Fri Mar 05 17:57:48 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.020493	96.106234	0.000000
-0.682301	94.705998	0.005005
-1.193123	52.258713	0.010010
-2.869140	8.024579	0.015014
-6.065990	-23.931106	0.020019
-11.460171	-27.351962	0.025024
-17.159829	-19.549404	0.030029
-21.917291	-25.126648	0.035034
-25.972008	-29.628499	0.040038
-29.477414	-25.393045	0.045043
-33.113110	-28.567656	0.050048
-37.165400	-27.594509	0.055053
-40.084311	-33.733106	0.060058
-44.217277	-26.256121	0.065062
-47.999209	-24.540738	0.070067
-51.263900	-27.383412	0.075072
-55.653877	-22.541583	0.080077
-58.716943	-24.451285	0.085082
-62.873409	-20.006255	0.090086
-66.565608	-22.611963	0.095091
-70.363117	-28.438457	0.100096
-74.570766	-19.957568	0.105101
-78.046951	-24.758221	0.110106
-81.866231	-20.557774	0.115110
-85.581243	-26.069388	0.120115
-89.106775	-30.956770	0.125120
-93.333497	-19.840785	0.130125
-96.798287	-26.363742	0.135130
-100.741394	-25.019966	0.140134
-104.478567	-27.016023	0.145139
-107.652161	-32.536714	0.150144
-111.867001	-27.437295	0.155149
-115.736333	-29.855384	0.160154
-119.567595	-23.154992	0.165158
-123.534693	-28.869180	0.170163
-126.915345	-25.971872	0.175168
-130.907774	-21.355777	0.180173
-134.767289	-27.946581	0.185178
-138.366954	-25.887970	0.190182
-142.441731	-19.355271	0.195187
-145.834873	-20.251794	0.200192
-149.780406	-20.457749	0.205197
-153.391545	-25.075899	0.210202
-157.168887	-35.537127	0.215206
-160.777352	-24.169602	0.220211
-164.201360	-28.171026	0.225216
-168.510823	-29.966841	0.230221
-172.055363	-32.354666	0.235226
-176.312785	-27.514856	0.240230
-179.979781	-30.286839	0.245235
-183.027369	-32.856461	0.250240
-187.136039	-30.880554	0.255245
-190.451561	-24.347521	0.260250
-194.709756	-33.482960	0.265254
-198.778582	-29.677762	0.270259
-202.496675	-28.085873	0.275264
-206.321311	-31.376722	0.280269
-210.228390	-30.428040	0.285274
-213.438290	-22.768506	0.290278
-216.836668	-29.040097	0.295283
-220.480725	-35.296123	0.300288
-224.666054	-26.394339	0.305293
-228.411533	-29.070140	0.310298
-232.674440	-25.536692	0.315302
-236.298410	-22.122566	0.320307
-239.806508	-27.696922	0.325312
-243.778385	-20.778348	0.330317
-247.112719	-29.230072	0.335322
-251.664270	-22.591134	0.340326
-255.288352	-25.623749	0.345331
-258.410325	-28.755429	0.350336
-262.135787	-25.815513	0.355341
-266.206998	-18.988283	0.360346
-269.889881	-22.304813	0.365350
-273.876918	-25.572785	0.370355
-277.650671	-17.827893	0.375360
-281.242676	-22.794264	0.380365
-284.872541	-33.102196	0.385370
-288.834705	-21.619683	0.390374
-292.687653	-23.866630	0.395379
-296.276507	-30.528754	0.400384
-299.899271	-36.187215	0.405389
-303.573748	-33.578661	0.410394
-307.643116	-28.864844	0.415398
-311.202725	-31.175936	0.420403
-315.086386	-26.565871	0.425408
-318.934638	-31.081252	0.430413
-322.705531	-28.204956	0.435418
-326.468846	-30.489811	0.440422
-330.335543	-28.735226	0.445427
-333.432709	-34.761407	0.450432
-337.742212	-19.608879	0.455437
-341.645740	-30.538524	0.460442
-345.473068	-23.712257	0.465446
-349.070846	-30.710352	0.470451
-352.526752	-30.804905	0.475456
-356.614900	-26.166858	0.480461
-360.011680	-31.795073	0.485466
-364.015494	-32.653709	0.490470
-368.040827	-38.906183	0.495475
-371.403939	-31.061927	0.500480
-375.755613	-27.742723	0.505485
-378.877017	-31.155038	0.510490
-382.830576	-23.557907	0.515494
-386.551102	-25.294395	0.520499
-390.015868	-30.191022	0.525504
-394.124281	-30.044127	0.530509
-397.790662	-33.302373	0.535514
-401.772685	-35.902277	0.540518
-405.957484	-26.586317	0.545523
-409.053033	-28.699330	0.550528
-412.998130	-16.559375	0.555533
-416.369658	-26.252317	0.560538
-420.551189	-37.196563	0.565542
-424.354106	-23.294137	0.570547
-427.643066	-38.239821	0.575552
-432.093292	-19.452552	0.580557
-435.897636	-32.431410	0.585562
-439.368467	-21.261314	0.590566
-442.856740	-22.917317	0.595571
-446.588281	-28.801037	0.600576
-450.564326	-23.469509	0.605581
-454.311935	-23.142004	0.610586
-457.762637	-24.511452	0.615590
-461.905391	-24.537157	0.620595
-465.343455	-21.373162	0.625600
-469.617264	-23.070043	0.630605
-473.549185	-23.246097	0.635610
-476.945623	-32.239509	0.640614
-480.593716	-28.972562	0.645619
-484.157020	-34.660730	0.650624
-488.282394	-36.389168	0.655629
-491.839084	-33.327620	0.660634
-495.865524	-33.251991	0.665638
-499.596371	-34.231269	0.670643
-503.170398	-38.889490	0.675648
-506.844194	-32.492792	0.680653
-510.795531	-34.793052	0.685658
-514.564782	-39.688163	0.690662
-518.186195	-22.375951	0.695667
-521.723817	-44.525704	0.700672
-525.992989	-32.036560	0.705677
-529.600118	-39.583243	0.710682
-533.139161	-34.513783	0.715686
-537.075550	-39.820565	0.720691
-540.750267	-36.751132	0.725696
-544.633226	-24.271603	0.730701
-548.395189	-31.364583	0.735706
-551.917783	-35.698200	0.740710
-555.932326	-37.346449	0.745715
-559.737341	-40.212487	0.750720
-563.759536	-24.987216	0.755725
-567.589445	-24.225327	0.760730
-570.902651	-30.227713	0.765734
-574.399708	-31.761475	0.770739
-578.128490	-37.426214	0.775744
-582.429775	-32.542426	0.780749
-585.661552	-32.249812	0.785754
-589.926067	-34.755379	0.790758
-593.506687	-29.404792	0.795763
-596.983496	-43.496216	0.800768
-600.851210	-28.251417	0.805773
-604.615450	-30.690223	0.810778
-608.625182	-38.426354	0.815782
-612.713218	-34.284654	0.820787
-616.008444	-33.846240	0.825792
-620.019360	-24.509607	0.830797
-623.474160	-27.860440	0.835802
-627.100372	-36.865794	0.840806
-631.272826	-33.010204	0.845811
-634.733795	-33.940922	0.850816
-638.864094	-21.074791	0.855821
-642.491860	-33.227558	0.860826
-646.384388	-32.439768	0.865830
-649.926356	-28.024124	0.870835
-653.085350	-32.265870	0.875840
-657.230722	-27.641834	0.880845
-661.398609	-39.090077	0.885850
-665.291118	-28.881294	0.890854
-669.141750	-26.652479	0.895859
-672.643153	-28.704233	0.900864
-676.406258	-27.292083	0.905869
-679.839679	-32.527602	0.910874
-683.372216	-32.434382	0.915878
-687.481910	-23.903472	0.920883
-690.915962	-32.658726	0.925888
-695.140684	-31.311555	0.930893
-699.032857	-36.070023	0.935898
-702.662504	-34.247063	0.940902
-706.682482	-25.604299	0.945907
-710.045503	-33.118741	0.950912
-713.874262	-23.960884	0.955917
-717.837234	-29.927024	0.960922
-721.385454	-30.316955	0.965926
-725.486458	-22.094884	0.970931
-728.671003	-32.765001	0.975936
-732.507768	-20.480232	0.980941
-736.375391	-34.959998	0.985946
-740.248568	-24.886655	0.990950
-744.049111	-26.442625	0.995955
-747.460750	-33.748961	1.000960
-751.665660	-28.957550	1.005965
-755.333115	-27.812882	1.010970
-759.345534	-28.179028	1.015974
-762.632646	-29.544210	1.020979
-766.320171	-35.588982	1.025984
-770.159264	-26.702208	1.030989
-774.030820	-33.534437	1.035994
-777.905102	-29.921799	1.040998
-782.186824	-25.129095	1.046003
-785.499971	-35.286549	1.051008
-788.844859	-25.460003	1.056013
-792.657805	-28.180887	1.061018
-796.495521	-27.576658	1.066022
-800.376068	-30.647854	1.071027
-804.264840	-30.904374	1.076032
-807.960142	-28.293301	1.081037
-811.725709	-25.852345	1.086042
-815.227448	-35.116992	1.091046
-819.458620	-24.055874	1.096051
-822.808968	-32.870036	1.101056
-826.911779	-26.915225	1.106061
-830.728518	-22.203074	1.111066
-834.314113	-25.136857	1.116070
-838.176837	-31.420017	1.121075
-841.826507	-27.770642	1.126080
-845.126913	-25.482846	1.131085
-848.856561	-27.980404	1.136090
-852.989766	-22.588406	1.141094
-857.244774	-20.185828	1.146099
-860.710707	-26.631738	1.151104
-864.105963	-32.051279	1.156109
-867.997809	-33.357478	1.161114
-871.774605	-29.678271	1.166118
-875.802295	-27.245770	1.171123
-878.967256	-37.486697	1.176128
-883.259100	-24.603811	1.181133
-886.968929	-30.939719	1.186138
-890.766552	-26.766708	1.191142
-894.788620	-22.147786	1.196147
-897.758618	-32.689527	1.201152
-901.868339	-31.089133	1.206157
-905.653718	-30.089385	1.211162
-909.752720	-24.727991	1.216166
-913.556107	-18.172764	1.221171
-917.296983	-28.895580	1.226176
-920.712655	-19.536944	1.231181
-924.169196	-22.929627	1.236186
-928.015724	-22.725907	1.241190
-931.981842	-18.970598	1.246195
-935.580327	-28.803073	1.251200
-939.514179	-18.404319	1.256205
-943.100177	-24.766246	1.261210
-947.266967	-28.942625	1.266214
-951.084903	-26.881014	1.271219
-954.450263	-32.328854	1.276224
-958.342749	-31.018574	1.281229
-962.448122	-39.232374	1.286234
-965.860882	-23.906819	1.291238
-969.766955	-26.010107	1.296243
-973.221473	-34.165544	1.301248
-977.324909	-27.436078	1.306253
-981.049411	-38.110932	1.311258
-984.805356	-35.305381	1.316262
-988.346845	-27.528758	1.321267
-992.163698	-31.404619	1.326272
-996.130238	-26.490051	1.331277
-999.757789	-27.576518	1.336282
-1003.470441	-24.583890	1.341286
-1007.324405	-27.933384	1.346291
-1010.904474	-33.080289	1.351296
-1014.791926	-18.443584	1.356301
-1018.597045	-24.208936	1.361306
-1022.357531	-27.579664	1.366310
-1025.986461	-24.236107	1.371315
-1029.821657	-40.300666	1.376320
-1033.582600	-33.905015	1.381325
-1037.203906	-33.059034	1.386330
-1041.450515	-21.982456	1.391334
-1045.307126	-24.506698	1.396339
-1048.500703	-36.570530	1.401344
-1052.452809	-34.982470	1.406349
-1056.129278	-29.388788	1.411354
-1059.646824	-30.432831	1.416358
-1063.994842	-28.751459	1.421363
-1067.231374	-30.157416	1.426368
-1071.534639	-22.396014	1.431373
-1075.137207	-29.955164	1.436378
-1078.759561	-26.980018	1.441382
-1082.533702	-25.379373	1.446387
-1085.904779	-34.126736	1.451392
-1090.095466	-17.170547	1.456397
-1093.745672	-30.150040	1.461402
-1097.233591	-35.336779	1.466406
-1101.550001	-25.739188	1.471411
-1104.843853	-34.394794	1.476416
-1108.707709	-23.068668	1.481421
-1112.669993	-27.758441	1.486426
-1116.605582	-18.828883	1.491430
-1120.489794	-21.435318	1.496435
-1123.901119	-41.164625	1.501440
-1127.338129	-29.186081	1.506445
-1131.288648	-27.568179	1.511450
-1135.023308	-30.805654	1.516454
-1138.993596	-25.812978	1.521459
-1142.635942	-27.784697	1.526464
-1146.595252	-29.275180	1.531469
-1150.122003	-27.321339	1.536474
-1153.643700	-25.532307	1.541478
-1157.799624	-21.191155	1.546483
-1161.343649	-25.651292	1.551488
-1165.229747	-20.905436	1.556493
-1169.337709	-26.238867	1.561498
-1172.991738	-25.117775	1.566502
-1176.730063	-25.862958	1.571507
-1179.891679	-31.221631	1.576512
-1184.065795	-29.853297	1.581517
-1187.927993	-26.008535	1.586522
-1191.404396	-30.085196	1.591526
-1195.187351	-28.484537	1.596531
-1198.814273	-37.947736	1.601536
-1202.995225	-27.737696	1.606541
-1207.065038	-25.406703	1.611546
-1210.317221	-28.238703	1.616550
-1214.499709	-24.924552	1.621555
-1217.671800	-31.353845	1.626560
-1221.820975	-20.641064	1.631565
-1225.521493	-31.243646	1.636570
-1229.243557	-31.060923	1.641574
-1233.224292	-25.407240	1.646579
-1236.469687	-37.517689	1.651584
-1240.208584	-26.030007	1.656589
-1244.300731	-28.440523	1.661594
-1247.729460	-29.033282	1.666598
-1251.949294	-27.225416	1.671603
-1255.684998	-32.124666	1.676608
-1259.389897	-23.594509	1.681613
-1262.889837	-28.212931	1.686618
-1266.478416	-24.369253	1.691622
-1270.581439	-31.045301	1.696627
-1274.353358	-30.394048	1.701632
-1278.111290	-28.753104	1.706637
-1281.878766	-24.713610	1.711642
-1285.440025	-39.443261	1.716646
-1289.346236	-26.656102	1.721651
-1292.935788	-37.334672	1.726656
-1296.857810	-21.034601	1.731661
-1300.808039	-36.406882	1.736666
-1304.056270	-36.725667	1.741670
-1308.143476	-30.077090	1.746675
-1311.984621	-34.126721	1.751680
-1315.803649	-18.935954	1.756685
-1319.513540	-30.774806	1.761690
-1323.435595	-29.085441	1.766694
-1327.052893	-21.942755	1.771699
-1330.807222	-35.638465	1.776704
-1334.419837	-21.829036	1.781709
-1338.504973	-29.070805	1.786714
-1341.897676	-24.187597	1.791718
-1345.858513	-21.370750	1.796723
-1349.458557	-29.630035	1.801728
-1353.340132	-26.762785	1.806733
-1356.906115	-32.529567	1.811738
-1360.462948	-32.451934	1.816742
-1364.542473	-26.151425	1.821747
-1368.643801	-36.729014	1.826752
-1372.318013	-33.073323	1.831757
-1375.930534	-32.292879	1.836762
-1379.418529	-29.390823	1.841766
-1383.172161	-27.135375	1.846771
-1386.910514	-36.864276	1.851776
-1391.206284	-29.124011	1.856781
-1394.905292	-34.568231	1.861786
-1398.684248	-31.129121	1.866790
-1402.424097	-29.347367	1.871795
-1405.660336	-40.247896	1.876800
-1409.593879	-36.684670	1.881805
-1413.037369	-33.841731	1.886810
-1417.103736	-26.603359	1.891814
-1421.284613	-26.473024	1.896819
-1424.913418	-41.672598	1.901824
-1428.581995	-34.321280	1.906829
-1432.317401	-30.609964	1.911834
-1435.988411	-31.464852	1.916838
-1439.995705	-32.000955	1.921843
-1443.627110	-36.339413	1.926848
-1447.436625	-38.148255	1.931853
-1451.267942	-29.957120	1.936858
-1454.791582	-32.207549	1.941862
-1458.620561	-30.886103	1.946867
-1462.021206	-37.212208	1.951872
-1466.007155	-34.648186	1.956877
-1469.720523	-26.023314	1.961882
-1473.483075	-41.627171	1.966886
-1477.527114	-35.981871	1.971891
-1481.314212	-34.802715	1.976896
-1485.389693	-34.865763	1.981901
-1489.028032	-32.833616	1.986906
-1492.145028	-37.905667	1.991910
-1496.112562	-26.401488	1.996915
-1500.328412	-30.545915	2.006912
-1500.832050	-29.207874	2.016909
-1498.407415	-30.719920	2.026906
-1495.777105	-29.604288	2.036902
-1493.515118	-30.266044	2.046899
-1491.659901	-31.937955	2.056896
-1490.035759	-35.557660	2.066893
-1487.940520	-32.824702	2.076890
-1486.017164	-33.692756	2.086886
-1484.032915	-33.860011	2.096883
-1481.888477	-38.275159	2.106880
-1480.551906	-35.147535	2.116877
-1478.521095	-37.264410	2.126874
-1476.474453	-31.528297	2.136870
-1474.670856	-30.420784	2.146867
-1472.649571	-35.079897	2.156864
-1470.844510	-29.996694	2.166861
-1468.966072	-27.222684	2.176858
-1466.843349	-28.921622	2.186854
-1464.977776	-33.468949	2.196851
-1463.125057	-34.396728	2.206848
-1461.432959	-37.709917	2.216845
-1459.694542	-30.460699	2.226842
-1457.631450	-35.737567	2.236838
-1455.526377	-34.864636	2.246835
-1453.994919	-24.541117	2.256832
-1451.870919	-36.356899	2.266829
-1449.878966	-29.047215	2.276826
-1448.007373	-31.332786	2.286822
-1446.351592	-30.681597	2.296819
-1444.386067	-30.894768	2.306816
-1442.405513	-37.934781	2.316813
-1440.735365	-34.481586	2.326810
-1438.775146	-36.309219	2.336806
-1437.027948	-28.440841	2.346803
-1435.137426	-28.544097	2.356800
-1433.113183	-37.959599	2.366797
-1431.362300	-39.226321	2.376794
-1429.307887	-35.552004	2.386790
-1427.214328	-33.650853	2.396787
-1425.513062	-34.232236	2.406784
-1423.539256	-33.050879	2.416781
-1422.016595	-39.393855	2.426778
-1419.937591	-34.829752	2.436774
-1418.038868	-34.741669	2.446771
-1416.507996	-33.854136	2.456768
-1414.459852	-37.443781	2.466765
-1412.283661	-30.701999	2.476762
-1410.374042	-37.163769	2.486758
-1408.824336	-29.195850	2.496755
-1406.953497	-34.321890	2.506752
-1404.808423	-34.066390	2.516749
-1402.877258	-35.079315	2.526746
-1401.004541	-30.684277	2.536742
-1399.239043	-28.959530	2.546739
-1397.305980	-35.167667	2.556736
-1395.631794	-38.160563	2.566733
-1393.447103	-27.903688	2.576730
-1391.855870	-27.485291	2.586726
-1390.242342	-25.333561	2.596723
-1387.954972	-23.686040	2.606720
-1385.908427	-27.831215	2.616717
-1384.053088	-29.763596	2.626714
-1382.530201	-28.396324	2.636710
-1380.439749	-25.518808	2.646707
-1378.479967	-30.175893	2.656704
-1376.772243	-29.769820	2.666701
-1374.770083	-26.355514	2.676698
-1373.061410	-26.088542	2.686694
-1371.007603	-27.414769	2.696691
-1369.281749	-33.523395	2.706688
-1367.492174	-30.902447	2.716685
-1365.389105	-32.083393	2.726682
-1363.643343	-30.303351	2.736678
-1361.592193	-26.151588	2.746675
-1359.781540	-21.036025	2.756672
-1357.990774	-31.031486	2.766669
-1355.881371	-23.214705	2.776666
-1354.252702	-26.182919	2.786662
-1352.469353	-23.600436	2.796659
-1350.109268	-22.172946	2.806656
-1348.587439	-24.708775	2.816653
-1346.664680	-27.610375	2.826650
-1344.788598	-25.840127	2.836646
-1342.745117	-25.520935	2.846643
-1341.084063	-24.673138	2.856640
-1339.435931	-23.796429	2.866637
-1337.414331	-29.364988	2.876634
-1335.464447	-27.821291	2.886630
-1333.544205	-24.161721	2.896627
-1331.544935	-26.358689	2.906624
-1329.841535	-31.917359	2.916621
-1327.749659	-24.994617	2.926618
-1326.073470	-25.972981	2.936614
-1324.139192	-26.229997	2.946611
-1322.298582	-22.852943	2.956608
-1320.162997	-25.655953	2.966605
-1318.397350	-22.464272	2.976602
-1316.815153	-25.305018	2.986598
-1314.914908	-23.979155	2.996595
-1312.920784	-30.181213	3.006592
-1310.912281	-32.412800	3.016589
-1309.005882	-34.157498	3.026586
-1307.308807	-26.006240	3.036582
-1305.185751	-29.037764	3.046579
-1303.625746	-26.166853	3.056576
-1301.672491	-25.278953	3.066573
-1299.720484	-31.024243	3.076570
-1297.937031	-24.999507	3.086566
-1296.132152	-28.136418	3.096563
-1293.700590	-31.803121	3.106560
-1292.272946	-31.435843	3.116557
-1290.712075	-27.191329	3.126554
-1288.663068	-26.591911	3.136550
-1286.201105	-25.902266	3.146547
-1284.781602	-25.318936	3.156544
-1282.684985	-29.361508	3.166541
-1281.002128	-28.528210	3.176538
-1279.316819	-22.806708	3.186534
-1277.357619	-20.566532	3.196531
-1275.076602	-31.952556	3.206528
-1273.389660	-29.810914	3.216525
-1271.522751	-23.537398	3.226522
-1269.607130	-22.447650	3.236518
-1268.138850	-22.007910	3.246515
-1265.993480	-21.125463	3.256512
-1264.038713	-26.558526	3.266509
-1262.229049	-26.426060	3.276506
-1260.262231	-25.537137	3.286502
-1258.481231	-24.760584	3.296499
-1256.649950	-26.643224	3.306496
-1254.555885	-26.123622	3.316493
-1252.584874	-25.284312	3.326490
-1251.035849	-25.631196	3.336486
-1249.087240	-23.839317	3.346483
-1247.382648	-22.199444	3.356480
-1245.175460	-18.912572	3.366477
-1243.378345	-27.536821	3.376474
-1241.933188	-22.233188	3.386470
-1239.728302	-21.440770	3.396467
-1237.697021	-23.375930	3.406464
-1236.096153	-24.825351	3.416461
-1233.880846	-24.970945	3.426458
-1231.825375	-19.316537	3.436454
-1230.484247	-26.479860	3.446451
-1228.462662	-23.303802	3.456448
-1226.485526	-25.012385	3.466445
-1224.703396	-25.240233	3.476442
-1222.593222	-25.062665	3.486438
-1220.811377	-22.326673	3.496435
-1219.175712	-25.949625	3.506432
-1217.718094	-25.636046	3.516429
-1215.490617	-24.138247	3.526426
-1213.112137	-27.158458	3.536422
-1211.333177	-28.427932	3.546419
-1209.489500	-28.471400	3.556416
-1207.647475	-25.970826	3.566413
-1206.004821	-26.451088	3.576410
-1204.080792	-25.593166	3.586406
-1202.289218	-27.407829	3.596403
-1200.137845	-35.180805	3.606400
-1198.275091	-30.801368	3.616397
-1196.497301	-21.410781	3.626394
-1194.597180	-25.777112	3.636390
-1192.726200	-25.160175	3.646387
-1191.197386	-18.301940	3.656384
-1189.021098	-25.556247	3.666381
-1187.074830	-24.921351	3.676378
-1185.373027	-22.712543	3.686374
-1183.362033	-28.151382	3.696371
-1181.483576	-30.038355	3.706368
-1179.583729	-25.075867	3.716365
-1177.559636	-24.488154	3.726362
-1175.988440	-22.743195	3.736358
-1174.209442	-24.521087	3.746355
-1171.865677	-27.715709	3.756352
-1170.069534	-25.968843	3.766349
-1168.170495	-26.880116	3.776346
-1166.564839	-24.471166	3.786342
-1164.915049	-22.713511	3.796339
-1162.726081	-23.996444	3.806336
-1160.836173	-19.488680	3.816333
-1158.976220	-19.809459	3.826330
-1157.288717	-22.338518	3.836326
-1155.237438	-23.187294	3.846323
-1153.229773	-27.774491	3.856320
-1151.601855	-18.361463	3.866317
-1149.624225	-20.259542	3.876314
-1147.737790	-21.231943	3.886310
-1145.704354	-21.784160	3.896307
-1143.932175	-18.727600	3.906304
-1142.118736	-21.756816	3.916301
-1140.303867	-24.462562	3.926298
-1138.254410	-27.044780	3.936294
-1136.589675	-25.316338	3.946291
-1134.691085	-24.801669	3.956288
-1132.553299	-23.771037	3.966285
-1130.742437	-30.009950	3.976282
-1128.809383	-20.282551	3.986278
-1127.195049	-16.791761	3.996275
-1125.517901	-17.716450	4.006272
-1123.361615	-16.286121	4.016269
-1121.212846	-24.254416	4.026266
-1119.615731	-20.279270	4.036262
-1117.650260	-15.275116	4.046259
-1115.739066	-12.591312	4.056256
-1114.210612	-24.646312	4.066253
-1111.825430	-26.409026	4.076250
-1110.061899	-19.353011	4.086246
-1108.501667	-20.596890	4.096243
-1106.627412	-21.826266	4.106240
-1104.423002	-20.484149	4.116237
-1102.675687	-16.908821	4.126234
-1100.836001	-23.269174	4.136230
-1098.909359	-21.541549	4.146227
-1097.139084	-18.304640	4.156224
-1095.248984	-16.312208	4.166221
-1093.055744	-22.277518	4.176218
-1091.581323	-21.964969	4.186214
-1089.657269	-23.465992	4.196211
-1087.875158	-17.121904	4.206208
-1085.745132	-20.329622	4.216205
-1083.631595	-25.483195	4.226202
-1081.940075	-26.478048	4.236198
-1080.357183	-17.387771	4.246195
-1078.411191	-17.532769	4.256192
-1076.271447	-15.605520	4.266189
-1074.509249	-19.284936	4.276186
-1072.739474	-18.465389	4.286182
-1070.616928	-21.002398	4.296179
-1068.646369	-21.350272	4.306176
-1066.968237	-25.069920	4.316173
-1065.301099	-25.590317	4.326170
-1063.436956	-25.270614	4.336166
-1061.499787	-26.382118	4.346163
-1059.433209	-24.801586	4.356160
-1057.870014	-23.478440	4.366157
-1055.819618	-26.733395	4.376154
-1053.823413	-25.114758	4.386150
-1051.841251	-21.802755	4.396147
-1050.210718	-22.997839	4.406144
-1048.350790	-24.550153	4.416141
-1046.176876	-24.570523	4.426138
-1044.302958	-30.056800	4.436134
-1042.860299	-20.037715	4.446131
-1040.736391	-21.444345	4.456128
-1038.844560	-26.960327	4.466125
-1037.147993	-24.902155	4.476122
-1035.184146	-24.124674	4.486118
-1033.453454	-19.712918	4.496115
-1031.357710	-21.156089	4.506112
-1029.436725	-25.241410	4.516109
-1027.559671	-28.978636	4.526106
-1025.676532	-24.716000	4.536102
-1024.031848	-16.180319	4.546099
-1022.264990	-22.165795	4.556096
-1020.081085	-18.256007	4.566093
-1018.231414	-28.154875	4.576090
-1016.281730	-23.890242	4.586086
-1014.348627	-22.683073	4.596083
-1012.366626	-23.119576	4.606080
-1010.852963	-20.744750	4.616077
-1009.200614	-21.082735	4.626074
-1006.833815	-22.742928	4.636070
-1005.021293	-23.932349	4.646067
-1003.559195	-21.839809	4.656064
-1001.369092	-23.160671	4.666061
-999.399052	-22.355729	4.676058
-997.543160	-27.736454	4.686054
-995.542815	-23.667806	4.696051
-994.019142	-28.798020	4.706048
-992.161733	-28.996677	4.716045
-989.891206	-29.147713	4.726042
-987.964171	-24.288884	4.736038
-986.160434	-25.268457	4.746035
-984.579186	-29.095716	4.756032
-982.974253	-30.728782	4.766029
-980.840809	-25.460834	4.776026
-978.719010	-31.954637	4.786022
-977.023426	-24.761327	4.796019
-975.040027	-26.453334	4.806016
-973.181471	-32.889244	4.816013
-971.430034	-34.105187	4.826010
-969.241123	-38.939121	4.836006
-967.788621	-33.972810	4.846003
-965.816842	-31.349100	4.856000
-963.889073	-30.744218	4.865997
-961.555513	-31.124789	4.875994
-959.913678	-29.315185	4.885990
-958.414810	-33.059777	4.895987
-956.603406	-29.077729	4.905984
-954.307908	-30.519616	4.915981
-952.732777	-33.087406	4.925978
-950.729217	-25.479095	4.935974
-948.676094	-30.305511	4.945971
-946.847666	-32.266408	4.955968
-945.261695	-27.793547	4.965965
-943.221803	-24.721216	4.975962
-941.238352	-26.939014	4.985958
-939.448914	-31.058493	4.995955
-937.428832	-26.072388	5.005952
-935.680392	-25.702501	5.015949
-933.687230	-36.322174	5.025946
-932.154972	-28.807438	5.035942
-930.264202	-26.642866	5.045939
-928.092795	-27.239064	5.055936
-926.196246	-31.285658	5.065933
-924.634758	-38.454059	5.075930
-922.785752	-30.560475	5.085926
-920.589684	-24.124541	5.095923
-919.000327	-21.840708	5.105920
-916.861849	-25.065419	5.115917
-914.908199	-28.189519	5.125914
-913.086878	-23.577415	5.135910
-911.062013	-30.131456	5.145907
-909.453572	-19.742450	5.155904
-907.690516	-24.985104	5.165901
-905.665347	-29.415420	5.175898
-903.694734	-30.967949	5.185894
-901.998023	-27.682809	5.195891
-900.091463	-27.901884	5.205888
-898.160279	-26.083235	5.215885
-896.260839	-24.025814	5.225882
-894.235802	-24.303303	5.235878
-892.716700	-28.085830	5.245875
-890.614880	-29.160360	5.255872
-888.569407	-27.104176	5.265869
-886.892133	-27.236053	5.275866
-884.950880	-28.093846	5.285862
-883.192320	-26.023364	5.295859
-881.531761	-31.434354	5.305856
-879.437365	-28.356470	5.315853
-877.346481	-26.050157	5.325850
-875.560315	-31.255427	5.335846
-873.922138	-27.176139	5.345843
-871.975501	-28.529012	5.355840
-869.974654	-29.667910	5.365837
-868.060091	-33.932084	5.375834
-866.498696	-30.080525	5.385830
-864.432946	-29.919216	5.395827
-862.345030	-27.666103	5.405824
-860.530996	-30.557829	5.415821
-858.682630	-25.228397	5.425818
-856.769722	-32.877698	5.435814
-855.099191	-30.774174	5.445811
-853.495685	-32.747992	5.455808
-851.113133	-25.732304	5.465805
-849.194377	-26.103294	5.475802
-847.473582	-26.289470	5.485798
-845.748344	-28.257480	5.495795
-843.877831	-30.365561	5.505792
-841.609787	-33.898298	5.515789
-839.914889	-31.558649	5.525786
-838.419498	-27.950738	5.535782
-836.211589	-29.928006	5.545779
-834.359821	-26.774975	5.555776
-832.539451	-25.162774	5.565773
-830.707603	-29.843189	5.575770
-828.470853	-39.685374	5.585766
-826.999998	-25.738908	5.595763
-825.092539	-30.576675	5.605760
-823.044234	-34.944303	5.615757
-821.212276	-32.217586	5.625754
-819.552524	-35.214098	5.635750
-817.276281	-30.868858	5.645747
-815.484294	-35.050237	5.655744
-813.827119	-32.805595	5.665741
-811.943041	-31.423046	5.675738
-809.937256	-32.507418	5.685734
-808.223597	-30.931827	5.695731
-806.091266	-33.160681	5.705728
-804.285358	-29.933976	5.715725
-802.403370	-33.782350	5.725722
-800.682431	-28.337760	5.735718
-798.907824	-29.197267	5.745715
-796.689776	-32.008258	5.755712
-794.720275	-30.617243	5.765709
-793.106226	-29.006771	5.775706
-791.027321	-29.813856	5.785702
-789.366494	-27.715049	5.795699
-787.522015	-30.952655	5.805696
-785.561157	-24.862689	5.815693
-783.632682	-27.439480	5.825690
-781.787715	-27.605982	5.835686
-779.979827	-28.101305	5.845683
-777.889801	-28.231181	5.855680
-776.304994	-32.404681	5.865677
-774.616858	-33.291403	5.875674
-772.560930	-27.115566	5.885670
-770.608845	-28.293957	5.895667
-768.423074	-34.339897	5.905664
-766.930192	-30.611533	5.915661
-764.631235	-29.786329	5.925658
-763.118580	-31.361867	5.935654
-761.533841	-36.392750	5.945651
-759.508276	-30.622592	5.955648
-757.371378	-32.422641	5.965645
-755.400416	-33.581931	5.975642
-753.371205	-36.880616	5.985638
-751.957384	-29.913684	5.995635
-749.806266	-33.399227	6.005632
-748.255766	-29.346887	6.015629
-746.243282	-35.417219	6.025626
-744.317030	-32.520766	6.035622
-742.378326	-28.775214	6.045619
-740.406281	-32.462664	6.055616
-738.814715	-33.896055	6.065613
-736.892321	-26.220887	6.075610
-734.576280	-33.268184	6.085606
-733.386279	-31.204620	6.095603
-731.355971	-34.421354	6.105600
-729.319689	-34.343642	6.115597
-727.207001	-34.383933	6.125594
-725.604025	-29.496772	6.135590
-723.291193	-30.150123	6.145587
-722.099570	-25.470386	6.155584
-720.179151	-26.728943	6.165581
-718.031624	-26.446359	6.175578
-715.987490	-24.426124	6.185574
-714.164658	-27.742326	6.195571
-712.560137	-27.414012	6.205568
-710.300436	-23.478141	6.215565
-708.690278	-24.240245	6.225562
-707.066050	-29.070556	6.235558
-704.781349	-30.887863	6.245555
-703.084074	-23.318798	6.255552
-701.173158	-26.979081	6.265549
-698.991175	-31.690089	6.275546
-697.473778	-25.775503	6.285542
-695.652707	-28.497701	6.295539
-693.839379	-25.598948	6.305536
-691.648641	-24.937966	6.315533
-689.703623	-30.811150	6.325530
-687.946836	-28.233372	6.335526
-686.043776	-20.888237	6.345523
-684.387008	-25.390564	6.355520
-682.586924	-24.335554	6.365517
-680.544741	-18.522182	6.375514
-678.322420	-27.240843	6.385510
-676.885131	-25.079390	6.395507
-674.776104	-26.908073	6.405504
-672.703557	-22.626454	6.415501
-671.206428	-17.531274	6.425498
-669.243136	-23.568425	6.435494
-667.564412	-19.184395	6.445491
-665.715388	-16.878717	6.455488
-663.501394	-16.294058	6.465485
-661.549340	-19.894567	6.475482
-659.964697	-29.081342	6.485478
-658.075037	-27.890620	6.495475
-656.228230	-23.253955	6.505472
-654.111766	-26.005953	6.515469
-652.386227	-28.275466	6.525466
-650.573225	-23.980778	6.535462
-648.494873	-27.917259	6.545459
-646.608664	-23.710058	6.555456
-644.952942	-19.724984	6.565453
-642.861897	-19.376462	6.575450
-641.099623	-20.473892	6.585446
-639.308329	-21.203311	6.595443
-637.584452	-26.813745	6.605440
-635.428936	-27.980318	6.615437
-633.500360	-27.378451	6.625434
-631.649078	-29.000118	6.635430
-629.660338	-24.705070	6.645427
-627.877520	-27.124250	6.655424
-626.071306	-19.419363	6.665421
-624.475352	-22.947156	6.675418
-622.401617	-19.265705	6.685414
-620.334648	-22.515052	6.695411
-618.624032	-26.122742	6.705408
-616.638131	-15.997500	6.715405
-614.818002	-22.987569	6.725402
-613.207646	-22.282735	6.735398
-610.920365	-21.853427	6.745395
-609.313907	-21.326397	6.755392
-607.332315	-17.999701	6.765389
-605.365733	-27.583798	6.775386
-603.633195	-24.722595	6.785382
-601.699003	-27.001723	6.795379
-599.956259	-23.526331	6.805376
-597.853639	-23.634376	6.815373
-595.926581	-27.286103	6.825370
-594.448802	-28.483317	6.835366
-592.029411	-22.139577	6.845363
-590.388727	-22.645941	6.855360
-588.581060	-22.518952	6.865357
-586.994475	-17.322738	6.875354
-584.713006	-18.480967	6.885350
-582.934056	-22.740631	6.895347
-581.172707	-24.919496	6.905344
-579.169888	-26.028466	6.915341
-577.343441	-24.574937	6.925338
-575.298705	-26.314312	6.935334
-573.575093	-25.337005	6.945331
-571.631848	-18.504263	6.955328
-569.974943	-18.580554	6.965325
-567.906271	-14.550860	6.975322
-566.141854	-18.612394	6.985318
-563.964672	-11.437258	6.995315
-562.092708	-23.219205	7.005312
-560.724616	-21.424009	7.015309
-558.739519	-19.841855	7.025306
-556.792471	-20.904002	7.035302
-554.907411	-26.514075	7.045299
-552.572188	-27.005042	7.055296
-550.878829	-25.304433	7.065293
-549.113675	-26.446469	7.075290
-547.289341	-23.625151	7.085286
-545.364827	-28.465432	7.095283
-543.625383	-22.560153	7.105280
-541.849310	-20.394308	7.115277
-539.622462	-25.056293	7.125274
-537.940290	-23.397310	7.135270
-535.873713	-25.287779	7.145267
-534.035006	-27.955830	7.155264
-532.522951	-20.921539	7.165261
-530.467586	-19.244002	7.175258
-528.351807	-27.763143	7.185254
-526.781474	-27.639251	7.195251
-524.806315	-25.010173	7.205248
-522.929849	-19.375458	7.215245
-521.063958	-24.776384	7.225242
-519.406575	-18.459274	7.235238
-517.176407	-27.580125	7.245235
-515.430029	-25.461625	7.255232
-513.276524	-23.029188	7.265229
-511.701907	-22.967552	7.275226
-509.589609	-19.601647	7.285222
-507.874682	-21.416187	7.295219
-506.129195	-26.384167	7.305216
-504.557635	-22.792935	7.315213
-502.033695	-19.606460	7.325210
-500.271432	-22.773879	7.335206
-498.487810	-25.005192	7.345203
-496.752082	-24.857169	7.355200
-494.908243	-23.392143	7.365197
-492.973541	-20.343661	7.375194
-490.933366	-16.898320	7.385190
-488.803254	-21.540863	7.395187
-487.031964	-23.335968	7.405184
-485.403502	-24.301382	7.415181
-483.551802	-28.348374	7.425178
-481.524031	-24.370495	7.435174
-479.807680	-26.562628	7.445171
-477.841188	-30.686373	7.455168
-476.000217	-26.943931	7.465165
-474.420856	-21.078558	7.475162
-472.114738	-25.842358	7.485158
-470.241080	-28.376990	7.495155
-468.287467	-31.257562	7.505152
-466.692830	-23.754025	7.515149
-464.839168	-21.753678	7.525146
-462.816111	-24.987984	7.535142
-461.096680	-21.620873	7.545139
-458.834587	-25.877080	7.555136
-457.285426	-30.632085	7.565133
-455.334928	-22.342176	7.575130
-453.430022	-23.801738	7.585126
-451.655369	-26.281069	7.595123
-449.652075	-26.381016	7.605120
-448.118489	-23.397918	7.615117
-446.084349	-30.715742	7.625114
-443.881876	-31.755428	7.635110
-442.204019	-30.347542	7.645107
-440.086995	-30.001411	7.655104
-438.712407	-26.283937	7.665101
-436.661322	-23.315576	7.675098
-434.701821	-24.509092	7.685094
-432.659631	-31.387646	7.695091
-430.802692	-31.168928	7.705088
-429.200196	-26.262525	7.715085
-427.223748	-28.316149	7.725082
-425.301968	-28.848341	7.735078
-423.675335	-24.665820	7.745075
-421.590140	-26.185727	7.755072
-419.556167	-26.473714	7.765069
-417.952469	-25.649257	7.775066
-415.737181	-30.608509	7.785062
-414.143272	-27.208687	7.795059
-412.156340	-27.549158	7.805056
-410.401072	-20.781786	7.815053
-408.365508	-26.920284	7.825050
-406.699276	-22.016146	7.835046
-404.690528	-29.355149	7.845043
-402.764503	-23.497711	7.855040
-400.782249	-25.124326	7.865037
-398.897125	-17.621329	7.875034
-397.562213	-28.348679	7.885030
-395.587582	-30.637261	7.895027
-393.230962	-22.315824	7.905024
-391.333124	-21.585688	7.915021
-389.735788	-19.236442	7.925018
-387.934893	-20.736189	7.935014
-386.085700	-25.098515	7.945011
-383.861290	-23.349943	7.955008
-382.219919	-23.467836	7.965005
-380.171428	-23.881271	7.975002
-378.476197	-20.454966	7.984998
-376.797083	-20.937320	7.994995
-374.628243	-24.772754	8.004992
-372.540499	-24.061872	8.014989
-370.866344	-19.383192	8.024986
-369.084442	-22.550496	8.034982
-367.075017	-28.825320	8.044979
-365.279668	-28.858835	8.054976
-363.517207	-24.653745	8.064973
-361.562516	-24.332154	8.074970
-359.596065	-24.519305	8.084966
-357.763449	-21.669157	8.094963
-355.734922	-24.564762	8.104960
-353.864476	-18.521555	8.114957
-352.397930	-18.355714	8.124954
-350.492209	-22.521767	8.134950
-348.145157	-24.392908	8.144947
-346.485997	-21.199253	8.154944
-344.747134	-17.865156	8.164941
-342.889088	-19.934548	8.174938
-341.048193	-21.881194	8.184934
-338.941994	-26.134511	8.194931
-337.484087	-23.731389	8.204928
-335.064260	-24.510401	8.214925
-333.360559	-21.949140	8.224922
-331.204662	-27.309383	8.234918
-329.883495	-21.126356	8.244915
-327.583796	-23.480993	8.254912
-325.833698	-25.694197	8.264909
-324.042699	-17.064477	8.274906
-322.089019	-27.904792	8.284902
-320.148723	-31.994231	8.294899
-318.096803	-21.358175	8.304896
-316.641493	-29.478797	8.314893
-314.910312	-26.252406	8.324890
-312.945887	-23.565378	8.334886
-310.632551	-23.934188	8.344883
-308.944242	-22.253125	8.354880
-307.243592	-24.434737	8.364877
-305.241139	-21.207431	8.374874
-303.440014	-18.865394	8.384870
-301.419172	-27.374727	8.394867
-299.522403	-20.580905	8.404864
-297.822063	-22.110326	8.414861
-295.760973	-22.380431	8.424858
-293.793038	-22.116165	8.434854
-291.929204	-26.949729	8.444851
-290.186066	-31.484536	8.454848
-288.781519	-25.163209	8.464845
-286.609436	-23.114073	8.474842
-284.696288	-29.711375	8.484838
-282.566532	-27.595476	8.494835
-280.937898	-23.806347	8.504832
-278.973421	-29.079144	8.514829
-277.047948	-19.635550	8.524826
-275.167652	-23.145353	8.534822
-273.517067	-25.330003	8.544819
-271.507591	-29.510979	8.554816
-269.512966	-23.487525	8.564813
-267.609908	-28.003633	8.574810
-265.660380	-30.076516	8.584807
-263.779810	-23.886423	8.594803
-262.069504	-18.848678	8.604800
-260.506506	-21.371461	8.614797
-258.680109	-21.850399	8.624794
-256.288747	-18.072468	8.634791
-254.425908	-25.545972	8.644787
-252.606482	-21.509369	8.654784
-250.834565	-19.505277	8.664781
-248.843728	-17.149266	8.674778
-247.233967	-24.874489	8.684775
-245.229356	-22.323297	8.694771
-243.254350	-23.009111	8.704768
-241.399441	-23.132570	8.714765
-239.704847	-22.245129	8.724762
-237.656680	-22.565229	8.734759
-235.849791	-26.344351	8.744755
-234.028551	-19.737374	8.754752
-232.370536	-22.539002	8.764749
-230.245381	-18.363274	8.774746
-228.204642	-18.320584	8.784743
-226.714399	-21.112801	8.794739
-224.449004	-28.066296	8.804736
-222.414464	-23.435552	8.814733
-220.717177	-21.327943	8.824730
-219.198720	-26.003694	8.834727
-217.042604	-20.275980	8.844723
-214.882989	-27.204689	8.854720
-213.563976	-27.127327	8.864717
-211.151068	-26.378197	8.874714
-209.875023	-24.108608	8.884711
-207.547500	-22.291058	8.894707
-205.349387	-35.463040	8.904704
-203.856808	-35.238103	8.914701
-202.166622	-28.190167	8.924698
-200.277326	-26.463731	8.934695
-198.336583	-31.031593	8.944691
-196.206660	-35.733860	8.954688
-194.592816	-28.937432	8.964685
-192.773158	-28.962066	8.974682
-190.537215	-28.705750	8.984679
-188.934399	-35.967171	8.994675
-187.094181	-32.451756	9.004672
-185.304451	-30.196237	9.014669
-182.966173	-31.682117	9.024666
-181.416388	-25.140730	9.034663
-179.655803	-26.772845	9.044659
-177.886910	-32.314367	9.054656
-175.810391	-30.941490	9.064653
-174.234535	-29.198172	9.074650
-171.993440	-28.871605	9.084647
-170.051301	-27.527807	9.094643
-168.055331	-36.074121	9.104640
-166.642042	-29.942016	9.114637
-164.599764	-32.004356	9.124634
-162.688506	-30.641413	9.134631
-160.598401	-35.913639	9.144627
-158.819624	-28.879808	9.154624
-157.082146	-27.167007	9.164621
-155.227710	-29.712546	9.174618
-153.145555	-27.704202	9.184615
-151.203618	-30.584244	9.194611
-149.788008	-30.171718	9.204608
-147.834673	-29.248130	9.214605
-145.888216	-24.037972	9.224602
-143.474992	-29.341221	9.234599
-142.004633	-30.232227	9.244595
-140.404158	-30.603969	9.254592
-138.250895	-30.989706	9.264589
-136.422908	-27.657043	9.274586
-134.494917	-27.571019	9.284583
-132.608231	-25.390932	9.294579
-130.510716	-26.361480	9.304576
-129.003376	-25.008270	9.314573
-127.190697	-31.646271	9.324570
-125.139068	-28.440869	9.334567
-123.190521	-32.076716	9.344563
-121.315813	-26.334011	9.354560
-119.725608	-31.775926	9.364557
-117.783924	-31.071517	9.374554
-115.535192	-28.538640	9.384551
-113.684231	-33.602137	9.394547
-112.054303	-32.377430	9.404544
-110.203160	-33.938678	9.414541
-108.115452	-35.583463	9.424538
-106.592169	-34.532798	9.434535
-104.555584	-38.946925	9.444531
-102.435380	-39.036815	9.454528
-100.526407	-34.112760	9.464525
-99.124028	-36.324010	9.474522
-97.003793	-31.389446	9.484519
-94.947591	-31.944404	9.494515
-93.297440	-32.597212	9.504512
-91.536447	-30.633892	9.514509
-89.636573	-26.518413	9.524506
-87.746646	-33.241347	9.534503
-85.679511	-30.376296	9.544499
-83.650821	-24.822346	9.554496
-82.020874	-31.728018	9.564493
-80.363881	-27.677996	9.574490
-78.321147	-24.744304	9.584487
-75.803380	-27.193502	9.594483
-74.300880	-33.647762	9.604480
-72.699568	-31.602107	9.614477
-70.612733	-26.103214	9.624474
-69.033168	-29.351714	9.634471
-67.048063	-34.010243	9.644467
-65.065065	-31.722306	9.654464
-63.254218	-31.816492	9.664461
-61.623388	-29.800803	9.674458
-59.464085	-31.254855	9.684455
-57.556090	-32.580385	9.694451
-55.590435	-29.760699	9.704448
-53.916537	-32.293151	9.714445
-51.891626	-28.942889	9.724442
-50.003799	-26.742391	9.734439
-48.239591	-31.269345	9.744435
-46.358027	-26.918792	9.754432
-44.351697	-27.383642	9.764429
-42.647651	-19.756708	9.774426
-40.726979	-22.623799	9.784423
-39.134767	-32.146188	9.794419
-36.950180	-26.863395	9.804416
-34.695320	-22.921348	9.814413
-33.301310	-29.964625	9.824410
-31.524777	-25.638359	9.834407
-29.455681	-28.150152	9.844403
-27.378026	-34.928256	9.854400
-25.556083	-31.289790	9.864397
-23.608792	-20.960458	9.874394
-22.273758	-22.543525	9.884391
-20.063363	-25.041534	9.894387
-18.103377	-25.172111	9.904384
-16.127185	-26.322164	9.914381
-14.522679	-33.016885	9.924378
-12.748021	-27.949743	9.934375
-10.807714	-29.013537	9.944371
-8.871173	-32.985293	9.954368
-7.066291	-22.285845	9.964365
-5.897796	-1.278032	9.974362
-4.438011	34.665201	9.984359
-2.345235	78.511692	9.994355
-1.134002	121.384134	10.004352
0.000000	162.782319	10.009357
1.034657	195.538011	10.014362
1.713921	224.623936	10.019367
2.318464	237.257578	10.024371
2.605809	262.436697	10.029376
2.453984	271.316238	10.034381
2.949374	272.734076	10.039386
3.270001	288.243838	10.044391
3.661427	291.577019	10.049395
3.349639	290.884217	10.054400
3.686325	278.357946	10.059405
3.780644	281.082469	10.064410
3.617904	294.147654	10.069415
3.864692	291.861253	10.074419
3.595480	285.938499	10.079424
3.729736	287.431292	10.084429
3.960502	283.486825	10.089434
3.787884	295.463851	10.094439
3.884382	286.240363	10.099443
3.954768	298.057197	10.104448
3.803926	295.564549	10.109453
4.285082	301.266330	10.114458
4.023182	308.963323	10.119463
4.102932	300.415896	10.124467
3.867865	313.151993	10.129472
3.895675	314.142921	10.134477
4.271046	307.226309	10.139482
3.882611	307.807367	10.144487
4.079147	297.681616	10.149491
4.330324	315.918152	10.154496
4.397511	312.822987	10.159501
4.317046	307.436275	10.164506
4.009841	320.791048	10.169511
4.435360	320.638261	10.174515
4.569254	320.211852	10.179520
4.325239	316.863535	10.184525
4.218687	321.362741	10.189530
4.438700	320.127765	10.194535
4.504959	327.083253	10.199539
4.507751	326.460124	10.204544
4.597511	327.447480	10.209549
4.737647	318.798941	10.214554
4.490634	333.577657	10.219559
4.941805	326.669446	10.224563
4.640669	345.647018	10.229568
4.852896	352.505113	10.234573
5.070037	353.152010	10.239578
4.881428	359.714481	10.244583
5.507209	355.009928	10.249587
5.131296	366.254572	10.254592
5.248070	355.952259	10.259597
5.351216	352.714146	10.264602
4.788622	340.526822	10.269607
5.134938	350.465579	10.274611
5.069540	363.005911	10.279616
4.942145	363.269348	10.284621
5.509726	362.767451	10.289626
5.201647	363.857696	10.294631
5.633558	362.669345	10.299635
5.397110	366.378682	10.304640
5.246593	363.390777	10.309645
5.678546	362.139338	10.314650
4.910919	379.024499	10.319655
5.465563	378.362229	10.324659
5.544748	396.608954	10.329664
5.692987	391.739275	10.334669
5.968422	400.396190	10.339674
5.733713	403.939669	10.344679
6.294623	396.258512	10.349683
6.053639	406.838226	10.354688
6.221094	409.904368	10.359693
6.329813	405.633961	10.364698
5.975436	417.589614	10.369703
6.374219	406.083146	10.374707
6.208827	413.280643	10.379712
6.129269	421.339719	10.384717
6.112397	419.634709	10.389722
6.072724	426.542483	10.394727
6.398425	415.850385	10.399731
6.365776	426.936235	10.404736
6.396832	418.068478	10.409741
6.345315	420.691704	10.414746
6.487304	428.997736	10.419751
6.527303	420.166401	10.424755
6.566122	430.412900	10.429760
6.372981	425.313794	10.434765
6.380205	426.621848	10.439770
6.167513	430.149204	10.444775
6.729002	436.415429	10.449779
6.601530	450.378781	10.454784
6.729413	461.532096	10.459789
6.981582	459.747894	10.464794
7.158576	461.948296	10.469799
7.145785	450.356047	10.474803
7.151284	464.156266	10.479808
7.190748	458.606855	10.484813
6.960195	462.025097	10.489818
6.888960	462.412050	10.494823
6.849150	464.585531	10.499827
7.018339	465.027180	10.504832
6.984776	470.085685	10.509837
7.434333	464.401467	10.514842
7.378974	474.079506	10.519847
7.411336	466.939971	10.524851
7.175929	477.711248	10.529856
7.401895	489.694245	10.534861
7.701584	497.423190	10.539866
7.478831	502.608086	10.544871
8.012397	496.847372	10.549875
7.968503	507.679592	10.554880
7.583324	492.196163	10.559885
8.150657	504.435401	10.564890
7.668138	498.112892	10.569895
7.754074	495.017852	10.574899
8.063539	510.166907	10.579904
7.787856	509.094570	10.584909
8.053237	516.934661	10.589914
8.120746	518.294612	10.594919
8.276994	516.114090	10.599923
8.294391	514.357867	10.604928
8.391697	517.501458	10.609933
8.447556	499.462214	10.614938
7.995627	504.835065	10.619943
8.594564	507.479139	10.624947
8.488010	519.387459	10.629952
8.499388	505.755317	10.634957
8.246203	502.704907	10.639962
7.909611	516.111857	10.644967
8.245907	504.194203	10.649971
8.115647	517.438922	10.654976
8.378431	513.161256	10.659981
8.713653	518.927407	10.664986
8.447122	523.747105	10.669991
8.799593	513.258840	10.674995
8.734263	521.987531	10.680000
8.665727	534.340841	10.685005
8.944778	539.997679	10.690010
8.805024	552.807098	10.695015
9.038227	543.948023	10.700019
9.022712	552.537890	10.705024
9.031398	552.864785	10.710029
9.478249	548.819541	10.715034
9.067056	554.219030	10.720039
9.312212	561.832120	10.725043
9.089272	558.649130	10.730048
8.717785	561.936900	10.735053
9.407820	559.944059	10.740058
9.291052	565.096300	10.745063
9.349852	553.714915	10.750067
8.912710	557.675526	10.755072
9.223758	556.845511	10.760077
9.136791	566.246357	10.765082
9.361344	577.904776	10.770087
9.696358	588.930526	10.775091
9.662623	600.425143	10.780096
9.624502	598.803932	10.785101
10.014629	596.723296	10.790106
9.916192	598.802062	10.795111
9.853377	593.839815	10.800115
9.657080	599.690782	10.805120
9.858394	604.568354	10.810125
10.032744	592.255382	10.815130
9.863116	593.514384	10.820135
9.729993	599.979795	10.825139
9.909601	608.104874	10.830144
9.913068	600.285432	10.835149
10.227043	603.667314	10.840154
9.918063	609.812247	10.845159
10.081810	604.917945	10.850163
10.224531	626.941382	10.855168
10.212550	627.706849	10.860173
10.282080	637.120628	10.865178
10.208639	637.142055	10.870183
10.461607	625.512006	10.875187
10.363979	642.419916	10.880192
10.401802	640.591029	10.885197
10.761027	629.759377	10.890202
10.418368	648.643032	10.895207
10.582378	642.116398	10.900211
10.153436	649.703008	10.905216
10.701595	657.663663	10.910221
11.016977	673.739269	10.915226
11.058964	673.012095	10.920231
11.182534	680.827583	10.925235
10.858874	682.040194	10.930240
10.973871	686.788048	10.935245
11.253662	675.275116	10.940250
11.026677	681.922706	10.945255
11.485175	675.060476	10.950259
11.242589	678.174733	10.955264
11.173464	677.831166	10.960269
11.411248	680.562845	10.965274
11.262440	692.266717	10.970279
11.661636	676.452953	10.975283
11.114410	682.932410	10.980288
11.156663	687.978898	10.985293
11.375938	676.762647	10.990298
11.326000	681.929502	10.995303
11.440067	683.147991	11.000307
11.660150	680.588224	11.005312
11.251450	682.200785	11.010317
11.876827	678.152263	11.015322
11.816719	678.967990	11.020327
12.020590	679.976595	11.025331
11.764440	687.584553	11.030336
11.826328	690.052530	11.035341
12.008683	695.254883	11.040346
12.038144	704.862771	11.045351
11.771805	710.616135	11.050355
12.193095	715.673140	11.055360
12.049522	716.972155	11.060365
12.223006	719.561121	11.065370
12.082209	724.064337	11.070375
12.156412	722.694877	11.075379
12.363053	718.273130	11.080384
12.353158	722.052084	11.085389
12.509633	718.299138	11.090394
12.731203	727.076814	11.095399
12.626376	725.247014	11.100403
12.440238	720.640315	11.105408
12.157263	726.897853	11.110413
12.408189	725.776195	11.115418
12.407473	730.468398	11.120423
12.590563	719.737321	11.125427
12.384081	723.722689	11.130432
12.305083	728.457343	11.135437
13.060717	746.902562	11.140442
12.820011	757.042477	11.145447
13.209168	756.446018	11.150451
12.903838	765.694939	11.155456
13.047529	761.552903	11.160461
13.024215	757.256930	11.165466
12.909122	769.747186	11.170471
13.349595	755.623705	11.175475
13.099985	763.198328	11.180480
12.875111	765.407681	11.185485
13.508655	757.642994	11.190490
13.083334	768.373809	11.195495
13.271742	770.582689	11.200499
13.172451	766.540917	11.205504
13.195753	763.250000	11.210509
13.179896	771.120896	11.215514
13.116624	770.554022	11.220519
13.286984	779.112796	11.225523
13.450547	789.325455	11.230528
13.161772	793.251423	11.235533
13.401436	794.375763	11.240538
13.521327	797.888007	11.245543
13.688950	787.127806	11.250547
13.493139	798.407925	11.255552
13.463002	801.979586	11.260557
14.219013	821.099049	11.265562
13.946469	830.072308	11.270567
14.447679	825.205324	11.275571
14.438070	810.024380	11.280576
13.867082	804.321453	11.285581
14.134942	804.719775	11.290586
14.065460	809.855097	11.295591
14.311512	830.945279	11.300595
13.991670	835.007901	11.305600
14.300860	839.478802	11.310605
14.452450	823.370818	11.315610
14.153850	839.710139	11.320615
14.405589	829.952931	11.325619
14.617782	829.473803	11.330624
14.311699	826.274051	11.335629
14.547041	825.303119	11.340634
14.404168	830.480120	11.345639
14.670130	823.874058	11.350643
14.575970	835.522803	11.355648
14.718465	834.430261	11.360653
14.983969	829.754641	11.365658
14.972744	834.313711	11.370663
14.599586	820.347549	11.375667
14.723768	829.709366	11.380672
14.426631	836.421048	11.385677
14.854945	853.078926	11.390682
14.980579	863.948243	11.395687
15.382434	850.296864	11.400691
14.843313	860.529398	11.405696
15.195016	852.465021	11.410701
15.251166	850.042559	11.415706
14.946988	863.715130	11.420711
15.189151	853.647955	11.425715
15.433174	867.934108	11.430720
15.731814	862.459120	11.435725
15.807326	860.343470	11.440730
15.513845	866.452129	11.445735
15.324170	854.846767	11.450739
15.070780	863.203499	11.455744
15.144529	864.993826	11.460749
15.823872	876.779445	11.465754
15.864187	888.469078	11.470759
15.843881	894.435606	11.475763
16.065837	895.226068	11.480768
15.941955	885.210162	11.485773
15.864503	870.308085	11.490778
15.659385	874.689129	11.495783
15.725135	876.249688	11.500787
16.032591	885.825180	11.505792
15.894240	902.672861	11.510797
15.969163	895.275567	11.515802
15.882292	902.054675	11.520807
16.001649	900.203287	11.525811
16.227773	897.148097	11.530816
16.181148	903.468156	11.535821
16.304014	898.771106	11.540826
16.163379	903.022802	11.545831
16.536622	901.850867	11.550835
16.257046	901.710402	11.555840
16.371452	925.887618	11.560845
16.825269	929.852094	11.565850
16.860855	935.121314	11.570855
17.129058	910.305543	11.575859
16.920836	904.566001	11.580864
16.824194	895.272002	11.585869
16.841696	892.122343	11.590874
16.607099	894.233120	11.595879
16.976261	894.304597	11.600883
16.871714	896.987622	11.605888
16.828275	892.304485	11.610893
17.141049	896.296180	11.615898
17.133783	903.503393	11.620903
16.825323	890.309088	11.625907
17.113223	912.226214	11.630912
17.226267	910.061199	11.635917
17.263818	922.234684	11.640922
17.204771	923.908203	11.645927
17.425734	920.030580	11.650931
17.073381	928.876267	11.655936
17.551918	928.737102	11.660941
17.980103	928.313414	11.665946
17.678930	925.071851	11.670951
17.712291	902.835853	11.675955
17.500579	903.617422	11.680960
17.875676	909.522463	11.685965
17.806407	893.335291	11.690970
17.336012	905.643405	11.695975
17.634273	909.395334	11.700979
17.586516	917.429896	11.705984
17.838448	927.150693	11.710989
18.095030	937.237433	11.715994
17.451784	937.243293	11.720999
18.075855	933.981891	11.726003
17.939294	936.998857	11.731008
17.980161	939.208430	11.736013
17.912460	930.526442	11.741018
17.710777	937.110181	11.746023
18.227311	934.983315	11.751027
18.092803	932.418558	11.756032
17.758634	935.942543	11.761037
18.286877	940.778333	11.766042
18.355534	957.697936	11.771047
18.499954	959.868915	11.776051
18.561702	966.259245	11.781056
18.471634	969.234105	11.786061
18.598884	961.603692	11.791066
18.441726	968.654266	11.796071
18.966074	967.043442	11.801075
19.101327	969.519479	11.806080
18.551195	958.124511	11.811085
18.644238	955.387821	11.816090
18.429534	971.817209	11.821095
18.855683	962.131451	11.826099
18.800960	974.544437	11.831104
18.989480	967.949875	11.836109
18.887084	967.371097	11.841114
18.735357	972.368981	11.846119
18.849364	965.040330	11.851123
18.791609	968.461879	11.856128
18.553698	974.352752	11.861133
19.122562	974.462557	11.866138
19.176472	987.787147	11.871143
19.561552	990.925156	11.876147
19.248859	992.781870	11.881152
19.298860	986.092688	11.886157
19.622061	981.706681	11.891162
19.766603	989.870687	11.896167
19.706208	976.293713	11.901171
19.533822	975.538422	11.906176
19.283258	979.601072	11.911181
19.359765	978.450441	11.916186
19.301497	992.529442	11.921191
19.589828	989.100785	11.926195
19.801268	989.775434	11.931200
19.834935	986.836876	11.936205
20.062955	980.918899	11.941210
19.913098	994.197930	11.946215
20.149786	986.262224	11.951219
20.335201	989.316162	11.956224
20.291638	984.819904	11.961229
20.246102	991.958351	11.966234
20.294866	988.379441	11.971239
20.056309	987.833420	11.976243
20.068426	990.374050	11.981248
20.160423	990.458195	11.986253
20.151543	988.993931	11.991258
20.089538	992.677966	11.996263
19.849456	982.092263	12.001267
20.173603	986.153929	12.006272
20.199989	993.012794	12.011277
20.561711	994.491459	12.016282
20.277142	1003.139490	12.021287
20.710331	996.381297	12.026291
20.989729	995.375727	12.031296
20.189973	996.584658	12.036301
20.552071	983.906271	12.041306
20.318693	992.805566	12.046311
20.507895	995.061669	12.051315
20.601965	999.416319	12.056320
20.689020	994.638210	12.061325
20.460395	993.865077	12.066330
20.450058	1000.784214	12.071335
20.541498	989.361010	12.076339
20.487318	1002.184772	12.081344
20.519111	987.265149	12.086349
20.762072	990.824049	12.091354
20.705677	990.948423	12.096359
20.389948	991.225350	12.101363
20.689747	990.186562	12.106368
20.666842	991.444273	12.111373
20.519142	986.631064	12.116378
20.297958	994.347944	12.121383
20.453592	982.001354	12.126387
20.462541	985.637007	12.131392
20.378880	992.488981	12.136397
20.720200	986.591569	12.141402
20.360162	998.421640	12.146407
20.490928	987.936069	12.151411
20.504350	990.969340	12.156416
20.709211	996.674466	12.161421
20.672710	998.769431	12.166426
20.555220	1000.061155	12.171431
20.871827	994.551710	12.176435
20.770324	990.148279	12.181440
20.436584	983.130760	12.186445
20.474377	976.411199	12.191450
20.298426	978.585180	12.196455
20.361827	982.472371	12.201459
20.581591	976.712635	12.206464
20.411937	982.930915	12.211469
20.894270	974.587776	12.216474
20.421910	978.741792	12.221479
20.583009	979.112990	12.226483
20.504798	974.002455	12.231488
20.336587	980.505172	12.236493
20.426848	978.279908	12.241498
20.303876	974.291534	12.246503
20.493590	975.770822	12.251507
20.428709	980.106661	12.256512
20.275104	983.007283	12.261517
20.673489	979.576845	12.266522
20.274002	984.481774	12.271527
20.422006	976.285012	12.276531
20.446549	984.702358	12.281536
20.373524	985.319869	12.286541
20.429933	978.803151	12.291546
20.585925	998.029597	12.296551
20.611160	994.280166	12.301555
20.656802	991.726880	12.306560
20.474155	989.223413	12.311565
20.695477	989.749814	12.316570
20.439110	992.721240	12.321575
20.448049	981.549346	12.326579
20.626927	980.921759	12.331584
20.338798	980.140770	12.336589
20.729209	977.676010	12.341594
20.636517	982.154283	12.346599
20.721806	977.580698	12.351603
20.604639	979.618345	12.356608
20.565611	979.366962	12.361613
20.733405	978.241197	12.366618
20.341353	979.291257	12.371623
20.554544	978.549376	12.376627
20.842819	986.323775	12.381632
20.474374	993.601259	12.386637
20.390209	987.630563	12.391642
20.543325	988.981636	12.396647
20.891700	979.805064	12.401651
20.719132	994.143597	12.406656
20.373871	976.174842	12.411661
20.859135	953.507890	12.416666
20.501349	961.927066	12.421671
20.607816	948.732763	12.426675
20.550346	946.779463	12.431680
20.446304	947.457906	12.436685
20.631947	945.226896	12.441690
20.091676	952.231328	12.446695
20.152712	947.350140	12.451699
20.330868	957.696223	12.456704
20.009432	953.036118	12.461709
20.610777	961.990715	12.466714
20.495559	985.778837	12.471719
20.644488	976.180659	12.476723
20.580860	979.853121	12.481728
20.260719	973.230871	12.486733
20.543608	975.578482	12.491738
20.164575	985.311643	12.496743
20.421604	982.376098	12.501747
20.261602	988.793923	12.506752
20.481798	997.199782	12.511757
20.570936	990.499624	12.516762
20.541731	1001.303846	12.521767
20.559453	995.351591	12.526771
