Fri Mar 05 17:54:18 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.930946	100.887432	0.000000
-1.285169	89.010854	0.005005
-1.828318	52.105590	0.010010
-3.997418	21.882955	0.015014
-7.572794	0.359566	0.020019
-12.918923	-2.289946	0.025024
-18.319906	-0.552911	0.030029
-22.629991	-0.100101	0.035034
-26.551153	7.800408	0.040038
-30.442699	-0.597490	0.045043
-33.791654	-1.042330	0.050048
-37.902681	7.285890	0.055053
-40.891665	0.120760	0.060058
-45.248453	8.215375	0.065062
-48.916095	3.430993	0.070067
-52.352611	-1.948514	0.075072
-56.092917	8.582028	0.080077
-59.647426	-1.716269	0.085082
-63.968650	7.733665	0.090086
-67.621403	4.620147	0.095091
-71.023914	0.294992	0.100096
-75.001546	4.522263	0.105101
-79.044766	4.601425	0.110106
-82.983390	9.339745	0.115110
-86.138784	12.634730	0.120115
-89.737514	8.817164	0.125120
-93.543861	11.113684	0.130125
-97.466280	4.283642	0.135130
-101.590537	5.968553	0.140134
-105.156120	-0.543079	0.145139
-109.126194	7.333819	0.150144
-112.736166	12.841372	0.155149
-116.206823	6.119059	0.160154
-120.113472	4.782421	0.165158
-124.160405	-2.272141	0.170163
-128.182047	-1.800510	0.175168
-132.050795	4.134726	0.180173
-135.499274	-5.819231	0.185178
-139.444079	2.146724	0.190182
-143.354950	8.229054	0.195187
-146.567608	2.949586	0.200192
-150.734918	11.684377	0.205197
-154.108649	5.184783	0.210202
-157.751953	9.967563	0.215206
-161.477955	2.014996	0.220211
-164.821088	0.148523	0.225216
-169.148741	4.706199	0.230221
-172.971260	4.065878	0.235226
-177.107559	12.696412	0.240230
-180.984752	5.185911	0.245235
-184.318781	11.231446	0.250240
-187.996522	11.455899	0.255245
-191.412756	6.631619	0.260250
-195.590302	8.309423	0.265254
-199.200840	7.088091	0.270259
-203.076081	8.687699	0.275264
-207.037082	12.127177	0.280269
-210.402204	5.829726	0.285274
-214.330389	4.274322	0.290278
-218.327347	5.965922	0.295283
-221.811180	7.312273	0.300288
-225.410330	8.402635	0.305293
-229.059108	4.678430	0.310298
-232.938591	1.681783	0.315302
-237.069905	5.556936	0.320307
-240.759710	-0.874732	0.325312
-244.380015	8.380051	0.330317
-248.258953	-4.633811	0.335322
-252.194102	1.111927	0.340326
-255.884255	9.401708	0.345331
-259.437902	3.347318	0.350336
-263.612075	6.825644	0.355341
-266.952284	-1.776552	0.360346
-270.512737	7.858235	0.365350
-274.259191	1.131299	0.370355
-277.995998	4.599761	0.375360
-282.018087	9.034740	0.380365
-285.644983	5.311862	0.385370
-289.503351	3.624007	0.390374
-293.247245	-2.477232	0.395379
-297.121285	0.193121	0.400384
-301.117852	8.735315	0.405389
-304.784758	1.098413	0.410394
-308.656151	3.962335	0.415398
-311.951160	7.458095	0.420403
-315.825561	2.871150	0.425408
-320.117474	14.882631	0.430413
-323.196976	5.284806	0.435418
-327.135342	13.082866	0.440422
-331.023187	14.746194	0.445427
-334.650367	7.309583	0.450432
-338.431662	4.349475	0.455437
-342.079107	-6.575373	0.460442
-345.888614	11.351752	0.465446
-349.643058	-1.006851	0.470451
-353.508637	8.571105	0.475456
-357.647547	8.654974	0.480461
-361.168006	0.772425	0.485466
-365.215815	7.318525	0.490470
-368.811562	12.798943	0.495475
-371.771024	10.270664	0.500480
-375.969189	11.072101	0.505485
-380.060040	10.839241	0.510490
-383.931261	11.825041	0.515494
-387.569347	8.317002	0.520499
-391.361925	7.486162	0.525504
-395.343245	9.516191	0.530509
-398.308231	-0.990820	0.535514
-402.260961	10.993445	0.540518
-406.041195	3.177676	0.545523
-409.942589	4.228261	0.550528
-413.949914	14.484981	0.555533
-417.436304	0.341097	0.560538
-421.534858	8.787798	0.565542
-424.780034	3.804081	0.570547
-428.587641	6.419879	0.575552
-432.439148	14.152192	0.580557
-436.235160	5.687689	0.585562
-440.281800	11.457839	0.590566
-443.822958	2.550516	0.595571
-447.735085	3.077734	0.600576
-451.586897	8.417807	0.605581
-454.974816	6.618822	0.610586
-459.087142	9.370067	0.615590
-462.463961	3.352410	0.620595
-466.335487	5.973744	0.625600
-470.522279	6.377702	0.630605
-473.808695	2.919296	0.635610
-477.663732	13.061904	0.640614
-481.506103	6.645525	0.645619
-485.266261	6.296951	0.650624
-489.101009	10.817470	0.655629
-492.455556	1.751105	0.660634
-496.956117	12.381630	0.665638
-500.227808	15.911769	0.670643
-503.750811	15.154750	0.675648
-507.850619	20.919314	0.680653
-511.177833	6.846349	0.685658
-515.275340	18.087491	0.690662
-519.293957	15.810573	0.695667
-522.822304	11.614991	0.700672
-527.059546	17.336879	0.705677
-530.065276	4.131990	0.710682
-534.110691	18.533041	0.715686
-537.735436	9.666023	0.720691
-541.398150	15.417594	0.725696
-545.416693	19.153827	0.730701
-549.488722	15.538732	0.735706
-553.238505	9.777909	0.740710
-556.646336	5.184648	0.745715
-560.187466	7.106784	0.750720
-564.146936	15.687626	0.755725
-567.675266	7.131696	0.760730
-572.164345	12.845003	0.765734
-575.665894	13.234300	0.770739
-579.407256	11.829435	0.775744
-582.947249	9.264850	0.780749
-586.439859	3.923485	0.785754
-590.389483	12.305669	0.790758
-594.280821	16.179360	0.795763
-597.865787	14.722729	0.800768
-602.340137	13.201605	0.805773
-605.659282	1.586051	0.810778
-609.345992	12.118293	0.815782
-613.228527	10.879543	0.820787
-617.107453	14.181990	0.825792
-620.848229	16.129805	0.830797
-624.331047	1.162490	0.835802
-628.271421	7.083131	0.840806
-631.978679	7.905936	0.845811
-635.553566	9.943966	0.850816
-639.385140	11.341749	0.855821
-643.040864	3.397671	0.860826
-647.142507	13.572052	0.865830
-650.738457	10.040346	0.870835
-654.349142	10.546548	0.875840
-658.172027	22.961488	0.880845
-661.913700	18.204096	0.885850
-665.996220	11.354874	0.890854
-669.089450	11.398359	0.895859
-672.721213	7.732057	0.900864
-677.219390	24.044465	0.905869
-680.945736	11.633042	0.910874
-685.040235	16.457157	0.915878
-688.454096	16.337430	0.920883
-691.894762	18.871354	0.925888
-695.945285	17.795206	0.930893
-699.835687	4.085357	0.935898
-703.631602	5.898604	0.940902
-707.008922	6.440135	0.945907
-710.717049	0.882660	0.950912
-714.916521	12.580396	0.955917
-718.487743	6.338712	0.960922
-722.524638	9.201357	0.965926
-725.941309	13.587623	0.970931
-729.385225	11.476276	0.975936
-733.482793	13.410321	0.980941
-737.145640	6.718094	0.985946
-741.197209	5.659541	0.990950
-744.825303	5.600154	0.995955
-748.617473	3.711657	1.000960
-752.894486	6.988054	1.005965
-755.418960	-0.422257	1.010970
-759.634359	10.551888	1.015974
-763.694904	2.037967	1.020979
-767.022827	12.365643	1.025984
-771.105829	9.978811	1.030989
-775.159087	6.928836	1.035994
-778.831728	18.073319	1.040998
-782.426115	10.274995	1.046003
-786.066080	6.600722	1.051008
-790.008029	13.658105	1.056013
-793.227591	5.708424	1.061018
-797.294056	17.570336	1.066022
-801.294848	16.065363	1.071027
-804.924350	8.386234	1.076032
-808.821293	8.272935	1.081037
-812.585776	1.622313	1.086042
-816.317977	8.836235	1.091046
-819.985036	8.359769	1.096051
-823.559193	9.683582	1.101056
-827.336765	10.005408	1.106061
-830.824657	7.369793	1.111066
-835.031155	7.306022	1.116070
-838.714051	11.981016	1.121075
-842.977327	13.634224	1.126080
-846.873022	23.169657	1.131085
-850.312620	13.203555	1.136090
-854.057014	13.523273	1.141094
-857.640182	10.276861	1.146099
-861.347480	16.072306	1.151104
-865.069719	27.483477	1.156109
-868.550691	6.073433	1.161114
-872.593151	14.563948	1.166118
-876.698363	11.560304	1.171123
-880.372249	14.180670	1.176128
-883.782710	9.266610	1.181133
-887.527128	6.170610	1.186138
-891.561725	6.090495	1.191142
-895.241752	7.609545	1.196147
-899.063068	3.738937	1.201152
-902.980087	6.406095	1.206157
-906.530412	-0.395308	1.211162
-909.846859	11.543197	1.216166
-914.078004	9.750389	1.221171
-917.752817	9.239044	1.226176
-921.933109	17.880994	1.231181
-925.639891	4.812417	1.236186
-929.216325	15.201331	1.241190
-932.858270	4.790678	1.246195
-936.217329	8.713852	1.251200
-940.352492	13.656866	1.256205
-944.098497	10.528094	1.261210
-947.755938	5.831825	1.266214
-951.684101	0.623752	1.271219
-955.456647	-5.948064	1.276224
-959.500319	12.141954	1.281229
-962.930619	6.095749	1.286234
-966.546478	14.005675	1.291238
-970.028890	11.172270	1.296243
-973.996177	-1.179605	1.301248
-978.176251	-3.615990	1.306253
-981.661962	-0.978252	1.311258
-985.431234	13.333602	1.316262
-989.454097	11.113373	1.321267
-993.059261	-3.419013	1.326272
-997.086030	6.769192	1.331277
-1000.242072	3.517776	1.336282
-1004.383526	-0.985870	1.341286
-1008.381083	7.153897	1.346291
-1011.734355	1.590627	1.351296
-1015.883967	7.553241	1.356301
-1019.012761	2.936547	1.361306
-1022.980229	5.394346	1.366310
-1026.764591	5.164053	1.371315
-1030.955416	4.434213	1.376320
-1034.620830	16.759865	1.381325
-1038.078494	2.487818	1.386330
-1041.779642	3.078470	1.391334
-1045.931553	-1.950144	1.396339
-1049.479941	-0.852467	1.401344
-1053.403936	9.455013	1.406349
-1056.822578	4.220819	1.411354
-1060.753777	3.722324	1.416358
-1064.486677	-2.961310	1.421363
-1068.161881	2.353060	1.426368
-1072.146072	14.051647	1.431373
-1075.745491	7.789810	1.436378
-1079.606012	8.894884	1.441382
-1083.198383	8.198721	1.446387
-1087.077196	0.601730	1.451392
-1090.839467	10.170598	1.456397
-1094.768421	7.839335	1.461402
-1098.312118	19.786056	1.466406
-1102.113801	9.940569	1.471411
-1105.625031	6.074320	1.476416
-1109.949649	17.171399	1.481421
-1113.353720	3.154259	1.486426
-1117.113974	4.702259	1.491430
-1120.806097	7.297527	1.496435
-1124.712792	11.816367	1.501440
-1128.950540	8.613600	1.506445
-1132.008788	2.913423	1.511450
-1135.989554	7.504055	1.516454
-1139.563930	3.964938	1.521459
-1143.266810	-1.884407	1.526464
-1147.321245	5.865706	1.531469
-1151.011566	4.592371	1.536474
-1154.909161	4.057120	1.541478
-1158.759296	10.158151	1.546483
-1162.060677	-4.436742	1.551488
-1166.180653	5.561639	1.556493
-1169.663687	-1.647511	1.561498
-1173.661660	2.617923	1.566502
-1177.455489	3.835492	1.571507
-1180.858527	8.101943	1.576512
-1185.097082	5.249502	1.581517
-1188.336198	2.621937	1.586522
-1192.442498	-4.380211	1.591526
-1196.207313	2.680227	1.596531
-1199.715151	-7.331947	1.601536
-1203.693186	2.411964	1.606541
-1207.056993	4.595277	1.611546
-1211.451662	4.587528	1.616550
-1214.981320	1.341003	1.621555
-1218.999277	4.974183	1.626560
-1222.876390	10.795775	1.631565
-1226.157556	-1.329531	1.636570
-1230.063339	4.203338	1.641574
-1233.767485	6.671393	1.646579
-1237.451735	4.854740	1.651584
-1241.327254	9.107000	1.656589
-1244.736838	6.274978	1.661594
-1248.445610	6.606974	1.666598
-1252.443939	1.662974	1.671603
-1256.349787	8.506376	1.676608
-1260.517354	11.988526	1.681613
-1263.837591	4.244100	1.686618
-1267.699979	13.051805	1.691622
-1271.493100	11.288901	1.696627
-1274.936066	8.870706	1.701632
-1278.909361	7.620787	1.706637
-1282.565717	7.099183	1.711642
-1286.219608	15.233290	1.716646
-1290.256264	12.657820	1.721651
-1293.735456	9.627271	1.726656
-1297.911786	3.765647	1.731661
-1301.275553	3.515794	1.736666
-1305.142080	6.850488	1.741670
-1308.864118	0.578696	1.746675
-1312.775147	9.313829	1.751680
-1316.551634	8.830430	1.756685
-1320.226556	-3.510828	1.761690
-1324.088675	-3.540527	1.766694
-1327.951661	5.256325	1.771699
-1331.433484	-6.907658	1.776704
-1335.527269	8.319261	1.781709
-1339.263562	1.754905	1.786714
-1342.579140	4.725494	1.791718
-1346.454864	5.546431	1.796723
-1350.182087	1.620521	1.801728
-1354.281143	11.070233	1.806733
-1357.769924	1.980952	1.811738
-1361.318439	8.969175	1.816742
-1365.376525	7.005989	1.821747
-1368.990866	2.804990	1.826752
-1373.361781	14.343610	1.831757
-1376.598163	2.563034	1.836762
-1380.289556	3.135316	1.841766
-1384.209031	-1.359013	1.846771
-1387.894403	-1.019500	1.851776
-1391.850821	4.370348	1.856781
-1395.393997	4.704455	1.861786
-1399.216328	6.497818	1.866790
-1403.048500	5.045745	1.871795
-1406.751750	3.967284	1.876800
-1410.905606	2.655039	1.881805
-1414.299666	3.931993	1.886810
-1417.997075	0.610141	1.891814
-1421.536261	-2.778040	1.896819
-1425.139437	1.736849	1.901824
-1429.565737	-0.089994	1.906829
-1432.951782	-5.314633	1.911834
-1436.947738	-0.210124	1.916838
-1440.792955	5.162001	1.921843
-1444.542098	1.977788	1.926848
-1448.450431	9.258724	1.931853
-1451.887651	2.925798	1.936858
-1455.853081	10.321547	1.941862
-1459.376647	0.744405	1.946867
-1463.162326	0.000940	1.951872
-1467.092492	5.803035	1.956877
-1470.555848	-5.359136	1.961882
-1474.235547	3.608873	1.966886
-1478.017851	-2.798063	1.971891
-1481.788731	1.746921	1.976896
-1485.874355	0.917482	1.981901
-1489.658921	10.676612	1.986906
-1493.455929	8.925740	1.991910
-1497.346977	8.169243	1.996915
-1500.936773	5.417631	2.006912
-1501.955175	1.463173	2.016909
-1499.453019	5.564707	2.026906
-1496.437225	5.532261	2.036902
-1494.099517	3.391486	2.046899
-1492.635731	5.991884	2.056896
-1490.407143	0.535308	2.066893
-1488.815601	1.621510	2.076890
-1487.139081	2.387779	2.086886
-1485.093519	6.570343	2.096883
-1482.998502	0.686725	2.106880
-1480.899936	-0.738348	2.116877
-1479.074882	5.052221	2.126874
-1477.408291	7.602784	2.136870
-1475.774929	6.721174	2.146867
-1473.306995	2.303168	2.156864
-1471.457078	-0.059485	2.166861
-1469.524508	-1.639552	2.176858
-1467.745252	7.742703	2.186854
-1465.800035	7.880150	2.196851
-1464.165562	3.095068	2.206848
-1462.243613	3.097292	2.216845
-1460.365886	0.428605	2.226842
-1458.272722	0.412890	2.236838
-1456.595524	3.206516	2.246835
-1454.753496	4.601594	2.256832
-1452.666473	4.244223	2.266829
-1450.807519	-2.795296	2.276826
-1448.918597	2.293467	2.286822
-1447.115529	-0.724848	2.296819
-1445.454524	-1.309272	2.306816
-1443.489733	1.490421	2.316813
-1441.176456	-6.204488	2.326810
-1439.549008	-7.208287	2.336806
-1437.842741	2.071989	2.346803
-1435.636791	3.003008	2.356800
-1434.040111	2.233095	2.366797
-1432.122263	3.020766	2.376794
-1430.118428	-5.311455	2.386790
-1428.196905	-0.215263	2.396787
-1426.285043	-2.459898	2.406784
-1424.282447	-8.777103	2.416781
-1422.401760	-6.521316	2.426778
-1420.906602	1.180610	2.436774
-1419.118779	-0.163075	2.446771
-1417.077013	-4.479630	2.456768
-1415.030802	-6.917878	2.466765
-1412.938187	-3.751768	2.476762
-1411.276013	3.130765	2.486758
-1409.481067	4.658159	2.496755
-1407.707655	3.365739	2.506752
-1405.859762	-1.834013	2.516749
-1403.693903	-1.730259	2.526746
-1401.800795	0.520400	2.536742
-1400.258236	4.074599	2.546739
-1398.399154	9.007127	2.556736
-1396.022293	4.109550	2.566733
-1394.319993	3.152222	2.576730
-1392.760241	7.717397	2.586726
-1390.781004	8.215791	2.596723
-1388.840767	7.883557	2.606720
-1386.853792	1.644670	2.616717
-1384.757326	3.348032	2.626714
-1383.189629	3.394403	2.636710
-1381.148981	7.759436	2.646707
-1379.467748	5.974933	2.656704
-1377.371283	9.086777	2.666701
-1375.780888	-0.641378	2.676698
-1374.180717	2.999936	2.686694
-1371.841922	2.603911	2.696691
-1369.817886	4.260459	2.706688
-1368.157972	6.850069	2.716685
-1366.346455	2.546729	2.726682
-1364.348340	4.439545	2.736678
-1362.462007	1.924299	2.746675
-1360.496080	7.386091	2.756672
-1358.867975	5.717480	2.766669
-1356.773558	7.545938	2.776666
-1355.158288	7.033638	2.786662
-1352.962867	2.820437	2.796659
-1351.161277	6.538477	2.806656
-1349.716217	10.615183	2.816653
-1347.668203	4.628671	2.826650
-1345.243297	5.488411	2.836646
-1343.831089	8.022951	2.846643
-1341.871145	4.619589	2.856640
-1340.053705	5.372882	2.866637
-1338.208754	3.658520	2.876634
-1335.955011	9.465858	2.886630
-1334.135368	2.110597	2.896627
-1332.537269	4.782763	2.906624
-1330.644818	2.277616	2.916621
-1328.407818	4.268020	2.926618
-1326.923838	2.414072	2.936614
-1325.238980	4.784976	2.946611
-1323.153900	0.778945	2.956608
-1321.111923	3.356383	2.966605
-1319.307946	1.688071	2.976602
-1317.513615	-1.245061	2.986598
-1315.598115	5.745428	2.996595
-1313.462320	3.507671	3.006592
-1311.757731	4.416424	3.016589
-1310.186931	1.113271	3.026586
-1307.828882	11.276218	3.036582
-1306.017932	5.449268	3.046579
-1304.602353	5.979531	3.056576
-1302.562345	2.190740	3.066573
-1300.450651	4.955994	3.076570
-1298.671688	4.884920	3.086566
-1296.634060	8.519435	3.096563
-1294.857259	0.782622	3.106560
-1293.180471	-2.352739	3.116557
-1291.100188	1.698126	3.126554
-1289.165684	3.763828	3.136550
-1287.585163	8.197856	3.146547
-1285.559441	3.192370	3.156544
-1283.524848	5.614703	3.166541
-1281.748838	1.800285	3.176538
-1280.046421	0.513007	3.186534
-1278.010768	7.588515	3.196531
-1276.071702	9.165585	3.206528
-1274.539747	9.033005	3.216525
-1272.496362	9.424915	3.226522
-1270.355961	4.967952	3.236518
-1268.597789	3.955981	3.246515
-1266.774065	9.009548	3.256512
-1264.643392	3.510422	3.266509
-1263.244678	3.332855	3.276506
-1261.235800	7.278332	3.286502
-1258.947183	6.397799	3.296499
-1257.457358	1.803378	3.306496
-1255.470232	4.539660	3.316493
-1253.483514	-1.861716	3.326490
-1251.891862	1.075233	3.336486
-1250.026661	9.802848	3.346483
-1247.995068	11.497771	3.356480
-1246.164135	2.395958	3.366477
-1244.528092	-1.754468	3.376474
-1242.175852	6.787837	3.386470
-1240.317023	7.005617	3.396467
-1238.616119	2.715335	3.406464
-1236.911795	1.852537	3.416461
-1234.550339	0.319295	3.426458
-1233.089309	0.569160	3.436454
-1231.270711	4.350894	3.446451
-1229.186055	8.194270	3.456448
-1227.348270	5.045821	3.466445
-1225.546492	2.574215	3.476442
-1223.661399	0.122437	3.486438
-1221.676438	-1.647398	3.496435
-1219.943232	4.312833	3.506432
-1217.867259	10.562442	3.516429
-1216.030955	3.773040	3.526426
-1214.484964	5.515697	3.536422
-1212.034175	7.735701	3.546419
-1210.518463	8.856339	3.556416
-1208.589824	3.263269	3.566413
-1206.840385	-0.396837	3.576410
-1204.658945	4.474799	3.586406
-1202.859483	7.219052	3.596403
-1201.214314	1.102904	3.606400
-1199.489993	-1.117858	3.616397
-1197.514922	0.402988	3.626394
-1195.248165	1.266085	3.636390
-1193.546410	5.166025	3.646387
-1191.760304	7.542936	3.656384
-1189.709001	7.733117	3.666381
-1187.753149	6.732209	3.676378
-1186.083164	7.435004	3.686374
-1183.871874	0.710368	3.696371
-1182.564139	1.191644	3.706368
-1180.639163	10.361354	3.716365
-1178.383877	2.085409	3.726362
-1176.532287	3.632347	3.736358
-1174.904446	5.890904	3.746355
-1172.878776	8.548459	3.756352
-1170.939165	10.472913	3.766349
-1169.281344	12.774049	3.776346
-1167.457425	2.501785	3.786342
-1165.304098	-1.736092	3.796339
-1163.592575	5.126111	3.806336
-1161.865917	3.801881	3.816333
-1159.745966	7.363347	3.826330
-1157.724924	2.682411	3.836326
-1155.865143	3.301176	3.846323
-1154.268860	4.726342	3.856320
-1152.396851	5.284729	3.866317
-1150.404716	-2.017470	3.876314
-1148.538495	4.943157	3.886310
-1146.765511	6.076363	3.896307
-1144.912972	6.871566	3.906304
-1142.727015	8.939796	3.916301
-1141.006756	11.603610	3.926298
-1139.044185	10.121647	3.936294
-1137.469685	12.984054	3.946291
-1135.581967	10.956678	3.956288
-1133.659855	8.360094	3.966285
-1131.221034	8.968349	3.976282
-1129.509372	6.493862	3.986278
-1128.097370	6.797429	3.996275
-1126.120491	10.913944	4.006272
-1124.189409	8.429622	4.016269
-1122.293536	10.282164	4.026266
-1120.275949	1.908502	4.036262
-1118.618275	1.736965	4.046259
-1116.848074	0.348957	4.056256
-1114.735606	9.010292	4.066253
-1112.730487	-3.596276	4.076250
-1110.967074	1.743395	4.086246
-1108.818151	4.374973	4.096243
-1107.420204	0.559579	4.106240
-1105.575849	2.343005	4.116237
-1103.427880	2.876234	4.126234
-1101.379127	-3.211250	4.136230
-1099.567235	2.505954	4.146227
-1098.142718	8.874103	4.156224
-1096.209521	7.497931	4.166221
-1093.983209	3.643193	4.176218
-1092.074807	5.582181	4.186214
-1090.473828	-0.143128	4.196211
-1088.400022	8.868643	4.206208
-1086.583152	4.864663	4.216205
-1084.715743	6.516518	4.226202
-1082.829657	3.218340	4.236198
-1080.701745	7.724437	4.246195
-1079.262026	1.188054	4.256192
-1077.456443	-3.922579	4.266189
-1075.340589	-1.869914	4.276186
-1073.274935	0.231836	4.286182
-1071.994300	1.754921	4.296179
-1069.824338	7.842788	4.306176
-1067.746788	0.640677	4.316173
-1065.987820	-4.759345	4.326170
-1063.970749	-2.436648	4.336166
-1062.214911	0.663656	4.346163
-1060.246401	0.579814	4.356160
-1058.610874	1.998769	4.366157
-1056.579441	2.365937	4.376154
-1054.461934	-2.477191	4.386150
-1052.941728	0.769762	4.396147
-1050.704846	1.656728	4.406144
-1049.007162	1.110930	4.416141
-1047.341249	-2.800977	4.426138
-1045.622242	-2.456461	4.436134
-1043.497598	1.791233	4.446131
-1041.491216	6.113112	4.456128
-1039.735335	4.700608	4.466125
-1037.869003	1.642477	4.476122
-1035.843164	-2.521209	4.486118
-1034.123959	-1.017721	4.496115
-1032.187314	-1.265397	4.506112
-1030.195651	2.305656	4.516109
-1028.565392	-2.446887	4.526106
-1026.305068	2.830746	4.536102
-1024.794233	-0.088408	4.546099
-1022.804327	-4.729513	4.556096
-1021.312066	3.372659	4.566093
-1018.971164	-1.555118	4.576090
-1017.045488	-3.252140	4.586086
-1015.183016	0.031681	4.596083
-1013.707150	7.332765	4.606080
-1011.442175	1.046554	4.616077
-1009.566066	0.974374	4.626074
-1007.908157	0.134955	4.636070
-1005.831482	0.667044	4.646067
-1003.945382	2.764415	4.656064
-1002.206409	0.732512	4.666061
-1000.218847	3.849492	4.676058
-998.461913	-5.679278	4.686054
-996.488214	2.568557	4.696051
-994.818052	-0.623965	4.706048
-992.613895	-1.424412	4.716045
-990.870631	0.092630	4.726042
-989.175230	-4.403452	4.736038
-987.290688	1.648032	4.746035
-985.171478	-0.384666	4.756032
-983.465530	-2.333902	4.766029
-981.495752	-0.076203	4.776026
-979.635392	-1.413788	4.786022
-977.822992	1.200674	4.796019
-975.743222	0.225916	4.806016
-974.288473	-0.314138	4.816013
-972.147758	-2.688171	4.826010
-969.916772	-4.266604	4.836006
-968.544163	1.874657	4.846003
-966.645850	-6.347171	4.856000
-964.968327	1.987531	4.865997
-962.714235	-4.944289	4.875994
-960.615667	-3.338774	4.885990
-958.954474	1.613139	4.895987
-957.094361	-0.090720	4.905984
-955.350915	-3.040712	4.915981
-953.632871	-0.622730	4.925978
-951.542516	-1.085980	4.935974
-949.414485	-5.779115	4.945971
-947.734958	-5.057147	4.955968
-945.987347	-4.303430	4.965965
-943.958495	1.412370	4.975962
-941.978739	-0.717995	4.985958
-940.242182	-6.433307	4.995955
-938.498085	3.480839	5.005952
-936.570534	5.660063	5.015949
-934.556506	3.355269	5.025946
-932.626697	-1.484586	5.035942
-930.860351	-1.790215	5.045939
-929.137771	-0.843001	5.055936
-927.315005	4.324691	5.065933
-925.264782	3.894724	5.075930
-923.138357	-7.542104	5.085926
-921.334727	-5.188311	5.095923
-919.706749	4.174394	5.105920
-917.736101	-0.795143	5.115917
-915.743320	3.737454	5.125914
-914.066353	4.082472	5.135910
-912.169152	6.114984	5.145907
-910.281615	6.862145	5.155904
-908.142569	4.924242	5.165901
-906.696932	4.589380	5.175898
-904.595340	4.208062	5.185894
-902.540135	10.282864	5.195891
-900.775569	1.005575	5.205888
-899.114552	7.380257	5.215885
-897.297500	7.101284	5.225882
-895.024722	-5.489499	5.235878
-893.597549	3.943229	5.245875
-891.189921	4.586725	5.255872
-889.584347	6.694304	5.265869
-887.704165	8.022158	5.275866
-885.944289	4.924317	5.285862
-883.973338	3.952826	5.295859
-882.083997	-1.101583	5.305856
-880.275875	0.220428	5.315853
-878.080170	1.644693	5.325850
-876.401236	5.884856	5.335846
-874.814671	3.893200	5.345843
-872.701561	8.954518	5.355840
-870.783508	3.649199	5.365837
-869.036815	4.897353	5.375834
-866.901385	4.543818	5.385830
-865.004133	7.537982	5.395827
-863.419076	1.895889	5.405824
-861.704175	2.307514	5.415821
-859.637531	3.133455	5.425818
-857.702696	-0.273399	5.435814
-855.713122	3.133925	5.445811
-853.708064	1.560138	5.455808
-852.094872	2.652797	5.465805
-850.248450	6.791201	5.475802
-848.497027	7.432272	5.485798
-846.322583	7.467273	5.495795
-844.394475	5.946849	5.505792
-842.599966	9.020618	5.515789
-840.735693	8.437285	5.525786
-838.951910	0.799930	5.535782
-837.195229	2.305470	5.545779
-835.293704	6.851938	5.555776
-833.387710	8.355718	5.565773
-831.704696	-2.549877	5.575770
-829.520730	8.062241	5.585766
-827.549534	5.548057	5.595763
-825.857657	7.139757	5.605760
-823.928482	6.917132	5.615757
-822.063320	4.160943	5.625754
-820.076204	-1.408808	5.635750
-818.029943	1.794480	5.645747
-816.362051	0.577002	5.655744
-814.700617	0.571664	5.665741
-812.660824	7.555369	5.675738
-810.849075	-0.082489	5.685734
-808.944055	7.123298	5.695731
-806.885728	9.518580	5.705728
-805.241039	14.166923	5.715725
-803.291086	5.051122	5.725722
-801.291797	3.598305	5.735718
-799.548836	2.068037	5.745715
-797.541734	2.387212	5.755712
-795.779798	7.837908	5.765709
-793.947427	7.420770	5.775706
-792.017186	8.753333	5.785702
-790.137939	2.555817	5.795699
-788.153704	10.690057	5.805696
-786.389161	5.003530	5.815693
-784.592248	10.557598	5.825690
-782.933565	6.722813	5.835686
-780.694058	3.273636	5.845683
-778.779830	5.800927	5.855680
-777.136220	6.470336	5.865677
-775.049753	2.644555	5.875674
-773.252734	-0.334398	5.885670
-771.247929	4.073243	5.895667
-769.551860	7.791252	5.905664
-767.633770	4.714000	5.915661
-765.580974	6.633339	5.925658
-763.839206	5.169605	5.935654
-761.993813	0.455483	5.945651
-760.058368	3.222566	5.955648
-758.363662	3.076944	5.965645
-756.564507	0.895065	5.975642
-754.624190	2.551325	5.985638
-752.534746	3.365822	5.995635
-750.738514	0.814924	6.005632
-748.710036	1.852335	6.015629
-747.010890	-2.339433	6.025626
-745.185684	-3.169090	6.035622
-743.144446	-2.885326	6.045619
-741.271852	2.053494	6.055616
-739.563194	2.044608	6.065613
-737.761241	0.934450	6.075610
-735.642495	-0.422135	6.085606
-733.598063	-4.752763	6.095603
-732.048954	-5.190902	6.105600
-730.287152	-6.815714	6.115597
-728.494220	-1.447293	6.125594
-726.519044	2.144034	6.135590
-724.300832	-2.028036	6.145587
-722.708806	1.561364	6.155584
-720.750039	12.924094	6.165581
-718.748805	5.505500	6.175578
-716.962176	5.899452	6.185574
-715.134475	3.150911	6.195571
-713.214630	7.226377	6.205568
-711.314130	1.286060	6.215565
-709.466642	-0.567177	6.225562
-707.420886	-0.137255	6.235558
-705.558894	-0.508529	6.245555
-704.067778	1.298508	6.255552
-701.940012	0.630543	6.265549
-700.217021	3.054243	6.275546
-698.042824	-3.889843	6.285542
-696.425887	-4.341955	6.295539
-694.513366	-5.981352	6.305536
-692.648010	-0.100240	6.315533
-690.601933	6.389921	6.325530
-688.723361	2.175835	6.335526
-686.990007	6.386918	6.345523
-684.888275	2.514561	6.355520
-683.076127	1.855992	6.365517
-681.496151	2.309837	6.375514
-679.428627	4.869560	6.385510
-677.499542	1.886941	6.395507
-675.963408	-1.274475	6.405504
-673.970668	0.280314	6.415501
-671.852035	1.881307	6.425498
-669.999802	-3.863362	6.435494
-668.200761	-0.352793	6.445491
-666.107950	-2.562580	6.455488
-664.366295	-0.632911	6.465485
-662.772846	-1.791806	6.475482
-660.622992	0.773726	6.485478
-658.815451	-2.247880	6.495475
-656.949118	-4.464105	6.505472
-654.978512	-5.860108	6.515469
-653.103281	-1.783781	6.525466
-651.328571	-1.675256	6.535462
-649.413025	0.476125	6.545459
-647.587660	1.452915	6.555456
-645.497056	0.620404	6.565453
-643.860922	-3.325953	6.575450
-641.741394	0.112903	6.585446
-640.237248	2.964790	6.595443
-638.133964	2.791869	6.605440
-636.070709	0.541038	6.615437
-634.412280	2.382971	6.625434
-632.654753	-0.636942	6.635430
-630.759601	2.049843	6.645427
-628.884320	-6.970207	6.655424
-626.752002	2.073718	6.665421
-625.083575	0.023354	6.675418
-623.222415	-3.482078	6.685414
-621.364081	-5.128550	6.695411
-619.456991	0.643320	6.705408
-617.433092	3.063220	6.715405
-615.757472	1.373308	6.725402
-613.709518	-3.020947	6.735398
-611.885333	-3.201363	6.745395
-609.888667	-6.129985	6.755392
-608.140073	3.647928	6.765389
-606.187303	2.059015	6.775386
-604.382103	-4.906571	6.785382
-602.460916	-4.114010	6.795379
-600.653973	-2.562635	6.805376
-598.986679	1.295894	6.815373
-597.158691	0.584331	6.825370
-595.192061	0.404857	6.835366
-592.897063	2.672515	6.845363
-591.121535	0.303471	6.855360
-589.388952	1.468821	6.865357
-587.638394	6.218837	6.875354
-585.551057	0.689312	6.885350
-583.395280	-1.352034	6.895347
-581.827769	-4.835788	6.905344
-580.254196	-7.624160	6.915341
-577.988161	-6.646659	6.925338
-576.131276	-6.368039	6.935334
-574.345826	-0.031936	6.945331
-572.326318	-2.228353	6.955328
-570.806987	4.676081	6.965325
-569.063745	6.105020	6.975322
-566.941057	1.646755	6.985318
-564.927213	0.812364	6.995315
-562.932972	-2.295842	7.005312
-561.376185	-6.407899	7.015309
-559.235104	-0.367025	7.025306
-557.407016	-1.629652	7.035302
-555.571672	-0.300684	7.045299
-553.740618	0.176300	7.055296
-552.006939	4.117422	7.065293
-550.050265	-4.596614	7.075290
-548.052242	-0.778246	7.085286
-545.919711	-2.397404	7.095283
-544.362237	-1.088781	7.105280
-542.617451	0.990487	7.115277
-540.610259	-0.291263	7.125274
-538.873376	2.750895	7.135270
-536.770936	2.600304	7.145267
-534.943530	5.302727	7.155264
-533.043577	-0.860014	7.165261
-530.990422	7.280823	7.175258
-529.421448	3.749495	7.185254
-527.544638	1.972242	7.195251
-525.544517	0.661633	7.205248
-523.667489	2.332932	7.215245
-522.033187	3.439816	7.225242
-519.951640	2.084625	7.235238
-517.808317	0.815889	7.245235
-516.269305	5.953452	7.255232
-514.669139	-0.219816	7.265229
-512.630638	7.144921	7.275226
-510.507884	-0.976639	7.285222
-508.807517	1.311864	7.295219
-506.611331	-5.851900	7.305216
-504.819471	-1.645285	7.315213
-502.910823	-0.616945	7.325210
-501.380477	4.360952	7.335206
-499.365697	4.848109	7.345203
-497.303228	3.363346	7.355200
-495.610837	-1.724061	7.365197
-493.656981	-1.216116	7.375194
-491.743531	-1.056995	7.385190
-489.900818	-2.122951	7.395187
-488.101241	-5.571076	7.405184
-486.229941	-3.046160	7.415181
-484.340250	-1.233161	7.425178
-482.200338	1.070428	7.435174
-480.597208	-2.813708	7.445171
-478.845367	2.171462	7.455168
-476.415660	-0.657259	7.465165
-474.827776	-1.055632	7.475162
-473.376243	4.275939	7.485158
-471.287264	6.372927	7.495155
-469.180098	-5.480499	7.505152
-467.604042	1.081775	7.515149
-465.244947	4.482535	7.525146
-463.476224	7.614408	7.535142
-461.678657	-3.341634	7.545139
-460.195427	-0.211538	7.555136
-458.263186	-1.910744	7.565133
-456.196800	0.262500	7.575130
-454.303604	2.341819	7.585126
-452.252111	3.753197	7.595123
-450.251960	10.276182	7.605120
-448.614920	4.902366	7.615117
-446.926646	9.455589	7.625114
-445.063118	8.608985	7.635110
-443.051145	2.314730	7.645107
-441.004983	5.901286	7.655104
-439.117214	5.436098	7.665101
-437.502238	0.414778	7.675098
-435.399828	1.505393	7.685094
-433.765761	2.144985	7.695091
-431.661947	1.198439	7.705088
-429.895753	2.672765	7.715085
-427.943727	-3.679801	7.725082
-426.112677	3.165484	7.735078
-424.115466	4.874517	7.745075
-422.448595	5.338344	7.755072
-420.566477	0.269638	7.765069
-418.652618	7.564362	7.775066
-416.833040	2.395114	7.785062
-414.813929	3.191139	7.795059
-412.863408	-3.014326	7.805056
-410.939709	6.802113	7.815053
-409.494074	-2.534466	7.825050
-407.379705	7.000466	7.835046
-405.828695	5.763247	7.845043
-403.650297	-3.941399	7.855040
-401.654452	2.814431	7.865037
-399.998443	1.663087	7.875034
-397.783033	1.382469	7.885030
-395.946120	1.206501	7.895027
-394.348925	2.951009	7.905024
-392.663201	2.544962	7.915021
-390.470577	1.208463	7.925018
-388.440341	3.018048	7.935014
-386.571863	-4.091711	7.945011
-384.557171	-2.072791	7.955008
-383.101841	-1.001974	7.965005
-381.123987	5.112507	7.975002
-379.285281	8.733822	7.984998
-377.248704	6.127449	7.994995
-375.491007	1.833416	8.004992
-373.431983	-3.861950	8.014989
-372.022573	11.465328	8.024986
-369.794004	5.517091	8.034982
-368.015356	7.864256	8.044979
-365.989292	9.112393	8.054976
-364.487499	7.932009	8.064973
-362.381464	7.739942	8.074970
-360.296058	5.550545	8.084966
-358.566745	0.193635	8.094963
-356.736709	0.153013	8.104960
-354.803841	7.173165	8.114957
-353.120453	9.827671	8.124954
-351.293937	6.597982	8.134950
-349.048703	6.761090	8.144947
-347.098032	6.715426	8.154944
-345.706927	5.789579	8.164941
-343.677706	8.933642	8.174938
-341.626506	13.367421	8.184934
-339.573385	8.768864	8.194931
-337.909280	11.320665	8.204928
-336.013624	8.515760	8.214925
-334.258471	6.428060	8.224922
-332.287993	5.073392	8.234918
-330.627864	10.085955	8.244915
-328.422805	7.489042	8.254912
-326.638828	6.296790	8.264909
-325.033585	6.974219	8.274906
-322.875880	4.700676	8.284902
-321.143316	3.785071	8.294899
-319.215943	2.637831	8.304896
-317.312748	4.851462	8.314893
-315.523500	2.066719	8.324890
-313.573118	9.366759	8.334886
-311.619972	5.120518	8.344883
-309.814896	0.680012	8.354880
-307.739595	-1.000859	8.364877
-306.114045	7.505310	8.374874
-304.395702	3.784478	8.384870
-302.269472	4.043999	8.394867
-300.229059	6.038361	8.404864
-298.501011	6.238285	8.414861
-296.782546	8.650378	8.424858
-294.782417	11.336474	8.434854
-293.147408	8.216349	8.444851
-291.072727	0.461076	8.454848
-289.045852	8.416854	8.464845
-287.276693	4.552125	8.474842
-285.247395	2.750715	8.484838
-283.567551	3.460475	8.494835
-281.551509	2.082784	8.504832
-279.742785	1.366641	8.514829
-278.049854	0.866361	8.524826
-276.004978	2.828450	8.534822
-274.222909	4.349309	8.544819
-272.309148	2.629513	8.554816
-270.546461	5.201943	8.564813
-268.523468	-0.241262	8.574810
-266.747757	-2.513783	8.584807
-264.869791	-1.682468	8.594803
-262.938425	2.221005	8.604800
-260.678339	5.579354	8.614797
-259.263095	4.000723	8.624794
-257.366504	5.165404	8.634791
-255.366730	4.341411	8.644787
-253.222163	0.216249	8.654784
-251.696186	-2.362207	8.664781
-249.838036	4.123620	8.674778
-247.757839	0.133480	8.684775
-245.952923	3.408171	8.694771
-244.134238	1.905687	8.704768
-242.389503	2.608277	8.714765
-240.564458	-7.221426	8.724762
-238.423303	4.057377	8.734759
-236.558982	2.705518	8.744755
-234.866807	-0.763183	8.754752
-232.733742	-3.016923	8.764749
-231.331376	3.014270	8.774746
-229.132842	0.427962	8.784743
-227.248083	4.111524	8.794739
-225.359674	4.775406	8.804736
-223.312369	4.272291	8.814733
-221.570736	6.380726	8.824730
-219.830346	2.995923	8.834727
-217.741619	7.775946	8.844723
-215.693052	-3.106312	8.854720
-213.989352	-1.413419	8.864717
-212.313381	-3.365230	8.874714
-210.419609	-5.571286	8.884711
-208.464387	-0.814163	8.894707
-206.686691	-3.660145	8.904704
-204.725743	-9.966597	8.914701
-202.917093	-1.593792	8.924698
-200.977169	-9.308536	8.934695
-199.065195	-5.506132	8.944691
-197.201921	-3.210241	8.954688
-195.192371	-5.141063	8.964685
-193.406162	-3.328684	8.974682
-191.872488	1.983648	8.984679
-189.503802	5.638962	8.994675
-187.764330	-4.372852	9.004672
-186.363627	-0.049874	9.014669
-184.190394	-1.479414	9.024666
-182.003161	-1.834289	9.034663
-180.293309	-2.640375	9.044659
-178.193231	8.105019	9.054656
-176.887289	-1.949716	9.064653
-174.814534	-1.604176	9.074650
-172.912634	0.731363	9.084647
-170.803892	-0.241009	9.094643
-169.235527	-1.395580	9.104640
-167.074866	-1.886735	9.114637
-165.279299	-0.099513	9.124634
-163.385389	-1.512883	9.134631
-161.636699	0.959225	9.144627
-159.830908	-1.516978	9.154624
-158.009204	-2.124571	9.164621
-156.134811	3.949774	9.174618
-154.173023	-0.046659	9.184615
-152.372710	2.221420	9.194611
-150.049554	-0.681563	9.204608
-148.121358	-0.595578	9.214605
-146.654792	-1.544407	9.224602
-144.715107	-1.494992	9.234599
-143.156551	1.552235	9.244595
-140.995375	-0.322208	9.254592
-139.065933	-1.927555	9.264589
-136.993236	1.857151	9.274586
-135.330577	-1.951002	9.284583
-133.458904	5.015948	9.294579
-131.640862	-0.623406	9.304576
-129.646247	-4.394519	9.314573
-127.850140	-1.435716	9.324570
-126.097001	-2.534475	9.334567
-124.042666	0.953157	9.344563
-121.643698	0.076631	9.354560
-120.426847	-2.682960	9.364557
-118.636864	-6.323512	9.374554
-116.694319	-2.582762	9.384551
-114.549677	5.169639	9.394547
-112.703622	3.193913	9.404544
-111.118280	-0.415563	9.414541
-109.171023	0.055853	9.424538
-106.974961	-0.710912	9.434535
-105.153472	6.265649	9.444531
-103.500729	-6.642427	9.454528
-101.689679	0.155790	9.464525
-99.815402	2.648962	9.474522
-97.607245	6.033125	9.484519
-95.900212	2.465824	9.494515
-94.234127	-3.297688	9.504512
-91.935998	-0.139466	9.514509
-90.237052	3.709651	9.524506
-88.469929	4.408782	9.534503
-86.545572	1.755811	9.544499
-84.664669	4.416894	9.554496
-82.795554	1.493251	9.564493
-80.645376	4.147694	9.574490
-79.098158	6.952025	9.584487
-77.391417	4.180614	9.594483
-75.392387	1.111506	9.604480
-73.334025	-2.805530	9.614477
-71.612705	9.527320	9.624474
-69.930522	3.312808	9.634471
-67.666820	-2.550768	9.644467
-65.814619	10.617041	9.654464
-63.945484	10.529348	9.664461
-62.386576	7.037807	9.674458
-60.260263	4.310003	9.684455
-58.253062	12.733371	9.694451
-56.152338	1.895012	9.704448
-54.659442	3.361112	9.714445
-52.994278	-1.475337	9.724442
-50.930035	3.520333	9.734439
-49.107287	7.262885	9.744435
-47.189773	10.878210	9.754432
-45.095908	10.691518	9.764429
-43.274286	5.132182	9.774426
-41.728486	9.495268	9.784423
-39.434317	7.640751	9.794419
-37.656974	9.934689	9.804416
-35.928330	0.114175	9.814413
-34.198168	9.664974	9.824410
-32.047110	4.736813	9.834407
-30.336226	6.476065	9.844403
-28.533433	7.486934	9.854400
-26.359824	1.914094	9.864397
-24.672802	0.345929	9.874394
-22.683820	0.074929	9.884391
-21.120047	4.769916	9.894387
-19.242261	4.875097	9.904384
-16.938517	2.692214	9.914381
-15.322602	-2.262677	9.924378
-13.311914	5.598037	9.934375
-11.578677	4.745704	9.944371
-9.547085	8.226014	9.954368
-7.437427	3.541333	9.964365
-6.080773	14.366013	9.974362
-4.859648	40.093143	9.984359
-3.571835	68.686690	9.994355
-1.565398	114.173534	10.004352
0.000000	147.247474	10.009357
0.384731	181.817926	10.014362
0.766711	198.322393	10.019367
1.253448	210.512748	10.024371
1.216886	238.610574	10.029376
1.875848	259.142841	10.034381
2.137850	268.445261	10.039386
2.279279	267.735359	10.044391
2.551364	269.173047	10.049395
2.186118	273.997374	10.054400
2.619114	273.740885	10.059405
2.506052	279.398669	10.064410
2.802275	278.851743	10.069415
2.766424	286.107373	10.074419
2.497940	286.377541	10.079424
3.082394	285.164861	10.084429
2.878766	285.987687	10.089434
2.769951	288.914936	10.094439
2.892272	294.923132	10.099443
3.121193	309.881405	10.104448
2.850968	314.021920	10.109453
2.823770	315.579896	10.114458
3.430927	320.734860	10.119463
3.377711	324.654672	10.124467
3.108685	326.978242	10.129472
3.534818	326.008445	10.134477
3.179317	313.592537	10.139482
3.062954	319.309213	10.144487
3.371549	316.077756	10.149491
3.431044	334.513657	10.154496
3.628431	333.018918	10.159501
3.406008	337.612314	10.164506
3.602799	337.019741	10.169511
3.611312	335.115133	10.174515
3.440786	343.840005	10.179520
3.632699	343.226131	10.184525
3.908348	340.504581	10.189530
3.624593	342.907777	10.194535
3.974537	343.733776	10.199539
3.907354	358.931730	10.204544
3.850166	352.811104	10.209549
3.930186	361.149070	10.214554
3.973454	346.113127	10.219559
4.384498	353.187113	10.224563
3.787355	361.014889	10.229568
4.238540	352.972754	10.234573
4.035662	352.656834	10.239578
4.008859	354.848725	10.244583
3.974716	355.811688	10.249587
4.077962	369.722406	10.254592
3.858777	360.760536	10.259597
4.245252	371.706957	10.264602
3.988382	366.726844	10.269607
4.242627	376.670854	10.274611
4.358077	399.267640	10.279616
4.714094	393.364957	10.284621
4.517799	405.308013	10.289626
4.497216	406.723008	10.294631
4.829226	403.842635	10.299635
4.411105	403.537391	10.304640
4.675158	406.033002	10.309645
4.714432	397.050385	10.314650
4.918716	397.461199	10.319655
4.932642	403.412609	10.324659
4.820463	401.552476	10.329664
4.835159	395.221657	10.334669
4.771553	411.176082	10.339674
4.926818	405.565630	10.344679
5.079491	406.352131	10.349683
4.914623	410.206191	10.354688
5.010865	405.083002	10.359693
4.903121	416.269149	10.364698
5.161867	428.043440	10.369703
5.589274	433.799589	10.374707
5.420258	443.937324	10.379712
5.557912	439.069310	10.384717
5.676267	441.208096	10.389722
5.712568	437.964849	10.394727
5.499396	423.594245	10.399731
5.548583	442.826765	10.404736
5.753619	442.100401	10.409741
5.608647	451.631869	10.414746
5.667389	441.562678	10.419751
5.714094	441.085512	10.424755
5.441465	453.802503	10.429760
5.731084	447.213328	10.434765
5.752061	448.657971	10.439770
5.399790	454.809748	10.444775
5.811920	455.302537	10.449779
5.576446	462.370885	10.454784
5.894698	456.868465	10.459789
6.449351	479.832166	10.464794
6.118530	475.717002	10.469799
6.529897	461.309824	10.474803
6.062167	464.513570	10.479808
6.126045	452.841257	10.484813
6.532482	471.844931	10.489818
6.532369	478.068288	10.494823
6.365425	467.771708	10.499827
6.348948	481.495035	10.504832
6.803280	488.462828	10.509837
6.540777	480.892457	10.514842
6.394771	487.047619	10.519847
6.773483	490.002806	10.524851
6.566032	501.550300	10.529856
6.810185	504.556918	10.534861
6.892410	507.086281	10.539866
6.624239	505.632667	10.544871
7.209099	503.833238	10.549875
6.947608	512.022323	10.554880
6.855255	506.061794	10.559885
7.048054	502.878732	10.564890
6.451730	505.743427	10.569895
6.793007	509.829038	10.574899
6.665442	516.454391	10.579904
7.196475	501.092886	10.584909
6.992661	507.127958	10.589914
7.184604	508.949065	10.594919
7.214524	511.668135	10.599923
7.089052	508.945876	10.604928
7.540259	530.533607	10.609933
7.674992	533.800553	10.614938
7.450004	537.328320	10.619943
7.460908	521.918861	10.624947
7.551489	529.081900	10.629952
7.355152	539.847002	10.634957
7.778645	546.603684	10.639962
7.726952	548.212903	10.644967
8.160216	552.518838	10.649971
7.600518	545.588816	10.654976
7.636883	533.602259	10.659981
7.643177	542.470945	10.664986
7.626164	543.418571	10.669991
7.757354	548.348319	10.674995
7.455836	560.358751	10.680000
7.840188	547.359393	10.685005
7.710039	554.193349	10.690010
7.841834	559.441572	10.695015
8.345065	567.680610	10.700019
8.409593	580.965300	10.705024
8.592807	575.014408	10.710029
8.383310	569.892616	10.715034
8.192741	566.975710	10.720039
8.117774	568.024052	10.725043
8.237056	586.054890	10.730048
8.746976	595.280126	10.735053
8.582693	588.359557	10.740058
8.602249	589.487448	10.745063
8.444723	590.859645	10.750067
8.600146	588.720242	10.755072
8.653482	591.785703	10.760077
8.610683	595.978337	10.765082
8.763018	593.577631	10.770087
8.827074	593.988740	10.775091
8.795926	597.823097	10.780096
8.573156	600.457900	10.785101
8.806134	604.343177	10.790106
8.926871	600.406706	10.795111
8.847106	600.077450	10.800115
8.720682	614.854579	10.805120
9.047573	609.861698	10.810125
9.310581	628.779638	10.815130
9.128707	629.980666	10.820135
9.370937	624.791532	10.825139
9.408820	643.858950	10.830144
9.500694	630.535556	10.835149
9.517304	631.186065	10.840154
9.368622	635.215813	10.845159
9.838108	626.648596	10.850163
9.495843	631.212309	10.855168
9.601360	619.452789	10.860173
9.358124	629.624571	10.865178
9.520216	639.618157	10.870183
9.444854	636.323286	10.875187
9.578764	638.369726	10.880192
9.756154	635.067658	10.885197
9.770309	643.145034	10.890202
9.484183	636.769046	10.895207
10.073000	636.404114	10.900211
9.822031	639.760994	10.905216
9.930316	641.103413	10.910221
9.925691	636.868358	10.915226
9.677874	645.332902	10.920231
10.050985	655.551481	10.925235
9.754551	672.205705	10.930240
9.981455	671.709250	10.935245
10.222058	689.987393	10.940250
10.036058	678.908314	10.945255
10.289139	674.573789	10.950259
10.111157	680.994353	10.955264
10.311056	678.179159	10.960269
10.459900	682.304976	10.965274
10.474453	682.367563	10.970279
10.554475	677.119121	10.975283
10.539408	687.470609	10.980288
10.894788	693.675205	10.985293
10.910555	688.190983	10.990298
10.568187	687.966696	10.995303
10.986714	688.672958	11.000307
10.721124	689.474147	11.005312
11.006174	704.647820	11.010317
10.953180	702.049594	11.015322
10.920318	714.656021	11.020327
11.399220	705.420148	11.025331
11.004107	699.872139	11.030336
11.240659	687.230574	11.035341
11.020583	693.189462	11.040346
11.309927	700.623683	11.045351
11.595643	701.201306	11.050355
11.051917	695.990844	11.055360
11.224522	702.412271	11.060365
11.501771	700.994651	11.065370
11.526359	714.265331	11.070375
11.430669	713.356667	11.075379
11.573036	723.591597	11.080384
11.714687	717.618889	11.085389
11.490079	711.912780	11.090394
11.737762	709.585164	11.095399
12.013725	711.353469	11.100403
11.505129	703.562014	11.105408
11.491812	708.792433	11.110413
11.549739	719.726863	11.115418
11.219777	713.055032	11.120423
11.612421	718.392604	11.125427
11.603503	719.427267	11.130432
11.637950	722.700790	11.135437
12.122695	729.321621	11.140442
12.046530	739.595363	11.145447
12.236335	737.252529	11.150451
12.441725	745.888503	11.155456
12.429611	725.822979	11.160461
12.085537	715.822582	11.165466
12.107726	721.610364	11.170471
12.393740	719.268747	11.175475
12.484867	737.961910	11.180480
12.758684	733.100467	11.185485
12.343439	729.635841	11.190490
12.364425	753.305684	11.195495
13.064971	735.621436	11.200499
12.451172	730.333820	11.205504
12.588932	730.256896	11.210509
12.906132	736.256270	11.215514
12.290367	740.124774	11.220519
12.714577	738.405353	11.225523
12.717773	749.499147	11.230528
13.105705	748.392693	11.235533
12.946163	750.339287	11.240538
12.863305	757.164218	11.245543
13.278513	748.085936	11.250547
12.925556	762.659630	11.255552
12.803030	755.465792	11.260557
13.076692	758.253272	11.265562
13.030367	762.844733	11.270567
13.073254	754.566280	11.275571
12.921752	764.096628	11.280576
13.103763	758.741207	11.285581
13.056333	760.065893	11.290586
13.001160	764.475034	11.295591
13.332784	770.856933	11.300595
13.386745	786.568281	11.305600
13.569119	781.898042	11.310605
13.438630	784.298153	11.315610
13.390518	789.125683	11.320615
13.804793	780.228897	11.325619
13.867601	783.769958	11.330624
13.883580	781.671695	11.335629
13.846652	778.201912	11.340634
13.616374	793.435797	11.345639
13.764578	782.478389	11.350643
13.730304	788.576429	11.355648
13.780327	775.662526	11.360653
13.912094	787.138790	11.365658
13.883848	791.516045	11.370663
13.987232	790.405296	11.375667
13.756872	789.703417	11.380672
14.253009	793.900039	11.385677
14.692339	806.342123	11.390682
14.304089	800.263074	11.395687
14.558289	793.010705	11.400691
14.189760	792.877328	11.405696
14.266139	780.797444	11.410701
14.291220	788.380316	11.415706
14.514742	806.608497	11.420711
14.770814	813.815461	11.425715
14.542054	823.041173	11.430720
14.577825	815.661980	11.435725
14.682366	816.506650	11.440730
14.729342	825.505438	11.445735
14.888151	819.482639	11.450739
14.840024	820.626864	11.455744
15.110255	822.440255	11.460749
14.884027	820.417682	11.465754
14.785058	815.824638	11.470759
15.075407	813.099080	11.475763
14.992925	824.293338	11.480768
14.890241	822.859031	11.485773
15.228177	822.156398	11.490778
15.019346	828.363518	11.495783
15.224055	823.211842	11.500787
14.820156	822.310539	11.505792
15.029208	820.460620	11.510797
14.996612	820.309145	11.515802
14.997600	818.688764	11.520807
15.120426	815.299944	11.525811
15.082977	822.502475	11.530816
15.369422	833.104834	11.535821
15.519399	836.759751	11.540826
15.573728	840.795023	11.545831
15.477565	829.479917	11.550835
15.425333	834.371991	11.555840
15.748792	832.132416	11.560845
15.570788	843.517772	11.565850
15.702852	837.251626	11.570855
15.999187	829.165328	11.575859
15.761395	842.190943	11.580864
15.729451	837.344328	11.585869
15.841341	836.937184	11.590874
16.073035	837.845948	11.595879
16.024691	843.024438	11.600883
15.840583	843.890704	11.605888
16.086028	837.552852	11.610893
15.909131	862.085569	11.615898
16.149343	862.441777	11.620903
16.313074	856.375596	11.625907
16.358762	868.561946	11.630912
16.472764	866.190967	11.635917
16.697136	873.253981	11.640922
16.638324	878.231495	11.645927
16.812733	864.636077	11.650931
16.479248	866.989725	11.655936
16.868891	865.777324	11.660941
16.663788	865.097434	11.665946
16.458058	857.955455	11.670951
16.815510	859.807773	11.675955
16.649010	867.349485	11.680960
16.679857	860.019945	11.685965
16.824234	864.748982	11.690970
16.501346	869.576208	11.695975
16.886541	862.750019	11.700979
16.750015	870.585814	11.705984
16.665331	859.171072	11.710989
17.001442	861.239703	11.715994
16.803867	862.742903	11.720999
17.253674	864.265069	11.726003
16.935102	867.492421	11.731008
16.905652	879.869767	11.736013
17.189352	892.167209	11.741018
17.116385	896.355279	11.746023
17.524976	896.086907	11.751027
17.351634	907.816956	11.756032
17.465494	899.486096	11.761037
17.079118	902.908792	11.766042
17.159097	910.084750	11.771047
17.432011	902.899523	11.776051
17.259654	914.373140	11.781056
17.468162	922.001737	11.786061
17.557402	931.205971	11.791066
17.622936	936.796883	11.796071
17.965331	933.054437	11.801075
17.722681	942.315559	11.806080
18.106452	935.180450	11.811085
18.097001	937.021907	11.816090
17.970214	944.925581	11.821095
18.150365	941.163275	11.826099
17.987707	945.351471	11.831104
18.023448	945.431970	11.836109
18.061871	937.742389	11.841114
18.171148	943.767918	11.846119
18.208337	937.948992	11.851123
17.679985	941.524454	11.856128
18.138717	936.940986	11.861133
18.174216	937.388203	11.866138
17.883792	954.792495	11.871143
18.352580	963.388163	11.876147
18.694281	963.169099	11.881152
18.786607	966.464987	11.886157
18.708543	969.726546	11.891162
18.746397	971.547845	11.896167
18.863053	960.216039	11.901171
18.671102	972.960041	11.906176
19.393532	966.641468	11.911181
19.072656	962.234388	11.916186
19.137458	957.816259	11.921191
19.166634	946.842228	11.926195
18.864108	944.283760	11.931200
19.036133	935.538283	11.936205
18.827449	936.573283	11.941210
18.851847	941.487079	11.946215
18.987731	947.968094	11.951219
18.994230	965.175212	11.956224
19.585080	967.969706	11.961229
19.380639	976.163355	11.966234
19.316559	976.767608	11.971239
19.576006	967.755041	11.976243
19.356290	968.208269	11.981248
19.651864	964.992944	11.986253
19.580945	968.548284	11.991258
19.335585	974.497913	11.996263
19.430723	967.356782	12.001267
19.321662	975.578588	12.006272
19.624649	968.545456	12.011277
19.453887	973.890979	12.016282
19.495179	971.738971	12.021287
19.703959	965.369850	12.026291
19.257780	982.799019	12.031296
19.512913	961.793163	12.036301
19.523189	972.043030	12.041306
19.451683	971.543696	12.046311
19.639693	968.231186	12.051315
19.210542	979.626742	12.056320
19.180308	991.956205	12.061325
19.628121	996.510717	12.066330
19.838282	1000.404471	12.071335
19.987937	998.376328	12.076339
19.726923	1005.806229	12.081344
19.931469	993.499912	12.086349
19.941705	974.159899	12.091354
19.475428	976.328931	12.096359
19.908486	971.121066	12.101363
19.529216	979.828356	12.106368
19.840638	973.604514	12.111373
20.048345	968.862359	12.116378
19.631600	975.048293	12.121383
19.808879	971.933845	12.126387
19.590996	981.963040	12.131392
19.677187	982.200301	12.136397
19.630131	978.012920	12.141402
19.763772	976.775104	12.146407
19.893329	975.548192	12.151411
19.564049	982.638060	12.156416
19.591606	976.587241	12.161421
19.854559	972.146966	12.166426
19.728400	984.037513	12.171431
19.745314	978.053053	12.176435
19.509687	975.433440	12.181440
19.740197	975.674493	12.186445
19.659379	980.637415	12.191450
19.608584	990.762981	12.196455
20.018771	980.674424	12.201459
19.895375	980.966406	12.206464
19.947048	991.499873	12.211469
20.119959	980.178792	12.216474
19.752437	973.555412	12.221479
19.629415	954.749243	12.226483
19.363526	964.626007	12.231488
19.540251	956.173112	12.236493
19.523339	963.142966	12.241498
19.661319	986.215726	12.246503
19.895716	981.802870	12.251507
19.752598	983.561564	12.256512
19.489539	964.441004	12.261517
19.291131	964.730756	12.266522
19.351130	981.179441	12.271527
19.960557	980.536011	12.276531
19.871741	990.203968	12.281536
19.998993	985.057493	12.286541
19.847975	966.665825	12.291546
19.708037	963.606707	12.296551
20.306460	954.929627	12.301555
19.688106	971.319327	12.306560
20.088420	956.422154	12.311565
19.791887	970.724465	12.316570
19.466794	961.586707	12.321575
19.698811	953.366294	12.326579
19.508344	963.860296	12.331584
19.760409	963.563267	12.336589
19.845631	964.033307	12.341594
19.616572	966.288305	12.346599
19.833366	963.837041	12.351603
19.757135	959.379112	12.356608
19.882474	969.485243	12.361613
19.916868	962.959415	12.366618
19.866279	962.889664	12.371623
20.073770	959.710469	12.376627
19.347422	951.945725	12.381632
19.532049	933.991044	12.386637
19.596357	945.146999	12.391642
19.596395	962.261307	12.396647
20.047090	957.509575	12.401651
19.705374	947.613518	12.406656
19.451694	941.461689	12.411661
19.530463	946.768190	12.416666
19.696775	960.269616	12.421671
19.763198	960.808104	12.426675
19.492464	958.258756	12.431680
19.611122	967.368426	12.436685
19.715626	976.921951	12.441690
19.256043	972.656065	12.446695
19.588691	967.626660	12.451699
19.581218	976.354289	12.456704
19.948132	979.942309	12.461709
20.069498	975.065674	12.466714
19.705743	962.735688	12.471719
19.677009	948.083596	12.476723
19.413535	954.301850	12.481728
19.731437	962.967321	12.486733
19.697016	968.050586	12.491738
19.531010	961.248397	12.496743
19.342841	962.084564	12.501747
19.502583	981.834016	12.506752
19.506926	970.187345	12.511757
19.874979	978.228173	12.516762
19.908562	980.342710	12.521767
20.057727	969.174464	12.526771
19.614324	963.864313	12.531776
19.808480	950.003076	12.536781
19.675607	949.829743	12.541786
19.468620	950.761961	12.546791
19.652626	943.631900	12.551795
19.571712	954.918269	12.556800
19.648608	959.355294	12.561805
20.087834	960.861811	12.566810
19.445039	952.515189	12.571815
19.811271	947.251753	12.576819
19.523859	950.206832	12.581824
19.708405	947.200050	12.586829
19.715517	953.595941	12.591834
19.293646	956.432104	12.596839
19.498044	962.880118	12.601843
19.596391	980.525237	12.606848
19.669639	981.842523	12.611853
19.534811	989.571655	12.616858
19.732172	989.386653	12.621863
20.140369	978.606059	12.626867
19.587634	973.405605	12.631872
19.956523	959.177409	12.636877
19.936487	960.996112	12.641882
19.427027	963.117619	12.646887
20.058095	953.157870	12.651891
19.712624	956.365086	12.656896
19.495502	950.415601	12.661901
19.745605	949.384739	12.666906
19.701520	953.049347	12.671911
19.752861	954.202951	12.676915
19.725590	962.042659	12.681920
19.577090	959.602348	12.686925
20.079507	949.372932	12.691930
19.815842	955.878253	12.696935
19.977998	958.382329	12.701939
19.808632	959.142160	12.706944
20.215133	957.109329	12.711949
19.973176	949.254707	12.716954
19.951572	932.447154	12.721959
19.807718	924.203123	12.726963
19.289374	931.137812	12.731968
19.179990	923.790392	12.736973
19.658381	940.077669	12.741978
19.964017	947.562252	12.746983
19.385511	925.817271	12.751987
19.533277	947.651164	12.756992
19.827521	956.335388	12.761997
19.890720	953.111393	12.767002
19.716137	939.537663	12.772007
19.914167	933.398163	12.777011
19.578944	932.196497	12.782016
19.698706	934.690772	12.787021
19.645343	933.883374	12.792026
19.589536	929.364632	12.797031
19.715657	928.402437	12.802035
19.379938	929.188801	12.807040
19.513755	935.096072	12.812045
19.580922	938.213021	12.817050
19.532860	955.316856	12.822055
19.662355	957.890014	12.827059
19.638688	963.974607	12.832064
19.323539	964.480120	12.837069
19.975631	964.668122	12.842074
20.040142	961.927303	12.847079
19.589586	943.984028	12.852083
19.593391	947.977711	12.857088
19.496228	945.585990	12.862093
19.741629	952.913010	12.867098
19.810021	960.351853	12.872103
19.754162	948.501103	12.877107
19.497140	943.707701	12.882112
19.488704	944.010523	12.887117
19.692944	949.461820	12.892122
19.825126	954.140786	12.897127
19.698327	945.999689	12.902131
19.675839	945.356117	12.907136
19.874079	940.132885	12.912141
19.455012	942.427648	12.917146
19.392671	950.280040	12.922151
19.765765	951.916176	12.927155
19.661365	962.959480	12.932160
19.820535	958.868533	12.937165
19.609626	954.625284	12.942170
19.445368	947.646974	12.947175
19.617469	953.612019	12.952179
19.629804	970.625805	12.957184
19.950064	964.600062	12.962189
19.805366	952.691719	12.967194
19.496603	949.698172	12.972199
19.638673	943.100768	12.977203
19.715316	939.273752	12.982208
19.618098	940.671846	12.987213
19.663283	946.210019	12.992218
19.315474	943.077606	12.997223
19.588020	957.457097	13.002227
19.514259	970.259523	13.007232
19.771202	967.510877	13.012237
20.089717	974.013241	13.017242
19.637787	966.799292	13.022247
19.634028	941.485860	13.027251
19.481853	954.496342	13.032256
19.552435	957.381703	13.037261
20.202517	969.265133	13.042266
19.711527	961.932035	13.047271
19.604940	945.403767	13.052275
19.395121	944.450996	13.057280
19.686728	939.833465	13.062285
19.687296	941.320052	13.067290
19.384836	947.308743	13.072295
20.188843	959.463322	13.077299
19.378087	953.580134	13.082304
19.357306	952.821160	13.087309
19.509592	967.807319	13.092314
19.722446	973.796625	13.097319
20.012495	971.541067	13.102323
19.498650	974.130890	13.107328
19.646409	970.031510	13.112333
19.792573	973.292790	13.117338
19.588886	964.283914	13.122343
19.821177	956.884344	13.127347
19.769496	952.292389	13.132352
19.596107	952.970064	13.137357
19.633326	958.224843	13.142362
19.246680	952.166765	13.147367
19.764357	964.523153	13.152371
19.708734	980.728478	13.157376
19.693905	979.599508	13.162381
19.891620	968.993646	13.167386
19.634673	970.263451	13.172391
19.628183	952.793441	13.177395
19.366272	961.585301	13.182400
19.669314	960.644564	13.187405
19.800523	970.503730	13.192410
19.516864	966.536248	13.197415
20.078410	964.313087	13.202419
19.385296	961.790893	13.207424
19.128797	962.383255	13.212429
19.660580	970.662130	13.217434
19.554998	981.025898	13.222439
19.929700	982.697266	13.227443
20.022358	980.548104	13.232448
19.833046	973.231544	13.237453
19.494855	957.996377	13.242458
19.337091	969.593880	13.247463
19.770314	967.839877	13.252467
19.734088	984.305491	13.257472
19.660824	986.470979	13.262477
19.767446	976.753365	13.267482
19.463407	977.721567	13.272487
20.007663	970.810816	13.277491
19.787388	975.815694	13.282496
19.846511	960.237214	13.287501
19.585680	956.272402	13.292506
19.462076	963.057403	13.297511
19.671374	959.609810	13.302515
19.483931	963.052045	13.307520
19.523955	957.877699	13.312525
19.736766	966.403800	13.317530
19.764263	981.446939	13.322535
19.904345	969.213221	13.327539
19.678322	966.868862	13.332544
19.811660	954.969791	13.337549
19.393472	964.582235	13.342554
19.723576	972.054254	13.347559
19.913109	952.842593	13.352563
19.541613	964.597986	13.357568
19.955046	960.707782	13.362573
20.059562	955.418272	13.367578
19.788787	957.871541	13.372583
19.585381	953.379488	13.377587
19.699003	962.706023	13.382592
19.731389	962.929786	13.387597
19.807247	961.526128	13.392602
19.520463	958.587427	13.397607
19.587032	956.434544	13.402611
19.554691	960.836948	13.407616
19.764620	965.080850	13.412621
19.383500	967.945212	13.417626
19.424651	969.713152	13.422631
19.722296	959.652811	13.427635
19.630169	963.219418	13.432640
19.890410	964.122849	13.437645
19.753058	963.323326	13.442650
19.610976	969.690188	13.447655
19.672157	957.168624	13.452659
19.616566	964.677713	13.457664
19.600815	967.416770	13.462669
20.219768	963.458299	13.467674
19.845143	972.540985	13.472679
19.501542	964.267284	13.477683
19.334398	969.074432	13.482688
19.774331	971.977373	13.487693
19.966123	966.640030	13.492698
19.760857	971.143356	13.497703
19.835299	973.120474	13.502707
19.974664	976.799198	13.507712
20.101590	963.498298	13.512717
19.893928	958.041727	13.517722
19.568094	945.085900	13.522727
19.479151	941.357842	13.527731
19.446204	935.561144	13.532736
19.581605	957.598894	13.537741
19.786847	968.944510	13.542746
19.523172	972.996634	13.547751
19.531927	967.019789	13.552755
19.656117	978.865669	13.557760
19.746786	968.611231	13.562765
19.873479	982.842105	13.567770
19.626282	970.573954	13.572775
19.839239	957.875989	13.577779
19.437902	953.074849	13.582784
19.606411	965.718767	13.587789
19.901493	964.484379	13.592794
19.568137	956.749210	13.597799
19.788044	950.816759	13.602803
19.748733	947.248745	13.607808
19.592247	940.847212	13.612813
19.730309	934.145573	13.617818
19.288511	943.704205	13.622823
19.926405	953.048834	13.627827
19.287662	953.390684	13.632832
19.581155	968.152449	13.637837
19.964356	971.770199	13.642842
19.605804	970.089654	13.647847
19.661671	954.501447	13.652851
19.900659	961.662320	13.657856
19.583573	946.571259	13.662861
19.625881	949.057388	13.667866
19.418334	943.426532	13.672871
19.859118	949.982719	13.677875
19.690366	958.460856	13.682880
19.715754	954.460642	13.687885
19.560636	953.400576	13.692890
19.737992	948.932955	13.697895
19.493783	945.728818	13.702899
19.431879	945.507103	13.707904
19.768209	967.018394	13.712909
19.820311	967.018216	13.717914
19.572291	954.763615	13.722919
19.931611	957.502775	13.727923
19.423618	953.697248	13.732928
19.861901	943.039628	13.737933
20.042953	942.857228	13.742938
19.614181	949.972413	13.747943
19.583121	943.786651	13.752947
19.468831	943.872155	13.757952
19.876179	947.965491	13.762957
19.679936	944.974500	13.767962
19.760810	949.561502	13.772967
19.691897	938.956396	13.777971
19.429829	945.516656	13.782976
19.845506	946.872370	13.787981
19.862623	944.287362	13.792986
19.687357	951.516670	13.797991
19.700957	943.140269	13.802995
19.617896	946.560332	13.808000
19.507679	954.063146	13.813005
19.666184	946.037407	13.818010
19.725127	954.204016	13.823015
19.864245	949.608440	13.828019
19.349653	964.449414	13.833024
19.458794	953.386133	13.838029
19.439064	951.035683	13.843034
19.433150	952.460220	13.848039
19.636517	951.820840	13.853043
19.424399	959.293385	13.858048
19.784099	968.868497	13.863053
19.946747	966.919508	13.868058
19.844096	970.371877	13.873063
19.940375	951.617474	13.878067
19.624729	963.994804	13.883072
19.380212	953.845096	13.888077
19.608275	956.557090	13.893082
19.425530	962.764048	13.898087
19.716747	956.265864	13.903091
