	23.019763
108.389737	3467.446210	23.024781
108.379022	3457.909627	23.029799
108.373539	3460.180363	23.034816
108.659761	3477.444447	23.039834
109.032556	3470.224854	23.044851
108.852952	3490.253703	23.049869
108.930721	3489.107959	23.054887
109.272562	3489.321982	23.059904
109.360693	3505.159956	23.064922
109.598143	3513.070276	23.069939
109.495813	3522.087372	23.074957
109.482637	3513.813781	23.079975
109.415016	3515.878095	23.084992
109.359422	3528.704756	23.090010
109.805176	3536.135032	23.095027
110.204369	3549.977181	23.100045
110.389726	3559.112843	23.105063
110.475426	3541.018158	23.110080
110.088004	3537.967279	23.115098
110.519597	3542.189336	23.120115
110.204342	3548.818971	23.125133
110.508857	3558.105555	23.130151
110.695153	3565.820308	23.135168
110.836298	3575.340642	23.140186
111.186276	3575.565956	23.145203
111.220714	3574.088050	23.150221
111.121805	3573.604547	23.155239
111.612867	3564.814693	23.160256
111.576942	3565.105477	23.165274
111.672394	3563.071094	23.170291
111.767158	3579.963044	23.175309
112.068946	3595.238388	23.180327
112.171629	3593.965939	23.185344
112.281089	3597.226120	23.190362
112.582187	3586.411704	23.195379
112.378939	3587.987878	23.200397
112.599137	3590.591605	23.205415
112.712943	3581.717935	23.210432
112.504566	3581.813585	23.215450
112.566945	3583.020924	23.220467
112.692053	3587.241519	23.225485
112.700763	3584.040925	23.230503
112.713745	3590.404257	23.235520
112.460556	3602.275978	23.240538
113.278499	3613.176050	23.245555
113.159113	3617.813254	23.250573
113.247928	3623.985928	23.255591
113.564448	3631.128477	23.260608
113.366858	3645.715692	23.265626
113.487386	3644.541090	23.270643
113.759720	3650.795435	23.275661
113.507301	3649.780213	23.280679
114.147347	3660.106866	23.285696
114.025550	3691.216045	23.290714
114.317987	3671.328390	23.295731
114.486532	3680.043565	23.300749
114.190448	3676.730282	23.305767
114.471115	3686.395219	23.310784
114.653860	3701.964215	23.315802
114.572519	3703.227523	23.320819
114.552487	3701.639500	23.325837
114.871978	3718.469813	23.330855
115.221699	3730.819787	23.335872
115.131660	3732.926254	23.340890
115.413489	3725.414230	23.345907
115.674867	3735.323006	23.350925
115.939970	3754.388395	23.355943
116.332012	3753.191730	23.360960
116.055792	3755.545804	23.365978
116.631413	3750.026837	23.370995
116.459608	3757.607625	23.376013
116.503998	3754.620009	23.381031
116.724018	3749.486587	23.386048
116.876388	3751.260175	23.391066
117.025657	3749.715166	23.396083
116.832408	3751.550161	23.401101
116.537220	3743.787924	23.406119
116.992410	3751.758057	23.411136
116.684158	3745.287306	23.416154
116.722116	3740.327672	23.421171
117.279240	3752.353514	23.426189
117.253060	3772.415710	23.431207
117.643873	3765.068016	23.436224
117.850038	3769.828003	23.441242
117.872504	3764.906232	23.446259
117.727992	3766.285037	23.451277
117.700526	3764.242692	23.456295
117.941607	3763.588535	23.461312
117.896355	3784.793720	23.466330
118.252026	3793.073971	23.471347
118.213635	3800.183513	23.476365
118.317520	3799.563032	23.481383
118.610465	3799.887917	23.486400
118.370075	3817.021605	23.491418
118.710765	3822.715218	23.496435
118.915347	3831.728405	23.501453
118.791822	3835.227974	23.506471
119.152148	3837.075404	23.511488
118.849007	3862.940574	23.516506
119.076741	3852.292645	23.521523
119.086350	3861.916744	23.526541
119.322236	3886.407376	23.531559
119.857058	3898.936454	23.536576
119.396390	3904.444772	23.541594
119.774413	3898.600094	23.546611
120.199570	3910.770622	23.551629
120.204065	3918.891385	23.556647
120.556122	3918.471273	23.561664
120.511721	3915.567013	23.566682
120.641342	3915.427037	23.571699
120.995033	3918.700268	23.576717
120.567436	3941.938142	23.581735
120.918307	3942.699859	23.586752
120.813794	3951.929191	23.591770
121.302510	3951.680031	23.596787
121.401683	3948.335913	23.601805
121.570117	3965.866383	23.606823
121.723512	3965.478735	23.611840
121.682074	3975.970138	23.616858
122.336720	3972.253436	23.621875
122.428734	3961.870164	23.626893
122.235549	3957.427996	23.631911
122.639015	3954.984916	23.636928
122.629175	3963.856153	23.641946
122.675770	3961.230030	23.646963
122.826999	3957.958641	23.651981
122.585413	3958.390793	23.656999
122.999466	3957.178016	23.662016
122.990740	3961.893661	23.667034
123.086886	3981.639258	23.672051
123.351388	3990.538356	23.677069
122.933408	3993.025211	23.682087
123.226332	3984.763123	23.687104
123.305531	3991.330842	23.692122
123.362217	4007.954792	23.697139
123.740773	4008.103181	23.702157
123.547457	4012.491107	23.707175
123.885219	4010.307098	23.712192
123.772547	4021.410156	23.717210
124.059117	4032.646239	23.722227
124.359270	4044.273523	23.727245
124.296163	4045.655107	23.732263
124.652609	4037.366339	23.737280
124.592280	4039.473619	23.742298
124.644496	4049.301886	23.747315
125.037730	4053.737904	23.752333
124.962808	4071.787203	23.757351
125.132794	4074.022186	23.762368
125.359343	4073.202763	23.767386
125.236187	4077.986254	23.772403
125.611694	4088.312913	23.777421
125.471338	4107.437907	23.782439
126.252377	4094.807940	23.787456
126.265534	4103.991855	23.792474
126.147380	4092.560264	23.797491
126.235004	4092.532404	23.802509
126.133682	4094.453481	23.807527
126.344626	4106.796007	23.812544
126.379505	4118.840129	23.817562
126.223696	4115.118884	23.822579
126.740991	4116.006697	23.827597
126.957273	4140.616527	23.832615
127.258138	4145.623515	23.837632
127.037375	4152.115621	23.842650
127.455982	4149.574902	23.847667
127.592481	4145.807825	23.852685
127.914131	4140.295385	23.857703
128.042236	4129.511306	23.862720
128.467254	4132.062016	23.867738
128.500638	4134.037931	23.872755
128.735608	4122.317139	23.877773
128.738928	4134.070499	23.882791
128.791380	4126.891443	23.887808
128.890142	4137.746886	23.892826
128.692429	4129.048437	23.897843
128.609425	4124.183487	23.902861
128.562254	4139.657440	23.907879
128.811760	4152.173228	23.912896
128.923801	4151.541992	23.917914
129.162974	4153.810012	23.922931
129.507216	4158.480451	23.927949
129.580853	4183.966694	23.932967
130.001605	4186.820983	23.937984
130.119813	4187.951025	23.943002
129.898058	4185.454980	23.948019
129.968154	4189.168429	23.953037
130.059498	4182.274233	23.958055
130.217263	4186.382012	23.963072
130.082887	4192.122413	23.968090
130.241184	4207.759569	23.973107
130.553981	4216.286849	23.978125
130.742664	4219.809104	23.983143
130.545769	4222.820892	23.988160
130.738047	4230.764766	23.993178
130.713211	4239.535498	23.998195
131.226062	4249.649983	24.003213
130.903721	4254.606904	24.008231
131.279162	4258.890051	24.013248
131.563323	4278.117507	24.018266
131.776951	4280.856151	24.023283
131.818842	4281.661649	24.028301
131.715031	4284.263669	24.033319
131.968294	4291.096430	24.038336
132.327066	4311.387493	24.043354
132.122044	4316.840249	24.048371
132.272900	4310.449452	24.053389
132.502088	4320.451871	24.058407
132.687941	4330.118192	24.063424
132.568897	4340.995927	24.068442
132.798894	4352.858862	24.073459
133.109578	4354.727651	24.078477
133.196871	4379.263253	24.083495
133.346137	4377.750437	24.088512
133.729554	4373.043906	24.093530
133.652248	4372.493204	24.098547
133.953388	4389.442077	24.103565
133.825142	4393.289480	24.108583
134.269502	4389.385924	24.113600
134.381838	4392.633237	24.118618
134.470538	4404.552573	24.123635
134.588734	4389.052617	24.128653
134.863426	4404.751669	24.133671
134.741762	4423.915002	24.138688
135.106294	4425.621800	24.143706
134.757534	4434.201984	24.148723
135.227585	4427.151306	24.153741
135.353120	4431.989665	24.158759
135.290428	4438.286755	24.163776
135.526316	4451.099996	24.168794
135.554000	4453.078436	24.173811
135.786938	4457.408753	24.178829
135.864545	4471.950540	24.183847
135.933795	4478.800142	24.188864
136.161003	4484.412194	24.193882
136.018186	4488.744217	24.198899
136.113802	4492.655079	24.203917
136.324394	4508.022230	24.208935
136.609608	4511.485106	24.213952
136.767060	4517.312846	24.218970
136.963475	4536.891358	24.223987
137.457106	4544.704742	24.229005
137.355237	4546.207417	24.234023
137.465858	4547.123916	24.239040
137.625629	4525.999052	24.244058
137.630492	4533.565441	24.249075
137.850790	4553.351014	24.254093
138.080954	4560.657270	24.259111
138.190743	4564.683903	24.264128
138.339663	4561.853327	24.269146
138.244905	4567.385362	24.274163
138.631143	4563.360430	24.279181
138.693074	4575.132331	24.284199
138.583467	4585.892303	24.289216
138.915841	4583.292096	24.294234
139.283885	4593.265480	24.299251
139.384806	4590.990913	24.304269
139.518628	4596.850776	24.309287
139.529119	4594.038332	24.314304
139.790486	4599.716575	24.319322
139.674104	4623.824813	24.324339
139.981295	4615.588424	24.329357
139.921147	4622.344647	24.334375
140.050063	4631.320826	24.339392
140.325619	4630.306314	24.344410
140.077115	4652.892853	24.349427
140.370585	4651.260246	24.354445
140.102044	4654.858658	24.359463
140.722111	4666.041264	24.364480
140.969246	4681.567200	24.369498
140.887294	4694.217336	24.374515
141.332094	4688.448247	24.379533
141.342968	4697.392149	24.384551
141.241468	4714.370980	24.389568
141.882486	4712.940218	24.394586
141.788893	4719.788361	24.399603
142.003412	4723.050137	24.404621
142.104111	4735.920586	24.409639
142.262919	4740.320240	24.414656
142.477161	4744.003765	24.419674
142.418638	4750.763721	24.424691
143.173025	4750.288881	24.429709
142.904980	4759.911419	24.434727
142.818949	4770.105235	24.439744
143.437104	4764.465039	24.444762
143.457106	4766.365284	24.449779
143.919849	4758.096146	24.454797
143.957542	4759.716632	24.459815
143.980668	4756.883261	24.464832
144.064138	4756.380863	24.469850
144.162057	4762.978985	24.474867
144.403996	4764.798210	24.479885
144.792501	4767.850514	24.484903
144.965278	4782.549732	24.489920
145.130506	4771.057481	24.494938
145.165509	4771.820046	24.499955
145.479014	4758.970611	24.504973
145.531990	4765.810353	24.509991
145.509345	4757.071029	24.515008
145.603149	4734.744784	24.520026
145.392611	4734.953286	24.525043
145.608445	4746.718880	24.530061
145.567851	4746.668193	24.535079
145.310756	4761.283302	24.540096
145.623620	4761.125904	24.545114
145.412841	4778.972716	24.550131
145.873177	4792.249271	24.555149
145.935014	4804.786884	24.560167
145.996485	4820.963323	24.565184
146.140995	4821.742261	24.570202
145.888705	4842.029997	24.575219
146.499819	4852.013580	24.580237
146.704987	4867.605411	24.585255
146.625531	4880.787158	24.590272
146.871907	4883.910142	24.595290
147.159206	4902.752401	24.600307
147.562262	4910.912438	24.605325
147.464855	4917.982361	24.610343
147.596307	4923.742813	24.615360
147.916489	4939.649182	24.620378
147.838815	4954.447512	24.625395
148.031304	4954.708197	24.630413
148.395511	4975.469008	24.635431
148.512786	4980.503983	24.640448
148.997505	4987.080656	24.645466
148.621858	4994.397179	24.650483
148.747406	4998.618111	24.655501
149.278809	5007.870227	24.660519
149.358980	5010.521715	24.665536
149.832256	5015.934235	24.670554
149.847335	5030.846882	24.675571
150.392539	5038.318719	24.680589
150.595796	5037.074171	24.685607
150.523026	5038.273283	24.690624
150.614942	5032.383306	24.695642
150.475932	5032.775525	24.700659
150.980395	5023.635717	24.705677
150.996698	5020.037070	24.710695
150.896385	5029.655854	24.715712
151.136858	5039.265939	24.720730
151.517518	5054.851229	24.725747
151.508923	5054.431951	24.730765
151.634146	5054.214778	24.735783
151.521937	5049.777462	24.740800
151.876549	5068.434537	24.745818
152.008795	5085.337185	24.750835
152.120634	5097.380062	24.755853
151.890090	5087.786211	24.760871
152.131891	5110.192202	24.765888
152.476386	5110.252416	24.770906
152.118210	5117.608698	24.775923
152.443499	5131.962156	24.780941
152.946254	5137.759475	24.785959
152.923294	5144.299151	24.790976
153.286644	5155.891276	24.795994
153.218143	5168.508988	24.801011
153.537837	5179.622652	24.806029
153.709581	5178.014906	24.811047
153.823905	5186.912712	24.816064
153.900760	5181.020357	24.821082
153.833217	5210.692145	24.826099
153.996658	5219.815026	24.831117
154.155183	5217.262102	24.836135
154.670764	5238.799303	24.841152
154.667781	5248.999875	24.846170
154.737460	5247.811228	24.851187
154.923537	5252.249961	24.856205
155.305336	5267.360079	24.861223
155.379393	5279.897720	24.866240
155.893759	5271.203075	24.871258
156.032807	5279.657183	24.876275
156.061246	5279.263465	24.881293
155.976056	5288.170326	24.886311
156.261397	5297.674291	24.891328
156.495824	5301.036878	24.896346
156.446544	5301.186630	24.901363
156.361801	5310.649690	24.906381
156.616023	5316.100396	24.911399
156.437834	5339.447816	24.916416
156.687066	5335.185673	24.921434
156.831268	5352.487193	24.926451
156.952330	5366.602788	24.931469
157.380810	5378.235845	24.936487
157.537281	5398.543353	24.941504
157.503127	5397.365741	24.946522
157.446119	5411.073889	24.951539
157.670239	5428.823814	24.956557
158.068856	5431.418309	24.961575
158.296540	5455.491135	24.966592
158.905198	5447.690099	24.971610
158.832960	5458.562762	24.976627
158.802846	5453.732214	24.981645
159.217289	5466.901037	24.986663
159.169218	5480.640870	24.991680
159.748872	5485.327704	24.996698
160.026664	5487.157040	25.001715
159.931317	5485.539133	25.006733
160.055554	5502.249982	25.011751
160.011941	5512.936372	25.016768
160.572116	5517.530334	25.021786
160.536038	5514.947803	25.026803
160.469699	5516.882368	25.031821
160.647994	5531.889875	25.036839
160.792907	5544.420376	25.041856
160.762853	5543.815674	25.046874
161.152220	5561.057105	25.051891
161.023636	5585.120068	25.056909
161.425098	5585.888765	25.061927
161.148489	5582.521582	25.066944
161.616884	5600.944819	25.071962
161.837259	5613.891366	25.076979
161.575451	5620.178217	25.081997
162.186502	5632.218254	25.087015
162.121741	5641.014277	25.092032
162.239410	5642.385281	25.097050
162.485333	5661.044699	25.102067
162.700316	5665.505699	25.107085
163.198567	5665.229830	25.112103
163.013408	5681.233307	25.117120
163.651875	5677.038830	25.122138
163.808523	5700.791350	25.127155
164.145582	5689.951578	25.132173
164.567286	5700.165790	25.137191
164.096802	5697.488834	25.142208
164.508595	5699.274802	25.147226
164.284304	5701.151173	25.152243
164.321696	5712.490428	25.157261
164.857700	5719.802000	25.162279
164.770971	5731.032023	25.167296
164.729848	5729.923948	25.172314
165.384981	5754.781220	25.177331
165.220046	5760.498771	25.182349
165.446393	5764.405651	25.187367
165.423363	5766.729894	25.192384
165.881011	5784.184152	25.197402
165.924475	5791.259567	25.202419
165.726138	5799.462483	25.207437
165.938478	5805.468456	25.212455
166.089594	5833.905167	25.217472
166.371156	5839.295845	25.222490
166.752281	5850.541847	25.227507
166.697057	5849.203115	25.232525
167.117277	5864.761709	25.237543
167.240328	5880.814611	25.242560
167.359306	5879.592876	25.247578
167.739399	5899.193476	25.252595
167.929374	5916.879404	25.257613
167.919510	5904.807559	25.262631
168.019790	5923.279662	25.267648
167.849477	5932.821279	25.272666
168.274377	5944.998259	25.277683
168.618343	5952.708010	25.282701
168.700379	5960.571255	25.287719
168.828732	5982.164986	25.292736
169.154467	5987.885435	25.297754
169.148200	5985.787472	25.302771
169.654021	6007.395017	25.307789
169.861270	6011.869158	25.312807
169.988661	6017.647994	25.317824
169.768155	6013.157628	25.322842
170.184705	6029.974322	25.327859
170.231314	6044.009587	25.332877
170.764816	6036.021165	25.337895
170.677380	6048.318471	25.342912
171.072605	6051.794075	25.347930
171.323142	6066.571082	25.352947
171.355680	6070.460947	25.357965
171.500051	6069.641149	25.362983
171.517855	6066.855586	25.368000
171.446857	6079.542923	25.373018
171.722788	6075.589470	25.378035
171.884234	6103.809460	25.383053
172.047215	6094.537758	25.388071
172.326349	6105.476043	25.393088
172.360674	6127.018882	25.398106
172.244824	6122.518090	25.403123
172.224257	6142.087686	25.408141
172.826935	6142.825121	25.413159
173.040017	6161.297632	25.418176
173.083842	6167.212595	25.423194
173.714418	6186.151257	25.428211
173.604196	6196.567072	25.433229
173.811207	6188.455161	25.438247
174.175553	6214.049618	25.443264
174.261996	6214.624659	25.448282
174.777612	6215.250873	25.453299
174.770522	6219.335149	25.458317
175.231764	6213.502273	25.463335
175.111199	6227.247271	25.468352
175.386809	6242.919019	25.473370
175.326223	6239.826468	25.478387
175.184093	6259.099292	25.483405
175.808914	6252.837461	25.488423
175.569750	6275.368320	25.493440
176.064092	6279.853422	25.498458
176.180331	6288.347151	25.503475
176.099942	6305.386593	25.508493
176.512080	6307.941323	25.513511
176.619294	6310.981365	25.518528
176.595299	6316.616071	25.523546
176.869274	6330.450907	25.528563
177.199198	6338.492785	25.533581
177.168336	6345.276594	25.538599
177.425665	6360.887648	25.543616
177.621891	6376.528130	25.548634
177.785484	6374.976638	25.553651
177.474851	6397.810993	25.558669
178.007049	6406.033499	25.563687
178.168061	6418.265532	25.568704
178.427158	6430.584228	25.573722
178.661203	6437.669694	25.578739
178.930932	6449.923763	25.583757
179.146780	6466.071087	25.588775
179.360091	6478.659928	25.593792
179.685844	6480.072586	25.598810
179.887886	6470.862877	25.603827
179.866607	6505.701809	25.608845
179.968066	6492.785549	25.613863
180.370584	6496.358453	25.618880
180.218288	6495.855034	25.623898
180.660000	6507.916493	25.628915
180.412999	6527.501451	25.633933
180.940887	6524.377965	25.638951
181.011523	6517.440352	25.643968
181.009915	6545.304769	25.648986
181.463646	6560.137999	25.654003
181.371740	6574.262730	25.659021
181.648486	6578.360865	25.664039
181.767303	6584.806179	25.669056
181.939121	6596.098709	25.674074
182.089601	6595.293647	25.679092
182.305576	6613.725343	25.684109
182.669972	6618.302085	25.689127
182.966576	6626.870329	25.694144
183.348081	6643.167690	25.699162
183.647014	6635.868653	25.704180
183.381682	6652.983615	25.709197
183.803377	6646.026954	25.714215
184.237858	6646.850250	25.719232
184.027066	6655.372723	25.724250
184.314052	6668.645560	25.729268
184.059358	6677.046000	25.734285
184.686815	6674.873656	25.739303
184.718012	6691.907552	25.744320
184.743142	6702.707372	25.749338
185.080713	6702.276133	25.754356
185.012739	6718.392657	25.759373
185.070637	6732.610110	25.764391
185.208699	6746.307270	25.769408
185.573928	6766.293801	25.774426
186.239016	6773.142318	25.779444
185.632284	6781.798019	25.784461
186.368186	6795.505350	25.789479
186.271931	6817.448487	25.794496
186.379329	6823.307938	25.799514
186.860117	6826.793692	25.804532
186.741029	6843.839131	25.809549
186.749866	6856.494728	25.814567
187.212382	6859.282306	25.819584
186.988821	6874.187637	25.824602
187.425987	6894.406013	25.829620
187.826754	6907.453976	25.834637
188.065608	6924.555749	25.839655
188.215655	6936.141577	25.844672
188.726155	6940.898925	25.849690
188.958639	6947.292439	25.854708
189.091794	6961.642896	25.859725
189.130615	6967.127770	25.864743
189.486744	6964.511572	25.869760
189.540859	6978.910843	25.874778
190.066922	6984.777575	25.879796
189.973317	6999.615886	25.884813
190.009310	6996.426732	25.889831
190.314843	7001.364710	25.894848
190.085235	7019.868736	25.899866
190.647022	7019.744034	25.904884
190.747412	7031.290640	25.909901
190.604566	7051.623734	25.914919
190.933424	7057.013614	25.919936
190.722564	7077.963481	25.924954
191.642155	7082.442411	25.929972
191.758288	7099.756736	25.934989
191.832775	7106.122787	25.940007
192.063843	7105.413440	25.945024
192.265778	7138.972634	25.950042
192.461044	7129.567668	25.955060
192.619442	7145.787840	25.960077
192.852535	7155.587755	25.965095
193.023124	7158.273213	25.970112
192.711663	7167.502121	25.975130
193.311612	7176.835171	25.980148
193.591867	7192.315181	25.985165
193.687485	7201.838816	25.990183
193.930809	7209.717139	25.995200
194.155882	7227.970309	26.000218
194.365551	7235.006536	26.005236
194.064900	7250.683088	26.010253
194.640009	7257.550506	26.015271
195.072571	7275.527114	26.020288
195.005636	7286.977446	26.025306
195.168955	7296.979006	26.030324
195.185212	7315.672789	26.035341
195.583531	7317.038159	26.040359
195.779036	7333.813278	26.045376
196.071665	7351.535694	26.050394
196.250390	7359.179279	26.055412
196.317915	7372.394092	26.060429
196.683698	7386.653181	26.065447
196.723272	7385.445559	26.070464
196.741256	7416.331722	26.075482
197.194547	7416.488715	26.080500
197.260299	7436.093852	26.085517
197.425851	7446.418964	26.090535
197.839876	7459.172574	26.095552
197.850800	7486.563822	26.100570
197.940084	7486.560091	26.105588
198.332890	7511.719056	26.110605
198.569188	7525.318253	26.115623
198.698322	7529.115196	26.120640
199.143979	7545.167248	26.125658
199.552139	7545.217732	26.130676
199.966968	7540.718464	26.135693
200.035265	7539.189522	26.140711
200.989295	7553.915265	26.145728
201.044139	7571.536570	26.150746
201.073569	7558.547069	26.155764
201.094072	7554.146074	26.160781
200.875700	7560.537762	26.165799
201.423218	7569.141306	26.170816
201.386705	7570.285656	26.175834
201.753556	7563.199217	26.180852
201.344701	7570.621431	26.185869
201.332715	7574.717481	26.190887
201.832141	7582.752292	26.195904
201.647585	7597.766224	26.200922
202.146961	7597.855675	26.205940
202.307678	7617.368794	26.210957
202.723507	7623.092828	26.215975
202.648134	7623.254630	26.220992
202.897795	7644.388402	26.226010
202.903273	7652.879321	26.231028
202.945080	7674.210736	26.236045
203.532124	7692.058167	26.241063
204.139578	7683.304411	26.246080
203.861389	7701.944108	26.251098
204.154113	7713.377560	26.256116
204.400243	7724.438371	26.261133
204.396498	7736.412499	26.266151
204.522030	7746.910237	26.271168
204.622386	7768.399278	26.276186
204.886646	7782.848447	26.281204
205.322146	7797.660247	26.286221
205.301325	7820.077961	26.291239
205.653985	7827.104262	26.296256
205.786524	7847.351252	26.301274
206.157720	7836.169266	26.306292
206.580309	7855.737738	26.311309
206.610154	7871.743117	26.316327
206.862606	7880.022063	26.321344
206.633785	7894.208032	26.326362
207.469644	7899.821932	26.331380
207.400544	7909.605206	26.336397
207.543326	7924.211983	26.341415
207.877510	7934.554224	26.346432
207.863975	7954.573224	26.351450
208.220258	7962.908453	26.356468
208.523844	7977.032050	26.361485
208.485688	7996.091835	26.366503
209.010059	8000.315357	26.371520
208.804874	8007.072626	26.376538
209.248918	8024.387683	26.381556
209.495713	8030.753021	26.386573
209.496781	8059.503158	26.391591
210.033921	8061.050678	26.396608
210.057520	8073.561729	26.401626
210.462032	8086.594394	26.406644
210.954953	8088.492067	26.411661
211.215595	8104.739081	26.416679
211.454760	8105.389792	26.421696
211.307139	8129.841941	26.426714
211.680628	8120.762851	26.431732
212.016337	8128.811469	26.436749
212.038484	8157.100439	26.441767
212.217677	8154.191966	26.446784
212.317787	8160.634649	26.451802
212.502059	8162.376541	26.456820
212.755391	8180.446163	26.461837
212.940808	8194.649005	26.466855
212.937958	8197.860433	26.471872
212.898205	8205.761198	26.476890
213.777926	8202.375112	26.481908
214.253965	8211.353991	26.486925
214.353597	8213.584693	26.491943
214.967865	8216.183087	26.496960
215.182520	8228.058654	26.501978
215.023799	8231.674242	26.506996
215.385461	8237.443351	26.512013
215.132631	8238.610826	26.517031
215.482670	8235.451611	26.522048
215.249638	8238.098915	26.527066
215.158702	8251.337406	26.532084
215.710250	8265.032604	26.537101
215.864501	8288.197457	26.542119
216.290926	8298.298213	26.547136
216.100556	8314.067676	26.552154
216.498758	8331.134642	26.557172
216.567531	8345.561615	26.562189
216.828763	8365.253273	26.567207
217.063040	8365.919728	26.572224
217.571396	8389.522881	26.577242
217.851138	8390.429583	26.582260
218.094916	8406.945208	26.587277
217.862186	8427.642326	26.592295
218.809787	8425.146035	26.597312
219.023917	8452.640436	26.602330
218.813451	8453.179483	26.607348
219.250755	8460.390116	26.612365
219.331387	8478.453004	26.617383
219.515950	8487.174753	26.622400
219.582091	8493.249193	26.627418
219.892306	8509.094481	26.632436
220.339293	8522.005861	26.637453
219.967598	8544.635622	26.642471
220.390945	8558.802060	26.647488
220.735650	8570.535976	26.652506
221.076461	8580.147707	26.657524
221.705332	8588.440227	26.662541
221.750764	8593.180969	26.667559
222.670934	8599.575741	26.672576
222.741477	8607.005453	26.677594
222.739812	8608.422515	26.682612
223.018572	8604.660367	26.687629
222.932511	8615.443487	26.692647
223.175841	8615.371130	26.697664
223.549731	8633.507072	26.702682
223.575361	8633.687408	26.707700
223.971299	8632.616468	26.712717
223.798064	8637.222100	26.717735
224.259002	8650.001912	26.722752
224.217953	8664.180707	26.727770
224.424585	8664.164959	26.732788
224.635950	8656.358334	26.737805
224.377874	8687.050314	26.742823
224.634330	8691.783024	26.747840
224.984339	8712.160989	26.752858
225.255090	8722.394665	26.757876
225.800923	8738.640974	26.762893
226.063657	8762.257116	26.767911
226.179062	8760.971583	26.772928
225.984991	8776.774779	26.777946
226.422805	8793.740343	26.782964
226.650457	8796.445727	26.787981
226.618369	8815.563820	26.792999
226.943602	8821.025357	26.798016
226.955746	8848.429522	26.803034
227.255386	8866.744815	26.808052
227.731538	8885.502601	26.813069
227.963387	8894.813575	26.818087
228.091943	8911.874611	26.823104
228.307849	8926.207465	26.828122
228.214162	8946.687960	26.833140
228.920187	8963.433890	26.838157
228.924370	8993.641619	26.843175
229.133910	8997.253377	26.848192
230.060990	9009.921414	26.853210
230.163158	9010.180056	26.858228
230.590213	9026.186697	26.863245
230.436729	9048.999241	26.868263
230.943015	9053.597015	26.873280
231.147089	9059.321918	26.878298
231.112518	9073.560662	26.883316
232.061793	9076.077085	26.888333
231.836600	9080.998845	26.893351
232.214604	9092.322961	26.898368
232.483191	9105.239676	26.903386
232.402537	9119.550737	26.908404
232.688268	9126.861408	26.913421
232.716179	9141.488077	26.918439
233.097605	9142.693413	26.923456
233.103921	9162.880454	26.928474
233.315123	9177.564508	26.933492
233.630619	9189.779302	26.938509
233.574280	9211.690063	26.943527
233.984905	9227.915174	26.948544
234.289090	9240.605187	26.953562
234.175549	9251.656784	26.958580
234.633402	9269.165471	26.963597
234.873194	9288.065717	26.968615
234.995231	9306.989873	26.973632
235.613366	9315.599311	26.978650
235.622581	9340.036293	26.983668
236.066460	9339.837526	26.988685
236.207440	9350.433088	26.993703
236.164617	9367.296486	26.998720
236.691787	9379.789735	27.003738
236.970407	9396.037646	27.008756
237.281183	9411.714202	27.013773
237.075187	9417.166595	27.018791
237.356239	9435.286040	27.023808
237.421198	9446.867702	27.028826
237.611028	9468.018700	27.033844
238.171426	9474.621527	27.038861
238.246346	9497.654114	27.043879
238.031583	9515.770452	27.048896
238.592724	9534.831093	27.053914
238.688655	9557.512172	27.058932
238.868616	9573.864146	27.063949
239.393934	9599.674849	27.068967
239.708244	9610.005679	27.073984
240.136731	9633.149745	27.079002
240.199378	9652.557583	27.084020
240.732892	9660.402749	27.089037
241.027089	9672.199098	27.094055
241.075238	9688.266061	27.099072
241.323944	9694.293980	27.104090
241.796676	9705.965486	27.109108
242.451823	9711.017848	27.114125
242.489335	9730.854783	27.119143
242.668321	9733.259979	27.124160
243.012617	9732.121254	27.129178
243.423237	9758.277125	27.134196
243.719920	9752.734360	27.139213
243.514271	9760.732429	27.144231
243.562791	9774.386034	27.149248
243.895594	9783.874288	27.154266
244.197010	9798.942013	27.159284
244.410467	9809.002189	27.164301
244.447978	9827.607957	27.169319
244.887871	9830.405621	27.174336
245.511574	9841.144552	27.179354
245.244820	9855.913722	27.184372
245.447402	9869.489336	27.189389
245.651647	9879.311773	27.194407
245.920867	9903.658638	27.199424
245.869738	9917.052404	27.204442
246.200826	9947.667588	27.209460
246.564254	9954.593621	27.214477
246.738893	9974.706907	27.219495
246.844385	10000.813461	27.224512
247.261751	10018.001284	27.229530
247.148373	10036.198101	27.234548
247.819786	10053.066858	27.239565
247.931095	10073.448911	27.244583
248.247881	10086.849897	27.249600
248.631636	10099.409897	27.254618
248.917483	10124.502546	27.259636
249.229137	10130.865525	27.264653
249.519006	10161.594751	27.269671
249.566369	10161.572127	27.274688
250.277391	10161.661329	27.279706
250.268601	10185.601992	27.284724
250.661672	10194.550040	27.289741
251.039138	10195.042253	27.294759
251.036001	10217.208469	27.299776
251.419564	10225.132929	27.304794
251.760251	10226.408997	27.309812
251.958305	10230.193281	27.314829
252.132350	10254.302850	27.319847
252.400167	10254.867636	27.324864
252.810343	10250.873210	27.329882
252.864937	10282.493735	27.334900
252.855652	10280.021018	27.339917
253.251952	10292.731867	27.344935
253.174145	10307.649229	27.349952
253.398403	10322.357505	27.354970
253.461320	10351.862446	27.359988
254.141350	10362.514855	27.365005
254.216462	10388.978733	27.370023
254.356663	10398.314301	27.375040
254.733894	10417.699736	27.380058
254.927723	10440.238640	27.385076
254.834017	10460.106499	27.390093
255.556730	10482.034620	27.395111
255.767138	10491.804134	27.400128
255.880623	10514.457486	27.405146
255.983023	10532.296628	27.410164
256.433169	10554.191958	27.415181
256.602078	10583.623983	27.420199
256.700970	10603.692921	27.425216
257.377731	10615.620286	27.430234
257.586970	10630.869804	27.435252
257.736722	10657.844273	27.440269
258.121059	10669.563678	27.445287
258.247582	10695.309373	27.450304
258.443830	10712.956285	27.455322
258.651005	10735.040740	27.460340
258.876288	10752.531559	27.465357
259.129856	10770.383485	27.470375
259.636057	10799.353871	27.475392
259.976171	10810.174712	27.480410
259.978890	10833.964824	27.485428
260.428786	10848.849762	27.490445
260.714008	10876.164884	27.495463
260.718514	10887.987506	27.500480
260.995851	10906.258463	27.505498
260.993604	10932.632907	27.510516
261.924739	10945.671878	27.515533
262.389543	10958.971731	27.520551
262.405687	10983.413411	27.525568
262.531323	10996.308689	27.530586
262.594136	11012.397349	27.535604
263.239811	11033.808256	27.540621
263.400220	11047.734035	27.545639
263.517823	11061.070431	27.550656
263.740249	11076.729352	27.555674
263.862576	11100.197394	27.560692
263.894656	11111.607691	27.565709
264.264449	11131.192197	27.570727
264.572614	11161.419358	27.575744
264.788868	11179.640169	27.580762
265.138051	11206.375836	27.585780
265.762521	11213.012121	27.590797
265.989198	11232.731731	27.595815
265.914611	11258.196584	27.600832
266.403632	11271.253772	27.605850
266.582332	11296.986071	27.610868
267.046556	11301.311439	27.615885
267.714647	11311.019352	27.620903
267.781222	11314.620419	27.625920
268.665796	11327.891469	27.630938
268.608819	11341.490496	27.635956
268.819333	11339.400127	27.640973
269.007824	11352.155621	27.645991
269.573942	11359.554134	27.651008
269.891007	11357.176804	27.656026
270.201961	11368.380699	27.661044
271.072817	11379.613815	27.666061
270.917953	11399.514296	27.671079
270.652807	11403.744222	27.676096
270.958281	11405.348328	27.681114
271.027097	11414.201994	27.686132
271.202839	11430.842370	27.691149
271.505349	11435.703795	27.696167
271.540395	11461.146593	27.701184
271.694471	11470.482185	27.706202
271.771881	11500.273753	27.711220
272.313386	11503.613799	27.716237
272.797213	11522.723916	27.721255
272.813912	11542.005330	27.726272
273.280581	11559.948190	27.731290
273.877521	11570.687710	27.736308
273.842655	11595.856746	27.741325
274.417469	11594.434192	27.746343
274.309888	11618.634113	27.751360
274.542215	11635.991414	27.756378
274.906598	11654.556375	27.761396
274.847633	11668.076315	27.766413
275.131475	11688.887207	27.771431
275.236137	11726.170601	27.776448
275.605847	11733.579748	27.781466
275.647359	11768.986979	27.786484
275.939571	11791.937847	27.791501
276.384531	11816.238526	27.796519
276.554185	11847.054090	27.801536
277.510461	11872.181702	27.806554
277.587660	11886.244305	27.811572
277.736207	11911.995834	27.816589
278.293876	11921.755788	27.821607
278.069589	11943.094126	27.826624
278.715762	11952.752228	27.831642
278.987943	11977.041151	27.836660
279.120589	11994.160900	27.841677
279.554400	11998.320904	27.846695
279.605223	12015.300621	27.851712
279.904521	12034.321546	27.856730
280.199755	12048.385754	27.861748
280.401636	12067.430513	27.866765
281.091328	12074.152228	27.871783
281.252840	12100.642115	27.876800
281.645999	12115.155386	27.881818
281.807426	12123.868172	27.886836
281.898803	12147.328793	27.891853
282.066810	12167.684551	27.896871
282.208401	12198.423928	27.901888
282.508391	12208.995460	27.906906
282.698504	12237.848071	27.911924
283.091696	12262.816066	27.916941
283.626357	12272.891724	27.921959
283.403534	12306.818614	27.926976
283.581551	12326.831169	27.931994
284.342812	12345.552840	27.937012
284.240842	12370.504395	27.942029
285.348778	12392.555922	27.947047
285.390648	12424.339969	27.952064
285.649877	12433.695504	27.957082
286.029058	12445.942144	27.962100
286.100765	12464.011409	27.967117
286.827594	12479.968037	27.972135
286.997682	12497.798797	27.977152
287.736106	12514.101635	27.982170
288.178608	12513.163927	27.987188
288.680539	12517.284488	27.992205
289.255893	12525.637327	27.997223
289.104151	12541.394887	28.002240
289.436551	12529.437144	28.007258
289.693431	12526.924786	28.012276
289.796990	12530.702672	28.017293
290.565295	12538.189094	28.022311
290.430553	12564.003015	28.027328
290.906294	12562.737368	28.032346
290.781271	12558.386845	28.037364
290.667106	12581.429974	28.042381
290.963790	12589.012058	28.047399
291.087778	12621.120136	28.052416
291.638898	12631.009017	28.057434
291.792664	12651.347422	28.062452
291.852537	12666.974659	28.067469
292.435866	12688.584506	28.072487
292.567792	12714.227278	28.077504
292.716379	12727.593752	28.082522
293.235342	12749.779430	28.087540
293.143774	12776.251595	28.092557
293.384022	12795.245592	28.097575
293.527368	12820.877178	28.102592
293.809039	12837.629831	28.107610
294.139627	12866.722979	28.112628
294.428983	12896.535251	28.117645
295.053686	12908.585893	28.122663
294.830236	12933.554482	28.127680
295.492860	12960.406618	28.132698
295.374018	12976.944498	28.137716
295.494979	13014.882103	28.142733
296.131039	13034.434597	28.147751
296.205764	13076.348132	28.152768
296.717367	13091.798222	28.157786
297.222328	13116.078526	28.162804
297.421862	13138.103927	28.167821
297.950494	13152.462086	28.172839
298.041029	13189.567891	28.177856
298.613140	13210.307858	28.182874
298.697894	13229.002656	28.187892
299.259566	13255.064524	28.192909
299.563903	13267.754945	28.197927
299.742375	13288.348560	28.202944
300.189482	13317.548767	28.207962
300.361626	13332.909246	28.212980
300.368966	13357.734484	28.217997
301.049269	13377.605189	28.223015
301.206042	13403.286459	28.228032
301.697223	13433.033268	28.233050
302.025694	13459.191399	28.238068
302.367527	13472.514933	28.243085
302.766516	13492.496750	28.248103
302.976415	13509.945863	28.253120
303.640988	13525.260524	28.258138
303.754495	13547.950169	28.263156
303.984337	13565.447730	28.268173
304.365637	13571.477125	28.273191
304.853772	13596.592372	28.278208
305.089904	13609.504332	28.283226
305.692089	13621.781323	28.288244
305.598113	13633.981725	28.293261
306.181540	13636.391381	28.298279
306.674265	13659.504399	28.303296
306.695387	13670.859905	28.308314
307.131669	13681.295510	28.313332
307.360063	13704.702735	28.318349
307.531802	13704.015944	28.323367
307.792322	13735.567911	28.328384
308.073357	13744.066345	28.333402
308.439593	13755.645193	28.338420
308.526172	13778.995821	28.343437
308.856153	13799.803424	28.348455
308.945527	13819.536263	28.353472
309.269875	13836.528728	28.358490
309.726452	13863.165645	28.363508
309.472596	13882.907020	28.368525
310.091442	13901.469887	28.373543
310.171424	13927.405980	28.378560
310.473142	13944.720607	28.383578
310.967951	13969.641646	28.388596
311.136066	13996.070985	28.393613
311.839760	14009.613536	28.398631
312.275567	14035.617780	28.403648
312.351953	14046.005505	28.408666
312.744662	14062.577961	28.413684
312.755846	14090.846867	28.418701
313.306673	14103.787517	28.423719
313.641254	14121.349713	28.428736
313.820457	14137.776491	28.433754
314.081877	14169.220863	28.438772
314.342587	14192.477451	28.443789
314.785429	14202.277355	28.448807
315.426100	14221.780454	28.453824
315.785603	14237.413988	28.458842
316.333276	14238.475178	28.463860
316.586676	14264.785601	28.468877
317.462591	14260.171443	28.473895
317.593193	14270.566228	28.478912
317.819402	14280.635113	28.483930
318.157062	14289.844867	28.488948
318.214825	14294.483279	28.493965
318.818332	14315.347774	28.498983
318.945221	14324.576774	28.504000
319.279583	14332.610430	28.509018
319.930807	14341.097925	28.514036
319.730449	14357.579823	28.519053
320.111041	14369.691692	28.524071
320.296522	14390.827502	28.529088
320.511176	14404.205774	28.534106
320.949856	14416.636020	28.539124
321.054356	14444.966577	28.544141
321.576502	14452.000661	28.549159
322.070202	14470.636718	28.554176
321.975142	14491.256650	28.559194
322.264477	14516.256693	28.564212
322.462289	14536.009090	28.569229
322.981749	14547.739582	28.574247
323.726640	14571.227400	28.579264
324.029881	14593.077567	28.584282
324.154637	14595.663419	28.589300
323.994130	14630.820342	28.594317
324.802827	14632.999708	28.599335
325.214558	14657.870160	28.604352
325.437827	14661.295102	28.609370
325.819143	14671.716332	28.614388
326.115176	14690.288408	28.619405
326.692246	14701.230141	28.624423
327.488640	14704.779269	28.629440
327.754550	14728.845455	28.634458
328.161786	14723.478140	28.639476
327.977440	14737.920231	28.644493
328.620760	14734.355935	28.649511
328.938997	14753.268785	28.654528
328.577252	14767.791529	28.659546
328.952786	14772.779970	28.664564
329.122888	14787.587598	28.669581
329.456823	14800.630426	28.674599
329.731109	14815.717887	28.679616
329.758095	14839.816223	28.684634
330.169621	14853.902474	28.689652
329.994295	14883.705283	28.694669
330.488775	14913.562402	28.699687
330.985946	14943.049913	28.704704
330.905582	14975.370463	28.709722
331.678156	14990.957930	28.714740
331.793819	15024.010419	28.719757
332.031999	15053.660661	28.724775
332.938819	15070.939960	28.729792
333.411711	15099.548496	28.734810
333.391541	15116.027286	28.739828
333.501798	15147.388810	28.744845
334.073838	15170.942788	28.749863
334.380010	15197.037469	28.754880
334.510303	15212.250813	28.759898
335.382068	15224.604233	28.764916
335.573244	15257.530439	28.769933
335.712406	15286.488928	28.774951
336.141569	15310.327079	28.779968
336.450338	15338.672291	28.784986
336.882329	15355.139702	28.790004
336.994282	15392.586348	28.795021
337.431165	15409.675798	28.800039
337.860440	15439.530749	28.805056
337.834259	15475.001218	28.810074
338.324558	15493.941881	28.815092
338.989442	15520.792647	28.820109
338.836277	15555.304905	28.825127
339.416491	15582.570804	28.830144
339.447415	15605.649540	28.835162
340.196265	15634.401686	28.840180
340.451263	15663.305220	28.845197
341.132515	15677.729518	28.850215
341.705774	15698.251147	28.855232
341.837671	15714.135728	28.860250
342.257808	15733.147507	28.865268
342.802170	15755.452190	28.870285
343.040138	15772.482217	28.875303
343.276878	15786.431840	28.880320
343.414364	15808.677832	28.885338
343.968259	15826.430728	28.890356
344.140922	15859.009624	28.895373
344.263556	15880.283368	28.900391
344.931613	15893.106962	28.905408
345.155939	15927.723854	28.910426
345.463343	15948.903685	28.915444
346.601198	15952.969912	28.920461
347.641632	15948.972015	28.925479
348.093225	15956.800852	28.930496
348.180538	15959.315350	28.935514
348.570690	15947.182786	28.940532
348.889433	15962.314284	28.945549
348.789679	15965.926420	28.950567
349.236637	15956.072800	28.955584
348.934145	15965.375641	28.960602
349.467449	15989.648802	28.965620
349.388960	15999.963323	28.970637
349.417798	16024.353740	28.975655
349.903226	16041.473753	28.980672
350.568401	16053.145077	28.985690
351.060385	16064.661741	28.990708
350.954347	16087.061107	28.995725
351.068216	16104.944092	29.000743
351.709256	16134.042284	29.005760
351.640770	16164.413563	29.010778
352.247879	16188.703620	29.015796
352.372661	16218.474952	29.020813
352.841641	16240.142787	29.025831
353.233490	16258.820967	29.030848
353.335397	16299.156860	29.035866
353.903619	16320.596800	29.040884
353.823841	16353.249249	29.045901
353.790132	16382.206436	29.050919
354.661208	16415.566888	29.055936
355.020329	16454.186297	29.060954
355.563730	16483.587111	29.065972
356.092350	16511.910859	29.070989
356.042296	16542.156323	29.076007
356.446242	16581.444467	29.081024
356.711106	16620.781251	29.086042
357.691797	16643.784980	29.091060
357.819380	16677.352666	29.096077
358.046733	16695.062150	29.101095
358.866831	16726.001953	29.106112
358.835556	16758.068014	29.111130
359.139159	16781.348347	29.116148
359.828512	16808.977359	29.121165
359.901727	16845.220142	29.126183
361.198588	16847.049919	29.131200
361.699791	16857.634235	29.136218
362.339994	16872.632919	29.141236
362.840784	16884.467291	29.146253
362.733083	16892.691240	29.151271
363.333188	16908.519166	29.156288
363.538929	16917.591585	29.161306
363.988905	16926.716820	29.166324
364.174611	16947.611121	29.171341
364.648972	16966.135080	29.176359
364.780245	16976.822524	29.181376
364.810123	16999.644058	29.186394
365.282352	17011.514969	29.191412
365.155992	17028.234759	29.196429
365.392085	17058.055317	29.201447
365.825900	17079.938593	29.206464
365.963366	17105.960037	29.211482
366.721054	17122.787473	29.216500
367.088882	17155.680906	29.221517
367.176411	17168.390797	29.226535
367.340035	17204.211351	29.231552
367.501577	17240.099248	29.236570
367.984280	17268.246658	29.241588
368.413539	17301.370374	29.246605
368.367118	17333.520350	29.251623
369.022591	17359.416757	29.256640
369.434442	17394.206451	29.261658
369.786002	17427.662112	29.266676
370.317199	17462.056164	29.271693
370.447435	17484.828164	29.276711
371.119180	17518.835765	29.281728
371.206013	17554.848499	29.286746
371.692509	17585.920745	29.291764
372.257770	17602.699839	29.296781
372.225353	17640.201100	29.301799
373.143326	17672.518576	29.306816
373.257067	17710.400270	29.311834
373.622671	17744.222102	29.316852
374.181560	17776.847812	29.321869
374.825041	17794.386724	29.326887
375.822318	17803.589443	29.331904
376.165381	17825.846908	29.336922
376.730902	17839.172543	29.341940
377.167333	17855.295249	29.346957
377.059487	17881.023602	29.351975
377.897251	17889.086389	29.356992
378.085114	17904.889293	29.362010
378.225401	17924.185775	29.367028
378.598296	17946.364246	29.372045
378.836204	17961.113515	29.377063
379.247477	17985.705331	29.382080
379.386467	18004.496977	29.387098
379.672550	18032.152275	29.392116
380.373911	18061.524612	29.397133
380.563618	18082.572564	29.402151
381.359860	18099.201998	29.407168
381.196039	18120.132311	29.412186
381.622713	18147.353969	29.417204
381.988269	18173.868441	29.422221
382.266221	18205.818122	29.427239
382.898367	18226.996961	29.432256
382.964584	18268.307880	29.437274
383.180948	18298.408780	29.442292
383.602531	18327.175370	29.447309
383.341425	18360.169994	29.452327
383.846000	18400.997208	29.457344
384.349833	18445.423352	29.462362
384.798182	18479.987986	29.467380
385.636050	18513.924045	29.472397
386.161138	18542.223713	29.477415
386.693026	18553.427191	29.482432
387.040269	18586.081237	29.487450
387.329275	18601.300176	29.492468
388.214628	18615.223603	29.497485
388.493808	18636.682887	29.502503
389.156240	18642.301348	29.507520
389.289491	18664.244594	29.512538
389.306288	18677.853289	29.517556
389.671280	18704.019507	29.522573
390.009592	18719.318115	29.527591
390.954141	18733.806682	29.532608
390.773973	18771.454291	29.537626
391.090326	18793.455952	29.542644
391.411454	18817.491735	29.547661
391.762399	18858.153268	29.552679
392.156732	18883.753243	29.557696
392.516015	18913.020656	29.562714
392.324779	18947.659498	29.567732
392.676493	18991.485382	29.572749
393.327223	19027.227776	29.577767
393.834724	19060.592007	29.582784
394.106645	19106.664260	29.587802
394.257836	19137.278007	29.592820
394.800776	19172.575649	29.597837
394.995578	19220.545799	29.602855
395.341225	19256.271180	29.607872
395.963801	19304.408493	29.612890
396.208328	19341.934671	29.617908
396.576034	19378.234058	29.622925
396.660984	19425.784878	29.627943
397.342130	19473.567266	29.632960
397.906229	19509.580508	29.637978
398.425499	19552.335833	29.642996
399.422544	19583.173990	29.648013
400.268116	19591.364404	29.653031
401.106365	19618.076126	29.658048
401.655455	19634.211075	29.663066
402.064141	19667.157632	29.668084
402.306559	19676.995622	29.673101
402.548214	19694.787745	29.678119
403.509004	19698.402448	29.683136
404.081387	19719.433760	29.688154
404.298379	19728.243386	29.693172
404.430191	19725.815973	29.698189
404.484813	19751.341556	29.703207
405.135812	19763.278625	29.708224
405.353283	19788.672791	29.713242
405.540691	19803.371601	29.718260
406.106268	19822.366793	29.723277
405.853072	19845.786890	29.728295
406.264701	19869.351523	29.733312
406.824989	19905.635623	29.738330
407.120940	19930.795428	29.743348
408.165306	19953.078062	29.748365
408.098042	19971.676548	29.753383
408.359306	20002.422501	29.758400
408.849165	20029.849614	29.763418
409.000658	20058.181236	29.768436
409.328823	20080.278116	29.773453
409.626194	20102.676051	29.778471
410.199860	20135.401205	29.783488
410.446965	20170.919133	29.788506
410.836102	20188.409525	29.793524
411.379450	20226.284766	29.798541
411.369970	20256.842816	29.803559
412.006922	20289.498354	29.808576
412.009950	20322.739314	29.813594
412.314880	20364.598538	29.818612
412.904820	20398.027299	29.823629
413.202906	20460.769268	29.828647
413.556610	20493.016723	29.833664
413.786943	20537.267527	29.838682
414.203181	20581.084810	29.843700
414.607978	20632.349746	29.848717
415.257242	20667.390451	29.853735
415.714866	20717.120139	29.858752
415.975879	20759.397736	29.863770
416.637602	20802.768555	29.868788
417.249346	20835.334733	29.873805
417.733957	20876.946952	29.878823
418.499921	20904.560785	29.883840
418.783761	20943.167449	29.888858
418.913567	20985.214529	29.893876
419.479196	21009.165093	29.898893