20.619305	993.499432	12.531776
20.454116	997.893858	12.536781
20.685796	993.841812	12.541786
20.392359	983.811878	12.546791
20.113899	983.204406	12.551795
20.573379	997.133011	12.556800
20.439181	1002.742397	12.561805
20.630744	991.540576	12.566810
20.385414	997.550925	12.571815
20.497250	991.045075	12.576819
20.901969	990.369636	12.581824
20.635488	980.256549	12.586829
20.416170	969.087953	12.591834
20.261007	965.703231	12.596839
20.110577	957.617166	12.601843
20.622634	969.697656	12.606848
20.383224	991.441942	12.611853
20.864331	987.425025	12.616858
20.368372	977.929710	12.621863
20.570028	971.197419	12.626867
20.621296	972.470898	12.631872
20.350807	969.666811	12.636877
20.478122	968.113798	12.641882
20.073637	968.242439	12.646887
20.520582	973.989375	12.651891
20.534857	994.257237	12.656896
20.415558	980.997981	12.661901
20.501109	972.321488	12.666906
20.370303	986.377357	12.671911
20.564614	978.423181	12.676915
20.402934	976.265703	12.681920
20.582255	978.672417	12.686925
20.677540	963.893305	12.691930
20.410630	970.488252	12.696935
20.502365	966.028771	12.701939
20.401133	964.919897	12.706944
20.427990	963.654171	12.711949
20.852650	961.172911	12.716954
20.627335	956.619699	12.721959
20.850097	958.670150	12.726963
20.486551	968.405561	12.731968
20.520900	966.904439	12.736973
20.426536	970.210390	12.741978
20.335358	964.984431	12.746983
20.333888	955.997732	12.751987
20.457679	969.667587	12.756992
20.188325	967.614027	12.761997
20.800531	967.525299	12.767002
20.287373	969.267315	12.772007
20.347902	968.860477	12.777011
20.434697	963.239451	12.782016
20.544980	966.496200	12.787021
20.582478	967.634665	12.792026
20.378458	969.107363	12.797031
20.245645	970.149191	12.802035
20.533707	974.539918	12.807040
20.276132	971.930910	12.812045
20.601762	961.396139	12.817050
20.308931	972.680828	12.822055
20.401188	961.255149	12.827059
20.311696	969.530599	12.832064
20.208750	975.960609	12.837069
20.581345	986.901812	12.842074
20.373452	1004.122651	12.847079
20.615201	995.930639	12.852083
20.708547	984.089987	12.857088
20.239155	984.985209	12.862093
20.827825	973.619913	12.867098
20.573583	975.842656	12.872103
20.283193	979.724771	12.877107
20.306148	980.664474	12.882112
20.284161	980.532599	12.887117
20.756993	977.935620	12.892122
20.537184	984.803787	12.897127
20.566937	975.444627	12.902131
20.566812	975.535581	12.907136
20.507911	979.457262	12.912141
20.408815	980.052908	12.917146
20.228284	975.579288	12.922151
20.588061	966.417466	12.927155
20.490508	988.142274	12.932160
20.524926	984.066496	12.937165
20.643634	973.323423	12.942170
20.666486	978.125498	12.947175
20.501925	977.864173	12.952179
20.644294	980.675791	12.957184
20.217438	989.995494	12.962189
20.494254	983.017007	12.967194
20.353290	986.526746	12.972199
20.477924	979.156966	12.977203
20.496850	977.556578	12.982208
20.527943	985.928721	12.987213
20.723118	976.665401	12.992218
20.793683	985.754355	12.997223
20.550303	985.105803	13.002227
20.835385	977.956460	13.007232
20.616449	984.735381	13.012237
20.770291	972.635115	13.017242
20.645862	985.675093	13.022247
20.662132	973.277405	13.027251
20.463004	968.572552	13.032256
20.138370	952.701252	13.037261
20.530044	961.907723	13.042266
20.233875	977.015873	13.047271
20.302427	979.273081	13.052275
20.738299	982.035518	13.057280
20.507986	976.410658	13.062285
20.530373	973.272820	13.067290
20.630614	981.863401	13.072295
20.838557	977.957086	13.077299
20.852263	964.502357	13.082304
20.647487	959.709301	13.087309
20.523732	949.496980	13.092314
20.289530	962.116009	13.097319
20.443592	954.621686	13.102323
20.536127	947.715192	13.107328
20.202284	961.853891	13.112333
20.399738	955.310743	13.117338
20.291633	964.616648	13.122343
20.533885	955.662044	13.127347
20.416863	956.244777	13.132352
20.082729	957.236706	13.137357
20.208504	965.428927	13.142362
20.338106	981.409128	13.147367
20.661604	980.279818	13.152371
20.896133	991.672812	13.157376
20.649403	970.162702	13.162381
20.760104	962.903973	13.167386
20.537672	967.570899	13.172391
20.156288	956.165574	13.177395
20.091713	958.802018	13.182400
20.409944	966.887051	13.187405
20.844510	954.336705	13.192410
20.287751	964.091892	13.197415
20.485371	959.768504	13.202419
20.421228	964.220927	13.207424
20.251992	954.985782	13.212429
20.413921	968.920816	13.217434
20.257857	986.663278	13.222439
20.577812	977.316181	13.227443
20.501984	992.062737	13.232448
20.513567	989.236522	13.237453
20.850192	989.214620	13.242458
20.611596	972.672706	13.247463
20.446922	962.701104	13.252467
20.408950	965.789881	13.257472
20.398077	966.108865	13.262477
20.551591	961.916315	13.267482
20.245501	966.118719	13.272487
20.234841	958.704290	13.277491
20.367493	972.533600	13.282496
20.541980	989.672926	13.287501
20.875236	987.346606	13.292506
20.633071	977.445707	13.297511
20.642523	971.672995	13.302515
20.539273	972.386799	13.307520
20.708761	976.104086	13.312525
20.380350	965.955151	13.317530
20.136135	972.748349	13.322535
20.602040	963.353536	13.327539
20.656570	970.800108	13.332544
20.303856	970.300686	13.337549
20.648028	972.431919	13.342554
20.275510	966.118467	13.347559
20.540934	966.519549	13.352563
20.460734	971.833274	13.357568
20.290910	969.666057	13.362573
20.770578	969.061462	13.367578
20.573457	976.138128	13.372583
20.613088	975.281203	13.377587
20.876466	975.077787	13.382592
20.539436	980.456927	13.387597
20.785154	967.486426	13.392602
20.628481	963.918999	13.397607
20.651093	964.143535	13.402611
20.633846	965.474466	13.407616
20.305056	968.251626	13.412621
20.752398	968.457305	13.417626
20.310154	971.448124	13.422631
20.588906	965.241335	13.427635
20.640680	953.396299	13.432640
20.538784	959.468917	13.437645
20.677158	947.336444	13.442650
20.464837	944.095686	13.447655
20.387924	933.312087	13.452659
20.321763	939.587965	13.457664
20.301764	945.089217	13.462669
20.655057	946.986368	13.467674
20.407325	954.166511	13.472679
20.506905	947.702062	13.477683
20.616788	935.507904	13.482688
20.434317	938.914643	13.487693
20.409404	927.158350	13.492698
20.336528	938.668152	13.497703
20.307417	940.683074	13.502707
20.700095	960.718626	13.507712
20.784348	955.243892	13.512717
20.447458	949.295386	13.517722
20.289396	946.598752	13.522727
20.301633	939.076591	13.527731
20.302807	944.610739	13.532736
20.654912	963.129277	13.537741
20.394607	953.540402	13.542746
20.315284	951.350866	13.547751
20.594062	948.810079	13.552755
20.571641	953.040568	13.557760
20.267901	940.095437	13.562765
20.385837	946.578520	13.567770
20.416583	965.357286	13.572775
20.681214	957.078848	13.577779
20.747734	956.240502	13.582784
20.407049	951.101660	13.587789
20.608259	943.809578	13.592794
20.379441	947.036036	13.597799
21.013090	951.511206	13.602803
20.614855	949.579141	13.607808
20.482570	949.819710	13.612813
20.376737	948.272345	13.617818
19.909246	948.759578	13.622823
19.853889	948.546285	13.627827
20.324160	954.767358	13.632832
20.758207	971.410265	13.637837
20.882760	957.985963	13.642842
20.392155	956.438464	13.647847
20.522891	947.231966	13.652851
20.619853	944.734375	13.657856
20.189466	950.758451	13.662861
20.260279	940.944864	13.667866
20.459763	954.794251	13.672871
20.540295	957.428052	13.677875
20.798636	953.739231	13.682880
20.293673	951.714580	13.687885
20.471056	954.585270	13.692890
20.481550	954.643776	13.697895
20.864126	940.581397	13.702899
20.660369	947.831802	13.707904
20.527268	953.014384	13.712909
20.913784	949.038587	13.717914
20.469060	954.552390	13.722919
20.630539	949.407574	13.727923
20.943113	943.831764	13.732928
21.036621	945.332704	13.737933
20.624477	941.007225	13.742938
20.430193	926.493558	13.747943
20.522431	922.506355	13.752947
20.377772	915.558066	13.757952
20.150230	925.498859	13.762957
20.677481	928.141832	13.767962
20.551149	945.301491	13.772967
20.469543	931.747655	13.777971
20.370959	930.332402	13.782976
20.200188	945.656295	13.787981
20.257208	944.389703	13.792986
20.352930	952.415593	13.797991
20.446274	945.517645	13.802995
20.384871	949.524881	13.808000
19.917761	959.316233	13.813005
20.874545	948.484446	13.818010
20.585492	951.574630	13.823015
20.413418	956.521343	13.828019
20.507817	948.024821	13.833024
20.387820	948.175901	13.838029
20.577995	939.075844	13.843034
20.134709	957.234706	13.848039
20.574558	945.322255	13.853043
20.503167	954.582082	13.858048
20.309842	962.083956	13.863053
20.550251	959.625777	13.868058
20.661957	957.020954	13.873063
20.714973	953.174842	13.878067
20.771842	952.136955	13.883072
20.519071	955.837214	13.888077
20.410057	951.696794	13.893082
20.233005	962.951179	13.898087
20.473728	960.017450	13.903091
20.358476	955.448260	13.908096
20.162509	955.837773	13.913101
20.315664	950.951353	13.918106
20.646126	954.091758	13.923111
20.179785	962.716714	13.928115
20.184062	963.548998	13.933120
20.321260	951.963178	13.938125
20.360989	953.426960	13.943130
20.301002	957.758069	13.948135
20.467683	953.377322	13.953139
20.620602	950.085402	13.958144
20.328242	958.187391	13.963149
20.296543	946.831963	13.968154
20.374320	958.579550	13.973159
20.557301	951.734329	13.978163
20.542210	954.739021	13.983168
20.321649	955.336693	13.988173
20.660496	951.948088	13.993178
20.623534	963.387519	13.998183
20.416498	954.609458	14.003187
20.981497	946.995181	14.008192
20.749576	956.573855	14.013210
20.872774	949.695783	14.018227
20.595557	960.615023	14.023245
20.651261	957.441330	14.028263
20.437964	963.910330	14.033280
20.514907	953.195787	14.038298
20.676117	952.788062	14.043315
20.529080	961.118469	14.048333
20.404476	956.405953	14.053351
20.710087	958.964853	14.058368
20.779166	957.701905	14.063386
20.951566	953.890588	14.068403
21.061721	963.078993	14.073421
20.844705	951.775810	14.078439
20.769305	940.269929	14.083456
20.392410	939.593305	14.088474
21.038518	936.293981	14.093491
20.560498	943.462749	14.098509
20.655947	947.828041	14.103527
21.106949	959.250921	14.108544
20.566240	957.912985	14.113562
20.619318	953.791138	14.118579
20.608497	963.940335	14.123597
20.571254	963.612244	14.128615
20.900733	962.041121	14.133632
20.567860	963.656546	14.138650
20.870829	957.899725	14.143667
20.565731	972.871770	14.148685
20.825064	970.397868	14.153703
21.044795	971.256586	14.158720
20.818090	972.170783	14.163738
20.802824	968.111746	14.168755
20.761341	976.671514	14.173773
21.109786	994.412590	14.178791
21.056857	1003.067012	14.183808
20.959390	1001.587582	14.188826
21.249548	993.066503	14.193843
21.081871	995.709555	14.198861
21.318304	1000.831843	14.203879
21.504784	1001.559794	14.208896
21.088680	993.761729	14.213914
20.655353	980.027989	14.218931
21.112804	1000.158517	14.223949
21.012566	993.021109	14.228967
21.009542	998.749479	14.233984
20.770642	1003.356103	14.239002
21.214586	1000.833086	14.244019
21.110799	1006.465055	14.249037
21.281869	1003.438912	14.254055
21.655431	1001.605912	14.259072
21.052820	1000.424143	14.264090
21.444813	995.304369	14.269107
21.412379	1006.169654	14.274125
21.280393	1001.551112	14.279143
21.384674	1002.392066	14.284160
21.195160	1009.785419	14.289178
21.444632	1018.560723	14.294195
21.352364	1033.843391	14.299213
21.576893	1037.289881	14.304231
21.852516	1034.777189	14.309248
21.610627	1021.734140	14.314266
21.648067	1001.881450	14.319283
21.471150	1006.204471	14.324301
21.304976	1005.338495	14.329319
21.731154	1024.807840	14.334336
21.775610	1028.821837	14.339354
21.949564	1023.889422	14.344371
21.499896	1017.663503	14.349389
21.331685	1017.419225	14.354407
22.021852	1028.682097	14.359424
21.450674	1030.385880	14.364442
21.538542	1031.454406	14.369459
21.632660	1037.839009	14.374477
21.587002	1030.547365	14.379495
21.665308	1033.784360	14.384512
21.694345	1036.519530	14.389530
21.708601	1030.850419	14.394547
21.779488	1031.776142	14.399565
21.673248	1032.500446	14.404583
21.759828	1033.057922	14.409600
21.752476	1036.719159	14.414618
21.739605	1037.655096	14.419635
22.149157	1034.270782	14.424653
21.955436	1038.181194	14.429671
22.046577	1031.827319	14.434688
22.048952	1047.855498	14.439706
21.946252	1030.895244	14.444723
21.669792	1046.823960	14.449741
21.593157	1067.989138	14.454759
22.156809	1068.894469	14.459776
22.418015	1072.212416	14.464794
22.764532	1069.472895	14.469811
22.239011	1056.202123	14.474829
22.230052	1036.426790	14.479847
22.431139	1029.809975	14.484864
22.323406	1036.491055	14.489882
22.401420	1022.922689	14.494899
22.351776	1030.295315	14.499917
22.333872	1029.002188	14.504935
22.627283	1025.412235	14.509952
22.440777	1031.942275	14.514970
22.279236	1030.215074	14.519987
22.070507	1043.311632	14.525005
22.134684	1039.620593	14.530023
22.436266	1038.436175	14.535040
22.265551	1043.215202	14.540058
22.481600	1039.800400	14.545075
22.732934	1037.132699	14.550093
22.430518	1043.106265	14.555111
22.423110	1038.229517	14.560128
22.064888	1043.750280	14.565146
22.575155	1047.928307	14.570163
22.672166	1067.178067	14.575181
22.886592	1056.366796	14.580199
22.955612	1035.483361	14.585216
22.432932	1041.315873	14.590234
22.390674	1033.800304	14.595251
22.505009	1037.889679	14.600269
22.358569	1047.778195	14.605287
22.753000	1058.680829	14.610304
22.617329	1068.267965	14.615322
22.718570	1072.484499	14.620339
22.581621	1074.152846	14.625357
22.835593	1073.647734	14.630375
23.024659	1060.605126	14.635392
22.640953	1066.544475	14.640410
22.956510	1061.432937	14.645427
23.334748	1052.522589	14.650445
22.934121	1050.833522	14.655463
22.842382	1036.976025	14.660480
22.881106	1032.426990	14.665498
22.960177	1033.274327	14.670515
22.877291	1045.428977	14.675533
22.844278	1047.315135	14.680551
23.014883	1052.386590	14.685568
22.973995	1061.275878	14.690586
23.128844	1061.885389	14.695603
23.191660	1060.256898	14.700621
23.021317	1060.776700	14.705639
23.302055	1061.606815	14.710656
23.067213	1042.811365	14.715674
23.065771	1037.518366	14.720691
23.224648	1045.577433	14.725709
23.130176	1046.949550	14.730727
23.400819	1044.594961	14.735744
23.084587	1049.324052	14.740762
23.138014	1053.298085	14.745779
23.457445	1053.407840	14.750797
23.085727	1052.268679	14.755815
23.033414	1050.132351	14.760832
23.090583	1058.291808	14.765850
23.199085	1060.131798	14.770867
22.948074	1063.370202	14.775885
22.868376	1068.229892	14.780903
23.304992	1063.268152	14.785920
23.352507	1066.342530	14.790938
23.130997	1066.771389	14.795955
23.291035	1058.286758	14.800973
23.247453	1066.329363	14.805991
23.499485	1073.694006	14.811008
23.319531	1086.310935	14.816026
23.545134	1077.046587	14.821043
23.692934	1078.480743	14.826061
23.611112	1091.487098	14.831079
23.834043	1083.808075	14.836096
23.622340	1082.928120	14.841114
23.350581	1085.569699	14.846131
23.821663	1085.061419	14.851149
23.655476	1091.602402	14.856167
23.846335	1098.021154	14.861184
23.638556	1097.356088	14.866202
23.383546	1090.635808	14.871219
23.513992	1092.491966	14.876237
23.680496	1095.154094	14.881255
23.894766	1090.742216	14.886272
23.960484	1088.414015	14.891290
23.669041	1081.454146	14.896307
23.761207	1084.637816	14.901325
23.460374	1090.673286	14.906343
24.054620	1082.196465	14.911360
23.568654	1089.067680	14.916378
23.592870	1096.644074	14.921395
23.898922	1096.081888	14.926413
23.518854	1103.896600	14.931431
23.824300	1106.717476	14.936448
23.843929	1118.780327	14.941466
23.845310	1121.530149	14.946483
24.402449	1116.300616	14.951501
24.260136	1122.396549	14.956519
24.460649	1114.190163	14.961536
24.298357	1125.916289	14.966554
24.699100	1112.480416	14.971571
24.465459	1093.093220	14.976589
24.006053	1099.145336	14.981607
24.172147	1087.645652	14.986624
24.201504	1089.897838	14.991642
23.966439	1084.988169	14.996659
24.303326	1096.846233	15.001677
24.367693	1106.419578	15.006695
24.513358	1106.162988	15.011712
24.567864	1091.254088	15.016730
24.249004	1095.031884	15.021747
24.424044	1079.834769	15.026765
24.166400	1094.353394	15.031783
24.528363	1100.248540	15.036800
24.574965	1112.100220	15.041818
24.568083	1110.121813	15.046835
24.404823	1099.907183	15.051853
24.463844	1099.101241	15.056871
24.732359	1108.599550	15.061888
24.656068	1119.384608	15.066906
24.613015	1116.768568	15.071923
24.863039	1095.146706	15.076941
24.404128	1097.983315	15.081959
24.631530	1100.779670	15.086976
24.910877	1109.882189	15.091994
24.863010	1109.632872	15.097011
24.712552	1092.341159	15.102029
24.771599	1086.568922	15.107047
24.710726	1082.616233	15.112064
24.854630	1086.260436	15.117082
24.610870	1092.060276	15.122099
25.033486	1094.764928	15.127117
24.232184	1114.941443	15.132135
24.783633	1103.550962	15.137152
24.714361	1108.628451	15.142170
24.847862	1118.178191	15.147187
24.963358	1116.814226	15.152205
24.898319	1110.551299	15.157223
25.004700	1114.372962	15.162240
24.815106	1120.648691	15.167258
25.149659	1117.564986	15.172275
25.318661	1118.910816	15.177293
24.756996	1122.196424	15.182311
24.864917	1122.453968	15.187328
24.984660	1120.815604	15.192346
24.968552	1125.424485	15.197363
24.829804	1127.349541	15.202381
25.138325	1123.051615	15.207399
25.019460	1120.723747	15.212416
25.216598	1117.631285	15.217434
25.248903	1121.576457	15.222451
25.442523	1122.582502	15.227469
25.139389	1130.868687	15.232487
25.386043	1116.817919	15.237504
25.587838	1115.293890	15.242522
25.304569	1123.048338	15.247539
25.485094	1115.559330	15.252557
25.462495	1117.682947	15.257575
25.072926	1120.173428	15.262592
25.352803	1132.171182	15.267610
25.408252	1145.403454	15.272627
25.820731	1142.526764	15.277645
25.682679	1159.413573	15.282663
25.518578	1144.309814	15.287680
25.608257	1146.335298	15.292698
25.752491	1132.230848	15.297715
25.462082	1128.627021	15.302733
25.461151	1128.719447	15.307751
25.970277	1143.269981	15.312768
26.001960	1132.140932	15.317786
25.418918	1137.011714	15.322803
25.626826	1131.155151	15.327821
25.477004	1147.394130	15.332839
25.826438	1155.029585	15.337856
25.879766	1150.530882	15.342874
25.780810	1146.375027	15.347891
26.219817	1143.962891	15.352909
25.710305	1148.306755	15.357927
25.984036	1137.585071	15.362944
26.082109	1142.908027	15.367962
25.859566	1147.359496	15.372979
26.227878	1142.410984	15.377997
25.973794	1151.528612	15.383015
25.974236	1142.149119	15.388032
26.218281	1136.981317	15.393050
25.884179	1135.512875	15.398067
25.909104	1130.926683	15.403085
25.821409	1134.349062	15.408103
26.069202	1146.911187	15.413120
26.584331	1138.815847	15.418138
25.971408	1149.532358	15.423155
26.093072	1126.504111	15.428173
25.938124	1143.117516	15.433191
25.934777	1143.174932	15.438208
26.271080	1134.979910	15.443226
25.919845	1138.522982	15.448243
25.996498	1140.572566	15.453261
25.972775	1139.469918	15.458279
26.044457	1134.266686	15.463296
26.241575	1147.223092	15.468314
26.269724	1163.625621	15.473331
26.854871	1168.952698	15.478349
26.519260	1156.213930	15.483367
26.395216	1143.251080	15.488384
26.463787	1140.297103	15.493402
26.257783	1151.721894	15.498419
26.614617	1170.325486	15.503437
26.350392	1166.470493	15.508455
26.369326	1174.658925	15.513472
26.697646	1161.310855	15.518490
26.868764	1169.309833	15.523507
26.796082	1168.464329	15.528525
27.048317	1171.835643	15.533543
26.818145	1153.345275	15.538560
27.054497	1145.052139	15.543578
26.879830	1143.491408	15.548595
26.825598	1139.333140	15.553613
27.088388	1134.103358	15.558631
26.694530	1133.230431	15.563648
26.704269	1133.173283	15.568666
26.680975	1137.581169	15.573683
27.048413	1129.031167	15.578701
26.835667	1137.116525	15.583719
26.741082	1136.191929	15.588736
26.623150	1148.464733	15.593754
27.066456	1155.560582	15.598771
27.715163	1156.992718	15.603789
27.204042	1155.142713	15.608807
26.804701	1139.167222	15.613824
27.231222	1140.893573	15.618842
26.956222	1147.203386	15.623859
27.328957	1149.109786	15.628877
27.433529	1161.837134	15.633895
27.133058	1146.368139	15.638912
27.294339	1134.774012	15.643930
26.826545	1143.666159	15.648947
27.413118	1145.602161	15.653965
27.542864	1159.612297	15.658983
27.523601	1148.055610	15.664000
27.478374	1130.252323	15.669018
27.149464	1135.696082	15.674035
27.407779	1134.783627	15.679053
27.240655	1125.489864	15.684071
27.126003	1140.185511	15.689088
27.663983	1155.380364	15.694106
27.583649	1153.808518	15.699123
27.636509	1145.090021	15.704141
27.701620	1147.380561	15.709159
27.623948	1135.614537	15.714176
27.693884	1120.736181	15.719194
27.513393	1131.695179	15.724211
27.704481	1122.990829	15.729229
27.558919	1120.452490	15.734247
27.486413	1130.427588	15.739264
28.018015	1138.038697	15.744282
27.481912	1142.005321	15.749299
27.841589	1143.985379	15.754317
27.869474	1160.788304	15.759335
27.735240	1153.406901	15.764352
27.976635	1139.938214	15.769370
27.500740	1150.011490	15.774387
27.815294	1153.829849	15.779405
27.843931	1164.564381	15.784423
27.545884	1165.135232	15.789440
27.890145	1154.742864	15.794458
27.561374	1167.367082	15.799475
27.787441	1158.641400	15.804493
27.706951	1164.697600	15.809511
27.823394	1168.063043	15.814528
27.979644	1154.237456	15.819546
27.677565	1174.468139	15.824563
28.163475	1178.620202	15.829581
28.209960	1190.650513	15.834599
28.224456	1190.778233	15.839616
28.363813	1193.922937	15.844634
28.334074	1194.542233	15.849651
28.502859	1187.597785	15.854669
28.364200	1183.224083	15.859687
28.161689	1167.173905	15.864704
28.448908	1166.824732	15.869722
28.342996	1184.292428	15.874739
28.398129	1188.148242	15.879757
28.632754	1186.171417	15.884775
28.491217	1175.069178	15.889792
28.402968	1178.096018	15.894810
28.275511	1175.230721	15.899827
28.518707	1179.979167	15.904845
28.783322	1186.774753	15.909863
28.485888	1193.804719	15.914880
28.764633	1180.421278	15.919898
28.565573	1188.712132	15.924915
28.399234	1179.459110	15.929933
28.820705	1188.844981	15.934951
28.721470	1188.802855	15.939968
28.819983	1186.071409	15.944986
28.371253	1199.335382	15.950003
28.709545	1185.669503	15.955021
28.303859	1182.998815	15.960039
28.457715	1188.817861	15.965056
28.751177	1183.937120	15.970074
28.572049	1181.741558	15.975091
28.721281	1183.477534	15.980109
28.970198	1188.184169	15.985127
28.726525	1187.681348	15.990144
28.756252	1181.981395	15.995162
28.940307	1193.791553	16.000179
29.057521	1212.007104	16.005197
29.288787	1210.192844	16.010215
28.875070	1214.758988	16.015232
29.314649	1216.422700	16.020250
29.009675	1211.465933	16.025267
28.941065	1219.234959	16.030285
29.223959	1209.423383	16.035303
29.199175	1214.856417	16.040320
29.794823	1206.754490	16.045338
29.267100	1200.476442	16.050355
29.330823	1197.478394	16.055373
29.583564	1186.536640	16.060391
29.103622	1195.341088	16.065408
29.434488	1184.305072	16.070426
29.339435	1196.408303	16.075443
29.103724	1208.482854	16.080461
29.538944	1211.823417	16.085479
29.383176	1214.889350	16.090496
29.779480	1219.290112	16.095514
29.348527	1229.022772	16.100531
29.674869	1217.450232	16.105549
29.824967	1215.412163	16.110567
29.743754	1216.402274	16.115584
29.677040	1216.368332	16.120602
29.683117	1218.164901	16.125619
29.427962	1210.415768	16.130637
29.628548	1219.357091	16.135655
29.608317	1212.961909	16.140672
29.405359	1211.139826	16.145690
29.444060	1218.947582	16.150707
29.606308	1218.214050	16.155725
29.882028	1224.202446	16.160743
29.421609	1228.067352	16.165760
29.553863	1223.494687	16.170778
29.847277	1234.708527	16.175795
30.033190	1243.705691	16.180813
30.145504	1250.866181	16.185831
30.193515	1254.425041	16.190848
30.182227	1241.872008	16.195866
29.850880	1230.054343	16.200883
30.114914	1247.589743	16.205901
30.302554	1242.880814	16.210919
29.918109	1242.518429	16.215936
30.143064	1245.339587	16.220954
30.109211	1249.727167	16.225971
30.248934	1252.321233	16.230989
30.554221	1251.707252	16.236007
30.201217	1251.756728	16.241024
30.460840	1246.406282	16.246042
30.431780	1252.156208	16.251059
30.371358	1254.910408	16.256077
30.624849	1245.298565	16.261095
30.292842	1238.174407	16.266112
30.405101	1240.490477	16.271130
30.478850	1240.781790	16.276147
30.300000	1250.481331	16.281165
30.636366	1243.437764	16.286183
30.327240	1246.000383	16.291200
30.990618	1244.939151	16.296218
30.666682	1241.602567	16.301235
30.646372	1251.343679	16.306253
31.018285	1243.421360	16.311271
30.561925	1236.202200	16.316288
30.367385	1238.871603	16.321306
30.686125	1254.838537	16.326323
30.702158	1248.941742	16.331341
30.641485	1247.146513	16.336359
30.506724	1252.880264	16.341376
30.671384	1248.493556	16.346394
30.555118	1250.844504	16.351411
30.627739	1240.525293	16.356429
30.840241	1238.808409	16.361447
30.479399	1247.035434	16.366464
30.540781	1258.672504	16.371482
31.102812	1276.872246	16.376499
30.951723	1276.542643	16.381517
31.195471	1275.534970	16.386535
31.194824	1272.732802	16.391552
31.452286	1273.123809	16.396570
31.226195	1276.778308	16.401587
31.458689	1271.876587	16.406605
31.498816	1266.436081	16.411623
31.514454	1268.530024	16.416640
31.303974	1264.546875	16.421658
31.331414	1273.401010	16.426675
31.098790	1279.560966	16.431693
31.560453	1277.346557	16.436711
31.512643	1274.542473	16.441728
31.815662	1266.280323	16.446746
31.443496	1251.001987	16.451763
31.354333	1245.555367	16.456781
31.474169	1252.407899	16.461799
31.639538	1269.126095	16.466816
31.532108	1267.946334	16.471834
31.606606	1254.784178	16.476851
31.844019	1264.607682	16.481869
31.901646	1269.615433	16.486887
31.959613	1255.625304	16.491904
31.945235	1237.897980	16.496922
31.638115	1233.721029	16.501939
31.847487	1241.676191	16.506957
31.922046	1232.117280	16.511975
31.831065	1235.584255	16.516992
31.542310	1231.919572	16.522010
31.815097	1237.429426	16.527027
31.802050	1252.183704	16.532045
32.077860	1248.185920	16.537063
31.789749	1259.561752	16.542080
31.885219	1262.675716	16.547098
32.182349	1267.033320	16.552115
31.664467	1279.098663	16.557133
31.875892	1272.853707	16.562151
31.847720	1278.491024	16.567168
31.579331	1269.842570	16.572186
31.944648	1274.380434	16.577203
31.530575	1265.921971	16.582221
31.893661	1280.001190	16.587239
31.962330	1297.848616	16.592256
32.139387	1298.091203	16.597274
32.225532	1296.852247	16.602291
32.103778	1301.356903	16.607309
32.431821	1293.377056	16.612327
32.489321	1293.648152	16.617344
32.570660	1299.692754	16.622362
32.631493	1302.307278	16.627379
32.843503	1292.714605	16.632397
32.904442	1298.863927	16.637415
32.442905	1301.944041	16.642432
32.448390	1296.011940	16.647450
32.667274	1296.948684	16.652467
32.716027	1298.153252	16.657485
32.611335	1297.750963	16.662503
32.542446	1301.011496	16.667520
32.310454	1298.818055	16.672538
32.837508	1297.331009	16.677555
32.715052	1297.970604	16.682573
32.728300	1295.061603	16.687591
32.513764	1295.989608	16.692608
32.562570	1310.666434	16.697626
33.098188	1320.846706	16.702643
32.753118	1333.505915	16.707661
33.117972	1331.358853	16.712679
33.185696	1325.996511	16.717696
33.210450	1332.761208	16.722714
33.104098	1326.249143	16.727731
33.203008	1329.080196	16.732749
33.537249	1322.801472	16.737767
33.157185	1318.250714	16.742784
33.043993	1303.622406	16.747802
33.370910	1319.529115	16.752819
33.298334	1327.143092	16.757837
33.235265	1324.048043	16.762855
33.424618	1335.232939	16.767872
33.241742	1327.616156	16.772890
33.702453	1336.710342	16.777907
33.598258	1324.465445	16.782925
33.344165	1306.472660	16.787943
33.141766	1307.489971	16.792960
33.506095	1319.693076	16.797978
33.715272	1316.859792	16.802995
33.373466	1339.356839	16.808013
33.618893	1330.882028	16.813031
33.591491	1334.118646	16.818048
33.297642	1318.453342	16.823066
33.790884	1325.078812	16.828083
33.457397	1330.041207	16.833101
33.570698	1323.390282	16.838119
33.470387	1329.901987	16.843136
33.571561	1333.000112	16.848154
33.802808	1321.369508	16.853171
33.638224	1324.231576	16.858189
33.477134	1330.425765	16.863207
33.222525	1339.088957	16.868224
33.695753	1352.628400	16.873242
33.910451	1348.822033	16.878259
33.947213	1353.409181	16.883277
34.001490	1356.101058	16.888295
33.815894	1358.765910	16.893312
33.845869	1362.547126	16.898330
33.994101	1357.182944	16.903347
33.595234	1361.405393	16.908365
33.987607	1382.868267	16.913383
34.365654	1389.075594	16.918400
34.152330	1390.627161	16.923418
34.554064	1392.980459	16.928435
34.329737	1393.953293	16.933453
34.871060	1390.573052	16.938471
34.749606	1389.690481	16.943488
34.561553	1378.827543	16.948506
34.811291	1357.663907	16.953523
34.359164	1353.867151	16.958541
34.420133	1356.277156	16.963559
34.832876	1355.504449	16.968576
34.646024	1355.142006	16.973594
34.722359	1344.127591	16.978611
34.379641	1355.681319	16.983629
34.466068	1363.874037	16.988647
34.389556	1381.146143	16.993664
34.718055	1389.732877	16.998682
34.897478	1383.931884	17.003699
34.509976	1389.412611	17.008717
34.768328	1388.464740	17.013735
35.031444	1386.458962	17.018752
34.791567	1390.044896	17.023770
34.935247	1394.043168	17.028787
34.938875	1392.156648	17.033805
35.601353	1392.494071	17.038823
35.467615	1380.652629	17.043840
35.234433	1383.950397	17.048858
35.177845	1379.659505	17.053875
35.177533	1389.904857	17.058893
35.453641	1380.537087	17.063911
35.239310	1382.379057	17.068928
35.001668	1386.275329	17.073946
35.212952	1387.645117	17.078963
35.168059	1387.812202	17.083981
35.496305	1378.303974	17.088999
35.288965	1373.251348	17.094016
34.946862	1391.263515	17.099034
35.425957	1372.512649	17.104051
35.379944	1380.537724	17.109069
35.212784	1378.675301	17.114087
35.169704	1383.488353	17.119104
35.046687	1386.206940	17.124122
35.498691	1376.467387	17.129139
35.236040	1388.684819	17.134157
35.829984	1404.149453	17.139175
35.662108	1408.300464	17.144192
35.573668	1411.609760	17.149210
35.954914	1408.048967	17.154227
36.004221	1409.646741	17.159245
35.876767	1411.693524	17.164263
35.826632	1412.410470	17.169280
35.528624	1416.592464	17.174298
35.923188	1411.333701	17.179315
35.775511	1418.146391	17.184333
35.837625	1405.269240	17.189351
36.191502	1413.604957	17.194368
35.746943	1409.425493	17.199386
36.038842	1403.240011	17.204403
36.014500	1406.768761	17.209421
35.936137	1409.595856	17.214439
36.115523	1406.316603	17.219456
36.431114	1395.039028	17.224474
36.302524	1402.503092	17.229491
36.160892	1408.782305	17.234509
36.079954	1405.653120	17.239527
36.247064	1404.956559	17.244544
36.186222	1424.360181	17.249562
36.716009	1432.306815	17.254579
36.739880	1436.714348	17.259597
36.503354	1421.665113	17.264615
36.393856	1422.380516	17.269632
36.497475	1426.705321	17.274650
36.687036	1440.045468	17.279667
36.800135	1441.095843	17.284685
36.593772	1429.630914	17.289703
36.840672	1416.468644	17.294720
36.384155	1441.494090	17.299738
36.799978	1436.063601	17.304755
36.681697	1445.157389	17.309773
36.771513	1442.056021	17.314791
36.773420	1434.153287	17.319808
36.523994	1441.113574	17.324826
36.666323	1436.072799	17.329843
36.412543	1441.006000	17.334861
36.519175	1444.461955	17.339879
37.103154	1441.766295	17.344896
36.555885	1453.972545	17.349914
37.181551	1457.114464	17.354931
37.106833	1464.273429	17.359949
37.346947	1468.787276	17.364967
37.794459	1468.329941	17.369984
37.426170	1460.705693	17.375002
37.466256	1429.456144	17.380019
37.488858	1432.088588	17.385037
37.426325	1426.945988	17.390055
37.497569	1422.414454	17.395072
36.936252	1431.261125	17.400090
37.454416	1424.788628	17.405107
37.227834	1435.332030	17.410125
37.354472	1445.440759	17.415143
37.560391	1451.247674	17.420160
37.491322	1464.633027	17.425178
37.801931	1460.909656	17.430195
37.883378	1470.489955	17.435213
37.464033	1466.294653	17.440231
38.224618	1465.860534	17.445248
37.649094	1456.798451	17.450266
37.962248	1459.076221	17.455283
38.314125	1448.272627	17.460301
37.800204	1429.658051	17.465319
38.008585	1423.111475	17.470336
37.485580	1434.280284	17.475354
37.966569	1438.546475	17.480371
37.842656	1447.547562	17.485389
37.731222	1454.890930	17.490407
38.059887	1447.220810	17.495424
37.899431	1463.535774	17.500442
38.103856	1462.983494	17.505459
38.026654	1459.119829	17.510477
38.058418	1460.192617	17.515495
38.321457	1454.617378	17.520512
38.317350	1461.986105	17.525530
38.551648	1449.440129	17.530547
38.426035	1462.247717	17.535565
38.003377	1463.069705	17.540583
38.724859	1452.886755	17.545600
38.617825	1454.794209	17.550618
38.355616	1460.172388	17.555635
38.162522	1460.635265	17.560653
38.521009	1450.905073	17.565671
38.553796	1457.821141	17.570688
38.234736	1465.551588	17.575706
38.628236	1473.004778	17.580723
38.755496	1483.406826	17.585741
38.628583	1488.326887	17.590759
38.834715	1487.653202	17.595776
38.751774	1487.555774	17.600794
38.852326	1481.745299	17.605811
38.894219	1485.953328	17.610829
38.937353	1484.585140	17.615847
39.111236	1487.184025	17.620864
38.994434	1496.499424	17.625882
39.173860	1484.540302	17.630899
39.090335	1497.648759	17.635917
39.140026	1490.042777	17.640935
39.262716	1487.653512	17.645952
39.123992	1491.985527	17.650970
39.256676	1492.937606	17.655987
39.412244	1486.322341	17.661005
39.257715	1492.423522	17.666023
39.336193	1483.093502	17.671040
39.242316	1487.244530	17.676058
39.357641	1484.925658	17.681075
39.337058	1481.526474	17.686093
39.195687	1483.707631	17.691111
39.521512	1476.649903	17.696128
39.508723	1488.548331	17.701146
39.021970	1486.674729	17.706163
39.110703	1483.985690	17.711181
39.053561	1499.013111	17.716199
39.752706	1500.501741	17.721216
39.716695	1511.853290	17.726234
39.723007	1507.132297	17.731251
39.851022	1507.764986	17.736269
39.680876	1509.187759	17.741287
39.984431	1503.836505	17.746304
39.733690	1509.086233	17.751322
39.597518	1508.319268	17.756339
39.795827	1509.643944	17.761357
39.836317	1506.120960	17.766375
39.853847	1501.653030	17.771392
39.687913	1518.872703	17.776410
39.916913	1531.607273	17.781427
40.181888	1531.728868	17.786445
39.928505	1537.283433	17.791463
40.307866	1527.969892	17.796480
40.077098	1536.224312	17.801498
40.071383	1528.779743	17.806515
40.440695	1529.763302	17.811533
40.205463	1529.995356	17.816551
40.557266	1529.168649	17.821568
40.216850	1528.589216	17.826586
40.578840	1529.577875	17.831603
40.572002	1525.066630	17.836621
40.613572	1532.230677	17.841639
40.531018	1531.544828	17.846656
40.650992	1532.041937	17.851674
40.824022	1539.633368	17.856691
40.769279	1528.847376	17.861709
40.651230	1532.655393	17.866727
40.953364	1540.549515	17.871744
40.705564	1551.197066	17.876762
40.835960	1555.616747	17.881779
41.356357	1549.479709	17.886797
41.035642	1546.153552	17.891815
40.912858	1528.796339	17.896832
41.186961	1537.269131	17.901850
41.218238	1534.151910	17.906867
41.124813	1524.061919	17.911885
40.961882	1521.943165	17.916903
41.484177	1519.091363	17.921920
41.028270	1537.008593	17.926938
40.946111	1548.046608	17.931955
41.385275	1541.772293	17.936973
40.976185	1552.827847	17.941991
41.381418	1546.212062	17.947008
41.350252	1555.150441	17.952026
41.296261	1543.223782	17.957043
41.717001	1552.544722	17.962061
41.348362	1545.434906	17.967079
41.667542	1547.219331	17.972096
41.455259	1547.177143	17.977114
41.552907	1542.071879	17.982131
41.934541	1544.108273	17.987149
41.740296	1554.931344	17.992167
41.664586	1547.573441	17.997184
41.864990	1551.888353	18.002202
41.641467	1552.858709	18.007219
41.779200	1551.090789	18.012237
41.690697	1560.651060	18.017255
41.801438	1549.262097	18.022272
41.911723	1564.440649	18.027290
41.713568	1587.350142	18.032307
42.037589	1573.174902	18.037325
42.023658	1585.572283	18.042343
42.353191	1583.994796	18.047360
43.114730	1558.742405	18.052378
43.226381	1549.672914	18.057395
43.228129	1532.152677	18.062413
43.136322	1529.467255	18.067431
43.275886	1517.534915	18.072448
43.072227	1495.796830	18.077466
42.570817	1492.700868	18.082483
42.795863	1489.254639	18.087501
42.861846	1481.609094	18.092519
43.066512	1477.005136	18.097536
42.964706	1479.611810	18.102554
42.760689	1489.221135	18.107571
43.022191	1478.593969	18.112589
42.656645	1465.560802	18.117607
42.417934	1456.272738	18.122624
42.692998	1475.614986	18.127642
42.557533	1481.165666	18.132659
42.883906	1480.681245	18.137677
42.664563	1486.404194	18.142695
42.745650	1489.142160	18.147712
42.811988	1488.350762	18.152730
42.874982	1482.770450	18.157747
43.018265	1487.382339	18.162765
42.662886	1498.373438	18.167783
42.843268	1494.830504	18.172800
42.901279	1510.353205	18.177818
42.831718	1520.784313	18.182835
42.948469	1511.380525	18.187853
42.857198	1518.972413	18.192871
42.822753	1511.930442	18.197888
43.283986	1521.514699	18.202906
43.438568	1538.580233	18.207923
43.529654	1548.348611	18.212941
43.367507	1551.197749	18.217959
43.903404	1547.465953	18.222976
43.729277	1556.144754	18.227994
43.560157	1552.309097	18.233011
43.804243	1545.892062	18.238029
43.597922	1551.597228	18.243047
43.499375	1555.426523	18.248064
43.729652	1556.378773	18.253082
43.339078	1552.923745	18.258099
43.974158	1538.152255	18.263117
43.798238	1552.011732	18.268135
43.606016	1544.980753	18.273152
43.844657	1536.956040	18.278170
43.818272	1543.578755	18.283187
43.944070	1535.255052	18.288205
44.090111	1555.405347	18.293223
44.327128	1562.164611	18.298240
44.400863	1568.651022	18.303258
44.545544	1557.593295	18.308275
44.388735	1546.191948	18.313293
44.442382	1546.149032	18.318311
44.380933	1540.591693	18.323328
44.593898	1540.668097	18.328346
44.034468	1542.914368	18.333363
44.661417	1547.859726	18.338381
44.820399	1564.423539	18.343399
44.609513	1563.489148	18.348416
44.611569	1567.681531	18.353434
44.819069	1566.180144	18.358451
44.948450	1554.893606	18.363469
44.824722	1558.675791	18.368487
44.873179	1560.335071	18.373504
45.212781	1558.298193	18.378522
44.709673	1558.995365	18.383539
44.872903	1549.405586	18.388557
44.579394	1557.830486	18.393575
45.020218	1557.683341	18.398592
45.046005	1555.492793	18.403610
44.890254	1560.972015	18.408627
44.917764	1562.331016	18.413645
45.073959	1565.865619	18.418663
44.877657	1561.317723	18.423680
44.941209	1561.052199	18.428698
44.628682	1573.649004	18.433715
45.004243	1576.273159	18.438733
45.543127	1596.364787	18.443751
45.484287	1596.711078	18.448768
45.353089	1599.488430	18.453786
45.185266	1601.077595	18.458803
45.608984	1597.279516	18.463821
45.423774	1610.424743	18.468839
45.525509	1602.827707	18.473856
45.736696	1603.137222	18.478874
45.336502	1594.532406	18.483891
45.459019	1591.182738	18.488909
45.369584	1605.848088	18.493927
45.909144	1611.363519	18.498944
46.232817	1614.980756	18.503962
46.100277	1625.952927	18.508979
46.467789	1612.437734	18.513997
46.029893	1603.041333	18.519015
46.106779	1602.289149	18.524032
46.073610	1587.152246	18.529050
45.943270	1598.487445	18.534067
46.153111	1611.925984	18.539085
46.467911	1609.272444	18.544103
46.428350	1628.464498	18.549120
46.699820	1618.764593	18.554138
46.414206	1621.383305	18.559155
46.601936	1611.642487	18.564173
46.101337	1610.993421	18.569191
46.064586	1611.142691	18.574208
46.374501	1615.890079	18.579226
46.062168	1618.331351	18.584243
46.403862	1610.663788	18.589261
46.446874	1619.341816	18.594279
46.575327	1613.159505	18.599296
47.108043	1627.819249	18.604314
46.619393	1625.083050	18.609331
46.513141	1630.724304	18.614349
46.952212	1640.636246	18.619367
47.145453	1647.190942	18.624384
47.404470	1634.180715	18.629402
47.329063	1641.144803	18.634419
47.361972	1633.092286	18.639437
47.141873	1621.466573	18.644455
47.030171	1613.186212	18.649472
47.184973	1632.389747	18.654490
47.274547	1639.523379	18.659507
47.301411	1639.397425	18.664525
47.566969	1643.585558	18.669543
47.143700	1646.524344	18.674560
47.598899	1635.698628	18.679578
47.483583	1642.751673	18.684595
47.125702	1634.105475	18.689613
47.391552	1636.618928	18.694631
47.606064	1634.357365	18.699648
47.880011	1631.996652	18.704666
47.414273	1643.831372	18.709683
47.632372	1633.670380	18.714701
47.846138	1636.237762	18.719719
47.746741	1632.725260	18.724736
47.989471	1633.302689	18.729754
47.866476	1633.506617	18.734771
47.974660	1632.158716	18.739789
47.829977	1638.114443	18.744807
48.088029	1638.889220	18.749824
48.067758	1638.712576	18.754842
47.760072	1639.034059	18.759859
48.115115	1648.113834	18.764877
48.402579	1656.080366	18.769895
47.876116	1662.573664	18.774912
48.492005	1659.657355	18.779930
48.586054	1663.710027	18.784947
48.560800	1661.223983	18.789965
48.857397	1662.747733	18.794983
48.685199	1662.332602	18.800000
48.676028	1658.890654	18.805018
48.268572	1666.206617	18.810035
48.552471	1661.092057	18.815053
48.534916	1662.960096	18.820071
48.453093	1667.321630	18.825088
48.604911	1654.081496	18.830106
48.250818	1663.102910	18.835123
48.660432	1660.972261	18.840141
48.822614	1681.319949	18.845159
48.787926	1682.037590	18.850176
49.215639	1688.219822	18.855194
48.986219	1698.106280	18.860211
49.542158	1696.078142	18.865229
49.337500	1699.251869	18.870247
49.057333	1693.609008	18.875264
49.346176	1682.237944	18.880282
49.185557	1692.619985	18.885299
49.424463	1690.370254	18.890317
49.424937	1693.263488	18.895335
49.050704	1694.597695	18.900352
49.248674	1681.668741	18.905370
49.416852	1695.397961	18.910387
49.277742	1687.977733	18.915405
49.489354	1683.953889	18.920423
49.496306	1707.836899	18.925440
50.048761	1711.090451	18.930458
50.238150	1714.862851	18.935475
49.727362	1702.522808	18.940493
49.833910	1692.567562	18.945511
50.026470	1696.462945	18.950528
50.354954	1692.807458	18.955546
50.313343	1683.065415	18.960563
50.178952	1680.816231	18.965581
50.050789	1672.827925	18.970599
49.650929	1680.949718	18.975616
50.211426	1695.432052	18.980634
50.024388	1701.481870	18.985651
50.115117	1708.100139	18.990669
50.403537	1717.089114	18.995687
50.134460	1714.356419	19.000704
50.489735	1712.004746	19.005722
50.145374	1718.595665	19.010739
50.107465	1719.265054	19.015757
50.497236	1706.543036	19.020775
50.291997	1710.593901	19.025792
50.525632	1706.475294	19.030810
50.817885	1719.515362	19.035827
50.861488	1729.764961	19.040845
51.065657	1725.931860	19.045863
51.010259	1717.362435	19.050880
50.839200	1704.128131	19.055898
50.709174	1721.141736	19.060915
50.894721	1723.343152	19.065933
51.371146	1734.595838	19.070951
50.817725	1730.161481	19.075968
51.406338	1735.322252	19.080986
51.419038	1738.175002	19.086003
51.339347	1725.748876	19.091021
51.608885	1731.311354	19.096039
51.599624	1734.167606	19.101056
51.669131	1718.723152	19.106074
51.336195	1707.999490	19.111091
51.128176	1713.797019	19.116109
51.534759	1721.200271	19.121127
51.487936	1735.373631	19.126144
51.639816	1726.973293	19.131162
51.509842	1732.818163	19.136179
51.391351	1729.888398	19.141197
51.322992	1732.331678	19.146215
51.580818	1734.691470	19.151232
51.531507	1724.293828	19.156250
51.537486	1748.420115	19.161267
51.530492	1758.931085	19.166285
51.796094	1753.206659	19.171303
51.950777	1757.811310	19.176320
51.883431	1757.487215	19.181338
52.124646	1752.977239	19.186355
51.773530	1752.547379	19.191373
52.123872	1769.998854	19.196391
52.252512	1782.023630	19.201408
52.980329	1783.301634	19.206426
52.596987	1792.261718	19.211443
52.643775	1795.220738	19.216461
52.973253	1783.906041	19.221479
52.652795	1769.060187	19.226496
52.866059	1763.773582	19.231514
52.321980	1756.266098	19.236531
52.486183	1772.325112	19.241549
52.813718	1775.044276	19.246567
52.833353	1785.874307	19.251584
53.034410	1785.527854	19.256602
52.852767	1789.557672	19.261619
52.802818	1787.518395	19.266637
53.176049	1781.384284	19.271655
52.772029	1787.171415	19.276672
52.957283	1784.891684	19.281690
52.998568	1781.401544	19.286707
52.990536	1784.859351	19.291725
52.980751	1778.649463	19.296743
52.644801	1792.205897	19.301760
53.690884	1793.086255	19.306778
53.565692	1806.468288	19.311795
53.375953	1812.906373	19.316813
53.542930	1808.744881	19.321831
53.351934	1822.016289	19.326848
53.843457	1811.637727	19.331866
53.185800	1814.783832	19.336883
53.488792	1812.795236	19.341901
53.496793	1805.515096	19.346919
53.584504	1811.781501	19.351936
53.556786	1810.563022	19.356954
53.810863	1824.771069	19.361971
53.671832	1838.173430	19.366989
54.233935	1831.762971	19.372007
54.313631	1848.941497	19.377024
54.347353	1843.356277	19.382042
54.306834	1843.048352	19.387059
54.413187	1835.857914	19.392077
54.509316	1842.925314	19.397095
54.166437	1848.487976	19.402112
54.490499	1839.223963	19.407130
54.554291	1832.441477	19.412147
54.383972	1840.259306	19.417165
54.825622	1836.442574	19.422183
54.813594	1837.329660	19.427200
54.977712	1832.573954	19.432218
54.732387	1827.111119	19.437235
54.947947	1828.208108	19.442253
55.244292	1828.902850	19.447271
54.773030	1831.816289	19.452288
55.034707	1833.281128	19.457306
54.790332	1836.237039	19.462323
54.728512	1834.930394	19.467341
54.876106	1834.262098	19.472359
54.558574	1837.156525	19.477376
54.800712	1839.882243	19.482394
54.988639	1831.092238	19.487411
54.963096	1843.828352	19.492429
55.124298	1843.492187	19.497447
55.141230	1853.488124	19.502464
54.968015	1853.370481	19.507482
55.224223	1855.728192	19.512499
55.206340	1850.697096	19.517517
55.299966	1859.094246	19.522535
55.615836	1868.406160	19.527552
55.738861	1884.017213	19.532570
55.682269	1889.575920	19.537587
55.587790	1892.158687	19.542605
55.825969	1889.794199	19.547623
55.459842	1888.678458	19.552640
55.593031	1886.424321	19.557658
55.903197	1893.290063	19.562675
55.865146	1883.080081	19.567693
55.659967	1889.493131	19.572711
56.085423	1900.360778	19.577728
56.481577	1907.568354	19.582746
56.264610	1908.426775	19.587763
56.318176	1915.906883	19.592781
56.405062	1902.475512	19.597799
56.297988	1913.050537	19.602816
56.611237	1909.085935	19.607834
56.945590	1901.489400	19.612851
56.987055	1895.263423	19.617869
56.739521	1901.768972	19.622887
56.844216	1898.324538	19.627904
57.107528	1898.550235	19.632922
57.340397	1896.841828	19.637939
56.989244	1891.517770	19.642957
57.211107	1874.444198	19.647975
57.250309	1869.182171	19.652992
56.985484	1861.219490	19.658010
56.982356	1859.710766	19.663027
56.531053	1870.575854	19.668045
56.900363	1879.023437	19.673063
57.413643	1883.759718	19.678080
57.592308	1881.614745	19.683098
57.786807	1876.427845	19.688115
57.950650	1881.952177	19.693133
57.894642	1881.697064	19.698151
57.460500	1873.949377	19.703168
57.414988	1878.740956	19.708186
57.657781	1876.785551	19.713203
57.708413	1878.851977	19.718221
57.823220	1879.805361	19.723239
57.532433	1881.599804	19.728256
57.686726	1884.341901	19.733274
57.880064	1882.147392	19.738291
57.973185	1880.220578	19.743309
57.990744	1873.246438	19.748327
58.044045	1883.592922	19.753344
57.949091	1883.196141	19.758362
58.139919	1876.177060	19.763379
58.132825	1885.607356	19.768397
58.417839	1894.853415	19.773415
58.506753	1914.090643	19.778432
58.479471	1913.441582	19.783450
58.593851	1908.881781	19.788467
58.626364	1924.846337	19.793485
58.792016	1912.843440	19.798503
58.757772	1915.349744	19.803520
58.756928	1910.380410	19.808538
59.216853	1899.845575	19.813555
58.854754	1887.684599	19.818573
58.691453	1882.397444	19.823591
58.442143	1890.356113	19.828608
58.895668	1893.214098	19.833626
59.028653	1904.828466	19.838643
58.867834	1908.102223	19.843661
58.823885	1911.756931	19.848679
58.910263	1911.422473	19.853696
58.721819	1914.655015	19.858714
58.879802	1919.200983	19.863731
58.924496	1938.892869	19.868749
59.290552	1926.401771	19.873767
59.373689	1924.815567	19.878784
59.714855	1935.249898	19.883802
59.455127	1928.183089	19.888819
59.346857	1939.333327	19.893837
59.811332	1934.229989	19.898855
59.362707	1941.024059	19.903872
59.717463	1941.958843	19.908890
59.452663	1942.576330	19.913907
59.815031	1959.090062	19.918925
60.048762	1972.103508	19.923943
60.077229	1964.622588	19.928960
60.035027	1968.094540	19.933978
60.251443	1959.281824	19.938995
59.974728	1966.859471	19.944013
60.067853	1959.999094	19.949031
60.172846	1958.573013	19.954048
60.126141	1966.401870	19.959066
60.402392	1953.193535	19.964083
60.251170	1970.269019	19.969101
60.435406	1980.637952	19.974119
60.616967	1977.808162	19.979136
60.686024	1986.465735	19.984154
60.841042	1981.952919	19.989171
60.772028	1990.309223	19.994189
61.087506	1986.680123	19.999207
61.189373	1973.970757	20.004224
61.325020	1980.323194	20.009242
61.326293	1973.379135	20.014259
61.232939	1989.037397	20.019277
61.175507	1974.917890	20.024295
61.601969	1983.055151	20.029312
61.221863	1978.449911	20.034330
61.224139	1978.612625	20.039347
61.086019	1985.693070	20.044365
61.069399	1982.444951	20.049383
61.319097	1981.127938	20.054400
61.265575	1986.962288	20.059418
61.420326	1981.622797	20.064435
61.432168	1996.867844	20.069453
61.949343	2010.515741	20.074471
61.695087	2011.170879	20.079488
61.551010	2016.186672	20.084506
61.780385	2004.995536	20.089523
61.535632	2020.828220	20.094541
62.007111	2014.984332	20.099559
61.961380	2015.175941	20.104576
61.953771	2017.991868	20.109594
62.132918	2017.589123	20.114611
62.115791	2024.968078	20.119629
62.186133	2035.376453	20.124647
62.291566	2045.610120	20.129664
62.314492	2048.990684	20.134682
62.526247	2039.849862	20.139699
62.249579	2044.884453	20.144717
62.148954	2044.448455	20.149735
62.684511	2041.340370	20.154752
62.269339	2049.192642	20.159770
62.283414	2054.892742	20.164787
62.603047	2065.923700	20.169805
62.699484	2071.301535	20.174823
62.958549	2070.584773	20.179840
62.895819	2070.651663	20.184858
62.834166	2067.854353	20.189875
62.851921	2077.837727	20.194893
63.000233	2082.256285	20.199911
63.442109	2092.927954	20.204928
63.460539	2103.122048	20.209946
63.628965	2099.248142	20.214963
63.417392	2103.008293	20.219981
63.396937	2095.711308	20.224999
63.814822	2098.368929	20.230016
63.750820	2102.827648	20.235034
63.606804	2099.120778	20.240051
63.942955	2101.149564	20.245069
63.880910	2103.875864	20.250087
63.962377	2096.197638	20.255104
63.826394	2095.107314	20.260122
63.886087	2083.448406	20.265139
64.274169	2099.224293	20.270157
64.049634	2084.418665	20.275175
63.935471	2090.935277	20.280192
63.915572	2101.281005	20.285210
64.430991	2097.886650	20.290227
64.352029	2110.223266	20.295245
64.369777	2130.077029	20.300263
64.896813	2123.871051	20.305280
64.967534	2122.617181	20.310298
64.913606	2105.649467	20.315315
64.588330	2096.826311	20.320333
64.680610	2109.737369	20.325351
64.823050	2118.126097	20.330368
64.642191	2129.571236	20.335386
65.271239	2111.762255	20.340403
65.116985	2121.098969	20.345421
64.888338	2128.543176	20.350439
65.072206	2119.759939	20.355456
64.835722	2118.127938	20.360474
65.323670	2113.227674	20.365491
65.120767	2122.333019	20.370509
64.724226	2115.501896	20.375527
64.816912	2125.331762	20.380544
65.032881	2136.925214	20.385562
65.734788	2136.894539	20.390579
65.708773	2141.718491	20.395597
65.971125	2139.726895	20.400615
65.854230	2138.056153	20.405632
65.563009	2144.180192	20.410650
65.868391	2141.075760	20.415667
65.882309	2148.247667	20.420685
65.907495	2142.043060	20.425703
65.969021	2131.305727	20.430720
65.926604	2143.727003	20.435738
65.853679	2140.752916	20.440755
66.123765	2161.550525	20.445773
66.171059	2168.680934	20.450791
66.385266	2165.693299	20.455808
66.199698	2180.573569	20.460826
66.479217	2180.917825	20.465843
66.629217	2176.622068	20.470861
66.420002	2179.268021	20.475879
66.519477	2170.187503	20.480896
66.366518	2181.258525	20.485914
66.851581	2188.131911	20.490931
66.675066	2202.850292	20.495949
66.671309	2214.618080	20.500967
67.488072	2197.092131	20.505984
67.235973	2208.019303	20.511002
67.287022	2202.066194	20.516019
67.270833	2210.487354	20.521037
67.405061	2200.512402	20.526055
67.257945	2197.798705	20.531072
66.796863	2204.944137	20.536090
67.114008	2192.647829	20.541107
67.427555	2205.523683	20.546125
67.396602	2215.363103	20.551143
67.425578	2226.831487	20.556160
67.530854	2242.238875	20.561178
67.775482	2232.598697	20.566195
67.540472	2236.119556	20.571213
67.709516	2230.085475	20.576231
68.036482	2221.398134	20.581248
67.988878	2224.424213	20.586266
68.292103	2225.828191	20.591283
68.393926	2235.375853	20.596301
68.196348	2233.940579	20.601319
68.524439	2238.339952	20.606336
68.858064	2240.517832	20.611354
68.655572	2230.506102	20.616371
68.521409	2231.580239	20.621389
68.535899	2231.722915	20.626407
69.085705	2242.804613	20.631424
68.444646	2236.712517	20.636442
68.763695	2237.557836	20.641459
68.992459	2239.634447	20.646477
69.009921	2247.597172	20.651495
69.037282	2243.028334	20.656512
69.025724	2246.897425	20.661530
69.263120	2235.895195	20.666547
69.357256	2243.534976	20.671565
68.947658	2240.445441	20.676583
69.518466	2227.102568	20.681600
69.354992	2234.381471	20.686618
69.148780	2234.934561	20.691635
69.843127	2230.368690	20.696653
69.382982	2231.151854	20.701671
69.340262	2232.938238	20.706688
69.296964	2238.067039	20.711706
69.215333	2238.421699	20.716723
69.390294	2250.537801	20.721741
69.424440	2255.406472	20.726759
69.652790	2249.484850	20.731776
69.502101	2262.041487	20.736794
69.955093	2278.086465	20.741811
70.368465	2283.916479	20.746829
70.336584	2288.998639	20.751847
70.756253	2288.987021	20.756864
70.770952	2288.812657	20.761882
70.717183	2280.227695	20.766899
70.419747	2268.638970	20.771917
70.404126	2274.966891	20.776935
70.881831	2278.221487	20.781952
70.744336	2288.038617	20.786970
70.776205	2285.266467	20.791987
70.859052	2284.129428	20.797005
70.805305	2284.137464	20.802023
70.622868	2293.033557	20.807040
70.774403	2290.115675	20.812058
70.960408	2283.038173	20.817075
71.019494	2282.162149	20.822093
70.912187	2314.024148	20.827111
71.787628	2311.154425	20.832128
71.432166	2314.765308	20.837146
71.454397	2316.737212	20.842163
71.736106	2310.081793	20.847181
71.566043	2313.784247	20.852199
71.640795	2311.356084	20.857216
71.802250	2311.898523	20.862234
71.507756	2311.870226	20.867251
71.894452	2306.362260	20.872269
71.401691	2312.184198	20.877287
71.873861	2316.437117	20.882304
71.977435	2338.124455	20.887322
72.156826	2341.070304	20.892339
72.250667	2336.833800	20.897357
72.047911	2345.701701	20.902375
72.690689	2344.111938	20.907392
72.361401	2342.571800	20.912410
72.350354	2330.876780	20.917427
72.244232	2333.828045	20.922445
72.150534	2341.371975	20.927463
72.508675	2353.250494	20.932480
72.641368	2360.398842	20.937498
72.678779	2368.949203	20.942515
73.125522	2359.969721	20.947533
73.178175	2367.610676	20.952551
73.232899	2364.719233	20.957568
73.300659	2365.492151	20.962586
73.264138	2362.815061	20.967603
73.488745	2352.713892	20.972621
73.260671	2362.965573	20.977639
73.410782	2352.350822	20.982656
73.537921	2358.055820	20.987674
73.524262	2356.481861	20.992691
73.462609	2353.676629	20.997709
73.547190	2351.148564	21.002727
73.668255	2357.428764	21.007744
73.880869	2365.501233	21.012762
73.922511	2372.571287	21.017779
74.049840	2381.686269	21.022797
73.669079	2394.041365	21.027815
73.816245	2391.586694	21.032832
74.227888	2396.357449	21.037850
73.667505	2396.167035	21.042867
74.157415	2389.574343	21.047885
74.046404	2397.465604	21.052903
74.082282	2407.107278	21.057920
74.339864	2414.832782	21.062938
74.383669	2416.160160	21.067955
74.922894	2408.800503	21.072973
75.059674	2409.759071	21.077991