19.787241	956.813166	13.908096
19.978998	951.528667	13.913101
19.632301	952.889277	13.918106
19.503439	957.756553	13.923111
19.944531	947.786104	13.928115
19.791476	955.953409	13.933120
19.435535	955.258934	13.938125
19.574161	951.408623	13.943130
19.517581	956.710694	13.948135
19.693912	951.325355	13.953139
19.434067	958.222768	13.958144
19.831595	951.251054	13.963149
19.654845	954.552008	13.968154
19.483627	960.590741	13.973159
19.829217	949.539428	13.978163
19.799329	961.344420	13.983168
19.529957	948.084665	13.988173
19.554417	952.903828	13.993178
19.563422	955.195764	13.998183
19.776459	953.495809	14.003187
19.773504	955.378026	14.008192
19.645637	963.229001	14.013210
19.810210	955.287196	14.018227
19.533828	964.825142	14.023245
20.177062	952.511661	14.028263
20.127212	953.995420	14.033280
20.107079	959.742239	14.038298
20.205105	949.120278	14.043315
19.940235	951.073293	14.048333
20.197676	946.597147	14.053351
20.227505	954.276403	14.058368
19.933858	940.683213	14.063386
19.572710	945.572027	14.068403
19.451447	943.120291	14.073421
19.648183	949.291857	14.078439
19.858581	955.711368	14.083456
19.864551	966.270836	14.088474
19.803211	956.819500	14.093491
19.477655	963.232475	14.098509
19.748727	960.283197	14.103527
19.923352	964.220572	14.108544
19.775368	960.358884	14.113562
19.839327	956.991951	14.118579
19.598734	964.059152	14.123597
19.988650	968.347597	14.128615
19.992092	983.968123	14.133632
19.691284	998.477823	14.138650
19.890414	988.699404	14.143667
19.624006	996.680774	14.148685
19.849799	998.258218	14.153703
19.931567	999.945154	14.158720
19.866647	994.687456	14.163738
20.234415	994.333302	14.168755
19.833119	1003.367356	14.173773
20.040396	1009.587605	14.178791
20.264983	1026.547791	14.183808
20.062358	1022.913463	14.188826
20.332108	1033.059654	14.193843
20.707116	1038.989668	14.198861
20.592259	1034.224436	14.203879
20.421400	1032.981657	14.208896
20.542346	1020.904016	14.213914
20.552394	1009.263304	14.218931
20.002831	1012.509204	14.223949
20.440346	1011.222088	14.228967
20.428782	1024.934524	14.233984
20.639965	1033.863826	14.239002
20.892217	1031.089790	14.244019
20.379177	1013.499670	14.249037
20.602537	1001.514254	14.254055
20.436524	1006.483653	14.259072
20.617395	1010.816465	14.264090
20.699681	1006.790615	14.269107
20.385917	1008.889083	14.274125
20.667704	1021.746153	14.279143
20.736839	1027.788661	14.284160
20.594318	1035.364883	14.289178
20.675805	1027.621131	14.294195
20.333597	1032.150646	14.299213
20.764710	1035.635764	14.304231
20.775101	1037.031268	14.309248
20.495552	1035.345693	14.314266
20.881662	1039.243851	14.319283
20.595921	1042.011140	14.324301
20.688374	1038.599529	14.329319
20.689459	1040.540811	14.334336
20.594678	1028.772079	14.339354
20.595208	1032.786007	14.344371
20.388983	1033.372880	14.349389
20.704018	1026.660799	14.354407
20.910199	1029.614690	14.359424
20.428890	1034.185270	14.364442
20.779059	1042.014047	14.369459
20.752860	1068.043888	14.374477
21.100719	1070.747877	14.379495
21.003391	1065.301830	14.384512
21.195659	1065.922676	14.389530
21.656567	1063.699760	14.394547
21.050050	1053.419773	14.399565
21.032275	1042.038316	14.404583
21.070022	1037.723032	14.409600
20.627934	1039.551735	14.414618
21.341507	1048.826436	14.419635
21.446807	1067.849944	14.424653
21.280442	1052.402109	14.429671
21.278032	1051.012905	14.434688
21.287649	1038.794909	14.439706
21.154547	1030.865936	14.444723
20.960637	1042.367378	14.449741
21.304590	1050.991569	14.454759
21.453479	1065.582197	14.459776
21.346439	1066.225614	14.464794
21.787892	1057.744850	14.469811
21.710993	1049.685772	14.474829
21.423349	1035.618032	14.479847
21.419012	1037.148813	14.484864
21.332239	1032.960362	14.489882
21.425800	1032.800961	14.494899
21.128971	1037.579655	14.499917
21.226401	1031.557477	14.504935
21.226437	1036.321068	14.509952
21.144634	1062.804170	14.514970
21.635370	1052.355461	14.519987
21.732565	1068.871164	14.525005
21.880886	1063.374925	14.530023
21.595107	1052.641851	14.535040
21.605801	1057.276328	14.540058
21.772340	1061.145016	14.545075
21.524063	1066.296665	14.550093
21.507364	1064.375670	14.555111
21.886697	1062.525221	14.560128
21.534349	1072.556724	14.565146
21.690464	1061.412583	14.570163
21.350020	1070.661140	14.575181
21.453371	1071.687084	14.580199
21.447998	1053.838181	14.585216
21.557801	1073.432800	14.590234
21.900252	1072.010611	14.595251
21.585132	1072.462263	14.600269
21.719183	1063.942433	14.605287
21.842546	1069.152002	14.610304
21.449848	1068.849140	14.615322
21.959292	1073.185408	14.620339
21.950945	1083.256434	14.625357
21.875609	1088.849293	14.630375
22.149618	1093.779999	14.635392
21.628210	1097.486279	14.640410
22.123277	1095.265776	14.645427
22.200287	1101.699549	14.650445
22.221789	1092.422112	14.655463
22.362874	1085.568641	14.660480
22.040996	1079.006106	14.665498
22.151891	1073.532350	14.670515
21.833798	1080.952546	14.675533
22.163184	1087.005480	14.680551
22.166418	1098.013028	14.685568
22.255144	1092.857423	14.690586
22.494908	1090.525838	14.695603
22.144319	1086.797897	14.700621
22.180522	1093.447398	14.705639
22.213684	1093.613825	14.710656
21.966105	1097.705887	14.715674
22.317582	1082.610386	14.720691
22.271962	1098.631351	14.725709
22.421620	1096.039630	14.730727
22.243208	1088.986207	14.735744
21.994969	1095.310612	14.740762
22.140037	1095.975955	14.745779
22.259348	1101.164158	14.750797
22.294771	1089.279437	14.755815
22.672450	1089.937567	14.760832
22.487507	1098.940317	14.765850
22.869934	1094.869715	14.770867
22.683802	1100.744532	14.775885
22.825168	1095.930546	14.780903
22.836251	1091.348138	14.785920
22.776227	1093.457271	14.790938
22.644061	1090.270248	14.795955
22.543199	1100.035129	14.800973
22.472300	1097.672866	14.805991
22.474990	1102.111208	14.811008
22.589268	1101.369598	14.816026
22.631697	1098.586543	14.821043
22.692298	1101.540074	14.826061
22.571834	1104.036394	14.831079
22.647991	1089.581795	14.836096
22.544164	1098.909825	14.841114
22.534464	1098.707116	14.846131
22.699384	1124.748262	14.851149
22.926650	1121.636829	14.856167
22.946104	1119.159472	14.861184
22.843523	1129.063867	14.866202
23.001232	1126.598278	14.871219
23.046168	1126.176844	14.876237
23.071829	1129.082467	14.881255
23.017531	1134.837950	14.886272
22.787449	1135.830562	14.891290
22.952854	1126.633976	14.896307
22.964266	1128.948022	14.901325
23.009350	1124.605586	14.906343
23.063767	1122.142315	14.911360
23.303597	1132.035357	14.916378
23.512883	1126.592295	14.921395
23.446656	1122.079627	14.926413
23.128339	1119.977059	14.931431
23.252742	1103.895234	14.936448
23.399675	1116.526134	14.941466
23.501472	1101.424031	14.946483
23.437046	1102.809452	14.951501
23.200474	1095.149431	14.956519
23.315259	1088.712307	14.961536
23.182885	1092.001011	14.966554
23.081524	1087.733857	14.971571
23.140621	1099.128132	14.976589
23.513646	1127.790710	14.981607
23.197005	1118.218747	14.986624
23.430073	1116.176105	14.991642
23.754377	1120.076277	14.996659
23.714786	1115.870838	15.001677
23.333922	1116.113528	15.006695
23.879841	1114.487413	15.011712
23.738258	1108.314554	15.016730
23.401756	1099.258605	15.021747
23.824681	1095.447399	15.026765
23.238360	1103.844029	15.031783
23.725430	1107.586882	15.036800
23.623227	1116.917023	15.041818
23.729987	1117.710394	15.046835
23.838503	1118.306846	15.051853
23.545846	1125.383216	15.056871
23.927312	1119.076585	15.061888
23.822007	1122.017254	15.066906
23.931176	1126.553457	15.071923
24.106916	1122.648743	15.076941
23.624264	1104.591958	15.081959
23.643804	1110.610162	15.086976
23.583561	1119.212342	15.091994
23.851299	1127.486919	15.097011
23.872675	1120.866468	15.102029
23.755361	1127.214051	15.107047
23.774395	1125.373083	15.112064
23.811982	1129.925424	15.117082
24.017329	1120.593475	15.122099
23.892672	1119.582432	15.127117
23.932131	1122.532260	15.132135
23.800403	1121.144012	15.137152
23.713593	1133.029586	15.142170
23.725245	1122.657242	15.147187
23.851713	1131.791249	15.152205
24.126408	1149.242263	15.157223
24.225984	1147.365635	15.162240
24.089021	1153.908283	15.167258
24.002552	1154.187393	15.172275
24.304072	1149.479199	15.177293
24.189360	1153.117477	15.182311
24.515406	1140.825329	15.187328
24.564829	1143.464455	15.192346
24.570465	1143.438634	15.197363
24.523625	1150.217030	15.202381
24.059574	1152.035091	15.207399
24.233512	1154.556826	15.212416
23.739265	1156.533082	15.217434
24.574910	1150.932686	15.222451
24.493460	1157.160511	15.227469
24.459122	1163.481503	15.232487
24.671327	1159.779400	15.237504
24.371370	1159.430281	15.242522
24.636040	1160.032503	15.247539
24.821744	1152.121830	15.252557
24.451307	1159.975156	15.257575
24.733855	1160.600483	15.262592
24.592917	1157.145842	15.267610
24.475668	1164.626072	15.272627
24.396878	1149.572388	15.277645
24.353991	1161.451766	15.282663
24.578924	1164.343703	15.287680
24.604043	1163.142017	15.292698
24.461251	1155.103617	15.297715
24.760411	1174.922228	15.302733
24.611764	1190.541278	15.307751
24.838193	1178.845467	15.312768
25.012877	1193.793141	15.317786
25.094801	1190.320249	15.322803
25.474951	1183.548944	15.327821
25.025405	1175.707333	15.332839
25.188679	1157.419247	15.337856
24.861032	1159.589166	15.342874
24.840296	1155.158900	15.347891
25.151404	1159.340415	15.352909
24.765247	1170.060895	15.357927
25.409975	1170.305966	15.362944
25.185333	1164.283191	15.367962
25.069218	1167.579544	15.372979
25.237328	1150.590088	15.377997
25.125779	1153.131402	15.383015
25.087278	1157.132713	15.388032
25.265240	1172.044446	15.393050
25.477705	1180.273597	15.398067
25.484584	1161.112202	15.403085
25.248655	1164.797347	15.408103
25.108615	1150.122327	15.413120
25.056818	1157.017141	15.418138
25.442021	1177.094180	15.423155
25.699219	1179.163740	15.428173
25.312625	1173.291070	15.433191
25.269508	1160.872159	15.438208
25.136745	1182.000073	15.443226
25.363999	1182.609838	15.448243
25.733017	1184.080296	15.453261
25.368440	1192.909610	15.458279
25.632084	1186.443194	15.463296
25.439508	1186.055709	15.468314
25.376886	1188.403597	15.473331
25.576347	1190.457984	15.478349
25.724157	1189.439659	15.483367
25.563589	1189.847785	15.488384
25.415826	1188.105777	15.493402
25.511134	1189.000085	15.498419
25.548975	1179.613801	15.503437
25.259552	1186.714067	15.508455
25.208223	1180.576335	15.513472
25.592994	1195.147561	15.518490
25.576438	1218.887247	15.523507
26.014053	1213.777417	15.528525
26.021977	1217.678526	15.533543
26.154221	1215.599252	15.538560
26.420762	1213.372709	15.543578
26.209778	1203.905754	15.548595
26.047209	1186.394811	15.553613
25.604388	1194.240036	15.558631
25.807938	1197.494061	15.563648
26.019445	1207.176942	15.568666
26.022454	1209.898993	15.573683
25.991832	1213.052724	15.578701
25.890112	1209.325957	15.583719
26.203504	1212.516059	15.588736
26.140736	1213.850885	15.593754
25.863677	1218.236349	15.598771
26.504064	1209.046540	15.603789
26.518263	1215.764105	15.608807
26.492326	1208.121554	15.613824
26.238628	1215.312096	15.618842
26.468777	1211.537902	15.623859
26.588850	1205.719693	15.628877
26.358121	1210.147318	15.633895
26.548115	1203.134185	15.638912
26.778342	1214.030105	15.643930
26.562696	1195.605769	15.648947
26.621159	1175.923290	15.653965
26.258138	1179.926815	15.658983
26.311360	1178.043419	15.664000
26.875566	1182.000518	15.669018
26.705466	1184.524433	15.674035
26.830996	1179.064034	15.679053
26.885935	1181.973650	15.684071
26.630560	1173.218551	15.689088
26.767973	1175.632065	15.694106
26.389909	1176.548389	15.699123
26.724066	1172.923579	15.704141
26.663991	1182.501888	15.709159
26.906240	1173.950578	15.714176
26.722897	1178.056013	15.719194
26.629103	1184.501335	15.724211
26.887148	1179.128345	15.729229
26.715344	1185.466553	15.734247
26.766079	1176.261483	15.739264
26.823212	1168.453110	15.744282
26.716219	1180.108334	15.749299
26.835736	1183.758814	15.754317
26.570884	1209.080528	15.759335
26.887725	1205.813210	15.764352
27.015942	1211.068464	15.769370
26.608483	1208.461758	15.774387
26.979978	1209.881484	15.779405
26.969435	1206.026124	15.784423
26.894931	1210.354895	15.789440
26.818839	1207.232053	15.794458
26.472946	1218.554942	15.799475
27.022372	1226.422042	15.804493
27.150482	1244.163195	15.809511
27.168545	1237.632887	15.814528
27.204163	1241.472953	15.819546
27.160220	1247.557185	15.824563
27.557974	1238.767876	15.829581
27.422516	1244.258692	15.834599
27.594121	1241.695694	15.839616
27.532740	1247.090533	15.844634
27.297567	1249.623265	15.849651
27.361223	1244.255300	15.854669
27.231700	1245.682579	15.859687
27.385965	1243.512481	15.864704
27.670181	1250.246773	15.869722
27.300222	1246.272540	15.874739
27.568303	1239.250867	15.879757
27.300760	1247.698986	15.884775
27.595473	1239.759867	15.889792
27.718361	1238.302680	15.894810
27.407597	1251.852253	15.899827
27.528583	1239.721726	15.904845
27.637759	1245.484214	15.909863
27.390426	1238.098771	15.914880
27.628579	1250.542980	15.919898
27.356288	1263.720677	15.924915
27.755985	1269.240196	15.929933
27.710868	1272.174441	15.934951
27.610798	1284.430365	15.939968
28.062322	1276.740725	15.944986
27.916174	1273.780849	15.950003
28.034739	1281.338365	15.955021
28.174371	1279.159584	15.960039
28.127141	1276.668452	15.965056
28.083049	1268.189502	15.970074
27.841663	1275.206639	15.975091
28.009486	1274.676719	15.980109
28.257591	1275.741728	15.985127
27.853756	1270.103805	15.990144
28.123465	1266.777920	15.995162
27.684142	1274.242719	16.000179
28.112355	1275.993988	16.005197
27.897942	1279.111763	16.010215
28.075643	1290.726386	16.015232
28.498724	1297.790144	16.020250
28.498335	1306.893369	16.025267
28.688852	1297.859421	16.030285
28.602178	1284.888892	16.035303
28.155554	1277.535215	16.040320
28.432561	1268.081624	16.045338
28.420283	1273.017154	16.050355
28.609928	1271.466726	16.055373
28.518007	1271.373876	16.060391
28.270798	1268.727441	16.065408
28.544473	1288.970298	16.070426
28.914124	1298.120681	16.075443
28.728052	1290.336877	16.080461
28.733510	1280.722083	16.085479
28.424663	1270.414126	16.090496
28.966383	1281.341430	16.095514
28.427851	1288.774080	16.100531
28.592303	1285.959728	16.105549
28.646516	1301.061230	16.110567
28.908015	1297.853845	16.115584
28.932524	1301.274100	16.120602
28.923469	1301.326919	16.125619
29.047244	1293.597518	16.130637
29.085460	1297.200428	16.135655
28.810761	1298.000379	16.140672
28.973187	1290.861818	16.145690
29.403645	1292.913985	16.150707
29.206135	1280.277336	16.155725
29.258427	1268.713055	16.160743
29.202609	1259.516275	16.165760
28.862815	1266.520788	16.170778
29.025961	1270.614244	16.175795
29.205458	1261.025977	16.180813
29.258007	1272.487503	16.185831
28.922504	1281.615846	16.190848
29.007164	1292.484703	16.195866
28.793987	1308.516106	16.200883
28.726643	1300.762913	16.205901
29.140728	1305.438527	16.210919
29.206058	1302.464578	16.215936
29.094030	1302.028059	16.220954
29.016679	1302.043004	16.225971
29.164988	1308.900467	16.230989
29.352533	1316.694767	16.236007
29.534732	1325.194687	16.241024
29.702414	1321.185020	16.246042
29.587952	1328.133170	16.251059
29.783381	1332.609272	16.256077
29.788294	1318.891811	16.261095
29.691006	1312.141539	16.266112
29.655727	1297.703721	16.271130
29.398769	1301.198759	16.276147
29.702479	1317.837546	16.281165
29.928183	1325.736670	16.286183
29.686308	1324.861507	16.291200
29.850825	1307.162960	16.296218
29.640373	1309.204875	16.301235
29.714700	1327.104154	16.306253
29.757854	1320.760157	16.311271
29.468629	1322.617210	16.316288
29.805175	1324.010274	16.321306
29.876872	1320.016703	16.326323
29.617532	1323.423244	16.331341
29.679912	1319.988834	16.336359
29.671997	1326.939655	16.341376
30.207818	1325.862579	16.346394
29.739940	1327.289560	16.351411
30.269068	1328.959455	16.356429
30.276421	1320.170228	16.361447
29.959642	1320.643387	16.366464
30.356915	1336.008766	16.371482
29.971958	1338.729010	16.376499
30.462148	1351.335254	16.381517
30.484196	1349.858744	16.386535
30.401528	1352.997210	16.391552
30.200791	1332.924822	16.396570
30.319009	1337.314920	16.401587
30.474387	1353.181401	16.406605
30.738642	1358.126339	16.411623
30.339003	1342.422012	16.416640
30.646013	1338.044028	16.421658
30.617595	1350.180819	16.426675
30.450933	1337.631228	16.431693
30.505804	1332.018437	16.436711
30.772940	1346.155516	16.441728
30.926261	1346.655163	16.446746
30.853844	1337.958878	16.451763
30.472699	1327.505885	16.456781
30.976328	1322.218737	16.461799
30.469365	1321.242700	16.466816
30.649519	1316.823604	16.471834
30.618333	1345.477932	16.476851
30.721815	1350.012753	16.481869
30.831152	1349.374173	16.486887
30.505656	1351.961444	16.491904
30.796656	1347.192727	16.496922
30.992507	1349.799096	16.501939
31.072677	1346.524663	16.506957
30.970656	1344.479590	16.511975
30.686353	1345.038025	16.516992
30.936948	1344.802448	16.522010
30.842214	1348.970881	16.527027
30.489588	1353.228429	16.532045
31.029358	1341.242608	16.537063
30.923603	1362.108481	16.542080
31.291441	1370.318464	16.547098
31.711779	1374.159341	16.552115
31.314017	1363.000274	16.557133
31.390683	1347.780794	16.562151
31.133476	1352.880481	16.567168
31.292010	1343.016272	16.572186
31.363362	1349.405436	16.577203
31.410980	1356.015482	16.582221
31.582035	1366.615766	16.587239
31.546136	1360.510892	16.592256
31.310319	1356.615913	16.597274
31.763986	1366.645694	16.602291
31.828419	1361.334982	16.607309
31.552434	1350.519896	16.612327
31.439728	1352.340932	16.617344
32.001220	1346.884874	16.622362
31.274894	1349.231674	16.627379
31.705175	1351.563110	16.632397
31.912759	1363.506529	16.637415
31.616546	1374.712282	16.642432
31.948005	1377.658849	16.647450
32.292737	1370.355096	16.652467
32.007040	1353.304069	16.657485
31.848639	1351.649473	16.662503
31.500834	1344.901388	16.667520
32.228899	1353.252908	16.672538
32.021719	1355.262058	16.677555
31.614096	1345.486576	16.682573
32.124438	1350.983760	16.687591
31.937728	1366.342423	16.692608
32.002102	1373.445341	16.697626
32.124929	1368.388813	16.702643
32.135765	1371.576081	16.707661
32.367279	1369.446344	16.712679
32.003605	1376.881038	16.717696
32.188495	1370.218662	16.722714
32.061084	1367.207011	16.727731
31.679056	1375.340744	16.732749
32.378069	1366.092720	16.737767
32.198335	1372.113714	16.742784
32.155030	1373.531972	16.747802
32.561623	1371.090359	16.752819
32.278651	1372.090634	16.757837
32.194856	1365.844736	16.762855
32.265929	1392.374844	16.767872
32.635462	1395.557605	16.772890
32.595077	1397.480378	16.777907
32.443498	1405.207684	16.782925
32.786550	1394.289110	16.787943
32.647349	1401.745433	16.792960
32.586710	1401.083621	16.797978
32.559531	1399.017951	16.802995
32.438514	1399.875198	16.808013
32.857098	1390.357260	16.813031
32.477740	1401.836649	16.818048
32.669555	1399.469403	16.823066
32.939432	1394.671004	16.828083
32.847529	1403.175360	16.833101
33.090712	1389.526802	16.838119
33.559776	1404.581907	16.843136
33.202088	1400.478249	16.848154
33.097538	1399.798271	16.853171
32.963798	1407.608469	16.858189
33.478969	1391.007003	16.863207
33.167400	1405.757152	16.868224
33.080540	1396.760306	16.873242
33.212517	1397.559896	16.878259
33.149418	1400.625246	16.883277
33.090480	1389.990245	16.888295
32.924369	1396.318984	16.893312
33.094990	1400.185539	16.898330
33.129456	1395.914720	16.903347
33.094720	1410.229794	16.908365
33.279159	1398.090588	16.913383
33.278927	1411.885743	16.918400
33.549118	1410.310656	16.923418
33.589779	1421.301467	16.928435
33.364808	1423.149857	16.933453
33.676348	1414.382061	16.938471
33.692881	1410.170731	16.943488
34.000495	1417.211278	16.948506
33.806774	1413.611612	16.953523
33.320194	1401.455938	16.958541
33.712274	1407.451814	16.963559
33.469075	1420.897165	16.968576
33.936422	1411.443013	16.973594
34.028525	1412.272561	16.978611
33.909428	1415.148630	16.983629
33.751119	1412.119086	16.988647
33.947581	1416.270982	16.993664
33.948045	1414.222925	16.998682
34.123881	1420.050362	17.003699
34.311452	1420.420271	17.008717
34.136935	1413.603613	17.013735
34.261254	1419.845137	17.018752
33.986745	1420.342233	17.023770
34.318276	1414.561792	17.028787
34.010735	1421.973397	17.033805
33.863850	1409.030451	17.038823
34.124689	1422.857914	17.043840
34.142733	1424.984533	17.048858
34.288851	1417.915370	17.053875
34.019013	1428.589168	17.058893
34.176814	1427.234154	17.063911
34.046912	1415.670499	17.068928
34.109985	1422.282043	17.073946
34.340330	1416.996761	17.078963
34.035437	1426.559218	17.083981
34.533477	1434.687119	17.088999
34.574488	1451.310539	17.094016
34.486280	1454.213152	17.099034
34.606646	1450.425731	17.104051
34.712774	1455.885172	17.109069
34.783614	1445.798123	17.114087
34.899229	1461.532627	17.119104
34.734664	1451.960571	17.124122
35.035388	1446.028503	17.129139
34.641769	1456.922640	17.134157
34.859697	1451.968114	17.139175
34.676133	1445.300760	17.144192
34.677492	1449.291861	17.149210
35.046085	1442.815673	17.154227
34.599493	1444.008803	17.159245
34.796659	1438.468451	17.164263
34.913799	1448.195647	17.169280
34.855677	1441.252651	17.174298
35.035614	1443.331426	17.179315
34.836319	1459.267964	17.184333
35.061596	1455.501564	17.189351
35.042294	1476.007719	17.194368
35.156666	1476.372786	17.199386
35.599311	1471.079581	17.204403
35.436344	1477.570674	17.209421
35.355764	1472.612626	17.214439
35.310046	1477.684916	17.219456
35.374660	1479.496564	17.224474
35.442444	1471.576997	17.229491
35.389478	1477.772098	17.234509
35.605060	1476.372468	17.239527
35.665589	1480.678208	17.244544
35.616687	1477.017673	17.249562
35.589462	1473.790230	17.254579
35.464144	1472.531496	17.259597
35.665788	1474.997741	17.264615
35.834934	1473.710132	17.269632
35.410811	1488.918798	17.274650
35.652297	1474.151922	17.279667
35.413088	1474.153354	17.284685
35.783653	1468.390264	17.289703
35.980519	1462.075175	17.294720
35.944081	1467.875922	17.299738
35.991332	1470.114302	17.304755
35.915088	1470.910138	17.309773
35.919409	1469.180807	17.314791
36.051899	1472.905588	17.319808
35.950608	1473.446636	17.324826
36.699823	1463.344978	17.329843
35.928814	1469.271540	17.334861
36.205488	1459.113110	17.339879
36.174463	1470.269559	17.344896
36.079591	1469.712313	17.349914
36.216097	1457.491820	17.354931
35.843116	1490.104711	17.359949
36.586300	1494.069534	17.364967
36.743467	1494.912307	17.369984
36.499461	1505.876220	17.375002
37.111833	1488.677075	17.380019
36.542989	1480.370580	17.385037
36.453535	1471.602995	17.390055
36.510046	1473.369527	17.395072
36.685611	1464.821605	17.400090
36.895871	1457.932543	17.405107
36.326826	1470.883243	17.410125
36.686506	1464.362059	17.415143
36.784581	1464.772201	17.420160
36.311320	1474.321427	17.425178
37.099156	1477.186573	17.430195
37.101491	1498.183276	17.435213
37.119765	1480.243555	17.440231
36.940209	1472.427937	17.445248
36.700735	1466.666184	17.450266
37.087412	1471.003279	17.455283
37.086358	1497.136064	17.460301
37.061706	1494.937832	17.465319
37.564409	1489.856856	17.470336
37.070495	1476.467365	17.475354
37.145740	1458.476109	17.480371
37.126314	1469.311359	17.485389
37.250649	1477.998364	17.490407
37.459695	1482.808995	17.495424
37.569834	1473.569092	17.500442
37.551777	1458.913633	17.505459
37.291477	1464.986056	17.510477
37.223434	1460.748873	17.515495
37.443763	1453.394129	17.520512
37.119259	1479.104167	17.525530
37.175242	1477.972257	17.530547
37.125011	1492.347303	17.535565
37.270887	1484.417634	17.540583
37.489609	1481.962706	17.545600
37.451092	1489.680676	17.550618
37.894061	1485.140167	17.555635
37.484070	1497.413451	17.560653
37.712146	1485.716346	17.565671
37.478038	1492.771755	17.570688
37.606102	1509.367198	17.575706
37.737307	1517.504888	17.580723
37.754001	1520.444269	17.585741
37.741720	1519.220202	17.590759
37.995394	1522.965783	17.595776
37.787487	1523.597776	17.600794
37.718651	1526.723847	17.605811
37.721253	1527.599927	17.610829
37.940041	1525.045086	17.615847
38.514570	1518.361399	17.620864
38.363281	1526.871366	17.625882
38.322655	1522.995551	17.630899
38.265119	1527.486890	17.635917
38.274408	1516.998229	17.640935
38.229469	1518.424628	17.645952
37.853970	1525.267417	17.650970
38.030943	1526.913274	17.655987
38.086824	1546.888396	17.661005
38.623520	1559.323010	17.666023
38.390848	1554.341210	17.671040
37.866300	1559.017953	17.676058
38.442458	1549.866496	17.681075
38.654592	1551.233018	17.686093
38.563893	1559.139474	17.691111
38.680889	1555.531903	17.696128
38.517830	1552.297004	17.701146
38.600754	1546.087363	17.706163
38.992769	1552.204444	17.711181
38.584034	1544.083965	17.716199
39.077125	1557.271208	17.721216
38.785623	1569.943327	17.726234
39.126909	1572.815216	17.731251
39.167500	1570.358008	17.736269
39.262924	1562.464661	17.741287
39.352041	1550.569426	17.746304
38.878041	1553.830130	17.751322
39.179623	1544.146694	17.756339
39.070352	1548.148388	17.761357
38.778895	1569.380044	17.766375
39.076078	1568.827122	17.771392
39.237008	1577.529587	17.776410
39.704029	1572.295386	17.781427
39.524781	1565.241863	17.786445
39.615777	1568.985873	17.791463
39.807950	1564.859752	17.796480
39.684841	1578.735230	17.801498
39.912931	1557.162562	17.806515
39.721319	1547.889722	17.811533
39.221226	1546.316346	17.816551
39.808656	1537.347944	17.821568
39.580517	1545.214173	17.826586
39.652637	1549.212893	17.831603
39.426456	1552.880061	17.836621
39.366001	1565.490941	17.841639
39.632531	1571.945822	17.846656
39.596726	1574.321745	17.851674
39.998867	1566.333066	17.856691
39.780724	1581.236032	17.861709
39.639554	1583.039612	17.866727
40.273956	1568.222559	17.871744
39.841637	1573.646005	17.876762
40.061481	1568.264022	17.881779
39.974632	1576.497090	17.886797
39.581607	1581.541433	17.891815
40.126414	1589.090906	17.896832
39.747690	1611.904197	17.901850
39.997002	1592.684690	17.906867
40.094778	1599.714745	17.911885
39.795929	1613.656042	17.916903
40.232219	1605.690213	17.921920
39.942060	1616.324913	17.926938
40.472897	1624.090582	17.931955
40.707845	1635.263730	17.936973
40.517237	1638.026181	17.941991
40.803620	1631.657413	17.947008
40.467327	1637.010506	17.952026
40.548888	1636.565124	17.957043
41.206982	1624.063869	17.962061
40.699784	1620.923959	17.967079
40.973838	1609.819584	17.972096
40.783027	1611.655470	17.977114
40.687809	1602.989407	17.982131
40.982516	1612.355668	17.987149
41.034118	1622.795065	17.992167
41.276780	1621.048940	17.997184
41.209392	1618.282515	18.002202
41.237022	1605.884977	18.007219
40.979343	1601.812504	18.012237
40.627031	1599.394361	18.017255
41.182787	1606.382051	18.022272
41.215798	1620.339643	18.027290
41.223481	1625.841594	18.032307
41.086327	1622.788967	18.037325
40.997492	1625.403824	18.042343
41.380673	1626.429227	18.047360
41.233662	1629.684989	18.052378
41.267286	1625.461432	18.057395
41.461988	1617.506599	18.062413
41.572375	1622.683827	18.067431
41.581407	1622.442727	18.072448
41.730361	1620.949882	18.077466
41.655119	1623.918892	18.082483
41.777491	1620.797343	18.087501
41.854639	1623.343250	18.092519
41.865893	1614.805716	18.097536
41.580409	1619.585146	18.102554
41.537107	1614.832694	18.107571
41.684387	1620.803991	18.112589
41.602017	1624.714104	18.117607
42.210493	1640.566053	18.122624
42.162608	1647.687010	18.127642
41.966629	1642.560889	18.132659
42.252788	1645.163135	18.137677
42.279337	1649.194321	18.142695
42.759692	1627.469619	18.147712
42.378308	1629.653681	18.152730
42.319059	1620.716792	18.157747
42.456971	1610.072258	18.162765
42.280791	1613.153328	18.167783
42.360581	1614.160259	18.172800
42.521079	1614.895533	18.177818
42.639973	1617.045423	18.182835
42.362243	1606.375941	18.187853
42.237734	1614.974504	18.192871
42.382772	1610.787456	18.197888
41.956785	1616.466333	18.202906
42.308874	1630.095381	18.207923
42.817227	1633.735871	18.212941
42.187678	1642.190826	18.217959
42.548823	1644.564015	18.222976
42.674749	1645.919125	18.227994
42.614744	1651.684375	18.233011
42.688593	1648.134791	18.238029
42.413324	1650.990979	18.243047
42.983559	1655.771591	18.248064
42.898295	1667.761968	18.253082
42.994869	1675.384551	18.258099
43.045358	1675.186392	18.263117
42.778647	1678.630372	18.268135
43.105827	1677.008413	18.273152
43.216301	1677.127120	18.278170
43.142303	1667.119653	18.283187
43.158596	1674.364107	18.288205
43.189504	1671.790439	18.293223
42.960355	1668.853944	18.298240
43.421339	1664.158697	18.303258
43.180087	1675.862474	18.308275
43.669063	1669.427554	18.313293
43.344430	1680.520871	18.318311
43.855646	1684.758723	18.323328
43.835421	1688.175978	18.328346
43.663771	1679.461493	18.333363
43.986401	1676.109772	18.338381
43.641348	1675.004054	18.343399
43.603240	1675.938550	18.348416
43.403275	1680.546256	18.353434
43.679901	1700.062411	18.358451
44.216224	1697.072256	18.363469
43.643077	1703.867205	18.368487
44.062735	1701.400645	18.373504
43.916839	1704.194519	18.378522
44.072442	1703.723168	18.383539
44.154946	1698.153811	18.388557
43.897962	1704.112535	18.393575
44.199106	1698.806423	18.398592
44.336765	1693.478405	18.403610
44.246598	1699.339728	18.408627
44.485243	1697.527375	18.413645
44.348674	1700.978920	18.418663
44.061608	1705.681545	18.423680
44.405455	1705.926641	18.428698
44.334018	1709.291501	18.433715
44.660594	1720.914974	18.438733
44.505894	1722.257429	18.443751
44.526293	1729.444621	18.448768
44.602935	1735.224292	18.453786
44.669920	1728.519206	18.458803
44.896200	1726.955810	18.463821
44.679979	1727.843991	18.468839
44.800657	1724.828879	18.473856
44.800561	1726.093188	18.478874
44.645205	1723.501237	18.483891
44.853552	1728.156317	18.488909
44.855144	1731.794280	18.493927
45.020198	1730.560790	18.498944
45.130340	1726.254994	18.503962
45.259095	1727.023654	18.508979
45.529615	1722.519230	18.513997
45.388733	1723.876786	18.519015
45.324817	1735.565698	18.524032
45.284261	1730.347897	18.529050
45.312581	1734.160939	18.534067
45.523432	1716.536312	18.539085
45.097906	1721.501720	18.544103
45.219623	1720.610230	18.549120
45.232046	1722.626093	18.554138
45.123744	1731.314957	18.559155
45.481235	1739.237337	18.564173
45.407611	1764.403659	18.569191
45.727202	1763.195860	18.574208
45.955362	1752.624140	18.579226
45.427567	1751.085047	18.584243
46.061554	1743.099412	18.589261
45.628161	1757.515379	18.594279
45.737401	1752.111641	18.599296
46.035194	1751.888983	18.604314
46.092867	1748.201943	18.609331
46.541565	1744.883588	18.614349
46.550200	1755.104182	18.619367
46.453579	1742.396764	18.624384
46.192729	1752.973400	18.629402
46.135137	1752.614709	18.634419
46.464202	1741.986000	18.639437
46.065767	1752.734818	18.644455
46.211150	1749.264259	18.649472
46.175897	1752.033416	18.654490
46.019021	1754.205286	18.659507
46.406790	1747.068319	18.664525
46.274746	1774.473168	18.669543
46.557251	1775.231467	18.674560
46.545120	1781.174768	18.679578
46.383383	1794.408460	18.684595
46.850564	1772.946006	18.689613
46.790251	1782.873206	18.694631
46.644129	1781.075015	18.699648
46.696900	1784.816524	18.704666
46.567977	1779.145564	18.709683
46.731650	1773.844832	18.714701
46.613948	1780.752025	18.719719
47.004139	1792.132578	18.724736
46.924365	1803.197946	18.729754
47.104286	1810.255119	18.734771
47.562954	1807.857046	18.739789
47.429445	1806.668022	18.744807
47.253916	1807.520614	18.749824
47.445095	1791.358949	18.754842
47.417731	1801.894447	18.759859
47.598852	1784.950162	18.764877
47.540496	1778.353142	18.769895
47.342068	1781.856261	18.774912
47.519744	1782.455870	18.779930
47.453288	1799.223469	18.784947
47.764054	1802.768089	18.789965
47.657884	1808.224553	18.794983
47.848096	1805.851992	18.800000
47.878446	1807.823319	18.805018
48.026331	1814.121822	18.810035
47.879568	1814.525401	18.815053
47.906145	1809.887594	18.820071
47.943725	1805.834046	18.825088
47.791206	1800.170774	18.830106
47.847014	1812.867941	18.835123
47.877612	1805.835894	18.840141
47.882397	1809.565398	18.845159
47.935769	1812.397518	18.850176
48.037375	1801.307131	18.855194
47.783969	1809.229446	18.860211
48.203573	1809.326381	18.865229
47.891520	1822.296181	18.870247
48.170432	1822.340043	18.875264
48.378564	1828.562083	18.880282
48.079074	1833.588446	18.885299
48.326940	1825.209699	18.890317
48.415716	1828.628480	18.895335
48.566854	1826.301478	18.900352
48.511060	1838.008054	18.905370
48.611692	1856.742298	18.910387
48.602103	1860.065078	18.915405
48.656462	1865.100303	18.920423
48.634376	1865.172507	18.925440
49.086980	1863.342528	18.930458
48.936378	1868.330211	18.935475
48.958587	1851.822583	18.940493
48.853635	1862.827511	18.945511
48.934589	1865.774018	18.950528
49.229805	1857.139924	18.955546
48.801567	1858.802113	18.960563
48.972609	1863.294069	18.965581
48.937954	1883.643566	18.970599
49.226238	1887.979176	18.975616
49.340099	1892.832656	18.980634
48.930027	1890.386704	18.985651
49.427598	1882.053051	18.990669
49.283981	1888.781151	18.995687
49.291081	1886.538467	19.000704
49.339930	1886.363378	19.005722
49.704052	1907.674242	19.010739
49.722849	1911.127015	19.015757
49.731446	1915.244517	19.020775
49.802459	1913.532814	19.025792
50.053864	1918.284132	19.030810
49.990987	1919.767707	19.035827
50.226816	1911.143839	19.040845
50.157933	1914.332928	19.045863
50.397550	1904.900624	19.050880
50.268652	1883.163378	19.055898
50.014427	1876.295501	19.060915
49.979445	1878.653249	19.065933
50.234101	1890.804336	19.070951
50.338206	1898.116702	19.075968
50.850781	1897.870013	19.080986
50.331021	1907.544923	19.086003
50.598985	1901.998612	19.091021
50.732787	1892.663425	19.096039
50.483817	1886.460952	19.101056
50.570843	1881.441422	19.106074
50.611267	1900.196336	19.111091
50.464178	1904.787813	19.116109
50.434517	1905.244298	19.121127
50.446813	1903.758276	19.126144
50.885651	1904.306798	19.131162
50.744546	1902.296197	19.136179
50.923118	1907.708071	19.141197
50.825508	1908.818044	19.146215
50.574774	1910.217522	19.151232
50.625647	1906.977526	19.156250
50.876074	1921.839929	19.161267
51.021050	1938.713980	19.166285
50.823616	1939.470174	19.171303
50.872640	1939.031546	19.176320
51.167721	1931.840840	19.181338
51.127798	1939.219460	19.186355
51.779869	1951.941213	19.191373
51.742852	1951.219760	19.196391
51.342969	1937.022738	19.201408
51.752502	1933.907238	19.206426
51.302690	1947.292418	19.211443
51.816651	1954.811607	19.216461
52.223320	1959.735613	19.221479
52.021337	1948.894904	19.226496
51.976273	1924.620027	19.231514
51.555405	1936.056110	19.236531
51.881934	1935.450514	19.241549
52.258429	1942.954651	19.246567
52.030863	1951.154524	19.251584
52.131305	1956.623713	19.256602
52.277623	1955.441963	19.261619
52.064834	1952.345480	19.266637
52.391948	1963.181676	19.271655
52.106376	1958.200307	19.276672
52.403125	1957.114914	19.281690
52.465962	1966.561649	19.286707
52.543103	1970.358314	19.291725
52.660591	1964.791929	19.296743
52.583942	1958.790841	19.301760
52.441892	1959.442238	19.306778
52.498541	1963.475004	19.311795
52.246085	1963.782173	19.316813
52.159864	1964.890334	19.321831
52.157712	1961.875098	19.326848
52.369698	1957.336677	19.331866
52.414706	1972.843868	19.336883
52.507075	1983.148019	19.341901
52.932729	1985.194764	19.346919
52.717405	1985.937295	19.351936
52.770741	1976.500045	19.356954
53.194164	1979.463535	19.361971
53.154526	1980.244907	19.366989
53.486461	1981.316268	19.372007
52.903613	1985.495869	19.377024
53.485908	1983.162218	19.382042
53.530892	1993.775989	19.387059
54.052013	1986.761587	19.392077
53.962843	1978.777892	19.397095
53.753554	1979.001877	19.402112
53.654870	1964.479906	19.407130
53.353621	1973.386897	19.412147
53.800411	1974.226770	19.417165
53.648192	1969.330320	19.422183
53.621243	1970.609159	19.427200
53.809636	1967.308674	19.432218
53.857404	1984.796886	19.437235
53.927814	1995.095108	19.442253
54.012638	1995.881015	19.447271
53.964855	2001.608269	19.452288
54.013824	1996.324178	19.457306
53.945790	1999.455728	19.462323
54.539753	1994.241250	19.467341
54.597207	1988.426426	19.472359
54.397544	1998.715809	19.477376
54.749787	1997.370636	19.482394
54.656104	1997.456619	19.487411
54.647360	1994.568285	19.492429
54.575856	1983.237138	19.497447
54.779138	1991.891408	19.502464
54.951240	1982.462743	19.507482
54.633344	1993.169786	19.512499
55.055776	1987.782085	19.517517
55.186573	1973.144058	19.522535
54.759150	1968.613220	19.527552
54.813961	1970.501220	19.532570
54.900753	1974.468613	19.537587
54.915910	1987.134659	19.542605
54.958940	1984.687219	19.547623
55.395784	1973.486599	19.552640
55.813933	1964.731364	19.557658
55.550418	1942.343743	19.562675
55.444984	1933.115906	19.567693
55.565209	1925.869711	19.572711
55.219837	1935.066106	19.577728
55.646296	1921.114086	19.582746
55.470556	1924.735543	19.587763
55.093909	1928.317464	19.592781
55.389855	1934.619936	19.597799
55.348518	1960.162947	19.602816
55.400105	1957.075427	19.607834
55.598190	1958.813932	19.612851
55.427159	1963.929975	19.617869
55.957864	1959.660081	19.622887
55.872282	1968.424908	19.627904
56.016176	1959.829834	19.632922
55.945809	1960.332143	19.637939
55.768875	1964.530379	19.642957
55.875596	1969.116792	19.647975
55.914768	1981.141856	19.652992
55.993776	1982.113542	19.658010
55.777795	1996.170200	19.663027
56.069479	1999.072900	19.668045
56.331856	1990.914353	19.673063
56.347703	1997.606844	19.678080
56.348103	1995.654681	19.683098
56.619736	1999.358980	19.688115
56.463314	2014.383904	19.693133
56.690780	2009.818613	19.698151
56.799639	2021.028687	19.703168
56.603199	2017.802153	19.708186
56.835027	2023.884416	19.713203
56.686112	2018.906401	19.718221
57.101220	2015.996873	19.723239
56.513317	2021.650598	19.728256
56.783139	2017.004608	19.733274
56.704200	2019.400067	19.738291
56.574315	2033.660920	19.743309
57.024915	2037.371296	19.748327
56.907955	2053.002731	19.753344
56.873253	2050.002108	19.758362
57.244974	2051.201638	19.763379
57.224235	2061.557708	19.768397
57.535307	2068.369120	19.773415
57.145264	2078.680270	19.778432
57.719272	2083.999251	19.783450
57.442317	2080.735988	19.788467
57.628947	2080.114942	19.793485
57.841409	2079.798126	19.798503
58.031006	2084.542839	19.803520
57.926338	2077.850024	19.808538
58.201557	2076.123826	19.813555
58.327208	2079.148988	19.818573
58.333280	2068.603808	19.823591
58.203038	2071.076679	19.828608
58.127139	2071.332093	19.833626
58.293202	2072.290687	19.838643
58.333431	2076.553432	19.843661
58.514482	2074.526037	19.848679
58.333359	2065.344799	19.853696
58.118259	2073.130570	19.858714
58.446188	2067.963217	19.863731
58.476105	2071.825649	19.868749
58.074389	2064.074247	19.873767
58.110407	2075.948077	19.878784
58.306166	2087.381112	19.883802
58.802147	2092.600843	19.888819
58.436603	2107.694612	19.893837
58.591786	2091.859293	19.898855
58.564518	2094.851425	19.903872
58.698956	2100.588200	19.908890
58.982869	2110.344304	19.913907
58.756474	2121.682652	19.918925
59.325148	2121.535567	19.923943
59.147193	2128.506022	19.928960
59.460728	2127.895412	19.933978
59.644016	2127.410194	19.938995
59.540615	2131.122424	19.944013
59.614031	2125.777751	19.949031
59.597020	2132.951443	19.954048
59.599289	2129.399787	19.959066
59.840860	2121.961875	19.964083
59.635881	2129.200154	19.969101
59.762970	2128.816719	19.974119
59.519398	2131.667156	19.979136
59.608958	2138.840372	19.984154
59.785764	2129.688536	19.989171
59.734370	2134.721056	19.994189
60.185697	2134.880586	19.999207
59.771971	2158.877077	20.004224
60.021465	2159.156111	20.009242
60.507080	2149.274593	20.014259
60.065242	2160.395616	20.019277
60.539905	2156.015826	20.024295
60.424425	2166.934561	20.029312
60.434707	2159.871760	20.034330
60.772034	2158.962376	20.039347
60.641466	2168.089259	20.044365
60.783814	2156.912657	20.049383
60.497646	2158.970696	20.054400
61.012807	2151.164264	20.059418
61.141824	2158.339064	20.064435
60.909816	2149.210726	20.069453
61.068965	2148.325826	20.074471
61.460221	2140.281940	20.079488
61.493219	2138.861027	20.084506
61.530450	2139.039403	20.089523
61.463556	2137.355962	20.094541
61.437937	2128.603757	20.099559
61.417117	2116.278802	20.104576
61.508605	2098.961437	20.109594
61.743588	2106.440247	20.114611
61.173924	2111.545977	20.119629
61.557690	2099.443622	20.124647
61.624064	2104.770418	20.129664
61.282570	2114.230606	20.134682
61.975917	2123.037272	20.139699
61.666214	2131.782879	20.144717
61.465602	2127.471464	20.149735
61.747649	2140.062826	20.154752
61.777973	2135.297675	20.159770
62.047882	2137.931708	20.164787
61.773527	2135.030645	20.169805
62.010488	2139.511387	20.174823
62.075689	2136.138479	20.179840
61.568591	2137.660672	20.184858
62.059834	2157.472016	20.189875
62.072439	2169.075915	20.194893
62.168821	2169.613779	20.199911
62.056435	2167.830611	20.204928
62.452196	2169.605264	20.209946
62.459641	2165.608338	20.214963
62.453178	2168.509066	20.219981
62.532016	2172.825464	20.224999
63.063946	2188.928568	20.230016
62.886083	2190.822241	20.235034
63.084660	2181.972106	20.240051
62.930067	2185.586321	20.245069
63.196166	2184.751224	20.250087
63.357453	2187.410457	20.255104
63.179666	2186.106538	20.260122
63.520945	2179.834973	20.265139
63.130107	2180.849354	20.270157
63.251881	2184.208680	20.275175
63.076588	2182.206638	20.280192
62.882406	2192.802062	20.285210
63.258398	2185.706881	20.290227
63.189395	2190.915282	20.295245
63.650996	2198.329679	20.300263
63.668283	2207.772037	20.305280
63.487277	2219.357298	20.310298
64.009426	2206.526405	20.315315
64.118773	2209.610044	20.320333
63.900049	2209.314011	20.325351
64.282841	2203.013003	20.330368
64.150125	2207.993229	20.335386
64.320805	2203.818442	20.340403
64.210618	2208.562237	20.345421
64.239906	2202.901276	20.350439
64.464387	2209.658917	20.355456
64.580431	2204.445075	20.360474
64.536971	2194.987723	20.365491
64.341662	2208.520551	20.370509
64.476723	2202.844294	20.375527
64.512024	2205.946821	20.380544
64.384791	2210.014488	20.385562
64.654138	2205.495160	20.390579
64.618114	2206.343616	20.395597
64.513338	2223.844644	20.400615
64.640944	2225.765118	20.405632
64.689996	2241.314428	20.410650
65.164575	2229.689117	20.415667
64.969231	2241.425352	20.420685
64.874359	2233.440067	20.425703
65.143213	2229.668882	20.430720
65.025164	2238.311617	20.435738
65.281882	2251.696091	20.440755
65.483914	2254.872724	20.445773
65.618797	2268.573985	20.450791
65.466806	2266.393586	20.455808
65.239243	2262.846302	20.460826
65.785589	2264.519076	20.465843
65.427050	2270.822243	20.470861
65.437244	2271.288902	20.475879
65.544657	2261.279627	20.480896
65.569967	2291.230224	20.485914
65.952230	2293.751187	20.490931
66.046423	2300.074984	20.495949
66.069937	2296.384601	20.500967
66.267640	2295.027866	20.505984
66.060761	2296.502192	20.511002
66.633410	2285.446441	20.516019
66.164789	2285.346011	20.521037
66.004923	2292.631452	20.526055
66.172770	2301.997155	20.531072
66.150295	2315.598484	20.536090
66.464512	2314.593663	20.541107
66.271038	2321.027063	20.546125
66.365203	2325.544009	20.551143
66.963406	2336.790343	20.556160
66.664167	2350.621487	20.561178
67.249339	2350.795860	20.566195
67.117241	2357.917220	20.571213
67.212436	2356.561096	20.576231
67.512435	2353.064950	20.581248
67.013667	2361.041638	20.586266
67.460253	2353.628335	20.591283
67.392336	2351.026259	20.596301
67.504818	2346.897685	20.601319
67.717873	2342.006569	20.606336
67.535933	2355.616061	20.611354
67.570773	2344.009662	20.616371
67.744937	2341.958158	20.621389
67.743716	2342.462824	20.626407
67.903188	2332.470369	20.631424
67.953738	2337.740778	20.636442
67.924538	2341.807792	20.641459
67.733922	2343.908040	20.646477
68.212172	2360.635033	20.651495
68.366936	2368.254992	20.656512
68.113214	2368.586754	20.661530
68.121072	2369.511603	20.666547
68.156720	2375.172207	20.671565
68.478602	2380.435543	20.676583
68.550079	2374.954216	20.681600
68.176899	2378.158111	20.686618
68.590286	2366.197912	20.691635
68.553276	2371.004031	20.696653
68.584822	2371.170731	20.701671
68.554019	2364.723230	20.706688
68.529435	2382.752067	20.711706
69.001098	2393.438098	20.716723
69.089960	2398.597798	20.721741
69.067384	2401.874002	20.726759
69.274564	2393.560419	20.731776
69.197346	2389.024725	20.736794
69.439404	2394.432949	20.741811
69.400802	2391.788432	20.746829
69.407947	2396.874635	20.751847
69.844436	2383.199831	20.756864
69.607089	2395.082906	20.761882
69.619993	2384.663842	20.766899
69.750883	2387.778695	20.771917
69.646275	2387.144302	20.776935
69.614144	2388.256453	20.781952
69.610205	2386.098835	20.786970
69.953395	2407.158904	20.791987
69.570784	2415.401854	20.797005
69.709738	2424.173622	20.802023
70.369141	2416.060863	20.807040
70.138626	2421.903166	20.812058
70.044503	2417.709981	20.817075
70.101188	2425.395955	20.822093
70.381109	2442.470110	20.827111
70.514352	2448.185187	20.832128
71.009888	2455.378769	20.837146
71.194572	2449.105320	20.842163
70.997723	2448.931652	20.847181
70.738732	2441.213922	20.852199
71.433901	2443.017950	20.857216
70.824576	2431.110676	20.862234
70.810341	2439.622126	20.867251
70.988095	2443.232171	20.872269
71.199785	2451.510939	20.877287
71.110209	2441.043676	20.882304
71.188155	2447.950657	20.887322
71.138167	2447.765367	20.892339
71.159120	2451.654502	20.897357
70.796876	2449.989809	20.902375
71.485888	2462.972790	20.907392
71.352749	2474.747275	20.912410
71.480052	2475.288086	20.917427
71.732447	2473.668532	20.922445
71.715914	2478.266110	20.927463
72.025375	2476.474623	20.932480
71.726518	2481.081830	20.937498
72.048112	2481.247112	20.942515
72.081354	2481.924851	20.947533
71.854181	2487.014630	20.952551
72.273845	2488.365454	20.957568
72.165465	2503.305340	20.962586
72.423026	2501.257033	20.967603
72.626778	2505.543382	20.972621
72.438154	2510.161336	20.977639
72.633814	2501.437336	20.982656
72.301928	2502.460427	20.987674
72.402539	2501.532139	20.992691
72.441680	2509.298831	20.997709
72.680833	2532.061421	21.002727
72.969089	2519.256547	21.007744
73.066038	2537.437678	21.012762
72.903536	2531.445327	21.017779
72.866696	2535.376739	21.022797
72.780513	2538.873148	21.027815
73.250776	2539.375784	21.032832
73.132334	2547.370580	21.037850
73.490074	2553.795622	21.042867
73.537093	2561.336109	21.047885
73.409423	2566.054488	21.052903
73.955280	2564.819984	21.057920
74.124937	2572.075036	21.062938
73.933755	2564.541511	21.067955
74.266422	2560.880420	21.072973
74.353698	2563.516915	21.077991
74.253829	2552.614631	21.083008
74.119424	2555.208601	21.088026
74.285906	2555.563028	21.093043
74.217091	2557.398451	21.098061
73.946183	2555.399019	21.103079
74.468049	2552.919957	21.108096
74.333502	2556.961353	21.113114
74.357529	2554.345363	21.118131
74.386786	2548.734618	21.123149
74.228224	2562.041653	21.128167
74.463346	2577.973054	21.133184
74.585248	2587.934670	21.138202
74.703906	2584.935438	21.143219
74.814827	2583.797829	21.148237
74.927364	2596.237268	21.153255
75.182123	2589.197414	21.158272
75.094365	2603.091036	21.163290
75.031479	2600.256842	21.168307
75.389232	2602.970562	21.173325
75.462254	2595.768537	21.178343
75.761428	2602.180129	21.183360
75.458236	2603.481052	21.188378
75.159367	2598.847701	21.193395
75.522171	2606.237160	21.198413
75.407346	2615.528576	21.203431
75.779717	2628.147648	21.208448
76.104166	2636.945812	21.213466
76.005680	2636.890182	21.218483
75.962103	2632.535480	21.223501
76.374806	2631.507853	21.228519
76.444713	2629.028487	21.233536
76.730524	2621.172644	21.238554
76.962187	2615.229885	21.243571
77.040038	2609.959846	21.248589
76.577554	2605.437542	21.253607
76.756309	2580.419483	21.258624
76.565158	2583.928710	21.263642
76.655431	2583.874442	21.268659
76.708350	2600.970040	21.273677
76.798734	2609.994309	21.278695
76.925758	2619.594851	21.283712
76.800939	2618.139276	21.288730
76.717178	2624.741744	21.293747
76.987077	2601.547481	21.298765
76.884656	2624.711596	21.303783
77.266497	2629.768803	21.308800
77.506239	2643.022615	21.313818
77.327789	2648.858278	21.318835
77.837406	2642.767344	21.323853
77.583114	2647.634951	21.328871
77.639658	2645.677681	21.333888
77.799318	2649.594305	21.338906
77.739328	2647.300846	21.343923
77.903522	2644.348618	21.348941
77.511116	2653.838508	21.353959
77.771417	2660.596940	21.358976
77.976978	2671.399559	21.363994
77.873246	2676.824491	21.369011
78.047752	2676.740271	21.374029
78.129644	2680.756622	21.379047
78.383476	2698.553440	21.384064
78.372356	2715.904815	21.389082
78.413343	2716.563238	21.394099
78.501498	2699.379425	21.399117
78.187993	2711.364578	21.404135
78.777013	2705.784858	21.409152
78.652040	2724.900743	21.414170
78.952750	2732.076763	21.419187
79.296693	2734.773045	21.424205
79.466088	2741.818190	21.429223
79.375097	2729.787101	21.434240
79.842879	2726.687323	21.439258
79.424738	2732.012955	21.444275
79.640198	2725.354532	21.449293
79.369182	2735.832017	21.454311
79.911719	2731.035330	21.459328
79.933244	2729.745199	21.464346
79.987147	2728.708709	21.469363
79.781086	2725.213732	21.474381
79.882698	2729.556556	21.479399
79.960148	2732.293764	21.484416
80.059760	2732.887773	21.489434
79.643769	2726.324547	21.494451
79.814036	2733.898959	21.499469
79.910715	2754.345931	21.504487
80.119951	2750.956205	21.509504
80.078598	2757.406440	21.514522
80.315158	2758.846277	21.519539
80.759326	2779.202467	21.524557
81.122155	2784.110151	21.529575
81.056483	2794.122274	21.534592
81.182812	2793.686240	21.539610
81.381748	2792.961727	21.544627
81.240246	2776.093709	21.549645
81.054657	2774.247408	21.554663
81.199491	2776.593930	21.559680
81.283166	2774.213821	21.564698
81.300642	2787.688860	21.569715
81.419631	2779.265621	21.574733
81.318496	2791.231129	21.579751
81.506385	2781.354981	21.584768
81.439100	2783.947727	21.589786
81.351084	2788.979231	21.594803
81.902318	2792.591159	21.599821
81.747823	2808.354461	21.604839
81.964873	2815.319670	21.609856
81.897255	2810.403150	21.614874
81.703319	2821.818672	21.619891
81.923459	2811.156220	21.624909
81.890092	2823.999071	21.629927
81.919459	2841.031839	21.634944
82.291937	2841.804171	21.639962
81.943754	2842.829097	21.644979
82.468817	2857.743054	21.649997
82.617980	2874.490869	21.655015
82.666294	2877.609557	21.660032
82.894144	2875.609203	21.665050
82.819741	2881.588841	21.670067
82.927516	2871.050464	21.675085
83.147901	2863.719395	21.680103
83.149660	2860.324973	21.685120
83.455889	2878.263903	21.690138
83.551463	2893.609036	21.695155
84.043852	2887.151025	21.700173
84.122864	2877.045955	21.705191
83.914465	2862.905593	21.710208
84.084101	2856.649317	21.715226
84.071728	2858.640972	21.720243
84.081650	2853.357293	21.725261
83.615895	2861.151200	21.730279
83.870843	2855.080341	21.735296
84.434916	2876.856326	21.740314
84.277353	2884.319475	21.745331
84.354470	2891.878145	21.750349
84.700066	2890.858058	21.755367
84.370570	2889.450044	21.760384
84.581152	2882.797048	21.765402
84.459262	2890.453533	21.770419
84.383776	2890.676641	21.775437
84.176090	2886.550991	21.780455
84.587788	2894.481095	21.785472
84.685963	2888.012007	21.790490
84.843838	2908.823094	21.795507
84.768283	2907.917369	21.800525
84.703810	2916.109073	21.805543
84.876481	2916.969127	21.810560
84.964542	2917.808848	21.815578
85.391101	2943.911422	21.820595
86.049889	2928.830314	21.825613
85.737326	2931.348923	21.830631
85.923742	2928.028088	21.835648
86.250699	2929.981370	21.840666
85.921786	2939.395239	21.845683
86.294198	2930.421747	21.850701
86.386445	2942.797851	21.855719
86.237468	2932.932058	21.860736
86.572590	2929.913182	21.865754
86.317729	2931.302396	21.870771
86.565275	2930.907599	21.875789
86.371879	2931.631729	21.880807
86.361285	2930.927253	21.885824
86.535192	2931.765870	21.890842
86.449558	2933.800685	21.895859
86.458010	2936.292487	21.900877
86.687526	2932.394454	21.905895
86.596168	2943.718979	21.910912
87.122784	2953.841285	21.915930
86.921749	2965.522365	21.920947
87.159833	2960.355659	21.925965
86.882462	2969.343613	21.930983
86.838024	2972.451940	21.936000
87.376772	2980.837756	21.941018
86.962169	3002.343638	21.946035
87.278598	3000.525806	21.951053
87.409187	2989.946732	21.956071
87.406542	3005.553084	21.961088
87.706356	3013.501096	21.966106
87.621463	3018.110533	21.971123
88.035443	3018.284691	21.976141
88.068675	3027.614115	21.981159
87.876916	3025.854511	21.986176
88.193537	3033.612630	21.991194
88.040944	3050.181424	21.996211
88.284983	3052.638822	22.001229
88.470993	3053.021615	22.006247
88.392298	3050.704329	22.011264
89.087151	3065.455331	22.016282
89.200045	3073.057162	22.021299
89.361919	3058.846548	22.026317
89.008050	3047.499033	22.031335
89.181098	3047.179047	22.036352
89.265743	3036.556134	22.041370
88.746800	3046.623409	22.046387
89.042832	3060.921960	22.051405
89.334542	3074.990724	22.056423
89.308894	3079.216280	22.061440
89.582807	3078.331906	22.066458
89.233165	3083.389500	22.071475
89.859110	3094.673694	22.076493
89.599706	3099.237827	22.081511
89.703483	3115.723331	22.086528
89.814589	3103.844570	22.091546
89.370526	3115.728938	22.096563
89.807124	3126.024625	22.101581
90.699108	3115.188733	22.106599
90.740651	3121.174363	22.111616
91.017520	3111.500136	22.116634
90.974509	3117.375744	22.121651
90.913105	3115.365635	22.126669
91.339088	3122.027847	22.131687
90.842174	3116.582609	22.136704
91.545306	3105.245056	22.141722
91.367660	3109.835486	22.146739
91.040035	3097.553126	22.151757
91.266516	3098.882114	22.156775
91.236579	3111.457204	22.161792
91.386433	3110.529679	22.166810
91.525549	3119.706183	22.171827
91.635236	3105.665112	22.176845
91.741344	3109.990812	22.181863
91.403396	3110.265219	22.186880
91.409399	3105.988215	22.191898
91.506211	3133.647026	22.196915
91.719171	3140.667323	22.201933
92.220390	3145.533395	22.206951
91.664440	3148.776038	22.211968
91.852776	3159.203381	22.216986
91.917864	3173.281633	22.222003
92.348423	3174.864428	22.227021
92.215963	3180.648912	22.232039
92.242755	3191.106759	22.237056
93.010146	3201.395374	22.242074
93.009450	3206.652242	22.247091
92.909774	3213.927752	22.252109
93.132666	3210.836251	22.257127
92.710901	3216.043845	22.262144
93.046346	3210.092952	22.267162
92.711919	3221.672787	22.272179
93.085544	3231.848005	22.277197
93.357760	3243.409780	22.282215
93.622133	3246.512184	22.287232
93.868314	3240.808368	22.292250
93.419215	3248.590380	22.297267
93.233761	3244.663256	22.302285
93.654362	3260.106408	22.307303
93.783131	3275.102086	22.312320
94.134625	3275.661456	22.317338
94.078828	3278.716592	22.322355
94.295764	3270.472547	22.327373
94.792078	3266.140905	22.332391
94.248382	3278.542401	22.337408
94.139596	3273.728264	22.342426
94.512910	3289.312722	22.347443
94.275155	3301.749622	22.352461
94.549395	3302.234779	22.357479
94.676315	3304.620430	22.362496
94.885280	3307.839458	22.367514
95.207760	3340.651564	22.372531
95.363137	3333.211055	22.377549
95.476554	3333.249070	22.382567
95.406668	3330.525984	22.387584
95.440625	3322.115209	22.392602
95.572789	3331.968707	22.397619
95.567806	3323.378487	22.402637
95.798460	3327.642695	22.407655
95.807702	3330.786591	22.412672
96.325622	3335.646917	22.417690
96.270058	3344.511619	22.422707
96.382041	3351.655108	22.427725
96.778273	3346.703770	22.432743
96.293317	3337.289341	22.437760
96.280620	3331.754215	22.442778
96.309658	3341.277243	22.447795
96.534814	3347.092870	22.452813
96.577315	3346.698509	22.457831
96.283973	3352.729772	22.462848
96.709459	3361.402128	22.467866
96.795754	3383.425771	22.472883
97.350156	3370.619411	22.477901
97.838459	3352.548946	22.482919
97.901457	3363.635202	22.487936
97.899791	3343.237231	22.492954
98.071199	3334.321511	22.497971
98.097964	3350.371943	22.502989
98.412036	3335.520038	22.508007
98.259327	3335.602852	22.513024
98.227651	3314.437979	22.518042
98.292062	3308.588482	22.523059
98.240256	3309.291623	22.528077
98.333952	3306.540095	22.533095
98.036706	3316.632771	22.538112
98.262570	3331.860039	22.543130
98.783956	3340.729492	22.548147
98.616923	3344.636255	22.553165
98.786870	3344.717962	22.558183
98.461216	3360.245613	22.563200
98.862582	3349.991265	22.568218
98.540379	3343.644869	22.573235
98.785842	3347.055540	22.578253
98.995930	3360.295067	22.583271
99.413328	3376.304473	22.588288
99.305956	3375.506060	22.593306
99.249876	3380.836330	22.598323
99.364239	3387.460251	22.603341
99.315721	3383.798389	22.608359
99.397395	3389.398551	22.613376
99.521372	3401.798303	22.618394
99.516608	3407.055105	22.623411
99.525606	3421.665681	22.628429
99.854349	3414.797720	22.633447
99.603537	3424.809903	22.638464
100.011349	3429.454177	22.643482
100.135350	3430.722444	22.648499
100.117071	3444.741877	22.653517
100.468647	3451.366546	22.658535
100.617544	3470.399605	22.663552
101.040975	3463.094861	22.668570
100.921626	3466.264012	22.673587
100.692413	3466.973425	22.678605
101.066697	3470.019016	22.683623
100.977396	3465.883761	22.688640
101.233140	3478.383713	22.693658
101.407613	3483.941579	22.698675
101.402851	3500.908181	22.703693
102.110943	3490.152479	22.708711
102.004249	3487.708999	22.713728
102.223362	3478.651848	22.718746
102.290996	3482.716322	22.723763
102.036222	3488.860279	22.728781
102.333121	3479.080350	22.733799
102.012218	3480.615454	22.738816
102.494633	3473.958178	22.743834
102.524241	3472.755588	22.748851
102.689764	3471.532111	22.753869
102.734896	3473.318008	22.758887
102.552008	3480.897205	22.763904
102.564285	3470.196625	22.768922
103.125032	3492.200625	22.773939
102.735571	3508.216123	22.778957
103.114399	3501.303162	22.783975
103.061260	3504.024367	22.788992
102.719037	3513.816756	22.794010
103.581991	3518.116285	22.799027
103.490989	3530.116965	22.804045
103.382108	3527.901965	22.809063
103.460679	3539.442148	22.814080
103.890660	3532.706673	22.819098
103.846133	3537.175311	22.824115
103.597009	3542.153308	22.829133
104.120667	3556.858163	22.834151
104.151913	3558.722594	22.839168
104.221041	3569.157439	22.844186
104.116289	3568.700806	22.849203
104.113748	3565.655408	22.854221
104.449743	3583.573150	22.859239
104.350244	3589.336017	22.864256
104.787451	3596.934391	22.869274
104.677300	3601.574784	22.874291
104.749899	3605.516564	22.879309
104.739443	3613.231175	22.884327
104.858723	3625.974862	22.889344
104.979327	3633.631610	22.894362
105.218983	3631.062858	22.899379
105.246282	3640.140303	22.904397
105.722994	3647.072370	22.909415
105.948025	3658.034673	22.914432
105.931088	3666.936677	22.919450
106.150370	3652.700602	22.924467
105.762720	3656.094304	22.929485
106.135277	3658.079751	22.934503
106.081413	3660.047450	22.939520
106.061730	3673.110707	22.944538
106.504805	3682.308322	22.949555
106.600875	3689.530823	22.954573
106.769663	3688.301301	22.959591
106.728372	3688.481206	22.964608
106.856039	3682.970765	22.969626
107.422165	3678.973231	22.974643
107.189863	3681.881165	22.979661
107.610985	3670.707735	22.984679
107.901747	3660.380340	22.989696
107.857839	3661.443330	22.994714
108.002287	3653.319982	22.999731
108.267924	3658.251331	23.004749
108.361779	3657.117937	23.009767
108.207760	3658.552497	23.014784
108.013387	3658.860656	23.019802
108.604465	3652.822406	23.024819
107.895339	3656.851886	23.029837
108.228617	3654.857432	23.034855
108.432282	3666.137825	23.039872
108.503635	3675.054076	23.044890
108.534133	3684.835128	23.049907
108.799344	3684.863099	23.054925
108.810309	3676.768105	23.059943
108.896054	3689.156103	23.064960
108.951836	3684.673532	23.069978
109.343860	3676.904824	23.074995
109.020726	3702.141006	23.080013
109.639389	3707.337047	23.085031
109.593520	3705.204015	23.090048
109.606569	3706.281525	23.095066
110.116852	3704.295814	23.100083
109.544685	3705.488675	23.105101
109.938350	3706.949972	23.110119
109.888302	3704.366831	23.115136
109.723529	3716.544632	23.120154
110.420321	3721.124824	23.125171
110.165177	3733.357173	23.130189
110.109687	3729.154303	23.135207
110.446474	3730.483067	23.140224
110.497472	3732.632301	23.145242
110.494084	3732.719625	23.150259
110.497579	3756.287941	23.155277
110.801748	3755.866789	23.160295
110.709926	3764.170317	23.165312
110.750097	3767.311734	23.170330
111.458303	3772.487226	23.175347
111.503745	3790.455489	23.180365
111.565863	3793.637466	23.185383
111.547021	3788.778922	23.190400
111.487555	3801.081606	23.195418
111.901271	3799.299303	23.200435
111.524138	3802.147752	23.205453
111.716663	3807.502254	23.210471
112.150427	3828.984975	23.215488
112.100341	3835.706913	23.220506
112.488889	3822.121033	23.225523
112.406664	3829.446772	23.230541
112.420023	3831.288129	23.235559
113.138664	3831.147816	23.240576
113.617452	3821.411820	23.245594
113.681046	3822.359340	23.250611
113.610613	3813.666772	23.255629
113.890941	3799.437341	23.260647
113.600498	3806.569704	23.265664
113.254800	3795.076337	23.270682
113.723930	3798.740954	23.275699
113.649425	3795.602354	23.280717
113.790281	3811.428981	23.285735
113.891269	3823.539316	23.290752
113.925514	3827.645399	23.295770
113.918982	3828.796844	23.300787
113.768585	3839.531220	23.305805
113.832726	3839.648684	23.310823
114.297513	3852.365006	23.315840
113.873903	3865.199406	23.320858
114.184591	3864.776426	23.325875
114.404931	3889.032568	23.330893
114.482801	3889.313052	23.335911
114.836643	3898.110440	23.340928
114.851369	3902.196842	23.345946
115.036407	3921.987040	23.350963
115.174671	3930.644176	23.355981
115.103898	3929.248293	23.360999
115.526289	3939.001636	23.366016
115.412197	3952.682027	23.371034
116.040202	3956.714703	23.376051
115.965356	3959.639276	23.381069
116.190230	3967.165499	23.386087
116.311626	3958.223550	23.391104
116.240435	3961.775334	23.396122
116.555123	3954.684369	23.401139
116.358757	3951.827928	23.406157
116.367383	3959.607334	23.411175
116.814833	3964.076319	23.416192