420.466445	21052.616261	29.903911
420.484411	21074.353626	29.908928
421.457483	21101.590627	29.913946
421.883507	21129.383459	29.918964
422.285404	21150.463545	29.923981
422.745300	21193.699053	29.928999
423.246567	21210.107093	29.934016
423.991459	21233.844351	29.939034
424.032925	21264.482869	29.944052
424.695306	21278.485171	29.949069
424.626547	21306.138195	29.954087
425.081830	21334.122840	29.959104
425.589155	21372.273576	29.964122
425.991393	21403.981162	29.969140
426.207525	21417.241088	29.974157
426.736899	21449.189995	29.979175
427.259944	21478.986638	29.984192
427.751225	21493.860717	29.989210
428.057179	21536.702680	29.994228
428.469161	21557.367417	29.999245
428.787617	21589.923601	30.004263
429.227060	21630.185571	30.009280
429.707060	21664.635606	30.014298
430.198439	21702.247007	30.019316
430.512063	21732.239745	30.024333
430.610852	21765.666963	30.029351
431.029635	21794.586066	30.034368
431.313079	21820.236061	30.039386
431.293369	21856.406768	30.044404
432.233099	21894.719071	30.049421
432.736338	21928.594942	30.054439
433.027332	21958.885504	30.059456
433.814740	21988.147137	30.064474
434.297683	22015.690655	30.069492
435.112023	22020.231894	30.074509
435.048277	22066.247740	30.079527
435.427278	22090.552618	30.084544
436.264965	22115.985613	30.089562
436.146015	22151.675799	30.094580
436.600431	22179.799131	30.099597
437.202376	22222.410692	30.104615
437.538859	22256.124797	30.109632
438.200928	22294.813913	30.114650
438.219510	22325.514049	30.119668
438.784302	22351.478462	30.124685
439.262157	22393.562044	30.129703
439.409631	22434.841399	30.134720
440.345892	22476.026694	30.139738
440.380705	22517.992942	30.144756
441.254835	22543.900509	30.149773
441.336947	22582.826872	30.154791
441.912190	22606.578263	30.159808
442.194242	22646.740290	30.164826
442.483419	22690.326091	30.169844
443.436616	22721.342025	30.174861
443.697418	22763.412334	30.179879
444.172630	22796.544656	30.184896
445.154988	22837.183198	30.189914
445.388665	22864.096012	30.194932
445.814934	22891.019935	30.199949
446.336924	22925.625134	30.204967
447.003204	22961.095144	30.209984
447.246904	22995.083174	30.215002
447.191121	23027.174181	30.220020
447.745454	23060.389759	30.225037
447.971213	23101.161335	30.230055
448.456941	23141.878994	30.235072
449.254306	23167.326407	30.240090
449.731776	23212.525203	30.245108
450.089500	23231.419780	30.250125
450.904401	23269.881334	30.255143
451.524856	23295.677734	30.260160
452.732318	23306.333905	30.265178
453.375422	23329.360332	30.270196
454.339179	23314.818824	30.275213
455.477285	23288.387511	30.280231
455.969512	23280.348038	30.285248
456.790353	23269.672548	30.290266
457.186089	23277.993302	30.295284
457.164985	23281.032747	30.300301
457.160807	23278.211343	30.305319
457.574574	23277.763659	30.310336
457.631631	23282.329826	30.315354
457.932105	23284.121517	30.320372
458.025389	23287.590156	30.325389
458.612524	23297.763040	30.330407
459.327983	23299.004180	30.335424
459.799611	23299.935214	30.340442
459.691485	23320.436203	30.345460
460.182747	23331.193107	30.350477
460.478902	23352.522987	30.355495
460.584291	23376.608760	30.360512
460.929057	23394.157039	30.365530
461.173655	23427.444003	30.370548
461.767902	23463.961670	30.375565
461.796560	23499.191815	30.380583
461.928290	23522.941196	30.385600
462.549955	23561.822592	30.390618
462.442123	23609.701058	30.395636
462.839162	23650.698826	30.400653
463.295945	23706.295532	30.405671
463.274380	23755.170553	30.410688
463.819070	23807.428609	30.415706
464.136532	23870.070694	30.420724
464.713295	23922.587907	30.425741
465.288047	23968.880909	30.430759
466.049619	24035.109566	30.435776
466.627794	24077.462845	30.440794
467.607362	24116.402009	30.445812
468.522720	24153.083575	30.450829
469.104038	24182.652295	30.455847
469.456238	24221.746019	30.460864
470.081885	24259.598105	30.465882
470.492549	24298.540120	30.470900
471.223533	24322.734832	30.475917
471.850957	24351.722247	30.480935
471.911280	24383.504434	30.485952
472.525715	24395.694277	30.490970
472.978911	24438.228339	30.495988
473.108006	24475.265146	30.501005
473.781823	24513.129065	30.506023
474.295564	24547.417696	30.511040
474.917992	24574.104459	30.516058
475.334551	24609.705371	30.521076
475.757366	24653.761302	30.526093
476.108836	24685.950674	30.531111
476.665510	24723.228744	30.536128
477.519046	24755.349300	30.541146
477.468093	24785.057677	30.546164
478.145177	24816.150056	30.551181
478.635659	24856.642093	30.556199
478.885657	24879.946881	30.561216
479.357411	24909.239771	30.566234
480.016779	24961.623555	30.571252
480.175046	24990.341820	30.576269
481.009338	25022.589662	30.581287
480.791008	25072.754205	30.586304
481.333371	25102.679038	30.591322
482.097081	25133.038978	30.596340
482.231478	25173.189917	30.601357
482.840204	25215.129323	30.606375
483.207247	25252.201706	30.611392
484.215379	25278.354730	30.616410
484.457154	25314.134734	30.621428
484.979481	25356.507386	30.626445
485.401293	25382.344327	30.631463
485.799612	25422.751635	30.636480
486.291005	25451.394020	30.641498
486.771933	25492.803833	30.646516
487.336143	25522.443144	30.651533
487.911318	25558.975726	30.656551
488.258206	25605.579982	30.661568
488.760162	25635.548486	30.666586
489.089560	25678.971374	30.671604
489.633496	25720.791645	30.676621
490.072997	25756.339451	30.681639
490.640169	25801.922825	30.686656
491.134278	25846.889279	30.691674
491.310477	25896.698886	30.696692
491.911402	25941.246793	30.701709
492.781845	25981.921428	30.706727
493.190440	26033.389072	30.711744
493.851058	26070.382696	30.716762
494.014009	26118.007263	30.721780
494.350903	26156.896996	30.726797
495.119482	26198.550364	30.731815
495.411929	26240.464834	30.736832
495.825342	26285.883412	30.741850
496.686607	26334.938414	30.746868
497.130079	26381.204930	30.751885
497.637578	26416.436096	30.756903
497.868042	26461.354872	30.761920
498.419463	26501.788558	30.766938
498.996218	26544.043002	30.771956
499.104272	26604.965865	30.776973
499.865077	26646.690175	30.781991
500.328239	26696.540837	30.787008
500.949035	26740.736397	30.792026
501.352974	26795.588765	30.797044
502.136996	26835.556053	30.802061
502.714394	26874.388717	30.807079
502.951984	26923.989225	30.812096
504.211038	26950.584831	30.817114
505.870114	26967.991479	30.822132
506.484017	26988.032297	30.827149
507.302550	26998.642637	30.832167
507.860176	27009.942189	30.837184
508.728467	27015.070380	30.842202
509.045124	27025.302136	30.847220
509.533570	27021.431712	30.852237
509.920054	27025.453251	30.857255
510.105880	27052.062413	30.862272
510.598756	27058.186432	30.867290
510.706632	27066.201262	30.872308
510.962322	27072.936653	30.877325
511.641203	27093.531383	30.882343
511.539913	27124.029730	30.887360
512.036328	27134.696201	30.892378
511.974767	27163.762208	30.897396
512.253248	27209.579918	30.902413
512.429021	27245.858488	30.907431
512.401233	27291.794551	30.912448
512.873843	27334.824040	30.917466
513.452827	27390.501477	30.922484
513.547202	27450.523610	30.927501
514.394593	27496.653338	30.932519
514.499510	27570.394907	30.937536
515.395508	27617.736928	30.942554
516.025097	27685.834333	30.947572
516.515450	27731.074524	30.952589
517.343638	27782.205123	30.957607
517.452096	27838.835222	30.962624
518.482941	27889.741625	30.967642
518.990605	27950.832813	30.972660
519.130299	27998.490250	30.977677
519.966928	28053.560033	30.982695
520.253429	28117.564623	30.987712
520.900150	28157.886411	30.992730
521.500926	28225.142840	30.997748
521.860964	28277.950678	31.002765
522.646865	28321.446619	31.007783
523.148657	28392.079325	31.012800
523.415652	28435.543187	31.017818
524.212438	28487.306645	31.022836
524.898639	28538.364536	31.027853
525.461473	28589.521034	31.032871
526.321293	28628.076526	31.037888
527.170313	28670.011055	31.042906
527.635348	28715.941975	31.047924
528.073229	28757.239351	31.052941
528.952666	28791.461418	31.057959
529.438679	28841.497840	31.062976
529.955736	28880.384320	31.067994
530.671308	28914.826591	31.073012
530.867166	28955.978635	31.078029
531.559853	28989.220675	31.083047
531.595182	29033.563021	31.088064
532.156882	29077.821643	31.093082
533.005435	29126.710620	31.098100
533.394393	29161.115606	31.103117
533.752144	29203.829500	31.108135
534.245414	29253.418450	31.113152
534.649804	29297.236231	31.118170
535.409293	29348.699475	31.123188
535.545220	29396.528651	31.128205
536.305199	29447.256133	31.133223
536.791835	29484.019710	31.138240
537.347225	29526.739215	31.143258
537.319636	29570.519368	31.148276
537.690550	29625.479525	31.153293
538.643826	29669.187234	31.158311
539.011865	29717.990612	31.163328
539.452393	29764.618688	31.168346
540.408594	29805.769962	31.173364
540.518862	29862.788192	31.178381
541.355333	29909.649911	31.183399
542.258721	29955.981006	31.188416
542.652008	29999.337500	31.193434
543.669180	30044.665685	31.198452
543.382900	30094.942433	31.203469
544.365683	30128.655963	31.208487
544.999348	30177.809268	31.213504
545.800911	30216.970405	31.218522
546.500491	30265.878639	31.223540
546.739013	30311.106206	31.228557
547.272539	30341.853031	31.233575
547.867030	30387.889387	31.238592
548.400626	30429.054380	31.243610
549.011447	30476.344538	31.248628
549.251137	30517.955323	31.253645
549.738189	30567.156789	31.258663
550.091865	30622.925278	31.263680
550.454733	30672.810388	31.268698
551.310452	30719.069277	31.273716
551.837295	30779.769224	31.278733
552.297955	30836.799644	31.283751
552.856755	30891.781400	31.288768
553.326260	30944.079190	31.293786
553.967867	30997.973176	31.298804
554.529500	31041.868296	31.303821
555.587521	31079.896791	31.308839
557.127189	31100.381567	31.313856
558.658115	31108.765941	31.318874
559.723409	31119.736898	31.323892
560.319412	31130.155292	31.328909
560.957593	31136.078042	31.333927
561.428554	31147.230369	31.338944
561.633168	31170.243273	31.343962
562.162339	31188.496479	31.348980
562.178796	31211.331354	31.353997
562.877941	31223.285916	31.359015
563.373391	31244.373796	31.364032
563.595197	31264.238037	31.369050
564.081844	31286.291997	31.374068
564.347750	31327.210286	31.379085
564.661725	31349.753657	31.384103
565.113726	31390.891502	31.389120
565.077659	31431.427844	31.394138
565.388219	31476.475336	31.399156
565.812375	31523.914880	31.404173
566.855923	31560.493535	31.409191
567.219321	31608.412710	31.414208
567.729116	31644.920520	31.419226
568.342203	31690.155268	31.424244
568.848924	31730.088891	31.429261
569.357512	31772.766531	31.434279
569.813511	31820.867026	31.439296
570.432448	31860.348050	31.444314
571.232233	31901.822685	31.449332
571.516324	31956.675212	31.454349
572.382700	31996.281081	31.459367
573.011369	32043.932290	31.464384
573.416688	32077.251590	31.469402
574.393567	32115.300140	31.474420
575.118298	32156.041796	31.479437
575.621575	32191.952874	31.484455
575.782347	32234.393917	31.489472
576.000284	32285.527028	31.494490
576.662287	32332.209076	31.499508
577.001133	32393.854424	31.504525
577.896572	32430.945678	31.509543
578.425522	32490.480401	31.514560
578.677241	32538.090610	31.519578
579.614652	32592.059343	31.524596
580.031953	32657.386469	31.529613
580.488588	32707.677368	31.534631
580.993567	32768.273040	31.539648
581.265135	32825.425569	31.544666
581.952698	32877.362148	31.549684
582.389429	32951.015121	31.554701
582.828020	33007.616752	31.559719
583.612193	33077.196837	31.564736
583.585613	33150.393250	31.569754
584.663762	33211.507729	31.574772
585.037082	33280.990159	31.579789
585.584886	33356.567755	31.584807
586.355351	33420.329883	31.589824
586.609999	33491.380103	31.594842
587.818839	33546.382238	31.599860
588.399880	33617.420424	31.604877
588.938505	33677.839072	31.609895
590.259328	33735.885392	31.614912
591.185220	33795.058900	31.619930
592.894756	33803.898637	31.624948
594.052221	33828.514890	31.629965
595.906715	33839.979959	31.634983
596.441166	33846.732082	31.640000
596.999828	33852.083637	31.645018
597.769134	33849.000858	31.650036
597.693509	33874.574978	31.655053
598.092367	33894.283334	31.660071
598.445313	33896.901027	31.665088
599.122918	33929.403505	31.670106
598.967927	33949.576900	31.675124
599.269449	33970.691267	31.680141
599.645121	34001.395960	31.685159
599.888967	34040.576184	31.690176
600.092421	34069.776124	31.695194
600.614295	34111.083006	31.700212
600.601137	34165.802569	31.705229
601.145736	34207.963665	31.710247
601.390676	34260.965080	31.715264
601.846690	34312.935141	31.720282
602.456107	34373.264639	31.725300
603.456848	34424.391587	31.730317
604.493526	34471.838177	31.735335
605.160031	34529.873244	31.740352
605.368248	34584.057595	31.745370
606.323292	34628.318919	31.750388
606.817784	34690.107211	31.755405
607.404810	34738.592569	31.760423
607.739761	34794.510500	31.765440
608.166500	34853.113006	31.770458
609.131179	34911.901212	31.775476
609.429172	34979.255479	31.780493
610.220594	35035.626506	31.785511
610.693254	35097.709863	31.790528
610.959393	35159.477920	31.795546
612.117080	35216.188517	31.800564
612.431391	35291.638639	31.805581
612.468231	35357.271838	31.810599
613.318261	35421.442007	31.815616
613.574666	35492.397974	31.820634
614.358339	35568.597568	31.825652
614.954938	35644.727975	31.830669
615.252450	35722.738370	31.835687
615.881530	35794.853403	31.840704
616.586497	35883.850128	31.845722
617.826112	35951.460377	31.850740
618.187952	36023.637868	31.855757
618.943095	36093.585156	31.860775
619.474911	36165.140215	31.865792
620.223577	36241.198652	31.870810
621.299162	36301.096643	31.875828
621.830134	36368.993279	31.880845
622.362842	36438.597447	31.885863
623.062131	36499.729113	31.890880
623.647439	36576.316461	31.895898
624.355647	36631.993437	31.900916
624.801192	36704.288224	31.905933
625.834728	36766.665251	31.910951
626.922840	36825.609211	31.915968
627.080650	36888.745793	31.920986
627.935568	36948.756912	31.926004
628.922006	37002.665875	31.931021
629.988021	37046.838654	31.936039
631.069450	37087.480369	31.941056
631.718043	37128.295174	31.946074
632.232044	37169.347524	31.951092
632.787480	37208.917544	31.956109
633.704737	37243.256733	31.961127
634.353996	37266.364914	31.966144
634.736030	37306.164600	31.971162
635.567840	37335.016296	31.976180
635.683255	37370.155131	31.981197
636.379402	37407.058985	31.986215
636.690727	37445.651422	31.991232
636.987671	37493.651665	31.996250
637.628695	37534.214798	32.001268
638.159446	37594.505314	32.006285
638.481170	37650.163626	32.011303
639.608892	37682.686853	32.016320
639.935434	37738.481869	32.021338
640.918996	37789.457818	32.026356
641.187970	37838.988257	32.031373
642.049188	37880.308710	32.036391
643.428022	37914.438584	32.041408
644.096407	37976.752089	32.046426
644.924955	38000.110246	32.051444
645.682525	38049.904090	32.056461
646.055727	38091.991844	32.061479
647.283283	38108.335970	32.066496
648.415677	38143.801706	32.071514
648.781336	38176.276941	32.076532
649.295457	38204.248806	32.081549
649.859015	38234.720019	32.086567
650.523861	38272.103800	32.091584
650.415268	38317.870342	32.096602
651.211153	38349.909996	32.101620
651.640279	38398.934052	32.106637
652.186525	38449.458114	32.111655
652.905525	38497.073889	32.116672
652.727453	38547.795577	32.121690
653.321434	38610.216292	32.126708
653.996554	38675.407507	32.131725
654.563957	38746.526292	32.136743
655.150676	38810.675588	32.141760
655.363826	38882.292878	32.146778
656.292286	38951.295596	32.151796
656.830727	39024.824933	32.156813
657.185502	39095.502804	32.161831
657.973011	39156.396632	32.166848
658.293095	39240.629561	32.171866
659.020843	39318.390888	32.176884
659.860687	39396.612535	32.181901
660.690158	39474.457724	32.186919
661.541358	39543.541373	32.191936
661.935046	39622.781274	32.196954
662.724449	39700.668566	32.201972
663.584091	39753.266043	32.206989
663.928181	39832.114259	32.212007
665.251791	39901.963091	32.217024
665.690097	39977.406440	32.222042
665.987481	40037.853160	32.227060
666.874373	40118.555979	32.232077
667.592179	40183.591610	32.237095
668.573670	40242.362565	32.242112
668.583150	40308.006640	32.247130
669.689178	40355.217453	32.252148
670.055025	40432.093672	32.257165
670.295423	40501.486616	32.262183
671.097949	40566.384045	32.267200
671.817825	40633.893875	32.272218
672.682572	40702.383916	32.277236
673.445361	40781.062584	32.282253
673.995792	40849.546486	32.287271
674.999660	40912.886555	32.292288
675.525174	40987.547686	32.297306
675.816475	41057.250186	32.302324
676.716211	41117.980146	32.307341
677.200023	41205.672593	32.312359
677.936234	41275.115880	32.317376
678.498743	41356.298836	32.322394
679.167525	41430.062192	32.327412
680.334559	41500.179042	32.332429
680.739177	41575.341421	32.337447
681.724054	41645.860075	32.342464
682.043831	41725.086742	32.347482
682.675807	41790.233594	32.352500
683.591294	41864.334893	32.357517
684.420942	41942.153394	32.362535
685.046817	42015.941859	32.367552
685.485901	42094.034574	32.372570
686.497718	42169.005071	32.377588
687.068105	42255.654423	32.382605
687.335370	42324.656123	32.387623
688.339149	42399.442789	32.392640
689.140502	42474.965452	32.397658
690.086851	42551.929032	32.402676
691.179525	42612.841735	32.407693
691.816829	42687.949820	32.412711
692.866821	42745.418770	32.417728
693.581002	42815.553134	32.422746
694.281209	42867.844841	32.427764
695.167907	42931.804036	32.432781
696.070334	42992.382441	32.437799
697.045196	43034.895986	32.442816
697.768955	43080.023740	32.447834
698.549554	43132.571584	32.452852
698.880615	43175.569683	32.457869
699.881926	43224.499060	32.462887
701.299765	43258.068761	32.467904
702.109096	43306.760797	32.472922
702.992808	43338.778458	32.477940
703.701605	43375.653748	32.482957
704.127475	43414.400691	32.487975
705.521264	43431.822885	32.492992
706.103193	43471.384240	32.498010
706.535813	43507.969392	32.503028
707.166921	43536.210520	32.508045
707.465321	43572.356599	32.513063
707.960530	43607.039202	32.518080
708.264316	43644.320251	32.523098
708.873760	43676.902725	32.528116
709.383092	43714.974570	32.533133
709.631459	43776.757682	32.538151
710.339611	43830.152015	32.543168
710.745889	43881.891030	32.548186
711.120226	43950.434176	32.553204
711.630301	44005.359076	32.558221
711.834988	44081.914380	32.563239
712.619094	44152.819081	32.568256
712.890190	44243.365348	32.573274
713.680803	44322.386943	32.578292
714.252213	44405.201167	32.583309
714.640044	44500.399291	32.588327
715.279375	44579.433515	32.593344
716.213093	44682.647343	32.598362
716.717556	44773.985773	32.603380
717.510169	44864.884443	32.608397
718.334492	44957.308665	32.613415
719.541948	45039.207507	32.618432
719.918084	45132.947050	32.623450
720.852378	45231.624070	32.628468
721.820631	45317.890897	32.633485
722.221614	45417.363738	32.638503
723.049361	45496.592953	32.643520
724.020582	45582.106561	32.648538
724.879827	45654.519795	32.653556
726.260071	45734.933604	32.658573
727.678115	45791.552640	32.663591
728.965612	45853.303848	32.668608
730.046493	45906.563153	32.673626
731.255981	45952.094277	32.678644
732.596185	45987.943823	32.683661
732.612496	46029.645522	32.688679
733.360287	46069.647004	32.693696
734.485901	46120.861644	32.698714
734.406518	46173.101224	32.703732
734.912017	46219.615934	32.708749
735.322795	46282.009895	32.713767
736.277997	46331.214057	32.718784
737.076882	46386.154083	32.723802
737.412857	46444.790112	32.728820
738.279678	46500.906026	32.733837
738.913815	46564.448621	32.738855
739.380641	46620.634906	32.743872
740.432245	46694.839204	32.748890
740.680361	46760.204570	32.753908
741.675065	46827.691541	32.758925
741.980120	46896.635855	32.763943
743.192772	46958.607959	32.768960
743.506734	47026.456486	32.773978
744.095837	47099.407744	32.778996
744.853265	47170.142728	32.784013
745.166778	47255.409472	32.789031
745.873607	47324.124259	32.794048
746.671363	47389.543284	32.799066
747.193051	47458.698262	32.804084
747.975544	47530.525604	32.809101
748.838517	47608.692202	32.814119
749.483665	47674.843382	32.819136
750.480052	47748.562346	32.824154
750.784239	47825.673446	32.829172
752.052483	47902.072897	32.834189
752.561012	47988.722600	32.839207
753.482111	48040.836817	32.844224
754.769460	48108.780656	32.849242
755.861681	48166.876015	32.854260
757.353761	48211.582288	32.859277
758.084381	48270.382427	32.864295
758.993950	48314.616859	32.869312
759.552305	48368.575803	32.874330
760.096838	48421.792409	32.879348
761.002617	48468.691091	32.884365
761.199604	48535.364910	32.889383
761.844933	48593.902009	32.894400
762.728661	48659.977861	32.899418
763.130658	48733.341140	32.904436
763.777528	48802.572939	32.909453
764.418978	48878.782909	32.914471
765.072615	48951.406483	32.919488
765.592119	49031.426414	32.924506
765.849738	49113.463826	32.929524
766.641444	49193.198166	32.934541
767.382364	49294.730886	32.939559
767.827838	49382.814311	32.944576
768.394325	49482.151099	32.949594
769.393979	49584.613082	32.954612
770.292861	49673.051783	32.959629
770.609885	49777.277145	32.964647
771.378756	49874.305433	32.969664
772.195661	49977.272122	32.974682
772.849549	50076.850761	32.979700
773.840264	50180.516788	32.984717
774.623402	50284.468925	32.989735
775.768238	50383.964806	32.994752
776.724210	50476.466302	32.999770
777.527919	50572.211532	33.004788
778.876659	50646.056814	33.009805
780.294167	50718.619616	33.014823
781.301815	50797.338922	33.019840
782.390036	50868.657657	33.024858
782.816468	50942.909766	33.029876
783.938953	51011.919760	33.034893
784.261265	51077.200771	33.039911
785.197039	51161.973682	33.044928
786.078519	51231.704581	33.049946
786.475754	51293.808965	33.054964
787.547497	51366.606164	33.059981
788.133511	51438.360578	33.064999
788.866563	51499.326532	33.070016
789.712353	51562.424035	33.075034
790.032409	51644.784992	33.080052
791.118587	51693.897935	33.085069
791.702859	51765.836982	33.090087
792.477360	51840.277247	33.095104
793.185196	51914.071954	33.100122
793.730817	51983.840288	33.105140
794.790719	52039.958698	33.110157
795.945518	52116.577284	33.115175
796.491591	52190.638739	33.120192
797.514298	52270.293161	33.125210
797.641729	52344.510256	33.130228
798.864342	52413.266653	33.135245
799.342627	52496.449013	33.140263
800.096226	52572.874583	33.145280
801.063017	52648.026129	33.150298
801.821421	52719.048027	33.155316
802.833465	52801.285162	33.160333
803.597237	52887.125657	33.165351
804.143742	52971.123131	33.170368
805.376960	53038.163177	33.175386
805.725675	53121.804601	33.180404
806.751183	53200.427385	33.185421
807.289938	53294.329092	33.190439
808.009520	53388.271940	33.195456
808.763611	53468.372088	33.200474
809.269381	53558.328585	33.205492
810.484292	53650.082296	33.210509
810.669864	53740.387362	33.215527
811.598210	53830.514675	33.220544
812.695386	53920.277817	33.225562
813.029780	54029.370128	33.230580
813.800151	54129.489148	33.235597
815.003511	54228.274027	33.240615
815.726051	54333.303881	33.245632
816.786766	54419.467339	33.250650
817.066564	54535.661020	33.255668
818.189796	54626.938653	33.260685
818.956300	54725.527441	33.265703
819.776522	54830.771880	33.270720
820.752578	54929.937647	33.275738
821.653275	55025.492081	33.280756
823.421858	55109.980414	33.285773
824.320266	55193.531202	33.290791
824.802566	55270.787814	33.295808
826.008001	55355.426891	33.300826
826.295688	55440.483910	33.305844
827.228029	55521.016096	33.310861
828.182968	55628.702788	33.315879
828.667833	55715.737408	33.320896
830.033923	55785.815870	33.325914
831.147432	55874.020220	33.330932
831.900278	55956.221272	33.335949
832.451697	56031.727506	33.340967
833.097300	56109.012157	33.345984
834.210506	56179.113428	33.351002
834.742814	56263.750177	33.356020
835.911840	56326.187674	33.361037
836.337040	56410.659044	33.366055
837.184975	56487.733135	33.371072
838.322926	56554.501341	33.376090
838.653125	56642.164769	33.381108
839.293490	56721.233340	33.386125
840.430781	56805.773129	33.391143
841.173469	56879.885419	33.396160
842.183131	56964.973468	33.401178
842.832660	57055.609288	33.406196
843.619790	57134.962500	33.411213
844.798522	57213.202429	33.416231
845.718634	57300.067906	33.421248
846.325173	57380.833708	33.426266
847.196294	57459.467758	33.431284
848.494984	57542.665565	33.436301
849.204559	57621.752224	33.441319
849.748571	57717.282665	33.446336
850.710031	57801.709761	33.451354
851.075068	57892.458091	33.456372
852.108240	57985.455785	33.461389
852.335630	58082.594984	33.466407
853.196211	58184.704401	33.471424
854.718288	58277.445784	33.476442
855.097808	58390.301174	33.481460
855.881449	58485.601671	33.486477
857.029768	58577.845200	33.491495
857.994821	58669.938388	33.496512
859.350318	58757.161306	33.501530
859.887066	58857.567325	33.506548
861.258961	58944.782197	33.511565
862.504549	59029.889521	33.516583
863.097441	59111.612212	33.521600
864.425959	59183.354521	33.526618
865.376522	59268.958236	33.531636
866.313088	59342.907409	33.536653
867.429691	59414.504361	33.541671
867.716674	59490.865573	33.546688
868.487026	59569.827687	33.551706
869.187888	59666.631386	33.556724
870.047740	59750.796151	33.561741
870.816499	59840.258277	33.566759
871.067544	59939.452569	33.571776
872.560053	60020.252995	33.576794
873.055325	60121.565971	33.581812
873.926252	60208.219167	33.586829
874.776853	60298.387217	33.591847
875.567295	60402.180787	33.596864
876.725381	60491.063053	33.601882
877.077998	60603.857114	33.606900
877.692433	60687.162051	33.611917
879.033945	60790.930062	33.616935
879.400693	60884.184004	33.621952
880.537424	60971.360480	33.626970
881.320723	61061.842877	33.631988
881.974352	61155.889297	33.637005
882.862880	61248.225208	33.642023
883.979627	61344.017718	33.647040
885.115223	61433.596399	33.652058
885.911915	61532.364883	33.657076
886.457871	61621.482520	33.662093
887.791296	61707.870071	33.667111
888.262954	61814.043125	33.672128
889.409874	61906.994803	33.677146
890.007782	62014.194132	33.682164
891.241645	62110.672933	33.687181
891.971601	62209.499779	33.692199
892.447562	62311.661256	33.697216
893.282847	62402.896531	33.702234
894.195073	62519.623515	33.707252
895.237845	62624.052295	33.712269
896.683885	62717.377197	33.717287
897.737975	62827.022266	33.722304
898.950641	62917.268350	33.727322
899.739279	63020.931302	33.732340
899.988262	63115.288683	33.737357
901.122355	63212.947961	33.742375
902.270833	63319.226989	33.747392
903.059677	63407.720633	33.752410
903.734215	63529.203497	33.757428
904.564209	63628.571301	33.762445
905.688966	63728.650671	33.767463
906.320924	63840.222568	33.772480
907.034309	63946.302721	33.777498
907.937870	64054.601833	33.782516
908.507904	64166.330761	33.787533
909.249464	64283.098848	33.792551
910.169944	64416.663188	33.797568
910.979705	64526.900113	33.802586
911.746170	64653.109724	33.807604
912.831317	64772.355907	33.812621
914.523627	64887.457233	33.817639
915.708773	64999.172084	33.822656
916.871307	65098.630402	33.827674
917.966186	65201.956386	33.832692
918.940387	65313.791908	33.837709
920.142031	65402.434370	33.842727
920.965730	65510.268002	33.847744
921.741941	65601.332108	33.852762
922.773904	65698.290702	33.857780
923.488903	65794.627463	33.862797
924.931962	65887.993575	33.867815
925.698669	65997.838327	33.872832
926.990735	66092.912945	33.877850
927.565599	66194.362387	33.882868
927.976903	66289.843438	33.887885
929.074734	66378.917519	33.892903
930.164406	66464.234587	33.897920
930.948311	66548.071921	33.902938
931.697203	66638.428258	33.907956
932.301459	66735.093708	33.912973
933.684995	66828.818128	33.917991
934.200564	66933.281588	33.923008
934.777360	67030.616199	33.928026
935.744669	67123.928154	33.933044
936.836806	67226.696831	33.938061
938.223025	67312.709587	33.943079
939.934978	67400.420838	33.948096
941.717546	67458.125733	33.953114
943.072871	67543.860144	33.958132
943.475637	67621.331516	33.963149
944.531098	67687.921555	33.968167
945.238148	67765.465118	33.973184
946.266852	67840.967758	33.978202
947.229018	67916.140125	33.983220
947.689571	68000.407917	33.988237
948.732954	68084.109509	33.993255
949.543938	68160.608321	33.998272
950.659147	68239.769342	34.003290
951.286435	68324.643779	34.008308
952.029240	68412.614884	34.013325
953.108614	68505.764003	34.018343
953.754083	68607.796035	34.023360
954.771714	68686.525824	34.028378
955.556697	68795.031433	34.033396
956.336946	68897.062480	34.038413
957.141687	68997.990829	34.043431
957.756334	69111.377512	34.048448
958.734532	69204.596597	34.053466
959.644348	69323.232077	34.058484
960.063192	69447.184130	34.063501
961.726449	69547.049938	34.068519
962.122963	69675.676114	34.073536
962.906164	69792.540196	34.078554
964.043787	69911.161930	34.083572
964.533872	70042.024918	34.088589
966.021255	70160.801012	34.093607
966.748081	70284.292312	34.098624
967.811419	70398.828150	34.103642
968.852228	70531.375923	34.108660
969.616528	70662.047743	34.113677
970.740160	70779.615408	34.118695
971.847478	70903.296460	34.123712
973.207867	71032.125630	34.128730
974.055056	71148.981232	34.133748
974.855469	71269.680431	34.138765
976.137162	71390.543904	34.143783
977.136901	71515.282165	34.148800
978.318732	71622.988244	34.153818
979.455839	71734.537578	34.158836
980.064021	71851.068842	34.163853
981.632973	71963.858770	34.168871
982.399407	72064.107467	34.173888
983.055051	72157.170626	34.178906
984.144239	72272.484088	34.183924
984.839419	72370.218043	34.188941
986.012544	72470.119720	34.193959
986.504571	72583.286702	34.198976
987.479108	72688.604974	34.203994
988.252382	72808.344659	34.209012
989.069540	72946.650360	34.214029
990.156280	73058.303580	34.219047
991.101592	73194.909676	34.224064
992.082550	73324.698745	34.229082
993.233746	73445.513282	34.234100
993.728972	73585.542931	34.239117
994.405165	73711.509160	34.244135
995.416367	73848.286164	34.249152
996.494378	73974.493453	34.254170
998.207968	74104.366910	34.259188
998.941741	74235.016413	34.264205
1000.193570	74364.876539	34.269223
1001.575034	74485.837645	34.274240
1002.385223	74619.321363	34.279258
1003.501953	74740.970732	34.284276
1004.596226	74871.826119	34.289293
1005.905864	74985.584371	34.294311
1007.271498	75102.064565	34.299328
1008.462159	75209.864354	34.304346
1009.648281	75320.212399	34.309364
1010.294995	75440.689393	34.314381
1011.563989	75545.956816	34.319399
1012.547561	75665.206021	34.324416
1013.287528	75782.257350	34.329434
1014.138794	75898.950358	34.334452
1015.058488	76029.329059	34.339469
1015.868217	76152.470433	34.344487
1017.183251	76266.304538	34.349504
1019.151535	76368.987431	34.354522
1020.385589	76482.620739	34.359540
1020.848285	76599.468064	34.364557
1021.710394	76702.297010	34.369575
1022.723905	76826.604601	34.374592
1023.982950	76950.861249	34.379610
1025.082399	77044.344062	34.384628
1026.619497	77146.631754	34.389645
1027.864878	77251.286023	34.394663
1028.705737	77355.335192	34.399680
1029.864350	77455.491382	34.404698
1031.171517	77549.171006	34.409716
1031.972202	77658.234091	34.414733
1033.157789	77751.099645	34.419751
1033.853593	77851.419884	34.424768
1034.821388	77953.233303	34.429786
1035.851061	78058.804607	34.434804
1036.457206	78162.718226	34.439821
1037.407547	78268.031427	34.444839
1038.413834	78371.806600	34.449856
1039.112041	78471.636449	34.454874
1040.064705	78569.112818	34.459892
1040.750328	78684.918880	34.464909
1042.263935	78785.202076	34.469927
1043.820859	78888.816411	34.474944
1045.082066	78966.643862	34.479962
1046.636357	79050.076092	34.484980
1047.733151	79143.530966	34.489997
1048.756608	79233.837326	34.495015
1049.305278	79326.179187	34.500032
1050.449769	79421.309179	34.505050
1051.338247	79511.202056	34.510068
1052.090620	79619.132733	34.515085
1053.028447	79728.058533	34.520103
1053.901015	79834.011591	34.525120
1054.617976	79940.963440	34.530138
1055.701230	80053.173918	34.535156
1056.294435	80175.602623	34.540173
1057.489363	80291.305052	34.545191
1058.804516	80406.856249	34.550208
1059.852544	80530.257753	34.555226
1060.877403	80643.435269	34.560244
1061.731398	80773.266571	34.565261
1063.002208	80881.532248	34.570279
1064.067285	81016.426784	34.575296
1064.962861	81148.510671	34.580314
1065.996749	81274.782600	34.585332
1067.175051	81397.182308	34.590349
1068.227992	81513.249165	34.595367
1069.339630	81634.813733	34.600384
1070.490590	81768.871291	34.605402
1071.703611	81890.288455	34.610420
1072.804993	82023.091123	34.615437
1073.891183	82150.972141	34.620455
1074.712242	82282.392245	34.625472
1075.644218	82404.792764	34.630490
1076.618967	82530.108049	34.635508
1077.417841	82680.260539	34.640525
1078.558661	82805.570015	34.645543
1079.521201	82946.935688	34.650560
1080.212027	83097.443416	34.655578
1081.307544	83237.386316	34.660596
1082.015747	83393.887041	34.665613
1083.217990	83539.884532	34.670631
1084.757849	83682.541606	34.675648
1086.099639	83836.447423	34.680666
1087.265170	83984.078723	34.685684
1088.135886	84126.756702	34.690701
1089.212402	84274.473730	34.695719
1090.468587	84420.234765	34.700736
1091.268586	84570.691331	34.705754
1092.786201	84712.410449	34.710772
1093.406693	84860.880625	34.715789
1094.829199	84986.449054	34.720807
1095.724655	85121.548571	34.725824
1097.164905	85256.309374	34.730842
1098.350665	85382.771399	34.735860
1099.235213	85519.525485	34.740877
1100.525764	85645.681537	34.745895
1101.393062	85781.257615	34.750912
1101.995078	85919.892915	34.755930
1103.294351	86047.788832	34.760948
1104.661302	86185.627602	34.765965
1105.296458	86322.540297	34.770983
1106.603058	86466.726447	34.776000
1107.856099	86611.307811	34.781018
1109.034589	86740.864832	34.786036
1109.522067	86900.866333	34.791053
1110.449410	87040.013580	34.796071
1111.291831	87194.130502	34.801088
1112.489490	87349.374544	34.806106
1114.126159	87506.219332	34.811124
1115.910381	87638.999019	34.816141
1117.221094	87780.853531	34.821159
1118.403240	87921.161120	34.826176
1119.469585	88072.889916	34.831194
1121.026536	88210.837895	34.836212
1122.044699	88356.682483	34.841229
1123.184074	88486.673570	34.846247
1124.367795	88627.168870	34.851264
1125.328542	88761.863449	34.856282
1126.294190	88897.222110	34.861300
1127.923194	89041.095891	34.866317
1128.789086	89179.103003	34.871335
1130.359758	89302.029523	34.876352
1131.295395	89438.174192	34.881370
1132.506205	89571.303537	34.886388
1133.596250	89719.005150	34.891405
1134.618402	89855.859633	34.896423
1136.132471	89993.186963	34.901440
1136.642521	90134.709817	34.906458
1138.382986	90271.496932	34.911476
1139.235704	90407.205451	34.916493
1140.247424	90546.886639	34.921511
1141.418134	90691.805496	34.926528
1142.532729	90833.508666	34.931546
1143.727482	90967.515517	34.936564
1144.619010	91115.953811	34.941581
1145.749885	91267.220158	34.946599
1146.767159	91408.512417	34.951616
1147.950947	91554.845300	34.956634
1149.439024	91695.748283	34.961652
1150.569540	91847.625850	34.966669
1151.483602	91989.349355	34.971687
1152.820057	92136.281651	34.976704
1153.807747	92287.059091	34.981722
1154.745337	92423.006851	34.986740
1156.139194	92580.609720	34.991757
1157.160693	92725.578284	34.996775
1158.537884	92853.773682	35.001792
1159.152265	93003.963851	35.006810
1160.037437	93141.695409	35.011828
1160.965976	93294.538477	35.016845
1162.036375	93428.883597	35.021863
1163.413149	93582.036876	35.026880
1163.996573	93747.468582	35.031898
1165.367073	93885.918233	35.036916
1166.767538	94034.314060	35.041933
1168.228044	94199.306002	35.046951
1169.064767	94352.733873	35.051968
1170.075082	94505.489968	35.056986
1171.481288	94665.161420	35.062004
1173.009727	94809.993295	35.067021
1174.199936	94957.549377	35.072039
1175.719036	95114.093767	35.077056
1176.649944	95275.344354	35.082074
1178.200449	95416.678401	35.087092
1179.366814	95560.029143	35.092109
1180.362276	95703.091670	35.097127
1182.133235	95839.977753	35.102144
1183.733619	95987.905517	35.107162
1185.194084	96115.960807	35.112180
1186.800650	96255.823525	35.117197
1188.079442	96379.411285	35.122215
1189.213076	96500.372107	35.127232
1190.400084	96641.202241	35.132250
1191.433035	96770.499566	35.137268
1192.452747	96901.216832	35.142285
1193.252620	97043.585052	35.147303
1194.743223	97165.935068	35.152320
1195.434721	97310.871736	35.157338
1196.639771	97454.924198	35.162356
1198.202727	97597.661678	35.167373
1199.337426	97736.425460	35.172391
1200.376730	97870.510901	35.177408
1201.853170	98007.608701	35.182426
1203.620439	98141.833047	35.187444
1204.604630	98276.777406	35.192461
1205.539394	98408.896025	35.197479
1207.187917	98547.140141	35.202496
1208.113445	98690.795615	35.207514
1208.905360	98823.616301	35.212532
1209.949341	98966.906684	35.217549
1210.501431	99124.214460	35.222567
1211.849541	99270.621852	35.227584
1212.932730	99436.629189	35.232602
1214.102411	99584.781572	35.237620
1215.275820	99742.848923	35.242637
1216.037403	99916.724845	35.247655
1217.517126	100074.625538	35.252672
1218.498793	100246.526481	35.257690
1219.507703	100413.229639	35.262708
1220.816671	100591.731100	35.267725
1221.483313	100761.502995	35.272743
1222.982937	100930.397045	35.277760
1223.592932	101088.379627	35.282778
1224.847349	101250.095306	35.287796
1226.293086	101424.202734	35.292813
1227.062241	101599.779473	35.297831
1228.763395	101768.172964	35.302848
1229.911871	101935.624118	35.307866
1231.159144	102116.349080	35.312884
1232.053656	102283.646933	35.317901
1233.401235	102466.048163	35.322919
1234.829467	102641.331734	35.327936
1235.885072	102812.132378	35.332954
1237.539722	102981.510135	35.337972
1238.719626	103159.937766	35.342989
1240.082426	103344.267096	35.348007
1241.688459	103503.423786	35.353024
1242.492660	103695.096713	35.358042
1243.932989	103858.433430	35.363060
1245.115342	104045.062410	35.368077
1246.648841	104204.121427	35.373095
1248.924275	104363.677405	35.378112
1250.193703	104540.987398	35.383130
1251.766715	104695.632513	35.388148
1252.551689	104854.340245	35.393165
1254.015551	105022.630105	35.398183
1255.432014	105178.163919	35.403200
1256.516332	105337.460127	35.408218
1257.570498	105498.287399	35.413236
1259.103685	105660.539500	35.418253
1260.090485	105833.271389	35.423271
1261.533780	105997.400715	35.428288
1262.441724	106175.799225	35.433306
1263.353240	106345.065890	35.438324
1264.796257	106515.274534	35.443341
1265.588276	106700.144545	35.448359
1267.012954	106873.295281	35.453376
1268.265298	107053.139177	35.458394
1269.795974	107229.351546	35.463412
1271.366871	107393.799202	35.468429
1273.143148	107569.361072	35.473447
1274.961723	107716.334558	35.478464
1276.542500	107872.131800	35.483482
1277.960585	108022.487360	35.488500
1279.529446	108165.908205	35.493517
1280.549442	108320.329054	35.498535
1282.573929	108464.698264	35.503552
1283.604243	108603.523509	35.508570
1285.006127	108744.948874	35.513588
1286.463148	108876.897276	35.518605
1287.608397	109013.978613	35.523623
1288.984706	109143.820874	35.528640
1290.250661	109286.581213	35.533658
1291.201105	109428.297501	35.538676
1292.310376	109574.534109	35.543693
1293.025378	109722.068568	35.548711
1294.178282	109862.577838	35.553728
1295.408322	110002.588251	35.558746
1296.332981	110133.032917	35.563764
1297.550964	110279.522287	35.568781
1298.454917	110423.941912	35.573799
1299.790731	110579.852295	35.578816
1300.943309	110747.085571	35.583834
1301.809142	110903.876621	35.588852
1303.385221	111061.081160	35.593869
1304.002444	111233.656817	35.598887
1305.148750	111409.833748	35.603904
1306.181639	111598.563852	35.608922
1307.185898	111787.749389	35.613940
1308.621585	111962.371288	35.618957
1309.820729	112153.769565	35.623975
1311.666817	112342.002538	35.628992
1313.344719	112520.616001	35.634010
1315.019988	112698.275250	35.639028
1316.732037	112865.047655	35.644045
1317.942075	113043.796197	35.649063
1319.584455	113221.590996	35.654080
1320.845197	113387.659941	35.659098
1322.416025	113559.410020	35.664116
1324.018423	113712.607042	35.669133
1325.234793	113893.696677	35.674151
1327.002759	114044.419367	35.679168
1327.978516	114221.662446	35.684186
1329.069602	114383.510543	35.689204
1330.494156	114547.376904	35.694221
1331.723056	114723.272740	35.699239
1333.116362	114895.319689	35.704256
1334.501759	115061.322838	35.709274
1335.848062	115229.941724	35.714292
1337.461930	115390.294963	35.719309
1338.548332	115564.972024	35.724327
1340.196524	115735.616591	35.729344
1341.290824	115915.169886	35.734362
1342.441491	116092.119617	35.739380
1343.933814	116258.113560	35.744397
1344.859027	116440.565547	35.749415
1345.906521	116617.649270	35.754432
1346.932123	116809.243281	35.759450
1348.374092	116998.702104	35.764468
1349.982294	117187.186154	35.769485
1351.288986	117371.882499	35.774503
1352.911343	117555.782848	35.779520
1354.587709	117743.791582	35.784538
1355.558827	117930.273832	35.789556
1357.212259	118112.621903	35.794573
1358.837781	118294.956699	35.799591
1360.205308	118477.890993	35.804608
1361.447100	118652.140051	35.809626
1362.929716	118827.586748	35.814644
1365.383869	118978.495348	35.819661
1366.839242	119137.390069	35.824679
1368.614536	119282.874054	35.829696
1370.198953	119416.269374	35.834714
1370.948428	119553.382114	35.839732
1372.676591	119690.669303	35.844749
1373.808191	119839.057548	35.849767
1374.932609	119974.061236	35.854784
1375.744718	120117.182679	35.859802
1376.757541	120266.263446	35.864820
1378.503465	120412.872881	35.869837
1379.323510	120577.006576	35.874855
1380.857939	120736.531674	35.879872
1382.334828	120913.532051	35.884890
1383.234086	121078.479506	35.889908
1384.997283	121232.677200	35.894925
1386.172350	121401.927020	35.899943
1387.554559	121571.790936	35.904960
1388.969794	121743.322538	35.909978
1390.206265	121920.469178	35.914996
1391.743476	122085.321507	35.920013
1392.464341	122276.573349	35.925031
1393.915023	122457.375251	35.930048
1395.137767	122645.434179	35.935066
1395.832083	122839.582101	35.940084
1397.210979	123034.559926	35.945101
1398.725792	123248.428214	35.950119
1400.501649	123434.213524	35.955136
1402.548246	123616.473840	35.960154
1404.125160	123819.798381	35.965172
1405.714605	123995.446017	35.970189
1407.057528	124188.423948	35.975207
1408.356898	124372.682796	35.980224
1410.038024	124556.476894	35.985242
1410.969209	124756.820405	35.990260
1412.487142	124946.913212	35.995277
1413.767726	125147.267415	36.000295
1414.987314	125344.149311	36.005312
1416.286582	125544.883489	36.010330
1417.421392	125738.842900	36.015348
1419.242183	125925.461556	36.020365
1420.415037	126139.052334	36.025383
1421.860743	126340.972510	36.030400
1423.663864	126544.496852	36.035418
1424.969689	126749.140493	36.040436
1426.725893	126949.077625	36.045453
1428.470971	127145.977653	36.050471
1429.914602	127347.449508	36.055488
1431.292363	127544.106716	36.060506
1432.820469	127745.327356	36.065524
1434.404158	127920.912488	36.070541
1436.243112	128105.300755	36.075559
1438.166641	128278.693184	36.080576
1440.184735	128442.152143	36.085594
1441.274453	128625.662108	36.090612
1442.695623	128787.887742	36.095629
1444.459171	128961.499887	36.100647
1445.723873	129109.183081	36.105664
1447.066192	129274.464617	36.110682
1447.985881	129426.638461	36.115700
1449.189821	129592.932054	36.120717
1450.062164	129767.653676	36.125735
1451.477973	129936.284783	36.130752
1453.129217	130108.300221	36.135770
1453.953068	130295.486821	36.140788
1455.638429	130473.174985	36.145805
1457.085235	130660.974520	36.150823
1458.716897	130826.637311	36.155840
1459.785373	131017.666756	36.160858
1461.146992	131223.715379	36.165876
1462.807266	131407.786352	36.170893
1464.000430	131604.957537	36.175911
1464.993582	131806.140290	36.180928
1466.766205	132002.613992	36.185946
1468.098868	132216.517276	36.190964
1469.287292	132404.128662	36.195981
1470.983841	132618.762702	36.200999
1472.394772	132825.055810	36.206016
1473.650471	133040.396585	36.211034
1474.809644	133263.065345	36.216052
1476.447145	133482.542792	36.221069
1478.303422	133702.684054	36.226087
1479.922184	133915.730928	36.231104
1481.684596	134126.754508	36.236122
1483.348400	134336.426800	36.241140
1485.113595	134543.930374	36.246157
1486.392062	134753.641565	36.251175
1487.881171	134964.511922	36.256192
1489.326523	135176.277771	36.261210
1490.629896	135396.304322	36.266228
1492.244872	135611.594456	36.271245
1493.472769	135833.232932	36.276263
1494.436726	136061.580485	36.281280
1495.978660	136274.200629	36.286298
1497.730529	136502.793915	36.291316
1499.566618	136729.702855	36.296333
1500.896348	136950.471856	36.301351
1502.524719	137176.834306	36.306368
1504.047580	137412.276137	36.311386
1505.011872	137631.524205	36.316404
1506.955040	137862.137907	36.321421
1508.677098	138085.032738	36.326439
1509.816798	138320.276505	36.331456
1511.778772	138541.831320	36.336474
1513.882637	138755.368484	36.341492
1515.290332	138977.293396	36.346509
1517.077800	139194.749296	36.351527
1518.890551	139399.491321	36.356544
1520.356544	139610.461824	36.361562
1521.925533	139817.488629	36.366580
1523.200400	140032.003028	36.371597
1524.654094	140237.378103	36.376615
1526.079143	140434.445078	36.381632
1527.796344	140623.963956	36.386650
1528.684269	140827.696584	36.391668
1530.145016	141028.095005	36.396685
1531.563298	141231.771428	36.401703
1532.809850	141434.487900	36.406720
1534.269135	141639.668767	36.411738
1535.347704	141866.926986	36.416756
1536.895840	142073.427459	36.421773
1538.480775	142290.278633	36.426791
1540.092106	142513.920784	36.431808
1541.818149	142740.208043	36.436826
1543.316731	142963.313675	36.441844
1544.618606	143187.123940	36.446861
1546.536148	143399.531854	36.451879
1548.918398	143616.088227	36.456896
1551.073968	143816.445139	36.461914
1552.353861	144027.551697	36.466932
1555.062779	144216.909835	36.471949
1556.752277	144409.105593	36.476967
1558.089245	144610.510289	36.481984
1559.622627	144796.775718	36.487002
1561.027669	144996.714384	36.492020
1562.076255	145194.327899	36.497037
1563.571642	145402.696877	36.502055
1565.050941	145612.400765	36.507072
1566.638362	145822.291688	36.512090
1567.633942	146048.541500	36.517108
1569.194904	146261.786043	36.522125
1570.629270	146487.297444	36.527143
1572.026322	146715.123479	36.532160
1573.308962	146946.100412	36.537178
1574.779443	147181.815575	36.542196
1575.964418	147427.998064	36.547213
1577.518435	147668.140381	36.552231