75.191907	2405.283585	21.083008
75.309095	2403.883048	21.088026
75.559770	2401.125537	21.093043
75.591758	2395.708720	21.098061
75.571124	2393.608832	21.103079
75.641194	2397.046461	21.108096
75.457896	2394.912733	21.113114
75.408399	2397.104542	21.118131
75.749892	2389.851946	21.123149
75.362758	2408.158870	21.128167
75.551165	2393.752750	21.133184
75.524851	2400.259421	21.138202
75.717025	2398.632965	21.143219
75.653490	2396.212683	21.148237
75.737517	2396.990088	21.153255
75.798915	2383.987904	21.158272
75.974840	2394.658161	21.163290
75.859123	2397.352957	21.168307
76.021962	2408.129146	21.173325
75.875215	2423.329920	21.178343
76.106266	2430.585329	21.183360
76.156283	2421.270263	21.188378
76.134424	2423.492280	21.193395
76.185933	2426.704755	21.198413
76.290722	2449.023723	21.203431
76.417864	2443.635765	21.208448
76.908911	2462.449306	21.213466
76.698385	2458.429647	21.218483
77.289542	2454.975150	21.223501
76.993821	2465.415469	21.228519
76.828620	2459.274916	21.233536
77.102470	2452.218721	21.238554
76.792625	2456.945665	21.243571
77.216613	2460.278880	21.248589
77.216512	2461.577867	21.253607
77.188432	2467.062235	21.258624
77.369987	2477.831557	21.263642
77.325885	2494.033929	21.268659
77.941007	2486.317587	21.273677
77.574500	2490.618573	21.278695
77.764511	2491.040830	21.283712
77.702377	2481.567408	21.288730
77.407277	2492.297125	21.293747
77.787029	2487.476139	21.298765
77.909002	2505.944272	21.303783
78.274036	2508.634786	21.308800
78.759694	2513.439400	21.313818
78.573895	2512.622870	21.318835
78.820910	2506.790204	21.323853
78.586974	2506.189807	21.328871
78.170291	2502.701738	21.333888
78.872015	2506.747406	21.338906
78.815377	2500.037309	21.343923
78.931558	2503.865643	21.348941
78.865154	2505.790351	21.353959
78.845784	2501.774806	21.358976
79.052541	2503.943855	21.363994
78.905026	2500.582769	21.369011
79.170717	2492.336901	21.374029
78.901226	2500.004917	21.379047
78.687467	2499.645945	21.384064
79.205658	2520.483160	21.389082
78.933542	2532.127237	21.394099
79.471794	2528.733866	21.399117
79.396124	2545.930125	21.404135
79.563142	2531.893064	21.409152
79.721997	2533.923444	21.414170
79.717129	2559.700003	21.419187
80.079428	2552.984425	21.424205
80.213931	2566.029174	21.429223
80.314878	2564.593455	21.434240
80.133162	2557.587053	21.439258
80.292992	2558.139987	21.444275
80.333320	2563.506499	21.449293
80.513178	2569.458828	21.454311
80.350582	2553.202522	21.459328
80.333295	2566.983381	21.464346
80.111755	2562.387275	21.469363
80.399370	2561.600648	21.474381
80.914067	2576.649681	21.479399
80.979188	2593.751957	21.484416
81.277505	2584.147826	21.489434
80.977441	2587.598905	21.494451
81.084300	2574.740335	21.499469
81.132175	2584.695652	21.504487
81.304989	2586.531875	21.509504
81.299104	2579.339307	21.514522
81.422451	2585.870177	21.519539
81.513157	2578.998883	21.524557
81.481064	2580.702592	21.529575
81.788819	2585.148580	21.534592
81.771964	2576.087937	21.539610
81.281014	2584.043038	21.544627
81.879199	2579.829866	21.549645
81.598413	2592.277738	21.554663
81.622106	2598.199133	21.559680
81.842625	2610.335801	21.564698
81.770100	2617.835592	21.569715
82.146641	2612.966307	21.574733
82.083445	2612.492856	21.579751
82.590245	2607.470644	21.584768
82.799484	2613.281430	21.589786
83.066026	2613.619903	21.594803
83.237380	2586.856718	21.599821
83.503202	2588.285579	21.604839
83.178191	2587.620253	21.609856
83.426411	2586.138232	21.614874
83.154496	2590.070175	21.619891
83.587876	2587.830988	21.624909
83.368189	2587.815144	21.629927
83.383389	2591.814573	21.634944
83.413550	2589.168499	21.639962
83.227755	2589.568884	21.644979
83.417116	2587.289951	21.649997
83.364986	2587.305595	21.655015
83.440412	2582.633803	21.660032
83.565997	2580.848034	21.665050
83.608889	2597.121603	21.670067
83.639102	2606.722621	21.675085
83.486782	2610.635496	21.680103
83.453374	2614.329603	21.685120
83.831648	2622.865870	21.690138
83.957235	2638.331795	21.695155
83.916504	2637.098803	21.700173
83.970320	2635.588783	21.705191
84.249879	2642.090832	21.710208
84.372769	2641.922809	21.715226
84.156429	2659.019706	21.720243
84.512490	2659.307718	21.725261
84.682800	2667.409915	21.730279
84.580384	2674.590407	21.735296
84.908750	2668.772236	21.740314
84.770323	2672.585369	21.745331
84.812586	2670.093104	21.750349
85.061338	2688.763081	21.755367
85.224402	2696.750027	21.760384
85.388798	2692.859303	21.765402
85.280552	2702.712163	21.770419
85.306018	2699.785201	21.775437
85.350512	2693.911603	21.780455
85.444711	2701.472950	21.785472
85.826059	2702.894411	21.790490
85.701078	2708.519399	21.795507
85.712297	2714.852669	21.800525
85.763448	2723.545002	21.805543
86.079393	2724.224867	21.810560
86.188949	2719.612093	21.815578
86.152170	2733.344299	21.820595
86.215225	2716.603438	21.825613
86.562564	2722.720273	21.830631
86.040927	2726.608694	21.835648
86.615624	2732.130759	21.840666
86.586070	2744.775472	21.845683
86.980101	2743.009017	21.850701
87.063251	2750.056901	21.855719
87.072766	2750.344332	21.860736
87.196788	2746.000634	21.865754
87.210791	2754.279629	21.870771
87.411323	2736.316405	21.875789
87.582138	2737.495334	21.880807
87.436175	2733.001184	21.885824
87.638232	2732.450027	21.890842
87.568833	2735.209082	21.895859
87.544871	2735.683565	21.900877
87.497411	2732.317482	21.905895
87.249435	2740.641396	21.910912
87.642842	2738.590277	21.915930
88.124852	2752.670844	21.920947
88.136769	2753.016889	21.925965
88.790255	2756.272670	21.930983
88.231226	2760.103344	21.936000
88.706725	2754.469349	21.941018
88.549308	2757.468211	21.946035
88.833065	2750.227794	21.951053
88.674265	2756.553585	21.956071
88.623706	2762.813345	21.961088
88.919147	2746.497934	21.966106
88.689584	2762.664890	21.971123
88.773187	2761.633105	21.976141
88.966070	2758.959477	21.981159
88.870999	2755.007852	21.986176
89.038172	2750.614006	21.991194
88.863517	2764.938546	21.996211
89.139654	2775.407453	22.001229
89.205871	2784.693694	22.006247
89.285602	2793.226541	22.011264
89.558271	2786.764292	22.016282
89.333065	2787.699592	22.021299
89.320510	2791.844312	22.026317
89.503236	2793.469733	22.031335
89.465587	2814.681568	22.036352
89.869132	2809.605745	22.041370
89.720057	2815.985076	22.046387
89.631431	2819.525205	22.051405
89.841504	2832.716256	22.056423
89.886728	2846.693511	22.061440
90.083996	2843.542459	22.066458
90.235238	2850.962630	22.071475
90.329654	2859.433389	22.076493
90.642474	2871.026927	22.081511
90.652905	2874.857278	22.086528
91.139514	2880.753734	22.091546
90.738989	2882.306986	22.096563
90.722863	2886.932944	22.101581
90.707031	2883.715178	22.106599
90.702393	2899.284745	22.111616
91.175500	2902.218480	22.116634
91.074288	2917.430596	22.121651
91.264787	2914.677081	22.126669
91.420529	2910.350303	22.131687
91.569664	2929.594209	22.136704
91.837549	2934.701945	22.141722
91.755773	2941.418297	22.146739
91.759752	2942.082634	22.151757
92.470555	2928.781311	22.156775
92.259892	2940.338817	22.161792
92.557378	2924.634899	22.166810
92.661761	2932.798103	22.171827
92.102810	2929.091115	22.176845
92.243510	2928.450618	22.181863
92.096827	2937.365784	22.186880
92.640792	2938.954066	22.191898
92.543426	2960.662572	22.196915
92.837302	2962.755652	22.201933
93.422949	2951.731963	22.206951
93.057145	2958.601391	22.211968
93.307634	2957.406887	22.216986
93.373594	2960.922397	22.222003
93.235069	2958.707498	22.227021
93.384775	2953.668961	22.232039
93.458108	2958.340461	22.237056
93.537624	2949.944672	22.242074
93.481038	2970.264541	22.247091
93.453103	2979.838891	22.252109
93.867807	2983.142245	22.257127
93.686838	2988.534765	22.262144
94.018276	2981.792450	22.267162
94.225726	2982.945891	22.272179
94.007882	2985.657081	22.277197
94.002596	2999.743228	22.282215
94.512126	3021.467529	22.287232
94.518467	3014.854137	22.292250
94.365240	3015.191913	22.297267
94.510376	3015.230376	22.302285
94.637967	3010.420331	22.307303
94.623305	3014.058056	22.312320
94.971786	3003.069006	22.317338
95.229982	2998.212963	22.322355
95.245422	2990.141245	22.327373
95.227315	2984.824239	22.332391
95.579835	2998.533155	22.337408
95.914211	3000.905338	22.342426
95.956144	3004.464023	22.347443
95.560631	2995.320336	22.352461
95.885748	2985.219225	22.357479
95.268129	2994.575323	22.362496
95.721135	3002.719155	22.367514
95.984362	3012.431956	22.372531
95.951041	3009.210658	22.377549
96.157876	3002.053971	22.382567
96.129415	3006.261073	22.387584
96.136911	3006.528378	22.392602
95.898379	3022.707276	22.397619
96.251208	3034.717785	22.402637
96.743041	3029.031523	22.407655
96.908170	3041.308755	22.412672
96.860299	3041.642316	22.417690
96.923244	3042.332653	22.422707
96.822857	3049.509071	22.427725
97.183482	3034.302361	22.432743
97.103589	3037.545367	22.437760
97.587606	3058.497363	22.442778
97.601539	3068.117799	22.447795
97.327385	3073.550384	22.452813
97.751279	3066.029440	22.457831
97.642336	3071.375891	22.462848
97.991992	3072.792219	22.467866
97.899523	3067.354096	22.472883
97.578502	3068.602836	22.477901
97.851909	3068.443846	22.482919
97.847367	3070.924370	22.487936
98.002334	3083.191458	22.492954
98.152807	3091.175122	22.497971
98.148451	3096.454557	22.502989
98.583644	3092.773847	22.508007
98.436676	3098.413503	22.513024
98.661262	3095.185670	22.518042
98.700592	3111.934735	22.523059
98.637365	3120.124773	22.528077
99.022159	3120.079392	22.533095
98.774380	3129.305794	22.538112
99.164608	3126.574668	22.543130
99.192958	3122.980072	22.548147
98.841543	3138.841982	22.553165
99.399460	3140.287250	22.558183
99.389568	3160.119284	22.563200
99.477630	3152.339548	22.568218
99.820494	3152.344907	22.573235
99.571666	3148.982520	22.578253
99.902209	3162.107457	22.583271
99.785908	3181.065986	22.588288
100.005877	3178.056777	22.593306
100.204917	3188.267664	22.598323
100.216940	3179.209909	22.603341
100.362968	3176.673478	22.608359
100.255014	3187.297547	22.613376
100.449464	3183.507315	22.618394
100.693251	3202.349446	22.623411
101.027815	3216.783590	22.628429
101.023600	3206.441422	22.633447
100.845368	3218.150520	22.638464
100.823155	3211.657233	22.643482
101.074380	3208.751593	22.648499
101.060325	3216.400484	22.653517
101.220135	3220.103263	22.658535
101.275789	3239.856512	22.663552
101.369310	3239.216447	22.668570
101.354383	3237.707888	22.673587
101.256266	3249.453009	22.678605
101.775217	3260.027502	22.683623
101.577960	3271.590996	22.688640
101.851235	3271.028464	22.693658
101.908933	3271.659076	22.698675
102.000234	3296.572777	22.703693
102.226449	3300.130465	22.708711
102.359895	3309.265504	22.713728
102.527437	3300.639143	22.718746
102.766083	3297.074688	22.723763
102.706406	3297.418004	22.728781
102.831735	3305.907691	22.733799
103.291831	3326.770273	22.738816
103.577810	3339.631861	22.743834
103.845892	3331.533826	22.748851
103.678639	3332.149967	22.753869
104.389309	3309.897564	22.758887
104.143339	3295.411940	22.763904
103.861574	3295.098403	22.768922
103.989966	3286.622254	22.773939
103.886843	3298.550719	22.778957
103.956482	3287.871821	22.783975
104.146602	3287.568777	22.788992
103.778577	3292.829185	22.794010
104.042119	3307.635827	22.799027
104.078559	3334.314192	22.804045
104.243478	3328.431362	22.809063
104.360324	3329.436440	22.814080
104.411443	3329.559913	22.819098
104.515334	3342.796678	22.824115
104.325270	3353.935073	22.829133
104.569543	3352.327740	22.834151
104.480695	3359.886365	22.839168
104.909228	3368.792660	22.844186
105.320414	3374.398478	22.849203
105.038430	3376.261704	22.854221
105.440761	3371.862426	22.859239
105.525192	3372.672074	22.864256
105.241254	3376.878330	22.869274
105.862772	3396.644604	22.874291
105.766295	3413.296095	22.879309
106.162705	3408.626348	22.884327
105.838884	3411.005230	22.889344
105.999560	3407.239994	22.894362
106.534859	3401.703208	22.899379
106.248982	3411.925501	22.904397
106.405894	3413.249093	22.909415
106.531653	3421.092130	22.914432
106.426848	3431.869275	22.919450
107.001501	3436.975469	22.924467
106.735174	3449.011110	22.929485
106.833655	3442.094907	22.934503
106.786188	3441.810083	22.939520
106.783002	3447.783308	22.944538
107.040076	3447.744922	22.949555
106.857560	3464.699690	22.954573
107.168043	3465.101194	22.959591
107.250239	3484.708150	22.964608
107.534126	3493.355171	22.969626
107.825163	3492.403538	22.974643
107.592403	3502.888828	22.979661
107.861116	3492.613069	22.984679
108.173880	3507.437238	22.989696
108.383673	3521.714577	22.994714
108.705345	3525.508837	22.999731
108.790642	3517.612921	23.004749
108.550634	3527.366982	23.009767
108.692865	3525.664982	23.014784
109.138738	3513.251072	23.019802
109.970375	3495.143013	23.024819
109.716391	3510.659377	23.029837
109.970753	3495.012864	23.034855
109.659410	3481.554660	23.039872
109.572173	3478.654169	23.044890
109.479698	3462.733383	23.049907
109.578134	3477.461111	23.054925
109.744156	3495.806253	23.059943
110.011756	3492.771292	23.064960
110.182348	3502.961761	23.069978
110.346535	3485.871130	23.074995
109.958789	3493.864537	23.080013
110.402299	3492.433887	23.085031
110.144518	3491.511562	23.090048
110.060176	3491.005266	23.095066
110.620621	3488.072288	23.100083
110.217062	3502.765240	23.105101
110.814534	3504.757279	23.110119
110.941548	3524.266673	23.115136
110.946907	3530.236209	23.120154
110.939445	3521.113696	23.125171
110.590656	3526.171300	23.130189
110.947536	3524.090502	23.135207
111.096349	3545.707119	23.140224
111.204151	3556.109030	23.145242
111.425599	3555.200746	23.150259
111.385405	3558.689274	23.155277
111.363122	3561.544024	23.160295
111.314256	3576.937278	23.165312
111.677268	3584.678060	23.170330
111.745958	3586.535736	23.175347
112.063941	3602.095508	23.180365
111.997537	3615.091415	23.185383
112.404198	3621.422591	23.190400
112.188645	3630.480534	23.195418
112.348353	3622.030667	23.200435
112.410908	3634.418370	23.205453
112.691109	3647.433768	23.210471
112.679461	3655.132851	23.215488
112.619050	3659.663845	23.220506
112.839493	3669.527870	23.225523
113.172546	3676.436439	23.230541
113.238849	3684.995548	23.235559
113.503373	3676.152109	23.240576
113.056807	3691.270626	23.245594
113.766535	3701.339856	23.250611
113.631182	3711.547005	23.255629
113.774544	3714.303781	23.260647
114.059120	3708.983872	23.265664
114.055379	3718.878961	23.270682
114.318929	3725.692433	23.275699
114.415851	3738.405941	23.280717
114.538412	3732.613883	23.285735
114.610081	3734.276790	23.290752
114.578954	3736.969352	23.295770
114.780419	3747.854440	23.300787
115.162507	3757.526755	23.305805
115.224188	3761.995042	23.310823
115.344112	3769.445061	23.315840
115.185289	3768.362183	23.320858
115.677864	3756.108190	23.325875
115.994722	3754.276833	23.330893
116.041712	3760.046296	23.335911
116.203873	3751.584163	23.340928
115.809794	3757.435762	23.345946
116.266430	3750.323842	23.350963
116.115812	3757.764290	23.355981
115.831623	3778.344992	23.360999
116.217802	3774.427272	23.366016
116.205287	3779.739721	23.371034
116.459520	3786.498065	23.376051
116.327458	3789.249215	23.381069
116.620840	3799.565848	23.386087
117.157194	3808.520515	23.391104
116.934485	3811.150026	23.396122
117.250355	3811.437398	23.401139
117.137703	3806.352300	23.406157
117.249966	3811.235780	23.411175
117.552747	3817.795229	23.416192
117.311980	3831.141679	23.421210
117.721619	3834.833882	23.426227
117.824814	3828.182652	23.431245
117.863138	3832.288869	23.436263
118.235931	3830.784504	23.441280
118.091669	3827.975641	23.446298
118.720069	3825.078179	23.451315
118.925669	3820.460760	23.456333
118.736344	3817.504105	23.461351
118.924317	3819.869878	23.466368
118.872208	3824.147068	23.471386
119.357956	3836.432841	23.476403
119.437936	3845.232952	23.481421
119.712559	3829.121063	23.486439
119.633772	3815.255717	23.491456
119.314674	3821.525708	23.496474
119.407847	3835.611116	23.501491
119.977085	3839.756971	23.506509
119.832966	3842.893963	23.511527
120.117063	3834.620026	23.516544
119.843536	3850.129635	23.521562
120.282785	3839.175840	23.526579
120.069382	3845.575313	23.531597
119.871820	3842.767867	23.536615
120.042241	3843.988647	23.541632
119.960758	3868.112703	23.546650
120.232546	3869.859358	23.551667
120.300967	3878.912290	23.556685
120.607208	3897.499905	23.561703
120.648129	3901.371291	23.566720
120.500360	3906.954739	23.571738
121.185336	3915.133684	23.576755
121.054155	3932.570919	23.581773
121.169954	3935.800222	23.586791
121.522826	3926.889050	23.591808
121.454434	3955.219244	23.596826
121.576819	3963.881284	23.601843
121.768148	3971.647290	23.606861
121.755069	3962.403460	23.611879
122.354910	3975.678928	23.616896
122.161743	3992.714671	23.621914
122.420983	3990.670622	23.626931
122.771019	3989.143909	23.631949
122.433745	3991.502998	23.636967
122.752640	3988.458971	23.641984
122.654261	4004.892729	23.647002
123.332822	4014.794859	23.652019
123.473920	4012.367639	23.657037
123.579200	4017.976860	23.662055
123.414655	4007.670709	23.667072
123.378546	4009.279244	23.672090
123.533067	4003.158646	23.677107
124.059142	4014.166030	23.682125
123.707014	4008.204107	23.687143
124.404639	3998.476382	23.692160
124.197689	4015.430958	23.697178
124.183513	4025.725992	23.702195
124.471962	4033.680301	23.707213
124.659266	4034.605750	23.712231
124.675356	4031.715420	23.717248
124.479209	4047.097249	23.722266
124.949104	4042.132372	23.727283
124.827745	4041.599704	23.732301
124.451371	4048.327349	23.737319
125.188053	4063.883780	23.742336
125.256924	4067.945070	23.747354
125.344416	4069.684164	23.752371
125.406888	4069.262215	23.757389
125.398854	4074.566188	23.762407
125.886475	4084.667958	23.767424
125.920312	4095.575315	23.772442
125.964572	4086.375760	23.777459
126.399505	4094.937688	23.782477
126.258371	4087.376526	23.787495
126.419987	4084.689553	23.792512
126.461780	4108.201948	23.797530
126.882411	4119.940564	23.802547
127.044226	4110.171548	23.807565
126.788313	4108.219859	23.812583
127.165013	4105.148497	23.817600
126.821139	4115.024927	23.822618
127.548060	4131.211572	23.827635
127.814555	4134.835422	23.832653
127.656895	4147.380615	23.837671
127.770669	4143.822498	23.842688
127.697018	4147.444735	23.847706
127.633454	4148.728815	23.852723
128.053687	4154.911732	23.857741
128.050284	4166.144486	23.862759
128.440330	4170.599084	23.867776
128.303160	4175.522461	23.872794
128.165069	4178.759262	23.877811
128.507885	4175.864006	23.882829
128.609688	4200.310253	23.887847
128.737760	4204.065548	23.892864
128.663371	4205.105116	23.897882
128.769450	4210.125817	23.902899
128.942933	4235.082286	23.907917
128.952092	4238.379012	23.912935
129.276673	4242.156477	23.917952
129.125329	4269.786946	23.922970
129.361373	4273.317345	23.927987
129.976246	4281.747628	23.933005
130.008720	4294.721286	23.938023
130.340277	4303.962243	23.943040
130.557049	4307.103148	23.948058
130.524165	4306.904094	23.953075
130.794676	4301.370655	23.958093
130.709366	4304.160074	23.963111
131.009384	4297.073657	23.968128
130.956400	4300.819298	23.973146
131.102980	4292.563890	23.978163
131.473578	4301.221951	23.983181
130.986510	4319.667543	23.988199
131.612247	4308.564871	23.993216
131.481840	4314.333731	23.998234
131.753727	4310.417577	24.003251
131.697912	4312.286546	24.008269
131.794023	4329.949198	24.013287
132.105228	4331.807634	24.018304
132.384031	4344.539867	24.023322
132.313076	4346.539492	24.028339
132.539767	4335.889862	24.033357
132.340153	4350.959442	24.038375
132.701303	4362.840695	24.043392
133.301390	4362.870344	24.048410
133.068275	4360.881943	24.053427
133.365813	4363.725186	24.058445
133.060410	4363.992847	24.063463
133.028336	4360.099188	24.068480
133.300430	4386.697826	24.073498
133.145058	4393.916706	24.078515
133.514585	4394.342656	24.083533
133.557548	4416.702797	24.088551
133.881968	4421.972763	24.093568
133.883940	4425.679777	24.098586
133.976492	4446.886575	24.103603
134.208313	4446.347924	24.108621
134.407140	4456.960963	24.113639
134.907190	4448.280125	24.118656
134.802070	4455.804142	24.123674
134.995621	4479.344066	24.128691
135.203721	4482.073356	24.133709
135.165517	4486.235230	24.138727
135.343501	4483.424419	24.143744
135.616076	4490.190392	24.148762
135.628030	4508.365468	24.153779
135.857363	4510.366794	24.158797
135.984959	4522.252376	24.163815
136.028125	4506.082251	24.168832
136.155264	4522.975480	24.173850
136.651280	4523.500849	24.178867
137.603822	4520.360395	24.183885
137.512667	4506.722951	24.188903
137.410386	4492.062177	24.193920
137.436941	4494.279933	24.198938
137.433015	4490.277115	24.203955
137.745534	4494.480620	24.208973
137.607367	4490.419748	24.213991
137.873091	4489.693954	24.219008
137.940132	4488.522293	24.224026
137.816533	4493.214671	24.229043
138.106496	4481.657969	24.234061
137.583456	4480.588271	24.239079
137.954492	4487.993106	24.244096
138.004947	4499.621121	24.249114
137.655514	4512.947749	24.254131
138.117925	4507.060285	24.259149
138.129336	4535.922503	24.264167
138.356103	4545.518620	24.269184
138.692854	4550.619092	24.274202
138.725305	4569.181196	24.279219
138.729080	4572.621255	24.284237
139.099158	4583.948973	24.289255
139.190466	4582.385573	24.294272
139.291210	4597.969242	24.299290
139.467758	4612.755671	24.304307
139.851825	4613.371276	24.309325
140.009616	4621.437215	24.314343
140.021233	4625.326839	24.319360
140.244225	4628.932573	24.324378
140.304409	4641.850980	24.329395
140.613866	4632.209919	24.334413
140.876078	4638.662130	24.339431
140.929209	4633.908277	24.344448
140.970348	4644.857360	24.349466
141.421775	4650.079621	24.354483
142.169220	4632.208620	24.359501
142.420173	4640.929232	24.364519
142.532885	4622.968277	24.369536
142.441558	4606.501644	24.374554
142.381091	4609.249395	24.379571
142.407152	4599.885633	24.384589
142.318557	4606.407931	24.389607
142.370040	4601.069016	24.394624
142.404236	4599.724781	24.399642
142.443538	4602.360639	24.404659
142.804334	4614.818836	24.409677
142.565833	4636.996824	24.414695
143.030760	4628.554359	24.419712
143.260568	4622.457691	24.424730
143.012967	4630.060375	24.429747
143.431183	4640.605521	24.434765
143.338554	4654.472729	24.439783
143.490942	4659.631747	24.444800
143.474881	4654.902295	24.449818
143.795932	4676.411288	24.454835
143.756340	4685.753367	24.459853
143.967561	4696.106551	24.464871
143.976058	4689.926346	24.469888
144.266056	4701.148127	24.474906
144.133514	4715.065027	24.479923
144.473826	4718.491580	24.484941
144.533799	4740.366437	24.489959
144.720502	4748.408954	24.494976
144.953311	4750.100568	24.499994
145.004199	4765.393399	24.505011
145.215441	4764.618060	24.510029
145.561626	4790.595096	24.515047
145.559665	4782.996435	24.520064
145.791579	4781.730802	24.525082
145.944122	4809.472746	24.530099
146.181471	4814.154087	24.535117
146.297581	4812.628406	24.540135
146.449696	4805.260073	24.545152
146.787998	4814.822847	24.550170
146.699685	4812.282596	24.555187
147.092580	4824.833409	24.560205
146.961980	4833.954854	24.565223
147.079341	4842.250800	24.570240
147.105261	4831.252040	24.575258
146.978319	4846.545775	24.580275
147.289688	4858.075035	24.585293
147.278438	4868.251391	24.590311
147.304430	4881.806437	24.595328
148.156718	4891.334507	24.600346
148.014179	4901.280845	24.605363
148.405416	4899.701844	24.610381
148.067511	4914.018305	24.615399
148.341330	4925.721185	24.620416
148.612240	4933.817251	24.625434
148.581860	4931.666627	24.630451
149.087475	4952.861001	24.635469
149.233080	4964.608746	24.640487
149.483083	4958.758123	24.645504
149.565416	4968.954243	24.650522
149.405955	4979.874193	24.655539
149.912464	4985.537033	24.660557
149.825354	4997.201537	24.665575
149.689182	4995.648404	24.670592
149.974311	5004.401548	24.675610
150.055807	5022.031955	24.680627
150.338108	5027.670768	24.685645
150.251088	5023.167300	24.690663
150.989868	5035.763059	24.695680
151.750626	5041.577351	24.700698
151.788148	5042.596772	24.705715
152.239211	5037.944558	24.710733
152.500301	5039.966859	24.715751
152.576593	5025.406897	24.720768
152.972823	4997.785249	24.725786
152.505428	4998.022886	24.730803
152.421618	4991.736113	24.735821
152.736438	4985.108840	24.740839
152.340984	4989.183055	24.745856
152.805770	4983.471263	24.750874
152.573642	4989.185009	24.755891
153.124431	5007.932513	24.760909
153.392386	5016.203757	24.765927
153.071507	5026.285615	24.770944
153.222841	5021.961287	24.775962
153.212761	5024.814374	24.780979
153.081591	5023.692373	24.785997
153.400702	5038.310947	24.791015
153.361479	5042.776044	24.796032
153.456156	5055.236923	24.801050
153.674638	5081.123900	24.806067
153.832963	5089.638468	24.811085
153.743252	5094.140741	24.816103
153.771874	5114.813463	24.821120
154.375162	5118.767799	24.826138
154.547661	5128.621570	24.831155
154.807339	5146.971931	24.836173
154.644969	5144.408813	24.841191
154.874146	5159.028472	24.846208
155.110816	5155.513460	24.851226
155.462178	5173.070332	24.856243
155.785317	5187.761582	24.861261
156.091993	5207.049437	24.866279
156.206782	5203.223404	24.871296
156.685210	5192.278107	24.876314
156.483077	5201.246748	24.881331
156.059208	5202.110799	24.886349
156.695641	5210.122771	24.891367
156.518136	5229.872592	24.896384
157.053263	5224.896141	24.901402
157.153098	5249.895182	24.906419
157.223111	5260.266558	24.911437
157.458575	5263.517986	24.916455
157.395982	5265.159203	24.921472
157.685595	5278.858257	24.926490
157.798359	5293.517855	24.931507
157.866350	5293.387673	24.936525
158.018675	5303.601188	24.941543
158.098645	5324.784502	24.946560
158.731842	5317.367531	24.951578
158.370333	5323.628389	24.956595
158.801650	5340.911502	24.961613
158.778987	5343.714729	24.966631
158.872765	5355.693708	24.971648
159.200711	5368.664469	24.976666
159.407274	5390.428793	24.981683
159.627319	5384.366416	24.986701
159.963104	5394.094406	24.991719
160.033189	5412.376194	24.996736
160.684670	5400.700554	25.001754
160.732741	5407.322576	25.006771
160.985051	5404.174800	25.011789
161.297453	5401.239317	25.016807
160.696736	5397.483262	25.021824
161.383134	5393.337082	25.026842
161.063309	5403.643260	25.031859
161.281864	5417.724348	25.036877
161.582976	5433.747447	25.041895
161.601588	5434.441034	25.046912
161.851835	5428.871072	25.051930
161.916058	5435.687227	25.056947
161.979984	5440.486116	25.061965
162.144981	5453.089541	25.066983
161.896982	5466.792666	25.072000
162.153993	5465.157906	25.077018
162.408910	5484.578689	25.082035
162.478116	5496.794590	25.087053
162.631668	5501.457255	25.092071
162.502460	5518.314605	25.097088
163.076031	5518.023555	25.102106
162.940133	5538.848988	25.107123
163.179832	5556.664879	25.112141
163.577836	5552.299493	25.117159
163.547221	5575.781707	25.122176
164.009721	5582.843635	25.127194
164.283511	5594.023833	25.132211
163.964832	5598.266146	25.137229
163.821639	5614.728504	25.142247
164.344535	5623.395324	25.147264
164.765805	5631.883228	25.152282
164.761494	5660.525907	25.157299
164.764642	5667.384953	25.162317
165.247030	5669.601802	25.167335
165.622441	5677.277201	25.172352
166.052589	5677.869775	25.177370
166.430062	5681.808346	25.182387
166.241564	5682.427963	25.187405
166.568132	5696.282020	25.192423
166.488645	5710.562761	25.197440
167.038660	5711.456452	25.202458
166.786898	5706.181228	25.207475
167.013203	5717.785309	25.212493
167.387853	5714.289867	25.217511
167.054491	5723.500837	25.222528
167.328315	5727.855641	25.227546
167.618870	5738.928632	25.232563
167.691760	5736.934522	25.237581
168.144650	5748.094935	25.242599
168.003548	5766.315630	25.247616
168.700776	5753.216964	25.252634
168.904222	5755.677364	25.257651
168.844007	5762.340415	25.262669
169.181995	5749.650734	25.267687
168.964193	5755.198046	25.272704
169.097908	5772.662873	25.277722
169.216879	5784.716076	25.282739
169.555698	5785.567914	25.287757
169.904690	5777.790043	25.292775
169.682952	5791.766234	25.297792
169.976360	5803.457247	25.302810
169.794514	5813.725970	25.307827
169.831118	5819.843302	25.312845
170.327988	5829.746532	25.317863
170.325085	5843.923921	25.322880
170.681985	5853.151587	25.327898
170.696050	5868.136705	25.332915
170.771252	5870.040842	25.337933
171.098977	5875.374540	25.342951
171.018041	5886.297584	25.347968
171.499997	5889.819853	25.352986
171.658624	5917.644732	25.358003
171.310447	5918.452689	25.363021
171.712823	5921.067086	25.368039
171.898402	5944.438303	25.373056
171.947430	5953.316994	25.378074
172.154079	5970.665779	25.383091
172.695911	5980.292851	25.388109
172.814832	5978.243374	25.393127
172.922033	5998.268266	25.398144
173.479960	5987.831372	25.403162
173.891478	5993.254039	25.408179
173.717933	5990.319603	25.413197
174.412334	5988.950232	25.418215
174.084254	5996.915000	25.423232
174.297912	5993.782707	25.428250
174.369893	6009.204071	25.433267
174.558346	6017.744269	25.438285
174.793367	6009.377816	25.443303
174.981878	6026.464402	25.448320
175.271605	6026.483763	25.453338
175.555073	6025.503292	25.458355
175.715172	6051.104644	25.463373
176.061448	6051.166919	25.468391
175.937036	6052.104435	25.473408
175.926872	6050.148704	25.478426
175.998597	6050.542729	25.483443
175.995485	6061.335470	25.488461
176.579192	6075.377061	25.493479
176.339178	6086.808722	25.498496
176.347290	6087.997350	25.503514
176.660465	6100.596584	25.508531
176.450105	6115.818375	25.513549
176.775180	6117.787350	25.518567
176.842391	6130.571389	25.523584
177.159395	6147.237921	25.528602
177.679745	6164.158454	25.533619
177.489596	6178.973446	25.538637
177.938085	6190.069591	25.543655
177.841484	6200.671191	25.548672
178.417622	6216.941626	25.553690
178.753560	6215.409867	25.558707
178.615568	6234.452871	25.563725
178.791518	6233.577655	25.568743
179.003294	6253.041732	25.573760
179.171855	6258.429273	25.578778
179.554467	6267.588579	25.583795
179.450792	6291.990000	25.588813
180.112681	6285.037721	25.593831
180.203116	6291.005822	25.598848
180.384760	6282.738999	25.603866
181.090699	6291.076462	25.608883
181.169051	6292.533232	25.613901
180.977228	6281.508317	25.618919
181.363933	6291.874769	25.623936
181.391859	6302.513239	25.628954
181.648253	6312.352849	25.633971
181.471153	6311.090146	25.638989
181.217983	6315.923353	25.644007
181.548901	6337.426897	25.649024
181.975005	6338.055555	25.654042
182.358594	6340.813868	25.659059
182.091362	6341.664804	25.664077
182.412488	6345.937501	25.669095
182.446726	6367.981737	25.674112
182.556930	6367.434090	25.679130
182.920775	6387.775024	25.684148
182.874182	6405.861045	25.689165
183.413995	6398.260154	25.694183
183.546355	6423.351194	25.699200
183.673299	6433.829191	25.704218
184.007159	6431.766627	25.709236
183.831547	6454.145021	25.714253
184.316203	6465.365435	25.719271
184.408056	6470.422222	25.724288
184.794001	6488.739953	25.729306
185.021341	6497.590539	25.734324
184.999124	6503.410663	25.739341
185.282539	6494.523203	25.744359
185.325071	6516.336971	25.749376
185.295728	6525.553465	25.754394
185.972347	6532.098592	25.759412
185.655322	6563.359552	25.764429
186.167807	6564.496128	25.769447
186.271180	6574.920543	25.774464
186.453081	6571.826242	25.779482
186.928535	6580.967007	25.784500
187.677433	6564.974037	25.789517
188.252418	6552.218351	25.794535
188.337467	6552.787305	25.799552
188.642645	6557.810110	25.804570
188.920508	6546.245086	25.809588
188.876346	6546.457744	25.814605
189.027115	6532.564266	25.819623
188.972017	6520.976811	25.824640
189.002579	6514.671942	25.829658
189.535643	6521.651472	25.834676
189.689171	6511.595792	25.839693
190.103686	6498.368058	25.844711
189.863274	6500.499637	25.849728
189.854965	6509.298889	25.854746
189.942799	6487.762664	25.859764
190.284523	6501.562343	25.864781
190.214061	6511.402661	25.869799
190.531681	6512.998344	25.874816
190.773047	6511.712967	25.879834
190.949789	6511.511933	25.884852
190.570928	6520.496166	25.889869
190.985371	6513.548616	25.894887
191.069711	6521.361353	25.899904
191.043417	6536.441706	25.904922
191.270962	6538.828368	25.909940
191.101643	6549.193168	25.914957
191.348743	6568.826708	25.919975
191.515849	6577.675143	25.924992
191.661328	6602.020825	25.930010
191.701988	6613.105202	25.935028
191.860087	6618.331666	25.940045
192.264450	6634.064995	25.945063
192.698588	6655.260623	25.950080
192.624943	6682.257647	25.955098
193.158914	6678.015829	25.960116
193.209547	6693.110829	25.965133
193.657783	6702.820182	25.970151
193.906441	6712.699849	25.975168
194.159710	6716.209211	25.980186
194.620310	6726.310823	25.985204
194.485531	6741.078988	25.990221
194.592378	6726.513277	25.995239
194.883776	6750.586504	26.000256
194.972004	6757.445864	26.005274
195.407766	6762.626536	26.010292
195.082009	6770.696781	26.015309
195.287698	6784.005382	26.020327
195.622518	6797.800929	26.025344
195.514022	6819.004621	26.030362
196.100398	6819.880004	26.035380
195.901099	6844.203152	26.040397
196.001017	6853.090004	26.045415
196.187360	6869.190397	26.050432
196.718854	6893.395537	26.055450
196.958713	6902.430069	26.060468
197.232124	6927.857494	26.065485
197.124253	6941.944864	26.070503
197.215305	6961.799732	26.075520
197.439681	6970.237968	26.080538
197.713753	6981.096557	26.085556
197.830877	7013.259446	26.090573
198.229031	7020.541636	26.095591
198.392779	7029.556905	26.100608
198.250361	7042.324790	26.105626
198.461359	7058.699222	26.110644
199.101515	7077.416225	26.115661
199.616657	7094.958710	26.120679
199.414196	7102.476763	26.125696
199.370883	7118.052212	26.130714
200.294147	7124.171929	26.135732
200.677761	7132.523494	26.140749
200.407471	7143.502827	26.145767
200.862229	7150.770548	26.150784
200.843190	7165.341271	26.155802
201.068336	7166.454466	26.160820
201.015626	7191.333160	26.165837
201.059432	7186.553226	26.170855
201.411702	7204.155644	26.175872
201.466584	7217.753854	26.180890
202.029850	7216.674407	26.185908
202.116501	7240.118516	26.190925
202.329705	7250.694287	26.195943
202.615768	7250.184669	26.200960
202.742319	7262.520353	26.205978
203.038790	7276.468032	26.210996
203.107415	7285.899146	26.216013
203.320754	7288.868915	26.221031
203.538922	7311.048892	26.226048
203.644879	7327.447449	26.231066
203.790676	7328.513504	26.236084
204.090052	7355.333452	26.241101
204.062073	7359.394563	26.246119
204.521553	7373.712935	26.251136
204.465262	7389.827394	26.256154
204.826945	7403.051481	26.261172
205.142146	7420.704130	26.266189
204.949622	7426.106780	26.271207
205.539520	7441.447841	26.276224
205.666235	7461.558148	26.281242
206.377511	7465.097359	26.286260
206.605701	7484.436496	26.291277
206.760819	7476.317247	26.296295
207.226460	7485.633255	26.301312
206.757620	7492.089959	26.306330
207.303951	7504.984498	26.311348
207.383550	7518.147036	26.316365
207.327895	7512.941013	26.321383
207.538259	7524.747348	26.326400
207.773272	7535.602734	26.331418
207.685470	7559.364735	26.336436
208.156187	7580.117155	26.341453
208.038304	7591.473048	26.346471
209.115338	7599.719833	26.351488
208.990451	7608.116933	26.356506
209.249118	7624.465108	26.361524
209.628340	7641.976794	26.366541
209.276773	7647.771182	26.371559
209.909812	7651.444095	26.376576
210.284315	7663.156305	26.381594
210.804389	7652.318651	26.386612
211.018313	7650.720828	26.391629
211.048408	7656.233251	26.396647
211.483448	7663.205347	26.401664
211.294566	7676.029967	26.406682
211.729126	7681.262305	26.411700
211.412319	7681.881601	26.416717
211.599938	7689.914163	26.421735
212.362674	7706.827721	26.426752
212.215930	7721.194290	26.431770
212.548274	7712.280999	26.436788
212.747721	7730.155492	26.441805
212.633514	7743.955045	26.446823
213.105975	7745.435686	26.451840
212.908932	7750.882846	26.456858
213.148958	7761.559363	26.461876
213.371464	7783.977392	26.466893
213.549445	7793.662875	26.471911
213.345497	7804.020291	26.476928
213.404557	7823.632347	26.481946
213.833120	7842.897511	26.486964
214.294207	7856.683747	26.491981
214.201377	7887.441546	26.496999
214.462764	7895.366061	26.502016
214.502003	7920.337148	26.507034
214.997931	7923.901756	26.512052
215.281940	7954.923431	26.517069
215.578678	7969.126284	26.522087
215.894365	7983.614143	26.527104
216.024737	8003.135193	26.532122
216.332049	8015.509569	26.537140
216.749978	8036.094376	26.542157
216.872588	8045.169936	26.547175
217.355850	8051.283470	26.552192
217.076081	8058.069501	26.557210
217.145072	8074.358306	26.562228
217.472538	8085.811187	26.567245
217.631573	8105.087788	26.572263
217.732168	8118.527259	26.577280
217.850022	8154.549214	26.582298
218.180724	8156.782769	26.587316
218.363571	8180.081598	26.592333
218.191547	8204.363650	26.597351
218.794692	8221.315827	26.602368
219.007393	8240.097329	26.607386
219.399291	8263.124518	26.612404
219.543006	8278.474229	26.617421
219.627516	8294.694303	26.622439
220.237625	8309.741874	26.627456
220.542075	8338.804367	26.632474
220.745888	8363.655128	26.637492
220.770740	8369.712425	26.642509
220.807705	8379.624587	26.647527
221.367024	8387.735588	26.652544
221.820436	8413.808106	26.657562
221.933763	8433.870703	26.662580
222.345425	8434.984952	26.667597
222.603867	8436.908997	26.672615
223.169228	8447.597881	26.677632
223.267718	8458.680702	26.682650
223.404467	8448.810545	26.687668
223.808936	8454.660591	26.692685
223.499885	8470.010676	26.697703
224.102612	8480.231296	26.702720
224.326401	8478.524003	26.707738
224.227160	8471.484717	26.712756
224.199924	8495.389638	26.717773
224.783540	8509.891559	26.722791
225.152894	8508.493935	26.727808
224.836030	8513.469023	26.732826
225.382648	8540.232008	26.737844
225.384293	8543.819302	26.742861
225.285805	8557.229916	26.747879
225.956583	8563.680881	26.752896
225.880798	8577.857531	26.757914
226.395877	8587.019191	26.762932
226.414278	8604.085881	26.767949
226.388762	8608.109558	26.772967
227.048840	8630.780172	26.777984
226.669689	8637.581518	26.783002
227.402944	8663.514244	26.788020
227.886150	8660.517070	26.793037
227.786872	8673.271200	26.798055
228.369567	8684.875476	26.803072
228.470988	8696.458510	26.808090
228.489868	8703.546233	26.813108
228.771234	8725.045384	26.818125
228.728467	8732.995619	26.823143
229.185302	8745.901176	26.828160
229.446177	8762.051143	26.833178
229.589684	8788.220544	26.838196
229.804602	8787.630150	26.843213
229.966591	8814.794911	26.848231
230.196032	8822.432263	26.853248
230.343782	8828.601969	26.858266
230.887855	8844.449540	26.863284
231.623842	8861.960476	26.868301
231.686592	8871.677619	26.873319
232.141738	8872.350567	26.878336
231.954783	8879.128857	26.883354
232.421369	8890.232012	26.888372
232.824161	8911.004589	26.893389
232.860332	8919.041889	26.898407
232.873794	8913.979787	26.903424
233.289399	8931.997535	26.908442
233.339677	8942.722067	26.913460
233.712352	8944.349775	26.918477
233.698410	8961.682514	26.923495
234.128370	8973.996816	26.928512
234.405100	8974.775729	26.933530
234.285281	8986.563456	26.938548
234.816858	8995.455955	26.943565
234.984081	9006.063124	26.948583
234.889240	9026.278138	26.953600
235.471406	9043.050445	26.958618
235.649435	9038.520031	26.963636
236.105742	9051.027334	26.968653
235.863140	9071.775138	26.973671
236.363819	9070.114142	26.978688
236.663487	9089.822888	26.983706
236.494374	9102.258377	26.988724
236.836057	9102.114047	26.993741
236.999633	9122.569733	26.998759
237.197799	9131.954600	27.003776
237.757439	9142.151461	27.008794
238.069736	9154.454372	27.013812
238.605813	9152.849895	27.018829
238.409341	9160.459306	27.023847
238.538414	9170.880649	27.028864
238.811846	9179.138395	27.033882
239.047860	9194.113892	27.038900
239.153814	9200.694137	27.043917
239.141331	9220.751478	27.048935
239.470866	9226.066822	27.053952
239.633116	9254.707541	27.058970
239.598234	9274.768131	27.063988
240.119158	9292.431907	27.069005
240.212104	9321.806256	27.074023
240.623081	9327.128327	27.079040
240.523382	9352.846794	27.084058
240.979242	9368.526010	27.089076
241.399067	9382.658249	27.094093
241.543644	9399.208741	27.099111
241.867554	9417.992484	27.104128
241.827660	9436.391955	27.109146
242.117392	9458.834038	27.114164
242.746349	9471.396805	27.119181
242.975078	9501.125256	27.124199
242.921355	9506.541934	27.129216
243.282555	9523.744293	27.134234
243.544801	9552.051687	27.139252
244.112512	9562.401409	27.144269
244.411158	9573.813986	27.149287
244.436551	9588.931272	27.154304
244.655566	9604.382484	27.159322
245.041554	9619.205428	27.164340
245.400911	9623.166053	27.169357
245.476069	9650.499632	27.174375
245.862206	9655.845063	27.179392
246.315483	9656.954746	27.184410
247.188966	9672.973407	27.189428
247.771260	9655.698098	27.194445
247.731087	9667.114784	27.199463
247.901263	9664.017396	27.204480
247.805627	9676.785172	27.209498
247.921032	9669.673723	27.214516
248.454401	9656.805586	27.219533
248.371040	9673.188487	27.224551
248.573422	9695.957685	27.229568
248.677039	9699.301160	27.234586
248.958469	9701.643939	27.239604
249.301202	9718.468553	27.244621
249.233468	9730.302074	27.249639
249.808337	9735.395511	27.254656
249.596789	9749.781427	27.259674
249.736608	9759.362904	27.264692
249.731008	9768.374555	27.269709
249.882124	9792.925999	27.274727
250.380590	9810.122348	27.279744
250.821010	9822.715074	27.284762
250.955124	9840.325074	27.289780
251.083018	9855.635635	27.294797
251.264451	9871.894690	27.299815
251.425661	9889.793199	27.304832
251.414543	9915.804261	27.309850
251.483126	9933.359887	27.314868
252.616138	9940.630255	27.319885
252.968837	9953.476723	27.324903
253.788418	9971.631621	27.329920
254.265599	9972.353845	27.334938
254.019453	9982.380665	27.339956
254.477103	9975.054356	27.344973
254.565995	9987.141323	27.349991
254.819094	9998.490259	27.355008
254.866729	10010.146628	27.360026
254.840101	10018.932756	27.365044
255.205040	10037.307777	27.370061
255.191375	10049.900280	27.375079
255.619649	10057.471150	27.380096
256.011090	10067.783999	27.385114
255.621547	10090.207023	27.390132
256.130232	10099.975076	27.395149
256.479668	10130.121541	27.400167
256.577061	10137.970288	27.405184
256.766230	10170.903685	27.410202
256.822643	10189.009718	27.415220
257.439283	10206.763990	27.420237
257.684752	10235.235505	27.425255
257.798666	10257.545464	27.430272
258.106200	10273.434619	27.435290
258.163996	10298.701833	27.440308
258.849189	10305.161105	27.445325
258.999427	10344.635888	27.450343
259.198822	10358.380364	27.455360
259.342952	10368.233858	27.460378
259.644858	10396.358644	27.465396
259.895154	10409.500440	27.470413
260.043887	10444.469490	27.475431
260.340264	10463.078300	27.480448
260.787499	10478.970981	27.485466
261.003096	10504.580150	27.490484
261.414550	10516.065972	27.495501
261.531719	10536.535696	27.500519
261.964473	10553.394117	27.505536
262.524157	10582.815363	27.510554
262.400730	10606.821603	27.515572
262.887642	10600.869254	27.520589
263.419066	10616.956443	27.525607
263.233215	10628.784702	27.530624
264.073052	10638.562890	27.535642
264.218257	10645.560947	27.540660
264.330921	10654.347670	27.545677
264.629643	10677.440247	27.550695
264.605560	10682.983666	27.555712
264.996161	10699.546936	27.560730
265.011852	10717.028868	27.565748
265.257024	10719.437800	27.570765
265.761298	10742.118148	27.575783
265.846262	10749.677785	27.580800
266.144813	10771.184599	27.585818
266.046419	10786.878287	27.590836
266.568784	10806.837913	27.595853
266.922237	10823.536123	27.600871
266.866909	10856.055848	27.605888
267.371118	10860.331761	27.610906
267.481092	10884.922233	27.615924
268.066106	10901.303419	27.620941
268.921218	10902.794631	27.625959
269.301197	10905.231296	27.630976
270.180697	10903.725780	27.635994
270.242471	10911.865725	27.641012
270.671703	10911.887870	27.646029
270.524671	10919.809831	27.651047
270.723249	10917.539008	27.656064
271.283073	10914.095714	27.661082
270.966382	10910.618984	27.666100
272.014142	10897.961976	27.671117
272.298830	10897.295059	27.676135
272.144363	10904.752251	27.681152
272.649537	10907.595947	27.686170
272.879506	10923.802553	27.691188
273.116324	10925.311652	27.696205
273.127447	10927.501537	27.701223
273.153086	10926.827705	27.706240
273.451576	10926.851014	27.711258
272.959918	10950.249254	27.716276
273.343425	10959.700759	27.721293
273.328606	10984.532061	27.726311
273.450049	11006.565268	27.731328
273.990711	11029.704822	27.736346
274.198852	11058.622636	27.741364
274.561370	11073.959604	27.746381
274.903211	11094.090457	27.751399
275.007605	11121.592833	27.756416
275.469340	11134.723596	27.761434
275.542672	11160.534828	27.766452
276.045597	11180.999817	27.771469
276.217362	11195.914741	27.776487
276.653865	11220.127855	27.781504
277.350838	11222.461113	27.786522
277.430555	11249.708112	27.791540
278.091905	11253.563185	27.796557
278.147640	11270.241460	27.801575
278.392048	11283.719273	27.806592
278.700900	11279.169703	27.811610
278.658275	11310.953235	27.816628
279.047577	11331.399941	27.821645
279.310127	11327.266632	27.826663
279.292095	11347.090565	27.831680
279.544019	11353.504247	27.836698
279.787533	11386.854692	27.841716
280.290088	11392.475779	27.846733
280.493055	11418.139079	27.851751
280.386606	11438.616545	27.856768
280.857460	11449.686880	27.861786
281.248179	11477.254847	27.866804
281.451395	11491.434029	27.871821
281.621996	11512.444379	27.876839
282.131475	11526.100151	27.881856
282.667458	11536.633399	27.886874
283.030167	11561.592994	27.891892
283.465081	11572.818698	27.896909
283.855164	11589.634509	27.901927
284.004765	11603.583848	27.906944
284.337413	11609.289953	27.911962
284.205209	11626.817760	27.916980
284.100092	11641.569461	27.921997
284.573936	11649.365088	27.927015
284.985513	11677.440340	27.932032
285.257750	11696.915029	27.937050
285.288042	11726.225716	27.942068
286.085228	11744.671859	27.947085
286.257172	11763.039799	27.952103
286.194502	11782.604778	27.957120
286.676328	11788.191931	27.962138
287.043856	11816.360257	27.967156
287.110977	11825.670090	27.972173
287.656571	11850.681493	27.977191
287.682810	11883.667017	27.982208
288.322084	11889.569345	27.987226
288.412642	11905.957435	27.992244
288.710504	11934.143184	27.997261
289.175557	11948.493384	28.002279
289.631694	11959.688641	28.007296
290.348659	11970.721507	28.012314
290.502578	11997.891705	28.017332
290.467577	11995.899408	28.022349
291.048863	12003.270361	28.027367
291.290444	12016.747113	28.032384
291.380968	12031.956224	28.037402
291.466144	12058.354489	28.042420
291.859423	12070.364887	28.047437
292.290280	12088.398940	28.052455
292.166134	12103.581928	28.057472
292.399500	12121.483776	28.062490
292.722141	12140.533228	28.067508
292.755811	12157.941537	28.072525
293.342458	12173.252751	28.077543
293.430677	12203.067353	28.082560
293.980652	12208.517858	28.087578
294.354665	12230.596019	28.092596
294.696961	12246.414014	28.097613
295.041089	12260.692084	28.102631
295.145012	12277.207732	28.107648
295.755304	12277.695552	28.112666
296.148228	12295.819533	28.117684
296.159315	12311.644833	28.122701
296.505693	12311.408534	28.127719
296.526321	12331.295773	28.132736
297.100212	12338.184270	28.137754
297.671992	12368.026416	28.142772
298.000245	12371.801556	28.147789
298.263860	12376.603995	28.152807
298.349998	12397.231915	28.157824
298.468812	12412.794067	28.162842
298.552446	12431.043468	28.167860
298.765464	12447.696882	28.172877
299.243495	12467.127753	28.177895
299.417936	12483.591354	28.182912
299.763634	12510.940593	28.187930
300.553063	12521.519934	28.192948
301.192678	12530.086100	28.197965
301.370229	12533.817409	28.202983
301.433558	12548.885256	28.208000
302.108747	12560.965149	28.213018
302.297394	12568.255209	28.218036
301.777723	12593.815666	28.223053
302.291177	12599.716587	28.228071
302.402998	12627.732156	28.233088
302.588865	12641.088166	28.238106
302.893486	12663.403047	28.243124
303.174538	12680.690165	28.248141
303.715255	12697.761483	28.253159
303.422582	12730.615574	28.258176
304.169206	12753.614634	28.263194
304.818987	12772.113770	28.268212
304.901341	12789.839452	28.273229
305.238920	12816.550369	28.278247
305.394692	12842.176265	28.283264
305.764961	12856.397693	28.288282
305.929538	12883.498008	28.293300
306.194017	12899.978900	28.298317
307.132189	12928.468253	28.303335
306.875119	12948.110187	28.308352
307.571750	12966.636237	28.313370
308.238923	12982.266346	28.318388
308.506826	12997.271329	28.323405
308.797020	13006.897804	28.328423
309.286855	13025.785141	28.333440
309.817500	13029.758144	28.338458
310.014625	13053.234308	28.343476
310.178416	13061.781468	28.348493
310.683811	13058.336546	28.353511
310.667517	13074.908329	28.358528
310.778278	13087.256610	28.363546
311.069949	13102.060619	28.368564
311.119324	13124.080436	28.373581
311.579949	13137.234469	28.378599
311.471174	13156.881471	28.383616
311.768768	13170.740764	28.388634
311.915293	13193.104153	28.393652
312.189841	13214.102941	28.398669
312.800238	13225.663028	28.403687
312.846131	13255.427491	28.408704
313.055911	13275.787745	28.413722
313.626800	13306.470925	28.418740
313.564707	13334.404417	28.423757
314.079203	13361.638341	28.428775
314.341051	13383.982348	28.433792
315.000927	13405.782756	28.438810
315.433355	13440.692126	28.443828
315.253203	13466.619596	28.448845
315.839658	13471.879954	28.453863
315.895306	13501.066318	28.458880
316.164958	13528.261213	28.463898
316.568735	13554.728381	28.468916
316.717877	13579.309681	28.473933
317.477736	13594.101932	28.478951
317.676548	13626.153698	28.483968
318.242033	13649.003895	28.488986
318.686111	13665.042225	28.494004
318.777063	13697.538199	28.499021
319.411528	13714.041690	28.504039
319.896069	13736.071846	28.509056
320.652588	13736.196049	28.514074
321.262077	13739.929466	28.519092
321.430714	13746.712475	28.524109
321.517219	13752.611246	28.529127
321.922440	13771.976766	28.534144
322.245595	13769.368620	28.539162
322.368112	13789.850332	28.544180
322.341204	13804.599131	28.549197
322.876444	13813.419324	28.554215
322.956009	13839.712334	28.559232
323.004427	13858.868554	28.564250
323.157238	13868.024079	28.569268
323.321416	13898.853176	28.574285
324.194943	13922.991103	28.579303
324.193900	13941.766813	28.584320
324.712009	13960.502510	28.589338
325.124148	13981.749459	28.594356
325.755276	14004.589924	28.599373
326.477768	14013.719391	28.604391
326.257597	14031.730209	28.609408
326.958448	14048.340486	28.614426
327.174668	14057.126744	28.619444
326.972519	14080.552791	28.624461
327.469680	14101.408877	28.629479
327.638100	14118.411407	28.634496
328.359835	14132.407968	28.639514
328.359551	14143.242636	28.644532
328.278878	14173.390789	28.649549
329.161881	14188.776370	28.654567
329.490445	14207.017292	28.659584
329.437722	14226.920357	28.664602
329.871435	14238.963618	28.669620
329.918762	14254.837995	28.674637
330.360243	14268.698675	28.679655
330.636654	14300.517481	28.684672
331.161164	14313.915746	28.689690
331.528309	14335.449536	28.694708
331.589389	14354.566667	28.699725
332.017494	14376.353445	28.704743
332.298691	14402.160843	28.709760
332.434860	14423.583861	28.714778
333.024460	14446.421962	28.719796
333.119668	14471.250744	28.724813
333.854914	14491.371415	28.729831
333.799631	14515.769515	28.734848
334.457240	14534.362346	28.739866
334.907708	14563.031391	28.744884
334.939940	14586.961209	28.749901
335.558345	14607.541719	28.754919
335.741223	14632.909054	28.759936
335.987473	14662.901061	28.764954
336.481565	14677.964148	28.769972
336.712647	14710.563927	28.774989
337.034557	14732.742482	28.780007
337.244690	14763.126006	28.785024
337.522007	14783.715846	28.790042
337.881824	14799.710442	28.795060
338.667314	14825.865668	28.800077
339.013272	14844.957884	28.805095
339.405112	14860.601039	28.810112
340.187949	14880.911065	28.815130
340.942263	14891.959407	28.820148
341.021605	14907.495353	28.825165
341.215025	14902.700958	28.830183
341.967327	14919.893756	28.835200
342.411292	14926.964853	28.840218
342.832308	14925.585610	28.845236
342.811453	14936.098772	28.850253
342.870814	14952.270920	28.855271
343.161758	14965.199974	28.860288
343.199289	14974.931338	28.865306
343.632036	15005.179680	28.870324
344.131106	15022.623551	28.875341
344.447248	15028.868934	28.880359
344.338603	15052.604834	28.885376
344.550716	15078.773146	28.890394
344.763119	15101.414013	28.895412
345.166263	15137.005145	28.900429
345.388522	15155.211488	28.905447
345.648038	15183.040889	28.910464
345.874678	15217.458142	28.915482
346.260806	15242.403296	28.920500
346.498890	15259.484361	28.925517
347.069111	15286.464144	28.930535
347.259466	15316.582657	28.935552
347.748733	15339.020910	28.940570
348.417668	15343.647012	28.945588
348.442606	15374.313784	28.950605
348.789758	15400.898665	28.955623
349.244823	15416.503968	28.960640
349.468439	15449.337378	28.965658
349.966860	15480.149542	28.970676
350.103161	15493.991573	28.975693
350.949562	15524.919215	28.980711
351.148346	15551.538630	28.985728
350.920631	15574.745552	28.990746
351.807592	15591.158283	28.995764
351.873013	15622.239717	29.000781
352.044861	15643.978495	29.005799
352.631203	15679.915267	29.010816
352.847483	15708.436882	29.015834
353.497601	15739.760373	29.020852
353.653266	15771.201110	29.025869
354.204004	15790.697058	29.030887
354.523034	15827.185779	29.035904
354.887163	15845.981292	29.040922
355.772332	15866.384576	29.045940
356.426075	15881.124122	29.050957
356.857800	15892.609607	29.055975
357.522586	15899.888266	29.060992
357.512057	15911.426531	29.066010
358.159254	15934.242023	29.071028
358.235361	15936.788574	29.076045
358.632606	15951.740311	29.081063
358.833401	15963.598449	29.086080
358.946787	15983.150957	29.091098
359.613659	15986.665480	29.096116
359.882681	16010.635353	29.101133
360.000228	16027.587870	29.106151
360.554634	16053.300368	29.111168
360.420482	16068.732935	29.116186
360.963809	16089.619307	29.121204
361.303888	16118.326068	29.126221
361.514698	16133.544288	29.131239
362.003259	16162.692196	29.136256
362.000242	16191.255360	29.141274
362.554183	16209.039447	29.146292
362.700056	16238.660782	29.151309
363.180536	16268.324904	29.156327
363.752535	16293.958036	29.161344
363.919654	16318.562892	29.166362
364.363585	16343.708085	29.171380
364.811792	16374.725894	29.176397
365.111380	16387.602605	29.181415
365.604233	16417.678797	29.186432
365.862104	16441.888110	29.191450
366.352691	16442.669577	29.196468
366.813887	16471.311631	29.201485
366.866148	16485.909045	29.206503
367.278744	16510.991397	29.211520
367.462792	16531.569502	29.216538
367.987033	16553.627989	29.221556
368.036751	16575.786143	29.226573
368.593032	16604.268022	29.231591
368.752023	16633.170338	29.236608
368.982119	16661.799182	29.241626
369.762445	16681.858071	29.246644
369.773306	16711.014050	29.251661
369.978763	16740.539057	29.256679
370.643616	16768.195699	29.261696
370.824425	16797.395620	29.266714
371.252232	16834.653213	29.271732
371.547650	16856.957647	29.276749
372.272508	16889.441015	29.281767
372.760136	16913.271153	29.286784
373.271724	16940.327348	29.291802
373.629256	16958.081595	29.296820
374.173359	16976.024628	29.301837
374.327826	17008.704261	29.306855
374.649852	17021.585208	29.311872
374.851776	17054.622722	29.316890