116.363906	3982.529124	23.421210
116.960412	3981.886701	23.426227
116.871941	3986.958021	23.431245
116.791353	3989.332820	23.436263
117.276388	3988.032389	23.441280
116.997123	3996.714450	23.446298
117.276632	4005.932846	23.451315
117.356174	4019.096233	23.456333
117.328789	4018.547790	23.461351
117.475367	4018.312252	23.466368
117.546256	4043.353229	23.471386
117.784226	4043.372172	23.476403
118.163629	4043.666726	23.481421
118.136243	4048.052540	23.486439
118.503744	4064.532458	23.491456
118.154778	4073.383807	23.496474
118.741397	4069.236576	23.501491
118.707948	4071.093294	23.506509
118.874440	4069.049859	23.511527
118.653744	4081.470533	23.516544
118.914260	4097.275239	23.521562
119.296832	4091.539907	23.526579
119.619404	4100.259012	23.531597
119.568922	4097.711273	23.536615
119.807172	4098.544422	23.541632
119.852322	4097.229163	23.546650
120.059288	4100.453407	23.551667
120.021185	4097.029654	23.556685
119.945396	4111.245343	23.561703
120.476127	4117.182481	23.566720
120.282886	4129.312452	23.571738
120.530338	4121.138593	23.576755
120.764820	4118.434482	23.581773
120.859955	4112.292617	23.586791
120.970664	4123.863536	23.591808
120.940505	4116.419179	23.596826
121.072585	4107.941959	23.601843
120.840617	4134.972213	23.606861
120.956329	4151.294913	23.611879
121.145456	4147.020660	23.616896
121.128475	4163.388135	23.621914
121.298435	4167.191026	23.626931
121.522094	4177.804634	23.631949
121.455166	4186.609503	23.636967
121.644011	4179.681681	23.641984
122.026737	4209.486363	23.647002
122.640607	4200.453937	23.652019
122.312888	4215.942690	23.657037
122.507614	4211.204148	23.662055
122.748657	4205.347372	23.667072
122.610852	4209.319719	23.672090
122.998134	4205.712459	23.677107
122.801834	4217.540890	23.682125
122.790569	4227.096093	23.687143
123.056046	4237.861994	23.692160
123.004517	4239.365231	23.697178
123.191529	4232.751579	23.702195
123.242765	4243.797105	23.707213
123.431609	4251.672230	23.712231
123.853460	4264.749783	23.717248
123.551254	4269.325030	23.722266
123.941488	4267.415823	23.727283
124.453925	4262.248975	23.732301
124.372693	4266.825960	23.737319
124.547251	4264.902368	23.742336
124.786299	4276.256261	23.747354
125.204327	4272.935171	23.752371
125.333931	4276.848373	23.757389
125.033130	4273.122670	23.762407
125.530929	4261.776866	23.767424
125.709202	4268.408303	23.772442
125.878764	4259.875455	23.777459
125.727691	4250.650287	23.782477
125.795277	4246.790322	23.787495
125.729333	4248.551544	23.792512
125.654605	4251.288916	23.797530
126.077750	4253.784833	23.802547
126.074444	4251.280681	23.807565
125.856358	4260.964866	23.812583
126.203688	4258.093258	23.817600
126.270508	4275.126436	23.822618
126.581667	4279.581850	23.827635
126.689097	4285.029557	23.832653
126.855844	4286.929904	23.837671
127.221212	4273.997929	23.842688
127.057033	4284.627830	23.847706
127.218361	4278.089059	23.852723
127.236035	4271.545662	23.857741
127.377965	4294.399660	23.862759
127.469972	4295.468557	23.867776
127.641798	4306.940188	23.872794
127.443105	4311.284952	23.877811
127.643532	4309.018150	23.882829
127.898607	4326.927678	23.887847
127.989721	4348.465800	23.892864
127.761417	4348.344321	23.897882
128.435973	4344.828111	23.902899
128.627700	4347.113913	23.907917
128.589945	4353.025364	23.912935
128.959494	4354.729742	23.917952
128.899495	4362.280352	23.922970
129.067091	4349.331858	23.927987
129.639824	4347.178763	23.933005
129.635521	4360.984422	23.938023
129.557701	4360.388151	23.943040
129.340847	4358.330279	23.948058
129.814304	4366.624253	23.953075
129.671867	4372.671987	23.958093
129.575909	4389.074334	23.963111
129.926603	4393.452673	23.968128
130.130891	4387.808597	23.973146
130.382932	4389.356276	23.978163
130.318434	4385.839896	23.983181
130.251963	4403.812592	23.988199
130.843204	4404.456515	23.993216
130.882308	4425.873234	23.998234
130.898027	4416.741735	24.003251
131.055861	4408.722048	24.008269
130.483675	4411.658357	24.013287
131.029335	4430.186462	24.018304
131.048499	4444.199301	24.023322
131.178100	4453.058745	24.028339
131.430467	4462.749864	24.033357
131.595135	4472.123758	24.038375
131.807558	4485.606244	24.043392
131.456541	4487.647398	24.048410
131.881748	4508.629756	24.053427
132.302974	4502.345256	24.058445
131.961664	4510.644142	24.063463
132.449455	4527.449203	24.068480
132.150030	4541.962951	24.073498
132.402822	4547.312835	24.078515
132.914515	4562.437585	24.083533
133.067034	4576.656653	24.088551
133.234439	4568.322231	24.093568
133.167587	4581.319073	24.098586
133.263291	4582.343344	24.103603
133.966829	4587.987990	24.108621
133.785251	4597.218130	24.113639
134.107517	4594.739106	24.118656
133.856311	4599.702839	24.123674
134.240148	4600.130447	24.128691
134.347877	4611.302560	24.133709
134.456814	4623.726197	24.138727
134.695245	4628.642546	24.143744
134.648618	4631.344037	24.148762
134.754250	4631.509965	24.153779
135.182851	4628.249266	24.158797
135.190075	4654.188091	24.163815
135.251621	4652.086572	24.168832
135.475329	4658.345891	24.173850
135.536730	4653.382217	24.178867
135.646022	4651.086625	24.183885
135.731107	4662.035805	24.188903
136.091376	4679.064355	24.193920
136.126229	4695.207798	24.198938
136.116488	4699.369916	24.203955
136.681299	4683.367367	24.208973
136.269297	4697.010194	24.213991
136.792298	4694.406309	24.219008
136.761526	4704.533749	24.224026
136.715465	4704.527180	24.229043
137.199686	4705.801061	24.234061
136.959000	4706.535172	24.239079
137.094770	4706.671906	24.244096
137.207874	4711.553195	24.249114
137.356955	4718.656032	24.254131
137.349655	4732.685952	24.259149
137.242565	4735.114661	24.264167
137.615030	4741.688597	24.269184
137.853996	4763.068428	24.274202
138.121517	4757.832680	24.279219
138.058024	4761.421192	24.284237
138.229259	4775.658710	24.289255
138.888806	4784.480268	24.294272
139.247181	4783.424197	24.299290
139.166364	4793.526634	24.304307
139.644925	4787.356394	24.309325
139.421366	4793.584025	24.314343
139.601790	4784.034234	24.319360
139.943334	4783.199564	24.324378
139.713634	4790.097699	24.329395
139.996002	4785.806036	24.334413
139.947741	4786.664457	24.339431
139.935946	4785.921532	24.344448
140.179613	4799.568475	24.349466
140.155756	4812.784463	24.354483
140.447857	4814.097643	24.359501
140.375421	4818.900767	24.364519
140.451330	4815.391793	24.369536
140.652658	4830.288585	24.374554
140.246435	4851.190011	24.379571
140.669307	4852.319484	24.384589
140.786373	4867.852073	24.389607
141.318289	4873.351112	24.394624
141.224817	4879.809798	24.399642
141.445664	4903.368103	24.404659
141.394449	4903.768323	24.409677
141.639443	4914.792110	24.414695
141.667202	4926.270674	24.419712
141.964262	4937.958856	24.424730
142.016106	4940.695841	24.429747
142.401276	4950.239438	24.434765
142.167315	4975.302282	24.439783
142.479313	4972.377954	24.444800
142.746517	4993.537256	24.449818
142.671744	5014.829795	24.454835
143.294452	5016.598527	24.459853
143.140938	5016.590996	24.464871
143.228440	5030.669023	24.469888
143.517091	5045.854226	24.474906
143.214339	5043.788710	24.479923
143.719142	5054.615395	24.484941
143.798267	5068.437522	24.489959
143.989401	5054.387120	24.494976
144.205265	5071.937173	24.499994
144.254808	5092.343770	24.505011
144.807602	5095.216480	24.510029
144.623849	5092.304303	24.515047
144.965323	5099.611889	24.520064
144.791221	5096.876769	24.525082
145.035292	5122.259382	24.530099
144.959073	5132.173278	24.535117
145.102153	5140.366165	24.540135
145.672247	5151.566455	24.545152
145.941550	5147.971491	24.550170
145.818039	5155.536566	24.555187
146.291018	5159.092345	24.560205
146.244488	5161.025242	24.565223
145.901337	5162.807956	24.570240
146.449064	5176.451610	24.575258
146.303348	5186.207468	24.580275
146.733586	5174.354836	24.585293
146.778580	5189.323337	24.590311
146.899909	5205.188406	24.595328
147.165398	5210.460192	24.600346
147.123562	5219.463874	24.605363
147.175910	5220.207144	24.610381
147.516511	5231.313484	24.615399
147.496298	5241.475012	24.620416
147.861756	5251.307547	24.625434
148.267073	5264.270613	24.630451
148.455093	5270.365153	24.635469
148.539913	5282.345513	24.640487
148.474501	5275.883370	24.645504
148.853663	5276.673667	24.650522
148.539238	5283.025352	24.655539
148.899867	5290.927931	24.660557
148.909673	5307.409631	24.665575
149.038690	5301.146215	24.670592
149.475874	5317.017688	24.675610
149.462062	5343.382002	24.680627
149.893910	5334.038818	24.685645
150.062854	5345.604558	24.690663
149.887626	5338.398294	24.695680
150.084355	5351.035137	24.700698
150.085887	5365.868339	24.705715
150.494302	5371.679943	24.710733
150.587788	5371.150728	24.715751
150.649983	5374.859394	24.720768
150.885576	5387.202895	24.725786
150.749570	5399.507310	24.730803
151.471494	5395.936104	24.735821
151.265167	5416.111719	24.740839
151.454498	5424.543652	24.745856
151.836788	5422.456971	24.750874
151.688522	5429.283407	24.755891
151.896283	5418.427508	24.760909
152.099112	5445.261789	24.765927
152.207601	5459.005640	24.770944
152.226698	5459.559888	24.775962
152.565607	5462.765757	24.780979
152.717436	5462.648954	24.785997
152.812406	5475.290327	24.791015
153.002013	5482.689984	24.796032
153.386421	5474.934935	24.801050
153.387819	5481.337056	24.806067
153.852919	5470.969594	24.811085
153.935219	5477.522465	24.816103
153.768006	5475.432915	24.821120
154.037181	5485.008731	24.826138
154.035932	5505.904724	24.831155
154.181878	5504.219214	24.836173
154.133957	5515.038383	24.841191
154.114061	5517.316414	24.846208
154.853360	5518.284552	24.851226
154.920886	5530.571571	24.856243
155.104689	5525.184466	24.861261
155.056225	5530.658277	24.866279
155.035385	5526.966291	24.871296
155.596558	5547.430411	24.876314
155.287091	5556.115834	24.881331
156.093476	5549.808825	24.886349
156.234662	5563.356370	24.891367
155.887065	5556.418242	24.896384
156.321770	5569.297425	24.901402
156.252719	5586.227891	24.906419
156.445265	5588.564901	24.911437
156.730069	5588.036645	24.916455
156.764405	5605.591099	24.921472
157.295528	5611.772697	24.926490
157.066657	5621.069235	24.931507
157.843535	5613.231080	24.936525
157.977634	5616.548319	24.941543
157.677013	5609.354835	24.946560
158.107271	5599.993644	24.951578
158.063293	5613.470835	24.956595
157.945284	5626.867001	24.961613
158.395208	5629.649219	24.966631
158.294337	5630.648259	24.971648
158.669431	5634.559661	24.976666
158.437558	5655.802636	24.981683
158.928520	5661.167668	24.986701
158.866269	5659.776555	24.991719
159.137078	5670.591437	24.996736
159.639329	5676.742261	25.001754
159.213616	5692.551092	25.006771
159.598259	5696.801672	25.011789
159.762436	5702.656286	25.016807
159.660253	5724.760683	25.021824
159.819761	5722.889662	25.026842
159.938498	5736.534574	25.031859
160.132942	5751.423951	25.036877
160.289193	5749.552659	25.041895
160.524183	5763.452080	25.046912
160.806023	5774.829418	25.051930
160.732173	5792.243982	25.056947
161.128937	5789.853598	25.061965
161.337353	5799.613190	25.066983
161.705810	5813.594449	25.072000
162.000238	5814.537553	25.077018
161.898429	5821.270212	25.082035
162.551660	5797.897309	25.087053
162.652487	5794.890834	25.092071
162.572916	5800.001480	25.097088
162.576525	5799.354398	25.102106
162.743888	5807.788480	25.107123
163.050678	5822.077779	25.112141
163.371962	5824.274706	25.117159
163.269621	5834.895855	25.122176
163.383792	5826.476374	25.127194
163.407113	5835.433847	25.132211
163.773998	5832.686290	25.137229
163.896092	5844.950707	25.142247
163.775795	5856.256110	25.147264
164.370861	5863.047625	25.152282
164.572028	5856.042314	25.157299
164.107521	5860.293004	25.162317
164.287729	5879.491771	25.167335
164.472245	5887.846056	25.172352
164.717332	5894.476229	25.177370
165.136740	5913.307226	25.182387
165.031390	5925.401043	25.187405
165.530681	5913.249631	25.192423
165.326564	5936.829345	25.197440
165.795441	5942.388412	25.202458
165.580004	5959.064898	25.207475
165.754457	5956.146576	25.212493
166.118920	5981.132223	25.217511
166.091229	5987.817733	25.222528
166.628226	5988.238282	25.227546
166.936106	6011.374544	25.232563
166.537988	6020.496103	25.237581
167.124138	6021.077195	25.242599
166.953304	6046.037360	25.247616
167.173108	6045.339273	25.252634
167.570179	6051.765889	25.257651
167.614221	6060.787075	25.262669
168.081541	6081.670540	25.267687
167.967904	6092.130801	25.272704
168.328326	6090.558952	25.277722
168.256065	6101.241587	25.282739
168.631678	6106.260878	25.287757
168.618511	6104.508613	25.292775
168.383141	6116.838118	25.297792
168.796966	6120.707282	25.302810
168.800523	6141.109279	25.307827
168.678959	6152.476480	25.312845
169.227247	6161.095516	25.317863
169.268418	6188.654045	25.322880
169.606349	6196.492278	25.327898
169.687749	6211.210516	25.332915
169.918988	6226.502080	25.337933
170.216883	6232.704606	25.342951
170.213376	6250.856763	25.347968
170.622873	6258.825248	25.352986
170.541910	6269.120697	25.358003
170.655641	6276.796438	25.363021
171.202851	6295.079581	25.368039
171.038312	6298.156609	25.373056
171.488788	6296.468880	25.378074
171.710226	6316.746678	25.383091
171.667517	6325.212189	25.388109
172.582009	6316.247019	25.393127
172.915178	6309.723236	25.398144
173.215181	6301.023645	25.403162
173.705831	6299.542742	25.408179
173.595818	6290.318407	25.413197
174.160031	6289.642507	25.418215
174.007246	6293.410858	25.423232
174.361285	6268.224070	25.428250
174.089412	6254.426543	25.433267
174.415365	6258.224777	25.438285
174.443883	6250.677144	25.443303
174.337014	6253.343685	25.448320
174.293035	6243.993973	25.453338
174.583363	6271.545191	25.458355
174.769353	6280.772845	25.463373
174.783740	6289.700544	25.468391
174.635399	6289.818076	25.473408
174.717974	6297.825331	25.478426
175.137701	6313.136503	25.483443
175.217617	6324.556689	25.488461
175.627909	6332.577019	25.493479
175.511069	6350.966109	25.498496
175.542762	6359.579504	25.503514
175.763497	6374.148221	25.508531
175.744728	6377.180779	25.513549
176.919394	6371.299408	25.518567
177.346519	6366.777280	25.523584
177.953106	6353.736591	25.528602
178.098152	6338.032106	25.533619
177.975397	6346.257818	25.538637
178.318417	6341.483944	25.543655
178.301448	6344.871857	25.548672
178.682778	6345.590272	25.553690
178.398487	6339.489886	25.558707
178.334545	6331.392007	25.563725
178.381751	6331.924496	25.568743
178.730939	6333.844808	25.573760
178.918191	6324.513257	25.578778
179.249397	6331.473742	25.583795
178.876118	6348.551936	25.588813
179.232853	6353.227329	25.593831
179.152584	6369.866986	25.598848
179.521814	6363.013255	25.603866
179.635673	6361.253296	25.608883
179.373135	6383.876011	25.613901
179.585564	6388.214839	25.618919
179.794382	6402.344070	25.623936
180.080777	6420.451787	25.628954
180.430428	6424.145572	25.633971
180.026025	6432.242345	25.638989
180.564763	6443.063861	25.644007
180.839524	6451.042917	25.649024
180.903267	6465.382606	25.654042
180.775373	6489.410556	25.659059
181.170543	6490.758606	25.664077
181.489687	6508.601945	25.669095
181.697268	6519.057715	25.674112
181.813849	6516.877917	25.679130
182.347088	6536.041705	25.684148
182.370362	6550.629490	25.689165
182.610280	6557.740761	25.694183
182.695377	6561.317030	25.699200
182.925250	6581.180753	25.704218
182.932348	6595.602775	25.709236
183.017106	6604.629602	25.714253
183.203929	6615.696196	25.719271
183.258922	6634.042502	25.724288
183.737445	6643.588840	25.729306
183.775777	6643.380756	25.734324
183.739430	6667.492752	25.739341
184.326889	6679.777299	25.744359
183.978189	6695.371901	25.749376
184.398704	6713.235125	25.754394
184.897678	6721.411489	25.759412
184.854604	6736.593092	25.764429
185.206129	6752.886573	25.769447
185.124036	6769.818103	25.774464
185.636915	6787.157595	25.779482
185.668160	6780.416575	25.784500
185.873873	6813.451733	25.789517
186.207676	6822.057358	25.794535
186.577639	6820.290349	25.799552
186.552457	6832.421692	25.804570
186.644304	6843.048006	25.809588
186.801109	6854.572008	25.814605
187.219604	6866.256521	25.819623
187.429319	6873.493150	25.824640
187.469862	6889.061302	25.829658
187.644648	6894.933582	25.834676
188.022419	6909.103240	25.839693
188.207291	6910.182704	25.844711
188.305207	6923.337089	25.849728
188.434154	6940.677384	25.854746
188.690956	6954.301403	25.859764
188.713465	6955.862352	25.864781
188.974207	6967.835696	25.869799
189.159470	6981.279937	25.874816
189.122439	6987.920172	25.879834
189.839421	6991.531929	25.884852
189.814159	7004.399145	25.889869
190.338232	6993.084861	25.894887
190.779461	6994.399650	25.899904
191.235286	6997.661973	25.904922
191.385641	6977.634488	25.909940
191.066291	6986.363229	25.914957
191.196264	6978.093232	25.919975
191.452940	6980.196772	25.924992
191.260760	6988.101846	25.930010
191.673164	7003.483359	25.935028
191.747149	6998.612896	25.940045
192.229918	7001.771779	25.945063
192.194684	7011.241318	25.950080
192.389098	7026.866130	25.955098
192.512617	7030.843986	25.960116
192.553975	7039.010864	25.965133
192.904440	7050.773254	25.970151
193.031504	7067.888952	25.975168
192.623200	7073.201949	25.980186
193.163438	7084.914437	25.985204
192.964150	7108.520411	25.990221
193.683595	7120.153209	25.995239
194.104346	7130.920076	26.000256
193.772311	7139.735123	26.005274
194.235822	7160.979535	26.010292
194.022894	7176.871675	26.015309
194.521265	7189.718518	26.020327
194.654584	7202.910783	26.025344
194.592934	7220.322709	26.030362
195.128769	7233.782104	26.035380
194.926411	7252.783181	26.040397
195.306370	7270.456822	26.045415
195.485254	7284.325697	26.050432
195.928654	7303.969063	26.055450
196.404115	7302.800524	26.060468
195.970339	7326.334062	26.065485
196.328617	7331.207817	26.070503
196.894658	7353.819503	26.075520
197.002980	7365.406320	26.080538
197.571730	7367.260291	26.085556
197.568575	7374.392217	26.090573
198.089933	7385.744411	26.095591
198.473709	7398.882756	26.100608
198.122597	7396.483492	26.105626
198.482190	7386.418357	26.110644
198.522085	7406.058911	26.115661
199.115799	7410.816861	26.120679
199.728785	7407.971953	26.125696
199.951063	7418.413029	26.130714
200.449451	7399.802552	26.135732
200.063992	7401.932987	26.140749
200.336316	7405.646824	26.145767
200.406208	7410.068088	26.150784
200.439473	7405.823661	26.155802
200.289413	7408.502014	26.160820
200.480335	7412.778867	26.165837
200.732216	7427.725294	26.170855
200.807562	7439.307983	26.175872
200.804191	7438.131185	26.180890
201.135954	7458.521216	26.185908
201.506743	7476.542798	26.190925
201.212638	7479.067470	26.195943
201.697794	7491.617662	26.200960
201.698414	7504.752268	26.205978
202.140083	7502.989489	26.210996
202.215656	7524.101906	26.216013
202.228910	7544.006957	26.221031
202.241587	7547.510812	26.226048
202.142868	7574.195567	26.231066
202.690264	7591.162228	26.236084
202.628407	7611.350824	26.241101
203.010400	7627.826116	26.246119
203.370598	7655.115767	26.251136
203.412825	7681.097177	26.256154
203.784978	7692.125976	26.261172
203.583434	7714.192896	26.266189
203.977014	7735.328093	26.271207
204.535451	7743.597843	26.276224
204.860019	7773.670783	26.281242
205.097920	7780.198289	26.286260
205.131014	7783.617106	26.291277
205.289204	7802.332012	26.296295
205.445165	7818.254548	26.301312
205.561047	7834.439236	26.306330
206.395869	7842.264833	26.311348
206.554700	7864.330785	26.316365
207.099377	7868.169325	26.321383
207.730983	7867.399607	26.326400
208.021112	7862.052552	26.331418
208.465601	7855.431665	26.336436
208.504212	7856.046632	26.341453
208.427602	7851.076356	26.346471
208.333976	7848.444353	26.351488
208.343566	7849.839450	26.356506
209.076651	7856.974627	26.361524
208.984751	7873.319964	26.366541
208.875932	7881.367240	26.371559
208.983410	7881.908275	26.376576
209.022846	7902.250695	26.381594
209.320409	7914.026137	26.386612
209.315913	7926.892016	26.391629
209.528154	7942.695150	26.396647
209.648408	7956.580686	26.401664
209.854201	7988.322376	26.406682
210.477388	7981.818525	26.411700
210.932568	7996.032752	26.416717
210.556281	8010.132456	26.421735
210.978758	8007.260367	26.426752
211.023921	8032.499852	26.431770
211.088784	8032.827742	26.436788
211.445229	8047.945802	26.441805
211.716397	8062.083586	26.446823
211.899141	8071.373857	26.451840
212.115714	8093.576523	26.456858
212.161507	8096.267054	26.461876
212.540041	8114.324371	26.466893
212.647976	8130.836828	26.471911
213.171133	8136.469132	26.476928
213.191663	8149.054607	26.481946
213.450512	8158.418968	26.486964
213.680641	8171.808340	26.491981
213.707488	8193.334344	26.496999
213.869701	8201.650601	26.502016
213.995206	8221.161716	26.507034
214.305496	8235.882053	26.512052
214.290006	8248.130251	26.517069
214.562027	8273.326892	26.522087
215.361538	8282.910074	26.527104
215.342903	8297.455093	26.532122
215.293163	8299.895299	26.537140
215.827779	8319.649406	26.542157
215.954002	8331.903803	26.547175
216.533779	8354.193749	26.552192
216.554119	8367.069031	26.557210
216.893778	8360.749116	26.562228
217.359693	8380.327751	26.567245
217.094078	8401.335655	26.572263
217.512519	8391.034617	26.577280
217.469521	8414.109364	26.582298
217.933327	8423.928728	26.587316
218.227876	8431.045960	26.592333
218.279126	8449.535953	26.597351
218.734653	8449.690613	26.602368
219.046312	8458.652878	26.607386
219.436790	8448.771373	26.612404
219.723899	8472.719031	26.617421
220.218204	8470.894242	26.622439
220.859609	8462.157867	26.627456
221.004715	8451.363274	26.632474
221.279187	8454.973551	26.637492
221.274638	8453.111038	26.642509
221.235990	8466.509684	26.647527
221.457731	8458.075118	26.652544
221.424675	8467.318196	26.657562
221.612739	8455.610978	26.662580
221.533406	8459.690806	26.667597
221.301140	8470.266465	26.672615
221.921187	8471.685490	26.677632
221.541942	8492.073028	26.682650
222.139236	8506.987505	26.687668
222.054952	8511.782686	26.692685
222.255027	8530.005886	26.697703
222.398172	8551.186885	26.702720
222.406957	8582.805427	26.707738
222.783217	8595.098086	26.712756
223.064766	8606.501645	26.717773
223.078240	8632.250448	26.722791
223.663308	8649.039968	26.727808
223.484155	8667.374156	26.732826
224.063816	8686.805606	26.737844
224.307202	8698.032745	26.742861
224.774979	8718.531481	26.747879
225.212897	8715.780353	26.752896
225.239572	8735.721441	26.757914
225.842695	8740.594798	26.762932
225.658284	8751.465611	26.767949
225.791322	8769.453470	26.772967
226.136476	8777.674385	26.777984
226.214586	8782.007392	26.783002
226.774135	8807.863033	26.788020
227.072980	8802.947482	26.793037
227.205931	8807.494465	26.798055
227.486062	8820.444011	26.803072
227.756885	8840.709893	26.808090
228.002661	8827.963441	26.813108
228.565190	8856.721018	26.818125
228.734635	8868.918205	26.823143
228.932881	8864.629358	26.828160
228.667618	8868.408412	26.833178
228.842050	8882.305449	26.838196
229.204513	8900.720415	26.843213
229.243924	8913.090646	26.848231
229.905721	8917.336151	26.853248
229.993806	8928.156175	26.858266
230.377219	8940.750963	26.863284
230.625765	8950.966212	26.868301
230.825611	8956.598433	26.873319
231.079825	8956.376365	26.878336
231.207337	8970.403338	26.883354
231.338322	8982.255365	26.888372
231.260672	8993.650377	26.893389
231.384799	9010.339472	26.898407
231.876257	9019.680277	26.903424
231.631900	9046.696998	26.908442
231.981728	9057.114560	26.913460
232.334151	9075.944111	26.918477
232.259759	9095.978912	26.923495
232.655594	9098.403303	26.928512
232.918914	9126.968282	26.933530
233.185916	9146.252642	26.938548
233.439499	9166.740100	26.943565
233.808591	9187.473206	26.948583
234.009423	9199.641654	26.953600
234.064886	9227.804759	26.958618
234.533431	9252.130428	26.963636
234.589109	9259.603293	26.968653
234.645880	9287.018268	26.973671
235.337172	9295.985837	26.978688
235.248166	9327.051357	26.983706
235.629460	9326.219176	26.988724
235.828741	9341.976272	26.993741
236.274370	9362.154394	26.998759
236.856193	9361.117499	27.003776
236.783821	9383.642011	27.008794
237.104157	9388.162446	27.013812
237.487369	9389.367877	27.018829
237.322483	9411.360611	27.023847
238.056751	9418.798175	27.028864
238.396457	9411.870650	27.033882
238.512689	9420.166976	27.038900
239.201794	9432.477348	27.043917
239.363955	9430.429558	27.048935
240.239997	9416.854166	27.053952
240.454735	9415.373684	27.058970
240.345746	9411.296569	27.063988
240.759126	9407.538731	27.069005
240.929315	9406.907829	27.074023
241.166058	9411.583651	27.079040
241.474823	9405.880511	27.084058
241.556536	9404.768694	27.089076
241.684000	9407.158007	27.094093
241.256673	9412.681039	27.099111
241.872269	9409.258885	27.104128
241.733916	9406.471616	27.109146
241.916409	9425.462485	27.114164
242.218244	9438.901766	27.119181
242.312293	9433.293443	27.124199
242.600090	9447.019075	27.129216
242.578690	9461.431084	27.134234
242.771875	9482.121023	27.139252
242.846310	9497.590862	27.144269
242.966050	9520.326562	27.149287
243.348116	9528.847758	27.154304
243.377176	9564.930971	27.159322
243.446690	9582.303475	27.164340
243.790310	9599.089270	27.169357
244.163225	9639.378298	27.174375
244.481499	9650.134995	27.179392
244.604044	9672.325474	27.184410
245.154682	9696.992147	27.189428
245.857678	9702.501550	27.194445
245.840209	9728.236697	27.199463
245.916328	9739.307121	27.204480
246.395951	9754.319126	27.209498
246.229242	9772.888383	27.214516
246.880230	9793.021953	27.219533
246.756556	9811.804368	27.224551
247.076077	9824.384508	27.229568
247.348924	9847.201754	27.234586
247.209725	9873.459457	27.239604
247.740935	9883.759748	27.244621
247.852539	9915.744040	27.249639
248.392398	9932.077081	27.254656
248.638933	9946.007682	27.259674
248.835951	9963.373679	27.264692
249.338928	9980.047136	27.269709
249.516175	9980.464585	27.274727
249.477783	10007.659539	27.279744
249.663155	10015.517030	27.284762
249.887809	10034.215074	27.289780
250.471553	10044.551175	27.294797
250.485866	10070.888244	27.299815
250.967366	10080.613800	27.304832
251.149712	10101.082012	27.309850
250.743382	10116.713730	27.314868
251.333035	10137.235118	27.319885
251.689528	10158.619694	27.324903
252.392448	10161.829175	27.329920
252.540110	10182.391175	27.334938
253.370198	10183.642315	27.339956
254.145682	10184.311882	27.344973
254.147005	10197.621482	27.349991
254.416617	10183.394399	27.355008
254.494590	10173.763859	27.360026
254.977288	10191.570967	27.365044
255.302145	10202.885414	27.370061
255.345062	10207.488100	27.375079
255.636705	10214.196602	27.380096
255.891270	10214.130691	27.385114
255.769285	10216.147097	27.390132
256.446614	10205.083427	27.395149
256.243330	10226.587634	27.400167
256.601143	10233.646847	27.405184
257.089638	10228.486928	27.410202
256.836614	10240.179215	27.415220
256.968145	10251.860188	27.420237
257.098934	10264.664787	27.425255
257.398081	10280.378221	27.430272
257.557860	10299.254182	27.435290
257.538200	10318.433055	27.440308
258.067223	10322.851644	27.445325
257.970540	10354.423028	27.450343
259.019461	10361.780218	27.455360
259.491464	10372.361815	27.460378
259.548180	10384.451094	27.465396
260.311449	10378.993502	27.470413
260.426070	10388.525493	27.475431
260.841924	10398.395126	27.480448
260.832687	10415.359679	27.485466
260.713749	10423.246215	27.490484
260.664930	10426.732603	27.495501
260.888082	10450.822292	27.500519
261.104568	10458.471209	27.505536
261.655017	10469.949020	27.510554
261.333585	10503.184554	27.515572
261.721323	10518.007338	27.520589
261.875414	10532.548624	27.525607
262.000752	10552.385087	27.530624
262.746592	10570.888957	27.535642
262.580842	10599.084373	27.540660
263.348512	10612.292643	27.545677
263.162342	10633.776006	27.550695
263.110316	10658.169422	27.555712
263.373035	10674.164347	27.560730
263.717603	10697.617428	27.565748
263.893418	10714.430823	27.570765
264.556683	10745.106625	27.575783
264.898721	10761.288717	27.580800
265.291633	10773.842605	27.585818
265.417188	10792.739986	27.590836
265.939090	10804.908729	27.595853
266.046872	10833.453529	27.600871
266.237266	10852.253874	27.605888
267.112301	10856.517708	27.610906
267.084940	10875.635941	27.615924
267.337341	10886.287734	27.620941
267.521602	10902.040200	27.625959
267.816385	10926.253029	27.630976
268.265879	10927.779191	27.635994
268.002736	10947.365038	27.641012
268.822515	10958.208608	27.646029
269.091364	10981.598050	27.651047
269.184235	11004.962452	27.656064
269.376199	11009.663228	27.661082
269.260462	11026.267642	27.666100
269.497781	11051.136221	27.671117
270.062385	11060.357242	27.676135
270.546687	11079.526206	27.681152
270.672878	11104.257334	27.686170
270.797129	11125.756845	27.691188
271.102163	11125.190175	27.696205
271.256021	11141.336358	27.701223
271.902623	11172.626267	27.706240
272.335689	11179.310691	27.711258
272.882268	11197.959649	27.716276
273.072119	11208.957727	27.721293
273.410767	11214.260922	27.726311
273.778104	11232.269468	27.731328
274.245894	11243.141804	27.736346
274.259092	11248.955761	27.741364
274.575769	11256.070223	27.746381
274.715539	11275.048978	27.751399
274.675875	11280.090577	27.756416
275.146104	11297.767177	27.761434
274.624441	11315.194188	27.766452
275.307172	11333.126607	27.771469
275.607565	11350.719753	27.776487
275.789132	11376.745142	27.781504
275.948704	11383.624375	27.786522
276.109786	11411.674750	27.791540
276.308782	11432.896939	27.796557
276.539587	11464.569161	27.801575
276.669835	11492.423889	27.806592
276.924743	11507.330999	27.811610
277.281087	11543.245936	27.816628
277.373165	11554.857461	27.821645
278.235607	11586.339525	27.826663
278.526115	11597.931850	27.831680
279.111996	11613.247948	27.836698
279.040208	11634.241635	27.841716
279.394144	11659.615658	27.846733
279.699156	11669.608480	27.851751
279.948463	11686.220364	27.856768
280.027996	11693.385624	27.861786
280.211495	11720.195258	27.866804
280.316832	11727.771231	27.871821
280.761881	11763.260101	27.876839
280.909535	11781.415694	27.881856
281.199666	11803.465698	27.886874
281.480300	11844.844614	27.891892
282.075292	11852.550400	27.896909
282.613651	11875.073161	27.901927
282.923267	11894.768859	27.906944
283.060897	11904.658443	27.911962
283.001511	11934.638944	27.916980
283.694013	11946.477785	27.921997
284.125728	11968.232722	27.927015
284.164132	11978.452825	27.932032
284.794129	11991.785796	27.937050
284.826653	12015.235754	27.942068
285.308893	12022.179159	27.947085
285.649440	12038.232979	27.952103
285.951270	12062.946330	27.957120
286.277277	12070.783852	27.962138
286.425561	12088.613642	27.967156
286.803593	12098.499077	27.972173
287.207557	12113.546356	27.977191
287.071803	12132.677346	27.982208
287.568859	12136.937850	27.987226
287.531674	12156.122033	27.992244
287.868574	12175.241693	27.997261
288.039071	12185.963935	28.002279
288.497835	12217.380203	28.007296
288.799506	12232.466732	28.012314
289.233850	12255.204014	28.017332
289.395911	12273.771935	28.022349
289.787559	12289.587341	28.027367
289.624378	12318.785697	28.032384
290.389506	12332.997632	28.037402
290.430139	12359.599744	28.042420
290.884047	12382.953486	28.047437
291.066167	12405.087700	28.052455
291.194325	12429.957831	28.057472
291.444693	12443.762310	28.062490
291.731936	12475.163944	28.067508
291.725519	12500.821443	28.072525
292.182254	12529.776950	28.077543
292.284326	12558.985143	28.082560
292.843105	12579.033132	28.087578
293.223089	12603.277564	28.092596
293.121684	12630.240184	28.097613
293.728242	12642.110687	28.102631
293.780203	12665.132027	28.107648
294.462331	12685.366438	28.112666
294.402482	12713.574665	28.117684
294.775448	12729.937341	28.122701
294.785130	12760.219778	28.127719
294.988100	12786.579795	28.132736
295.765729	12811.535065	28.137754
295.629617	12837.987395	28.142772
296.012746	12864.270321	28.147789
296.589490	12884.905936	28.152807
296.752010	12912.671331	28.157824
297.080880	12943.378218	28.162842
297.343105	12968.253047	28.167860
297.775455	12996.525234	28.172877
298.457084	13007.668217	28.177895
298.549212	13034.663873	28.182912
299.276079	13046.420269	28.187930
299.770866	13059.746213	28.192948
300.099901	13087.745158	28.197965
300.563138	13085.286497	28.202983
301.025503	13100.203135	28.208000
301.286327	13109.306952	28.213018
301.496304	13118.275117	28.218036
301.479081	13125.731792	28.223053
301.781303	13146.204290	28.228071
301.670973	13162.601954	28.233088
302.558342	13175.700415	28.238106
302.895858	13174.190368	28.243124
303.256839	13197.634759	28.248141
303.738774	13194.645486	28.253159
303.476442	13216.604736	28.258176
303.797318	13224.872596	28.263194
304.220694	13237.755575	28.268212
304.577491	13258.284568	28.273229
304.983183	13265.856828	28.278247
305.133303	13287.730367	28.283264
305.382604	13298.252495	28.288282
305.454064	13317.055362	28.293300
305.640172	13328.240169	28.298317
306.585108	13343.067734	28.303335
306.640619	13355.164978	28.308352
306.933802	13379.471417	28.313370
307.174572	13387.488815	28.318388
307.456773	13404.356125	28.323405
307.975602	13424.523480	28.328423
307.858230	13441.705241	28.333440
308.636436	13451.083403	28.338458
308.751524	13471.705131	28.343476
308.925722	13488.594447	28.348493
309.242058	13506.848605	28.353511
309.617224	13525.500591	28.358528
309.931459	13546.323989	28.363546
309.876300	13565.565448	28.368564
309.883552	13587.802065	28.373581
310.289251	13591.684631	28.378599
310.333702	13627.333502	28.383616
310.702753	13653.403254	28.388634
311.114326	13674.940864	28.393652
311.368264	13704.388198	28.398669
311.762814	13717.760219	28.403687
312.331769	13730.544447	28.408704
312.915175	13749.841411	28.413722
313.201566	13770.877280	28.418740
313.375840	13783.954326	28.423757
314.252862	13781.975547	28.428775
314.224771	13809.599762	28.433792
314.883034	13808.729914	28.438810
315.308548	13819.661718	28.443828
315.602856	13834.884541	28.448845
316.295007	13841.956713	28.453863
316.345321	13845.261780	28.458880
316.724890	13865.918542	28.463898
317.895003	13853.376892	28.468916
318.881383	13822.215200	28.473933
319.488992	13806.734989	28.478951
319.358774	13792.114836	28.483968
319.531801	13778.689093	28.488986
319.578118	13776.319311	28.494004
319.492834	13776.361983	28.499021
319.964372	13771.306329	28.504039
319.925987	13776.858864	28.509056
320.161313	13775.252673	28.514074
320.469013	13783.168788	28.519092
320.233351	13784.430429	28.524109
320.753303	13786.917200	28.529127
320.523082	13812.044982	28.534144
320.623600	13827.590352	28.539162
320.878756	13849.664147	28.544180
321.063047	13879.689527	28.549197
321.240187	13903.260542	28.554215
321.342022	13932.867472	28.559232
321.781365	13961.780157	28.564250
321.724794	13993.035817	28.569268
321.657837	14025.205699	28.574285
322.423825	14061.245003	28.579303
322.258484	14108.482103	28.584320
322.821172	14141.327601	28.589338
323.291534	14178.208621	28.594356
323.608114	14217.143361	28.599373
323.825552	14242.033011	28.604391
324.005595	14288.383990	28.609408
324.659565	14323.112890	28.614426
325.004719	14353.340187	28.619444
325.411244	14390.006442	28.624461
326.280142	14409.100799	28.629479
326.465077	14436.310962	28.634496
326.924894	14455.226525	28.639514
327.696071	14485.922701	28.644532
327.567488	14495.983240	28.649549
328.131769	14525.832611	28.654567
328.242674	14544.793561	28.659584
328.466431	14560.738066	28.664602
329.072401	14585.479162	28.669620
329.058202	14609.344996	28.674637
329.668489	14620.137120	28.679655
329.895950	14653.941611	28.684672
329.982863	14675.908490	28.689690
330.532596	14693.234106	28.694708
330.568415	14730.859907	28.699725
331.268789	14746.589199	28.704743
330.922882	14772.821351	28.709760
331.359360	14809.215374	28.714778
331.633885	14839.027689	28.719796
331.787665	14873.932125	28.724813
332.702825	14896.487480	28.729831
332.853774	14927.654492	28.734848
332.982889	14965.966873	28.739866
333.697814	14986.224509	28.744884
333.894773	15024.259530	28.749901
334.326022	15052.534710	28.754919
334.532625	15079.664025	28.759936
335.238443	15084.090302	28.764954
335.792671	15108.225320	28.769972
336.061740	15138.291607	28.774989
336.836246	15157.851095	28.780007
337.239408	15165.085483	28.785024
337.589768	15183.771984	28.790042
337.633718	15199.819913	28.795060
337.738340	15225.224834	28.800077
338.657534	15228.145103	28.805095
339.012324	15250.623972	28.810112
339.166674	15258.123422	28.815130
339.728522	15277.531153	28.820148
339.876108	15304.544106	28.825165
340.255681	15310.476784	28.830183
340.504302	15322.131960	28.835200
340.674147	15340.123892	28.840218
340.973351	15353.573753	28.845236
341.264830	15379.966344	28.850253
341.579240	15382.731290	28.855271
341.798224	15418.296366	28.860288
341.840721	15439.636648	28.865306
342.708289	15462.146493	28.870324
342.507393	15495.285852	28.875341
342.871426	15521.069160	28.880359
343.245550	15553.182662	28.885376
343.461249	15577.670563	28.890394
343.792911	15613.596436	28.895412
344.242313	15644.062483	28.900429
344.809753	15660.591575	28.905447
345.018172	15686.231671	28.910464
345.402475	15714.049259	28.915482
345.787860	15730.964687	28.920500
345.822691	15763.923367	28.925517
346.376886	15777.678006	28.930535
346.465348	15801.022089	28.935552
346.671474	15827.671150	28.940570
347.534579	15853.904562	28.945588
347.844319	15887.239141	28.950605
348.056104	15909.023521	28.955623
348.091791	15939.450582	28.960640
348.061313	15969.451671	28.965658
348.549172	15997.261336	28.970676
349.016084	16035.811490	28.975693
349.188040	16062.356371	28.980711
349.944403	16097.787572	28.985728
350.149691	16128.187187	28.990746
350.566393	16166.849599	28.995764
350.870985	16196.878235	29.000781
351.798682	16212.995416	29.005799
351.965526	16240.498830	29.010816
352.781057	16267.219235	29.015834
353.170563	16288.424683	29.020852
353.069598	16312.193400	29.025869
353.607335	16330.548498	29.030887
354.023822	16361.524717	29.035904
354.357122	16374.628523	29.040922
354.665554	16395.764170	29.045940
354.858722	16423.537123	29.050957
355.397044	16439.164068	29.055975
355.650034	16473.275250	29.060992
355.861943	16497.361691	29.066010
356.704371	16513.632732	29.071028
357.007075	16536.044220	29.076045
357.146429	16563.207527	29.081063
357.399613	16584.058156	29.086080
357.928818	16604.866399	29.091098
358.152421	16630.389701	29.096116
358.225100	16662.837984	29.101133
358.787728	16685.514159	29.106151
358.741965	16723.231624	29.111168
359.157983	16745.062386	29.116186
359.956728	16757.752591	29.121204
360.568865	16782.638656	29.126221
361.307841	16806.217189	29.131239
361.676444	16820.835382	29.136256
362.104806	16843.126507	29.141274
362.126541	16849.609707	29.146292
362.329973	16876.055498	29.151309
362.851740	16890.251328	29.156327
362.998561	16917.230606	29.161344
363.065317	16947.537964	29.166362
363.489464	16963.868267	29.171380
363.794790	16999.626165	29.176397
364.010526	17024.730906	29.181415
364.527369	17050.721938	29.186432
364.911008	17082.105025	29.191450
365.125839	17106.113208	29.196468
365.239344	17134.158393	29.201485
365.958997	17156.787008	29.206503
366.349473	17188.320400	29.211520
366.361504	17211.360284	29.216538
366.839679	17225.531481	29.221556
367.233044	17263.193662	29.226573
367.682151	17283.731334	29.231591
368.017617	17310.285169	29.236608
368.292839	17350.901821	29.241626
369.090635	17366.350562	29.246644
369.255595	17397.362440	29.251661
369.743864	17427.143716	29.256679
370.169601	17441.097088	29.261696
370.262333	17467.883577	29.266714
370.536037	17492.895190	29.271732
370.844104	17531.939741	29.276749
371.073825	17563.671561	29.281767
371.594561	17593.073960	29.286784
371.787644	17613.603261	29.291802
372.799458	17637.165568	29.296820
373.233296	17664.805930	29.301837
373.567529	17691.396441	29.306855
373.648830	17715.121719	29.311872
374.180759	17744.876567	29.316890
374.928369	17760.433310	29.321908
375.393933	17780.169782	29.326925
375.794659	17806.719185	29.331943
375.965987	17818.212573	29.336960
375.913619	17848.635160	29.341978
376.636284	17869.261515	29.346996
377.132729	17900.287715	29.352013
377.142947	17930.402839	29.357031
377.717397	17953.825476	29.362048
377.921032	17987.417511	29.367066
378.479559	17996.049996	29.372084
378.647512	18025.018071	29.377101
378.955886	18050.655399	29.382119
379.459426	18083.920704	29.387136
380.155887	18091.149305	29.392154
380.926818	18113.432550	29.397172
381.576614	18134.539399	29.402189
382.035904	18138.489503	29.407207
382.457138	18147.587676	29.412224
382.424752	18164.414065	29.417242
383.329320	18167.723897	29.422260
383.818078	18188.813567	29.427277
384.197307	18195.459270	29.432295
384.629519	18195.966266	29.437312
384.827589	18203.410963	29.442330
385.090990	18218.748856	29.447348
385.140989	18236.782345	29.452365
385.194971	18247.544706	29.457383
385.577760	18274.750562	29.462400
385.746264	18311.547122	29.467418
385.837216	18313.866096	29.472436
386.277362	18339.430537	29.477453
386.793941	18367.190863	29.482471
387.202257	18390.943410	29.487488
386.895660	18417.950294	29.492506
387.245578	18441.836249	29.497524
387.762600	18484.377310	29.502541
387.781718	18522.016736	29.507559
388.468159	18546.964273	29.512576
388.400727	18592.175342	29.517594
389.043221	18621.314989	29.522612
389.441635	18662.552097	29.527629
390.024646	18692.855786	29.532647
390.258673	18731.093020	29.537664
390.719243	18772.072459	29.542682
391.366367	18792.978248	29.547700
391.543939	18836.437433	29.552717
392.164455	18861.830274	29.557735
392.661326	18890.449087	29.562752
392.777078	18934.900779	29.567770
393.248210	18968.542073	29.572788
393.596154	19000.387519	29.577805
393.614335	19041.303497	29.582823
394.573826	19065.930766	29.587840
394.938215	19113.027107	29.592858
395.286078	19136.354939	29.597876
395.341427	19176.563297	29.602893
396.128068	19215.959081	29.607911
396.812815	19254.044265	29.612928
396.760459	19281.352320	29.617946
397.213589	19318.811100	29.622964
398.122165	19340.300058	29.627981
399.040533	19369.823577	29.632999
399.839548	19383.089211	29.638016
399.808975	19407.049478	29.643034
400.684192	19412.378711	29.648052
401.181601	19422.932227	29.653069
401.663341	19451.049686	29.658087
402.065295	19448.675727	29.663104
402.347536	19463.945298	29.668122
402.496605	19479.560165	29.673140
403.414485	19478.973541	29.678157
403.464905	19500.088764	29.683175
403.738292	19512.713361	29.688192
404.040858	19528.705843	29.693210
404.486378	19535.099794	29.698228
404.508799	19569.595882	29.703245
404.735796	19591.957685	29.708263
405.284352	19613.399256	29.713280
405.171842	19653.371766	29.718298
405.532008	19674.782801	29.723316
406.117166	19704.416358	29.728333
406.493186	19734.558959	29.733351
406.857346	19765.372117	29.738368
407.738153	19786.399116	29.743386
408.612290	19793.441525	29.748404
408.755166	19806.710089	29.753421
408.899666	19821.225850	29.758439
409.551252	19838.595941	29.763456
409.577245	19863.359045	29.768474
409.558158	19885.980200	29.773492
410.265391	19911.113648	29.778509
410.365134	19937.214159	29.783527
410.663891	19970.124316	29.788544
411.073012	20006.366351	29.793562
411.355415	20033.161662	29.798580
411.784668	20070.418135	29.803597
412.076349	20094.280849	29.808615
412.748427	20128.209208	29.813632
413.014574	20153.687394	29.818650
413.624615	20179.039158	29.823668
414.521939	20199.827032	29.828685
415.087993	20236.221790	29.833703
415.619523	20245.213052	29.838720
415.588760	20282.435433	29.843738
416.405538	20306.017125	29.848756
416.521728	20328.216496	29.853773
416.848295	20357.944472	29.858791
417.509056	20381.866160	29.863808
417.828929	20408.145805	29.868826
418.128393	20435.068243	29.873844
418.547228	20454.774201	29.878861
418.528244	20488.980417	29.883879
418.989734	20529.341345	29.888896
419.033204	20570.884963	29.893914
419.593932	20611.053086	29.898932
420.339970	20642.979806	29.903949
420.505047	20678.247886	29.908967
421.314813	20705.084750	29.913984
421.789806	20742.922270	29.919002
422.176236	20775.286168	29.924020
422.482434	20802.526341	29.929037
422.859667	20842.647898	29.934055
423.309337	20874.984598	29.939072
423.527150	20911.312755	29.944090
424.025345	20940.582890	29.949108
424.587892	20974.938500	29.954125
424.982126	21019.591926	29.959143
425.634768	21039.192844	29.964160
425.743873	21083.264961	29.969178
426.075584	21116.359711	29.974196
426.428026	21150.798799	29.979213
426.926509	21199.425287	29.984231
427.234302	21232.301988	29.989248
427.338777	21272.886313	29.994266
427.816082	21319.615279	29.999284
428.417438	21357.616076	30.004301
428.594353	21410.808998	30.009319
428.976605	21447.680052	30.014336
429.430791	21500.402213	30.019354
429.470479	21543.358812	30.024372
430.393421	21582.973927	30.029389
430.690299	21616.950315	30.034407
431.269277	21651.177185	30.039424
431.508224	21689.498802	30.044442
432.095656	21738.115924	30.049460
432.456764	21772.430542	30.054477
432.413214	21825.316578	30.059495
433.358827	21863.370070	30.064512
433.735165	21908.606190	30.069530
434.422046	21952.417752	30.074548
434.802470	21990.231583	30.079565
435.231291	22028.266209	30.084583
435.968336	22060.977784	30.089600
436.256906	22092.729862	30.094618
436.725458	22137.940130	30.099636
437.811875	22161.098852	30.104653
438.206714	22197.482884	30.109671
438.356497	22225.678279	30.114688
438.745932	22263.455095	30.119706
439.185786	22294.063435	30.124724
439.953607	22325.916055	30.129741
440.064455	22359.336087	30.134759
440.758239	22391.502307	30.139776
441.263250	22419.819459	30.144794
442.175952	22442.319437	30.149812
442.879524	22458.436499	30.154829
443.400691	22482.682933	30.159847
443.795930	22496.856380	30.164864
444.254828	22520.269208	30.169882
444.521957	22540.034239	30.174900
444.907361	22569.113482	30.179917
445.243540	22596.751315	30.184935
445.661635	22623.276563	30.189952
445.954049	22648.002365	30.194970
446.101609	22677.108673	30.199988
446.661157	22709.975112	30.205005
446.625051	22737.366101	30.210023
447.034100	22775.749884	30.215040
447.361937	22809.237901	30.220058
447.669303	22853.964690	30.225076
448.084270	22895.749015	30.230093
448.444244	22945.449758	30.235111
449.072791	22985.048340	30.240128
449.304919	23028.192543	30.245146
449.819407	23073.723473	30.250164
450.540012	23112.309703	30.255181
451.014798	23154.956365	30.260199
451.577769	23191.942892	30.265216
452.040022	23235.658306	30.270234
452.395497	23279.830388	30.275252
453.288181	23317.327881	30.280269
453.486863	23355.527599	30.285287
453.874028	23390.633206	30.290304
454.258992	23428.458404	30.295322
454.549468	23464.805251	30.300340
455.467509	23488.011657	30.305357
455.266528	23519.191570	30.310375
455.930324	23564.158169	30.315392
456.365597	23598.089178	30.320410
456.843545	23643.395182	30.325428
457.013248	23670.498187	30.330445
457.613681	23715.669088	30.335463
458.312482	23751.505683	30.340480
459.081684	23795.039028	30.345498
458.971011	23832.173754	30.350516
460.161491	23864.227591	30.355533
461.051444	23884.307046	30.360551
462.596471	23877.443428	30.365568
463.134019	23887.500046	30.370586
463.289879	23896.025478	30.375604
464.024327	23902.623324	30.380621
463.896060	23913.866801	30.385639
464.212909	23925.743603	30.390656
465.306207	23949.948392	30.395674
465.206036	23955.710320	30.400692
465.445760	23978.737993	30.405709
466.225223	23988.241744	30.410727
467.221993	24003.559812	30.415744
467.831547	24002.836697	30.420762
468.181206	24016.325560	30.425780
468.289624	24024.411974	30.430797
468.066851	24055.201748	30.435815
468.559375	24071.689659	30.440832
468.941138	24102.068115	30.445850
468.800445	24130.276924	30.450868
469.070971	24164.137707	30.455885
469.227732	24200.364165	30.460903
469.771280	24247.735570	30.465920
470.026906	24291.811353	30.470938
470.375854	24345.333286	30.475956
471.154390	24381.632825	30.480973
471.462772	24433.565528	30.485991
471.810795	24479.221525	30.491008
472.345465	24517.807701	30.496026
472.685809	24570.774812	30.501044
473.024243	24615.511042	30.506061
473.316195	24676.889306	30.511079
473.994737	24732.421613	30.516096
474.713555	24783.195058	30.521114
474.992152	24832.666492	30.526132
475.661369	24878.229915	30.531149
476.078849	24933.041939	30.536167
476.362357	24982.496509	30.541184
477.469388	25029.325904	30.546202
477.421167	25078.774536	30.551220
478.180809	25126.456012	30.556237
478.477956	25171.328780	30.561255
479.093270	25221.310252	30.566272
479.795651	25257.463201	30.571290
480.131759	25298.334413	30.576308
481.142367	25337.362747	30.581325
481.755226	25379.337901	30.586343
482.097613	25407.610644	30.591360
482.569439	25445.031297	30.596378
482.873097	25483.764531	30.601396
483.352155	25510.848940	30.606413
483.582349	25555.169374	30.611431
483.969438	25588.058978	30.616448
484.554813	25633.363744	30.621466
484.889816	25677.165979	30.626484
485.565253	25712.766473	30.631501
485.567917	25759.309127	30.636519
486.228011	25806.415254	30.641536
487.178388	25842.177069	30.646554
487.098594	25889.380039	30.651572
487.679068	25929.147993	30.656589
488.168257	25972.444316	30.661607
488.539626	26022.991053	30.666624
489.044411	26066.775178	30.671642
489.275698	26126.150201	30.676660
490.249405	26165.550412	30.681677
490.444123	26220.362918	30.686695
491.166552	26271.371332	30.691712
491.976977	26304.683424	30.696730
492.612576	26354.328775	30.701748
493.254782	26397.678286	30.706765
493.671003	26445.214332	30.711783
493.833905	26485.789978	30.716800
494.548274	26521.834353	30.721818
495.161634	26569.950739	30.726836
495.565761	26609.232416	30.731853
495.723414	26654.055901	30.736871
496.372441	26700.698415	30.741888
497.144375	26737.966326	30.746906
497.291683	26788.573214	30.751924
497.872519	26832.811360	30.756941
498.424761	26877.712846	30.761959
499.115757	26925.094653	30.766976
499.818391	26962.268547	30.771994
500.061904	27017.375376	30.777012
500.657810	27047.456619	30.782029
501.072816	27093.779849	30.787047
501.818416	27125.231949	30.792064
502.529966	27154.485021	30.797082
503.171808	27200.317021	30.802100
503.613600	27228.328937	30.807117
504.675458	27264.808111	30.812135
504.809279	27299.381948	30.817152
505.179478	27330.134718	30.822170
505.692499	27378.857269	30.827188
506.583524	27389.126889	30.832205
507.675508	27414.006862	30.837223
507.585749	27442.904335	30.842240
508.653370	27455.240113	30.847258
508.865825	27488.791735	30.852276
509.434270	27501.175552	30.857293
509.844599	27524.946182	30.862311
509.783888	27546.314701	30.867328
510.332508	27567.099254	30.872346
510.531299	27592.293553	30.877364
510.838534	27622.618831	30.882381
511.479448	27661.263381	30.887399
511.697598	27697.324821	30.892416
512.373655	27726.015709	30.897434
512.479102	27768.345017	30.902452
512.815623	27812.437238	30.907469
513.350394	27859.170633	30.912487
513.624945	27908.726992	30.917504
514.364986	27956.751685	30.922522
514.305155	28007.086504	30.927540
514.838586	28062.045116	30.932557
515.551016	28114.192411	30.937575
515.754911	28165.678644	30.942592
516.191912	28214.620680	30.947610
516.536667	28282.738763	30.952628
517.881656	28336.899274	30.957645
518.594931	28382.844584	30.962663
518.795451	28425.847548	30.967680
519.529807	28481.913374	30.972698
520.093917	28539.899183	30.977716
520.619967	28577.629696	30.982733
521.445766	28638.642480	30.987751
521.594320	28692.359667	30.992768
522.484269	28729.161077	30.997786
522.939949	28778.287792	31.002804
523.305497	28835.959579	31.007821
523.573486	28883.742289	31.012839
524.191208	28936.595995	31.017856
524.884357	28979.692150	31.022874
525.536581	29040.890110	31.027892
525.860077	29086.217104	31.032909
526.196198	29140.865651	31.037927
526.756139	29186.661146	31.042944
528.087558	29222.580146	31.047962
528.820360	29263.147594	31.052980
529.899416	29308.517178	31.057997
530.654540	29335.070735	31.063015
531.091020	29359.523864	31.068032
532.319780	29369.214579	31.073050
532.114043	29401.254460	31.078068
532.623805	29428.485532	31.083085
533.404774	29449.301679	31.088103
533.545908	29483.362060	31.093120
534.254437	29512.507976	31.098138
535.000997	29542.796796	31.103156
535.236924	29569.925155	31.108173
535.696199	29600.067571	31.113191
535.963810	29636.093901	31.118208
536.404818	29664.228346	31.123226
536.577372	29706.972792	31.128244
537.009379	29731.430344	31.133261
537.603892	29762.645280	31.138279
538.003071	29800.972510	31.143296
538.503750	29843.237940	31.148314
539.034808	29883.394625	31.153332
539.367628	29924.544373	31.158349
540.088620	29965.783694	31.163367
540.214946	30009.920066	31.168384
540.827673	30052.529106	31.173402
541.131479	30112.905564	31.178420
541.718630	30155.922419	31.183437
542.306786	30205.461014	31.188455
542.661234	30273.853787	31.193472
542.965329	30325.140156	31.198490
543.343319	30374.567739	31.203508
544.158555	30438.819916	31.208525
544.549681	30497.423381	31.213543
545.294932	30555.146345	31.218560
546.008151	30610.069134	31.223578
546.085958	30665.875073	31.228596
546.976362	30719.564277	31.233613
547.560085	30777.094669	31.238631
547.800828	30845.211617	31.243648
548.241549	30895.494496	31.248666
548.927594	30962.543305	31.253684
549.181833	31036.813744	31.258701
549.947367	31088.591680	31.263719
550.412569	31156.229686	31.268736
551.643175	31202.987904	31.273754
553.676491	31220.626304	31.278772
554.532288	31264.969815	31.283789
555.249348	31291.264668	31.288807
555.708169	31332.720990	31.293824
555.955312	31358.999382	31.298842
556.280443	31383.413375	31.303860
557.060275	31417.301953	31.308877
557.526949	31456.150319	31.313895
557.933519	31500.696843	31.318912
558.647814	31525.641712	31.323930
558.872967	31563.594115	31.328948
559.190023	31600.873112	31.333965
559.605353	31640.816098	31.338983
560.275971	31679.987155	31.344000
560.560222	31718.103884	31.349018
561.108132	31776.790961	31.354036
561.484206	31824.257652	31.359053
562.078449	31867.807471	31.364071
562.503153	31926.350776	31.369088
563.089615	31965.613151	31.374106
563.294977	32026.141555	31.379124
563.557504	32084.812131	31.384141
564.521267	32148.791976	31.389159
564.947433	32205.751896	31.394176
565.128641	32263.288537	31.399194
565.802531	32316.106352	31.404212
566.710792	32363.983202	31.409229
567.288785	32421.676297	31.414247
567.300431	32474.436163	31.419264
568.596000	32510.242004	31.424282
569.242185	32566.707846	31.429300
569.633522	32617.070041	31.434317
570.640815	32654.143745	31.439335
571.185242	32704.563791	31.444352
572.178274	32747.795474	31.449370
572.341095	32789.901599	31.454388
572.926933	32830.797620	31.459405
573.846129	32866.512856	31.464423
574.532552	32907.835995	31.469440
575.118055	32934.405064	31.474458
575.707547	32972.876455	31.479476
575.819591	33024.487117	31.484493
576.977026	33060.590440	31.489511
576.970101	33109.321416	31.494528
577.809840	33149.771087	31.499546
578.585788	33192.836737	31.504564
578.830209	33231.969010	31.509581
579.607393	33273.790925	31.514599
579.921148	33317.389234	31.519616
580.593296	33364.304016	31.524634
580.786054	33417.372222	31.529652
581.328643	33470.644983	31.534669
582.204491	33512.732382	31.539687
582.524428	33569.866817	31.544704
583.162033	33617.785673	31.549722
583.829748	33675.155136	31.554740
584.329216	33722.626527	31.559757
585.307908	33766.700229	31.564775
585.465502	33816.754903	31.569792
586.456053	33871.954924	31.574810
587.025232	33911.584090	31.579828
587.023657	33978.817696	31.584845
587.372983	34026.094741	31.589863
588.159889	34089.771313	31.594880
588.511552	34152.694542	31.599898
589.115794	34220.269309	31.604916
589.605709	34282.866754	31.609933
590.445313	34327.359786	31.614951
590.830637	34397.456222	31.619968
591.884498	34452.707990	31.624986
592.128420	34506.870318	31.630004
592.972448	34570.055646	31.635021
593.580727	34621.027833	31.640039
594.348030	34680.432758	31.645056
595.124262	34727.552362	31.650074
595.955226	34782.096613	31.655092
597.013945	34823.243830	31.660109
598.060609	34851.110933	31.665127
598.176199	34896.146451	31.670144
598.741428	34937.508125	31.675162
599.318441	34968.445615	31.680180
599.706833	35002.377075	31.685197
600.539147	35036.356144	31.690215
600.822656	35085.022980	31.695232
601.424116	35116.680481	31.700250
602.456300	35143.024290	31.705268
602.852101	35186.784684	31.710285
603.562519	35219.216453	31.715303
603.799470	35261.080527	31.720320
604.274524	35308.535092	31.725338
604.987441	35343.380413	31.730356
605.151263	35397.036536	31.735373
606.175794	35438.733056	31.740391
606.318309	35498.065393	31.745408
606.708865	35549.790851	31.750426
607.583737	35597.950355	31.755444
607.967145	35656.800291	31.760461
608.553091	35705.207921	31.765479
608.626341	35769.855911	31.770496
608.886716	35833.179954	31.775514
609.786451	35906.197907	31.780532
609.769206	35976.760790	31.785549
610.553573	36043.261047	31.790567
611.134302	36120.633347	31.795584
611.844637	36199.677097	31.800602
612.436186	36274.899422	31.805620
612.600879	36356.340593	31.810637
613.777678	36416.209906	31.815655
614.110409	36506.075942	31.820672
614.604064	36587.915193	31.825690
615.815114	36659.045275	31.830708
616.277065	36743.752010	31.835725
617.024574	36808.602480	31.840743
617.597735	36873.971320	31.845760
618.411989	36950.345295	31.850778
619.250921	37022.756548	31.855796
619.232825	37100.184558	31.860813
620.464226	37165.303063	31.865831
621.238655	37233.346912	31.870848
622.020331	37290.417327	31.875866
623.172575	37341.823585	31.880884
623.952419	37411.590673	31.885901
624.785193	37458.109771	31.890919
625.569984	37510.494311	31.895936
625.900480	37559.236496	31.900954
626.610343	37611.272201	31.905972
627.094166	37667.237126	31.910989
627.766890	37704.995014	31.916007
628.281315	37770.304142	31.921024
628.624168	37831.282589	31.926042
629.105649	37883.380729	31.931060
629.686067	37958.265425	31.936077
630.157524	38013.796689	31.941095
630.947979	38070.647586	31.946112
632.061245	38128.000730	31.951130
632.817207	38178.949140	31.956148
633.252835	38228.744018	31.961165
634.158305	38264.247491	31.966183
635.163612	38292.713491	31.971200
635.678272	38333.574360	31.976218
636.286984	38366.873581	31.981236
636.441215	38419.039671	31.986253
636.987393	38467.243951	31.991271
637.679080	38521.533938	31.996288
638.106479	38572.682501	32.001306
638.685805	38628.859304	32.006324
639.039395	38689.090110	32.011341
640.066635	38737.615922	32.016359
640.249321	38798.672230	32.021376
640.499433	38869.609840	32.026394
641.456074	38919.889877	32.031412
641.930231	38976.969214	32.036429
642.388275	39046.704390	32.041447
643.141085	39115.520880	32.046464
643.782519	39193.387970	32.051482
644.241053	39263.630146	32.056500
644.803545	39338.547428	32.061517
646.047056	39392.500009	32.066535
647.201288	39461.030045	32.071552
647.900370	39519.679133	32.076570
648.329987	39571.234039	32.081588
648.720522	39641.769297	32.086605
649.378982	39701.311728	32.091623
649.868990	39776.518443	32.096640
650.535494	39839.359102	32.101658
651.206711	39913.635532	32.106676
652.123685	39972.137933	32.111693
652.822272	40026.007404	32.116711
653.614397	40094.162394	32.121728
654.335081	40161.613071	32.126746
655.852834	40191.445199	32.131764
656.826580	40241.366856	32.136781
657.267618	40281.236406	32.141799
658.242285	40329.776706	32.146816
658.781786	40367.192700	32.151834
659.626729	40412.953095	32.156852
659.854251	40467.416234	32.161869
660.598819	40504.304684	32.166887
660.949375	40553.134245	32.171904
661.323013	40611.567650	32.176922
661.710343	40655.449175	32.181940
662.418619	40721.957803	32.186957
663.032918	40779.180125	32.191975
663.478128	40834.429838	32.196992
664.168756	40898.595282	32.202010
664.869552	40954.170563	32.207028
665.167240	41029.258845	32.212045
665.834197	41093.394089	32.217063
666.590383	41151.118652	32.222080
667.265344	41230.998895	32.227098
668.236054	41271.410939	32.232116
668.754836	41335.330960	32.237133
669.033230	41386.420190	32.242151
669.652289	41454.434661	32.247168
670.210311	41505.965476	32.252186
671.017321	41574.023039	32.257204
671.437840	41648.154486	32.262221
672.038839	41711.974492	32.267239
672.785415	41776.266781	32.272256
673.511325	41852.684669	32.277274
674.118080	41918.324569	32.282292
675.044808	41988.922876	32.287309
675.807549	42039.895913	32.292327
676.683662	42099.279524	32.297344
677.272211	42162.188411	32.302362
678.249964	42218.048575	32.307380
678.476232	42285.614702	32.312397
679.433119	42352.670454	32.317415
680.083306	42410.753639	32.322432
680.508420	42492.830827	32.327450
681.131020	42551.234320	32.332468
681.565195	42629.496980	32.337485
682.250478	42697.578357	32.342503
682.822291	42773.501209	32.347520
683.490619	42854.897869	32.352538
684.325084	42920.499007	32.357556
685.009681	43000.171391	32.362573
685.671498	43077.210566	32.367591
686.512305	43151.180585	32.372608
687.202306	43228.875249	32.377626
688.094940	43288.736655	32.382644
689.055156	43367.581349	32.387661
689.760353	43432.179760	32.392679
690.356129	43499.095556	32.397696
690.788431	43577.151426	32.402714
691.730836	43630.996503	32.407732
692.521339	43712.510226	32.412749
693.190618	43778.304951	32.417767
694.135324	43849.125654	32.422784
694.412951	43923.762788	32.427802
695.138481	43989.801732	32.432820
696.369329	44057.489259	32.437837
697.014140	44123.850727	32.442855
697.328544	44186.744356	32.447872
697.904677	44255.609513	32.452890
698.655209	44324.671162	32.457908
699.177773	44411.543458	32.462925
699.491748	44483.766940	32.467943
700.835799	44552.160816	32.472960
701.070972	44632.934393	32.477978
702.021073	44708.676111	32.482996
702.784327	44777.078162	32.488013
703.450630	44841.893060	32.493031
704.432248	44923.170638	32.498048
705.020706	44994.469159	32.503066