1578.898713	147915.892866	36.557248
1580.478884	148160.116662	36.562266
1582.022057	148408.671069	36.567284
1584.349729	148636.603800	36.572301
1587.063551	148858.226919	36.577319
1588.644394	149086.623740	36.582336
1590.826129	149298.255910	36.587354
1592.292177	149525.418989	36.592372
1593.849809	149742.312931	36.597389
1595.415969	149968.144724	36.602407
1596.692671	150199.767085	36.607424
1598.423501	150405.658974	36.612442
1599.841690	150642.485264	36.617460
1601.092360	150871.213253	36.622477
1602.805685	151101.225901	36.627495
1604.111506	151342.487059	36.632512
1605.545697	151570.138451	36.637530
1606.980427	151814.463402	36.642548
1608.467153	152061.114733	36.647565
1610.085620	152288.437501	36.652583
1611.315776	152524.711237	36.657600
1612.690386	152749.210502	36.662618
1614.014518	152988.464774	36.667636
1615.273505	153230.393676	36.672653
1617.147269	153463.376721	36.677671
1618.411781	153721.309199	36.682688
1619.571360	153969.839665	36.687706
1620.938417	154227.759725	36.692724
1622.959252	154476.321951	36.697741
1624.300787	154748.019848	36.702759
1626.172974	155014.792027	36.707776
1627.970646	155281.603490	36.712794
1629.154280	155549.972738	36.717812
1630.597140	155818.594555	36.722829
1632.268884	156088.538880	36.727847
1633.655811	156378.958193	36.732864
1635.792688	156646.030713	36.737882
1637.354117	156921.654451	36.742900
1639.232666	157201.554032	36.747917
1641.191099	157476.497787	36.752935
1643.190429	157747.544276	36.757952
1645.123155	158012.871776	36.762970
1646.847588	158285.018595	36.767988
1648.383322	158540.522128	36.773005
1650.249093	158815.085342	36.778023
1651.620869	159098.212797	36.783040
1653.462428	159358.999756	36.788058
1655.354047	159626.336905	36.793076
1656.575307	159900.516342	36.798093
1658.725052	160166.167985	36.803111
1660.239705	160442.613029	36.808128
1662.053505	160711.961700	36.813146
1663.607551	160988.062299	36.818164
1665.456669	161251.398263	36.823181
1667.557263	161513.757754	36.828199
1669.015057	161799.771785	36.833216
1671.113346	162058.850957	36.838234
1673.244329	162318.992097	36.843252
1674.996266	162565.675952	36.848269
1677.111284	162802.056445	36.853287
1678.966954	163053.901551	36.858304
1681.171433	163291.501210	36.863322
1683.333115	163512.875426	36.868340
1685.242489	163745.895734	36.873357
1687.511924	163974.484776	36.878375
1688.785588	164200.975815	36.883392
1689.983932	164418.665551	36.888410
1691.252328	164646.314302	36.893428
1692.719310	164891.384871	36.898445
1694.224966	165118.453465	36.903463
1695.338796	165370.660489	36.908480
1697.030859	165621.788091	36.913498
1698.351478	165882.767983	36.918516
1699.823506	166140.922584	36.923533
1701.806481	166388.267478	36.928551
1702.973038	166631.849744	36.933568
1705.263369	166849.240704	36.938586
1707.731982	167057.472238	36.943604
1709.805597	167274.405386	36.948621
1711.576883	167500.050945	36.953639
1713.159901	167707.006063	36.958656
1714.932204	167922.443298	36.963674
1716.752421	168142.097977	36.968692
1717.819445	168375.661326	36.973709
1719.437408	168596.581099	36.978727
1721.026106	168830.039003	36.983744
1722.450292	169056.852392	36.988762
1724.115699	169303.987562	36.993780
1725.056591	169547.104150	36.998797
1726.737784	169794.721956	37.003815
1727.997112	170074.780008	37.008832
1729.741966	170327.135216	37.013850
1731.366042	170605.832609	37.018868
1732.739618	170870.808428	37.023885
1734.788788	171124.160620	37.028903
1737.014570	171402.768119	37.033920
1738.549713	171676.514585	37.038938
1740.273131	171949.091356	37.043956
1742.048054	172222.334151	37.048973
1743.803044	172498.969042	37.053991
1745.259370	172774.892126	37.059008
1746.782274	173054.231701	37.064026
1748.825792	173357.086290	37.069044
1750.318494	173644.794754	37.074061
1752.525967	173932.214171	37.079079
1754.007934	174226.893123	37.084096
1755.560378	174521.588392	37.089114
1757.495089	174822.809304	37.094132
1759.327143	175111.654091	37.099149
1761.685038	175386.208524	37.104167
1763.480962	175665.573431	37.109184
1766.203207	175938.957283	37.114202
1768.795602	176211.843403	37.119220
1770.789338	176478.901610	37.124237
1772.495255	176728.105973	37.129255
1774.297639	176990.427557	37.134272
1776.003170	177246.536806	37.139290
1777.933592	177501.038706	37.144308
1780.082332	177749.544488	37.149325
1781.963502	177993.831280	37.154343
1783.023777	178248.513904	37.159360
1784.835660	178506.669280	37.164378
1786.377077	178768.713489	37.169396
1787.951063	179038.899587	37.174413
1789.391190	179306.456915	37.179431
1790.971515	179582.088457	37.184448
1792.836170	179845.407469	37.189466
1794.495283	180124.772895	37.194484
1796.222051	180394.727564	37.199501
1799.326581	180645.851755	37.204519
1800.961211	180892.490759	37.209536
1802.976235	181128.704485	37.214554
1804.799859	181358.897556	37.219572
1806.044706	181601.580252	37.224589
1807.695510	181848.209389	37.229607
1808.802274	182107.767046	37.234624
1810.355067	182354.287685	37.239642
1811.931378	182623.924697	37.244660
1813.449860	182891.884922	37.249677
1815.228364	183160.693698	37.254695
1816.738517	183448.833806	37.259712
1818.477389	183739.033138	37.264730
1820.515442	184026.369878	37.269748
1821.721220	184316.632179	37.274765
1823.549376	184605.350970	37.279783
1825.083370	184918.126453	37.284800
1826.649732	185224.998376	37.289818
1828.482919	185528.073916	37.294836
1829.581401	185856.710659	37.299853
1831.537771	186178.132733	37.304871
1833.307210	186512.936326	37.309888
1834.905615	186843.899084	37.314906
1836.910877	187185.091138	37.319924
1838.619957	187528.375790	37.324941
1840.336315	187866.293878	37.329959
1841.860327	188211.402195	37.334976
1844.021740	188556.107280	37.339994
1846.314992	188909.804116	37.345012
1848.347144	189248.659084	37.350029
1850.707101	189585.763879	37.355047
1852.671032	189918.124141	37.360064
1854.627377	190261.401936	37.365082
1856.979284	190582.143908	37.370100
1859.073912	190919.718915	37.375117
1861.031659	191249.157665	37.380135
1863.089287	191575.410001	37.385152
1865.126077	191905.792437	37.390170
1867.140620	192226.814465	37.395188
1868.893938	192548.108477	37.400205
1871.348844	192865.688836	37.405223
1872.929675	193189.692241	37.410240
1874.639796	193506.569929	37.415258
1876.680825	193817.076639	37.420276
1878.523800	194137.732003	37.425293
1880.887053	194453.851982	37.430311
1882.903072	194763.035801	37.435328
1884.977405	195075.791366	37.440346
1887.028424	195383.298027	37.445364
1888.848957	195692.569230	37.450381
1890.886695	195987.795622	37.455399
1892.537561	196294.838130	37.460416
1894.685638	196606.740848	37.465434
1896.916670	196898.019773	37.470452
1898.576329	197197.488800	37.475469
1900.877241	197476.130808	37.480487
1902.748452	197764.565026	37.485504
1904.736034	198032.369416	37.490522
1906.280085	198295.257293	37.495540
1907.750616	198577.679667	37.500557
1909.967757	198849.729185	37.505575
1911.662398	199123.348073	37.510592
1913.044776	199401.282750	37.515610
1914.779210	199685.941072	37.520628
1916.400571	199985.672884	37.525645
1918.120140	200273.547984	37.530663
1919.643518	200589.901358	37.535680
1921.523080	200882.374596	37.540698
1923.558038	201196.390825	37.545716
1925.383351	201517.385434	37.550733
1927.119616	201829.548601	37.555751
1929.120634	202158.871356	37.560768
1930.488621	202486.430517	37.565786
1932.953563	202808.168748	37.570804
1934.662288	203146.594284	37.575821
1936.466947	203471.005192	37.580839
1938.426526	203813.329963	37.585856
1940.076033	204152.189708	37.590874
1942.322697	204487.935454	37.595892
1944.114570	204843.774093	37.600909
1946.114739	205175.437276	37.605927
1948.197364	205527.285981	37.610944
1950.132568	205873.066834	37.615962
1952.065455	206224.283316	37.620980
1953.943653	206585.247290	37.625997
1955.814464	206928.683258	37.631015
1957.833785	207289.781384	37.636032
1960.029692	207647.273691	37.641050
1962.143400	207992.416307	37.646068
1964.029601	208357.756563	37.651085
1966.410861	208705.996373	37.656103
1968.588731	209056.657089	37.661120
1970.608683	209411.496155	37.666138
1973.129260	209754.603544	37.671156
1974.586952	210110.272089	37.676173
1976.794482	210448.113571	37.681191
1979.040777	210787.321799	37.686208
1981.190929	211124.033362	37.691226
1983.472661	211457.831209	37.696244
1985.240929	211793.464249	37.701261
1987.570890	212134.989569	37.706279
1989.978267	212466.868286	37.711296
1992.226548	212794.051064	37.716314
1993.861562	213122.234176	37.721332
1995.684628	213455.137356	37.726349
1997.808394	213784.731596	37.731367
1999.659334	214122.407365	37.736384
2001.816213	214453.231132	37.741402
2004.120231	214776.364644	37.746420
2005.502041	215106.844795	37.751437
2007.429442	215434.573730	37.756455
2009.538461	215739.904351	37.761472
2011.192850	216058.487360	37.766490
2012.847060	216379.877774	37.771508
2014.885499	216694.695351	37.776525
2016.913304	217010.036578	37.781543
2018.805843	217329.552477	37.786560
2020.430414	217657.847671	37.791578
2022.642663	217982.915010	37.796596
2024.131987	218321.633352	37.801613
2026.265849	218657.330715	37.806631
2028.753132	218985.037937	37.811648
2030.652463	219323.949795	37.816666
2032.832164	219660.444364	37.821684
2034.638418	220005.329023	37.826701
2036.688049	220382.579907	37.831719
2038.717078	220741.043988	37.836736
2040.922056	221091.393646	37.841754
2043.370299	221424.260113	37.846772
2044.765827	221779.718699	37.851789
2046.692382	222124.073238	37.856807
2048.655743	222487.799911	37.861824
2050.340789	222853.997662	37.866842
2052.989821	223211.460544	37.871860
2054.623862	223567.422652	37.876877
2057.200257	223926.817605	37.881895
2059.359895	224285.670775	37.886912
2061.317043	224658.499931	37.891930
2063.347689	225021.402020	37.896948
2065.076661	225398.968958	37.901965
2067.213276	225774.771394	37.906983
2070.553722	226120.366185	37.912000
2072.994888	226460.467069	37.917018
2075.249944	226805.982877	37.922036
2076.824342	227165.779319	37.927053
2079.336336	227518.926977	37.932071
2081.720818	227870.064554	37.937088
2083.464152	228218.765559	37.942106
2085.995539	228553.374608	37.947124
2090.342628	228849.245787	37.952141
2092.739485	229150.024194	37.957159
2095.657584	229443.584309	37.962176
2097.524630	229747.242435	37.967194
2099.537809	230040.490870	37.972212
2101.099124	230342.345454	37.977229
2103.346883	230632.079104	37.982247
2104.961740	230936.771642	37.987264
2107.744881	231209.862923	37.992282
2110.604555	231497.927524	37.997300
2112.307829	231783.992218	38.002317
2113.897279	232079.777816	38.007335
2115.594245	232375.471070	38.012352
2117.337266	232673.418344	38.017370
2119.049291	232983.308560	38.022388
2120.406391	233298.818256	38.027405
2122.176183	233608.904449	38.032423
2124.044217	233911.051725	38.037440
2125.405685	234228.798706	38.042458
2127.043767	234536.317993	38.047476
2129.349018	234860.495451	38.052493
2130.626769	235195.605947	38.057511
2132.336814	235532.579253	38.062528
2134.097080	235892.430035	38.067546
2136.070734	236242.088612	38.072564
2137.601575	236611.502805	38.077581
2139.326660	236981.573223	38.082599
2141.724949	237355.500386	38.087616
2143.809791	237742.279769	38.092634
2145.848674	238134.249252	38.097652
2147.678362	238530.748979	38.102669
2149.671848	238934.615370	38.107687
2151.974185	239334.624241	38.112704
2153.877373	239752.045801	38.117722
2156.071956	240162.005870	38.122740
2158.226265	240582.946489	38.127757
2160.121144	241004.971115	38.132775
2162.632903	241419.914332	38.137792
2164.698114	241859.542514	38.142810
2167.313071	242285.495906	38.147828
2169.170388	242715.177730	38.152845
2171.455007	243145.733024	38.157863
2173.827702	243575.691552	38.162880
2176.241344	244012.579334	38.167898
2178.923753	244442.567727	38.172916
2180.804480	244885.918401	38.177933
2182.951820	245318.102645	38.182951
2185.619049	245751.272600	38.187968
2187.456185	246187.547427	38.192986
2189.985436	246625.085454	38.198004
2192.388997	247050.807788	38.203021
2194.585425	247485.988022	38.208039
2197.039590	247917.242231	38.213056
2199.298241	248347.233178	38.218074
2201.910191	248773.867087	38.223092
2204.010984	249201.980277	38.228109
2206.426079	249641.348433	38.233127
2208.791516	250058.296011	38.238144
2210.865956	250490.811186	38.243162
2212.900933	250917.389703	38.248180
2215.288314	251345.767706	38.253197
2217.280478	251780.940904	38.258215
2219.463802	252219.133059	38.263232
2221.829868	252646.171208	38.268250
2223.993239	253082.768226	38.273268
2226.288495	253520.107381	38.278285
2228.459028	253967.907567	38.283303
2231.017983	254388.695424	38.288320
2233.025716	254829.512318	38.293338
2235.660336	255243.583715	38.298356
2238.250732	255665.842480	38.303373
2240.856564	256086.727882	38.308391
2243.179622	256474.915166	38.313408
2245.027532	256869.300449	38.318426
2247.705251	257244.782348	38.323444
2249.734224	257619.377006	38.328461
2252.024954	258009.172290	38.333479
2254.212070	258388.061475	38.338496
2256.282192	258779.442483	38.343514
2258.488400	259169.633969	38.348532
2260.843488	259553.045279	38.353549
2263.825298	259935.240024	38.358567
2266.892953	260295.905486	38.363584
2269.715109	260648.811648	38.368602
2272.682248	261009.671742	38.373620
2275.014028	261361.106913	38.378637
2277.125966	261714.736581	38.383655
2278.601928	262063.564701	38.388672
2280.587792	262433.422216	38.393690
2282.857756	262804.149592	38.398708
2284.987900	263169.895123	38.403725
2287.057942	263554.042366	38.408743
2289.060028	263930.249603	38.413760
2291.162740	264313.274681	38.418778
2293.404232	264705.499452	38.423796
2295.125147	265111.677245	38.428813
2297.029601	265518.156548	38.433831
2299.180078	265928.077437	38.438848
2300.983231	266342.067445	38.443866
2303.255603	266768.659612	38.448884
2305.554023	267197.229437	38.453901
2307.564256	267639.309009	38.458919
2310.309028	268063.210696	38.463936
2312.684369	268504.597901	38.468954
2315.411740	268932.465805	38.473972
2317.969951	269359.649473	38.478989
2320.496902	269791.639551	38.484007
2324.032133	270188.997614	38.489024
2326.973202	270583.782679	38.494042
2329.699348	270981.370928	38.499060
2331.944488	271372.278259	38.504077
2334.205360	271773.903438	38.509095
2336.517503	272159.364022	38.514112
2338.808999	272566.141416	38.519130
2340.941119	272962.986007	38.524148
2343.785980	273362.410420	38.529165
2345.714584	273763.580536	38.534183
2347.978914	274160.353466	38.539200
2350.361080	274559.902095	38.544218
2352.550547	274961.107080	38.549236
2355.141466	275366.871818	38.554253
2356.938190	275778.097126	38.559271
2359.221740	276183.072170	38.564288
2361.660532	276582.459184	38.569306
2364.427205	276983.775596	38.574324
2367.247677	277383.330540	38.579341
2369.378136	277777.177369	38.584359
2371.437976	278159.527532	38.589376
2373.743714	278541.330510	38.594394
2375.182412	278918.977609	38.599412
2377.575980	279301.426834	38.604429
2379.343924	279699.064623	38.609447
2381.304724	280099.999464	38.614464
2383.687958	280509.580443	38.619482
2385.798004	280907.823801	38.624500
2388.029400	281324.261803	38.629517
2389.741018	281757.294000	38.634535
2392.136098	282195.603000	38.639552
2394.187783	282644.228948	38.644570
2396.372034	283089.048397	38.649588
2398.607245	283546.433898	38.654605
2400.869849	284011.943578	38.659623
2403.062242	284479.750147	38.664640
2405.577067	284959.139661	38.669658
2408.040117	285421.059498	38.674676
2411.020749	285885.030565	38.679693
2413.390100	286377.396803	38.684711
2415.998874	286842.771875	38.689728
2418.722818	287313.818270	38.694746
2421.025453	287792.043529	38.699764
2423.334460	288270.724270	38.704781
2425.792934	288756.442501	38.709799
2428.264845	289238.194940	38.714816
2430.873694	289722.769923	38.719834
2433.834576	290196.796939	38.724852
2437.057499	290657.343586	38.729869
2439.474176	291131.505904	38.734887
2442.081805	291610.133268	38.739904
2444.453021	292083.665837	38.744922
2446.806852	292557.250986	38.749940
2449.381159	293015.685809	38.754957
2452.038167	293490.745041	38.759975
2454.709411	293947.460562	38.764992
2457.071914	294438.339091	38.770010
2459.255398	294897.365183	38.775028
2462.014909	295370.600261	38.780045
2464.324278	295844.286549	38.785063
2466.533508	296322.255038	38.790080
2468.987317	296809.480601	38.795098
2471.322640	297290.500198	38.800116
2473.910445	297767.566617	38.805133
2476.638830	298252.687162	38.810151
2479.712445	298724.568210	38.815168
2482.115766	299197.671813	38.820186
2484.517437	299673.974885	38.825204
2487.514148	300142.765062	38.830221
2489.822583	300611.078687	38.835239
2492.854605	301076.786915	38.840256
2495.357460	301535.719279	38.845274
2497.337794	302006.011087	38.850292
2500.075612	302475.749542	38.855309
2502.460377	302931.749754	38.860327
2504.859794	303365.622112	38.865344
2507.188879	303806.921274	38.870362
2509.471957	304241.393552	38.875380
2511.823326	304672.297548	38.880397
2514.210019	305123.845126	38.885415
2516.435974	305570.971570	38.890432
2518.756138	306014.195310	38.895450
2520.778380	306488.783151	38.900468
2523.330612	306939.713956	38.905485
2525.308732	307416.591294	38.910503
2528.233160	307893.418439	38.915520
2530.563567	308371.709422	38.920538
2532.857747	308862.881873	38.925556
2535.601077	309336.785595	38.930573
2537.898595	309838.748245	38.935591
2540.287572	310327.816731	38.940608
2542.640678	310828.597840	38.945626
2544.702516	311339.912693	38.950644
2547.433192	311854.751255	38.955661
2549.963295	312375.867281	38.960679
2552.704321	312884.628950	38.965696
2555.113232	313407.384643	38.970714
2557.616642	313944.066524	38.975732
2560.533185	314459.142323	38.980749
2562.928696	314991.137099	38.985767
2565.617516	315521.025330	38.990784
2568.684379	316051.739756	38.995802
2570.603436	316587.865104	39.000820
2573.404921	317125.092149	39.005837
2576.298847	317676.270166	39.010855
2579.310048	318198.752709	39.015872
2582.051880	318738.087971	39.020890
2585.010190	319278.096884	39.025908
2587.720803	319788.909928	39.030925
2590.102506	320327.581674	39.035943
2593.101379	320848.527091	39.040960
2596.013618	321373.927521	39.045978
2598.640198	321901.223952	39.050996
2601.256328	322422.449103	39.056013
2603.335213	322947.210017	39.061031
2606.242823	323476.229844	39.066048
2608.677207	324002.883274	39.071066
2611.022202	324544.403875	39.076084
2614.189290	325063.874421	39.081101
2616.773804	325602.099373	39.086119
2619.595259	326140.232354	39.091136
2622.030428	326666.741209	39.096154
2624.754037	327191.804103	39.101172
2627.873485	327706.693696	39.106189
2630.546368	328234.652459	39.111207
2633.081495	328753.969946	39.116224
2636.031551	329281.979027	39.121242
2638.368854	329800.152434	39.126260
2641.459694	330303.601482	39.131277
2643.946793	330811.815079	39.136295
2646.233395	331309.620217	39.141312
2649.098902	331780.794392	39.146330
2651.726680	332269.067148	39.151348
2654.422689	332742.674082	39.156365
2657.092067	333222.147705	39.161383
2659.806408	333697.700452	39.166400
2662.352063	334181.884589	39.171418
2664.720693	334666.575771	39.176436
2667.388718	335152.841129	39.181453
2670.130787	335643.306248	39.186471
2672.447064	336137.770870	39.191488
2675.115489	336633.115482	39.196506
2677.473033	337140.642530	39.201524
2680.048472	337651.304956	39.206541
2682.282054	338172.021409	39.211559
2684.710830	338690.036695	39.216576
2687.195682	339224.390197	39.221594
2689.371263	339781.639180	39.226612
2691.906449	340327.273848	39.231629
2694.178796	340892.089076	39.236647
2696.783945	341457.633451	39.241664
2699.485327	342025.848558	39.246682
2702.029248	342611.398448	39.251700
2704.723343	343192.094968	39.256717
2707.346070	343779.778891	39.261735
2709.541690	344377.045110	39.266752
2712.921636	344960.205084	39.271770
2715.854564	345556.098363	39.276788
2719.052297	346144.555783	39.281805
2722.149154	346740.080675	39.286823
2725.007987	347315.251364	39.291840
2727.811350	347906.646900	39.296858
2730.253046	348512.792034	39.301876
2733.212673	349100.951343	39.306893
2736.362382	349686.764099	39.311911
2739.520319	350265.892834	39.316928
2742.412415	350842.239662	39.321946
2745.208661	351429.942466	39.326964
2748.419901	352009.170712	39.331981
2751.239425	352586.347692	39.336999
2754.002836	353163.095626	39.342016
2756.934501	353747.324064	39.347034
2759.695300	354317.535852	39.352052
2762.329085	354885.273815	39.357069
2765.343196	355467.565716	39.362087
2768.177394	356033.177605	39.367104
2771.198095	356608.221140	39.372122
2773.827772	357175.019994	39.377140
2776.645339	357734.675679	39.382157
2779.351960	358318.454864	39.387175
2781.807487	358897.723560	39.392192
2784.312887	359474.490070	39.397210
2787.007413	360059.874424	39.402228
2789.525998	360641.370873	39.407245
2791.974620	361225.764537	39.412263
2794.557920	361791.171059	39.417280
2797.513622	362348.035075	39.422298
2799.512550	362926.895151	39.427316
2801.682941	363497.092055	39.432333
2804.653635	364073.042884	39.437351
2807.045747	364663.619588	39.442368
2809.458446	365261.468671	39.447386
2811.762687	365871.431909	39.452404
2814.115203	366486.987437	39.457421
2816.966447	367116.640924	39.462439
2819.147247	367752.126547	39.467456
2822.031619	368386.527222	39.472474
2824.881659	369042.214032	39.477492
2827.360603	369692.570080	39.482509
2830.393172	370360.159458	39.487527
2832.700965	371027.066468	39.492544
2836.004721	371693.729102	39.497562
2838.851534	372378.113363	39.502580
2841.999196	373056.196944	39.507597
2844.870459	373735.860857	39.512615
2847.758636	374425.253722	39.517632
2851.130029	375104.638040	39.522650
2854.034879	375791.036528	39.527668
2856.677952	376479.469009	39.532685
2859.689151	377169.252056	39.537703
2862.796577	377858.779510	39.542720
2865.996619	378543.459988	39.547738
2868.587412	379237.230937	39.552756
2871.961496	379919.728635	39.557773
2875.242745	380612.071797	39.562791
2877.940328	381302.389310	39.567808
2881.469070	381985.180835	39.572826
2884.643153	382672.176320	39.577844
2888.146792	383332.218722	39.582861
2891.554984	383990.945526	39.587879
2895.259396	384643.044080	39.592896
2898.221346	385293.067235	39.597914
2900.952641	385945.702559	39.602932
2904.218423	386577.037177	39.607949
2907.522784	387217.434882	39.612967
2910.323509	387853.994985	39.617984
2913.968720	388480.772239	39.623002
2916.759874	389104.351185	39.628020
2920.194633	389724.038354	39.633037
2923.087120	390351.129914	39.638055
2926.002840	390972.728599	39.643072
2929.079670	391585.262341	39.648090
2931.870684	392200.772271	39.653108
2934.762037	392804.184141	39.658125
2937.770353	393414.413868	39.663143
2940.253597	394034.199962	39.668160
2943.534793	394647.559589	39.673178
2945.877886	395254.996041	39.678196
2948.771112	395869.941648	39.683213
2951.620475	396480.267933	39.688231
2954.534680	397070.566532	39.693248
2957.541018	397642.964047	39.698266
2959.787130	398235.857805	39.703284
2963.042049	398806.040500	39.708301
2966.144886	399385.010012	39.713319
2968.547793	399974.956933	39.718336
2971.793431	400557.660667	39.723354
2974.653797	401158.440996	39.728372
2977.116541	401756.281359	39.733389
2979.754586	402363.311005	39.738407
2982.113491	402974.353449	39.743424
2985.206730	403601.999715	39.748442
2987.808002	404229.102884	39.753460
2990.359144	404865.454263	39.758477
2993.768076	405518.590509	39.763495
2996.210822	406171.916580	39.768512
2998.822422	406835.417586	39.773530
3001.851443	407511.233394	39.778548
3004.558342	408171.699238	39.783565
3007.477007	408858.021815	39.788583
3010.300400	409551.415508	39.793600
3013.306029	410245.474032	39.798618
3016.380298	410960.440710	39.803636
3019.099361	411665.384592	39.808653
3022.540995	412365.381957	39.813671
3025.502641	413080.543273	39.818688
3028.941436	413790.162906	39.823706
3032.010735	414507.603743	39.828724
3035.134468	415213.918605	39.833741
3038.358619	415930.843433	39.838759
3041.335083	416661.980056	39.843776
3044.655489	417380.829821	39.848794
3047.507606	418106.450292	39.853812
3050.564349	418832.931906	39.858829
3054.247841	419553.670592	39.863847
3057.043005	420289.023998	39.868864
3060.380246	421000.684069	39.873882
3063.513033	421731.613280	39.878900
3066.867596	422458.282379	39.883917
3069.821692	423183.424831	39.888935
3072.754751	423925.423509	39.893952
3075.807137	424641.847400	39.898970
3078.917404	425391.757687	39.903988
3081.605032	426116.914315	39.909005
3084.786676	426865.480131	39.914023
3087.659353	427610.628855	39.919040
3090.833236	428357.330014	39.924058
3094.001632	429107.430233	39.929076
3097.019947	429849.199813	39.934093
3100.254294	430611.251881	39.939111
3103.143888	431371.082047	39.944128
3106.334450	432123.421784	39.949146
3109.584684	432872.513767	39.954164
3112.471391	433639.596211	39.959181
3115.808376	434372.296266	39.964199
3118.691084	435107.199423	39.969216
3121.499211	435818.340865	39.974234
3124.357888	436540.038473	39.979252
3127.175324	437261.569830	39.984269
3130.451679	437983.944482	39.989287
3133.302525	438712.796425	39.994304
3136.623672	439446.413534	39.999322
3139.506586	440193.141912	40.004340
3141.920709	440946.250822	40.009357
3145.276625	441702.630391	40.014375
3148.731316	442455.224032	40.019392
3152.264359	443200.288683	40.024410
3155.730194	443952.074243	40.029428
3159.252726	444697.600190	40.034445
3162.727030	445453.893310	40.039463
3165.810986	446199.846386	40.044480
3169.509339	446933.074037	40.049498
3172.689555	447682.356426	40.054516
3175.826696	448428.888227	40.059533
3179.612515	449163.196199	40.064551
3182.881726	449917.504684	40.069568
3186.305585	450657.238144	40.074586
3189.737015	451395.428222	40.079604
3192.831341	452139.670305	40.084621
3196.046290	452879.870941	40.089639
3199.055564	453620.383562	40.094656
3201.951642	454380.423132	40.099674
3204.829051	455154.659321	40.104692
3207.580682	455921.399656	40.109709
3210.576119	456689.643610	40.114727
3213.821777	457471.786282	40.119744
3216.993713	458250.573589	40.124762
3220.277055	459034.273887	40.129780
3223.233144	459821.286368	40.134797
3227.108001	460606.000323	40.139815
3230.264824	461394.340650	40.144832
3233.777505	462180.521880	40.149850
3237.164849	462977.165235	40.154868
3239.631507	463782.928314	40.159885
3243.256607	464572.494183	40.164903
3245.985482	465392.469250	40.169920
3248.873609	466203.586942	40.174938
3252.030285	467031.877003	40.179956
3254.684827	467857.786246	40.184973
3257.700954	468705.755717	40.189991
3260.071959	469571.592854	40.195008
3263.032025	470428.957085	40.200026
3266.466291	471308.610750	40.205044
3269.146930	472196.536959	40.210061
3272.641855	473067.914254	40.215079
3275.660921	473969.310323	40.220096
3278.558395	474867.197097	40.225114
3281.771954	475781.373150	40.230132
3284.726770	476688.926211	40.235149
3288.350887	477587.890474	40.240167
3291.176071	478475.820122	40.245184
3294.733620	479344.589397	40.250202
3298.516782	480221.573542	40.255220
3301.408371	481092.645171	40.260237
3304.793977	481971.028811	40.265255
3308.087489	482845.091789	40.270272
3311.553485	483715.348544	40.275290
3315.251581	484591.289769	40.280308
3318.726830	485463.638694	40.285325
3322.277427	486343.262130	40.290343
3325.732100	487224.678888	40.295360
3329.195005	488096.302676	40.300378
3332.828406	488977.609381	40.305396
3335.909664	489869.974642	40.310413
3339.505206	490748.627660	40.315431
3342.881638	491635.961885	40.320448
3346.097393	492510.702190	40.325466
3349.919171	493400.861394	40.330484
3353.212722	494288.182248	40.335501
3357.464346	495156.723825	40.340519
3360.840024	496050.410378	40.345536
3364.883977	496927.232704	40.350554
3368.333890	497792.492624	40.355572
3371.687173	498669.087041	40.360589
3375.362795	499536.751928	40.365607
3379.024859	500403.013660	40.370624
3382.135223	501268.007841	40.375642
3386.071280	502119.804775	40.380660
3389.956935	502976.111798	40.385677
3394.052010	503814.878740	40.390695
3397.533685	504673.438338	40.395712
3400.912372	505513.751317	40.400730
3404.220816	506358.879957	40.405748
3406.702525	507222.973058	40.410765
3409.783239	508080.922845	40.415783
3412.920142	508957.845414	40.420800
3416.251691	509832.017934	40.425818
3419.614297	510709.218676	40.430836
3422.668871	511600.348412	40.435853
3426.017578	512482.454705	40.440871
3429.421432	513398.105586	40.445888
3432.449692	514299.792175	40.450906
3435.765609	515199.770507	40.455924
3438.447820	516119.623890	40.460941
3442.101287	517045.829809	40.465959
3445.137284	517970.770144	40.470976
3448.604169	518908.753419	40.475994
3452.085731	519840.780463	40.481012
3455.330487	520788.424182	40.486029
3459.325904	521729.742354	40.491047
3463.590953	522654.778059	40.496064
3468.021785	523557.449665	40.501082
3472.463273	524469.194158	40.506100
3476.269099	525373.576603	40.511117
3479.823906	526248.875585	40.516122
3483.023696	527085.524081	40.521127
3486.578816	527856.934443	40.526132
3489.949563	528557.845040	40.531136
3493.004461	529198.796075	40.536141
3496.402638	529766.149230	40.541146
3499.236907	530277.133593	40.546151
3501.590798	530708.500164	40.551156
3503.973203	531112.264643	40.556160
3505.885862	531439.905628	40.561165
3507.971233	531708.200501	40.566170
3509.694865	531915.519090	40.571175
3511.217177	532098.768683	40.576180
3512.995166	532208.570755	40.581184
3514.257572	532302.742013	40.586189
3515.851336	532332.145245	40.591194
3517.017190	532342.115629	40.596199
3517.919230	532303.123972	40.601204
3519.101339	532238.070382	40.606208
3520.330179	532133.300515	40.611213
3520.679810	531999.670234	40.616218
3520.884286	531855.755500	40.621223
3521.785867	531690.964990	40.626228
3522.519773	531494.521974	40.631232
3522.428154	531291.234830	40.636237
3522.854232	531067.148641	40.641242
3523.229047	530836.701301	40.646247
3523.314013	530589.421057	40.651252
3523.548614	530314.879863	40.656256
3523.288791	530064.563749	40.661261
3523.546404	529789.403397	40.666266
3523.337070	529506.985406	40.671271
3523.650162	529208.967260	40.676276
3523.584158	528918.987179	40.681280
3523.503531	528637.847037	40.686285
3523.598824	528339.088898	40.691290
3523.818587	528032.169601	40.696295
3523.546435	527725.069424	40.701300
3522.909499	527403.062545	40.706304
3522.867938	527104.909157	40.711309
3523.009186	526788.527927	40.716314
3522.673930	526495.867532	40.721319
3522.813466	526177.958288	40.726324
3522.225087	525866.424713	40.731328
3521.973129	525568.376871	40.736333
3521.919366	525261.447305	40.741338
3521.461695	524956.091973	40.746343
3521.121509	524671.233051	40.751348
3520.934454	524359.202332	40.756352
3520.586692	524077.265658	40.761357
3520.726735	523775.078845	40.766362
3520.747329	523500.403101	40.771367
3520.214627	523212.667545	40.776372
3520.212936	522914.682515	40.781376
3519.826998	522640.814626	40.786381
3519.838215	522356.566910	40.791386
3519.802789	522073.231512	40.796391
3519.229632	521805.900287	40.801396
3518.751837	521517.114832	40.806400
3518.510213	521250.682583	40.811405
3518.458701	520987.603130	40.816410
3518.149554	520727.087954	40.821415
3517.654972	520468.822427	40.826420
3518.094889	520206.613280	40.831424
3517.688877	519969.206191	40.836429
3517.611817	519719.154410	40.841434
3517.187646	519466.777348	40.846439
3516.997971	519221.842336	40.851444
3516.954468	518972.633392	40.856448
3516.755573	518742.304967	40.861453
3516.454862	518492.168704	40.866458
3516.094068	518267.117767	40.871463
3515.800881	518043.317178	40.876468
3515.589023	517812.977796	40.881472
3515.107004	517593.094457	40.886477
3515.216189	517376.351003	40.891482
3515.007489	517174.521680	40.896487
3514.717683	516966.533453	40.901492
3514.758494	516761.119912	40.906496
3514.679473	516562.246163	40.911501
3514.576601	516354.170136	40.916506
3514.087016	516160.666271	40.921511
3513.705927	515958.141404	40.926516
3514.087742	515757.314060	40.931520
3513.853023	515566.696141	40.936525
3513.489146	515377.411341	40.941530
3513.611256	515195.936986	40.946535
3513.318914	515005.119460	40.951540
3513.294056	514818.353991	40.956544
3513.108667	514654.775058	40.961549
3513.090596	514465.020660	40.966554
3512.480734	514289.215434	40.971559
3512.296116	514114.959595	40.976564
3512.470304	513949.698496	40.981568
3511.830194	513789.925674	40.986573
3511.618370	513621.384246	40.991578
3511.500386	513468.556162	40.996583
3511.314890	513311.488741	41.001588
3510.969645	513174.525059	41.006592
3510.826811	513025.743215	41.011597
3511.107845	512885.339937	41.016602
3511.195702	512738.643459	41.021607
3510.817068	512588.225865	41.026612
3511.043782	512455.617063	41.031616
3510.418702	512317.476693	41.036621
3510.496391	512174.772882	41.041626
3510.499447	512038.301326	41.046631
3510.343832	511912.375013	41.051636
3510.326434	511777.725575	41.056640
3509.926041	511647.283472	41.061645
3509.844300	511510.568145	41.066650
3509.801677	511403.993927	41.071655
3509.538942	511259.970431	41.076660
3509.727909	511150.626431	41.081664
3509.319466	511032.068399	41.086669
3509.345979	510919.662866	41.091674
3509.270157	510802.517653	41.096679
3509.228124	510692.195488	41.101684
3509.251195	510572.959011	41.106688
3508.846062	510462.389224	41.111693
3508.965954	510348.953415	41.116698
3508.550605	510239.597900	41.121703
3507.932635	510151.267839	41.126708
3508.412423	510047.688433	41.131712
3507.993494	509951.687006	41.136717
3507.902973	509850.473041	41.141722
3507.996584	509769.566311	41.146727
3508.251225	509669.460274	41.151732
3508.395645	509587.026959	41.156736
3507.670899	509498.153904	41.161741
3507.813282	509399.784097	41.166746
3507.741864	509311.160940	41.171751
3507.718178	509223.136871	41.176756
3507.779580	509128.572629	41.181760
3507.385501	509041.213264	41.186765
3507.501695	508953.671616	41.191770
3507.439390	508890.239528	41.196775
3507.415125	508790.728949	41.201780
3507.454196	508716.048708	41.206784
3506.868777	508641.820996	41.211789
3507.025914	508558.824205	41.216794
3507.000668	508491.236162	41.221799
3506.696768	508419.745615	41.226804
3507.085073	508336.508839	41.231808
3506.590381	508271.928562	41.236813
3506.595793	508205.447612	41.241818
3506.752117	508131.606396	41.246823
3506.681094	508069.336319	41.251828
3506.529126	508007.331785	41.256832
3506.303337	507945.895237	41.261837
3506.493929	507874.981999	41.266842
3506.527483	507808.343283	41.271847
3506.141711	507755.330134	41.276852
3506.504202	507687.424672	41.281856
3506.232115	507620.681753	41.286861
3506.178521	507548.490279	41.291866
3506.131419	507493.095382	41.296871
3506.287004	507436.858731	41.301876
3506.103937	507377.589042	41.306880
3506.034868	507335.503963	41.311885
3505.930485	507274.956572	41.316890
3505.772705	507214.468005	41.321895
3505.593550	507170.831420	41.326900
3505.770049	507116.513107	41.331904
3505.797587	507069.453585	41.336909
3505.724301	507003.638207	41.341914
3505.461584	506961.380433	41.346919
3505.315656	506908.933945	41.351924
3505.639630	506864.508694	41.356928
3505.499042	506821.725297	41.361933
3505.494264	506766.877960	41.366938
3505.535923	506724.419703	41.371943
3505.546762	506687.127255	41.376948
3505.639318	506641.422451	41.381952
3505.787473	506586.297377	41.386957
3505.725223	506536.417069	41.391962
3505.604356	506488.165051	41.396967
3505.437243	506441.185187	41.401972
3505.466709	506384.863853	41.406976
3505.195084	506345.641942	41.411981
3505.269072	506298.269386	41.416986
3505.298336	506251.763965	41.421991
3505.311447	506211.029354	41.426996
3505.341473	506159.564782	41.432000
3505.268252	506125.674611	41.437005
3505.385327	506075.157431	41.442010
3505.063538	506026.025081	41.447015
3504.837720	505991.905765	41.452020
3504.991656	505949.579667	41.457024
3504.672522	505920.838623	41.462029
3504.928684	505885.630904	41.467034
3504.941772	505851.271148	41.472039
3504.803117	505822.046006	41.477044
3505.067302	505784.509171	41.482048
3504.761864	505756.575306	41.487053
3504.922146	505709.389910	41.492058
3504.886060	505677.567647	41.497063
3504.674572	505637.272001	41.502068
3504.993630	505607.265732	41.507072
3504.896894	505576.667309	41.512077
3505.302036	505536.071558	41.517082
3505.225058	505492.971218	41.522087
3504.956196	505451.469765	41.527092
3504.868286	505407.814320	41.532096
3504.653848	505385.937735	41.537101
3504.600290	505340.961035	41.542106
3504.706254	505308.862634	41.547111
3504.717603	505280.624921	41.552116
3504.724461	505239.534805	41.557120
3504.465244	505214.173498	41.562125
3504.620038	505179.739416	41.567130
3504.576332	505155.659634	41.572135
3504.618461	505132.780723	41.577140
3504.600732	505095.337565	41.582144
3504.399848	505074.166889	41.587149
3504.576681	505038.362760	41.592154
3504.638305	505010.673299	41.597159
3504.615429	504978.493448	41.602164
3504.819353	504935.246123	41.607168
3504.991440	504910.119824	41.612173
3504.607025	504869.647320	41.617178
3504.567132	504853.106471	41.622183
3504.306039	504816.004802	41.627188
3504.134051	504784.657824	41.632192
3504.274311	504763.685869	41.637197
3504.509021	504735.614387	41.642202
3504.398125	504716.959258	41.647207
3504.089828	504678.144216	41.652212
3504.437205	504660.074448	41.657216
3504.048295	504644.803070	41.662221
3504.420713	504613.521550	41.667226
3504.306173	504593.095708	41.672231
3504.470606	504555.470787	41.677236
3504.647594	504533.379449	41.682240
3504.418366	504505.380927	41.687245
3504.571676	504479.852139	41.692250
3504.049412	504456.757920	41.697255
3503.904847	504430.466463	41.702260
3504.248363	504411.587370	41.707264
3504.182632	504390.445106	41.712269
3504.104333	504372.492929	41.717274
3504.425293	504344.356581	41.722279
3504.433599	504318.192608	41.727284
3504.305785	504287.445020	41.732288
3504.105925	504266.627440	41.737293
3504.082469	504243.251675	41.742298
3504.200070	504211.908503	41.747303
3504.084112	504199.022662	41.752308
3504.173406	504163.331790	41.757312
3504.172956	504152.654311	41.762317
3504.246056	504125.012240	41.767322
3504.127660	504105.041891	41.772327
3503.943296	504075.011351	41.777332
3504.324018	504049.850840	41.782336
3504.124975	504037.939528	41.787341
3504.278737	504012.359381	41.792346
3504.060202	503980.208619	41.797351
3504.038131	503974.392653	41.802356
3503.888326	503937.018496	41.807360
3503.951646	503928.000813	41.812365
3503.664563	503900.162285	41.817370
3503.982161	503890.750146	41.822375
3503.859574	503866.984696	41.827380
3504.215397	503844.358157	41.832384
3504.045925	503831.075650	41.837389
3504.154773	503800.947689	41.842394
3504.338786	503791.354184	41.847399
3504.052455	503767.766301	41.852404
3504.414391	503746.656877	41.857408
3504.395991	503727.986074	41.862413
3504.235772	503694.661609	41.867418
3504.031774	503682.649624	41.872423
3503.876096	503651.955932	41.877428
3504.159987	503632.427531	41.882432
3504.020273	503613.370923	41.887437
3504.028593	503590.039872	41.892442
3504.143717	503569.424714	41.897447
3503.956613	503542.278320	41.902452
3504.104160	503518.823954	41.907456
3503.608808	503504.732378	41.912461
3503.952898	503490.052640	41.917466
3503.959552	503461.003009	41.922471
3503.980490	503450.574762	41.927476
3504.111421	503421.859678	41.932480
3503.617105	503416.978504	41.937485
3503.696819	503394.850500	41.942490
3503.651976	503375.981070	41.947495
3503.596738	503367.791568	41.952500
3503.716570	503344.796822	41.957504
3503.607998	503328.012347	41.962509
3503.831567	503322.207947	41.967514
3504.170186	503304.087562	41.972519
3504.053626	503280.067323	41.977524
3504.338267	503252.744701	41.982528
3504.014449	503242.522647	41.987533
3504.144975	503216.641364	41.992538
3504.143874	503195.538053	41.997543
3503.788249	503174.541361	42.002548
3503.966281	503157.205335	42.007552
3504.011261	503142.370151	42.012557
3504.030246	503113.975911	42.017562
3503.943046	503104.121247	42.022567
3503.857750	503085.359117	42.027572
3503.927199	503072.443143	42.032576
3503.918683	503047.039067	42.037581
3503.533105	503028.627993	42.042586
3503.809302	503019.171324	42.047591
3503.802202	503011.277701	42.052596
3504.012847	502989.229710	42.057600
3503.645757	502963.730363	42.062605
3504.111322	502945.387107	42.067610
3503.979484	502930.883348	42.072615
3503.903371	502912.473847	42.077620
3504.241210	502898.705574	42.082624
3503.831081	502874.376916	42.087629
3503.997505	502852.436963	42.092634
3503.896700	502829.273981	42.097639
3503.739659	502809.207046	42.102644
3503.967722	502786.447514	42.107648
3503.695341	502780.721326	42.112653
3504.111767	502776.910654	42.117658
3503.699490	502748.229722	42.122663
3503.691390	502732.339774	42.127668
3503.911033	502704.267428	42.132672
3503.498404	502692.287741	42.137677
3503.741232	502680.761156	42.142682
3503.609973	502660.943028	42.147687
3503.805729	502640.212816	42.152692
3503.857326	502628.665813	42.157696
3503.652263	502613.515433	42.162701
3503.740714	502595.585692	42.167706
3504.012102	502589.925325	42.172711
3503.768366	502567.746186	42.177716
3503.935675	502539.074524	42.182720
3503.536094	502536.809871	42.187725
3503.802854	502514.701808	42.192730
3503.841647	502516.214262	42.197735
3503.563794	502488.979365	42.202740
3503.704435	502471.547355	42.207744
3503.691750	502473.067949	42.212749
3503.931498	502433.553988	42.217754
3503.670567	502426.965492	42.222759
3503.173902	502427.550372	42.227764
3503.839848	502400.115550	42.232768
3503.623223	502399.947617	42.237773
3504.138689	502384.936208	42.242778
3503.704024	502369.568855	42.247783
3503.705235	502360.813241	42.252788
3503.991911	502329.136324	42.257792
3503.532049	502322.781677	42.262797
3504.006468	502298.312411	42.267802
3503.554270	502278.443358	42.272807
3503.613289	502265.477830	42.277812
3503.675522	502257.471688	42.282816
3503.799660	502242.218345	42.287821
3503.938711	502219.269706	42.292826
3503.406961	502205.486506	42.297831
3503.521563	502188.513836	42.302836
3503.699587	502193.698946	42.307840
3503.401955	502189.140619	42.312845
3503.745092	502159.731990	42.317850
3503.303540	502149.730354	42.322855
3503.435553	502155.833756	42.327860
3503.657392	502136.161674	42.332864
3503.688281	502118.898499	42.337869
3503.536010	502103.334443	42.342874
3503.543846	502096.905788	42.347879
3503.679374	502085.952504	42.352884
3503.889256	502068.863435	42.357888
3503.383294	502065.147793	42.362893
3504.036737	502027.490784	42.367898
3503.702810	502028.151178	42.372903
3503.656088	502010.545881	42.377908
3503.800891	501988.709497	42.382912
3503.758546	501982.541792	42.387917
3503.690954	501957.246710	42.392922
3503.770351	501947.010781	42.397927
3503.643312	501933.163400	42.402932
3503.752731	501898.679448	42.407936
3503.495747	501905.451769	42.412941
3503.364510	501888.770729	42.417946
3503.528628	501881.102599	42.422951
3503.365304	501861.997215	42.427956
3503.709060	501855.110478	42.432960
3503.627313	501852.846111	42.437965
3503.566159	501834.281283	42.442970
3503.504931	501816.779311	42.447975
3503.096400	501817.299666	42.452980
3503.670952	501809.769082	42.457984
3503.623998	501793.783207	42.462989
3503.379407	501769.730534	42.467994
3503.661349	501775.658532	42.472999
3503.176504	501758.021008	42.478004
3503.559404	501731.136016	42.483008
3503.497892	501725.477379	42.488013
3503.664509	501714.974467	42.493018
3503.226221	501698.443006	42.498023
3503.335960	501682.179199	42.503028
3503.902431	501671.359996	42.508032
3503.659480	501676.206894	42.513037
3503.663843	501647.458317	42.518042
3503.623793	501636.228829	42.523047
3503.702457	501628.371644	42.528052
3503.178275	501607.247886	42.533056
3503.120264	501597.235927	42.538061
3503.412684	501590.458429	42.543066
3503.285450	501597.514037	42.548071
3503.182880	501585.585815	42.553076
3503.486690	501571.062692	42.558080
3503.230009	501561.841313	42.563085
3503.381385	501558.578409	42.568090
3503.565676	501551.413080	42.573095
3503.534541	501534.918338	42.578100
3503.505799	501511.944690	42.583104
3503.289239	501509.144841	42.588109
3503.698833	501494.756775	42.593114
3503.599697	501489.357077	42.598119
3503.711981	501473.042062	42.603124
3503.940763	501455.848188	42.608128
3503.400707	501438.168458	42.613133
3503.393066	501419.999646	42.618138
3503.684382	501419.650189	42.623143
3503.591138	501408.175896	42.628148
3503.378201	501393.228168	42.633152
3503.483007	501392.047757	42.638157
3503.567875	501385.252373	42.643162
3503.353781	501362.864580	42.648167
3503.542434	501350.991397	42.653172
3503.844053	501337.885617	42.658176
3503.415477	501333.904517	42.663181
3503.559079	501309.131880	42.668186
3503.506007	501293.855116	42.673191
3503.707435	501294.329688	42.678196
3503.434677	501280.302372	42.683200
3503.328453	501265.033984	42.688205
3503.823046	501254.377732	42.693210
3503.677622	501254.755287	42.698215
3503.257078	501236.702165	42.703220
3503.596352	501222.021309	42.708224
3503.324206	501220.698011	42.713229
3503.402553	501201.908015	42.718234
3503.448899	501182.465070	42.723239
3503.577795	501174.903432	42.728244
3503.777344	501167.128165	42.733248
3503.456856	501152.500919	42.738253
3503.641201	501136.376663	42.743258
3503.838435	501136.548216	42.748263
3503.768876	501110.746091	42.753268
3503.774049	501097.889449	42.758272
3503.349520	501096.337154	42.763277
3503.296178	501072.911295	42.768282
3503.702976	501064.344006	42.773287
3503.536693	501064.623632	42.778292
3503.634819	501052.005338	42.783296
3503.364140	501033.877708	42.788301
3503.617946	501014.907936	42.793306
3503.704520	501018.842476	42.798311
3503.583721	500995.224718	42.803316
3503.529894	500977.923207	42.808321
3503.765956	500977.278786	42.813325
3503.717882	500956.332071	42.818330
3503.761184	500932.941367	42.823335
3503.719602	500932.593904	42.828340
3503.842349	500910.253529	42.833345
3503.682472	500906.533552	42.838349
3503.680952	500884.162170	42.843354
3503.435420	500856.464113	42.848359
3503.580729	500848.444204	42.853364
3503.699788	500840.883979	42.858369
3503.392949	500816.991697	42.863373
3503.386719	500801.757721	42.868378
3503.529720	500795.965231	42.873383
3503.460806	500793.597469	42.878388
3503.485850	500762.364033	42.883393
3503.225845	500763.569556	42.888397
3503.387595	500751.244686	42.893402
3503.589230	500744.430600	42.898407
3503.553432	500739.121893	42.903412
3503.624790	500725.849596	42.908417
3503.337353	500719.163420	42.913421
3503.645755	500709.093044	42.918426
3503.544056	500685.066929	42.923431