375.405387	17072.991117	29.321908
375.635207	17101.439718	29.326925
376.211155	17127.348205	29.331943
376.729087	17153.460862	29.336960
377.050355	17183.558012	29.341978
377.658419	17203.434405	29.346996
377.965407	17223.054081	29.352013
378.357707	17253.002253	29.357031
378.544809	17262.801770	29.362048
378.801606	17296.707822	29.367066
379.216501	17311.571450	29.372084
379.534967	17346.541403	29.377101
379.886220	17375.070761	29.382119
380.518222	17390.197112	29.387136
380.453412	17429.625196	29.392154
380.906925	17457.632106	29.397172
381.338213	17482.873685	29.402189
381.711175	17519.902293	29.407207
382.026495	17537.412746	29.412224
382.245427	17566.935995	29.417242
382.642748	17597.325376	29.422260
383.024844	17624.225445	29.427277
383.250778	17665.995634	29.432295
383.956060	17691.178534	29.437312
384.043753	17731.783108	29.442330
384.642889	17753.499472	29.447348
385.125015	17782.031556	29.452365
385.164255	17828.106462	29.457383
385.993736	17845.486901	29.462400
386.312922	17886.805406	29.467418
386.867985	17901.194098	29.472436
387.265282	17929.789580	29.477453
387.075853	17951.725195	29.482471
387.841892	17967.035877	29.487488
387.870782	18002.853090	29.492506
388.132966	18024.303436	29.497524
388.833572	18059.699944	29.502541
389.135626	18091.778778	29.507559
389.758962	18112.073216	29.512576
390.030294	18142.523504	29.517594
390.329596	18162.716487	29.522612
390.686143	18198.713049	29.527629
391.361968	18226.585520	29.532647
391.674114	18247.088394	29.537664
391.373325	18288.876861	29.542682
392.185882	18311.575413	29.547700
392.536561	18342.264250	29.552717
393.069107	18389.573705	29.557735
393.584971	18415.216734	29.562752
393.876430	18450.394271	29.567770
394.161568	18471.677391	29.572788
394.423268	18508.088629	29.577805
394.762537	18538.776915	29.582823
395.801237	18573.439167	29.587840
395.987401	18608.171991	29.592858
396.278511	18632.768034	29.597876
397.041279	18664.236002	29.602893
397.391490	18691.947790	29.607911
397.893179	18708.825874	29.612928
397.817160	18751.638905	29.617946
398.337779	18768.871945	29.622964
398.934116	18796.166316	29.627981
399.487462	18825.591804	29.632999
400.164570	18839.854036	29.638016
400.298061	18871.009272	29.643034
400.563103	18893.728988	29.648052
401.385140	18921.300243	29.653069
401.603540	18943.650653	29.658087
401.977003	18962.715417	29.663104
402.152116	18993.820166	29.668122
402.540736	19009.689321	29.673140
403.057182	19043.775536	29.678157
403.371020	19077.819300	29.683175
404.088644	19099.296593	29.688192
404.217850	19131.390537	29.693210
404.438531	19150.292847	29.698228
405.048813	19178.740918	29.703245
405.036803	19217.848918	29.708263
405.630360	19242.606020	29.713280
406.033054	19277.321969	29.718298
406.424414	19305.737038	29.723316
407.042457	19330.471084	29.728333
407.074617	19361.344191	29.733351
407.702342	19384.387191	29.738368
408.032046	19424.681575	29.743386
408.277167	19444.248151	29.748404
409.042499	19462.672264	29.753421
409.593948	19492.568273	29.758439
410.139974	19514.621590	29.763456
410.423378	19531.790897	29.768474
411.010979	19550.164290	29.773492
411.572175	19560.980600	29.778509
411.822065	19588.159491	29.783527
412.251627	19606.290378	29.788544
412.265125	19625.902751	29.793562
412.481045	19649.568143	29.798580
412.618900	19680.311633	29.803597
413.192564	19707.461977	29.808615
413.968542	19735.746844	29.813632
414.324059	19767.845800	29.818650
414.577464	19802.062209	29.823668
415.169273	19823.356580	29.828685
415.323907	19860.190056	29.833703
415.917086	19884.357197	29.838720
416.190742	19914.461295	29.843738
416.529202	19947.702106	29.848756
417.319005	19958.776803	29.853773
417.544611	20004.849680	29.858791
418.035171	20028.822335	29.863808
418.284590	20066.002670	29.868826
418.857590	20094.814317	29.873844
419.225880	20127.970427	29.878861
419.295480	20166.994937	29.883879
419.664673	20191.989724	29.888896
419.915833	20230.242018	29.893914
420.377051	20265.940778	29.898932
420.911942	20308.024366	29.903949
421.009198	20338.511782	29.908967
421.878060	20373.182654	29.913984
422.086991	20416.731345	29.919002
422.504799	20460.137402	29.924020
423.411905	20485.687230	29.929037
423.225425	20530.267938	29.934055
424.241533	20557.492197	29.939072
424.579647	20600.556937	29.944090
424.906777	20642.348472	29.949108
426.201788	20649.241512	29.954125
426.291050	20691.849198	29.959143
426.894855	20716.056094	29.964160
426.902894	20748.269911	29.969178
427.454381	20772.663222	29.974196
427.988259	20785.433982	29.979213
428.158808	20838.959079	29.984231
428.421959	20859.688191	29.989248
429.111687	20897.691082	29.994266
429.185994	20932.066074	29.999284
430.065077	20955.041015	30.004301
430.242813	20984.706434	30.009319
430.816472	21011.364826	30.014336
430.917181	21038.488479	30.019354
431.615441	21068.525554	30.024372
432.482785	21087.066860	30.029389
432.365871	21110.261372	30.034407
432.930456	21136.471709	30.039424
433.549469	21164.871590	30.044442
433.637368	21195.341676	30.049460
434.174285	21216.520671	30.054477
434.336204	21252.241792	30.059495
435.198890	21271.070743	30.064512
435.524420	21301.118034	30.069530
435.849996	21324.916542	30.074548
436.283469	21351.455292	30.079565
436.404066	21387.380990	30.084583
436.901619	21411.989452	30.089600
437.374498	21446.799037	30.094618
437.798860	21473.554460	30.099636
438.633861	21509.648571	30.104653
438.587037	21544.043407	30.109671
439.360578	21570.073100	30.114688
439.537271	21595.160646	30.119706
439.992456	21645.052384	30.124724
440.586453	21671.240809	30.129741
440.639973	21712.407722	30.134759
441.139371	21742.280076	30.139776
441.650517	21772.891769	30.144794
442.127964	21817.491610	30.149812
442.644052	21851.744652	30.154829
442.870598	21889.051859	30.159847
442.943980	21927.316900	30.164864
443.625490	21969.237426	30.169882
444.031296	22017.343188	30.174900
445.020037	22043.640253	30.179917
445.303852	22091.202516	30.184935
445.743248	22123.028257	30.189952
446.267820	22161.753633	30.194970
446.934143	22188.398465	30.199988
447.500820	22217.098434	30.205005
447.877291	22247.255977	30.210023
448.353222	22276.266668	30.215040
448.896528	22308.870177	30.220058
449.107834	22341.477028	30.225076
450.086149	22365.707919	30.230093
450.334404	22399.189598	30.235111
450.315782	22422.368004	30.240128
450.692623	22456.921797	30.245146
451.133512	22498.255874	30.250164
451.834566	22537.204526	30.255181
452.116362	22571.781589	30.260199
452.314717	22606.099490	30.265216
452.689909	22645.014470	30.270234
452.922664	22689.628971	30.275252
453.720455	22727.868742	30.280269
454.216911	22762.894074	30.285287
454.691497	22802.011788	30.290304
455.508063	22831.596211	30.295322
455.564415	22863.541181	30.300340
456.700063	22882.451454	30.305357
457.202263	22907.556166	30.310375
457.895053	22935.591447	30.315392
457.989125	22948.085096	30.320410
457.983522	22988.618049	30.325428
458.981417	23006.768248	30.330445
459.520785	23034.899829	30.335463
459.609239	23060.235330	30.340480
460.009081	23084.083727	30.345498
460.318612	23118.693795	30.350516
460.793689	23144.741344	30.355533
461.101979	23188.651254	30.360551
461.261302	23219.709343	30.365568
461.875879	23261.216233	30.370586
462.360029	23297.013497	30.375604
463.215507	23336.315241	30.380621
463.543477	23358.448859	30.385639
463.698393	23394.954167	30.390656
464.259697	23426.962390	30.395674
464.798365	23466.077043	30.400692
465.603955	23491.992157	30.405709
465.862430	23539.085437	30.410727
466.439561	23574.321840	30.415744
467.020034	23598.317890	30.420762
467.280690	23640.256321	30.425780
467.355320	23671.712402	30.430797
467.882944	23713.983445	30.435815
468.189149	23762.933527	30.440832
468.716927	23799.413439	30.445850
468.821076	23847.333331	30.450868
469.387448	23895.185238	30.455885
470.182575	23932.669753	30.460903
470.412879	23986.614221	30.465920
471.442924	24016.149514	30.470938
471.774818	24060.183312	30.475956
472.578670	24088.799252	30.480973
473.108206	24123.261439	30.485991
473.708582	24159.796780	30.491008
474.292993	24181.584255	30.496026
474.471751	24221.543482	30.501044
475.244862	24251.641634	30.506061
475.138806	24299.745255	30.511079
475.913613	24325.424795	30.516096
476.483916	24369.221373	30.521114
476.525153	24405.543073	30.526132
476.961124	24437.778898	30.531149
477.608813	24483.007415	30.536167
477.882647	24513.050110	30.541184
478.283634	24553.794819	30.546202
478.537914	24596.776618	30.551220
479.184280	24639.078459	30.556237
479.633419	24685.372729	30.561255
479.833217	24736.116005	30.566272
480.703187	24769.091608	30.571290
481.144642	24813.437736	30.576308
481.718098	24845.075041	30.581325
482.215534	24873.838104	30.586343
482.409332	24921.317588	30.591360
482.605231	24957.577295	30.596378
483.053414	25003.485048	30.601396
484.104246	25037.529772	30.606413
484.714589	25078.821484	30.611431
484.691630	25119.695044	30.616448
485.544577	25144.514217	30.621466
485.937950	25194.360746	30.626484
486.322897	25231.013211	30.631501
486.672020	25286.094091	30.636519
487.084660	25322.825071	30.641536
487.767692	25354.763408	30.646554
488.227938	25412.092731	30.651572
488.539583	25459.677928	30.656589
489.354444	25496.498849	30.661607
490.036430	25540.547903	30.666624
490.504583	25576.638797	30.671642
491.117770	25622.941150	30.676660
491.789101	25659.658474	30.681677
492.116026	25697.707014	30.686695
492.548384	25725.607496	30.691712
493.041320	25755.687729	30.696730
493.851966	25797.701749	30.701748
494.252734	25829.582796	30.706765
494.888224	25860.667049	30.711783
495.286324	25900.922459	30.716800
495.759726	25930.326235	30.721818
496.461765	25970.008704	30.726836
496.851653	26004.787109	30.731853
497.288788	26042.165794	30.736871
497.462057	26081.222936	30.741888
498.476894	26108.163094	30.746906
498.711797	26145.950823	30.751924
499.656500	26177.782935	30.756941
499.931520	26205.483994	30.761959
500.421276	26252.789476	30.766976
500.922229	26282.516463	30.771994
501.103489	26321.219959	30.777012
501.690559	26353.385928	30.782029
502.309116	26393.490059	30.787047
502.800619	26428.890564	30.792064
503.157158	26461.060384	30.797082
503.272620	26501.166144	30.802100
504.257204	26541.245423	30.807117
504.747165	26574.048135	30.812135
505.158214	26621.935286	30.817152
506.229963	26636.305594	30.822170
506.763924	26674.169037	30.827188
507.597282	26696.120397	30.832205
508.205821	26726.096575	30.837223
509.008713	26749.708960	30.842240
509.153614	26769.948543	30.847258
508.936483	26798.370349	30.852276
509.728309	26817.117129	30.857293
510.215226	26839.724233	30.862311
510.254394	26874.260207	30.867328
510.700945	26903.006648	30.872346
510.889776	26939.535882	30.877364
511.332064	26970.416695	30.882381
511.908139	27013.130714	30.887399
512.404872	27051.792007	30.892416
512.793213	27091.463395	30.897434
513.060774	27144.111718	30.902452
513.690976	27182.110720	30.907469
514.081356	27224.881668	30.912487
514.078336	27288.098222	30.917504
514.886986	27325.917859	30.922522
515.350850	27389.667114	30.927540
515.879918	27438.711853	30.932557
516.558575	27491.113021	30.937575
517.121358	27539.782379	30.942592
517.841468	27583.795492	30.947610
518.582437	27622.797438	30.952628
519.027840	27660.128912	30.957645
519.839320	27709.165726	30.962663
519.962693	27762.043881	30.967680
520.841961	27796.180097	30.972698
521.410566	27834.820780	30.977716
521.872923	27877.394459	30.982733
522.798661	27920.904554	30.987751
523.031148	27954.386151	30.992768
524.102018	27982.677339	30.997786
524.314720	28025.116255	31.002804
525.418699	28057.669732	31.007821
526.331419	28082.606061	31.012839
526.106753	28120.549613	31.017856
526.486541	28147.274452	31.022874
526.899169	28182.366731	31.027892
527.540893	28217.852807	31.032909
528.147902	28253.382312	31.037927
528.130399	28302.067602	31.042944
529.144223	28338.325161	31.047962
529.786053	28373.666579	31.052980
529.708373	28422.631293	31.057997
530.522736	28453.181457	31.063015
530.928440	28503.731991	31.068032
531.612229	28536.112253	31.073050
531.907728	28588.543332	31.078068
532.267089	28629.550018	31.083085
532.927927	28667.033872	31.088103
533.367294	28716.679853	31.093120
533.770435	28753.814127	31.098138
534.033000	28807.302302	31.103156
534.586688	28863.067215	31.108173
535.205039	28914.856936	31.113191
535.767287	28958.897349	31.118208
537.102105	28988.137950	31.123226
537.610255	29023.254650	31.128244
538.065212	29063.528564	31.133261
538.757514	29085.541895	31.138279
539.205113	29127.692536	31.143296
539.675175	29157.455729	31.148314
540.102641	29202.288919	31.153332
540.513228	29225.701078	31.158349
541.584954	29263.423444	31.163367
542.006263	29303.990140	31.168384
542.491458	29341.142626	31.173402
542.629423	29362.675702	31.178420
542.910246	29402.754401	31.183437
543.908470	29439.322649	31.188455
544.382739	29477.580384	31.193472
544.680310	29516.406925	31.198490
545.118801	29552.601241	31.203508
545.396989	29604.719987	31.208525
546.658841	29645.095329	31.213543
547.009358	29688.433863	31.218560
547.415781	29724.372048	31.223578
548.192263	29768.577526	31.228596
548.643606	29820.568513	31.233613
549.195828	29855.771395	31.238631
549.461612	29899.486473	31.243648
550.254160	29931.737138	31.248666
550.956151	29989.881018	31.253684
551.168116	30036.602683	31.258701
552.080210	30072.656518	31.263719
552.119295	30130.228783	31.268736
552.970750	30169.729886	31.273754
553.613503	30218.079299	31.278772
553.886719	30271.576869	31.283789
554.646311	30328.444034	31.288807
555.151447	30371.327899	31.293824
555.771816	30410.934166	31.298842
556.211996	30457.615950	31.303860
556.481296	30507.162065	31.308877
557.114873	30545.939101	31.313895
557.837529	30601.281123	31.318912
558.277020	30649.635814	31.323930
558.817104	30701.438933	31.328948
559.149754	30747.780891	31.333965
560.036931	30800.025514	31.338983
560.395990	30847.797823	31.344000
560.934103	30898.889467	31.349018
561.831816	30943.849540	31.354036
562.738872	30994.454005	31.359053
563.397717	31033.959502	31.364071
564.327929	31077.329158	31.369088
564.881896	31116.794818	31.374106
565.764956	31143.174876	31.379124
566.681174	31170.043034	31.384141
567.074356	31201.398354	31.389159
567.539446	31232.665049	31.394176
568.156957	31248.859813	31.399194
568.367558	31283.470794	31.404212
569.074951	31310.697137	31.409229
569.543503	31326.833744	31.414247
569.761769	31364.677993	31.419264
570.098384	31396.398913	31.424282
570.998947	31426.619380	31.429300
570.914443	31453.738817	31.434317
571.660418	31491.805086	31.439335
571.794150	31537.121748	31.444352
572.331783	31580.355086	31.449370
573.329220	31628.975282	31.454388
573.197367	31678.347657	31.459405
573.894816	31721.918440	31.464423
574.092129	31774.821414	31.469440
574.743380	31822.829004	31.474458
575.307354	31881.841692	31.479476
575.942934	31943.705633	31.484493
576.545242	31988.562722	31.489511
577.055655	32043.379107	31.494528
577.704396	32114.388553	31.499546
578.467414	32160.714800	31.504564
579.205404	32207.853787	31.509581
580.166439	32246.759220	31.514599
580.892109	32292.784416	31.519616
581.429801	32351.453036	31.524634
582.159867	32389.591694	31.529652
582.786882	32422.420592	31.534669
583.782943	32457.783768	31.539687
584.189878	32501.787496	31.544704
584.855458	32539.298374	31.549722
585.563950	32568.706640	31.554740
585.791371	32610.046933	31.559757
586.973874	32640.714957	31.564775
587.442317	32679.384609	31.569792
588.033644	32712.505081	31.574810
588.718952	32755.415324	31.579828
588.840659	32791.764957	31.584845
589.606728	32824.288771	31.589863
589.744029	32871.035087	31.594880
590.645835	32900.818272	31.599898
591.007110	32942.275215	31.604916
591.250821	32994.829480	31.609933
591.897447	33034.511964	31.614951
592.418462	33085.731328	31.619968
592.962867	33132.446643	31.624986
593.433587	33185.640034	31.630004
593.827741	33234.209716	31.635021
594.783023	33286.944777	31.640039
595.186243	33347.766434	31.645056
595.513465	33403.719958	31.650074
596.300689	33451.888751	31.655092
596.646234	33511.637220	31.660109
597.626206	33568.445778	31.665127
597.781729	33627.193966	31.670144
598.260030	33680.684096	31.675162
599.021336	33737.832306	31.680180
599.741273	33785.902435	31.685197
600.741996	33829.249180	31.690215
600.839805	33884.503094	31.695232
601.474124	33932.388654	31.700250
602.377491	33979.728621	31.705268
602.558647	34041.102094	31.710285
603.306962	34078.377848	31.715303
604.058864	34139.302931	31.720320
604.517155	34190.975516	31.725338
605.286532	34241.521997	31.730356
605.483443	34295.117244	31.735373
606.224571	34338.978025	31.740391
606.389464	34405.203054	31.745408
607.258725	34460.342315	31.750426
607.866728	34515.977394	31.755444
608.157625	34581.855147	31.760461
608.869381	34639.925552	31.765479
609.667059	34705.172884	31.770496
610.589764	34766.612218	31.775514
611.324956	34826.935519	31.780532
611.808019	34885.664345	31.785549
612.542483	34937.203817	31.790567
613.164310	34990.493988	31.795584
613.719053	35052.620433	31.800602
614.855625	35100.673719	31.805620
615.121522	35162.383072	31.810637
616.085453	35203.492684	31.815655
616.682518	35245.447522	31.820672
617.082279	35300.484603	31.825690
617.786185	35348.249631	31.830708
618.338054	35405.481051	31.835725
619.123319	35460.543973	31.840743
619.961707	35514.329474	31.845760
620.221277	35565.222864	31.850778
621.010246	35604.173033	31.855796
621.321260	35666.848231	31.860813
621.738608	35717.537224	31.865831
622.310243	35780.117734	31.870848
623.020949	35834.331358	31.875866
623.907262	35897.221657	31.880884
624.586955	35961.310216	31.885901
624.846544	36002.289586	31.890919
625.604853	36072.886954	31.895936
625.927483	36127.262655	31.900954
626.814272	36182.657062	31.905972
627.263601	36249.274493	31.910989
628.017546	36306.085792	31.916007
628.803140	36370.025029	31.921024
629.224641	36433.644093	31.926042
630.188540	36488.577880	31.931060
630.416654	36561.175804	31.936077
631.239965	36613.166666	31.941095
631.727442	36667.183601	31.946112
632.457955	36732.928829	31.951130
633.254550	36770.341644	31.956148
633.988504	36823.460530	31.961165
635.112728	36862.647190	31.966183
635.687375	36916.425574	31.971200
635.789355	36954.892288	31.976218
636.399412	36996.486788	31.981236
637.020320	37055.064070	31.986253
637.868784	37102.424768	31.991271
638.769489	37143.049385	31.996288
638.634080	37208.254795	32.001306
639.310010	37254.650055	32.006324
639.882041	37315.515986	32.011341
640.209836	37375.120213	32.016359
641.264239	37433.536745	32.021376
641.697418	37492.523860	32.026394
642.564557	37537.011526	32.031412
643.208597	37603.289516	32.036429
644.391662	37653.703138	32.041447
645.333870	37702.685708	32.046464
645.445663	37757.243720	32.051482
646.440283	37802.329884	32.056500
646.886969	37850.783153	32.061517
647.867197	37899.126368	32.066535
648.753591	37947.303332	32.071552
649.656310	37985.610184	32.076570
650.660152	38007.489599	32.081588
650.852734	38046.102044	32.086605
651.645843	38093.919001	32.091623
652.571929	38125.940419	32.096640
653.081341	38170.986573	32.101658
653.678640	38210.375390	32.106676
654.016112	38255.993155	32.111693
654.406824	38297.073897	32.116711
654.928700	38343.673284	32.121728
655.463941	38409.637465	32.126746
656.270115	38453.175377	32.131764
656.631816	38507.276561	32.136781
657.209690	38563.741895	32.141799
657.800356	38620.637441	32.146816
657.961346	38687.947443	32.151834
659.069564	38739.938903	32.156852
659.838474	38802.835069	32.161869
660.143983	38862.246228	32.166887
660.437283	38927.777879	32.171904
661.168445	39007.649764	32.176922
661.888424	39068.569387	32.181940
662.696911	39142.710155	32.186957
663.016075	39203.725626	32.191975
663.852748	39275.404068	32.196992
664.272146	39345.490326	32.202010
665.382864	39407.396022	32.207028
666.119397	39481.029331	32.212045
666.589937	39538.014878	32.217063
667.516927	39601.018129	32.222080
668.292713	39665.335644	32.227098
669.208420	39712.025874	32.232116
670.011479	39765.988232	32.237133
670.474308	39810.536782	32.242151
671.622425	39863.523549	32.247168
671.867801	39914.430683	32.252186
672.575263	39946.744247	32.257204
674.066307	39980.342928	32.262221
674.850256	40011.307149	32.267239
675.764982	40057.077519	32.272256
676.044834	40095.997687	32.277274
676.960911	40137.876023	32.282292
677.254780	40174.753495	32.287309
677.442220	40216.271791	32.292327
678.215073	40262.219849	32.297344
678.468838	40326.436890	32.302362
679.272320	40375.512341	32.307380
679.664133	40428.665450	32.312397
680.740936	40485.204363	32.317415
680.931613	40541.635390	32.322432
681.515593	40613.783910	32.327450
682.158680	40666.333162	32.332468
682.663768	40731.114132	32.337485
683.329777	40805.278493	32.342503
684.093211	40863.076584	32.347520
684.468828	40935.839997	32.352538
685.519987	41004.676454	32.357556
686.554039	41073.443365	32.362573
687.085212	41142.684899	32.367591
687.879738	41200.460250	32.372608
688.271789	41271.247934	32.377626
689.482900	41327.465435	32.382644
690.106728	41388.208337	32.387661
690.912516	41453.092397	32.392679
691.758148	41512.097124	32.397696
691.963159	41573.459363	32.402714
692.764763	41627.367885	32.407732
693.470150	41697.050743	32.412749
694.398228	41763.654518	32.417767
694.896022	41822.848177	32.422784
695.257780	41883.849048	32.427802
696.515291	41946.016559	32.432820
696.803297	42020.946610	32.437837
697.331958	42085.394561	32.442855
698.627667	42159.060732	32.447872
699.127042	42224.551657	32.452890
699.710069	42287.130614	32.457908
700.403645	42358.672813	32.462925
700.873049	42425.626611	32.467943
701.719186	42480.871343	32.472960
702.042050	42565.542260	32.477978
702.460008	42628.726001	32.482996
703.495400	42713.009750	32.488013
703.886675	42785.052935	32.493031
704.478122	42864.629053	32.498048
705.264619	42946.499361	32.503066
705.999825	43018.788435	32.508084
706.423490	43090.064332	32.513101
707.403691	43160.810270	32.518119
708.275326	43223.927099	32.523136
708.896124	43292.500517	32.528154
709.482177	43361.710658	32.533172
710.084224	43432.697727	32.538189
710.315885	43512.558077	32.543207
711.317440	43582.573617	32.548224
712.285295	43665.273347	32.553242
712.860064	43735.505724	32.558260
713.678581	43818.479179	32.563277
714.622498	43896.606381	32.568295
715.571553	43963.865150	32.573312
715.845112	44045.898022	32.578330
716.901287	44114.342266	32.583348
717.849399	44186.151171	32.588365
717.997524	44263.185835	32.593383
719.118828	44328.339601	32.598400
719.529701	44408.541476	32.603418
720.429808	44481.901933	32.608436
721.795088	44550.834995	32.613453
722.878958	44604.020092	32.618471
723.972383	44653.888103	32.623488
725.436021	44708.849169	32.628506
726.694935	44740.853624	32.633524
727.519191	44776.874062	32.638541
727.941993	44818.608845	32.643559
729.024815	44849.925385	32.648576
729.750646	44884.611435	32.653594
730.262452	44928.364048	32.658612
730.652081	44956.588943	32.663629
731.061413	45000.168757	32.668647
731.801106	45050.406559	32.673664
732.027573	45105.382866	32.678682
732.858869	45163.610423	32.683700
733.282211	45216.322048	32.688717
733.559892	45282.885136	32.693735
734.273535	45339.791159	32.698752
734.593852	45421.031146	32.703770
735.320799	45488.135549	32.708788
735.940616	45562.734599	32.713805
736.548163	45647.879959	32.718823
737.354984	45717.225199	32.723840
737.815691	45795.097086	32.728858
738.785445	45864.079377	32.733876
739.603588	45934.871842	32.738893
739.915198	46027.467931	32.743911
740.702268	46099.521727	32.748928
741.495373	46184.116397	32.753946
742.492231	46268.436091	32.758964
743.094760	46348.228247	32.763981
743.583794	46432.762093	32.768999
744.921443	46498.719309	32.774016
745.551690	46581.126892	32.779034
745.678153	46648.309240	32.784052
747.279071	46715.518984	32.789069
748.041239	46795.644289	32.794087
748.757748	46861.960484	32.799104
749.143710	46935.466704	32.804122
749.626382	46996.851132	32.809140
750.571126	47074.134151	32.814157
751.150580	47150.548013	32.819175
752.190767	47215.788542	32.824192
752.540911	47302.702512	32.829210
753.474998	47372.630364	32.834228
754.524651	47452.668708	32.839245
754.582281	47539.923857	32.844263
755.577471	47619.495168	32.849280
756.263728	47708.796715	32.854298
756.639298	47781.361490	32.859316
757.282293	47873.658909	32.864333
758.134171	47964.137586	32.869351
759.154324	48044.334761	32.874368
759.953320	48131.954421	32.879386
761.004941	48234.491220	32.884404
761.825731	48302.115199	32.889421
762.409304	48396.526349	32.894439
763.327560	48476.924721	32.899456
764.257088	48555.740743	32.904474
764.790467	48637.021548	32.909492
765.641261	48725.503663	32.914509
766.207871	48822.106573	32.919527
767.169220	48891.767854	32.924544
768.021345	48985.072785	32.929562
768.625343	49070.885242	32.934580
769.641503	49149.210447	32.939597
770.282038	49239.145465	32.944615
771.343911	49316.990784	32.949632
772.041003	49403.638894	32.954650
772.991025	49485.573580	32.959668
773.928069	49554.969935	32.964685
774.652803	49645.600474	32.969703
775.593759	49715.284000	32.974720
776.677013	49793.014387	32.979738
777.312600	49877.493967	32.984756
778.369011	49938.923452	32.989773
779.015757	50010.845073	32.994791
779.442988	50077.112026	32.999808
780.118415	50157.626062	33.004826
780.737277	50234.018490	33.009844
781.755790	50319.458527	33.014861
782.566800	50400.248719	33.019879
783.714302	50473.036080	33.024896
784.617628	50550.893080	33.029914
785.126094	50614.917882	33.034932
786.197147	50684.619189	33.039949
786.774738	50768.449461	33.044967
787.232502	50839.299918	33.049984
787.839078	50915.776103	33.055002
788.913533	50985.313928	33.060020
789.874410	51061.529196	33.065037
790.489307	51134.710156	33.070055
791.386870	51188.534897	33.075072
792.086859	51252.998571	33.080090
792.568383	51318.238916	33.085108
793.884701	51381.976896	33.090125
794.354294	51441.141083	33.095143
795.318965	51519.106131	33.100160
796.048187	51586.400479	33.105178
796.780560	51665.656095	33.110196
797.964590	51720.468865	33.115213
798.319557	51792.854358	33.120231
799.235062	51857.992857	33.125248
800.418200	51929.682125	33.130266
800.605266	52008.625224	33.135284
801.500864	52068.632624	33.140301
802.140257	52154.356349	33.145319
802.922711	52224.706079	33.150336
803.923670	52307.892227	33.155354
804.239099	52393.738091	33.160372
805.208882	52463.452941	33.165389
806.041755	52557.202436	33.170407
807.130952	52618.888367	33.175424
807.952558	52699.365247	33.180442
808.767173	52778.050838	33.185460
810.061035	52858.715224	33.190477
810.434313	52936.253427	33.195495
811.254163	53013.228493	33.200512
811.726631	53094.782191	33.205530
812.287619	53187.842801	33.210548
813.547273	53259.664043	33.215565
814.237427	53354.709231	33.220583
814.681260	53436.909764	33.225600
815.720134	53524.141943	33.230618
816.021857	53618.410734	33.235636
817.104740	53707.145551	33.240653
817.693922	53810.819933	33.245671
818.087684	53908.175204	33.250688
819.086877	54005.377808	33.255706
819.823001	54105.185880	33.260724
820.778344	54195.101809	33.265741
821.484321	54308.378327	33.270759
822.412126	54398.517442	33.275776
823.436229	54498.932077	33.280794
824.318355	54588.893164	33.285812
825.821924	54686.101183	33.290829
826.815775	54762.983345	33.295847
827.772395	54842.368647	33.300864
828.736370	54927.356159	33.305882
829.363427	55012.776491	33.310900
830.068379	55095.454303	33.315917
831.186723	55179.607151	33.320935
831.842778	55263.875005	33.325952
833.226384	55335.975119	33.330970
833.665058	55402.550134	33.335988
834.436404	55473.296149	33.341005
835.581993	55536.059439	33.346023
836.466384	55597.308238	33.351040
837.262825	55674.683379	33.356058
837.600480	55735.672417	33.361076
838.719368	55806.705333	33.366093
839.085502	55892.108151	33.371111
839.850632	55971.083711	33.376128
840.726528	56047.109282	33.381146
841.240682	56135.100368	33.386164
842.027469	56216.611639	33.391181
842.609646	56314.972518	33.396199
843.414852	56400.200472	33.401216
844.295725	56492.276737	33.406234
844.515084	56583.154940	33.411252
846.006312	56683.308290	33.416269
847.124252	56767.667361	33.421287
848.068960	56860.998088	33.426304
848.869924	56948.988444	33.431322
849.801632	57046.539911	33.436340
850.864178	57136.778355	33.441357
851.344741	57223.043609	33.446375
852.041638	57319.977227	33.451392
853.368217	57412.489109	33.456410
853.858487	57508.856759	33.461428
854.666730	57598.272886	33.466445
855.497605	57694.318936	33.471463
855.990937	57800.938763	33.476480
857.110697	57900.652688	33.481498
857.818981	58008.278195	33.486516
858.850114	58102.204438	33.491533
859.646447	58204.137294	33.496551
860.515113	58303.107200	33.501568
861.356630	58407.884948	33.506586
862.078982	58515.312242	33.511604
862.862546	58608.727925	33.516621
863.751559	58710.999262	33.521639
864.587426	58829.331351	33.526656
866.020366	58922.692615	33.531674
866.758398	59028.102838	33.536692
867.862691	59119.162017	33.541709
868.700272	59228.741024	33.546727
869.689976	59318.000763	33.551744
871.050788	59411.003380	33.556762
871.657182	59513.185164	33.561780
872.468881	59591.344635	33.566797
873.604601	59684.460214	33.571815
874.171408	59780.925304	33.576832
875.289181	59861.578951	33.581850
876.037276	59962.367129	33.586868
876.946646	60054.396503	33.591885
877.929040	60144.292849	33.596903
878.516150	60233.586293	33.601920
879.590905	60330.497520	33.606938
880.104364	60415.458750	33.611956
881.154178	60493.138866	33.616973
881.804190	60586.352011	33.621991
882.498463	60680.707946	33.627008
883.422609	60765.924318	33.632026
884.434424	60860.300085	33.637044
885.198726	60942.817648	33.642061
886.441610	61041.764578	33.647079
886.987188	61132.047774	33.652096
887.841235	61219.358272	33.657114
888.557534	61320.076682	33.662132
889.462526	61412.059711	33.667149
890.141292	61511.376762	33.672167
890.985021	61613.734279	33.677184
892.086846	61706.997895	33.682202
893.023770	61816.983528	33.687220
893.844801	61914.697995	33.692237
894.626365	62012.075043	33.697255
895.409630	62123.621621	33.702272
896.249857	62228.240884	33.707290
897.228538	62341.355528	33.712308
898.082277	62447.224375	33.717325
898.922209	62556.658153	33.722343
899.861498	62661.901944	33.727360
901.209451	62754.417851	33.732378
902.308987	62879.810419	33.737396
903.875842	62951.989794	33.742413
905.605285	63027.137361	33.747431
906.881998	63103.039406	33.752448
908.049513	63170.157697	33.757466
908.706398	63250.074926	33.762484
909.437036	63324.912071	33.767501
910.229177	63394.629968	33.772519
911.100581	63476.348845	33.777536
912.051680	63554.534115	33.782554
913.487283	63627.308561	33.787572
914.123554	63705.013986	33.792589
914.970711	63788.162370	33.797607
915.632915	63867.519191	33.802624
916.448735	63939.247050	33.807642
917.043985	64030.136165	33.812660
917.360900	64117.933922	33.817677
918.301208	64201.997789	33.822695
918.705489	64316.813618	33.827712
919.631163	64408.801539	33.832730
920.753544	64514.092738	33.837748
921.313700	64622.215361	33.842765
922.020312	64719.305498	33.847783
923.123574	64836.852507	33.852800
924.236944	64924.833570	33.857818
924.836234	65046.252042	33.862836
925.924946	65152.392218	33.867853
926.990483	65259.547347	33.872871
927.413845	65373.409462	33.877888
928.471743	65472.310952	33.882906
929.535674	65589.376107	33.887924
930.164076	65687.816432	33.892941
931.035745	65792.914488	33.897959
931.834239	65894.771527	33.902976
933.054620	65996.261912	33.907994
933.480272	66107.929680	33.913012
934.349894	66222.989197	33.918029
935.400523	66331.134955	33.923047
936.230015	66440.030343	33.928064
937.363448	66544.310664	33.933082
938.413694	66666.722532	33.938100
939.341319	66771.485347	33.943117
940.514437	66883.291334	33.948135
941.204428	67003.873788	33.953152
942.295820	67110.513889	33.958170
943.024074	67234.547278	33.963188
943.834714	67333.627136	33.968205
945.279146	67450.636683	33.973223
946.214212	67568.397639	33.978240
947.251841	67694.532683	33.983258
947.704613	67807.993774	33.988276
949.069353	67908.725725	33.993293
950.321400	68020.184540	33.998311
951.477037	68136.921965	34.003328
952.685774	68225.329305	34.008346
953.788363	68331.285681	34.013364
954.940447	68435.465777	34.018381
955.831879	68528.878124	34.023399
956.700299	68628.631375	34.028416
957.667827	68734.560884	34.033434
958.707775	68834.376342	34.038452
959.686461	68936.451244	34.043469
960.841016	69040.691032	34.048487
961.663646	69138.533501	34.053504
962.777105	69232.482497	34.058522
963.437978	69335.962107	34.063540
964.121054	69439.306049	34.068557
965.554898	69547.895178	34.073575
966.189414	69660.933722	34.078592
967.162220	69757.738153	34.083610
968.228798	69870.058377	34.088628
968.986604	69979.957923	34.093645
969.659605	70093.030732	34.098663
970.172723	70215.701932	34.103680
971.494862	70323.030485	34.108698
972.388651	70447.797128	34.113716
973.368404	70567.654070	34.118733
974.751161	70674.393591	34.123751
975.440208	70791.745471	34.128768
976.633267	70899.293570	34.133786
977.608855	71021.788771	34.138804
978.304465	71141.631212	34.143821
979.435014	71242.177421	34.148839
980.321265	71367.285949	34.153856
981.063187	71480.892813	34.158874
982.291008	71587.971531	34.163892
982.610764	71690.980649	34.168909
984.223461	71796.331086	34.173927
985.142342	71913.627757	34.178944
986.258216	72016.025338	34.183962
986.918268	72118.464374	34.188980
988.120732	72224.337315	34.193997
989.207714	72332.080667	34.199015
990.146265	72446.312618	34.204032
991.274574	72539.244957	34.209050
992.167618	72647.368420	34.214068
993.070048	72762.998138	34.219085
994.229670	72871.200463	34.224103
995.127844	72984.614103	34.229120
995.930265	73097.291626	34.234138
996.895088	73211.511133	34.239156
997.893319	73320.424051	34.244173
999.400610	73423.189973	34.249191
1000.180069	73548.360767	34.254208
1001.484465	73650.161667	34.259226
1002.506972	73767.029328	34.264244
1003.642354	73879.822583	34.269261
1004.500547	73987.516458	34.274279
1005.406454	74097.396214	34.279296
1006.815547	74202.621113	34.284314
1007.831110	74318.286037	34.289332
1008.697000	74421.810042	34.294349
1009.936815	74531.607447	34.299367
1010.405612	74654.679524	34.304384
1011.778658	74743.235153	34.309402
1013.268272	74855.035869	34.314420
1014.118876	74960.056546	34.319437
1015.234961	75062.526539	34.324455
1016.719985	75167.687521	34.329472
1017.496370	75260.448292	34.334490
1018.360203	75365.949289	34.339508
1019.077874	75471.347688	34.344525
1020.630212	75576.373687	34.349543
1021.709891	75672.646281	34.354560
1023.253073	75757.456769	34.359578
1024.434678	75851.394521	34.364596
1024.958466	75953.925334	34.369613
1026.301865	76041.707672	34.374631
1027.182196	76148.373031	34.379648
1027.720191	76244.292096	34.384666
1028.799030	76346.275208	34.389684
1029.513169	76450.288789	34.394701
1030.608695	76549.356598	34.399719
1031.379069	76661.288026	34.404736
1032.409219	76771.295258	34.409754
1033.458024	76879.119560	34.414772
1033.808691	76998.211148	34.419789
1034.893218	77110.278355	34.424807
1035.954938	77237.051421	34.429824
1037.246367	77341.679289	34.434842
1038.141084	77457.084263	34.439860
1038.979844	77562.929307	34.444877
1040.290921	77662.044075	34.449895
1041.031233	77782.993411	34.454912
1041.495301	77889.215783	34.459930
1042.828226	78001.823546	34.464948
1043.804569	78120.872691	34.469965
1044.968896	78227.004375	34.474983
1045.744137	78363.981293	34.480000
1046.814609	78478.877344	34.485018
1047.643536	78598.471021	34.490036
1048.671925	78720.043746	34.495053
1049.881724	78843.016887	34.500071
1050.648825	78983.684392	34.505088
1051.651246	79108.013211	34.510106
1053.050148	79243.120520	34.515124
1053.859442	79375.142934	34.520141
1054.964965	79502.845899	34.525159
1056.135613	79637.429503	34.530176
1056.980999	79773.778805	34.535194
1058.145899	79905.305538	34.540212
1059.036046	80045.872188	34.545229
1060.346096	80174.798401	34.550247
1061.210020	80312.905661	34.555264
1062.243733	80453.901061	34.560282
1063.475631	80603.817259	34.565300
1064.242962	80745.514454	34.570317
1065.300369	80877.968434	34.575335
1066.462512	81032.418808	34.580352
1067.441050	81173.263488	34.585370
1068.844521	81310.412809	34.590388
1069.569813	81466.807138	34.595405
1070.939276	81605.228174	34.600423
1072.067975	81743.998199	34.605440
1073.082588	81878.684329	34.610458
1074.654156	82007.738326	34.615476
1075.714879	82147.723020	34.620493
1076.899718	82289.048156	34.625511
1078.258464	82427.684960	34.630528
1079.210554	82555.348839	34.635546
1080.247351	82692.527600	34.640564
1081.039005	82834.171831	34.645581
1082.224249	82961.301627	34.650599
1083.474096	83099.852703	34.655616
1084.544132	83243.231979	34.660634
1085.598772	83375.177412	34.665652
1086.392796	83526.948116	34.670669
1087.727056	83656.271260	34.675687
1088.696483	83800.005409	34.680704
1090.161694	83935.258950	34.685722
1091.427231	84062.578603	34.690740
1092.665412	84191.003517	34.695757
1094.376091	84300.923379	34.700775
1095.506512	84421.887080	34.705792
1096.757803	84533.613648	34.710810
1098.264202	84636.410371	34.715828
1099.302698	84733.376493	34.720845
1100.082376	84825.667375	34.725863
1101.699013	84920.481144	34.730880
1102.688650	85005.815857	34.735898
1104.060848	85098.412023	34.740916
1104.654078	85206.193793	34.745933
1106.055077	85280.025931	34.750951
1107.456680	85389.608566	34.755968
1108.097450	85486.869010	34.760986
1108.845860	85589.354610	34.766004
1109.570178	85696.675389	34.771021
1110.607386	85803.807832	34.776039
1111.479413	85923.354189	34.781056
1112.274095	86047.061544	34.786074
1113.588848	86172.817831	34.791092
1114.379092	86293.953752	34.796109
1115.486203	86413.863821	34.801127
1116.393597	86556.273231	34.806144
1117.110280	86691.378764	34.811162
1118.442939	86815.548794	34.816180
1119.234776	86960.407460	34.821197
1120.333821	87099.438535	34.826215
1121.406094	87242.401700	34.831232
1122.461431	87389.921505	34.836250
1124.063077	87525.270931	34.841268
1124.932499	87676.863077	34.846285
1126.021316	87820.908792	34.851303
1127.028470	87968.819634	34.856320
1128.033688	88126.508425	34.861338
1129.042970	88271.840877	34.866356
1130.307198	88435.909449	34.871373
1131.453696	88592.643218	34.876391
1132.633359	88738.900291	34.881408
1133.737367	88897.306226	34.886426
1135.185202	89048.506082	34.891444
1135.970240	89202.595019	34.896461
1137.047765	89357.068571	34.901479
1138.072177	89505.682782	34.906496
1139.581976	89669.923971	34.911514
1140.560180	89830.810509	34.916532
1141.520107	89980.886474	34.921549
1143.156381	90144.902411	34.926567
1144.214407	90297.956392	34.931584
1145.085779	90459.244000	34.936602
1147.114418	90602.874031	34.941620
1147.839276	90760.670708	34.946637
1149.149287	90914.688196	34.951655
1150.180745	91060.238052	34.956672
1151.423583	91224.122229	34.961690
1152.946256	91370.348654	34.966708
1153.873144	91527.144675	34.971725
1154.975143	91670.252286	34.976743
1156.490524	91823.244134	34.981760
1157.349008	91971.268911	34.986778
1158.854031	92100.855763	34.991796
1159.701010	92237.758532	34.996813
1160.972336	92357.384213	35.001831
1162.859429	92476.033430	35.006848
1163.692541	92610.998909	35.011866
1165.220464	92733.963428	35.016884
1165.927596	92864.731607	35.021901
1167.749559	92973.438001	35.026919
1169.044053	93086.042935	35.031936
1170.075144	93221.220992	35.036954
1171.480579	93325.460117	35.041972
1172.651853	93453.944083	35.046989
1173.422491	93574.307447	35.052007
1174.695080	93694.091929	35.057024
1175.513830	93829.193577	35.062042
1176.655427	93956.717359	35.067060
1177.455643	94096.308343	35.072077
1178.763829	94228.709473	35.077095
1179.515873	94369.227025	35.082112
1180.402079	94529.561372	35.087130
1181.882821	94675.227906	35.092148
1182.827601	94823.896780	35.097165
1183.870456	94975.606393	35.102183
1185.175563	95120.234681	35.107200
1186.229349	95288.347525	35.112218
1187.276349	95447.492552	35.117236
1187.996314	95611.840035	35.122253
1189.395433	95770.077335	35.127271
1190.602978	95939.568620	35.132288
1191.356944	96107.741557	35.137306
1192.803513	96274.312635	35.142324
1194.268778	96444.899096	35.147341
1195.186861	96608.064603	35.152359
1196.697567	96779.449782	35.157376
1198.211013	96948.577316	35.162394
1199.584278	97102.658967	35.167412
1200.769189	97270.550553	35.172429
1202.038539	97429.231264	35.177447
1203.188684	97592.657936	35.182464
1204.415109	97757.990593	35.187482
1205.781674	97913.628789	35.192500
1207.144105	98083.010171	35.197517
1208.298730	98237.235464	35.202535
1209.895922	98396.541380	35.207552
1210.844455	98551.048295	35.212570
1211.882296	98716.316619	35.217588
1213.125765	98877.092992	35.222605
1214.336201	99037.591030	35.227623
1215.405086	99203.731028	35.232640
1216.568267	99368.110975	35.237658
1217.976612	99518.457693	35.242676
1219.055525	99687.478378	35.247693
1220.091903	99851.964179	35.252711
1221.248423	100018.425106	35.257728
1222.393650	100188.337358	35.262746
1223.814177	100339.598591	35.267764
1224.763154	100495.466139	35.272781
1225.894634	100647.718105	35.277799
1227.247396	100794.171634	35.282816
1228.484713	100963.265001	35.287834
1230.073237	101105.639773	35.292852
1230.957197	101263.117317	35.297869
1232.010348	101414.779307	35.302887
1233.699637	101577.990242	35.307904
1235.032327	101741.309637	35.312922
1236.034606	101884.934003	35.317940
1237.287182	102054.045490	35.322957
1238.604773	102210.460678	35.327975
1239.796660	102360.904457	35.332992
1241.030473	102541.096105	35.338010
1242.006376	102696.784201	35.343028
1243.423978	102865.875291	35.348045
1244.428260	103030.818867	35.353063
1245.533104	103198.215540	35.358080
1246.723136	103368.358897	35.363098
1247.915269	103543.420097	35.368116
1249.259195	103714.199598	35.373133
1250.444941	103899.598354	35.378151
1251.855978	104069.458479	35.383168
1252.867954	104253.318214	35.388186
1254.445244	104425.622497	35.393204
1255.739816	104603.516663	35.398221
1256.786176	104790.045665	35.403239
1258.348283	104955.584747	35.408256
1260.048783	105133.443643	35.413274
1261.416289	105305.382611	35.418292
1263.208585	105465.471355	35.423309
1264.296171	105622.591144	35.428327
1266.117953	105780.348354	35.433344
1267.011991	105952.810256	35.438362
1268.637317	106103.594884	35.443380
1270.176102	106261.166082	35.448397
1271.516611	106405.156403	35.453415
1273.003651	106553.503904	35.458432
1274.046673	106711.739132	35.463450
1275.523336	106856.577573	35.468468
1276.988154	107014.412291	35.473485
1278.212354	107152.533228	35.478503
1279.708058	107297.200401	35.483520
1280.759393	107444.793533	35.488538
1282.509773	107582.985176	35.493556
1283.600846	107738.814392	35.498573
1284.798250	107877.209550	35.503591
1286.159251	108018.997313	35.508608
1287.330177	108160.854097	35.513626
1288.239613	108305.253383	35.518644
1289.203984	108466.557000	35.523661
1290.412197	108621.620045	35.528679
1291.723120	108769.097664	35.533696
1292.685946	108932.164204	35.538714
1294.009269	109080.793710	35.543732
1295.318893	109221.590229	35.548749
1296.157954	109377.552263	35.553767
1297.023530	109520.092118	35.558784
1298.297639	109691.114956	35.563802
1299.224866	109848.490154	35.568820
1300.286395	110018.213478	35.573837
1301.736725	110189.737142	35.578855
1303.360646	110348.308734	35.583872
1304.711740	110517.856538	35.588890
1305.698600	110682.608304	35.593908
1306.970496	110854.633375	35.598925
1308.355389	111042.074419	35.603943
1309.707326	111206.075323	35.608960
1310.952127	111388.116336	35.613978
1312.152853	111558.581394	35.618996
1313.775812	111739.343134	35.624013
1314.804864	111924.878697	35.629031
1316.343380	112096.787696	35.634048
1317.712609	112285.107861	35.639066
1318.550204	112460.327638	35.644084
1320.008992	112654.200807	35.649101
1321.019306	112848.925425	35.654119
1322.051288	113032.607563	35.659136
1323.488981	113238.599023	35.664154
1325.027850	113437.511038	35.669172
1326.800089	113630.613896	35.674189
1327.725161	113823.941532	35.679207
1329.433035	114013.221098	35.684224
1330.924406	114208.316594	35.689242
1332.303750	114389.648970	35.694260
1333.675516	114582.487231	35.699277
1335.065899	114775.760841	35.704295
1336.453690	114964.275369	35.709312
1337.682326	115158.786841	35.714330
1339.033148	115352.343365	35.719348
1340.433015	115541.917560	35.724365
1341.778812	115746.867738	35.729383
1343.430554	115924.432320	35.734400
1344.774874	116115.494801	35.739418
1345.943387	116310.391827	35.744436
1347.444576	116490.295231	35.749453
1348.930554	116682.073870	35.754471
1350.771534	116858.652464	35.759488
1352.018123	117056.050033	35.764506
1353.908455	117219.523209	35.769524
1355.882789	117387.675840	35.774541
1357.070879	117562.406555	35.779559
1359.059623	117710.044258	35.784576
1360.477901	117875.179563	35.789594
1361.635385	118030.391077	35.794612
1363.593679	118192.536266	35.799629
1364.660369	118354.058027	35.804647
1365.897379	118500.224085	35.809664
1367.121398	118657.379014	35.814682
1368.188531	118802.718958	35.819700
1369.562812	118934.485637	35.824717
1370.412614	119088.663266	35.829735
1371.781798	119235.034067	35.834752
1373.053744	119394.338746	35.839770
1374.024124	119560.645080	35.844788
1375.052131	119714.329494	35.849805
1376.053821	119889.852679	35.854823
1377.269471	120061.087712	35.859840
1378.271343	120248.188747	35.864858
1379.854904	120427.105842	35.869876
1381.229502	120608.375044	35.874893
1381.929354	120801.303208	35.879911
1383.347538	120996.854270	35.884928
1384.694368	121197.230891	35.889946
1385.628605	121396.661382	35.894964
1387.281604	121604.325621	35.899981
1388.171107	121817.419668	35.904999
1389.498533	122029.229925	35.910016
1390.674949	122246.423453	35.915034
1391.977930	122464.193928	35.920052
1393.815602	122689.696056	35.925069
1395.122670	122915.018432	35.930087
1396.964600	123124.805053	35.935104
1398.648242	123351.008540	35.940122
1399.357301	123585.551264	35.945140
1401.436651	123796.103380	35.950157
1402.949635	124009.584456	35.955175
1404.505349	124227.443082	35.960192
1405.655857	124434.322486	35.965210
1407.257953	124662.259954	35.970228
1408.628179	124885.486094	35.975245
1410.131166	125089.350424	35.980263
1411.914775	125314.389115	35.985280
1413.779876	125526.800160	35.990298
1415.138158	125733.998468	35.995316
1416.657953	125929.949353	36.000333
1418.115537	126141.125206	36.005351
1419.740096	126343.991540	36.010368
1421.444134	126537.903354	36.015386
1423.321449	126733.271135	36.020404
1425.156141	126912.951592	36.025421
1426.759509	127105.730645	36.030439
1428.902803	127274.254630	36.035456
1430.695585	127443.468757	36.040474
1431.358857	127616.955244	36.045492
1432.951561	127785.544519	36.050509
1434.451172	127958.241492	36.055527
1435.854781	128136.959632	36.060544
1437.298868	128317.876813	36.065562
1438.188712	128499.288645	36.070580
1439.805064	128665.801870	36.075597
1440.989779	128849.386143	36.080615
1442.328405	129032.035012	36.085632
1444.197179	129188.515545	36.090650
1446.094025	129352.315164	36.095668
1448.047289	129486.714593	36.100685
1449.400474	129648.663982	36.105703
1450.555850	129780.949185	36.110720
1451.886710	129931.932258	36.115738
1453.106652	130075.395532	36.120756
1454.269701	130231.601300	36.125773
1455.074748	130403.448245	36.130791
1456.336016	130567.786729	36.135808
1457.849258	130735.823664	36.140826
1459.413041	130907.020988	36.145844
1460.360245	131085.843162	36.150861
1461.648548	131265.347114	36.155879
1463.099153	131440.581991	36.160896
1464.522950	131629.683188	36.165914
1465.888487	131832.351896	36.170932
1467.275111	132022.399199	36.175949
1468.228926	132226.175087	36.180967
1469.812557	132434.755779	36.185984
1471.573650	132622.973731	36.191002
1472.883500	132826.684656	36.196020
1474.233281	133034.686026	36.201037
1475.097056	133247.923109	36.206055
1476.569643	133460.469506	36.211072
1478.356896	133668.988810	36.216090
1479.741677	133905.018959	36.221108
1481.352273	134109.717534	36.226125
1482.422736	134344.331367	36.231143
1483.456215	134565.863525	36.236160
1485.382250	134789.726472	36.241178
1486.429275	135026.275591	36.246196
1488.279981	135252.232193	36.251213
1489.815734	135490.151983	36.256231
1491.518479	135724.232966	36.261248
1493.492196	135957.639172	36.266266
1495.764305	136163.172130	36.271284
1497.793280	136363.410219	36.276301
1499.789082	136574.717742	36.281319
1501.356856	136771.192224	36.286336
1503.089972	136958.872492	36.291354
1504.740139	137158.897391	36.296372
1506.142466	137346.379231	36.301389
1507.230510	137541.617121	36.306407
1508.366196	137749.407336	36.311424
1510.312136	137944.321479	36.316442
1511.458280	138136.309822	36.321460
1513.221129	138335.222214	36.326477
1514.899820	138537.710418	36.331495
1516.328669	138741.253538	36.336512
1517.905854	138931.885859	36.341530
1519.541731	139130.811050	36.346548
1521.155293	139336.166487	36.351565
1522.605525	139526.734047	36.356583
1523.744639	139735.158516	36.361600
1525.027158	139922.574177	36.366618
1525.905291	140128.343351	36.371636
1527.486795	140313.242568	36.376653
1528.638750	140512.874780	36.381671
1529.832556	140712.666418	36.386688
1531.457013	140924.773450	36.391706
1532.602273	141132.116591	36.396724
1534.060082	141339.449509	36.401741
1535.201711	141568.532413	36.406759
1536.732984	141776.135458	36.411776
1538.641100	142005.353347	36.416794
1539.923674	142230.933340	36.421812
1541.447668	142454.017755	36.426829
1543.402152	142694.095584	36.431847
1544.512021	142920.341803	36.436864
1545.966047	143147.333524	36.441882
1547.375181	143386.286581	36.446900
1548.676961	143624.662805	36.451917
1550.213357	143870.874893	36.456935
1552.013628	144119.239838	36.461952
1553.563753	144352.816268	36.466970
1555.079774	144601.952713	36.471988
1556.821493	144846.289255	36.477005
1558.808877	145075.529937	36.482023
1560.646893	145311.767711	36.487040
1562.627204	145550.570537	36.492058
1564.163773	145779.964028	36.497076
1566.187061	146006.708621	36.502093
1568.054068	146226.609186	36.507111
1569.241661	146453.236214	36.512128
1571.408978	146683.131836	36.517146
1572.779613	146902.342680	36.522164
1574.556057	147121.870863	36.527181
1576.110164	147354.835054	36.532199
1577.504569	147578.623026	36.537216
1579.263370	147797.562848	36.542234
1581.006123	148020.284424	36.547252
1582.612183	148238.858537	36.552269
1584.086170	148472.452067	36.557287
1585.322036	148699.733864	36.562304
1587.339889	148920.275525	36.567322
1588.543757	149138.120950	36.572340
1590.232999	149379.787645	36.577357
1591.969497	149599.757429	36.582375
1593.403538	149829.221545	36.587392
1595.217070	150059.704595	36.592410
1596.695750	150291.408817	36.597428
1598.380274	150501.123948	36.602445
1600.010286	150736.116195	36.607463
1601.619772	150968.577778	36.612480
1603.334352	151172.752129	36.617498
1605.188475	151409.906901	36.622516
1606.559164	151633.980110	36.627533
1608.135411	151855.841506	36.632551
1609.478520	152091.205935	36.637568
1611.321899	152303.633160	36.642586
1612.693152	152517.607455	36.647604
1614.190718	152726.631047	36.652621
1615.580559	152931.818711	36.657639
1616.669530	153144.003435	36.662656
1618.587655	153361.801357	36.667674
1620.092437	153588.681131	36.672692
1621.433380	153806.332712	36.677709
1623.443185	154032.475948	36.682727
1624.498903	154257.745222	36.687744
1626.023436	154489.103699	36.692762
1627.308853	154741.105839	36.697780
1628.919766	154973.201984	36.702797
1630.473760	155208.643495	36.707815
1631.908757	155474.765094	36.712832
1633.494306	155715.454494	36.717850
1635.385570	155973.100783	36.722868
1636.718386	156227.021025	36.727885
1638.576317	156484.739846	36.732903
1640.096583	156747.776506	36.737920
1641.392104	157002.164866	36.742938
1643.301686	157262.797754	36.747956
1645.099380	157540.847991	36.752973
1646.547140	157808.481868	36.757991
1647.810945	158064.886574	36.763008
1650.345875	158331.058358	36.768026
1652.228279	158598.160062	36.773044
1653.824750	158863.242214	36.778061
1656.166616	159107.804162	36.783079
1657.896987	159367.783745	36.788096
1659.884577	159594.182534	36.793114
1661.860796	159850.956318	36.798132
1663.637796	160097.161945	36.803149
1665.862671	160321.549395	36.808167
1667.666978	160573.245062	36.813184
1669.648267	160793.210255	36.818202
1671.513528	161015.630120	36.823220
1673.270417	161246.983890	36.828237
1675.368144	161456.573626	36.833255
1677.219247	161666.267161	36.838272
1678.877195	161868.015595	36.843290
1680.358611	162097.123129	36.848308
1682.092336	162307.625321	36.853325
1683.925750	162528.677226	36.858343
1685.299811	162747.127454	36.863360
1686.742849	162962.143786	36.868378
1688.289409	163180.023869	36.873396
1689.378395	163405.676234	36.878413
1691.211266	163637.071234	36.883431
1692.831312	163866.586400	36.888448
1694.275877	164103.753232	36.893466
1695.581511	164348.705579	36.898484
1696.994448	164590.801522	36.903501
1698.763739	164843.217198	36.908519
1699.916088	165099.030180	36.913536
1701.871573	165341.399988	36.918554
1703.095041	165588.073110	36.923572
1704.326689	165821.124597	36.928589
1706.152511	166064.788026	36.933607
1707.464403	166319.797648	36.938624
1708.901659	166561.445898	36.943642
1710.250706	166824.469095	36.948660
1712.074640	167095.460249	36.953677
1713.869236	167337.323072	36.958695
1715.272689	167616.578519	36.963712
1717.120903	167891.452796	36.968730
1718.928652	168157.799029	36.973748
1720.233153	168437.951400	36.978765
1722.375333	168716.158932	36.983783
1723.831998	168997.305963	36.988800
1725.722661	169273.578684	36.993818
1727.303827	169562.079770	36.998836
1728.985484	169849.983545	37.003853
1730.968214	170132.273006	37.008871
1732.032788	170427.966037	37.013888
1734.406614	170722.425919	37.018906
1736.533377	171012.512826	37.023924
1738.223371	171294.844461	37.028941
1740.469265	171575.516871	37.033959
1741.911483	171863.917426	37.038976
1743.698293	172143.829523	37.043994
1745.746346	172429.854602	37.049012
1747.703607	172713.079936	37.054029
1749.348574	172999.591723	37.059047
1750.974948	173291.220897	37.064064
1753.298146	173570.575744	37.069082
1755.070888	173842.725478	37.074100
1756.584958	174132.374173	37.079117
1758.693268	174419.799302	37.084135
1760.725675	174694.336578	37.089152
1762.946692	174960.269782	37.094170
1764.597992	175232.511525	37.099188
1766.219779	175502.691858	37.104205
1768.772398	175766.306752	37.109223
1770.144744	176036.885417	37.114240
1772.412223	176303.834868	37.119258
1774.806651	176558.890998	37.124276
1776.246374	176817.373500	37.129293
1778.028985	177070.081327	37.134311
1779.414897	177335.248936	37.139328
1781.179394	177589.256854	37.144346
1782.848235	177864.012431	37.149364
1784.501672	178134.052561	37.154381
1786.352457	178391.020442	37.159399
1787.767743	178665.516985	37.164416
1789.342608	178941.715471	37.169434
1791.001844	179222.457213	37.174452
1792.767570	179494.835369	37.179469