705.957559	45051.931870	32.508084
706.805408	45124.110852	32.513101
707.097791	45178.916038	32.518119
708.157430	45228.728012	32.523136
709.219456	45281.748328	32.528154
710.461641	45318.839151	32.533172
710.756274	45367.770048	32.538189
711.756242	45417.614148	32.543207
712.452251	45469.077964	32.548224
713.034522	45522.557149	32.553242
714.138169	45559.026923	32.558260
714.510702	45611.334564	32.563277
714.965330	45662.509260	32.568295
715.951001	45710.529717	32.573312
716.311409	45773.784552	32.578330
717.060118	45831.529029	32.583348
717.834836	45885.795838	32.588365
718.591519	45946.337957	32.593383
719.320709	46003.947286	32.598400
719.654698	46060.174695	32.603418
720.434763	46114.416120	32.608436
721.062360	46171.124039	32.613453
721.464151	46242.930622	32.618471
722.194680	46308.447466	32.623488
722.748536	46381.511387	32.628506
723.502549	46451.098314	32.633524
724.166683	46526.798767	32.638541
725.144148	46597.268850	32.643559
725.808541	46667.634455	32.648576
726.173644	46747.359009	32.653594
727.230135	46814.567515	32.658612
727.958919	46882.778177	32.663629
728.398750	46964.501698	32.668647
729.215062	47040.094935	32.673664
729.643789	47120.685052	32.678682
730.951231	47185.561135	32.683700
731.866012	47255.075155	32.688717
732.704867	47326.898603	32.693735
733.540603	47391.068024	32.698752
734.199258	47466.479934	32.703770
735.142540	47520.721792	32.708788
735.970483	47592.387135	32.713805
736.629705	47656.427853	32.718823
737.254613	47722.910221	32.723840
737.883229	47796.166881	32.728858
738.323201	47861.625310	32.733876
739.183710	47940.351835	32.738893
739.732566	48014.294199	32.743911
740.725888	48083.843149	32.748928
740.954918	48167.240302	32.753946
741.704811	48233.944502	32.758964
742.402423	48317.302470	32.763981
742.889025	48401.959779	32.768999
743.919821	48482.292994	32.774016
744.591839	48557.985104	32.779034
745.597961	48623.065898	32.784052
746.612757	48687.407150	32.789069
747.202596	48747.625699	32.794087
748.431431	48807.973080	32.799104
749.031335	48856.672550	32.804122
749.967142	48911.254349	32.809140
750.919332	48981.911512	32.814157
751.407741	49034.147719	32.819175
752.224871	49094.479572	32.824192
752.727270	49158.361335	32.829210
753.479685	49223.210176	32.834228
754.325210	49272.136756	32.839245
755.064769	49338.512246	32.844263
756.147949	49400.339592	32.849280
756.325271	49469.818752	32.854298
756.970736	49540.618477	32.859316
757.901190	49605.257334	32.864333
758.661184	49685.310896	32.869351
759.635212	49748.381249	32.874368
759.950454	49823.889385	32.879386
760.560585	49889.394449	32.884404
761.569370	49966.739887	32.889421
762.249785	50031.095045	32.894439
763.522133	50105.656745	32.899456
763.811941	50181.302980	32.904474
764.625257	50259.308809	32.909492
765.603583	50321.512647	32.914509
765.696291	50410.789755	32.919527
766.508448	50488.711558	32.924544
767.182285	50573.608135	32.929562
767.851480	50659.345322	32.934580
768.571640	50745.320967	32.939597
769.016284	50837.330842	32.944615
770.134646	50919.147528	32.949632
770.226796	51019.192682	32.954650
770.916922	51106.083750	32.959668
772.506080	51206.377657	32.964685
772.714601	51298.026662	32.969703
773.562375	51387.734406	32.974720
774.870067	51490.091403	32.979738
776.069873	51568.180255	32.984756
776.857326	51640.259646	32.989773
777.801229	51726.261168	32.994791
779.078413	51789.394591	32.999808
780.062415	51867.336041	33.004826
780.956305	51929.385302	33.009844
782.177420	51992.004446	33.014861
782.726712	52058.764307	33.019879
783.525427	52116.940992	33.024896
783.921043	52186.651545	33.029914
784.923677	52253.150589	33.034932
785.850963	52314.845524	33.039949
786.226071	52384.654790	33.044967
786.708354	52442.665117	33.049984
787.213841	52521.913330	33.055002
787.823566	52596.294156	33.060020
788.956896	52663.121090	33.065037
789.329687	52725.922006	33.070055
790.255507	52803.520098	33.075072
791.150275	52879.220223	33.080090
791.423705	52951.282508	33.085108
792.377993	53021.715355	33.090125
792.634479	53108.918649	33.095143
793.763372	53182.534314	33.100160
794.871281	53260.070654	33.105178
795.282454	53339.731996	33.110196
796.018285	53423.899824	33.115213
796.734166	53506.073217	33.120231
797.800462	53585.344120	33.125248
798.595913	53660.387839	33.130266
799.409847	53750.197901	33.135284
800.016714	53839.536334	33.140301
800.633121	53929.299809	33.145319
801.482507	54010.036970	33.150336
801.948420	54111.535858	33.155354
802.464699	54204.899257	33.160372
803.341453	54302.448136	33.165389
803.912378	54414.667372	33.170407
804.944602	54516.526597	33.175424
805.703930	54616.002410	33.180442
806.683648	54715.008072	33.185460
807.774659	54815.221325	33.190477
808.355514	54932.881020	33.195495
809.268980	55020.736992	33.200512
809.912612	55123.245429	33.205530
810.710053	55222.664807	33.210548
811.930119	55324.495471	33.215565
812.856672	55408.676809	33.220583
814.095927	55492.622512	33.225600
815.303269	55583.411210	33.230618
816.262741	55660.520490	33.235636
817.516772	55734.524288	33.240653
818.331744	55810.555481	33.245671
819.525771	55885.626966	33.250688
820.174645	55957.341438	33.255706
820.722503	56030.871663	33.260724
821.499395	56097.067103	33.265741
822.563926	56178.710848	33.270759
823.243888	56253.556286	33.275776
823.940113	56335.379309	33.280794
824.769845	56399.648041	33.285812
825.829939	56466.980414	33.290829
826.350019	56554.123421	33.295847
827.262330	56632.769077	33.300864
828.349362	56728.125406	33.305882
828.396431	56797.397588	33.310900
829.447248	56878.213177	33.315917
830.266720	56973.578633	33.320935
830.904119	57049.747383	33.325952
831.444604	57134.522123	33.330970
832.328089	57215.987755	33.335988
832.924684	57287.046424	33.341005
833.611000	57371.568574	33.346023
834.656149	57451.740374	33.351040
835.487613	57527.128816	33.356058
836.020273	57612.633118	33.361076
837.156418	57704.365468	33.366093
837.589405	57788.396285	33.371111
838.717828	57883.789867	33.376128
839.123468	57974.547447	33.381146
839.960142	58064.406527	33.386164
840.892868	58153.189938	33.391181
841.735723	58244.861137	33.396199
842.655296	58332.514059	33.401216
844.143148	58410.355812	33.406234
845.142725	58491.511787	33.411252
846.469652	58554.073410	33.416269
847.669053	58630.702250	33.421287
848.389820	58702.210690	33.426304
849.169725	58775.879056	33.431322
850.157527	58866.254698	33.436340
851.126294	58922.863041	33.441357
851.814729	59011.768362	33.446375
852.445194	59067.613237	33.451392
853.527634	59144.218603	33.456410
853.878079	59228.161700	33.461428
854.837174	59305.668266	33.466445
855.380159	59404.178121	33.471463
856.589157	59480.654216	33.476480
857.033047	59561.293905	33.481498
857.545911	59657.094493	33.486516
858.823983	59739.310365	33.491533
859.380035	59840.371663	33.496551
860.397976	59923.027585	33.501568
861.546228	59997.368365	33.506586
861.934295	60090.690286	33.511604
863.126491	60176.597100	33.516621
864.183522	60268.278875	33.521639
864.850079	60363.780745	33.526656
865.444922	60439.594369	33.531674
866.102912	60541.887303	33.536692
867.190760	60632.798656	33.541709
868.056539	60727.212866	33.546727
868.781565	60834.612078	33.551744
869.843230	60935.466172	33.556762
870.413836	61029.436277	33.561780
871.510307	61124.703072	33.566797
871.899381	61228.952936	33.571815
872.847448	61323.379139	33.576832
873.927483	61416.916433	33.581850
874.592195	61527.698499	33.586868
875.441514	61624.807075	33.591885
876.244969	61731.264203	33.596903
877.051376	61839.458257	33.601920
878.765918	61917.366933	33.606938
880.132081	61989.843052	33.611956
881.064366	62058.043297	33.616973
881.811086	62135.172173	33.621991
882.789982	62207.186551	33.627008
883.631565	62291.914604	33.632026
884.422096	62377.724847	33.637044
885.710996	62427.200160	33.642061
886.487319	62508.510077	33.647079
886.916897	62580.616451	33.652096
888.127482	62654.522000	33.657114
888.845165	62739.739147	33.662132
889.367598	62813.189551	33.667149
890.318366	62902.482018	33.672167
891.099386	62991.602963	33.677184
891.927150	63077.508339	33.682202
892.649582	63164.867771	33.687220
894.345914	63239.670971	33.692237
895.048193	63337.118041	33.697255
896.136204	63415.757886	33.702272
897.031597	63484.834442	33.707290
897.735651	63581.477166	33.712308
898.486948	63662.366493	33.717325
899.220925	63758.338988	33.722343
900.059803	63850.436017	33.727360
900.888286	63938.442167	33.732378
901.309016	64045.121586	33.737396
902.138151	64138.355337	33.742413
903.133556	64245.137070	33.747431
903.329246	64354.146882	33.752448
904.400492	64454.575989	33.757466
905.026004	64574.149308	33.762484
906.153163	64687.263809	33.767501
907.460079	64792.887304	33.772519
908.674258	64897.619702	33.777536
909.738822	65010.723962	33.782554
910.667428	65102.196850	33.787572
911.399242	65205.902264	33.792589
912.552796	65315.709454	33.797607
913.378037	65410.617632	33.802624
914.420403	65516.476708	33.807642
915.144640	65624.253625	33.812660
916.428723	65717.470022	33.817677
916.968539	65828.653813	33.822695
917.924717	65934.882649	33.827712
918.964249	66038.271944	33.832730
919.664342	66147.312707	33.837748
920.468465	66252.578868	33.842765
921.631427	66352.602151	33.847783
922.361135	66472.625495	33.852800
923.752621	66575.677387	33.857818
924.258346	66677.152491	33.862836
925.557033	66784.983446	33.867853
926.185745	66889.333391	33.872871
927.199978	66988.353907	33.877888
928.465533	67091.220108	33.882906
928.942577	67190.895698	33.887924
930.004376	67285.500626	33.892941
931.108651	67374.697840	33.897959
932.494934	67451.657871	33.902976
933.765808	67535.377340	33.907994
934.206544	67629.299397	33.913012
935.225192	67714.285371	33.918029
935.615498	67796.528786	33.923047
936.679857	67889.203065	33.928064
937.917915	67985.482789	33.933082
938.395191	68088.587098	33.938100
938.978637	68182.211131	33.943117
940.136402	68278.580891	33.948135
941.100591	68384.111105	33.953152
942.164998	68479.883890	33.958170
942.892142	68582.887869	33.963188
943.642564	68695.921462	33.968205
944.444501	68804.739785	33.973223
945.193753	68918.318187	33.978240
946.347892	69023.992212	33.983258
947.103156	69140.268719	33.988276
948.299519	69251.484469	33.993293
949.535571	69364.627868	33.998311
950.297473	69477.702047	34.003328
951.692103	69587.005351	34.008346
952.677404	69702.256631	34.013364
953.463795	69798.111683	34.018381
954.260153	69904.934111	34.023399
955.214334	70017.108875	34.028416
956.350961	70124.636549	34.033434
957.104762	70249.430635	34.038452
958.092301	70354.531756	34.043469
959.019628	70465.866679	34.048487
960.011680	70580.907194	34.053504
961.319370	70690.552697	34.058522
961.952350	70817.265146	34.063540
962.729668	70923.856010	34.068557
963.835929	71042.748013	34.073575
964.952012	71166.630911	34.078592
966.124117	71271.423199	34.083610
966.727558	71391.427244	34.088628
968.088880	71494.383447	34.093645
969.502285	71599.120119	34.098663
970.426587	71712.686749	34.103680
971.206514	71810.441912	34.108698
972.077446	71925.458950	34.113716
973.213501	72029.123571	34.118733
974.145698	72132.631599	34.123751
974.967844	72245.888938	34.128768
975.796996	72359.088935	34.133786
976.959975	72476.002631	34.138804
977.816322	72592.081123	34.143821
978.943798	72706.960747	34.148839
979.556295	72821.411112	34.153856
980.801872	72921.214562	34.158874
981.641339	73027.535079	34.163892
982.704887	73123.273625	34.168909
983.792189	73217.789222	34.173927
984.404104	73332.539610	34.178944
985.668535	73418.743312	34.183962
986.663621	73518.962441	34.188980
987.884191	73631.936743	34.193997
989.122856	73724.958223	34.199015
989.947109	73830.211108	34.204032
990.779353	73924.606312	34.209050
991.679192	74034.518377	34.214068
992.252406	74138.454108	34.219085
993.337974	74245.032624	34.224103
994.005160	74367.351048	34.229120
995.225804	74466.666904	34.234138
996.155909	74583.528825	34.239156
996.938197	74697.817513	34.244173
998.303378	74811.559086	34.249191
999.478523	74922.771996	34.254208
1000.486380	75036.085054	34.259226
1001.327981	75159.859383	34.264244
1002.696606	75261.007344	34.269261
1003.933268	75374.665095	34.274279
1004.375326	75489.334704	34.279296
1005.536162	75604.933418	34.284314
1007.151050	75706.082346	34.289332
1008.238561	75815.500240	34.294349
1009.725286	75896.730529	34.299367
1010.824882	76001.527475	34.304384
1011.669356	76085.053798	34.309402
1012.737127	76193.402435	34.314420
1013.813040	76291.290301	34.319437
1015.057296	76385.536645	34.324455
1015.778623	76487.463656	34.329472
1017.384592	76571.281655	34.334490
1018.132283	76662.460741	34.339508
1018.909707	76765.088100	34.344525
1020.211555	76857.197486	34.349543
1020.751574	76959.490684	34.354560
1022.092204	77056.189789	34.359578
1022.732007	77162.506934	34.364596
1023.548127	77267.387095	34.369613
1024.714711	77373.305506	34.374631
1025.382487	77493.133381	34.379648
1025.994849	77595.114857	34.384666
1026.947896	77711.093578	34.389684
1027.477934	77837.247124	34.394701
1028.404415	77965.556974	34.399719
1029.030107	78093.928117	34.404736
1030.100304	78222.418975	34.409754
1031.074117	78362.859845	34.414772
1032.259152	78503.634688	34.419789
1033.694496	78632.095302	34.424807
1034.220418	78766.396639	34.429824
1035.427407	78898.788999	34.434842
1036.505430	79006.815877	34.439860
1037.483008	79141.629348	34.444877
1038.643093	79253.247517	34.449895
1040.199638	79365.820938	34.454912
1041.533725	79472.747556	34.459930
1042.829539	79576.216754	34.464948
1043.848737	79687.783827	34.469965
1045.347918	79785.538860	34.474983
1045.821837	79902.472154	34.480000
1047.068300	80006.893242	34.485018
1047.745651	80111.784673	34.490036
1048.666071	80220.329711	34.495053
1049.533423	80340.989454	34.500071
1050.277479	80466.537105	34.505088
1051.118252	80582.777393	34.510106
1052.215472	80715.944778	34.515124
1053.249802	80845.064509	34.520141
1054.700043	80969.327027	34.525159
1055.333780	81110.561297	34.530176
1056.422629	81227.284100	34.535194
1057.824956	81350.304797	34.540212
1058.039237	81493.094001	34.545229
1059.606180	81616.355598	34.550247
1060.939297	81746.179356	34.555264
1062.129121	81872.062834	34.560282
1063.507258	81997.676877	34.565300
1064.531528	82127.899841	34.570317
1066.047268	82253.101560	34.575335
1066.895380	82380.123521	34.580352
1068.236588	82492.836619	34.585370
1069.294638	82606.714391	34.590388
1070.561588	82725.162138	34.595405
1071.497607	82838.276618	34.600423
1072.786951	82958.226815	34.605440
1073.923702	83078.992259	34.610458
1075.031236	83197.461698	34.615476
1075.726670	83314.941509	34.620493
1077.219482	83418.569117	34.625511
1078.175316	83540.864400	34.630528
1079.276747	83665.533466	34.635546
1080.417818	83781.705775	34.640564
1081.390613	83900.700070	34.645581
1082.554502	84028.288695	34.650599
1082.944882	84144.708851	34.655616
1083.967448	84261.610779	34.660634
1085.036059	84401.925421	34.665652
1085.633477	84548.752523	34.670669
1086.866833	84674.253787	34.675687
1087.667891	84810.680892	34.680704
1088.640594	84948.535835	34.685722
1089.872476	85094.949642	34.690740
1090.764875	85242.082364	34.695757
1092.053856	85387.730341	34.700775
1093.043407	85526.199670	34.705792
1094.198846	85669.866399	34.710810
1095.199799	85798.541184	34.715828
1096.049215	85941.290967	34.720845
1097.702567	86062.927038	34.725863
1098.645865	86198.872462	34.730880
1099.999276	86310.383513	34.735898
1101.504907	86431.052413	34.740916
1102.575942	86557.368328	34.745933
1104.137165	86669.638617	34.750951
1104.888707	86794.299420	34.755968
1105.993842	86919.309409	34.760986
1106.767865	87039.743976	34.766004
1107.598656	87164.868582	34.771021
1109.208614	87291.602652	34.776039
1110.402195	87420.572695	34.781056
1111.603393	87531.184715	34.786074
1112.690001	87662.614149	34.791092
1113.796493	87790.645375	34.796109
1114.729343	87909.061230	34.801127
1116.151991	88041.419704	34.806144
1116.996812	88175.205219	34.811162
1118.257901	88297.675169	34.816180
1118.874905	88434.970329	34.821197
1120.198311	88570.528749	34.826215
1121.352800	88709.188344	34.831232
1122.588557	88842.150588	34.836250
1123.506180	88980.634568	34.841268
1124.654861	89114.472399	34.846285
1125.966312	89242.144411	34.851303
1127.047357	89389.028769	34.856320
1128.376686	89512.639388	34.861338
1129.984017	89636.921137	34.866356
1131.122718	89772.301388	34.871373
1132.393137	89893.279971	34.876391
1133.501175	90009.914905	34.881408
1134.310339	90147.582391	34.886426
1135.716408	90268.117738	34.891444
1136.673523	90405.320601	34.896461
1137.885855	90527.406062	34.901479
1139.157010	90664.769312	34.906496
1140.581620	90797.061985	34.911514
1141.903646	90893.428868	34.916532
1142.606412	91035.185575	34.921549
1144.152165	91149.271357	34.926567
1145.314518	91273.247345	34.931584
1146.186678	91408.793922	34.936602
1147.380619	91532.165488	34.941620
1148.373498	91665.651528	34.946637
1149.535293	91793.640484	34.951655
1150.436183	91925.472952	34.956672
1151.598303	92046.164355	34.961690
1152.651630	92186.297781	34.966708
1153.387353	92327.931035	34.971725
1154.526021	92472.391675	34.976743
1155.991521	92610.729162	34.981760
1156.888516	92736.728985	34.986778
1158.096182	92874.261546	34.991796
1158.864625	92997.443277	34.996813
1159.856435	93127.098865	35.001831
1160.779589	93263.224261	35.006848
1161.672515	93409.115302	35.011866
1163.151960	93535.153523	35.016884
1164.174061	93701.001493	35.021901
1165.343971	93826.242972	35.026919
1166.907221	93962.093723	35.031936
1167.669939	94112.058378	35.036954
1168.904880	94244.471351	35.041972
1170.237536	94385.466086	35.046989
1172.013838	94527.377961	35.052007
1173.139183	94672.398959	35.057024
1174.117402	94817.229212	35.062042
1175.574825	94950.129680	35.067060
1176.476446	95087.363940	35.072077
1177.657056	95228.267949	35.077095
1179.073357	95357.653859	35.082112
1180.100350	95505.106023	35.087130
1181.544330	95649.778998	35.092148
1182.541376	95784.832515	35.097165
1183.659755	95928.123042	35.102183
1184.904018	96074.000809	35.107200
1185.783004	96232.583548	35.112218
1187.113158	96373.293780	35.117236
1188.173195	96531.697990	35.122253
1189.138363	96682.191580	35.127271
1190.394175	96842.357155	35.132288
1191.408484	96996.742016	35.137306
1192.631413	97158.281534	35.142324
1193.573253	97326.769040	35.147341
1194.694901	97487.017416	35.152359
1195.715665	97657.165000	35.157376
1196.812364	97824.163791	35.162394
1198.174804	97991.975639	35.167412
1199.104230	98170.638221	35.172429
1200.525853	98332.116473	35.177447
1201.590058	98514.847363	35.182464
1202.742406	98690.859261	35.187482
1204.514490	98853.538161	35.192500
1205.539520	99026.675168	35.197517
1207.086583	99192.789797	35.202535
1208.624998	99362.709525	35.207552
1209.696758	99531.616452	35.212570
1211.492318	99676.904381	35.217588
1213.066146	99828.688479	35.222605
1214.556753	99974.792352	35.227623
1216.015274	100116.694656	35.232640
1217.397199	100250.954040	35.237658
1218.871875	100384.592036	35.242676
1220.350920	100525.936780	35.247693
1222.126252	100649.873011	35.252711
1223.287093	100769.788481	35.257728
1224.209362	100889.957633	35.262746
1225.492355	100996.428071	35.267764
1226.287103	101110.873317	35.272781
1226.926809	101236.404263	35.277799
1228.490719	101353.765611	35.282816
1229.457703	101479.612826	35.287834
1230.592893	101602.434686	35.292852
1231.191466	101734.985843	35.297869
1232.226574	101872.055912	35.302887
1233.493751	102013.183920	35.307904
1233.933799	102162.100877	35.312922
1235.657758	102298.874083	35.317940
1237.138077	102446.671949	35.322957
1238.435942	102594.854114	35.327975
1239.587860	102725.411862	35.332992
1240.716288	102879.760837	35.338010
1241.729096	103036.438923	35.343028
1242.872048	103196.172783	35.348045
1243.988556	103353.083275	35.353063
1245.636227	103504.290987	35.358080
1246.417927	103667.932967	35.363098
1247.719436	103820.071019	35.368116
1249.156261	103982.370683	35.373133
1250.332342	104143.630775	35.378151
1251.443293	104311.553397	35.383168
1252.570250	104484.467752	35.388186
1253.764396	104648.879932	35.393204
1254.938874	104829.427646	35.398221
1256.316239	104990.528574	35.403239
1256.898214	105170.818672	35.408256
1258.345597	105363.307007	35.413274
1259.695642	105532.276069	35.418292
1261.007382	105701.467590	35.423309
1261.927112	105891.841670	35.428327
1263.438304	106071.079465	35.433344
1264.912330	106267.475690	35.438362
1266.438208	106440.688839	35.443380
1267.500423	106626.704456	35.448397
1268.991315	106816.279870	35.453415
1270.292872	106984.260533	35.458432
1271.585397	107166.566521	35.463450
1272.936315	107347.497506	35.468468
1274.279685	107525.582911	35.473485
1275.455533	107704.360824	35.478503
1277.035745	107881.284584	35.483520
1277.927094	108056.382374	35.488538
1279.243335	108248.287970	35.493556
1280.784732	108428.114400	35.498573
1282.638327	108595.239933	35.503591
1284.077666	108763.059089	35.508608
1285.097203	108932.490544	35.513626
1286.460993	109098.501105	35.518644
1287.932314	109271.426644	35.523661
1289.324029	109442.448167	35.528679
1290.782424	109595.199041	35.533696
1291.808925	109769.717940	35.538714
1293.102585	109912.084515	35.543732
1294.315698	110065.782468	35.548749
1296.026274	110209.780886	35.553767
1298.003170	110347.192682	35.558784
1299.009408	110489.051253	35.563802
1300.282433	110618.626044	35.568820
1301.286891	110771.298127	35.573837
1302.220322	110918.374012	35.578855
1303.778707	111064.807036	35.583872
1304.880989	111222.346853	35.588890
1306.001317	111364.382209	35.593908
1307.069156	111532.456544	35.598925
1308.098670	111693.910330	35.603943
1309.350737	111852.892622	35.608960
1310.323576	112026.834590	35.613978
1311.242041	112204.780885	35.618996
1312.822202	112385.585904	35.624013
1313.592849	112571.635937	35.629031
1314.871489	112768.836952	35.634048
1316.055931	112961.325553	35.639066
1317.211437	113159.099970	35.644084
1318.477173	113350.401135	35.649101
1320.350190	113540.587977	35.654119
1322.216064	113717.995574	35.659136
1323.486063	113912.250469	35.664154
1324.921829	114095.540781	35.669172
1326.471603	114275.363958	35.674189
1327.739052	114462.349280	35.679207
1329.056863	114639.628890	35.684224
1330.296049	114835.877378	35.689242
1331.561834	115011.756035	35.694260
1333.173036	115214.994821	35.699277
1334.031435	115403.951439	35.704295
1335.621253	115584.258697	35.709312
1336.844049	115788.019640	35.714330
1338.112293	115975.212228	35.719348
1339.782856	116160.829040	35.724365
1341.098426	116355.392938	35.729383
1342.487013	116545.761606	35.734400
1343.771059	116737.104362	35.739418
1345.564506	116928.323253	35.744436
1346.955503	117100.182167	35.749453
1348.180987	117302.536436	35.754471
1349.601699	117481.693569	35.759488
1350.837302	117673.734807	35.764506
1352.101568	117869.666967	35.769524
1353.323947	118056.267805	35.774541
1354.802587	118245.456987	35.779559
1356.133540	118441.857765	35.784576
1357.387426	118636.796925	35.789594
1358.860458	118825.845590	35.794612
1360.290143	119022.716295	35.799629
1361.226393	119217.254375	35.804647
1362.857471	119409.023957	35.809664
1364.186609	119601.463493	35.814682
1365.579212	119780.545957	35.819700
1367.086859	119960.244591	35.824717
1368.398892	120147.549030	35.829735
1369.985362	120314.306916	35.834752
1370.718477	120503.035700	35.839770
1372.654971	120662.977131	35.844788
1374.255193	120833.877559	35.849805
1375.159986	121015.870269	35.854823
1376.772100	121184.364707	35.859840
1378.102863	121371.459559	35.864858
1379.336700	121542.967412	35.869876
1380.694329	121728.616666	35.874893
1382.389581	121915.670095	35.879911
1384.124852	122101.261935	35.884928
1385.310432	122286.841108	35.889946
1386.576890	122457.589738	35.894964
1388.019494	122639.736086	35.899981
1389.238982	122826.288895	35.904999
1391.072128	123008.781002	35.910016
1392.278997	123190.221270	35.915034
1393.565313	123372.701435	35.920052
1394.999403	123569.117635	35.925069
1396.615028	123751.358043	35.930087
1397.873449	123928.235199	35.935104
1398.882055	124120.682437	35.940122
1400.545938	124317.042240	35.945140
1401.688641	124508.685599	35.950157
1402.504445	124715.633156	35.955175
1404.312852	124910.378276	35.960192
1405.305725	125123.634280	35.965210
1406.753716	125344.027234	35.970228
1407.954840	125539.392730	35.975245
1409.448248	125761.998617	35.980263
1410.558869	125967.515438	35.985280
1412.100081	126189.344499	35.990298
1413.360352	126396.664888	35.995316
1415.128044	126618.474102	36.000333
1416.064753	126847.232467	36.005351
1417.793836	127062.844164	36.010368
1419.178133	127289.685557	36.015386
1420.775396	127511.440382	36.020404
1422.225403	127729.685948	36.025421
1423.434863	127955.623146	36.030439
1425.081001	128170.661265	36.035456
1426.665045	128406.335323	36.040474
1428.138700	128625.597670	36.045492
1429.680725	128842.177772	36.050509
1430.777440	129056.600606	36.055527
1432.673298	129273.913302	36.060544
1433.726894	129495.795702	36.065562
1435.482542	129713.260785	36.070580
1436.749286	129941.042001	36.075597
1438.327235	130157.537895	36.080615
1439.725832	130368.058640	36.085632
1441.251864	130581.069277	36.090650
1442.928399	130784.669408	36.095668
1444.834578	130977.908695	36.100685
1445.755011	131173.155736	36.105703
1447.047573	131365.722321	36.110720
1448.722388	131561.460315	36.115738
1449.961001	131758.586661	36.120756
1451.433774	131961.556116	36.125773
1453.293526	132144.370523	36.130791
1455.086507	132341.818264	36.135808
1456.238456	132552.635157	36.140826
1457.461382	132748.111011	36.145844
1458.849580	132942.332889	36.150861
1459.999594	133166.103949	36.155879
1461.302874	133367.577162	36.160896
1462.670864	133580.027145	36.165914
1464.089997	133805.952477	36.170932
1465.521381	134024.553754	36.175949
1466.791835	134254.675001	36.180967
1468.266229	134469.826250	36.185984
1469.639639	134697.856569	36.191002
1471.101686	134927.407840	36.196020
1472.591598	135148.403193	36.201037
1473.984178	135384.216180	36.206055
1475.769333	135608.931593	36.211072
1477.452428	135840.685157	36.216090
1478.701249	136073.878129	36.221108
1480.335828	136297.596324	36.226125
1481.809969	136529.578612	36.231143
1483.407702	136748.135851	36.236160
1485.238434	136986.236461	36.241178
1487.082966	137209.700122	36.246196
1489.193303	137416.104025	36.251213
1490.809323	137638.872229	36.256231
1492.111271	137840.376498	36.261248
1493.882213	138052.135948	36.266266
1495.301667	138266.297237	36.271284
1496.918035	138474.954049	36.276301
1498.211006	138695.145506	36.281319
1499.652833	138901.653260	36.286336
1501.383629	139110.853948	36.291354
1502.302781	139338.003771	36.296372
1504.607830	139549.473520	36.301389
1505.819196	139766.327342	36.306407
1507.236693	139973.074448	36.311424
1508.903622	140185.739979	36.316442
1510.338233	140403.374023	36.321460
1511.585844	140611.508579	36.326477
1513.106478	140835.937934	36.331495
1514.596411	141062.046800	36.336512
1515.875693	141270.244205	36.341530
1517.280335	141501.008619	36.346548
1519.129936	141714.403607	36.351565
1520.614023	141945.120728	36.356583
1522.149502	142172.155807	36.361600
1523.377064	142387.175249	36.366618
1524.402343	142607.716477	36.371636
1526.132458	142806.638181	36.376653
1527.044195	143022.890988	36.381671
1528.915576	143235.291758	36.386688
1530.502601	143459.793137	36.391706
1531.651671	143684.188267	36.396724
1532.931377	143903.861750	36.401741
1534.200232	144138.748900	36.406759
1535.756922	144362.577148	36.411776
1537.111274	144595.109196	36.416794
1538.624985	144835.501886	36.421812
1540.213486	145072.918422	36.426829
1541.634542	145322.253261	36.431847
1543.589221	145557.739265	36.436864
1545.362978	145780.072737	36.441882
1546.361028	146028.453605	36.446900
1548.136443	146268.904393	36.451917
1550.105544	146522.585633	36.456935
1551.514529	146776.053648	36.461952
1552.996916	147016.189029	36.466970
1554.168926	147257.896714	36.471988
1556.030175	147508.091524	36.477005
1558.024672	147762.133539	36.482023
1559.666147	148000.083305	36.487040
1561.286628	148249.929167	36.492058
1562.443333	148499.368913	36.497076
1564.053350	148747.673691	36.502093
1565.824928	148998.071815	36.507111
1567.026485	149252.555795	36.512128
1568.719685	149504.580305	36.517146
1570.382585	149763.901181	36.522164
1571.821093	150013.523318	36.527181
1573.460141	150276.008789	36.532199
1575.360509	150536.578529	36.537216
1576.907724	150781.802716	36.542234
1578.591900	151051.450270	36.547252
1579.979278	151302.637060	36.552269
1581.637225	151564.711439	36.557287
1583.300552	151819.915369	36.562304
1584.872766	152072.929686	36.567322
1586.291942	152342.135393	36.572340
1588.001946	152599.036819	36.577357
1589.775692	152866.009706	36.582375
1591.197261	153114.846514	36.587392
1593.384819	153369.662069	36.592410
1594.760014	153635.829549	36.597428
1596.715969	153876.903621	36.602445
1598.454956	154133.761482	36.607463
1600.097211	154381.964002	36.612480
1602.267276	154620.498866	36.617498
1603.842173	154857.976110	36.622516
1606.337835	155080.917429	36.627533
1608.544726	155294.370968	36.632551
1610.754333	155511.248945	36.637568
1612.228403	155708.350491	36.642586
1613.363794	155911.656713	36.647604
1614.900566	156097.985313	36.652621
1616.741302	156289.617618	36.657639
1618.308228	156471.480084	36.662656
1619.824794	156659.831075	36.667674
1621.016974	156856.400690	36.672692
1622.461476	157051.714036	36.677709
1623.545359	157254.009250	36.682727
1624.868668	157467.730752	36.687744
1626.563482	157684.856349	36.692762
1627.733374	157907.189645	36.697780
1629.253056	158122.177395	36.702797
1630.595295	158356.583567	36.707815
1631.421136	158593.850435	36.712832
1633.117997	158836.078308	36.717850
1634.229097	159088.964196	36.722868
1635.919989	159338.424670	36.727885
1637.425560	159593.660935	36.732903
1639.035317	159853.232186	36.737920
1640.614511	160119.848375	36.742938
1642.066899	160390.265792	36.747956
1643.380014	160667.149636	36.752973
1645.179570	160934.916306	36.757991
1646.906393	161224.978461	36.763008
1648.505569	161499.527892	36.768026
1650.133290	161796.978584	36.773044
1651.937049	162067.264053	36.778061
1653.810209	162342.220249	36.783079
1655.095016	162634.126746	36.788096
1657.442004	162898.612414	36.793114
1658.913099	163192.776630	36.798132
1660.743588	163470.170473	36.803149
1663.018107	163737.945834	36.808167
1664.450217	164022.040160	36.813184
1666.493484	164295.322584	36.818202
1667.813860	164577.219424	36.823220
1669.584520	164849.395085	36.828237
1671.252782	165132.648718	36.833255
1672.688465	165420.215699	36.838272
1674.742116	165696.068802	36.843290
1676.168690	165978.162314	36.848308
1678.014813	166247.862915	36.853325
1679.851457	166536.960231	36.858343
1681.469112	166821.617182	36.863360
1683.233883	167092.414859	36.868378
1684.807807	167389.119970	36.873396
1686.795082	167652.922838	36.878413
1688.366348	167928.145866	36.883431
1690.465774	168211.163885	36.888448
1693.241591	168451.508139	36.893466
1695.619698	168701.138584	36.898484
1697.583586	168958.206087	36.903501
1699.551579	169198.493030	36.908519
1700.838509	169439.904386	36.913536
1702.776118	169672.017529	36.918554
1704.141279	169899.783302	36.923572
1705.916604	170107.037346	36.928589
1707.275896	170321.284503	36.933607
1708.521637	170545.977899	36.938624
1710.475336	170769.494620	36.943642
1711.995865	171001.618475	36.948660
1713.514495	171230.407799	36.953677
1714.972495	171467.466177	36.958695
1716.336290	171704.376026	36.963712
1718.088199	171939.259423	36.968730
1719.660963	172192.236785	36.973748
1721.250431	172437.411479	36.978765
1722.911345	172701.680914	36.983783
1724.592744	172956.789745	36.988800
1726.225579	173205.006830	36.993818
1728.097086	173459.238717	36.998836
1729.443483	173723.983453	37.003853
1731.325416	173986.209164	37.008871
1732.805047	174255.731549	37.013888
1734.888798	174523.079255	37.018906
1735.721040	174806.117412	37.023924
1737.785693	175085.625319	37.028941
1739.455145	175367.265780	37.033959
1740.802483	175655.124987	37.038976
1742.555441	175951.371113	37.043994
1743.907567	176249.509896	37.049012
1745.208158	176552.099398	37.054029
1746.931018	176860.967519	37.059047
1748.450353	177170.504591	37.064064
1750.373071	177486.869010	37.069082
1752.087980	177805.400260	37.074100
1754.141224	178113.857218	37.079117
1755.872267	178424.258007	37.084135
1758.127132	178731.964272	37.089152
1760.327312	179037.689495	37.094170
1762.351119	179348.507295	37.099188
1764.005581	179650.885186	37.104205
1765.948901	179947.649371	37.109223
1767.767621	180255.321640	37.114240
1769.753611	180551.829444	37.119258
1771.346986	180865.758963	37.124276
1773.193625	181162.470691	37.129293
1775.205097	181463.586482	37.134311
1776.541120	181789.198666	37.139328
1778.422160	182080.112549	37.144346
1780.101864	182390.791033	37.149364
1781.889357	182692.407573	37.154381
1784.103590	182997.473191	37.159399
1785.956428	183293.208545	37.164416
1788.263434	183584.572212	37.169434
1790.205788	183898.379047	37.174452
1791.933399	184196.665349	37.179469
1794.386432	184479.877935	37.184487
1796.042903	184763.028417	37.189504
1798.023167	185033.947518	37.194522
1799.926017	185297.939425	37.199540
1801.384257	185563.703830	37.204557
1803.034511	185823.322938	37.209575
1804.485778	186088.469699	37.214592
1806.157213	186351.032407	37.219610
1807.656177	186635.145801	37.224628
1808.964474	186908.416019	37.229645
1810.906344	187185.990655	37.234663
1812.657584	187480.779437	37.239680
1814.538195	187754.458657	37.244698
1816.308123	188038.499498	37.249716
1817.790885	188339.237195	37.254733
1819.694914	188631.889660	37.259751
1820.956488	188938.059640	37.264768
1823.312724	189235.149111	37.269786
1824.971120	189536.602537	37.274804
1826.541985	189846.422172	37.279821
1828.339508	190158.251020	37.284839
1829.870564	190475.365469	37.289856
1831.553748	190778.751710	37.294874
1833.648144	191102.481593	37.299892
1835.780070	191429.989586	37.304909
1838.094367	191724.220117	37.309927
1840.201217	192046.114036	37.314944
1842.368261	192343.074854	37.319962
1843.876640	192656.095016	37.324980
1845.551191	192964.115728	37.329997
1848.024104	193273.166532	37.335015
1849.365278	193592.260241	37.340032
1850.981488	193901.336668	37.345050
1853.255484	194235.820954	37.350068
1854.889490	194552.373955	37.355085
1856.600409	194868.624797	37.360103
1858.121802	195194.693185	37.365120
1860.601379	195525.269527	37.370138
1862.390573	195848.621517	37.375156
1864.069804	196171.815285	37.380173
1866.200052	196500.181384	37.385191
1867.613984	196830.567100	37.390208
1869.676600	197159.036906	37.395226
1871.891241	197489.642357	37.400244
1873.589323	197811.345495	37.405261
1875.893348	198132.218222	37.410279
1877.681571	198456.766799	37.415296
1880.013103	198772.942680	37.420314
1882.061940	199100.741221	37.425332
1883.849888	199419.596521	37.430349
1886.275858	199721.584892	37.435367
1888.072519	200042.955683	37.440384
1889.494804	200352.341927	37.445402
1891.377684	200665.629798	37.450420
1893.321887	200987.909295	37.455437
1894.999597	201307.199231	37.460455
1897.265474	201620.241298	37.465472
1899.282632	201919.615545	37.470490
1901.138620	202219.512017	37.475508
1903.019813	202505.011434	37.480525
1904.947373	202789.045147	37.485543
1906.396292	203086.510142	37.490560
1908.064654	203372.745849	37.495578
1910.187558	203672.163324	37.500596
1911.481112	203973.884659	37.505613
1913.218040	204281.338392	37.510631
1914.575275	204606.625824	37.515648
1916.761306	204918.695785	37.520666
1918.425598	205247.568590	37.525684
1920.151439	205577.601342	37.530701
1922.039074	205900.666399	37.535719
1923.786695	206240.905702	37.540736
1925.773434	206583.914492	37.545754
1927.787933	206919.291349	37.550772
1929.774645	207265.566546	37.555789
1931.565538	207613.550505	37.560807
1933.395466	207960.565442	37.565824
1935.631456	208306.223015	37.570842
1938.138856	208645.783934	37.575860
1939.461179	208996.909571	37.580877
1941.774114	209318.046385	37.585895
1943.814404	209669.138027	37.590912
1945.845212	210027.774127	37.595930
1947.873811	210370.429157	37.600948
1949.890481	210714.332075	37.605965
1952.095954	211048.545611	37.610983
1953.844192	211405.406139	37.616000
1956.218305	211751.796984	37.621018
1957.858531	212103.600238	37.626036
1959.753772	212457.307364	37.631053
1962.058346	212814.201564	37.636071
1964.082348	213153.609180	37.641088
1966.552411	213492.477990	37.646106
1968.567703	213840.193635	37.651124
1970.593151	214177.574846	37.656141
1972.825858	214504.234692	37.661159
1974.376757	214854.796996	37.666176
1977.016704	215190.447903	37.671194
1979.360280	215521.259385	37.676212
1980.771268	215857.578312	37.681229
1983.010938	216192.104128	37.686247
1984.837344	216527.522392	37.691264
1986.623653	216864.954673	37.696282
1988.481178	217214.591426	37.701300
1990.270710	217555.352989	37.706317
1992.346711	217902.368307	37.711335
1993.974959	218253.074934	37.716352
1995.942043	218599.488729	37.721370
1998.180958	218953.720440	37.726388
1999.816932	219315.985156	37.731405
2002.340050	219667.496128	37.736423
2004.421722	220066.274037	37.741440
2006.153759	220401.953686	37.746458
2008.454503	220716.581437	37.751476
2010.114616	221053.748264	37.756493
2012.332056	221366.487321	37.761511
2014.178738	221691.882301	37.766528
2015.830743	222015.811237	37.771546
2018.098136	222346.843366	37.776564
2020.054836	222686.446257	37.781581
2021.713808	223001.820001	37.786599
2023.364468	223347.962768	37.791616
2025.316099	223690.999127	37.796634
2027.564525	224035.399312	37.801652
2029.173601	224397.133363	37.806669
2031.612199	224748.134664	37.811687
2033.588625	225100.721848	37.816704
2035.386800	225461.325855	37.821722
2037.496808	225805.539552	37.826740
2039.690477	226166.934620	37.831757
2041.909283	226524.086058	37.836775
2044.035846	226894.688336	37.841792
2045.734480	227253.703096	37.846810
2047.955110	227607.633389	37.851828
2049.806266	227990.271262	37.856845
2051.788373	228359.734453	37.861863
2054.109258	228726.478754	37.866880
2056.046232	229106.872897	37.871898
2058.093376	229479.936780	37.876916
2060.490238	229851.880027	37.881933
2062.664021	230220.888683	37.886951
2064.363304	230598.101281	37.891968
2066.454784	230979.291400	37.896986
2068.660552	231364.452368	37.902004
2070.531548	231756.322230	37.907021
2072.709616	232127.877465	37.912039
2074.912128	232509.386260	37.917056
2076.803437	232908.800773	37.922074
2079.003153	233291.532166	37.927092
2080.953096	233677.301656	37.932109
2083.226708	234060.202062	37.937127
2085.526763	234460.675468	37.942144
2087.324280	234854.143961	37.947162
2089.797629	235238.744198	37.952180
2091.652720	235636.448099	37.957197
2093.881350	236014.587920	37.962215
2096.406251	236406.397519	37.967232
2098.485225	236791.116756	37.972250
2100.709051	237166.086510	37.977268
2102.466656	237557.793389	37.982285
2105.046139	237945.408985	37.987303
2107.004125	238318.392862	37.992320
2109.784057	238702.880544	37.997338
2112.501780	239073.435030	38.002356
2114.184087	239439.913208	38.007373
2116.371940	239819.748794	38.012391
2118.530555	240186.356943	38.017408
2120.964934	240540.197140	38.022426
2122.700626	240889.196212	38.027444
2125.075691	241228.493659	38.032461
2127.438241	241549.886968	38.037479
2129.765631	241895.823230	38.042496
2131.702105	242220.003664	38.047514
2134.232147	242534.464069	38.052532
2135.665615	242860.249933	38.057549
2137.862129	243197.498169	38.062567
2140.066985	243527.176610	38.067584
2141.936963	243875.349779	38.072602
2144.003280	244212.824458	38.077620
2146.018954	244567.605865	38.082637
2147.942630	244915.950997	38.087655
2149.488133	245280.105481	38.092672
2151.929202	245646.023927	38.097690
2154.248823	245993.165893	38.102708
2156.487017	246356.679848	38.107725
2158.641716	246720.284157	38.112743
2160.858940	247080.628102	38.117760
2163.241374	247446.814383	38.122778
2165.781163	247805.711839	38.127796
2167.778398	248162.054451	38.132813
2170.053506	248523.865899	38.137831
2172.467861	248886.418134	38.142848
2174.569408	249252.704015	38.147866
2176.835550	249605.120787	38.152884
2178.962976	249964.875966	38.157901
2181.607967	250323.305155	38.162919
2183.734253	250679.277199	38.167936
2185.528709	251041.449825	38.172954
2187.826598	251406.820188	38.177972
2189.840820	251773.049149	38.182989
2191.760393	252148.082917	38.188007
2193.894750	252519.654125	38.193024
2196.017657	252897.984817	38.198042
2198.250491	253275.790787	38.203060
2200.220416	253658.668804	38.208077
2202.365148	254038.547790	38.213095
2204.949413	254418.967444	38.218112
2206.708215	254806.834556	38.223130
2209.177201	255185.419539	38.228148
2211.322446	255577.291149	38.233165
2213.350239	255965.524149	38.238183
2216.379543	256353.522798	38.243200
2218.567189	256745.237332	38.248218
2220.817857	257116.696742	38.253236
2222.738616	257521.384769	38.258253
2224.968935	257907.505898	38.263271
2227.232946	258287.119214	38.268288
2229.344500	258682.913365	38.273306
2232.287883	259057.593582	38.278324
2234.492391	259434.220491	38.283341
2236.592966	259828.671738	38.288359
2239.143928	260198.614627	38.293376
2241.381347	260567.540791	38.298394
2243.835841	260921.521514	38.303412
2245.806023	261275.071391	38.308429
2248.128777	261615.762691	38.313447
2250.329485	261964.119993	38.318464
2251.959712	262321.001910	38.323482
2254.426845	262672.442269	38.328500
2256.054713	263036.742976	38.333517
2258.071075	263402.709856	38.338535
2260.048027	263774.551454	38.343552
2261.649721	264168.604413	38.348570
2263.852406	264555.068542	38.353588
2265.860538	264951.877556	38.358605
2267.873964	265362.022756	38.363623
2270.096043	265770.661856	38.368640
2271.722948	266192.529139	38.373658
2273.933071	266616.260351	38.378676
2276.557702	267039.951582	38.383693
2279.284447	267467.564452	38.388711
2281.744605	267892.450942	38.393728
2284.070233	268315.682430	38.398746
2286.486939	268740.119101	38.403764
2288.575434	269170.552440	38.408781
2290.356104	269595.496890	38.413799
2292.911365	270038.964803	38.418816
2294.882403	270482.068293	38.423834
2297.590038	270929.856419	38.428852
2299.855646	271376.800275	38.433869
2301.936296	271825.119982	38.438887
2305.044324	272261.972409	38.443904
2307.329865	272705.255384	38.448922
2309.965393	273134.841316	38.453940
2312.100883	273587.471268	38.458957
2314.653451	274031.956848	38.463975
2316.872574	274475.225138	38.468992
2319.505328	274922.492390	38.474010
2322.430100	275348.044207	38.479028
2325.478975	275768.724254	38.484045
2327.657343	276198.814493	38.489063
2330.332223	276624.608968	38.494080
2332.063023	277052.102620	38.499098
2334.654266	277476.868595	38.504116
2336.579610	277909.386416	38.509133
2338.867602	278343.599414	38.514151
2341.698038	278769.825790	38.519168
2343.629320	279216.720413	38.524186
2345.924332	279649.280466	38.529204
2348.166903	280082.356656	38.534221
2350.134979	280517.559168	38.539239
2352.571871	280967.344765	38.544256
2354.596642	281416.458672	38.549274
2357.335813	281859.870266	38.554292
2359.304769	282313.412464	38.559309
2361.523468	282764.857012	38.564327
2364.238099	283217.467278	38.569344
2366.465485	283660.907594	38.574362
2368.808740	284099.426292	38.579380
2371.365588	284506.004388	38.584397
2373.451550	284927.492109	38.589415
2375.537648	285345.067280	38.594432
2377.822026	285776.480593	38.599450
2380.744238	286203.626190	38.604468
2383.286997	286626.284280	38.609485
2385.319203	287063.680243	38.614503
2387.800218	287490.970331	38.619520
2389.569621	287937.170733	38.624538
2391.688678	288372.976107	38.629556
2394.166635	288822.034986	38.634573
2396.332103	289261.032401	38.639591
2398.808740	289723.528071	38.644608
2401.077005	290195.708965	38.649626
2403.193392	290651.553802	38.654644
2405.623810	291120.938391	38.659661
2408.029503	291592.104168	38.664679
2410.596252	292071.499271	38.669696
2412.615872	292553.774359	38.674714
2415.130860	293039.602426	38.679732
2417.528139	293520.672443	38.684749
2419.838246	294019.714551	38.689767
2422.896227	294498.010378	38.694784
2424.896407	294994.381206	38.699802
2427.997015	295473.531618	38.704820
2431.223513	295946.513614	38.709837
2433.482553	296443.652555	38.714855
2435.958582	296913.880635	38.719872
2438.829332	297390.979613	38.724890
2441.227804	297872.216428	38.729908
2443.804148	298343.796504	38.734925
2446.204329	298831.380767	38.739943
2448.654108	299298.482155	38.744960
2450.903295	299787.840226	38.749978
2453.427808	300272.377721	38.754996
2456.208125	300754.714078	38.760013
2457.995022	301246.909614	38.765031
2460.436310	301723.479785	38.770048
2462.680963	302222.559477	38.775066
2464.886161	302719.357638	38.780084
2467.337815	303226.249952	38.785101
2469.579771	303734.011904	38.790119
2472.331718	304229.778282	38.795136
2474.707963	304743.839986	38.800154
2477.504239	305248.561998	38.805172
2480.065063	305756.138832	38.810189
2482.358459	306274.830568	38.815207
2484.964330	306772.058366	38.820224
2488.094027	307273.468394	38.825242
2490.548971	307778.615513	38.830260
2493.416618	308279.326371	38.835277
2495.808482	308779.780345	38.840295
2498.603552	309273.259616	38.845312
2501.020289	309755.646372	38.850330
2503.207986	310222.929359	38.855348
2505.733092	310679.997239	38.860365
2507.862037	311147.285715	38.865383
2510.319887	311610.354652	38.870400
2512.972607	312078.953129	38.875418
2515.325771	312548.866987	38.880436
2517.433342	313025.573764	38.885453
2519.626275	313517.402448	38.890471
2522.326254	313994.442725	38.895488
2524.847146	314482.989244	38.900506
2527.130477	314966.770785	38.905524
2529.883602	315447.046804	38.910541
2531.970352	315953.814640	38.915559
2534.708025	316463.321281	38.920576
2536.960517	316967.746375	38.925594
2539.471653	317471.543685	38.930612
2541.791140	317991.394491	38.935629
2544.034754	318516.384692	38.940647
2547.075699	319028.978729	38.945664
2549.382418	319568.403921	38.950682
2551.515345	320107.472471	38.955700
2554.526606	320633.928795	38.960717
2556.876960	321177.172250	38.965735
2559.620927	321721.340414	38.970752
2562.230069	322263.266234	38.975770
2564.640729	322803.924851	38.980788
2567.260333	323338.959785	38.985805
2569.932174	323889.144282	38.990823
2572.670231	324433.930745	38.995840
2575.472169	324996.962758	39.000858
2577.981307	325548.990291	39.005876
2580.965907	326091.720258	39.010893
2583.577955	326641.260556	39.015911
2586.531972	327192.850568	39.020928
2589.261339	327730.022736	39.025946
2591.823261	328269.731698	39.030964
2594.572417	328810.397520	39.035981
2597.094614	329367.753854	39.040999
2600.171614	329899.979815	39.046016
2602.283442	330444.797699	39.051034
2604.647709	330994.802553	39.056052
2607.723843	331539.941898	39.061069
2610.249509	332089.328740	39.066087
2613.060046	332638.158322	39.071104
2615.411966	333193.379020	39.076122
2618.234735	333738.312922	39.081140
2621.411949	334272.191514	39.086157
2623.484060	334819.343272	39.091175
2626.158687	335359.056907	39.096192
2629.380622	335910.943635	39.101210
2631.842878	336451.545367	39.106228
2634.839399	336989.544287	39.111245
2637.481494	337533.688742	39.116263
2640.023200	338061.619808	39.121280
2642.667307	338588.438504	39.126298
2644.725370	339093.357610	39.131316
2647.246057	339605.613313	39.136333
2649.739037	340131.021196	39.141351
2652.446707	340637.272153	39.146368
2654.824824	341140.803686	39.151386
2657.406351	341657.983686	39.156404
2660.153273	342175.412351	39.161421
2662.443357	342709.487858	39.166439
2664.985671	343251.135220	39.171456
2667.344171	343786.028037	39.176474
2669.434168	344341.903749	39.181492
2672.438812	344881.584114	39.186509
2674.776681	345449.850034	39.191527
2677.174775	346008.021974	39.196544
2679.817256	346567.469863	39.201562
2682.200136	347145.079588	39.206580
2685.385076	347723.851037	39.211597
2688.011358	348303.720397	39.216615
2690.605855	348885.949601	39.221632
2693.185057	349479.497116	39.226650
2695.262251	350078.118604	39.231668
2698.158869	350680.614526	39.236685
2699.983458	351291.828182	39.241703
2703.053427	351897.151371	39.246720
2705.731162	352526.035659	39.251738
2708.570896	353143.438483	39.256756
2711.707699	353770.432724	39.261773
2714.419377	354407.919239	39.266791
2717.481673	355021.659765	39.271808
2720.091280	355648.638223	39.276826
2723.157006	356275.638133	39.281844
2725.968096	356902.492791	39.286861
2728.580858	357536.300150	39.291879
2731.245380	358167.857536	39.296896
2734.228074	358797.224308	39.301914
2737.113824	359437.131288	39.306932
2740.284386	360053.736036	39.311949
2743.081515	360682.244487	39.316967
2745.952472	361307.788810	39.321984
2749.404173	361932.090734	39.327002
2752.050753	362556.334125	39.332020
2755.301022	363165.347683	39.337037
2757.798547	363780.410931	39.342055
2760.673668	364386.980527	39.347072
2764.043557	365003.792417	39.352090
2766.595365	365606.082580	39.357108
2769.487159	366214.756573	39.362125
2772.181610	366813.074351	39.367143
2774.749771	367424.193731	39.372160
2777.766185	368034.320056	39.377178
2780.174042	368645.701468	39.382196
2783.217897	369240.251144	39.387213
2785.815528	369862.445889	39.392231
2788.594729	370463.770219	39.397248
2791.616072	371065.073047	39.402266
2794.220840	371649.686454	39.407284
2797.167278	372222.514996	39.412301
2799.701263	372795.654693	39.417319
2801.860554	373373.514388	39.422336
2804.309947	373953.552811	39.427354
2806.513761	374561.607377	39.432372
2809.328751	375159.153647	39.437389
2811.690186	375761.964027	39.442407
2814.263967	376371.556535	39.447424
2817.049622	376997.470231	39.452442
2819.524394	377624.488821	39.457460
2822.554174	378247.553352	39.462477
2825.168287	378890.157482	39.467495
2828.053551	379531.667948	39.472512
2831.197499	380173.380508	39.477530
2833.891555	380821.013628	39.482548
2837.145584	381465.452260	39.487565
2839.669828	382123.262578	39.492583
2842.412593	382782.980085	39.497600
2845.391664	383436.560658	39.502618
2848.648501	384096.731673	39.507636
2851.750490	384748.088269	39.512653
2854.454794	385402.311831	39.517671
2857.273564	386070.760471	39.522688
2859.870238	386729.644379	39.527706
2862.660469	387412.581092	39.532724
2866.113872	388081.551585	39.537741
2868.868000	388769.058920	39.542759
2871.519078	389442.848348	39.547776
2874.807949	390117.259452	39.552794
2877.086794	390806.324107	39.557812
2880.080712	391489.733340	39.562829
2883.526634	392171.434516	39.567847
2886.479371	392852.642389	39.572864
2889.439314	393535.636103	39.577882
2892.269584	394226.979675	39.582900
2895.369451	394910.988694	39.587917
2897.759376	395602.373866	39.592935
2900.295790	396306.095864	39.597952
2903.624616	397006.812282	39.602970
2906.335543	397719.579741	39.607988
2908.987535	398423.517413	39.613005
2911.454773	399141.135512	39.618023
2914.252192	399856.631839	39.623040
2917.595554	400574.966983	39.628058
2920.589888	401306.550381	39.633076
2923.609228	402012.329464	39.638093
2926.753997	402739.140631	39.643111
2929.846288	403461.836476	39.648128
2933.346948	404162.294383	39.653146
2936.214588	404870.441923	39.658164
2939.445257	405580.974823	39.663181
2942.864494	406283.045639	39.668199
2945.787767	406984.722676	39.673216
2948.924626	407665.843264	39.678234
2951.686527	408323.155981	39.683252
2954.754408	408984.943125	39.688269
2957.432881	409634.078841	39.693287
2960.332418	410281.568747	39.698304
2963.848477	410921.622248	39.703322
2966.439665	411576.077456	39.708340
2969.176314	412222.511750	39.713357
2972.250564	412882.893459	39.718375
2975.100723	413536.453132	39.723392
2978.086843	414183.184855	39.728410
2980.873630	414848.560044	39.733428
2984.066864	415501.108892	39.738445
2987.593872	416170.973877	39.743463
2990.306243	416836.036120	39.748480
2993.635992	417503.265696	39.753498
2996.257817	418171.529151	39.758516
2998.795303	418849.849467	39.763533
3001.550913	419538.634053	39.768551
3004.289901	420236.322965	39.773568
3007.332455	420926.573427	39.778586
3010.527574	421622.077731	39.783604
3013.741490	422312.545135	39.788621
3016.566024	423021.576339	39.793639
3019.100669	423737.019142	39.798656
3022.181576	424449.772670	39.803674
3024.906308	425168.542251	39.808692
3028.051278	425889.075353	39.813709
3031.271368	426615.656659	39.818727
3034.072477	427356.418858	39.823744
3037.299603	428087.087691	39.828762
3040.087348	428830.672980	39.833780
3043.109094	429569.615755	39.838797
3045.982871	430315.424833	39.843815
3049.167957	431074.991739	39.848832
3052.143677	431827.300877	39.853850
3055.183479	432585.377412	39.858868
3058.186375	433350.325663	39.863885
3061.894772	434107.339580	39.868903
3065.000521	434880.607741	39.873920
3067.978362	435629.689627	39.878938
3070.918581	436402.481469	39.883956
3074.189809	437160.536320	39.888973
3077.521630	437925.901308	39.893991
3080.429458	438694.550602	39.899008
3083.152167	439453.786764	39.904026
3086.165624	440229.055475	39.909044
3089.217602	441015.432899	39.914061
3092.070529	441802.778391	39.919079
3095.206949	442589.445844	39.924096
3098.141589	443374.904434	39.929114
3100.941127	444172.863542	39.934132
3103.869094	444971.180641	39.939149
3106.929149	445775.676705	39.944167
3110.033861	446585.149876	39.949184
3113.468566	447374.649247	39.954202
3116.273615	448159.159754	39.959220
3119.074345	448925.726181	39.964237
3122.234101	449683.200974	39.969255
3125.118307	450462.255851	39.974272
3128.279430	451226.107604	39.979290
3131.891545	452002.413805	39.984308
3135.059702	452771.020713	39.989325
3138.881678	453531.148047	39.994343
3141.413452	454313.112802	39.999360
3144.396203	455089.918713	40.004378
3147.513680	455874.013553	40.009396
3150.073481	456653.868070	40.014413
3153.450506	457449.908987	40.019431
3156.995470	458260.365086	40.024448
3160.243476	459052.219681	40.029466
3162.829660	459865.399069	40.034484
3165.769507	460673.989646	40.039501
3168.877562	461494.057651	40.044519
3171.692649	462322.841748	40.049536
3174.646222	463170.288269	40.054554
3177.651805	464014.759242	40.059572
3180.947365	464864.158354	40.064589
3184.380836	465715.474205	40.069607
3187.023841	466580.334088	40.074624
3190.698396	467433.868891	40.079642
3193.673798	468305.786605	40.084660
3197.018064	469169.164286	40.089677
3200.591298	470046.072582	40.094695
3203.571597	470935.577723	40.099712
3206.919439	471799.653874	40.104730
3210.254152	472685.032533	40.109748
3213.623149	473566.575333	40.114765
3216.497917	474462.516159	40.119783
3219.882913	475354.494348	40.124800
3222.838121	476241.142340	40.129818
3226.047855	477146.818759	40.134836
3229.985325	478029.895583	40.139853
3233.611529	478916.773208	40.144871
3236.703291	479811.984611	40.149888
3240.095931	480695.179924	40.154906
3243.337173	481592.358548	40.159924
3246.392493	482489.222015	40.164941
3250.075191	483389.128411	40.169959
3252.957823	484279.316206	40.174976
3256.716943	485167.909318	40.179994
3259.847718	486057.368957	40.185012
3263.084490	486955.864751	40.190029
3266.993428	487846.178626	40.195047
3270.064033	488749.263602	40.200064
3273.852032	489622.083309	40.205082
3277.275882	490510.478588	40.210100
3280.886153	491377.334122	40.215117
3284.234322	492245.907988	40.220135
3287.434592	493123.404371	40.225152
3290.873557	493986.982649	40.230170
3293.847332	494826.857267	40.235188
3296.579493	495652.793195	40.240205
3300.133002	496480.581713	40.245223
3303.090278	497311.406006	40.250240
3306.399754	498149.912481	40.255258
3309.733852	498968.936647	40.260276
3313.006755	499799.040747	40.265293
3316.373098	500634.544085	40.270311
3319.068858	501482.987813	40.275328
3322.172102	502322.340642	40.280346
3325.456302	503193.023409	40.285364
3328.568616	504051.424254	40.290381
3331.767869	504918.450958	40.295399
3334.994317	505799.360629	40.300416
3337.924492	506675.780692	40.305434
3340.916698	507581.821249	40.310452
3344.599239	508482.406284	40.315469
3348.139478	509378.626873	40.320487
3351.082115	510302.697967	40.325504
3354.839980	511202.724189	40.330522
3358.122005	512114.129992	40.335540
3361.071671	513054.800738	40.340557
3364.545961	513970.212833	40.345575
3367.514574	514923.186217	40.350592
3370.683885	515852.718661	40.355610
3374.273293	516799.181328	40.360628
3377.610087	517751.984879	40.365645
3381.126743	518712.017866	40.370663
3384.141028	519692.196055	40.375680
3387.460539	520648.566258	40.380698
3391.564024	521628.607313	40.385716
3394.931160	522594.032887	40.390733
3398.815576	523540.815356	40.395751
3402.005801	524527.833235	40.400768
3405.867294	525496.434895	40.405786
3409.557376	526460.770509	40.410804
3413.069066	527433.292129	40.415821
3417.099185	528378.907887	40.420839
3420.767136	529331.177099	40.425856
3424.711987	530290.400494	40.430874
3428.425671	531227.780952	40.435892
3431.611793	532171.084270	40.440909
3435.245008	533113.151130	40.445927
3438.826258	534050.684612	40.450944
3442.593360	534991.255427	40.455962
3446.526379	535925.898484	40.460980
3449.315470	536862.428466	40.465997
3453.249070	537785.471989	40.471015
3456.758626	538715.830100	40.476032
3460.034489	539651.758696	40.481050
3463.785252	540586.194359	40.486068
3467.163088	541513.026457	40.491085
3471.009780	542430.813851	40.496103
3474.426408	543357.676542	40.501120
3478.012704	544255.478157	40.506125
3481.718508	545119.235635	40.511130
3485.220129	545920.084071	40.516135
3488.810057	546634.517969	40.521140
3492.118756	547295.918161	40.526144
3494.917912	547898.625010	40.531149
3497.913953	548425.022496	40.536154
3500.299119	548898.157172	40.541159
3502.975943	549286.100118	40.546164
3505.330065	549634.269679	40.551168
3507.510722	549916.254320	40.556173
3509.584655	550129.827118	40.561178
3511.230709	550315.510089	40.566183
3512.861673	550431.509805	40.571188
3514.333178	550510.144167	40.576192
3515.669578	550554.134684	40.581197
3516.741183	550562.139797	40.586202
3517.558251	550527.800198	40.591207
3518.445234	550461.408316	40.596212
3519.190328	550374.754106	40.601216
3519.413902	550267.897206	40.606221
3520.556811	550114.319928	40.611226
3520.887377	549949.667224	40.616231
3521.894737	549770.978469	40.621236
3521.803021	549567.331335	40.626240
3522.092493	549353.024000	40.631245
3522.571998	549120.920433	40.636250
3522.598160	548885.150480	40.641255
3523.082190	548616.704018	40.646260
3523.176076	548357.902796	40.651264
3523.095751	548079.291075	40.656269
3523.182652	547793.026977	40.661274
3523.087311	547510.217961	40.666279
3523.708271	547212.805449	40.671284
3523.392525	546915.181656	40.676288
3523.028248	546612.461842	40.681293
3522.850860	546304.002815	40.686298
3522.529742	545994.550558	40.691303
3522.793605	545688.734500	40.696308
3522.255413	545385.108386	40.701312
3522.019761	545069.818471	40.706317
3522.157775	544765.719417	40.711322
3521.753405	544470.180346	40.716327
3521.976842	544160.300734	40.721332
3521.596655	543853.488450	40.726336
3521.142902	543551.931617	40.731341
3521.050887	543234.611169	40.736346
3520.539230	542949.458371	40.741351
3520.780894	542647.470404	40.746356
3520.401963	542355.570717	40.751360
3520.399445	542068.149696	40.756365
3520.025407	541763.767302	40.761370
3519.645709	541483.816460	40.766375
3519.381772	541192.380802	40.771380
3519.403426	540914.627967	40.776384
3518.962805	540624.269524	40.781389
3519.052896	540346.495378	40.786394
3518.782267	540069.328556	40.791399
3518.746783	539783.989777	40.796404
3518.046949	539525.917412	40.801408
3518.189193	539250.286160	40.806413
3518.203606	538977.800948	40.811418
3517.693266	538726.199186	40.816423
3517.631669	538461.089478	40.821428
3517.063489	538206.458265	40.826432
3516.804734	537944.602714	40.831437
3517.013943	537696.859750	40.836442
3516.617496	537462.288696	40.841447
3516.707867	537200.264151	40.846452
3516.326501	536968.208287	40.851456
3515.912720	536724.083281	40.856461
3515.892550	536481.811389	40.861466
3515.685002	536268.556146	40.866471
3515.477203	536025.246037	40.871476
3515.221123	535806.587726	40.876480
3514.891707	535576.674388	40.881485
3514.697394	535360.171835	40.886490
3514.887527	535144.817716	40.891495
3514.466144	534931.880744	40.896500
3514.314842	534710.765735	40.901504
3513.756762	534500.471012	40.906509
3514.033424	534299.841043	40.911514
3513.491621	534107.369521	40.916519
3513.585913	533899.640726	40.921524
3513.172940	533721.843741	40.926528
3513.186697	533522.962745	40.931533
3513.115360	533325.254518	40.936538
3512.650117	533148.671598	40.941543
3512.736840	532952.095515	40.946548
3512.304776	532776.917607	40.951552
3512.312871	532601.516596	40.956557
3512.130050	532405.026705	40.961562
3511.737844	532249.033881	40.966567
3511.676063	532073.941079	40.971572
3511.521985	531916.644274	40.976576
3511.386867	531743.933834	40.981581
3511.316195	531591.824279	40.986586
3511.066555	531422.715442	40.991591
3511.219830	531266.373947	40.996596
3510.903774	531115.157421	41.001600
3510.805675	530964.662842	41.006605
3510.740126	530804.157814	41.011610
3510.213284	530667.672906	41.016615
3510.373739	530515.667917	41.021620
3510.207808	530378.870820	41.026624
3510.399278	530241.056039	41.031629
3509.901609	530084.148773	41.036634
3509.950318	529960.703715	41.041639
3509.737264	529808.447741	41.046644
3509.403481	529691.073817	41.051648
3509.257432	529546.030229	41.056653
3509.348866	529439.956151	41.061658
3509.001085	529319.701517	41.066663
3509.135124	529187.747973	41.071668
3509.148156	529073.346407	41.076672
3509.022346	528947.091288	41.081677
3508.999573	528819.100821	41.086682
3508.807857	528708.064006	41.091687
3508.945537	528591.516928	41.096692
3508.558886	528475.001331	41.101696