3503.644923	500680.343991	42.928436
3503.703266	500674.109301	42.933441
3503.354718	500656.347903	42.938445
3503.381331	500639.539507	42.943450
3503.664731	500629.624885	42.948455
3503.512885	500622.613545	42.953460
3503.491690	500596.448718	42.958465
3503.342105	500590.449327	42.963469
3503.519460	500579.842816	42.968474
3503.254279	500590.160053	42.973479
3503.177884	500571.545698	42.978484
3503.748983	500550.854951	42.983489
3503.465349	500546.648297	42.988493
3503.577234	500538.228603	42.993498
3503.205116	500520.673259	42.998503
3503.214581	500517.483212	43.003508
3503.062485	500505.460859	43.008513
3503.414812	500517.603952	43.013517
3503.243041	500501.788490	43.018522
3503.541785	500499.058879	43.023527
3503.680246	500490.634962	43.028532
3503.621320	500477.889236	43.033537
3503.266704	500466.151948	43.038541
3503.383811	500445.380988	43.043546
3503.532974	500434.373915	43.048551
3503.517083	500435.996423	43.053556
3503.653928	500421.144438	43.058561
3503.746102	500401.693397	43.063565
3503.703927	500396.537445	43.068570
3503.601451	500390.176225	43.073575
3503.431665	500363.427142	43.078580
3503.761956	500354.112357	43.083585
3503.407377	500350.878587	43.088589
3503.284949	500328.778702	43.093594
3503.581611	500321.595118	43.098599
3503.353838	500308.521641	43.103604
3503.400798	500297.024469	43.108609
3503.317004	500296.278732	43.113613
3503.555812	500272.451323	43.118618
3503.275021	500265.207138	43.123623
3503.098895	500265.184630	43.128628
3503.379825	500267.570109	43.133633
3503.506259	500248.518421	43.138637
3503.282445	500234.836860	43.143642
3503.370763	500223.130636	43.148647
3503.314685	500218.432383	43.153652
3503.578378	500218.087272	43.158657
3503.164469	500201.398708	43.163661
3503.477560	500193.098899	43.168666
3503.377937	500180.511244	43.173671
3503.300294	500179.005272	43.178676
3503.409926	500157.830221	43.183681
3503.343831	500154.044645	43.188685
3503.762438	500145.019495	43.193690
3503.497709	500143.239386	43.198695
3503.286991	500121.760606	43.203700
3503.597781	500107.437657	43.208705
3503.635356	500112.696195	43.213709
3503.638050	500092.499699	43.218714
3503.410791	500081.501289	43.223719
3503.353734	500070.678439	43.228724
3503.569144	500056.623613	43.233729
3503.468750	500042.669309	43.238733
3503.463471	500025.359198	43.243738
3503.566321	500020.483921	43.248743
3503.418805	500008.814832	43.253748
3503.346153	499984.530092	43.258753
3503.189973	499984.403195	43.263757
3503.408388	499970.550297	43.268762
3503.439210	499977.480328	43.273767
3503.222328	499982.779124	43.278772
3503.809482	499951.708508	43.283777
3503.419251	499945.746937	43.288781
3503.595765	499938.632808	43.293786
3503.284731	499923.952438	43.298791
3503.364821	499906.325011	43.303796
3503.534152	499898.047789	43.308801
3503.431547	499901.708770	43.313805
3503.508869	499886.055861	43.318810
3503.276988	499861.138087	43.323815
3502.993114	499863.005478	43.328820
3503.656067	499849.284694	43.333825
3503.309494	499847.871819	43.338829
3503.287122	499841.244650	43.343834
3503.492206	499823.496149	43.348839
3503.503021	499816.357544	43.353844
3503.344476	499812.839599	43.358849
3503.309359	499821.399896	43.363853
3503.302611	499788.246287	43.368858
3503.415201	499775.270476	43.373863
3503.291409	499777.112572	43.378868
3503.523258	499769.534065	43.383873
3503.318965	499756.709564	43.388877
3503.389637	499755.888769	43.393882
3503.704460	499741.159943	43.398887
3503.552984	499740.880445	43.403892
3503.601174	499716.424385	43.408897
3503.403791	499707.395142	43.413901
3503.485146	499696.094621	43.418906
3503.675970	499692.976998	43.423911
3503.025155	499668.125171	43.428916
3503.352341	499654.001743	43.433921
3503.451055	499654.441978	43.438925
3503.354513	499660.329272	43.443930
3503.388270	499645.695411	43.448935
3503.359120	499616.999469	43.453940
3503.312386	499607.338938	43.458945
3503.453252	499613.340579	43.463949
3503.683656	499607.635127	43.468954
3503.427418	499589.503741	43.473959
3503.305705	499575.198110	43.478964
3503.796165	499574.918382	43.483969
3503.509973	499553.349609	43.488973
3503.860222	499540.741015	43.493978
3503.601638	499521.091361	43.498983
3503.448323	499504.259715	43.503988
3503.621533	499486.617156	43.508993
3503.274379	499487.988395	43.513997
3503.372370	499486.353364	43.519002
3503.545133	499472.557916	43.524007
3503.335032	499454.267243	43.529012
3503.493682	499439.664092	43.534017
3503.382365	499431.481633	43.539021
3503.250352	499432.464536	43.544026
3503.336537	499409.723107	43.549031
3503.429460	499405.304805	43.554036
3503.696784	499399.137877	43.559041
3503.201307	499399.520179	43.564045
3503.521310	499366.162283	43.569050
3503.500712	499365.406516	43.574055
3503.420212	499355.548709	43.579060
3503.469870	499357.717769	43.584065
3503.381142	499329.891315	43.589069
3503.850541	499310.480700	43.594074
3503.371669	499315.821103	43.599079
3503.023070	499307.018037	43.604084
3503.632881	499269.513961	43.609089
3503.200696	499267.203414	43.614093
3503.402243	499264.640840	43.619098
3503.484476	499271.664258	43.624103
3503.878843	499251.809862	43.629108
3503.935861	499231.097609	43.634113
3504.002921	499233.213314	43.639117
3503.635328	499205.633223	43.644122
3503.649302	499200.366811	43.649127
3503.568211	499174.918046	43.654132
3503.659206	499143.620734	43.659137
3503.494616	499144.507561	43.664141
3503.702932	499139.615374	43.669146
3503.533094	499109.776593	43.674151
3503.272323	499106.122805	43.679156
3503.612512	499101.462865	43.684161
3503.367157	499083.329245	43.689165
3503.619886	499072.963029	43.694170
3503.552700	499073.682602	43.699175
3503.244669	499074.743967	43.704180
3503.430143	499039.786877	43.709185
3502.899453	499039.314204	43.714189
3503.272723	499024.474311	43.719194
3503.505019	499019.072096	43.724199
3503.275499	499025.132478	43.729204
3503.592667	499011.921296	43.734209
3503.374833	498993.935097	43.739213
3503.317246	498980.428783	43.744218
3503.082614	498980.921724	43.749223
3503.447570	498976.460319	43.754228
3503.312707	498954.816284	43.759233
3503.142819	498943.757483	43.764237
3503.356266	498932.992429	43.769242
3503.368334	498936.635482	43.774247
3503.243435	498936.351770	43.779252
3503.273308	498922.527864	43.784257
3502.973334	498913.919401	43.789261
3503.261691	498894.587574	43.794266
3503.201437	498908.264982	43.799271
3503.150142	498898.857893	43.804276
3503.409114	498894.565082	43.809281
3503.562260	498901.931783	43.814285
3503.258111	498882.845458	43.819290
3503.282494	498862.441662	43.824295
3503.281206	498855.253966	43.829300
3503.395381	498857.311648	43.834305
3502.845147	498869.649146	43.839309
3503.467370	498845.354269	43.844314
3503.351669	498825.428161	43.849319
3503.016952	498825.076369	43.854324
3503.219745	498810.162003	43.859329
3503.240929	498820.283132	43.864333
3503.306125	498812.224353	43.869338
3502.927378	498790.770531	43.874343
3502.812654	498781.727755	43.879348
3503.356450	498766.253242	43.884353
3503.185291	498773.924361	43.889357
3503.255450	498772.293665	43.894362
3503.680770	498771.163664	43.899367
3503.202324	498762.228990	43.904372
3503.310349	498740.951275	43.909377
3503.400688	498738.861794	43.914381
3503.641407	498729.256597	43.919386
3503.802372	498724.776752	43.924391
3503.040173	498696.549551	43.929396
3503.344964	498679.897828	43.934401
3503.100845	498690.010343	43.939405
3503.406836	498682.318417	43.944410
3503.138088	498689.802512	43.949415
3503.111484	498667.077968	43.954420
3503.563050	498652.174771	43.959425
3503.572554	498646.706417	43.964429
3503.362979	498651.396991	43.969434
3503.195602	498633.048104	43.974439
3503.187534	498613.307234	43.979444
3503.364435	498608.774220	43.984449
3503.352239	498612.724903	43.989453
3503.218252	498608.139785	43.994458
3503.448590	498603.800809	43.999463
3503.257786	498587.024849	44.004468
3503.428411	498570.444853	44.009473
3503.351522	498575.721935	44.014477
3503.156454	498568.261023	44.019482
3503.355904	498563.167594	44.024487
3503.405247	498536.330519	44.029492
3503.599830	498528.149918	44.034497
3503.038543	498530.921863	44.039501
3503.284012	498525.213688	44.044506
3503.306150	498516.452876	44.049511
3503.158696	498499.619359	44.054516
3503.277996	498484.717920	44.059521
3503.286107	498488.969154	44.064525
3503.436201	498480.036233	44.069530
3503.422438	498476.849494	44.074535
3503.433417	498460.902095	44.079540
3503.155604	498449.151338	44.084545
3502.906048	498443.723869	44.089549
3503.427593	498437.870785	44.094554
3503.525625	498436.488764	44.099559
3503.016232	498430.697384	44.104564
3503.239901	498416.488102	44.109569
3503.140062	498409.619537	44.114573
3503.367556	498413.076780	44.119578
3503.262546	498420.383239	44.124583
3503.042379	498421.785107	44.129588
3503.325995	498394.100836	44.134593
3503.062352	498381.487218	44.139597
3503.120452	498375.302388	44.144602
3503.357048	498382.403001	44.149607
3503.358400	498371.215535	44.154612
3503.272857	498370.267503	44.159617
3503.253967	498357.412693	44.164621
3502.979168	498340.143554	44.169626
3503.233301	498334.940173	44.174631
3503.062472	498339.574081	44.179636
3503.401801	498343.823618	44.184641
3502.887797	498345.018825	44.189645
3503.207071	498343.196847	44.194650
3503.123039	498339.008743	44.199655
3503.054980	498311.886155	44.204660
3503.301149	498297.825090	44.209665
3503.007260	498294.581351	44.214669
3503.208378	498285.690891	44.219674
3503.217776	498288.625783	44.224679
3503.075475	498288.395433	44.229684
3503.400308	498287.028174	44.234689
3502.939822	498262.296175	44.239693
3502.724363	498252.762828	44.244698
3503.012487	498248.364011	44.249703
3503.512090	498253.246331	44.254708
3503.214869	498250.610581	44.259713
3503.417678	498247.085833	44.264717
3503.514999	498233.149490	44.269722
3503.464828	498225.209929	44.274727
3502.985212	498209.491719	44.279732
3503.250680	498212.791130	44.284737
3503.339593	498208.423790	44.289741
3503.658063	498199.261626	44.294746
3503.549746	498180.194222	44.299751
3503.243973	498172.446907	44.304756
3503.379726	498168.122777	44.309761
3503.000493	498176.890119	44.314765
3503.207486	498154.026759	44.319770
3503.036044	498131.375054	44.324775
3503.210686	498127.095391	44.329780
3503.354908	498121.352468	44.334785
3502.987673	498126.523706	44.339789
3503.359445	498125.047770	44.344794
3503.226724	498128.055774	44.349799
3503.229893	498110.944970	44.354804
3503.084637	498084.441718	44.359809
3502.864542	498095.563231	44.364813
3503.435321	498084.538698	44.369818
3503.056767	498087.838681	44.374823
3502.705248	498090.121928	44.379828
3503.085353	498086.164141	44.384833
3502.754403	498090.570307	44.389837
3502.782619	498089.401786	44.394842
3502.904276	498084.877372	44.399847
3503.243311	498088.620786	44.404852
3503.158808	498076.586115	44.409857
3503.087761	498061.916905	44.414861
3503.213563	498045.090395	44.419866
3503.298451	498041.432376	44.424871
3502.970860	498048.672921	44.429876
3502.795011	498041.259375	44.434881
3502.915754	498054.605085	44.439885
3502.951146	498048.271862	44.444890
3503.513275	498054.156818	44.449895
3503.395812	498043.241045	44.454900
3503.454146	498011.339444	44.459905
3503.363697	498009.582195	44.464909
3503.664836	498004.168795	44.469914
3503.707987	497991.152047	44.474919
3503.265973	497984.084288	44.479924
3503.371000	497961.641788	44.484929
3503.117638	497963.251431	44.489933
3503.297642	497963.526990	44.494938
3503.181003	497942.486336	44.499943
3503.140182	497928.622216	44.504948
3503.287154	497926.321196	44.509953
3503.051669	497920.182615	44.514957
3503.477814	497912.724487	44.519962
3503.461605	497914.195403	44.524967
3503.199776	497893.127016	44.529972
3503.434585	497884.231034	44.534977
3503.436086	497878.206851	44.539981
3503.307582	497879.898014	44.544986
3503.376867	497856.448559	44.549991
3503.188229	497849.391321	44.554996
3503.284389	497837.530429	44.560001
3503.121958	497843.074366	44.565005
3503.520576	497837.696133	44.570010
3503.566491	497832.221776	44.575015
3503.431277	497804.450929	44.580020
3503.623754	497792.169793	44.585025
3503.359893	497792.566136	44.590029
3503.222964	497783.880734	44.595034
3503.320116	497774.955833	44.600039
3503.156980	497773.007554	44.605044
3503.182759	497757.462184	44.610049
3503.168669	497765.868266	44.615053
3503.379031	497759.456662	44.620058
3503.218756	497723.691057	44.625063
3503.153344	497722.992929	44.630068
3503.473996	497719.398828	44.635073
3503.264042	497721.811617	44.640077
3503.263394	497717.458316	44.645082
3503.697932	497701.088927	44.650087
3503.434103	497686.854876	44.655092
3503.425031	497679.414820	44.660097
3503.405494	497684.024982	44.665101
3503.549989	497656.310944	44.670106
3503.379217	497632.646021	44.675111
3503.135219	497645.745939	44.680116
3503.418429	497634.209718	44.685121
3503.342105	497628.805245	44.690125
3503.363502	497610.071105	44.695130
3503.135015	497597.451379	44.700135
3503.111558	497606.415885	44.705140
3503.442288	497596.745234	44.710145
3503.262813	497594.192024	44.715149
3503.064427	497563.545196	44.720154
3503.543937	497553.851005	44.725159
3503.200230	497557.297449	44.730164
3503.458522	497546.423231	44.735169
3503.193157	497547.832310	44.740173
3503.349316	497530.342401	44.745178
3503.244501	497512.944351	44.750183
3503.125797	497506.129048	44.755188
3503.237323	497505.858566	44.760193
3503.233101	497508.188241	44.765197
3503.124246	497512.761940	44.770202
3503.041696	497488.576636	44.775207
3503.051279	497479.817304	44.780212
3503.052348	497469.692444	44.785217
3502.779888	497472.975768	44.790221
3503.044303	497459.164291	44.795226
3503.180378	497470.837389	44.800231
3503.018020	497462.003977	44.805236
3503.325588	497464.284375	44.810241
3503.226427	497470.020924	44.815245
3503.292883	497458.468228	44.820250
3503.588976	497441.361114	44.825255
3503.213646	497439.142589	44.830260
3503.402009	497430.557475	44.835265
3503.236986	497432.102577	44.840269
3503.089302	497397.549333	44.845274
3503.281486	497386.027342	44.850279
3503.279114	497388.407365	44.855284
3503.440792	497379.674569	44.860289
3503.400018	497389.198796	44.865293
3503.074746	497363.127936	44.870298
3503.344816	497345.822345	44.875303
3503.274740	497330.949886	44.880308
3503.334387	497330.029474	44.885313
3503.378279	497340.299722	44.890317
3503.292341	497324.417261	44.895322
3503.359374	497300.258686	44.900327
3503.293251	497306.344442	44.905332
3503.465265	497296.850594	44.910337
3503.006054	497310.136648	44.915341
3503.221711	497314.405978	44.920346
3502.861051	497288.694981	44.925351
3502.850062	497281.305689	44.930356
3503.303676	497273.437955	44.935361
3502.970213	497275.313446	44.940365
3503.242285	497273.043196	44.945370
3503.247106	497278.155866	44.950375
3502.936669	497286.355885	44.955380
3503.186369	497272.647842	44.960385
3503.330866	497272.827774	44.965389
3503.274609	497250.966762	44.970394
3503.148168	497241.925063	44.975399
3503.243530	497233.810185	44.980404
3503.153235	497227.699043	44.985409
3502.926996	497231.329483	44.990413
3502.998973	497231.065249	44.995418
3503.267725	497230.972415	45.000423
3503.010799	497220.230063	45.005428
3503.347765	497198.256208	45.010433
3503.136144	497198.441804	45.015437
3503.064295	497197.035915	45.020442
3503.110595	497192.877568	45.025447
3503.181313	497196.106698	45.030452
3503.171883	497190.792772	45.035457
3503.095573	497183.464390	45.040461
3503.338892	497160.087774	45.045466
3503.314436	497146.473594	45.050471
3502.794503	497142.708490	45.055476
3503.068873	497137.906573	45.060481
3503.168185	497128.879760	45.065485
3503.147959	497131.363890	45.070490
3503.232172	497136.970309	45.075495
3503.229659	497119.910090	45.080500
3503.184196	497095.009635	45.085505
3502.985997	497111.950266	45.090509
3503.075291	497111.126409	45.095514
3503.363422	497099.740948	45.100519
3502.993003	497106.887386	45.105524
3503.194633	497106.096398	45.110529
3503.160795	497099.723160	45.115533
3503.081790	497072.701690	45.120538
3503.307425	497057.731640	45.125543
3502.999493	497054.844276	45.130548
3503.355071	497050.637012	45.135553
3503.021572	497063.346489	45.140557
3503.240258	497054.148893	45.145562
3503.124423	497065.811445	45.150567
3503.117741	497042.069184	45.155572
3503.477428	497017.053957	45.160577
3503.156652	497030.773969	45.165581
3503.146990	497013.765405	45.170586
3503.226467	497026.865268	45.175591
3503.471543	497016.043447	45.180596
3503.565553	496991.272682	45.185601
3503.198580	496997.001086	45.190605
3503.401463	496987.654075	45.195610
3503.309426	496980.378723	45.200615
3503.286857	496963.270899	45.205620
3503.279399	496941.654931	45.210625
3503.354763	496939.111974	45.215629
3503.408417	496938.394996	45.220634
3503.482493	496935.902868	45.225639
3503.252571	496913.410756	45.230644
3503.458011	496893.533003	45.235649
3503.313175	496899.681963	45.240653
3503.362756	496888.334076	45.245658
3503.233279	496887.696668	45.250663
3503.066590	496861.650644	45.255668
3502.955631	496850.074975	45.260673
3503.147672	496851.766194	45.265677
3503.016961	496848.243266	45.270682
3503.195310	496857.682510	45.275687
3503.003331	496855.688063	45.280692
3503.388239	496851.425491	45.285697
3503.270732	496845.014762	45.290701
3503.145214	496824.429846	45.295706
3503.213753	496805.282408	45.300711
3503.126278	496818.358183	45.305716
3503.156314	496806.507067	45.310721
3503.479024	496810.253330	45.315725
3503.774377	496790.462505	45.320730
3503.348946	496782.682876	45.325735
3503.217339	496778.299421	45.330740
3503.602176	496764.316500	45.335745
3503.002230	496765.120374	45.340749
3503.169824	496735.376202	45.345754
3503.333494	496726.794658	45.350759
3503.265984	496728.324406	45.355764
3503.375858	496725.168442	45.360769
3503.374050	496730.181060	45.365773
3503.222347	496700.132911	45.370778
3503.117319	496692.251973	45.375783
3503.186664	496682.976539	45.380788
3503.554185	496676.843475	45.385793
3503.392607	496681.729479	45.390797
3503.313392	496666.756665	45.395802
3503.314309	496648.936053	45.400807
3503.152065	496636.760829	45.405812
3503.130855	496628.056579	45.410817
3503.174099	496636.454123	45.415821
3503.373962	496634.853361	45.420826
3503.405650	496618.597298	45.425831
3503.108810	496609.683470	45.430836
3503.381794	496594.300536	45.435841
3503.184216	496598.888489	45.440845
3503.190568	496589.319201	45.445850
3503.285478	496588.545061	45.450855
3503.142805	496570.493932	45.455860
3503.095842	496550.402561	45.460865
3502.984203	496550.319223	45.465869
3503.161634	496548.468862	45.470874
3503.481360	496549.127379	45.475879
3503.260430	496561.515650	45.480884
3503.770742	496532.729523	45.485889
3503.650025	496515.333025	45.490893
3503.303654	496502.528657	45.495898
3503.474866	496501.539942	45.500903
3503.038516	496481.459414	45.505908
3503.033557	496470.322396	45.510913
3503.114732	496469.752932	45.515917
3503.342124	496461.313074	45.520922
3503.635092	496462.887121	45.525927
3503.107636	496459.426827	45.530932
3503.310377	496436.663224	45.535937
3503.104879	496439.936149	45.540941
3503.247663	496429.079519	45.545946
3503.464892	496426.210301	45.550951
3503.309801	496431.095347	45.555956
3503.442303	496404.748237	45.560961
3502.969905	496399.659139	45.565965
3503.453861	496393.051926	45.570970
3503.514041	496384.030927	45.575975
3503.111647	496382.879732	45.580980
3503.379315	496353.676023	45.585985
3503.041457	496346.996178	45.590989
3502.878326	496347.579141	45.595994
3503.256675	496340.887345	45.600999
3503.172033	496343.331136	45.606004
3503.323113	496340.826756	45.611009
3502.949249	496343.366890	45.616013
3503.055497	496333.022258	45.621018
3503.064356	496313.630594	45.626023
3503.222881	496300.796905	45.631028
3503.029537	496290.094578	45.636033
3503.179878	496299.487912	45.641037
3503.145276	496298.076065	45.646042
3503.120000	496297.118397	45.651047
3503.335970	496291.717951	45.656052
3503.099406	496271.048702	45.661057
3503.200011	496273.058197	45.666061
3503.186980	496264.960019	45.671066
3503.256994	496261.962159	45.676071
3503.257362	496266.215139	45.681076
3503.260264	496262.822862	45.686081
3503.117772	496248.619126	45.691085
3503.040257	496227.266521	45.696090
3503.406879	496220.272765	45.701095
3503.222299	496217.213883	45.706100
3503.251374	496213.159291	45.711105
3503.220779	496216.455238	45.716109
3503.210225	496201.116788	45.721114
3503.485856	496188.061996	45.726119
3503.349164	496180.287097	45.731124
3503.296163	496176.954268	45.736129
3503.337692	496179.074368	45.741133
3503.482040	496154.750160	45.746138
3503.277708	496139.138516	45.751143
3503.216699	496124.162375	45.756148
3503.519503	496120.975811	45.761153
3503.224240	496134.084923	45.766157
3503.404082	496126.361225	45.771162
3503.358977	496099.332945	45.776167
3503.190247	496093.183189	45.781172
3503.483181	496094.807903	45.786177
3503.312250	496089.772324	45.791181
3503.350602	496054.225166	45.796186
3503.376758	496051.740492	45.801191
3503.140430	496045.297631	45.806196
3503.464632	496037.905480	45.811201
3503.093260	496038.571995	45.816205
3503.095162	496024.649034	45.821210
3503.317951	496010.184859	45.826215
3503.096388	496004.195310	45.831220
3502.970430	495998.545050	45.836225
3502.979279	495998.189519	45.841229
3503.295211	495990.646769	45.846234
3503.355972	495990.890580	45.851239
3503.183981	495987.779040	45.856244
3503.293480	495959.511020	45.861249
3503.347825	495956.161183	45.866253
3503.255324	495952.125750	45.871258
3503.392712	495944.054282	45.876263
3503.208205	495945.956992	45.881268
3503.149763	495922.018930	45.886273
3503.165752	495915.282995	45.891277
3503.245350	495912.030417	45.896282
3503.228110	495905.552877	45.901287
3502.956811	495911.519644	45.906292
3503.506165	495907.585264	45.911297
3503.031583	495895.661427	45.916301
3502.959980	495876.130126	45.921306
3503.262563	495870.108315	45.926311
3503.085268	495862.035920	45.931316
3502.980280	495859.166914	45.936321
3502.907314	495874.671283	45.941325
3503.133612	495862.180978	45.946330
3503.486254	495874.782832	45.951335
3503.017425	495871.262527	45.956340
3503.422534	495845.580328	45.961345
3502.981236	495836.486435	45.966349
3503.166203	495831.141383	45.971354
3503.088016	495821.585053	45.976359
3502.881305	495831.136326	45.981364
3503.281746	495827.427984	45.986369
3503.168930	495830.078815	45.991373
3502.920856	495834.776201	45.996378
3502.996212	495825.904415	46.001383
3502.798357	495794.140660	46.006388
3503.262356	495787.333865	46.011393
3503.055264	495800.631798	46.016397
3502.954679	495790.775215	46.021402
3503.286294	495788.951036	46.026407
3503.000489	495787.730744	46.031412
3503.097078	495790.753518	46.036417
3502.964178	495789.914093	46.041421
3502.934194	495779.286901	46.046426
3503.262306	495780.551678	46.051431
3503.301322	495774.115828	46.056436
3503.209949	495754.739411	46.061441
3502.867086	495754.692615	46.066445
3503.115821	495753.539718	46.071450
3503.145571	495753.535286	46.076455
3502.965060	495757.310680	46.081460
3503.102702	495752.023714	46.086465
3503.051437	495759.373381	46.091469
3502.555670	495758.945717	46.096474
3503.168836	495761.988104	46.101479
3502.622822	495734.025863	46.106484
3502.718050	495733.403526	46.111489
3502.931738	495744.457914	46.116493
3502.996052	495734.879015	46.121498
3503.199651	495722.544091	46.126503
3503.111347	495708.027589	46.131508
3503.002714	495715.436970	46.136513
3503.074700	495715.476492	46.141517
3502.841266	495713.842879	46.146522
3503.092396	495713.499676	46.151527
3502.780240	495717.650294	46.156532
3502.897808	495710.442560	46.161537
3502.973922	495719.442890	46.166541
3502.852507	495718.956054	46.171546
3503.016342	495716.145794	46.176551
3502.946483	495712.359877	46.181556
3503.212382	495708.976556	46.186561
3502.880397	495691.815182	46.191565
3503.076591	495675.481643	46.196570
3502.723929	495669.360816	46.201575
3502.597603	495677.583087	46.206580
3502.994937	495666.533878	46.211585
3502.702509	495670.276349	46.216589
3502.820720	495675.725957	46.221594
3502.701135	495679.441107	46.226599
3502.489111	495683.727794	46.231604
3502.846613	495673.748112	46.236609
3502.756503	495681.306469	46.241613
3502.639429	495677.730527	46.246618
3503.011430	495697.772027	46.251623
3502.378915	495705.770516	46.256628
3502.868217	495714.199242	46.261633
3502.797654	495723.526532	46.266637
3502.954916	495726.235949	46.271642
3503.181487	495711.112753	46.276647
3502.844342	495690.357481	46.281652
3502.983620	495681.323632	46.286657
3502.959010	495685.378177	46.291661
3502.883046	495679.112357	46.296666
3503.287037	495683.656085	46.301671
3502.906742	495689.285744	46.306676
3502.965791	495685.783224	46.311681
3503.066035	495687.387803	46.316685
3503.280102	495680.114175	46.321690
3503.135765	495682.972529	46.326695
3502.903536	495673.491099	46.331700
3503.193940	495653.902340	46.336705
3502.942522	495661.131793	46.341709
3502.669747	495650.947942	46.346714
3503.105212	495637.918123	46.351719
3502.907766	495653.087946	46.356724
3503.299006	495648.419056	46.361729
3502.758329	495651.998249	46.366733
3503.084862	495649.314152	46.371738
3502.939991	495652.982674	46.376743
3502.651104	495650.092072	46.381748
3503.023358	495643.755394	46.386753
3502.819966	495649.863402	46.391757
3503.151559	495650.925118	46.396762
3503.385155	495644.812877	46.401767
3503.069056	495627.041371	46.406772
3503.109176	495620.200253	46.411777
3503.237647	495610.104847	46.416781
3503.092592	495607.394024	46.421786
3503.351380	495613.834031	46.426791
3503.050649	495617.476566	46.431796
3503.132920	495602.882388	46.436801
3503.253259	495588.940373	46.441805
3503.167813	495576.752298	46.446810
3503.085722	495570.892450	46.451815
3503.038124	495571.102765	46.456820
3502.734111	495560.063088	46.461825
3503.000320	495563.818541	46.466829
3502.929584	495568.336075	46.471834
3502.982265	495566.555963	46.476839
3503.028979	495558.599917	46.481844
3503.163872	495564.451963	46.486849
3503.228315	495556.898155	46.491853
3503.010325	495541.693196	46.496858
3503.037191	495531.158135	46.501863
3503.054921	495531.611274	46.506868
3503.141167	495530.332157	46.511873
3503.156111	495530.886997	46.516877
3503.110106	495519.806515	46.521882
3503.309468	495527.521702	46.526887
3503.017940	495514.049772	46.531892
3503.140484	495482.184199	46.536897
3503.317496	495481.599556	46.541901
3502.985561	495484.335703	46.546906
3503.184325	495482.178080	46.551911
3503.040195	495489.795686	46.556916
3503.164943	495481.219707	46.561921
3503.131494	495492.009530	46.566925
3503.375150	495457.340102	46.571930
3503.191505	495451.597528	46.576935
3502.734027	495454.657305	46.581940
3503.444983	495439.507952	46.586945
3503.402998	495437.236486	46.591949
3503.033999	495446.357937	46.596954
3503.112665	495433.738783	46.601959
3502.822628	495413.887098	46.606964
3503.368721	495400.940885	46.611969
3502.736774	495408.078694	46.616973
3503.070082	495402.102502	46.621978
3503.214345	495403.902671	46.626983
3502.928144	495399.796471	46.631988
3503.445379	495396.018952	46.636993
3502.934405	495404.048991	46.641997
3503.053165	495399.473737	46.647002
3503.404865	495374.508145	46.652007
3503.086603	495367.622318	46.657012
3503.284376	495362.528258	46.662017
3503.065916	495367.372975	46.667021
3503.132356	495363.767964	46.672026
3503.198423	495356.922646	46.677031
3502.989790	495368.752846	46.682036
3503.102447	495342.356705	46.687041
3503.159928	495336.474721	46.692045
3503.078227	495319.881004	46.697050
3503.249639	495312.563341	46.702055
3503.381965	495327.377525	46.707060
3503.446468	495320.684333	46.712065
3503.284100	495315.039615	46.717069
3503.036187	495292.548337	46.722074
3503.514228	495284.118947	46.727079
3503.256895	495286.995223	46.732084
3503.408451	495291.376427	46.737089
3503.420966	495276.590491	46.742093
3503.354166	495248.197341	46.747098
3503.250787	495246.695021	46.752103
3503.090956	495240.695462	46.757108
3503.290992	495239.145182	46.762113
3502.918128	495242.394144	46.767117
3503.090091	495233.608062	46.772122
3503.170326	495210.052193	46.777127
3503.016749	495198.380944	46.782132
3503.091618	495195.635298	46.787137
3502.990325	495202.385522	46.792141
3503.082145	495193.612089	46.797146
3503.438806	495201.707601	46.802151
3503.154707	495199.170588	46.807156
3503.218464	495177.440003	46.812161
3503.039535	495167.089153	46.817165
3503.140197	495161.402812	46.822170
3503.491618	495154.613577	46.827175
3503.125959	495157.405733	46.832180
3503.289932	495158.190186	46.837185
3502.789723	495152.446923	46.842189
3503.114578	495139.940546	46.847194
3503.048109	495121.825302	46.852199
3503.316256	495122.643921	46.857204
3503.142676	495112.747878	46.862209
3503.030516	495110.284938	46.867213
3502.915784	495112.986807	46.872218
3503.233203	495118.405095	46.877223
3502.895216	495120.484043	46.882228
3502.798337	495115.790908	46.887233
3502.997721	495121.886059	46.892237
3503.073988	495111.950524	46.897242
3502.985470	495085.079494	46.902247
3502.710967	495070.541284	46.907252
3503.034833	495070.946047	46.912257
3502.718807	495078.742888	46.917261
3502.905648	495080.384465	46.922266
3503.020189	495075.860428	46.927271
3503.088701	495076.406815	46.932276
3503.164617	495067.635835	46.937281
3503.049467	495077.628713	46.942285
3503.208932	495074.464625	46.947290
3503.182409	495073.810878	46.952295
3503.004876	495075.611312	46.957300
3503.469156	495053.159062	46.962305
3503.581700	495050.711228	46.967309
3503.433747	495039.393410	46.972314
3503.432717	495030.229521	46.977319
3503.379244	495023.808026	46.982324
3503.309130	495002.655341	46.987329
3503.072372	494999.401973	46.992333
3503.011312	494989.893131	46.997338
3503.042380	494987.255640	47.002343
3502.893246	494980.899882	47.007348
3502.980466	494975.924453	47.012353
3503.116792	494990.383857	47.017357
3502.905050	494977.759658	47.022362
3503.176513	494951.996063	47.027367
3503.060038	494944.976917	47.032372
3503.032882	494947.816863	47.037377
3503.048026	494948.067899	47.042381
3503.124375	494943.397971	47.047386
3503.009559	494952.884545	47.052391
3502.573555	494957.966282	47.057396
3503.044822	494949.335283	47.062401
3503.079479	494951.405981	47.067405
3503.094822	494950.087398	47.072410
3503.198534	494947.387787	47.077415
3502.824453	494939.801774	47.082420
3503.015394	494913.038215	47.087425
3502.684361	494913.141441	47.092429
3502.906405	494906.777620	47.097434
3502.912291	494906.473168	47.102439
3502.940924	494911.329580	47.107444
3503.123790	494906.946598	47.112449
3502.768184	494908.775195	47.117453
3502.769657	494913.889059	47.122458
3502.959937	494900.492415	47.127463
3502.947259	494908.342645	47.132468
3503.103870	494905.381507	47.137473
3503.093081	494911.003630	47.142477
3503.125126	494905.935639	47.147482
3503.121910	494909.278127	47.152487
3503.000965	494916.639147	47.157492
3503.262819	494897.509777	47.162497
3503.243248	494880.298256	47.167501
3502.980746	494870.719928	47.172506
3503.053072	494869.291069	47.177511
3502.873015	494866.990724	47.182516
3503.222674	494865.720556	47.187521
3503.072714	494869.491303	47.192525
3502.886779	494865.318500	47.197530
3503.275018	494865.510565	47.202535
3503.202645	494851.902240	47.207540
3503.403319	494830.048336	47.212545
3503.325762	494827.782417	47.217549
3503.165769	494827.099125	47.222554
3503.368488	494829.092641	47.227559
3503.356606	494816.082314	47.232564
3502.947789	494793.919647	47.237569
3503.389008	494784.533835	47.242573
3502.976818	494784.599257	47.247578
3503.365955	494779.626685	47.252583
3502.964722	494787.183957	47.257588
3503.394265	494770.762093	47.262593
3503.433206	494758.098119	47.267597
3503.123923	494740.780361	47.272602
3503.264981	494736.657109	47.277607
3503.478953	494741.889331	47.282612
3503.267685	494726.328202	47.287617
3503.150474	494713.131921	47.292621
3502.942683	494693.570246	47.297626
3503.548659	494691.651963	47.302631
3503.344692	494699.583150	47.307636
3503.180343	494695.356264	47.312641
3503.349061	494696.241252	47.317645
3503.162518	494666.043352	47.322650
3503.060461	494655.882592	47.327655
3503.134004	494650.706705	47.332660
3503.191014	494643.001796	47.337665
3503.024397	494646.015731	47.342669
3503.181690	494646.143037	47.347674
3503.388994	494640.237148	47.352679
3502.809802	494629.898627	47.357684
3503.021352	494611.536401	47.362689
3503.063395	494616.998365	47.367693
3502.853186	494611.563522	47.372698
3502.764602	494613.957535	47.377703
3502.821582	494608.834888	47.382708
3503.122440	494612.078734	47.387713
3502.619808	494614.133130	47.392717
3502.917396	494612.820544	47.397722
3503.027412	494618.322396	47.402727
3502.997909	494624.403261	47.407732
3502.918167	494615.302238	47.412737
3502.836428	494615.568592	47.417741
3502.974373	494619.648313	47.422746
3502.991018	494615.089003	47.427751
3503.017281	494611.490195	47.432756
3502.909220	494613.279693	47.437761
3502.851998	494614.757358	47.442765
3503.097514	494610.870730	47.447770
3503.316029	494586.077013	47.452775
3503.187837	494573.034265	47.457780
3503.173982	494569.036727	47.462785
3502.941872	494567.301533	47.467789
3502.995303	494569.774370	47.472794
3503.042871	494561.159527	47.477799
3503.037181	494568.249304	47.482804
3503.311832	494556.358059	47.487809
3502.978515	494557.069243	47.492813
3503.034159	494540.655640	47.497818
3503.344716	494534.277699	47.502823
3502.938072	494537.987820	47.507828
3503.155814	494525.143523	47.512833
3503.016496	494524.203787	47.517837
3503.158325	494521.447456	47.522842
3502.936599	494523.001764	47.527847
3503.135861	494518.818629	47.532852
3503.414490	494493.610221	47.537857
3503.005159	494482.687803	47.542861
3503.104391	494485.507844	47.547866
3503.552009	494473.082875	47.552871
3503.209528	494482.605678	47.557876
3503.238674	494482.246909	47.562881
3503.033189	494472.507460	47.567885
3503.464966	494456.186229	47.572890
3502.847710	494447.727049	47.577895
3502.919659	494453.842567	47.582900
3503.349094	494438.534355	47.587905
3503.040120	494448.963278	47.592909
3503.065008	494450.934310	47.597914
3503.060475	494444.859309	47.602919
3502.936688	494433.385395	47.607924
3503.243101	494412.678845	47.612929
3503.136431	494408.240242	47.617933
3503.118118	494414.167507	47.622938
3503.294278	494409.481666	47.627943
3503.184542	494410.005615	47.632948
3502.983879	494401.834999	47.637953
3503.050328	494413.116003	47.642957
3502.898122	494392.076853	47.647962
3502.986674	494373.986998	47.652967
3502.841143	494370.415296	47.657972
3503.009352	494365.730701	47.662977
3503.027996	494367.652096	47.667981
3503.069868	494369.569819	47.672986
3503.208426	494360.991133	47.677991
3503.201739	494367.372277	47.682996
3503.319416	494353.024673	47.688001
3503.286601	494361.587189	47.693005
3503.054160	494333.725134	47.698010
3503.261500	494323.008949	47.703015
3503.045239	494331.499208	47.708020
3503.014705	494322.339628	47.713025
3503.236119	494329.292334	47.718029
3502.994421	494322.748444	47.723034
3503.184697	494328.693400	47.728039
3503.137245	494316.954180	47.733044
3503.336172	494297.429062	47.738049
3503.161996	494284.950347	47.743053
3503.121415	494287.843151	47.748058
3503.340808	494291.201200	47.753063
3503.382640	494288.106204	47.758068
3503.057052	494262.841081	47.763073
3502.851274	494252.595224	47.768077
3503.041210	494239.400686	47.773082
3503.179066	494231.885361	47.778087
3502.989589	494240.371428	47.783092
3503.170725	494238.925321	47.788097
3503.042531	494245.224446	47.793101
3502.769845	494244.103240	47.798106
3503.127856	494242.224105	47.803111
3503.066677	494245.575876	47.808116
3502.978764	494240.931733	47.813121
3502.921953	494236.080136	47.818125
3503.006018	494217.180694	47.823130
3503.067043	494214.487723	47.828135
3502.792675	494213.062978	47.833140
3502.851914	494200.395409	47.838145
3502.712969	494211.253297	47.843149
3503.110989	494209.621005	47.848154
3503.114976	494202.683800	47.853159
3503.299368	494201.692880	47.858164
3503.098105	494201.724963	47.863169
3503.094794	494202.991604	47.868173
3502.937652	494205.599042	47.873178
3502.963120	494202.253449	47.878183
3502.790709	494180.761544	47.883188
3502.714211	494168.014140	47.888193
3502.905073	494166.414588	47.893197
3502.745410	494167.452775	47.898202
3502.829093	494172.908291	47.903207
3502.912104	494182.870334	47.908212
3503.242738	494174.919443	47.913217
3502.903673	494177.049300	47.918221
3503.041774	494164.723679	47.923226
3503.091064	494161.424947	47.928231
3502.754448	494167.453238	47.933236
3503.205762	494161.154188	47.938241
3503.130773	494157.216857	47.943245
3502.815733	494154.330149	47.948250
3502.868056	494161.967888	47.953255
3502.793446	494167.600327	47.958260
3502.722380	494154.548251	47.963265
3502.945809	494167.323615	47.968269
3502.948408	494161.855000	47.973274
3502.966275	494157.346017	47.978279
3502.744801	494166.444785	47.983284
3503.065794	494167.710803	47.988289
3502.984234	494148.685567	47.993293
3502.960903	494129.246035	47.998298
3502.937544	494128.237315	48.003303
3503.207623	494129.612651	48.008308
3503.173353	494125.162535	48.013313
3502.991733	494131.571412	48.018317
3502.924245	494121.658061	48.023322
3503.085012	494123.810188	48.028327
3502.927936	494132.341818	48.033332
3503.209714	494124.550530	48.038337
3502.915770	494132.496184	48.043341
3503.000032	494124.077872	48.048346
3503.085423	494093.025897	48.053351
3502.685919	494095.114682	48.058356
3503.134097	494084.056485	48.063361
3502.965623	494087.982221	48.068365
3502.767661	494089.988517	48.073370
3502.958638	494080.287461	48.078375
3503.212054	494090.425157	48.083380
3503.318870	494086.509708	48.088385
3503.244639	494087.129322	48.093389
3502.872028	494082.074430	48.098394
3502.862598	494090.076400	48.103399
3502.915061	494087.992375	48.108404
3503.056108	494060.425309	48.113409
3502.973804	494056.792918	48.118413
3502.858454	494052.507504	48.123418
3503.037738	494042.453836	48.128423
3503.118886	494048.264230	48.133428
3503.212079	494047.237083	48.138433
3502.866971	494049.013469	48.143437
3502.962042	494044.188450	48.148442
3502.891755	494046.123935	48.153447
3502.871562	494047.291987	48.158452
3503.076506	494041.791353	48.163457
3503.055458	494049.643274	48.168461
3502.933477	494051.283123	48.173466
3502.866384	494050.281312	48.178471
3503.120881	494039.760046	48.183476
3502.790687	494017.989084	48.188481
3503.031958	494013.242216	48.193485
3502.938968	494005.510114	48.198490
3502.923024	494004.044505	48.203495
3502.620146	494008.092771	48.208500
3503.144674	494003.402398	48.213505
3502.733337	494007.569076	48.218509
3502.917465	494009.514986	48.223514
3502.722537	494001.849629	48.228519
3502.594589	494010.629884	48.233524
3503.033428	494008.332875	48.238529
3502.889916	494007.089968	48.243533
3503.250255	494006.121862	48.248538
3503.054814	494003.671935	48.253543
3502.961427	494006.370593	48.258548
3502.857272	494005.729078	48.263553
3502.855920	494007.197961	48.268557
3503.089243	494006.249932	48.273562
3503.295105	494006.015125	48.278567
3503.079365	493993.745319	48.283572
3503.206089	493971.395735	48.288577
3503.102865	493980.121462	48.293581
3503.255013	493968.704911	48.298586
3503.250623	493963.996860	48.303591
3503.040833	493973.144511	48.308596
3503.183605	493960.716746	48.313601
3503.055897	493945.040476	48.318605
3502.802765	493930.143537	48.323610
3503.166765	493925.529151	48.328615
3502.994833	493928.037697	48.333620
3503.046763	493920.738365	48.338625
3502.989799	493936.089944	48.343629
3503.126144	493924.523959	48.348634
3503.410552	493918.453747	48.353639
3503.028808	493926.919715	48.358644
3502.967906	493901.004640	48.363649
3503.031366	493898.108699	48.368653
3502.867113	493895.957637	48.373658
3502.802737	493892.423649	48.378663
3502.647838	493894.169985	48.383668
3503.083933	493886.202300	48.388673
3503.086481	493894.759444	48.393677
3502.976671	493889.055342	48.398682
3503.305756	493889.155501	48.403687
3503.161277	493890.647016	48.408692
3503.183657	493880.567426	48.413697
3503.165573	493873.785490	48.418701
3503.286391	493854.677326	48.423706
3503.456536	493844.523725	48.428711
3502.969161	493851.993725	48.433716
3503.080419	493846.102763	48.438721
3502.998417	493843.280440	48.443725
3503.047090	493850.108728	48.448730
3503.219566	493844.663802	48.453735
3503.012667	493841.506777	48.458740
3503.130845	493819.107723	48.463745
3503.242660	493818.077620	48.468749
3503.131821	493827.564148	48.473754
3503.068892	493814.864988	48.478759
3502.978528	493812.347792	48.483764
3503.285311	493808.198137	48.488769
3503.152386	493805.181317	48.493773
3502.999751	493788.597423	48.498778
3503.223469	493776.207374	48.503783
3502.924804	493775.140880	48.508788
3503.040123	493763.730023	48.513793
3502.869223	493775.454016	48.518797
3503.399174	493770.155105	48.523802
3503.557875	493758.636118	48.528807
3503.369762	493751.425296	48.533812
3503.471614	493732.522544	48.538817
3503.615614	493732.500053	48.543821
3503.503225	493726.897578	48.548826
3503.705178	493696.130320	48.553831
3503.307731	493682.420602	48.558836
3503.243949	493677.671230	48.563841
3502.946903	493680.807209	48.568845
3503.178759	493670.036134	48.573850
3503.534850	493651.093112	48.578855
3503.597169	493638.829752	48.583860
3503.585162	493632.350579	48.588865
3503.316289	493635.279571	48.593869
3503.246160	493606.226138	48.598874
3503.631293	493585.759392	48.603879
3503.504360	493597.122100	48.608884
3503.727098	493583.364915	48.613889
3503.444723	493570.295188	48.618893
3503.550705	493547.036925	48.623898
3503.422740	493549.184122	48.628903
3503.028897	493530.967142	48.633908
3503.410534	493505.336010	48.638913
3503.225816	493503.441315	48.643917
3503.210908	493507.697352	48.648922
3503.165284	493506.185759	48.653927
3503.073138	493503.516895	48.658932
3503.315453	493497.503834	48.663937
3503.198883	493479.850607	48.668941
3503.190375	493459.192760	48.673946
3503.335639	493452.182305	48.678951
3502.981140	493453.605780	48.683956
3503.225412	493446.529038	48.688961
3503.065254	493453.390481	48.693965
3502.958106	493455.382491	48.698970
3503.050236	493440.430580	48.703975
3502.658283	493427.276799	48.708980
3503.228051	493409.515020	48.713985
3502.940475	493414.472446	48.718989
3502.716286	493420.078121	48.723994
3503.154173	493406.539978	48.728999
3502.986740	493419.985277	48.734004
3503.157099	493407.603414	48.739009
3503.093314	493407.613766	48.744013
3502.970524	493411.431153	48.749018
3503.108467	493406.953642	48.754023
3503.048173	493415.622215	48.759028
3503.114372	493391.458594	48.764033
3502.809803	493373.024801	48.769037
3503.182233	493370.535667	48.774042
3502.894089	493369.062395	48.779047
3502.882207	493370.634266	48.784052
3502.956623	493359.381533	48.789057
3502.997526	493364.033871	48.794061
3502.821754	493367.606460	48.799066
3502.817884	493370.037880	48.804071
3502.894843	493373.317339	48.809076
3503.225657	493370.480328	48.814081
3502.893280	493371.039497	48.819085
3503.235855	493369.719714	48.824090
3503.255946	493362.475829	48.829095
3502.964762	493352.293604	48.834100
3503.145101	493327.959949	48.839105
3502.992978	493326.768993	48.844109
3503.111565	493318.648704	48.849114
3503.124995	493321.178669	48.854119
3502.818416	493322.594580	48.859124
3503.200487	493319.445641	48.864129
3502.973406	493330.064798	48.869133
3502.890301	493320.356029	48.874138
3503.055299	493311.975220	48.879143
3502.959685	493329.460142	48.884148
3503.118209	493302.041086	48.889153
3503.058703	493288.277657	48.894157
3502.736509	493286.404670	48.899162
3503.047804	493283.975823	48.904167
3502.752476	493287.364779	48.909172
3502.925324	493270.577060	48.914177
3503.126054	493277.482799	48.919181
3503.000620	493281.503176	48.924186
3503.098067	493282.905864	48.929191
3502.904970	493279.442740	48.934196
3502.931833	493280.957858	48.939201
3503.091523	493278.401064	48.944205
3502.712812	493287.980847	48.949210
3502.922042	493283.593312	48.954215
3503.035544	493279.372816	48.959220
3503.230131	493264.202022	48.964225
3503.229263	493241.162808	48.969229
3503.044130	493234.508313	48.974234
3503.261357	493225.612844	48.979239
3503.032754	493236.637388	48.984244
3503.263988	493224.904056	48.989249
3503.079431	493238.301557	48.994253
3502.836048	493227.655978	48.999258
3502.995414	493212.591982	49.004263
3502.747088	493204.681549	49.009268
3502.978184	493196.644697	49.014273
3502.773632	493196.272206	49.019277
3503.158994	493194.793737	49.024282
3503.285630	493198.571742	49.029287
3502.841818	493209.782229	49.034292
3502.874157	493197.928408	49.039297
3502.939448	493193.209146	49.044301
3503.159186	493200.162546	49.049306
3503.109549	493202.196129	49.054311
3502.807396	493210.852391	49.059316
3502.784877	493205.083642	49.064321
3502.877383	493204.461650	49.069325
3502.801788	493204.929599	49.074330
3503.089661	493199.314333	49.079335
3503.057768	493202.357845	49.084340
3502.996866	493175.175830	49.089345
3502.939127	493156.196438	49.094349
3502.956064	493158.168866	49.099354
3502.907697	493158.278055	49.104359
3502.814939	493162.242656	49.109364
3503.429227	493159.765901	49.114369
3503.187419	493150.537858	49.119373
3502.993224	493161.101277	49.124378
3503.406301	493153.136915	49.129383
3503.215042	493146.888451	49.134388
3502.940480	493127.690117	49.139393
3503.029269	493133.651504	49.144397
3503.073049	493121.897099	49.149402
3502.982085	493120.291366	49.154407
3502.927256	493128.604752	49.159412
3503.068848	493116.379151	49.164417
3503.008187	493118.313212	49.169421
3503.015113	493127.528301	49.174426
3503.200360	493121.119043	49.179431
3502.835897	493117.986797	49.184436
3502.988115	493124.849625	49.189441
3502.969549	493098.825454	49.194445
3502.961554	493080.243216	49.199450
3503.186137	493078.587604	49.204455
3502.582906	493076.151372	49.209460
3503.056866	493070.405379	49.214465
3502.691253	493078.210904	49.219469
3502.709387	493080.588247	49.224474
3503.300048	493079.988786	49.229479
3502.945685	493082.475644	49.234484
3502.846459	493079.757200	49.239489
3503.018742	493082.211452	49.244493
3502.836033	493078.544100	49.249498
3503.084852	493081.695173	49.254503
3502.860173	493083.604525	49.259508
3503.039799	493080.639457	49.264513
3502.655921	493079.029383	49.269517
3503.179356	493080.111569	49.274522
3503.546868	493073.977307	49.279527
3503.103604	493050.754596	49.284532
3502.852386	493046.591696	49.289537