1794.715065	179777.768023	37.184487
1796.187844	180062.072071	37.189504
1798.102902	180328.684185	37.194522
1799.715837	180593.607647	37.199540
1801.068250	180865.590617	37.204557
1803.240111	181119.694400	37.209575
1804.670789	181407.389002	37.214592
1806.458881	181666.784465	37.219610
1807.741315	181947.514863	37.224628
1810.037337	182204.104845	37.229645
1812.187626	182473.649123	37.234663
1813.961682	182746.985240	37.239680
1815.894562	183016.986063	37.244698
1817.985456	183298.624462	37.249716
1819.546568	183577.531806	37.254733
1821.489554	183851.710717	37.259751
1822.896804	184136.520955	37.264768
1824.583424	184417.063157	37.269786
1826.644764	184703.118177	37.274804
1828.186496	184997.822762	37.279821
1830.185623	185281.442262	37.284839
1831.553289	185573.932181	37.289856
1833.424571	185866.496291	37.294874
1835.217308	186161.333482	37.299892
1836.948988	186461.917994	37.304909
1839.061337	186758.434056	37.309927
1840.789754	187075.913167	37.314944
1842.743453	187375.592743	37.319962
1844.529128	187684.463114	37.324980
1846.000225	187992.865158	37.329997
1848.580470	188290.166889	37.335015
1850.000819	188616.829568	37.340032
1851.841371	188926.410005	37.345050
1853.859416	189233.794211	37.350068
1855.542295	189551.893642	37.355085
1857.663641	189849.633288	37.360103
1859.446144	190174.891220	37.365120
1861.371683	190488.338900	37.370138
1863.740685	190792.009704	37.375156
1865.692160	191115.609996	37.380173
1867.270834	191433.192605	37.385191
1868.805611	191755.479943	37.390208
1870.882218	192055.143836	37.395226
1872.878417	192355.507635	37.400244
1874.941349	192677.869441	37.405261
1877.314839	192973.887414	37.410279
1879.200556	193293.755734	37.415296
1881.269234	193600.702407	37.420314
1883.501745	193900.606462	37.425332
1885.267875	194205.028426	37.430349
1887.375487	194505.615855	37.435367
1889.329735	194806.851300	37.440384
1891.036780	195093.468556	37.445402
1893.042752	195400.766032	37.450420
1894.947794	195701.722618	37.455437
1896.983053	195990.983491	37.460455
1898.542546	196290.779893	37.465472
1900.029640	196592.214124	37.470490
1901.998186	196875.220488	37.475508
1903.396005	197162.659778	37.480525
1905.448168	197444.018601	37.485543
1906.590883	197740.652828	37.490560
1908.380124	198034.317553	37.495578
1910.499525	198328.896140	37.500596
1911.994733	198635.138556	37.505613
1914.167883	198933.354763	37.510631
1916.109574	199236.775381	37.515648
1917.784746	199547.893884	37.520666
1919.803581	199853.869693	37.525684
1921.636178	200164.002049	37.530701
1923.706142	200476.967154	37.535719
1925.747932	200792.680260	37.540736
1927.758895	201111.408388	37.545754
1929.819839	201415.075985	37.550772
1931.546344	201741.824348	37.555789
1933.841043	202052.630144	37.560807
1935.648022	202372.527556	37.565824
1937.504140	202691.758904	37.570842
1939.682012	203006.003093	37.575860
1941.506391	203335.918574	37.580877
1943.436122	203653.125288	37.585895
1945.538767	203974.634964	37.590912
1947.380028	204299.107549	37.595930
1949.187770	204622.533647	37.600948
1951.213420	204958.976619	37.605965
1953.114556	205281.617187	37.610983
1954.839479	205612.526129	37.616000
1956.691736	205954.308539	37.621018
1958.699328	206295.801673	37.626036
1960.307280	206644.672258	37.631053
1962.712745	206985.369889	37.636071
1964.856456	207333.930933	37.641088
1966.795158	207678.743457	37.646106
1968.746826	208013.336497	37.651124
1970.581131	208366.395735	37.656141
1972.619229	208705.155454	37.661159
1974.617541	209052.987624	37.666176
1976.504797	209404.724075	37.671194
1978.850563	209740.711133	37.676212
1981.218607	210087.398579	37.681229
1983.103744	210432.501460	37.686247
1985.237424	210766.801044	37.691264
1987.519239	211116.161114	37.696282
1989.820938	211442.959908	37.701300
1991.276710	211782.971080	37.706317
1993.659332	212112.312222	37.711335
1995.776076	212441.290948	37.716352
1997.929547	212773.452141	37.721370
2000.466430	213098.101681	37.726388
2002.584192	213425.091885	37.731405
2004.936890	213730.069629	37.736423
2006.602788	214047.752227	37.741440
2008.425109	214362.326341	37.746458
2010.608295	214657.305237	37.751476
2012.599079	214948.088094	37.756493
2014.941186	215230.005219	37.761511
2017.700486	215487.074069	37.766528
2019.509784	215769.725455	37.771546
2021.792154	216031.658536	37.776564
2023.578829	216320.536996	37.781581
2025.743244	216584.319154	37.786599
2027.575398	216865.663597	37.791616
2029.003843	217141.473999	37.796634
2031.128455	217425.681782	37.801652
2032.936146	217724.199404	37.806669
2034.452314	218014.790941	37.811687
2036.755757	218305.246035	37.816704
2038.332756	218610.063453	37.821722
2040.448467	218913.628549	37.826740
2042.110980	219215.920924	37.831757
2043.905877	219542.203635	37.836775
2046.114593	219853.858551	37.841792
2047.833521	220169.617471	37.846810
2049.702404	220555.937708	37.851828
2051.183657	220898.503117	37.856845
2053.271361	221236.085374	37.861863
2055.517839	221578.354655	37.866880
2057.188649	221929.693877	37.871898
2059.239463	222283.920215	37.876916
2060.906048	222634.234780	37.881933
2063.135099	223001.247908	37.886951
2065.138103	223364.260737	37.891968
2066.878399	223734.389527	37.896986
2069.249555	224099.582074	37.902004
2071.272689	224474.164395	37.907021
2073.298932	224841.586322	37.912039
2076.113046	225197.710691	37.917056
2078.059672	225570.773686	37.922074
2080.695159	225929.938958	37.927092
2082.788139	226293.458398	37.932109
2084.728446	226661.244808	37.937127
2086.967039	227033.861600	37.942144
2088.950684	227411.168022	37.947162
2090.788580	227770.975493	37.952180
2093.199611	228147.785558	37.957197
2095.156003	228526.497932	37.962215
2096.916541	228888.531760	37.967232
2098.740335	229270.519138	37.972250
2100.774790	229661.871680	37.977268
2102.456328	230044.240437	37.982285
2104.779735	230434.026597	37.987303
2107.198558	230810.719528	37.992320
2109.409677	231199.942560	37.997338
2111.672669	231581.971407	38.002356
2114.157408	231973.516196	38.007373
2116.164470	232360.465132	38.012391
2118.876287	232733.512678	38.017408
2120.958189	233103.562995	38.022426
2123.561415	233436.653778	38.027444
2126.465460	233742.115403	38.032461
2128.851446	234069.070970	38.037479
2131.613662	234369.299534	38.042496
2133.445494	234684.839488	38.047514
2135.686551	234987.489201	38.052532
2137.762247	235304.160704	38.057549
2139.544433	235615.571383	38.062567
2141.870914	235926.033087	38.067584
2143.788982	236243.214997	38.072602
2145.645909	236562.947444	38.077620
2147.393050	236903.220695	38.082637
2149.263232	237230.496530	38.087655
2151.161582	237567.090386	38.092672
2152.663626	237917.666937	38.097690
2154.839003	238264.023086	38.102708
2156.779150	238631.321360	38.107725
2158.609037	238998.587505	38.112743
2160.723470	239367.333662	38.117760
2162.648111	239752.011303	38.122778
2164.840432	240122.423862	38.127796
2166.533301	240512.804883	38.132813
2168.738222	240904.299749	38.137831
2170.886116	241289.607311	38.142848
2172.859417	241700.978877	38.147866
2175.045507	242089.254675	38.152884
2177.286557	242494.490326	38.157901
2179.655142	242905.650715	38.162919
2181.780447	243305.446199	38.167936
2184.048717	243714.085002	38.172954
2186.554366	244121.264978	38.177972
2188.454055	244536.873705	38.182989
2190.928458	244939.565173	38.188007
2193.470602	245344.888751	38.193024
2195.158052	245752.254117	38.198042
2198.033337	246153.894851	38.203060
2200.711478	246557.523847	38.208077
2202.951864	246963.865093	38.213095
2205.527515	247360.755849	38.218112
2207.627712	247756.707002	38.223130
2210.208016	248143.565579	38.228148
2212.401082	248541.713929	38.233165
2214.341232	248940.487623	38.238183
2217.384976	249314.270049	38.243200
2219.911848	249700.353442	38.248218
2222.090481	250069.905724	38.253236
2224.529588	250463.853895	38.258253
2226.642643	250836.441047	38.263271
2228.910022	251225.160043	38.268288
2230.732473	251600.995530	38.273306
2233.152112	251977.727773	38.278324
2235.247737	252361.294491	38.283341
2237.182838	252744.481026	38.288359
2239.550800	253120.156903	38.293376
2241.396552	253510.420910	38.298394
2243.709305	253875.285725	38.303412
2246.063667	254239.814382	38.308429
2248.339832	254596.354400	38.313447
2250.388380	254954.556874	38.318464
2252.077540	255324.247979	38.323482
2254.311048	255682.320741	38.328500
2256.261092	256052.733792	38.333517
2258.619239	256423.794013	38.338535
2261.601826	256788.506816	38.343552
2263.978676	257167.719464	38.348570
2265.943068	257528.530474	38.353588
2268.073999	257913.346453	38.358605
2270.027195	258294.355417	38.363623
2272.243220	258685.052494	38.368640
2274.498701	259081.815145	38.373658
2277.131717	259458.602781	38.378676
2279.110968	259850.482231	38.383693
2281.355790	260241.659645	38.388711
2283.721379	260641.023555	38.393728
2285.639176	261048.486311	38.398746
2287.976685	261448.541620	38.403764
2289.984559	261860.614484	38.408781
2292.268589	262263.499013	38.413799
2294.589855	262688.986787	38.418816
2296.402204	263117.375505	38.423834
2298.927116	263528.326864	38.428852
2301.035667	263961.724804	38.433869
2302.917715	264400.595401	38.438887
2305.425822	264837.843015	38.443904
2307.545877	265278.429610	38.448922
2309.970029	265722.702691	38.453940
2312.314447	266166.277541	38.458957
2314.421265	266609.560216	38.463975
2317.217095	267053.699345	38.468992
2319.511521	267506.174389	38.474010
2322.462040	267944.878785	38.479028
2324.722154	268390.577241	38.484045
2326.589210	268840.834692	38.489063
2329.699176	269270.750516	38.494080
2332.068396	269723.088153	38.499098
2334.554916	270161.994450	38.504116
2337.269878	270587.070697	38.509133
2339.685464	271036.454805	38.514151
2342.361031	271463.722314	38.519168
2344.515381	271903.494846	38.524186
2347.462217	272329.881281	38.529204
2349.843586	272745.535602	38.534221
2352.299841	273175.683467	38.539239
2355.120491	273587.915018	38.544256
2357.035652	273999.248610	38.549274
2359.392903	274423.518682	38.554292
2361.754857	274845.120647	38.559309
2363.715261	275274.585097	38.564327
2366.183242	275694.290340	38.569344
2368.048653	276117.952367	38.574362
2370.572875	276517.783101	38.579380
2373.018816	276911.529346	38.584397
2374.915978	277318.597654	38.589415
2377.482909	277705.973662	38.594432
2379.663219	278116.781938	38.599450
2381.580441	278517.445016	38.604468
2383.930405	278932.163595	38.609485
2386.213900	279356.113931	38.614503
2388.774597	279768.969659	38.619520
2390.703775	280195.007972	38.624538
2393.017676	280629.520548	38.629556
2395.538024	281051.679520	38.634573
2397.479937	281494.963788	38.639591
2399.848965	281934.572750	38.644608
2402.037554	282384.879304	38.649626
2404.430232	282830.809164	38.654644
2407.126374	283284.870329	38.659661
2409.403615	283745.932502	38.664679
2411.896507	284203.937032	38.669696
2414.272518	284662.874094	38.674714
2416.505019	285134.230062	38.679732
2419.148206	285590.532566	38.684749
2421.380989	286067.247341	38.689767
2423.685345	286529.038587	38.694784
2426.048422	287002.911678	38.699802
2428.492675	287495.620142	38.704820
2430.808593	287984.639352	38.709837
2432.904327	288466.732297	38.714855
2435.512502	288964.086480	38.719872
2437.811092	289468.906435	38.724890
2440.128634	289956.372428	38.729908
2443.196246	290459.188820	38.734925
2445.245398	290962.013219	38.739943
2448.059180	291468.195544	38.744960
2450.455356	291967.939956	38.749978
2453.090261	292473.056164	38.754996
2455.496966	292972.060043	38.760013
2457.953961	293475.246191	38.765031
2460.775139	293978.830674	38.770048
2463.594268	294477.460844	38.775066
2466.374831	294969.999400	38.780084
2469.163245	295464.542247	38.785101
2471.537642	295959.657484	38.790119
2474.220076	296446.797214	38.795136
2476.347708	296944.489139	38.800154
2478.624589	297433.214622	38.805172
2481.578852	297934.176623	38.810189
2483.846907	298427.015802	38.815207
2487.064568	298906.849880	38.820224
2489.649687	299393.234789	38.825242
2492.018460	299891.845198	38.830260
2494.934169	300360.089019	38.835277
2496.899047	300850.784405	38.840295
2500.398822	301316.011650	38.845312
2503.816583	301753.766501	38.850330
2506.450501	302175.540048	38.855348
2509.693244	302584.363031	38.860365
2512.077910	302981.661842	38.865383
2515.073407	303374.290608	38.870400
2517.245436	303763.772077	38.875418
2519.551898	304163.035800	38.880436
2521.992476	304555.622157	38.885453
2524.112700	304967.918124	38.890471
2526.645207	305370.749331	38.895488
2528.568126	305789.601913	38.900506
2530.636658	306208.836474	38.905524
2532.882171	306634.290061	38.910541
2534.821273	307072.719412	38.915559
2536.934929	307507.868364	38.920576
2539.242478	307971.966339	38.925594
2541.362285	308446.252207	38.930612
2543.913826	308914.956053	38.935629
2545.866205	309391.931647	38.940647
2548.464376	309866.720202	38.945664
2550.943863	310362.581688	38.950682
2553.253846	310853.540405	38.955700
2555.752178	311352.391659	38.960717
2558.109003	311870.464748	38.965735
2560.806505	312359.653624	38.970752
2563.574247	312881.898376	38.975770
2565.680904	313398.124220	38.980788
2568.464974	313918.405544	38.985805
2570.772812	314449.554024	38.990823
2573.402826	314973.613363	38.995840
2575.753734	315514.375372	39.000858
2578.352436	316053.393505	39.005876
2581.258599	316595.102925	39.010893
2583.928804	317145.278734	39.015911
2586.829073	317668.493494	39.020928
2589.466944	318218.236440	39.025946
2591.738336	318763.157923	39.030964
2594.581063	319297.852204	39.035981
2597.152492	319844.903850	39.040999
2599.683885	320391.780726	39.046016
2602.357826	320948.231581	39.051034
2605.137533	321494.630528	39.056052
2607.871454	322045.807791	39.061069
2610.090668	322595.590068	39.066087
2612.901171	323154.646222	39.071104
2615.173084	323719.574213	39.076122
2617.380417	324284.432387	39.081140
2620.304890	324845.693865	39.086157
2622.657637	325414.000330	39.091175
2625.576015	325993.488578	39.096192
2628.615311	326563.252558	39.101210
2630.956499	327130.481923	39.106228
2633.634144	327694.962003	39.111245
2635.748746	328279.614055	39.116263
2638.945148	328853.602426	39.121280
2641.259214	329422.037919	39.126298
2643.696743	329973.105540	39.131316
2646.814811	330514.690978	39.136333
2649.469498	331054.187344	39.141351
2652.107256	331589.263926	39.146368
2654.885998	332124.441123	39.151386
2657.336954	332666.903145	39.156404
2660.449941	333191.582817	39.161421
2663.230294	333734.035133	39.166439
2666.405394	334259.712542	39.171456
2669.523051	334786.461458	39.176474
2672.048516	335318.911665	39.181492
2674.741637	335832.439693	39.186509
2677.643113	336358.397945	39.191527
2680.226102	336885.646610	39.196544
2682.915626	337422.497341	39.201562
2685.551006	337964.176448	39.206580
2688.101815	338499.592894	39.211597
2690.618108	339041.510239	39.216615
2693.154525	339577.529218	39.221632
2696.271756	340126.070413	39.226650
2698.525307	340689.241084	39.231668
2701.079743	341227.756524	39.236685
2703.480231	341790.309837	39.241703
2706.023798	342364.311091	39.246720
2708.524871	342933.642047	39.251738
2710.881502	343508.195078	39.256756
2713.647529	344095.498750	39.261773
2715.946002	344696.097731	39.266791
2718.680886	345289.284311	39.271808
2721.422693	345882.133636	39.276826
2723.828376	346495.289032	39.281844
2726.722027	347099.652772	39.286861
2729.256025	347722.243808	39.291879
2731.487393	348345.155048	39.296896
2734.669392	348951.103100	39.301914
2737.212731	349578.038098	39.306932
2740.207068	350208.270692	39.311949
2743.256353	350837.725636	39.316967
2745.797172	351467.507522	39.321984
2748.839438	352086.439419	39.327002
2751.712231	352723.337552	39.332020
2754.639137	353351.918753	39.337037
2757.917635	353971.044654	39.342055
2760.375802	354598.897942	39.347072
2763.192243	355226.026773	39.352090
2765.765903	355854.506151	39.357108
2768.893009	356473.320813	39.362125
2771.826095	357111.423500	39.367143
2774.693577	357732.065649	39.372160
2778.147862	358337.860366	39.377178
2781.133633	358958.112817	39.382196
2783.959169	359569.067898	39.387213
2786.887482	360179.745093	39.392231
2789.899010	360785.832827	39.397248
2792.632678	361390.383219	39.402266
2794.964016	361965.600036	39.407284
2798.019917	362523.005694	39.412301
2800.911970	363095.429506	39.417319
2803.635619	363652.645693	39.422336
2806.318278	364207.272981	39.427354
2808.521663	364783.033087	39.432372
2811.527704	365358.633363	39.437389
2814.332641	365925.782058	39.442407
2816.959507	366506.807552	39.447424
2819.714237	367089.200879	39.452442
2822.486716	367679.399576	39.457460
2825.147703	368256.184061	39.462477
2827.949816	368858.923167	39.467495
2830.432355	369457.136897	39.472512
2833.593546	370051.403207	39.477530
2836.138005	370659.790992	39.482548
2838.841741	371275.452569	39.487565
2841.392880	371888.363543	39.492583
2844.060367	372510.686013	39.497600
2846.676224	373148.408756	39.502618
2849.385363	373788.973972	39.507636
2852.640784	374426.220404	39.512653
2855.621855	375073.420680	39.517671
2858.201632	375713.976072	39.522688
2860.981265	376353.855334	39.527706
2864.014518	377021.109814	39.532724
2866.774383	377673.529425	39.537741
2869.425534	378333.439525	39.542759
2872.124894	378999.064339	39.547776
2875.440393	379659.506442	39.552794
2878.079173	380335.316203	39.557812
2881.039257	381001.448735	39.562829
2884.020946	381686.566519	39.567847
2886.739045	382372.779074	39.572864
2889.585220	383046.300908	39.577882
2892.673129	383734.459373	39.582900
2895.319559	384421.939395	39.587917
2898.008969	385116.146980	39.592935
2901.192908	385813.991780	39.597952
2904.584493	386490.053199	39.602970
2907.341453	387191.769179	39.607988
2910.300047	387889.609730	39.613005
2913.500632	388575.325697	39.618023
2916.470959	389264.438098	39.623040
2919.971431	389939.859235	39.628058
2923.014139	390633.498578	39.633076
2926.025007	391308.767976	39.638093
2929.041985	391993.153015	39.643111
2931.819211	392677.638539	39.648128
2935.108518	393361.395393	39.653146
2937.813542	394035.239682	39.658164
2941.123768	394703.294550	39.663181
2944.311050	395398.463162	39.668199
2947.096028	396065.458419	39.673216
2950.855244	396709.743967	39.678234
2953.865086	397320.893503	39.683252
2957.047897	397945.265477	39.688269
2960.322216	398545.726350	39.693287
2963.030878	399143.147084	39.698304
2965.965898	399754.136377	39.703322
2968.962059	400371.468322	39.708340
2971.765868	400973.023677	39.713357
2974.518360	401580.635253	39.718375
2976.879010	402198.843941	39.723392
2979.981953	402811.624551	39.728410
2983.072171	403442.547001	39.733428
2985.344431	404081.571834	39.738445
2988.474764	404709.242909	39.743463
2990.922168	405355.793767	39.748480
2993.879350	406001.642082	39.753498
2996.369978	406669.173337	39.758516
2999.708879	407334.020997	39.763533
3002.748471	407983.211273	39.768551
3005.688789	408649.386058	39.773568
3008.458480	409327.257998	39.778586
3011.755299	410011.646581	39.783604
3014.713112	410684.414233	39.788621
3017.874746	411367.880696	39.793639
3020.612254	412057.151693	39.798656
3023.654431	412736.626363	39.803674
3026.471341	413439.994219	39.808692
3029.497865	414148.456500	39.813709
3032.446289	414857.547411	39.818727
3034.851499	415574.486670	39.823744
3037.795460	416301.889854	39.828762
3040.835951	417019.883462	39.833780
3043.701371	417759.399782	39.838797
3046.492600	418496.121272	39.843815
3049.083344	419248.108710	39.848832
3052.119669	420001.221650	39.853850
3055.045632	420772.320720	39.858868
3057.852181	421544.861388	39.863885
3061.404332	422310.193906	39.868903
3064.287166	423100.362788	39.873920
3067.140586	423875.971864	39.878938
3070.286858	424661.746985	39.883956
3073.462641	425440.756175	39.888973
3076.571421	426227.504829	39.893991
3079.529812	427041.814015	39.899008
3082.879236	427820.321045	39.904026
3086.103156	428626.509905	39.909044
3089.068694	429425.952225	39.914061
3092.460921	430218.185511	39.919079
3095.320429	431027.245402	39.924096
3098.511455	431823.285894	39.929114
3101.836743	432617.127882	39.934132
3105.227467	433436.158194	39.939149
3108.781595	434212.643056	39.944167
3111.609358	435014.314158	39.949184
3115.303950	435778.750951	39.954202
3118.205403	436542.150494	39.959220
3121.205030	437284.900153	39.964237
3124.355608	438032.338583	39.969255
3127.145487	438774.722366	39.974272
3130.622742	439511.050533	39.979290
3133.743394	440254.400689	39.984308
3136.643535	441012.294988	39.989325
3140.051993	441753.022210	39.994343
3142.725108	442512.728308	39.999360
3146.114616	443264.145849	40.004378
3149.191230	444017.462561	40.009396
3152.121551	444785.713254	40.014413
3155.008075	445567.462681	40.019431
3157.640246	446342.443109	40.024448
3160.610647	447126.608127	40.029466
3163.608730	447920.663865	40.034484
3166.704671	448716.043764	40.039501
3170.451432	449516.304404	40.044519
3174.081354	450293.830210	40.049536
3178.383273	451068.844664	40.054554
3181.744367	451857.292255	40.059572
3184.978431	452635.560339	40.064589
3188.696134	453420.152314	40.069607
3191.755612	454202.392123	40.074624
3195.023553	454973.590823	40.079642
3198.163740	455761.228721	40.084660
3201.140960	456541.679404	40.089677
3204.489402	457323.157096	40.094695
3207.544596	458122.615226	40.099712
3210.741383	458908.917970	40.104730
3213.710674	459710.709823	40.109748
3216.002604	460526.289439	40.114765
3219.330264	461339.904009	40.119783
3222.302933	462168.467243	40.124800
3225.345984	462987.679836	40.129818
3228.314554	463829.635232	40.134836
3231.315429	464683.337650	40.139853
3234.362032	465517.727967	40.144871
3237.696487	466379.907692	40.149888
3240.978148	467225.674218	40.154906
3244.538066	468108.128961	40.159924
3247.135785	468975.072250	40.164941
3250.890297	469838.762275	40.169959
3253.954094	470710.059831	40.174976
3257.143634	471586.609842	40.179994
3260.591016	472473.396204	40.185012
3263.902737	473344.036874	40.190029
3267.543904	474211.756863	40.195047
3270.323115	475101.820302	40.200064
3273.569280	475974.380212	40.205082
3277.189720	476865.445673	40.210100
3279.718528	477742.338655	40.215117
3283.357189	478634.181325	40.220135
3286.447534	479537.291255	40.225152
3289.710051	480403.133677	40.230170
3293.333441	481271.559352	40.235188
3296.175144	482116.216291	40.240205
3299.671139	482961.743730	40.245223
3302.745255	483808.362106	40.250240
3306.060476	484656.926370	40.255258
3308.943620	485506.835160	40.260276
3312.259742	486365.985032	40.265293
3315.965141	487225.186109	40.270311
3318.933366	488095.579555	40.275328
3322.259864	488953.650496	40.280346
3325.896052	489821.585132	40.285364
3329.383554	490698.696682	40.290381
3333.156256	491563.144266	40.295399
3336.311509	492434.063969	40.300416
3339.580185	493322.400301	40.305434
3343.042013	494200.511679	40.310452
3346.014483	495080.072430	40.315469
3349.725792	495969.826515	40.320487
3352.420333	496859.293825	40.325504
3355.673545	497762.919249	40.330522
3359.209211	498667.262595	40.335540
3362.288075	499586.173757	40.340557
3365.869451	500494.204388	40.345575
3368.766652	501422.086962	40.350592
3372.360878	502346.327488	40.355610
3375.937066	503277.539134	40.360628
3378.977302	504216.509150	40.365645
3382.350784	505150.682014	40.370663
3385.894176	506093.206685	40.375680
3389.593728	507021.978461	40.380698
3393.835019	507961.818136	40.385716
3396.975334	508904.354180	40.390733
3400.979725	509825.407473	40.395751
3404.312368	510746.618190	40.400768
3407.668839	511695.374128	40.405786
3411.362243	512637.666677	40.410804
3414.313781	513576.946454	40.415821
3417.646194	514505.418837	40.420839
3420.582361	515473.298859	40.425856
3424.324294	516417.893427	40.430874
3428.205395	517372.348481	40.435892
3431.122248	518324.732141	40.440909
3434.825312	519290.502624	40.445927
3438.317536	520238.750663	40.450944
3441.698205	521195.029444	40.455962
3445.173176	522143.824883	40.460980
3448.221961	523118.195138	40.465997
3451.599178	524088.370848	40.471015
3454.839451	525053.821121	40.476032
3458.223359	526039.758123	40.481050
3461.915467	527019.032402	40.486068
3465.350438	527998.085294	40.491085
3469.289991	528968.782339	40.496103
3473.349434	529917.326030	40.501120
3477.247257	530858.180616	40.506125
3480.999329	531748.156747	40.511130
3484.358783	532591.464743	40.516135
3488.240478	533343.058449	40.521140
3491.505470	534045.209391	40.526144
3494.615683	534664.765861	40.531149
3498.010538	535210.659127	40.536154
3500.404448	535708.556551	40.541159
3503.036779	536140.033805	40.546164
3505.255977	536498.684190	40.551168
3507.119274	536802.988615	40.556173
3509.446067	537038.023084	40.561178
3510.567745	537259.103429	40.566183
3511.957896	537414.787425	40.571188
3513.483791	537514.744063	40.576192
3514.626660	537580.469477	40.581197
3515.546065	537637.392037	40.586202
3516.990210	537641.608227	40.591207
3518.071395	537588.460672	40.596212
3518.856165	537534.652746	40.601216
3519.225448	537456.769967	40.606221
3520.150782	537328.194728	40.611226
3520.510482	537197.637157	40.616231
3521.199165	537028.239260	40.621236
3521.287659	536876.560513	40.626240
3521.799681	536679.409034	40.631245
3522.251589	536475.395690	40.636250
3522.017468	536251.790411	40.641255
3522.059561	536017.632634	40.646260
3522.273439	535795.162062	40.651264
3522.211339	535535.658196	40.656269
3522.835643	535297.710240	40.661274
3522.719412	535023.861449	40.666279
3522.771190	534767.104704	40.671284
3522.561713	534501.090659	40.676288
3522.490938	534218.279629	40.681293
3522.485712	533944.242563	40.686298
3522.293635	533670.886867	40.691303
3522.354087	533374.046902	40.696308
3522.102118	533099.831807	40.701312
3522.176861	532811.768791	40.706317
3521.993818	532524.094805	40.711322
3521.739021	532248.147459	40.716327
3521.714329	531957.962492	40.721332
3521.632329	531660.152382	40.726336
3521.489559	531372.955969	40.731341
3521.697427	531089.538653	40.736346
3521.151156	530798.151455	40.741351
3520.987016	530507.203686	40.746356
3520.690698	530231.732502	40.751360
3520.457306	529954.427548	40.756365
3520.602339	529663.516312	40.761370
3520.062360	529391.454286	40.766375
3519.810276	529099.685861	40.771380
3519.421073	528852.754652	40.776384
3519.471829	528568.710283	40.781389
3519.429651	528297.106530	40.786394
3518.819478	528036.957922	40.791399
3518.466837	527757.460209	40.796404
3518.456602	527513.530768	40.801408
3517.984642	527262.999807	40.806413
3517.977856	527002.435625	40.811418
3518.027064	526766.065815	40.816423
3517.839177	526511.435099	40.821428
3517.637615	526277.523508	40.826432
3517.078696	526032.293501	40.831437
3516.687606	525788.246171	40.836442
3516.781782	525559.179741	40.841447
3516.899635	525330.055745	40.846452
3516.652884	525096.791043	40.851456
3516.068190	524876.363871	40.856461
3516.203429	524646.570282	40.861466
3516.233236	524427.556140	40.866471
3516.047137	524207.309496	40.871476
3515.433269	523987.986733	40.876480
3515.663314	523766.050787	40.881485
3515.699999	523550.561903	40.886490
3514.701693	523358.435407	40.891495
3514.686764	523137.793237	40.896500
3514.855842	522926.773951	40.901504
3514.127295	522732.575377	40.906509
3514.062591	522552.171021	40.911514
3513.975509	522362.567838	40.916519
3514.023864	522162.678972	40.921524
3513.695216	521978.720752	40.926528
3513.780286	521795.150033	40.931533
3513.530657	521604.299847	40.936538
3512.945295	521439.434848	40.941543
3512.938532	521265.376858	40.946548
3512.876617	521088.039626	40.951552
3512.895868	520919.888807	40.956557
3512.555387	520740.872924	40.961562
3512.370207	520575.986482	40.966567
3512.445651	520423.797656	40.971572
3511.890187	520254.214091	40.976576
3511.944305	520094.087963	40.981581
3511.910184	519938.979549	40.986586
3511.517323	519798.133555	40.991591
3511.304529	519645.932487	40.996596
3511.132379	519493.319099	41.001600
3510.992520	519360.872922	41.006605
3510.930893	519219.868478	41.011610
3510.506552	519091.863913	41.016615
3510.764340	518942.615629	41.021620
3510.497333	518822.168392	41.026624
3510.312674	518701.505004	41.031629
3510.548961	518562.015270	41.036634
3510.112017	518443.918028	41.041639
3510.168333	518315.325807	41.046644
3510.075852	518182.407568	41.051648
3509.909382	518062.393957	41.056653
3510.134656	517943.076030	41.061658
3509.453435	517824.608437	41.066663
3509.451503	517703.453768	41.071668
3509.150956	517599.285070	41.076672
3509.091077	517491.133491	41.081677
3509.317085	517374.187962	41.086682
3509.226352	517277.923062	41.091687
3508.940634	517172.839124	41.096692
3509.240772	517069.077815	41.101696
3509.056837	516966.656571	41.106701
3508.920475	516864.732857	41.111706
3508.556570	516749.443778	41.116711
3508.784729	516654.591344	41.121716
3508.531223	516549.194944	41.126720
3508.266508	516455.076675	41.131725
3508.328204	516362.069387	41.136730
3508.268208	516268.676252	41.141735
3508.340085	516164.995940	41.146740
3507.981168	516083.988211	41.151744
3507.888395	515989.233277	41.156749
3507.978048	515905.524083	41.161754
3507.746978	515812.408282	41.166759
3507.748093	515737.663404	41.171764
3507.620024	515650.750748	41.176768
3507.257186	515588.048300	41.181773
3507.273991	515499.038491	41.186778
3507.055595	515436.160923	41.191783
3507.544706	515353.801855	41.196788
3507.464846	515277.196512	41.201792
3507.328855	515189.928693	41.206797
3507.558294	515117.218457	41.211802
3507.180909	515045.817594	41.216807
3507.403870	514972.146847	41.221812
3507.131788	514889.197767	41.226816
3506.744502	514829.631943	41.231821
3506.985017	514760.104599	41.236826
3506.782764	514695.906747	41.241831
3506.900933	514619.064786	41.246836
3506.677149	514563.720485	41.251840
3506.572111	514490.402913	41.256845
3506.508718	514430.683320	41.261850
3506.478566	514373.841089	41.266855
3506.478844	514306.069414	41.271860
3506.556676	514239.954226	41.276864
3506.574466	514185.582018	41.281869
3506.530165	514128.943498	41.286874
3506.269025	514070.619449	41.291879
3506.430552	514015.869934	41.296884
3506.334476	513955.597468	41.301888
3506.283438	513887.933369	41.306893
3506.471806	513831.813421	41.311898
3506.177713	513781.585983	41.316903
3505.994549	513721.427597	41.321908
3505.796263	513669.920234	41.326912
3505.743701	513635.940307	41.331917
3505.981725	513567.015349	41.336922
3505.990616	513528.979223	41.341927
3505.978957	513471.372335	41.346932
3505.924451	513425.759198	41.351936
3505.550263	513372.660206	41.356941
3505.693502	513319.630998	41.361946
3505.160351	513287.446019	41.366951
3505.875569	513242.469408	41.371956
3505.448701	513200.101013	41.376960
3505.280251	513150.610522	41.381965
3505.529742	513108.994843	41.386970
3505.268547	513079.598945	41.391975
3505.523320	513029.029603	41.396980
3505.395150	512989.496523	41.401984
3505.470232	512943.709857	41.406989
3505.714893	512895.468403	41.411994
3505.296010	512853.047292	41.416999
3505.357919	512815.810463	41.422004
3505.278247	512781.074386	41.427008
3505.337353	512738.577434	41.432013
3505.469109	512708.967035	41.437018
3505.007170	512672.520824	41.442023
3505.161891	512630.615460	41.447028
3504.947587	512599.896202	41.452032
3504.863653	512552.919659	41.457037
3504.904213	512528.381498	41.462042
3504.835554	512504.214635	41.467047
3504.984605	512459.173685	41.472052
3505.078815	512428.455932	41.477056
3505.323863	512397.056717	41.482061
3505.299490	512350.474851	41.487066
3505.207941	512312.502439	41.492071
3505.324979	512277.936562	41.497076
3504.707184	512252.945658	41.502080
3504.629194	512217.247092	41.507085
3504.759951	512174.889143	41.512090
3504.800888	512145.342695	41.517095
3504.652030	512117.191927	41.522100
3504.870107	512083.874252	41.527104
3504.949457	512063.628822	41.532109
3505.141254	512027.027302	41.537114
3504.830471	512009.069124	41.542119
3504.920177	511966.160729	41.547124
3504.702627	511940.043851	41.552128
3504.423492	511902.656584	41.557133
3504.739365	511874.229621	41.562138
3504.780785	511848.071667	41.567143
3504.749651	511821.874557	41.572148
3504.747189	511804.525014	41.577152
3504.893396	511769.498237	41.582157
3504.810366	511736.682726	41.587162
3504.567621	511698.985754	41.592167
3504.919374	511665.949631	41.597172
3504.517351	511645.526870	41.602176
3504.436803	511632.084469	41.607181
3504.854023	511583.204989	41.612186
3504.502426	511565.606882	41.617191
3504.811536	511536.016982	41.622196
3504.573057	511513.089572	41.627200
3504.567117	511486.432701	41.632205
3504.945547	511448.788741	41.637210
3504.227288	511432.462483	41.642215
3504.488754	511397.416719	41.647220
3504.570385	511364.523876	41.652224
3504.337572	511352.976965	41.657229
3504.676152	511328.491128	41.662234
3504.129502	511298.074963	41.667239
3504.198534	511271.911756	41.672244
3504.492943	511269.032695	41.677248
3504.350222	511246.797983	41.682253
3504.201080	511223.198451	41.687258
3504.348424	511203.244760	41.692263
3504.672333	511182.605525	41.697268
3504.719675	511155.079758	41.702272
3504.141436	511138.933426	41.707277
3504.435120	511111.166308	41.712282
3504.109036	511082.485392	41.717287
3504.535832	511073.919763	41.722292
3504.542860	511030.465626	41.727296
3504.200813	511018.682823	41.732301
3504.195621	510982.970150	41.737306
3504.269657	510972.993232	41.742311
3504.551249	510950.235788	41.747316
3504.386851	510929.471085	41.752320
3504.218367	510907.290587	41.757325
3504.662841	510886.834282	41.762330
3504.474770	510864.859170	41.767335
3504.358077	510840.899873	41.772340
3504.663216	510803.063722	41.777344
3504.284167	510784.912690	41.782349
3504.378811	510763.044519	41.787354
3504.724530	510734.712108	41.792359
3504.764121	510710.373816	41.797364
3504.400414	510689.893259	41.802368
3504.149118	510661.351571	41.807373
3504.632373	510640.130035	41.812378
3504.437519	510619.875640	41.817383
3504.388494	510597.018221	41.822388
3504.225133	510575.949399	41.827392
3504.115639	510564.534221	41.832397
3504.687556	510533.838705	41.837402
3504.262855	510525.913267	41.842407
3504.466463	510486.625427	41.847412
3504.265851	510475.730467	41.852416
3504.399388	510455.778082	41.857421
3504.349783	510430.947614	41.862426
3504.128986	510412.922933	41.867431
3504.350363	510381.574322	41.872436
3504.266507	510349.059789	41.877440
3504.214728	510335.763579	41.882445
3504.596488	510298.774195	41.887450
3504.156119	510292.722886	41.892455
3504.562069	510261.547233	41.897460
3504.443756	510250.183825	41.902464
3503.965753	510223.194885	41.907469
3504.074462	510212.655570	41.912474
3504.091895	510181.642358	41.917479
3503.970327	510163.804083	41.922484
3504.178309	510156.233764	41.927488
3503.957038	510133.858247	41.932493
3504.379668	510127.164582	41.937498
3504.103035	510102.470698	41.942503
3504.127339	510072.771509	41.947508
3503.982464	510057.921545	41.952512
3504.051890	510036.865850	41.957517
3504.322478	510030.145591	41.962522
3504.415864	510007.011926	41.967527
3504.067450	509988.399900	41.972532
3504.007805	509963.570337	41.977536
3503.996863	509953.049775	41.982541
3504.517744	509932.175538	41.987546
3503.811337	509929.909751	41.992551
3504.262738	509899.586270	41.997556
3503.954369	509880.512492	42.002560
3504.108799	509882.461315	42.007565
3503.935312	509847.582294	42.012570
3503.786340	509840.523563	42.017575
3503.754013	509819.938989	42.022580
3503.936937	509807.870008	42.027584
3503.718719	509795.763245	42.032589
3504.186255	509778.387936	42.037594
3503.998748	509762.532660	42.042599
3504.067066	509756.147804	42.047604
3504.045712	509726.859949	42.052608
3503.983637	509721.558076	42.057613
3504.043784	509700.301074	42.062618
3504.014515	509683.004195	42.067623
3504.045183	509661.094135	42.072628
3504.066087	509645.104628	42.077632
3503.814998	509635.583040	42.082637
3503.993727	509626.701769	42.087642
3503.954140	509608.242873	42.092647
3503.761851	509589.808094	42.097652
3503.769339	509588.441222	42.102656
3503.848329	509561.767914	42.107661
3503.861606	509548.460808	42.112666
3503.785062	509558.742991	42.117671
3503.969150	509530.332951	42.122676
3504.220877	509517.645805	42.127680
3503.859127	509493.571579	42.132685
3504.057369	509468.751125	42.137690
3504.073719	509462.829689	42.142695
3504.211559	509438.575236	42.147700
3504.006702	509430.310993	42.152704
3503.867097	509414.447822	42.157709
3503.976165	509386.251764	42.162714
3503.603537	509383.730779	42.167719
3503.704341	509368.689610	42.172724
3503.986832	509349.319480	42.177728
3503.873257	509332.996801	42.182733
3504.075428	509328.209539	42.187738
3504.145402	509315.196836	42.192743
3504.072769	509305.292719	42.197748
3504.036332	509277.625392	42.202752
3503.968818	509260.283540	42.207757
3504.044399	509248.281724	42.212762
3503.951909	509231.702659	42.217767
3504.139011	509215.838254	42.222772
3504.192959	509190.028379	42.227776
3503.851850	509181.583186	42.232781
3504.069719	509160.300583	42.237786
3503.664089	509145.035718	42.242791
3503.868509	509133.671146	42.247796
3504.044998	509126.914817	42.252800
3504.129791	509103.174190	42.257805
3503.870508	509091.174602	42.262810
3503.844145	509080.251207	42.267815
3504.210150	509055.403638	42.272820
3504.245659	509036.932256	42.277824
3503.961426	509025.341301	42.282829
3504.110788	509012.467595	42.287834
3504.091043	508990.564645	42.292839
3504.208484	508966.160972	42.297844
3504.097136	508955.655667	42.302848
3503.984222	508927.240982	42.307853
3504.348823	508909.273959	42.312858
3503.835843	508901.058162	42.317863
3504.182496	508877.326425	42.322868
3503.983983	508858.183548	42.327872
3503.920177	508853.286419	42.332877
3503.955958	508832.183969	42.337882
3504.092918	508812.431498	42.342887
3503.860491	508792.383243	42.347892
3504.145738	508786.267293	42.352896
3504.124193	508774.381683	42.357901
3504.170786	508753.378612	42.362906
3503.758326	508725.010939	42.367911
3504.045890	508707.460624	42.372916
3504.186861	508700.962706	42.377920
3504.155350	508677.239874	42.382925
3503.976375	508664.620178	42.387930
3503.960435	508640.439497	42.392935
3504.082220	508616.742943	42.397940
3504.150751	508606.866702	42.402944
3504.008120	508609.216778	42.407949
3504.107027	508590.077184	42.412954
3503.944652	508571.636580	42.417959
3504.125160	508549.600228	42.422964
3504.158524	508540.083660	42.427968
3504.056123	508525.529212	42.432973
3504.257460	508499.189067	42.437978
3504.372239	508474.380369	42.442983
3504.217005	508458.114035	42.447988
3504.030650	508444.635253	42.452992
3503.936646	508427.499121	42.457997
3504.061236	508405.572610	42.463002
3503.667187	508395.263429	42.468007
3503.858345	508372.618042	42.473012
3504.074444	508366.057529	42.478016
3503.692653	508338.443276	42.483021
3503.701393	508334.546411	42.488026
3503.881161	508333.911116	42.493031
3503.823954	508308.876395	42.498036
3504.049123	508296.496111	42.503040
3503.913911	508285.387039	42.508045
3503.897414	508263.634431	42.513050
3503.630320	508258.718672	42.518055
3504.091356	508238.509563	42.523060
3504.243698	508226.191334	42.528064
3503.987844	508206.146098	42.533069
3504.203096	508181.219907	42.538074
3503.985786	508170.275521	42.543079
3504.178105	508145.555282	42.548084
3504.339805	508130.149242	42.553088
3503.912009	508112.660800	42.558093
3503.947821	508088.977109	42.563098
3503.817113	508073.263075	42.568103
3503.914310	508063.685560	42.573108
3504.200631	508042.947297	42.578112
3503.862031	508037.992182	42.583117
3503.711229	508001.385595	42.588122
3503.910581	507991.994272	42.593127
3503.870186	507986.486057	42.598132
3503.666881	507973.970888	42.603136
3503.535741	507954.158620	42.608141
3504.261213	507945.898392	42.613146
3503.779215	507945.570066	42.618151
3504.002258	507921.198814	42.623156
3503.764596	507914.153306	42.628160
3503.891220	507915.449013	42.633165
3504.245411	507885.997465	42.638170
3503.770435	507875.346596	42.643175
3503.850273	507838.197253	42.648180
3503.996081	507844.650661	42.653184
3503.196617	507843.006439	42.658189
3503.919292	507822.502511	42.663194
3503.495556	507805.519069	42.668199
3503.394147	507804.675222	42.673204
3503.961113	507792.240550	42.678208
3503.606259	507789.412943	42.683213
3503.591862	507760.677184	42.688218
3503.506100	507754.821896	42.693223
3503.892979	507747.778794	42.698228
3503.928453	507738.868598	42.703232
3503.781484	507732.264042	42.708237
3504.102652	507715.769916	42.713242
3503.689314	507708.701497	42.718247
3503.534611	507687.830135	42.723252
3503.862786	507674.977761	42.728256
3503.350835	507668.380276	42.733261
3503.681454	507667.670517	42.738266
3503.407105	507643.326898	42.743271
3503.759778	507630.116447	42.748276
3503.664755	507630.688270	42.753280
3503.491432	507631.373662	42.758285
3503.645232	507615.260067	42.763290
3503.298618	507598.365422	42.768295
3503.429793	507588.326907	42.773300
3503.395141	507584.892096	42.778304
3503.418892	507581.701033	42.783309
3503.420556	507568.242441	42.788314
3503.558271	507550.512250	42.793319
3503.683528	507538.349600	42.798324
3503.756494	507546.787888	42.803329
3503.680699	507541.993473	42.808333
3504.050331	507520.836645	42.813338
3503.586302	507511.347534	42.818343
3503.857894	507494.861034	42.823348
3504.091614	507482.832990	42.828353
3503.952464	507460.896370	42.833357
3504.035789	507463.463868	42.838362
3503.551621	507442.340707	42.843367
3503.731104	507411.398069	42.848372
3503.605949	507422.448162	42.853377
3503.276212	507417.693852	42.858381
3503.685843	507388.536273	42.863386
3503.576578	507382.482186	42.868391
3503.630289	507383.334088	42.873396
3503.605099	507373.168374	42.878401
3503.668152	507365.569142	42.883405
3503.956413	507338.403936	42.888410
3503.716955	507349.927514	42.893415
3503.654749	507334.050188	42.898420
3503.924291	507299.753722	42.903425
3503.494128	507303.920317	42.908429
3504.198056	507286.150954	42.913434
3503.629562	507286.949418	42.918439
3503.536008	507279.273708	42.923444
3503.462352	507272.505596	42.928449
3503.754526	507261.277712	42.933453
3503.710526	507244.436080	42.938458
3503.229006	507242.437958	42.943463
3503.616550	507221.075544	42.948468
3503.565055	507217.491530	42.953473
3503.384775	507215.091608	42.958477
3503.677184	507216.816537	42.963482
3503.810465	507198.833701	42.968487
3504.006737	507176.995494	42.973492
3503.656716	507171.282972	42.978497
3503.813568	507165.439732	42.983501
3503.752287	507140.555751	42.988506
3503.872986	507147.974740	42.993511
3503.739621	507122.343165	42.998516
3503.754346	507114.447876	43.003521
3503.448489	507115.660212	43.008525
3503.606822	507104.402784	43.013530
3503.372594	507085.820153	43.018535
3503.536961	507075.877290	43.023540
3503.685939	507064.216533	43.028545
3503.516043	507067.633678	43.033549
3503.839521	507052.707082	43.038554
3503.608407	507041.764160	43.043559
3503.662088	507021.112042	43.048564
3503.671392	507019.845875	43.053569
3503.584651	507013.889294	43.058573
3503.429041	506983.302444	43.063578
3503.462310	506977.731664	43.068583
3503.631299	506981.702435	43.073588
3503.241453	506982.776261	43.078593
3503.103866	506982.241680	43.083597
3503.542413	506977.719993	43.088602
3503.543181	506969.422061	43.093607
3503.648003	506949.874929	43.098612
3503.932542	506936.269936	43.103617
3503.777221	506933.764833	43.108621
3503.806738	506906.943437	43.113626
3503.599912	506906.419798	43.118631
3504.030389	506891.627945	43.123636
3504.035307	506877.358730	43.128641
3503.782972	506864.344524	43.133645
3503.879223	506848.593499	43.138650
3503.519423	506843.438995	43.143655
3503.673386	506818.520527	43.148660
3503.649582	506817.664365	43.153665
3503.679986	506809.462869	43.158669
3503.662153	506788.467589	43.163674
3503.500971	506776.147286	43.168679
3503.757082	506771.704982	43.173684
3503.430987	506779.498343	43.178689
3503.505684	506781.510723	43.183693
3503.872947	506736.369618	43.188698
3503.559419	506738.746959	43.193703
3503.379274	506730.123319	43.198708
3503.512530	506724.536653	43.203713
3503.332283	506702.757363	43.208717
3503.478991	506689.781147	43.213722
3503.435895	506684.880128	43.218727
3503.896262	506678.988749	43.223732
3503.679529	506684.285527	43.228737
3503.508897	506657.444783	43.233741
3503.672187	506642.796149	43.238746
3503.519343	506640.341211	43.243751
3503.654951	506647.353267	43.248756
3503.547817	506633.000365	43.253761
3503.913698	506617.206511	43.258765
3504.187749	506618.226019	43.263770
3503.377904	506591.435611	43.268775
3504.055378	506571.595140	43.273780
3503.884006	506573.444042	43.278785
3503.549166	506562.163018	43.283789
3503.873126	506532.562150	43.288794
3503.964118	506531.434832	43.293799
3503.892305	506519.656812	43.298804
3504.027154	506498.029855	43.303809
3503.682936	506493.985968	43.308813
3503.942635	506476.184797	43.313818
3503.588384	506459.138445	43.318823
3503.853709	506448.976867	43.323828
3503.589676	506453.370401	43.328833
3503.511208	506439.316403	43.333837
3503.619386	506414.050395	43.338842
3503.709474	506413.024412	43.343847
3503.335389	506404.481864	43.348852
3503.418342	506405.076194	43.353857
3503.582443	506396.802770	43.358861
3503.658185	506373.464615	43.363866
3503.490115	506378.551394	43.368871
3503.654681	506361.018141	43.373876
3503.572844	506360.626526	43.378881
3503.596149	506343.216783	43.383885
3503.721743	506327.055849	43.388890
3503.860125	506325.111431	43.393895
3503.804925	506310.345253	43.398900
3503.360205	506289.669844	43.403905
3503.441551	506296.184621	43.408909
3503.401425	506278.228240	43.413914
3503.442848	506294.211515	43.418919
3503.858182	506275.424140	43.423924
3503.629469	506251.020745	43.428929
3503.433059	506248.977437	43.433933
3503.768823	506243.004408	43.438938
3503.333774	506245.704624	43.443943
3503.302380	506225.925207	43.448948
3503.571084	506203.669525	43.453953
3503.456540	506197.059255	43.458957
3503.558254	506192.995410	43.463962
3503.375363	506201.525397	43.468967
3503.478907	506183.596809	43.473972
3503.821210	506162.645046	43.478977
3503.575757	506164.556302	43.483981
3503.689070	506143.235909	43.488986
3503.669211	506158.267589	43.493991
3503.295712	506137.428940	43.498996
3503.625633	506123.512536	43.504001
3503.438084	506115.648765	43.509005
3503.417474	506113.122249	43.514010
3503.268678	506108.338975	43.519015
3503.602651	506109.197241	43.524020
3503.610552	506091.992082	43.529025
3503.092557	506084.737135	43.534029
3503.623349	506074.179174	43.539034
3503.953078	506066.891424	43.544039
3503.502556	506061.346220	43.549044
3503.728140	506035.656300	43.554049
3503.439633	506038.788790	43.559053
3503.797885	506031.698919	43.564058
3503.206436	506037.814132	43.569063
3503.586111	506014.427453	43.574068
3503.376411	505997.661402	43.579073
3503.176187	505990.305585	43.584077
3503.318944	505981.731733	43.589082
3503.568919	505988.169371	43.594087
3503.314130	505984.263029	43.599092
3503.762043	505988.999553	43.604097
3503.384944	505978.686242	43.609101
3503.583958	505968.534866	43.614106
3503.477052	505960.810080	43.619111
3503.519094	505964.446945	43.624116
3503.431041	505964.916518	43.629121
3503.410771	505947.614468	43.634125
3503.418688	505929.751334	43.639130
3503.474607	505923.771829	43.644135
3503.611156	505922.384266	43.649140
3503.517649	505929.534031	43.654145
3503.309626	505909.276163	43.659149
3503.780573	505870.239141	43.664154
3503.396950	505886.289977	43.669159
3503.485472	505878.129455	43.674164
3503.648578	505876.434084	43.679169
3503.312364	505862.167355	43.684173
3503.308321	505841.826564	43.689178
3503.449392	505842.462329	43.694183
3503.587599	505835.710768	43.699188
3503.476971	505835.526097	43.704193
3503.320665	505845.924301	43.709197
3503.419767	505840.747561	43.714202
3503.386688	505824.155829	43.719207
3503.457973	505815.491990	43.724212
3503.635379	505807.975203	43.729217
3503.286849	505806.664306	43.734221
3503.445766	505801.174490	43.739226
3503.366733	505801.288433	43.744231
3503.263220	505772.259853	43.749236
3503.586432	505772.310214	43.754241
3503.378096	505767.738663	43.759245
3503.546241	505748.584981	43.764250
3503.496227	505757.650798	43.769255
3503.322514	505765.268721	43.774260
3503.732901	505733.375766	43.779265
3503.480028	505729.418463	43.784269
3503.486636	505720.511792	43.789274
3503.312506	505723.373251	43.794279
3503.736766	505722.749821	43.799284
3503.612871	505694.179746	43.804289
3503.417406	505691.022986	43.809293
3503.601980	505687.856756	43.814298
3503.567064	505674.048263	43.819303
3503.356882	505677.978064	43.824308
3503.682523	505648.679036	43.829313
3503.306241	505648.536353	43.834317
3503.255051	505647.026639	43.839322
3503.406054	505648.774080	43.844327
3503.493268	505644.813603	43.849332
3503.657408	505640.284346	43.854337
3503.518622	505612.728527	43.859341
3503.888850	505601.436633	43.864346
3503.529111	505601.898558	43.869351
3503.221502	505605.135349	43.874356
3503.679684	505581.634476	43.879361
3503.277222	505568.238209	43.884365
3503.677119	505563.013841	43.889370
3503.483820	505566.080763	43.894375
3503.712841	505544.690746	43.899380
3503.736577	505530.113837	43.904385
3503.429823	505515.892767	43.909389
3503.744561	505511.036059	43.914394
3503.590106	505510.706506	43.919399
3503.522353	505493.411509	43.924404
3503.760266	505482.950089	43.929409
3503.775126	505470.095009	43.934413
3503.800187	505469.990090	43.939418
3503.597238	505445.530889	43.944423
3503.620213	505431.156426	43.949428
3503.526224	505428.894422	43.954433
3503.382037	505429.170472	43.959437
3503.774017	505416.609960	43.964442
3503.651657	505396.489761	43.969447
3503.462370	505402.035601	43.974452
3503.584583	505397.968331	43.979457
3503.588027	505388.151146	43.984461
3503.616014	505355.407099	43.989466
3503.607847	505353.991764	43.994471
3503.541433	505355.267575	43.999476
3503.891857	505357.185935	44.004481
3503.601245	505338.154918	44.009485
3503.845094	505318.381566	44.014490
3503.637843	505317.554326	44.019495
3503.611563	505310.626151	44.024500
3503.567486	505285.028350	44.029505
3503.439023	505280.494648	44.034509
3503.538546	505283.869555	44.039514
3503.664029	505272.312517	44.044519
3503.425051	505259.345596	44.049524
3503.616278	505245.146797	44.054529
3503.306682	505244.740555	44.059533
3503.461442	505226.853490	44.064538
3503.090846	505229.189451	44.069543
3503.333322	505222.269362	44.074548
3503.199407	505232.968010	44.079553
3503.468144	505229.990806	44.084557
3503.743922	505197.966341	44.089562
3503.209237	505184.944900	44.094567
3503.405544	505183.649040	44.099572
3503.135636	505192.193274	44.104577
3502.988601	505189.180577	44.109581
3503.738332	505179.953755	44.114586
3503.559343	505177.502740	44.119591
3503.343136	505155.069352	44.124596
3503.285676	505157.355826	44.129601
3503.063616	505156.783935	44.134605
3503.476880	505143.663228	44.139610
3503.431996	505152.880358	44.144615
3503.618654	505144.653378	44.149620
3503.540280	505118.099292	44.154625
3503.495460	505118.663261	44.159629
3503.570461	505110.706931	44.164634
3503.488100	505112.693727	44.169639
3503.297294	505101.844414	44.174644
3503.385071	505118.580493	44.179649
3503.210663	505087.639051	44.184653
3503.822884	505059.862442	44.189658
3503.616180	505080.389763	44.194663
3503.646787	505067.127069	44.199668
3503.814425	505056.980123	44.204673
3503.496717	505034.005984	44.209677
3503.663504	505025.782089	44.214682
3503.543066	505028.736381	44.219687
3503.464365	505027.079151	44.224692
3503.735092	505003.657735	44.229697
3503.540719	505003.283877	44.234701
3503.276483	504984.855549	44.239706
3503.044949	504988.181635	44.244711
3503.327325	504992.742184	44.249716
3503.557937	504973.375363	44.254721
3503.342573	504974.067500	44.259725
3503.480078	504955.069602	44.264730
3503.524402	504950.812124	44.269735
3503.170582	504940.089686	44.274740
3503.597712	504935.113846	44.279745
3503.191776	504951.067859	44.284749
3503.662260	504937.128292	44.289754
3503.360949	504918.149111	44.294759
3503.371424	504916.376567	44.299764
3503.444458	504907.914416	44.304769
3503.554122	504905.114113	44.309773
3503.323778	504903.784464	44.314778
3503.226279	504904.306162	44.319783
3503.635403	504892.704039	44.324788
3503.453579	504871.732367	44.329793
3503.258358	504875.811794	44.334797
3503.368677	504867.900375	44.339802
3503.059279	504870.682146	44.344807
3503.467697	504863.634478	44.349812
3503.937122	504851.617964	44.354817
3503.635494	504839.773924	44.359821
3503.779408	504820.572450	44.364826
3503.517349	504823.245537	44.369831
3503.726820	504817.848631	44.374836
3503.345185	504791.595005	44.379841
3503.372405	504792.653639	44.384845
3503.598135	504782.902186	44.389850
3503.592180	504777.185089	44.394855
3503.590366	504777.236227	44.399860
3504.004485	504758.700435	44.404865
3503.830630	504746.886739	44.409869
3503.984104	504731.580194	44.414874
3503.529090	504724.921973	44.419879
3503.491977	504700.182490	44.424884
3503.848868	504696.735821	44.429889
3503.542735	504701.541284	44.434893
3503.869289	504666.420943	44.439898
3503.489423	504668.859652	44.444903
3503.432268	504661.177030	44.449908
3503.298635	504676.835228	44.454913
3503.667107	504661.545242	44.459917
3503.544628	504645.725590	44.464922
3503.351153	504640.189903	44.469927
3503.665289	504624.200008	44.474932
3503.403743	504634.969800	44.479937
3503.399650	504626.114867	44.484941
3503.839053	504594.620086	44.489946
3503.477071	504586.125331	44.494951
3503.519871	504581.007722	44.499956
3503.829615	504578.327556	44.504961
3503.552236	504561.115375	44.509965
3503.456942	504544.987705	44.514970
3503.246565	504545.729675	44.519975
3503.656795	504536.252551	44.524980
3503.772139	504545.444675	44.529985
3503.344352	504525.422354	44.534989
3503.607798	504507.011322	44.539994
3503.572925	504506.764057	44.544999
3503.585922	504501.802950	44.550004
3503.844674	504495.892105	44.555009
3503.639171	504474.670673	44.560013
3503.974671	504460.853274	44.565018
3503.604661	504468.958236	44.570023
3503.599990	504434.041601	44.575028
3503.921999	504423.869887	44.580033
3503.036057	504419.860535	44.585037
3503.541651	504414.517909	44.590042
3503.540815	504420.692140	44.595047
3503.503484	504395.648629	44.600052
3503.033321	504383.426074	44.605057
3503.427027	504367.929423	44.610061
3503.457494	504369.139386	44.615066
3503.390177	504377.803810	44.620071
3503.276583	504373.874787	44.625076
3503.394858	504372.287569	44.630081
3503.139249	504353.148734	44.635085
3503.494198	504336.797886	44.640090
3503.029210	504346.840929	44.645095
3503.126724	504337.413128	44.650100
3503.207564	504334.870319	44.655105
3503.248992	504336.584607	44.660109
3503.760992	504322.486173	44.665114
3503.266957	504341.997059	44.670119
3503.427124	504332.711169	44.675124
3503.822303	504317.517873	44.680129
3503.331533	504312.433920	44.685133
3503.402855	504286.917627	44.690138
3503.576235	504292.153464	44.695143
3503.656596	504281.463201	44.700148
3503.238430	504260.173911	44.705153
3503.213282	504255.016341	44.710157
3503.909934	504241.597137	44.715162
3503.281920	504242.911193	44.720167
3503.402616	504250.331421	44.725172
3503.304136	504255.509029	44.730177