3508.610677	528358.617706	41.106701
3508.523140	528243.164835	41.111706
3508.219817	528135.123062	41.116711
3508.153039	528019.917945	41.121716
3507.906866	527918.485544	41.126720
3507.731751	527816.535920	41.131725
3507.915659	527723.776696	41.136730
3507.715133	527627.995073	41.141735
3507.774822	527525.955932	41.146740
3507.748180	527420.948191	41.151744
3507.356798	527326.508833	41.156749
3507.569079	527236.723881	41.161754
3507.193483	527148.800109	41.166759
3507.026973	527052.201051	41.171764
3506.958410	526967.916917	41.176768
3506.863452	526891.924590	41.181773
3506.867728	526796.813098	41.186778
3506.670113	526729.275959	41.191783
3506.739880	526632.889695	41.196788
3506.588371	526553.821879	41.201792
3506.657191	526485.180290	41.206797
3506.641819	526404.624602	41.211802
3506.499157	526328.637125	41.216807
3506.323394	526245.427422	41.221812
3506.355787	526167.945875	41.226816
3506.222111	526097.363586	41.231821
3506.361694	526017.236304	41.236826
3506.074156	525954.713537	41.241831
3506.302918	525874.824145	41.246836
3506.105586	525811.932779	41.251840
3505.849331	525758.754289	41.256845
3506.108836	525676.028766	41.261850
3506.002213	525616.761240	41.266855
3506.254658	525549.805001	41.271860
3506.131960	525476.539541	41.276864
3505.946805	525409.146463	41.281869
3505.950941	525337.073319	41.286874
3505.684736	525269.490295	41.291879
3505.993521	525200.855798	41.296884
3505.922892	525135.869504	41.301888
3505.492584	525069.676225	41.306893
3505.498135	525015.746283	41.311898
3505.510567	524962.168873	41.316903
3505.703735	524893.096443	41.321908
3505.520305	524854.156668	41.326912
3505.409500	524783.160612	41.331917
3505.302552	524733.897526	41.336922
3505.062519	524679.600917	41.341927
3505.357546	524611.522057	41.346932
3505.106916	524571.379152	41.351936
3505.191985	524512.987041	41.356941
3505.364232	524452.154788	41.361946
3505.077591	524408.883391	41.366951
3505.137177	524340.284599	41.371956
3505.126720	524297.929608	41.376960
3504.957109	524258.025840	41.381965
3505.025065	524204.639307	41.386970
3504.721331	524166.980517	41.391975
3505.082558	524120.320471	41.396980
3504.861902	524062.025588	41.401984
3504.814284	524022.405229	41.406989
3504.802726	523969.990861	41.411994
3504.923298	523918.667461	41.416999
3504.896429	523883.744302	41.422004
3504.751601	523832.917496	41.427008
3504.796873	523781.251732	41.432013
3504.612978	523738.265570	41.437018
3504.513549	523700.118471	41.442023
3504.724460	523656.463122	41.447028
3504.451095	523601.005548	41.452032
3504.596446	523574.900304	41.457037
3504.442330	523531.807788	41.462042
3504.198932	523504.803469	41.467047
3504.476673	523446.427580	41.472052
3504.470846	523418.930635	41.477056
3504.453755	523380.921410	41.482061
3504.361541	523342.620679	41.487066
3504.176344	523315.556295	41.492071
3504.205060	523266.469464	41.497076
3503.975044	523230.919868	41.502080
3504.271842	523195.337476	41.507085
3504.283066	523168.949482	41.512090
3504.084555	523135.113355	41.517095
3504.303627	523091.455188	41.522100
3504.228228	523053.353309	41.527104
3504.239334	523026.510158	41.532109
3504.267268	522979.242351	41.537114
3503.883842	522958.679024	41.542119
3504.122371	522918.505228	41.547124
3503.993057	522895.525824	41.552128
3503.881851	522851.767564	41.557133
3504.026780	522831.373313	41.562138
3503.858252	522810.118681	41.567143
3504.033305	522768.488597	41.572148
3504.279287	522749.038721	41.577152
3504.239693	522707.088555	41.582157
3504.237103	522662.958764	41.587162
3504.038128	522649.796797	41.592167
3504.132143	522604.792221	41.597172
3504.175469	522573.191469	41.602176
3503.878427	522538.712507	41.607181
3504.106140	522500.662517	41.612186
3503.973973	522481.373191	41.617191
3503.968043	522444.522671	41.622196
3504.159828	522407.337509	41.627200
3503.887562	522381.599653	41.632205
3504.095532	522339.862162	41.637210
3503.601693	522327.150949	41.642215
3503.720848	522300.795030	41.647220
3503.878938	522266.799618	41.652224
3503.657633	522233.268516	41.657229
3503.923872	522216.089627	41.662234
3503.557569	522186.069419	41.667239
3503.876814	522154.828655	41.672244
3503.632986	522143.695444	41.677248
3503.993502	522121.244142	41.682253
3503.964551	522085.356934	41.687258
3503.574983	522059.839315	41.692263
3503.550067	522031.786953	41.697268
3503.636555	522027.982099	41.702272
3503.728196	521987.525897	41.707277
3503.771711	521977.509863	41.712282
3503.551442	521938.922732	41.717287
3503.517902	521912.843081	41.722292
3503.226013	521887.360304	41.727296
3503.524716	521866.637217	41.732301
3503.704999	521847.196644	41.737306
3503.412780	521828.235155	41.742311
3503.666046	521802.817738	41.747316
3503.441991	521785.816996	41.752320
3503.426871	521763.525679	41.757325
3503.676704	521737.603170	41.762330
3503.289869	521717.139908	41.767335
3503.622675	521691.659191	41.772340
3503.445894	521676.571893	41.777344
3503.771043	521643.357626	41.782349
3503.443490	521624.047608	41.787354
3503.712682	521606.513734	41.792359
3503.848288	521570.447716	41.797364
3503.640935	521552.230797	41.802368
3503.636156	521528.218691	41.807373
3503.710007	521496.964896	41.812378
3503.370713	521486.250754	41.817383
3503.669891	521448.641990	41.822388
3503.239521	521432.330692	41.827392
3503.322087	521422.105926	41.832397
3503.455890	521400.498332	41.837402
3503.092196	521379.525442	41.842407
3503.190208	521359.844519	41.847412
3502.979690	521355.934789	41.852416
3502.974390	521319.081613	41.857421
3503.047717	521308.908791	41.862426
3503.152830	521311.116825	41.867431
3503.423964	521277.960905	41.872436
3503.192247	521274.155615	41.877440
3503.134642	521250.303112	41.882445
3503.431481	521230.186168	41.887450
3502.960560	521216.358250	41.892455
3503.076520	521195.157643	41.897460
3503.286941	521184.255305	41.902464
3503.356867	521177.015128	41.907469
3503.128385	521135.343528	41.912474
3503.071725	521146.828747	41.917479
3503.412332	521105.724338	41.922484
3503.041674	521103.862069	41.927488
3503.207295	521081.591804	41.932493
3503.302451	521060.849309	41.937498
3503.015028	521048.256130	41.942503
3503.056914	521031.515896	41.947508
3503.265668	521016.164825	41.952512
3503.386484	521003.456529	41.957517
3503.516275	520964.154530	41.962522
3503.226931	520965.565512	41.967527
3503.517913	520938.472446	41.972532
3503.392731	520932.375227	41.977536
3503.065530	520916.653773	41.982541
3503.451227	520897.887381	41.987546
3503.315650	520871.721076	41.992551
3503.630452	520849.426915	41.997556
3503.427298	520832.775764	42.002560
3502.882940	520815.470741	42.007565
3503.151985	520800.059381	42.012570
3503.166596	520791.361646	42.017575
3503.410659	520763.719588	42.022580
3503.613754	520751.554210	42.027584
3503.459054	520733.125826	42.032589
3503.148486	520726.754493	42.037594
3503.107904	520694.860011	42.042599
3503.312301	520680.722671	42.047604
3502.993323	520670.611458	42.052608
3503.118413	520652.694882	42.057613
3503.305420	520635.425737	42.062618
3503.002499	520631.732664	42.067623
3503.191563	520601.520631	42.072628
3503.368847	520597.397751	42.077632
3503.219512	520575.277691	42.082637
3503.206227	520565.421436	42.087642
3503.222275	520551.060969	42.092647
3503.358301	520519.744914	42.097652
3503.147577	520517.098941	42.102656
3502.977836	520493.566397	42.107661
3503.250760	520476.081275	42.112666
3503.035013	520468.683709	42.117671
3502.969696	520442.252823	42.122676
3503.213463	520429.322418	42.127680
3503.069589	520417.312748	42.132685
3503.056675	520396.434818	42.137690
3502.984653	520397.912612	42.142695
3503.347994	520382.587070	42.147700
3502.986120	520358.225221	42.152704
3503.122701	520356.181575	42.157709
3503.340515	520342.951858	42.162714
3503.300091	520322.229854	42.167719
3503.755572	520296.626454	42.172724
3503.428334	520266.697639	42.177728
3503.569308	520259.900847	42.182733
3503.639139	520227.128516	42.187738
3503.362790	520206.949235	42.192743
3503.747539	520175.037068	42.197748
3503.162177	520163.754249	42.202752
3503.043211	520143.802805	42.207757
3503.200676	520127.548958	42.212762
3503.225043	520100.901112	42.217767
3503.141165	520095.302634	42.222772
3503.318167	520080.511846	42.227776
3503.116658	520061.685634	42.232781
3503.389228	520042.835026	42.237786
3502.926792	520026.931853	42.242791
3503.334319	520002.346745	42.247796
3502.929006	520012.421668	42.252800
3503.149911	519984.680836	42.257805
3503.412366	519963.404917	42.262810
3503.115726	519960.974667	42.267815
3503.151821	519927.650921	42.272820
3503.296193	519921.409600	42.277824
3503.051074	519903.045128	42.282829
3503.501360	519883.407863	42.287834
3503.390101	519875.235126	42.292839
3503.379206	519847.176785	42.297844
3503.384264	519836.154331	42.302848
3503.414885	519806.370346	42.307853
3503.710063	519789.083211	42.312858
3503.014889	519776.502937	42.317863
3503.338281	519744.043476	42.322868
3503.211741	519740.322320	42.327872
3503.308770	519706.280659	42.332877
3503.475182	519697.710028	42.337882
3502.961930	519677.972015	42.342887
3503.266175	519666.598799	42.347892
3503.377502	519650.200092	42.352896
3503.218623	519617.816609	42.357901
3503.598871	519611.740127	42.362906
3503.104996	519592.757347	42.367911
3503.083584	519566.368665	42.372916
3503.264457	519549.200465	42.377920
3503.003206	519532.456049	42.382925
3503.370802	519527.797220	42.387930
3503.044527	519504.338553	42.392935
3503.365815	519478.552846	42.397940
3503.550356	519471.040997	42.402944
3503.058649	519444.018608	42.407949
3503.261958	519434.380240	42.412954
3503.141916	519415.742649	42.417959
3503.339837	519394.931237	42.422964
3503.213920	519388.681875	42.427968
3503.289039	519375.473932	42.432973
3503.677172	519357.767166	42.437978
3503.331784	519343.614449	42.442983
3503.319912	519316.718251	42.447988
3503.361055	519296.032616	42.452992
3503.102312	519281.512224	42.457997
3503.007346	519247.702202	42.463002
3503.199780	519248.834934	42.468007
3503.113696	519232.315329	42.473012
3502.792044	519214.214986	42.478016
3503.052771	519195.870889	42.483021
3503.414471	519193.488150	42.488026
3502.900003	519171.474464	42.493031
3502.815356	519157.533180	42.498036
3503.012075	519155.024829	42.503040
3503.098466	519132.663313	42.508045
3502.818435	519115.213579	42.513050
3503.081001	519111.835270	42.518055
3503.265010	519098.154840	42.523060
3503.236877	519079.097848	42.528064
3503.185090	519066.718700	42.533069
3503.218209	519038.854265	42.538074
3503.131919	519036.592875	42.543079
3503.370589	519015.218363	42.548084
3503.172879	518995.075719	42.553088
3502.942355	518987.882064	42.558093
3502.999558	518954.906937	42.563098
3502.805697	518942.246780	42.568103
3502.904697	518934.697645	42.573108
3503.036194	518943.525448	42.578112
3502.848817	518917.869823	42.583117
3503.349882	518887.858126	42.588122
3502.844962	518885.612321	42.593127
3503.149369	518867.968824	42.598132
3503.085475	518853.012757	42.603136
3502.772507	518845.528697	42.608141
3502.891677	518846.723600	42.613146
3503.046084	518820.204804	42.618151
3502.888914	518799.499326	42.623156
3503.101421	518807.303150	42.628160
3503.049463	518789.159710	42.633165
3503.081090	518763.873728	42.638170
3502.822589	518761.032769	42.643175
3502.885352	518741.505956	42.648180
3503.034232	518734.454471	42.653184
3502.912204	518726.434550	42.658189
3502.953821	518720.562953	42.663194
3502.715614	518712.965890	42.668199
3502.655108	518696.997893	42.673204
3503.010243	518697.902697	42.678208
3502.643100	518693.258641	42.683213
3503.169114	518652.068208	42.688218
3502.720674	518651.734830	42.693223
3502.926765	518635.977450	42.698228
3503.040940	518646.325037	42.703232
3502.694192	518612.047874	42.708237
3502.843147	518608.687419	42.713242
3502.639270	518613.422244	42.718247
3502.821138	518605.202542	42.723252
3503.165511	518593.569428	42.728256
3502.695314	518573.267083	42.733261
3503.126519	518567.637232	42.738266
3502.486013	518560.356501	42.743271
3502.537652	518536.128832	42.748276
3502.859260	518519.999139	42.753280
3502.565463	518519.287373	42.758285
3502.929407	518526.814578	42.763290
3502.617512	518523.729201	42.768295
3502.886056	518497.343534	42.773300
3502.892762	518485.409773	42.778304
3503.102447	518480.371102	42.783309
3503.414012	518475.973651	42.788314
3503.068187	518443.465709	42.793319
3503.251382	518449.403487	42.798324
3503.072528	518420.661368	42.803329
3502.790591	518411.806988	42.808333
3503.078810	518389.210307	42.813338
3502.717092	518385.222632	42.818343
3503.061253	518355.841531	42.823348
3502.960989	518366.829954	42.828353
3502.871645	518355.568608	42.833357
3503.092772	518325.903518	42.838362
3502.867800	518315.371476	42.843367
3503.359724	518306.495851	42.848372
3503.064461	518279.794441	42.853377
3503.302130	518272.930981	42.858381
3503.217031	518259.039570	42.863386
3503.024621	518243.547058	42.868391
3503.275914	518228.085528	42.873396
3503.353509	518205.420758	42.878401
3502.763044	518199.345496	42.883405
3503.137491	518185.887030	42.888410
3503.025834	518161.836314	42.893415
3503.122764	518144.427094	42.898420
3503.002571	518141.867552	42.903425
3503.207504	518111.698993	42.908429
3503.297503	518106.375740	42.913434
3502.976084	518094.898075	42.918439
3503.062851	518067.529162	42.923444
3503.294735	518056.115709	42.928449
3502.753320	518057.819599	42.933453
3503.195475	518036.866738	42.938458
3502.888200	518029.634228	42.943463
3502.994636	518024.763433	42.948468
3503.076983	517996.484935	42.953473
3503.010391	517988.152503	42.958477
3503.101434	517981.564922	42.963482
3503.006319	517963.831913	42.968487
3502.808831	517940.502349	42.973492
3502.635230	517947.861960	42.978497
3502.989934	517934.204150	42.983501
3503.262666	517909.081007	42.988506
3503.114408	517896.109445	42.993511
3503.032294	517888.790719	42.998516
3503.001127	517867.356240	43.003521
3502.615257	517859.074207	43.008525
3503.062895	517847.879335	43.013530
3502.758108	517832.758156	43.018535
3503.070428	517809.145565	43.023540
3503.003619	517805.262831	43.028545
3502.772457	517791.748071	43.033549
3503.106631	517773.694176	43.038554
3503.016610	517763.140450	43.043559
3503.174070	517752.598166	43.048564
3502.985425	517727.598238	43.053569
3502.765780	517727.380372	43.058573
3503.245644	517705.713212	43.063578
3503.040875	517703.874890	43.068583
3503.117677	517673.220125	43.073588
3503.073495	517668.019070	43.078593
3502.408927	517649.971204	43.083597
3502.749744	517631.359879	43.088602
3502.799378	517638.380947	43.093607
3503.175277	517631.596505	43.098612
3502.952554	517611.001026	43.103617
3502.445843	517597.529659	43.108621
3502.817399	517583.059839	43.113626
3502.668569	517584.903988	43.118631
3502.905077	517580.113635	43.123636
3503.038372	517563.709379	43.128641
3502.565552	517552.457530	43.133645
3502.926344	517537.180312	43.138650
3502.807423	517533.963113	43.143655
3502.881340	517517.821027	43.148660
3502.938439	517507.193317	43.153665
3502.637163	517498.796599	43.158669
3502.859006	517496.890824	43.163674
3502.523980	517480.358242	43.168679
3503.049965	517454.739282	43.173684
3503.075566	517459.185332	43.178689
3502.758412	517453.926224	43.183693
3502.641285	517434.679130	43.188698
3502.620324	517423.456905	43.193703
3502.452551	517406.139314	43.198708
3502.812551	517426.612707	43.203713
3502.835874	517421.198639	43.208717
3503.276792	517397.362868	43.213722
3502.664734	517389.773717	43.218727
3502.857934	517373.258669	43.223732
3502.689653	517374.145147	43.228737
3502.682294	517364.184901	43.233741
3502.813330	517348.033622	43.238746
3502.802879	517344.344139	43.243751
3502.750391	517336.514817	43.248756
3502.780548	517338.179002	43.253761
3502.961592	517323.283966	43.258765
3503.186428	517298.774270	43.263770
3502.714125	517303.855298	43.268775
3503.007952	517277.514255	43.273780
3503.215653	517267.873928	43.278785
3502.986435	517255.218061	43.283789
3502.701722	517246.768030	43.288794
3502.751736	517225.319886	43.293799
3502.911661	517221.502312	43.298804
3502.882900	517214.174854	43.303809
3502.498024	517217.067698	43.308813
3502.989052	517187.357904	43.313818
3502.495791	517191.228663	43.318823
3502.688737	517173.196437	43.323828
3503.026783	517167.024597	43.328833
3503.015432	517161.211385	43.333837
3502.882289	517147.528902	43.338842
3502.839286	517132.618540	43.343847
3503.194498	517118.504871	43.348852
3502.823102	517111.433794	43.353857
3502.813065	517096.973297	43.358861
3503.009068	517079.699001	43.363866
3502.863311	517078.154686	43.368871
3502.595116	517055.138453	43.373876
3502.935198	517045.881615	43.378881
3502.652521	517042.589068	43.383885
3502.860116	517030.571934	43.388890
3502.845745	517025.214262	43.393895
3502.910505	517003.611798	43.398900
3502.697502	517014.568370	43.403905
3502.608140	517010.941853	43.408909
3502.965389	516998.496500	43.413914
3502.532943	516983.445287	43.418919
3502.389800	516961.774493	43.423924
3502.747594	516963.083521	43.428929
3502.969849	516966.891804	43.433933
3502.825118	516950.480317	43.438938
3502.602690	516938.632223	43.443943
3502.932258	516906.317906	43.448948
3502.897028	516925.590187	43.453953
3502.312771	516924.064599	43.458957
3502.935007	516903.486388	43.463962
3502.678408	516899.987417	43.468967
3502.540062	516891.969182	43.473972
3503.112780	516871.297621	43.478977
3502.897352	516879.271137	43.483981
3502.871815	516851.210006	43.488986
3502.707330	516846.027708	43.493991
3502.950589	516831.324670	43.498996
3502.737896	516833.886954	43.504001
3502.643393	516815.545794	43.509005
3502.687223	516790.153724	43.514010
3502.850935	516797.713372	43.519015
3502.744983	516796.718993	43.524020
3502.743558	516795.202408	43.529025
3502.901695	516762.712634	43.534029
3502.872960	516751.541751	43.539034
3502.425384	516767.339584	43.544039
3502.833978	516760.145071	43.549044
3503.048139	516746.103949	43.554049
3502.702838	516721.683517	43.559053
3502.877689	516715.537305	43.564058
3503.007216	516715.618214	43.569063
3502.949342	516709.609922	43.574068
3502.568737	516691.768966	43.579073
3502.660028	516679.415981	43.584077
3502.706584	516679.054884	43.589082
3502.570336	516686.560857	43.594087
3502.696748	516663.785121	43.599092
3502.769406	516645.113938	43.604097
3502.609805	516647.111599	43.609101
3502.715822	516637.486979	43.614106
3502.757735	516633.384509	43.619111
3502.835831	516618.201698	43.624116
3502.437621	516601.678223	43.629121
3502.393986	516601.988780	43.634125
3502.581544	516597.509297	43.639130
3502.696929	516602.851630	43.644135
3502.557390	516592.203845	43.649140
3502.786155	516600.410699	43.654145
3502.403183	516582.671138	43.659149
3502.638488	516548.955088	43.664154
3502.533131	516557.518191	43.669159
3502.512313	516559.392788	43.674164
3502.700428	516561.992900	43.679169
3502.453171	516559.554333	43.684173
3502.382072	516552.030998	43.689178
3502.285486	516556.496603	43.694183
3502.557212	516539.867176	43.699188
3502.427280	516520.368196	43.704193
3502.265522	516527.220871	43.709197
3502.719689	516509.298343	43.714202
3502.612112	516525.346082	43.719207
3502.457570	516525.067338	43.724212
3502.238351	516527.377853	43.729217
3502.462934	516523.853315	43.734221
3502.642443	516525.544545	43.739226
3502.521098	516514.590418	43.744231
3502.587178	516491.621704	43.749236
3502.844265	516487.030063	43.754241
3502.313255	516478.365720	43.759245
3502.584037	516480.598792	43.764250
3502.635621	516479.276076	43.769255
3502.728275	516470.563722	43.774260
3502.839830	516446.525799	43.779265
3502.387238	516447.103276	43.784269
3502.961476	516439.022761	43.789274
3502.718285	516444.371252	43.794279
3502.624080	516429.063794	43.799284
3502.838635	516415.376318	43.804289
3502.618217	516399.532514	43.809293
3502.783403	516399.152662	43.814298
3502.553673	516415.169245	43.819303
3502.715775	516403.613976	43.824308
3502.759681	516378.423543	43.829313
3502.637572	516366.407474	43.834317
3502.844510	516347.461883	43.839322
3502.669145	516355.277606	43.844327
3502.617564	516348.610781	43.849332
3503.004721	516331.103212	43.854337
3503.105285	516318.647353	43.859341
3503.182049	516311.505096	43.864346
3502.794454	516301.402032	43.869351
3502.864420	516275.398203	43.874356
3503.227544	516276.554735	43.879361
3502.661775	516262.231920	43.884365
3502.974845	516228.604069	43.889370
3502.750259	516234.607101	43.894375
3502.516810	516235.655649	43.899380
3503.143767	516233.281136	43.904385
3502.916811	516212.128312	43.909389
3502.963918	516189.061039	43.914394
3503.004086	516182.531356	43.919399
3502.778033	516169.520165	43.924404
3503.000797	516159.876815	43.929409
3502.759068	516150.964294	43.934413
3502.997464	516122.708503	43.939418
3502.914179	516124.137888	43.944423
3502.669952	516108.550423	43.949428
3503.054747	516098.426292	43.954433
3502.730142	516099.388115	43.959437
3502.837906	516070.950602	43.964442
3502.624957	516061.224352	43.969447
3502.754001	516057.917100	43.974452
3502.917894	516059.813129	43.979457
3502.800502	516045.722680	43.984461
3503.033838	516032.739913	43.989466
3503.000518	516017.422451	43.994471
3502.854132	516019.367527	43.999476
3503.123602	515991.258314	44.004481
3503.201760	515991.195635	44.009485
3502.919414	515971.871814	44.014490
3502.806731	515951.914301	44.019495
3502.733451	515937.867359	44.024500
3502.700214	515926.544920	44.029505
3502.711685	515942.574404	44.034509
3502.730868	515920.927163	44.039514
3502.713595	515911.726180	44.044519
3502.640111	515895.454102	44.049524
3502.725236	515897.514313	44.054529
3502.765213	515901.098798	44.059533
3502.979355	515881.696397	44.064538
3502.424980	515868.180581	44.069543
3502.735841	515848.358283	44.074548
3502.949629	515845.341023	44.079553
3502.695091	515851.399497	44.084557
3502.844689	515830.894669	44.089562
3502.773662	515812.801548	44.094567
3502.927439	515815.761206	44.099572
3502.757580	515813.967724	44.104577
3502.463107	515788.931026	44.109581
3503.075838	515779.579820	44.114586
3502.612982	515777.326929	44.119591
3502.888761	515762.162663	44.124596
3503.020692	515750.358852	44.129601
3502.669311	515744.346031	44.134605
3502.810951	515723.538898	44.139610
3502.863198	515723.429741	44.144615
3502.807453	515718.634476	44.149620
3502.782909	515706.501364	44.154625
3502.971520	515688.063639	44.159629
3503.246047	515683.671308	44.164634
3503.147518	515682.523973	44.169639
3503.255989	515647.308987	44.174644
3503.145350	515632.812545	44.179649
3502.566441	515620.969282	44.184653
3503.119758	515601.158940	44.189658
3503.351989	515596.823845	44.194663
3502.974759	515578.627152	44.199668
3502.831717	515565.046072	44.204673
3502.629403	515567.101186	44.209677
3503.001090	515547.673495	44.214682
3502.683233	515536.193488	44.219687
3502.918767	515512.589771	44.224692
3502.997927	515515.763566	44.229697
3502.792860	515504.872579	44.234701
3502.908285	515468.948103	44.239706
3502.789410	515472.001490	44.244711
3503.154619	515461.121481	44.249716
3502.872903	515451.304598	44.254721
3502.645199	515427.167109	44.259725
3502.882320	515411.300617	44.264730
3502.766846	515429.171278	44.269735
3502.796543	515417.585682	44.274740
3503.078730	515387.956261	44.279745
3502.871962	515389.152362	44.284749
3502.849670	515381.216199	44.289754
3502.839116	515371.659846	44.294759
3502.805111	515361.500319	44.299764
3502.651076	515358.237673	44.304769
3502.461818	515356.042625	44.309773
3502.800065	515347.341438	44.314778
3502.844079	515338.787899	44.319783
3502.707063	515324.952806	44.324788
3502.823223	515302.176828	44.329793
3502.461705	515311.843094	44.334797
3502.756735	515307.447425	44.339802
3502.848702	515294.385282	44.344807
3502.711675	515274.228512	44.349812
3502.742692	515266.031002	44.354817
3502.630894	515271.359100	44.359821
3502.503159	515252.970896	44.364826
3502.119240	515272.805938	44.369831
3502.685480	515254.965496	44.374836
3502.508127	515236.635690	44.379841
3502.337883	515230.037745	44.384845
3502.676785	515222.246709	44.389850
3502.545419	515217.918413	44.394855
3502.876974	515215.236439	44.399860
3502.647439	515223.668134	44.404865
3502.700296	515218.198107	44.409869
3502.861303	515189.598955	44.414874
3502.429710	515184.357209	44.419879
3502.508348	515181.664633	44.424884
3502.910971	515174.318664	44.429889
3502.852095	515173.316746	44.434893
3502.940033	515148.926669	44.439898
3502.630063	515138.810626	44.444903
3502.329084	515124.900136	44.449908
3502.724397	515133.384833	44.454913
3502.651750	515139.617109	44.459917
3502.997206	515118.726433	44.464922
3502.739062	515106.478087	44.469927
3503.063447	515100.712235	44.474932
3502.704191	515098.392301	44.479937
3502.596363	515069.177977	44.484941
3502.858169	515047.288958	44.489946
3502.235545	515045.263515	44.494951
3502.596362	515045.156155	44.499956
3502.729759	515047.613433	44.504961
3502.401964	515054.998693	44.509965
3502.836588	515037.836284	44.514970
3502.241456	515022.050395	44.519975
3502.341867	515004.435039	44.524980
3502.445007	515009.628099	44.529985
3502.425587	515011.603797	44.534989
3502.650048	514996.851539	44.539994
3502.493519	515007.193616	44.544999
3502.641243	515009.496913	44.550004
3502.736977	515001.187896	44.555009
3502.370802	514977.021068	44.560013
3502.921489	514956.755213	44.565018
3502.665142	514961.752239	44.570023
3502.384501	514957.599191	44.575028
3502.918038	514958.880606	44.580033
3502.654869	514953.612166	44.585037
3502.927536	514921.606439	44.590042
3502.624687	514928.279774	44.595047
3502.741165	514918.652508	44.600052
3502.671720	514909.256921	44.605057
3502.671360	514900.103281	44.610061
3502.777605	514878.086906	44.615066
3502.563353	514882.065814	44.620071
3502.694594	514872.891358	44.625076
3502.747603	514872.579778	44.630081
3502.531161	514864.977503	44.635085
3502.720296	514845.426129	44.640090
3502.390424	514842.646344	44.645095
3502.718307	514837.284445	44.650100
3503.128222	514826.498107	44.655105
3502.697452	514823.177948	44.660109
3503.023555	514804.666941	44.665114
3502.666462	514785.758155	44.670119
3502.867596	514792.402457	44.675124
3502.891277	514781.373691	44.680129
3502.605696	514762.200702	44.685133
3502.669251	514754.149522	44.690138
3502.619265	514754.258817	44.695143
3502.973247	514755.315755	44.700148
3502.793254	514739.716855	44.705153
3502.119894	514725.814316	44.710157
3502.615069	514705.658082	44.715162
3502.488489	514705.172586	44.720167
3502.698281	514709.792558	44.725172
3502.872598	514700.965223	44.730177
3502.639452	514715.820753	44.735181
3502.822290	514689.644887	44.740186
3502.249991	514684.273498	44.745191
3502.715269	514685.009399	44.750196
3502.908727	514667.783581	44.755201
3502.548970	514674.466010	44.760205
3502.524183	514675.380522	44.765210
3502.956255	514662.719304	44.770215
3502.678072	514638.993253	44.775220
3502.924382	514641.533894	44.780225
3502.746985	514640.702402	44.785229
3502.836853	514609.584749	44.790234
3502.428790	514611.166747	44.795239
3502.586821	514589.293533	44.800244
3502.872576	514583.735911	44.805249
3502.502322	514589.206228	44.810253
3502.771470	514586.938621	44.815258
3502.660427	514561.011306	44.820263
3502.663273	514556.509898	44.825268
3502.686349	514548.616744	44.830273
3502.459136	514549.411533	44.835277
3502.735276	514540.669170	44.840282
3502.027424	514541.944532	44.845287
3502.350936	514549.227068	44.850292
3502.337122	514546.194975	44.855297
3502.277768	514544.333314	44.860301
3502.352242	514521.006532	44.865306
3502.504230	514526.040295	44.870311
3502.310920	514517.624999	44.875316
3502.469767	514511.632234	44.880321
3502.195006	514518.857621	44.885325
3502.613028	514507.513467	44.890330
3502.642772	514503.462973	44.895335
3502.552142	514514.755871	44.900340
3503.050452	514506.332402	44.905345
3502.541640	514487.497833	44.910349
3502.731545	514468.047048	44.915354
3502.338112	514465.530124	44.920359
3502.525959	514455.537282	44.925364
3502.719748	514468.555403	44.930369
3502.784577	514461.110788	44.935373
3503.230722	514446.778187	44.940378
3502.489690	514436.831003	44.945383
3502.846882	514427.317135	44.950388
3502.783476	514425.253798	44.955393
3502.390984	514401.343174	44.960397
3502.582749	514378.756292	44.965402
3502.380201	514394.163605	44.970407
3502.536891	514375.274295	44.975412
3502.421574	514378.327319	44.980417
3502.096542	514390.719443	44.985421
3502.667970	514377.378498	44.990426
3502.494583	514381.249913	44.995431
3502.644950	514383.350576	45.000436
3502.791731	514364.260517	45.005441
3502.608783	514342.997212	45.010445
3502.378154	514337.875161	45.015450
3502.271390	514336.526730	45.020455
3502.520526	514333.200157	45.025460
3502.633653	514349.569134	45.030465
3502.408016	514347.025670	45.035469
3502.566138	514347.203226	45.040474
3502.315739	514326.709201	45.045479
3502.593532	514311.340998	45.050484
3502.655819	514295.703388	45.055489
3502.268633	514308.762886	45.060493
3502.782950	514303.978263	45.065498
3502.779591	514301.905419	45.070503
3502.684891	514293.373271	45.075508
3502.727161	514269.393740	45.080513
3502.516043	514270.843488	45.085517
3502.809345	514251.628989	45.090522
3502.881304	514253.033995	45.095527
3502.785331	514248.649276	45.100532
3502.414891	514220.486503	45.105537
3502.570126	514216.163222	45.110541
3502.509069	514212.127009	45.115546
3502.136789	514220.986381	45.120551
3502.562090	514209.387995	45.125556
3502.408688	514208.653841	45.130561
3502.154229	514214.915198	45.135565
3502.679698	514208.763224	45.140570
3502.667185	514216.756511	45.145575
3502.417037	514191.760985	45.150580
3502.570516	514183.442436	45.155585
3502.546771	514177.073800	45.160589
3502.876492	514174.948294	45.165594
3502.946931	514173.268382	45.170599
3502.821762	514161.453511	45.175604
3502.600110	514141.460480	45.180609
3502.464185	514137.385507	45.185613
3502.490026	514135.763216	45.190618
3502.654773	514130.022266	45.195623
3502.312107	514136.803360	45.200628
3502.421295	514131.880417	45.205633
3502.650179	514133.564088	45.210637
3502.699144	514119.091681	45.215642
3502.290281	514112.379280	45.220647
3502.492163	514093.482511	45.225652
3502.638839	514081.523462	45.230657
3502.342467	514096.136651	45.235661
3502.533845	514076.988639	45.240666
3502.516257	514087.916242	45.245671
3502.470066	514090.199741	45.250676
3502.429715	514087.121183	45.255681
3502.608335	514060.995579	45.260685
3502.861568	514055.898115	45.265690
3502.937098	514051.890852	45.270695
3502.790374	514050.548713	45.275700
3502.923449	514037.327362	45.280705
3502.508210	514032.032089	45.285709
3502.418824	514027.494541	45.290714
3502.364170	514019.461693	45.295719
3502.555028	514018.217924	45.300724
3502.519278	514028.136897	45.305729
3502.660965	514024.372055	45.310733
3502.834333	514014.128355	45.315738
3502.602434	513991.911379	45.320743
3502.401018	513980.563626	45.325748
3502.645283	513968.133878	45.330753
3502.497871	513975.440523	45.335757
3502.545580	513978.720737	45.340762
3502.349880	513981.533652	45.345767
3502.433280	513965.285472	45.350772
3502.759940	513950.364410	45.355777
3502.258423	513937.597325	45.360781
3502.632517	513931.317445	45.365786
3502.500224	513936.952669	45.370791
3502.689883	513943.548546	45.375796
3502.796040	513932.759072	45.380801
3502.828233	513931.338066	45.385805
3502.881503	513904.321642	45.390810
3502.633766	513893.739811	45.395815
3502.299462	513896.726381	45.400820
3502.544579	513888.393201	45.405825
3502.579755	513898.301041	45.410829
3502.684109	513885.488728	45.415834
3502.293931	513872.653417	45.420839
3502.551710	513850.207122	45.425844
3502.510814	513851.124225	45.430849
3502.486629	513855.882572	45.435853
3502.437404	513851.035163	45.440858
3502.521020	513843.334418	45.445863
3502.311781	513851.763593	45.450868
3502.584761	513849.394128	45.455873
3502.259891	513835.233452	45.460877
3502.694854	513816.602995	45.465882
3502.013081	513812.917685	45.470887
3502.000038	513814.740784	45.475892
3502.529065	513805.098249	45.480897
3502.542263	513809.951855	45.485901
3502.780691	513808.902863	45.490906
3502.635210	513805.992603	45.495911
3502.411797	513797.227659	45.500916
3502.517970	513814.306345	45.505921
3502.345795	513816.660371	45.510925
3502.895709	513791.537790	45.515930
3502.524924	513794.327833	45.520935
3502.644228	513778.832462	45.525940
3502.463503	513773.854083	45.530945
3502.384015	513786.966506	45.535949
3502.803066	513766.770602	45.540954
3502.462356	513777.243703	45.545959
3502.701613	513753.384032	45.550964
3502.757057	513725.608310	45.555969
3502.354879	513741.098353	45.560973
3502.713332	513721.114284	45.565978
3502.732553	513733.958257	45.570983
3502.693057	513731.486432	45.575988
3503.006427	513706.906891	45.580993
3502.506797	513691.913893	45.585997
3503.030615	513688.897822	45.591002
3502.600619	513690.432793	45.596007
3502.627587	513673.788628	45.601012
3502.779811	513655.961353	45.606017
3502.349779	513646.773787	45.611021
3502.490277	513647.662229	45.616026
3502.567060	513642.390218	45.621031
3502.315003	513643.745334	45.626036
3502.573085	513650.633980	45.631041
3502.778428	513643.925464	45.636045
3502.837047	513617.362936	45.641050
3502.641587	513604.597798	45.646055
3502.592878	513593.579693	45.651060
3502.440323	513602.657550	45.656065
3502.364665	513604.895194	45.661069
3502.581522	513597.223854	45.666074
3502.666611	513580.317519	45.671079
3502.625145	513566.567025	45.676084
3502.769316	513566.645639	45.681089
3502.301551	513558.526132	45.686093
3502.595637	513551.752974	45.691098
3502.445138	513554.862286	45.696103
3502.862818	513549.738677	45.701108
3502.726456	513530.793582	45.706113
3502.596901	513513.263587	45.711117
3502.806271	513516.619495	45.716122
3502.682991	513516.841540	45.721127
3502.596317	513518.018788	45.726132
3502.515408	513485.105219	45.731137
3502.692615	513478.552820	45.736141
3502.623071	513474.062564	45.741146
3502.415929	513475.511750	45.746151
3502.615626	513470.068522	45.751156
3502.563207	513476.399376	45.756161
3502.391679	513480.624753	45.761165
3502.734034	513463.475323	45.766170
3502.628230	513441.338844	45.771175
3502.624371	513435.270256	45.776180
3502.437318	513434.490807	45.781185
3502.242788	513430.778976	45.786189
3502.558240	513434.421605	45.791194
3502.205633	513441.052813	45.796199
3502.114221	513436.414268	45.801204
3502.138038	513431.201141	45.806209
3501.987353	513432.691986	45.811213
3502.322759	513433.043846	45.816218
3502.662659	513433.243259	45.821223
3502.394510	513439.962276	45.826228
3502.324329	513430.414239	45.831233
3502.299040	513416.559908	45.836237
3502.450355	513401.059130	45.841242
3502.080191	513408.300072	45.846247
3502.310519	513409.376644	45.851252
3502.531259	513392.650994	45.856257
3502.049768	513406.282464	45.861261
3502.347684	513402.897419	45.866266
3502.661084	513405.528803	45.871271
3502.657033	513400.067179	45.876276
3502.613693	513400.883535	45.881281
3502.600403	513400.228356	45.886285
3502.455083	513393.271694	45.891290
3502.434054	513384.373387	45.896295
3502.711003	513369.965457	45.901300
3502.691546	513374.217404	45.906305
3502.325692	513367.953115	45.911309
3502.452032	513370.007125	45.916314
3502.299341	513373.268553	45.921319
3502.361715	513368.909154	45.926324
3502.339411	513372.402868	45.931329
3502.348723	513370.783117	45.936333
3502.354652	513367.950006	45.941338
3502.453995	513351.951608	45.946343
3502.441519	513329.142704	45.951348
3502.982594	513327.236581	45.956353
3502.392764	513329.100321	45.961357
3502.368534	513327.587025	45.966362
3502.391871	513334.512905	45.971367
3502.489687	513321.144828	45.976372
3502.291253	513324.615812	45.981377
3502.369399	513327.739604	45.986381
3502.417848	513319.437230	45.991386
3502.322764	513320.362926	45.996391
3502.381748	513310.996722	46.001396
3502.447189	513299.454591	46.006401
3502.408200	513280.999615	46.011405
3502.058422	513283.027733	46.016410
3502.217645	513281.536015	46.021415
3502.132485	513282.004933	46.026420
3502.416917	513277.812729	46.031425
3502.417476	513290.407094	46.036429
3502.215689	513281.840779	46.041434
3502.289924	513288.354000	46.046439
3502.247615	513289.827727	46.051444
3502.727728	513281.710000	46.056449
3502.496866	513286.450597	46.061453
3502.878869	513285.935249	46.066458
3502.634597	513279.297655	46.071463
3502.408950	513260.922739	46.076468
3502.653731	513251.830611	46.081473
3502.383409	513251.064315	46.086477
3502.677125	513243.582983	46.091482
3502.532785	513246.236164	46.096487
3502.338753	513250.009943	46.101492
3502.536410	513241.633367	46.106497
3502.338512	513226.541680	46.111501
3502.133810	513216.053778	46.116506
3502.086342	513215.201676	46.121511
3502.498266	513217.210565	46.126516
3502.451389	513210.390005	46.131521
3502.459088	513209.630343	46.136525
3502.725082	513204.530606	46.141530
3502.451578	513211.756353	46.146535
3502.411810	513202.405698	46.151540
3502.479846	513200.877807	46.156545
3502.625171	513205.862441	46.161549
3502.304777	513189.677337	46.166554
3502.311690	513165.701819	46.171559
3502.337702	513171.109959	46.176564
3502.471324	513159.911012	46.181569
3502.335614	513167.873691	46.186573
3502.585809	513154.380236	46.191578
3502.513933	513165.468758	46.196583
3502.285803	513167.022447	46.201588
3502.417437	513162.955524	46.206593
3502.549815	513172.342633	46.211597
3502.551024	513169.055020	46.216602
3502.302263	513160.344328	46.221607
3502.482893	513139.730144	46.226612
3502.752519	513120.568676	46.231617
3502.312683	513126.556260	46.236621
3502.500952	513123.846026	46.241626
3502.349752	513123.263214	46.246631
3502.273914	513127.675874	46.251636
3502.548724	513124.749643	46.256641
3502.178679	513132.445900	46.261645
3502.483790	513123.546485	46.266650
3502.423703	513128.816508	46.271655
3502.387917	513128.013136	46.276660
3502.518239	513100.578604	46.281665
3502.233415	513095.161260	46.286669
3502.400269	513093.516581	46.291674
3502.499018	513091.730926	46.296679
3502.395837	513090.027769	46.301684
3502.525275	513083.583927	46.306689
3502.447979	513091.790308	46.311693
3502.603267	513079.778607	46.316698
3502.427108	513100.847866	46.321703
3502.770221	513082.231116	46.326708
3502.744031	513069.742296	46.331713
3502.603187	513062.026092	46.336717
3502.758297	513048.699322	46.341722
3502.763650	513051.177134	46.346727
3502.637726	513046.847415	46.351732
3502.351317	513011.183507	46.356737
3502.561647	513009.279048	46.361741
3502.540945	512996.081185	46.366746
3502.462454	513000.393137	46.371751
3502.399855	512994.890055	46.376756
3502.650065	512999.757013	46.381761
3502.377294	512999.850952	46.386765
3502.674003	512991.003375	46.391770
3502.611501	512984.084033	46.396775
3502.385263	512962.168280	46.401780
3502.192908	512967.206360	46.406785
3502.420278	512966.108484	46.411789
3502.509031	512962.351772	46.416794
3502.507834	512970.950824	46.421799
3502.370977	512955.292865	46.426804
3502.255200	512967.602379	46.431809
3502.154962	512963.976700	46.436813
3502.345634	512962.378823	46.441818
3502.308432	512970.376605	46.446823
3502.212605	512967.357190	46.451828
3502.245780	512967.301612	46.456833
3502.203194	512968.876571	46.461837
3502.616603	512963.247660	46.466842
3502.400114	512974.106264	46.471847
3502.201856	512949.100686	46.476852
3502.311400	512937.298435	46.481857
3502.077862	512928.028835	46.486861
3502.198160	512930.994298	46.491866
3502.109328	512932.273089	46.496871
3502.309239	512935.377708	46.501876
3502.529895	512927.654884	46.506881
3502.015791	512931.428745	46.511885
3502.452018	512909.610534	46.516890
3502.419348	512934.197939	46.521895
3501.883829	512933.018324	46.526900
3502.231415	512926.641102	46.531905
3502.055196	512937.341624	46.536909
3502.483450	512936.161414	46.541914
3502.330613	512936.792779	46.546919
3502.340806	512931.935713	46.551924
3502.265674	512928.306058	46.556929
3502.058760	512935.116756	46.561933
3502.492632	512930.496204	46.566938
3502.308561	512930.272642	46.571943
3502.479624	512937.782299	46.576948
3502.504859	512929.786882	46.581953
3502.266155	512938.170591	46.586957
3502.364392	512930.821179	46.591962
3502.437211	512941.381175	46.596967
3502.543975	512923.964953	46.601972
3502.319979	512910.697996	46.606977
3502.236758	512899.988374	46.611981
3502.460135	512893.529611	46.616986
3502.650412	512890.313220	46.621991
3502.374226	512900.017960	46.626996
3502.676628	512887.932290	46.632001
3502.532793	512906.619405	46.637005
3502.536345	512898.829723	46.642010
3502.628629	512894.161992	46.647015
3502.637699	512878.329154	46.652020
3502.512656	512866.007549	46.657025
3502.400352	512863.547104	46.662029
3502.598371	512856.839434	46.667034
3502.658664	512854.048224	46.672039
3502.415154	512866.226261	46.677044
3502.771061	512855.801264	46.682049
3502.508395	512838.999732	46.687053
3502.684201	512826.327061	46.692058
3502.349926	512815.960551	46.697063
3502.787800	512821.758928	46.702068
3502.589110	512817.693554	46.707073
3502.324078	512821.276328	46.712077
3502.482049	512812.804651	46.717082
3502.667945	512831.439732	46.722087
3502.526552	512806.172051	46.727092
3502.521653	512789.633210	46.732097
3502.515446	512776.028239	46.737101
3502.189048	512776.231817	46.742106
3502.334232	512777.625373	46.747111
3502.567629	512782.292728	46.752116
3502.441438	512778.367627	46.757121
3502.440272	512790.406252	46.762125
3502.544975	512776.429686	46.767130
3502.626960	512778.490780	46.772135
3502.435234	512761.020408	46.777140
3502.661547	512744.090912	46.782145
3502.312157	512747.434132	46.787149
3502.574549	512750.326586	46.792154
3502.555158	512759.232107	46.797159
3502.613779	512752.951074	46.802164
3502.525097	512748.615392	46.807169
3502.072974	512729.162915	46.812173
3502.557953	512719.374984	46.817178
3502.805673	512707.095504	46.822183
3502.488556	512702.745335	46.827188
3502.735339	512709.636155	46.832193
3502.453095	512710.136239	46.837197
3502.547780	512700.561730	46.842202
3502.581847	512717.855250	46.847207
3502.667589	512676.820822	46.852212
3502.841099	512671.432057	46.857217
3502.566945	512670.767501	46.862221
3502.648714	512678.544293	46.867226
3502.883750	512672.488251	46.872231
3502.613474	512649.466270	46.877236
3502.441760	512623.545554	46.882241
3502.389041	512620.822750	46.887245
3502.835253	512618.425733	46.892250
3502.666301	512616.530599	46.897255
3502.542371	512627.880607	46.902260
3502.831985	512610.131673	46.907265
3502.405989	512595.783611	46.912269
3502.507757	512582.768392	46.917274
3502.816366	512574.272786	46.922279
3502.576705	512576.182419	46.927284
3502.804603	512575.236179	46.932289
3502.497141	512560.060050	46.937293
3502.931915	512544.564262	46.942298
3502.607956	512532.830249	46.947303
3502.545393	512528.540963	46.952308
3502.756738	512523.196752	46.957313
3502.587085	512527.118583	46.962317
3502.559259	512502.844125	46.967322
3502.665840	512495.847275	46.972327
3502.695850	512494.881728	46.977332
3502.837983	512483.782150	46.982337
3502.517100	512488.941851	46.987341
3502.616172	512470.818236	46.992346
3502.502177	512462.996350	46.997351
3502.621928	512444.920021	47.002356
3502.751101	512444.899848	47.007361
3502.521994	512447.617134	47.012365
3502.382539	512443.188235	47.017370
3502.674323	512447.188893	47.022375
3502.721573	512432.462399	47.027380
3502.654523	512417.855122	47.032385
3502.460503	512408.933062	47.037389
3502.914028	512401.476681	47.042394
3502.687750	512409.099960	47.047399
3502.659130	512389.833061	47.052404
3502.637554	512374.156340	47.057409
3502.395788	512363.724346	47.062413
3502.821175	512359.914291	47.067418
3502.587801	512363.390994	47.072423
3502.839047	512357.180532	47.077428
3502.793430	512348.133819	47.082433
3502.360129	512333.129121	47.087437
3502.638174	512319.276525	47.092442
3502.376550	512323.718760	47.097447
3502.520225	512318.840419	47.102452
3502.822903	512311.407842	47.107457
3502.406283	512317.088547	47.112461
3502.556800	512300.575244	47.117466
3502.467872	512284.251518	47.122471
3502.621182	512276.184967	47.127476
3502.654944	512267.631485	47.132481
3502.420501	512271.462451	47.137485
3502.743513	512263.014995	47.142490
3502.855445	512262.491725	47.147495
3502.568906	512247.312007	47.152500
3502.850851	512228.501658	47.157505
3502.398050	512237.020718	47.162509
3502.386438	512229.384871	47.167514
3502.534224	512220.813343	47.172519
3502.590276	512233.956131	47.177524
3502.656334	512220.845114	47.182529
3502.646071	512209.263621	47.187533
3502.362447	512189.986218	47.192538
3502.572039	512187.930036	47.197543
3502.202855	512189.253196	47.202548
3502.736870	512177.433905	47.207553
3501.913895	512190.867415	47.212557
3502.542585	512174.430155	47.217562
3502.322611	512192.472522	47.222567
3502.576662	512188.031939	47.227572
3502.421104	512168.380192	47.232577
3502.422193	512158.617840	47.237581
3502.204895	512141.859024	47.242586
3502.323397	512156.104819	47.247591
3502.091416	512146.379299	47.252596
3502.417295	512146.580948	47.257601
3502.471883	512145.459748	47.262605
3502.416010	512148.149700	47.267610
3502.333997	512142.902321	47.272615
3502.190818	512143.481605	47.277620
3502.477059	512141.615634	47.282625
3502.325709	512150.137672	47.287629
3502.611484	512134.715644	47.292634
3502.321591	512144.271235	47.297639
3502.347981	512150.691294	47.302644
3502.534729	512140.140848	47.307649
3502.487399	512122.596408	47.312653
3502.542522	512106.401490	47.317658
3502.407279	512113.656433	47.322663
3502.684180	512110.729699	47.327668
3502.666349	512107.444888	47.332673
3502.381191	512115.532850	47.337677
3502.711069	512099.850906	47.342682
3502.741902	512096.052574	47.347687
3502.605576	512081.810036	47.352692
3502.819816	512071.761029	47.357697
3502.550108	512071.652156	47.362701
3502.939266	512077.407909	47.367706
3502.853765	512049.550539	47.372711
3502.804067	512036.862339	47.377716
3502.961240	512026.114165	47.382721
3502.201408	512031.039887	47.387725
3502.554226	512030.680867	47.392730
3502.592540	512016.815333	47.397735
3502.443488	511999.033930	47.402740
3502.331589	511988.985841	47.407745
3502.478538	511989.923936	47.412749
3502.541891	511990.419997	47.417754
3502.214042	511982.682274	47.422759
3502.593131	511993.548535	47.427764
3502.510810	511984.962677	47.432769
3502.478659	511995.135192	47.437773
3502.564917	511985.966275	47.442778
3502.658741	511967.235954	47.447783
3502.306199	511961.727780	47.452788
3502.728792	511939.961059	47.457793
3502.524585	511948.693886	47.462797
3502.494211	511940.959707	47.467802
3502.466562	511941.773653	47.472807
3502.364354	511950.642106	47.477812
3502.672535	511941.842753	47.482817
3502.226845	511924.057574	47.487821
3502.451125	511917.497131	47.492826
3502.452576	511909.403825	47.497831
3502.551258	511898.209565	47.502836
3502.260052	511912.924991	47.507841
3502.537093	511904.079956	47.512845
3502.510364	511904.135009	47.517850
3502.604314	511905.182653	47.522855
3502.667283	511911.647604	47.527860
3502.664398	511882.866403	47.532865
3502.506178	511867.564894	47.537869
3502.289775	511869.420346	47.542874
3502.260238	511856.931158	47.547879
3502.167533	511868.833157	47.552884
3502.699090	511863.589876	47.557889
3502.529373	511859.367940	47.562893
3502.703705	511860.655798	47.567898
3502.494654	511859.930335	47.572903
3502.294035	511862.592627	47.577908
3502.668017	511827.631170	47.582913
3502.460111	511826.753774	47.587917
3502.603777	511821.571791	47.592922
3502.370993	511816.550476	47.597927
3502.359360	511830.817114	47.602932
3502.527839	511825.125375	47.607937
3502.510872	511817.996024	47.612941
3502.413624	511815.229545	47.617946
3502.430065	511817.705785	47.622951
3502.320567	511787.221432	47.627956
3502.716664	511779.925607	47.632961
3502.467850	511777.638332	47.637965
3502.377174	511771.886370	47.642970
3502.115162	511768.994175	47.647975
3502.499608	511766.353885	47.652980
3502.504834	511768.073150	47.657985
3502.276798	511784.700881	47.662989
3502.629530	511768.306848	47.667994
3502.310823	511767.952799	47.672999
3502.318294	511780.850700	47.678004
3502.586535	511759.664565	47.683009
3502.598608	511747.522805	47.688013
3502.814722	511737.169801	47.693018
3502.848862	511734.382541	47.698023
3502.352961	511732.134314	47.703028
3502.964669	511723.995045	47.708033
3502.358041	511711.698133	47.713037
3502.774936	511681.130387	47.718042
3502.598478	511683.637136	47.723047
3502.601918	511688.695231	47.728052
3502.615517	511688.187487	47.733057
3502.394189	511687.362789	47.738061
3502.648173	511683.023253	47.743066
3502.622148	511664.260957	47.748071
3502.116001	511655.033745	47.753076
3502.615834	511646.507450	47.758081
3502.288312	511653.489478	47.763085
3502.425089	511647.650939	47.768090
3502.541848	511646.469295	47.773095
3502.350028	511650.698335	47.778100
3502.677181	511641.996996	47.783105
3502.548409	511635.644001	47.788109
3502.851167	511607.168110	47.793114
3503.079879	511607.840382	47.798119
3502.741988	511606.123589	47.803124
3502.829813	511598.067066	47.808129
3502.328906	511584.387577	47.813133
3502.499973	511570.652447	47.818138
3502.138169	511565.550282	47.823143
3502.463282	511563.425183	47.828148
3502.409109	511571.780398	47.833153
3502.532352	511564.578194	47.838157
3502.494384	511559.475425	47.843162
3502.071334	511562.223506	47.848167
3502.469417	511562.059661	47.853172
3502.548772	511563.666060	47.858177
3502.438234	511565.504812	47.863181
3502.630791	511546.151408	47.868186
3502.366908	511525.807855	47.873191
3502.044679	511525.403772	47.878196
3502.599407	511519.600295	47.883201
3502.430690	511517.350908	47.888205
3502.684721	511515.793467	47.893210
3502.457217	511525.592467	47.898215
3502.708287	511530.105624	47.903220
3502.935728	511521.925828	47.908225
3502.295148	511499.264317	47.913229
3502.570598	511475.395709	47.918234
3502.580299	511485.865423	47.923239
3502.560078	511479.545796	47.928244
3502.555382	511473.476635	47.933249
3502.567839	511475.650047	47.938253
3502.636852	511477.713351	47.943258
3502.797386	511441.267300	47.948263
3502.904980	511443.830356	47.953268
3503.134939	511420.424124	47.958273
3502.541310	511424.564976	47.963277
3502.640469	511408.210676	47.968282
3502.567346	511399.319558	47.973287
3502.506795	511401.808028	47.978292
3502.622539	511394.556352	47.983297
3502.342531	511409.422198	47.988301
3502.542334	511408.885014	47.993306
3502.638022	511399.056687	47.998311
3502.595255	511396.787375	48.003316
3502.793151	511357.300150	48.008321
3502.127393	511365.499211	48.013325
3502.558661	511357.843553	48.018330
3502.447168	511359.227213	48.023335
3502.447428	511364.032983	48.028340
3502.520037	511365.084034	48.033345
3502.276682	511358.647876	48.038349
3502.457851	511355.280880	48.043354
3502.195787	511331.547616	48.048359
3502.170265	511322.800688	48.053364
3502.156396	511326.192321	48.058369
3501.966875	511343.421418	48.063373
3502.265252	511342.818066	48.068378
3502.524053	511347.026540	48.073383
3502.572009	511338.520931	48.078388
3502.576453	511318.286472	48.083393
3502.604029	511323.543201	48.088397
3502.596671	511312.314731	48.093402
3502.644196	511321.261015	48.098407
3502.530423	511325.781310	48.103412
3502.797820	511310.310854	48.108417
3502.479968	511290.279059	48.113421
3502.845632	511280.913842	48.118426
3502.721303	511278.606821	48.123431
3502.458669	511273.488893	48.128436
3502.902611	511272.306093	48.133441
3502.401709	511251.645579	48.138445
3502.674212	511231.925084	48.143450
3502.649651	511222.672100	48.148455
3502.552287	511220.714907	48.153460
3502.673662	511227.120302	48.158465
3502.435845	511234.796516	48.163469
3502.569610	511209.432372	48.168474
3502.564409	511196.837679	48.173479
3502.268271	511194.304877	48.178484
3502.562778	511186.569588	48.183489
3502.352545	511189.537017	48.188493
3502.844264	511183.793972	48.193498
3502.412942	511183.862393	48.198503
3502.239885	511192.944782	48.203508
3502.667484	511173.098533	48.208513
3502.378577	511175.774888	48.213517
3502.389680	511154.325129	48.218522
3502.485197	511151.730414	48.223527
3502.327771	511134.910552	48.228532
3502.444170	511148.854013	48.233537
3502.190039	511149.552039	48.238541
3502.595685	511143.316729	48.243546
3502.671536	511135.970078	48.248551
3502.265880	511150.400740	48.253556
3502.790280	511130.640312	48.258561
3502.327088	511129.550301	48.263565
3502.386703	511111.937326	48.268570
3502.967066	511102.791004	48.273575
3502.758440	511105.859365	48.278580
3502.712092	511094.434571	48.283585
3502.457435	511105.755675	48.288589
3502.612841	511084.687705	48.293594
3502.455924	511072.167487	48.298599
3502.506134	511065.634230	48.303604
3502.714128	511054.270379	48.308609
3502.498896	511065.130006	48.313613
3502.619212	511049.682561	48.318618
3502.778352	511064.479295	48.323623
3502.605135	511033.548387	48.328628
3502.707902	511022.504662	48.333633
3502.328152	511020.187393	48.338637
3502.384491	511000.247867	48.343642
3502.445553	511002.312486	48.348647
3502.475785	511004.179633	48.353652
3502.601112	511002.693075	48.358657
3502.886542	511006.492738	48.363661
3502.982958	510985.737486	48.368666
3502.570082	510987.017055	48.373671
3502.405069	510967.112478	48.378676
3502.621751	510961.918693	48.383681
3502.481979	510977.622713	48.388685
3502.788604	510955.013099	48.393690
3502.549561	510939.824699	48.398695
3502.349995	510930.750976	48.403700
3502.548866	510918.629684	48.408705
3502.387966	510926.091534	48.413709
3502.523582	510916.307204	48.418714
3502.415438	510923.710130	48.423719
3502.391359	510927.356387	48.428724
3502.486230	510924.154706	48.433729
3502.149418	510940.142836	48.438733
3502.586720	510912.251549	48.443738
3502.344572	510892.257904	48.448743
3502.249042	510891.008591	48.453748
3502.337778	510877.134156	48.458753
3502.519810	510879.432600	48.463757
3502.680631	510879.002735	48.468762
3502.478912	510878.579587	48.473767
3502.568752	510884.585405	48.478772
3502.675988	510868.988104	48.483777
3502.298543	510888.220233	48.488781
3502.609166	510859.235983	48.493786
3502.177610	510848.883639	48.498791
3502.216385	510835.269999	48.503796
3502.138788	510833.157877	48.508801
3502.108644	510842.824901	48.513805
3502.317522	510835.507680	48.518810
3502.277832	510826.358045	48.523815
3502.477823	510848.989415	48.528820
3502.454955	510835.587865	48.533825
3502.316176	510844.715607	48.538829
3502.177029	510838.869818	48.543834
3502.316374	510842.136157	48.548839
3502.106007	510834.531097	48.553844
3502.354245	510828.118208	48.558849
3502.079815	510829.780597	48.563853
3502.184565	510834.114722	48.568858
3502.218984	510843.265677	48.573863
3502.415832	510843.083048	48.578868
3502.599138	510831.722950	48.583873
3502.168500	510844.387292	48.588877
3502.491497	510839.126079	48.593882
3502.636720	510839.508061	48.598887
3502.218251	510833.099382	48.603892
3502.226147	510819.996476	48.608897
3502.487860	510804.577045	48.613901
3502.487459	510789.148444	48.618906
3502.484949	510794.663025	48.623911
3502.150340	510801.292415	48.628916
3502.401052	510782.890096	48.633921
3502.143384	510794.970681	48.638925
3502.372116	510789.269073	48.643930
3502.412813	510793.663920	48.648935
3502.456101	510811.564968	48.653940
3502.556135	510792.933543	48.658945
3502.338445	510805.614841	48.663949
3502.346529	510804.905596	48.668954
3502.127597	510800.134722	48.673959
3502.024689	510805.311063	48.678964
3502.603213	510798.947130	48.683969
3502.369601	510792.964496	48.688973
3502.279927	510760.654048	48.693978
3502.564146	510756.461259	48.698983
3502.264158	510753.423131	48.703988
3502.517529	510753.180981	48.708993
3502.166742	510744.383994	48.713997
3502.213488	510748.170855	48.719002
3502.680036	510749.817305	48.724007
3502.388064	510756.187039	48.729012
3502.554375	510740.782631	48.734017
3502.388674	510749.813506	48.739021
3502.476342	510753.088031	48.744026
3502.388212	510753.304552	48.749031
3502.299197	510733.944144	48.754036
3502.470773	510704.222807	48.759041
3501.977620	510706.375062	48.764045
3502.279747	510696.918394	48.769050
3502.262635	510697.933081	48.774055
3502.016431	510703.739145	48.779060
3502.613282	510696.866409	48.784065
3502.334446	510706.471646	48.789069
3502.370351	510707.983821	48.794074
3502.573214	510696.468782	48.799079
3502.530709	510700.775630	48.804084
3502.801067	510690.008721	48.809089
3502.435128	510698.464231	48.814093
3502.281703	510692.064191	48.819098
3502.456477	510688.242793	48.824103
3502.162698	510674.529828	48.829108
3502.300460	510657.055791	48.834113
3502.475742	510667.044554	48.839117
3502.336662	510661.097518	48.844122
3502.508678	510659.552964	48.849127
3502.169618	510661.832629	48.854132
3502.298133	510650.126962	48.859137
3501.846111	510661.277209	48.864141
3502.116756	510647.222073	48.869146
3502.033535	510660.286921	48.874151
3502.141116	510661.281902	48.879156
3501.889767	510662.839485	48.884161
3502.403457	510665.641992	48.889165
3502.578850	510656.761791	48.894170
3502.400670	510664.732357	48.899175
3502.032556	510658.416826	48.904180
3502.215853	510667.038473	48.909185
3502.318712	510666.314242	48.914189
3502.664483	510662.364636	48.919194
3502.595680	510654.534772	48.924199
3502.119014	510667.206520	48.929204
3502.431948	510664.830301	48.934209
3502.250857	510668.653192	48.939213
3502.354267	510656.951498	48.944218
3502.062988	510661.955309	48.949223
3502.373427	510663.677029	48.954228
3502.711715	510654.265209	48.959233
3502.373286	510643.543910	48.964237
3502.602261	510628.281256	48.969242
3502.303327	510619.526596	48.974247
3502.088521	510624.670091	48.979252
3502.309112	510610.066378	48.984257
3502.316951	510623.673319	48.989261
3502.306500	510613.962490	48.994266
3502.496583	510622.127803	48.999271
3502.415440	510626.339603	49.004276
3502.577577	510617.259128	49.009281
3502.476807	510625.217476	49.014285
3502.642923	510618.665728	49.019290
3502.387957	510594.323266	49.024295
3502.165142	510589.097661	49.029300
3502.670507	510577.888838	49.034305
3502.005206	510571.772010	49.039309
3502.138122	510579.389920	49.044314
3502.262102	510578.358823	49.049319
3502.256676	510575.931738	49.054324
3502.549438	510581.298543	49.059329
3502.446212	510581.568040	49.064333
3502.514964	510578.319835	49.069338
3502.652461	510578.045410	49.074343
3502.653424	510583.053639	49.079348
3502.827788	510568.760721	49.084353
3502.588184	510562.981301	49.089357
3502.669215	510536.056283	49.094362
3502.764436	510551.976488	49.099367
3502.625819	510547.546959	49.104372
3502.908261	510526.711156	49.109377
3502.505707	510513.622303	49.114381
3502.237212	510501.220475	49.119386
3502.402838	510496.995781	49.124391
3502.095186	510498.916390	49.129396
3502.250045	510497.374533	49.134401
3502.121091	510506.197380	49.139405
3501.990534	510501.918327	49.144410
3502.624833	510499.794814	49.149415
3502.098230	510506.353490	49.154420
3502.468152	510501.944743	49.159425
3502.218463	510500.669180	49.164429
3502.363289	510499.432434	49.169434
3502.611201	510503.339315	49.174439
3502.702117	510502.009916	49.179444
3502.789002	510502.350540	49.184449
3502.448034	510479.943831	49.189453
3502.755634	510454.905198	49.194458
3502.805989	510465.267939	49.199463
3502.612127	510464.034137	49.204468
3502.672869	510459.927187	49.209473
3502.313387	510450.676133	49.214477
3502.234883	510425.850250	49.219482
3502.452531	510417.924411	49.224487
3502.245210	510420.284460	49.229492
3502.271161	510409.303068	49.234497
3501.791693	510416.714319	49.239501
3502.220616	510414.825609	49.244506
3502.110784	510418.131416	49.249511
3502.036328	510428.058618	49.254516
3502.325633	510433.274253	49.259521
3502.376686	510425.779451	49.264525
3502.503819	510418.070271	49.269530
3502.540956	510410.425900	49.274535
3502.395509	510420.465503	49.279540
3502.427259	510414.643142	49.284545
3502.399529	510416.215989	49.289549
3502.318235	510410.512670	49.294554
3502.407193	510415.001162	49.299559
3502.116309	510420.359095	49.304564
3502.425122	510405.842438	49.309569
3502.377973	510420.672339	49.314573
3502.201106	510407.952433	49.319578
3502.407688	510413.939966	49.324583
3502.247878	510412.144312	49.329588
3502.189837	510408.612590	49.334593
3502.279898	510417.451451	49.339597
3502.608549	510389.677659	49.344602
3502.450776	510380.040570	49.349607
3502.246469	510387.661280	49.354612
3502.718660	510371.247021	49.359617
3502.599990	510369.242509	49.364621
3502.239470	510374.560875	49.369626
3502.379370	510375.399000	49.374631
3502.691470	510369.532311	49.379636
3502.670791	510368.979358	49.384641
3502.651264	510356.538072	49.389645
3502.519756	510334.047476	49.394650
3502.383492	510325.418715	49.399655
3502.118717	510335.274877	49.404660
3502.744307	510325.109233	49.409665
3502.432428	510326.777590	49.414669
3502.195646	510326.865849	49.419674
3502.175983	510333.647990	49.424679
3502.129598	510329.254414	49.429684
3502.214102	510332.883635	49.434689
3502.365613	510325.322323	49.439693
3501.976420	510329.077008	49.444698
3502.354074	510325.628165	49.449703
3502.336300	510340.959372	49.454708
3502.409347	510323.596398	49.459713
3502.471676	510338.004363	49.464717
3502.474159	510321.057244	49.469722
3502.398441	510300.884833	49.474727
3502.403456	510296.584299	49.479732
3502.607318	510282.286479	49.484737
3502.064063	510289.353750	49.489741
3502.276056	510277.634633	49.494746
3502.440596	510285.197088	49.499751
3502.353473	510301.955759	49.504756
3502.665219	510294.723223	49.509761
3502.505859	510291.612195	49.514765
3502.590029	510284.972095	49.519770
3502.226570	510279.212156	49.524775
3502.382086	510259.559616	49.529780
3502.371756	510246.813267	49.534785
3502.524866	510245.069311	49.539789
3502.715358	510242.155917	49.544794
3502.637606	510247.884921	49.549799