3502.703933	493040.792164	49.294541
3502.871001	493035.297218	49.299546
3502.962417	493047.739768	49.304551
3502.900784	493041.318868	49.309556
3503.166466	493034.137309	49.314561
3503.233941	493036.253674	49.319565
3502.878134	493041.880267	49.324570
3503.355032	493042.463440	49.329575
3503.169711	493038.948404	49.334580
3503.301449	493010.267220	49.339585
3503.172337	493002.742954	49.344589
3503.138431	492993.937706	49.349594
3503.097689	492994.855886	49.354599
3502.877779	493002.537137	49.359604
3503.153881	492995.100731	49.364609
3503.113308	492997.031629	49.369613
3502.952410	492985.360126	49.374618
3503.081256	492967.718254	49.379623
3502.890960	492968.254976	49.384628
3503.203217	492958.027787	49.389633
3503.078622	492963.314034	49.394637
3502.944227	492962.525350	49.399642
3502.817910	492962.494949	49.404647
3502.775080	492959.919485	49.409652
3502.861131	492957.981935	49.414657
3502.940202	492955.842938	49.419661
3502.370396	492963.630149	49.424666
3502.837231	492956.315491	49.429671
3502.688686	492958.263460	49.434676
3502.919176	492954.632046	49.439681
3503.068855	492967.875639	49.444685
3502.970691	492964.498725	49.449690
3502.941295	492962.174324	49.454695
3502.919191	492968.457116	49.459700
3502.609677	492964.809785	49.464705
3503.071566	492972.282007	49.469709
3503.010759	492963.025260	49.474714
3503.095938	492967.164327	49.479719
3502.553578	492945.729453	49.484724
3502.653973	492949.005283	49.489729
3503.035315	492969.149575	49.494733
3502.953426	492954.427326	49.499738
3503.272714	492929.109073	49.504743
3502.777657	492927.617833	49.509748
3503.048740	492915.422269	49.514753
3503.087472	492917.340641	49.519757
3503.052754	492915.472813	49.524762
3503.181293	492915.098304	49.529767
3502.900746	492925.574232	49.534772
3502.791756	492911.970255	49.539777
3502.820223	492918.346346	49.544781
3502.927538	492919.696865	49.549786
3503.071438	492913.800445	49.554791
3502.695515	492923.278700	49.559796
3502.968416	492921.007787	49.564801
3503.067020	492916.536377	49.569805
3503.007883	492912.039260	49.574810
3502.839832	492895.355721	49.579815
3502.974755	492885.308435	49.584820
3503.260125	492872.705484	49.589825
3502.857873	492884.669162	49.594829
3503.207072	492872.359947	49.599834
3503.018283	492873.149622	49.604839
3503.127171	492881.943616	49.609844
3502.880453	492882.691809	49.614849
3502.959042	492884.451972	49.619853
3502.919398	492878.635190	49.624858
3502.808459	492880.982323	49.629863
3502.980405	492888.702959	49.634868
3503.101624	492868.986058	49.639873
3502.760791	492857.950567	49.644877
3502.666994	492837.811881	49.649882
3503.262296	492849.516630	49.654887
3503.141061	492843.054444	49.659892
3503.141589	492834.699415	49.664897
3503.298287	492828.750308	49.669901
3502.841758	492835.456275	49.674906
3502.856937	492829.630812	49.679911
3502.679746	492835.988801	49.684916
3502.904503	492833.117835	49.689921
3502.933413	492846.431242	49.694925
3502.800281	492837.388414	49.699930
3502.950415	492837.263678	49.704935
3502.724058	492842.667320	49.709940
3502.707219	492841.606861	49.714945
3502.928431	492842.838107	49.719949
3502.512122	492851.056842	49.724954
3502.818015	492846.350098	49.729959
3502.721933	492848.694887	49.734964
3503.060253	492830.361484	49.739969
3503.134268	492851.415323	49.744973
3502.987769	492849.311968	49.749978
3503.224224	492843.299621	49.754983
3503.232431	492837.576538	49.759988
3503.418340	492816.532777	49.764993
3503.165336	492809.686306	49.769997
3503.122827	492809.794570	49.775002
3503.284992	492804.756071	49.780007
3503.077545	492812.891171	49.785012
3503.169801	492790.140499	49.790017
3503.139854	492773.435021	49.795021
3502.982097	492755.736971	49.800026
3503.404009	492753.088020	49.805031
3503.042083	492765.450504	49.810036
3503.181560	492756.111358	49.815041
3503.042423	492766.311834	49.820045
3502.896278	492750.991925	49.825050
3503.123058	492738.398143	49.830055
3503.042405	492729.093778	49.835060
3503.281975	492708.851620	49.840065
3503.079856	492713.036155	49.845069
3502.859896	492712.868641	49.850074
3502.942896	492713.969828	49.855079
3502.755710	492711.062681	49.860084
3503.148957	492719.507978	49.865089
3502.603544	492721.721254	49.870093
3502.881938	492713.980544	49.875098
3503.100349	492717.237762	49.880103
3502.981307	492726.472963	49.885108
3503.213473	492709.523444	49.890113
3502.894415	492711.143924	49.895117
3503.036181	492697.702707	49.900122
3503.405989	492687.770100	49.905127
3503.272955	492676.043359	49.910132
3503.319184	492675.479303	49.915137
3503.424866	492668.525446	49.920141
3503.320398	492656.946092	49.925146
3503.416112	492642.904455	49.930151
3503.026271	492637.649333	49.935156
3503.522776	492628.810709	49.940161
3503.469233	492618.691791	49.945165
3502.955097	492612.190351	49.950170
3502.879984	492594.175254	49.955175
3502.810714	492591.401364	49.960180
3503.201284	492585.516489	49.965185
3503.127987	492582.186212	49.970189
3502.945360	492576.493212	49.975194
3503.171317	492585.116929	49.980199
3502.635228	492586.518533	49.985204
3503.187042	492586.127751	49.990209
3503.453559	492586.237810	49.995213
3503.132876	492578.591736	50.000218
3503.326772	492551.469804	50.005223
3503.288503	492548.640369	50.010228
3503.149591	492542.332787	50.015233
3503.229612	492544.143394	50.020237
3503.277955	492540.692606	50.025242
3503.179200	492516.655190	50.030247
3502.949041	492512.286285	50.035252
3503.121302	492494.485182	50.040257
3503.446271	492490.990661	50.045261
3503.216899	492501.914487	50.050266
3503.290750	492495.320066	50.055271
3503.117771	492495.297039	50.060276
3502.941663	492480.994413	50.065281
3502.725074	492470.647992	50.070285
3503.040883	492463.914038	50.075290
3503.206826	492455.684608	50.080295
3502.730875	492464.875076	50.085300
3502.723331	492460.825442	50.090305
3503.184793	492461.968101	50.095309
3503.102211	492463.196753	50.100314
3503.130978	492453.267289	50.105319
3503.041853	492457.434022	50.110324
3503.340105	492461.134414	50.115329
3503.203514	492465.258009	50.120333
3503.025010	492448.879550	50.125338
3503.122099	492429.267272	50.130343
3502.887177	492431.482143	50.135348
3502.863064	492415.129889	50.140353
3503.364240	492422.039099	50.145357
3503.196013	492428.446449	50.150362
3503.295764	492416.530832	50.155367
3503.085931	492408.310138	50.160372
3502.889187	492382.161203	50.165377
3502.939081	492380.482503	50.170381
3502.786650	492380.709422	50.175386
3503.211904	492374.261970	50.180391
3503.296805	492384.528523	50.185396
3502.980396	492373.893992	50.190401
3503.099325	492380.154692	50.195405
3502.912027	492374.563645	50.200410
3502.841375	492378.322364	50.205415
3502.501304	492374.375911	50.210420
3502.807692	492363.845489	50.215425
3502.921933	492378.158525	50.220429
3502.600594	492374.361028	50.225434
3503.422324	492369.825824	50.230439
3503.090519	492370.790042	50.235444
3503.125365	492363.695349	50.240449
3503.077553	492342.991826	50.245453
3503.123386	492332.249375	50.250458
3503.343946	492326.543207	50.255463
3502.915348	492324.535021	50.260468
3503.031946	492320.060622	50.265473
3502.749948	492326.080877	50.270477
3502.771629	492326.887946	50.275482
3503.119221	492323.035344	50.280487
3502.597394	492331.676099	50.285492
3502.925315	492326.560630	50.290497
3503.134164	492319.894169	50.295501
3503.041346	492337.582145	50.300506
3503.002514	492323.561533	50.305511
3502.838019	492312.902954	50.310516
3502.858599	492286.213141	50.315521
3502.811295	492294.221878	50.320525
3502.986951	492289.029188	50.325530
3503.260744	492283.820985	50.330535
3503.040042	492285.729790	50.335540
3503.255190	492290.759971	50.340545
3503.038482	492294.541793	50.345549
3503.173903	492288.494597	50.350554
3503.444996	492286.426450	50.355559
3503.267512	492276.428213	50.360564
3503.738923	492251.084987	50.365569
3503.416874	492242.021089	50.370573
3502.752763	492247.190261	50.375578
3503.004971	492243.302080	50.380583
3502.809358	492240.801304	50.385588
3502.827175	492221.150696	50.390593
3502.862501	492223.474793	50.395597
3502.693776	492233.173847	50.400602
3502.954941	492237.589097	50.405607
3502.804503	492214.825439	50.410612
3503.096629	492197.055744	50.415617
3503.240305	492193.083429	50.420621
3502.822594	492196.137450	50.425626
3503.162888	492193.197485	50.430631
3502.849735	492197.602244	50.435636
3502.962339	492199.812850	50.440641
3502.970292	492207.154578	50.445645
3502.802585	492204.851944	50.450650
3503.085898	492195.996174	50.455655
3503.041122	492204.612223	50.460660
3502.934922	492199.464059	50.465665
3503.040920	492198.687984	50.470669
3503.287872	492202.447176	50.475674
3503.216305	492173.037236	50.480679
3502.670773	492172.262864	50.485684
3502.959766	492152.265483	50.490689
3503.029602	492163.800528	50.495693
3503.225594	492156.325809	50.500698
3503.267621	492147.862631	50.505703
3502.639546	492163.103400	50.510708
3502.930963	492155.917434	50.515713
3502.809202	492157.861253	50.520717
3502.734799	492160.962295	50.525722
3502.955916	492160.117382	50.530727
3502.665840	492140.971111	50.535732
3502.948683	492107.150043	50.540737
3502.878852	492088.424662	50.545741
3502.638347	492034.430282	50.550746
3502.815734	491981.281211	50.555751
3502.620891	491922.772326	50.560756
3502.629808	491844.329385	50.565761
3502.647459	491761.529640	50.570765
3502.277275	491670.384444	50.575770
3502.325995	491563.018064	50.580775
3502.110212	491447.792803	50.585780
3502.108265	491318.606530	50.590785
3501.694015	491191.206362	50.595789
3501.778275	491043.621433	50.600794
3501.656896	490892.826686	50.605799
3500.920968	490740.861771	50.610804
3501.176101	490586.713211	50.615809
3500.937546	490415.017209	50.620813
3500.816060	490227.297373	50.625818
3500.291454	490035.385164	50.630823
3500.101973	489834.352405	50.635828
3499.851300	489629.984495	50.640833
3499.529497	489417.370141	50.645837
3499.521649	489195.688482	50.650842
3499.627947	488965.578561	50.655847
3498.952819	488732.297165	50.660852
3498.688797	488477.472508	50.665857
3498.298190	488233.756803	50.670861
3497.882703	487977.024611	50.675866
3497.872551	487709.385420	50.680871
3497.359300	487453.066771	50.685876
3497.119181	487167.424045	50.690881
3497.043788	486887.373546	50.695885
3496.578313	486599.883701	50.700890
3496.206741	486293.429566	50.705895
3495.801457	486001.919390	50.710900
3495.391499	485688.015124	50.715905
3495.267633	485364.131540	50.720909
3494.544323	485046.365604	50.725914
3494.407781	484712.847846	50.730919
3493.600157	484382.419330	50.735924
3493.635413	484041.871614	50.740929
3492.980681	483708.975607	50.745933
3492.562256	483362.914754	50.750938
3492.542076	483001.129556	50.755943
3491.707288	482653.247233	50.760948
3491.342340	482273.719522	50.765953
3490.730409	481910.234180	50.770957
3490.092082	481543.959479	50.775962
3489.869417	481175.180080	50.780967
3489.480417	480803.582497	50.785972
3489.272272	480412.491683	50.790977
3488.454462	480036.082907	50.795981
3487.731460	479635.531680	50.800986
3487.390131	479240.536754	50.805991
3486.856304	478854.483105	50.810996
3486.356403	478434.463723	50.816001
3485.751063	478036.648586	50.821005
3485.350779	477627.035767	50.826010
3484.814574	477213.229626	50.831015
3484.174960	476813.165518	50.836020
3483.417911	476382.804659	50.841025
3482.866513	475964.464383	50.846029
3482.516775	475547.705354	50.851034
3482.061495	475124.466763	50.856039
3481.258527	474698.739958	50.861044
3480.609987	474268.823459	50.866049
3480.099531	473840.143167	50.871053
3479.348899	473411.846584	50.876058
3478.883081	472973.864896	50.881063
3478.205700	472545.842607	50.886068
3478.067997	472102.923999	50.891073
3477.805228	471663.462680	50.896077
3476.722678	471209.470935	50.901082
3476.154108	470749.405860	50.906087
3475.746615	470311.510014	50.911092
3475.241527	469847.815324	50.916097
3474.505640	469395.351092	50.921101
3473.457639	468942.317918	50.926106
3473.390092	468490.742290	50.931111
3472.625792	468035.717880	50.936116
3472.101792	467570.606371	50.941121
3471.512747	467108.030005	50.946125
3470.780248	466647.950665	50.951130
3470.121938	466172.130560	50.956135
3469.168647	465716.071546	50.961140
3468.868545	465251.481804	50.966145
3468.069329	464783.512512	50.971149
3467.407013	464312.215058	50.976154
3467.065885	463842.935578	50.981159
3466.045787	463380.092239	50.986164
3465.835992	462903.874396	50.991169
3465.088917	462439.344708	50.996173
3464.352267	461956.494724	51.001178
3463.719067	461482.645284	51.006183
3462.947854	461012.256135	51.011188
3462.414897	460534.211149	51.016193
3461.673548	460050.913617	51.021197
3460.872916	459584.251530	51.026202
3460.323543	459093.395578	51.031207
3459.765890	458630.935466	51.036212
3459.204374	458143.915206	51.041217
3458.758399	457663.409605	51.046221
3457.686509	457182.231578	51.051226
3457.148053	456700.857297	51.056231
3456.551784	456214.560931	51.061236
3455.632177	455741.292128	51.066241
3455.006699	455261.878961	51.071245
3454.364200	454785.451450	51.076250
3453.769195	454296.322803	51.081255
3452.919162	453818.131884	51.086260
3452.361962	453332.578516	51.091265
3451.392812	452853.016108	51.096269
3450.653492	452377.263333	51.101274
3450.285488	451891.192536	51.106279
3449.410353	451412.751884	51.111284
3448.608944	450933.832886	51.116289
3447.968072	450460.409443	51.121293
3447.164765	449982.485744	51.126298
3446.696672	449511.857119	51.131303
3445.586107	449044.517460	51.136308
3445.350670	448559.776125	51.141313
3444.260141	448087.136350	51.146317
3443.565836	447609.501708	51.151322
3443.294016	447135.546000	51.156327
3442.705882	446664.980274	51.161332
3441.788841	446186.793584	51.166337
3440.733593	445718.109838	51.171341
3440.352389	445226.470950	51.176346
3439.684445	444754.255609	51.181351
3438.657316	444294.015327	51.186356
3437.943939	443827.930258	51.191361
3437.151818	443355.706834	51.196365
3436.294778	442889.981513	51.201370
3435.544507	442426.920561	51.206375
3434.916093	441967.740034	51.211380
3434.245899	441501.856822	51.216385
3433.611580	441047.837483	51.221389
3433.023526	440595.325260	51.226394
3432.298068	440123.231175	51.231399
3431.358996	439668.777440	51.236404
3430.865763	439197.441031	51.241409
3430.241023	438740.991286	51.246413
3429.115465	438275.778540	51.251418
3428.648399	437824.693771	51.256423
3427.813477	437370.257334	51.261428
3427.159442	436914.514707	51.266433
3426.409737	436464.033801	51.271437
3425.786551	436003.700163	51.276442
3425.240386	435547.052406	51.281447
3424.231987	435106.844379	51.286452
3423.500776	434653.408493	51.291457
3422.954993	434199.376613	51.296461
3421.926178	433752.445688	51.301466
3421.603604	433293.792330	51.306471
3420.617785	432854.912653	51.311476
3420.259933	432404.424400	51.316481
3419.154538	431963.339400	51.321485
3418.592675	431517.565115	51.326490
3418.151368	431079.508474	51.331495
3417.005349	430634.446094	51.336500
3416.471388	430185.064170	51.341505
3415.825875	429740.313615	51.346509
3415.199629	429297.736251	51.351514
3414.342736	428858.108142	51.356519
3413.516354	428426.111463	51.361524
3413.029192	427983.464549	51.366529
3412.039146	427540.051691	51.371533
3411.470245	427105.656355	51.376538
3410.883204	426660.742929	51.381543
3409.624189	426231.826333	51.386548
3408.973598	425793.587681	51.391553
3408.452035	425371.753322	51.396557
3407.654288	424934.463587	51.401562
3407.263176	424500.277186	51.406567
3406.475342	424074.908923	51.411572
3405.796947	423636.080803	51.416577
3404.801565	423216.395789	51.421581
3404.053262	422791.026572	51.426586
3403.556186	422361.597840	51.431591
3402.521587	421943.728267	51.436596
3401.928624	421509.475325	51.441601
3401.361222	421092.560383	51.446605
3400.587119	420675.925852	51.451610
3400.035842	420253.280414	51.456615
3398.860749	419844.698365	51.461620
3398.517725	419409.306121	51.466625
3397.743262	418998.006474	51.471629
3396.777874	418574.181765	51.476634
3396.328098	418156.137390	51.481639
3395.567243	417747.052825	51.486644
3394.476438	417334.991393	51.491649
3393.987757	416930.628033	51.496653
3393.138228	416520.701453	51.501658
3392.705910	416103.792723	51.506663
3391.693604	415703.635872	51.511668
3391.224795	415296.426205	51.516673
3390.397260	414885.202451	51.521677
3389.580214	414477.731408	51.526682
3389.281097	414065.192908	51.531687
3388.557335	413672.838550	51.536692
3387.985391	413260.738307	51.541697
3387.287328	412852.895388	51.546701
3386.572648	412443.956848	51.551706
3385.918313	412033.529351	51.556711
3385.072136	411640.811418	51.561716
3384.704440	411229.615960	51.566721
3383.633034	410824.776959	51.571725
3382.869472	410421.865783	51.576730
3382.427431	410019.152433	51.581735
3381.500922	409628.504316	51.586740
3380.680941	409229.092734	51.591745
3380.142224	408818.983837	51.596749
3379.705317	408430.682289	51.601754
3378.947058	408017.573197	51.606759
3377.829141	407627.259814	51.611764
3377.225211	407222.577980	51.616769
3377.047408	406828.344577	51.621773
3376.223395	406434.157461	51.626778
3375.487394	406034.868552	51.631783
3374.590982	405623.426321	51.636788
3374.069431	405234.868883	51.641793
3373.655325	404841.206572	51.646797
3372.491248	404437.339218	51.651802
3371.955072	404042.466183	51.656807
3370.934718	403642.505272	51.661812
3370.379853	403257.283409	51.666817
3369.941387	402865.735093	51.671821
3368.967087	402476.452520	51.676826
3368.584212	402084.275739	51.681831
3367.457041	401688.856692	51.686836
3367.010266	401309.923064	51.691841
3366.148114	400926.805788	51.696845
3365.484609	400533.052992	51.701850
3365.166474	400139.698305	51.706855
3364.004270	399757.529639	51.711860
3363.277844	399364.789315	51.716865
3362.673968	398974.439742	51.721869
3361.997494	398593.731183	51.726874
3361.516821	398204.471406	51.731879
3360.758618	397823.817661	51.736884
3360.152857	397434.771911	51.741889
3359.375841	397056.679798	51.746893
3358.763279	396665.922852	51.751898
3358.510721	396271.087726	51.756903
3357.286875	395902.027044	51.761908
3356.538637	395506.015569	51.766913
3355.853137	395124.810948	51.771917
3355.215373	394750.433250	51.776922
3354.392920	394361.157130	51.781927
3353.757152	393994.219767	51.786932
3353.013418	393603.142847	51.791937
3352.325035	393225.400367	51.796941
3351.695718	392852.195344	51.801946
3351.189100	392473.220873	51.806951
3350.395139	392095.914868	51.811956
3349.536878	391715.691000	51.816961
3349.104149	391344.447156	51.821965
3348.348289	390973.072464	51.826970
3347.857431	390592.727352	51.831975
3346.804881	390218.213287	51.836980
3346.207951	389831.138693	51.841985
3345.819104	389464.978708	51.846989
3344.653751	389100.285365	51.851994
3343.937879	388722.193211	51.856999
3343.147770	388348.329772	51.862004
3342.824661	387981.355823	51.867009
3341.919211	387611.011964	51.872013
3341.329989	387246.183112	51.877018
3340.746747	386872.932704	51.882023
3339.836696	386511.808900	51.887028
3339.180736	386128.466999	51.892033
3338.734859	385769.322172	51.897037
3337.877007	385403.525504	51.902042
3337.106910	385022.529572	51.907047
3336.724191	384672.798543	51.912052
3336.138006	384303.107978	51.917057
3335.087469	383928.273842	51.922061
3334.537748	383560.960597	51.927066
3333.864213	383196.715064	51.932071
3333.065097	382831.570305	51.937076
3332.194215	382459.007254	51.942081
3331.592617	382088.661377	51.947085
3330.790846	381729.152245	51.952090
3330.683652	381370.318259	51.957095
3329.709653	381012.864177	51.962100
3329.187417	380650.172396	51.967105
3328.326817	380285.826661	51.972109
3327.698069	379918.363347	51.977114
3327.352617	379546.426255	51.982119
3326.285129	379202.806047	51.987124
3325.632896	378823.789022	51.992129
3324.664504	378469.311679	51.997133
3323.946449	378120.412588	52.002138
3323.702182	377748.696661	52.007143
3322.797009	377404.806044	52.012148
3322.119387	377033.914962	52.017153
3321.520768	376678.472757	52.022157
3320.665020	376324.924853	52.027162
3320.256526	375961.840870	52.032167
3319.183511	375607.405279	52.037172
3318.766422	375244.697705	52.042177
3318.151293	374894.685680	52.047181
3316.837956	374548.367661	52.052186
3316.824970	374180.728178	52.057191
3316.082834	373841.512518	52.062196
3315.457513	373486.402505	52.067201
3314.621082	373122.343254	52.072205
3313.954054	372775.373798	52.077210
3313.372677	372410.352154	52.082215
3312.424335	372058.282650	52.087220
3312.118600	371711.730485	52.092225
3311.400379	371357.227429	52.097229
3310.637649	371009.724173	52.102234
3309.966749	370648.415403	52.107239
3308.998333	370292.950817	52.112244
3308.271830	369943.754049	52.117249
3307.604786	369601.312044	52.122253
3306.955385	369248.917393	52.127258
3306.322527	368901.528985	52.132263
3305.427105	368554.510026	52.137268
3304.977239	368199.174991	52.142273
3304.254560	367864.487400	52.147277
3303.417466	367519.308118	52.152282
3303.122230	367170.834790	52.157287
3302.368615	366833.676374	52.162292
3301.643174	366475.674089	52.167297
3300.734409	366130.902295	52.172301
3300.111623	365790.789393	52.177306
3299.509592	365439.170648	52.182311
3298.474121	365111.737259	52.187316
3298.005236	364762.814495	52.192321
3297.784195	364424.103341	52.197325
3296.785314	364087.141038	52.202330
3296.465564	363740.731104	52.207335
3295.481704	363394.321801	52.212340
3295.066135	363048.812291	52.217345
3294.143250	362708.443760	52.222349
3293.384974	362367.385129	52.227354
3292.876928	362010.763379	52.232359
3291.950187	361676.901602	52.237364
3291.500733	361332.453291	52.242369
3290.769162	360991.151338	52.247373
3290.040057	360651.500443	52.252378
3289.604300	360300.553908	52.257383
3288.786796	359978.418473	52.262388
3288.353716	359626.906730	52.267393
3287.542886	359275.375810	52.272397
3286.784025	358945.412267	52.277402
3286.410710	358583.730478	52.282407
3285.274780	358247.358475	52.287412
3284.544638	357909.978433	52.292417
3283.951025	357572.981604	52.297421
3283.237311	357233.507657	52.302426
3282.889140	356884.380013	52.307431
3281.887277	356555.965532	52.312436
3281.497625	356220.657587	52.317441
3280.642251	355875.012996	52.322445
3279.820609	355548.191991	52.327450
3279.519371	355202.327862	52.332455
3278.658206	354868.332376	52.337460
3277.747275	354524.646778	52.342465
3277.445000	354180.684438	52.347469
3276.254910	353854.394276	52.352474
3276.003082	353519.428296	52.357479
3275.107974	353192.934573	52.362484
3274.383013	352842.133463	52.367489
3273.743474	352512.821072	52.372493
3272.963059	352172.661989	52.377498
3272.596173	351833.300567	52.382503
3272.149934	351515.785365	52.387508
3271.355591	351177.454416	52.392513
3270.805137	350832.465717	52.397517
3269.653763	350505.843079	52.402522
3269.413729	350168.232437	52.407527
3268.523833	349835.201758	52.412532
3267.766605	349496.676139	52.417537
3266.994510	349166.447727	52.422541
3266.280422	348834.070251	52.427546
3265.853401	348495.715228	52.432551
3265.200706	348172.511887	52.437556
3264.234366	347832.940079	52.442561
3263.502775	347498.012151	52.447565
3262.818412	347168.088731	52.452570
3262.490298	346840.601298	52.457575
3261.578592	346517.938349	52.462580
3260.980451	346182.981445	52.467585
3260.154988	345846.709544	52.472589
3259.662785	345529.981363	52.477594
3258.947690	345189.412109	52.482599
3258.363408	344864.168176	52.487604
3257.657970	344532.705605	52.492609
3257.230003	344203.131682	52.497613
3256.402332	343876.266256	52.502618
3255.927216	343545.703405	52.507623
3255.165528	343216.940318	52.512628
3254.615036	342880.709527	52.517633
3253.690585	342557.542875	52.522637
3252.846882	342235.405309	52.527642
3252.068877	341887.750643	52.532647
3251.562443	341567.668833	52.537652
3250.822918	341241.436797	52.542657
3250.255453	340919.579418	52.547661
3249.459777	340587.345507	52.552666
3249.101835	340253.589633	52.557671
3247.875505	339925.467580	52.562676
3247.567508	339588.161986	52.567681
3246.944292	339277.428710	52.572685
3246.042974	338950.319226	52.577690
3245.621803	338625.092157	52.582695
3244.761743	338296.216333	52.587700
3243.970944	337965.520499	52.592705
3243.612803	337640.329336	52.597709
3242.692299	337317.032859	52.602714
3242.400769	336988.340405	52.607719
3241.447747	336668.787878	52.612724
3240.837001	336334.796820	52.617729
3239.830919	336011.532855	52.622733
3239.504107	335701.524549	52.627738
3238.834859	335371.432722	52.632743
3237.945878	335051.047612	52.637748
3237.339929	334727.535906	52.642753
3236.730587	334406.008835	52.647757
3236.035551	334086.555824	52.652762
3235.320699	333758.550796	52.657767
3234.263731	333442.894253	52.662772
3234.018367	333120.208877	52.667777
3233.337825	332815.513028	52.672781
3232.163209	332492.182547	52.677786
3232.011504	332166.753952	52.682791
3231.159892	331861.317272	52.687796
3230.553288	331536.339602	52.692801
3230.087652	331219.153821	52.697805
3229.106687	330901.640824	52.702810
3228.810126	330568.641248	52.707815
3227.811983	330257.569121	52.712820
3227.454289	329937.509269	52.717825
3226.778050	329611.821099	52.722829
3225.762803	329295.070275	52.727834
3225.375611	328976.080181	52.732839
3224.573852	328669.196466	52.737844
3223.907164	328345.512498	52.742849
3223.482338	328036.122479	52.747853
3222.220923	327723.681116	52.752858
3221.802678	327396.109413	52.757863
3221.088001	327089.511035	52.762868
3220.615407	326770.932519	52.767873
3219.850367	326455.275923	52.772877
3219.097836	326144.708061	52.777882
3218.498713	325819.271489	52.782887
3217.956304	325505.307137	52.787892
3217.265592	325190.270215	52.792897
3216.329385	324873.437743	52.797901
3215.527249	324561.547603	52.802906
3214.891219	324244.003200	52.807911
3214.228749	323937.435284	52.812916
3213.598913	323614.948090	52.817921
3212.982508	323303.736667	52.822925
3212.070980	323001.431176	52.827930
3211.702152	322683.176508	52.832935
3211.066711	322379.959421	52.837940
3210.338588	322065.400206	52.842945
3209.702691	321750.239628	52.847949
3208.600604	321440.116621	52.852954
3208.643100	321130.422494	52.857959
3207.543748	320831.983704	52.862964
3206.860770	320509.773199	52.867969
3206.474653	320200.678285	52.872973
3205.924344	319892.473973	52.877978
3205.203349	319569.705905	52.882983
3204.472906	319259.363646	52.887988
3203.579487	318932.903120	52.892993
3203.085264	318632.069643	52.897997
3202.268453	318326.142833	52.903002
3201.797020	318012.292491	52.908007
3200.638439	317711.382888	52.913012
3200.206393	317399.204776	52.918017
3199.788229	317084.018845	52.923021
3198.730092	316780.187641	52.928026
3198.464042	316471.977868	52.933031
3197.558180	316164.453982	52.938036
3197.032591	315849.230071	52.943041
3196.197916	315548.949924	52.948045
3195.655090	315237.724475	52.953050
3195.304890	314919.821679	52.958055
3194.184591	314617.928799	52.963060
3193.813550	314306.953373	52.968065
3193.331201	313986.318500	52.973069
3192.469703	313681.835551	52.978074
3191.740854	313372.390781	52.983079
3190.946536	313062.879058	52.988084
3190.346442	312750.585608	52.993089
3189.531998	312442.501215	52.998093
3188.707824	312139.051897	53.003098
3188.461471	311820.028216	53.008103
3187.516459	311528.335183	53.013108
3186.944030	311217.153316	53.018113
3186.030492	310912.568830	53.023117
3185.568125	310603.455884	53.028122
3184.702616	310301.357624	53.033127
3184.009020	310003.713087	53.038132
3183.602388	309683.511800	53.043137
3182.716458	309379.504492	53.048141
3182.281708	309077.258450	53.053146
3181.771230	308770.261720	53.058151
3180.781701	308474.671782	53.063156
3180.163378	308157.224529	53.068161
3179.614862	307852.243164	53.073165
3178.740065	307545.963016	53.078170
3177.869751	307246.811582	53.083175
3177.470424	306954.154879	53.088180
3176.675424	306647.121386	53.093185
3176.169166	306348.954261	53.098189
3175.185500	306043.298802	53.103194
3174.806804	305735.840720	53.108199
3174.196204	305444.054313	53.113204
3173.342810	305133.868726	53.118209
3172.734521	304835.434131	53.123213
3172.041566	304531.893695	53.128218
3171.529553	304228.578600	53.133223
3170.493821	303934.869833	53.138228
3169.839594	303627.043021	53.143233
3169.486794	303331.595107	53.148237
3168.411766	303039.927916	53.153242
3168.198060	302726.554277	53.158247
3167.484799	302426.017404	53.163252
3166.667582	302120.530495	53.168257
3165.986704	301829.104070	53.173261
3165.283074	301532.332798	53.178266
3164.600125	301225.727750	53.183271
3164.023012	300937.670154	53.188276
3163.520974	300632.588715	53.193281
3162.692697	300330.003051	53.198285
3161.866721	300029.632004	53.203290
3161.365290	299722.384051	53.208295
3160.595867	299422.945161	53.213300
3159.943157	299124.938835	53.218305
3159.365194	298829.364920	53.223309
3158.491746	298540.280264	53.228314
3158.168116	298243.697338	53.233319
3157.111426	297944.021089	53.238324
3156.969165	297637.501894	53.243329
3156.226810	297350.202609	53.248333
3155.211303	297056.426587	53.253338
3154.886194	296751.360917	53.258343
3154.109864	296449.192947	53.263348
3153.516438	296142.971770	53.268353
3152.555975	295847.376936	53.273357
3152.044570	295551.532312	53.278362
3151.566370	295261.004577	53.283367
3150.965293	294963.874419	53.288372
3150.459637	294651.117395	53.293377
3149.719695	294352.021858	53.298381
3148.769783	294060.089903	53.303386
3147.972435	293749.389542	53.308391
3147.009609	293449.869546	53.313396
3146.558521	293146.116987	53.318401
3146.162065	292854.401384	53.323405
3145.149038	292552.596022	53.328410
3144.680648	292257.376517	53.333415
3143.776138	291970.044127	53.338420
3143.351773	291668.806584	53.343425
3142.511257	291374.281510	53.348429
3141.585178	291082.367292	53.353434
3141.017802	290790.523298	53.358439
3140.304603	290501.579864	53.363444
3139.920973	290214.494014	53.368449
3139.344643	289923.592722	53.373453
3138.349214	289627.460150	53.378458
3137.812320	289327.383602	53.383463
3136.928274	289045.163572	53.388468
3136.362026	288761.135689	53.393473
3135.581751	288468.329543	53.398477
3134.692367	288182.849613	53.403482
3134.342254	287892.419718	53.408487
3133.437043	287614.505674	53.413492
3133.119012	287322.873162	53.418497
3132.343608	287035.998838	53.423501
3131.509417	286744.039978	53.428506
3130.882547	286457.116162	53.433511
3129.947439	286184.732130	53.438516
3129.360067	285896.120699	53.443521
3129.031101	285609.709319	53.448525
3128.077455	285320.569611	53.453530
3127.866570	285039.156286	53.458535
3127.114753	284751.996168	53.463540
3126.493891	284461.071307	53.468545
3125.750193	284174.266031	53.473549
3124.853647	283890.922931	53.478554
3124.514651	283588.772349	53.483559
3123.476685	283317.497662	53.488564
3123.092853	283033.996458	53.493569
3122.322912	282745.284271	53.498573
3121.542933	282456.624432	53.503578
3121.100418	282169.158962	53.508583
3120.428624	281885.320627	53.513588
3119.768104	281590.096062	53.518593
3118.940910	281308.548685	53.523597
3118.091671	281029.449607	53.528602
3117.780956	280743.261407	53.533607
3116.951902	280460.134888	53.538612
3116.317284	280168.038109	53.543617
3115.999624	279881.010171	53.548621
3115.052804	279600.041262	53.553626
3114.666687	279311.215683	53.558631
3113.843028	279025.642777	53.563636
3112.947455	278732.771744	53.568641
3112.136491	278436.831025	53.573645
3111.425088	278153.073793	53.578650
3110.943055	277858.583476	53.583655
3110.361829	277580.433992	53.588660
3109.582137	277297.171241	53.593665
3109.027262	277005.646568	53.598669
3108.364665	276728.222890	53.603674
3107.489612	276435.297076	53.608679
3106.900131	276160.841531	53.613684
3106.243982	275864.824780	53.618689
3105.778602	275591.903094	53.623693
3104.917430	275300.095536	53.628698
3104.465047	275015.074257	53.633703
3103.344738	274731.126462	53.638708
3102.920645	274458.223630	53.643713
3102.639206	274178.319876	53.648717
3101.711556	273891.871136	53.653722
3101.153747	273599.811762	53.658727
3100.061134	273325.130072	53.663732
3099.562377	273035.226191	53.668737
3098.993518	272753.610652	53.673741
3098.132567	272472.296048	53.678746
3097.723630	272189.738396	53.683751
3096.691407	271908.272687	53.688756
3096.311148	271629.658174	53.693761
3095.726308	271348.911273	53.698765
3095.073931	271061.196781	53.703770
3094.581344	270793.577066	53.708775
3093.511142	270501.471861	53.713780
3093.081091	270222.508962	53.718785
3092.392254	269940.785574	53.723789
3091.366195	269658.275180	53.728794
3090.791850	269369.886608	53.733799
3090.130001	269088.362956	53.738804
3089.449088	268807.300849	53.743809
3088.915980	268533.524852	53.748813
3088.343304	268267.268364	53.753818
3087.794361	267979.589401	53.758823
3086.990198	267698.929258	53.763828
3086.458412	267420.645615	53.768833
3085.614224	267131.154577	53.773837
3084.747372	266858.323491	53.778842
3084.488117	266572.076499	53.783847
3083.577549	266294.744736	53.788852
3083.172945	266006.992958	53.793857
3082.380404	265730.890760	53.798861
3081.596616	265453.539393	53.803866
3081.036168	265159.980571	53.808871
3080.230351	264883.804565	53.813876
3079.516365	264599.897359	53.818881
3078.841335	264334.041055	53.823885
3077.677763	264060.469007	53.828890
3077.628067	263780.812264	53.833895
3077.022374	263507.203236	53.838900
3076.135325	263232.238189	53.843905
3075.763142	262954.797865	53.848909
3074.880626	262676.139652	53.853914
3074.450158	262395.423610	53.858919
3073.543111	262121.735970	53.863924
3072.879526	261837.338957	53.868929
3072.358297	261552.028279	53.873933
3071.526339	261280.825300	53.878938
3071.071453	261000.496314	53.883943
3070.174441	260723.650246	53.888948
3069.357795	260448.854602	53.893953
3068.819828	260172.512503	53.898957
3068.334519	259892.189360	53.903962
3067.696652	259614.361005	53.908967
3066.329748	259335.756940	53.913972
3066.177622	259069.210849	53.918977
3065.610804	258789.869483	53.923981
3064.703345	258516.923764	53.928986
3064.123463	258240.335550	53.933991
3063.542866	257967.364143	53.938996
3062.866925	257698.635734	53.944001
3062.250763	257422.716311	53.949005
3061.426679	257147.288522	53.954010
3060.942386	256868.012614	53.959015
3059.933202	256605.883297	53.964020
3059.659156	256332.712400	53.969025
3059.106931	256044.585570	53.974029
3058.002587	255774.450039	53.979034
3057.479376	255507.431737	53.984039
3056.705831	255236.964363	53.989044
3056.079005	254960.209161	53.994049
3055.231785	254688.964652	53.999053
3054.519005	254421.824899	54.004058
3054.161485	254145.053610	54.009063
3053.256559	253881.688640	54.014068
3052.863397	253610.297281	54.019073
3052.449998	253334.834766	54.024077
3051.572208	253067.009844	54.029082
3051.027025	252789.760797	54.034087
3050.400829	252514.002055	54.039092
3049.749959	252238.374956	54.044097
3048.683359	251959.197769	54.049101
3047.826018	251695.802784	54.054106
3047.298139	251420.157439	54.059111
3046.546164	251161.967245	54.064116
3045.706464	250886.397542	54.069121
3045.285950	250609.768722	54.074125
3044.451422	250357.322776	54.079130
3043.689934	250095.264732	54.084135
3043.066439	249828.117404	54.089140
3042.485153	249560.174356	54.094145
3041.929547	249305.113713	54.099149
3041.110160	249038.609853	54.104154
3040.946926	248758.683645	54.109159
3040.047997	248498.407063	54.114164
3039.435343	248228.764923	54.119169
3038.779552	247963.230139	54.124173
3037.897486	247698.903069	54.129178
3037.328921	247430.681435	54.134183
3036.601674	247166.712765	54.139188
3035.827271	246904.738374	54.144193
3035.142950	246647.104875	54.149197
3034.479237	246377.830597	54.154202
3034.352742	246105.415861	54.159207
3033.197347	245844.191233	54.164212
3032.825524	245576.603911	54.169217
3031.980425	245311.282063	54.174221
3031.364272	245047.019499	54.179226
3030.605941	244776.540835	54.184231
3029.652005	244517.655073	54.189236
3029.290892	244248.387847	54.194241
3028.763984	243984.062250	54.199245
3027.946236	243725.971325	54.204250
3027.421833	243452.809834	54.209255
3026.642431	243190.308346	54.214260
3026.080186	242927.136371	54.219265
3025.391271	242661.412978	54.224269
3024.638026	242401.608252	54.229274
3024.153342	242136.490240	54.234279
3023.089257	241875.997291	54.239284
3022.690737	241601.571970	54.244289
3022.261460	241336.497790	54.249293
3021.094418	241084.910080	54.254298
3020.613608	240800.058898	54.259303
3020.090891	240545.874732	54.264308
3019.274054	240279.565464	54.269313
3018.914915	240022.529905	54.274317
3018.448345	239754.638466	54.279322
3017.464239	239486.702229	54.284327
3016.763747	239229.773346	54.289332
3016.234857	238958.455856	54.294337
3015.352686	238688.901042	54.299341
3014.413809	238434.558100	54.304346
3014.081282	238167.540339	54.309351
3013.357612	237903.462588	54.314356
3012.918845	237637.685179	54.319361
3012.298777	237378.277685	54.324365
3011.453153	237100.750572	54.329370
3010.908431	236837.054442	54.334375
3010.014033	236573.465228	54.339380
3009.483636	236303.860467	54.344385
3008.698781	236040.993660	54.349389
3007.703538	235783.126247	54.354394
3007.427804	235514.068824	54.359399
3006.593474	235269.367413	54.364404
3005.693391	235009.398796	54.369409
3005.086530	234741.414312	54.374413
3004.281472	234490.267808	54.379418
3004.055610	234223.319283	54.384423
3002.804117	233973.721592	54.389428
3002.317341	233717.001046	54.394433
3001.951308	233464.208842	54.399437
3000.999372	233219.734632	54.404442
3000.523783	232951.759538	54.409447
2999.726564	232690.685644	54.414452
2999.242819	232436.972547	54.419457
2998.490912	232194.378929	54.424461
2997.966765	231929.291617	54.429466
2997.251362	231663.598737	54.434471
2996.287826	231414.038309	54.439476
2995.956442	231156.765126	54.444481
2995.316725	230905.830708	54.449485
2994.740396	230645.975040	54.454490
2994.095737	230376.658878	54.459495
2993.249912	230136.911689	54.464500
2992.692210	229865.266163	54.469505
2991.912795	229607.609836	54.474509
2991.220854	229349.991308	54.479514
2990.761839	229082.864738	54.484519
2989.967580	228835.728780	54.489524
2989.574701	228578.243333	54.494529
2988.763068	228315.783466	54.499533
2987.865699	228055.094807	54.504538
2987.346498	227800.279629	54.509543
2986.626420	227545.573371	54.514548
2985.814981	227275.910913	54.519553
2985.263082	227028.996236	54.524557
2984.499515	226768.875832	54.529562
2984.057195	226508.068823	54.534567
2983.282278	226252.534817	54.539572
2982.530846	226003.719613	54.544577
2982.087304	225742.253145	54.549581
2981.365106	225485.134514	54.554586
2980.800913	225232.269097	54.559591
2979.992098	224979.532284	54.564596
2979.520709	224712.306546	54.569601
2978.768935	224451.427588	54.574605
2978.252333	224200.327303	54.579610
2977.415521	223935.758923	54.584615
2976.451070	223693.540450	54.589620
2975.676953	223428.047221	54.594625
2975.189201	223169.867563	54.599629
2974.260736	222922.388156	54.604634
2973.523627	222667.750378	54.609639
2973.036057	222428.248117	54.614644
2972.648011	222159.770078	54.619649
2971.922620	221920.217900	54.624653
2971.227110	221672.005381	54.629658
2970.697658	221412.666911	54.634663
2969.753735	221161.529289	54.639668
2969.064677	220906.087656	54.644673
2968.609622	220655.854482	54.649677
2967.783500	220405.502658	54.654682
2967.080336	220144.948459	54.659687
2966.324105	219901.690386	54.664692
2966.022709	219651.550763	54.669697
2965.242887	219404.288216	54.674701
2964.515755	219153.568452	54.679706
2964.321460	218895.789436	54.684711
2963.554449	218634.817802	54.689716
2962.787759	218397.981917	54.694721
2962.470030	218129.061472	54.699725
2961.219963	217881.814827	54.704730
2960.473750	217624.076744	54.709735
2959.434504	217373.616150	54.714740
2959.084484	217113.882327	54.719745
2958.471045	216873.984895	54.724749
2957.573674	216630.734564	54.729754
2957.280984	216377.549807	54.734759
2956.507812	216122.838177	54.739764
2956.100764	215884.527994	54.744769
2955.261196	215626.302765	54.749773
2954.433123	215378.437935	54.754778
2953.877860	215124.904676	54.759783
2952.893260	214878.199277	54.764788
2952.705095	214633.901677	54.769793
2951.950178	214388.816399	54.774797
2950.957095	214136.692606	54.779802
2950.466008	213886.921421	54.784807
2949.902323	213644.290614	54.789812
2949.161364	213388.183849	54.794817
2948.420830	213139.014977	54.799821
2947.422310	212894.546458	54.804826
2947.027244	212646.979410	54.809831
2945.993840	212414.368242	54.814836
2945.304623	212159.416275	54.819841
2945.076393	211918.431485	54.824845
2943.741354	211683.490485	54.829850
2943.148307	211441.865161	54.834855
2942.533288	211203.248028	54.839860
2941.973234	210958.971842	54.844865
2941.423596	210720.371591	54.849869
2940.976809	210494.420197	54.854874
2940.611781	210244.922857	54.859879
2939.659824	210008.259946	54.864884
2939.263921	209763.275019	54.869889
2938.230372	209519.639311	54.874893
2937.614812	209278.102062	54.879898
2937.135187	209022.429305	54.884903
2936.407703	208785.799069	54.889908
2935.769980	208545.680908	54.894913
2935.133788	208301.987015	54.899917
2934.402204	208062.127404	54.904922
2934.079682	207815.153002	54.909927
2933.033825	207578.883234	54.914932
2932.533647	207330.411630	54.919937
2931.593735	207081.285209	54.924941
2930.541559	206848.315613	54.929946
2930.312126	206600.389567	54.934951
2930.106232	206361.598833	54.939956
2929.280180	206126.750790	54.944961
2928.585688	205878.074094	54.949965
2927.651511	205632.299934	54.954970
2927.372902	205382.554027	54.959975
2926.245246	205140.350597	54.964980
2925.758765	204893.261383	54.969985
2925.229092	204661.146627	54.974989
2924.727844	204416.250743	54.979994
2924.183211	204170.217359	54.984999
2923.411054	203937.062106	54.990004
2922.636426	203680.529640	54.995009
2922.128579	203424.834191	55.000013
2921.093963	203186.849295	55.005018
2920.721190	202934.074426	55.010023
2919.667402	202696.769091	55.015028
2919.177832	202453.152291	55.020033
2918.396491	202207.470190	55.025037
2917.730493	201966.835875	55.030042
2917.159981	201728.529056	55.035047
2916.605260	201483.335984	55.040052
2916.108818	201240.692667	55.045057
2915.263329	201002.025237	55.050061
2914.484220	200759.314232	55.055066
2913.819647	200503.313179	55.060071
2913.132489	200275.860644	55.065076
2912.021108	200033.192704	55.070081
2911.904451	199791.755417	55.075085
2911.114889	199551.672844	55.080090
2910.631170	199310.613934	55.085095
2909.951510	199071.203245	55.090100
2909.365749	198835.252769	55.095105
2908.576638	198591.993010	55.100109
2907.913308	198347.416452	55.105114
2907.578943	198100.880135	55.110119
2906.580471	197865.750036	55.115124
2905.929443	197618.324418	55.120129
2905.403935	197382.587100	55.125133
2904.171159	197139.773209	55.130138
2903.890673	196901.199736	55.135143
2903.249321	196658.065357	55.140148
2902.456617	196415.274185	55.145153
2901.892777	196176.456190	55.150157
2900.820934	195949.121041	55.155162
2900.688344	195692.753253	55.160167
2900.078122	195462.407743	55.165172
2899.203546	195220.067730	55.170177
2898.670012	194973.208569	55.175181
2898.149808	194740.218061	55.180186
2897.468153	194487.556913	55.185191
2896.447687	194246.784227	55.190196
2896.148998	194008.710434	55.195201
2895.534853	193763.536734	55.200205
2894.745676	193527.476931	55.205210
2894.174319	193279.932113	55.210215
2893.155050	193035.500464	55.215220
2892.456301	192802.483483	55.220225
2891.942140	192558.495850	55.225229
2890.980279	192324.250373	55.230234
2890.380920	192085.737043	55.235239
2889.814203	191853.276149	55.240244
2889.505579	191613.892008	55.245249
2888.701810	191372.259024	55.250253
2887.662226	191129.672135	55.255258
2887.293068	190889.932111	55.260263
2886.493972	190656.381274	55.265268
2885.743044	190419.235957	55.270273
2885.335098	190178.360468	55.275277
2884.480116	189946.883043	55.280282
2884.088008	189699.047853	55.285287
2882.728313	189475.451868	55.290292
2882.419801	189237.198986	55.295297
2881.952168	188990.282731	55.300301
2881.340633	188760.210144	55.305306
2880.789052	188520.663414	55.310311
2879.701386	188289.866957	55.315316
2878.890172	188053.951500	55.320321
2878.468133	187822.492113	55.325325
2878.010242	187581.026898	55.330330
2877.074542	187336.343463	55.335335
2876.490587	187115.612786	55.340340
2875.741475	186870.151612	55.345345
2875.513739	186639.468786	55.350349
2874.328123	186402.017901	55.355354
2873.747765	186161.355455	55.360359
2872.840927	185930.389301	55.365364
2872.332021	185703.826714	55.370369
2872.016230	185476.662171	55.375373
2871.053715	185235.479856	55.380378
2870.827433	185002.616792	55.385383
2869.901307	184779.470676	55.390388
2868.740262	184537.674668	55.395393
2868.660057	184297.909625	55.400397
2867.557976	184073.370011	55.405402
2867.138304	183830.837006	55.410407
2866.464047	183606.384618	55.415412
2865.951067	183383.523423	55.420417
2865.347576	183145.195829	55.425421
2864.558979	182908.603462	55.430426
2863.724085	182674.691126	55.435431
2863.056961	182449.556457	55.440436
2862.274715	182209.672025	55.445441
2862.003639	181981.029608	55.450445
2860.950324	181755.221804	55.455450
2860.643096	181517.670149	55.460455
2860.020840	181291.427552	55.465460
2859.269234	181060.016553	55.470465
2858.616157	180823.731887	55.475469
2857.875499	180596.557580	55.480474
2857.019652	180356.008002	55.485479
2856.132707	180133.578586	55.490484
2855.745801	179893.186275	55.495489
2855.167743	179661.818825	55.500493
2854.591651	179445.131457	55.505498
2853.656400	179203.863085	55.510503
2852.942522	178975.891674	55.515508
2852.341654	178751.363428	55.520513
2851.960370	178525.809428	55.525517
2851.207470	178297.707893	55.530522
2850.920793	178063.122952	55.535527
2849.767882	177833.268324	55.540532
2849.296754	177600.724874	55.545537
2848.851678	177361.500778	55.550541
2847.936896	177132.171917	55.555546
2847.428808	176902.678144	55.560551
2846.915332	176672.525071	55.565556
2846.241429	176435.759175	55.570561
2845.444382	176200.209736	55.575565
2844.885659	175961.075231	55.580570
2844.339220	175724.140565	55.585575
2843.339511	175498.077511	55.590580
2842.521416	175253.468100	55.595585
2842.286491	175018.701244	55.600589
2841.341564	174797.301194	55.605594
2840.746251	174560.050267	55.610599
2840.351878	174331.074194	55.615604
2839.422435	174091.284290	55.620609
2838.881404	173863.224371	55.625613
2838.244468	173624.751775	55.630618
2837.764879	173379.896464	55.635623
2836.342945	173158.771641	55.640628
2835.942105	172926.383282	55.645633
2835.747388	172689.359639	55.650637
2834.260229	172464.331764	55.655642