3503.294189	504241.897879	44.735181
3503.309215	504227.523683	44.740186
3503.196631	504207.805416	44.745191
3503.296448	504226.261049	44.750196
3503.570735	504212.655554	44.755201
3503.235191	504209.419454	44.760205
3503.489969	504204.774287	44.765210
3503.033564	504213.854536	44.770215
3503.167396	504214.997566	44.775220
3503.523470	504182.047643	44.780225
3503.077919	504179.436198	44.785229
3503.258578	504171.108498	44.790234
3503.589163	504175.509823	44.795239
3503.333050	504167.909039	44.800244
3503.492241	504180.383818	44.805249
3503.372111	504181.921235	44.810253
3503.245255	504150.869406	44.815258
3503.536507	504135.641775	44.820263
3503.467449	504143.142648	44.825268
3503.710616	504133.590502	44.830273
3503.227138	504138.373545	44.835277
3503.365500	504135.821614	44.840282
3503.300870	504125.204780	44.845287
3503.630577	504110.021654	44.850292
3503.851661	504085.442915	44.855297
3503.728447	504096.089959	44.860301
3503.704556	504078.887841	44.865306
3503.377493	504066.288201	44.870311
3503.458934	504056.812183	44.875316
3503.840355	504045.669338	44.880321
3503.533971	504042.934661	44.885325
3503.430306	504036.321852	44.890330
3503.395059	504018.261159	44.895335
3503.260350	503996.572498	44.900340
3503.317603	504000.612220	44.905345
3503.167281	503998.460147	44.910349
3503.621765	503996.718539	44.915354
3503.303973	503997.325691	44.920359
3503.202832	503988.789415	44.925364
3503.399807	503961.127310	44.930369
3503.426980	503958.137469	44.935373
3503.429821	503947.965323	44.940378
3503.437718	503952.316498	44.945383
3503.391919	503952.779445	44.950388
3503.521985	503952.657920	44.955393
3503.497735	503943.603401	44.960397
3503.551275	503915.559043	44.965402
3503.212988	503918.699777	44.970407
3503.409918	503916.138557	44.975412
3503.371862	503919.130620	44.980417
3503.274629	503910.694902	44.985421
3503.133553	503908.794390	44.990426
3503.112844	503913.706771	44.995431
3503.219651	503895.269251	45.000436
3503.358087	503878.344919	45.005441
3503.165076	503875.592295	45.010445
3503.760359	503867.451947	45.015450
3503.578167	503865.102467	45.020455
3503.336480	503871.770425	45.025460
3503.568597	503864.699619	45.030465
3503.378799	503848.839280	45.035469
3503.423427	503840.634140	45.040474
3503.047153	503835.734376	45.045479
3503.104194	503831.221581	45.050484
3503.369500	503829.003790	45.055489
3503.240203	503839.044667	45.060493
3503.526323	503828.422818	45.065498
3503.223484	503836.163204	45.070503
3503.414034	503822.671858	45.075508
3503.342035	503806.742254	45.080513
3502.763780	503786.540442	45.085517
3503.107607	503782.285946	45.090522
3502.944027	503789.447661	45.095527
3503.347669	503792.167500	45.100532
3503.286884	503791.570070	45.105537
3503.003554	503790.349923	45.110541
3503.389252	503788.568561	45.115546
3503.268843	503793.699164	45.120551
3503.323273	503795.360844	45.125556
3502.935962	503803.063989	45.130561
3502.906553	503802.461600	45.135565
3503.383968	503793.226493	45.140570
3503.103752	503799.647533	45.145575
3503.171679	503789.414400	45.150580
3503.478687	503768.060492	45.155585
3503.445140	503777.529590	45.160589
3503.467349	503752.273319	45.165594
3503.409753	503759.519508	45.170599
3503.260591	503761.314587	45.175604
3503.060570	503759.676412	45.180609
3503.068230	503761.851560	45.185613
3503.245776	503747.147638	45.190618
3503.361871	503755.833985	45.195623
3503.116724	503745.245455	45.200628
3503.691312	503714.588051	45.205633
3503.401323	503714.583529	45.210637
3503.490879	503716.897560	45.215642
3503.383197	503710.032225	45.220647
3503.319856	503712.674068	45.225652
3503.515769	503706.266817	45.230657
3503.502917	503685.013976	45.235661
3503.651672	503676.539262	45.240666
3503.403954	503677.135348	45.245671
3503.418249	503679.714317	45.250676
3503.672431	503673.753311	45.255681
3503.157118	503651.668917	45.260685
3503.465734	503631.680993	45.265690
3503.308121	503626.949038	45.270695
3503.199888	503633.595992	45.275700
3503.477311	503626.011852	45.280705
3503.364529	503635.746589	45.285709
3503.488833	503618.368772	45.290714
3503.193941	503604.245484	45.295719
3503.244467	503595.027142	45.300724
3503.132326	503588.263680	45.305729
3502.902385	503592.348892	45.310733
3503.211341	503584.203065	45.315738
3503.227087	503582.682591	45.320743
3503.186962	503584.055591	45.325748
3503.270007	503592.747243	45.330753
3503.354990	503591.215825	45.335757
3503.694956	503590.909297	45.340762
3503.365816	503569.099017	45.345767
3503.496445	503551.011624	45.350772
3503.361218	503556.094030	45.355777
3503.317927	503548.003866	45.360781
3503.262077	503546.899568	45.365786
3503.373543	503547.388275	45.370791
3503.306313	503544.514502	45.375796
3503.156386	503536.694227	45.380801
3503.000251	503528.773714	45.385805
3503.164325	503513.565647	45.390810
3502.970154	503512.888075	45.395815
3502.924357	503514.616232	45.400820
3503.210088	503507.435592	45.405825
3502.842687	503505.570810	45.410829
3502.876374	503506.021205	45.415834
3503.325211	503512.833190	45.420839
3503.675179	503508.780090	45.425844
3503.672818	503520.116892	45.430849
3503.172207	503518.222560	45.435853
3503.943453	503509.345723	45.440858
3503.551235	503494.377394	45.445863
3503.140865	503482.195365	45.450868
3503.741211	503469.549918	45.455873
3503.511245	503473.989418	45.460877
3503.565545	503472.361624	45.465882
3503.350145	503455.998896	45.470887
3503.335350	503439.908093	45.475892
3503.438259	503442.270657	45.480897
3503.018129	503439.806905	45.485901
3503.198298	503421.762157	45.490906
3502.899428	503437.751228	45.495911
3503.055402	503435.449453	45.500916
3503.351606	503426.344014	45.505921
3502.890521	503431.427356	45.510925
3503.372578	503428.466739	45.515930
3503.376712	503428.061467	45.520935
3503.368621	503419.560814	45.525940
3503.675481	503407.619620	45.530945
3503.150184	503409.221147	45.535949
3503.448219	503392.271120	45.540954
3503.129519	503387.918820	45.545959
3503.000914	503402.615802	45.550964
3503.261372	503399.184125	45.555969
3503.047453	503389.450784	45.560973
3503.328063	503388.445119	45.565978
3503.304544	503401.101158	45.570983
3503.265381	503395.945551	45.575988
3503.407777	503367.633231	45.580993
3502.903285	503372.571626	45.585997
3503.224195	503355.820381	45.591002
3503.046420	503365.160674	45.596007
3503.193860	503363.113280	45.601012
3503.076135	503367.028982	45.606017
3503.046125	503367.337623	45.611021
3503.008270	503364.003701	45.616026
3502.957832	503360.722376	45.621031
3503.160613	503360.386920	45.626036
3502.967574	503361.480457	45.631041
3502.973955	503378.585324	45.636045
3503.249145	503372.165421	45.641050
3503.443407	503377.448839	45.646055
3503.296131	503368.464078	45.651060
3503.332703	503380.705767	45.656065
3503.260330	503380.869279	45.661069
3503.560762	503359.971391	45.666074
3503.256658	503332.235675	45.671079
3503.398566	503335.401826	45.676084
3503.543438	503326.472081	45.681089
3503.335201	503331.262442	45.686093
3503.343191	503330.401082	45.691098
3503.624218	503314.820098	45.696103
3503.251503	503305.162419	45.701108
3503.461298	503292.932839	45.706113
3503.197895	503288.774209	45.711117
3503.599303	503298.680899	45.716122
3503.197575	503298.440995	45.721127
3503.330477	503285.464435	45.726132
3503.311673	503294.779637	45.731137
3503.007262	503281.770982	45.736141
3503.418177	503246.533250	45.741146
3503.457482	503256.851461	45.746151
3503.526582	503247.376958	45.751156
3503.528271	503238.317975	45.756161
3503.517503	503257.956108	45.761165
3503.245160	503256.886012	45.766170
3502.873541	503233.209507	45.771175
3503.157898	503218.285825	45.776180
3503.301895	503212.898777	45.781185
3503.152416	503221.829803	45.786189
3503.355050	503210.309820	45.791194
3503.370106	503212.686303	45.796199
3502.987811	503209.305578	45.801204
3503.095342	503222.092858	45.806209
3503.392861	503221.135119	45.811213
3503.543486	503215.848242	45.816218
3503.489645	503221.525186	45.821223
3503.100225	503194.713698	45.826228
3503.395621	503181.761986	45.831233
3503.336199	503187.338605	45.836237
3503.453247	503175.882737	45.841242
3503.419706	503183.125362	45.846247
3503.372331	503180.906305	45.851252
3503.237419	503176.322467	45.856257
3503.059556	503182.626334	45.861261
3503.705415	503168.202166	45.866266
3503.519237	503155.731427	45.871271
3503.004334	503138.099911	45.876276
3503.575687	503139.275072	45.881281
3503.045816	503141.788308	45.886285
3502.879924	503132.806369	45.891290
3503.247555	503136.847839	45.896295
3503.198536	503145.358151	45.901300
3503.181759	503142.729381	45.906305
3503.111950	503138.691941	45.911309
3503.497170	503130.027760	45.916314
3503.322679	503116.644183	45.921319
3503.111058	503104.379866	45.926324
3503.439645	503091.524060	45.931329
3503.186596	503097.030096	45.936333
3503.370057	503095.230024	45.941338
3503.493012	503103.662564	45.946343
3503.411546	503097.956855	45.951348
3503.524732	503089.183826	45.956353
3503.104262	503088.187744	45.961357
3503.565019	503067.112339	45.966362
3503.056867	503068.407530	45.971367
3503.297003	503066.294841	45.976372
3503.531497	503060.691006	45.981377
3503.260199	503065.643234	45.986381
3503.372552	503059.400784	45.991386
3503.365078	503056.618703	45.996391
3503.495060	503036.658341	46.001396
3503.590449	503019.993035	46.006401
3503.430044	503023.611902	46.011405
3503.805106	503007.206033	46.016410
3503.358685	503009.402440	46.021415
3503.338874	503003.130251	46.026420
3503.240618	502985.786989	46.031425
3503.301512	502970.999639	46.036429
3503.520546	502987.868835	46.041434
3503.484324	502985.546772	46.046439
3503.558432	502979.259730	46.051444
3503.459193	502965.307439	46.056449
3502.809560	502955.339072	46.061453
3503.298957	502934.916907	46.066458
3503.639379	502938.355408	46.071463
3503.387779	502938.496645	46.076468
3503.477704	502942.784494	46.081473
3503.524952	502948.040671	46.086477
3503.411747	502926.094240	46.091482
3503.232714	502906.283795	46.096487
3503.082149	502895.629192	46.101492
3503.493159	502897.639471	46.106497
3503.428914	502913.693149	46.111501
3503.456158	502899.822033	46.116506
3503.196268	502901.432262	46.121511
3503.167176	502907.004175	46.126516
3503.498723	502898.854463	46.131521
3503.238418	502875.109270	46.136525
3503.239800	502868.732464	46.141530
3503.205516	502863.474710	46.146535
3503.146165	502852.147735	46.151540
3503.270702	502861.035630	46.156545
3503.298338	502866.851639	46.161549
3503.439068	502858.175361	46.166554
3503.779399	502863.334626	46.171559
3503.229223	502853.198651	46.176564
3503.532607	502839.233228	46.181569
3503.238398	502820.908579	46.186573
3503.221157	502822.784120	46.191578
3503.142847	502824.972973	46.196583
3503.282485	502819.535884	46.201588
3503.571752	502831.080083	46.206593
3503.244438	502829.006452	46.211597
3503.334085	502796.956418	46.216602
3503.167863	502791.010957	46.221607
3502.778365	502780.798932	46.226612
3503.205829	502780.377341	46.231617
3503.231475	502780.019265	46.236621
3503.470859	502771.124910	46.241626
3503.135080	502777.757543	46.246631
3503.143826	502778.920440	46.251636
3503.530103	502780.377932	46.256641
3503.209624	502784.427031	46.261645
3503.321009	502780.917578	46.266650
3503.334447	502767.048539	46.271655
3503.428897	502755.292310	46.276660
3503.590062	502749.244476	46.281665
3503.508964	502750.269745	46.286669
3503.672095	502743.462446	46.291674
3503.116395	502752.154258	46.296679
3502.997559	502729.550541	46.301684
3503.328789	502716.491603	46.306689
3502.948854	502712.705527	46.311693
3503.374885	502702.415158	46.316698
3503.308122	502691.544744	46.321703
3503.547926	502698.491308	46.326708
3503.518574	502703.506614	46.331713
3503.394535	502702.413042	46.336717
3503.457345	502687.574541	46.341722
3503.331777	502667.249273	46.346727
3503.247090	502668.325725	46.351732
3503.453879	502654.628477	46.356737
3503.118784	502659.590902	46.361741
3503.339770	502658.290959	46.366746
3503.495120	502665.807600	46.371751
3503.132202	502660.956005	46.376756
3503.407218	502657.015780	46.381761
3503.196407	502636.552119	46.386765
3503.544331	502611.192115	46.391770
3503.384099	502618.353776	46.396775
3503.470436	502623.958144	46.401780
3503.613039	502621.000441	46.406785
3503.275168	502620.345547	46.411789
3503.577614	502605.266656	46.416794
3503.373952	502587.281726	46.421799
3503.197822	502579.870052	46.426804
3503.291084	502576.565866	46.431809
3503.304121	502597.213185	46.436813
3503.556254	502579.459863	46.441818
3503.261316	502587.908095	46.446823
3503.247088	502562.402823	46.451828
3503.626517	502540.327432	46.456833
3503.318546	502544.121555	46.461837
3503.217570	502538.823635	46.466842
3503.239730	502548.183367	46.471847
3503.370661	502545.480550	46.476852
3503.268727	502537.196747	46.481857
3503.153017	502539.644601	46.486861
3503.236944	502530.521644	46.491866
3503.230055	502512.910421	46.496871
3503.131925	502502.348513	46.501876
3503.388599	502497.044658	46.506881
3503.175399	502500.165869	46.511885
3503.354703	502493.254695	46.516890
3503.558431	502488.313483	46.521895
3503.556202	502498.183206	46.526900
3503.559589	502488.769293	46.531905
3503.521592	502478.046033	46.536909
3503.528139	502452.436097	46.541914
3503.464198	502457.254496	46.546919
3503.018203	502457.224019	46.551924
3503.440293	502448.148789	46.556929
3503.049807	502464.153222	46.561933
3503.276877	502457.436928	46.566938
3503.063494	502446.893205	46.571943
3503.501030	502424.555429	46.576948
3503.546432	502411.693281	46.581953
3503.560150	502422.117247	46.586957
3503.864670	502412.453251	46.591962
3503.689691	502409.950601	46.596967
3503.434122	502378.713542	46.601972
3503.395621	502373.506920	46.606977
3503.304160	502376.608909	46.611981
3503.523587	502367.211394	46.616986
3503.607809	502373.170455	46.621991
3503.534998	502349.597362	46.626996
3503.697838	502330.238344	46.632001
3503.393799	502333.778833	46.637005
3503.666763	502321.538596	46.642010
3503.606510	502317.600679	46.647015
3503.451481	502303.251792	46.652020
3503.788782	502286.699389	46.657025
3503.550173	502276.665666	46.662029
3503.619420	502278.375759	46.667034
3503.473756	502265.999208	46.672039
3503.367031	502246.277815	46.677044
3503.583718	502239.765526	46.682049
3503.502964	502247.876395	46.687053
3503.673469	502236.866973	46.692058
3503.458284	502217.010856	46.697063
3503.645016	502208.984940	46.702068
3503.416402	502196.165947	46.707073
3503.263778	502206.059606	46.712077
3503.372191	502193.744067	46.717082
3503.352255	502201.288614	46.722087
3503.231215	502189.313012	46.727092
3503.442072	502163.113632	46.732097
3503.044543	502159.684499	46.737101
3503.141368	502161.440856	46.742106
3503.273551	502156.207190	46.747111
3502.974636	502154.837554	46.752116
3503.444370	502155.016611	46.757121
3503.322740	502160.097269	46.762125
3503.146886	502152.584148	46.767130
3503.249652	502162.133791	46.772135
3503.408081	502156.744140	46.777140
3503.502060	502135.877439	46.782145
3503.178339	502136.283139	46.787149
3503.533520	502113.553094	46.792154
3503.505969	502113.304637	46.797159
3503.402075	502116.864145	46.802164
3503.467296	502116.752859	46.807169
3503.241415	502108.032939	46.812173
3503.578177	502089.759629	46.817178
3503.474185	502088.713462	46.822183
3503.233572	502087.739501	46.827188
3503.520036	502086.732839	46.832193
3502.961324	502086.365893	46.837197
3503.623320	502073.152974	46.842202
3503.478213	502064.369652	46.847207
3502.961173	502047.445948	46.852212
3503.240433	502039.607779	46.857217
3503.453319	502045.192328	46.862221
3503.523318	502031.819893	46.867226
3503.310597	502043.089671	46.872231
3503.312117	502046.328858	46.877236
3503.633974	502032.258655	46.882241
3502.872658	502016.588226	46.887245
3502.923595	502008.330623	46.892250
3503.092443	501997.928662	46.897255
3503.063617	501994.542441	46.902260
3503.540319	501994.619174	46.907265
3503.245972	501999.322281	46.912269
3503.448204	501988.408914	46.917274
3503.313819	501997.287559	46.922279
3503.210462	502002.567823	46.927284
3503.262679	501986.667550	46.932289
3502.875348	501995.991077	46.937293
3503.236047	501991.834713	46.942298
3503.247517	501996.793154	46.947303
3503.294740	501989.092865	46.952308
3503.374836	501959.472214	46.957313
3503.188806	501956.920633	46.962317
3503.412312	501951.166347	46.967322
3503.365754	501953.097226	46.972327
3503.321735	501958.469349	46.977332
3503.657854	501948.142143	46.982337
3503.376757	501957.803185	46.987341
3503.288402	501927.045021	46.992346
3503.298988	501913.378213	46.997351
3503.183324	501911.321629	47.002356
3503.153157	501913.452372	47.007361
3503.257547	501917.687572	47.012365
3503.170038	501909.097519	47.017370
3503.687091	501920.606310	47.022375
3503.120565	501921.303457	47.027380
3503.649560	501906.795512	47.032385
3503.293303	501894.705052	47.037389
3503.412865	501878.490362	47.042394
3503.569139	501875.732824	47.047399
3503.462641	501878.482989	47.052404
3503.218411	501875.383857	47.057409
3503.172623	501877.415848	47.062413
3503.339132	501855.980612	47.067418
3503.213428	501839.349140	47.072423
3502.864877	501840.619188	47.077428
3503.429161	501832.533424	47.082433
3503.380263	501822.165778	47.087437
3503.289175	501829.772343	47.092442
3503.483672	501829.944298	47.097447
3503.387058	501834.514967	47.102452
3503.348685	501824.044433	47.107457
3503.248931	501811.508469	47.112461
3503.189841	501793.449265	47.117466
3503.253692	501795.413322	47.122471
3503.049341	501794.636065	47.127476
3503.552841	501794.354274	47.132481
3503.386159	501795.443739	47.137485
3503.657232	501790.188011	47.142490
3503.345817	501795.399998	47.147495
3503.156947	501775.286160	47.152500
3503.563740	501758.013699	47.157505
3503.231145	501760.141651	47.162509
3503.851118	501750.073140	47.167514
3503.821689	501746.332676	47.172519
3503.289071	501736.851249	47.177524
3503.745526	501709.296438	47.182529
3503.531589	501703.712444	47.187533
3503.295715	501699.042952	47.192538
3503.259086	501705.578086	47.197543
3503.001514	501712.553046	47.202548
3503.351011	501701.919904	47.207553
3503.017087	501690.534358	47.212557
3503.333246	501662.596746	47.217562
3503.129066	501650.785760	47.222567
3503.322740	501662.345835	47.227572
3503.424617	501664.050830	47.232577
3503.508491	501659.128333	47.237581
3503.467086	501646.279349	47.242586
3503.393535	501661.222143	47.247591
3503.255816	501652.336222	47.252596
3503.488511	501626.638730	47.257601
3503.303662	501625.149795	47.262605
3503.470028	501616.924378	47.267610
3503.567342	501607.798830	47.272615
3503.092163	501619.667111	47.277620
3503.333434	501623.121544	47.282625
3503.392666	501617.190663	47.287629
3503.413501	501596.233660	47.292634
3503.088611	501582.569012	47.297639
3503.246060	501583.101120	47.302644
3503.509208	501570.203941	47.307649
3503.127862	501581.551280	47.312653
3503.542850	501581.334091	47.317658
3503.352330	501574.177336	47.322663
3503.237354	501559.669672	47.327668
3503.335838	501542.749417	47.332673
3503.109202	501545.316168	47.337677
3503.075977	501529.580831	47.342682
3503.208282	501528.598506	47.347687
3503.302690	501525.142103	47.352692
3503.350760	501519.010499	47.357697
3503.056816	501538.948372	47.362701
3503.649573	501537.792038	47.367706
3503.256156	501529.401995	47.372711
3503.287406	501536.078303	47.377716
3503.225670	501508.402634	47.382721
3503.315015	501503.428616	47.387725
3503.262403	501493.618116	47.392730
3503.032391	501507.320427	47.397735
3503.029775	501494.009678	47.402740
3503.259294	501486.432196	47.407745
3503.139913	501496.978974	47.412749
3503.275932	501488.150929	47.417754
3503.384522	501491.727589	47.422759
3503.171640	501501.023800	47.427764
3503.646109	501494.976629	47.432769
3503.504802	501480.118766	47.437773
3503.415545	501458.014885	47.442778
3502.775517	501462.975229	47.447783
3502.652837	501456.971821	47.452788
3503.162519	501449.856178	47.457793
3503.152590	501451.427025	47.462797
3503.007742	501447.957811	47.467802
3503.275227	501452.572254	47.472807
3502.889805	501454.253068	47.477812
3503.208946	501458.555660	47.482817
3503.118859	501456.090069	47.487821
3503.013043	501447.350844	47.492826
3503.042776	501458.228372	47.497831
3503.186867	501454.915943	47.502836
3503.543595	501447.267723	47.507841
3503.142703	501449.254666	47.512845
3502.999341	501458.742366	47.517850
3503.020542	501456.562867	47.522855
3503.117653	501461.052397	47.527860
3503.187455	501457.802325	47.532865
3503.213700	501455.267731	47.537869
3503.117274	501448.146666	47.542874
3503.187368	501436.848936	47.547879
3503.131155	501424.255201	47.552884
3503.213508	501422.268488	47.557889
3503.069945	501430.794569	47.562893
3503.255984	501425.400333	47.567898
3503.199311	501419.842005	47.572903
3503.051780	501427.407050	47.577908
3503.087798	501425.275819	47.582913
3503.251166	501421.909723	47.587917
3503.476498	501417.825236	47.592922
3503.433154	501428.511877	47.597927
3503.187993	501416.049231	47.602932
3503.420992	501385.138103	47.607937
3503.338838	501377.306156	47.612941
3503.278217	501379.947917	47.617946
3503.303184	501386.321590	47.622951
3503.227939	501383.549958	47.627956
3503.169909	501376.878321	47.632961
3503.010710	501379.940578	47.637965
3503.381633	501383.425179	47.642970
3503.446863	501384.882923	47.647975
3502.981776	501368.152811	47.652980
3503.215034	501352.375195	47.657985
3503.297681	501343.606129	47.662989
3503.296801	501340.974579	47.667994
3503.381619	501336.203685	47.672999
3503.233277	501343.414595	47.678004
3503.453969	501342.873817	47.683009
3503.205049	501342.761568	47.688013
3503.219477	501337.849959	47.693018
3503.394020	501338.784287	47.698023
3502.897618	501324.184879	47.703028
3502.965828	501318.910464	47.708033
3503.100584	501332.909551	47.713037
3502.990795	501316.882443	47.718042
3503.136360	501307.850342	47.723047
3503.131236	501304.359014	47.728052
3503.280090	501288.442840	47.733057
3503.149807	501299.345759	47.738061
3503.002463	501301.242026	47.743066
3503.062630	501301.182148	47.748071
3502.990044	501296.284282	47.753076
3503.576076	501306.264142	47.758081
3503.548659	501298.524736	47.763085
3503.381761	501300.575937	47.768090
3503.436837	501304.110479	47.773095
3503.331960	501281.907619	47.778100
3503.280605	501267.339045	47.783105
3502.838423	501276.114861	47.788109
3503.288303	501264.858218	47.793114
3503.554119	501258.692106	47.798119
3503.068225	501272.536273	47.803124
3503.382641	501264.034218	47.808129
3503.584812	501265.571556	47.813133
3503.455955	501258.151854	47.818138
3503.372838	501241.006944	47.823143
3503.242137	501230.044508	47.828148
3503.630212	501218.949450	47.833153
3502.962369	501221.687217	47.838157
3503.431644	501218.120885	47.843162
3503.392953	501214.786689	47.848167
3503.057007	501226.430765	47.853172
3503.451554	501227.077250	47.858177
3503.146049	501204.956621	47.863181
3502.845955	501186.681820	47.868186
3502.816474	501195.696128	47.873191
3503.073697	501204.766341	47.878196
3503.270554	501198.509879	47.883201
3503.452491	501183.803132	47.888205
3503.299085	501182.207960	47.893210
3503.363858	501178.654944	47.898215
3503.158033	501183.597346	47.903220
3503.071626	501179.359622	47.908225
3503.254622	501183.329500	47.913229
3503.535041	501172.150200	47.918234
3503.379447	501174.503316	47.923239
3503.345368	501165.448925	47.928244
3503.454042	501147.666233	47.933249
3503.746759	501142.255049	47.938253
3503.231757	501141.577480	47.943258
3503.193088	501135.358225	47.948263
3503.162718	501135.262043	47.953268
3503.388171	501135.429113	47.958273
3502.799063	501125.348908	47.963277
3503.408212	501113.611462	47.968282
3503.254273	501114.091576	47.973287
3503.038721	501099.548819	47.978292
3503.117398	501094.576372	47.983297
3502.746995	501096.001770	47.988301
3503.342558	501085.835515	47.993306
3503.483866	501093.709350	47.998311
3503.269246	501097.084104	48.003316
3503.748641	501090.226180	48.008321
3503.539346	501096.940675	48.013325
3503.465483	501073.062360	48.018330
3503.165571	501061.164883	48.023335
3503.217664	501054.323873	48.028340
3503.526948	501050.428493	48.033345
3503.321402	501057.800405	48.038349
3503.190363	501050.836496	48.043354
3503.306884	501061.093169	48.048359
3503.072472	501052.627151	48.053364
3503.284451	501057.048011	48.058369
3503.300404	501054.261912	48.063373
3503.510822	501017.634218	48.068378
3503.439513	501017.139586	48.073383
3503.142032	501009.797049	48.078388
3503.320934	501018.069897	48.083393
3503.250690	501013.424657	48.088397
3503.420867	501016.536142	48.093402
3503.583080	501013.018307	48.098407
3503.154012	500987.981261	48.103412
3503.431586	500977.308440	48.108417
3502.939772	500977.943195	48.113421
3503.166243	500975.933652	48.118426
3503.214597	500977.292867	48.123431
3502.660095	500988.617338	48.128436
3503.340270	500978.589493	48.133441
3502.966037	500988.670704	48.138445
3503.305656	500967.966261	48.143450
3503.493723	500972.492153	48.148455
3503.164160	500975.733253	48.153460
3503.673815	500974.994942	48.158465
3503.514439	500962.164110	48.163469
3503.693149	500941.889994	48.168474
3503.372213	500938.397899	48.173479
3503.212859	500937.259182	48.178484
3503.562809	500929.105659	48.183489
3503.029801	500926.558159	48.188493
3503.115049	500910.044316	48.193498
3503.216559	500890.440344	48.198503
3503.252085	500889.372052	48.203508
3503.411735	500898.609692	48.208513
3502.804494	500900.477465	48.213517
3503.242190	500888.665742	48.218522
3503.338759	500887.638415	48.223527
3503.149115	500891.515415	48.228532
3503.586137	500890.231812	48.233537
3503.184572	500895.458311	48.238541
3503.528940	500885.939033	48.243546
3503.382583	500866.374214	48.248551
3503.032921	500844.614424	48.253556
3503.289858	500844.928367	48.258561
3503.180519	500842.162040	48.263565
3503.376638	500843.042368	48.268570
3502.980538	500849.179097	48.273575
3503.165365	500852.591989	48.278580
3503.315934	500836.928217	48.283585
3503.122579	500858.470652	48.288589
3503.276619	500856.877469	48.293594
3503.138307	500855.229265	48.298599
3503.242303	500851.821831	48.303604
3503.385204	500825.276910	48.308609
3503.049659	500820.471093	48.313613
3503.187086	500800.000878	48.318618
3503.211506	500795.796160	48.323623
3503.284561	500806.312930	48.328628
3503.525184	500800.606183	48.333633
3503.469320	500800.159719	48.338637
3503.431116	500797.989529	48.343642
3503.406699	500793.944378	48.348647
3503.365590	500775.577600	48.353652
3503.562432	500771.244391	48.358657
3503.227490	500782.635518	48.363661
3503.197014	500777.629621	48.368666
3503.257879	500781.264584	48.373671
3502.997087	500773.156912	48.378676
3503.193491	500774.239662	48.383681
3503.170793	500781.532170	48.388685
3503.075618	500777.903126	48.393690
3503.335693	500770.927900	48.398695
3503.219431	500757.735795	48.403700
3503.187850	500744.580911	48.408705
3502.813198	500746.108239	48.413709
3502.885759	500734.556594	48.418714
3503.006710	500733.980948	48.423719
3502.588344	500738.045982	48.428724
3503.131451	500755.068547	48.433729
3503.471078	500771.110943	48.438733
3503.499736	500749.392468	48.443738
3503.290650	500740.264291	48.448743
3503.045924	500749.009153	48.453748
3503.130265	500728.800327	48.458753
3502.783733	500744.445048	48.463757
3503.172915	500738.006176	48.468762
3503.177037	500742.055043	48.473767
3502.945923	500741.585664	48.478772
3503.078176	500740.046530	48.483777
3503.227899	500731.367791	48.488781
3503.116039	500725.767352	48.493786
3502.648136	500739.609089	48.498791
3502.849904	500734.465237	48.503796
3503.141150	500732.546659	48.508801
3502.653339	500735.357273	48.513805
3503.373264	500740.204082	48.518810
3503.259027	500734.401558	48.523815
3502.989962	500734.393720	48.528820
3503.057163	500740.153558	48.533825
3503.131084	500732.246040	48.538829
3503.222612	500734.104609	48.543834
3503.069497	500745.062092	48.548839
3502.751576	500736.052348	48.553844
3503.082343	500745.870410	48.558849
3502.957010	500745.789237	48.563853
3502.790108	500735.490225	48.568858
3503.305824	500746.797529	48.573863
3502.801666	500743.638052	48.578868
3503.404304	500739.544386	48.583873
3503.333942	500740.466842	48.588877
3503.443502	500729.263656	48.593882
3503.314667	500717.693218	48.598887
3503.243583	500716.540535	48.603892
3503.571426	500692.446364	48.608897
3503.091918	500699.153105	48.613901
3503.042852	500709.638619	48.618906
3503.249332	500705.911261	48.623911
3503.130787	500693.326861	48.628916
3503.297881	500700.791867	48.633921
3503.232369	500706.724541	48.638925
3503.368212	500690.556809	48.643930
3503.387432	500676.482755	48.648935
3503.124588	500673.386353	48.653940
3503.572780	500658.029693	48.658945
3503.288358	500662.276036	48.663949
3503.353485	500661.354899	48.668954
3503.395004	500662.613987	48.673959
3503.315262	500663.487313	48.678964
3503.127737	500631.831489	48.683969
3503.251434	500626.143168	48.688973
3503.551139	500631.056431	48.693978
3503.409011	500628.852031	48.698983
3503.160040	500626.917601	48.703988
3503.598230	500622.596822	48.708993
3503.498022	500622.157363	48.713997
3503.165805	500600.900679	48.719002
3503.351308	500587.761981	48.724007
3503.294225	500582.507153	48.729012
3503.179791	500572.250368	48.734017
3502.878280	500579.890729	48.739021
3502.774022	500571.960688	48.744026
3503.071794	500577.582900	48.749031
3502.679327	500583.921611	48.754036
3503.255337	500576.440823	48.759041
3502.937294	500577.756752	48.764045
3502.727534	500586.445550	48.769050
3502.833949	500583.493229	48.774055
3503.224283	500581.963904	48.779060
3502.982174	500581.040710	48.784065
3502.746014	500579.661029	48.789069
3503.353056	500578.401147	48.794074
3503.374607	500583.611471	48.799079
3502.871717	500591.840438	48.804084
3503.409136	500573.432622	48.809089
3503.079263	500582.849037	48.814093
3502.910413	500581.205635	48.819098
3503.161901	500587.240091	48.824103
3503.028790	500582.149129	48.829108
3503.375951	500580.120464	48.834113
3503.170252	500584.556848	48.839117
3503.103984	500588.465027	48.844122
3503.304233	500586.257120	48.849127
3503.313896	500591.418705	48.854132
3503.219929	500583.740124	48.859137
3503.089208	500575.662419	48.864141
3503.278182	500562.016989	48.869146
3502.952065	500555.286187	48.874151
3503.080836	500552.684642	48.879156
3503.188638	500540.975451	48.884161
3503.251118	500545.015139	48.889165
3503.388595	500545.702286	48.894170
3503.302132	500544.400173	48.899175
3503.034849	500544.543902	48.904180
3503.398278	500544.486704	48.909185
3503.743581	500549.392781	48.914189
3503.543147	500533.176828	48.919194
3503.700459	500516.803079	48.924199
3503.372599	500516.197135	48.929204
3503.758416	500507.885902	48.934209
3503.111614	500499.029256	48.939213
3503.448123	500480.501251	48.944218
3503.388885	500456.012397	48.949223
3503.257348	500474.204822	48.954228
3503.497467	500466.726466	48.959233
3503.476108	500467.236256	48.964237
3503.352083	500468.977074	48.969242
3503.654563	500457.641990	48.974247
3503.280494	500427.230089	48.979252
3503.110010	500416.020356	48.984257
3502.871403	500425.321194	48.989261
3503.463210	500417.989694	48.994266
3503.267375	500422.373942	48.999271
3503.019277	500430.208390	49.004276
3503.322314	500415.178166	49.009281
3503.142385	500412.574780	49.014285
3503.373664	500415.322395	49.019290
3503.015636	500416.695272	49.024295
3503.189673	500430.435777	49.029300
3503.672526	500405.658699	49.034305
3503.000554	500385.822117	49.039309
3503.214729	500387.863803	49.044314
3503.435316	500369.100922	49.049319
3502.959878	500377.882434	49.054324
3503.043065	500373.364626	49.059329
3502.980594	500383.245047	49.064333
3503.292590	500374.287400	49.069338
3503.529086	500374.199649	49.074343
3503.342753	500375.596007	49.079348
3503.363410	500373.922630	49.084353
3503.050100	500379.793348	49.089357
3503.210238	500355.016594	49.094362
3502.905891	500340.335400	49.099367
3502.667073	500348.370885	49.104372
3502.987428	500363.505590	49.109377
3503.055198	500369.670394	49.114381
3503.159114	500376.841820	49.119386
3503.205485	500369.798984	49.124391
3503.272302	500346.353009	49.129396
3503.659069	500334.700822	49.134401
3503.542913	500333.707089	49.139405
3503.457985	500327.545480	49.144410
3503.418344	500334.840849	49.149415
3503.645424	500330.958307	49.154420
3503.335418	500314.708857	49.159425
3503.426349	500306.697228	49.164429
3503.396531	500291.820748	49.169434
3503.591131	500295.637140	49.174439
3503.352934	500298.610833	49.179444
3503.031135	500277.099030	49.184449
3502.887507	500272.414579	49.189453
3502.815427	500285.131138	49.194458
3503.246024	500294.528733	49.199463
3502.994954	500277.713145	49.204468
3503.278723	500255.751274	49.209473
3503.282417	500258.231184	49.214477
3503.556210	500256.770870	49.219482
3503.294601	500250.535927	49.224487
3503.029753	500250.476804	49.229492
3503.573166	500257.528191	49.234497
3503.121521	500257.194891	49.239501
3503.081361	500256.087907	49.244506
3503.464135	500258.406661	49.249511
3503.321792	500242.586199	49.254516
3503.394826	500212.255110	49.259521
3503.378342	500217.420937	49.264525
3503.235524	500210.559795	49.269530
3503.144350	500215.130019	49.274535
3503.060919	500216.206419	49.279540
3503.587733	500208.480168	49.284545
3503.370538	500220.511068	49.289549
3503.250276	500213.696979	49.294554
3503.255567	500200.130925	49.299559
3503.276862	500185.448746	49.304564
3503.443685	500174.944806	49.309569
3503.330644	500175.570331	49.314573
3503.300130	500166.818573	49.319578
3503.361457	500179.261033	49.324583
3502.860153	500175.898531	49.329588
3503.158969	500172.966348	49.334593
3502.982570	500169.451253	49.339597
3503.037971	500172.176089	49.344602
3503.197324	500163.799257	49.349607
3503.056518	500168.782279	49.354612
3503.479628	500162.590926	49.359617
3503.166777	500160.160366	49.364621
3503.420731	500142.809264	49.369626
3503.398923	500137.346258	49.374631
3503.018297	500138.419023	49.379636
3503.384200	500129.857674	49.384641
3503.347450	500140.695899	49.389645
3503.255629	500143.393392	49.394650
3503.440216	500142.099023	49.399655
3503.208493	500127.659262	49.404660
3503.381278	500098.931977	49.409665
3503.122566	500102.566976	49.414669
3503.233019	500104.270766	49.419674
3503.408816	500083.338104	49.424679
3503.199824	500105.440715	49.429684
3503.173232	500102.155016	49.434689
3502.864214	500099.622606	49.439693
3503.403574	500097.917831	49.444698
3503.161365	500095.881038	49.449703
3503.139437	500095.985987	49.454708
3502.928580	500104.118397	49.459713
3503.009105	500097.930556	49.464717
3503.477469	500099.223449	49.469722
3503.301629	500078.700688	49.474727
3502.897392	500063.579495	49.479732
3503.228966	500055.377861	49.484737
3503.222580	500060.137194	49.489741
3502.829260	500058.579842	49.494746
3503.125788	500052.459078	49.499751
3503.238158	500055.377398	49.504756
3503.311109	500063.515584	49.509761
3503.159127	500054.378029	49.514765
3503.607747	500056.433313	49.519770
3503.334198	500056.881742	49.524775
3503.079207	500057.732181	49.529780
3503.329095	500055.415127	49.534785
3503.220445	500024.353169	49.539789
3502.939419	500019.336045	49.544794
3503.328779	500008.189415	49.549799
3503.236255	500017.973553	49.554804
3503.656724	499999.937959	49.559809
3503.138263	500021.937737	49.564813
3503.003241	500013.404895	49.569818
3503.220254	500009.878200	49.574823
3502.860395	500010.542745	49.579828
3503.401666	500011.014233	49.584833
3503.230730	500014.432903	49.589837
3503.182388	500006.392535	49.594842
3503.020419	500007.633216	49.599847
3503.049735	499997.910177	49.604852
3503.460978	499982.761249	49.609857
3503.212523	499976.878458	49.614861
3503.621472	499975.346140	49.619866
3503.158999	499980.329441	49.624871
3503.263545	499975.453830	49.629876
3503.192405	499975.971503	49.634881
3503.481350	499982.607660	49.639885
3503.349451	499968.708789	49.644890
3503.199647	499946.764455	49.649895
3503.150376	499937.914313	49.654900
3502.983732	499918.351659	49.659905
3502.858746	499936.442360	49.664909
3502.815267	499930.223444	49.669914
3503.186278	499925.963736	49.674919
3503.265407	499929.494750	49.679924
3503.169891	499927.333513	49.684929
3503.267067	499930.456728	49.689933
3503.406012	499927.651012	49.694938
3503.311852	499933.892180	49.699943
3502.659639	499937.994358	49.704948
3503.607153	499928.834797	49.709953
3503.161791	499942.116786	49.714957
3503.321923	499926.855650	49.719962
3503.481202	499934.119740	49.724967
3503.120264	499912.968010	49.729972
3503.204964	499891.897669	49.734977
3503.213188	499890.681777	49.739981
3503.097929	499881.993893	49.744986
3503.011766	499886.259699	49.749991
3502.949870	499894.318041	49.754996
3503.307028	499884.745591	49.760001
3502.859642	499897.926697	49.765005
3502.883084	499903.440631	49.770010
3503.013019	499894.005339	49.775015
3502.970052	499897.150713	49.780020
3503.215877	499890.531725	49.785025
3502.884269	499895.291891	49.790029
3503.039020	499894.204693	49.795034
3502.949020	499886.221474	49.800039
3503.065635	499885.241540	49.805044
3503.688284	499888.534794	49.810049
3503.071763	499900.983357	49.815053
3502.887075	499898.937449	49.820058
3503.272495	499896.295241	49.825063
3502.893925	499902.176431	49.830068
3503.079414	499892.226174	49.835073
3503.141638	499899.505620	49.840077
3503.235704	499897.516885	49.845082
3503.125608	499897.483917	49.850087
3502.953694	499909.356014	49.855092
3503.286502	499896.750324	49.860097
3502.906254	499882.991879	49.865101
3503.190885	499885.073105	49.870106
3502.902977	499867.351823	49.875111
3502.999707	499861.009483	49.880116
3503.195198	499885.022548	49.885121
3503.337356	499867.840706	49.890125
3503.119882	499853.044141	49.895130
3503.081917	499855.581310	49.900135
3503.073153	499857.607679	49.905140
3503.512628	499853.235895	49.910145
3503.185865	499866.499193	49.915149
3503.307091	499858.533193	49.920154
3503.425339	499858.565367	49.925159
3503.380316	499862.925913	49.930164
3503.358233	499851.540511	49.935169
3503.296778	499833.580927	49.940173
3503.394242	499824.859390	49.945178
3503.352458	499815.754912	49.950183
3503.195162	499827.979081	49.955188
3503.390192	499805.473881	49.960193
3503.212694	499813.449295	49.965197
3503.371235	499820.561692	49.970202
3503.546175	499811.068625	49.975207
3503.447734	499781.017001	49.980212
3503.172623	499775.593924	49.985217
3502.719804	499777.994204	49.990221
3503.311079	499769.245203	49.995226
3503.201093	499777.918623	50.000231
3503.099083	499774.189216	50.005236
3503.181210	499764.305846	50.010241
3503.104439	499772.720924	50.015245
3502.844944	499778.178383	50.020250
3503.016244	499776.734232	50.025255
3502.896591	499782.625153	50.030260
3503.037566	499770.404027	50.035265
3503.070915	499776.118909	50.040269
3502.899427	499778.474721	50.045274
3503.278209	499774.163130	50.050279
3502.771149	499783.962303	50.055284
3503.258764	499770.977724	50.060289
3503.179848	499776.305403	50.065293
3503.343419	499776.431651	50.070298
3503.230821	499783.991870	50.075303
3503.056367	499783.867838	50.080308
3503.233305	499773.564537	50.085313
3503.081955	499760.934045	50.090317
3503.433765	499749.641334	50.095322
3503.094729	499740.938134	50.100327
3502.931174	499745.216207	50.105332
3503.203197	499747.704392	50.110337
3503.202133	499737.429207	50.115341
3503.287136	499734.277656	50.120346
3503.242670	499727.653875	50.125351
3502.937851	499739.040905	50.130356
3503.043973	499736.847772	50.135361
3502.934954	499742.787644	50.140365
3503.256405	499735.346745	50.145370
3503.327643	499738.474094	50.150375
3503.207674	499738.189592	50.155380
3503.260049	499729.019567	50.160385
3503.128205	499734.051912	50.165389
3503.041331	499714.678901	50.170394
3503.002198	499704.409714	50.175399
3503.108351	499699.635011	50.180404
3503.376455	499691.898814	50.185409
3502.927920	499694.146572	50.190413
3503.009974	499695.146226	50.195418
3502.993498	499692.061328	50.200423
3502.988603	499697.731661	50.205428
3503.266633	499693.334739	50.210433
3503.418277	499696.955574	50.215437
3503.237280	499695.972055	50.220442
3503.033056	499701.977607	50.225447
3502.895515	499699.164941	50.230452
3503.169543	499699.881156	50.235457
3502.952673	499693.993278	50.240461
3503.151780	499696.999184	50.245466
3503.139808	499696.596373	50.250471
3503.054582	499700.710219	50.255476
3503.270488	499695.057646	50.260481
3502.983465	499698.494726	50.265485
3503.114902	499701.359472	50.270490
3502.950273	499702.195643	50.275495
3502.881029	499708.078620	50.280500
3503.155241	499700.594555	50.285505
3503.125679	499689.767040	50.290509
3502.968759	499701.738142	50.295514
3503.617213	499700.471656	50.300519
3503.255357	499680.079077	50.305524
3503.372555	499669.025876	50.310529
3503.260483	499659.628715	50.315533
3503.152120	499653.166863	50.320538
3503.073177	499664.872569	50.325543
3503.214768	499657.105735	50.330548
3503.467256	499668.910906	50.335553
3503.083632	499673.578115	50.340557
3502.881090	499671.332526	50.345562
3503.367680	499661.486404	50.350567
3503.141942	499656.359200	50.355572
3503.187873	499660.756037	50.360577
3503.064692	499654.245909	50.365581
3503.028483	499638.914324	50.370586
3503.093829	499616.429385	50.375591
3503.036741	499621.956135	50.380596
3503.415598	499616.581495	50.385601
3503.145557	499617.738047	50.390605
3503.057304	499623.269723	50.395610
3503.177419	499616.670505	50.400615
3503.318914	499621.406580	50.405620
3503.378692	499617.499710	50.410625
3503.559672	499624.203686	50.415629
3503.153320	499625.280546	50.420634
3503.284189	499629.005917	50.425639
3503.317125	499616.649907	50.430644
3503.568623	499595.097279	50.435649
3503.227767	499597.074932	50.440653
3502.933569	499595.856205	50.445658
3503.399115	499585.254080	50.450663
3503.151337	499593.240701	50.455668
3503.372731	499586.878559	50.460673
3503.313445	499593.519287	50.465677
3503.204926	499567.012236	50.470682
3503.463866	499580.132546	50.475687
3502.982247	499556.772225	50.480692
3503.343367	499537.075112	50.485697
3503.346664	499536.669883	50.490701
3503.333570	499550.643124	50.495706
3503.334652	499544.720745	50.500711
3503.051983	499543.145856	50.505716
3503.312163	499535.056509	50.510721
3503.178210	499546.770987	50.515725
3503.265651	499538.658327	50.520730
3503.005510	499526.399200	50.525735
3502.977193	499505.447507	50.530740
3503.189079	499465.323656	50.535745
3503.174711	499415.314031	50.540749
3503.077392	499361.065316	50.545754
3503.308787	499303.423559	50.550759
3503.110316	499235.118095	50.555764
3502.888967	499131.128603	50.560769
3502.751594	499034.262757	50.565773
3502.822360	498914.837129	50.570778
3502.542364	498795.769879	50.575783
3502.571218	498679.639701	50.580788
3502.451868	498525.363131	50.585793
3502.240845	498394.639218	50.590797
3501.642174	498238.411049	50.595802
3501.964703	498078.492271	50.600807
3501.750359	497919.213799	50.605812
3501.618012	497712.384666	50.610817
3501.444378	497531.985932	50.615821
3501.067289	497325.545427	50.620826
3500.801720	497127.590119	50.625831
3500.519171	496930.647861	50.630836
3500.371574	496698.445572	50.635841
3499.721134	496476.496005	50.640845
3499.419960	496233.629549	50.645850
3499.168125	496006.953402	50.650855
3498.745713	495765.264322	50.655860
3498.547827	495507.233494	50.660865
3498.022458	495253.605072	50.665869
3497.827346	494993.591916	50.670874
3498.122978	494725.801308	50.675879
3497.201473	494454.806730	50.680884
3496.790568	494166.866210	50.685889
3496.569863	493877.827765	50.690893
3496.211814	493587.439311	50.695898
3496.196064	493280.332678	50.700903
3495.386243	492983.372687	50.705908
3494.983535	492660.214132	50.710913
3494.880222	492351.434803	50.715917
3494.213255	492032.915226	50.720922
3494.111229	491699.057907	50.725927
3493.235660	491362.328979	50.730932
3493.408167	491010.488605	50.735937
3492.552112	490681.593922	50.740941
3492.263296	490331.332959	50.745946
3492.045564	489972.545701	50.750951
3491.174473	489611.322503	50.755956
3490.533302	489254.715584	50.760961
3489.967186	488894.342021	50.765965
3489.369861	488524.545643	50.770970
3489.355213	488164.780030	50.775975
3488.833199	487790.196178	50.780980
3488.213444	487402.754571	50.785985
3487.519554	487026.257958	50.790989
3487.125419	486626.810545	50.795994
3486.938278	486243.886466	50.800999
3486.348717	485857.928235	50.806004
3485.855056	485448.340469	50.811009
3485.416789	485054.946037	50.816013
3484.705455	484640.917407	50.821018
3484.118303	484238.664252	50.826023
3483.262553	483824.539530	50.831028
3482.663292	483419.738062	50.836033
3482.365865	483005.608820	50.841037
3481.667228	482593.611419	50.846042
3481.336506	482168.475140	50.851047
3480.894952	481755.709976	50.856052
3480.251247	481318.799043	50.861057
3479.281659	480905.187295	50.866061
3478.942692	480479.255415	50.871066
3478.547271	480045.722396	50.876071
3477.842942	479607.870743	50.881076
3477.066055	479169.716769	50.886081
3476.622493	478738.493567	50.891085
3475.983738	478304.910015	50.896090
3475.655640	477853.986785	50.901095
3474.583235	477417.563749	50.906100
3474.595907	476965.451550	50.911105
3473.571550	476535.133844	50.916109
3473.115200	476073.902329	50.921114
3472.662183	475628.219445	50.926119
3471.621874	475175.219579	50.931124
3470.943859	474713.434311	50.936129
3470.598489	474271.303025	50.941133
3469.818849	473799.730381	50.946138
3469.158611	473356.969949	50.951143
3468.464126	472905.283813	50.956148
3467.918023	472443.882161	50.961153
3467.138420	471986.866535	50.966157
3466.266670	471536.749581	50.971162
3465.890046	471064.086727	50.976167
3465.151890	470620.011906	50.981172
3464.612829	470159.064660	50.986177
3464.202703	469710.254269	50.991181
3463.286128	469236.874417	50.996186
3462.716769	468770.222714	51.001191
3461.780916	468321.009070	51.006196
3461.441458	467857.646858	51.011201
3460.666722	467395.255850	51.016205
3459.741788	466930.799482	51.021210
3459.135160	466459.842864	51.026215
3458.341421	466003.153967	51.031220
3458.118543	465533.282237	51.036225
3457.433705	465083.604677	51.041229
3456.490824	464607.436869	51.046234
3455.888986	464147.634996	51.051239
3454.990031	463694.259955	51.056244
3454.687374	463219.227723	51.061249
3453.936211	462760.180299	51.066253
3452.880553	462290.875882	51.071258
3452.426710	461822.581859	51.076263
3451.582989	461362.859944	51.081268
3451.033598	460898.719881	51.086273
3449.936387	460449.669671	51.091277
3449.433475	459985.756346	51.096282
3448.686548	459523.849897	51.101287
3447.881461	459068.993430	51.106292
3447.308297	458604.808278	51.111297
3446.637028	458157.520418	51.116301
3445.894841	457700.190832	51.121306
3445.211186	457242.233785	51.126311
3444.792594	456789.653317	51.131316
3443.595674	456317.605015	51.136321
3442.750557	455889.271689	51.141325
3442.440526	455428.681648	51.146330
3441.682968	454974.748131	51.151335
3440.609096	454519.333415	51.156340
3440.347160	454056.830430	51.161345
3439.564196	453612.918909	51.166349
3438.647112	453162.576291	51.171354
3438.164477	452706.067485	51.176359
3437.507059	452262.617021	51.181364
3436.631370	451804.376390	51.186369
3435.818634	451371.740734	51.191373
3434.929630	450921.349322	51.196378
3434.734668	450470.788591	51.201383
3433.783007	450034.597677	51.206388
3433.162460	449579.672087	51.211393
3432.401090	449138.613401	51.216397
3431.375591	448702.865737	51.221402
3430.895888	448258.142765	51.226407
3429.768763	447814.579385	51.231412
3429.573855	447371.570682	51.236417
3428.712901	446937.997006	51.241421
3427.915147	446494.813299	51.246426
3427.574912	446064.592282	51.251431
3426.321428	445633.949528	51.256436
3425.613940	445192.097418	51.261441
3425.216859	444745.112474	51.266445
3424.460870	444314.062560	51.271450
3423.737976	443890.511666	51.276455
3422.787709	443462.522515	51.281460
3422.381751	443018.247572	51.286465
3421.434731	442601.511024	51.291469
3420.793083	442168.577085	51.296474
3420.446409	441738.989774	51.301479
3419.437732	441311.530014	51.306484
3418.625379	440882.051911	51.311489
3418.071363	440455.063598	51.316493
3417.657650	440032.716026	51.321498
3416.550826	439606.460237	51.326503
3415.619104	439184.687609	51.331508
3415.379442	438749.421009	51.336513
3414.326506	438328.947469	51.341517
3413.730478	437900.753717	51.346522
3413.225517	437476.752116	51.351527
3412.143404	437067.278964	51.356532
3411.678840	436637.494139	51.361537
3411.051006	436223.645069	51.366541
3410.403643	435799.815195	51.371546
3409.818118	435386.783397	51.376551
3409.005714	434965.123475	51.381556
3408.757817	434532.881934	51.386561
3407.237527	434122.516075	51.391565
3406.609901	433706.188349	51.396570
3406.303798	433284.902815	51.401575
3405.364493	432877.319406	51.406580
3404.502335	432467.787646	51.411585
3403.793451	432049.236821	51.416589
3402.748004	431628.701116	51.421594
3402.397599	431227.396959	51.426599
3401.347460	430828.558660	51.431604
3400.994336	430418.406028	51.436609
3400.044999	430012.175491	51.441613
3399.639106	429610.753549	51.446618
3399.116348	429204.366808	51.451623
3398.091669	428805.950609	51.456628
3397.646791	428394.917339	51.461633
3396.930951	427988.262980	51.466637
3396.187421	427576.400761	51.471642
3395.309530	427170.267348	51.476647
3394.306816	426774.407356	51.481652
3393.959288	426364.063649	51.486657
3393.268036	425973.069364	51.491661
3392.333018	425572.177720	51.496666
3391.987630	425169.688411	51.501671
3391.099538	424769.259917	51.506676
3390.316541	424375.488549	51.511681
3389.784195	423978.344622	51.516685
3389.005935	423583.113278	51.521690
3388.493085	423187.783424	51.526695
3387.300997	422799.133721	51.531700
3387.054055	422395.038309	51.536705
3386.332633	422004.575711	51.541709
3385.390226	421617.520793	51.546714
3385.019026	421217.161609	51.551719
3383.878389	420829.441159	51.556724
3383.121607	420434.034078	51.561729
3382.603735	420059.667292	51.566733
3381.800700	419665.983950	51.571738
3381.206357	419275.183377	51.576743
3380.670653	418898.415994	51.581748
3380.018518	418503.396896	51.586753
3379.179369	418125.219145	51.591757
3378.221059	417734.200681	51.596762
3378.112661	417349.418946	51.601767
3377.033674	416963.057952	51.606772
3376.805680	416577.801999	51.611777
3375.636565	416192.867511	51.616781
3375.060533	415802.244771	51.621786
3374.176763	415415.781186	51.626791
3373.551557	415037.960561	51.631796
3373.026461	414654.377210	51.636801
3372.254007	414283.810972	51.641805
3371.502496	413902.413087	51.646810
3370.855641	413519.443774	51.651815
3369.941505	413147.716715	51.656820
3369.274638	412764.384959	51.661825
3368.780242	412395.732643	51.666829
3367.864756	412010.575525	51.671834
3367.388296	411647.043659	51.676839
3366.316502	411263.578548	51.681844
3365.846260	410881.461730	51.686849
3364.959333	410515.109562	51.691853
3364.113584	410150.626781	51.696858
3363.696133	409783.174966	51.701863
3363.243166	409411.937972	51.706868
3362.631466	409032.767637	51.711873
3361.639410	408665.291390	51.716877
3360.963101	408296.998378	51.721882
3360.610603	407928.319323	51.726887
3359.558015	407557.332284	51.731892
3359.046724	407189.685920	51.736897
3358.024644	406813.958164	51.741901
3357.517320	406460.254460	51.746906
3356.861815	406089.288501	51.751911
3356.009675	405725.109424	51.756916
3355.202272	405354.870272	51.761921
3354.767889	404993.844208	51.766925
3354.147669	404629.259779	51.771930
3353.417744	404269.822400	51.776935
3352.222202	403908.904154	51.781940
3352.007777	403541.218376	51.786945
3351.624628	403186.771579	51.791949
3350.653318	402827.279620	51.796954
3350.069498	402456.640440	51.801959
3349.041932	402111.840344	51.806964
3348.775421	401744.929872	51.811969
3347.618461	401384.815509	51.816973
3346.990126	401025.960660	51.821978
3346.671030	400671.018185	51.826983
3345.390665	400311.851782	51.831988
3344.704458	399957.798330	51.836993
3344.202491	399606.863870	51.841997
3343.275954	399254.010029	51.847002
3342.777342	398894.526349	51.852007
3341.947729	398554.003680	51.857012
3341.477247	398189.881330	51.862017
3340.856791	397855.546343	51.867021
3340.080393	397498.023258	51.872026
3339.584820	397151.052559	51.877031
3338.669768	396794.789440	51.882036
3338.044538	396454.111075	51.887041
3337.419043	396094.540671	51.892045
3336.765955	395751.469859	51.897050
3335.972559	395399.189322	51.902055
3335.189821	395053.233697	51.907060
3334.541473	394703.007605	51.912065
3333.953610	394363.344446	51.917069
3333.280436	394017.208347	51.922074
3332.669135	393669.406383	51.927079
3331.960255	393328.658796	51.932084
3331.200541	392979.195278	51.937089
3330.533739	392635.459480	51.942093
3329.867991	392279.694088	51.947098
3329.270428	391934.211445	51.952103
3328.624112	391599.640575	51.957108
3327.863979	391238.514637	51.962113
3327.353337	390902.466331	51.967117
3326.511920	390556.627169	51.972122
3325.931405	390203.700202	51.977127
3324.994692	389871.599633	51.982132
3324.332096	389518.399076	51.987137
3323.834872	389181.035399	51.992141
3322.656408	388832.435620	51.997146
3322.148050	388499.618736	52.002151
3321.462371	388170.666403	52.007156
3321.370580	387821.732304	52.012161
3320.412079	387477.788712	52.017165
3319.390682	387149.744675	52.022170
3318.956411	386806.576335	52.027175
3318.109237	386472.421092	52.032180
3317.565356	386128.297358	52.037185
3317.022569	385799.605955	52.042189
3316.112130	385462.628763	52.047194
3315.687851	385111.941074	52.052199
3314.907486	384789.228810	52.057204
3314.167673	384434.820891	52.062209
3313.681573	384106.639415	52.067213
3312.678992	383773.603114	52.072218
3312.097311	383429.231237	52.077223
3311.397996	383101.125474	52.082228
3310.919098	382771.862980	52.087233
3310.207215	382434.343654	52.092237
3309.492859	382097.101447	52.097242
3308.861212	381760.453524	52.102247
3307.558882	381422.331869	52.107252
3307.749104	381090.303900	52.112257
3306.961186	380760.157193	52.117261
3305.854068	380424.284780	52.122266
3305.449609	380090.154933	52.127271
3304.617856	379755.911732	52.132276
3304.184565	379414.862634	52.137281
3303.701804	379090.884647	52.142285
3303.055315	378752.432293	52.147290
3302.292042	378416.004801	52.152295
3301.569574	378075.015138	52.157300
3300.759868	377735.257190	52.162305
3300.157998	377408.944093	52.167309
3299.398827	377066.654307	52.172314
3299.026492	376737.043631	52.177319
3298.269279	376407.618277	52.182324
3297.616475	376061.080661	52.187329
3296.486273	375724.917245	52.192333
3296.053706	375390.115986	52.197338
3295.559720	375057.280286	52.202343
3294.617351	374735.781313	52.207348
3294.066836	374394.351433	52.212353
3293.424692	374058.910952	52.217357
3292.480525	373728.781055	52.222362
3291.998366	373399.567492	52.227367
3290.872507	373066.408477	52.232372
3290.655997	372735.137987	52.237377
3289.653925	372414.342504	52.242381
3288.763704	372092.356677	52.247386
3288.257844	371762.396120	52.252391
3287.766671	371446.243975	52.257396
3287.053278	371118.880504	52.262401
3286.392799	370792.320175	52.267405
3285.709563	370470.518110	52.272410