3502.508130	510249.575042	49.554804
3502.464056	510246.749313	49.559809
3502.154297	510244.572638	49.564813
3502.564262	510245.418671	49.569818
3502.521989	510243.351480	49.574823
3502.525933	510223.874621	49.579828
3502.486011	510216.343520	49.584833
3502.400680	510213.271365	49.589837
3502.644214	510207.010752	49.594842
3502.412805	510211.954642	49.599847
3502.286719	510209.141870	49.604852
3502.655130	510212.726242	49.609857
3502.350240	510210.144086	49.614861
3502.416977	510208.363190	49.619866
3502.171666	510181.438606	49.624871
3502.407555	510177.253315	49.629876
3502.473489	510155.135982	49.634881
3502.166610	510169.197739	49.639885
3502.332439	510156.423478	49.644890
3502.582732	510158.306524	49.649895
3502.112465	510167.942321	49.654900
3502.645197	510163.760695	49.659905
3502.472883	510166.014069	49.664909
3502.587709	510165.540868	49.669914
3502.441238	510163.186606	49.674919
3502.514824	510158.318726	49.679924
3502.704405	510140.937147	49.684929
3502.081421	510131.879335	49.689933
3502.394028	510124.292471	49.694938
3502.466240	510123.724827	49.699943
3502.342504	510129.714082	49.704948
3502.395866	510116.502271	49.709953
3502.506750	510120.734432	49.714957
3502.555227	510124.116450	49.719962
3502.511410	510124.073032	49.724967
3502.602078	510120.264801	49.729972
3502.636895	510101.238221	49.734977
3502.446215	510095.501497	49.739981
3502.338661	510084.895119	49.744986
3502.585644	510073.726807	49.749991
3502.192151	510078.291645	49.754996
3502.410051	510071.883268	49.760001
3502.356904	510072.347212	49.765005
3502.660563	510064.053494	49.770010
3502.412200	510074.716632	49.775015
3502.413413	510073.957854	49.780020
3502.735579	510056.959943	49.785025
3502.447817	510058.219803	49.790029
3502.290214	510049.594275	49.795034
3502.310962	510050.299484	49.800039
3502.298361	510051.768795	49.805044
3502.309422	510044.330737	49.810049
3502.243752	510048.236701	49.815053
3502.121144	510053.466972	49.820058
3502.251525	510051.928944	49.825063
3502.225831	510050.415586	49.830068
3502.491196	510041.824377	49.835073
3502.435676	510055.391198	49.840077
3502.369374	510056.767820	49.845082
3502.382306	510047.761215	49.850087
3502.238949	510045.760566	49.855092
3502.162363	510042.434054	49.860097
3502.080537	510059.090948	49.865101
3502.304712	510051.416853	49.870106
3502.272012	510053.546996	49.875111
3502.168200	510058.824883	49.880116
3502.320485	510049.138598	49.885121
3502.026118	510058.190176	49.890125
3502.006759	510051.515761	49.895130
3502.176193	510047.543298	49.900135
3501.923948	510048.241067	49.905140
3501.891048	510045.919427	49.910145
3502.126798	510059.693150	49.915149
3502.333525	510052.780644	49.920154
3502.512129	510052.347948	49.925159
3501.901506	510058.161242	49.930164
3502.287756	510050.562706	49.935169
3502.268827	510060.987232	49.940173
3502.212459	510052.699826	49.945178
3502.073647	510055.858517	49.950183
3501.925046	510051.025726	49.955188
3502.531007	510054.117285	49.960193
3502.055041	510053.686875	49.965197
3502.321738	510046.562532	49.970202
3502.348021	510049.341007	49.975207
3502.042151	510056.168497	49.980212
3502.374591	510043.570172	49.985217
3502.311765	510056.480492	49.990221
3502.247302	510056.339160	49.995226
3502.066342	510052.675026	50.000231
3502.216316	510047.440919	50.005236
3502.210688	510054.828018	50.010241
3502.117088	510061.116066	50.015245
3502.101404	510054.896370	50.020250
3502.300854	510060.278089	50.025255
3502.043381	510062.241404	50.030260
3502.413279	510049.940696	50.035265
3502.366034	510051.921371	50.040269
3502.381584	510057.332159	50.045274
3502.384790	510062.744896	50.050279
3502.168945	510056.152128	50.055284
3502.322779	510046.971485	50.060289
3502.145837	510059.090419	50.065293
3502.267007	510049.004342	50.070298
3502.436594	510031.170512	50.075303
3502.345803	510026.227399	50.080308
3502.574460	510010.812477	50.085313
3502.686307	510015.803345	50.090317
3502.322981	510019.351652	50.095322
3502.334861	510026.837174	50.100327
3502.106782	510015.642736	50.105332
3502.623161	510011.514248	50.110337
3502.253404	510022.904851	50.115341
3502.169724	510010.675808	50.120346
3502.358802	510019.094515	50.125351
3502.175598	510019.781373	50.130356
3502.391171	510012.462741	50.135361
3502.462426	510014.930580	50.140365
3502.664363	510000.379884	50.145370
3502.327614	509987.431991	50.150375
3501.982005	509980.303225	50.155380
3502.450538	509979.571755	50.160385
3501.974654	509983.137861	50.165389
3502.209535	509971.920807	50.170394
3502.474802	509975.521533	50.175399
3502.408635	509982.715876	50.180404
3502.432920	509976.793368	50.185409
3502.322128	509986.625392	50.190413
3502.175445	509972.230954	50.195418
3502.067386	509984.895532	50.200423
3502.258994	509974.899456	50.205428
3502.444053	509981.801145	50.210433
3502.125115	509985.291854	50.215437
3502.051971	509973.263475	50.220442
3502.296507	509981.015777	50.225447
3501.743122	509979.029342	50.230452
3502.280215	509976.162296	50.235457
3502.435182	509984.282877	50.240461
3502.324622	509972.209822	50.245466
3502.415059	509985.551272	50.250471
3502.281569	509978.743101	50.255476
3502.505158	509976.077376	50.260481
3502.236661	509987.451997	50.265485
3502.516236	509984.271534	50.270490
3502.505648	509978.253361	50.275495
3502.482187	509964.800630	50.280500
3502.678943	509944.787086	50.285505
3502.554139	509947.640048	50.290509
3502.585546	509942.019937	50.295514
3502.261319	509945.916203	50.300519
3502.552712	509943.846825	50.305524
3502.814036	509936.622108	50.310529
3502.341758	509934.724026	50.315533
3502.202152	509928.625049	50.320538
3502.479641	509908.952827	50.325543
3502.496315	509900.299677	50.330548
3502.502821	509892.154023	50.335553
3502.516224	509894.479255	50.340557
3502.666920	509900.829927	50.345562
3502.451944	509903.697149	50.350567
3502.388410	509898.344976	50.355572
3502.745220	509896.366431	50.360577
3502.685104	509877.911088	50.365581
3502.467232	509865.197259	50.370586
3502.476200	509857.759450	50.375591
3502.355912	509854.085683	50.380596
3502.504262	509852.898923	50.385601
3502.347590	509855.858116	50.390605
3502.377496	509858.534871	50.395610
3502.633343	509864.363042	50.400615
3502.538252	509864.985389	50.405620
3502.767775	509826.703763	50.410625
3502.466409	509828.926989	50.415629
3502.547696	509825.069586	50.420634
3502.364986	509810.427758	50.425639
3502.426127	509815.224342	50.430644
3502.686707	509813.564534	50.435649
3502.351998	509814.325937	50.440653
3502.323472	509816.151913	50.445658
3502.424206	509790.436752	50.450663
3502.286011	509787.271697	50.455668
3502.529298	509778.532077	50.460673
3502.230495	509787.331551	50.465677
3502.322891	509775.833353	50.470682
3502.290515	509781.909468	50.475687
3502.277993	509784.845888	50.480692
3502.432329	509770.150751	50.485697
3502.417554	509772.379275	50.490701
3502.580579	509774.630285	50.495706
3502.614378	509778.065281	50.500711
3502.258810	509771.443898	50.505716
3502.465993	509771.765522	50.510721
3502.450594	509765.748034	50.515725
3502.510931	509744.187540	50.520730
3502.326492	509741.990990	50.525735
3502.280729	509713.516434	50.530740
3502.459894	509672.611753	50.535745
3502.441010	509633.205388	50.540749
3502.027117	509570.741653	50.545754
3502.300248	509500.934667	50.550759
3501.873051	509438.978458	50.555764
3501.959132	509350.836023	50.560769
3501.875014	509257.812696	50.565773
3501.663715	509146.393679	50.570778
3501.779516	509038.261294	50.575783
3501.648315	508906.591327	50.580788
3501.326345	508762.858874	50.585793
3501.092228	508629.280527	50.590797
3501.017091	508475.742203	50.595802
3500.999141	508313.845472	50.600807
3500.724334	508155.074075	50.605812
3500.515281	507963.555911	50.610817
3500.199825	507777.314371	50.615821
3500.064272	507572.372427	50.620826
3500.092240	507378.938249	50.625831
3499.547674	507177.243854	50.630836
3499.389601	506944.621295	50.635841
3498.969575	506733.946205	50.640845
3498.766309	506494.999925	50.645850
3498.692598	506251.830077	50.650855
3498.231866	506015.043080	50.655860
3498.216279	505754.804655	50.660865
3497.967738	505499.203956	50.665869
3497.665598	505228.781321	50.670874
3497.049179	504940.743458	50.675879
3496.804861	504655.931324	50.680884
3496.560826	504361.499470	50.685889
3496.321650	504067.314926	50.690893
3496.042833	503768.222815	50.695898
3495.488702	503455.555559	50.700903
3494.911278	503146.176003	50.705908
3494.686343	502822.817576	50.710913
3494.301520	502493.557022	50.715917
3493.603087	502168.186391	50.720922
3493.364751	501834.082268	50.725927
3492.650177	501496.099251	50.730932
3492.444930	501147.045897	50.735937
3492.037379	500810.722191	50.740941
3491.802397	500455.383611	50.745946
3491.363353	500089.136782	50.750951
3490.377096	499734.661855	50.755956
3490.456029	499357.536358	50.760961
3489.906567	498985.564332	50.765965
3489.498833	498610.879227	50.770970
3488.918036	498231.252615	50.775975
3488.234866	497853.355391	50.780980
3487.814577	497452.070521	50.785985
3487.537173	497060.575637	50.790989
3486.750272	496661.761230	50.795994
3486.475290	496266.603630	50.800999
3485.620889	495869.301322	50.806004
3485.023045	495459.140220	50.811009
3484.540741	495054.875545	50.816013
3483.936915	494640.798338	50.821018
3483.579229	494231.533724	50.826023
3482.868245	493822.012008	50.831028
3482.465853	493399.368197	50.836033
3481.816509	492982.982133	50.841037
3481.265102	492556.696639	50.846042
3481.198112	492127.843382	50.851047
3480.383665	491693.223985	50.856052
3479.919825	491248.359887	50.861057
3479.337188	490825.685754	50.866061
3478.563288	490376.241267	50.871066
3478.042033	489937.584229	50.876071
3477.703203	489483.643310	50.881076
3477.141942	489043.502888	50.886081
3475.953964	488599.449917	50.891085
3475.682420	488137.058012	50.896090
3474.899665	487688.411603	50.901095
3474.077400	487238.798383	50.906100
3473.790434	486788.380713	50.911105
3473.242285	486327.153370	50.916109
3472.544654	485870.294959	50.921114
3472.243811	485414.933276	50.926119
3471.222670	484957.749565	50.931124
3470.659088	484487.614874	50.936129
3469.709702	484031.056311	50.941133
3469.246500	483566.962626	50.946138
3469.035137	483098.359529	50.951143
3468.139600	482637.554351	50.956148
3467.800837	482167.124901	50.961153
3466.910053	481699.456711	50.966157
3466.320438	481220.025150	50.971162
3465.421939	480754.564937	50.976167
3464.947321	480279.297732	50.981172
3464.614368	479797.561189	50.986177
3463.788689	479326.988303	50.991181
3463.003458	478861.363934	50.996186
3462.735001	478371.271608	51.001191
3461.432373	477900.993511	51.006196
3461.018386	477422.303153	51.011201
3460.538049	476951.315110	51.016205
3459.894166	476473.398480	51.021210
3459.034190	475990.233617	51.026215
3458.208412	475520.533517	51.031220
3457.611088	475033.249391	51.036225
3457.047741	474566.729343	51.041229
3455.835839	474092.495220	51.046234
3455.594734	473616.778606	51.051239
3454.785498	473145.195807	51.056244
3454.209471	472655.468620	51.061249
3453.485234	472177.412233	51.066253
3452.969006	471695.307018	51.071258
3451.853766	471225.502471	51.076263
3450.973447	470754.281252	51.081268
3451.020101	470267.440232	51.086273
3450.302789	469800.480641	51.091277
3449.610912	469316.218148	51.096282
3448.717533	468847.084833	51.101287
3447.939799	468367.478185	51.106292
3447.450229	467889.082501	51.111297
3446.653871	467410.470843	51.116301
3445.821886	466942.451167	51.121306
3445.332187	466457.938240	51.126311
3444.180707	465988.071703	51.131316
3443.841624	465516.443603	51.136321
3442.892024	465047.690518	51.141325
3441.966531	464570.302489	51.146330
3441.722544	464102.228342	51.151335
3440.910865	463633.929391	51.156340
3440.228549	463157.485521	51.161345
3439.654110	462686.440493	51.166349
3439.149854	462214.866878	51.171354
3438.423265	461740.275059	51.176359
3437.471633	461269.309376	51.181364
3436.712571	460797.694367	51.186369
3435.762891	460319.049103	51.191373
3435.296385	459858.424503	51.196378
3434.811766	459380.902413	51.201383
3433.587929	458924.587826	51.206388
3433.210842	458451.086350	51.211393
3432.387552	458000.826925	51.216397
3431.411092	457534.958642	51.221402
3431.179730	457061.454995	51.226407
3430.346155	456606.856907	51.231412
3429.780376	456137.698376	51.236417
3428.863988	455678.731616	51.241421
3428.349869	455215.886907	51.246426
3427.618405	454752.001591	51.251431
3426.952874	454293.068217	51.256436
3426.249393	453827.028539	51.261441
3425.369607	453373.792663	51.266445
3424.956677	452907.485129	51.271450
3423.934078	452441.974734	51.276455
3422.918275	451992.791825	51.281460
3422.349556	451534.193140	51.286465
3421.636133	451080.428568	51.291469
3420.991384	450628.724590	51.296474
3420.423419	450177.557769	51.301479
3419.653652	449727.479649	51.306484
3418.927765	449268.251644	51.311489
3418.113963	448826.637434	51.316493
3417.386767	448364.346946	51.321498
3416.850611	447920.134246	51.326503
3415.711891	447484.077502	51.331508
3415.375881	447031.797876	51.336513
3414.620225	446588.914114	51.341517
3413.775611	446139.895059	51.346522
3413.011161	445695.473317	51.351527
3412.442346	445264.056097	51.356532
3411.796708	444808.433015	51.361537
3410.834017	444378.432360	51.366541
3409.910976	443946.641184	51.371546
3409.552680	443499.677833	51.376551
3408.516921	443066.416612	51.381556
3407.511182	442630.757123	51.386561
3407.286778	442205.473655	51.391565
3406.366748	441770.444956	51.396570
3405.484645	441346.367119	51.401575
3404.864003	440911.224898	51.406580
3404.636100	440481.444567	51.411585
3403.717396	440061.868142	51.416589
3402.813890	439628.778373	51.421594
3402.455827	439189.756525	51.426599
3401.437065	438769.183849	51.431604
3400.853349	438340.843766	51.436609
3400.152612	437909.950904	51.441613
3399.430822	437488.167162	51.446618
3398.358539	437067.040934	51.451623
3397.847897	436654.678508	51.456628
3397.669593	436231.492872	51.461633
3396.402689	435823.145829	51.466637
3395.772314	435391.462122	51.471642
3395.114994	434961.349315	51.476647
3394.133094	434554.713774	51.481652
3393.916282	434146.198915	51.486657
3393.004539	433727.961832	51.491661
3392.189562	433309.093228	51.496666
3391.762380	432890.029479	51.501671
3390.466060	432483.308989	51.506676
3390.308081	432064.519242	51.511681
3389.466293	431653.067248	51.516685
3388.616214	431242.473307	51.521690
3388.014391	430832.849263	51.526695
3386.949188	430427.481736	51.531700
3386.438208	430016.383086	51.536705
3385.839981	429613.366731	51.541709
3385.107107	429205.083620	51.546714
3384.218741	428805.071722	51.551719
3383.499865	428407.261620	51.556724
3383.146566	427999.813945	51.561729
3382.426658	427605.166231	51.566733
3381.567033	427200.275005	51.571738
3381.143754	426799.143362	51.576743
3380.152884	426399.365231	51.581748
3379.472696	425996.179646	51.586753
3378.504279	425605.782794	51.591757
3377.816842	425205.684878	51.596762
3377.380261	424800.995169	51.601767
3376.373329	424418.333449	51.606772
3376.038992	424006.275646	51.611777
3375.503976	423623.477275	51.616781
3374.820268	423225.051183	51.621786
3374.312066	422829.182262	51.626791
3373.226166	422431.671771	51.631796
3372.569157	422039.040734	51.636801
3371.772084	421650.007716	51.641805
3371.290068	421247.101281	51.646810
3370.610873	420856.768394	51.651815
3369.386828	420466.973395	51.656820
3369.087004	420080.557657	51.661825
3368.561953	419676.085693	51.666829
3367.798997	419296.514764	51.671834
3366.990823	418905.057207	51.676839
3366.238254	418516.100339	51.681844
3365.531960	418125.733575	51.686849
3364.692862	417752.987467	51.691853
3364.006244	417355.620830	51.696858
3363.486377	416971.204122	51.701863
3362.451862	416591.944637	51.706868
3361.912579	416207.520703	51.711873
3361.564179	415820.368404	51.716877
3360.591137	415444.234314	51.721882
3360.037170	415066.250583	51.726887
3358.985641	414680.540686	51.731892
3358.614492	414294.641835	51.736897
3357.657767	413917.570635	51.741901
3357.054779	413537.923236	51.746906
3356.676043	413152.772679	51.751911
3355.710131	412794.083921	51.756916
3354.991865	412396.984318	51.761921
3354.210406	412031.066378	51.766925
3353.685746	411649.578111	51.771930
3352.942212	411269.898222	51.776935
3352.059657	410908.098766	51.781940
3351.430893	410528.950280	51.786945
3350.837218	410165.647729	51.791949
3350.236871	409777.642279	51.796954
3349.857091	409415.338657	51.801959
3348.642475	409042.362730	51.806964
3348.332823	408669.721906	51.811969
3347.356007	408301.730801	51.816973
3347.045804	407923.286878	51.821978
3346.192553	407559.587386	51.826983
3345.295610	407187.402448	51.831988
3344.938490	406814.543101	51.836993
3344.097949	406445.542336	51.841997
3343.221918	406073.670957	51.847002
3342.524815	405703.850785	51.852007
3341.990847	405344.496688	51.857012
3341.074017	404971.805243	51.862017
3340.218789	404604.538479	51.867021
3339.556135	404240.159736	51.872026
3338.837054	403878.047694	51.877031
3338.014003	403526.622735	51.882036
3337.207286	403156.789703	51.887041
3336.635691	402805.444016	51.892045
3335.989630	402445.083134	51.897050
3335.596660	402083.254761	51.902055
3334.874305	401726.786660	51.907060
3334.230845	401370.734205	51.912065
3333.728021	401015.545186	51.917069
3332.839722	400653.550197	51.922074
3332.049071	400298.373353	51.927079
3331.304937	399936.652537	51.932084
3330.751898	399578.456171	51.937089
3329.823421	399235.922890	51.942093
3329.355332	398880.679498	51.947098
3328.983116	398517.841861	51.952103
3327.980714	398173.733074	51.957108
3327.524035	397814.510717	51.962113
3326.857302	397469.121274	51.967117
3326.313425	397099.304356	51.972122
3325.636860	396740.028826	51.977127
3324.573124	396387.954179	51.982132
3324.673971	396017.565663	51.987137
3323.878650	395667.042553	51.992141
3322.632827	395301.968997	51.997146
3322.412845	394935.737741	52.002151
3321.655121	394583.341511	52.007156
3320.730369	394220.112203	52.012161
3320.318833	393871.035133	52.017165
3319.669583	393505.568172	52.022170
3318.892151	393149.524553	52.027175
3318.083883	392796.227958	52.032180
3317.561468	392436.068672	52.037185
3316.715177	392091.669531	52.042189
3315.936983	391733.653642	52.047194
3315.573715	391372.237680	52.052199
3314.660741	391018.151266	52.057204
3314.011609	390659.849646	52.062209
3313.402485	390315.929346	52.067213
3312.404928	389949.539131	52.072218
3311.987254	389599.072320	52.077223
3311.063589	389262.819533	52.082228
3310.669069	388900.696517	52.087233
3309.891917	388548.775948	52.092237
3309.059151	388196.962410	52.097242
3308.825463	387844.618380	52.102247
3307.647788	387506.939787	52.107252
3307.291515	387148.912363	52.112257
3306.472224	386802.346749	52.117261
3306.002153	386450.636760	52.122266
3305.343446	386096.817132	52.127271
3304.431902	385747.992827	52.132276
3303.877629	385401.117640	52.137281
3302.785690	385054.171627	52.142285
3302.318879	384701.350784	52.147290
3301.680861	384352.927700	52.152295
3301.079502	384010.980391	52.157300
3300.558676	383664.083572	52.162305
3299.485701	383321.365285	52.167309
3298.846181	382984.424540	52.172314
3297.899015	382635.881690	52.177319
3297.319341	382294.652753	52.182324
3296.935862	381955.144517	52.187329
3296.229489	381611.640550	52.192333
3295.161277	381268.419596	52.197338
3294.703946	380929.778576	52.202343
3294.149703	380584.537273	52.207348
3293.581589	380234.691619	52.212353
3292.805238	379901.076899	52.217357
3292.149032	379561.336180	52.222362
3291.677027	379219.961001	52.227367
3290.789043	378884.676526	52.232372
3289.922679	378528.351450	52.237377
3289.463781	378189.915564	52.242381
3288.793743	377860.412367	52.247386
3288.610441	377513.152018	52.252391
3287.601393	377169.631039	52.257396
3286.962891	376824.318851	52.262401
3286.314506	376484.499353	52.267405
3285.203964	376148.005864	52.272410
3284.547191	375800.983487	52.277415
3283.766692	375464.279433	52.282420
3283.457704	375123.682486	52.287425
3282.522278	374793.331057	52.292429
3281.828918	374458.436288	52.297434
3281.579381	374124.257114	52.302439
3280.810527	373782.602416	52.307444
3280.099990	373430.099183	52.312449
3279.475443	373102.635664	52.317453
3278.613855	372763.276567	52.322458
3278.085113	372420.682247	52.327463
3277.387566	372090.602117	52.332468
3276.876891	371736.144947	52.337473
3276.088822	371408.795686	52.342477
3275.223074	371061.868018	52.347482
3274.980497	370727.940188	52.352487
3273.829871	370402.395762	52.357492
3273.390629	370052.034317	52.362497
3272.225871	369728.318620	52.367501
3271.566277	369385.084291	52.372506
3271.109008	369052.881761	52.377511
3270.088295	368733.002689	52.382516
3270.097461	368391.867975	52.387521
3269.140901	368072.228271	52.392525
3268.620371	367734.046994	52.397530
3267.865476	367386.588640	52.402535
3266.836848	367064.205283	52.407540
3266.503865	366722.755452	52.412545
3265.704433	366402.951490	52.417549
3264.777513	366071.360257	52.422554
3264.324186	365731.346567	52.427559
3263.395367	365407.714117	52.432564
3262.817926	365080.538102	52.437569
3262.287672	364762.842413	52.442573
3261.446466	364428.579383	52.447578
3261.029527	364101.777958	52.452583
3260.077648	363773.913845	52.457588
3259.832129	363446.113742	52.462593
3259.002603	363127.079987	52.467597
3258.166416	362796.010089	52.472602
3257.954974	362465.296981	52.477607
3256.784366	362146.921044	52.482612
3256.187493	361806.875260	52.487617
3255.697017	361487.165883	52.492621
3254.792877	361156.629371	52.497626
3254.065320	360840.031901	52.502631
3253.377358	360521.008749	52.507636
3253.103125	360179.195303	52.512641
3252.228330	359864.955565	52.517645
3251.243335	359534.267823	52.522650
3250.819912	359211.046384	52.527655
3249.894262	358895.459687	52.532660
3249.193557	358574.288066	52.537665
3248.696756	358254.736071	52.542669
3247.922167	357933.571890	52.547674
3247.211341	357608.782073	52.552679
3246.706778	357288.359780	52.557684
3245.972495	356961.177376	52.562689
3245.411069	356639.640185	52.567693
3244.375708	356317.692376	52.572698
3243.843006	356003.246331	52.577703
3242.896237	355698.254005	52.582708
3242.374658	355377.720267	52.587713
3241.749751	355057.531654	52.592717
3241.128595	354748.741199	52.597722
3240.588587	354421.994952	52.602727
3240.027190	354117.542869	52.607732
3239.482647	353800.209292	52.612737
3238.538810	353484.514742	52.617741
3238.094327	353164.845570	52.622746
3237.615121	352826.958345	52.627751
3236.570987	352510.204846	52.632756
3236.089121	352193.436822	52.637761
3235.386850	351867.209051	52.642765
3234.559516	351550.237297	52.647770
3234.161503	351229.759987	52.652775
3233.363352	350912.856145	52.657780
3233.165169	350583.690305	52.662785
3232.063936	350271.309832	52.667789
3231.301445	349952.893083	52.672794
3231.133166	349622.698597	52.677799
3230.039130	349303.872358	52.682804
3229.446115	348982.292637	52.687809
3228.875125	348661.496522	52.692813
3228.093279	348339.561128	52.697818
3228.018254	348012.905329	52.702823
3226.525983	347700.546518	52.707828
3226.209691	347371.405402	52.712833
3225.311394	347050.142684	52.717837
3224.636136	346737.496518	52.722842
3224.437786	346420.013620	52.727847
3223.357585	346091.087657	52.732852
3222.405400	345775.629324	52.737857
3221.750372	345458.289652	52.742861
3221.112604	345139.469233	52.747866
3220.804633	344812.933567	52.752871
3219.784428	344513.310731	52.757876
3219.270124	344194.618287	52.762881
3218.648742	343883.246127	52.767885
3217.883098	343570.087944	52.772890
3217.236023	343245.175258	52.777895
3216.052212	342925.385527	52.782900
3215.516666	342614.883972	52.787905
3215.173233	342304.808580	52.792909
3214.610492	341991.889969	52.797914
3213.812743	341682.214140	52.802919
3212.890399	341371.003724	52.807924
3212.648146	341046.753253	52.812929
3211.974432	340739.496628	52.817933
3210.930204	340424.558846	52.822938
3210.525054	340112.547476	52.827943
3209.472869	339800.204165	52.832948
3209.261439	339486.809890	52.837953
3208.556205	339183.088791	52.842957
3207.912455	338869.047077	52.847962
3207.120999	338551.819778	52.852967
3206.348349	338245.941120	52.857972
3205.542658	337923.112703	52.862977
3204.950058	337622.650105	52.867981
3204.140033	337309.568882	52.872986
3203.675078	336994.649624	52.877991
3203.145301	336696.387466	52.882996
3202.617605	336373.481880	52.888001
3201.686002	336073.931274	52.893005
3200.940955	335762.334288	52.898010
3200.429579	335436.850423	52.903015
3199.521391	335139.786651	52.908020
3198.724208	334830.077361	52.913025
3198.268481	334520.821766	52.918029
3197.427742	334218.957335	52.923034
3196.715782	333919.871492	52.928039
3196.214895	333618.994386	52.933044
3195.618221	333301.405538	52.938049
3194.855733	333002.400069	52.943053
3194.325044	332694.853759	52.948058
3193.579965	332387.187265	52.953063
3192.741379	332092.237734	52.958068
3192.158789	331778.000177	52.963073
3191.759081	331471.166079	52.968077
3190.636134	331161.390094	52.973082
3190.168078	330851.916492	52.978087
3189.772822	330549.100170	52.983092
3188.966478	330241.383195	52.988097
3187.901162	329936.633646	52.993101
3187.265377	329630.974730	52.998106
3186.917312	329334.434235	53.003111
3186.001175	329036.327595	53.008116
3185.554894	328728.038151	53.013121
3184.752642	328428.714489	53.018125
3183.981716	328120.499374	53.023130
3183.079200	327813.805932	53.028135
3182.404028	327519.830512	53.033140
3182.063728	327224.833515	53.038145
3181.132004	326926.390061	53.043149
3180.659443	326630.775228	53.048154
3179.966416	326322.158675	53.053159
3179.073679	326032.311081	53.058164
3178.322120	325730.219229	53.063169
3177.756777	325439.299255	53.068173
3177.196816	325144.023657	53.073178
3176.698479	324848.304394	53.078183
3175.861447	324548.691260	53.083188
3175.545104	324252.839183	53.088193
3174.788814	323956.062676	53.093197
3173.938183	323652.425616	53.098202
3173.484845	323349.870318	53.103207
3172.703000	323061.496725	53.108212
3172.104740	322759.191361	53.113217
3171.550610	322457.030696	53.118221
3171.009201	322165.942572	53.123226
3170.259093	321854.797499	53.128231
3169.231206	321547.361690	53.133236
3168.870369	321248.807150	53.138241
3168.147859	320957.183435	53.143245
3167.360090	320657.625033	53.148250
3166.805566	320354.209443	53.153255
3165.974492	320057.074721	53.158260
3165.187121	319755.043403	53.163265
3164.545062	319463.554809	53.168269
3163.944342	319168.850509	53.173274
3163.483340	318866.611806	53.178279
3161.982598	318576.682115	53.183284
3162.152108	318273.526902	53.188289
3161.202828	317987.429305	53.193293
3160.484681	317693.706435	53.198298
3160.043726	317391.459749	53.203303
3159.450454	317099.421261	53.208308
3158.549599	316798.136648	53.213313
3157.855403	316511.765061	53.218317
3157.603562	316209.943046	53.223322
3156.654799	315905.429441	53.228327
3155.838297	315620.475045	53.233332
3155.540239	315322.960864	53.238337
3154.914084	315018.851812	53.243341
3154.178685	314736.173735	53.248346
3153.257648	314423.197394	53.253351
3152.686803	314127.581661	53.258356
3151.979353	313827.861602	53.263361
3151.353748	313540.019208	53.268365
3150.717970	313241.686607	53.273370
3149.954803	312935.403170	53.278375
3149.039793	312655.065004	53.283380
3148.708098	312353.575193	53.288385
3147.770507	312059.437624	53.293389
3147.219919	311771.731335	53.298394
3146.781971	311485.890802	53.303399
3145.940282	311186.770207	53.308404
3145.526787	310890.433037	53.313409
3144.446762	310594.124154	53.318413
3144.054054	310289.684467	53.323418
3143.492446	309988.377343	53.328423
3142.519305	309710.892889	53.333428
3141.952430	309403.677307	53.338433
3141.493784	309108.794115	53.343437
3140.771208	308820.114390	53.348442
3139.862095	308518.960299	53.353447
3139.479120	308235.827652	53.358452
3138.628680	307935.528610	53.363457
3137.993911	307645.278798	53.368461
3137.339613	307347.340967	53.373466
3136.761457	307041.470744	53.378471
3135.893429	306757.112709	53.383476
3135.350203	306464.681112	53.388481
3134.773674	306163.315822	53.393485
3133.799622	305872.173367	53.398490
3133.155221	305580.137735	53.403495
3132.675656	305292.379013	53.408500
3131.864923	304994.562288	53.413505
3131.113309	304713.339040	53.418509
3130.559158	304423.603928	53.423514
3129.759888	304119.187867	53.428519
3128.999929	303845.578349	53.433524
3128.675197	303550.100774	53.438529
3128.009141	303259.336817	53.443533
3127.270359	302973.880657	53.448538
3126.624998	302680.209132	53.453543
3125.871260	302392.156657	53.458548
3125.165718	302091.744989	53.463553
3124.681335	301803.139406	53.468557
3123.975016	301513.396942	53.473562
3123.444494	301222.047199	53.478567
3122.690895	300938.244713	53.483572
3121.916199	300640.922481	53.488577
3121.035102	300348.760699	53.493581
3120.328103	300060.721829	53.498586
3119.717795	299776.563484	53.503591
3119.019513	299488.598596	53.508596
3118.628199	299200.559152	53.513601
3117.694053	298918.054929	53.518605
3116.574140	298627.659531	53.523610
3116.304466	298342.349728	53.528615
3115.584450	298062.713365	53.533620
3114.938765	297781.027450	53.538625
3114.348294	297483.924986	53.543629
3113.575677	297205.034098	53.548634
3113.020023	296919.003205	53.553639
3111.942814	296645.482203	53.558644
3111.603892	296355.188630	53.563649
3111.032869	296076.034898	53.568653
3110.270838	295800.731016	53.573658
3109.616897	295513.287349	53.578663
3108.573205	295232.628221	53.583668
3108.078027	294954.199386	53.588673
3107.503943	294674.662092	53.593677
3106.961304	294392.343514	53.598682
3106.149961	294117.885482	53.603687
3105.461773	293833.730062	53.608692
3104.901741	293556.302787	53.613697
3104.088148	293278.329527	53.618701
3103.497401	292997.544706	53.623706
3103.035900	292721.832533	53.628711
3102.108833	292431.346225	53.633716
3101.623988	292152.479089	53.638721
3100.983089	291880.741716	53.643725
3100.180180	291598.002258	53.648730
3099.877206	291314.597590	53.653735
3098.897923	291045.153940	53.658740
3098.218501	290753.480312	53.663745
3097.663644	290474.596811	53.668749
3097.007428	290186.942722	53.673754
3096.347605	289897.811758	53.678759
3095.388126	289640.104040	53.683764
3094.958872	289349.076843	53.688769
3094.435107	289073.650524	53.693773
3093.530760	288794.973354	53.698778
3093.110031	288508.731851	53.703783
3092.063925	288225.033939	53.708788
3092.023294	287945.939105	53.713793
3091.191769	287673.820019	53.718797
3090.378522	287387.282995	53.723802
3089.841384	287100.574669	53.728807
3088.983246	286821.429914	53.733812
3088.124571	286538.057330	53.738817
3087.601146	286262.806654	53.743821
3087.084045	285981.136828	53.748826
3086.543858	285707.289097	53.753831
3085.569143	285437.431994	53.758836
3084.687792	285149.299348	53.763841
3084.042066	284879.364303	53.768845
3083.302123	284596.175122	53.773850
3082.894621	284316.498654	53.778855
3082.111794	284042.713585	53.783860
3081.930588	283759.358986	53.788865
3080.920984	283476.109835	53.793869
3080.458183	283201.917026	53.798874
3079.972692	282920.418281	53.803879
3078.856591	282638.127784	53.808884
3078.175012	282344.256734	53.813889
3077.374865	282063.927891	53.818893
3076.380953	281798.655808	53.823898
3076.021990	281529.488337	53.828903
3075.222913	281251.985874	53.833908
3074.551631	280977.290028	53.838913
3073.988052	280707.415980	53.843917
3073.204222	280438.417128	53.848922
3072.852358	280150.936232	53.853927
3071.726145	279896.712016	53.858932
3071.365189	279614.173187	53.863937
3070.602613	279353.422284	53.868941
3070.152363	279087.451794	53.873946
3069.862853	278807.830226	53.878951
3068.834327	278537.010235	53.883956
3068.541288	278257.057968	53.888961
3067.430094	277984.569997	53.893965
3066.689448	277707.056981	53.898970
3066.526148	277430.114699	53.903975
3065.602879	277157.749602	53.908980
3065.080277	276881.449844	53.913985
3064.248044	276618.951964	53.918989
3063.298238	276339.459775	53.923994
3062.911506	276066.984105	53.928999
3062.066863	275802.476075	53.934004
3061.691445	275526.127357	53.939009
3061.003354	275244.836297	53.944013
3060.345088	274971.410230	53.949018
3059.759805	274689.084128	53.954023
3058.378712	274415.823378	53.959028
3058.245290	274140.378616	53.964033
3057.306962	273870.103992	53.969037
3056.849577	273601.154014	53.974042
3056.671483	273323.933552	53.979047
3055.399190	273047.548469	53.984052
3054.932749	272780.968531	53.989057
3054.183162	272509.568972	53.994061
3053.553048	272233.973719	53.999066
3052.618201	271966.067248	54.004071
3051.931015	271701.814531	54.009076
3051.599033	271424.134742	54.014081
3050.833811	271153.731125	54.019085
3050.044882	270890.207771	54.024090
3049.571375	270609.749031	54.029095
3048.760574	270344.650222	54.034100
3048.214411	270071.359725	54.039105
3047.472234	269810.910898	54.044109
3046.812258	269537.689503	54.049114
3046.184708	269256.389604	54.054119
3045.348264	268990.403850	54.059124
3044.558251	268728.587637	54.064129
3043.888523	268461.964439	54.069133
3043.411620	268195.540034	54.074138
3042.946126	267925.726648	54.079143
3042.018294	267666.912436	54.084148
3041.289876	267386.316883	54.089153
3040.760351	267127.032363	54.094157
3040.184600	266870.862398	54.099162
3039.446249	266595.235106	54.104167
3038.372107	266337.157757	54.109172
3038.130914	266066.596625	54.114177
3037.674935	265799.456901	54.119181
3036.834453	265534.644851	54.124186
3036.204009	265257.829676	54.129191
3035.453038	264993.793279	54.134196
3034.728203	264722.367149	54.139201
3033.789995	264456.654349	54.144205
3033.360504	264190.453705	54.149210
3032.628572	263929.802209	54.154215
3031.882110	263669.076779	54.159220
3031.220776	263401.232470	54.164225
3030.394032	263133.363596	54.169229
3029.947760	262878.092285	54.174234
3029.506048	262606.444524	54.179239
3028.705215	262346.059718	54.184244
3027.851655	262077.813862	54.189249
3027.242190	261824.861267	54.194253
3026.463574	261564.931969	54.199258
3026.331764	261298.533528	54.204263
3025.312015	261039.687008	54.209268
3024.538679	260771.149391	54.214273
3024.465483	260495.497538	54.219277
3023.533351	260232.715793	54.224282
3022.702824	259966.887538	54.229287
3022.216510	259713.000348	54.234292
3021.443068	259440.873016	54.239297
3020.894246	259179.432293	54.244301
3019.920424	258916.734777	54.249306
3019.899217	258651.339964	54.254311
3018.631000	258387.747269	54.259316
3017.648788	258120.747850	54.264321
3017.389989	257863.082666	54.269325
3016.500549	257601.366364	54.274330
3016.084359	257337.869106	54.279335
3015.380844	257072.864099	54.284340
3014.409580	256814.574241	54.289345
3014.120925	256553.553470	54.294349
3013.396349	256292.703866	54.299354
3012.798999	256020.272237	54.304359
3012.117867	255762.421515	54.309364
3011.264763	255508.214673	54.314369
3010.875972	255237.329965	54.319373
3009.882684	254984.699431	54.324378
3009.226324	254714.596288	54.329383
3008.705733	254459.726843	54.334388
3008.279526	254190.632101	54.339393
3007.722188	253942.212301	54.344397
3006.673936	253679.481616	54.349402
3006.208859	253406.803214	54.354407
3005.338231	253147.661438	54.359412
3004.584289	252885.954839	54.364417
3003.843607	252631.937515	54.369421
3003.019114	252369.835321	54.374426
3002.812279	252099.791922	54.379431
3001.762254	251852.446012	54.384436
3001.130257	251594.745674	54.389441
3000.516179	251340.200746	54.394445
2999.710815	251088.920736	54.399450
2999.326486	250824.611885	54.404455
2998.547296	250570.297936	54.409460
2997.752989	250308.601435	54.414465
2997.019321	250060.443954	54.419469
2996.618909	249804.110256	54.424474
2996.384336	249550.246414	54.429479
2995.023329	249298.267531	54.434484
2994.643435	249031.057600	54.439489
2994.038182	248770.148513	54.444493
2992.874277	248524.429825	54.449498
2992.767596	248262.373054	54.454503
2991.785328	248014.130707	54.459508
2991.154544	247753.431066	54.464513
2990.740297	247504.844952	54.469517
2989.822011	247241.110285	54.474522
2989.283401	246981.517877	54.479527
2988.516143	246737.012546	54.484532
2987.958214	246473.884297	54.489537
2987.365096	246216.109939	54.494541
2986.256414	245959.410823	54.499546
2985.726602	245700.404994	54.504551
2984.727109	245456.269628	54.509556
2984.192911	245205.185262	54.514561
2984.000953	244965.073826	54.519565
2983.260555	244707.070848	54.524570
2982.750434	244442.869212	54.529575
2981.908872	244201.206671	54.534580
2981.449940	243938.347581	54.539585
2980.739212	243690.324317	54.544589
2980.064901	243438.883378	54.549594
2979.302027	243176.481347	54.554599
2978.634268	242929.012942	54.559604
2977.991655	242664.275550	54.564609
2977.338855	242418.766574	54.569613
2976.468703	242154.855672	54.574618
2976.087967	241902.301686	54.579623
2975.155654	241659.384937	54.584628
2974.583364	241405.512621	54.589633
2973.831840	241149.326418	54.594637
2973.177223	240899.669895	54.599642
2972.727454	240646.976592	54.604647
2972.096071	240394.312565	54.609652
2971.111487	240140.406278	54.614657
2970.481373	239894.669519	54.619661
2969.960385	239639.468596	54.624666
2969.545325	239377.121360	54.629671
2968.803846	239127.227629	54.634676
2967.851898	238873.140647	54.639681
2967.637913	238619.777719	54.644685
2966.896025	238362.322763	54.649690
2965.894844	238105.240475	54.654695
2965.604625	237860.116284	54.659700
2964.935027	237590.963533	54.664705
2964.317847	237342.098069	54.669709
2963.439568	237092.561506	54.674714
2963.462085	236826.051160	54.679719
2962.101831	236566.610193	54.684724
2961.255195	236307.648737	54.689729
2960.773846	236056.829436	54.694733
2960.177705	235798.211508	54.699738
2959.601950	235547.204640	54.704743
2958.893633	235298.918505	54.709748
2958.306336	235042.694611	54.714753
2957.613993	234787.888472	54.719757
2956.807533	234521.744308	54.724762
2956.349751	234269.957930	54.729767
2955.487177	234020.706205	54.734772
2954.690013	233760.062638	54.739777
2954.330036	233504.595954	54.744781
2953.313890	233259.011665	54.749786
2952.634992	233000.923126	54.754791
2951.836112	232741.020914	54.759796
2951.537512	232492.269356	54.764801
2950.814422	232238.060183	54.769805
2949.458733	231989.604580	54.774810
2949.333048	231731.253559	54.779815
2948.489707	231489.542153	54.784820
2948.000660	231237.870294	54.789825
2947.040101	230990.806093	54.794829
2946.452323	230748.037606	54.799834
2946.027609	230501.119013	54.804839
2945.044445	230256.784802	54.809844
2944.240950	230000.811972	54.814849
2943.789277	229756.267620	54.819853
2942.897920	229517.344286	54.824858
2942.481584	229272.897477	54.829863
2941.606413	229030.917402	54.834868
2940.843503	228789.200283	54.839873
2940.569205	228546.591672	54.844877
2939.692670	228301.023649	54.849882
2939.272321	228061.418515	54.854887
2938.640416	227826.277859	54.859892
2938.191253	227569.772054	54.864897
2937.357183	227317.936482	54.869901
2936.553671	227085.422064	54.874906
2935.802583	226833.421989	54.879911
2934.927810	226589.029711	54.884916
2934.296795	226342.486251	54.889921
2933.859012	226108.516198	54.894925
2932.993461	225862.164029	54.899930
2932.651452	225609.262581	54.904935
2931.669410	225372.249031	54.909940
2931.109432	225127.874780	54.914945
2930.409655	224890.295959	54.919949
2929.860720	224645.603118	54.924954
2929.548688	224393.986382	54.929959
2928.658322	224156.898144	54.934964
2927.488905	223907.977444	54.939969
2927.244443	223665.021563	54.944973
2926.513206	223418.375351	54.949978
2925.976826	223176.141862	54.954983
2924.940908	222933.797249	54.959988
2924.472274	222687.340852	54.964993
2923.911006	222451.924091	54.969997
2923.008345	222217.134936	54.975002
2922.536281	221967.689781	54.980007
2921.943899	221730.230587	54.985012
2921.063150	221484.976175	54.990017
2920.550193	221253.348875	54.995021
2919.781167	221006.627090	55.000026
2919.294233	220756.398940	55.005031
2918.276046	220525.133887	55.010036
2917.748724	220277.446917	55.015041
2917.283343	220032.424171	55.020045
2916.264794	219806.151386	55.025050
2915.934328	219565.513236	55.030055
2915.156592	219328.256353	55.035060
2914.566687	219089.633891	55.040065
2913.882574	218849.308641	55.045069
2913.449067	218609.008141	55.050074
2912.852343	218367.486794	55.055079
2912.023934	218128.828834	55.060084
2911.007173	217867.123335	55.065089
2910.672368	217636.242787	55.070093
2909.728885	217397.249039	55.075098
2909.352245	217147.766631	55.080103
2908.556497	216912.646218	55.085108
2907.920423	216669.609290	55.090113
2906.963953	216435.190545	55.095117
2906.256752	216193.974030	55.100122
2905.643172	215950.936011	55.105127
2905.188229	215728.036249	55.110132
2904.574602	215481.295767	55.115137
2904.016283	215237.169531	55.120141
2903.004762	215003.591671	55.125146
2902.782545	214756.066256	55.130151
2901.661566	214530.042724	55.135156
2900.877475	214272.934246	55.140161
2900.522845	214041.877741	55.145165
2899.741226	213808.789429	55.150170
2899.134834	213572.581154	55.155175
2898.281468	213345.411815	55.160180
2897.644938	213107.580707	55.165185
2896.941483	212867.724509	55.170189
2896.109565	212647.185613	55.175194
2895.540966	212411.140926	55.180199
2894.964413	212178.954989	55.185204
2894.612879	211937.569962	55.190209
2893.801655	211706.517475	55.195213
2892.854170	211470.027040	55.200218
2892.552270	211224.716541	55.205223
2891.778844	210997.593545	55.210228
2891.033824	210767.170316	55.215233
2890.448855	210530.116794	55.220237
2889.821737	210307.109630	55.225242
2889.325961	210063.577969	55.230247
2888.476112	209832.461948	55.235252
2887.864523	209587.206751	55.240257
2887.238864	209362.013509	55.245261
2886.406957	209128.962617	55.250266
2885.692264	208884.808328	55.255271
2885.254837	208654.433160	55.260276
2884.450251	208424.155166	55.265281
2884.039027	208186.879297	55.270285
2883.109832	207953.708207	55.275290
2882.413236	207716.224789	55.280295
2881.742045	207482.505538	55.285300
2881.059689	207245.530779	55.290305
2880.269438	207014.390343	55.295309
2879.442879	206784.669247	55.300314
2879.149212	206541.463030	55.305319
2878.452686	206318.417553	55.310324
2877.903213	206090.755179	55.315329
2877.091080	205855.600923	55.320333
2876.646472	205626.078307	55.325338
2875.762558	205388.086443	55.330343
2875.099349	205170.716140	55.335348
2874.453574	204932.612034	55.340353
2873.765776	204699.542582	55.345357
2872.719612	204466.543532	55.350362
2872.707769	204233.979766	55.355367
2871.726398	204010.020871	55.360372
2871.136467	203783.811897	55.365377
2870.720038	203542.533696	55.370381
2869.837244	203304.181063	55.375386
2869.173823	203070.796120	55.380391
2868.321240	202850.371971	55.385396
2867.595695	202608.981198	55.390401
2867.336865	202384.939657	55.395405
2866.424225	202159.691746	55.400410
2865.769502	201928.295376	55.405415
2865.351484	201702.703710	55.410420
2864.744223	201463.717027	55.415425
2863.989701	201233.484654	55.420429
2863.118475	200996.603363	55.425434
2862.869190	200766.318358	55.430439
2861.864013	200535.059596	55.435444
2861.162444	200300.915891	55.440449
2860.557474	200066.694252	55.445453
2859.783178	199841.879182	55.450458
2859.078843	199601.859667	55.455463
2858.349200	199384.432937	55.460468
2857.592578	199155.558460	55.465473
2857.389931	198915.793376	55.470477
2856.406421	198701.590923	55.475482
2855.863981	198463.459593	55.480487
2855.094222	198241.908087	55.485492
2854.474443	198011.896964	55.490497
2853.889243	197785.609807	55.495501
2853.005680	197566.916816	55.500506
2852.543486	197325.125748	55.505511
2852.033344	197104.288623	55.510516
2850.929262	196867.945769	55.515521
2850.281689	196642.258710	55.520525
2849.758789	196417.443608	55.525530
2849.385031	196184.792872	55.530535
2848.401091	195958.742107	55.535540
2847.635785	195738.091106	55.540545
2847.041710	195513.965569	55.545549
2846.169790	195289.694136	55.550554
2845.817972	195049.041296	55.555559
2844.956374	194835.624149	55.560564
2844.381625	194610.608766	55.565569
2843.807643	194392.630773	55.570573
2843.076458	194170.136059	55.575578
2842.432647	193930.628995	55.580583
2841.885059	193706.720296	55.585588
2841.515766	193483.115175	55.590593
2841.020962	193254.886662	55.595597
2840.177059	193033.000094	55.600602
2839.326447	192792.920423	55.605607
2838.464877	192563.149929	55.610612
2838.110394	192332.256834	55.615617
2837.428040	192102.027473	55.620621
2836.628047	191877.950604	55.625626
2836.035383	191645.482519	55.630631
2835.261450	191429.215836	55.635636
2834.574401	191193.520328	55.640641
2833.855840	190959.561325	55.645645
2833.299364	190729.649239	55.650650
2832.930895	190509.263648	55.655655
2832.059688	190282.826077	55.660660
2831.262493	190052.051962	55.665665
2830.425828	189824.987622	55.670669
2829.756296	189592.426967	55.675674
2829.242458	189367.285724	55.680679
2828.135728	189154.211713	55.685684
2828.044488	188926.053888	55.690689
2827.335446	188691.608146	55.695693
2826.559771	188478.077586	55.700698
2826.144609	188240.864849	55.705703
2825.314729	188023.120986	55.710708
2824.708910	187788.625183	55.715713
2824.434966	187560.591906	55.720717
2823.099159	187342.333355	55.725722
2822.867016	187114.003006	55.730727
2821.881454	186883.210465	55.735732
2820.881091	186649.011843	55.740737
2820.416324	186421.446891	55.745741
2819.681143	186212.818253	55.750746
2819.314649	185979.438608	55.755751
2818.527586	185766.863632	55.760756
2818.028727	185534.245078	55.765761
2817.329246	185317.561837	55.770765
2816.436135	185085.427820	55.775770
2816.175214	184861.654826	55.780775
2815.431949	184638.849843	55.785780
2814.343666	184420.095191	55.790785
2814.173992	184196.107468	55.795789
2813.087219	183974.454207	55.800794
2812.958246	183738.593128	55.805799
2812.071595	183526.349689	55.810804
2811.434174	183291.958110	55.815809
2810.733064	183068.988814	55.820813
2809.997537	182845.860704	55.825818
2809.450838	182613.315606	55.830823
2808.429908	182395.959462	55.835828
2807.755789	182169.937331	55.840833
2807.142904	181940.637374	55.845837
2806.460019	181730.431006	55.850842
2806.229236	181500.118750	55.855847
2805.550547	181277.892712	55.860852
2804.439881	181056.016075	55.865857
2803.743261	180835.766825	55.870861
2803.183446	180625.037435	55.875866
2802.779883	180399.401338	55.880871
2801.941762	180175.514337	55.885876
2801.275599	179957.668869	55.890881
2800.863340	179731.986740	55.895885
2799.927916	179509.975759	55.900890
2799.384241	179277.346140	55.905895
2798.411357	179063.586063	55.910900
2798.043775	178843.333002	55.915905
2797.345365	178618.299889	55.920909
2796.076145	178406.765149	55.925914
2796.001267	178170.925480	55.930919
2795.394827	177958.435765	55.935924
2794.726922	177741.403197	55.940929
2794.099277	177517.573082	55.945933
2793.372169	177303.922844	55.950938
2792.518563	177067.691172	55.955943
2791.849577	176858.625733	55.960948
2791.475245	176635.408884	55.965953
2790.634535	176418.728504	55.970957
2790.314756	176201.712354	55.975962
2789.541373	175969.366272	55.980967
2788.400093	175757.570229	55.985972
2787.659371	175541.921552	55.990977
2787.325784	175320.638605	55.995981
2786.720068	175097.046953	56.000986
2786.110170	174870.977009	56.005991
2785.312427	174657.313415	56.010996
2784.763419	174436.667132	56.016001
2784.360863	174215.299318	56.021005
2783.280742	173999.763380	56.026010
2782.655299	173765.142430	56.031015
2782.423886	173554.167544	56.036020
2781.389544	173322.857119	56.041025
2781.149972	173106.607746	56.046029
2780.214143	172882.317449	56.051034
2779.608055	172651.795160	56.056039
2778.626544	172437.511036	56.061044
2777.712742	172217.685006	56.066049
2777.303897	172007.153312	56.071053
2776.750725	171791.622036	56.076058
2776.121982	171570.253715	56.081063
2775.336768	171352.841188	56.086068
2774.542671	171129.364944	56.091073
2774.188624	170905.133510	56.096077
2773.513478	170689.831030	56.101082
2773.023881	170465.585415	56.106087
2772.404110	170261.531436	56.111092
2771.893720	170032.255514	56.116097
2771.113132	169806.622709	56.121101
2770.204018	169589.239560	56.126106
2769.465107	169354.662615	56.131111
2768.547272	169137.283374	56.136116
2768.067818	168921.018585	56.141121
2767.355280	168705.097130	56.146125
2766.756653	168486.068660	56.151130
2766.134666	168269.677494	56.156135
2765.450095	168063.063841	56.161140
2764.656068	167839.593746	56.166145
2763.949659	167620.091339	56.171149
2762.981012	167408.579500	56.176154
2762.959524	167188.958359	56.181159
2762.169995	166980.752206	56.186164
2761.405667	166762.090474	56.191169
2760.978159	166540.884287	56.196173
2760.120155	166318.641288	56.201178
2759.494306	166094.302832	56.206183
2758.802291	165875.723786	56.211188
2758.387026	165658.666219	56.216193
2757.817518	165436.548034	56.221197
2756.936138	165228.340674	56.226202
2756.209887	165007.483288	56.231207
2755.526734	164793.779234	56.236212
2754.523685	164570.247161	56.241217
2753.947394	164346.470816	56.246221
2753.229299	164139.744096	56.251226
2752.813663	163926.434980	56.256231
2752.201251	163713.933892	56.261236
2751.624595	163490.099211	56.266241
2751.122396	163277.557752	56.271245
2749.937372	163061.451070	56.276250
2749.548995	162838.989177	56.281255
2748.775981	162627.956597	56.286260
2748.065283	162407.557328	56.291265
2747.670352	162186.219346	56.296269
2746.987336	161978.062498	56.301274
2746.354446	161762.626211	56.306279
2745.335622	161545.485038	56.311284
2744.670233	161328.912184	56.316289
2744.477259	161106.480802	56.321293
2743.792068	160899.131510	56.326298
2743.017451	160679.884454	56.331303
2742.307164	160462.700936	56.336308
2741.481536	160235.721830	56.341313
2741.016153	160022.278235	56.346317
2740.426767	159812.161150	56.351322
2739.599800	159587.233307	56.356327
2739.088008	159373.572106	56.361332
2738.520275	159155.229746	56.366337
2738.106847	158925.447573	56.371341
2736.977752	158722.440292	56.376346
2736.294947	158491.394138	56.381351
2735.818040	158276.551705	56.386356
2734.823914	158051.113456	56.391361
2734.355308	157838.192081	56.396365
2733.332838	157628.004053	56.401370
2733.216214	157398.273841	56.406375
2732.494146	157187.074696	56.411380
2731.880996	156984.694963	56.416385
2731.326546	156679.524996	56.421389
2730.467271	156465.237375	56.426394
2730.211028	156246.139206	56.431399
2728.930499	156032.098983	56.436404
2728.567854	155802.278484	56.441409
2728.080397	155579.547314	56.446413
2727.028654	155370.343767	56.451418
2726.566965	155148.259638	56.456423
2725.773784	154927.729485	56.461428
2724.862378	154712.507657	56.466433
2724.560197	154492.499996	56.471437
2723.510503	154284.650240	56.476442
2723.130255	154058.861180	56.481447
2722.646047	153843.844122	56.486452
2721.992828	153617.872439	56.491457
2721.231478	153402.698711	56.496461
2720.277147	153195.260023	56.501466
2719.875872	152964.193682	56.506471
2719.411363	152752.104066	56.511476
2718.469455	152532.795238	56.516481
2717.721222	152310.381093	56.521485
2717.233789	152097.142557	56.526490
2716.350517	151882.226706	56.531495
2715.365571	151668.968044	56.536500
2714.733928	151448.790995	56.541505
2714.349301	151239.138806	56.546509
2713.613347	151035.949723	56.551514
2713.124550	150819.770762	56.556519
2712.208981	150620.463966	56.561524
2711.627045	150401.201171	56.566529
2711.182271	150177.533080	56.571533
2710.443545	149964.093905	56.576538
2709.655229	149738.894467	56.581543
2709.020563	149529.648667	56.586548
2708.530692	149315.132084	56.591553
2708.129918	149099.128461	56.596557
2706.914011	148890.830407	56.601562
2706.491915	148665.580367	56.606567
2705.702362	148458.043672	56.611572
2705.055970	148240.152829	56.616577
2704.273453	148025.119215	56.621581
2703.457502	147820.450411	56.626586
2703.240384	147589.430795	56.631591
2702.382630	147389.550019	56.636596
2701.893536	147177.055541	56.641601
2701.179031	146954.723322	56.646605
2700.430122	146754.930935	56.651610
2699.835690	146530.777983	56.656615
2699.035427	146313.725257	56.661620
2698.639303	146111.517192	56.666625
2698.248754	145887.641475	56.671629
2697.002825	145676.509640	56.676634
2696.537073	145447.578278	56.681639
2695.862276	145240.069709	56.686644
2695.287357	145022.913877	56.691649
2694.586235	144815.005616	56.696653
2693.503620	144602.685952	56.701658
2692.956710	144389.075597	56.706663
2692.326777	144175.962749	56.711668
2691.520116	143966.170662	56.716673
2691.126246	143749.261827	56.721677
2690.308939	143548.687295	56.726682
2689.608628	143333.303988	56.731687
2688.862925	143135.071666	56.736692
2688.375961	142921.970159	56.741697
2687.799873	142709.799160	56.746701
2686.493187	142502.116634	56.751706
2686.311503	142301.856091	56.756711
2685.640189	142090.428738	56.761716
2684.828231	141876.776000	56.766721
2684.531554	141662.496713	56.771725
2683.364985	141469.233901	56.776730
2683.140388	141254.043869	56.781735
2682.363394	141056.071311	56.786740
2681.597450	140835.696774	56.791745
2680.830195	140629.910962	56.796749
2679.731385	140430.367041	56.801754
2679.140730	140225.229420	56.806759
2679.110367	140029.927898	56.811764
2678.198312	139827.613827	56.816769
2677.491867	139621.647333	56.821773
2676.880459	139422.159887	56.826778
2676.679567	139206.967889	56.831783
2675.904450	139004.332701	56.836788
2675.075473	138798.950294	56.841793
2674.456037	138580.169880	56.846797
2673.883005	138375.448623	56.851802
2673.392905	138162.177634	56.856807
2672.691877	137960.643127	56.861812
2671.796876	137748.938464	56.866817
2671.367836	137538.228703	56.871821
2670.604526	137331.613584	56.876826
2669.680035	137112.993903	56.881831
2668.968046	136923.067736	56.886836
2668.500505	136707.758123	56.891841
2668.287181	136491.291790	56.896845
2667.330029	136288.195735	56.901850
2666.858195	136077.515852	56.906855
2665.974638	135859.877203	56.911860
2665.416459	135650.979962	56.916865
2664.995489	135453.267554	56.921869
2664.173668	135234.023040	56.926874
2663.645686	135007.085809	56.931879
2662.994920	134805.666513	56.936884
2662.169103	134588.091693	56.941889
2661.721928	134365.897872	56.946893
2660.686676	134155.321108	56.951898
2660.364062	133945.217316	56.956903
2659.457417	133732.425536	56.961908
2658.968629	133517.904975	56.966913
2658.553063	133307.642693	56.971917
2657.493345	133094.524178	56.976922
2657.004229	132874.850972	56.981927
2655.976957	132667.357933	56.986932
2655.263648	132443.061566	56.991937
2654.844001	132227.675872	56.996941
2654.089737	132023.269118	57.001946
2653.423764	131819.802530	57.006951
2652.707411	131610.845196	57.011956
2651.983734	131390.331375	57.016961
2651.505730	131183.448007	57.021965
2650.579047	130975.951323	57.026970
2650.044572	130752.668793	57.031975
2649.130945	130554.991854	57.036980
2648.357591	130352.505442	57.041985
2648.186477	130135.114714	57.046989
2647.340373	129935.233997	57.051994
2646.926462	129727.576314	57.056999
2646.370340	129522.648130	57.062004
2645.360826	129303.504143	57.067009
2644.910350	129093.354757	57.072013
2643.808238	128879.207697	57.077018
2643.133189	128666.302827	57.082023
2642.544561	128471.002276	57.087028
2641.821585	128267.786266	57.092033
2641.734756	128046.080049	57.097037
2640.596810	127847.251168	57.102042
2640.200330	127634.627567	57.107047
2639.294171	127434.571052	57.112052
2638.969898	127223.323531	57.117057
2638.503132	127014.614886	57.122061
2637.482666	126805.881256	57.127066
2636.833597	126581.367488	57.132071
2636.060500	126382.402436	57.137076
2635.758661	126179.350940	57.142081
2634.841905	125965.197050	57.147085
2633.947934	125747.370973	57.152090
2633.612387	125545.053408	57.157095
2632.620791	125348.657736	57.162100
2631.934188	125138.893324	57.167105
2631.759734	124929.773238	57.172109
2630.660407	124725.449280	57.177114
2630.316836	124512.650990	57.182119
2629.478488	124305.634694	57.187124
2629.002727	124101.813481	57.192129
2628.586871	123884.637703	57.197133
2627.626931	123673.073892	57.202138
2627.123629	123458.759942	57.207143
2626.277843	123255.499006	57.212148
2625.430435	123042.119110	57.217153
2625.029319	122837.876571	57.222157
2623.893190	122631.517150	57.227162
2623.454763	122409.556875	57.232167
2622.649573	122205.243511	57.237172
2621.960883	122005.662326	57.242177
2621.521740	121803.681266	57.247181
2620.856372	121604.645400	57.252186
2620.338993	121390.947033	57.257191
2619.266820	121183.407791	57.262196
2618.812929	120983.022512	57.267201
2618.443436	120772.441993	57.272205
2617.387969	120570.453705	57.277210
2616.903201	120360.859732	57.282215
2616.116416	120148.242568	57.287220
2615.582890	119948.347549	57.292225
2614.841149	119737.973943	57.297229
2613.945716	119537.085554	57.302234
2613.550988	119328.272742	57.307239
2612.679795	119134.722336	57.312244
2612.043576	118923.697357	57.317249
2611.568760	118717.942937	57.322253
2610.980070	118524.269756	57.327258
2610.353183	118304.786156	57.332263
2609.360292	118105.003405	57.337268
2608.589553	117894.585751	57.342273
2607.923656	117695.217739	57.347277
2607.354974	117499.574794	57.352282
2606.894434	117289.842902	57.357287
2606.181367	117082.679172	57.362292
2605.193439	116881.095938	57.367297
2604.954173	116679.668589	57.372301
2604.046508	116482.335092	57.377306
2603.532217	116277.304549	57.382311
2602.899619	116082.272813	57.387316
2602.205476	115871.643694	57.392321
2601.560928	115665.788109	57.397325
2600.590526	115477.352431	57.402330
2600.290940	115264.780585	57.407335
2599.529945	115073.045796	57.412340
2598.980857	114860.370870	57.417345
2598.597896	114645.779915	57.422349
2597.423276	114454.731016	57.427354
2596.744169	114247.800640	57.432359
2596.328538	114041.198328	57.437364
2595.589626	113840.583415	57.442369
2595.064575	113630.529965	57.447373
2594.215763	113438.523134	57.452378
2593.377154	113230.439481	57.457383
2592.831140	113038.952579	57.462388
2592.013241	112837.253812	57.467393
2591.644383	112632.166157	57.472397
2590.485439	112428.798408	57.477402
2590.108338	112227.402790	57.482407
2589.342495	112039.975765	57.487412
2588.562952	111838.710521	57.492417
2588.260856	111641.331437	57.497421
2587.857626	111434.240861	57.502426
2587.231204	111228.107601	57.507431
2586.314191	111046.417394	57.512436
2585.968054	110829.587527	57.517441
2585.266988	110625.216324	57.522445
2584.174501	110424.430966	57.527450
2583.656242	110216.759535	57.532455
2582.967004	110014.618986	57.537460
2582.426183	109815.978609	57.542465
2581.715627	109619.099181	57.547469
2580.602038	109423.287856	57.552474
2580.375314	109208.629929	57.557479
2579.423863	109010.004020	57.562484
2578.809862	108815.324066	57.567489
2578.403111	108611.113287	57.572493
2577.601223	108422.437543	57.577498
2577.002024	108214.783152	57.582503
2576.336317	108018.575749	57.587508
2575.751994	107821.735167	57.592513
2575.295090	107611.753592	57.597517
2574.713825	107405.886316	57.602522
2574.054456	107203.872093	57.607527
2572.861338	106995.941504	57.612532
2572.037727	106797.465640	57.617537
2571.778130	106595.539067	57.622541
2570.946777	106396.223812	57.627546
2570.077332	106198.648445	57.632551
2569.625493	106004.307923	57.637556
2569.129715	105805.464655	57.642561
2568.389185	105604.441098	57.647565
2567.367015	105410.589147	57.652570
2567.049334	105199.191551	57.657575
2566.592039	105000.558222	57.662580
2565.557865	104809.821964	57.667585
2565.203330	104602.064652	57.672589
2564.529421	104406.446230	57.677594
2564.077667	104195.034340	57.682599
2563.184348	103998.489667	57.687604
2562.240191	103789.665494	57.692609
2561.706738	103594.494621	57.697613
2560.671762	103407.557313	57.702618
2560.272542	103197.084928	57.707623
2559.509173	103011.890435	57.712628
2558.810689	102818.966238	57.717633
2558.086666	102613.797156	57.722637
2557.275566	102426.096200	57.727642
2556.912106	102229.393404	57.732647
2556.188173	102042.347810	57.737652
2555.639352	101842.207475	57.742657
2555.375248	101639.010381	57.747661
2554.433919	101451.160214	57.752666
2553.990499	101245.432049	57.757671
2553.134584	101047.688008	57.762676
2552.411079	100854.371551	57.767681
2551.934973	100644.720784	57.772685
2551.045464	100455.760269	57.777690
2550.295353	100252.461938	57.782695
2549.710505	100067.332155	57.787700
2549.042130	99868.509031	57.792705
2548.441787	99661.582741	57.797709
2547.755353	99466.235724	57.802714
2547.018351	99267.009975	57.807719
2546.205969	99079.488340	57.812724
2545.408650	98896.196696	57.817729
2545.197118	98687.606330	57.822733
2544.545050	98496.194754	57.827738
2543.850357	98288.870716	57.832743
2543.267400	98094.641596	57.837748
2542.245462	97907.073909	57.842753
2541.776969	97698.539570	57.847757
2541.062517	97521.810518	57.852762
2540.638133	97319.406062	57.857767
2539.999530	97112.667280	57.862772
2539.110097	96923.107747	57.867777
2538.370016	96724.234326	57.872781
2537.827781	96536.899931	57.877786
2537.081797	96327.489733	57.882791
2536.595382	96131.054818	57.887796
2535.775700	95941.505079	57.892801
2535.309548	95739.533510	57.897805
2534.202286	95548.034835	57.902810
2533.795255	95346.425243	57.907815
2533.093866	95157.529232	57.912820
2532.209101	94962.867254	57.917825
2531.586805	94774.259984	57.922829
2530.875953	94587.145995	57.927834
2530.167445	94392.086831	57.932839
2529.595542	94207.636578	57.937844
2529.271085	94013.629634	57.942849
2528.860090	93810.512374	57.947853
2527.717938	93627.324147	57.952858
2527.239957	93432.014819	57.957863
2526.549368	93232.479381	57.962868
2526.020373	93043.415260	57.967873
2525.384346	92841.712215	57.972877
2524.420965	92654.330966	57.977882
2524.099759	92440.964249	57.982887
2523.298248	92251.062256	57.987892
2522.481245	92062.635500	57.992897
2522.034522	91855.844754	57.997901
2521.106034	91673.488425	58.002906
2520.605335	91476.177027	58.007911