2833.787645	172218.350493	55.660647
2833.439164	171994.912723	55.665652
2832.725205	171757.188317	55.670657
2831.825886	171531.118761	55.675661
2831.065379	171305.308297	55.680666
2830.685464	171069.620808	55.685671
2829.886394	170857.490490	55.690676
2829.155177	170625.778306	55.695681
2828.710674	170388.985970	55.700685
2827.817517	170164.347613	55.705690
2827.250563	169927.119631	55.710695
2826.647760	169704.498128	55.715700
2825.917284	169476.111814	55.720705
2825.378818	169254.996028	55.725709
2824.373591	169018.644163	55.730714
2823.690437	168783.514421	55.735719
2823.010743	168572.776462	55.740724
2822.539729	168350.981160	55.745729
2822.386316	168115.733433	55.750733
2821.180339	167896.129977	55.755738
2820.923695	167664.741782	55.760743
2819.926631	167436.257160	55.765748
2819.425185	167205.749801	55.770753
2818.776296	166980.531743	55.775757
2817.851364	166756.884689	55.780762
2817.696972	166525.029430	55.785767
2816.923889	166293.845805	55.790772
2816.115976	166058.078631	55.795777
2815.623267	165837.687433	55.800781
2814.652712	165606.933490	55.805786
2814.123982	165373.682274	55.810791
2813.435734	165143.852866	55.815796
2813.016142	164909.773450	55.820801
2812.214752	164687.492418	55.825805
2811.263738	164466.889423	55.830810
2810.918454	164233.069516	55.835815
2810.023600	164002.402517	55.840820
2809.472398	163767.308489	55.845825
2809.085131	163547.944062	55.850829
2807.964160	163310.069568	55.855834
2807.439948	163080.112538	55.860839
2806.735262	162854.457744	55.865844
2806.421817	162613.395572	55.870849
2805.343428	162392.354729	55.875853
2804.437818	162171.122570	55.880858
2803.900568	161942.039365	55.885863
2803.193899	161723.206910	55.890868
2802.209914	161495.951885	55.895873
2801.926290	161274.652107	55.900877
2800.939112	161056.033406	55.905882
2800.550575	160822.890593	55.910887
2799.961695	160615.972117	55.915892
2799.163884	160382.744416	55.920897
2798.694122	160184.442401	55.925901
2798.304379	159894.525251	55.930906
2797.708385	159647.984387	55.935911
2797.103025	159421.941197	55.940916
2796.666759	159186.769711	55.945921
2795.920826	158960.065194	55.950925
2794.947668	158737.936826	55.955930
2794.440397	158508.260598	55.960935
2793.648139	158272.986307	55.965940
2792.988586	158042.116766	55.970945
2792.407952	157823.402704	55.975949
2791.561393	157594.167589	55.980954
2790.896163	157361.205785	55.985959
2790.604366	157134.072448	55.990964
2789.770034	156897.046987	55.995969
2789.397369	156667.030993	56.000973
2788.387632	156433.608751	56.005978
2787.967350	156195.708893	56.010983
2786.923274	155975.261972	56.015988
2786.049380	155738.352416	56.020993
2785.614650	155508.493805	56.025997
2784.533935	155286.874859	56.031002
2784.443135	155060.257233	56.036007
2783.508470	154840.461301	56.041012
2782.838747	154607.455242	56.046017
2782.321614	154386.515585	56.051021
2781.386773	154160.711358	56.056026
2781.109891	153924.266423	56.061031
2780.081391	153704.263891	56.066036
2779.665520	153469.191581	56.071041
2779.058687	153244.917738	56.076045
2778.080931	153018.009336	56.081050
2777.664275	152793.593975	56.086055
2777.184524	152578.443846	56.091060
2776.607976	152334.774028	56.096065
2775.591953	152111.055602	56.101069
2774.827720	151895.293961	56.106074
2774.474617	151659.677825	56.111079
2773.663489	151431.800488	56.116084
2773.069532	151212.647959	56.121089
2772.330894	150978.928061	56.126093
2771.730447	150763.948599	56.131098
2771.216618	150531.162257	56.136103
2770.367179	150305.917093	56.141108
2769.676046	150070.823396	56.146113
2769.073877	149840.203967	56.151117
2768.454462	149628.158267	56.156122
2768.011231	149387.361527	56.161127
2766.954923	149163.682184	56.166132
2765.986763	148937.524719	56.171137
2765.638962	148712.833851	56.176141
2764.657932	148491.701857	56.181146
2764.498859	148270.288656	56.186151
2763.969563	148045.872643	56.191156
2763.168724	147813.240135	56.196161
2762.763110	147581.016942	56.201165
2761.711835	147364.911241	56.206170
2761.277479	147122.058353	56.211175
2760.666780	146901.920754	56.216180
2759.735638	146678.988640	56.221185
2759.390414	146437.829817	56.226189
2758.478888	146214.808879	56.231194
2757.541131	145978.614831	56.236199
2756.974836	145762.430447	56.241204
2756.213747	145526.986995	56.246209
2755.546964	145311.850988	56.251213
2754.693446	145090.455442	56.256218
2754.288181	144850.830483	56.261223
2753.433653	144636.021116	56.266228
2752.871451	144413.669202	56.271233
2752.587094	144198.149818	56.276237
2751.744675	143979.505247	56.281242
2751.125291	143756.862068	56.286247
2750.422033	143533.407768	56.291252
2749.532739	143294.455945	56.296257
2748.659284	143075.619311	56.301261
2747.801683	142868.053125	56.306266
2747.496105	142643.131715	56.311271
2746.990423	142430.328154	56.316276
2746.283199	142213.555256	56.321281
2745.815849	141982.374279	56.326285
2744.948962	141766.862395	56.331290
2744.432016	141535.235187	56.336295
2743.625050	141320.301458	56.341300
2743.124348	141092.423502	56.346305
2742.258326	140880.043545	56.351309
2741.736738	140654.840532	56.356314
2741.041101	140426.236045	56.361319
2740.312403	140209.302846	56.366324
2739.471231	139980.724765	56.371329
2739.239371	139766.371611	56.376333
2738.431749	139544.932311	56.381338
2737.943594	139320.763085	56.386343
2737.162702	139106.717586	56.391348
2736.392922	138887.182988	56.396353
2735.688938	138655.531135	56.401357
2735.128888	138437.631030	56.406362
2734.300591	138207.247473	56.411367
2733.779211	137995.023779	56.416372
2732.804129	137772.874458	56.421377
2732.250765	137555.576868	56.426381
2731.462151	137336.285327	56.431386
2731.097685	137117.525341	56.436391
2730.234239	136912.097176	56.441396
2729.626110	136691.498616	56.446401
2729.183857	136458.323219	56.451405
2728.117509	136243.492282	56.456410
2727.863171	136018.523148	56.461415
2727.346888	135806.187265	56.466420
2726.092458	135587.223881	56.471425
2725.863886	135362.281095	56.476429
2725.173405	135146.814238	56.481434
2724.681098	134920.849481	56.486439
2723.793390	134711.946929	56.491444
2722.956645	134485.049210	56.496449
2722.817257	134262.311225	56.501453
2721.470555	134042.764268	56.506458
2721.326250	133816.143178	56.511463
2720.568497	133601.867138	56.516468
2719.949346	133379.161128	56.521473
2719.039990	133162.803610	56.526477
2718.374815	132938.037671	56.531482
2717.928207	132719.730107	56.536487
2717.254116	132511.635290	56.541492
2716.512044	132284.981199	56.546497
2715.860982	132066.571263	56.551501
2714.958367	131848.240954	56.556506
2714.705833	131625.642889	56.561511
2713.636343	131415.154398	56.566516
2713.090519	131184.705320	56.571521
2712.358735	130969.593778	56.576525
2711.775114	130754.854160	56.581530
2711.434695	130532.532617	56.586535
2710.567394	130322.477471	56.591540
2709.803927	130101.229797	56.596545
2709.322944	129879.011874	56.601549
2708.292274	129661.429988	56.606554
2707.811054	129451.548794	56.611559
2706.944288	129222.462124	56.616564
2706.497764	129013.556722	56.621569
2705.864787	128797.442693	56.626573
2704.997758	128588.302257	56.631578
2704.877484	128366.267792	56.636583
2703.787462	128143.575873	56.641588
2703.113194	127922.661494	56.646593
2702.497537	127703.009662	56.651597
2701.820223	127483.572549	56.656602
2701.308830	127259.627584	56.661607
2700.518763	127042.256625	56.666612
2700.061632	126830.575195	56.671617
2699.534191	126613.953422	56.676621
2698.625479	126394.993428	56.681626
2697.961509	126173.011885	56.686631
2697.297179	125956.620180	56.691636
2696.757909	125737.162400	56.696641
2696.296434	125511.306072	56.701645
2695.317885	125294.918583	56.706650
2694.773391	125068.278993	56.711655
2694.013024	124855.733786	56.716660
2693.319250	124632.982106	56.721665
2693.001637	124417.779505	56.726669
2692.116178	124191.379035	56.731674
2691.307444	123961.463367	56.736679
2690.581481	123753.505699	56.741684
2689.966550	123537.277794	56.746689
2689.229496	123318.429634	56.751693
2688.343928	123102.946524	56.756698
2687.810643	122888.349017	56.761703
2687.337045	122669.591380	56.766708
2686.986589	122446.879536	56.771713
2686.165339	122237.247117	56.776717
2685.339105	122023.210883	56.781722
2684.723110	121800.457609	56.786727
2683.970778	121586.552847	56.791732
2682.970118	121367.940169	56.796737
2682.695496	121141.811491	56.801741
2681.616197	120937.207692	56.806746
2681.136049	120728.421944	56.811751
2680.293663	120516.876414	56.816756
2680.112243	120296.263556	56.821761
2679.383426	120076.374133	56.826765
2678.319793	119868.233614	56.831770
2678.062079	119651.142640	56.836775
2677.087041	119438.496753	56.841780
2676.207840	119222.333093	56.846785
2675.877297	119007.925301	56.851789
2675.310212	118803.714005	56.856794
2674.704176	118588.001120	56.861799
2674.011017	118378.366339	56.866804
2673.498612	118157.436669	56.871809
2672.545905	117949.427150	56.876813
2671.875124	117732.982532	56.881818
2671.431052	117513.685297	56.886823
2670.720922	117302.722459	56.891828
2670.319951	117084.240911	56.896833
2669.560594	116860.987309	56.901837
2668.813675	116647.229917	56.906842
2668.347359	116438.990430	56.911847
2667.228075	116223.403939	56.916852
2666.656590	116002.006922	56.921857
2666.026282	115791.037462	56.926861
2665.439755	115574.813421	56.931866
2665.247093	115359.328576	56.936871
2664.403539	115136.522236	56.941876
2663.081315	114926.272546	56.946881
2662.567642	114702.313294	56.951885
2662.077648	114496.625923	56.956890
2661.689215	114271.165369	56.961895
2660.852378	114068.443428	56.966900
2659.925946	113847.863961	56.971905
2659.467006	113635.438068	56.976909
2658.633240	113427.459102	56.981914
2658.157715	113195.471863	56.986919
2657.722051	112991.863545	56.991924
2656.876296	112768.703902	56.996929
2656.166559	112554.778234	57.001933
2655.595222	112343.326707	57.006938
2655.049948	112121.978432	57.011943
2654.170772	111924.306987	57.016948
2653.126430	111702.413193	57.021953
2652.609211	111479.498567	57.026957
2651.554492	111270.829952	57.031962
2650.958160	111062.033335	57.036967
2650.568332	110855.756964	57.041972
2649.424391	110645.064227	57.046977
2649.000143	110444.362394	57.051981
2648.434381	110240.892303	57.056986
2648.066951	110037.836684	57.061991
2646.664493	109826.684189	57.066996
2646.440165	109621.483391	57.072001
2646.213429	109411.119086	57.077005
2644.981260	109217.713461	57.082010
2644.716754	108999.743591	57.087015
2643.909987	108805.797862	57.092020
2643.370603	108593.878263	57.097025
2642.848099	108382.827180	57.102029
2642.077595	108178.023231	57.107034
2641.542445	107954.039135	57.112039
2640.593474	107750.231580	57.117044
2639.740914	107545.141361	57.122049
2639.384148	107330.386405	57.127053
2638.512285	107124.972827	57.132058
2638.177127	106915.884504	57.137063
2637.564989	106716.676993	57.142068
2636.726816	106507.449819	57.147073
2636.267712	106290.404295	57.152077
2635.437945	106075.380083	57.157082
2634.603871	105865.003022	57.162087
2633.732166	105661.924122	57.167092
2633.127765	105456.069923	57.172097
2632.568805	105241.797011	57.177101
2631.576629	105050.696070	57.182106
2631.361536	104834.716309	57.187111
2630.717376	104644.432689	57.192116
2629.978269	104432.473306	57.197121
2629.182471	104224.591663	57.202125
2628.568124	104035.735699	57.207130
2627.883022	103808.692353	57.212135
2627.513621	103609.376989	57.217140
2626.682527	103411.570286	57.222145
2626.181986	103196.957527	57.227149
2625.061203	103005.683999	57.232154
2624.949553	102790.353491	57.237159
2624.310068	102582.347253	57.242164
2623.748219	102370.638284	57.247169
2623.052856	102157.302925	57.252173
2622.225994	101944.326567	57.257178
2621.771488	101738.043054	57.262183
2620.986225	101535.061822	57.267188
2620.123936	101321.658993	57.272193
2619.680243	101107.189459	57.277197
2618.650110	100903.281909	57.282202
2618.062166	100697.802622	57.287207
2617.365804	100497.366437	57.292212
2616.641449	100289.000661	57.297217
2615.923241	100089.580064	57.302221
2615.107107	99887.493429	57.307226
2614.912801	99677.222226	57.312231
2614.028591	99473.189885	57.317236
2613.067240	99274.024147	57.322241
2612.840106	99058.746242	57.327245
2611.978543	98872.660486	57.332250
2611.445975	98651.935271	57.337255
2611.027173	98441.349306	57.342260
2610.407674	98237.806042	57.347265
2609.495783	98037.380880	57.352269
2608.879834	97835.394624	57.357274
2608.424069	97631.114036	57.362279
2607.612402	97419.197928	57.367284
2606.815540	97213.180124	57.372289
2605.945394	97002.412479	57.377293
2605.090272	96798.468995	57.382298
2604.837829	96600.806042	57.387303
2604.062671	96400.950698	57.392308
2603.567959	96194.672211	57.397313
2602.961872	95991.641493	57.402317
2602.114121	95794.815588	57.407322
2601.859248	95574.418505	57.412327
2601.069464	95375.360931	57.417332
2600.055814	95170.023840	57.422337
2600.015647	94962.251197	57.427341
2598.801825	94756.277330	57.432346
2598.406931	94552.972354	57.437351
2597.677345	94343.291586	57.442356
2596.958264	94142.242324	57.447361
2596.124957	93931.782757	57.452365
2595.148178	93730.429222	57.457370
2594.918296	93537.013019	57.462375
2593.975079	93332.017633	57.467380
2593.194651	93133.974015	57.472385
2592.748977	92920.177596	57.477389
2592.009863	92730.653950	57.482394
2591.550758	92524.003895	57.487399
2591.076063	92320.211812	57.492404
2590.063939	92124.027490	57.497409
2589.587693	91915.045880	57.502413
2588.670161	91717.765809	57.507418
2588.249521	91506.972003	57.512423
2587.622943	91317.505973	57.517428
2586.853466	91114.894029	57.522433
2586.325755	90911.554467	57.527437
2585.429450	90708.579553	57.532442
2584.983942	90504.025955	57.537447
2584.236689	90304.264941	57.542452
2583.652510	90095.266900	57.547457
2583.077118	89891.208787	57.552461
2582.033265	89697.276591	57.557466
2581.578883	89493.608790	57.562471
2581.021427	89299.514257	57.567476
2580.067019	89094.667665	57.572481
2579.619192	88894.922747	57.577485
2578.815539	88686.923965	57.582490
2578.425580	88483.819637	57.587495
2577.462811	88286.640918	57.592500
2576.906929	88090.826018	57.597505
2576.201310	87891.612996	57.602509
2575.410079	87696.289092	57.607514
2574.805811	87497.044606	57.612519
2574.298845	87287.534983	57.617524
2573.806055	87096.816293	57.622529
2573.060887	86890.866849	57.627533
2572.615130	86698.730454	57.632538
2572.016705	86487.512343	57.637543
2571.187355	86284.561648	57.642548
2570.495078	86077.774762	57.647553
2569.992580	85868.449367	57.652557
2568.770957	85667.861540	57.657562
2568.268208	85452.638277	57.662567
2567.932153	85249.714261	57.667572
2566.621469	85057.647203	57.672577
2566.419023	84857.387209	57.677581
2565.789546	84662.445530	57.682586
2565.201178	84454.294936	57.687591
2564.484198	84260.461110	57.692596
2563.756933	84056.425045	57.697601
2563.096045	83848.076345	57.702605
2562.081046	83657.261825	57.707610
2561.767151	83447.847847	57.712615
2561.173371	83252.964131	57.717620
2560.185666	83054.791523	57.722625
2559.740850	82846.849434	57.727629
2558.791748	82660.033072	57.732634
2557.921370	82462.151671	57.737639
2557.113954	82261.986675	57.742644
2556.652941	82064.766693	57.747649
2556.419009	81872.621191	57.752653
2555.565635	81684.232760	57.757658
2554.815438	81492.388059	57.762663
2554.137861	81299.975851	57.767668
2553.570294	81101.926153	57.772673
2552.951414	80901.110436	57.777677
2552.309845	80712.031684	57.782682
2551.743930	80512.123964	57.787687
2550.958759	80326.760080	57.792692
2550.634017	80120.632211	57.797697
2549.950581	79919.525616	57.802701
2548.994944	79727.640947	57.807706
2548.452096	79523.632289	57.812711
2547.680755	79323.641783	57.817716
2547.152278	79123.031669	57.822721
2546.398467	78924.170296	57.827725
2545.284428	78725.760843	57.832730
2545.122380	78524.762566	57.837735
2544.186337	78343.508805	57.842740
2543.631247	78139.217875	57.847745
2543.414425	77943.221246	57.852749
2542.139566	77757.051760	57.857754
2541.655201	77558.838889	57.862759
2541.005793	77363.499343	57.867764
2540.160429	77163.154950	57.872769
2539.451490	76971.858779	57.877773
2538.551489	76775.062746	57.882778
2538.638126	76585.373995	57.887783
2537.814891	76391.154831	57.892788
2537.113638	76195.783942	57.897793
2536.516312	75995.164542	57.902797
2535.515828	75805.363871	57.907802
2535.090958	75611.399468	57.912807
2534.313767	75405.320788	57.917812
2533.707099	75210.704705	57.922817
2533.316248	75014.896762	57.927821
2532.119580	74830.553693	57.932826
2531.573829	74625.422001	57.937831
2531.146834	74442.880274	57.942836
2530.209576	74247.920333	57.947841
2529.932838	74042.130993	57.952845
2529.146053	73851.902902	57.957850
2528.608851	73664.659182	57.962855
2527.874795	73473.799064	57.967860
2527.382723	73264.098343	57.972865
2526.502363	73071.655989	57.977869
2526.141810	72882.186782	57.982874
2525.676467	72674.768743	57.987879
2524.396035	72471.555678	57.992884
2523.880960	72277.238464	57.997889
2523.639056	72070.899933	58.002893
2522.719437	71878.240860	58.007898
2521.694466	71683.592121	58.012903
2521.221264	71487.483116	58.017908
2520.706495	71283.292873	58.022913
2520.156668	71093.864276	58.027917
2519.393768	70898.997950	58.032922
2518.508415	70701.010893	58.037927
2517.978640	70508.258939	58.042932
2517.030617	70312.800575	58.047937
2516.693117	70108.581636	58.052941
2515.763754	69916.937648	58.057946
2515.176607	69718.691429	58.062951
2514.545842	69533.084923	58.067956
2513.794566	69336.388818	58.072961
2513.409456	69144.583707	58.077965
2512.382313	68950.209195	58.082970
2512.065271	68737.659023	58.087975
2511.480424	68556.082965	58.092980
2510.632057	68368.811723	58.097985
2509.863566	68177.488530	58.102989
2509.207542	67972.347788	58.107994
2508.905140	67774.734747	58.112999
2507.851027	67588.586665	58.118004
2507.235273	67387.220609	58.123009
2506.739785	67199.201576	58.128013
2505.841732	66997.972957	58.133018
2505.613162	66804.842207	58.138023
2504.751217	66611.801109	58.143028
2503.862014	66401.590065	58.148033
2503.517614	66214.189931	58.153037
2502.585922	66024.984721	58.158042
2502.196999	65819.532964	58.163047
2501.335229	65633.813253	58.168052
2500.721021	65435.820561	58.173057
2500.320661	65230.104548	58.178061
2499.361815	65045.612315	58.183066
2498.787773	64849.031517	58.188071
2497.979061	64652.125787	58.193076
2496.922620	64459.599282	58.198081
2496.374603	64260.702571	58.203085
2495.745018	64077.250309	58.208090
2495.006382	63883.608978	58.213095
2494.184887	63700.453541	58.218100
2493.878233	63514.390799	58.223105
2493.490251	63314.484326	58.228109
2492.467173	63142.520679	58.233114
2492.183303	62947.724386	58.238119
2491.170919	62752.659305	58.243124
2490.482701	62560.008028	58.248129
2490.003267	62374.195897	58.253133
2489.165569	62185.469494	58.258138
2489.019555	61991.813534	58.263143
2488.305564	61796.109408	58.268148
2487.540781	61603.809204	58.273153
2486.860942	61407.929540	58.278157
2485.767966	61210.559800	58.283162
2485.262809	61021.003958	58.288167
2484.873136	60837.544827	58.293172
2483.881115	60640.019407	58.298177
2483.561480	60444.757413	58.303181
2482.508969	60257.796911	58.308186
2482.193490	60056.244900	58.313191
2481.283750	59871.142831	58.318196
2480.441973	59682.410377	58.323201
2480.343676	59498.842098	58.328205
2479.595478	59307.274899	58.333210
2478.900365	59105.695124	58.338215
2477.749939	58917.532099	58.343220
2477.035558	58723.160911	58.348225
2476.973948	58535.566652	58.353229
2476.325458	58348.871316	58.358234
2475.806517	58148.210867	58.363239
2475.006093	57957.865415	58.368244
2474.465174	57771.025860	58.373249
2473.989371	57568.513129	58.378253
2473.071387	57378.401138	58.383258
2472.325638	57173.140636	58.388263
2471.657251	56982.689267	58.393268
2471.267104	56783.687961	58.398273
2470.610170	56584.066422	58.403277
2469.593400	56395.942493	58.408282
2469.337541	56193.394061	58.413287
2468.244834	56001.532498	58.418292
2467.478202	55815.390900	58.423297
2466.991773	55613.942457	58.428301
2466.076018	55416.140572	58.433306
2465.584928	55226.163402	58.438311
2464.981281	55035.120510	58.443316
2464.374133	54839.329848	58.448321
2463.753145	54648.170300	58.453325
2462.815758	54459.297179	58.458330
2462.181494	54266.893651	58.463335
2461.002074	54066.970801	58.468340
2460.456747	53886.921375	58.473345
2460.265703	53694.956757	58.478349
2459.621012	53507.689456	58.483354
2458.862067	53318.793485	58.488359
2458.032136	53136.258647	58.493364
2457.595484	52941.802979	58.498369
2457.146377	52754.907952	58.503373
2456.071531	52570.734148	58.508378
2455.805005	52373.096376	58.513383
2454.790892	52181.148449	58.518388
2453.978928	51997.837438	58.523393
2453.561699	51802.894080	58.528397
2452.602374	51628.533316	58.533402
2452.205299	51437.004878	58.538407
2451.547849	51247.772615	58.543412
2450.895395	51053.491628	58.548417
2450.347541	50859.753024	58.553421
2449.139523	50680.090397	58.558426
2448.784926	50491.476166	58.563431
2448.169952	50307.056325	58.568436
2447.435423	50122.771230	58.573441
2446.836051	49934.207974	58.578445
2446.125429	49744.509520	58.583450
2445.582000	49563.588374	58.588455
2444.948295	49375.523660	58.593460
2444.305395	49181.283522	58.598465
2443.580946	48985.536661	58.603469
2442.805778	48808.190622	58.608474
2442.560338	48615.121132	58.613479
2441.502612	48437.269932	58.618484
2440.841306	48248.322973	58.623489
2440.376590	48066.338356	58.628493
2439.651402	47874.264058	58.633498
2439.188362	47682.207213	58.638503
2438.488914	47498.282098	58.643508
2437.477748	47305.876502	58.648513
2436.940721	47114.694814	58.653517
2435.848879	46930.793507	58.658522
2435.701223	46743.571574	58.663527
2435.066964	46558.949928	58.668532
2434.129837	46375.703643	58.673537
2433.744050	46187.927484	58.678541
2432.924159	46009.949023	58.683546
2432.412154	45815.456032	58.688551
2431.632819	45630.718422	58.693556
2430.877204	45443.986228	58.698561
2430.520519	45260.526648	58.703565
2429.371943	45083.495324	58.708570
2428.979883	44888.285035	58.713575
2428.362529	44701.991111	58.718580
2427.817966	44516.016570	58.723585
2426.933270	44326.947673	58.728589
2426.230647	44152.979989	58.733594
2425.724395	43959.876151	58.738599
2425.096973	43780.067970	58.743604
2424.469848	43587.246764	58.748609
2423.834604	43396.048298	58.753613
2422.703801	43216.698939	58.758618
2422.230349	43039.907009	58.763623
2421.477246	42850.096335	58.768628
2420.763466	42669.206377	58.773633
2420.311815	42485.161601	58.778637
2419.462934	42309.783877	58.783642
2419.164382	42120.626994	58.788647
2418.241312	41945.818151	58.793652
2417.609673	41756.756001	58.798657
2417.067942	41571.603046	58.803661
2416.134737	41392.067277	58.808666
2415.405422	41197.694957	58.813671
2414.968044	41019.080582	58.818676
2414.217737	40837.048658	58.823681
2413.596087	40659.906055	58.828685
2412.908176	40476.973125	58.833690
2412.529393	40288.769210	58.838695
2411.664039	40106.393276	58.843700
2410.688173	39923.701617	58.848705
2410.319630	39741.358294	58.853709
2409.647969	39567.766907	58.858714
2408.958386	39379.236468	58.863719
2408.392233	39206.650175	58.868724
2407.668273	39020.581247	58.873729
2407.192444	38832.418177	58.878733
2406.425979	38645.417823	58.883738
2405.721023	38470.786778	58.888743
2404.830608	38290.019824	58.893748
2404.329745	38107.134705	58.898753
2403.971323	37925.830381	58.903757
2403.089132	37740.793282	58.908762
2402.424594	37565.271928	58.913767
2401.769494	37381.113295	58.918772
2401.196302	37194.746357	58.923777
2400.711797	37014.749028	58.928781
2399.992136	36829.155462	58.933786
2399.363306	36643.541621	58.938791
2398.704996	36461.133893	58.943796
2397.366500	36288.987348	58.948801
2397.330846	36088.632299	58.953805
2396.194746	35911.419826	58.958810
2395.624435	35728.274200	58.963815
2395.338362	35543.577555	58.968820
2394.837074	35365.176353	58.973825
2394.054851	35179.564994	58.978829
2393.010873	35010.463841	58.983834
2392.626845	34811.478461	58.988839
2391.583481	34631.414979	58.993844
2390.999240	34450.564640	58.998849
2390.909310	34270.891224	59.003853
2389.703236	34091.110651	59.008858
2389.297864	33901.867488	59.013863
2388.695417	33729.775844	59.018868
2388.007444	33544.036463	59.023873
2387.050366	33358.318114	59.028877
2386.119428	33182.007531	59.033882
2385.686493	32998.740329	59.038887
2385.206508	32823.313435	59.043892
2384.636166	32641.562259	59.048897
2383.823140	32452.476031	59.053901
2383.032820	32281.762945	59.058906
2382.372360	32094.597253	59.063911
2381.802417	31918.546237	59.068916
2381.407766	31747.660537	59.073921
2380.562433	31571.753270	59.078925
2379.764720	31377.727452	59.083930
2379.336560	31202.344229	59.088935
2378.520263	31020.156784	59.093940
2377.760670	30850.060381	59.098945
2377.366666	30660.629496	59.103949
2376.256877	30485.938738	59.108954
2375.683928	30303.184941	59.113959
2374.991993	30126.086793	59.118964
2374.746409	29945.473535	59.123969
2374.065419	29770.646522	59.128973
2373.442697	29598.624675	59.133978
2372.801222	29413.562584	59.138983
2371.747120	29234.339927	59.143988
2371.197834	29052.203021	59.148993
2370.349260	28869.387215	59.153997
2369.563480	28693.826730	59.159002
2369.269204	28516.660766	59.164007
2368.371688	28350.860670	59.169012
2367.869802	28170.424520	59.174017
2367.186187	27992.103107	59.179021
2366.304900	27820.583328	59.184026
2366.063340	27631.397068	59.189031
2365.248133	27461.524737	59.194036
2364.191806	27295.199705	59.199041
2363.760645	27123.208286	59.204045
2362.976661	26939.343791	59.209050
2362.611079	26759.702625	59.214055
2361.867865	26586.936970	59.219060
2361.129347	26418.998622	59.224065
2360.550555	26236.430245	59.229069
2360.199810	26060.074050	59.234074
2359.742011	25873.197637	59.239079
2358.566965	25699.028949	59.244084
2357.804240	25513.786333	59.249089
2357.319798	25345.310970	59.254093
2356.642512	25173.830274	59.259098
2356.181173	24988.573536	59.264103
2354.784227	24819.049441	59.269108
2354.493452	24640.419062	59.274113
2354.138998	24465.947961	59.279117
2352.866156	24296.214620	59.284122
2352.304335	24121.915983	59.289127
2351.782391	23950.636140	59.294132
2351.222755	23779.315138	59.299137
2350.958829	23601.474703	59.304141
2349.627105	23429.941869	59.309146
2349.081950	23252.398678	59.314151
2348.118689	23092.248728	59.319156
2347.659104	22918.837775	59.324161
2347.238590	22745.894752	59.329165
2346.368154	22576.382755	59.334170
2345.800621	22398.858128	59.339175
2344.867388	22227.794631	59.344180
2344.536753	22061.876887	59.349185
2344.081683	21887.929973	59.354189
2342.963014	21726.550189	59.359194
2342.303773	21554.239150	59.364199
2341.450021	21392.162185	59.369204
2341.138619	21218.473818	59.374209
2340.563139	21037.961096	59.379213
2339.233344	20878.754613	59.384218
2339.120969	20702.445661	59.389223
2338.531016	20547.644877	59.394228
2337.667278	20379.389410	59.399233
2337.373180	20205.249867	59.404237
2336.407000	20041.507751	59.409242
2335.820580	19866.934292	59.414247
2334.917945	19704.266512	59.419252
2334.310791	19545.421544	59.424257
2333.918689	19364.679356	59.429261
2333.143112	19207.332658	59.434266
2331.987140	19030.414410	59.439271
2331.410434	18869.416832	59.444276
2330.645483	18707.296501	59.449281
2330.543890	18549.213158	59.454285
2329.522217	18386.748421	59.459290
2328.911843	18217.128621	59.464295
2328.314923	18062.292195	59.469300
2327.698542	17893.620666	59.474305
2327.042168	17727.780789	59.479309
2326.279277	17575.144538	59.484314
2325.857422	17403.740027	59.489319
2325.209393	17243.482151	59.494324
2324.586615	17073.227022	59.499329
2324.066845	16907.025270	59.504333
2322.987474	16735.369646	59.509338
2322.517265	16568.807224	59.514343
2321.519662	16410.165712	59.519348
2320.834969	16252.126642	59.524353
2320.586275	16073.947843	59.529357
2319.770091	15924.892931	59.534362
2319.106189	15755.459554	59.539367
2318.565353	15583.543573	59.544372
2317.839343	15417.809004	59.549377
2317.209452	15257.139520	59.554381
2316.212291	15103.549209	59.559386
2315.567585	14929.551243	59.564391
2314.947007	14776.766382	59.569396
2314.102462	14618.001532	59.574401
2313.622719	14455.272086	59.579405
2313.183857	14298.414570	59.584410
2312.602367	14131.005295	59.589415
2311.638642	13974.529904	59.594420
2310.748291	13813.002590	59.599425
2310.231809	13660.128226	59.604429
2309.564211	13504.544230	59.609434
2309.231416	13328.271346	59.614439
2308.521958	13178.360037	59.619444
2307.588988	13011.752989	59.624449
2307.419138	12848.528701	59.629453
2306.495114	12697.260411	59.634458
2305.944418	12525.312424	59.639463
2305.075369	12367.360834	59.644468
2304.365493	12202.427844	59.649473
2303.840008	12041.894240	59.654477
2302.779812	11896.089869	59.659482
2302.517944	11729.788439	59.664487
2301.944110	11584.139943	59.669492
2300.900899	11421.415441	59.674497
2300.666353	11251.393628	59.679501
2299.835222	11100.086768	59.684506
2299.232139	10929.089710	59.689511
2298.363581	10780.517547	59.694516
2297.638640	10622.779058	59.699521
2297.257427	10462.801133	59.704525
2296.110207	10305.804819	59.709530
2295.930108	10143.708487	59.714535
2295.176373	9990.070484	59.719540
2294.092297	9830.972146	59.724545
2293.482441	9676.562140	59.729549
2292.714568	9523.653481	59.734554
2292.167620	9376.265688	59.739559
2291.508917	9229.969534	59.744564
2290.683425	9075.868919	59.749569
2290.129883	8924.676041	59.754573
2289.458000	8779.534144	59.759578
2288.872395	8613.529350	59.764583
2287.917045	8470.399973	59.769588
2287.345077	8319.526152	59.774593
2286.693174	8180.544395	59.779597
2285.906097	8033.576254	59.784602
2285.312387	7881.135517	59.789607
2284.498497	7735.887743	59.794612
2283.391340	7589.308440	59.799617
2283.315809	7443.324304	59.804621
2282.195462	7323.650941	59.809626
2281.661218	7167.137583	59.814631
2280.867979	7037.088156	59.819636
2280.174492	6895.258798	59.824641
2279.498004	6761.576148	59.829645
2278.525883	6632.043783	59.834650
2277.910506	6492.404869	59.839655
2277.322257	6367.532969	59.844660
2276.492699	6232.298435	59.849665
2275.891424	6098.927692	59.854669
2275.012371	5967.771143	59.859674
2274.255009	5830.506189	59.864679
2273.610080	5710.570362	59.869684
2272.937187	5583.423728	59.874689
2272.118917	5456.238922	59.879693
2270.840452	5347.820773	59.884698
2270.282988	5222.177387	59.889703
2269.607175	5111.409373	59.894708
2269.166342	5003.633895	59.899713
2268.704471	4894.471894	59.904718
2267.540428	4790.364616	59.909722
2266.855866	4675.927068	59.914727
2266.609361	4573.745526	59.919732
2265.190835	4468.623128	59.924737
2264.467484	4367.159920	59.929742
2263.272987	4270.966912	59.934746
2263.102803	4173.036115	59.939751
2262.035703	4077.145181	59.944756
2261.159485	3992.053260	59.949761
2260.513793	3886.557643	59.954766
2259.930274	3811.134443	59.959770
2259.147235	3727.351185	59.964775
2258.303226	3647.462550	59.969780
2257.778376	3566.005430	59.974785
2256.842963	3483.409514	59.979790
2255.915681	3419.257625	59.984794
2255.572816	3333.200747	59.989799
2254.477531	3262.534637	59.994804
2253.378436	3197.653811	59.999809
2253.239114	3128.297377	60.004814
2252.139467	3070.545457	60.009818
2251.557709	3004.435078	60.014823
2250.537387	2941.359245	60.019828
2250.217013	2883.377181	60.024833
2249.698196	2822.326517	60.029838
2248.666674	2764.944348	60.034842
2248.005243	2699.711580	60.039847
2247.051710	2655.342451	60.044852
2246.257374	2595.695318	60.049857
2245.800549	2544.914710	60.054862
2244.994595	2492.840256	60.059866
2244.245743	2445.250724	60.064871
2243.629972	2407.509521	60.069876
2242.712047	2365.085978	60.074881
2242.179162	2312.843449	60.079886
2241.517183	2266.687109	60.084890
2241.048565	2218.738396	60.089895
2240.447621	2183.654745	60.094900
2239.965582	2146.632750	60.099905
2239.396636	2090.059185	60.104910
2238.428497	2048.458406	60.109914
2237.889441	1993.042141	60.114919
2237.598875	1945.166234	60.119924
2236.713086	1898.039474	60.124929
2236.022762	1856.593116	60.129934
2235.186944	1810.950798	60.134938
2234.747019	1757.838263	60.139943
2234.068423	1720.599322	60.144948
2233.125813	1681.162676	60.149953
2233.054479	1636.842801	60.154958
2232.103959	1586.811792	60.159962
2231.659813	1544.503951	60.164967
2231.069760	1497.373364	60.169972
2230.207482	1455.473583	60.174977
2229.635966	1404.738779	60.179982
2228.684026	1365.052115	60.184986
2228.254413	1319.565336	60.189991
2227.615020	1278.821491	60.194996
2227.023770	1239.178101	60.200001
2226.420786	1189.083860	60.205006
2225.642469	1150.525527	60.210010
2224.839410	1096.756960	60.215015
2223.996149	1058.102716	60.220020
2223.463402	1021.451212	60.225025
2223.183718	969.058969	60.230030
2222.197895	931.837662	60.235034
2221.853517	887.119403	60.240039
2221.049913	849.895421	60.245044
2220.383158	807.994873	60.250049
2219.871192	759.328392	60.255054
2219.083952	722.425455	60.260058
2218.373602	679.457373	60.265063
2217.536314	639.968989	60.270068
2216.732898	596.224199	60.275073
2216.581560	545.146575	60.280078
2215.461832	527.048841	60.285082
2215.119711	482.075185	60.290087
2214.355755	441.304555	60.295092
2213.795840	400.072697	60.300097
2212.849864	368.455483	60.305102
2212.114441	336.546292	60.310106
2211.314428	288.319781	60.315111
2210.592868	264.907496	60.320116
2209.943276	237.232008	60.325121
2209.429731	201.056593	60.330126
2207.964656	179.292175	60.335130
2207.593126	152.556832	60.340135
2206.836467	134.045574	60.345140
2206.206991	112.932496	60.350145
2205.821264	89.520836	60.355150
2204.791979	61.243554	60.360154
2204.414651	35.149637	60.365159
2203.147417	17.976452	60.370164
2202.470823	3.032593	60.375169
2201.725187	-11.436641	60.380174
2200.227702	-7.188330	60.385178
2199.536554	-4.451026	60.390183
2198.884447	-3.771670	60.395188
2198.041833	12.662782	60.400193
2197.156192	10.862200	60.405198
2196.332689	12.156994	60.410202
2195.861443	16.732963	60.415207
2195.712350	20.636461	60.420212
2195.424744	22.371396	60.425217
2195.012425	16.710771	60.430222
2193.613817	20.552294	60.435226
2193.165087	26.154516	60.440231
2192.694135	23.400256	60.445236
2191.882272	26.543100	60.450241
2191.309585	26.127994	60.455246
2190.936596	34.290392	60.460250
2189.961569	31.234456	60.465255
2189.105687	32.718907	60.470260
2188.385427	33.850658	60.475265
2188.681919	36.358732	60.480270
2187.316040	30.220143	60.485274
2186.616720	30.375524	60.490279
2185.918502	40.157126	60.495284
2185.523429	46.045755	60.500289
2184.919896	37.829075	60.505294
2183.892233	38.683147	60.510298
2183.587653	34.178759	60.515303
2183.442533	46.509464	60.520308
2182.651014	41.487777	60.525313
2181.901879	32.470975	60.530318
2180.548308	39.140924	60.535322
2180.258095	35.460638	60.540327
2179.465826	41.010133	60.545332
2179.004939	43.143175	60.550337
2178.635432	42.312607	60.555342
2177.901552	50.358797	60.560346
2177.140697	42.827868	60.565351
2176.329941	40.658992	60.570356
2175.535589	44.377848	60.575361
2175.209172	35.978424	60.580366
2174.648573	49.963153	60.585370
2174.180340	41.923718	60.590375
2173.047740	40.685909	60.595380
2172.322150	36.212049	60.600385
2172.037756	40.048704	60.605390
2170.860791	42.705397	60.610394
2170.202212	35.191366	60.615399
2169.985885	41.901671	60.620404
2169.348951	42.994974	60.625409
2168.823952	43.841842	60.630414
2168.060179	42.685875	60.635418
2167.491069	40.126976	60.640423
2166.894313	45.588680	60.645428
2165.654691	39.753365	60.650433
2164.780536	45.304818	60.655438
2164.284662	44.070073	60.660442
2164.244336	34.377801	60.665447
2164.223863	45.408150	60.670452
2163.083501	43.502902	60.675457
2161.791832	35.666669	60.680462
2161.535449	46.641403	60.685466
2161.241768	47.645550	60.690471
2160.631781	44.970127	60.695476
2159.105207	57.543685	60.700481
2158.921245	45.972256	60.705486
2158.285116	47.171097	60.710490
2157.719294	44.704724	60.715495
2157.135502	41.873748	60.720500
2155.999617	45.810815	60.725505
2155.613626	38.057979	60.730510
2154.537901	51.206595	60.735514
2154.050791	44.898622	60.740519
2153.272915	44.530274	60.745524
2152.567330	49.403657	60.750529
2152.433723	39.943819	60.755534
2151.384174	46.705903	60.760538
2151.065907	42.973297	60.765543
2150.959817	41.993698	60.770548
2149.703486	48.507876	60.775553
2148.524875	45.146764	60.780558
2148.070569	52.506736	60.785562
2148.240232	37.595756	60.790567
2147.192232	52.716036	60.795572
2145.933042	49.186348	60.800577
2146.109581	43.295083	60.805582
2145.263376	54.959542	60.810586
2144.612626	48.299039	60.815591
2143.273891	46.800616	60.820596
2142.956795	45.083314	60.825601
2142.861911	37.169165	60.830606
2141.737342	45.447674	60.835610
2141.542001	43.625891	60.840615
2140.129443	48.671383	60.845620
2139.461789	55.743489	60.850625
2139.203871	43.388959	60.855630
2138.499001	55.433144	60.860634
2138.112787	45.579694	60.865639
2137.491214	44.298663	60.870644
2136.158653	43.578334	60.875649
2136.028351	44.812044	60.880654
2135.464917	55.160522	60.885658
2134.337762	48.003142	60.890663
2133.528102	44.528296	60.895668
2132.811587	50.428510	60.900673
2133.096497	37.082618	60.905678
2132.105556	35.514822	60.910682
2131.615929	40.658313	60.915687
2130.126440	45.775945	60.920692
2129.789651	41.961120	60.925697
2129.652035	39.862078	60.930702
2128.866162	48.668786	60.935706
2127.917698	46.116470	60.940711
2126.885027	44.498523	60.945716
2126.756253	46.563103	60.950721
2126.519456	44.254278	60.955726
2124.857025	53.144884	60.960730
2124.245686	49.611761	60.965735
2124.388408	40.368294	60.970740
2123.350466	43.638504	60.975745
2122.838860	43.249992	60.980750
2121.688994	51.212382	60.985754
2121.175121	43.609163	60.990759
2120.914116	46.640964	60.995764
2120.265364	47.777157	61.000769
2119.549209	42.568479	61.005774
2118.648830	50.642678	61.010778
2118.295721	42.124487	61.015783
2117.402891	38.145569	61.020788
2116.813123	37.714265	61.025793
2116.222452	38.655149	61.030798
2115.342049	38.437132	61.035802
2115.065569	38.597979	61.040807
2114.234126	45.092059	61.045812
2113.739048	44.789242	61.050817
2113.377278	43.769787	61.055822
2112.660969	41.980210	61.060826
2111.372194	31.057238	61.065831
2110.515155	38.744483	61.070836
2109.756478	47.251967	61.075841
2109.973887	42.070204	61.080846
2108.722089	48.511135	61.085850
2107.846490	37.946824	61.090855
2107.797470	37.694659	61.095860
2107.135436	41.485582	61.100865
2106.275527	41.019872	61.105870
2105.524549	49.806854	61.110874
2104.877597	47.690860	61.115879
2104.484045	49.718604	61.120884
2103.601770	53.069784	61.125889
2103.305168	45.509367	61.130894
2102.703050	51.962331	61.135898
2101.996206	46.570819	61.140903
2101.258004	50.451108	61.145908
2099.976321	50.249463	61.150913
2099.254253	46.000585	61.155918
2099.071526	50.229573	61.160922
2098.606544	48.289722	61.165927
2097.606822	47.212222	61.170932
2096.912599	55.332567	61.175937
2096.444849	49.445764	61.180942
2095.375953	47.251641	61.185946
2095.072670	50.466785	61.190951
2094.634110	49.260807	61.195956
2093.711362	50.707011	61.200961
2093.456913	47.640847	61.205966
2092.961276	52.051965	61.210970
2092.356215	43.595840	61.215975
2091.110327	53.218356	61.220980
2090.286999	53.260968	61.225985
2089.557905	52.832854	61.230990
2088.797301	50.004720	61.235994
2088.135068	43.568425	61.240999
2087.986097	54.974004	61.246004
2087.438669	50.121785	61.251009
2087.019550	48.956882	61.256014
2086.033653	52.125801	61.261018
2085.836348	49.632505	61.266023
2084.829068	53.241665	61.271028
2083.443348	53.545428	61.276033
2082.982007	43.028933	61.281038
2082.277299	52.095603	61.286042
2082.069198	47.161149	61.291047
2081.276658	49.526624	61.296052
2080.644196	49.436440	61.301057
2080.222623	44.498016	61.306062
2079.278846	48.481902	61.311066
2078.970351	43.344171	61.316071
2078.713592	41.309775	61.321076
2077.062285	45.440639	61.326081
2076.343512	40.757554	61.331086
2075.470282	46.957058	61.336090
2074.924376	45.511059	61.341095
2074.728248	45.644964	61.346100
2073.945560	36.903203	61.351105
2073.692890	36.834756	61.356110
2073.106231	43.867204	61.361114
2072.374326	43.441119	61.366119
2071.767828	40.424520	61.371124
2070.638008	43.058003	61.376129
2069.905509	45.429722	61.381134
2068.609570	49.690289	61.386138
2068.769937	41.213631	61.391143
2067.833305	40.750647	61.396148
2067.099445	44.579788	61.401153
2067.254291	41.331970	61.406158
2066.618223	51.184165	61.411162
2066.355722	42.839276	61.416167
2065.128846	39.030095	61.421172
2063.671777	42.420462	61.426177
2063.332051	32.632207	61.431182
2062.580124	38.798266	61.436186
2061.995367	41.761593	61.441191
2061.438971	43.750527	61.446196
2060.997120	42.041995	61.451201
2060.741360	38.540776	61.456206
2060.011822	43.395899	61.461210
2059.105708	41.276891	61.466215
2058.272812	42.924904	61.471220
2057.223955	47.766048	61.476225
2056.750554	38.726031	61.481230
2056.083852	46.802584	61.486234
2055.819963	48.111117	61.491239
2055.294585	37.609528	61.496244
2054.475419	44.183682	61.501249
2053.434915	35.156395	61.506254
2052.063864	43.136560	61.511258
2052.021927	45.969583	61.516263
2051.729790	43.710553	61.521268
2050.783572	54.174987	61.526273
2050.393568	43.525745	61.531278
2049.786687	41.852870	61.536282
2049.617154	35.584418	61.541287
2049.193682	36.792113	61.546292
2047.921329	49.460994	61.551297
2046.767258	40.858613	61.556302
2046.157479	44.854160	61.561306
2045.709675	37.820839	61.566311
2045.370172	32.771623	61.571316
2044.499577	39.014870	61.576321
2043.104260	38.766629	61.581326
2042.409885	42.490154	61.586330
2042.488793	45.218835	61.591335
2041.729558	42.563977	61.596340
2040.942839	39.571258	61.601345
2040.773478	34.938193	61.606350
2039.900383	43.757182	61.611354
2039.498782	35.055884	61.616359
2038.720659	50.388838	61.621364
2037.603667	43.370255	61.626369
2037.111746	40.554693	61.631374
2036.193367	46.578433	61.636378
2035.540461	42.665552	61.641383
2035.303788	46.032565	61.646388
2034.653532	46.255897	61.651393
2034.363102	29.558605	61.656398
2033.136645	39.930307	61.661402
2032.253615	40.058112	61.666407
2031.530502	42.910931	61.671412
2030.925630	38.939963	61.676417
2030.465956	36.176059	61.681422
2029.777300	38.217531	61.686426
2029.806720	37.590194	61.691431
2029.202975	25.654894	61.696436
2027.913128	39.397374	61.701441
2027.094274	36.329331	61.706446
2026.544330	45.661622	61.711450
2025.621496	41.616533	61.716455
2025.492510	36.617491	61.721460
2024.800828	45.160092	61.726465
2024.254955	37.683417	61.731470
2023.319768	41.098213	61.736474
2022.508143	49.046377	61.741479
2021.756737	35.313002	61.746484
2020.901235	41.456084	61.751489
2020.812565	40.544694	61.756494
2020.203164	51.021910	61.761498
2019.548132	42.919118	61.766503
2018.530099	42.200971	61.771508
2017.481135	41.992394	61.776513
2017.438897	37.777576	61.781518
2016.314441	42.312165	61.786522
2016.030782	44.860256	61.791527
2015.486919	41.907853	61.796532
2015.213035	38.418978	61.801537
2014.219830	40.229653	61.806542
2012.969262	44.779529	61.811546
2012.153295	34.330387	61.816551
2011.790607	39.467938	61.821556
2010.941964	44.703125	61.826561
2010.684650	43.064668	61.831566
2010.213064	46.541512	61.836570
2009.996718	35.460996	61.841575
2009.820225	33.544765	61.846580
2007.848158	44.916402	61.851585
2007.397922	36.733799	61.856590
2006.722342	44.188829	61.861594
2006.242603	39.988257	61.866599
2005.941814	36.568314	61.871604
2004.569386	41.038181	61.876609
2003.990113	35.413553	61.881614
2002.884383	39.298579	61.886618
2002.573422	41.275376	61.891623
2002.445570	37.723898	61.896628
2001.804876	34.957192	61.901633
2001.537879	34.230237	61.906638
1999.866969	38.671783	61.911642
1999.020302	36.005584	61.916647
1998.825871	38.735068	61.921652
1998.124247	40.600398	61.926657
1997.979854	37.056277	61.931662
1997.752092	43.301589	61.936666
1996.729488	41.595360	61.941671
1995.407101	41.792915	61.946676
1994.736266	37.755152	61.951681
1994.049278	31.258164	61.956686
1993.758000	34.764739	61.961690
1993.371563	28.341479	61.966695
1992.168958	31.905971	61.971700
1990.898924	36.164034	61.976705
1990.739638	25.752608	61.981710
1990.096655	34.049342	61.986714
1989.620504	25.747853	61.991719
1989.636104	26.002709	61.996724
1988.628034	26.790662	62.001729
1987.657569	17.596173	62.006734
1986.584304	26.350736	62.011738
1986.247863	31.906772	62.016743
1985.664705	28.520616	62.021748
1985.029264	31.061464	62.026753
1984.836907	23.784176	62.031758
1983.905741	32.762210	62.036762
1982.871613	26.110581	62.041767
1982.191033	30.033790	62.046772
1981.345382	39.764705	62.051777
1981.301742	27.667969	62.056782
1980.677371	37.895228	62.061786
1980.087187	32.658719	62.066791
1978.867939	35.295393	62.071796
1978.330827	34.851031	62.076801
1978.063740	28.061877	62.081806
1977.535579	35.357880	62.086810
1977.034069	31.089805	62.091815
1975.667977	34.509933	62.096820
1974.443299	37.912345	62.101825
1974.037816	33.488669	62.106830
1973.439885	34.394463	62.111834
1973.091765	28.250574	62.116839
1972.760976	31.553673	62.121844
1972.126959	31.394372	62.126849
1971.178661	26.362958	62.131854
1970.266770	30.695073	62.136858
1969.911694	29.463251	62.141863
1969.787725	22.578838	62.146868
1968.698154	30.555354	62.151873
1967.914452	29.219673	62.156878
1966.777054	33.267444	62.161882
1966.260772	27.635984	62.166887
1966.171351	29.166004	62.171892
1965.322342	37.233657	62.176897
1965.281243	30.064831	62.181902
1964.059260	38.909253	62.186906
1963.647423	39.146799	62.191911
1962.871680	35.188782	62.196916
1961.456305	35.188213	62.201921
1960.547451	28.745381	62.206926
1960.131452	37.182720	62.211930
1960.224818	36.102078	62.216935
1959.418631	30.699578	62.221940
1958.482734	42.703175	62.226945
1958.098824	24.449998	62.231950
1957.475056	30.154155	62.236954
1956.780092	36.632913	62.241959
1955.685211	33.384771	62.246964
1954.823793	34.040640	62.251969
1954.582565	38.867158	62.256974
1953.930585	33.476452	62.261978
1953.613668	35.241296	62.266983
1953.391393	37.659790	62.271988
1951.994227	42.147802	62.276993
1951.467005	36.888688	62.281998
1950.561071	35.510910	62.287002
1950.179174	34.909442	62.292007
1949.916763	29.255032	62.297012
1948.596744	33.393306	62.302017
1947.901206	30.159050	62.307022
1947.101254	37.957127	62.312026
1946.449134	40.344504	62.317031
1946.107619	29.927316	62.322036
1945.771731	38.542763	62.327041
1945.039262	33.667920	62.332046
1944.008847	29.321379	62.337050
1943.434441	31.090827	62.342055
1942.916962	34.287939	62.347060