3285.134216	370141.497097	52.277415
3284.309831	369815.972756	52.282420
3283.614019	369490.476473	52.287425
3282.804608	369166.318579	52.292429
3282.163232	368833.634537	52.297434
3282.055883	368516.026102	52.302439
3280.769882	368202.392458	52.307444
3280.569748	367871.666490	52.312449
3279.839435	367551.681753	52.317453
3278.993513	367222.172425	52.322458
3278.259307	366892.922807	52.327463
3277.716144	366572.774116	52.332468
3277.229288	366250.807816	52.337473
3276.426357	365918.814071	52.342477
3275.329119	365599.483815	52.347482
3275.159769	365275.908250	52.352487
3274.233034	364961.380550	52.357492
3273.657058	364618.248217	52.362497
3272.932363	364315.133357	52.367501
3272.335470	363986.629312	52.372506
3271.603556	363666.006279	52.377511
3270.780873	363345.039138	52.382516
3270.249913	363024.812358	52.387521
3269.421076	362705.597337	52.392525
3268.723253	362385.850498	52.397530
3268.363168	362062.892926	52.402535
3267.393110	361748.960620	52.407540
3267.061767	361427.368094	52.412545
3265.960132	361102.205700	52.417549
3265.314604	360788.012050	52.422554
3264.927499	360467.439571	52.427559
3263.910508	360153.834810	52.432564
3263.696302	359838.828711	52.437569
3262.627306	359518.026894	52.442573
3261.522948	359203.386423	52.447578
3261.336483	358894.425835	52.452583
3260.579117	358577.079987	52.457588
3260.114805	358264.113370	52.462593
3259.308690	357952.343898	52.467597
3258.742837	357642.722841	52.472602
3257.956206	357322.319830	52.477607
3257.326573	357010.058391	52.482612
3256.603652	356694.959644	52.487617
3255.795286	356374.630252	52.492621
3255.088168	356069.754867	52.497626
3254.588723	355746.827815	52.502631
3253.873818	355442.382442	52.507636
3253.169184	355126.176630	52.512641
3252.704174	354818.125233	52.517645
3251.913683	354509.970759	52.522650
3251.085178	354181.639803	52.527655
3250.641217	353874.597296	52.532660
3250.248466	353567.748438	52.537665
3249.319400	353256.478132	52.542669
3248.731652	352927.642987	52.547674
3248.059652	352621.494358	52.552679
3247.078773	352313.509536	52.557684
3246.722323	351990.892433	52.562689
3245.519507	351686.578316	52.567693
3245.211413	351381.764604	52.572698
3244.453236	351061.419494	52.577703
3243.808052	350761.796440	52.582708
3243.088843	350448.822016	52.587713
3242.617381	350144.307013	52.592717
3241.600789	349839.927423	52.597722
3241.396989	349512.435538	52.602727
3240.219970	349204.540100	52.607732
3239.629997	348899.400565	52.612737
3239.199039	348592.350786	52.617741
3238.306140	348285.245109	52.622746
3237.717959	347978.674899	52.627751
3236.897750	347670.841666	52.632756
3236.438359	347356.943042	52.637761
3236.014254	347053.446881	52.642765
3234.724752	346749.780557	52.647770
3234.348742	346429.067861	52.652775
3233.773484	346137.731345	52.657780
3233.051864	345829.159756	52.662785
3232.601660	345516.547508	52.667789
3231.412383	345213.467969	52.672794
3231.134505	344908.486404	52.677799
3230.405195	344600.214856	52.682804
3229.855060	344292.982353	52.687809
3229.204820	343993.272767	52.692813
3228.208389	343680.049776	52.697818
3227.952404	343373.529512	52.702823
3226.963176	343073.436153	52.707828
3226.205736	342759.152323	52.712833
3225.856011	342449.256762	52.717837
3225.111810	342152.861721	52.722842
3224.490366	341846.875044	52.727847
3223.615576	341542.250517	52.732852
3222.958391	341231.633705	52.737857
3222.304877	340934.429263	52.742861
3221.076794	340626.470597	52.747866
3220.936383	340325.694744	52.752871
3220.314201	340028.455510	52.757876
3219.761739	339717.890847	52.762881
3218.754105	339422.415184	52.767885
3217.993481	339121.273434	52.772890
3217.760182	338815.210293	52.777895
3216.987414	338514.780319	52.782900
3216.315443	338208.936384	52.787905
3215.694375	337910.057805	52.792909
3214.914557	337611.482962	52.797914
3214.592678	337308.786785	52.802919
3213.747968	337004.237243	52.807924
3213.257558	336698.968361	52.812929
3212.377424	336395.007071	52.817933
3211.566703	336086.400316	52.822938
3211.263066	335780.741226	52.827943
3209.996331	335479.077060	52.832948
3209.532087	335169.596610	52.837953
3208.801828	334875.660085	52.842957
3208.183979	334579.566102	52.847962
3207.853623	334273.955278	52.852967
3206.971782	333979.606071	52.857972
3206.221222	333669.680371	52.862977
3205.649360	333373.472043	52.867981
3204.448450	333058.777921	52.872986
3204.138793	332767.973445	52.877991
3203.582939	332470.918628	52.882996
3203.125987	332160.557867	52.888001
3202.494850	331868.222131	52.893005
3201.397513	331563.535375	52.898010
3201.024650	331262.322306	52.903015
3200.253067	330959.669010	52.908020
3199.573013	330661.200607	52.913025
3198.631463	330361.983130	52.918029
3197.842079	330069.894234	52.923034
3197.325002	329766.610144	52.928039
3196.618987	329482.856197	52.933044
3196.004950	329181.112572	52.938049
3195.411541	328887.307690	52.943053
3194.610524	328583.809094	52.948058
3194.125938	328297.062332	52.953063
3193.172116	328000.714160	52.958068
3192.674656	327699.353489	52.963073
3191.884778	327410.614924	52.968077
3191.105883	327119.149352	52.973082
3190.445849	326827.740252	52.978087
3189.853672	326536.548461	52.983092
3189.275306	326247.823015	52.988097
3188.576961	325951.273794	52.993101
3187.774104	325658.864539	52.998106
3187.309148	325362.658090	53.003111
3186.540396	325091.908018	53.008116
3185.895299	324789.922997	53.013121
3185.282034	324497.861412	53.018125
3184.645662	324216.801413	53.023130
3183.947315	323907.667109	53.028135
3183.134071	323615.252100	53.033140
3182.465280	323329.611255	53.038145
3181.911090	323046.039095	53.043149
3181.428328	322754.739975	53.048154
3180.279751	322462.934127	53.053159
3179.632492	322169.978581	53.058164
3179.031061	321880.273825	53.063169
3178.306976	321596.927385	53.068173
3177.581764	321320.352944	53.073178
3177.168937	321030.564568	53.078183
3176.440173	320748.641944	53.083188
3175.616241	320451.660130	53.088193
3175.109897	320162.647539	53.093197
3174.320609	319881.444655	53.098202
3174.027429	319583.561181	53.103207
3172.985061	319306.012139	53.108212
3172.423270	319020.773028	53.113217
3171.768898	318727.934471	53.118221
3170.676472	318445.374673	53.123226
3170.169626	318156.533998	53.128231
3169.497657	317876.477637	53.133236
3169.210768	317600.688137	53.138241
3168.432941	317320.519554	53.143245
3167.756168	317025.642188	53.148250
3167.231270	316733.846337	53.153255
3166.185972	316463.367944	53.158260
3165.768597	316165.391354	53.163265
3165.342917	315877.473045	53.168269
3164.286457	315604.345882	53.173274
3163.785714	315304.419212	53.178279
3163.073749	315021.840038	53.183284
3162.441055	314743.016088	53.188289
3161.627807	314457.828637	53.193293
3160.947011	314167.857768	53.198298
3160.597237	313883.766691	53.203303
3159.741956	313613.632456	53.208308
3159.383376	313323.302661	53.213313
3158.747182	313028.967260	53.218317
3157.478145	312755.764243	53.223322
3157.432873	312459.602215	53.228327
3156.538327	312170.016119	53.233332
3155.788944	311885.448140	53.238337
3155.039596	311608.416763	53.243341
3154.180945	311321.343660	53.248346
3153.820078	311033.885472	53.253351
3153.183559	310756.528528	53.258356
3152.472418	310466.501486	53.263361
3151.930064	310172.856514	53.268365
3151.005730	309892.461800	53.273370
3150.463192	309601.005326	53.278375
3149.929815	309326.633380	53.283380
3149.284634	309028.952895	53.288385
3148.370052	308745.192534	53.293389
3147.636157	308466.317595	53.298394
3147.023049	308190.198553	53.303399
3146.056072	307910.035032	53.308404
3145.455646	307628.616010	53.313409
3145.009869	307356.772163	53.318413
3143.810735	307073.307550	53.323418
3144.056602	306782.763527	53.328423
3142.800962	306512.904939	53.333428
3142.169571	306233.575802	53.338433
3141.584890	305964.984998	53.343437
3141.191119	305678.817829	53.348442
3140.586572	305384.738190	53.353447
3139.721425	305112.752182	53.358452
3139.017490	304827.752714	53.363457
3138.472128	304543.211390	53.368461
3137.559939	304268.608156	53.373466
3137.148854	303983.433233	53.378471
3136.257288	303703.503283	53.383476
3136.014591	303417.180053	53.388481
3135.114119	303142.547258	53.393485
3134.406821	302857.009450	53.398490
3133.809369	302568.041258	53.403495
3132.920320	302301.401324	53.408500
3132.039106	302014.055819	53.413505
3131.470475	301731.982689	53.418509
3130.803514	301457.386143	53.423514
3130.311665	301185.970117	53.428519
3129.693582	300908.716361	53.433524
3129.149996	300621.569421	53.438529
3128.498310	300344.701960	53.443533
3127.680358	300066.434207	53.448538
3127.003982	299782.770159	53.453543
3126.080645	299520.791127	53.458548
3125.383634	299239.981623	53.463553
3124.987887	298965.770713	53.468557
3124.027850	298692.463575	53.473562
3123.389031	298408.154533	53.478567
3122.764515	298142.611640	53.483572
3122.260294	297863.475575	53.488577
3121.662431	297589.778282	53.493581
3120.513471	297317.237374	53.498586
3119.797661	297035.281197	53.503591
3119.708138	296771.536100	53.508596
3118.952085	296490.553177	53.513601
3118.315888	296216.223180	53.518605
3117.277024	295946.846149	53.523610
3116.870729	295665.933963	53.528615
3115.636686	295408.683858	53.533620
3115.462925	295133.616969	53.538625
3114.850125	294857.982494	53.543629
3113.988491	294586.690954	53.548634
3113.437908	294310.918542	53.553639
3112.531056	294046.254886	53.558644
3111.789519	293781.259123	53.563649
3111.414530	293502.223505	53.568653
3110.667878	293234.884878	53.573658
3110.057978	292956.165862	53.578663
3109.164011	292692.237028	53.583668
3108.654792	292424.579691	53.588673
3108.346260	292157.934438	53.593677
3107.230860	291887.188974	53.598682
3106.788056	291607.346740	53.603687
3106.055963	291347.058043	53.608692
3105.660116	291075.662952	53.613697
3105.208180	290802.722914	53.618701
3103.966259	290528.557814	53.623706
3103.402163	290262.613044	53.628711
3102.695449	289985.382946	53.633716
3102.199186	289718.993929	53.638721
3101.493614	289445.099338	53.643725
3100.483813	289177.415797	53.648730
3100.251905	288895.779913	53.653735
3099.633563	288640.691354	53.658740
3098.859919	288367.646901	53.663745
3098.402718	288100.842654	53.668749
3097.554899	287820.831254	53.673754
3096.949254	287542.742289	53.678759
3096.243647	287279.694929	53.683764
3095.823751	286996.176891	53.688769
3095.016621	286726.548957	53.693773
3093.818982	286460.624517	53.698778
3093.422092	286195.948405	53.703783
3092.809827	285929.192333	53.708788
3092.254422	285650.813658	53.713793
3091.662303	285375.649545	53.718797
3090.919376	285114.261823	53.723802
3090.340437	284836.191869	53.728807
3089.511966	284580.649501	53.733812
3089.006287	284290.113683	53.738817
3088.179650	284021.072586	53.743821
3087.307085	283754.687269	53.748826
3087.010545	283476.317007	53.753831
3086.110223	283210.954474	53.758836
3085.356096	282925.550679	53.763841
3084.783447	282665.789904	53.768845
3084.139293	282408.281505	53.773850
3083.654048	282127.877385	53.778855
3082.693154	281864.663028	53.783860
3081.924730	281597.801592	53.788865
3081.562052	281331.894541	53.793869
3080.475442	281069.107195	53.798874
3080.091096	280793.729141	53.803879
3079.381740	280537.809224	53.808884
3078.750574	280259.413810	53.813889
3078.286899	280006.994894	53.818893
3077.268787	279733.932445	53.823898
3076.850511	279452.523228	53.828903
3076.134313	279186.798607	53.833908
3075.515245	278910.310895	53.838913
3074.911581	278650.273199	53.843917
3073.919596	278383.140287	53.848922
3073.605953	278111.188296	53.853927
3072.644879	277849.016678	53.858932
3071.904198	277581.283484	53.863937
3071.242119	277312.544523	53.868941
3070.734388	277056.846351	53.873946
3070.040594	276772.398323	53.878951
3069.228248	276522.351315	53.883956
3068.740408	276256.105959	53.888961
3068.086937	275996.457624	53.893965
3067.276022	275728.480550	53.898970
3066.655165	275466.789527	53.903975
3065.654390	275202.357093	53.908980
3065.026904	274941.252854	53.913985
3064.846725	274688.762528	53.918989
3063.852715	274422.316983	53.923994
3063.307357	274152.973432	53.928999
3062.307846	273898.040469	53.934004
3061.905570	273636.696821	53.939009
3061.154822	273367.920631	53.944013
3060.687704	273124.644357	53.949018
3060.018237	272846.381096	53.954023
3059.462426	272602.380315	53.959028
3058.723775	272326.038185	53.964033
3057.938053	272076.827363	53.969037
3057.341639	271816.074905	53.974042
3056.681923	271538.854470	53.979047
3055.976116	271286.651316	53.984052
3055.070557	271025.846050	53.989057
3054.657686	270757.245943	53.994061
3053.711167	270511.167978	53.999066
3053.108557	270242.165062	54.004071
3052.544930	269981.025761	54.009076
3051.979640	269728.724305	54.014081
3051.429730	269472.065401	54.019085
3050.840897	269213.146055	54.024090
3050.361836	268950.796662	54.029095
3049.574328	268686.713399	54.034100
3048.676675	268417.171982	54.039105
3048.010061	268156.176909	54.044109
3047.194338	267903.304447	54.049114
3046.734292	267641.843920	54.054119
3045.681697	267384.246594	54.059124
3045.346390	267122.562799	54.064129
3044.521866	266870.430738	54.069133
3043.864228	266621.761520	54.074138
3043.512316	266353.051488	54.079143
3042.762600	266097.444273	54.084148
3041.680151	265832.110076	54.089153
3041.512232	265577.557107	54.094157
3040.666079	265320.997774	54.099162
3040.052241	265056.506690	54.104167
3039.331897	264798.730737	54.109172
3038.890874	264537.548934	54.114177
3038.124973	264285.052398	54.119181
3037.181824	264017.048550	54.124186
3036.877627	263765.727190	54.129191
3035.601185	263514.763630	54.134196
3035.039719	263249.246696	54.139201
3034.588999	262993.950558	54.144205
3033.920675	262739.478550	54.149210
3033.147569	262479.649570	54.154215
3032.608708	262230.403838	54.159220
3032.042637	261968.734247	54.164225
3031.747150	261713.083391	54.169229
3030.258900	261459.939117	54.174234
3030.204606	261191.083598	54.179239
3029.142299	260937.719511	54.184244
3028.702814	260681.226374	54.189249
3028.168529	260428.874244	54.194253
3027.468345	260163.407216	54.199258
3026.436342	259907.721637	54.204263
3025.818393	259657.802856	54.209268
3025.025465	259397.801315	54.214273
3024.544133	259153.617064	54.219277
3024.094586	258900.412448	54.224282
3023.253044	258645.920338	54.229287
3022.239455	258394.588225	54.234292
3021.580217	258139.099983	54.239297
3021.144274	257878.559542	54.244301
3020.319026	257634.762233	54.249306
3019.980870	257384.495716	54.254311
3019.189832	257131.168645	54.259316
3018.444884	256876.815848	54.264321
3017.785368	256627.466886	54.269325
3016.994122	256387.103570	54.274330
3016.810560	256127.951257	54.279335
3016.043463	255876.888360	54.284340
3015.202795	255620.540190	54.289345
3014.159268	255378.078635	54.294349
3013.905690	255118.989521	54.299354
3013.630846	254860.566234	54.304359
3012.904594	254613.292950	54.309364
3012.379051	254356.667206	54.314369
3011.826478	254094.927166	54.319373
3010.921020	253838.973422	54.324378
3010.374444	253578.888463	54.329383
3009.189042	253318.573901	54.334388
3008.897100	253060.206544	54.339393
3008.364577	252804.093243	54.344397
3007.485612	252553.485050	54.349402
3006.938034	252285.481775	54.354407
3006.029660	252036.534278	54.359412
3005.451905	251775.769105	54.364417
3004.985920	251522.371981	54.369421
3004.014540	251265.413474	54.374426
3003.526157	251004.940870	54.379431
3002.666264	250756.420402	54.384436
3001.552018	250503.280159	54.389441
3001.003921	250255.678783	54.394445
3000.612866	250003.010526	54.399450
3000.006238	249744.392139	54.404455
2999.166479	249499.486563	54.409460
2998.657006	249248.289783	54.414465
2998.027403	248999.888245	54.419469
2997.492001	248750.122457	54.424474
2996.795397	248497.861409	54.429479
2995.773897	248245.015538	54.434484
2995.095237	248000.290467	54.439489
2994.304386	247749.497116	54.444493
2993.727941	247507.048600	54.449498
2992.998650	247246.925705	54.454503
2992.063448	247009.780798	54.459508
2991.491580	246761.679279	54.464513
2991.158318	246519.321182	54.469517
2990.178055	246272.227377	54.474522
2989.675125	246023.810593	54.479527
2989.164471	245783.315344	54.484532
2988.579177	245540.438526	54.489537
2987.928035	245298.896767	54.494541
2986.966981	245045.461049	54.499546
2986.760128	244787.653620	54.504551
2985.775588	244557.829209	54.509556
2984.881369	244302.856326	54.514561
2984.554819	244059.202622	54.519565
2983.368619	243825.133155	54.524570
2983.115523	243576.833968	54.529575
2982.432420	243342.125459	54.534580
2981.702148	243094.972263	54.539585
2981.123961	242843.288093	54.544589
2980.416858	242603.950013	54.549594
2979.769741	242355.129813	54.554599
2978.871909	242122.112737	54.559604
2978.440999	241868.777382	54.564609
2977.813663	241620.923161	54.569613
2976.885522	241391.579204	54.574618
2976.107628	241138.402117	54.579623
2975.607060	240907.972764	54.584628
2975.024620	240662.787168	54.589633
2974.625638	240424.830501	54.594637
2973.663309	240181.081122	54.599642
2973.514096	239931.906844	54.604647
2972.599920	239690.926497	54.609652
2971.836299	239443.302002	54.614657
2971.622763	239190.014199	54.619661
2970.484736	238948.154091	54.624666
2969.978562	238692.825609	54.629671
2969.030585	238457.047914	54.634676
2968.420635	238216.378961	54.639681
2967.652821	237970.107900	54.644685
2966.974924	237730.825810	54.649690
2966.735561	237480.728913	54.654695
2965.966523	237246.427809	54.659700
2965.047416	237007.338248	54.664705
2964.653369	236755.663244	54.669709
2963.780929	236519.699435	54.674714
2963.278372	236277.871808	54.679719
2962.664108	236034.330867	54.684724
2961.823674	235788.381764	54.689729
2961.287991	235547.554120	54.694733
2960.366969	235306.380613	54.699738
2959.959553	235062.376275	54.704743
2958.716085	234826.525894	54.709748
2958.076563	234588.492425	54.714753
2957.449370	234347.554720	54.719757
2957.053630	234116.791755	54.724762
2956.468511	233871.417883	54.729767
2955.702579	233636.309464	54.734772
2955.037457	233401.134708	54.739777
2954.546876	233160.789314	54.744781
2954.014616	232927.453448	54.749786
2953.366830	232669.182660	54.754791
2952.326886	232444.280187	54.759796
2951.860051	232195.734311	54.764801
2951.374081	231952.844849	54.769805
2950.723199	231708.123325	54.774810
2949.920599	231475.648543	54.779815
2949.154875	231238.406974	54.784820
2948.613377	230994.510225	54.789825
2947.578116	230745.548855	54.794829
2946.946114	230511.368903	54.799834
2946.293926	230274.977507	54.804839
2945.382208	230049.551137	54.809844
2944.715990	229807.306821	54.814849
2944.230201	229573.029702	54.819853
2943.590558	229344.150050	54.824858
2942.849669	229105.305878	54.829863
2942.336188	228882.722005	54.834868
2941.785061	228628.240847	54.839873
2941.016309	228402.617687	54.844877
2940.246789	228172.488483	54.849882
2940.053881	227930.352493	54.854887
2938.892043	227703.622111	54.859892
2938.580998	227466.394739	54.864897
2937.924435	227215.269806	54.869901
2937.081332	226981.234302	54.874906
2936.402494	226746.842425	54.879911
2935.544878	226513.370639	54.884916
2935.037066	226275.948534	54.889921
2934.344980	226047.773211	54.894925
2933.433148	225818.258395	54.899930
2933.094606	225569.112093	54.904935
2932.431287	225345.937204	54.909940
2931.513475	225111.002085	54.914945
2931.227736	224881.518008	54.919949
2930.508511	224645.305184	54.924954
2930.017100	224402.628148	54.929959
2928.917094	224170.041474	54.934964
2928.415461	223939.079306	54.939969
2928.056613	223706.223842	54.944973
2926.926336	223473.491195	54.949978
2926.580942	223233.506061	54.954983
2925.790098	223003.050650	54.959988
2925.024344	222760.447440	54.964993
2924.585697	222524.272767	54.969997
2923.860121	222292.077801	54.975002
2923.227833	222058.557564	54.980007
2922.418504	221825.244274	54.985012
2922.083869	221579.075716	54.990017
2921.204038	221344.120148	54.995021
2920.279235	221119.292613	55.000026
2919.863224	220871.560698	55.005031
2919.427687	220639.541158	55.010036
2918.719435	220403.224683	55.015041
2918.036149	220168.190685	55.020045
2917.026782	219935.309435	55.025050
2916.637078	219698.193678	55.030055
2915.880843	219463.975394	55.035060
2914.777825	219225.446541	55.040065
2914.454143	219001.828532	55.045069
2913.389430	218769.608889	55.050074
2912.992768	218532.968941	55.055079
2912.159708	218299.784859	55.060084
2911.701863	218076.394578	55.065089
2910.887203	217856.969362	55.070093
2910.154008	217620.067434	55.075098
2909.709217	217387.003013	55.080103
2908.478800	217166.283711	55.085108
2908.357975	216937.408252	55.090113
2907.765493	216709.308310	55.095117
2906.792711	216488.613956	55.100122
2906.386467	216254.554270	55.105127
2905.963301	216042.353606	55.110132
2905.119828	215796.654065	55.115137
2904.418149	215577.014329	55.120141
2903.253413	215347.672891	55.125146
2903.006127	215110.524223	55.130151
2901.785629	214893.807319	55.135156
2901.661519	214668.669304	55.140161
2900.967855	214444.487762	55.145165
2900.389370	214217.946658	55.150170
2899.613174	213992.710469	55.155175
2898.715203	213766.603317	55.160180
2897.979084	213538.676579	55.165185
2897.521639	213326.133333	55.170189
2896.927325	213097.752870	55.175194
2896.901116	212864.280991	55.180199
2895.978192	212642.598314	55.185204
2895.083076	212412.842265	55.190209
2894.454880	212173.396769	55.195213
2893.395007	211954.945594	55.200218
2892.851864	211724.105233	55.205223
2892.242708	211495.554465	55.210228
2891.642553	211275.441757	55.215233
2890.996842	211046.172861	55.220237
2890.234909	210827.805570	55.225242
2890.089421	210601.679210	55.230247
2889.189509	210375.482194	55.235252
2888.182146	210145.013724	55.240257
2887.628502	209909.319497	55.245261
2886.616577	209693.350305	55.250266
2886.114881	209461.556925	55.255271
2885.376524	209249.135133	55.260276
2884.622632	209032.516418	55.265281
2884.390767	208809.922937	55.270285
2883.849624	208584.324628	55.275290
2883.077685	208354.716358	55.280295
2882.200567	208136.312975	55.285300
2881.514638	207908.805488	55.290305
2881.247324	207690.128937	55.295309
2880.226473	207463.185228	55.300314
2879.638072	207239.241139	55.305319
2879.251241	207025.129506	55.310324
2878.479887	206795.946973	55.315329
2877.865852	206569.247628	55.320333
2876.857105	206339.773516	55.325338
2876.625856	206121.325985	55.330343
2875.810457	205897.753714	55.335348
2875.181832	205676.163550	55.340353
2874.763524	205445.466673	55.345357
2874.008468	205211.184160	55.350362
2873.148736	204987.355072	55.355367
2872.527538	204762.101851	55.360372
2871.805548	204538.265385	55.365377
2871.183544	204309.832369	55.370381
2870.282496	204084.333361	55.375386
2869.912984	203849.715246	55.380391
2869.282980	203642.246643	55.385396
2868.402345	203416.734271	55.390401
2867.698670	203187.885910	55.395405
2867.006498	202966.201539	55.400410
2866.673344	202729.469660	55.405415
2866.109618	202524.997989	55.410420
2864.961994	202287.989687	55.415425
2864.733908	202064.173695	55.420429
2863.567635	201841.576151	55.425434
2863.025747	201606.561850	55.430439
2862.436932	201399.158518	55.435444
2861.821826	201173.600272	55.440449
2861.300287	200951.896774	55.445453
2860.638283	200730.585450	55.450458
2860.138921	200509.961892	55.455463
2859.118029	200282.117264	55.460468
2858.249075	200061.095904	55.465473
2857.846180	199825.443561	55.470477
2856.931071	199613.224689	55.475482
2856.423256	199392.199734	55.480487
2855.914848	199175.858725	55.485492
2855.088617	198954.440584	55.490497
2854.581335	198726.317492	55.495501
2853.731598	198502.079903	55.500506
2853.091907	198282.963695	55.505511
2852.283241	198059.548585	55.510516
2851.397123	197841.923873	55.515521
2851.223248	197620.496983	55.520525
2850.034089	197415.138065	55.525530
2849.648717	197185.767898	55.530535
2849.003920	196972.536810	55.535540
2848.536073	196755.308405	55.540545
2847.631995	196535.948593	55.545549
2846.996062	196320.021086	55.550554
2846.536035	196092.219922	55.555559
2845.838149	195890.123017	55.560564
2844.919043	195663.312606	55.565569
2844.465442	195437.765538	55.570573
2843.672850	195226.651799	55.575578
2842.827449	195010.470240	55.580583
2842.413072	194794.208601	55.585588
2841.577442	194576.474946	55.590593
2841.166763	194357.771492	55.595597
2840.090144	194148.450392	55.600602
2839.964415	193926.598949	55.605607
2839.156131	193704.016784	55.610612
2838.125656	193490.988372	55.615617
2837.837307	193265.322916	55.620621
2837.199563	193056.013168	55.625626
2836.755152	192829.203781	55.630631
2835.460350	192618.383988	55.635636
2835.305094	192393.388458	55.640641
2834.806277	192175.917175	55.645645
2833.838514	191957.426878	55.650650
2833.791653	191725.762728	55.655655
2833.056935	191508.382628	55.660660
2832.261341	191277.997002	55.665665
2831.700012	191061.990995	55.670669
2830.818797	190837.193859	55.675674
2830.268874	190600.767076	55.680679
2829.290272	190382.374559	55.685684
2828.781479	190154.226265	55.690689
2827.610524	189936.769564	55.695693
2826.902590	189723.617245	55.700698
2826.602104	189496.864042	55.705703
2825.879991	189285.039102	55.710708
2825.171635	189074.434316	55.715713
2824.660875	188844.256867	55.720717
2823.895798	188630.749487	55.725722
2823.048875	188405.767403	55.730727
2822.402988	188192.548457	55.735732
2821.585050	187977.233043	55.740737
2821.305163	187763.410989	55.745741
2820.490409	187548.326032	55.750746
2820.148068	187325.788223	55.755751
2819.450388	187104.109258	55.760756
2818.517880	186887.862798	55.765761
2817.675249	186669.045931	55.770765
2817.240381	186463.205764	55.775770
2816.808135	186234.491681	55.780775
2815.903853	186022.773854	55.785780
2815.175959	185810.367515	55.790785
2814.536550	185586.778257	55.795789
2813.938936	185372.966606	55.800794
2813.513131	185157.831111	55.805799
2812.772683	184941.156239	55.810804
2811.988124	184723.268097	55.815809
2811.473460	184497.221830	55.820813
2810.603838	184281.575566	55.825818
2809.906119	184068.243864	55.830823
2809.380116	183853.092241	55.835828
2808.672757	183639.255232	55.840833
2808.111188	183413.730665	55.845837
2807.417007	183200.733264	55.850842
2806.791969	182968.046183	55.855847
2805.862513	182759.311596	55.860852
2805.270757	182539.851491	55.865857
2804.865071	182322.016732	55.870861
2803.820929	182115.058839	55.875866
2803.373274	181893.403819	55.880871
2802.600942	181678.517949	55.885876
2801.626183	181466.018537	55.890881
2801.117748	181245.737527	55.895885
2800.369423	181043.648017	55.900890
2800.117393	180820.491822	55.905895
2799.334150	180615.242392	55.910900
2798.555209	180395.924391	55.915905
2798.105001	180181.325585	55.920909
2797.370889	179959.623969	55.925914
2796.820751	179744.597943	55.930919
2796.065296	179528.155403	55.935924
2795.265681	179315.626037	55.940929
2794.827910	179098.588373	55.945933
2793.920756	178879.527350	55.950938
2793.298594	178660.880226	55.955943
2792.970257	178451.307857	55.960948
2792.332171	178234.115515	55.965953
2791.574454	178015.480459	55.970957
2790.723021	177799.608833	55.975962
2789.989833	177582.256821	55.980967
2789.206043	177371.019344	55.985972
2788.540038	177153.951450	55.990977
2788.298481	176937.033677	55.995981
2787.195637	176720.342489	56.000986
2786.830089	176506.702749	56.005991
2785.772023	176293.377306	56.010996
2785.203214	176086.576719	56.016001
2784.861127	175871.422939	56.021005
2784.158667	175657.344883	56.026010
2783.503373	175443.629316	56.031015
2782.653715	175232.095142	56.036020
2781.780521	175012.133176	56.041025
2781.414339	174801.376798	56.046029
2780.107421	174594.751482	56.051034
2779.946291	174376.969504	56.056039
2779.355688	174179.301234	56.061044
2778.678784	173968.763711	56.066049
2778.221487	173743.629842	56.071053
2777.229300	173537.074506	56.076058
2776.667845	173325.504562	56.081063
2776.090707	173108.723719	56.086068
2775.291908	172896.443243	56.091073
2774.777132	172683.457554	56.096077
2773.964450	172477.108144	56.101082
2773.596597	172253.812547	56.106087
2772.898159	172055.802940	56.111092
2772.165645	171837.616455	56.116097
2771.509321	171623.056387	56.121101
2770.382390	171417.283671	56.126106
2769.802154	171205.880522	56.131111
2769.063002	170997.784816	56.136116
2768.668015	170782.246805	56.141121
2768.064463	170566.501380	56.146125
2767.134295	170360.601267	56.151130
2766.801028	170159.274939	56.156135
2765.926402	169957.424973	56.161140
2765.268517	169739.619793	56.166145
2764.864051	169524.611603	56.171149
2764.146662	169320.756155	56.176154
2763.703628	169103.721673	56.181159
2763.035227	168898.093026	56.186164
2761.976670	168680.815062	56.191169
2761.529695	168460.948955	56.196173
2760.717280	168258.754621	56.201178
2760.389287	168046.324023	56.206183
2759.694645	167844.583729	56.211188
2758.656839	167631.186965	56.216193
2758.080691	167407.392527	56.221197
2757.595935	167201.336946	56.226202
2757.104628	166981.905992	56.231207
2756.138507	166778.345051	56.236212
2755.267602	166563.427323	56.241217
2754.827183	166350.680650	56.246221
2753.923937	166141.950451	56.251226
2753.519053	165935.838238	56.256231
2752.620853	165730.186777	56.261236
2752.120870	165515.750331	56.266241
2751.637962	165306.309682	56.271245
2750.615800	165100.185405	56.276250
2750.039915	164886.769125	56.281255
2749.341587	164682.528624	56.286260
2749.055584	164474.561882	56.291265
2748.241686	164260.271391	56.296269
2747.370285	164055.019102	56.301274
2746.767881	163842.134357	56.306279
2746.490015	163630.038626	56.311284
2745.705563	163429.734947	56.316289
2744.977454	163208.939572	56.321293
2744.261780	163000.171870	56.326298
2743.552225	162775.841417	56.331303
2742.884383	162568.301943	56.336308
2742.393026	162366.063150	56.341313
2741.759111	162155.621699	56.346317
2740.871776	161946.251493	56.351322
2740.237815	161736.524494	56.356327
2739.442903	161526.315631	56.361332
2738.925485	161315.097742	56.366337
2738.196927	161101.981972	56.371341
2737.092075	160897.267580	56.376346
2736.999027	160689.215536	56.381351
2736.075081	160488.772185	56.386356
2735.494351	160280.303927	56.391361
2735.217919	160066.092854	56.396365
2734.067846	159855.632193	56.401370
2733.903962	159645.970074	56.406375
2732.918891	159443.088533	56.411380
2732.487686	159223.465603	56.416385
2732.058872	159016.595308	56.421389
2731.154340	158809.471039	56.426394
2730.178603	158606.338551	56.431399
2729.740125	158327.223843	56.436404
2728.804764	158113.942618	56.441409
2728.156791	157909.185801	56.446413
2727.630774	157701.639417	56.451418
2727.103372	157488.640625	56.456423
2725.941809	157288.787021	56.461428
2725.051727	157068.029833	56.466433
2725.001174	156870.557895	56.471437
2724.440342	156667.930305	56.476442
2723.689835	156459.257334	56.481447
2722.833293	156249.420158	56.486452
2722.205425	156051.408730	56.491457
2721.904510	155837.837564	56.496461
2720.657593	155629.489797	56.501466
2720.388203	155425.463122	56.506471
2719.271717	155219.754032	56.511476
2718.660863	155019.292422	56.516481
2718.342205	154810.586473	56.521485
2717.214554	154610.488805	56.526490
2716.535730	154402.211063	56.531495
2716.026668	154198.661896	56.536500
2715.176083	153996.261262	56.541505
2714.972002	153803.496495	56.546509
2713.921628	153600.329052	56.551514
2713.314656	153386.478531	56.556519
2712.536935	153197.748653	56.561524
2711.900694	152996.146299	56.566529
2711.451734	152790.346206	56.571533
2710.809890	152599.132191	56.576538
2710.550763	152386.529465	56.581543
2709.651650	152179.647740	56.586548
2709.124572	151985.190467	56.591553
2708.472462	151774.293611	56.596557
2707.531865	151571.108382	56.601562
2706.790240	151359.859730	56.606567
2706.324469	151163.198611	56.611572
2705.858820	150956.281255	56.616577
2705.162457	150744.470101	56.621581
2704.125890	150551.373009	56.626586
2703.828968	150341.293323	56.631591
2702.944605	150142.365924	56.636596
2702.015207	149932.986438	56.641601
2701.640300	149730.269471	56.646605
2700.945299	149531.544563	56.651610
2700.583893	149316.562912	56.656615
2699.888211	149120.141108	56.661620
2699.147156	148913.775966	56.666625
2698.314112	148707.032711	56.671629
2697.600482	148513.273738	56.676634
2697.088835	148298.678496	56.681639
2696.529828	148091.628856	56.686644
2695.475834	147886.654333	56.691649
2694.697724	147688.004733	56.696653
2694.246013	147489.012336	56.701658
2693.804927	147280.220788	56.706663
2692.856650	147086.342360	56.711668
2692.247154	146868.950765	56.716673
2691.511433	146675.358876	56.721677
2690.832571	146476.205426	56.726682
2690.302065	146270.090776	56.731687
2689.560595	146073.898177	56.736692
2689.058457	145870.768145	56.741697
2688.468473	145666.026653	56.746701
2687.602189	145471.369864	56.751706
2687.195554	145262.675052	56.756711
2686.332552	145058.654293	56.761716
2685.401486	144861.457187	56.766721
2685.105191	144669.409161	56.771725
2684.347002	144458.945423	56.776730
2683.636111	144261.806155	56.781735
2682.948249	144055.591121	56.786740
2682.330289	143850.484650	56.791745
2681.911003	143659.733075	56.796749
2681.032654	143455.737899	56.801754
2680.642854	143258.719293	56.806759
2680.095287	143053.988141	56.811764
2678.933300	142837.881010	56.816769
2678.721083	142630.519942	56.821773
2677.838869	142434.308910	56.826778
2677.112230	142239.065625	56.831783
2676.552796	142024.647700	56.836788
2675.579159	141817.171314	56.841793
2675.143842	141619.280896	56.846797
2674.534087	141419.437148	56.851802
2673.801077	141210.592536	56.856807
2673.263861	141013.522695	56.861812
2672.366378	140817.222771	56.866817
2671.997356	140615.211456	56.871821
2671.169116	140422.905609	56.876826
2670.830487	140206.953396	56.881831
2670.044967	140005.952384	56.886836
2668.902210	139798.630884	56.891841
2668.911454	139594.393698	56.896845
2667.873454	139396.422639	56.901850
2667.860239	139186.563075	56.906855
2666.876691	138977.227188	56.911860
2665.859216	138766.436993	56.916865
2665.693547	138564.762914	56.921869
2664.742401	138358.602586	56.926874
2663.713965	138148.085292	56.931879
2663.189411	137948.276391	56.936884
2662.613487	137748.260980	56.941889
2661.750385	137542.168572	56.946893
2660.948291	137345.609369	56.951898
2660.566972	137145.935617	56.956903
2659.804378	136951.850219	56.961908
2659.231408	136748.016926	56.966913
2658.684957	136546.175465	56.971917
2657.891399	136346.788405	56.976922
2657.380913	136150.254459	56.981927
2656.992228	135946.029075	56.986932
2656.107915	135725.571333	56.991937
2655.372116	135513.590821	56.996941
2654.706530	135322.994439	57.001946
2654.280776	135119.568338	57.006951
2653.638033	134917.029201	57.011956
2652.773151	134709.965987	57.016961
2652.516544	134497.599318	57.021965
2651.298814	134288.346451	57.026970
2650.809421	134090.743193	57.031975
2650.045466	133883.720688	57.036980
2649.185223	133677.223057	57.041985
2648.794214	133479.087543	57.046989
2647.938904	133277.088962	57.051994
2647.489175	133075.421326	57.056999
2646.773082	132871.434544	57.062004
2645.957887	132667.833299	57.067009
2645.461566	132465.034062	57.072013
2644.698834	132268.172561	57.077018
2643.935758	132061.772753	57.082023
2643.152812	131873.529593	57.087028
2642.441373	131668.826591	57.092033
2642.067162	131462.902998	57.097037
2641.110399	131271.223601	57.102042
2640.760128	131060.497647	57.107047
2639.856557	130874.452294	57.112052
2639.313872	130680.907563	57.117057
2638.745175	130470.144397	57.122061
2637.926385	130277.116155	57.127066
2637.500718	130062.344975	57.132071
2636.641454	129870.875546	57.137076
2636.065028	129676.250704	57.142081
2635.465232	129466.071547	57.147085
2634.258009	129270.749280	57.152090
2633.778494	129066.485627	57.157095
2633.291124	128872.868356	57.162100
2632.592615	128680.136862	57.167105
2631.986334	128474.779918	57.172109
2631.134812	128290.521577	57.177114
2630.564157	128080.907062	57.182119
2629.872229	127897.108672	57.187124
2628.937590	127695.975378	57.192129
2628.839433	127499.740434	57.197133
2628.068004	127306.166381	57.202138
2627.077614	127108.361032	57.207143
2626.836764	126915.658168	57.212148
2626.329401	126717.779075	57.217153
2625.655392	126506.872036	57.222157
2624.795234	126321.929670	57.227162
2624.019483	126113.556391	57.232167
2623.702292	125914.471847	57.237172
2623.003632	125709.480295	57.242177
2622.730705	125502.479759	57.247181
2621.745818	125300.813155	57.252186
2620.850089	125090.536344	57.257191
2620.227100	124892.980849	57.262196
2619.359625	124694.652776	57.267201
2619.175422	124494.173296	57.272205
2618.145252	124299.505875	57.277210
2617.556148	124092.159804	57.282215
2616.883023	123905.794606	57.287220
2616.068677	123696.214154	57.292225
2615.608775	123505.779691	57.297229
2614.716681	123300.138560	57.302234
2614.140172	123100.163347	57.307239
2613.543320	122899.557923	57.312244
2612.812501	122694.949841	57.317249
2612.459751	122490.664355	57.322253
2611.754201	122296.226646	57.327258
2610.904893	122099.413192	57.332263
2609.981399	121899.882876	57.337268
2609.255861	121697.376767	57.342273
2608.941435	121496.699021	57.347277
2608.333757	121314.430173	57.352282
2607.526390	121103.180127	57.357287
2607.139205	120908.321175	57.362292
2606.093929	120716.577243	57.367297
2605.638623	120512.958067	57.372301
2604.776697	120312.058626	57.377306
2604.070023	120109.333115	57.382311
2603.401591	119929.826024	57.387316
2602.552138	119724.523208	57.392321
2602.355986	119523.968664	57.397325
2601.394787	119327.574471	57.402330
2600.676307	119131.448004	57.407335
2600.194452	118942.300369	57.412340
2599.362687	118759.932352	57.417345
2598.898266	118547.524840	57.422349
2598.269492	118355.789282	57.427354
2597.578244	118159.951466	57.432359
2596.772720	117968.049986	57.437364
2595.916687	117778.455908	57.442369
2595.518171	117577.561164	57.447373
2594.596140	117383.555907	57.452378
2594.262318	117184.037808	57.457383
2593.494193	117002.814661	57.462388
2592.874403	116805.693499	57.467393
2592.296530	116609.227364	57.472397
2591.400209	116407.760449	57.477402
2590.914925	116210.038544	57.482407
2590.294891	116015.824336	57.487412
2589.466780	115824.259758	57.492417
2588.960769	115629.649554	57.497421
2587.995979	115439.499615	57.502426
2587.383870	115241.481567	57.507431
2587.039664	115050.817242	57.512436
2586.283063	114856.614442	57.517441
2585.787665	114667.963644	57.522445
2585.020916	114472.165883	57.527450
2584.422565	114270.313157	57.532455
2583.433544	114082.969937	57.537460
2582.621266	113876.927085	57.542465
2582.558832	113682.674027	57.547469
2581.664539	113500.899114	57.552474
2581.175463	113297.672235	57.557479
2580.322603	113102.825366	57.562484
2579.616131	112907.588691	57.567489
2579.213493	112706.123643	57.572493
2578.162724	112508.628073	57.577498
2577.524683	112311.620803	57.582503
2576.985935	112112.612861	57.587508
2576.060824	111926.024468	57.592513
2575.557668	111734.109341	57.597517
2574.668999	111541.380980	57.602522
2574.044920	111366.020367	57.607527
2573.428848	111176.646952	57.612532
2572.939904	110983.973787	57.617537
2572.046369	110776.636571	57.622541
2571.286977	110604.431482	57.627546
2570.905616	110412.919749	57.632551
2570.378818	110226.046174	57.637556
2569.432438	110027.113177	57.642561
2569.189728	109834.968375	57.647565
2568.428073	109637.919388	57.652570
2567.720788	109445.921056	57.657575
2567.299919	109255.173383	57.662580
2566.595843	109062.726977	57.667585
2565.669956	108865.494452	57.672589
2564.910151	108670.712021	57.677594
2564.540014	108467.264656	57.682599
2564.025672	108280.435617	57.687604
2562.896305	108089.041495	57.692609
2562.670964	107885.702933	57.697613
2561.815922	107701.927405	57.702618
2561.010493	107496.444085	57.707623
2560.238136	107309.409567	57.712628
2559.681021	107116.986930	57.717633
2559.175197	106915.401479	57.722637
2558.510546	106728.703356	57.727642
2557.945436	106529.541693	57.732647
2557.559286	106337.193330	57.737652
2556.173921	106152.054235	57.742657
2555.880795	105956.489907	57.747661
2555.035713	105763.362286	57.752666
2554.541217	105567.287370	57.757671
2553.610523	105373.719615	57.762676
2553.065106	105181.862555	57.767681
2552.210785	104990.189232	57.772685
2551.307208	104814.672521	57.777690
2550.804328	104608.061878	57.782695
2550.340488	104430.340143	57.787700
2549.414517	104241.615386	57.792705
2548.970779	104060.486195	57.797709
2548.203913	103866.517663	57.802714
2547.972335	103675.206649	57.807719
2546.939285	103485.261360	57.812724
2546.191215	103304.966517	57.817729
2545.981877	103113.294880	57.822733
2545.185440	102927.694091	57.827738
2544.409307	102726.427829	57.832743
2543.747684	102549.113136	57.837748
2543.024502	102353.151678	57.842753
2542.491716	102151.674113	57.847757
2542.136074	101969.157614	57.852762
2541.001915	101778.436397	57.857767
2540.251779	101595.046437	57.862772
2539.568443	101401.624128	57.867777
2539.542490	101208.156307	57.872781
2538.217414	101025.680277	57.877786
2537.930368	100832.942061	57.882791
2537.384748	100637.747047	57.887796
2536.467415	100452.445062	57.892801
2535.567574	100267.059313	57.897805
2534.859417	100071.679124	57.902810
2534.843453	99885.090618	57.907815
2533.531567	99702.832190	57.912820
2532.968187	99520.748340	57.917825
2532.365181	99327.032374	57.922829
2531.441422	99147.755197	57.927834
2530.938423	98959.081972	57.932839
2530.493307	98774.505082	57.937844
2529.590724	98585.803099	57.942849
2529.097716	98397.722779	57.947853
2528.466985	98215.241253	57.952858
2527.903386	98018.441018	57.957863
2527.187325	97840.143259	57.962868
2526.485423	97646.057491	57.967873
2526.338889	97455.500679	57.972877
2524.960502	97272.295238	57.977882
2524.667665	97080.223471	57.982887
2524.200984	96890.641786	57.987892
2523.186298	96695.205616	57.992897
2522.368569	96506.278965	57.997901
2521.788272	96327.914392	58.002906
2521.380504	96135.221873	58.007911
2520.197670	95945.634724	58.012916
2519.429878	95768.464901	58.017921
2519.189124	95576.093131	58.022925
2518.533166	95389.801155	58.027930
2518.174339	95212.247403	58.032935
2517.437971	95017.035241	58.037940
2516.428096	94835.776086	58.042945
2515.757470	94641.558783	58.047949
2515.336498	94458.852133	58.052954
2514.968751	94267.799028	58.057959
2513.917893	94085.804070	58.062964
2513.178009	93898.478638	58.067969
2512.916885	93698.649215	58.072973
2511.909382	93511.344072	58.077978
2510.793752	93323.176160	58.082983
2510.579093	93142.223154	58.087988
2510.145012	92950.494219	58.092993
2509.646898	92763.380933	58.097997
2508.523965	92580.027220	58.103002
2508.016000	92385.848066	58.108007
2507.589633	92201.936814	58.113012
2506.554471	92017.635318	58.118017
2505.856294	91830.054297	58.123021
2505.314047	91640.693664	58.128026
2504.629737	91449.714844	58.133031
2504.042061	91263.820492	58.138036
2503.267403	91075.224407	58.143041
2502.844561	90886.631229	58.148045
2502.034531	90710.154918	58.153050
2501.472440	90515.062297	58.158055
2500.597615	90327.401553	58.163060
2499.361521	90158.491915	58.168065
2499.431803	89960.089255	58.173069
2498.346416	89784.741920	58.178074
2497.721882	89604.459772	58.183079
2497.039972	89421.861262	58.188084
2496.616596	89235.374675	58.193089
2496.221796	89050.850650	58.198093
2494.921174	88867.898343	58.203098
2494.603809	88683.599735	58.208103
2494.245252	88498.859062	58.213108
2493.053257	88325.461409	58.218113
2492.779051	88131.720189	58.223117
2492.079842	87947.722923	58.228122
2491.354116	87756.770148	58.233127
2490.825792	87584.141776	58.238132
2490.096798	87396.895193	58.243137
2489.423777	87203.415677	58.248141
2488.724664	87028.105382	58.253146
2488.024393	86830.043555	58.258151
2487.251885	86659.103254	58.263156
2486.342956	86477.402307	58.268161
2486.003929	86288.886308	58.273165
2485.193976	86115.623311	58.278170
2484.352726	85923.164569	58.283175
2483.951887	85749.123316	58.288180
2483.358295	85567.969625	58.293185
2482.729533	85386.055989	58.298189
2481.757446	85207.716586	58.303194
2481.282035	85013.439376	58.308199
2480.810363	84832.354990	58.313204
2479.871973	84651.377825	58.318209
2479.246945	84470.751873	58.323213
2478.351141	84287.489011	58.328218
2477.767650	84108.044930	58.333223
2477.421304	83932.551889	58.338228
2476.809532	83752.601846	58.343233
2475.986463	83559.090278	58.348237
2474.856444	83395.769476	58.353242
2474.305630	83217.120079	58.358247
2473.978693	83033.606714	58.363252
2473.156958	82859.471970	58.368257
2472.964207	82680.668920	58.373261
2471.852169	82498.317838	58.378266
2471.547021	82315.111503	58.383271
2471.135592	82135.827994	58.388276
2470.186541	81954.786820	58.393281
2469.459512	81762.886397	58.398285
2468.712342	81587.058058	58.403290
2468.219421	81394.268243	58.408295
2467.577839	81214.319223	58.413300
2466.967479	81042.999097	58.418305
2466.325515	80849.185825	58.423309
2465.472651	80668.888380	58.428314
2464.821358	80486.709900	58.433319
2464.255389	80299.683792	58.438324
2463.417814	80127.665683	58.443329
2462.920010	79941.684037	58.448333
2461.949510	79769.366744	58.453338
2461.743824	79588.209201	58.458343
2461.020363	79401.045027	58.463348
2460.262435	79208.298417	58.468353
2459.891353	79028.908425	58.473357
2458.739507	78847.368684	58.478362
2458.303527	78663.264533	58.483367
2457.560017	78482.632854	58.488372
2456.629556	78297.476004	58.493377
2456.340109	78104.380240	58.498381
2455.240349	77935.717177	58.503386
2454.621848	77749.818718	58.508391
2454.197414	77574.638551	58.513396
2453.391881	77403.195668	58.518401
2452.683663	77214.382317	58.523405
2451.931400	77043.301530	58.528410
2451.444269	76855.685757	58.533415
2450.708969	76682.793002	58.538420
2450.008268	76509.636424	58.543425
2449.436701	76328.071293	58.548429
2448.827682	76144.821880	58.553434
2447.982654	75972.332724	58.558439
2447.725177	75791.159785	58.563444
2447.093345	75617.987184	58.568449
2446.347684	75427.536178	58.573453
2445.978057	75251.676579	58.578458
2444.990172	75055.653609	58.583463
2444.377307	74877.643519	58.588468
2443.481656	74703.367385	58.593473
2443.046220	74522.937270	58.598477
2442.327794	74345.297074	58.603482
2441.617715	74156.271615	58.608487
2440.841901	73966.326988	58.613492
2440.228738	73791.944233	58.618497
2439.645102	73609.898485	58.623501
2438.525827	73445.286212	58.628506
2438.086952	73256.276879	58.633511
2437.674262	73074.088500	58.638516
2436.806599	72896.440396	58.643521
2436.218238	72721.581498	58.648525
2435.369759	72549.438878	58.653530
2434.770297	72376.333305	58.658535
2434.180618	72202.233050	58.663540
2433.278461	72032.909889	58.668545
2432.928036	71852.534606	58.673549
2431.909336	71668.820642	58.678554
2431.337216	71495.154553	58.683559
2430.551372	71332.451641	58.688564
2430.005969	71159.778827	58.693569
2429.643141	70984.392593	58.698573
2428.697002	70805.749297	58.703578
2428.022752	70627.279881	58.708583
2427.508389	70451.573971	58.713588
2426.588685	70291.326993	58.718593
2426.079092	70110.916732	58.723597
2425.185175	69943.656130	58.728602
2424.776941	69764.221143	58.733607
2424.169458	69589.538497	58.738612
2423.474581	69418.494493	58.743617
2422.817200	69238.388013	58.748621
2421.909560	69077.509214	58.753626
2421.562371	68911.139819	58.758631
2421.050250	68728.943695	58.763636
2420.248127	68557.094416	58.768641
2419.401166	68373.409173	58.773645
2418.875538	68213.578996	58.778650
2418.488896	68032.876918	58.783655
2417.790508	67852.130930	58.788660
2416.848963	67686.778233	58.793665
2416.610376	67505.392504	58.798669
2415.789610	67326.032536	58.803674
2415.057698	67150.251281	58.808679
2414.166669	66982.515108	58.813684
2413.445778	66808.894925	58.818689
2413.032329	66628.013764	58.823693
2412.413312	66455.203930	58.828698
2411.779783	66276.121618	58.833703
2410.979081	66100.962419	58.838708
2410.286231	65932.627562	58.843713
2409.732655	65754.281543	58.848717
2409.097244	65590.636579	58.853722
2408.709699	65408.850714	58.858727
2408.059169	65219.128713	58.863732
2406.936028	65047.643140	58.868737
2406.745356	64869.703709	58.873741
2405.787473	64697.837238	58.878746
2405.372998	64511.650135	58.883751
2404.914387	64328.897809	58.888756
2404.019760	64156.057249	58.893761
2403.693738	63969.649224	58.898765
2402.575989	63796.967597	58.903770
2401.870037	63610.249692	58.908775
2400.939079	63449.782189	58.913780
2400.388633	63269.280355	58.918785
2399.889304	63081.679978	58.923789
2398.847592	62913.809956	58.928794
2398.384916	62734.749330	58.933799
2397.799882	62564.593713	58.938804
2397.092085	62398.932668	58.943809
2396.436780	62219.065270	58.948813
2395.695976	62051.297603	58.953818
2395.340711	61866.532542	58.958823
2394.627486	61694.046419	58.963828
2393.837129	61523.498946	58.968833
2393.362006	61345.748211	58.973837
2392.539084	61180.590925	58.978842
2391.860100	60987.654636	58.983847
2391.411247	60815.334036	58.988852
2390.320221	60638.140316	58.993857
2389.991472	60465.357496	58.998861
2388.878688	60284.096300	59.003866
2388.449084	60119.683670	59.008871
2387.911033	59933.690717	59.013876
2387.028983	59768.374728	59.018881
2386.978981	59588.388876	59.023885
2385.858037	59417.653283	59.028890
2385.308409	59240.428024	59.033895
2384.709559	59059.913833	59.038900
2383.771801	58890.492983	59.043905
2383.481494	58712.250312	59.048909
2382.621721	58530.190408	59.053914
2382.112820	58355.967833	59.058919
2381.350254	58186.152074	59.063924
2380.618953	58016.700077	59.068929
2380.257246	57832.361794	59.073933
2379.379951	57664.955577	59.078938
2378.841203	57483.858355	59.083943
2378.016072	57300.858571	59.088948
2377.179470	57129.595554	59.093953
2376.579451	56950.921908	59.098957
2375.821362	56781.915864	59.103962
2375.388621	56600.361007	59.108967
2374.626508	56429.928212	59.113972
2373.569994	56263.480915	59.118977
2373.392386	56080.941198	59.123981
2372.616700	55913.512528	59.128986
2371.576113	55744.310734	59.133991
2371.347867	55565.661139	59.138996
2370.427322	55402.352254	59.144001
2369.880847	55218.588308	59.149005
2368.902419	55059.481849	59.154010
2368.439374	54883.699087	59.159015
2367.968815	54726.841061	59.164020
2366.903684	54554.704582	59.169025
2366.631328	54374.462722	59.174029
2365.884514	54216.731949	59.179034
2364.913616	54034.964926	59.184039
2364.836022	53868.573943	59.189044
2363.949693	53703.107026	59.194049
2363.268652	53527.375009	59.199053
2362.746479	53364.616032	59.204058
2362.148575	53186.627327	59.209063
2361.521361	53009.100685	59.214068
2360.781438	52844.748038	59.219073
2360.389540	52663.570543	59.224077
2359.401275	52491.235647	59.229082
2358.594149	52320.731108	59.234087
2358.211478	52141.911593	59.239092
2357.365363	51972.729681	59.244097
2356.923963	51794.369065	59.249101
2355.862630	51626.680054	59.254106
2355.241788	51453.366488	59.259111
2354.818279	51278.678535	59.264116
2353.934146	51118.164523	59.269121
2353.541845	50933.871929	59.274125
2352.799068	50769.529070	59.279130
2351.884506	50592.986077	59.284135
2351.157177	50423.461290	59.289140
2350.621966	50261.083456	59.294145
2349.814168	50088.553020	59.299149
2349.003420	49923.640179	59.304154
2348.751941	49757.055066	59.309159
2348.060621	49586.368167	59.314164
2347.279972	49421.701945	59.319169
2346.813468	49245.031543	59.324173
2345.768941	49074.620674	59.329178
2345.372020	48912.445089	59.334183
2344.768337	48737.709168	59.339188
2344.076912	48573.498503	59.344193
2343.557807	48400.584221	59.349197
2342.342099	48238.459195	59.354202
2341.977543	48066.817547	59.359207
2341.898956	47896.960718	59.364212
2341.283740	47729.057079	59.369217
2340.640074	47538.974157	59.374221
2339.793760	47371.550268	59.379226
2338.948951	47202.482752	59.384231
2338.428279	47027.585959	59.389236
2337.416351	46857.491672	59.394241
2337.009736	46662.970848	59.399245
2336.055930	46509.671018	59.404250
2335.486234	46331.859679	59.409255
2334.760926	46163.830170	59.414260
2333.839475	46001.084260	59.419265
2333.727085	45832.868963	59.424269
2332.964816	45663.733486	59.429274
2332.289836	45489.784208	59.434279
2331.450674	45314.755616	59.439284
2330.543901	45145.505702	59.444289
2330.039405	44983.199674	59.449293
2329.148276	44824.160562	59.454298
2328.728463	44650.944561	59.459303
2328.362084	44483.399229	59.464308
2327.344583	44318.745268	59.469313
2326.794440	44144.647195	59.474317
2326.003010	43988.380009	59.479322
2325.573336	43817.571240	59.484327
2324.763530	43655.262686	59.489332
2324.138645	43487.091066	59.494337
2323.603127	43305.297781	59.499341
2322.680707	43147.923489	59.504346
2322.385042	42981.235270	59.509351
2321.483313	42818.888998	59.514356
2320.721963	42650.370752	59.519361
2320.057755	42487.205587	59.524365
2319.313445	42323.640370	59.529370
2318.811905	42145.639361	59.534375
2318.028696	41992.064267	59.539380
2317.305751	41821.884524	59.544385
2317.057093	41646.767457	59.549389
2315.994046	41493.525787	59.554394
2315.670412	41315.267921	59.559399
2314.873865	41158.084632	59.564404
2314.223483	40988.461316	59.569409
2313.825017	40814.378888	59.574413
2312.867215	40658.636092	59.579418
2312.381198	40491.056531	59.584423
2311.767841	40318.708130	59.589428
2311.083309	40151.270878	59.594433
2310.619977	39977.577171	59.599437
2309.824951	39806.846928	59.604442
2309.062829	39641.501267	59.609447
2308.576073	39468.164255	59.614452
2307.940795	39304.585096	59.619457
2307.350089	39128.709973	59.624461
2306.250044	38958.855503	59.629466
2305.644505	38787.267468	59.634471
2305.023461	38625.995968	59.639476
2304.138250	38458.286173	59.644481
2303.999868	38291.246857	59.649485
2303.246220	38120.027334	59.654490
2302.487058	37946.500771	59.659495
2301.839082	37777.109638	59.664500
2300.848222	37608.218791	59.669505
2300.393870	37439.816780	59.674509
2299.739140	37283.188803	59.679514
2298.964114	37111.140269	59.684519
2298.386997	36946.129695	59.689524
2297.674627	36770.163870	59.694529
2297.196358	36594.717580	59.699533
2296.617713	36438.312970	59.704538
2295.851453	36272.471151	59.709543
2295.287839	36102.716648	59.714548
2294.110815	35936.709338	59.719553
2293.532946	35764.091584	59.724557
2293.019776	35604.529327	59.729562
2292.542356	35439.125660	59.734567
2291.809627	35265.824712	59.739572
2290.943642	35106.794157	59.744577
2290.756576	34933.229898	59.749581
2290.080795	34760.890858	59.754586
2288.927397	34598.073106	59.759591
2288.523815	34434.407798	59.764596
2287.705490	34271.604872	59.769601
2287.332264	34101.487918	59.774605
2286.265262	33936.451778	59.779610
2285.570638	33768.857902	59.784615
2285.196580	33596.876518	59.789620
2283.864268	33442.283560	59.794625
2283.713373	33270.417121	59.799629
2283.044637	33113.823867	59.804634
2282.311874	32957.612053	59.809639
2282.013297	32787.373375	59.814644
2280.996481	32636.105637	59.819649
2280.397737	32462.594396	59.824653
2279.523588	32302.259600	59.829658
2278.939993	32134.672456	59.834663
2278.514592	31975.889452	59.839668
2277.572522	31826.873900	59.844673
2277.013633	31658.892573	59.849677
2276.519742	31496.594708	59.854682
2275.697282	31335.794888	59.859687
2275.297581	31168.839401	59.864692
2274.494468	31010.114512	59.869697