2519.722525	91282.478905	58.012916
2519.155585	91091.224394	58.017921
2518.572392	90898.192328	58.022925
2517.935247	90702.653199	58.027930
2517.389092	90504.444602	58.032935
2516.864784	90316.525285	58.037940
2515.715020	90126.189478	58.042945
2515.177455	89924.414958	58.047949
2514.359562	89738.683897	58.052954
2513.738910	89535.169797	58.057959
2513.352532	89353.330057	58.062964
2512.637300	89164.233507	58.067969
2512.237426	88967.011041	58.072973
2511.193632	88769.600776	58.077978
2510.533103	88571.833554	58.082983
2509.786345	88375.831674	58.087988
2509.434530	88192.575929	58.092993
2508.960500	87987.011507	58.097997
2507.968027	87806.827703	58.103002
2507.501929	87604.974526	58.108007
2506.779567	87416.680432	58.113012
2505.909719	87220.486597	58.118017
2505.295316	87025.813627	58.123021
2504.816660	86835.463580	58.128026
2504.352110	86630.658609	58.133031
2503.479437	86440.659787	58.138036
2502.601192	86255.969704	58.143041
2502.387136	86050.756503	58.148045
2501.551332	85859.615864	58.153050
2500.872840	85665.897232	58.158055
2500.036371	85472.008874	58.163060
2499.636274	85269.545847	58.168065
2499.091938	85069.358004	58.173069
2498.041574	84882.088958	58.178074
2497.592197	84680.748660	58.183079
2496.840381	84483.115807	58.188084
2495.917292	84286.608573	58.193089
2495.697201	84088.052013	58.198093
2494.576817	83889.988659	58.203098
2494.329531	83708.123740	58.208103
2493.445708	83518.165332	58.213108
2492.754566	83321.687301	58.218113
2492.155964	83128.967885	58.223117
2491.380900	82933.926601	58.228122
2491.081737	82742.037959	58.233127
2490.170121	82542.680077	58.238132
2489.219728	82349.909443	58.243137
2488.756435	82155.884430	58.248141
2488.105839	81970.314425	58.253146
2487.320453	81758.894949	58.258151
2486.406936	81578.808242	58.263156
2485.861489	81389.842134	58.268161
2485.366901	81202.397128	58.273165
2484.349370	81022.147889	58.278170
2483.853013	80822.936973	58.283175
2483.063557	80635.962087	58.288180
2482.069264	80456.994284	58.293185
2481.860593	80266.337111	58.298189
2481.235286	80083.999382	58.303194
2480.475052	79896.151898	58.308199
2480.012407	79713.778949	58.313204
2479.213622	79519.609754	58.318209
2478.709568	79332.728076	58.323213
2477.784632	79145.534561	58.328218
2477.555359	78960.336446	58.333223
2476.803406	78767.523061	58.338228
2475.898554	78581.351765	58.343233
2475.501846	78394.651652	58.348237
2474.996226	78195.714543	58.353242
2474.242738	78002.110073	58.358247
2473.652171	77821.890647	58.363252
2472.978256	77626.534424	58.368257
2472.836593	77427.413961	58.373261
2471.175162	77244.910660	58.378266
2470.451894	77060.872506	58.383271
2469.921464	76865.621176	58.388276
2469.419038	76675.715382	58.393281
2468.978469	76480.085958	58.398285
2467.913387	76304.853258	58.403290
2467.502892	76110.179422	58.408295
2466.694834	75925.170110	58.413300
2465.915371	75735.811216	58.418305
2465.375267	75555.255247	58.423309
2464.887715	75365.473344	58.428314
2464.243219	75175.908179	58.433319
2463.515782	74988.829015	58.438324
2462.587809	74800.142333	58.443329
2462.056839	74613.314273	58.448333
2461.634516	74419.000654	58.453338
2461.174564	74234.566148	58.458343
2460.136746	74052.702241	58.463348
2459.674190	73866.567176	58.468353
2458.830514	73670.876668	58.473357
2457.806564	73492.544599	58.478362
2457.475936	73291.308790	58.483367
2456.844934	73106.506248	58.488372
2456.095395	72908.996272	58.493377
2455.753786	72738.234953	58.498381
2454.806532	72551.206920	58.503386
2453.939932	72356.369121	58.508391
2453.684641	72175.500484	58.513396
2452.724514	71992.920702	58.518401
2452.482363	71801.575010	58.523405
2451.565056	71620.119498	58.528410
2450.910591	71427.556749	58.533415
2450.324344	71232.191346	58.538420
2449.579462	71054.717321	58.543425
2449.021192	70867.250644	58.548429
2448.268574	70675.116170	58.553434
2447.876034	70482.901129	58.558439
2446.963955	70303.008812	58.563444
2445.767478	70116.017830	58.568449
2445.650142	69924.746431	58.573453
2445.100974	69741.115005	58.578458
2444.124556	69545.625383	58.583463
2443.500195	69359.678376	58.588468
2442.607786	69185.855062	58.593473
2442.426843	68996.705717	58.598477
2441.248924	68821.258662	58.603482
2440.676872	68628.976117	58.608487
2440.245807	68448.676081	58.613492
2439.746454	68267.533443	58.618497
2438.810942	68079.887032	58.623501
2438.072929	67897.778560	58.628506
2437.489834	67707.172610	58.633511
2436.756214	67536.017935	58.638516
2436.288449	67354.796399	58.643521
2435.308909	67161.009460	58.648525
2434.752262	66988.165792	58.653530
2434.755778	66792.902937	58.658535
2433.691544	66613.727244	58.663540
2432.961609	66422.574458	58.668545
2432.184938	66227.466313	58.673549
2431.590796	66056.163202	58.678554
2431.180083	65867.707566	58.683559
2430.195772	65677.447937	58.688564
2429.425075	65499.081477	58.693569
2429.242937	65314.303000	58.698573
2428.417528	65135.274107	58.703578
2427.936197	64948.276207	58.708583
2427.223840	64761.965864	58.713588
2426.529137	64574.676112	58.718593
2425.934592	64383.924144	58.723597
2425.077017	64195.862817	58.728602
2424.711022	64004.413449	58.733607
2424.027569	63826.491923	58.738612
2423.111588	63637.726585	58.743617
2422.557185	63443.358599	58.748621
2421.801426	63268.828883	58.753626
2421.080556	63071.603522	58.758631
2420.538649	62879.053485	58.763636
2419.687919	62710.214423	58.768641
2419.430915	62509.476630	58.773645
2418.693662	62326.416948	58.778650
2418.038908	62133.971478	58.783655
2417.258027	61947.917841	58.788660
2416.565961	61760.500096	58.793665
2415.888257	61577.716783	58.798669
2415.176749	61404.691432	58.803674
2414.783177	61207.962187	58.808679
2414.110499	61011.298234	58.813684
2413.226768	60825.309911	58.818689
2412.557358	60633.762072	58.823693
2412.112404	60460.870871	58.828698
2411.383660	60265.622810	58.833703
2410.758097	60074.250975	58.838708
2409.982725	59885.582940	58.843713
2409.221754	59698.978467	58.848717
2408.316570	59512.256263	58.853722
2407.967584	59327.802864	58.858727
2407.310139	59138.278443	58.863732
2406.571494	58958.081557	58.868737
2405.831329	58767.000779	58.873741
2405.314093	58582.426287	58.878746
2404.451639	58397.601316	58.883751
2403.817060	58220.582544	58.888756
2402.844145	58039.804921	58.893761
2402.450063	57847.694264	58.898765
2401.745723	57671.479915	58.903770
2401.152439	57477.774565	58.908775
2400.554710	57308.399402	58.913780
2399.830053	57135.345861	58.918785
2399.540427	56940.154660	58.923789
2398.566379	56759.266226	58.928794
2397.923237	56568.888929	58.933799
2397.093385	56383.752802	58.938804
2396.212179	56206.706862	58.943809
2396.059299	56019.808582	58.948813
2394.982119	55849.487842	58.953818
2394.380521	55661.528133	58.958823
2393.683193	55477.282070	58.963828
2392.887756	55298.468420	58.968833
2392.738176	55118.516042	58.973837
2391.784873	54940.832248	58.978842
2391.008933	54763.280284	58.983847
2390.477718	54586.178596	58.988852
2389.903325	54406.034721	58.993857
2389.317106	54208.007957	58.998861
2388.435888	54037.983064	59.003866
2387.700984	53856.078882	59.008871
2387.490964	53668.473049	59.013876
2386.334780	53489.838668	59.018881
2386.330797	53299.729300	59.023885
2385.301405	53123.723904	59.028890
2384.706217	52939.955493	59.033895
2383.816664	52763.770016	59.038900
2383.051673	52573.481954	59.043905
2383.039527	52393.233971	59.048909
2382.025682	52216.329896	59.053914
2381.449796	52029.096404	59.058919
2381.000760	51846.894835	59.063924
2380.090554	51662.477351	59.068929
2379.431038	51476.980984	59.073933
2378.677272	51292.343123	59.078938
2378.298491	51102.325675	59.083943
2377.504497	50922.124549	59.088948
2376.772063	50737.846516	59.093953
2376.142738	50546.833681	59.098957
2375.354454	50379.985988	59.103962
2374.841020	50178.577701	59.108967
2374.172754	49994.455300	59.113972
2373.231594	49818.708530	59.118977
2372.992604	49634.230672	59.123981
2372.204282	49460.567127	59.128986
2371.253899	49276.208928	59.133991
2370.624938	49090.975921	59.138996
2370.029961	48907.640832	59.144001
2369.805836	48723.891318	59.149005
2368.976447	48544.656125	59.154010
2368.176489	48364.171602	59.159015
2367.734088	48183.942235	59.164020
2366.953675	48000.864155	59.169025
2366.483895	47807.485743	59.174029
2365.415005	47630.679855	59.179034
2364.921087	47433.063948	59.184039
2364.075204	47253.752632	59.189044
2363.111858	47079.092953	59.194049
2362.766469	46893.840992	59.199053
2361.955787	46720.251998	59.204058
2360.954893	46543.477805	59.209063
2360.233100	46365.225001	59.214068
2359.759814	46196.047842	59.219073
2359.413017	46023.622621	59.224077
2358.617778	45841.745911	59.229082
2358.283135	45660.332603	59.234087
2357.347553	45488.894824	59.239092
2356.600436	45300.066746	59.244097
2356.182440	45119.988061	59.249101
2355.088248	44947.751998	59.254106
2354.572526	44775.713720	59.259111
2354.087501	44589.195483	59.264116
2353.493057	44413.358740	59.269121
2352.734180	44231.084922	59.274125
2351.902939	44054.220288	59.279130
2351.479035	43876.214326	59.284135
2350.796011	43709.020532	59.289140
2349.747500	43537.350919	59.294145
2349.473162	43345.619299	59.299149
2348.700345	43183.881485	59.304154
2348.141827	42993.217194	59.309159
2347.516061	42824.700815	59.314164
2346.642334	42646.962173	59.319169
2346.549272	42459.389342	59.324173
2345.360448	42288.133815	59.329178
2344.791283	42107.977338	59.334183
2344.627587	41924.450500	59.339188
2343.658106	41749.917666	59.344193
2342.992199	41568.166147	59.349197
2341.918360	41395.421218	59.354202
2341.870002	41212.965160	59.359207
2341.210343	41019.252188	59.364212
2340.526803	40846.030274	59.369217
2339.639334	40668.475409	59.374221
2338.755492	40489.830844	59.379226
2338.214601	40308.958178	59.384231
2337.812779	40118.933140	59.389236
2336.766721	39955.030068	59.394241
2336.344124	39763.213028	59.399245
2335.583858	39589.503687	59.404250
2334.880551	39408.612509	59.409255
2334.306670	39236.315896	59.414260
2333.579122	39057.632996	59.419265
2333.025730	38870.627529	59.424269
2332.050364	38700.766665	59.429274
2331.881702	38527.946550	59.434279
2331.372281	38345.281056	59.439284
2330.385910	38165.747425	59.444289
2329.959958	37975.288398	59.449293
2328.772696	37795.646673	59.454298
2328.338037	37610.228113	59.459303
2327.619746	37435.787884	59.464308
2327.050552	37269.006900	59.469313
2326.252704	37090.180318	59.474317
2325.328147	36918.136653	59.479322
2324.963413	36731.014123	59.484327
2324.263116	36555.084714	59.489332
2323.242841	36384.321500	59.494337
2322.958794	36205.544489	59.499341
2322.072050	36036.518189	59.504346
2321.811974	35859.097270	59.509351
2320.894462	35683.339427	59.514356
2320.227548	35513.371470	59.519361
2319.654417	35331.270177	59.524365
2318.717305	35165.146815	59.529370
2318.192831	34979.646479	59.534375
2317.524147	34807.364059	59.539380
2316.904082	34636.128345	59.544385
2316.456300	34461.257110	59.549389
2315.669955	34282.068099	59.554394
2315.158963	34116.342727	59.559399
2314.413305	33934.532089	59.564404
2313.407093	33756.406154	59.569409
2313.314653	33580.531575	59.574413
2312.324902	33406.983746	59.579418
2311.778949	33227.085168	59.584423
2311.329354	33054.994658	59.589428
2310.275402	32884.583747	59.594433
2310.058975	32706.994874	59.599437
2309.066283	32530.412853	59.604442
2308.699719	32341.138126	59.609447
2307.613112	32173.159180	59.614452
2307.015927	31999.987289	59.619457
2306.422190	31811.551103	59.624461
2305.929218	31644.957759	59.629466
2305.320264	31463.266213	59.634471
2304.605003	31282.581170	59.639476
2303.676977	31112.294913	59.644481
2303.286195	30930.870114	59.649485
2302.333877	30749.071797	59.654490
2301.906424	30581.159328	59.659495
2300.806945	30408.301835	59.664500
2300.148836	30235.222879	59.669505
2299.525272	30059.397180	59.674509
2299.022067	29885.760090	59.679514
2298.190269	29724.784444	59.684519
2297.829903	29548.149805	59.689524
2297.051513	29376.568430	59.694529
2296.636037	29201.213466	59.699533
2295.348912	29030.912487	59.704538
2295.030038	28852.313218	59.709543
2294.750192	28680.489417	59.714548
2293.696219	28515.362874	59.719553
2293.300851	28330.902368	59.724557
2292.290206	28164.797668	59.729562
2291.934360	27990.136658	59.734567
2291.156131	27815.234854	59.739572
2290.431853	27637.681645	59.744577
2289.858799	27458.220025	59.749581
2289.036381	27300.082092	59.754586
2288.188280	27119.354982	59.759591
2287.885110	26955.913530	59.764596
2286.956059	26786.760908	59.769601
2286.436916	26615.396526	59.774605
2285.195532	26439.352342	59.779610
2284.908458	26276.014711	59.784615
2284.334297	26108.318383	59.789620
2283.607874	25940.359646	59.794625
2283.203819	25769.752122	59.799629
2282.250527	25604.749778	59.804634
2281.644667	25423.596400	59.809639
2281.191503	25253.977559	59.814644
2280.215289	25086.074440	59.819649
2279.680564	24916.404164	59.824653
2279.089977	24752.927888	59.829658
2278.801453	24576.125786	59.834663
2277.794412	24404.125385	59.839668
2277.151132	24238.287820	59.844673
2276.572042	24070.590571	59.849677
2275.949583	23902.713991	59.854682
2275.096966	23729.608829	59.859687
2274.379919	23556.322137	59.864692
2273.791016	23392.220552	59.869697
2273.415124	23222.933112	59.874701
2272.484968	23045.591818	59.879706
2271.719599	22874.005440	59.884711
2271.047674	22711.458419	59.889716
2270.502084	22542.004529	59.894721
2269.982551	22361.315060	59.899725
2269.096561	22203.073837	59.904730
2268.208167	22025.892039	59.909735
2267.847827	21855.037315	59.914740
2267.157373	21700.519372	59.919745
2266.677492	21524.413880	59.924750
2265.989102	21359.877586	59.929754
2264.985786	21189.934277	59.934759
2264.348586	21020.017624	59.939764
2263.646295	20856.484468	59.944769
2263.091860	20683.546730	59.949774
2262.312691	20526.691031	59.954778
2261.746618	20358.219102	59.959783
2261.150865	20190.796707	59.964788
2260.202007	20025.627883	59.969793
2259.892480	19849.365565	59.974798
2259.081958	19690.474245	59.979802
2258.267670	19529.769179	59.984807
2257.654637	19359.691277	59.989812
2257.049846	19205.369279	59.994817
2256.544605	19036.383898	59.999822
2255.327237	18878.397076	60.004826
2254.839196	18715.364927	60.009831
2254.630033	18538.913465	60.014836
2253.723365	18386.456128	60.019841
2253.215347	18224.839897	60.024846
2252.395493	18065.729258	60.029850
2251.797942	17891.696150	60.034855
2251.144605	17728.151819	60.039860
2250.815930	17558.986203	60.044865
2250.017885	17382.544084	60.049870
2249.549614	17224.107389	60.054874
2248.510869	17059.747039	60.059879
2248.074519	16896.248444	60.064884
2247.084373	16731.685705	60.069889
2246.746283	16554.845286	60.074894
2246.062126	16387.219805	60.079898
2244.986374	16221.882710	60.084903
2244.496938	16061.038221	60.089908
2243.652412	15904.895920	60.094913
2243.365856	15740.341986	60.099918
2242.289235	15583.887685	60.104922
2241.636930	15418.864943	60.109927
2241.343352	15241.745692	60.114932
2240.456333	15087.909581	60.119937
2239.670492	14928.224375	60.124942
2239.130966	14775.550009	60.129946
2238.247321	14604.706170	60.134951
2237.627579	14447.476585	60.139956
2237.051564	14281.091582	60.144961
2236.877764	14120.141623	60.149966
2235.752397	13965.486022	60.154970
2235.226846	13795.432738	60.159975
2234.369455	13641.947309	60.164980
2233.588955	13477.997694	60.169985
2233.038698	13320.926141	60.174990
2232.381230	13156.909457	60.179994
2231.993142	13006.340065	60.184999
2231.297624	12842.893384	60.190004
2230.752982	12692.389891	60.195009
2230.260346	12521.437526	60.200014
2229.639087	12355.281972	60.205018
2228.188792	12186.143636	60.210023
2227.965874	12018.088138	60.215028
2227.129181	11864.066302	60.220033
2226.673007	11698.119005	60.225038
2225.850949	11543.266427	60.230042
2225.232406	11382.443771	60.235047
2224.421996	11219.996298	60.240052
2223.468371	11073.802918	60.245057
2223.274280	10903.493040	60.250062
2222.386155	10754.679816	60.255066
2221.698820	10599.627268	60.260071
2221.070910	10446.759132	60.265076
2219.955832	10293.679050	60.270081
2219.556744	10145.420147	60.275086
2218.924806	9988.008325	60.280090
2218.159721	9834.739664	60.285095
2217.666421	9678.056691	60.290100
2216.535343	9535.468404	60.295105
2216.086170	9377.803338	60.300110
2215.156142	9228.577985	60.305114
2214.480426	9076.060684	60.310119
2214.051929	8927.227808	60.315124
2213.290724	8783.183922	60.320129
2212.699769	8633.358367	60.325134
2211.762306	8491.048653	60.330138
2211.360106	8346.298320	60.335143
2210.836629	8198.375692	60.340148
2209.733958	8056.752710	60.345153
2209.317167	7902.758082	60.350158
2208.673260	7764.196402	60.355162
2207.726935	7619.054196	60.360167
2207.318362	7477.083178	60.365172
2206.402236	7333.871013	60.370177
2205.359731	7187.708451	60.375182
2205.018298	7061.317185	60.380186
2204.517937	6912.287264	60.385191
2203.590145	6775.493631	60.390196
2202.651515	6636.943769	60.395201
2202.228619	6490.986328	60.400206
2201.519260	6370.743045	60.405210
2200.827466	6238.946688	60.410215
2200.252049	6095.158667	60.415220
2199.395850	5965.348737	60.420225
2198.728359	5840.025302	60.425230
2197.544868	5723.805855	60.430234
2196.988595	5606.857534	60.435239
2196.269961	5472.489600	60.440244
2195.339392	5360.697572	60.445249
2194.969391	5238.754654	60.450254
2193.976871	5131.781947	60.455258
2192.904543	5012.150702	60.460263
2192.219090	4899.670923	60.465268
2190.896807	4801.291543	60.470273
2190.049871	4705.210830	60.475278
2188.754108	4623.126936	60.480282
2187.845187	4541.333124	60.485287
2187.293180	4458.127252	60.490292
2186.142501	4392.696886	60.495297
2185.979937	4317.741184	60.500302
2184.923081	4248.143770	60.505306
2183.653517	4191.036362	60.510311
2183.156867	4128.088133	60.515316
2182.052130	4059.579000	60.520321
2181.808863	4012.211330	60.525326
2180.565148	3959.880484	60.530330
2179.853507	3900.351809	60.535335
2179.665364	3842.843861	60.540340
2178.551218	3799.294481	60.545345
2178.125449	3750.642585	60.550350
2177.534659	3704.940041	60.555354
2176.837338	3644.434476	60.560359
2176.334214	3605.758452	60.565364
2175.971222	3557.949047	60.570369
2175.252435	3495.488329	60.575374
2174.350888	3447.187394	60.580378
2173.831744	3395.800464	60.585383
2173.622193	3339.387867	60.590388
2172.599583	3297.065296	60.595393
2172.049755	3240.756755	60.600398
2171.443107	3193.412301	60.605402
2170.758849	3141.380487	60.610407
2170.346661	3080.970018	60.615412
2169.534896	3034.642117	60.620417
2169.384090	2965.737494	60.625422
2168.001412	2917.193647	60.630426
2167.443475	2867.558491	60.635431
2167.246466	2809.092215	60.640436
2166.146086	2773.056625	60.645441
2165.699183	2710.083688	60.650446
2165.071981	2664.453249	60.655450
2164.553604	2606.316380	60.660455
2163.977990	2557.778166	60.665460
2163.281146	2506.689895	60.670465
2162.677741	2457.000249	60.675470
2161.957408	2400.753526	60.680474
2161.145438	2344.780236	60.685479
2161.079963	2278.911060	60.690484
2159.953983	2224.676547	60.695489
2159.594463	2183.590311	60.700494
2158.799391	2125.235056	60.705498
2158.036801	2063.445891	60.710503
2157.575906	2008.549084	60.715508
2156.806355	1966.722533	60.720513
2156.205054	1900.721623	60.725518
2155.790418	1840.956219	60.730522
2155.065241	1785.208673	60.735527
2154.674059	1730.040026	60.740532
2153.596807	1679.179033	60.745537
2152.626445	1619.991651	60.750542
2151.986629	1573.503082	60.755546
2151.633856	1520.344818	60.760551
2151.105790	1463.176121	60.765556
2150.019798	1411.805644	60.770561
2149.602253	1353.969242	60.775566
2148.638650	1314.053003	60.780570
2148.069786	1252.257029	60.785575
2147.602182	1198.801140	60.790580
2146.839056	1162.372981	60.795585
2146.233754	1106.265969	60.800590
2145.260170	1060.818512	60.805594
2144.609376	1004.055126	60.810599
2144.129654	963.962917	60.815604
2143.299806	922.701720	60.820609
2142.812206	871.354908	60.825614
2142.157507	832.440564	60.830618
2141.459747	777.895871	60.835623
2140.616622	722.920236	60.840628
2139.776539	680.898019	60.845633
2139.438017	633.157351	60.850638
2138.453284	599.032874	60.855642
2137.815722	559.887859	60.860647
2137.288313	509.330098	60.865652
2136.554078	480.624510	60.870657
2136.274814	424.613481	60.875662
2135.557240	391.359450	60.880666
2134.689864	335.567463	60.885671
2133.940694	296.283158	60.890676
2132.807324	254.839401	60.895681
2132.439958	225.125916	60.900686
2131.524301	186.721524	60.905690
2130.751442	154.519252	60.910695
2130.440413	124.715026	60.915700
2129.149624	98.649409	60.920705
2128.649930	56.930613	60.925710
2127.905782	45.820313	60.930714
2127.154774	13.137041	60.935719
2126.170615	-11.068801	60.940724
2125.068480	-33.920123	60.945729
2124.102481	-49.888716	60.950734
2123.004728	-36.728891	60.955738
2122.247360	-40.301902	60.960743
2120.627896	-13.337396	60.965748
2118.774410	22.833270	60.970753
2118.804139	28.403677	60.975758
2118.726321	42.716986	60.980762
2118.727524	36.973413	60.985767
2118.922499	45.420958	60.990772
2118.546251	46.146426	60.995777
2118.422865	32.340226	61.000782
2117.393449	28.528076	61.005786
2115.861131	40.750773	61.010791
2114.896806	46.786454	61.015796
2114.047887	50.353082	61.020801
2113.378783	52.273119	61.025806
2113.025447	61.556784	61.030810
2112.694134	61.292617	61.035815
2112.292878	50.413353	61.040820
2111.745519	63.452812	61.045825
2111.072301	60.965633	61.050830
2110.111666	60.203628	61.055834
2109.045807	70.325814	61.060839
2109.042410	73.431823	61.065844
2108.219488	74.641365	61.070849
2107.676366	70.629028	61.075854
2106.718609	71.806347	61.080858
2106.208622	75.264001	61.085863
2106.103939	65.730206	61.090868
2105.275148	77.111117	61.095873
2104.286133	68.635502	61.100878
2103.605634	80.992738	61.105882
2102.501066	76.500180	61.110887
2102.604984	77.466441	61.115892
2101.656954	81.506155	61.120897
2101.252686	78.370705	61.125902
2100.110785	85.970641	61.130906
2099.748560	84.325147	61.135911
2099.928132	80.972458	61.140916
2099.160908	83.737605	61.145921
2098.292641	80.402959	61.150926
2097.229898	75.277674	61.155930
2096.196319	83.010240	61.160935
2095.755662	73.610188	61.165940
2094.729474	80.814843	61.170945
2094.556297	75.419072	61.175950
2094.614195	84.055557	61.180954
2093.743372	75.233160	61.185959
2092.914376	77.001948	61.190964
2092.408806	86.998962	61.195969
2091.635056	74.015076	61.200974
2090.174005	86.458339	61.205978
2089.819283	84.136675	61.210983
2089.499035	86.616412	61.215988
2087.993523	81.848420	61.220993
2088.245024	79.170336	61.225998
2087.492654	73.934297	61.231002
2086.562772	87.602224	61.236007
2086.221592	78.561724	61.241012
2085.466609	79.809380	61.246017
2084.989913	74.299341	61.251022
2084.232286	75.173654	61.256026
2083.278730	85.885202	61.261031
2082.590810	72.655873	61.266036
2081.870636	84.486365	61.271041
2081.775490	75.572414	61.276046
2081.308065	82.981732	61.281050
2080.821837	85.667595	61.286055
2079.625053	81.404160	61.291060
2078.656114	91.026831	61.296065
2078.476338	90.645573	61.301070
2077.889194	80.177444	61.306074
2076.947637	86.556493	61.311079
2076.334928	86.005806	61.316084
2075.505786	88.769747	61.321089
2074.792746	76.056948	61.326094
2074.325848	83.953494	61.331098
2073.514505	84.207089	61.336103
2073.004352	84.329301	61.341108
2072.023553	91.933646	61.346113
2071.812895	82.583832	61.351118
2071.440796	81.591234	61.356122
2070.249702	95.767435	61.361127
2070.019569	82.090110	61.366132
2069.051843	85.582568	61.371137
2068.820756	77.740512	61.376142
2067.870216	84.658764	61.381146
2066.867086	87.297345	61.386151
2067.054411	84.045934	61.391156
2065.600730	98.222810	61.396161
2065.247119	87.414822	61.401166
2065.067628	85.374455	61.406170
2063.963364	90.259048	61.411175
2063.013875	81.220471	61.416180
2061.765798	82.204170	61.421185
2062.171231	80.583515	61.426190
2061.582246	85.536150	61.431194
2060.950218	83.649611	61.436199
2060.355705	80.694183	61.441204
2058.505000	89.971068	61.446209
2058.169824	80.081164	61.451214
2058.337762	88.641832	61.456218
2057.652443	88.569482	61.461223
2057.136740	82.144637	61.466228
2055.516903	85.052998	61.471233
2055.278211	76.860468	61.476238
2055.232356	76.000611	61.481242
2053.717769	85.514329	61.486247
2052.962161	76.683124	61.491252
2052.919068	84.796280	61.496257
2052.353257	81.009921	61.501262
2051.325123	78.460805	61.506266
2050.275289	83.738912	61.511271
2050.550345	78.481754	61.516276
2049.575377	91.888748	61.521281
2048.673929	86.015591	61.526286
2047.744595	81.048938	61.531290
2047.618257	87.476817	61.536295
2046.726465	80.148084	61.541300
2046.046635	83.744677	61.546305
2045.719313	76.409941	61.551310
2044.821617	78.670649	61.556314
2044.174576	83.976298	61.561319
2043.422805	75.671226	61.566324
2042.435710	81.835145	61.571329
2042.070353	82.017965	61.576334
2042.267291	86.082571	61.581338
2041.313011	82.009340	61.586343
2040.652742	79.187364	61.591348
2039.863496	78.193165	61.596353
2039.324570	78.231635	61.601358
2038.414276	77.084750	61.606362
2036.986205	81.077664	61.611367
2037.117024	78.805110	61.616372
2036.299166	86.107616	61.621377
2035.764306	79.378292	61.626382
2034.555535	76.916206	61.631386
2034.300300	88.204528	61.636391
2033.725112	83.071277	61.641396
2032.578256	87.063719	61.646401
2032.449798	75.422022	61.651406
2031.647235	77.129859	61.656410
2030.600212	80.240651	61.661415
2030.594251	80.968865	61.666420
2029.734267	80.107330	61.671425
2028.900383	81.682936	61.676430
2028.414476	77.879170	61.681434
2027.513908	75.254621	61.686439
2027.235247	74.442755	61.691444
2026.022687	85.972915	61.696449
2025.851704	78.004624	61.701454
2025.425210	74.407486	61.706458
2024.724573	78.355914	61.711463
2024.474676	75.941925	61.716468
2023.375152	80.996100	61.721473
2022.805028	77.653586	61.726478
2021.733441	78.610867	61.731482
2020.772671	86.453335	61.736487
2020.289159	77.181536	61.741492
2019.405871	82.904758	61.746497
2019.037904	80.239833	61.751502
2018.486761	87.627751	61.756506
2017.956413	86.062575	61.761511
2017.560153	84.925576	61.766516
2016.795293	87.889080	61.771521
2016.523237	82.737684	61.776526
2015.974976	85.774047	61.781530
2014.716377	80.127916	61.786535
2013.852460	77.223147	61.791540
2012.847661	89.212378	61.796545
2012.693944	75.153913	61.801550
2011.891378	77.656592	61.806554
2010.797802	86.368598	61.811559
2010.575932	72.846112	61.816564
2009.599972	80.637371	61.821569
2008.987692	77.355172	61.826574
2008.698622	79.213338	61.831578
2008.011281	80.048129	61.836583
2007.733650	75.227227	61.841588
2007.166608	80.460256	61.846593
2006.605476	78.620830	61.851598
2005.362646	74.885172	61.856602
2004.402728	87.862402	61.861607
2003.953701	77.785566	61.866612
2003.225522	81.025542	61.871617
2002.537138	82.854046	61.876622
2002.448444	86.170725	61.881626
2001.543505	79.135853	61.886631
2001.259431	77.203563	61.891636
2000.228298	84.751255	61.896641
1999.089482	77.583186	61.901646
1998.550992	78.440087	61.906650
1997.423032	76.138668	61.911655
1997.902828	76.199959	61.916660
1996.804137	84.677799	61.921665
1996.419153	82.827762	61.926670
1995.592036	77.567345	61.931674
1995.015156	83.997347	61.936679
1994.595713	79.873935	61.941684
1993.559546	88.857551	61.946689
1992.512902	81.782093	61.951694
1991.800447	84.456567	61.956698
1990.940815	82.153560	61.961703
1991.522573	78.639251	61.966708
1990.145988	76.083968	61.971713
1989.584348	83.255921	61.976718
1989.072643	79.907296	61.981722
1988.440787	80.738016	61.986727
1987.777118	72.781704	61.991732
1987.172689	76.531930	61.996737
1986.004016	74.672246	62.001742
1985.195177	65.606657	62.006746
1984.097373	79.772792	62.011751
1984.659016	74.752434	62.016756
1983.723276	75.724438	62.021761
1983.143491	77.231335	62.026766
1982.652621	79.925835	62.031770
1982.139370	77.078961	62.036775
1981.249728	70.229344	62.041780
1980.082557	78.065155	62.046785
1979.273630	77.323274	62.051790
1978.878903	74.648412	62.056794
1977.988639	83.802847	62.061799
1977.831896	74.387722	62.066804
1977.149216	79.651728	62.071809
1976.498456	79.769468	62.076814
1975.986664	79.127088	62.081818
1975.345056	83.547159	62.086823
1974.435016	75.101646	62.091828
1973.478028	80.811346	62.096833
1972.684176	74.818636	62.101838
1972.218879	69.505526	62.106842
1971.733022	82.193026	62.111847
1971.076170	65.902484	62.116852
1970.304705	79.239330	62.121857
1969.673434	73.044183	62.126862
1969.330104	73.318141	62.131866
1968.817579	72.571792	62.136871
1968.562976	68.040575	62.141876
1966.875473	73.503516	62.146881
1966.427078	70.160619	62.151886
1966.027112	75.477524	62.156890
1965.225346	80.285744	62.161895
1965.084054	76.286929	62.166900
1963.589772	78.353766	62.171905
1962.592775	70.898262	62.176910
1961.941234	75.427150	62.181914
1961.696496	76.631690	62.186919
1961.023026	77.448521	62.191924
1960.274660	80.287986	62.196929
1959.862580	71.421211	62.201934
1959.620676	75.851954	62.206938
1958.753382	71.668751	62.211943
1958.436610	69.938789	62.216948
1957.326087	76.749993	62.221953
1956.792333	72.542229	62.226958
1955.921453	63.798759	62.231962
1955.148103	79.484140	62.236967
1954.838519	70.006547	62.241972
1954.071065	77.394113	62.246977
1953.511511	68.464015	62.251982
1952.571770	69.536019	62.256986
1951.642615	70.231005	62.261991
1951.033553	61.816582	62.266996
1950.384911	66.414401	62.272001
1950.383593	68.879790	62.277006
1949.631352	66.400470	62.282010
1948.801378	75.263043	62.287015
1948.501007	71.256367	62.292020
1947.387397	72.214040	62.297025
1946.776583	65.228706	62.302030
1946.169815	72.152341	62.307034
1945.321114	73.102656	62.312039
1945.203776	71.033510	62.317044
1943.671101	72.723229	62.322049
1942.804564	71.293448	62.327054
1942.675004	68.961298	62.332058
1941.960499	76.987052	62.337063
1941.795301	64.165268	62.342068
1940.884383	70.515829	62.347073
1939.984768	67.263495	62.352078
1939.988057	69.009017	62.357082
1939.010742	69.542908	62.362087
1938.134915	65.952464	62.367092
1936.955469	74.745932	62.372097
1936.503693	66.024250	62.377102
1935.912148	64.971888	62.382106
1935.295027	73.250280	62.387111
1935.298670	65.068196	62.392116
1934.683116	70.976028	62.397121
1933.515316	71.557508	62.402126
1932.270779	69.470182	62.407130
1931.700662	72.289239	62.412135
1931.368107	65.762815	62.417140
1930.859889	66.832556	62.422145
1930.267709	72.411805	62.427150
1929.847659	68.865708	62.432154
1929.620353	66.903914	62.437159
1928.602870	65.797742	62.442164
1927.866340	72.864991	62.447169
1927.310883	66.645207	62.452174
1926.589395	77.225322	62.457178
1925.383258	70.257229	62.462183
1924.490346	63.253606	62.467188
1923.972753	70.424877	62.472193
1923.703978	68.704648	62.477198
1923.015628	65.412473	62.482202
1922.222463	75.071928	62.487207
1922.006007	63.575127	62.492212
1921.500357	78.956220	62.497217
1920.063838	71.174673	62.502222
1919.383323	81.704129	62.507226
1918.842380	72.321625	62.512231
1918.978656	71.016514	62.517236
1918.123231	78.011174	62.522241
1916.863630	74.532130	62.527246
1916.166535	66.384021	62.532250
1915.289866	66.154419	62.537255
1915.051973	74.008308	62.542260
1914.205073	68.746334	62.547265
1914.065567	70.257467	62.552270
1913.774041	68.607087	62.557274
1912.253806	69.474781	62.562279
1911.686176	74.903471	62.567284
1910.691026	75.828158	62.572289
1910.414689	69.955173	62.577294
1910.224936	68.104121	62.582298
1909.224407	76.567977	62.587303
1908.308194	76.224799	62.592308
1907.454549	71.853356	62.597313
1907.018392	74.659036	62.602318
1906.256575	75.135070	62.607322
1905.859578	72.443233	62.612327
1905.541681	69.462855	62.617332
1904.927864	75.430345	62.622337
1903.687585	76.023347	62.627342
1902.898511	77.763774	62.632346
1901.905155	85.450589	62.637351
1901.685537	73.783964	62.642356
1900.896780	81.320014	62.647361
1900.589137	79.719505	62.652366
1900.337524	74.596426	62.657370
1899.711146	75.218126	62.662375
1899.054005	71.127744	62.667380
1898.154570	84.267290	62.672385
1897.501369	78.599227	62.677390
1896.441981	76.230192	62.682394
1895.214548	81.252679	62.687399
1894.736246	75.988961	62.692404
1894.382402	80.568376	62.697409
1893.939589	72.236388	62.702414
1893.415409	75.779913	62.707418
1893.218585	78.418278	62.712423
1892.586067	76.497167	62.717428
1891.144443	77.508520	62.722433
1890.600630	72.635276	62.727438
1890.081804	64.955645	62.732442
1889.355861	73.798559	62.737447
1889.093865	71.919552	62.742452
1887.724358	78.875986	62.747457
1887.062659	78.019290	62.752462
1886.573145	69.757802	62.757466
1885.860176	72.112240	62.762471
1885.811532	69.929683	62.767476
1884.601920	68.737332	62.772481
1884.138517	70.995372	62.777486
1883.236549	71.837462	62.782490
1882.307648	72.814723	62.787495
1881.910043	71.144918	62.792500
1881.081760	71.763984	62.797505
1880.966519	72.228834	62.802510
1880.591732	67.910689	62.807514
1879.456280	78.337329	62.812519
1878.480215	69.452884	62.817524
1877.769400	76.113914	62.822529
1877.507452	67.936153	62.827534
1876.848900	80.529643	62.832538
1876.398661	85.409813	62.837543
1876.193734	75.325799	62.842548
1874.640219	71.510221	62.847553
1873.933478	69.523625	62.852558
1873.384451	67.641307	62.857562
1872.686986	73.513267	62.862567
1872.370314	66.282544	62.867572
1871.319177	73.590581	62.872577
1870.584113	72.613065	62.877582
1869.804000	66.679720	62.882586
1869.166552	79.891217	62.887591
1868.870054	65.260914	62.892596
1868.342643	76.338534	62.897601
1867.962252	74.301698	62.902606
1867.658409	70.178885	62.907610
1866.490586	77.237354	62.912615
1865.604374	68.764453	62.917620
1865.194713	74.166491	62.922625
1864.184318	73.637997	62.927630
1863.256218	75.463592	62.932634
1862.473358	85.014189	62.937639
1862.260503	76.961104	62.942644
1861.544148	77.117675	62.947649
1861.181748	69.749124	62.952654
1860.735877	73.715486	62.957658
1859.465026	69.258910	62.962663
1858.942771	74.453308	62.967668
1858.440949	74.347143	62.972673
1857.861231	72.750416	62.977678
1856.966286	66.325921	62.982682
1855.764101	71.137818	62.987687
1855.159681	63.183188	62.992692
1854.668703	77.327121	62.997697
1854.246672	76.489151	63.002702
1853.795786	66.183988	63.007706
1853.359080	72.566516	63.012711
1853.212576	69.749754	63.017716
1851.742640	74.200443	63.022721
1850.732766	65.515360	63.027726
1850.284047	65.083777	63.032730
1849.712509	71.790508	63.037735
1849.383323	66.078900	63.042740
1848.278902	71.151260	63.047745
1847.567950	68.230149	63.052750
1847.230729	69.693826	63.057754
1846.335215	71.112105	63.062759
1846.241395	64.191375	63.067764
1845.326855	73.174638	63.072769
1844.244980	67.282910	63.077774
1843.761700	63.560779	63.082778
1843.025582	70.648480	63.087783
1842.805064	69.869984	63.092788
1841.844893	77.945805	63.097793
1840.446003	76.908117	63.102798
1840.223122	72.207867	63.107802
1839.417256	78.011888	63.112807
1839.170639	79.871213	63.117812
1838.430271	74.037228	63.122817
1838.324408	74.735570	63.127822
1837.918385	71.613068	63.132826
1836.518853	74.732593	63.137831
1835.967410	71.093830	63.142836
1835.406900	74.941196	63.147841
1834.654658	75.865189	63.152846
1833.811651	79.178637	63.157850
1832.639945	73.135586	63.162855
1832.381307	73.205289	63.167860
1831.735108	82.403008	63.172865
1831.335973	71.373649	63.177870
1831.321396	73.284443	63.182874
1830.160906	82.809849	63.187879
1829.019320	68.711167	63.192884
1828.417941	79.466203	63.197889
1828.144260	67.931193	63.202894
1827.681613	72.442729	63.207898
1826.092924	82.039287	63.212903
1825.443576	74.779390	63.217908
1824.822551	68.402879	63.222913
1824.184199	67.012603	63.227918
1824.098672	79.456752	63.232922
1823.394698	76.151315	63.237927
1823.402076	73.575063	63.242932
1822.439734	75.123818	63.247937
1821.592328	75.824792	63.252942
1821.116518	69.032536	63.257946
1819.872729	81.651155	63.262951
1818.796744	75.253843	63.267956
1817.834619	79.023055	63.272961
1817.862716	74.456427	63.277966
1817.553097	78.618792	63.282970
1816.586857	79.250324	63.287975
1816.350570	67.393969	63.292980
1815.796399	81.767152	63.297985
1814.850244	73.880991	63.302990
1814.131774	75.091381	63.307994
1812.931710	79.726331	63.312999
1813.136163	69.433812	63.318004
1812.473266	74.032346	63.323009
1811.596921	66.748577	63.328014
1810.744325	64.149611	63.333018
1810.066906	68.248948	63.338023
1809.624214	67.008966	63.343028
1808.867220	65.325279	63.348033
1807.976007	68.091265	63.353038
1807.211501	65.292219	63.358042
1806.458198	78.678248	63.363047
1806.268664	64.817925	63.368052
1805.840531	70.934150	63.373057
1805.183369	70.647647	63.378062
1804.238132	76.486426	63.383066
1803.186807	66.054267	63.388071
1803.008285	61.162466	63.393076
1802.546851	74.588879	63.398081
1801.969292	63.803924	63.403086
1800.765835	60.595166	63.408090
1799.901153	65.145316	63.413095
1799.718708	56.194813	63.418100
1799.070742	63.908803	63.423105
1798.155711	68.451179	63.428110
1797.311104	63.250393	63.433114
1796.196201	71.038540	63.438119
1795.953257	66.819330	63.443124
1795.496917	75.062748	63.448129
1795.158728	66.917613	63.453134
1795.067248	63.385601	63.458138
1793.604882	72.887986	63.463143
1793.050491	54.573676	63.468148
1792.502032	63.554006	63.473153
1791.710812	70.081153	63.478158
1790.870823	63.567529	63.483162
1789.403188	77.991154	63.488167
1789.272489	70.090629	63.493172
1788.672020	72.832527	63.498177
1788.297126	75.917094	63.503182
1788.363182	73.872454	63.508186
1787.479471	72.967458	63.513191
1786.779386	69.667724	63.518196
1785.643358	72.685499	63.523201
1785.145444	70.167417	63.528206
1784.900133	70.187697	63.533210
1783.408597	75.882991	63.538215
1782.656079	67.000940	63.543220
1781.777241	78.151727	63.548225
1781.572279	70.206222	63.553230
1781.553637	67.651453	63.558234
1780.896912	78.751195	63.563239
1780.187704	66.183007	63.568244
1779.211969	77.823874	63.573249
1778.533841	65.082008	63.578254
1777.609925	73.899609	63.583258
1776.497010	75.778241	63.588263
1776.185709	60.106311	63.593268
1775.490618	63.706960	63.598273
1775.160973	69.578874	63.603278
1774.836760	64.721252	63.608282
1774.096967	61.014644	63.613287
1773.481891	60.969063	63.618292
1772.480138	76.452602	63.623297
1772.047603	63.747433	63.628302
1771.354545	65.548346	63.633306
1770.149292	67.321788	63.638311
1769.432842	65.180638	63.643316
1768.766568	67.067190	63.648321
1768.332733	70.733589	63.653326
1768.056989	63.751870	63.658330
1767.476302	69.797704	63.663335
1766.947008	67.393426	63.668340
1765.597356	73.510923	63.673345
1765.096639	75.345950	63.678350
1764.873865	58.779971	63.683354
1764.015332	71.845224	63.688359
1763.196416	73.044771	63.693364
1762.022050	68.766901	63.698369
1761.782989	66.881113	63.703374
1761.373484	62.480193	63.708378
1760.774692	71.610459	63.713383
1760.684978	69.188411	63.718388
1759.118594	61.099570	63.723393
1758.485253	64.434933	63.728398
1758.036820	59.625433	63.733402
1757.521214	64.047608	63.738407
1756.754843	69.479498	63.743412
1755.863325	70.689001	63.748417
1755.134049	68.702865	63.753422
1754.820968	68.306531	63.758426
1753.964561	64.484400	63.763431
1753.650142	71.120343	63.768436
1752.448327	74.785709	63.773441
1751.897872	70.134345	63.778446
1751.650377	66.046759	63.783450
1751.135052	77.579814	63.788455
1750.157308	58.167316	63.793460
1749.523021	59.870585	63.798465
1748.792632	68.373584	63.803470
1748.155232	61.044009	63.808474
1746.961419	73.911767	63.813479
1746.150824	58.896349	63.818484
1745.354407	70.552896	63.823489
1745.050519	60.636032	63.828494
1744.942017	62.310990	63.833498
1744.179768	72.851870	63.838503
1744.238666	60.989656	63.843508
1743.259723	69.726111	63.848513
1742.442799	69.334104	63.853518
1741.713874	61.918136	63.858522
1740.673008	67.589181	63.863527
1739.837419	65.487464	63.868532
1738.931168	68.544460	63.873537
1738.534957	65.981849	63.878542
1737.939223	67.494483	63.883546
1737.467642	64.090659	63.888551
1737.433816	62.669048	63.893556
1736.654519	69.088651	63.898561
1735.398914	65.684768	63.903566
1735.068148	68.390147	63.908570
1734.367505	70.696931	63.913575
1733.288908	69.843410	63.918580
1732.051446	72.129795	63.923585
1731.617141	73.547401	63.928590
1731.443110	70.739753	63.933594
1730.837389	73.047231	63.938599
1730.546941	70.322733	63.943604
1729.905082	71.748072	63.948609
1728.964044	64.461998	63.953614
1728.207536	69.556417	63.958618
1727.365057	75.501906	63.963623
1727.286588	67.952662	63.968628
1726.918854	71.682688	63.973633
1725.760337	59.466609	63.978638
1724.964372	58.101394	63.983642
1724.322618	75.035420	63.988647
1724.075076	66.088956	63.993652
1722.707729	68.985792	63.998657
1722.133620	64.711955	64.003662
1721.645174	70.686371	64.008666
1721.334138	70.428497	64.013671
1720.579017	69.105683	64.018676
1719.280988	64.549416	64.023681
1718.419898	73.140997	64.028686
1718.338419	65.783056	64.033690
1717.769372	66.370458	64.038695
1717.639228	70.234645	64.043700
1716.490355	66.649805	64.048705
1715.559146	63.356842	64.053710
1715.291757	60.124030	64.058714
1714.514828	70.637281	64.063719
1713.802497	54.544922	64.068724
1712.697953	65.107053	64.073729
1712.063923	68.543467	64.078734
1711.776740	63.430802	64.083738
1711.412621	69.243537	64.088743
1710.779535	65.630392	64.093748
1709.575474	65.733577	64.098753
1708.911770	67.266476	64.103758
1708.659146	57.309939	64.108762
1707.640678	66.909018	64.113767
1707.409748	58.466155	64.118772
1705.937321	64.540095	64.123777
1705.246138	65.227330	64.128782
1705.226736	52.589040	64.133786
1704.439118	72.503198	64.138791
1704.538897	53.061511	64.143796
1703.304050	70.509237	64.148801
1702.477599	69.265572	64.153806
1701.874794	61.086795	64.158810
1701.444253	71.940868	64.163815
1700.563241	60.245306	64.168820
1699.687212	61.010793	64.173825
1698.996056	62.953356	64.178830
1698.849543	56.015784	64.183834
1697.813504	59.213263	64.188839
1697.167817	51.031843	64.193844
1696.379599	59.417869	64.198849
1695.977020	57.931825	64.203854
1695.581157	51.270422	64.208858
1694.537256	61.416046	64.213863
1693.946522	48.750237	64.218868
1693.011019	65.932777	64.223873
1692.384189	61.714635	64.228878
1692.576954	58.260490	64.233882
1691.413460	62.754050	64.238887
1690.745417	59.737858	64.243892
1690.064954	64.917981	64.248897
1689.529005	65.526942	64.253902
1688.577109	65.088579	64.258906
1687.800625	69.517512	64.263911
1687.164862	56.992901	64.268916
1686.561582	67.757708	64.273921
1686.119823	66.924479	64.278926
1685.604448	56.382020	64.283930
1684.233946	66.483330	64.288935
1683.876234	60.817291	64.293940
1683.049128	66.359776	64.298945
1682.654338	71.877747	64.303950
1682.827308	67.146180	64.308954
1681.006988	71.343513	64.313959
1680.225702	59.983802	64.318964
1679.759289	67.785675	64.323969
1679.621795	62.838483	64.328974
1679.343409	63.870183	64.333978
1678.348475	70.620540	64.338983
1677.141770	65.136677	64.343988
1676.826779	66.016488	64.348993
1676.184778	73.641241	64.353998
1675.540668	62.592496	64.359002
1674.499508	58.176811	64.364007
1673.963935	64.551402	64.369012
1673.529995	64.429759	64.374017
1673.015935	57.588426	64.379022
1672.697110	63.040708	64.384026
1671.351807	63.893367	64.389031
1670.997437	63.836359	64.394036
1670.313277	62.883935	64.399041
1669.285726	65.403523	64.404046
1668.381837	61.172627	64.409050
1667.531665	64.925677	64.414055
1667.665147	60.004831	64.419060
1667.078641	66.098915	64.424065
1666.443545	64.577268	64.429070
1665.788026	59.007430	64.434074
1664.572255	75.542186	64.439079
1664.085517	62.973402	64.444084
1663.832518	61.204966	64.449089
1663.155023	62.703794	64.454094
1662.176786	58.697613	64.459098
1661.163470	65.356270	64.464103
1660.888783	62.712864	64.469108
1660.751135	63.025153	64.474113
1659.277388	71.815005	64.479118
1658.334743	60.160796	64.484122
1657.640710	71.760091	64.489127
1657.680496	65.690266	64.494132
1657.274326	62.935275	64.499137
1656.582705	65.262722	64.504142
1656.266982	63.568909	64.509146
1654.782965	72.365126	64.514151
1654.645763	56.389596	64.519156
1653.765072	64.014417	64.524161
1652.672891	69.655795	64.529166
1652.069209	56.875350	64.534170
1651.238979	68.049976	64.539175
1651.010114	62.242041	64.544180
1650.829950	69.500096	64.549185
1649.889252	63.729547	64.554190
1649.114520	62.067653	64.559194
1648.326341	66.414869	64.564199
1648.156184	64.764168	64.569204
1647.092190	71.500273	64.574209
1646.141330	69.916825	64.579214
1645.950878	61.530623	64.584218
1645.195071	69.965136	64.589223
1644.738890	57.435667	64.594228
1643.644520	61.498770	64.599233
1642.611749	61.590544	64.604238
1642.507944	63.138594	64.609242
1641.850706	64.086974	64.614247
1641.117578	63.184917	64.619252
1640.259129	62.851583	64.624257
1639.780131	61.798760	64.629262
1639.598337	61.550327	64.634266
1638.521468	61.649109	64.639271
1637.720403	58.740804	64.644276
1636.668174	60.262900	64.649281
1636.224695	56.644888	64.654286
1635.892891	56.267314	64.659290
1635.181379	58.273054	64.664295
1634.827850	60.201419	64.669300
1633.531700	67.084803	64.674305
1632.950165	60.230544	64.679310
1632.539300	57.821678	64.684314
1632.298703	60.463852	64.689319
1631.517408	53.269150	64.694324
1630.300856	67.047353	64.699329
1629.758255	68.073724	64.704334
1629.491232	61.406056	64.709338
1628.191519	63.763882	64.714343
1627.450493	66.187500	64.719348
1626.737084	66.130766	64.724353
1626.102530	67.181208	64.729358
1626.217659	63.148001	64.734362
1625.571789	66.977421	64.739367
1625.085600	56.901881	64.744372
1623.849435	66.742163	64.749377
1622.908814	67.992629	64.754382
1622.996105	61.778057	64.759386
1622.253374	73.072840	64.764391
1621.276360	56.387021	64.769396
1620.244776	66.167992	64.774401
1619.669366	64.485478	64.779406
1619.638464	56.804108	64.784410
1618.947584	67.652231	64.789415
1617.886894	61.585350	64.794420
1617.150566	52.596716	64.799425
1616.467683	58.218809	64.804430
1616.290262	60.134968	64.809434
1615.508183	65.504727	64.814439
1614.519036	59.152076	64.819444
1613.841891	66.093250	64.824449
1613.357505	57.094550	64.829454
1613.274985	64.531065	64.834458
1611.891430	59.209386	64.839463
1611.265059	53.581317	64.844468
1610.718656	59.851973	64.849473
1610.232838	56.786352	64.854478
1609.662118	59.302771	64.859482
1608.618678	59.061921	64.864487
1607.899930	63.489584	64.869492
1607.366596	69.341828	64.874497
1606.947841	63.381131	64.879502
1606.139226	60.310023	64.884506
1605.283932	60.507664	64.889511
1604.627289	54.565843	64.894516
1604.139657	68.023228	64.899521
1603.734743	66.092843	64.904526
1602.694025	68.663437	64.909530
1601.744337	67.620747	64.914535
1601.369667	53.606959	64.919540
1600.854048	62.637288	64.924545
1600.495868	64.867613	64.929550
1599.738212	56.473764	64.934554
1598.475338	65.883034	64.939559
1598.175816	59.824545	64.944564
1597.922075	59.357297	64.949569
1596.956970	61.732941	64.954574
1596.247068	57.841859	64.959578
1595.450877	64.144322	64.964583
1595.197323	64.025572	64.969588
1594.436236	58.374754	64.974593
1593.176340	65.214544	64.979598
1592.773091	59.558913	64.984602
1592.219553	69.874257	64.989607
1591.930020	51.823899	64.994612
1591.003550	62.554904	64.999617
1589.874840	61.799299	65.004622
1589.478658	61.689018	65.009626
1588.807348	61.840084	65.014631
1588.757184	55.872873	65.019636
1587.416192	63.242821	65.024641
1586.324688	60.495805	65.029646
1586.204160	58.712638	65.034650
1585.875517	67.460935	65.039655
1585.523684	58.256667	65.044660
1584.384523	57.163660	65.049665
1583.522506	65.244453	65.054670
1583.210047	59.473468	65.059674
1582.412085	67.944655	65.064679
1581.278791	51.127568	65.069684
1580.454859	60.864514	65.074689
1579.823290	57.700625	65.079694
1579.500118	57.555090	65.084698
1579.267916	57.604847	65.089703
1579.062632	61.211297	65.094708
1577.880553	58.396670	65.099713
1577.263417	62.734073	65.104718
1576.710642	56.368879	65.109722
1575.393427	59.732512	65.114727
1574.935034	50.270777	65.119732
1573.954831	66.386473	65.124737
1573.360388	63.844351	65.129742
1573.330291	57.459189	65.134746
1572.620086	57.950773	65.139751
1571.884743	65.934166	65.144756
1571.194468	57.472848	65.149761
1570.645125	60.932105	65.154766
1570.047224	57.404880	65.159770
1568.678869	57.784987	65.164775
1568.091440	60.885998	65.169780
1567.606005	67.452923	65.174785
1566.741680	66.067080	65.179790
1566.861852	61.194083	65.184794
1566.134612	63.188147	65.189799
1565.491153	59.400064	65.194804
1564.482421	58.887195	65.199809
1563.901434	58.497182	65.204814
1563.346415	55.611312	65.209818
1562.132815	57.662155	65.214823
1561.569407	59.377860	65.219828
1561.256699	52.808936	65.224833
1560.299010	57.432280	65.229838
1560.415730	54.034371	65.234842
1559.267337	65.355769	65.239847
1558.541189	55.763106	65.244852
1557.752403	59.902270	65.249857
1557.464334	57.852396	65.254862
1556.492698	54.922335	65.259866
1555.134161	60.602914	65.264871
1555.250834	56.646739	65.269876
1554.840113	58.103203	65.274881
1554.182743	52.363376	65.279886
1553.614736	51.103929	65.284890
1552.625232	55.303374	65.289895
1552.124296	45.469918	65.294900
1551.303470	58.245339	65.299905
1550.317575	55.752810	65.304910
1549.093297	54.790045	65.309914
1548.486317	58.286852	65.314919
1548.375167	52.334068	65.319924
1547.675256	57.395876	65.324929
1547.633388	60.113716	65.329934
1547.651008	51.997265	65.334938
1546.632395	53.532978	65.339943
1546.073129	55.309532	65.344948
1545.187133	58.232474	65.349953
1543.893999	60.512019	65.354958
1543.287412	50.334208	65.359962
1542.440444	59.086014	65.364967
1542.407109	59.492127	65.369972
1541.167647	61.032973	65.374977
1540.427617	55.131233	65.379982
1540.213829	53.599446	65.384986
1539.405122	54.357441	65.389991
1538.912072	55.125205	65.394996
1537.619435	57.360517	65.400001
1537.264965	56.081334	65.405006
1536.818095	50.574584	65.410010
1536.196417	60.186354	65.415015
1535.597108	60.258179	65.420020
1534.757463	57.359194	65.425025
1533.889655	62.174858	65.430030
1533.674547	62.034234	65.435034
1533.036448	64.703310	65.440039
1532.181640	57.954013	65.445044
1531.183432	61.828402	65.450049
1530.796147	57.848225	65.455054
1530.449184	57.083544	65.460058
1529.352540	64.651245	65.465063
1528.205412	60.069528	65.470068
1527.569176	60.577757	65.475073
1527.060988	61.866776	65.480078
1526.875675	62.172454	65.485082
1526.744621	52.065744	65.490087
1526.211690	52.764150	65.495092
1525.028172	52.786881	65.500097
1524.080391	57.746150	65.505102
1523.800235	60.665869	65.510106
1522.776903	67.110108	65.515111
1522.241050	57.900403	65.520116
1521.610225	58.989702	65.525121
1520.843942	59.305698	65.530126
1520.505725	47.822035	65.535130
1519.501284	56.892200	65.540135
1518.617767	54.433881	65.545140
1517.842612	58.853180	65.550145
1517.620189	54.848384	65.555150
1517.184185	54.821718	65.560154
1515.973591	66.015811	65.565159
1515.309715	54.798375	65.570164
1514.795026	56.638818	65.575169
1514.283824	53.198763	65.580174
1514.051670	53.333678	65.585178
1512.917763	54.499774	65.590183
1512.221068	49.955303	65.595188
1511.631591	54.635271	65.600193
1511.148570	49.090115	65.605198
1510.967613	56.561190	65.610202
1509.412819	64.980766	65.615207
1508.822543	50.288449	65.620212
1508.314225	54.372014	65.625217
1507.841279	58.547735	65.630222
1507.315422	53.629165	65.635226
1506.324590	59.697635	65.640231
1506.042315	50.898677	65.645236
1505.116444	47.819431	65.650241
1503.994511	54.045937	65.655246
1503.516196	50.772556	65.660250
1503.001863	54.634714	65.665255
1502.815407	52.974001	65.670260
1502.061348	49.277637	65.675265
1501.080978	57.027151	65.680270
1500.533558	47.989618	65.685274
1499.858616	53.022234	65.690279
1499.397668	50.298059	65.695284
1498.642230	61.826699	65.700289
1497.659711	52.893006	65.705294
1497.543545	50.232316	65.710298
1496.391257	53.853643	65.715303
1495.634468	42.483823	65.720308
1495.203957	46.719034	65.725313
1494.217554	53.069093	65.730318
1494.224472	50.551278	65.735322
1492.969681	52.228631	65.740327
1492.154424	43.339331	65.745332
1491.462171	49.694684	65.750337
1491.221137	51.482178	65.755342
1490.969151	49.891808	65.760346
1489.958191	56.042333	65.765351
1489.056392	49.103395	65.770356
1488.306083	57.936051	65.775361
1488.021385	52.237950	65.780366
1487.837342	43.207333	65.785370
1486.384628	56.496372	65.790375
1485.862732	56.929665	65.795380
1485.457607	57.697659	65.800385
1484.264148	54.566324	65.805390
1483.082085	51.034187	65.810394
1483.210977	58.437094	65.815399
1482.614447	56.505644	65.820404
1481.577599	55.161444	65.825409
1481.133479	57.610455	65.830414
1481.243198	39.761638	65.835418
1480.097863	55.514056	65.840423
1479.147058	44.906825	65.845428
1478.716913	53.653902	65.850433
1477.934921	51.904902	65.855438
1477.741565	47.018658	65.860442
1476.405573	59.607872	65.865447
1475.908587	58.551633	65.870452
1475.694340	60.983036	65.875457
1474.968119	52.145824	65.880462
1473.964231	43.382711	65.885466
1473.190635	60.156329	65.890471
1472.841215	50.842893	65.895476
1472.409567	51.287078	65.900481
1470.880703	55.998075	65.905486
1470.213738	56.020740	65.910490
1469.731511	65.711290	65.915495
1469.564309	54.290347	65.920500
1469.028937	60.258055	65.925505
1468.161507	57.611105	65.930510
1467.557915	48.377495	65.935514
1466.620294	57.861281	65.940519
1466.443864	53.563737	65.945524
1465.119403	57.575161	65.950529
1464.432118	58.471586	65.955534
1464.041128	53.514245	65.960538
1463.444760	56.452684	65.965543
1463.244266	56.795474	65.970548
1462.332724	49.273013	65.975553
1461.295361	48.930326	65.980558
1461.036166	47.109280	65.985562
1460.319375	52.178520	65.990567
1459.362421	52.960102	65.995572
1458.554402	57.108656	66.000577
1457.966860	50.452540	66.005582
1457.767560	56.485111	66.010586
1456.989376	53.508573	66.015591
1455.913694	52.626322	66.020596
1455.386636	50.440974	66.025601
1454.873752	53.615318	66.030606
1454.236243	51.553187	66.035610
1453.947080	58.341252	66.040615
1452.691481	48.045841	66.045620
1452.357014	53.593665	66.050625
1451.672183	53.360540	66.055630
1451.301374	51.576159	66.060634
1450.131986	56.083367	66.065639
1449.192108	51.061874	66.070644
1448.976754	56.478797	66.075649
1448.554286	57.475069	66.080654
1447.824506	47.375224	66.085658
1446.573669	61.146313	66.090663
1446.132820	54.435342	66.095668
1445.521716	52.982486	66.100673
1444.975433	61.265454	66.105678
1444.353113	58.093825	66.110682
1443.265008	59.331523	66.115687
1442.595151	51.450515	66.120692
1442.390143	47.446118	66.125697
1442.233076	58.157371	66.130702
1441.278240	51.545445	66.135706
1440.069912	57.773092	66.140711
1439.856252	51.284649	66.145716
1439.299048	54.308336	66.150721
1437.850113	56.371408	66.155726
1437.271466	51.965901	66.160730
1436.438738	58.799362	66.165735
1436.332118	54.230514	66.170740
1435.837243	50.188606	66.175745
1435.295880	58.559106	66.180750
1434.693987	55.073556	66.185754
1433.422260	57.617849	66.190759
1433.116547	48.366867	66.195764
1432.634417	54.977434	66.200769
1431.682572	56.407955	66.205774
1431.106952	48.701220	66.210778
1430.282352	62.615890	66.215783
1430.001933	57.475390	66.220788
1429.400108	57.041409	66.225793
1428.166405	53.828185	66.230798
1427.688444	52.899826	66.235802
1427.020224	58.871308	66.240807
1426.820958	53.063438	66.245812
1425.757469	57.132753	66.250817
1424.932044	51.755591	66.255822
1424.334100	52.959541	66.260826
1423.904631	57.186714	66.265831
1423.518994	53.646292	66.270836
1422.422241	51.381184	66.275841
1421.534580	54.236615	66.280846
1420.843832	51.962169	66.285850
1420.745635	52.118381	66.290855
1420.358794	50.415406	66.295860
1419.111634	50.241710	66.300865
1418.452805	54.521110	66.305870
1418.125291	49.654621	66.310874
1417.156194	46.801489	66.315879
1416.105037	50.386271	66.320884
1415.695864	49.475368	66.325889
1415.199814	55.432100	66.330894
1415.013042	52.553968	66.335898
1414.161670	54.145154	66.340903
1413.276055	50.234752	66.345908
1413.067564	45.958084	66.350913
1412.073813	51.192790	66.355918
1411.007436	46.703961	66.360922
1410.292096	54.942836	66.365927
1409.805129	56.521833	66.370932
1409.579750	56.630449	66.375937
1408.464110	54.448778	66.380942
1407.936030	48.462931	66.385946
1407.097978	53.641349	66.390951
1406.791494	56.872785	66.395956
1406.506701	59.678126	66.400961
1405.615545	51.759765	66.405966
1404.559052	47.963266	66.410970
1403.719801	52.492135	66.415975
1403.490099	48.561057	66.420980
1402.761735	46.649008	66.425985
1401.860398	53.567501	66.430990
1401.624614	50.747628	66.435994
1400.881636	54.773888	66.440999
1400.217041	59.183527	66.446004
1399.221988	56.544274	66.451009
1398.453101	61.796863	66.456014
1398.338058	56.934449	66.461018
1397.460193	60.144744	66.466023
1396.796559	51.893735	66.471028
1396.054080	55.202363	66.476033
1395.213733	59.595784	66.481038
1395.028318	53.454538	66.486042
1393.823290	57.142641	66.491047
1393.009663	53.504670	66.496052
1392.463373	52.743307	66.501057
1392.136787	57.165453	66.506062
1391.591622	56.574232	66.511066
1391.116626	57.577286	66.516071
1390.276613	60.259565	66.521076
1389.415339	52.128291	66.526081
1389.006014	54.682177	66.531086
1388.552734	61.464794	66.536090
1387.518608	61.392874	66.541095
1386.331828	58.733638	66.546100
1386.016134	62.266179	66.551105
1385.685092	67.848163	66.556110
1385.332636	59.722739	66.561114
1383.861070	65.091766	66.566119
1383.353155	51.769471	66.571124
1382.602836	63.319395	66.576129
1382.400556	69.658393	66.581134
1381.603191	57.695783	66.586138
1380.586361	60.183810	66.591143
1380.227217	59.091485	66.596148
1379.778073	59.650437	66.601153
1379.181556	61.472372	66.606158
1378.123596	65.807348	66.611162
1377.439810	64.528497	66.616167
1376.999625	55.890291	66.621172
1376.712795	55.634919	66.626177
1375.570954	67.346442	66.631182
1374.942398	57.244721	66.636186
1374.162351	63.386965	66.641191
1373.986291	50.597002	66.646196
1372.693960	54.615977	66.651201
1371.820841	53.990159	66.656206
1371.622638	52.304515	66.661210
1370.856815	59.373375	66.666215
1370.603318	58.524468	66.671220
1369.947149	57.239653	66.676225
1368.622115	60.973655	66.681230
1368.456781	62.501529	66.686234
1367.985989	62.239132	66.691239
1367.319912	59.147024	66.696244
1366.338531	54.849717	66.701249
1365.055569	60.368552	66.706254
1365.156321	64.093526	66.711258
1364.459859	68.396272	66.716263
1363.762491	54.120025	66.721268
1362.727462	56.934244	66.726273
1362.211070	64.679432	66.731278
1361.843258	58.705964	66.736282
1361.704255	60.885702	66.741287
1360.841709	57.436878	66.746292
1359.958735	53.768941	66.751297
1359.009044	57.031668	66.756302
1358.000570	58.950640	66.761306
1356.876247	55.568667	66.766311
1356.564541	61.887209	66.771316
1356.374215	64.511948	66.776321
1355.945165	68.411040	66.781326
1355.632438	60.066406	66.786330
1355.099703	67.667529	66.791335
1354.138084	56.003874	66.796340
1353.520313	51.528913	66.801345
1352.315655	58.926176	66.806350
1351.467888	54.372655	66.811354
1350.717875	63.216333	66.816359
1350.424995	59.736875	66.821364
1350.298664	50.839036	66.826369
1349.615242	59.810906	66.831374
1348.579649	49.917421	66.836378
1347.770073	61.733828	66.841383
1347.586368	54.967807	66.846388
1346.482780	53.342522	66.851393
1345.301763	55.561757	66.856398
1345.186561	48.515174	66.861402
1344.195939	50.967506	66.866407
1344.189704	55.903305	66.871412
1343.786629	61.029937	66.876417
1342.470313	58.156338	66.881422
1341.996263	60.466618	66.886426
1340.978543	72.834974	66.891431
1340.868597	57.829794	66.896436
1339.733886	63.533241	66.901441
1338.982855	62.788670	66.906446
1338.538778	65.218773	66.911450
1338.082696	66.510582	66.916455
1337.487309	63.142301	66.921460
1336.828630	62.151223	66.926465
1335.797586	57.354017	66.931470
1335.365898	55.366433	66.936474
1334.749510	60.143759	66.941479
1333.832023	53.522788	66.946484
1333.390092	60.207407	66.951489
1332.569619	60.607771	66.956494
1332.267418	51.356251	66.961498
1331.410516	61.448595	66.966503
1330.563018	54.805458	66.971508
1329.892020	61.928642	66.976513
1329.398841	65.229195	66.981518
1328.954109	54.981565	66.986522
1327.472459	65.283632	66.991527
1326.732854	51.689093	66.996532
1326.541017	47.934942	67.001537
1326.055918	63.948314	67.006542
1325.821469	51.815807	67.011546
1325.206792	64.661006	67.016551
1324.321368	60.676484	67.021556
1323.291147	63.496263	67.026561
1322.712707	52.000377	67.031566
1322.356538	43.506539	67.036570
1321.247655	56.433459	67.041575
1320.530911	46.277973	67.046580
1320.370069	49.812706	67.051585
1319.670317	52.572058	67.056590
1318.659961	49.657714	67.061594
1317.709079	55.141117	67.066599
1317.810220	48.875471	67.071604
1317.188927	59.327771	67.076609
1316.146614	53.740692	67.081614
1315.346999	47.624568	67.086618
1314.362761	57.549491	67.091623
1314.575192	44.741935	67.096628
1314.173854	45.493581	67.101633
1312.681994	52.173233	67.106638
1312.413184	54.734752	67.111642
1311.482116	58.311520	67.116647
1310.889632	51.962180	67.121652
1309.859008	51.175335	67.126657
1309.029095	57.357062	67.131662
1308.800224	47.414186	67.136666
1308.283384	48.649424	67.141671
1308.025513	50.855947	67.146676
1307.235746	47.341955	67.151681
1306.139132	58.686736	67.156686
1305.992108	55.646168	67.161690
1305.374219	53.538377	67.166695
1304.197393	50.548000	67.171700
1303.867979	58.933705	67.176705
1303.009037	58.035982	67.181710
1302.151639	49.197616	67.186714
1301.060839	56.778657	67.191719
1300.499649	59.803005	67.196724
1300.529433	53.799452	67.201729
1299.766944	53.274347	67.206734
1299.450424	46.504222	67.211738
1298.045321	49.747911	67.216743
1297.464709	56.661173	67.221748
1296.859667	50.104089	67.226753
1296.347242	55.311191	67.231758
1296.194409	55.479249	67.236762
1295.141845	56.930565	67.241767
1294.571473	63.928941	67.246772
1293.869097	55.895449	67.251777
1292.541453	64.026693	67.256782
1291.890990	58.382050	67.261786
1291.278486	61.297858	67.266791