1942.232594	34.836853	62.352065
1941.487149	32.741272	62.357070
1940.624448	34.214266	62.362074
1939.919653	32.538039	62.367079
1939.201074	28.581996	62.372084
1938.533417	40.159787	62.377089
1938.664235	32.413277	62.382094
1937.829430	36.733166	62.387098
1937.112621	35.746444	62.392103
1936.330495	31.027731	62.397108
1935.436412	28.744423	62.402113
1935.318843	20.348177	62.407118
1933.900310	39.310677	62.412122
1932.740727	27.898920	62.417127
1932.194968	27.660958	62.422132
1932.126952	28.102564	62.427137
1931.550773	21.357759	62.432142
1930.964004	36.923703	62.437146
1930.204909	25.538263	62.442151
1930.117033	23.508618	62.447156
1929.064469	29.085298	62.452161
1928.603885	28.187221	62.457166
1927.631504	29.387452	62.462170
1926.999423	29.723051	62.467175
1926.863930	23.447639	62.472180
1925.396413	30.337649	62.477185
1924.935961	26.126153	62.482190
1923.955616	30.664705	62.487194
1923.432005	26.975779	62.492199
1923.256609	29.818945	62.497204
1922.436119	30.741158	62.502209
1921.744076	29.288431	62.507214
1920.645061	31.447118	62.512218
1920.051947	35.403768	62.517223
1919.319967	31.235378	62.522228
1918.931374	40.901631	62.527233
1918.888309	27.341302	62.532238
1918.081908	34.504854	62.537242
1916.855184	32.968268	62.542247
1916.253793	34.459713	62.547252
1915.795347	36.644449	62.552257
1915.615380	24.512594	62.557262
1914.408238	34.662057	62.562266
1913.562013	30.196395	62.567271
1913.390423	32.925409	62.572276
1912.335115	40.336654	62.577281
1912.048927	27.611339	62.582286
1910.814016	28.536267	62.587290
1910.008961	30.597823	62.592295
1909.474376	28.585479	62.597300
1908.633356	34.432954	62.602305
1908.783007	26.289194	62.607310
1908.131034	43.111373	62.612314
1907.651848	32.932106	62.617319
1906.875709	31.902770	62.622324
1905.958691	37.719732	62.627329
1905.774469	27.670271	62.632334
1904.443706	29.279092	62.637338
1903.630463	30.651199	62.642343
1902.785612	22.319956	62.647348
1902.415162	32.737158	62.652353
1902.244223	18.220943	62.657358
1901.254772	35.533538	62.662362
1900.504019	18.005727	62.667367
1899.637463	29.441616	62.672372
1898.878977	36.163875	62.677377
1898.759904	27.589661	62.682382
1898.018377	39.302195	62.687386
1897.729706	29.756628	62.692391
1896.730629	23.509511	62.697396
1895.491578	25.895458	62.702401
1895.318364	22.978864	62.707406
1894.792117	32.830982	62.712410
1894.343728	17.374735	62.717415
1893.265684	24.382707	62.722420
1892.451876	31.711453	62.727425
1891.987534	29.169108	62.732430
1891.698901	23.966758	62.737434
1890.678523	32.528443	62.742439
1889.785730	24.957073	62.747444
1888.994637	31.078919	62.752449
1888.725453	24.588179	62.757454
1887.864135	27.565481	62.762458
1887.752981	22.658251	62.767463
1886.513137	26.987263	62.772468
1885.358142	31.104095	62.777473
1885.274684	19.292842	62.782478
1884.629414	28.619770	62.787482
1884.389444	26.081230	62.792487
1883.922058	18.174224	62.797492
1882.840080	28.127190	62.802497
1881.970632	20.940075	62.807502
1881.418199	30.476208	62.812506
1881.089433	22.886258	62.817511
1880.165540	23.714507	62.822516
1878.760877	23.715436	62.827521
1878.390227	20.754493	62.832526
1877.950000	24.934471	62.837530
1877.858281	17.508752	62.842535
1877.476638	17.435568	62.847540
1876.110973	22.863267	62.852545
1875.349595	15.371974	62.857550
1874.602863	23.254656	62.862554
1874.118015	19.318300	62.867559
1873.788393	24.319712	62.872564
1872.513454	30.046843	62.877569
1872.092869	15.759523	62.882574
1871.121264	23.239489	62.887578
1870.988907	19.179353	62.892583
1870.594245	19.455190	62.897588
1869.553637	29.469406	62.902593
1868.902777	18.577779	62.907598
1867.861588	27.612734	62.912602
1867.470274	22.202750	62.917607
1867.191323	21.182799	62.922612
1866.453570	22.408881	62.927617
1865.643807	23.207974	62.932622
1864.809634	30.954725	62.937626
1864.108715	23.333977	62.942631
1863.787764	17.734616	62.947636
1862.835313	21.313060	62.952641
1861.517936	15.748901	62.957646
1861.223162	34.339011	62.962650
1860.785177	22.057314	62.967655
1860.110408	26.794964	62.972660
1859.520119	28.718348	62.977665
1859.616014	15.574398	62.982670
1858.923669	18.785093	62.987674
1858.094737	14.267822	62.992679
1856.899422	24.112625	62.997684
1856.274457	28.523803	63.002689
1855.659528	20.861018	63.007694
1854.612634	21.158413	63.012698
1854.160563	20.235343	63.017703
1853.619759	22.322769	63.022708
1853.066135	30.069135	63.027713
1852.725372	16.972439	63.032718
1851.753294	22.233568	63.037722
1851.160880	25.549832	63.042727
1850.407633	22.835736	63.047732
1849.616123	27.407410	63.052737
1849.413960	13.985915	63.057742
1848.325511	27.245428	63.062746
1847.763009	17.804864	63.067751
1847.314835	20.398012	63.072756
1846.662795	25.838576	63.077761
1845.999833	17.166222	63.082766
1845.179027	14.842927	63.087770
1844.694578	16.708504	63.092775
1843.961375	17.471791	63.097780
1842.448887	23.660880	63.102785
1842.326209	8.731722	63.107790
1841.389111	16.796033	63.112794
1841.016507	20.694023	63.117799
1840.716970	18.399929	63.122804
1840.331169	23.522234	63.127809
1839.469128	21.142406	63.132814
1838.270110	31.818916	63.137818
1837.429258	15.502432	63.142823
1837.395505	18.542318	63.147828
1836.439400	30.419822	63.152833
1835.393341	24.654887	63.157838
1834.676954	20.034591	63.162842
1834.299381	18.345863	63.167847
1833.647364	22.587863	63.172852
1833.428041	25.816500	63.177857
1833.531540	21.154329	63.182862
1832.192849	23.253331	63.187866
1830.976128	21.418713	63.192871
1830.810123	22.716452	63.197876
1830.069718	21.355015	63.202881
1829.157543	19.309602	63.207886
1828.475935	23.991570	63.212890
1827.676954	13.781114	63.217895
1827.284671	13.132426	63.222900
1826.727141	28.196950	63.227905
1826.489147	20.933244	63.232910
1825.164896	16.895210	63.237914
1824.462355	25.789664	63.242919
1824.112210	30.765953	63.247924
1823.508224	31.761056	63.252929
1822.459663	23.044275	63.257934
1821.615417	24.523837	63.262938
1821.316615	17.421186	63.267943
1820.783180	22.920196	63.272948
1819.935733	26.761120	63.277953
1819.863979	23.560323	63.282958
1818.618234	25.811741	63.287962
1818.067635	21.038959	63.292967
1817.362603	21.870324	63.297972
1816.850715	21.022996	63.302977
1815.574697	12.867503	63.307982
1814.891500	25.058086	63.312986
1814.529089	16.743319	63.317991
1814.363660	14.694456	63.322996
1813.510937	26.585510	63.328001
1813.024013	14.841496	63.333006
1811.875469	33.840009	63.338010
1811.183588	26.678342	63.343015
1810.812856	19.096651	63.348020
1810.118826	25.835499	63.353025
1810.057604	17.947598	63.358030
1808.967086	27.274274	63.363034
1807.895231	17.094541	63.368039
1807.273410	14.555145	63.373044
1806.467522	22.494546	63.378049
1806.554009	16.677520	63.383054
1805.301406	23.859907	63.388058
1804.588333	25.078931	63.393063
1804.379432	15.083882	63.398068
1803.882319	20.701713	63.403073
1803.155887	9.639180	63.408078
1801.875637	21.840991	63.413082
1801.492595	21.059943	63.418087
1801.085476	20.473542	63.423092
1800.553815	27.150335	63.428097
1799.361971	24.310351	63.433102
1798.741152	24.063836	63.438106
1798.623842	26.087174	63.443111
1797.898796	22.349839	63.448116
1796.703244	26.411641	63.453121
1796.094932	23.497916	63.458126
1795.234055	29.135670	63.463130
1794.844342	25.351390	63.468135
1794.280554	28.186849	63.473140
1793.640971	22.619174	63.478145
1793.240502	18.245209	63.483150
1791.986727	23.623637	63.488154
1791.357549	27.955067	63.493159
1791.170360	23.255475	63.498164
1790.401870	23.462949	63.503169
1789.669644	21.281734	63.508174
1788.864932	27.585549	63.513178
1788.355493	22.553909	63.518183
1788.155725	21.280103	63.523188
1786.823103	25.448838	63.528193
1785.951234	12.791346	63.533198
1785.077148	29.148864	63.538202
1784.719394	22.651708	63.543207
1784.169338	23.507359	63.548212
1783.622519	21.963795	63.553217
1783.821359	16.677742	63.558222
1782.300101	31.466363	63.563226
1781.611552	26.977288	63.568231
1781.078448	28.440569	63.573236
1780.566486	26.648603	63.578241
1779.890139	21.200320	63.583246
1778.523818	26.497274	63.588250
1778.102979	24.902163	63.593255
1777.811956	23.666506	63.598260
1777.185915	17.082642	63.603265
1777.078708	20.090035	63.608270
1775.894550	24.038064	63.613274
1774.985753	18.013226	63.618279
1774.585787	15.459107	63.623284
1773.836484	24.886155	63.628289
1772.943882	27.496275	63.633294
1772.509381	34.739578	63.638298
1771.868912	20.651220	63.643303
1771.238919	21.346093	63.648308
1770.397396	26.029814	63.653313
1769.620469	26.675478	63.658318
1768.596945	31.279289	63.663322
1768.019330	32.074662	63.668327
1768.218206	21.699443	63.673332
1767.235930	36.380397	63.678337
1767.165596	16.057288	63.683342
1766.251065	33.190839	63.688346
1765.279933	31.632660	63.693351
1764.634274	26.707819	63.698356
1763.347651	37.191679	63.703361
1762.628366	18.736358	63.708366
1761.959360	23.558273	63.713370
1761.783463	25.576723	63.718375
1761.301877	21.021669	63.723380
1760.741554	26.308903	63.728385
1760.692756	24.651554	63.733390
1759.391255	25.829994	63.738394
1758.652707	14.073918	63.743399
1758.315921	19.689948	63.748404
1757.158086	20.260484	63.753409
1756.607634	21.874767	63.758414
1755.952574	23.120863	63.763418
1755.158321	23.240969	63.768423
1754.895832	19.497999	63.773428
1754.136994	28.511802	63.778433
1753.341568	18.540522	63.783438
1752.337236	29.889507	63.788442
1751.987107	23.845337	63.793447
1751.617375	26.239948	63.798452
1750.509084	30.004041	63.803457
1749.891066	27.705344	63.808462
1749.047896	29.441818	63.813466
1748.271988	31.844167	63.818471
1748.057799	31.238172	63.823476
1747.642594	35.001006	63.828481
1747.284217	27.086181	63.833486
1746.172678	35.197157	63.838490
1745.818995	31.433973	63.843495
1744.858555	32.644990	63.848500
1743.550529	40.796639	63.853505
1743.351989	27.749920	63.858510
1742.515945	29.378025	63.863514
1742.704644	28.118223	63.868519
1741.868064	31.189419	63.873524
1740.597642	20.557100	63.878529
1740.145173	23.900046	63.883534
1739.415981	37.517303	63.888538
1738.983754	29.584243	63.893543
1738.002505	24.244327	63.898548
1737.049964	32.326898	63.903553
1736.739077	25.667754	63.908558
1736.526642	29.310068	63.913562
1735.507581	27.504030	63.918567
1734.525336	27.461601	63.923572
1733.756088	36.775129	63.928577
1733.706796	34.628972	63.933582
1733.033583	39.147194	63.938586
1732.321831	26.393317	63.943591
1731.494312	27.709391	63.948596
1730.373400	40.198192	63.953601
1730.374039	21.808322	63.958606
1729.530730	33.306793	63.963610
1729.239622	24.845090	63.968615
1727.994165	31.583224	63.973620
1727.400253	38.555367	63.978625
1726.961964	27.354038	63.983630
1726.281395	29.933650	63.988634
1725.912416	25.657204	63.993639
1725.057884	26.059724	63.998644
1723.966419	29.024742	64.003649
1723.689764	22.442173	64.008654
1723.067643	19.655249	64.013658
1722.455455	26.207638	64.018663
1721.577845	23.464448	64.023668
1720.922237	24.529278	64.028673
1720.719567	17.163781	64.033678
1719.381797	22.561888	64.038682
1718.482419	23.438342	64.043687
1718.031871	17.722388	64.048692
1717.492411	29.793956	64.053697
1717.551131	22.826937	64.058702
1716.554230	27.040158	64.063706
1715.349896	28.535944	64.068711
1714.939477	27.063777	64.073716
1714.123212	28.359144	64.078721
1714.070376	20.339025	64.083726
1713.122742	28.725192	64.088730
1711.889739	18.678344	64.093735
1711.573560	20.121375	64.098740
1710.844866	26.946178	64.103745
1710.911942	18.569524	64.108750
1709.977167	21.260483	64.113754
1709.253086	26.110082	64.118759
1708.513531	28.150253	64.123764
1707.917110	35.917631	64.128769
1707.248242	28.405392	64.133774
1706.240425	34.885003	64.138778
1705.637260	32.875712	64.143783
1705.087752	27.727446	64.148788
1704.383739	28.467210	64.153793
1703.916231	27.258019	64.158798
1702.848251	34.893705	64.163802
1702.146584	29.596132	64.168807
1701.735118	25.389521	64.173812
1701.149865	31.281584	64.178817
1700.812322	23.863388	64.183822
1699.642681	33.013424	64.188826
1699.062650	27.254956	64.193831
1698.176061	29.577122	64.198836
1697.767835	31.731834	64.203841
1697.743731	27.704983	64.208846
1696.884589	29.715263	64.213850
1695.998255	25.420070	64.218855
1695.763483	26.108956	64.223860
1694.673569	30.808499	64.228865
1693.722550	17.006062	64.233870
1692.955404	34.712342	64.238874
1692.522623	30.332487	64.243879
1692.396759	20.439391	64.248884
1690.916341	39.181552	64.253889
1690.591267	21.660343	64.258894
1689.788882	24.014869	64.263898
1689.358779	25.592701	64.268903
1689.134343	20.015890	64.273908
1687.768677	21.857457	64.278913
1687.321338	21.428860	64.283918
1686.542528	19.348123	64.288922
1685.969639	20.354087	64.293927
1685.321777	17.427750	64.298932
1684.462567	24.654937	64.303937
1683.706097	21.883056	64.308942
1683.076375	23.995677	64.313946
1683.073381	22.370482	64.318951
1682.514515	21.527490	64.323956
1681.207354	24.840621	64.328961
1680.748241	23.527592	64.333966
1680.118005	28.313402	64.338970
1679.280526	32.042390	64.343975
1678.549435	23.989656	64.348980
1677.526400	26.946976	64.353985
1677.596007	22.840582	64.358990
1676.796444	27.904042	64.363994
1676.182821	25.674057	64.368999
1675.120505	18.785765	64.374004
1674.001685	31.258472	64.379009
1673.890168	24.659140	64.384014
1673.594743	25.411283	64.389018
1673.151424	20.206734	64.394023
1672.540420	20.281986	64.399028
1671.331685	20.873262	64.404033
1671.282232	19.004696	64.409038
1669.926643	20.210696	64.414042
1668.959484	21.110550	64.419047
1668.564568	17.599954	64.424052
1667.750974	22.746073	64.429057
1667.586521	20.099364	64.434062
1667.039757	24.140163	64.439066
1666.573249	22.847236	64.444071
1665.731916	16.281837	64.449076
1664.983915	23.328925	64.454081
1664.356427	15.303901	64.459086
1663.135356	22.188003	64.464090
1662.479327	23.666102	64.469095
1662.217269	20.150172	64.474100
1661.284080	20.287647	64.479105
1661.537111	23.281973	64.484110
1660.274395	23.293589	64.489114
1659.476294	26.286150	64.494119
1658.975486	29.498007	64.499124
1658.482665	29.985023	64.504129
1657.725427	14.207318	64.509134
1656.430307	19.614448	64.514138
1655.938459	21.766678	64.519143
1655.816554	15.301475	64.524148
1655.229438	22.420784	64.529153
1654.419708	23.699360	64.534158
1653.478112	21.650801	64.539162
1652.788999	30.196203	64.544167
1652.045576	17.906321	64.549172
1651.818052	23.973387	64.554177
1651.033209	18.823097	64.559182
1650.218258	21.173322	64.564186
1649.464139	20.735117	64.569191
1648.915903	20.234241	64.574196
1648.416815	29.645222	64.579201
1648.033472	15.560228	64.584206
1647.005484	23.222692	64.589210
1646.604219	18.798417	64.594215
1646.000055	22.430420	64.599220
1644.914250	13.968824	64.604225
1644.275551	19.312682	64.609230
1643.786703	18.233057	64.614234
1643.069176	18.025599	64.619239
1642.197093	18.260612	64.624244
1641.034948	22.389715	64.629249
1640.998537	12.026654	64.634254
1640.222631	18.423701	64.639258
1640.047223	19.300293	64.644263
1639.537121	23.570253	64.649268
1638.116033	20.724188	64.654273
1637.818583	18.404558	64.659278
1636.990223	18.686248	64.664282
1636.657982	7.840298	64.669287
1635.872187	13.007238	64.674292
1634.759893	16.672654	64.679297
1634.448014	14.353741	64.684302
1633.942232	15.858442	64.689306
1632.985947	15.020248	64.694311
1631.963138	19.996173	64.699316
1630.975637	23.354743	64.704321
1631.304402	11.506436	64.709326
1630.646357	13.133104	64.714330
1630.383823	19.177344	64.719335
1629.636868	12.415606	64.724340
1628.247382	18.701964	64.729345
1627.997048	11.891294	64.734350
1627.520119	14.082161	64.739354
1626.526248	12.139696	64.744359
1625.801161	11.644843	64.749364
1625.038849	16.938952	64.754369
1624.588553	12.535090	64.759374
1624.019037	19.424511	64.764378
1622.916102	6.548330	64.769383
1622.470007	4.537766	64.774388
1621.596266	12.472213	64.779393
1621.514230	6.259320	64.784398
1620.930119	12.785182	64.789402
1620.083434	9.732747	64.794407
1619.552455	10.749414	64.799412
1618.641755	17.844436	64.804417
1617.711869	10.903596	64.809422
1616.694826	16.053661	64.814426
1615.701422	12.267553	64.819431
1615.785860	5.020479	64.824436
1614.853866	11.298816	64.829441
1615.055594	6.920686	64.834446
1614.407625	10.263165	64.839450
1613.906995	14.689327	64.844455
1612.944482	17.239636	64.849460
1612.004884	19.445662	64.854465
1611.638974	14.088472	64.859470
1610.277508	20.045516	64.864474
1609.691217	14.945704	64.869479
1609.472802	9.185014	64.874484
1608.586712	20.952087	64.879489
1608.267568	14.731129	64.884494
1607.164283	25.687413	64.889498
1606.345303	18.270031	64.894503
1606.131922	13.011620	64.899508
1605.258557	16.776291	64.904513
1605.476499	5.306741	64.909518
1604.117744	13.491726	64.914522
1603.394871	11.061486	64.919527
1603.216741	8.006925	64.924532
1601.771050	24.234495	64.929537
1601.445395	11.032966	64.934542
1600.548998	8.500979	64.939546
1600.092451	10.560870	64.944551
1599.965947	6.764779	64.949556
1598.707903	13.632699	64.954561
1598.186862	19.077728	64.959566
1597.501309	16.378192	64.964570
1597.011136	11.920744	64.969575
1595.867993	7.175934	64.974580
1595.080719	17.418070	64.979585
1594.761736	15.371544	64.984590
1594.093989	15.082069	64.989594
1593.779839	13.839071	64.994599
1593.238042	9.523877	64.999604
1591.922355	15.727558	65.004609
1591.778232	12.399495	65.009614
1591.295932	22.284078	65.014618
1590.470564	15.310870	65.019623
1589.431250	5.764795	65.024628
1588.359401	11.164865	65.029633
1588.670336	8.698116	65.034638
1587.549006	9.111530	65.039642
1586.685312	13.385633	65.044647
1586.447386	12.876471	65.049652
1585.738951	15.567781	65.054657
1585.268115	13.110118	65.059662
1584.043621	14.941923	65.064666
1583.188047	15.067094	65.069671
1582.996708	10.199448	65.074676
1582.572360	17.283441	65.079681
1581.936636	9.165133	65.084686
1580.753869	14.035594	65.089690
1580.360882	17.965235	65.094695
1579.992911	13.355902	65.099700
1578.602605	15.357567	65.104705
1578.014082	8.837198	65.109710
1577.326804	14.518389	65.114714
1576.844604	13.704244	65.119719
1576.706205	13.595610	65.124724
1576.149894	10.755691	65.129729
1575.015414	4.378846	65.134734
1574.235474	15.548701	65.139738
1573.537303	15.896463	65.144743
1573.318889	12.092897	65.149748
1571.942878	18.145314	65.154753
1571.336897	8.759066	65.159758
1570.862134	16.070280	65.164762
1570.353691	10.699476	65.169767
1570.349026	15.985185	65.174772
1569.062801	20.340625	65.179777
1568.413072	4.175282	65.184782
1567.569924	13.096846	65.189786
1567.173641	15.828453	65.194791
1566.889325	11.948622	65.199796
1565.609372	12.469256	65.204801
1565.058391	4.116704	65.209806
1564.378198	11.023716	65.214810
1563.912508	13.993447	65.219815
1563.031341	15.597233	65.224820
1562.165177	18.214257	65.229825
1561.884553	5.007166	65.234830
1561.347312	12.087019	65.239834
1560.344322	9.035786	65.244839
1559.736537	11.827811	65.249844
1558.799160	19.311889	65.254849
1558.363640	8.450828	65.259854
1557.679004	14.642567	65.264858
1557.599927	10.252280	65.269863
1556.750353	17.137321	65.274868
1556.015710	16.036842	65.279873
1555.525839	10.089044	65.284878
1554.393769	10.300740	65.289882
1553.796348	13.666742	65.294887
1553.362496	5.923247	65.299892
1552.448471	6.819431	65.304897
1552.312157	9.833026	65.309902
1551.024815	14.250155	65.314906
1550.519567	5.395146	65.319911
1549.936622	7.462513	65.324916
1549.532035	11.606900	65.329921
1548.879158	5.341211	65.334926
1547.752873	14.979593	65.339930
1547.009448	9.767566	65.344935
1546.706193	10.910498	65.349940
1546.040339	18.081759	65.354945
1545.025003	9.541206	65.359950
1544.397464	9.884060	65.364954
1544.104671	11.421169	65.369959
1543.806140	13.534813	65.374964
1542.688533	19.451560	65.379969
1541.656312	4.679616	65.384974
1540.932769	10.609441	65.389978
1540.821733	9.689012	65.394983
1540.530849	1.474923	65.399988
1539.300808	13.534793	65.404993
1538.882017	17.388110	65.409998
1538.265750	12.558027	65.415002
1537.469914	14.386397	65.420007
1536.240285	15.244423	65.425012
1535.586719	14.487480	65.430017
1535.370234	9.723190	65.435022
1534.751078	10.542560	65.440026
1534.041181	14.584069	65.445031
1533.810431	5.832111	65.450036
1532.628394	18.936252	65.455041
1532.545756	-0.020671	65.460046
1531.521206	6.792822	65.465050
1530.681017	5.311707	65.470055
1530.114059	-1.734072	65.475060
1528.933540	10.363665	65.480065
1529.009080	4.037428	65.485070
1528.238158	3.789599	65.490074
1527.273027	4.299650	65.495079
1526.822857	6.415312	65.500084
1526.201678	5.984406	65.505089
1525.860380	8.633159	65.510094
1524.639025	7.095914	65.515098
1524.050582	8.910256	65.520103
1523.629973	4.343996	65.525108
1522.782500	8.971952	65.530113
1522.554757	0.687905	65.535118
1521.067890	1.837566	65.540122
1520.448259	9.714308	65.545127
1520.368830	-2.228403	65.550132
1519.776176	4.743555	65.555137
1519.150904	-2.553167	65.560142
1518.171208	3.259661	65.565146
1517.534082	2.069577	65.570151
1516.829365	-1.609387	65.575156
1516.260321	9.575849	65.580161
1515.630918	4.815676	65.585166
1514.523633	6.037492	65.590170
1513.935346	5.804801	65.595175
1513.793278	12.596344	65.600180
1513.093590	8.194291	65.605185
1512.388521	5.083120	65.610190
1511.431207	13.891944	65.615194
1511.189483	6.214128	65.620199
1510.826251	8.431102	65.625204
1509.541462	12.661752	65.630209
1509.061519	0.653370	65.635214
1508.493827	6.712984	65.640218
1507.679552	8.006519	65.645223
1506.670312	3.753016	65.650228
1505.725132	14.838748	65.655233
1505.435610	5.921084	65.660238
1504.899635	12.022972	65.665242
1504.541794	3.598743	65.670247
1504.509835	0.915226	65.675252
1503.190265	11.101608	65.680257
1502.777395	8.014972	65.685262
1501.321786	7.689867	65.690266
1500.506462	3.142183	65.695271
1500.049009	10.176245	65.700276
1499.372790	12.148052	65.705281
1499.486399	8.681263	65.710286
1498.786345	8.062613	65.715290
1497.936961	7.690058	65.720295
1497.367522	4.601496	65.725300
1496.296605	15.240407	65.730305
1495.934808	4.727217	65.735310
1494.876685	15.975991	65.740314
1494.055380	17.423621	65.745319
1493.834883	10.718626	65.750324
1493.000135	15.062278	65.755329
1492.689212	7.392308	65.760334
1491.350200	21.603266	65.765338
1490.653082	16.593645	65.770343
1490.781963	11.829671	65.775348
1489.908931	15.520201	65.780353
1489.658170	9.729975	65.785358
1488.426842	15.027685	65.790362
1487.740233	7.229753	65.795367
1487.227196	9.267098	65.800372
1486.705249	16.066971	65.805377
1485.932873	9.626314	65.810382
1485.414529	12.847290	65.815386
1484.847584	17.914830	65.820391
1483.720278	11.749790	65.825396
1482.739480	13.976600	65.830401
1482.297117	12.589981	65.835406
1481.927024	5.336296	65.840410
1481.511913	10.731386	65.845415
1481.068696	13.142437	65.850420
1479.886713	14.953339	65.855425
1479.623100	7.436712	65.860430
1478.531511	13.390349	65.865434
1477.445650	1.935617	65.870439
1476.632163	11.664666	65.875444
1475.777080	11.387647	65.880449
1475.864921	8.232478	65.885454
1475.492085	13.275477	65.890458
1475.075525	9.033455	65.895463
1474.411123	10.134437	65.900468
1473.186606	12.800554	65.905473
1472.995014	9.167792	65.910478
1472.269642	12.147266	65.915482
1471.240297	14.388104	65.920487
1470.405845	13.488029	65.925492
1470.010003	4.095231	65.930497
1469.705103	8.600697	65.935502
1468.521418	8.762283	65.940506
1467.529258	14.629155	65.945511
1467.346378	10.291644	65.950516
1466.254068	22.471592	65.955521
1466.404889	13.770969	65.960526
1465.953813	15.673885	65.965530
1464.473323	14.288248	65.970535
1463.907283	7.499397	65.975540
1463.493911	9.090372	65.980545
1462.813440	4.656895	65.985550
1462.137980	10.736800	65.990554
1461.400901	8.441335	65.995559
1460.652932	3.927118	66.000564
1460.247631	13.901975	66.005569
1459.761808	4.190723	66.010574
1458.389253	11.012241	66.015578
1458.007680	10.011804	66.020583
1457.885186	2.832322	66.025588
1456.595731	9.853533	66.030593
1456.089131	8.548096	66.035598
1455.358405	17.896548	66.040602
1454.928511	12.101678	66.045607
1454.777620	11.750594	66.050612
1453.563454	12.718172	66.055617
1452.736202	3.561113	66.060622
1452.417840	14.786945	66.065626
1451.492481	13.229502	66.070631
1450.746138	16.314823	66.075636
1449.839987	19.998014	66.080641
1449.610036	4.630227	66.085646
1449.176888	12.529385	66.090650
1448.135500	5.806628	66.095655
1447.457420	12.839490	66.100660
1446.728143	13.192229	66.105665
1446.591359	7.084256	66.110670
1445.516144	9.826010	66.115674
1444.527393	15.760161	66.120679
1444.317384	5.763786	66.125684
1443.463453	15.267447	66.130689
1443.322998	7.236058	66.135694
1442.492449	11.900773	66.140698
1441.483118	14.097438	66.145703
1441.167062	1.895862	66.150708
1440.190302	16.542872	66.155713
1439.347714	5.150424	66.160718
1438.319609	10.239224	66.165722
1437.754954	20.856041	66.170727
1437.381788	12.817481	66.175732
1436.832170	16.257915	66.180737
1436.654588	10.818786	66.185742
1436.519363	16.716632	66.190746
1435.581139	17.957346	66.195751
1434.911045	7.986788	66.200756
1433.324403	16.274306	66.205761
1432.720836	15.358046	66.210766
1432.183273	6.799962	66.215770
1431.609093	12.538904	66.220775
1431.438032	4.094466	66.225780
1429.986450	17.484346	66.230785
1429.275584	9.422191	66.235790
1428.960892	7.676224	66.240794
1428.343730	8.665623	66.245799
1428.248751	9.136758	66.250804
1426.839085	13.357330	66.255809
1426.654005	4.945085	66.260814
1425.706910	12.235188	66.265818
1425.404227	19.763510	66.270823
1424.888683	14.080038	66.275828
1423.589824	11.460691	66.280833
1423.231286	1.284493	66.285838
1422.596694	13.118863	66.290842
1421.723126	12.007388	66.295847
1420.758639	5.761306	66.300852
1420.090079	14.166269	66.305857
1419.938469	13.088282	66.310862
1419.547156	15.144141	66.315866
1418.122071	4.793673	66.320871
1417.652740	4.633565	66.325876
1416.915299	6.977844	66.330881
1416.991814	7.204088	66.335886
1416.047818	14.886387	66.340890
1415.141819	11.807183	66.345895
1414.472268	4.905483	66.350900
1413.837699	10.523132	66.355905
1413.613712	-0.062404	66.360910
1412.456843	7.592225	66.365914
1411.239279	14.250349	66.370919
1411.053325	3.450596	66.375924
1410.565740	10.393256	66.380929
1410.237648	5.925862	66.385934
1409.375277	13.546300	66.390938
1408.493508	10.631991	66.395943
1408.292040	10.864572	66.400948
1407.246153	23.264253	66.405953
1406.310778	12.365985	66.410958
1405.262077	12.204927	66.415962
1405.315823	20.091357	66.420967
1404.499407	16.777130	66.425972
1404.250759	14.254223	66.430977
1403.622675	6.371319	66.435982
1402.439647	7.611531	66.440986
1401.794711	15.290454	66.445991
1401.661608	13.654407	66.450996
1400.802295	12.353005	66.456001
1399.981434	5.830197	66.461006
1398.965265	13.224334	66.466010
1398.425648	12.342075	66.471015
1398.330658	14.107969	66.476020
1397.393057	13.533415	66.481025
1396.744248	13.389224	66.486030
1395.752639	13.553428	66.491034
1395.177011	12.347292	66.496039
1395.323465	9.531333	66.501044
1394.118566	16.561211	66.506049
1393.257494	8.634917	66.511054
1392.949453	14.400950	66.516058
1392.274771	17.927509	66.521063
1391.000259	12.555515	66.526068
1390.509331	20.298276	66.531073
1389.894916	7.393461	66.536078
1389.505169	10.944115	66.541082
1389.227894	12.532392	66.546087
1388.363505	12.170144	66.551092
1387.489954	17.589232	66.556097
1386.980346	10.605340	66.561102
1385.665853	13.479776	66.566106
1385.184391	20.008284	66.571111
1384.601770	8.874172	66.576116
1383.746354	16.170217	66.581121
1383.667916	6.597666	66.586126
1383.190846	14.592127	66.591130
1382.418981	13.839836	66.596135
1381.482043	3.686202	66.601140
1380.874165	15.246657	66.606145
1380.417012	9.922945	66.611150
1379.397580	18.727490	66.616154
1378.492400	15.381648	66.621159
1378.194428	10.307038	66.626164
1377.706863	16.763971	66.631169
1376.999902	15.033058	66.636174
1375.780179	17.308927	66.641178
1375.436360	14.958857	66.646183
1375.200013	6.351330	66.651188
1374.275429	14.979938	66.656193
1373.625965	6.005972	66.661198
1372.625060	11.763870	66.666202
1372.188375	16.014313	66.671207
1372.048232	9.493695	66.676212
1370.940994	16.063331	66.681217
1369.811217	10.012290	66.686222
1369.606339	10.504051	66.691226
1368.995235	12.058661	66.696231
1368.742821	9.097939	66.701236
1367.702575	16.503800	66.706241
1366.875904	7.846606	66.711246
1366.274757	15.539076	66.716250
1365.736784	18.589719	66.721255
1364.735504	13.149071	66.726260
1363.597670	23.122112	66.731265
1363.746567	18.429075	66.736270
1363.271618	18.318759	66.741274
1363.053120	20.124790	66.746279
1361.855969	16.448455	66.751284
1361.066544	20.021649	66.756289
1360.735109	21.418254	66.761294
1359.659499	21.365578	66.766298
1358.714684	7.779971	66.771303
1358.240503	10.899325	66.776308
1357.754209	16.780436	66.781313
1357.409406	12.867673	66.786318
1356.198152	19.404963	66.791322
1355.271943	19.453124	66.796327
1354.722076	19.379952	66.801332
1354.522032	18.194545	66.806337
1354.339119	13.506948	66.811342
1352.999632	17.904071	66.816346
1352.130333	30.927020	66.821351
1351.962578	18.870620	66.826356
1351.495503	24.354419	66.831361
1350.680284	16.575399	66.836366
1349.660388	17.669845	66.841370
1348.873000	22.624212	66.846375
1348.817945	18.195425	66.851380
1347.425351	25.173159	66.856385
1346.918186	17.203232	66.861390
1346.320574	22.785058	66.866394
1345.640166	23.469122	66.871399
1345.541152	17.039743	66.876404
1344.428249	26.890551	66.881409
1343.900013	15.935470	66.886414
1343.213232	20.055356	66.891418
1342.539978	16.158539	66.896423
1342.224336	10.530048	66.901428
1341.402107	18.442185	66.906433
1340.803758	14.572887	66.911438
1340.043325	17.427074	66.916442
1339.166451	22.712657	66.921447
1338.294848	18.148743	66.926452
1337.586926	27.525137	66.931457
1337.388838	9.067604	66.936462
1336.889817	13.758494	66.941466
1335.735890	18.514077	66.946471
1335.050134	21.763272	66.951476
1334.402878	20.942297	66.956481
1334.410600	14.327207	66.961486
1333.457536	14.119433	66.966490
1332.360442	19.490493	66.971495
1331.967454	9.479072	66.976500
1331.354587	13.948351	66.981505
1331.135875	8.045817	66.986510
1329.710231	14.845871	66.991514
1329.112517	12.585063	66.996519
1328.510635	16.640988	67.001524
1328.014135	18.806629	67.006529
1327.689552	8.689711	67.011534
1326.346463	14.555647	67.016538
1325.860246	8.634138	67.021543
1325.568826	19.991317	67.026548
1324.942653	16.601137	67.031553
1324.283021	14.022149	67.036558
1323.411907	16.337240	67.041562
1322.909134	14.315244	67.046567
1322.116647	13.498437	67.051572
1320.823842	19.332728	67.056577
1320.464515	16.362199	67.061582
1319.612311	16.251942	67.066586
1319.387566	18.270293	67.071591
1319.004525	15.068555	67.076596
1318.258491	18.731061	67.081601
1317.515706	11.863113	67.086606
1316.663541	16.709507	67.091610
1316.373755	16.888324	67.096615
1316.277658	10.437985	67.101620
1314.909327	11.062686	67.106625
1314.706052	3.009765	67.111630
1313.294768	5.137912	67.116634
1312.341368	19.369630	67.121639
1312.037643	12.622700	67.126644
1311.592905	16.259382	67.131649
1310.905544	9.023059	67.136654
1309.669564	13.088335	67.141658
1309.070976	7.913292	67.146663
1308.999871	8.498913	67.151668
1308.152390	13.183705	67.156673
1307.959145	15.512457	67.161678
1307.020276	20.875718	67.166682
1305.993519	12.262976	67.171687
1305.672382	11.965779	67.176692
1304.550998	14.557224	67.181697
1304.290527	10.262034	67.186702
1303.258487	23.400753	67.191706
1302.460378	17.550914	67.196711
1302.019915	11.014973	67.201716
1301.629015	24.780350	67.206721
1301.622913	19.780777	67.211726
1300.410183	17.420630	67.216730
1299.569991	18.620572	67.221735
1299.416037	1.963337	67.226740
1297.949525	17.544583	67.231745
1297.411089	13.579034	67.236750
1296.862223	22.926989	67.241754
1296.145404	14.919445	67.246759
1296.059094	19.847516	67.251764
1294.775796	20.360930	67.256769
1294.205800	21.838054	67.261774
1293.396142	18.600067	67.266778
1293.083921	24.789423	67.271783
1292.867706	22.674558	67.276788
1291.645460	19.883817	67.281793
1291.304915	15.375842	67.286798
1290.551222	18.391407	67.291802
1289.824035	16.165388	67.296807
1288.997436	14.943984	67.301812
1287.872553	19.918910	67.306817
1287.748943	13.414597	67.311822
1286.987759	19.703724	67.316826
1286.313561	21.381932	67.321831
1285.825931	17.810453	67.326836
1284.942881	14.875892	67.331841
1284.528093	14.407498	67.336846
1283.889382	19.689922	67.341850
1282.726798	13.271957	67.346855
1282.458894	13.442567	67.351860
1281.783834	16.458247	67.356865
1281.358512	14.509106	67.361870
1280.368585	16.455149	67.366874
1279.508758	22.646416	67.371879
1279.277863	19.117700	67.376884
1278.410273	20.251039	67.381889
1277.878991	14.286239	67.386894
1277.233499	21.783915	67.391898
1276.179719	11.426541	67.396903
1275.889027	10.610391	67.401908
1275.432909	22.933679	67.406913
1274.814724	13.383879	67.411918
1273.805178	15.202150	67.416922
1273.159523	23.597192	67.421927
1272.817458	7.745774	67.426932
1271.483462	11.836114	67.431937
1271.124839	9.859022	67.436942
1270.466009	8.935819	67.441946
1270.061868	16.710526	67.446951
1269.783081	9.719929	67.451956
1268.560135	18.261959	67.456961
1268.102207	18.401281	67.461966
1267.476063	14.104313	67.466970
1266.509530	9.423053	67.471975
1265.627894	12.632442	67.476980
1264.951159	21.423534	67.481985
1264.684115	12.238975	67.486990
1264.096344	20.881872	67.491994
1263.054712	14.708051	67.496999
1262.520434	10.254543	67.502004
1261.723399	21.200083	67.507009
1261.742374	13.116557	67.512014
1260.807971	17.782067	67.517018
1259.401432	14.150119	67.522023
1259.202016	12.840035	67.527028
1258.584911	16.098832	67.532033
1258.387666	13.995150	67.537038
1257.567116	17.596976	67.542042
1256.689783	18.110514	67.547047
1256.231926	11.342370	67.552052
1255.055837	21.367264	67.557057
1254.447643	13.645256	67.562062
1253.654172	22.998994	67.567066
1253.016673	18.550860	67.572071
1252.715123	17.428915	67.577076
1252.151838	23.328594	67.582081
1251.883460	13.708985	67.587086
1250.742472	18.596594	67.592090
1250.228772	19.183206	67.597095
1249.885290	9.305868	67.602100
1248.650434	17.453962	67.607105
1248.143439	13.502350	67.612110
1247.185113	10.921993	67.617114
1246.931429	11.462528	67.622119
1246.167325	5.053766	67.627124
1244.986643	7.205206	67.632129
1244.796300	1.528425	67.637134
1244.490140	9.912058	67.642138
1243.330263	9.853907	67.647143
1242.791428	8.678228	67.652148
1241.864368	13.000356	67.657153
1241.205849	9.318861	67.662158
1240.823720	7.548950	67.667162
1240.536231	8.845535	67.672167
1239.448454	4.918470	67.677172
1238.714251	18.080806	67.682177
1238.393806	5.126150	67.687182
1237.757032	17.755722	67.692186
1236.577763	7.900903	67.697191
1236.242390	11.338843	67.702196
1235.402693	13.607962	67.707201
1235.323953	6.497247	67.712206
1234.214463	19.949513	67.717210
1233.087491	18.771162	67.722215
1232.897846	7.699198	67.727220
1232.107143	15.532225	67.732225
1231.902894	11.010473	67.737230
1230.964798	14.711427	67.742234
1230.071734	23.727750	67.747239
1229.748664	16.026644	67.752244
1228.989305	22.511048	67.757249
1228.304500	13.255728	67.762254
1227.482054	16.876788	67.767258
1226.703278	11.045985	67.772263
1226.579143	13.523032	67.777268
1225.615796	13.785317	67.782273
1225.012315	8.461256	67.787278
1224.114487	10.419484	67.792282
1223.871816	11.161708	67.797287
1223.495007	14.489538	67.802292
1221.984550	14.949221	67.807297
1221.855789	13.848691	67.812302
1221.256834	20.386441	67.817306
1220.193803	14.085149	67.822311
1219.502120	5.967979	67.827316
1218.469644	21.313071	67.832321
1218.408227	7.287416	67.837326
1217.979958	15.077002	67.842330
1217.079476	20.500422	67.847335
1216.388485	10.112196	67.852340
1215.210925	15.384124	67.857345
1214.815550	5.127098	67.862350
1214.442006	7.905597	67.867354
1214.203214	9.650205	67.872359
1213.331582	7.537074	67.877364
1212.466266	16.425974	67.882369
1211.974632	3.105867	67.887374
1211.029370	10.386278	67.892378
1210.012816	11.044982	67.897383
1209.474611	12.845092	67.902388
1208.970196	14.545207	67.907393
1208.754976	8.003432	67.912398
1208.246787	15.425662	67.917402
1207.212187	12.925264	67.922407
1206.682661	0.969022	67.927412
1205.693011	15.118210	67.932417
1204.785081	4.529514	67.937422
1204.007026	18.980965	67.942426
1203.498788	10.301584	67.947431
1203.066586	13.524678	67.952436
1202.544990	13.253067	67.957441
1202.427469	10.102171	67.962446
1201.442748	13.712773	67.967450
1200.557205	10.989966	67.972455
1200.006301	17.755055	67.977460
1199.012005	19.077314	67.982465
1198.364437	10.942094	67.987470
1197.800725	15.319998	67.992474
1197.303561	17.310715	67.997479
1196.967942	8.178082	68.002484
1195.768303	17.240012	68.007489
1195.334633	4.655056	68.012494
1194.745000	14.058388	68.017498
1193.824972	15.053429	68.022503
1193.085353	7.492703	68.027508
1192.169681	11.871386	68.032513
1191.975471	7.802232	68.037518
1191.470295	8.258182	68.042522
1190.961927	7.320535	68.047527
1190.075119	7.236326	68.052532
1189.081416	5.896445	68.057537
1188.825488	3.764255	68.062542
1188.013880	9.376983	68.067546
1186.979604	7.855887	68.072551
1186.729627	10.419184	68.077556
1186.082734	18.169424	68.082561
1185.860080	1.764430	68.087566
1184.494874	4.535058	68.092570
1183.558916	7.338349	68.097575
1183.295279	5.689960	68.102580
1182.793558	11.546736	68.107585
1182.530875	-0.890354	68.112590
1181.652728	14.638365	68.117594
1180.458891	10.743965	68.122599
1180.070691	7.831674	68.127604
1179.300558	9.236566	68.132609
1178.719865	2.702460	68.137614
1177.603380	7.482112	68.142618
1177.027843	13.703887	68.147623
1177.082923	5.725023	68.152628
1176.222434	10.746252	68.157633
1175.839760	5.708807	68.162638
1174.893120	6.094616	68.167642
1174.333282	15.956864	68.172647
1173.523101	7.696122	68.177652
1172.384277	14.614647	68.182657
1172.015835	8.584554	68.187662
1171.255508	4.542361	68.192666
1171.021579	4.012103	68.197671
1170.473111	10.996015	68.202676
1169.303387	11.199675	68.207681
1168.802998	2.031755	68.212686
1168.164143	10.807369	68.217690
1167.489512	17.107989	68.222695
1166.351092	7.292448	68.227700
1165.742767	10.314887	68.232705
1165.696262	6.750554	68.237710
1165.117768	14.411064	68.242714
1164.355574	13.876512	68.247719
1163.597203	13.161569	68.252724
1162.830169	10.006742	68.257729
1162.824115	5.574910	68.262734
1161.681267	14.359721	68.267738
1160.718836	6.425992	68.272743
1160.282940	5.476824	68.277748
1159.646476	10.686367	68.282753
1158.996101	2.097424	68.287758
1158.290315	11.445113	68.292762
1157.423335	10.279065	68.297767
1157.052408	13.057155	68.302772
1156.310757	15.097804	68.307777
1155.311755	0.344456	68.312782
1154.937211	7.365364	68.317786
1154.313642	5.529785	68.322791
1154.009518	1.154826	68.327796
1153.055628	6.518942	68.332801
1152.249650	2.040867	68.337806
1151.669657	4.580959	68.342810
1151.017126	9.901874	68.347815
1149.903914	7.560671	68.352820
1149.141531	4.321527	68.357825
1148.920465	3.666216	68.362830
1148.231250	12.271639	68.367834
1147.732986	11.209383	68.372839
1147.543494	6.313114	68.377844
1146.365925	3.742439	68.382849
1145.895631	0.794325	68.387854
1145.076169	6.843576	68.392858
1144.425485	10.035193	68.397863
1143.406880	7.049704	68.402868
1142.524637	11.710108	68.407873
1142.164308	8.454326	68.412878
1141.923322	8.101822	68.417882
1141.403513	6.085731	68.422887
1140.748693	-1.245594	68.427892
1139.881419	12.521422	68.432897
1139.564922	7.009807	68.437902
1138.146706	19.153372	68.442906
1137.268677	10.004520	68.447911
1136.973020	5.934161	68.452916
1135.998872	14.763115	68.457921
1135.816433	6.680099	68.462926
1135.779586	9.671573	68.467930
1134.662033	5.993735	68.472935
1133.802838	13.180051	68.477940
1133.243260	11.058316	68.482945
1132.929417	2.171411	68.487950
1131.785949	11.014680	68.492954
1131.000079	12.996133	68.497959
1130.751740	6.376057	68.502964
1129.676176	12.622177	68.507969
1129.352366	7.640036	68.512974
1128.579216	8.428800	68.517978
1128.041336	14.562586	68.522983
1127.583442	3.506506	68.527988
1125.961973	11.802878	68.532993
1125.285869	3.202268	68.537998
1125.012504	9.607810	68.543002
1125.101464	6.313684	68.548007
1124.575826	6.373911	68.553012
1123.515344	7.897547	68.558017
1122.996572	3.167206	68.563022
1121.498465	9.575163	68.568026
1120.521406	10.520950	68.573031
1120.330141	5.255939	68.578036
1119.360861	13.730865	68.583041
1119.473333	1.584218	68.588046
1118.780426	10.393670	68.593050
1118.313626	12.254983	68.598055
1117.516066	2.172353	68.603060
1116.900356	5.492460	68.608065
1116.610745	6.026105	68.613070
1115.054173	11.452984	68.618074
1114.246122	3.595652	68.623079
1114.069708	-0.496823	68.628084
1113.357320	9.227259	68.633089
1113.028410	0.822177	68.638094
1111.946591	8.654223	68.643098
1111.676114	9.476578	68.648103
1110.953921	1.074129	68.653108
1109.514840	6.657371	68.658113
1109.000382	7.300905	68.663118
1108.293857	9.424293	68.668122
1107.802418	8.819879	68.673127
1107.698292	2.307763	68.678132
1107.111413	14.311210	68.683137
1106.433204	2.187830	68.688142
1105.642705	10.151745	68.693146
1104.735145	17.411999	68.698151
1103.943489	4.727890	68.703156
1103.170263	9.577555	68.708161
1102.651601	2.927942	68.713166
1102.092887	11.512613	68.718170
1101.597854	9.538324	68.723175
1101.214726	-1.975941	68.728180
1099.995101	11.194237	68.733185
1099.696661	2.121953	68.738190
1099.058339	2.463476	68.743194
1097.660175	10.361621	68.748199
1097.059249	3.242521	68.753204
1096.161388	8.343839	68.758209
1096.115951	6.312224	68.763214
1095.658805	7.978029	68.768218
1095.452314	13.382553	68.773223
1094.740431	5.672365	68.778228
1093.763668	15.787036	68.783233
1092.854994	8.041917	68.788238
1091.720886	3.813192	68.793242
1090.999126	9.851647	68.798247
1090.611657	11.809161	68.803252
1090.408190	20.113387	68.808257
1090.004322	9.564412	68.813262
1089.131169	16.517982	68.818266
1088.152405	6.066772	68.823271
1087.661410	5.519066	68.828276
1086.942040	12.948093	68.833281
1086.537214	8.846220	68.838286
1085.585549	4.678368	68.843290
1084.945730	9.874265	68.848295
1084.868445	8.789211	68.853300
1083.624494	17.941815	68.858305
1083.064928	10.500728	68.863310
1082.397118	18.282699	68.868314
1081.630895	5.228680	68.873319
1080.732841	3.922515	68.878324
1080.133558	10.610155	68.883329
1079.796577	3.346563	68.888334
1079.141003	21.870973	68.893338
1078.094363	11.652925	68.898343
1077.532931	8.317177	68.903348
1076.863806	8.794501	68.908353
1076.765841	-0.169313	68.913358
1075.968165	13.938325	68.918362
1074.887335	9.492962	68.923367
1074.217782	11.881728	68.928372
1073.885158	10.488769	68.933377
1073.139074	8.078157	68.938382
1072.242665	9.963665	68.943386
1071.268568	8.803649	68.948391
1071.278960	7.475977	68.953396
1070.549158	4.069241	68.958401
1069.766659	5.192264	68.963406
1068.640342	8.115769	68.968410
1068.081461	9.064439	68.973415
1068.055320	10.179107	68.978420
1067.325515	13.649848	68.983425
1066.836371	2.936245	68.988430
1065.904951	11.244304	68.993434
1065.212185	5.918726	68.998439
1064.731242	12.669549	69.003444
1063.433611	10.677863	69.008449
1062.994053	4.528215	69.013454
1062.357500	4.308039	69.018458
1061.956695	3.559899	69.023463
1061.385742	2.920834	69.028468
1060.236936	16.365207	69.033473
1059.494267	12.001679	69.038478
1059.070400	13.840401	69.043482
1058.803880	17.535503	69.048487
1058.346396	11.183689	69.053492
1056.663591	9.043539	69.058497
1056.775130	3.842333	69.063502
1056.050174	-6.169810	69.068506
1055.137450	5.040181	69.073511
1054.373223	2.258704	69.078516
1053.487181	7.911695	69.083521
1053.573778	5.021668	69.088526
1052.981282	4.087971	69.093530
1051.994542	10.460344	69.098535
1051.388147	1.965373	69.103540
1050.353756	1.508856	69.108545
1049.992373	3.943221	69.113550
1048.915818	16.352605	69.118554
1048.113161	8.366698	69.123559
1047.885185	0.371374	69.128564
1047.367485	11.245697	69.133569
1047.409122	6.142349	69.138574
1046.030052	12.643378	69.143578
1044.943889	6.046218	69.148583
1044.710089	-1.828322	69.153588
1043.986857	13.647386	69.158593
1043.709438	7.137613	69.163598
1042.318826	8.776886	69.168602
1041.602959	9.379933	69.173607
1041.279224	6.460566	69.178612
1040.920884	13.032605	69.183617
1040.360135	11.999237	69.188622
1039.616417	3.781597	69.193626
1038.904077	7.773143	69.198631
1037.929672	-0.038764	69.203636
1036.656259	11.435213	69.208641
1036.436993	5.207942	69.213646
1035.997838	6.667456	69.218650
1035.849747	12.710853	69.223655
1035.450622	7.665014	69.228660
1034.327401	14.399749	69.233665
1033.598529	6.140322	69.238670
1032.965782	10.313183	69.243674
1031.414782	15.534208	69.248679
1031.119891	6.909250	69.253684
1030.491010	10.218856	69.258689
1030.274824	4.940475	69.263694
1029.967969	13.824149	69.268698
1028.945251	10.855134	69.273703
1028.232740	10.829989	69.278708
1027.478611	15.373844	69.283713
1026.807040	6.225314	69.288718
1025.689735	12.814023	69.293722
1025.083877	10.523050	69.298727
1024.695147	14.664974	69.303732
1024.208662	21.307871	69.308737
1023.801999	11.552610	69.313742
1022.615666	16.356054	69.318746
1021.988869	22.787874	69.323751
1021.725527	13.683206	69.328756
1021.069586	16.364727	69.333761
1020.808378	7.764376	69.338766
1019.697375	4.252718	69.343770
1018.787821	12.879028	69.348775
1018.215426	9.712206	69.353780
1017.110018	13.310534	69.358785
1016.576637	10.777784	69.363790
1015.820592	12.095322	69.368794
1015.583397	10.684033	69.373799
1015.245908	7.539765	69.378804
1014.855640	14.673581	69.383809
1014.016246	6.023292	69.388814
1012.929892	17.513255	69.393818
1012.247351	12.648139	69.398823
1011.405370	4.208011	69.403828
1010.579837	13.164749	69.408833
1010.175462	11.825795	69.413838
1009.791241	11.063985	69.418842
1009.209735	17.401862	69.423847
1008.430364	11.189590	69.428852
1007.190322	21.033925	69.433857
1007.292110	11.885358	69.438862
1006.459378	16.230402	69.443866
1005.564176	7.595305	69.448871
1005.064225	-0.724187	69.453876
1003.993023	13.422252	69.458881
1003.773864	4.001463	69.463886
1003.406077	7.608594	69.468890
1002.507831	7.348066	69.473895
1001.620003	6.865095	69.478900
1001.049756	10.504441	69.483905
1000.643195	7.543062	69.488910
999.400431	10.415735	69.493914
998.646084	9.924143	69.498919
998.501658	7.361050	69.503924
998.020996	12.783968	69.508929
997.454528	6.364352	69.513934
996.135632	6.423085	69.518938
995.519305	14.587983	69.523943
995.249655	-1.057229	69.528948
994.618151	10.201079	69.533953
993.726167	2.404463	69.538958
992.800672	4.950673	69.543962
992.208787	5.967692	69.548967
992.123806	-1.419558	69.553972
991.298438	4.968157	69.558977
990.465547	13.430881	69.563982
989.996943	8.713092	69.568986
989.354355	8.181641	69.573991
988.865023	3.147013	69.578996
987.627067	10.713772	69.584001
987.367933	1.554830	69.589006
986.826306	10.442741	69.594010
985.626609	11.080211	69.599015
984.856423	1.726605	69.604020
984.097096	10.764281	69.609025
984.004566	14.822807	69.614030
983.502894	14.204277	69.619034
983.128589	20.302596	69.624039
982.091752	14.356819	69.629044
981.036969	16.951994	69.634049
980.578525	3.730769	69.639054
979.822888	10.944803	69.644058
978.901875	13.681128	69.649063
978.776449	16.577879	69.654068
978.230352	14.247445	69.659073
977.803717	13.807797	69.664078
976.500706	14.958478	69.669082
975.556213	8.515437	69.674087
975.456176	8.405464	69.679092
974.507395	9.714257	69.684097
973.651881	10.303272	69.689102
973.121532	17.112434	69.694106
972.755696	24.105167	69.699111
972.765477	6.277022	69.704116
971.389136	15.966427	69.709121
970.872429	2.741861	69.714126
970.417370	13.055838	69.719130
969.149851	2.833575	69.724135
968.485162	4.832063	69.729140
967.630437	11.746459	69.734145
967.452182	8.860727	69.739150
967.112393	8.755788	69.744154
965.702990	10.775005	69.749159
965.133287	3.236217	69.754164
964.306006	17.738116	69.759169
964.152093	15.920897	69.764174
963.700903	11.697110	69.769178
962.766031	17.553454	69.774183
962.308838	11.859244	69.779188
960.979402	20.921416	69.784193
961.191487	16.281405	69.789198
960.273419	14.117405	69.794202
959.168441	14.020684	69.799207
958.630412	8.913381	69.804212
958.060264	14.531905	69.809217
957.889854	6.620478	69.814222
957.005288	17.794480	69.819226
955.987580	8.660052	69.824231
955.757189	8.288534	69.829236
954.765466	21.372038	69.834241
953.545437	12.179914	69.839246
953.140608	13.022088	69.844250
952.547943	19.828554	69.849255
952.460340	7.745296	69.854260
951.749365	19.041494	69.859265
951.457988	11.570386	69.864270
950.463188	16.300801	69.869274
949.802434	15.581430	69.874279
948.973378	4.918799	69.879284
947.789968	8.733004	69.884289
947.515889	4.296525	69.889294
946.829950	6.929216	69.894298
946.281796	11.014512	69.899303
946.025235	4.296423	69.904308
945.058332	11.594550	69.909313
944.665814	4.395022	69.914318
943.193821	16.384790	69.919322
942.409643	8.684584	69.924327
942.180229	7.488120	69.929332
941.744771	9.388632	69.934337
941.636651	5.392546	69.939342
940.190270	5.365934	69.944346
939.181971	13.878662	69.949351
939.013087	6.801250	69.954356
938.247001	10.903881	69.959361
937.805315	6.090353	69.964366
937.042183	13.190466	69.969370
936.100892	11.626292	69.974375
935.755434	-0.296066	69.979380
935.143409	8.590437	69.984385
934.156875	15.273493	69.989390
933.559504	11.918269	69.994394
932.725780	9.718780	69.999399
932.437275	8.528566	70.004404
932.031321	13.655737	70.009409
931.143839	13.945485	70.014414
930.130572	17.645886	70.019418
929.462492	18.843789	70.024423
929.592696	10.712627	70.029428
928.045671	19.095042	70.034433
927.514541	8.690952	70.039438
927.001209	14.231048	70.044442
926.632383	20.959317	70.049447
926.380782	11.133671	70.054452
925.010542	15.373457	70.059457
924.605705	10.134574	70.064462
924.010560	11.551118	70.069466
922.941051	15.353517	70.074471
922.431560	8.259345	70.079476
921.667057	12.587246	70.084481
921.274870	1.255831	70.089486
920.790303	1.798445	70.094490
919.850838	5.718927	70.099495
919.135479	8.980813	70.104500
918.259078	5.040763	70.109505
917.928368	-1.176635	70.114510
916.714853	5.119899	70.119514
915.771680	11.589467	70.124519
915.625219	-8.276551	70.129524
914.980726	5.164872	70.134529
914.951310	2.581906	70.139534
914.453047	-4.070897	70.144538
913.440242	0.977800	70.149543
912.900320	-5.969586	70.154548
912.258469	0.379479	70.159553
911.242016	4.761671	70.164558
910.259661	-3.339084	70.169562
909.556649	3.674188	70.174567
909.589422	-1.732109	70.179572
908.458667	4.254774	70.184577
907.745294	5.839956	70.189582
907.133806	9.121586	70.194586
906.444635	2.648984	70.199591
906.428972	-1.494282	70.204596
905.327527	8.618200	70.209601
904.667939	1.480112	70.214606
903.930749	6.850822	70.219610
903.434250	5.045552	70.224615
902.639198	7.943214	70.229620
901.830053	6.708126	70.234625
901.589815	3.362310	70.239630
900.870440	9.741067	70.244634
899.903532	-0.513223	70.249639
899.583217	3.698253	70.254644
898.992584	10.252073	70.259649
898.474593	6.843224	70.264654
897.259792	10.990471	70.269658
896.572904	9.213926	70.274663
896.277039	5.612021	70.279668
894.890550	12.533795	70.284673
894.204073	3.313567	70.289678
893.636230	7.700065	70.294682
893.206492	6.756274	70.299687
893.012701	-2.906658	70.304692
892.632935	10.584107	70.309697
891.833855	-7.676696	70.314702
890.931755	3.955865	70.319706
890.160453	14.492077	70.324711
889.083120	7.537179	70.329716
888.217486	11.192018	70.334721
887.586349	4.587176	70.339726
887.380262	5.484465	70.344730
886.757615	4.670732	70.349735
886.738368	0.367179	70.354740
885.658506	5.986407	70.359745
884.995739	2.562755	70.364750
884.705843	3.631087	70.369754
883.134508	7.942324	70.374759
882.220815	1.167980	70.379764
881.875874	12.290803	70.384769
881.445541	6.709040	70.389774
881.181515	-0.326408	70.394778
880.615898	-0.477399	70.399783
879.742187	-3.154653	70.404788
878.868088	18.386720	70.409793
878.331494	4.736396	70.414798
877.096848	5.026222	70.419802
876.425422	2.351466	70.424807
876.327103	-0.252071	70.429812
875.661325	8.412749	70.434817
875.340828	3.658800	70.439822
874.079999	10.713554	70.444826
873.284306	11.725190	70.449831
873.024799	8.432909	70.454836
872.100925	9.105382	70.459841
871.862152	-0.734902	70.464846
871.036776	-0.106493	70.469850
870.461374	0.333888	70.474855
869.914634	7.700785	70.479860
869.167741	7.536070	70.484865
868.232687	-4.651988	70.489870
867.400347	10.912071	70.494874
866.909416	3.354468	70.499879
866.975002	2.295572	70.504884
865.430860	11.081277	70.509889
864.946486	4.788991	70.514894
864.276155	7.379792	70.519898
863.785134	16.136657	70.524903
862.741217	6.098077	70.529908
861.755456	9.893476	70.534913
861.400688	9.253165	70.539918
861.099405	5.893415	70.544922
860.783426	-1.304080	70.549927
859.964243	5.577875	70.554932
858.689895	15.922913	70.559937
858.404497	12.743569	70.564942
858.265083	9.648229	70.569946
857.166986	10.285357	70.574951
856.604393	4.458134	70.579956
855.846770	10.713672	70.584961
855.009383	7.306783	70.589966
854.133693	7.870663	70.594970
853.568379	3.698186	70.599975
853.227746	1.562173	70.604980
852.911378	9.898555	70.609985
852.047474	3.811771	70.614990
851.193714	3.495329	70.619994
850.489310	11.199579	70.624999
849.814042	2.731408	70.630004
848.911195	8.443907	70.635009
848.394679	-1.889932	70.640014
847.886641	-3.313286	70.645018
847.387048	0.494622	70.650023
846.463637	-3.628736	70.655028
845.168523	7.288917	70.660033
844.994629	0.522995	70.665038
844.544022	-3.998913	70.670042
844.013307	0.370642	70.675047
843.824598	-1.347981	70.680052
842.562548	2.392049	70.685057
841.938157	2.658875	70.690062
841.469258	-2.098254	70.695066
840.150007	4.445390	70.700071
840.057493	-3.808013	70.705076
839.297731	4.580020	70.710081
838.702092	2.943518	70.715086
837.518274	4.431706	70.720090
836.981302	5.271276	70.725095
836.466545	-5.173229	70.730100
835.417593	8.884549	70.735105
835.344749	-1.201348	70.740110
834.907785	1.618830	70.745114
833.969774	1.719526	70.750119
833.637554	-2.526319	70.755124
832.790301	9.840313	70.760129
832.170218	-0.704129	70.765134
830.971310	2.603209	70.770138
830.580161	9.355534	70.775143
830.281735	-1.337885	70.780148
829.380301	1.802247	70.785153
828.687280	-4.467852	70.790158
827.752329	2.244871	70.795162
827.221584	1.783974	70.800167
826.845916	-8.690552	70.805172
825.895030	8.515151	70.810177
825.110811	3.120629	70.815182
824.602745	8.081128	70.820186
824.189321	6.977049	70.825191
824.041242	5.878043	70.830196
822.569908	0.135561	70.835201
822.237215	2.861868	70.840206
821.547253	0.708925	70.845210
820.639656	5.195253	70.850215
819.777521	-3.889742	70.855220
819.125771	7.537398	70.860225
818.772233	8.306769	70.865230
818.576349	6.325924	70.870234
817.192942	3.526391	70.875239
816.736226	-4.028756	70.880244
816.141158	5.421219	70.885249
815.725174	-1.708304	70.890254
814.963387	0.627392	70.895258
813.678555	-0.486208	70.900263
813.297314	1.266912	70.905268
812.789635	10.677747	70.910273
812.738123	3.707833	70.915278
811.780064	7.069886	70.920282
810.570698	3.498290	70.925287
810.238810	5.048002	70.930292
809.658555	10.114618	70.935297
809.025395	5.872524	70.940302
808.287128	8.663397	70.945306
807.554477	10.406224	70.950311
807.182994	-2.598533	70.955316
805.496955	10.931436	70.960321
805.308366	14.702461	70.965326
804.650574	10.533678	70.970330
804.319843	5.380803	70.975335
803.955218	-2.469713	70.980340
802.735854	6.103462	70.985345
802.334820	3.720016	70.990350
801.763910	2.133206	70.995354
801.308523	9.416181	71.000359
800.421714	-6.212729	71.005364
799.517693	8.594734	71.010369
799.326353	5.362578	71.015374
797.933485	2.897317	71.020378
796.941872	12.520819	71.025383
796.555871	0.433055	71.030388
796.004521	4.036311	71.035393
795.882283	11.668397	71.040398
795.484439	1.375608	71.045402
794.457628	10.306086	71.050407
793.775926	3.923801	71.055412
793.027020	8.045813	71.060417
792.647853	-3.196166	71.065422
791.763369	3.828671	71.070426
790.762632	11.190581	71.075431
790.388325	0.668531	71.080436
789.816755	10.717200	71.085441
789.010638	-5.298309	71.090446
788.365777	-4.094606	71.095450
787.841103	1.384230	71.100455
787.484608	5.510007	71.105460
786.274272	8.074824	71.110465
785.487470	-1.143581	71.115470
785.113283	2.464591	71.120474
784.796976	6.588701	71.125479
783.531916	-2.939937	71.130484
782.388646	-0.680702	71.135489
782.060958	3.303287	71.140494
781.933362	-7.641251	71.145498
781.324310	4.583381	71.150503
781.091613	0.067798	71.155508
779.894147	4.959850	71.160513
779.072764	-0.261571	71.165518
778.759245	-1.581829	71.170522
777.789099	1.810545	71.175527
776.928944	-4.278378	71.180532
776.480625	6.083422	71.185537
776.065987	-5.389460	71.190542
774.778094	4.268596	71.195546
773.886947	-0.802937	71.200551
773.636794	3.756943	71.205556
773.323781	9.763512	71.210561
773.015437	4.968220	71.215566
772.117225	-1.182456	71.220570
770.998352	8.977002	71.225575
770.682900	-9.264532	71.230580
770.198685	1.475160	71.235585
769.313886	4.221558	71.240590
768.634070	-4.209583	71.245594
767.623821	7.255714	71.250599
767.529532	-0.715109	71.255604
766.463011	3.473245	71.260609
765.566779	-2.509000	71.265614
765.309373	0.019237	71.270618
764.792775	3.328368	71.275623
764.291019	-3.423191	71.280628
762.999895	3.839869	71.285633
762.391734	1.793774	71.290638
761.940412	9.943476	71.295642
761.740615	-3.996973	71.300647
760.717627	-4.833673	71.305652
759.839295	2.492985	71.310657
759.229658	-4.127851	71.315662
758.937878	8.263905	71.320666
757.930346	3.296067	71.325671
757.318058	8.779397	71.330676
756.555752	11.761779	71.335681
755.943630	1.476307	71.340686
755.821360	4.238509	71.345690
754.485304	3.926343	71.350695
753.912812	3.790670	71.355700
753.541140	5.578547	71.360705
752.722833	0.280949	71.365710
751.719223	-4.972951	71.370714
750.746637	8.612197	71.375719
750.467971	4.887722	71.380724
749.937261	2.957040	71.385729
749.927643	7.078059	71.390734
749.186688	4.477492	71.395738
748.180716	4.704164	71.400743
747.801070	-0.034035	71.405748
746.505834	11.826746	71.410753
745.811573	-3.738172	71.415758
745.238044	-1.626405	71.420762
744.639412	10.576076	71.425767
744.910849	4.953580	71.430772
743.175721	0.839647	71.435777
742.801515	4.026758	71.440782
742.092903	8.992390	71.445786
741.438101	6.335528	71.450791
741.214842	0.044284	71.455796
740.067551	5.814658	71.460801
739.227902	3.165150	71.465806
738.770313	11.607603	71.470810
738.420050	8.965336	71.475815
737.758978	0.308857	71.480820
737.082186	14.234868	71.485825
736.167003	4.341448	71.490830
735.750627	6.866612	71.495834
734.275369	2.271316	71.500839
733.948153	0.743499	71.505844
733.336510	-0.800536	71.510849
732.791207	1.469175	71.515854
732.624075	-2.282516	71.520858
731.234753	9.519129	71.525863
730.833347	3.044927	71.530868
729.966571	2.460926	71.535873
729.563861	5.420754	71.540878
729.168200	2.669017	71.545882
728.466977	0.270300	71.550887
727.650856	1.200073	71.555892
726.837393	11.148485	71.560897
726.622269	3.744136	71.565902
725.790459	-0.723358	71.570906
724.897559	4.169111	71.575911
724.188740	9.585812	71.580916
723.880316	6.321842	71.585921
722.800420	5.199314	71.590926
721.976834	1.345555	71.595930
721.307926	0.955568	71.600935
720.950108	7.964381	71.605940
720.765941	13.278622	71.610945
719.976522	9.832605	71.615950
718.733694	4.769779	71.620954
718.193377	7.022929	71.625959
717.910371	3.143024	71.630964
717.031357	8.183104	71.635969
716.481847	7.610095	71.640974
715.725775	10.178312	71.645978
715.272069	3.540544	71.650983
714.841930	9.005918	71.655988
713.332223	9.134608	71.660993
713.263329	13.039549	71.665998
712.977453	7.936322	71.671002
711.613058	13.309171	71.676007
710.956021	8.668764	71.681012
710.300954	12.845246	71.686017
710.053263	11.984471	71.691022
709.242591	4.820040	71.696026
708.147408	7.786049	71.701031
707.768288	6.141914	71.706036
707.073115	7.779448	71.711041
706.953705	-1.177745	71.716046
705.842621	12.248112	71.721050
704.991349	13.864769	71.726055
704.631408	14.838612	71.731060
703.891086	6.057559	71.736065
702.950992	-1.147763	71.741070
702.014045	1.789897	71.746074
701.217460	9.362190	71.751079
701.325004	0.493445	71.756084
700.682249	12.780232	71.761089
700.143079	7.193764	71.766094
699.026125	4.140549	71.771098
698.673864	5.299260	71.776103
698.362833	3.587512	71.781108
697.258018	15.067892	71.786113
696.471987	7.932659	71.791118
696.118547	9.023746	71.796122
695.354693	14.237895	71.801127
695.180828	1.512376	71.806132
693.540714	12.063960	71.811137
693.383623	8.070963	71.816142
692.595177	7.111784	71.821146
690.939814	9.774320	71.826151
690.900158	1.678105	71.831156
690.576432	-0.015849	71.836161
689.889650	3.935438	71.841166
689.411516	9.607164	71.846170
689.137648	7.492086	71.851175
688.347358	11.846232	71.856180
687.432981	13.636954	71.861185
686.975514	1.043334	71.866190
686.247594	5.274000	71.871194
684.965852	1.896932	71.876199
684.776248	-3.101763	71.881204
683.991129	15.802852	71.886209
683.507609	12.282903	71.891214
682.606869	10.220338	71.896218
681.484942	9.949811	71.901223
681.839760	5.066281	71.906228
680.995818	13.800511	71.911233
679.860846	3.517895	71.916238
679.226365	11.487025	71.921242
678.632593	13.026414	71.926247
678.638937	4.142243	71.931252
677.700945	7.048538	71.936257
676.750568	-1.688011	71.941262
676.091875	-0.463153	71.946266
674.952994	7.652533	71.951271
674.715613	3.680210	71.956276
673.763069	5.708838	71.961281
673.319733	4.051280	71.966286
672.988576	0.644276	71.971290
672.341580	17.069881	71.976295
671.624852	13.770008	71.981300
670.952313	11.180649	71.986305
670.755208	7.025284	71.991310
669.503143	12.900687	71.996314
668.319126	11.898847	72.001319
668.177401	8.874859	72.006324
667.404081	17.490610	72.011329
667.066252	13.662020	72.016334
665.948565	12.122890	72.021338
665.022655	17.955820	72.026343
664.614097	12.681314	72.031348
664.347871	15.199927	72.036353
663.950247	7.636982	72.041358
663.063770	10.224403	72.046362
662.113724	10.450089	72.051367
661.614931	5.361853	72.056372
660.893874	9.324915	72.061377
659.841270	14.763261	72.066382
659.400959	11.074003	72.071386
658.567895	10.358496	72.076391
658.197116	2.490067	72.081396
657.711673	18.158204	72.086401
657.329169	5.093734	72.091406
656.207055	6.657339	72.096410
655.060357	11.968738	72.101415
654.855992	6.434626	72.106420
654.423548	11.950840	72.111425
653.995682	5.567606	72.116430
653.004226	7.807453	72.121434
652.617985	10.977569	72.126439
652.113144	3.311849	72.131444
650.837255	12.024983	72.136449
650.162479	6.151026	72.141454
649.679777	0.951417	72.146458
649.110312	13.639722	72.151463
647.910168	6.307094	72.156468
647.246977	7.105299	72.161473
646.970552	12.095171	72.166478
646.638687	11.097990	72.171482
645.992480	14.099762	72.176487
645.300278	6.116933	72.181492
644.523756	12.328220	72.186497
644.247933	7.105126	72.191502
643.259632	-0.915702	72.196506
642.100667	10.732596	72.201511
641.887216	8.445468	72.206516
641.102194	5.222718	72.211521
640.259191	0.495252	72.216526
639.245227	9.682366	72.221530
638.519361	11.179719	72.226535
638.703925	-3.992072	72.231540
638.325080	2.304121	72.236545
637.223815	2.918193	72.241550
636.624077	5.701243	72.246554
635.936964	3.111063	72.251559
635.614148	5.198696	72.256564
634.324174	10.039309	72.261569
633.442163	8.628249	72.266574
633.087761	9.558640	72.271578
632.637571	4.833274	72.276583
631.620306	4.831545	72.281588
630.443492	14.505093	72.286593
630.093815	10.769866	72.291598
629.653685	4.467443	72.296602
629.374060	1.947993	72.301607
629.434743	0.710093	72.306612
628.128831	5.584786	72.311617
627.395468	5.498418	72.316622
626.990797	5.053757	72.321626
625.942391	8.242597	72.326631
625.376936	0.108699	72.331636
624.913110	3.671237	72.336641
623.707959	1.761261	72.341646
622.798300	1.390720	72.346650
622.034629	13.761433	72.351655
621.942864	3.369478	72.356660
621.581694	2.189302	72.361665
621.118480	3.602248	72.366670
619.956303	3.642527	72.371674
619.322256	5.159956	72.376679
619.062584	-5.842371	72.381684
617.490737	8.730850	72.386689
616.861836	5.573135	72.391694
616.596146	4.314671	72.396698
616.523900	1.582413	72.401703
615.757251	5.488088	72.406708
614.463516	14.443790	72.411713
614.039307	8.913156	72.416718
613.533902	-0.783679	72.421722
612.753646	5.149073	72.426727
611.834707	2.196834	72.431732
610.769462	12.459777	72.436737
610.687605	4.439680	72.441742
610.215671	6.710346	72.446746
609.825508	11.038634	72.451751
608.688026	7.928804	72.456756
607.588302	3.463022	72.461761
607.619193	-1.663826	72.466766
606.733252	7.480828	72.471770
606.046907	5.193325	72.476775
605.410939	0.412396	72.481780
604.585007	7.995694	72.486785
604.333821	6.512559	72.491790
603.458479	10.798268	72.496794
602.615412	6.515548	72.501799
601.840034	5.150597	72.506804
601.216828	-0.946030	72.511809
601.149651	3.543713	72.516814
599.985532	4.918480	72.521818
599.075839	2.354300	72.526823
598.639567	7.727619	72.531828
598.055688	7.207422	72.536833
597.928358	2.337598	72.541838
596.772044	4.335628	72.546842
595.708928	10.305553	72.551847
595.642683	3.461016	72.556852
595.007170	7.369466	72.561857
594.471033	-2.185265	72.566862
593.787750	1.525777	72.571866
592.805820	3.011885	72.576871
592.591763	-0.101504	72.581876
591.241062	8.022719	72.586881
590.565091	1.300531	72.591886
590.262416	-0.914028	72.596890
589.760139	7.114487	72.601895
589.376857	1.104234	72.606900
587.914087	9.104376	72.611905
587.481585	5.716681	72.616910
587.138804	-2.716034	72.621914
586.187894	3.327488	72.626919
585.732431	3.102247	72.631924
584.289950	5.852373	72.636929
584.372847	0.703049	72.641934
584.215434	-2.610182	72.646938
583.034396	1.042944	72.651943
582.245111	-5.757388	72.656948
581.543611	0.834641	72.661953
581.209580	-3.466066	72.666958
580.455782	5.455685	72.671962
579.420028	3.034601	72.676967
579.038763	0.214365	72.681972
578.342951	6.277185	72.686977
577.886578	0.026252	72.691982
576.896168	-0.356643	72.696986
576.376885	1.877413	72.701991
576.354397	-12.942823	72.706996
574.857440	2.402268	72.712001
574.039847	2.587965	72.717006
573.429907	7.596268	72.722010
572.982543	-1.114691	72.727015
572.841283	-4.692281	72.732020
571.458311	1.136200	72.737025
570.779334	-0.263019	72.742030
570.321219	-1.976552	72.747034
569.711876	4.633919	72.752039
569.645613	7.141188	72.757044
568.427082	4.523707	72.762049
567.953727	1.103098	72.767054
567.563401	0.895872	72.772058
565.998808	4.739418	72.777063
565.221495	-8.268432	72.782068
564.534557	5.540930	72.787073
564.192046	4.228473	72.792078
564.152079	4.731877	72.797082
563.697322	10.368355	72.802087
563.323528	-0.603169	72.807092
561.998923	4.386502	72.812097
561.336627	-1.129846	72.817102
560.261450	-1.902952	72.822106
559.450592	4.334323	72.827111
559.429445	1.753210	72.832116
558.877677	1.827179	72.837121
558.321631	-2.775643	72.842126
557.391816	-2.344972	72.847130
556.392135	2.859462	72.852135
555.090366	-2.463554	72.857140
554.509836	-3.436881	72.862145
554.513094	0.418713	72.867150
553.819350	-2.668726	72.872154
553.102283	3.540994	72.877159
552.934055	3.645338	72.882164
552.235738	3.157575	72.887169
551.124801	7.681110	72.892174
550.550987	2.757827	72.897178
550.168441	9.442569	72.902183
549.394908	-2.334219	72.907188
548.262986	9.212026	72.912193
547.671496	8.144247	72.917198
547.077374	1.763868	72.922202
546.611058	0.813351	72.927207
546.398432	-0.636492	72.932212
545.200002	12.491074	72.937217
544.614803	-3.050124	72.942222
544.216630	6.251823	72.947226
543.701526	5.439973	72.952231
542.903617	-4.695969	72.957236
541.918431	6.610849	72.962241
541.348203	3.756062	72.967246
540.653818	1.119759	72.972250
539.487565	5.879203	72.977255
539.091885	-3.458176	72.982260
538.577842	7.794093	72.987265
538.283180	2.294885	72.992270
537.952022	9.925547	72.997274
536.814537	6.476691	73.002279
536.277163	-2.718261	73.007284
535.599748	4.939170	73.012289
534.807186	-0.824514	73.017294
534.314715	0.091612	73.022298
533.537714	3.626778	73.027303
532.999385	-5.342504	73.032308
531.807377	1.332405	73.037313
531.365018	-2.354919	73.042318
530.892131	7.971386	73.047322
530.144042	-2.505241	73.052327
529.294547	-0.089257	73.057332
528.737439	4.538458	73.062337
528.205796	12.131669	73.067342
527.867313	-1.346642	73.072346
526.588499	2.982860	73.077351
525.969117	-5.289076	73.082356
525.178131	-2.194826	73.087361
525.185500	1.011952	73.092366
524.744053	-4.643649	73.097370
523.638398	3.990373	73.102375
523.056165	-7.842106	73.107380
522.069316	8.057294	73.112385
520.840307	8.931476	73.117390
520.183663	-4.847823	73.122394
519.699500	8.979710	73.127399
519.450754	-7.744226	73.132404
518.952676	2.989809	73.137409
518.766964	-5.073653	73.142414
518.192615	3.420534	73.147418
517.121696	6.005844	73.152423
516.754532	-1.796889	73.157428
515.518579	9.049967	73.162433
514.521202	6.261658	73.167438
513.885304	5.737152	73.172442
513.543442	3.632931	73.177447
513.515808	-0.268699	73.182452
511.984084	5.539353	73.187457
511.564139	-2.250240	73.192462
511.128131	4.999712	73.197466
510.500038	8.791875	73.202471
509.849069	7.571146	73.207476
508.945526	5.889160	73.212481
508.480779	10.196222	73.217486
507.929676	2.132618	73.222490
506.762106	3.104257	73.227495
506.370040	3.316808	73.232500
505.393898	9.372263	73.237505
505.311800	-2.519389	73.242510
504.665613	-1.029963	73.247514
503.429325	12.346511	73.252519
502.840151	0.002603	73.257524
502.272409	1.064775	73.262529
501.903567	-1.033569	73.267534
500.946923	11.484606	73.272538
499.924039	10.925557	73.277543
499.856925	8.572552	73.282548
499.346929	12.052576	73.287553
498.502992	1.375175	73.292558
497.622142	8.817431	73.297562
496.939817	4.362481	73.302567
496.394352	5.186127	73.307572
495.961782	6.679373	73.312577
495.160127	3.260619	73.317582
494.166786	2.640093	73.322586
493.527361	-1.697104	73.327591
493.490464	1.623964	73.332596
492.882552	-0.862089	73.337601
491.760714	0.441333	73.342606
490.928293	0.282473	73.347610
490.576369	1.732908	73.352615
489.916029	1.213879	73.357620
488.625793	-0.173091	73.362625
488.290681	7.426660	73.367630
488.188545	5.456146	73.372634
487.347990	11.455312	73.377639
486.819397	-0.830428	73.382644
485.644222	3.255490	73.387649
485.205115	-2.651223	73.392654
484.693764	-1.375671	73.397658
483.966672	6.305455	73.402663
482.926759	1.986332	73.407668
482.158160	12.444916	73.412673
482.046760	0.963230	73.417678
481.800302	-1.763342	73.422682
480.417429	3.432780	73.427687
480.182205	-11.351970	73.432692
479.421060	-4.105414	73.437697
478.396767	0.193022	73.442702
477.553661	1.469389	73.447706
476.779904	6.150555	73.452711
476.706802	-1.987616	73.457716
476.016341	7.282052	73.462721
475.682944	3.033304	73.467726
474.736422	2.348553	73.472730
473.623931	7.067919	73.477735
473.479607	-5.963466	73.482740
472.840467	14.206344	73.487745
471.918519	-2.609032	73.492750
471.442574	-3.458646	73.497754
470.574673	1.360528	73.502759
470.272912	-4.937088	73.507764
469.455038	4.671440	73.512769
468.565196	2.465290	73.517774
467.831893	10.390273	73.522778
467.244817	2.537427	73.527783
466.882826	-3.600775	73.532788
465.385834	14.202969	73.537793
464.732957	1.320418	73.542798
464.325727	9.816376	73.547802
464.238642	7.999591	73.552807
464.351494	1.986015	73.557812
463.183098	13.446635	73.562817
462.306054	2.448081	73.567822
461.964174	5.524413	73.572826
460.651994	12.989671	73.577831
459.959101	4.374632	73.582836
459.252664	8.226599	73.587841
459.135985	7.871706	73.592846
457.939000	9.415786	73.597850
456.767443	12.731551	73.602855
456.701314	-2.234693	73.607860
455.881696	3.317997	73.612865
455.808659	0.677343	73.617870
455.319193	3.045449	73.622874
453.931614	8.956731	73.627879
453.627512	-7.990189	73.632884
452.888182	12.283897	73.637889
452.137115	10.684875	73.642894
451.186494	-4.615123	73.647898
450.599352	10.671803	73.652903
450.479289	-4.375735	73.657908
449.703440	3.705845	73.662913
449.028695	-3.196268	73.667918
447.914481	3.828997	73.672922
447.155947	9.867147	73.677927
447.092206	-2.513146	73.682932
446.441615	-5.091738	73.687937
445.366676	-1.149514	73.692942
445.008397	6.386118	73.697946
444.195289	-7.732510	73.702951
444.127522	-2.236534	73.707956
443.397040	2.229576	73.712961
442.729889	3.698703	73.717966
441.768724	-2.962218	73.722970
440.233205	-0.734956	73.727975
439.956042	-0.201642	73.732980
439.197139	3.981980	73.737985
439.143125	-7.016803	73.742990
438.717468	-3.332581	73.747994
437.207951	3.545930	73.752999
436.986895	0.253894	73.758004
436.175996	3.928536	73.763009
435.860694	-2.183982	73.768014
435.550826	-3.515812	73.773018
434.445773	-0.291065	73.778023
434.046511	1.841888	73.783028
433.102979	4.496825	73.788033
431.978530	-3.137911	73.793038
431.655380	-1.062820	73.798042
430.796816	-1.955543	73.803047
430.769101	-9.422814	73.808052
429.374972	4.308428	73.813057
428.377818	-5.305259	73.818062
427.927087	-12.530074	73.823066
427.388105	1.810840	73.828071
427.448141	-6.630826	73.833076
427.033058	-7.140028	73.838081
426.237141	-11.826021	73.843086
425.304109	-8.269120	73.848090
424.727135	-3.267622	73.853095
423.988697	-5.799091	73.858100
422.868347	2.154453	73.863105
422.479614	-4.179760	73.868110
421.892891	-6.074629	73.873114
420.646205	-5.565029	73.878119
419.754274	-4.744509	73.883124
419.414746	-4.453581	73.888129
418.845062	-6.742267	73.893134
418.847688	-9.989513	73.898138
418.514329	2.025638	73.903143
417.910874	-14.144975	73.908148
416.906137	-14.003526	73.913153
416.129767	-7.943610	73.918158
414.818811	-7.248715	73.923162
414.173727	-8.025632	73.928167
413.743686	-5.635448	73.933172
413.135931	3.947495	73.938177
412.877778	-1.934416	73.943182
411.616642	-6.667704	73.948186
410.990190	-3.437207	73.953191
410.532292	-13.343399	73.958196
410.118269	-10.424310	73.963201
409.599164	-9.988064	73.968206
408.505862	-10.002818	73.973210
407.819837	2.972168	73.978215
407.654206	-8.641211	73.983220
406.476522	-0.970276	73.988225
405.615713	-11.233331	73.993230
405.005303	-7.484970	73.998234
404.458734	0.519079	74.003239
404.405302	-10.099725	74.008244
403.024113	-3.801492	74.013249
402.648817	-10.584138	74.018254
402.396823	-11.518313	74.023258
401.279631	-3.128430	74.028263
400.770442	-17.046288	74.033268
399.568047	-2.818867	74.038273
399.394202	-8.165402	74.043278
399.333510	-5.302615	74.048282
398.096205	-0.732075	74.053287
397.390456	-6.113703	74.058292
396.720676	5.871479	74.063297
396.389458	-7.579560	74.068302
395.242283	-6.961220	74.073306
394.409950	-8.225556	74.078311
394.278148	-14.078706	74.083316
393.647181	-3.886488	74.088321
392.492178	-9.336878	74.093326
391.896511	-9.255875	74.098330
391.227545	-0.940569	74.103335
390.979888	-5.937858	74.108340
389.758471	-6.741202	74.113345
389.033961	-7.171124	74.118350
388.559316	-2.741040	74.123354
387.895179	2.616572	74.128359
387.986708	-5.867959	74.133364
386.791496	-0.496683	74.138369
385.869550	0.293937	74.143374
385.838304	-3.663882	74.148378
385.052226	-1.213801	74.153383
384.537330	-3.295158	74.158388
383.403903	-4.153523	74.163393
382.713016	-10.258215	74.168398
382.323592	-4.222105	74.173402
381.606609	1.347366	74.178407
380.579327	-9.784901	74.183412
379.642732	-9.032947	74.188417
379.410831	-5.660306	74.193422
379.196250	-1.276395	74.198426
378.281498	-2.636407	74.203431
377.589751	-12.353929	74.208436
376.857356	-8.171365	74.213441
376.509781	-7.294071	74.218446
375.756861	-5.451697	74.223450
374.643641	-2.750774	74.228455
374.371285	-3.106086	74.233460
373.908262	-8.777134	74.238465
372.706953	-8.229008	74.243470
372.000006	-7.879519	74.248474
371.061006	8.373429	74.253479
370.873611	-7.975446	74.258484
370.378596	-3.554729	74.263489
369.983515	-1.282079	74.268494
369.002729	-5.309356	74.273498
368.195067	-0.359397	74.278503
367.912408	-5.523000	74.283508
366.610321	-7.037331	74.288513
365.996296	-0.648441	74.293518
365.400098	-10.116247	74.298522
364.726136	1.626740	74.303527
364.849425	-9.168463	74.308532
363.975145	-4.196848	74.313537
363.249686	-4.839510	74.318542
362.494807	-9.828501	74.323546
361.816825	-0.642811	74.328551
360.909423	-3.054288	74.333556
360.050721	-3.066982	74.338561
359.661005	-0.206954	74.343566
359.236689	-4.374954	74.348570
358.543595	-6.330128	74.353575
357.727878	-10.757462	74.358580
356.861802	-2.664639	74.363585
356.761397	-8.344586	74.368590
355.864279	-7.087958	74.373594
354.360799	3.166050	74.378599
354.116506	-5.585094	74.383604
353.676891	1.067752	74.388609
353.359785	-5.735198	74.393614
353.127215	-5.617431	74.398618
351.790658	0.719449	74.403623
351.509922	3.221472	74.408628
350.580977	2.592319	74.413633
349.808915	2.070633	74.418638
348.948506	-2.064135	74.423642
348.040872	4.675921	74.428647
348.078915	-2.071663	74.433652
347.277012	4.247823	74.438657
346.325753	-2.780504	74.443662
345.874112	-3.878405	74.448666
345.685940	1.442784	74.453671
344.579081	1.685698	74.458676
344.112054	-5.814058	74.463681
343.310196	1.090497	74.468686
342.752463	-2.105288	74.473690
341.398044	3.581555	74.478695
340.823623	-5.897600	74.483700
340.228583	-1.471976	74.488705
339.812416	-2.414673	74.493710
339.539849	-11.632836	74.498714
338.503051	-4.149918	74.503719
337.875655	-3.937683	74.508724
337.278150	-1.329977	74.513729
336.875742	-6.386175	74.518734
336.342775	-9.913926	74.523738
335.145765	0.098848	74.528743
334.807335	-2.811752	74.533748
333.778639	-3.836604	74.538753
332.892297	-3.818074	74.543758
332.303352	-4.241199	74.548762
331.690766	-4.752025	74.553767
331.278999	-8.606612	74.558772
330.993370	-0.484862	74.563777
330.478888	-8.456466	74.568782
329.433322	2.508354	74.573786
328.583959	1.647318	74.578791
328.154921	-5.744942	74.583796
326.956317	10.505236	74.588801
326.396817	0.801342	74.593806
325.627426	-0.465118	74.598810
325.344004	6.188072	74.603815
325.314822	-6.445299	74.608820
324.061491	2.365301	74.613825
323.397752	-7.886548	74.618830
322.795128	-9.190626	74.623834
321.933948	-4.468679	74.628839
321.363871	-11.737525	74.633844
320.554836	-3.663247	74.638849
319.999105	-9.131839	74.643854
319.842125	-6.441372	74.648858
318.744404	1.942286	74.653863
317.819834	-8.074013	74.658868
317.268664	-0.006138	74.663873
316.649078	-2.811994	74.668878
316.118289	-5.805476	74.673882
315.493498	-4.431383	74.678887
314.609147	-7.868428	74.683892
313.530133	2.570270	74.688897
313.482363	-7.278260	74.693902
313.247737	-0.227554	74.698906
312.245141	2.786940	74.703911
311.503977	-9.553163	74.708916
310.961932	-2.270523	74.713921
310.477496	-7.980723	74.718926
309.855533	-11.472203	74.723930
308.613245	-3.082849	74.728935
308.374575	-12.798440	74.733940
307.686062	-8.302717	74.738945
306.498679	-3.831560	74.743950
305.932006	-11.826376	74.748954
305.435886	-5.997191	74.753959
305.158391	-13.213314	74.758964
304.435439	-9.133166	74.763969
303.350835	-6.198644	74.768974
302.684325	-10.241289	74.773978
302.092616	-5.660064	74.778983
302.086848	-7.948714	74.783988
301.229665	-1.038485	74.788993
300.427097	-5.059444	74.793998
299.921344	-8.746072	74.799002
298.976039	-2.009463	74.804007
298.055932	-11.775714	74.809012
297.161622	-8.619197	74.814017
296.963209	-10.586967	74.819022
296.750761	-1.811377	74.824026
295.476358	-4.009781	74.829031
295.065631	0.012718	74.834036
294.171811	3.692733	74.839041
293.908997	-12.112637	74.844046
292.533820	-12.623328	74.849050
292.039723	-0.500553	74.854055
291.684626	-2.135828	74.859060
291.175858	0.650141	74.864065
290.604296	-1.696563	74.869070
289.765670	-2.985093	74.874074
288.811758	5.757295	74.879079
288.514137	-8.052321	74.884084
288.178959	5.950175	74.889089
287.091338	-4.300331	74.894094
286.549938	-4.040287	74.899098
285.961315	7.733270	74.904103
284.801498	-2.661854	74.909108
283.536728	2.376764	74.914113
283.044615	-3.313283	74.919118
282.975293	-4.008468	74.924122
282.366966	4.216766	74.929127
282.032100	-3.893848	74.934132
281.688131	-1.925814	74.939137
280.481399	-3.076812	74.944142
279.679761	3.438199	74.949146
279.245858	4.272495	74.954151
278.833544	-11.509041	74.959156
277.682047	6.433672	74.964161
277.075202	-2.406331	74.969166
276.637777	-3.649993	74.974170
275.964398	-0.799934	74.979175
275.247365	-9.787955	74.984180
274.343699	-10.798016	74.989185
273.744018	-14.996390	74.994190
273.377380	-12.690414	74.999194
272.198205	-5.350366	75.004199
271.879211	-9.620293	75.009204
271.419755	-2.834961	75.014209
270.755286	-0.448388	75.019214
269.788337	-8.887190	75.024218
268.696347	-9.200148	75.029223
268.505424	-1.408899	75.034228
267.996561	-10.106810	75.039233
267.525187	-14.333521	75.044238
266.599451	-3.487141	75.049242
265.929013	-11.206772	75.054247
265.579783	-9.870285	75.059252
264.541019	-14.654705	75.064257
263.491242	-8.309883	75.069262
263.131523	-12.731019	75.074266
262.468531	-3.238606	75.079271
262.205810	-7.949607	75.084276
261.498592	1.720177	75.089281
260.792200	-4.708447	75.094286
260.318358	-5.156212	75.099290
259.348494	-2.258885	75.104295
258.609571	-7.034330	75.109300
257.711440	-3.266882	75.114305
257.120375	-5.555272	75.119310
256.827737	-14.429578	75.124314
256.161985	-8.136510	75.129319
255.349374	-10.151451	75.134324
254.347944	2.876989	75.139329
254.366929	-2.257407	75.144334
253.628924	-6.525194	75.149338
252.239024	-4.533931	75.154343
252.020352	-12.216758	75.159348
251.395479	-5.323050	75.164353
251.100944	-2.640615	75.169358
250.498112	-1.908701	75.174362
249.499904	-1.752454	75.179367
248.845940	-3.363734	75.184372
247.536234	0.956631	75.189377
246.565169	-4.090900	75.194382
246.619461	-8.885553	75.199386
245.903004	1.291932	75.204391
245.832853	-6.163827	75.209396
244.914712	-1.035366	75.214401
244.641843	-2.075010	75.219406
243.648026	-5.414148	75.224410
242.830860	-2.271487	75.229415
242.353340	-5.096816	75.234420
241.128740	-0.924062	75.239425
240.573028	1.497222	75.244430
240.002958	-0.313519	75.249434
239.272873	-0.993255	75.254439
239.227953	-7.069984	75.259444
238.169732	-0.630760	75.264449
237.167197	-4.301258	75.269454
236.729561	-8.126469	75.274458
236.307254	-6.092322	75.279463
235.949506	-10.915908	75.284468
234.338776	-11.278623	75.289473
233.868228	-12.247325	75.294478
233.690375	-11.811827	75.299482
232.968675	-5.345822	75.304487
232.967078	-13.947963	75.309492
231.836204	-3.158761	75.314497
231.044422	2.465249	75.319502
229.929287	-8.712858	75.324506
228.863836	-6.678685	75.329511
228.628871	-11.890868	75.334516
228.096419	-4.418928	75.339521
227.819613	-10.580117	75.344526
227.764016	-11.608663	75.349530
226.469322	-1.266448	75.354535
226.107848	-7.830475	75.359540
224.757532	-1.045044	75.364545
224.083265	-5.742471	75.369550
223.069466	-7.037744	75.374554
222.392940	-7.680280	75.379559
222.377511	-15.122678	75.384564
221.893172	-6.887244	75.389569
221.385606	-10.477364	75.394574
220.330136	-14.185147	75.399578
219.479946	-12.145864	75.404583
219.233793	-14.610661	75.409588
218.649117	-9.002323	75.414593
218.024674	-9.954372	75.419598
216.988609	-7.141099	75.424602
216.479877	-9.556149	75.429607
215.771446	-21.201220	75.434612
215.051577	-8.085198	75.439617
214.555344	-9.630146	75.444622
214.140097	-23.756880	75.449626
212.879919	-3.650507	75.454631
212.154895	-7.447242	75.459636
211.630636	-6.724692	75.464641
210.832886	-8.582707	75.469646
210.622943	-10.209570	75.474650
209.632021	-8.896932	75.479655
208.904929	-15.101449	75.484660
208.087355	-7.314380	75.489665
207.679000	-15.149891	75.494670
207.594893	-21.841711	75.499674
206.958419	-8.817835	75.504679
205.765191	-17.674708	75.509684
205.338491	-11.932275	75.514689
204.485986	-13.048242	75.519694
203.262651	-16.464313	75.524698
202.732276	-8.276734	75.529703
202.503711	-10.744334	75.534708
201.931485	-6.569914	75.539713
201.571994	-6.758342	75.544718
200.480076	-12.538822	75.549722
199.523767	-7.883678	75.554727
199.429912	-9.694635	75.559732
198.762408	-7.127782	75.564737
197.707393	-4.454988	75.569742
196.978667	-8.087117	75.574746
196.238302	-10.160866	75.579751
196.145593	-14.323347	75.584756
195.631687	-5.069170	75.589761
194.757883	-6.605957	75.594766
193.938094	-13.891722	75.599770
193.271942	-6.527777	75.604775
193.019251	-6.436752	75.609780
191.675731	-0.174383	75.614785
191.160200	-3.895698	75.619790
190.889851	-6.116928	75.624794
189.747522	3.379383	75.629799
189.049361	-14.335710	75.634804
188.192843	-2.412199	75.639809
188.090578	-12.499613	75.644814
187.744834	-9.337479	75.649818
186.528910	1.605657	75.654823
186.142442	-1.562198	75.659828
185.128176	2.608586	75.664833
184.877463	-0.891587	75.669838
184.530247	0.182804	75.674842
183.054347	5.510609	75.679847
182.731743	-9.050389	75.684852
182.078468	-1.322623	75.689857
181.488939	-7.295166	75.694862
180.636160	0.890207	75.699866
179.661275	-3.828665	75.704871
179.568152	-7.964271	75.709876
179.103864	-6.379182	75.714881
178.060447	-6.821274	75.719886
177.163517	-7.163715	75.724890
176.503326	-4.380392	75.729895
176.482361	-18.885390	75.734900
175.448053	-10.833512	75.739905
174.619655	-15.411723	75.744910
174.064761	-11.345723	75.749914
173.493990	-5.485692	75.754919
173.059687	-12.191064	75.759924
171.875505	-4.613624	75.764929
171.290042	-10.493766	75.769934
171.028619	-7.624207	75.774938
170.088061	-1.165871	75.779943
169.610043	-7.794885	75.784948
168.908992	-6.127886	75.789953
168.252501	-3.323073	75.794958
168.219490	-16.271205	75.799962
166.999941	-5.138246	75.804967
166.591345	-1.286389	75.809972
164.974017	-3.396926	75.814977
164.363585	-9.743038	75.819982
163.837032	-4.647026	75.824986
163.265656	-4.607690	75.829991
163.096178	-6.826075	75.834996
162.867877	-9.590194	75.840001
161.980064	-6.898313	75.845006
161.329837	-11.678402	75.850010
160.157208	-4.135916	75.855015
160.045427	-4.717089	75.860020
158.828622	-0.723745	75.865025
158.208206	-8.596400	75.870030
157.852052	-8.717541	75.875034
156.362666	-6.018049	75.880039
155.540811	-6.728860	75.885044
155.143422	0.601703	75.890049
154.924509	-5.854148	75.895054
154.822266	-8.512204	75.900058
153.885776	-4.338041	75.905063
153.052625	-11.408761	75.910068
151.959271	-2.670913	75.915073
151.779033	-9.590265	75.920078
151.470211	-14.617185	75.925082
150.011591	-0.918128	75.930087
149.756357	-9.836227	75.935092
148.838276	-10.623159	75.940097
148.568304	-10.193467	75.945102
147.504792	-13.843160	75.950106
146.621579	2.437203	75.955111
146.578136	-11.390823	75.960116
146.138222	-0.188197	75.965121
145.121548	-3.665579	75.970126
144.105298	-9.011799	75.975130
143.575111	-1.382505	75.980135
143.391460	-0.638556	75.985140
142.554304	-9.582138	75.990145
141.690148	-7.288278	75.995150
141.137616	-12.162790	76.000154
140.539567	-0.625851	76.005159
140.075653	-11.152352	76.010164
138.887818	-8.735912	76.015169
138.410340	-14.778348	76.020174
137.707961	-9.001409	76.025178
136.870144	-6.377419	76.030183
136.483566	-9.163605	76.035188
135.443243	-2.668849	76.040193
135.382310	-2.972687	76.045198
134.836925	-9.982050	76.050202
133.887756	-2.464147	76.055207
132.998019	-3.988909	76.060212
132.310675	-6.728711	76.065217
131.748311	-5.922794	76.070222
131.480409	-11.669051	76.075226
130.317248	-6.954089	76.080231
129.720070	-7.177147	76.085236
128.983960	-3.394490	76.090241
128.743829	-10.403640	76.095246
128.348909	-15.971938	76.100250
127.031425	-3.058657	76.105255
126.666191	-15.884416	76.110260
125.826019	-13.917666	76.115265
125.387019	-12.035390	76.120270
124.425429	-14.657336	76.125274
123.820098	-10.523357	76.130279
123.864242	-12.993432	76.135284
122.876337	-12.821429	76.140289
121.708818	-6.337926	76.145294
121.161412	-12.055380	76.150298
120.505110	-9.804121	76.155303
119.884292	-12.474099	76.160308
118.690054	-7.508161	76.165313
118.484690	-12.762895	76.170318
118.259987	-14.680719	76.175322
117.588037	-7.866217	76.180327
117.332217	-17.656304	76.185332
116.026402	-4.953048	76.190337
115.071642	-13.494645	76.195342
114.632624	-15.860861	76.200346
113.505195	-2.011168	76.205351
112.994591	-17.072036	76.210356
112.700406	-10.757765	76.215361
112.231070	-16.631174	76.220366
111.943286	-16.922490	76.225370
110.594978	-5.904601	76.230375
110.111188	-13.357459	76.235380
109.334917	-4.200209	76.240385
108.519183	-8.190610	76.245390
107.574178	-14.122209	76.250394
106.423952	-5.823151	76.255399
106.752239	-10.429671	76.260404
105.924152	-6.187621	76.265409
105.493803	-8.662456	76.270414
105.434349	-13.659747	76.275418
104.364071	-2.836008	76.280423
103.507916	-10.442381	76.285428
102.987604	-2.701111	76.290433
102.300891	-7.401244	76.295438
101.701885	-12.702014	76.300442
100.714548	-13.146708	76.305447
100.319178	-13.580145	76.310452
98.869164	-7.765973	76.315457
98.136805	-9.413594	76.320462
97.754824	-9.723004	76.325466
97.056978	0.011549	76.330471
97.200605	-7.941930	76.335476
96.670842	-2.534721	76.340481
95.919476	-1.326477	76.345486
95.204350	-7.427204	76.350490
94.290498	-2.316725	76.355495
93.498733	-12.816158	76.360500
92.705738	-6.610001	76.365505
92.072432	-4.997942	76.370510
91.644352	-10.225040	76.375514
91.130272	-5.676656	76.380519
90.247408	-8.536657	76.385524
89.388076	-10.574052	76.390529
89.174052	-4.493344	76.395534
88.360983	-19.135364	76.400538
87.212639	-6.643300	76.405543
86.759212	-14.854809	76.410548
86.133673	-10.752294	76.415553
85.778680	-11.110164	76.420558
85.273986	-8.387890	76.425562
84.147384	-10.256496	76.430567
83.673522	-14.066432	76.435572
83.120329	-6.453965	76.440577
82.186463	-12.305324	76.445582
81.526437	-20.815053	76.450586
80.615766	-16.058335	76.455591
80.422770	-21.422271	76.460596
79.734286	-10.285665	76.465601
79.069620	-1.240828	76.470606
78.475003	-17.978852	76.475610
77.596042	-13.030062	76.480615
77.419996	-16.876453	76.485620
76.271709	-9.274738	76.490625
75.715600	-5.851950	76.495630
75.198082	-7.126956	76.500634
74.368793	-13.132191	76.505639
73.555607	-15.099664	76.510644
72.744811	-9.556167	76.515649
72.138344	-3.354519	76.520654
72.079323	-5.893301	76.525658
71.425259	-14.708346	76.530663
70.702945	-17.754800	76.535668
69.714498	-15.556218	76.540673
68.948210	-6.963550	76.545678
68.392695	-11.192564	76.550682
67.370953	-2.398295	76.555687
67.178867	-7.874347	76.560692
66.448411	-7.202463	76.565697
66.251429	-5.877616	76.570702
65.272114	-2.016728	76.575706
64.048885	-6.161327	76.580711
63.514123	-15.846988	76.585716
63.062710	-8.447879	76.590721
62.609729	-11.031064	76.595726
62.119494	-12.163755	76.600730
61.075699	-13.141923	76.605735
60.879588	-21.776100	76.610740
59.880074	-8.880394	76.615745
58.861652	-13.671114	76.620750
58.373237	-19.396378	76.625754
57.655291	-15.359549	76.630759
57.725497	-16.562701	76.635764
56.681363	-9.561088	76.640769
55.616339	-15.386784	76.645774
55.422370	-15.513276	76.650778
54.472638	-11.865272	76.655783
53.344854	-18.352767	76.660788
52.480655	-16.986160	76.665793
52.315205	-7.792277	76.670798
51.988631	-16.470304	76.675802
51.404826	-4.298513	76.680807
51.067175	-12.255655	76.685812
50.201454	-7.324736	76.690817
49.153629	-12.563367	76.695822
48.493091	-13.870752	76.700826
48.094551	-8.033439	76.705831
47.352821	-14.839562	76.710836
46.503481	-19.245640	76.715841
46.149986	-10.591070	76.720846
45.782833	-11.519452	76.725850
44.501375	-3.169474	76.730855
43.995575	-13.367551	76.735860
43.270692	-7.356757	76.740865
42.633154	-12.575666	76.745870
41.723529	-15.186940	76.750874
41.059927	-9.326275	76.755879
40.809211	-19.828394	76.760884
40.048173	-10.293502	76.765889
39.751998	-16.790624	76.770894
38.809316	-11.300202	76.775898
38.038514	-8.579632	76.780903
37.815070	-10.347832	76.785908
36.664205	-11.308912	76.790913
35.625927	-12.316335	76.795918
35.483579	-12.764887	76.800922
34.881593	-10.009739	76.805927
34.610469	-18.611447	76.810932
33.480208	-10.589950	76.815937
32.976173	-11.660507	76.820942
32.416274	-18.287457	76.825946
30.940135	-7.007861	76.830951
30.767281	-21.155853	76.835956
30.123198	-13.896330	76.840961
29.621783	-15.210165	76.845966
28.700569	-12.486103	76.850970
27.797271	-3.537242	76.855975
27.195584	-11.069048	76.860980
26.610291	-10.074939	76.865985
26.437377	-8.678231	76.870990
25.935558	-13.065615	76.875994
24.914734	-3.325267	76.880999
24.373309	-14.418133	76.886004
23.538003	-7.743142	76.891009
22.572501	-10.134177	76.896014
22.191458	-1.038371	76.901018
21.377340	1.971401	76.906023
21.145173	-8.159927	76.911028
20.146805	-8.913501	76.916033
19.301184	-12.517460	76.921038
19.008212	-7.118048	76.926042
18.048317	-1.892964	76.931047
17.991895	-16.363894	76.936052
16.684887	-5.352551	76.941057
15.947967	-10.535099	76.946062
15.597040	-12.446971	76.951066
15.079656	-8.016325	76.956071
14.608882	-11.192775	76.961076
13.513801	-7.420641	76.966081
12.789159	-5.234152	76.971086
12.674726	-21.995119	76.976090
11.587903	-12.179587	76.981095
10.715235	-14.255826	76.986100
10.216384	-4.518308	76.991105
9.676078	-8.566798	76.996110
9.413089	-11.501989	77.001114
7.917346	-13.379487	77.006119
7.494927	-15.656861	77.011124
6.728123	-2.662632	77.016129
6.372445	-7.224718	77.021134
6.120685	-17.278791	77.026139
4.594181	-14.497594	77.031143
3.934773	-7.303430	77.036148
3.324423	-13.901825	77.041153
2.855154	-8.177811	77.046158