1291.410746	53.978530	67.271796
1290.813206	56.040357	67.276801
1289.808041	59.906473	67.281806
1289.065175	53.421768	67.286810
1288.311428	58.443305	67.291815
1287.975771	51.412857	67.296820
1287.458610	52.626072	67.301825
1286.464849	50.469236	67.306830
1285.832218	53.374050	67.311834
1285.195836	56.981245	67.316839
1284.421129	52.655843	67.321844
1283.523148	57.485837	67.326849
1282.653730	60.180709	67.331854
1282.630525	45.333659	67.336858
1281.760017	50.935186	67.341863
1281.571562	50.875507	67.346868
1280.644819	52.567034	67.351873
1279.901591	55.429508	67.356878
1279.278951	51.343294	67.361882
1278.411141	54.758618	67.366887
1277.161494	52.751289	67.371892
1276.564097	48.452894	67.376897
1275.940870	60.859460	67.381902
1275.850262	54.655843	67.386906
1275.356443	56.092442	67.391911
1275.382090	57.596261	67.396916
1274.498621	50.495219	67.401921
1273.418817	42.359322	67.406926
1273.037849	49.191952	67.411930
1271.543765	53.036462	67.416935
1271.291207	47.916795	67.421940
1270.282338	55.733989	67.426945
1269.956159	62.452252	67.431950
1269.706011	47.453621	67.436954
1268.273902	51.551644	67.441959
1267.954230	50.910401	67.446964
1267.202151	56.067302	67.451969
1266.635558	57.507590	67.456974
1265.868453	50.542598	67.461978
1265.169070	53.147355	67.466983
1264.507756	53.539780	67.471988
1264.278160	49.793217	67.476993
1263.529732	51.938969	67.481998
1262.697230	48.116380	67.487002
1261.967267	52.209994	67.492007
1261.766163	51.414273	67.497012
1260.830353	57.691703	67.502017
1259.764012	56.732353	67.507022
1259.329579	57.386762	67.512026
1258.774676	58.612293	67.517031
1258.214151	60.881141	67.522036
1257.212001	49.933653	67.527041
1256.242591	61.051632	67.532046
1256.225655	54.785837	67.537050
1255.817759	59.492174	67.542055
1254.821494	55.231977	67.547060
1253.965554	56.465952	67.552065
1253.295027	55.942008	67.557070
1252.916095	51.047453	67.562074
1252.069205	62.264229	67.567079
1250.964812	51.763534	67.572084
1250.386420	49.993272	67.577089
1249.844722	60.549625	67.582094
1249.617701	54.807697	67.587098
1249.079672	58.563272	67.592103
1248.432066	48.269079	67.597108
1247.331305	61.593724	67.602113
1246.466708	69.782252	67.607118
1246.465256	52.520447	67.612122
1245.656451	60.299529	67.617127
1244.878043	53.186523	67.622132
1244.187615	52.348761	67.627137
1243.595444	55.297616	67.632142
1243.399129	42.924093	67.637146
1242.202170	58.752601	67.642151
1241.419629	49.829813	67.647156
1241.073586	55.590816	67.652161
1239.886768	56.082585	67.657166
1239.341812	55.436168	67.662170
1238.812636	53.937218	67.667175
1238.110910	52.815811	67.672180
1237.851033	52.646060	67.677185
1237.092661	60.100140	67.682190
1236.254396	57.768777	67.687194
1235.538390	56.496668	67.692199
1234.949245	52.422488	67.697204
1234.364395	51.815534	67.702209
1233.052737	51.516561	67.707214
1232.495164	40.119905	67.712218
1231.898871	52.503260	67.717223
1231.590165	50.324243	67.722228
1231.328853	57.331827	67.727233
1230.716566	58.443479	67.732238
1230.025310	47.126428	67.737242
1228.874460	57.434281	67.742247
1228.396255	58.511995	67.747252
1227.534122	48.810197	67.752257
1226.758403	52.102075	67.757262
1226.566689	52.107577	67.762266
1225.782712	47.361025	67.767271
1224.812719	40.373123	67.772276
1224.138094	45.642299	67.777281
1223.343548	56.306674	67.782286
1222.965082	45.222175	67.787290
1222.605124	58.427438	67.792295
1222.285889	60.396132	67.797300
1221.437292	55.784442	67.802305
1220.089426	68.164325	67.807310
1219.813628	48.558520	67.812314
1218.915793	56.274490	67.817319
1218.187411	52.705031	67.822324
1217.577391	46.107762	67.827329
1217.273578	46.530082	67.832334
1217.300055	43.646446	67.837338
1215.708935	53.363539	67.842343
1215.157777	43.564983	67.847348
1214.675411	48.526029	67.852353
1213.605499	46.649430	67.857358
1212.763281	41.174094	67.862362
1212.296020	55.030387	67.867367
1212.032777	50.689908	67.872372
1211.439769	46.387679	67.877377
1210.134803	52.466774	67.882382
1209.784938	48.559563	67.887386
1208.808689	51.216250	67.892391
1208.458190	48.274288	67.897396
1208.641669	49.828701	67.902401
1207.151832	54.489477	67.907406
1206.547114	52.389080	67.912410
1205.671682	59.924864	67.917415
1205.294614	53.646958	67.922420
1204.474339	46.144793	67.927425
1203.263434	59.925383	67.932430
1202.996532	46.203683	67.937434
1202.469010	53.616322	67.942439
1201.931518	45.616575	67.947444
1201.659675	46.237250	67.952449
1200.702611	55.415096	67.957454
1200.156741	48.906982	67.962458
1199.270090	52.945102	67.967463
1198.761286	58.180030	67.972468
1197.980893	57.578951	67.977473
1196.890618	54.357230	67.982478
1196.820711	49.881920	67.987482
1196.021614	55.213481	67.992487
1195.183725	55.171934	67.997492
1194.505850	53.743955	68.002497
1193.729598	61.230851	68.007502
1193.693662	56.985115	68.012506
1192.913329	56.335141	68.017511
1191.889061	48.460123	68.022516
1191.359621	55.103475	68.027521
1191.139143	60.147462	68.032526
1190.051452	56.204625	68.037530
1189.298478	60.223067	68.042535
1188.545410	59.407899	68.047540
1188.437475	56.501481	68.052545
1186.808777	64.472482	68.057550
1186.312763	46.658537	68.062554
1185.749730	59.388292	68.067559
1185.424035	55.699602	68.072564
1185.017276	57.119217	68.077569
1184.281187	64.246473	68.082574
1183.550481	53.880357	68.087578
1182.727321	63.398058	68.092583
1182.370089	54.562198	68.097588
1181.323970	54.375568	68.102593
1180.176207	63.090141	68.107598
1179.781606	59.814556	68.112602
1179.407064	59.156819	68.117607
1179.161002	55.035973	68.122612
1178.574503	57.897202	68.127617
1177.251834	60.738316	68.132622
1177.087315	50.780498	68.137626
1176.401949	65.193491	68.142631
1175.371730	57.797266	68.147636
1174.643396	56.363124	68.152641
1173.684810	52.551158	68.157646
1173.855610	55.810786	68.162650
1173.238362	52.359292	68.167655
1172.471782	52.839450	68.172660
1171.699766	56.581788	68.177665
1170.759977	56.704697	68.182670
1170.233337	51.128716	68.187674
1168.779360	55.000021	68.192679
1168.527622	45.183821	68.197684
1168.247556	51.511530	68.202689
1167.537810	64.316668	68.207694
1167.484694	52.483380	68.212698
1166.322177	56.320946	68.217703
1165.595457	47.529669	68.222708
1165.382133	57.361981	68.227713
1164.181973	54.118326	68.232718
1163.454489	52.106857	68.237722
1162.766502	48.171428	68.242727
1162.373094	54.993431	68.247732
1162.211400	45.142409	68.252737
1160.532874	56.207607	68.257742
1160.373514	49.672723	68.262746
1159.653986	52.449452	68.267751
1159.208004	53.007939	68.272756
1158.233531	47.895874	68.277761
1157.122910	52.925315	68.282766
1156.558866	50.545634	68.287770
1156.245529	48.785280	68.292775
1155.893374	51.664435	68.297780
1155.472482	49.719327	68.302785
1153.941691	49.401630	68.307790
1153.751746	56.218081	68.312794
1153.529245	55.072516	68.317799
1152.450442	49.309961	68.322804
1151.562785	45.360561	68.327809
1150.707183	55.119980	68.332814
1150.883609	49.189312	68.337818
1149.764825	56.711775	68.342823
1148.678365	56.988916	68.347828
1148.226731	51.219651	68.352833
1147.473865	55.409981	68.357838
1147.317411	45.742641	68.362842
1146.561984	55.066635	68.367847
1145.846338	48.954568	68.372852
1144.660499	39.206526	68.377857
1144.035022	55.888804	68.382862
1144.397205	53.672477	68.387866
1143.385707	51.887548	68.392871
1142.489270	52.610732	68.397876
1142.100180	50.485517	68.402881
1141.129302	53.179223	68.407886
1139.959767	44.318036	68.412890
1139.346010	51.988839	68.417895
1138.843277	45.858679	68.422900
1138.632113	48.119290	68.427905
1138.081100	49.770025	68.432910
1137.645308	48.065423	68.437914
1136.691417	51.841430	68.442919
1135.720533	58.337377	68.447924
1135.422061	45.330384	68.452929
1134.339649	52.094818	68.457934
1133.655801	48.951989	68.462938
1133.202643	49.921651	68.467943
1132.741670	48.416608	68.472948
1132.350498	49.485226	68.477953
1131.191516	54.006678	68.482958
1130.494261	54.390661	68.487962
1130.073651	58.359403	68.492967
1129.106514	56.132161	68.497972
1128.401693	52.431244	68.502977
1127.301366	55.290633	68.507982
1127.087541	47.912818	68.512986
1126.662263	57.723648	68.517991
1126.280350	57.242143	68.522996
1125.427710	51.536670	68.528001
1124.224475	65.293992	68.533006
1124.108384	53.032311	68.538010
1123.550524	53.935046	68.543015
1122.809496	52.217495	68.548020
1122.010968	52.335300	68.553025
1120.997396	53.313680	68.558030
1120.912230	46.494173	68.563034
1120.246095	55.832356	68.568039
1119.351313	48.666945	68.573044
1118.921379	51.872307	68.578049
1118.065758	60.710750	68.583054
1117.829966	54.266880	68.588058
1116.645801	58.525826	68.593063
1115.944695	53.024922	68.598068
1115.652290	48.321647	68.603073
1114.620942	58.249388	68.608078
1114.095630	47.245049	68.613082
1113.196788	63.721652	68.618087
1112.884958	54.842314	68.623092
1112.141672	54.763668	68.628097
1111.006746	54.834057	68.633102
1110.828441	55.304238	68.638106
1110.039074	62.187658	68.643111
1109.765740	49.149860	68.648116
1108.804492	56.886987	68.653121
1107.961232	59.539903	68.658126
1107.703560	56.393946	68.663130
1107.079972	56.761486	68.668135
1106.069318	52.858477	68.673140
1105.225392	56.544459	68.678145
1104.256400	64.856864	68.683150
1104.494565	51.199929	68.688154
1103.825686	61.077901	68.693159
1102.617366	64.142148	68.698164
1102.334691	55.944186	68.703169
1101.608388	57.605467	68.708174
1100.968840	57.918774	68.713178
1099.648877	55.266674	68.718183
1099.034103	54.782791	68.723188
1098.469888	56.128113	68.728193
1098.261567	58.530208	68.733198
1098.194268	38.976448	68.738202
1097.360638	43.941344	68.743207
1096.517055	44.697139	68.748212
1095.948875	45.216724	68.753217
1094.244987	51.078618	68.758222
1093.796173	51.883583	68.763226
1093.257574	51.792882	68.768231
1092.648894	52.077625	68.773236
1092.699938	51.153493	68.778241
1091.964839	51.901494	68.783246
1091.183668	46.525307	68.788250
1090.387898	58.296984	68.793255
1089.689467	57.033161	68.798260
1089.367831	56.868520	68.803265
1087.853390	50.911932	68.808270
1087.487087	50.588808	68.813274
1086.902928	50.478547	68.818279
1086.565903	51.234189	68.823284
1085.624853	55.992242	68.828289
1084.748641	52.143553	68.833294
1084.552662	43.345152	68.838298
1084.060473	55.145807	68.843303
1082.863941	49.941361	68.848308
1081.870254	44.865506	68.853313
1081.168472	55.589271	68.858318
1081.099421	43.684418	68.863322
1080.626401	53.222131	68.868327
1079.833187	56.852741	68.873332
1078.958935	52.579520	68.878337
1078.209349	60.448574	68.883342
1078.004572	52.547326	68.888346
1077.267832	43.450157	68.893351
1076.132022	47.151039	68.898356
1075.473709	53.045314	68.903361
1074.589715	50.503654	68.908366
1074.586823	44.786029	68.913370
1074.232090	60.590993	68.918375
1073.319404	63.570373	68.923380
1072.943752	48.842508	68.928385
1071.834546	65.808350	68.933390
1071.008888	54.571089	68.938394
1070.113813	60.149778	68.943399
1069.380948	53.333962	68.948404
1069.197370	55.650117	68.953409
1068.472766	56.863258	68.958414
1068.140249	59.567403	68.963418
1067.213121	51.505095	68.968423
1066.468839	50.809999	68.973428
1066.303879	48.571865	68.978433
1064.761313	62.578740	68.983438
1064.162033	48.184517	68.988442
1063.334166	50.942234	68.993447
1063.120480	53.461886	68.998452
1062.940489	49.111338	69.003457
1062.163125	55.636447	69.008462
1061.527067	50.934233	69.013466
1060.662067	57.705109	69.018471
1060.034292	57.264307	69.023476
1059.026853	58.957710	69.028481
1057.947828	58.361606	69.033486
1057.612438	48.654934	69.038490
1057.287342	56.954800	69.043495
1056.839871	49.680403	69.048500
1056.665984	49.161082	69.053505
1055.285674	58.921997	69.058510
1054.892829	53.517158	69.063514
1053.990696	51.897804	69.068519
1052.777303	53.959884	69.073524
1052.172276	50.840812	69.078529
1051.591250	50.561317	69.083534
1051.244866	48.825160	69.088538
1050.897215	56.475721	69.093543
1050.384378	51.201944	69.098548
1049.581964	48.495919	69.103553
1048.601763	56.321238	69.108558
1048.199241	48.186516	69.113562
1047.416086	46.806869	69.118567
1046.041557	65.368309	69.123572
1045.723712	52.766561	69.128577
1045.084442	54.287847	69.133582
1044.818655	49.924142	69.138586
1044.677587	56.945717	69.143591
1043.608606	55.606814	69.148596
1042.919504	57.359969	69.153601
1042.216060	55.336826	69.158606
1041.246394	54.122480	69.163610
1040.338093	58.869029	69.168615
1039.922523	47.517654	69.173620
1039.397435	52.778850	69.178625
1038.527457	59.831238	69.183630
1038.669616	41.531025	69.188634
1037.438171	53.723703	69.193639
1036.874466	49.691266	69.198644
1036.211545	54.755184	69.203649
1035.302463	58.867891	69.208654
1034.682670	53.970698	69.213658
1034.040773	56.438627	69.218663
1033.559282	61.625077	69.223668
1033.238151	52.179506	69.228673
1031.723537	55.488068	69.233678
1031.146718	48.339919	69.238682
1030.655144	55.754747	69.243687
1030.303846	52.831866	69.248692
1029.993686	45.439432	69.253697
1028.895761	53.906415	69.258702
1028.382493	59.362863	69.263706
1027.524407	54.721218	69.268711
1026.955639	61.530132	69.273716
1026.570831	52.157775	69.278721
1025.515818	51.016942	69.283726
1025.290988	46.865932	69.288730
1023.784988	48.451005	69.293735
1023.203766	60.466117	69.298740
1022.686694	50.564421	69.303745
1021.930616	60.632907	69.308750
1021.891915	55.673225	69.313754
1021.312351	47.148764	69.318759
1020.468523	52.695655	69.323764
1019.708270	51.689285	69.328769
1019.074655	57.264236	69.333774
1018.212367	50.364948	69.338778
1017.125239	53.187587	69.343783
1016.427444	52.754782	69.348788
1016.505547	51.228648	69.353793
1015.784661	47.839423	69.358798
1015.324975	44.343982	69.363802
1014.232818	53.576491	69.368807
1013.545308	45.668482	69.373812
1013.233949	40.772690	69.378817
1012.095177	54.095559	69.383822
1011.415206	52.820937	69.388826
1010.636388	58.866872	69.393831
1010.321989	47.389015	69.398836
1010.099653	38.875536	69.403841
1009.056224	51.473568	69.408846
1008.105992	46.663658	69.413850
1007.475449	48.905845	69.418855
1007.090677	48.891617	69.423860
1007.091805	47.041822	69.428865
1005.930062	48.591054	69.433870
1005.363988	43.984962	69.438874
1004.488314	47.545129	69.443879
1004.040099	51.606591	69.448884
1002.803995	43.322230	69.453889
1002.174759	53.572392	69.458894
1002.032990	46.168940	69.463898
1001.356810	41.712841	69.468903
1000.352625	45.331306	69.473908
999.677020	44.369823	69.478913
999.140892	51.656116	69.483918
998.707667	44.851003	69.488922
997.465989	49.436132	69.493927
996.413111	50.990124	69.498932
996.404315	43.649098	69.503937
995.650375	51.312265	69.508942
995.477079	46.282537	69.513946
995.272886	50.745164	69.518951
993.915024	46.682978	69.523956
993.396489	46.626954	69.528961
992.435421	54.663722	69.533966
991.748601	43.385489	69.538970
990.787734	42.428398	69.543975
990.215039	46.703643	69.548980
990.158531	41.373044	69.553985
989.568627	40.628175	69.558990
988.700751	38.118680	69.563994
987.737589	40.669277	69.568999
987.473851	43.318326	69.574004
986.690832	39.136290	69.579009
985.397073	54.379423	69.584014
984.979739	43.463609	69.589018
984.532891	54.255639	69.594023
984.079058	51.377469	69.599028
983.723662	52.353678	69.604033
982.739364	61.480726	69.609038
982.073502	40.287499	69.614042
981.461118	41.936991	69.619047
980.500426	49.527399	69.624052
980.224226	35.629042	69.629057
979.216503	49.811048	69.634062
979.176746	45.228452	69.639066
977.978605	43.813933	69.644071
977.015133	42.592319	69.649076
976.549027	45.907539	69.654081
975.981913	43.060015	69.659086
975.573108	44.762274	69.664090
974.158761	45.102705	69.669095
973.854494	48.873168	69.674100
973.442453	43.050337	69.679105
972.547173	51.740572	69.684110
972.750646	38.707374	69.689114
971.443584	52.533297	69.694119
970.727679	55.629637	69.699124
970.350256	53.961512	69.704129
969.041781	54.412838	69.709134
968.247421	50.158489	69.714138
968.084983	51.116611	69.719143
967.145133	52.763022	69.724148
967.004189	45.408331	69.729153
966.497468	52.478627	69.734158
965.985458	44.555325	69.739162
964.926437	50.798829	69.744167
963.979550	48.213600	69.749172
963.039882	40.298429	69.754177
961.990063	51.287339	69.759182
962.099923	50.104675	69.764186
961.476048	53.128022	69.769191
961.060825	53.426167	69.774196
960.813893	49.341764	69.779201
959.863550	52.658349	69.784206
959.118206	41.996602	69.789210
958.308796	53.168043	69.794215
957.041576	52.221865	69.799220
956.587012	49.963592	69.804225
956.046486	48.614754	69.809230
955.769528	49.621065	69.814234
955.266065	44.975060	69.819239
954.121512	48.486562	69.824244
953.656862	43.493742	69.829249
952.951328	52.155364	69.834254
952.348569	46.873845	69.839258
951.256907	52.362419	69.844263
950.699332	50.760815	69.849268
950.220988	44.147407	69.854273
949.567246	52.086391	69.859278
949.195788	49.549952	69.864282
948.037996	47.703227	69.869287
947.109968	51.536686	69.874292
946.891131	45.960672	69.879297
946.367698	57.942938	69.884302
946.033627	49.757921	69.889306
945.195779	46.928256	69.894311
944.156314	52.378561	69.899316
944.015883	48.013848	69.904321
942.652074	54.334251	69.909326
942.271317	50.993429	69.914330
941.422740	52.018165	69.919335
940.590152	56.803160	69.924340
940.626806	51.487700	69.929345
939.845028	50.797033	69.934350
939.317677	53.831832	69.939354
938.582376	51.124628	69.944359
937.930019	54.559387	69.949364
936.709686	48.133452	69.954369
935.965898	47.736376	69.959374
935.581315	47.733168	69.964378
935.287948	52.523819	69.969383
934.873506	52.377121	69.974388
934.239090	46.685886	69.979393
933.510833	55.728040	69.984398
933.052338	50.838328	69.989402
931.561348	49.826845	69.994407
930.881338	48.580640	69.999412
930.633312	41.263499	70.004417
929.505359	52.255393	70.009422
929.034258	45.349086	70.014426
928.332821	50.475928	70.019431
927.618636	59.380221	70.024436
927.455394	54.788891	70.029441
926.336925	53.937334	70.034446
925.539794	49.274990	70.039450
924.882005	51.706046	70.044455
924.239008	46.651724	70.049460
923.932033	49.093184	70.054465
923.071964	55.264039	70.059470
923.001217	52.279180	70.064474
921.852645	57.926642	70.069479
921.531491	53.884019	70.074484
920.761055	43.008650	70.079489
919.792020	55.162762	70.084494
919.154069	57.417189	70.089498
918.699420	51.123308	70.094503
918.074069	52.323848	70.099508
917.128544	48.155080	70.104513
916.448724	53.567083	70.109518
916.070981	43.901884	70.114522
915.342070	53.455103	70.119527
914.370838	52.832444	70.124532
913.948138	37.318881	70.129537
913.205717	49.952615	70.134542
912.796318	46.616357	70.139546
911.789876	40.312525	70.144551
910.678616	47.376531	70.149556
910.535617	37.010048	70.154561
909.681488	49.844496	70.159566
909.922810	47.712036	70.164570
908.775334	45.644480	70.169575
907.632171	54.462498	70.174580
907.344255	46.107712	70.179585
906.435640	52.016624	70.184590
906.050799	46.310910	70.189594
905.374966	45.139745	70.194599
904.736915	49.510567	70.199604
904.347442	44.614610	70.204609
903.436689	40.736798	70.209614
902.789858	39.154144	70.214618
901.743910	36.255109	70.219623
901.253018	46.423335	70.224628
901.162655	32.774560	70.229633
900.114801	53.293179	70.234638
899.027674	46.929648	70.239642
898.424879	43.299306	70.244647
897.664964	42.783377	70.249652
897.680313	43.006696	70.254657
896.942681	51.621394	70.259662
896.107254	38.731473	70.264666
895.407680	43.769710	70.269671
894.498372	43.386375	70.274676
894.555883	41.261091	70.279681
893.678137	47.139858	70.284686
892.747876	38.740651	70.289690
892.303434	44.460563	70.294695
891.783657	46.235692	70.299700
890.701007	42.509830	70.304705
889.760341	46.176575	70.309710
889.557486	41.384967	70.314714
889.358623	41.112497	70.319719
888.195641	54.092310	70.324724
887.442777	43.597377	70.329729
887.022007	45.796741	70.334734
886.372741	37.452167	70.339738
885.316290	41.951089	70.344743
884.290138	45.924770	70.349748
884.380510	43.724866	70.354753
883.496059	47.428400	70.359758
883.298037	49.622276	70.364762
881.921097	46.898938	70.369767
881.253702	51.143543	70.374772
880.885493	44.582013	70.379777
880.630089	54.173420	70.384782
879.728640	42.027332	70.389786
878.777569	54.735287	70.394791
878.238907	49.774765	70.399796
877.865892	47.399444	70.404801
876.984349	52.974457	70.409806
875.946845	53.109875	70.414810
875.470938	47.544824	70.419815
875.080203	46.550651	70.424820
874.565928	49.406752	70.429825
873.250322	53.316118	70.434830
872.721481	38.480239	70.439834
872.310891	51.422304	70.444839
872.021970	49.675451	70.449844
871.264401	47.063281	70.454849
870.017843	53.910709	70.459854
869.741824	46.916593	70.464858
869.262599	49.519523	70.469863
868.428385	58.036057	70.474868
867.565954	57.735161	70.479873
866.954923	48.148107	70.484878
866.722416	49.806551	70.489882
865.694936	62.832622	70.494887
864.994726	47.315926	70.499892
864.428950	48.096967	70.504897
863.484169	52.672748	70.509902
863.149772	56.473251	70.514906
862.513363	51.189229	70.519911
861.397633	54.429665	70.524916
861.142915	46.257271	70.529921
860.449043	46.027324	70.534926
859.842201	45.676286	70.539930
859.303414	41.636778	70.544935
858.207195	43.938929	70.549940
857.973089	43.692573	70.554945
857.187569	48.127881	70.559950
856.336825	43.273815	70.564954
855.751056	38.981577	70.569959
855.088750	40.675316	70.574964
854.871946	39.076268	70.579969
853.796080	49.739756	70.584974
853.178346	37.351396	70.589978
852.375782	44.039840	70.594983
852.041293	44.290458	70.599988
851.474722	35.793955	70.604993
850.147934	47.653346	70.609998
849.714232	47.867715	70.615002
849.482062	38.496349	70.620007
848.685443	43.043816	70.625012
847.767010	35.820791	70.630017
846.698211	42.070620	70.635022
846.736457	41.768297	70.640026
846.351813	36.016835	70.645031
845.202117	41.208737	70.650036
844.496318	36.181789	70.655041
843.747610	48.952157	70.660046
843.408609	42.401758	70.665050
842.844652	44.288013	70.670055
841.932536	49.918366	70.675060
841.382755	37.169092	70.680065
840.889723	50.897025	70.685070
840.089867	36.192614	70.690074
839.013199	43.891413	70.695079
838.165160	48.776670	70.700084
838.345140	41.858218	70.705089
837.289934	48.124813	70.710094
836.448711	43.318128	70.715098
835.754059	43.835824	70.720103
835.158465	40.893517	70.725108
834.800409	42.743844	70.730113
834.437261	51.690047	70.735118
833.466921	49.944431	70.740122
832.832758	42.706122	70.745127
832.010235	46.883962	70.750132
831.447513	43.240952	70.755137
830.406215	49.014880	70.760142
829.852819	52.373982	70.765146
829.556069	41.500525	70.770151
828.713518	49.960040	70.775156
827.708717	47.060795	70.780161
826.771124	50.440053	70.785166
826.491621	50.719770	70.790170
825.742675	46.600178	70.795175
825.499332	52.355901	70.800180
825.492400	37.249293	70.805185
824.190711	49.968914	70.810190
823.583526	44.162989	70.815194
822.917989	44.770676	70.820199
822.123084	46.950756	70.825204
821.473639	39.337974	70.830209
820.746147	44.997291	70.835214
820.536431	42.059796	70.840218
819.643510	44.917832	70.845223
818.503457	48.878129	70.850228
817.968164	46.621697	70.855233
817.635636	45.891094	70.860238
816.997605	39.031895	70.865242
816.156709	41.370692	70.870247
814.959137	45.556199	70.875252
814.565535	41.086717	70.880257
814.064406	47.345545	70.885262
814.126808	43.975205	70.890266
812.985363	50.112028	70.895271
812.082649	45.518578	70.900276
812.013118	37.674704	70.905281
811.014024	44.325055	70.910286
810.253084	41.112595	70.915290
809.198126	41.112040	70.920295
808.677472	47.788737	70.925300
808.664402	38.257914	70.930305
807.626600	53.279002	70.935310
806.731767	52.327240	70.940314
806.110320	46.506242	70.945319
805.721102	58.415111	70.950324
805.472517	44.212760	70.955329
803.830878	51.145187	70.960334
803.505643	51.837484	70.965338
803.059584	45.528073	70.970343
802.313921	44.700808	70.975348
801.976499	43.366983	70.980353
800.823444	47.367205	70.985358
800.847350	38.338301	70.990362
799.813286	39.708018	70.995367
798.778729	49.910762	71.000372
798.106081	36.627527	71.005377
797.428122	47.544668	71.010382
797.187782	39.507203	71.015386
796.539201	45.049880	71.020391
795.344252	50.483987	71.025396
795.261411	40.461199	71.030401
794.836093	46.242736	71.035406
793.960607	38.460936	71.040410
793.157875	40.326864	71.045415
792.289754	42.520185	71.050420
791.743305	44.277501	71.055425
790.747944	43.005842	71.060430
789.987175	38.459194	71.065434
789.346312	41.053174	71.070439
788.903259	39.575311	71.075444
788.774715	41.043735	71.080449
788.301503	49.862375	71.085454
787.163629	41.590889	71.090458
786.462932	35.490767	71.095463
785.988788	43.248210	71.100468
785.212525	37.374595	71.105473
784.374172	34.288016	71.110478
783.904454	42.181955	71.115482
783.551482	35.285272	71.120487
782.277765	39.128082	71.125492
781.648076	37.888102	71.130497
780.826819	53.644313	71.135502
780.458930	43.900306	71.140506
780.194285	41.061452	71.145511
779.160054	36.083659	71.150516
778.563461	44.959788	71.155521
777.834298	41.067310	71.160526
777.264583	38.415804	71.165530
776.521098	42.571613	71.170535
775.543308	41.546334	71.175540
775.096136	40.165329	71.180545
774.514285	40.393835	71.185550
774.159622	44.169182	71.190554
773.567228	38.641631	71.195559
772.476612	42.166699	71.200564
772.005065	37.987193	71.205569
771.458095	42.517014	71.210574
770.942415	37.522903	71.215578
769.889330	43.828608	71.220583
768.992283	44.734955	71.225588
768.660090	41.812234	71.230593
767.686690	47.259967	71.235598
766.953927	31.521423	71.240602
766.379217	38.367583	71.245607
765.768759	49.083163	71.250612
765.617718	36.235740	71.255617
764.996236	47.512919	71.260622
763.973984	36.977349	71.265626
763.308813	43.049401	71.270631
762.524622	41.307296	71.275636
762.304626	41.661128	71.280641
761.081246	47.148664	71.285646
760.370433	45.398030	71.290650
760.167923	37.269391	71.295655
759.705676	50.732216	71.300660
758.735653	45.569157	71.305665
757.728626	42.462129	71.310670
757.209928	45.222756	71.315674
756.846813	47.589587	71.320679
756.192858	49.759862	71.325684
755.545929	38.804976	71.330689
754.388326	40.342620	71.335694
754.164544	40.862644	71.340698
753.518734	43.129398	71.345703
753.093881	47.778559	71.350708
752.466035	40.840484	71.355713
751.485159	48.473600	71.360718
750.829205	40.049708	71.365722
749.796582	44.144322	71.370727
749.076187	47.686153	71.375732
748.994115	40.268503	71.380737
748.398651	49.491406	71.385742
747.907386	38.057554	71.390746
747.026561	36.332418	71.395751
746.051910	40.178094	71.400756
745.685294	35.477239	71.405761
744.388759	35.920472	71.410766
743.901421	39.669635	71.415770
743.310318	37.349565	71.420775
742.705980	41.426455	71.425780
742.689318	36.732962	71.430785
741.828398	34.078943	71.435790
740.926094	30.185662	71.440794
740.239521	37.188416	71.445799
739.578364	37.350705	71.450804
738.928091	25.992648	71.455809
737.860342	44.328694	71.460814
737.416034	28.858066	71.465818
737.057392	40.047660	71.470823
736.240649	43.150649	71.475828
735.348478	34.513629	71.480833
734.461922	36.004972	71.485838
734.244600	37.340870	71.490842
733.772179	35.924467	71.495847
733.381720	35.736136	71.500852
732.564044	32.214178	71.505857
731.422904	39.517981	71.510862
731.193872	36.875324	71.515866
730.582676	32.177144	71.520871
729.268448	43.499968	71.525876
728.966636	40.629190	71.530881
728.475889	45.279383	71.535886
727.839359	36.770403	71.540890
726.898300	33.999834	71.545895
726.183365	44.968605	71.550900
725.933209	35.234258	71.555905
725.284011	40.969443	71.560910
724.022283	34.901902	71.565914
723.347484	37.226896	71.570919
722.943741	44.172006	71.575924
722.776752	30.731019	71.580929
722.059647	41.294838	71.585934
720.848751	41.437427	71.590938
720.442325	37.561394	71.595943
719.812825	37.079951	71.600948
719.646078	29.484972	71.605953
718.364731	38.323474	71.610958
717.430139	40.129992	71.615962
717.048408	38.580875	71.620967
716.564279	42.578703	71.625972
715.713099	32.861209	71.630977
714.843380	46.895140	71.635982
714.496237	35.162373	71.640986
714.230453	39.828787	71.645991
712.989255	47.500211	71.650996
712.219757	42.549683	71.656001
711.449010	46.946406	71.661006
711.030228	42.589769	71.666010
710.887461	39.647935	71.671015
709.836403	33.016976	71.676020
709.179121	32.492649	71.681025
708.552444	37.121907	71.686030
708.153228	44.100992	71.691034
707.204958	31.975070	71.696039
706.430407	29.763073	71.701044
705.955815	23.712141	71.706049
705.557531	42.946156	71.711054
704.270414	45.204648	71.716058
703.826233	38.398201	71.721063
703.204170	42.279216	71.726068
703.095654	41.456186	71.731073
701.727891	47.386227	71.736078
700.797481	38.681189	71.741082
700.425530	44.107292	71.746087
699.547287	45.132100	71.751092
699.319632	36.138533	71.756097
699.146151	47.475275	71.761102
697.952146	37.845494	71.766106
697.553502	40.279493	71.771111
696.591137	55.827943	71.776116
696.495581	53.995126	71.781121
694.746017	40.189524	71.786126
694.502366	35.582644	71.791130
693.709365	37.227845	71.796135
693.344405	42.020446	71.801140
693.236954	28.423323	71.806145
691.723560	42.890928	71.811150
691.212857	38.875380	71.816154
690.883308	35.953829	71.821159
689.991959	43.892841	71.826164
689.209886	40.811527	71.831169
688.290179	48.911184	71.836174
688.041995	41.259782	71.841178
687.758265	39.057945	71.846183
686.898056	38.946002	71.851188
686.126267	33.341385	71.856193
685.332455	40.011128	71.861198
684.970210	33.896573	71.866202
684.141970	39.988298	71.871207
683.010956	39.375405	71.876212
682.732234	42.014248	71.881217
682.136282	49.918842	71.886222
681.350890	43.244009	71.891226
680.542696	38.233421	71.896231
680.016500	43.480651	71.901236
679.610807	38.675639	71.906241
679.372291	39.983376	71.911246
678.264623	41.913668	71.916250
677.538338	48.733520	71.921255
676.842447	46.743981	71.926260
676.269864	44.102419	71.931265
674.918542	37.312700	71.936270
674.394646	39.107450	71.941274
673.984502	37.348390	71.946279
673.396370	37.805011	71.951284
673.287890	33.238114	71.956289
672.331523	37.468852	71.961294
671.616445	43.488942	71.966298
671.011203	34.514509	71.971303
670.129255	34.607893	71.976308
669.618509	37.605399	71.981313
668.406411	41.503108	71.986318
667.918017	39.187203	71.991322
667.787963	41.873337	71.996327
666.964714	38.694504	72.001332
666.757417	37.412522	72.006337
665.801070	36.715049	72.011342
665.246879	32.338987	72.016346
664.214294	38.578381	72.021351
662.934059	45.260937	72.026356
662.905004	37.024263	72.031361
662.221678	44.031250	72.036366
661.901547	35.631187	72.041370
661.137227	36.295650	72.046375
660.055894	37.016906	72.051380
659.903346	34.704292	72.056385
658.902525	46.239022	72.061390
658.342734	36.117163	72.066394
657.685166	41.360084	72.071399
656.836440	42.127882	72.076404
656.595423	39.837241	72.081409
655.954884	44.110734	72.086414
654.937788	43.118573	72.091418
654.270255	38.044592	72.096423
653.777167	40.435287	72.101428
653.544887	33.601418	72.106433
652.021009	37.925696	72.111438
651.505668	41.780263	72.116442
651.386074	39.189575	72.121447
650.439620	46.000338	72.126452
649.521137	34.019518	72.131457
648.410901	46.405924	72.136462
648.203973	35.920351	72.141466
647.988335	34.909371	72.146471
647.415343	41.755278	72.151476
646.513323	36.502591	72.156481
645.678191	49.039161	72.161486
645.288836	45.691881	72.166490
644.992711	38.207404	72.171495
643.538271	37.974060	72.176500
643.170153	38.444536	72.181505
642.728292	45.174941	72.186510
641.537325	48.432179	72.191514
640.679862	38.390849	72.196519
639.756900	51.286779	72.201524
639.607586	36.663373	72.206529
639.240485	34.987354	72.211534
638.991635	40.890619	72.216538
638.271498	42.428034	72.221543
637.333287	39.986646	72.226548
636.703670	32.189416	72.231553
635.775451	43.783554	72.236558
634.909657	37.733434	72.241562
634.411314	40.744741	72.246567
633.900052	42.860778	72.251572
633.789742	39.254584	72.256577
632.610327	48.080047	72.261582
631.822444	46.228182	72.266586
631.183744	44.164891	72.271591
630.141187	41.702275	72.276596
630.236728	38.254118	72.281601
629.079422	43.403163	72.286606
628.083672	48.830847	72.291610
627.716704	48.861153	72.296615
627.396548	49.927995	72.301620
627.229620	49.607881	72.306625
625.912141	50.579662	72.311630
625.410351	45.835698	72.316634
624.945932	42.785819	72.321639
623.786711	52.765611	72.326644
623.017840	40.172739	72.331649
622.535057	46.968014	72.336654
621.874720	44.256859	72.341658
621.635011	44.419869	72.346663
620.595658	47.757053	72.351668
620.121996	41.365350	72.356673
618.860847	42.077415	72.361678
618.635940	39.050895	72.366682
618.331570	38.563430	72.371687
616.985075	42.687581	72.376692
616.576407	40.811596	72.381697
615.890505	44.622369	72.386702
615.677115	44.003713	72.391706
615.373206	34.763675	72.396711
613.936592	39.629190	72.401716
613.541851	34.033936	72.406721
612.829492	46.317557	72.411726
612.108051	43.213996	72.416730
611.445806	37.265513	72.421735
610.651790	36.204723	72.426740
610.579526	35.148833	72.431745
609.230362	41.571140	72.436750
608.591452	31.301046	72.441754
608.162248	29.563959	72.446759
607.643114	35.070281	72.451764
607.261321	29.733178	72.456769
605.916127	37.630949	72.461774
605.322302	36.607665	72.466778
605.126959	30.999580	72.471783
603.625161	44.851916	72.476788
603.470104	35.272768	72.481793
602.468716	30.292983	72.486798
601.720959	29.928182	72.491802
601.665142	39.315893	72.496807
601.016603	35.625111	72.501812
600.618810	35.952080	72.506817
599.490997	39.585648	72.511822
598.977413	37.352622	72.516826
598.334367	37.143039	72.521831
597.120318	45.560850	72.526836
596.906010	33.972546	72.531841
596.128755	43.615523	72.536846
595.833897	37.474482	72.541850
595.216474	33.818172	72.546855
594.174707	36.770954	72.551860
593.787957	32.178999	72.556865
593.220165	39.546081	72.561870
592.294620	41.325970	72.566874
591.371885	39.476674	72.571879
590.752139	36.268609	72.576884
590.458387	32.809916	72.581889
589.506429	46.729231	72.586894
588.589370	44.371229	72.591898
588.210364	46.054605	72.596903
587.688432	39.788876	72.601908
587.436346	41.429957	72.606913
586.276559	46.538414	72.611918
585.581175	44.476279	72.616922
585.269937	37.140886	72.621927
584.432406	35.262252	72.626932
583.221295	35.690384	72.631937
582.445853	48.903466	72.636942
582.127532	41.767904	72.641946
581.878886	43.173461	72.646951
581.031817	43.994639	72.651956
580.738074	45.516194	72.656961
579.630194	43.379410	72.661966
578.900262	41.001068	72.666970
579.072344	43.699006	72.671975
577.621310	46.795838	72.676980
576.907397	43.107590	72.681985
576.429924	45.200908	72.686990
575.890187	39.934699	72.691994
575.332895	48.246331	72.696999
574.209915	47.971270	72.702004
573.708838	34.991977	72.707009
572.628311	39.245680	72.712014
572.626597	41.089743	72.717018
572.030027	40.721370	72.722023
570.858699	43.667991	72.727028
570.449531	47.097211	72.732033
569.971327	39.170221	72.737038
569.616770	39.234830	72.742042
568.355086	38.972403	72.747047
567.629138	48.630872	72.752052
567.710427	43.150619	72.757057
566.716846	46.578308	72.762062
565.403750	43.643127	72.767066
565.294375	38.086009	72.772071
565.099526	47.319241	72.777076
563.868118	32.251606	72.782081
563.008378	43.136231	72.787086
562.454926	34.547842	72.792090
562.064369	42.061748	72.797095
560.850626	41.193995	72.802100
560.517904	36.112446	72.807105
559.937816	31.932935	72.812110
559.388216	39.849083	72.817114
558.997068	32.769288	72.822119
557.452746	37.399665	72.827124
557.360857	42.561961	72.832129
556.407432	42.923827	72.837134
556.420467	35.440587	72.842138
555.467451	42.014292	72.847143
554.150334	42.853581	72.852148
553.597979	36.376657	72.857153
553.091121	34.752880	72.862158
552.964285	35.825206	72.867162
551.905379	39.807380	72.872167
550.744724	43.581825	72.877172
550.443715	32.649192	72.882177
550.028325	37.538152	72.887182
549.700952	32.452600	72.892186
549.015909	31.741919	72.897191
548.076826	42.700690	72.902196
547.667951	37.729050	72.907201
546.577810	45.698192	72.912206
545.710931	40.282245	72.917210
545.454400	36.374485	72.922215
544.675469	34.732546	72.927220
544.451802	30.013693	72.932225
543.510172	33.720131	72.937230
542.648104	39.022461	72.942234
542.610890	36.376080	72.947239
541.407915	41.152373	72.952244
540.713426	39.936973	72.957249
539.789875	44.807534	72.962254
539.384932	40.735749	72.967258
539.051781	43.203494	72.972263
537.651780	39.670287	72.977268
537.445507	37.752613	72.982273
536.594728	48.946495	72.987278
536.375453	43.793256	72.992282
535.876317	39.864217	72.997287
534.654864	44.208199	73.002292
534.173912	38.774935	73.007297
533.400161	41.159897	73.012302
532.723398	41.665364	73.017306
531.926004	37.730221	73.022311
531.108210	38.053143	73.027316
530.726137	42.143555	73.032321
530.027237	44.593869	73.037326
529.613904	40.260060	73.042330
529.572059	39.675588	73.047335
528.148564	47.089110	73.052340
527.541806	36.413356	73.057345
527.037752	41.843170	73.062350
525.980941	43.571451	73.067354
525.379006	36.760219	73.072359
524.972726	42.838386	73.077364
524.764049	37.152006	73.082369
523.215427	32.760929	73.087374
522.825592	36.247000	73.092378
522.364320	29.574220	73.097383
521.543670	44.849372	73.102388
521.271215	37.242874	73.107393
520.251256	42.710721	73.112398
519.559884	38.793386	73.117402
519.441068	43.259773	73.122407
517.921414	42.178990	73.127412
517.164751	41.126473	73.132417
516.606418	37.115403	73.137422
515.949308	36.482286	73.142426
515.963976	39.539624	73.147431
515.518129	47.341477	73.152436
514.585970	38.234665	73.157441
513.548819	45.031532	73.162446
512.973941	41.936195	73.167450
512.587220	30.831139	73.172455
511.372348	43.491309	73.177460
511.057830	33.325696	73.182465
510.369447	41.066833	73.187470
509.993402	40.448867	73.192474
509.088004	32.381788	73.197479
508.152825	47.132695	73.202484
507.919285	35.150063	73.207489
507.269626	41.265427	73.212494
506.005569	37.406216	73.217498
505.331557	38.906356	73.222503
504.759751	41.125106	73.227508
504.626719	33.059564	73.232513
504.280530	33.096040	73.237518
503.021849	44.066315	73.242522
502.450433	37.032599	73.247527
501.434253	42.562931	73.252532
501.515472	30.933876	73.257537
500.438330	40.831238	73.262542
499.377477	44.033115	73.267546
499.006692	38.591771	73.272551
498.281669	34.381749	73.277556
498.228464	36.150431	73.282561
497.098135	52.298139	73.287566
496.463124	43.114028	73.292570
495.944070	30.538194	73.297575
495.412085	41.277572	73.302580
494.504023	39.872274	73.307585
493.547095	36.902469	73.312590
492.765508	39.730258	73.317594
492.750147	34.982954	73.322599
492.073682	45.256476	73.327604
491.480471	36.608208	73.332609
490.477928	39.572129	73.337614
490.019399	39.443570	73.342618
489.371613	34.172524	73.347623
488.438582	37.812953	73.352628
487.860137	37.183081	73.357633
486.977887	46.942164	73.362638
486.761995	40.503119	73.367642
485.925882	42.341341	73.372647
484.834263	42.750484	73.377652
484.705061	31.391508	73.382657
484.049589	42.760871	73.387662
483.267255	39.985613	73.392666
482.296397	42.129168	73.397671
481.225653	46.895460	73.402676
481.291964	26.853782	73.407681
480.620428	34.701052	73.412686
480.321822	38.336603	73.417690
479.696678	33.531906	73.422695
478.718099	35.638843	73.427700
478.505579	40.222665	73.432705
477.492349	31.015245	73.437710
476.100214	36.961891	73.442714
475.941155	35.533464	73.447719
475.313011	32.205341	73.452724
475.297778	29.746281	73.457729
474.138719	37.035689	73.462734
473.158101	34.235255	73.467738
472.785286	27.639863	73.472743
472.328356	38.190655	73.477748
471.329468	27.771379	73.482753
470.764677	34.448839	73.487758
470.010054	39.372933	73.492762
469.665978	44.395628	73.497767
468.577581	35.162339	73.502772
467.994415	29.418937	73.507777
467.354196	31.429388	73.512782
467.024572	31.915835	73.517786
466.018179	32.926446	73.522791
464.904225	42.629404	73.527796
464.659914	43.365622	73.532801
464.101857	36.782395	73.537806
463.714446	39.326604	73.542810
463.289808	41.272744	73.547815
462.188047	41.830176	73.552820
461.711517	38.758609	73.557825
460.709338	45.835364	73.562830
459.696277	40.907966	73.567834
459.112293	40.799402	73.572839
458.437389	42.760187	73.577844
458.425481	35.886506	73.582849
458.102032	40.060629	73.587854
456.985377	37.843297	73.592858
456.381095	35.049142	73.597863
455.519371	44.991049	73.602868
455.051264	33.529952	73.607873
453.775154	41.225967	73.612878
453.176223	40.878501	73.617882
453.053053	37.156095	73.622887
452.099114	38.771817	73.627892
452.209807	33.252191	73.632897
450.873647	46.471052	73.637902
450.154303	37.760890	73.642906
449.942749	38.468234	73.647911
448.535235	38.399423	73.652916
448.031721	37.872744	73.657921
447.270647	40.369256	73.662926
447.007501	41.190482	73.667930
446.487276	33.774873	73.672935
445.616637	41.828928	73.677940
444.922985	36.361767	73.682945
444.238686	37.174402	73.687950
443.882684	40.538392	73.692954
443.285612	39.298037	73.697959
442.079650	38.758702	73.702964
441.707439	45.626269	73.707969
441.201103	41.359340	73.712974
440.502071	41.598710	73.717978
439.736444	38.666257	73.722983
438.302129	47.768963	73.727988
438.220501	44.935688	73.732993
437.966037	46.258602	73.737998
437.365925	42.848747	73.743002
436.316509	36.272856	73.748007
435.586759	43.444987	73.753012
435.345972	32.105378	73.758017
434.671439	43.591330	73.763022
433.586912	38.828304	73.768026
433.323826	36.500206	73.773031
432.455308	43.945196	73.778036
431.912008	35.025633	73.783041
430.893719	36.486028	73.788046
430.460665	40.185587	73.793050
429.953684	40.055297	73.798055
429.046348	46.878820	73.803060
428.488320	39.232684	73.808065
427.834762	43.768508	73.813070
427.086834	43.861125	73.818074
426.851470	37.956651	73.823079
425.519084	43.351308	73.828084
424.856755	39.516113	73.833089
424.006617	43.971294	73.838094
423.620793	46.139925	73.843098
423.847028	37.730126	73.848103
422.575109	46.327547	73.853108
421.976597	35.641055	73.858113
421.127249	32.111643	73.863118
420.681241	34.423910	73.868122
419.898327	38.030980	73.873127
418.876708	44.051086	73.878132
418.599779	36.724453	73.883137
418.222768	37.953351	73.888142
417.247570	37.457684	73.893146
416.579017	36.919463	73.898151
415.573260	40.621971	73.903156
415.572998	35.314000	73.908161
414.682460	43.462702	73.913166
413.406059	47.829687	73.918170
413.062781	41.945564	73.923175
412.487117	49.971551	73.928180
412.130260	40.509748	73.933185
411.383497	48.258634	73.938190
410.427715	43.192815	73.943194
410.133957	42.810923	73.948199
409.404709	44.477591	73.953204
408.865489	43.142866	73.958209
407.601276	45.847306	73.963214
407.283311	49.325095	73.968218
406.964308	30.839846	73.973223
406.032571	45.752658	73.978228
405.310041	41.608503	73.983233
404.538985	43.483694	73.988238
404.017441	43.267417	73.993242
403.517507	36.326424	73.998247
402.643915	50.502968	74.003252
402.009702	35.824417	74.008257
401.184030	42.440958	74.013262
400.839522	47.758632	74.018266
400.554782	39.936484	74.023271
399.180545	46.575787	74.028276
398.494919	41.690860	74.033281
398.143077	40.170153	74.038286
397.619613	50.952346	74.043290
396.292142	41.277775	74.048295
395.755995	37.223776	74.053300
395.480575	36.973010	74.058305
395.014505	38.223988	74.063310
394.323260	47.459047	74.068314
393.503898	39.012437	74.073319
392.748876	42.086768	74.078324
392.263074	50.333414	74.083329
391.565072	40.720968	74.088334
390.445534	46.789807	74.093338
390.065641	40.734897	74.098343
389.295480	49.435308	74.103348
388.956447	41.547694	74.108353
388.583647	47.666274	74.113358
387.666789	44.557656	74.118362
387.363152	43.116004	74.123367
386.250107	46.211121	74.128372
385.261269	39.478938	74.133377
384.427037	39.400810	74.138382
383.906079	40.271012	74.143386
383.928203	38.201834	74.148391
383.194588	48.553872	74.153396
382.667229	36.217528	74.158401
382.179357	45.177316	74.163406
380.970092	43.025243	74.168410
380.206273	32.904455	74.173415
379.306605	37.274496	74.178420
379.031875	39.745563	74.183425
377.753010	37.820637	74.188430
376.823275	41.328110	74.193434
376.317506	29.134996	74.198439
375.729787	46.371139	74.203444
376.048617	34.399860	74.208449
375.260549	36.293541	74.213454
374.696537	38.050585	74.218458
374.217996	41.583929	74.223463
373.179480	35.328046	74.228468
372.649021	25.889198	74.233473
371.655504	42.496118	74.238478
370.755350	45.210369	74.243482
370.457648	44.740796	74.248487
369.612478	47.130880	74.253492
368.676333	34.427586	74.258497
368.045584	40.748130	74.263502
367.460949	43.456254	74.268506
367.129358	38.617422	74.273511
366.775224	40.072926	74.278516
366.085938	42.220538	74.283521
365.219486	39.745746	74.288526
364.465085	46.448715	74.293530
363.667637	42.221892	74.298535
362.464180	44.520838	74.303540
361.793786	37.271118	74.308545
361.472990	49.531800	74.313550
361.131536	46.038163	74.318554
360.953575	36.301849	74.323559
359.838725	41.218725	74.328564
358.914394	36.721955	74.333569
358.709825	33.872009	74.338574
358.328167	39.914726	74.343578
357.203427	35.082451	74.348583
356.277822	39.354128	74.353588
355.804374	39.601726	74.358593
355.582543	38.148618	74.363598
354.399501	43.055863	74.368602
353.853389	34.538914	74.373607
352.809264	42.587525	74.378612
352.607770	31.997066	74.383617
351.593130	36.868008	74.388622
350.953252	41.040531	74.393626
350.365569	31.762200	74.398631
349.888691	39.095904	74.403636
349.480359	39.156499	74.408641
348.215855	36.320935	74.413646
347.482356	45.545388	74.418650
347.204256	46.408433	74.423655
346.838857	42.723065	74.428660
346.397572	41.341206	74.433665
345.355445	42.734469	74.438670
344.559864	37.704652	74.443674
344.471394	34.181740	74.448679
343.004340	41.769458	74.453684
342.315168	35.259207	74.458689
341.954588	44.100936	74.463694
341.273884	34.053653	74.468698
340.975110	26.639055	74.473703
339.808270	38.761747	74.478708
339.243077	36.958072	74.483713
338.581378	35.280170	74.488718
338.044764	32.896328	74.493722
337.304371	35.315455	74.498727
336.333340	42.379399	74.503732
335.612465	32.573498	74.508737
335.385384	35.409150	74.513742
335.128451	27.762371	74.518746
334.069203	37.893486	74.523751
333.209951	37.198016	74.528756
332.747552	34.445940	74.533761
332.199199	36.884924	74.538766
331.064375	34.657933	74.543770
330.532426	30.822490	74.548775
329.984050	36.404481	74.553780
329.530956	31.332702	74.558785
329.091078	29.761380	74.563790
328.047320	40.014615	74.568794
327.303222	29.559534	74.573799
326.640002	41.415874	74.578804
326.236184	44.027375	74.583809
325.086420	33.561252	74.588814
324.184574	51.063522	74.593818
323.972918	34.890449	74.598823
323.356744	41.103019	74.603828
323.572819	33.607938	74.608833
322.042700	41.142637	74.613838
321.156010	44.996522	74.618842
321.082273	43.934570	74.623847
320.596853	38.986219	74.628852
319.500170	40.394496	74.633857
318.469806	52.749354	74.638862
317.975502	38.373403	74.643866
317.854334	44.186941	74.648871
316.805376	49.451317	74.653876
315.818523	39.236786	74.658881
315.651555	45.123858	74.663886
314.867579	41.344358	74.668890
314.227907	33.085197	74.673895
313.085375	40.288452	74.678900
312.756996	35.117945	74.683905
312.342602	39.579401	74.688910
311.748056	44.667265	74.693914
311.202620	34.767174	74.698919
310.310756	40.377110	74.703924
309.518169	36.692029	74.708929
308.919845	39.476466	74.713934
308.058813	41.717703	74.718938
307.345530	37.348172	74.723943
306.755617	47.207365	74.728948
306.359948	32.610689	74.733953
305.901916	36.377327	74.738958
304.820246	39.353930	74.743962
304.409159	37.604551	74.748967
303.396875	34.495410	74.753972
303.176436	38.489117	74.758977
301.996516	35.018750	74.763982
301.278105	37.229370	74.768986
301.172210	40.966689	74.773991
300.355577	45.326676	74.778996
300.146863	43.940872	74.784001
298.818684	39.253022	74.789006
298.198541	31.845500	74.794010
297.937708	38.261640	74.799015
297.206398	37.768150	74.804020
296.375093	35.926475	74.809025
295.467621	38.100998	74.814030
294.760883	36.909702	74.819034
294.822050	31.983049	74.824039
293.649480	34.814866	74.829044
293.238569	37.801255	74.834049
292.569725	31.196316	74.839054
291.754614	38.897768	74.844058
290.973049	28.577991	74.849063
290.278959	35.488988	74.854068
290.294448	32.313800	74.859073
289.455430	29.227513	74.864078
288.104019	35.144105	74.869082
287.809189	25.027455	74.874087
286.959689	38.465279	74.879092
286.719090	30.964144	74.884097
285.847921	36.400469	74.889102
285.026140	38.797889	74.894106
284.530479	29.140622	74.899111
283.836631	43.778985	74.904116
282.920369	34.644520	74.909121
282.134983	35.761906	74.914126
281.564940	33.624691	74.919130
281.543454	30.778688	74.924135
280.848440	33.591159	74.929140
279.504599	39.306269	74.934145
278.953763	38.403953	74.939150
278.308337	43.452622	74.944154
278.269925	40.263948	74.949159
277.368713	33.754404	74.954164
276.461499	37.586340	74.959169
275.804374	38.101363	74.964174
275.419789	43.975814	74.969178
275.063045	38.607977	74.974183
273.821123	36.634638	74.979188
273.197868	39.684843	74.984193
272.725870	38.173847	74.989198
271.795762	42.706479	74.994202
270.730355	38.777884	74.999207
269.823145	39.575636	75.004212
269.761784	38.368204	75.009217
269.301176	40.036244	75.014222
269.113846	41.591333	75.019226
268.550290	27.850949	75.024231
267.532638	45.653970	75.029236
266.921961	31.545764	75.034241
265.874366	42.141845	75.039246
264.705166	40.861846	75.044250
264.333527	35.212523	75.049255
263.784930	37.817147	75.054260
263.635692	33.641580	75.059265
262.906763	30.438400	75.064270
261.965705	37.434507	75.069274
261.209736	28.190922	75.074279
260.407843	45.227811	75.079284
260.301929	36.667527	75.084289
259.587328	30.342719	75.089294
258.305574	30.777541	75.094298
258.161325	25.858405	75.099303
257.249717	40.870540	75.104308
257.015638	32.852684	75.109313
255.939819	33.738823	75.114318
255.354162	23.871979	75.119322
255.453800	23.736488	75.124327
253.718358	36.036587	75.129332
253.057775	30.203086	75.134337
252.626076	37.649451	75.139342
252.247965	43.712115	75.144346
251.968275	31.192830	75.149351
250.829210	32.691475	75.154356
250.314650	20.927185	75.159361
249.745789	28.956831	75.164366
248.505405	34.281707	75.169370
247.690750	32.410588	75.174375
246.947702	36.500226	75.179380
246.731736	38.184465	75.184385
246.147300	25.909318	75.189390
245.971958	29.764943	75.194394
245.371388	30.805567	75.199399
244.462085	36.268485	75.204404
243.955911	27.918680	75.209409
242.484820	30.881692	75.214414
241.614584	30.381980	75.219418
241.372782	31.631926	75.224423
240.819965	29.017293	75.229428
240.667821	28.046696	75.234433
239.457500	38.673455	75.239438
238.723422	36.045139	75.244442
238.420440	26.693076	75.249447
237.553554	31.054781	75.254452
236.873829	35.167444	75.259457
236.210704	30.217484	75.264462
235.673055	37.437881	75.269466
235.207323	26.630944	75.274471
234.167194	31.849781	75.279476
233.456365	34.246875	75.284481
232.895857	36.528538	75.289486
232.274438	35.224307	75.294490
232.089419	22.221567	75.299495
230.811324	35.442288	75.304500
230.285477	27.906212	75.309505
229.793254	31.284055	75.314510
228.886025	33.761349	75.319514
228.223351	36.228042	75.324519
227.251911	32.092093	75.329524
227.012532	35.896425	75.334529
226.842720	30.172356	75.339534
225.395476	37.487304	75.344538
225.190142	24.970370	75.349543
224.259196	31.882868	75.354548
223.654807	30.814055	75.359553
223.495378	35.343686	75.364558
222.517584	34.082081	75.369562
222.133003	31.517905	75.374567
220.972734	33.977194	75.379572
220.075748	41.434664	75.384577
219.549909	34.567243	75.389582
218.759660	38.039914	75.394586
218.321269	34.139119	75.399591
217.921167	40.265218	75.404596
217.319061	32.687683	75.409601
216.415440	38.482455	75.414606
215.323733	41.660977	75.419610
215.227707	34.256657	75.424615
214.770448	32.984608	75.429620
213.936628	27.677078	75.434625
212.932063	27.498427	75.439630
212.412758	34.895681	75.444634
212.235107	28.707643	75.449639
210.750651	43.159813	75.454644
209.949674	29.566118	75.459649
209.627106	31.434519	75.464654
209.117565	38.281416	75.469658
208.871888	28.792484	75.474663
208.014798	34.057845	75.479668
206.894341	24.618497	75.484673
206.432130	24.708207	75.489678
205.988087	41.183400	75.494682
205.601545	31.147621	75.499687
204.220091	44.258678	75.504692
203.882599	27.323506	75.509697
203.475655	36.458069	75.514702
202.810469	33.642155	75.519706
201.972970	30.927835	75.524711
201.092190	41.849014	75.529716
200.808187	37.885758	75.534721
200.099818	33.726801	75.539726
199.105709	38.268083	75.544730
198.946411	27.800246	75.549735
198.149857	41.005711	75.554740
197.331701	31.909266	75.559745
196.170610	27.893459	75.564750
195.501928	37.850379	75.569754
195.410504	27.824325	75.574759
194.898660	26.491595	75.579764
194.128256	29.795521	75.584769
193.180183	23.400728	75.589774
192.633799	40.401614	75.594778
192.470593	25.354739	75.599783
191.059741	33.737850	75.604788
190.629239	31.625720	75.609793
189.701938	24.715085	75.614798
189.302359	34.502936	75.619802
189.052018	32.754759	75.624807
187.815598	34.765715	75.629812
187.247883	38.359039	75.634817
186.989449	37.747606	75.639822
186.287252	34.240555	75.644826
185.367212	35.543452	75.649831
184.323388	35.186560	75.654836
184.012184	34.151438	75.659841
183.716608	42.211647	75.664846
182.822352	37.864704	75.669850
182.300424	36.423193	75.674855
181.599065	39.104232	75.679860
180.885338	35.796149	75.684865
179.938096	34.465032	75.689870
178.896808	43.314375	75.694874
178.731475	27.189160	75.699879
178.218431	33.334844	75.704884
177.692012	33.778587	75.709889
177.138561	37.464260	75.714894
176.009417	48.994355	75.719898
175.543387	35.861373	75.724903
174.790747	34.057664	75.729908
174.204808	36.283467	75.734913
173.479544	32.582972	75.739918
172.619935	36.437315	75.744922
172.291681	30.979800	75.749927
171.820265	35.302124	75.754932
170.441538	37.378360	75.759937
170.164428	26.161306	75.764942
169.334613	31.277243	75.769946
169.309566	24.582313	75.774951
168.024141	30.630372	75.779956
167.615842	25.903166	75.784961
166.932562	30.366509	75.789966
166.461085	37.899653	75.794970
165.683460	27.656577	75.799975
164.594951	36.497680	75.804980
164.229582	26.714017	75.809985
163.921073	27.848444	75.814990
163.225910	33.649417	75.819994
162.122085	32.340122	75.824999
161.190694	34.395497	75.830004
161.086815	27.205337	75.835009
160.767210	28.469273	75.840014
159.553069	34.827682	75.845018
159.076241	26.395951	75.850023
158.239830	37.280099	75.855028
157.730484	25.574932	75.860033
156.800692	32.053588	75.865038
155.668285	29.616555	75.870042
155.523162	21.245480	75.875047
155.104096	32.889434	75.880052
154.671155	24.755071	75.885057
154.047445	28.082927	75.890062
153.336865	40.628114	75.895066
152.919042	21.343402	75.900071
151.473490	37.792201	75.905076
150.849425	25.606992	75.910081
150.286290	28.676021	75.915086
149.455736	31.385554	75.920090
149.328771	28.278821	75.925095
147.916698	33.006621	75.930100
147.417244	27.391900	75.935105
146.857435	22.969568	75.940110
146.159902	29.403305	75.945114
146.183573	15.048927	75.950119
145.469677	27.116796	75.955124
144.208402	18.549954	75.960129
143.726339	22.460798	75.965134
143.124227	35.794542	75.970138
142.713170	29.798281	75.975143
141.814864	33.852777	75.980148
140.901585	34.020735	75.985153
140.629974	38.055726	75.990158
139.999478	36.308248	75.995162
138.946769	27.689222	76.000167
138.142307	37.331898	76.005172
137.952251	38.346511	76.010177
137.645429	36.397603	76.015182
136.633139	39.505143	76.020186
135.787079	30.602417	76.025191
135.092447	41.998574	76.030196
134.811845	39.274322	76.035201
133.664312	29.744708	76.040206
132.858938	37.108741	76.045210
132.445489	27.365871	76.050215
131.742270	33.873062	76.055220
131.527297	34.330230	76.060225
130.801165	34.764828	76.065230
129.698288	25.619199	76.070234
129.698001	30.255921	76.075239
128.793790	34.115813	76.080244
127.706066	27.997218	76.085249
127.113776	27.174092	76.090254
126.584664	38.179561	76.095258
126.375627	27.183483	76.100263
125.114717	38.731445	76.105268
124.413087	35.470339	76.110273
123.969838	32.598556	76.115278
123.380030	29.893654	76.120282
122.961885	19.892909	76.125287
121.924644	34.395223	76.130292
121.211960	23.184564	76.135297
121.030782	26.853457	76.140302
119.822969	30.958894	76.145306
119.221195	24.161966	76.150311
118.197452	38.651094	76.155316
118.090898	38.655717	76.160321
117.683373	32.368726	76.165326
116.627384	30.837349	76.170330
115.770336	22.084630	76.175335
115.082636	26.840436	76.180340
114.471832	29.429776	76.185345
114.241232	33.210636	76.190350
113.594033	37.180940	76.195354
112.537525	25.977803	76.200359
111.717725	28.811793	76.205364
111.196173	35.252170	76.210369
111.326709	30.170952	76.215374
110.163070	36.694801	76.220378
109.791979	14.794275	76.225383
109.133445	29.173113	76.230388
108.317464	37.994431	76.235393
107.410868	36.414000	76.240398
106.631137	26.789477	76.245402
106.486479	30.157646	76.250407
105.588839	32.329089	76.255412
104.470260	33.073873	76.260417
104.228543	35.184868	76.265422
103.753485	44.145794	76.270426
102.979989	25.725251	76.275431
101.662818	33.855335	76.280436
101.083481	37.062583	76.285441
100.846603	30.614336	76.290446
100.284923	37.972631	76.295450
99.931607	33.676656	76.300455
98.568883	34.860941	76.305460
97.948577	26.624004	76.310465
97.882055	25.942550	76.315470
96.866124	32.545353	76.320474
96.078970	31.788006	76.325479
95.396173	36.063625	76.330484
94.971413	36.219926	76.335489
94.531574	41.303657	76.340494
93.358465	33.970198	76.345498
92.827911	30.672357	76.350503
91.926417	47.472835	76.355508
91.620303	40.284966	76.360513
91.373719	31.266153	76.365518
90.361304	39.412300	76.370522
89.791033	26.485222	76.375527
89.122474	32.099034	76.380532
88.575181	33.180086	76.385537
87.268236	31.587816	76.390542
86.467606	32.797585	76.395546
86.369114	24.333923	76.400551
85.912614	29.988035	76.405556
85.226914	38.738116	76.410561
84.189540	25.451857	76.415566
83.456373	40.019237	76.420570
83.420517	23.780355	76.425575
82.374811	34.880832	76.430580
81.117449	34.873444	76.435585
81.140023	27.114324	76.440590
80.348789	37.622263	76.445594
79.968655	25.844474	76.450599
78.969208	31.771268	76.455604
78.321576	33.563789	76.460609
77.802287	36.149582	76.465614
77.450320	33.608617	76.470618
76.829203	29.219736	76.475623
75.843157	32.178027	76.480628
75.235554	30.803824	76.485633
74.116943	38.772939	76.490638
73.125500	35.728390	76.495642
72.807004	39.952221	76.500647
72.334073	37.205035	76.505652
72.004599	33.351560	76.510657
71.784476	33.724396	76.515662
70.354092	43.940025	76.520666
69.975603	32.184049	76.525671
69.277455	39.529421	76.530676
68.557773	37.493400	76.535681
67.713279	35.515134	76.540686
66.835960	43.739097	76.545690
66.807065	28.700790	76.550695
66.101805	40.049763	76.555700
64.864026	27.899389	76.560705
64.534059	29.762677	76.565710
63.775874	36.059446	76.570714
63.460563	26.223669	76.575719
62.301209	30.584764	76.580724
61.638485	27.561912	76.585729
61.171415	30.823804	76.590734
60.398229	44.432440	76.595738
60.364970	27.978670	76.600743
59.397439	34.572190	76.605748
58.798658	31.064458	76.610753
58.409094	31.815995	76.615758
56.983641	35.391602	76.620762
56.269880	25.718731	76.625767
55.664116	26.634066	76.630772
55.175860	32.372098	76.635777
54.878764	30.181946	76.640782
54.155381	40.048263	76.645786
53.291194	29.743344	76.650791
52.563239	35.429719	76.655796
51.910456	29.773244	76.660801
51.434152	34.720863	76.665806
50.411096	46.467476	76.670810
49.970226	32.329121	76.675815
49.351130	37.425678	76.680820
48.934855	34.212126	76.685825
47.948087	30.540768	76.690830
46.796543	46.744022	76.695834
46.460817	33.924629	76.700839
46.073344	42.680771	76.705844
45.745070	38.342963	76.710849
45.035939	37.806587	76.715854
44.032265	37.556897	76.720858
43.728467	28.261781	76.725863
42.405201	37.850029	76.730868
41.727362	38.109787	76.735873
41.282662	31.054429	76.740878
40.648749	43.834999	76.745882
40.577772	35.122511	76.750887
39.405958	47.541009	76.755892
38.311428	40.472598	76.760897
38.137377	29.803707	76.765902
37.442579	37.262095	76.770906
37.222886	31.509735	76.775911
36.110123	40.976098	76.780916
35.129258	38.387213	76.785921
35.181192	39.874188	76.790926
34.306692	37.968532	76.795930
33.727269	34.948171	76.800935
32.690611	42.798572	76.805940
31.990209	39.024769	76.810945
31.890034	37.498673	76.815950
30.591760	37.806933	76.820954
29.803713	35.900105	76.825959
29.458664	29.861802	76.830964
29.057873	37.869407	76.835969
28.390571	33.385400	76.840974
27.133165	34.822595	76.845978
26.809313	32.501090	76.850983
26.240139	42.412205	76.855988
25.693087	34.866953	76.860993
24.999662	36.635252	76.865998
23.983958	44.956997	76.871002
23.753951	35.101309	76.876007
22.966684	45.662251	76.881012
22.590031	43.065305	76.886017
21.548186	36.671349	76.891022
20.806074	29.478928	76.896026
20.285032	39.379209	76.901031
19.059297	39.882494	76.906036
18.416242	27.145255	76.911041
18.131454	34.841031	76.916046
17.415622	33.561380	76.921050
17.221539	26.112803	76.926055
16.871206	39.247122	76.931060
15.922053	40.699810	76.936065
15.383228	38.045153	76.941070
14.556720	36.494563	76.946074
13.729640	38.288916	76.951079
12.829451	37.227916	76.956084
12.261546	41.598774	76.961089
11.942954	36.302180	76.966094
10.642607	37.572761	76.971098
10.314892	34.988513	76.976103
9.320005	41.578531	76.981108
9.090128	36.505916	76.986113
8.675153	31.511716	76.991118
7.408398	43.686735	76.996122
7.048061	33.727257	77.001127
6.208937	46.430177	77.006132
6.198320	40.160323	77.011137
5.385344	41.659104	77.016142
4.044041	45.795353	77.021147
3.977379	34.281401	77.026151
3.242103	42.815471	77.031156
2.369835	35.372569	77.036161