2273.999227	30840.469025	59.874701
2273.139845	30680.422551	59.879706
2272.684763	30513.940721	59.884711
2271.920609	30343.274817	59.889716
2271.066048	30185.360839	59.894721
2270.729691	30016.575599	59.899725
2269.926578	29856.017839	59.904730
2269.245475	29689.426931	59.909735
2268.699029	29533.401199	59.914740
2267.730139	29361.145763	59.919745
2267.306674	29192.597692	59.924750
2266.309600	29036.709789	59.929754
2265.771351	28862.640625	59.934759
2265.329669	28697.865674	59.939764
2264.475128	28538.741481	59.944769
2264.044972	28377.842009	59.949774
2263.288330	28214.079348	59.954778
2262.565440	28046.239941	59.959783
2261.735504	27886.257149	59.964788
2261.141843	27725.284195	59.969793
2261.026306	27562.029904	59.974798
2259.902458	27404.439842	59.979802
2259.209849	27241.572580	59.984807
2258.771932	27076.781814	59.989812
2257.681164	26921.802641	59.994817
2257.139562	26741.589075	59.999822
2256.488527	26581.633399	60.004826
2255.318404	26437.129585	60.009831
2254.992148	26276.335520	60.014836
2254.486181	26123.081612	60.019841
2253.825614	25958.770377	60.024846
2253.105500	25797.483539	60.029850
2252.237281	25645.419531	60.034855
2251.976856	25477.748166	60.039860
2250.887669	25326.116348	60.044865
2250.499629	25159.835724	60.049870
2249.713380	25008.447914	60.054874
2249.029017	24843.847730	60.059879
2248.518725	24688.406949	60.064884
2248.005021	24537.511079	60.069889
2247.257222	24368.041772	60.074894
2246.247061	24215.933228	60.079898
2245.655246	24062.328705	60.084903
2245.259049	23890.245088	60.089908
2244.298276	23747.393852	60.094913
2243.852122	23587.650996	60.099918
2243.230044	23423.460637	60.104922
2242.796883	23262.859730	60.109927
2241.929655	23113.803121	60.114932
2241.069226	22959.474709	60.119937
2240.646805	22794.532603	60.124942
2240.009792	22635.434453	60.129946
2239.209071	22480.364419	60.134951
2238.888665	22314.553492	60.139956
2237.856144	22155.658701	60.144961
2237.496795	21994.913549	60.149966
2236.795269	21842.006363	60.154970
2235.805947	21684.177836	60.159975
2235.354229	21521.631194	60.164980
2234.682394	21373.940170	60.169985
2234.141886	21199.775674	60.174990
2233.158609	21045.996205	60.179994
2232.492059	20889.689402	60.184999
2231.911407	20731.203061	60.190004
2231.182753	20578.677948	60.195009
2230.565771	20414.403352	60.200014
2230.311800	20251.475954	60.205018
2229.588371	20091.051056	60.210023
2228.672642	19937.853566	60.215028
2227.664632	19783.983715	60.220033
2227.464645	19626.461858	60.225038
2226.925184	19472.091998	60.230042
2226.223705	19314.823356	60.235047
2225.528103	19151.165753	60.240052
2224.664395	18998.854600	60.245057
2224.171748	18831.909800	60.250062
2223.199604	18681.460451	60.255066
2222.608154	18506.166901	60.260071
2221.884326	18367.120091	60.265076
2221.152552	18222.558134	60.270081
2220.637933	18047.532263	60.275086
2219.906688	17899.045615	60.280090
2219.007583	17748.372598	60.285095
2218.690530	17585.737044	60.290100
2217.912474	17426.032100	60.295105
2217.317768	17275.786248	60.300110
2216.505411	17132.943634	60.305114
2215.858226	16969.399048	60.310119
2215.305749	16817.278825	60.315124
2214.144177	16666.705263	60.320129
2214.080459	16513.494909	60.325134
2213.249409	16366.397228	60.330138
2212.176106	16216.326729	60.335143
2211.933161	16063.740481	60.340148
2211.139542	15912.633748	60.345153
2210.394798	15756.468496	60.350158
2210.071022	15605.318238	60.355162
2209.349493	15452.875100	60.360167
2208.931402	15299.759187	60.365172
2207.796048	15154.711174	60.370177
2207.353976	14994.038833	60.375182
2206.696765	14843.258326	60.380186
2206.205730	14692.184961	60.385191
2205.503422	14526.334421	60.390196
2204.702958	14385.666631	60.395201
2204.171808	14225.776197	60.400206
2203.168351	14082.888032	60.405210
2202.565454	13923.223644	60.410215
2201.989985	13780.956146	60.415220
2201.081178	13633.906473	60.420225
2200.383805	13476.304567	60.425230
2199.708160	13329.686561	60.430234
2199.345402	13193.128753	60.435239
2198.735049	13030.997458	60.440244
2197.588735	12887.025463	60.445249
2196.975743	12739.567785	60.450254
2196.270338	12595.427758	60.455258
2195.300091	12442.456375	60.460263
2195.236055	12294.780615	60.465268
2194.120539	12157.497362	60.470273
2193.660245	12011.980982	60.475278
2193.129199	11875.842958	60.480282
2192.278553	11732.327852	60.485287
2191.895284	11584.244825	60.490292
2190.845577	11452.019199	60.495297
2190.468085	11283.277206	60.500302
2189.914097	11147.435776	60.505306
2188.833291	11005.292510	60.510311
2188.355841	10870.755466	60.515316
2187.437316	10727.303018	60.520321
2187.055909	10580.816122	60.525326
2186.382293	10441.904004	60.530330
2185.486534	10295.958931	60.535335
2185.063295	10154.550782	60.540340
2184.308884	10018.309571	60.545345
2183.676672	9870.612557	60.550350
2182.666390	9748.360002	60.555354
2182.082671	9601.190131	60.560359
2181.777640	9465.044154	60.565364
2181.015137	9329.808149	60.570369
2180.211787	9186.872769	60.575374
2179.458776	9052.319449	60.580378
2179.039111	8916.817349	60.585383
2178.418566	8770.925778	60.590388
2177.290636	8630.743539	60.595393
2177.072060	8489.024993	60.600398
2175.898491	8358.447262	60.605402
2175.190194	8216.378601	60.610407
2175.007280	8088.978203	60.615412
2173.926278	7955.486329	60.620417
2173.008528	7811.655926	60.625422
2172.512208	7688.885680	60.630426
2171.966691	7564.794902	60.635431
2171.138711	7439.834032	60.640436
2170.078875	7324.482489	60.645441
2169.726635	7189.071247	60.650446
2168.715472	7067.702489	60.655450
2167.820824	6947.862462	60.660455
2167.482708	6816.142403	60.665460
2166.380780	6700.036738	60.670465
2166.035512	6583.549222	60.675470
2165.264652	6474.296229	60.680474
2164.674718	6356.741729	60.685479
2164.364703	6240.764841	60.690484
2163.093661	6130.162350	60.695489
2162.607825	5999.721677	60.700494
2162.024784	5891.179933	60.705498
2161.339344	5775.417689	60.710503
2160.951864	5665.862093	60.715508
2159.519283	5548.046161	60.720513
2159.258962	5429.520597	60.725518
2158.572543	5319.653706	60.730522
2157.728877	5213.583054	60.735527
2156.909642	5106.865625	60.740532
2156.269538	5002.073586	60.745537
2155.585171	4888.497506	60.750542
2154.764553	4794.552983	60.755546
2153.758194	4694.927006	60.760551
2153.257741	4582.933185	60.765556
2152.506334	4493.851025	60.770561
2152.138598	4398.934014	60.775566
2151.220629	4292.671929	60.780570
2150.934432	4197.711718	60.785575
2150.387926	4085.930090	60.790580
2149.211632	3992.460395	60.795585
2148.566634	3896.398029	60.800590
2147.858460	3804.541553	60.805594
2146.823582	3716.866455	60.810599
2146.013530	3618.282935	60.815604
2145.367641	3538.640207	60.820609
2145.087349	3452.933876	60.825614
2144.276532	3365.556570	60.830618
2144.092056	3273.837980	60.835623
2142.956013	3179.646179	60.840628
2142.092100	3101.904090	60.845633
2141.565951	3005.099129	60.850638
2141.145861	2924.367052	60.855642
2140.118947	2834.110648	60.860647
2139.733770	2746.245956	60.865652
2138.860633	2670.604688	60.870657
2138.341354	2580.962525	60.875662
2137.519959	2509.677544	60.880666
2136.666079	2417.415921	60.885671
2136.255792	2326.245378	60.890676
2135.087406	2256.089253	60.895681
2134.320768	2175.831892	60.900686
2133.604158	2112.548748	60.905690
2132.892845	2029.962447	60.910695
2132.316816	1962.409279	60.915700
2131.578449	1902.648569	60.920705
2130.869681	1829.385345	60.925710
2130.116775	1759.072615	60.930714
2129.318662	1686.437040	60.935719
2128.512836	1624.239525	60.940724
2127.820103	1573.714652	60.945729
2127.373284	1505.349749	60.950734
2126.817401	1448.049197	60.955738
2125.682799	1390.132544	60.960743
2124.939940	1319.057760	60.965748
2124.111391	1275.035356	60.970753
2123.466877	1219.174753	60.975758
2122.465216	1186.756581	60.980762
2122.197187	1130.813704	60.985767
2121.448761	1071.337149	60.990772
2120.597059	1029.836312	60.995777
2120.133787	978.917493	61.000782
2119.606960	937.806179	61.005786
2118.865237	875.715235	61.010791
2118.452001	831.721317	61.015796
2117.140373	787.682418	61.020801
2116.775836	746.997736	61.025806
2116.465079	694.394994	61.030810
2115.589940	645.207352	61.035815
2114.679866	590.050537	61.040820
2113.863786	561.071590	61.045825
2113.497626	503.430798	61.050830
2112.705339	462.227321	61.055834
2111.845061	411.869483	61.060839
2111.271512	373.288946	61.065844
2110.429807	336.790235	61.070849
2110.070550	300.667676	61.075854
2109.065910	266.644202	61.080858
2108.451727	223.219429	61.085863
2107.720508	194.188323	61.090868
2106.979641	147.820569	61.095873
2106.385317	113.175639	61.100878
2105.377812	86.666154	61.105882
2104.756579	62.095122	61.110887
2104.589780	32.058504	61.115892
2103.685973	-8.044082	61.120897
2102.903266	-41.744060	61.125902
2101.831606	-69.395894	61.130906
2101.155631	-79.931804	61.135911
2100.698115	-96.230171	61.140916
2099.456816	-102.448314	61.145921
2098.389002	-118.968364	61.150926
2095.804834	-70.668154	61.155930
2093.255672	-22.076855	61.160935
2093.028807	-9.958864	61.165940
2093.481043	12.155507	61.170945
2094.230541	9.978763	61.175950
2094.173024	15.531463	61.180954
2093.920259	9.241555	61.185959
2094.242768	6.090147	61.190964
2092.911241	-6.204271	61.195969
2092.137025	-12.577005	61.200974
2091.181697	-15.853642	61.205978
2090.399739	-14.242143	61.210983
2089.733320	-7.846878	61.215988
2088.475629	2.138538	61.220993
2088.069780	-4.030869	61.225998
2087.408644	6.279370	61.231002
2087.152613	2.450179	61.236007
2086.776204	2.432888	61.241012
2085.752311	10.361010	61.246017
2085.217653	-3.647956	61.251022
2084.750620	-0.436844	61.256026
2083.865107	8.376118	61.261031
2082.951465	6.556363	61.266036
2082.359490	13.617955	61.271041
2081.968041	14.478314	61.276046
2081.360525	11.884534	61.281050
2080.471729	18.182632	61.286055
2080.250981	7.277935	61.291060
2079.376667	12.947646	61.296065
2078.676483	11.680677	61.301070
2077.993302	19.116314	61.306074
2076.863690	14.388065	61.311079
2076.808839	20.922843	61.316084
2076.223439	23.070892	61.321089
2075.727842	15.720320	61.326094
2074.516001	22.203740	61.331098
2073.864291	24.590986	61.336103
2073.794111	19.893305	61.341108
2072.665207	28.550932	61.346113
2072.057768	16.501158	61.351118
2071.442426	12.042975	61.356122
2071.181097	19.416393	61.361127
2070.937928	21.828692	61.366132
2070.205912	28.128725	61.371137
2069.148186	19.828092	61.376142
2067.782142	35.743090	61.381146
2067.245477	27.381835	61.386151
2066.979427	22.497608	61.391156
2066.069651	31.896369	61.396161
2065.664242	25.778927	61.401166
2065.478642	20.546022	61.406170
2064.974976	24.851120	61.411175
2064.212835	17.948154	61.416180
2063.146072	29.043501	61.421185
2062.398144	21.296135	61.426190
2061.422096	19.008446	61.431194
2060.792527	26.776223	61.436199
2060.028824	22.273773	61.441204
2059.560938	34.415859	61.446209
2059.546411	29.354508	61.451214
2059.033298	26.703168	61.456218
2058.141624	37.565717	61.461223
2057.506362	19.524419	61.466228
2056.402648	30.925273	61.471233
2055.703983	30.027097	61.476238
2055.027908	31.243313	61.481242
2054.426900	28.981262	61.486247
2053.900201	31.279281	61.491252
2053.103492	35.495268	61.496257
2053.109385	38.334848	61.501262
2052.446029	37.837947	61.506266
2051.183886	34.376607	61.511271
2050.299090	26.745589	61.516276
2049.864806	31.872360	61.521281
2049.661071	29.089912	61.526286
2049.257455	27.217605	61.531290
2048.291939	37.293890	61.536295
2047.598693	27.617000	61.541300
2046.866639	39.160737	61.546305
2046.215041	34.045948	61.551310
2045.298567	41.884505	61.556314
2044.650141	35.105425	61.561319
2044.109744	23.759417	61.566324
2043.195868	30.186098	61.571329
2042.832525	36.851852	61.576334
2042.158076	36.320443	61.581338
2041.289445	39.984842	61.586343
2040.797397	33.699793	61.591348
2039.730779	41.073297	61.596353
2039.707045	36.811393	61.601358
2039.457616	39.393435	61.606362
2038.256035	40.803457	61.611367
2037.161516	36.609000	61.616372
2037.093800	38.856253	61.621377
2037.020349	35.384457	61.626382
2035.667040	38.089665	61.631386
2034.853546	40.325970	61.636391
2033.897440	39.418196	61.641396
2033.442112	40.799666	61.646401
2033.255275	30.613444	61.651406
2032.982020	36.739743	61.656410
2031.707920	39.121701	61.661415
2030.908197	29.294550	61.666420
2029.942420	42.454014	61.671425
2029.775573	30.799541	61.676430
2029.589211	33.680674	61.681434
2028.419680	34.882174	61.686439
2027.410369	31.975264	61.691444
2026.855801	32.177083	61.696449
2026.561710	39.199299	61.701454
2026.364090	37.849420	61.706458
2025.027655	37.058790	61.711463
2024.108404	33.645547	61.716468
2023.175786	34.208590	61.721473
2023.485610	34.388333	61.726478
2022.987029	35.589001	61.731482
2021.487880	44.007359	61.736487
2021.253923	30.081549	61.741492
2020.234892	37.592593	61.746497
2020.050136	36.806832	61.751502
2019.194624	33.317238	61.756506
2018.141460	38.704685	61.761511
2018.464298	37.311621	61.766516
2017.150879	42.465973	61.771521
2016.154506	36.983268	61.776526
2015.866214	41.515982	61.781530
2015.605593	43.579376	61.786535
2015.102199	32.697458	61.791540
2014.071338	44.419528	61.796545
2013.541083	42.303959	61.801550
2012.705681	36.585958	61.806554
2012.064188	32.046776	61.811559
2011.580909	28.909710	61.816564
2010.836122	38.096209	61.821569
2010.207178	37.103395	61.826574
2009.828056	33.979760	61.831578
2008.414546	42.480730	61.836583
2007.340903	38.932717	61.841588
2007.204923	43.802399	61.846593
2007.118114	31.160609	61.851598
2006.134830	32.252126	61.856602
2004.930925	43.233642	61.861607
2004.562254	25.549037	61.866612
2004.425379	37.416222	61.871617
2003.648727	39.201960	61.876622
2002.719641	36.488918	61.881626
2001.819851	36.991561	61.886631
2001.357064	32.291543	61.891636
2000.596309	36.315745	61.896641
2000.192882	28.726615	61.901646
1999.427540	34.700776	61.906650
1998.802319	30.020235	61.911655
1998.405149	31.118072	61.916660
1997.771726	35.112599	61.921665
1997.299224	31.374548	61.926670
1996.739304	32.968179	61.931674
1995.461943	35.757550	61.936679
1994.498844	27.675332	61.941684
1993.754304	36.617351	61.946689
1993.857261	33.907658	61.951694
1992.842985	30.116826	61.956698
1991.932206	34.838243	61.961703
1991.693682	39.178543	61.966708
1990.732896	36.396417	61.971713
1990.265549	36.152288	61.976718
1989.979608	22.796173	61.981722
1989.312260	30.658275	61.986727
1988.680823	26.694705	61.991732
1988.233407	30.702287	61.996737
1986.822309	31.478499	62.001742
1986.029759	31.820612	62.006746
1985.123797	39.324757	62.011751
1985.105553	30.518510	62.016756
1984.090672	35.876235	62.021761
1983.685895	37.289114	62.026766
1982.959192	34.316859	62.031770
1982.489941	40.125746	62.036775
1981.907193	25.676540	62.041780
1981.409905	40.158909	62.046785
1981.048730	35.004345	62.051790
1980.520963	28.674518	62.056794
1978.763998	38.296104	62.061799
1978.353801	32.917498	62.066804
1977.216312	31.895027	62.071809
1976.594843	31.065048	62.076814
1976.464326	37.717502	62.081818
1975.514489	33.523763	62.086823
1975.123306	33.786395	62.091828
1974.561483	45.905557	62.096833
1974.237762	30.360185	62.101838
1973.835188	36.615830	62.106842
1972.744450	38.692724	62.111847
1972.002430	27.703616	62.116852
1970.817392	39.946938	62.121857
1970.127985	36.284327	62.126862
1969.317988	33.145516	62.131866
1968.939495	31.109953	62.136871
1968.514421	28.903577	62.141876
1968.008714	36.177020	62.146881
1967.596645	36.184332	62.151886
1967.202083	28.448715	62.156890
1966.417842	36.397193	62.161895
1965.349904	34.064199	62.166900
1963.891174	38.475195	62.171905
1963.765603	34.521216	62.176910
1963.129169	31.410052	62.181914
1962.703298	31.689231	62.186919
1962.274921	32.639053	62.191924
1961.485427	39.820346	62.196929
1961.097730	27.344611	62.201934
1960.418148	32.029334	62.206938
1959.213187	38.287773	62.211943
1958.553540	27.179932	62.216948
1957.789087	37.143891	62.221953
1957.273045	35.715250	62.226958
1956.462168	33.391916	62.231962
1955.713944	28.800306	62.236967
1955.903218	33.621505	62.241972
1955.091093	36.330729	62.246977
1954.418754	39.473530	62.251982
1953.215757	31.563462	62.256986
1952.343256	33.749230	62.261991
1951.809401	31.793530	62.266996
1951.075129	23.626118	62.272001
1950.794718	29.556422	62.277006
1950.360390	34.566511	62.282010
1949.632142	32.307337	62.287015
1949.123673	33.847076	62.292020
1948.523087	30.351733	62.297025
1947.738255	30.582239	62.302030
1946.653261	38.647858	62.307034
1945.609024	48.197323	62.312039
1945.499626	36.666214	62.317044
1944.964381	34.977256	62.322049
1944.136242	37.627522	62.327054
1943.971892	34.239554	62.332058
1942.827567	38.971253	62.337063
1941.960213	42.215984	62.342068
1940.831533	36.413675	62.347073
1940.665889	38.747442	62.352078
1940.379511	31.839952	62.357082
1939.292189	37.254927	62.362087
1939.095003	34.801053	62.367092
1938.446885	35.784188	62.372097
1938.048853	44.070355	62.377102
1937.310882	40.360266	62.382106
1936.177751	42.607919	62.387111
1935.474378	35.315594	62.392116
1934.549041	43.854221	62.397121
1934.228583	30.388469	62.402126
1933.898528	46.487579	62.407130
1933.052934	41.253801	62.412135
1933.081601	25.854363	62.417140
1931.697192	41.453765	62.422145
1930.865845	39.064299	62.427150
1930.057991	39.266924	62.432154
1929.327741	39.569199	62.437159
1929.046814	35.076882	62.442164
1928.264515	42.268081	62.447169
1927.826370	35.635437	62.452174
1927.574812	34.220009	62.457178
1926.185045	41.741053	62.462183
1925.583570	35.981215	62.467188
1924.917821	37.481270	62.472193
1924.617100	33.575604	62.477198
1923.892816	43.656206	62.482202
1923.360742	38.535093	62.487207
1922.663327	39.835160	62.492212
1921.524024	43.468447	62.497217
1920.854352	38.421223	62.502222
1920.157498	36.385745	62.507226
1919.614402	44.229716	62.512231
1919.478294	34.395026	62.517236
1918.479445	38.054902	62.522241
1918.156348	36.152486	62.527246
1917.020843	39.718934	62.532250
1915.987212	42.278824	62.537255
1915.518659	45.476018	62.542260
1914.856064	41.014333	62.547265
1914.622135	35.453204	62.552270
1913.994797	39.536674	62.557274
1913.157725	33.457834	62.562279
1913.016210	36.205687	62.567284
1912.030903	32.556956	62.572289
1911.031874	47.831820	62.577294
1910.567066	31.610233	62.582298
1909.821058	36.534186	62.587303
1909.188472	35.458392	62.592308
1908.664922	35.652157	62.597313
1908.323637	40.063973	62.602318
1907.356034	29.664249	62.607322
1906.238606	41.013712	62.612327
1905.863390	36.765041	62.617332
1905.231214	45.107311	62.622337
1904.721391	27.027230	62.627342
1904.315256	39.593211	62.632346
1903.453713	45.016511	62.637351
1902.183646	28.597910	62.642356
1901.292845	39.570750	62.647361
1901.037910	38.334067	62.652366
1900.356887	38.738928	62.657370
1899.758329	43.741983	62.662375
1899.898790	40.433363	62.667380
1899.024981	43.202863	62.672385
1898.559049	34.376235	62.677390
1897.556889	42.643199	62.682394
1896.468467	47.703531	62.687399
1896.192646	38.075540	62.692404
1895.548588	49.464978	62.697409
1894.850462	38.276525	62.702414
1893.960533	34.853945	62.707418
1892.904055	39.738883	62.712423
1892.139303	41.284629	62.717428
1891.855658	39.144126	62.722433
1891.498637	39.921771	62.727438
1891.210182	36.310648	62.732442
1890.470241	35.945805	62.737447
1889.944561	38.842970	62.742452
1888.646369	45.193518	62.747457
1887.828363	47.365923	62.752462
1887.204815	33.366375	62.757466
1886.512054	43.519254	62.762471
1886.688038	38.306229	62.767476
1886.113965	38.832892	62.772481
1885.138622	37.256406	62.777486
1884.124940	35.588231	62.782490
1883.494670	34.300752	62.787495
1883.190411	26.501929	62.792500
1882.255292	37.220018	62.797505
1881.090316	45.814057	62.802510
1880.886397	31.782579	62.807514
1880.101581	42.549352	62.812519
1879.712227	24.784490	62.817524
1879.198700	43.741945	62.822529
1878.538704	36.218812	62.827534
1877.246772	32.610896	62.832538
1876.175966	41.242023	62.837543
1875.878691	32.270344	62.842548
1875.032237	43.866970	62.847553
1874.718091	30.425465	62.852558
1874.424930	34.621471	62.857562
1873.774998	36.909126	62.862567
1873.546007	33.353223	62.867572
1872.658987	35.732144	62.872577
1871.812876	29.943355	62.877582
1871.156097	34.490428	62.882586
1870.327795	35.517959	62.887591
1870.296762	29.850501	62.892596
1868.625281	43.338111	62.897601
1867.833135	36.529865	62.902606
1867.517940	37.215712	62.907610
1866.942610	40.387286	62.912615
1866.660973	42.786786	62.917620
1866.230092	37.946105	62.922625
1865.345582	40.968065	62.927630
1864.663230	34.880446	62.932634
1863.892997	49.959710	62.937639
1863.181238	33.381512	62.942644
1861.965773	50.510667	62.947649
1860.828894	38.674337	62.952654
1861.015892	36.121619	62.957658
1860.069414	50.500274	62.962663
1859.986700	38.682649	62.967668
1859.345589	40.841167	62.972673
1858.944495	42.827524	62.977678
1858.180348	33.717081	62.982682
1856.630551	41.966929	62.987687
1856.471298	32.886600	62.992692
1855.690109	39.606100	62.997697
1855.229623	40.882755	63.002702
1854.936897	28.838274	63.007706
1853.733992	52.688385	63.012711
1853.132119	37.352800	63.017716
1852.240314	37.784835	63.022721
1851.703941	34.571074	63.027726
1851.183096	35.985055	63.032730
1850.340298	43.507595	63.037735
1850.094141	36.614234	63.042740
1849.051082	34.783572	63.047745
1848.513460	44.739924	63.052750
1847.961670	34.879784	63.057754
1847.260490	37.424756	63.062759
1846.975156	31.094317	63.067764
1845.924533	38.255595	63.072769
1845.135455	31.366444	63.077774
1844.637357	33.380822	63.082778
1843.819919	31.938560	63.087783
1843.484363	27.898084	63.092788
1842.515696	35.405914	63.097793
1841.562329	34.754835	63.102798
1840.999270	25.744943	63.107802
1840.094354	36.772078	63.112807
1840.048864	22.370089	63.117812
1839.434413	34.936027	63.122817
1839.007181	34.072085	63.127822
1838.580348	33.856244	63.132826
1837.295591	28.673320	63.137831
1836.446481	20.860099	63.142836
1836.226388	28.307408	63.147841
1835.623707	26.816853	63.152846
1834.770364	30.436302	63.157850
1833.337902	40.178338	63.162855
1833.220157	27.044725	63.167860
1832.407409	34.231314	63.172865
1831.852413	29.320461	63.177870
1831.342426	31.904465	63.182874
1831.287811	38.838194	63.187879
1830.538989	37.378732	63.192884
1829.472224	27.269200	63.197889
1828.823806	21.311835	63.202894
1828.162412	30.642824	63.207898
1827.180702	30.545064	63.212903
1826.424082	27.172309	63.217908
1825.525633	32.915319	63.222913
1825.003536	34.490362	63.227918
1825.113039	29.820938	63.232922
1824.260746	36.319909	63.237927
1823.966135	30.355246	63.242932
1822.982809	37.753440	63.247937
1821.824663	32.960449	63.252942
1821.480487	35.177483	63.257946
1821.030124	38.168362	63.262951
1820.454803	26.591415	63.267956
1819.532053	34.185005	63.272961
1818.552571	30.800333	63.277966
1818.287036	33.962144	63.282970
1817.470378	44.696137	63.287975
1817.211433	29.118448	63.292980
1816.500281	37.615203	63.297985
1815.386386	28.397885	63.302990
1814.685447	30.188998	63.307994
1813.553580	39.465390	63.312999
1813.551562	24.256938	63.318004
1813.161121	34.685105	63.323009
1812.490307	30.876080	63.328014
1811.528388	32.222910	63.333018
1810.472125	38.309551	63.338023
1810.234254	35.851112	63.343028
1809.563349	39.080455	63.348033
1809.443534	32.867248	63.353038
1808.676363	33.736848	63.358042
1807.481009	37.338076	63.363047
1807.064928	31.602452	63.368052
1806.197524	31.764107	63.373057
1805.614189	38.050051	63.378062
1805.376668	35.074286	63.383066
1804.168440	41.334883	63.388071
1803.411003	41.258288	63.393076
1802.975429	38.810745	63.398081
1802.617107	30.008060	63.403086
1802.149434	31.798404	63.408090
1800.439312	43.096938	63.413095
1800.237953	30.995378	63.418100
1799.397580	33.412647	63.423105
1799.048372	32.703487	63.428110
1798.768185	27.476173	63.433114
1797.575717	28.701917	63.438119
1796.821299	21.600691	63.443124
1796.070638	38.204999	63.448129
1795.583448	36.454824	63.453134
1795.148120	27.416775	63.458138
1794.549770	29.628443	63.463143
1794.432407	23.470048	63.468148
1792.939664	27.593200	63.473153
1792.553115	30.957169	63.478158
1791.860619	30.753563	63.483162
1791.393945	31.706340	63.488167
1790.525513	26.063063	63.493172
1789.316792	26.379860	63.498177
1788.897445	29.425744	63.503182
1788.782807	31.027551	63.508186
1787.822474	31.459452	63.513191
1787.466356	28.130343	63.518196
1786.220344	28.084036	63.523201
1785.742375	25.542300	63.528206
1785.072821	26.270240	63.533210
1784.681670	29.133440	63.538215
1784.288802	22.719164	63.543220
1783.117780	32.900695	63.548225
1782.370873	30.792779	63.553230
1781.992771	20.774190	63.558234
1781.054900	33.511353	63.563239
1780.823545	27.508265	63.568244
1779.767040	33.047718	63.573249
1778.624212	27.452756	63.578254
1778.275558	23.477454	63.583258
1777.764687	31.436173	63.588263
1777.424710	28.699048	63.593268
1776.783489	32.201242	63.598273
1776.221376	30.268994	63.603278
1775.425091	23.620729	63.608282
1774.313689	37.990888	63.613287
1773.771629	32.576495	63.618292
1773.489694	36.324421	63.623297
1772.847563	29.974965	63.628302
1771.677627	31.148254	63.633306
1771.061314	34.461979	63.638311
1770.723581	28.349624	63.643316
1770.021156	26.466473	63.648321
1769.329249	25.532609	63.653326
1769.049721	25.022134	63.658330
1768.031656	36.846315	63.663335
1767.665179	28.029163	63.668340
1767.012920	28.937298	63.673345
1765.774369	27.855275	63.678350
1764.958069	19.107995	63.683354
1764.028404	38.959482	63.688359
1763.905276	23.445402	63.693364
1763.367613	27.683400	63.698369
1762.902983	20.676519	63.703374
1763.004000	25.670990	63.708378
1761.716219	36.085553	63.713383
1761.222005	21.393704	63.718388
1760.308439	35.019619	63.723393
1759.086649	22.383092	63.728398
1758.459788	21.128223	63.733402
1757.775960	29.294195	63.738407
1757.433800	26.185239	63.743412
1756.749296	25.379520	63.748417
1756.197934	31.658813	63.753422
1755.982074	26.621574	63.758426
1754.728928	27.789161	63.763431
1754.325591	19.857863	63.768436
1753.423898	31.187293	63.773441
1752.855267	29.891635	63.778446
1751.893062	28.519708	63.783450
1750.964944	31.772568	63.788455
1750.635357	30.268622	63.793460
1750.040137	34.892679	63.798465
1749.603458	26.861012	63.803470
1749.437780	23.949544	63.808474
1748.490824	29.512610	63.813479
1747.709827	23.063788	63.818484
1747.136513	27.646516	63.823489
1746.256360	28.912569	63.828494
1745.184035	22.543138	63.833498
1744.246175	29.995635	63.838503
1744.006890	23.594823	63.843508
1743.571908	20.522691	63.848513
1742.849989	30.246527	63.853518
1742.781488	24.510910	63.858522
1741.907815	26.625962	63.863527
1741.002531	24.760846	63.868532
1740.473138	25.348257	63.873537
1739.626384	28.580311	63.878542
1739.346081	26.830406	63.883546
1738.186922	32.709472	63.888551
1737.432524	26.049835	63.893556
1737.125454	25.480656	63.898561
1736.614615	27.356719	63.903566
1735.439141	22.359934	63.908570
1734.498423	29.237267	63.913575
1734.279640	26.802617	63.918580
1733.452022	23.598875	63.923585
1733.073681	17.264311	63.928590
1732.901996	26.608997	63.933594
1731.767701	24.896961	63.938599
1731.160857	21.621882	63.943604
1730.419276	20.599719	63.948609
1729.858814	22.690257	63.953614
1729.226957	16.697177	63.958618
1727.845337	25.355632	63.963623
1727.740574	15.818799	63.968628
1727.288688	20.304965	63.973633
1726.313014	20.846564	63.978638
1726.136683	15.364636	63.983642
1725.073222	26.418549	63.988647
1724.427362	16.046671	63.993652
1723.462304	20.532343	63.998657
1723.216594	21.420069	64.003662
1722.691408	29.481997	64.008666
1721.588468	30.387608	64.013671
1721.003023	18.504788	64.018676
1720.247731	28.334858	64.023681
1719.955923	16.574142	64.028686
1719.625053	15.245458	64.033690
1718.596687	26.323762	64.038695
1717.853726	20.614852	64.043700
1716.863833	25.919804	64.048705
1716.402856	24.857805	64.053710
1716.316396	19.478302	64.058714
1715.033206	21.060711	64.063719
1714.488562	20.524541	64.068724
1713.679613	22.955767	64.073729
1713.574222	25.637958	64.078734
1712.749789	22.786976	64.083738
1711.288648	27.796180	64.088743
1711.051420	23.363195	64.093748
1710.411762	23.688990	64.098753
1710.052519	27.259953	64.103758
1709.736329	21.223044	64.108762
1708.678384	31.601115	64.113767
1707.963252	26.302549	64.118772
1707.325590	26.124951	64.123777
1706.922662	27.775708	64.128782
1705.745381	30.255983	64.133786
1704.704320	27.593963	64.138791
1704.207690	24.364465	64.143796
1703.697241	27.699236	64.148801
1703.680101	27.293753	64.153806
1703.521225	20.407063	64.158810
1702.002300	31.240006	64.163815
1701.688711	26.289265	64.168820
1700.845092	30.738310	64.173825
1700.051772	25.226649	64.178830
1698.972965	29.823446	64.183834
1697.803085	33.062684	64.188839
1697.572543	31.656560	64.193844
1697.341335	30.010832	64.198849
1696.916354	26.370961	64.203854
1696.639261	23.008815	64.208858
1695.703652	30.024128	64.213863
1694.971787	29.553974	64.218868
1694.095715	33.864665	64.223873
1693.359778	28.954206	64.228878
1692.731642	23.813724	64.233882
1691.635127	32.201392	64.238887
1691.468011	21.572113	64.243892
1690.760808	27.510296	64.248897
1690.301142	31.461511	64.253902
1689.740441	32.274691	64.258906
1688.683860	32.680914	64.263911
1687.949691	33.256707	64.268916
1687.394427	33.343585	64.273921
1686.979272	37.357121	64.278926
1686.159704	25.489420	64.283930
1685.088671	29.086720	64.288935
1684.801590	26.519414	64.293940
1683.913995	30.887135	64.298945
1683.732692	31.769364	64.303950
1683.415479	29.246270	64.308954
1682.339331	30.000976	64.313959
1681.389796	25.761578	64.318964
1680.956000	21.802974	64.323969
1680.399561	19.962894	64.328974
1679.132083	23.840574	64.333978
1678.268672	29.732608	64.338983
1678.189090	28.964863	64.343988
1677.927971	24.573527	64.348993
1677.346730	28.462050	64.353998
1676.231151	18.423441	64.359002
1675.256940	29.764408	64.364007
1675.197562	24.005270	64.369012
1674.272113	32.704833	64.374017
1673.824809	24.878313	64.379022
1672.849222	18.334270	64.384026
1671.673960	28.797223	64.389031
1671.449342	22.228504	64.394036
1670.853537	23.854709	64.399041
1670.402944	26.650090	64.404046
1670.264065	25.136362	64.409050
1668.975320	25.756103	64.414055
1668.389244	19.530252	64.419060
1667.843107	32.145280	64.424065
1666.835720	27.609132	64.429070
1666.094341	13.659950	64.434074
1665.004193	31.448933	64.439079
1664.828229	26.153042	64.444084
1664.329640	37.344338	64.449089
1664.164871	25.084026	64.454094
1663.476973	30.713203	64.459098
1662.138573	29.812682	64.464103
1661.786270	29.922518	64.469108
1661.220459	29.897529	64.474113
1660.395474	27.087655	64.479118
1659.731230	26.269282	64.484122
1659.010504	36.062336	64.489127
1658.682476	21.894510	64.494132
1657.932194	30.870617	64.499137
1656.942106	27.093437	64.504142
1656.468174	27.206826	64.509146
1655.981237	33.906432	64.514151
1655.532339	27.956848	64.519156
1654.377075	22.701413	64.524161
1653.390592	30.366676	64.529166
1653.205463	25.234678	64.534170
1652.286360	24.530916	64.539175
1652.232005	26.794969	64.544180
1650.993846	29.729665	64.549185
1650.340097	30.567098	64.554190
1649.923447	25.760480	64.559194
1649.171892	31.735683	64.564199
1648.799281	22.056896	64.569204
1647.856340	26.278869	64.574209
1646.643091	24.636189	64.579214
1646.386198	30.171663	64.584218
1645.946734	25.591034	64.589223
1645.464789	17.284299	64.594228
1644.386200	20.915930	64.599233
1643.328111	22.235518	64.604238
1643.110505	20.727992	64.609242
1642.303648	34.959909	64.614247
1642.394899	28.383589	64.619252
1641.606379	32.954791	64.624257
1640.527534	30.771914	64.629262
1640.078171	25.599891	64.634266
1639.010378	25.427564	64.639271
1639.060041	27.514233	64.644276
1637.965119	33.476178	64.649281
1636.746785	30.295117	64.654286
1636.802057	27.629269	64.659290
1636.076145	32.335614	64.664295
1635.678167	20.539741	64.669300
1634.571388	32.012174	64.674305
1633.522969	23.785975	64.679310
1633.334303	23.428246	64.684314
1632.497218	25.450781	64.689319
1632.502449	19.272930	64.694324
1631.272424	25.753106	64.699329
1630.460288	26.221447	64.704334
1630.138432	20.917200	64.709338
1629.687488	25.061012	64.714343
1628.857878	20.786814	64.719348
1627.719629	24.429508	64.724353
1626.855488	29.392794	64.729358
1626.531604	13.431231	64.734362
1626.215998	26.154718	64.739367
1625.804641	19.680334	64.744372
1624.646733	25.663327	64.749377
1624.151280	23.565976	64.754382
1623.856806	20.518856	64.759386
1622.521032	24.315944	64.764391
1621.477077	21.326396	64.769396
1620.878376	22.032081	64.774401
1620.338129	24.116274	64.779406
1620.356634	23.433878	64.784410
1619.703040	21.125097	64.789415
1619.410240	22.425613	64.794420
1617.968552	32.487768	64.799425
1617.561374	29.087950	64.804430
1617.003314	26.325573	64.809434
1616.371942	30.966436	64.814439
1615.303890	27.081805	64.819444
1614.565852	34.083099	64.824449
1614.071374	26.189968	64.829454
1613.962764	21.367535	64.834458
1612.829781	31.573043	64.839463
1612.248697	25.627126	64.844468
1611.353435	30.417156	64.849473
1610.954571	25.689727	64.854478
1610.415778	23.753814	64.859482
1609.374564	26.113158	64.864487
1608.836743	22.087513	64.869492
1608.051637	28.632635	64.874497
1607.373315	27.650923	64.879502
1607.272446	27.969990	64.884506
1606.117860	26.021526	64.889511
1605.606425	26.377439	64.894516
1604.842183	28.191279	64.899521
1604.538451	32.362172	64.904526
1603.942305	19.310929	64.909530
1602.912240	31.077127	64.914535
1602.243399	23.885101	64.919540
1601.626823	31.811746	64.924545
1601.056890	28.398364	64.929550
1599.908932	18.355479	64.934554
1599.161373	31.783150	64.939559
1598.996955	25.354694	64.944564
1598.375860	30.154786	64.949569
1597.816423	23.973609	64.954574
1597.402924	15.249137	64.959578
1596.271078	20.180844	64.964583
1595.767147	22.334969	64.969588
1595.176522	23.455714	64.974593
1594.570114	29.135038	64.979598
1593.632884	23.365570	64.984602
1593.038088	35.814864	64.989607
1592.700276	24.840540	64.994612
1591.333880	29.883640	64.999617
1590.378733	28.188938	65.004622
1590.030153	24.171077	65.009626
1589.205343	26.084437	65.014631
1589.005715	28.685404	65.019636
1588.378584	23.962708	65.024641
1588.220051	33.615980	65.029646
1587.879441	29.394991	65.034650
1586.547899	31.030879	65.039655
1586.207266	19.982888	65.044660
1584.927641	30.400949	65.049665
1584.070587	25.637513	65.054670
1583.725815	20.869956	65.059674
1582.796310	20.361848	65.064679
1582.449073	26.203430	65.069684
1582.286510	25.735896	65.074689
1581.134914	25.179495	65.079694
1580.726543	20.622327	65.084698
1579.891338	32.122592	65.089703
1579.310917	29.120913	65.094708
1578.318580	23.950020	65.099713
1577.319143	33.295336	65.104718
1577.189278	21.382755	65.109722
1576.367099	17.547391	65.114727
1576.112818	23.683302	65.119732
1575.731320	28.385399	65.124737
1574.459004	25.372229	65.129742
1574.073879	21.838022	65.134746
1573.159094	37.834462	65.139751
1572.973332	19.460167	65.144756
1571.743095	25.156612	65.149761
1571.021219	30.483683	65.154766
1570.731516	26.617328	65.159770
1570.011186	29.610135	65.164775
1569.169428	20.537379	65.169780
1568.336462	30.619531	65.174785
1567.602989	26.071443	65.179790
1567.218050	27.903874	65.184794
1566.720218	30.960680	65.189799
1566.231704	24.895982	65.194804
1565.291841	22.773062	65.199809
1564.407300	23.621955	65.204814
1564.283491	26.903196	65.209818
1563.524550	30.381560	65.214823
1562.335774	20.204824	65.219828
1561.566476	34.397667	65.224833
1561.413986	35.560770	65.229838
1560.810812	29.686188	65.234842
1560.406230	31.964891	65.239847
1559.534449	26.013139	65.244852
1559.003709	27.151186	65.249857
1558.000966	24.226084	65.254862
1557.272412	24.791559	65.259866
1556.288678	26.171909	65.264871
1555.888686	21.514062	65.269876
1555.535248	29.980827	65.274881
1555.154758	32.612113	65.279886
1554.509285	22.192920	65.284890
1553.095086	30.290474	65.289895
1552.754549	28.584859	65.294900
1552.305223	21.277540	65.299905
1551.425784	29.499865	65.304910
1550.480891	23.906684	65.309914
1549.584035	32.316292	65.314919
1549.433890	28.697437	65.319924
1548.968712	21.701737	65.324929
1548.740335	27.366731	65.329934
1547.781152	24.100379	65.334938
1546.896782	30.470467	65.339943
1546.308516	24.576176	65.344948
1544.989562	28.320163	65.349953
1544.227364	28.772710	65.354958
1543.618312	26.920521	65.359962
1543.290529	25.275963	65.364967
1542.941172	25.107788	65.369972
1542.643870	32.841774	65.374977
1541.804951	28.450806	65.379982
1540.906648	27.272245	65.384986
1540.049675	30.900242	65.389991
1539.806598	26.400397	65.394996
1539.079815	22.549886	65.400001
1538.071271	23.629817	65.405006
1537.572831	20.894258	65.410010
1536.711319	27.060432	65.415015
1536.551682	23.487245	65.420020
1535.452621	22.539296	65.425025
1534.231873	25.576938	65.430030
1534.226894	22.386051	65.435034
1533.405610	28.802891	65.440039
1533.287397	27.389973	65.445044
1532.858806	24.340524	65.450049
1531.921304	32.702977	65.455054
1531.460361	21.249894	65.460058
1530.219772	27.561470	65.465063
1529.419972	26.430341	65.470068
1528.679058	27.841504	65.475073
1528.230713	30.398416	65.480078
1527.562653	29.419826	65.485082
1526.782234	29.529902	65.490087
1526.763605	23.302229	65.495092
1525.608494	28.119384	65.500097
1524.667467	26.914500	65.505102
1524.546379	21.130488	65.510106
1523.977825	28.574823	65.515111
1523.071931	14.725968	65.520116
1522.100564	25.809461	65.525121
1521.681696	32.420990	65.530126
1521.498813	19.778792	65.535130
1520.376351	33.239244	65.540135
1519.377065	27.356658	65.545140
1518.998109	34.674667	65.550145
1518.583877	33.028079	65.555150
1518.387413	21.619707	65.560154
1517.283986	25.001431	65.565159
1516.595775	20.302658	65.570164
1515.625025	23.652259	65.575169
1514.709118	30.670800	65.580174
1513.822904	20.796111	65.585178
1513.315433	27.502148	65.590183
1512.984604	22.464290	65.595188
1512.668583	29.942616	65.600193
1512.083212	25.492442	65.605198
1511.703988	21.386421	65.610202
1510.601694	26.248807	65.615207
1509.895847	30.846330	65.620212
1509.526782	27.583987	65.625217
1508.417712	32.127313	65.630222
1508.098615	16.821070	65.635226
1507.276399	24.252098	65.640231
1506.493025	24.638632	65.645236
1505.239997	22.663280	65.650241
1504.447878	30.699842	65.655246
1504.272598	17.182762	65.660250
1503.947059	24.757220	65.665255
1503.557755	24.723139	65.670260
1503.429119	26.035426	65.675265
1502.139694	27.447031	65.680270
1501.453369	19.377832	65.685274
1500.526777	16.511620	65.690279
1499.732697	18.822266	65.695284
1498.764556	15.893269	65.700289
1498.105459	19.641223	65.705294
1497.978783	24.854791	65.710298
1497.342449	28.441427	65.715303
1497.143523	10.200150	65.720308
1496.042862	25.863413	65.725313
1494.972512	18.702118	65.730318
1494.713242	25.748777	65.735322
1494.187880	29.085951	65.740327
1493.028465	17.106767	65.745332
1492.090917	25.306798	65.750337
1491.720593	18.406433	65.755342
1491.194873	14.189652	65.760346
1490.610045	24.650295	65.765351
1490.680041	18.317073	65.770356
1489.629677	17.752510	65.775361
1488.372026	18.635495	65.780366
1488.179821	12.074274	65.785370
1487.613892	27.614707	65.790375
1487.026522	15.740165	65.795380
1486.108818	29.500836	65.800385
1485.410295	25.054460	65.805390
1485.176745	19.365602	65.810394
1483.992905	23.288426	65.815399
1483.124537	14.743516	65.820404
1482.528483	13.557943	65.825409
1482.272362	24.603468	65.830414
1481.631562	27.572616	65.835418
1480.354832	23.774833	65.840423
1479.434251	20.119154	65.845428
1479.120525	17.989799	65.850433
1478.614629	22.495620	65.855438
1478.640269	10.977843	65.860442
1477.441242	26.139477	65.865447
1476.529811	13.015388	65.870452
1476.068884	18.660567	65.875457
1475.291597	18.192965	65.880462
1475.123535	23.122935	65.885466
1474.463099	17.831527	65.890471
1473.601928	22.803845	65.895476
1472.999450	28.291743	65.900481
1472.515553	31.319540	65.905486
1471.818235	19.531864	65.910490
1470.301341	17.863411	65.915495
1469.865353	25.684096	65.920500
1469.359968	27.590880	65.925505
1469.132531	25.783719	65.930510
1468.481690	16.601813	65.935514
1467.097559	23.470843	65.940519
1466.815808	18.483546	65.945524
1466.414790	17.634427	65.950529
1465.642164	29.526911	65.955534
1465.248190	20.504461	65.960538
1464.008576	30.570838	65.965543
1463.800645	29.169030	65.970548
1463.280900	25.413376	65.975553
1462.365082	30.929000	65.980558
1461.437014	20.699846	65.985562
1460.623969	24.620520	65.990567
1460.627177	20.884256	65.995572
1459.705425	23.563732	66.000577
1458.840937	27.456311	66.005582
1458.685324	22.286530	66.010586
1458.148491	30.102745	66.015591
1457.031112	19.137243	66.020596
1455.988321	24.316638	66.025601
1455.320948	25.302948	66.030606
1455.209515	19.955826	66.035610
1454.330804	27.971467	66.040615
1453.504992	17.607788	66.045620
1453.086978	21.353705	66.050625
1452.430620	25.634274	66.055630
1452.047962	19.486547	66.060634
1450.819632	26.975831	66.065639
1450.232311	14.634492	66.070644
1449.550305	20.988209	66.075649
1448.900902	23.488774	66.080654
1448.955668	21.488520	66.085658
1447.562528	21.705472	66.090663
1446.959458	30.126759	66.095668
1446.249607	21.924115	66.100673
1445.807162	24.041684	66.105678
1445.560111	23.311606	66.110682
1444.371404	27.618442	66.115687
1443.518671	29.435353	66.120692
1443.206589	23.689593	66.125697
1442.770390	25.714701	66.130702
1442.105515	20.513899	66.135706
1441.255080	29.474426	66.140711
1440.731250	15.815633	66.145716
1439.686298	18.210329	66.150721
1438.528904	20.684402	66.155726
1438.313384	10.252116	66.160730
1437.897791	19.755410	66.165735
1437.216616	24.314331	66.170740
1436.968218	25.648810	66.175745
1436.205410	25.398127	66.180750
1435.594906	17.085076	66.185754
1434.464890	19.297743	66.190759
1433.563162	22.456617	66.195764
1432.684583	16.748864	66.200769
1432.023421	22.211401	66.205774
1431.747195	17.693188	66.210778
1431.126050	22.412888	66.215783
1431.084421	22.362980	66.220788
1430.315883	20.238112	66.225793
1429.083285	20.752848	66.230798
1428.810957	15.325644	66.235802
1428.158084	16.366429	66.240807
1427.138027	14.238962	66.245812
1426.391362	14.559757	66.250817
1425.615748	13.215073	66.255822
1425.372064	10.555748	66.260826
1424.620245	16.829097	66.265831
1424.358299	8.159436	66.270836
1423.195556	17.678986	66.275841
1422.559687	19.190180	66.280846
1422.321454	11.399890	66.285850
1421.500953	19.467786	66.290855
1420.433202	11.087069	66.295860
1419.956951	17.143143	66.300865
1419.614139	29.968730	66.305870
1419.054063	26.441860	66.310874
1417.620228	25.138724	66.315879
1417.104967	19.835296	66.320884
1416.612306	16.468033	66.325889
1416.164362	21.442493	66.330894
1415.940881	13.146783	66.335898
1414.547873	23.628661	66.340903
1413.786354	18.488966	66.345908
1413.555957	16.934609	66.350913
1412.701227	23.303174	66.355918
1412.012707	19.837727	66.360922
1411.209881	26.786278	66.365927
1410.972108	19.574684	66.370932
1410.603909	26.615005	66.375937
1409.249220	15.914348	66.380942
1408.591602	19.288328	66.385946
1408.002870	18.707191	66.390951
1407.685931	13.578834	66.395956
1406.924961	21.383369	66.400961
1405.677696	23.843356	66.405966
1405.432232	17.697487	66.410970
1404.616027	23.768179	66.415975
1404.279503	15.271231	66.420980
1403.845674	18.874580	66.425985
1402.695195	22.535079	66.430990
1402.286177	15.994141	66.435994
1401.635366	25.318778	66.440999
1401.135769	20.068060	66.446004
1399.892926	17.777314	66.451009
1399.256851	19.133997	66.456014
1399.087561	12.337322	66.461018
1398.284345	26.223319	66.466023
1397.734659	18.305911	66.471028
1396.280579	18.067352	66.476033
1396.005181	18.012026	66.481038
1395.867274	21.046337	66.486042
1395.386758	27.451620	66.491047
1394.405285	22.096147	66.496052
1393.775344	24.174139	66.501057
1392.855574	20.758075	66.506062
1392.471072	19.519970	66.511066
1390.959497	23.537512	66.516071
1390.545524	18.318921	66.521076
1390.079376	22.936714	66.526081
1389.651616	19.904510	66.531086
1389.436328	18.590617	66.536090
1388.234274	15.139002	66.541095
1387.665584	19.238480	66.546100
1387.082094	22.692150	66.551105
1386.516181	21.968611	66.556110
1385.941739	21.074532	66.561114
1384.797003	10.015649	66.566119
1384.295322	17.990290	66.571124
1383.787462	20.987213	66.576129
1383.054708	24.893567	66.581134
1381.994080	13.015447	66.586138
1381.394344	19.296171	66.591143
1380.651343	23.781350	66.596148
1380.497902	21.689609	66.601153
1379.999891	20.384390	66.606158
1379.414904	14.306694	66.611162
1378.211653	13.421112	66.616167
1377.636495	23.016013	66.621172
1377.346404	19.089825	66.626177
1376.493542	19.835969	66.631182
1375.634676	19.710967	66.636186
1374.968553	16.253012	66.641191
1374.707237	20.489718	66.646196
1374.082169	16.561587	66.651201
1372.762426	25.144126	66.656206
1372.268345	20.419269	66.661210
1371.909596	21.397540	66.666215
1371.369361	23.633173	66.671220
1370.144283	7.288232	66.676225
1369.501431	20.984723	66.681230
1369.545822	10.342388	66.686234
1368.729712	18.449024	66.691239
1367.929480	13.104178	66.696244
1366.789748	23.366030	66.701249
1366.242997	21.786273	66.706254
1366.122099	19.667281	66.711258
1365.485695	21.126532	66.716263
1364.961031	21.628105	66.721268
1364.178441	15.772650	66.726273
1363.410384	19.075884	66.731278
1362.489525	13.866918	66.736282
1361.559040	20.758498	66.741287
1360.893566	27.014985	66.746292
1360.563393	22.147371	66.751297
1360.054122	27.410725	66.756302
1359.322538	21.622858	66.761306
1358.309748	25.439690	66.766311
1357.552246	26.516051	66.771316
1357.307580	14.924559	66.776321
1356.835077	18.111417	66.781326
1356.296167	10.944559	66.786330
1355.072594	23.689381	66.791335
1354.602866	23.929896	66.796340
1354.129390	24.241975	66.801345
1353.014881	23.883219	66.806350
1352.604941	16.462453	66.811354
1351.635519	23.219872	66.816359
1351.205087	25.035908	66.821364
1350.808744	26.322949	66.826369
1350.126701	29.082630	66.831374
1349.516360	12.980603	66.836378
1348.539287	25.127968	66.841383
1348.375902	18.831857	66.846388
1347.563457	23.436899	66.851393
1346.429073	26.462471	66.856398
1346.051980	20.422698	66.861402
1345.215826	28.554609	66.866407
1345.195870	18.772523	66.871412
1344.230047	20.776187	66.876417
1343.122118	24.903056	66.881422
1342.871485	22.391508	66.886426
1342.197706	26.402043	66.891431
1341.271725	15.447181	66.896436
1340.617515	21.611987	66.901441
1339.782736	28.332235	66.906446
1339.789885	20.496633	66.911450
1338.966145	34.185627	66.916455
1337.932715	28.975638	66.921460
1337.230294	20.939020	66.926465
1336.365623	24.981482	66.931470
1336.080748	18.890778	66.936474
1335.848985	27.700924	66.941479
1334.849015	26.683689	66.946484
1334.097296	22.927100	66.951489
1333.604335	26.683372	66.956494
1333.234648	18.824102	66.961498
1331.746694	18.545231	66.966503
1331.099224	13.939396	66.971508
1330.895340	17.922533	66.976513
1330.325583	24.606953	66.981518
1329.987272	22.203969	66.986522
1328.485583	29.072833	66.991527
1327.959125	24.397290	66.996532
1327.629838	20.172974	67.001537
1327.066893	24.659501	67.006542
1326.667553	24.355793	67.011546
1325.297642	26.087803	67.016551
1324.780965	16.581826	67.021556
1324.553707	24.828252	67.026561
1323.335380	27.540734	67.031566
1322.520227	23.374743	67.036570
1321.696423	26.715240	67.041575
1321.670798	22.412679	67.046580
1321.061684	26.455517	67.051585
1320.920928	32.668012	67.056590
1320.078933	14.967440	67.061594
1319.178648	24.509959	67.066599
1318.543863	18.224144	67.071604
1317.489839	24.498259	67.076609
1316.758214	25.337116	67.081614
1316.236519	19.120057	67.086618
1315.536246	32.923470	67.091623
1315.123457	23.752653	67.096628
1314.406779	25.024396	67.101633
1313.287554	27.918254	67.106638
1313.076643	23.265088	67.111642
1312.362080	25.711387	67.116647
1311.814735	25.972137	67.121652
1310.632980	29.528832	67.126657
1309.683389	25.366873	67.131662
1309.744463	19.341022	67.136666
1309.512205	24.602917	67.141671
1308.771017	18.803979	67.146676
1307.590045	21.836974	67.151681
1307.135502	27.353421	67.156686
1306.627283	8.872780	67.161690
1305.609948	13.910975	67.166695
1304.653800	24.720853	67.171700
1304.403387	28.211472	67.176705
1303.586896	23.123134	67.181710
1303.526461	16.102572	67.186714
1302.519402	22.430728	67.191719
1301.489543	18.443972	67.196724
1301.054018	17.609829	67.201729
1300.630589	28.364971	67.206734
1300.250112	18.290113	67.211738
1298.852169	21.124209	67.216743
1298.543424	29.503449	67.221748
1297.842512	18.855036	67.226753
1297.324618	26.302385	67.231758
1296.444922	14.838689	67.236762
1295.739171	33.348846	67.241767
1294.905045	25.142361	67.246772
1294.718125	27.179897	67.251777
1293.935418	28.320212	67.256782
1293.617834	19.572681	67.261786
1292.535046	30.446859	67.266791
1291.980519	29.865041	67.271796
1291.515221	22.462552	67.276801
1290.208430	21.296993	67.281806
1289.757792	25.343024	67.286810
1289.290469	16.035802	67.291815
1288.822333	29.149412	67.296820
1287.768370	20.083710	67.301825
1286.855880	21.008107	67.306830
1286.463902	27.170655	67.311834
1285.902264	26.806023	67.316839
1285.511966	13.600742	67.321844
1284.405363	23.885740	67.326849
1283.571807	26.756265	67.331854
1283.231462	21.997522	67.336858
1282.992281	27.844023	67.341863
1282.334708	25.176405	67.346868
1281.526553	28.213212	67.351873
1280.657494	27.574172	67.356878
1280.248336	18.666154	67.361882
1278.912444	26.855466	67.366887
1278.368717	19.337713	67.371892
1277.672147	27.187234	67.376897
1277.056955	23.274906	67.381902
1277.167559	18.826101	67.386906
1276.194970	26.795210	67.391911
1275.529790	15.138132	67.396916
1275.063056	19.964201	67.401921
1274.283835	23.463210	67.406926
1273.546849	10.330412	67.411930
1272.483822	15.793798	67.416935
1271.980324	20.261419	67.421940
1271.544385	18.321847	67.426945
1270.639458	14.799389	67.431950
1270.155544	15.149414	67.436954
1269.210199	15.558621	67.441959
1268.756743	20.235915	67.446964
1268.619442	13.189732	67.451969
1267.296041	26.294253	67.456974
1266.967598	12.908823	67.461978
1266.347933	19.583839	67.466983
1265.548772	31.559429	67.471988
1264.152543	22.344726	67.476993
1263.371167	17.984143	67.481998
1263.305327	20.426648	67.487002
1262.793280	19.205691	67.492007
1262.355906	22.599878	67.497012
1262.322823	15.909302	67.502017
1260.960748	22.281309	67.507022
1260.625497	7.394055	67.512026
1259.560676	20.083698	67.517031
1258.631439	21.736204	67.522036
1258.226568	22.628778	67.527041
1257.547996	21.423264	67.532046
1257.300071	25.629462	67.537050
1256.035638	23.063086	67.542055
1255.071283	20.642968	67.547060
1254.622866	21.492003	67.552065
1254.443439	29.700862	67.557070
1254.013148	17.418204	67.562074
1252.920129	31.787153	67.567079
1252.685354	16.082780	67.572084
1251.872511	16.508771	67.577089
1250.520495	21.496125	67.582094
1249.853679	19.978068	67.587098
1249.267259	21.249616	67.592103
1248.949949	19.094054	67.597108
1248.886140	15.977193	67.602113
1247.802270	22.774921	67.607118
1247.030739	14.847105	67.612122
1246.454776	18.980883	67.617127
1245.829770	16.438992	67.622132
1244.774793	13.134382	67.627137
1243.579701	20.298321	67.632142
1243.534533	14.483346	67.637146
1243.022787	20.388960	67.642151
1243.111778	18.123053	67.647156
1241.768265	10.354014	67.652161
1240.635737	12.466230	67.657166
1240.503983	13.255446	67.662170
1239.717426	15.074512	67.667175
1239.029729	15.370214	67.672180
1238.153146	8.462104	67.677185
1237.505763	24.930178	67.682190
1237.366765	6.799304	67.687194
1236.408176	26.981894	67.692199
1235.760375	20.425347	67.697204
1234.973552	18.948458	67.702209
1234.197953	24.766718	67.707214
1234.148253	11.497828	67.712218
1233.133092	21.498626	67.717223
1232.405398	15.793770	67.722228
1231.700727	8.847285	67.727233
1230.740503	14.124017	67.732238
1230.875810	5.829637	67.737242
1229.463243	16.281582	67.742247
1228.824750	19.963237	67.747252
1228.503991	18.741831	67.752257
1227.941720	25.291028	67.757262
1227.915923	19.409890	67.762266
1226.248277	18.369564	67.767271
1225.671947	13.842339	67.772276
1225.315853	22.569747	67.777281
1224.656278	26.455040	67.782286
1223.907160	14.037008	67.787290
1223.101498	25.009064	67.792295
1222.578847	25.748479	67.797300
1222.053803	24.510673	67.802305
1220.670473	24.429705	67.807310
1220.250701	20.035284	67.812314
1219.626467	20.860244	67.817319
1219.242537	22.580590	67.822324
1219.233025	20.057521	67.827329
1218.009875	21.476072	67.832334
1217.442817	18.522829	67.837338
1216.355268	26.273683	67.842343
1216.216165	22.660992	67.847348
1215.035511	18.277188	67.852353
1214.100624	28.932316	67.857358
1213.975455	13.552742	67.862362
1213.181424	16.330263	67.867367
1212.964372	21.834182	67.872372
1212.027318	13.994209	67.877377
1210.849273	28.753599	67.882382
1210.720076	15.123595	67.887386
1210.300688	25.762973	67.892391
1209.342163	17.472228	67.897396
1208.503026	23.237518	67.902401
1207.765528	18.877861	67.907406
1207.482915	19.099684	67.912410
1206.826774	26.002876	67.917415
1205.884122	27.950863	67.922420
1205.119560	23.515081	67.927425
1204.383638	26.758052	67.932430
1204.418345	12.666723	67.937434
1203.667412	19.976092	67.942439
1202.839836	28.827378	67.947444
1202.070912	24.173083	67.952449
1201.691993	30.828751	67.957454
1200.821615	13.624793	67.962458
1199.804530	20.673703	67.967463
1199.273135	22.335499	67.972468
1199.166889	14.428057	67.977473
1197.842697	21.609393	67.982478
1197.001582	13.036619	67.987482
1196.374201	24.390355	67.992487
1195.821781	24.921609	67.997492
1195.829581	18.590407	68.002497
1195.171869	18.614833	68.007502
1194.240337	8.190814	68.012506
1193.296154	20.058579	68.017511
1192.814573	17.274684	68.022516
1192.596168	14.911003	68.027521
1191.170541	15.835040	68.032526
1190.968842	7.468097	68.037530
1190.302463	15.052615	68.042535
1189.403546	18.778852	68.047540
1188.615182	13.178283	68.052545
1187.670312	24.274994	68.057550
1187.679877	19.004855	68.062554
1186.857564	15.663265	68.067559
1186.767806	17.037192	68.072564
1185.442208	13.447627	68.077569
1184.413387	19.763511	68.082574
1184.288391	9.771064	68.087578
1183.583507	15.343108	68.092583
1183.078224	10.536500	68.097588
1182.207762	17.297153	68.102593
1181.233980	18.713907	68.107598
1181.139291	13.242722	68.112602
1180.735700	18.758962	68.117607
1179.782411	14.047264	68.122612
1178.966503	8.542550	68.127617
1178.430804	26.808030	68.132622
1177.995364	18.946639	68.137626
1176.536201	19.846054	68.142631
1176.302905	23.895380	68.147636
1176.091411	21.685150	68.152641
1174.854867	20.923238	68.157646
1174.017515	14.329051	68.162650
1173.330662	16.319945	68.167655
1172.874775	13.311184	68.172660
1172.593588	17.704033	68.177665
1171.698097	16.410037	68.182670
1171.099286	19.509775	68.187674
1170.126525	25.722128	68.192679
1169.783580	15.357471	68.197684
1169.130024	18.607850	68.202689
1168.233808	20.934836	68.207694
1167.771943	15.179836	68.212698
1167.141231	21.189543	68.217703
1166.531354	18.670499	68.222708
1165.759918	24.349335	68.227713
1164.628571	24.967947	68.232718
1164.264724	18.276369	68.237722
1163.817087	30.831609	68.242727
1163.218468	13.144454	68.247732
1162.386322	26.162992	68.252737
1161.362776	30.964098	68.257742
1161.174481	21.032180	68.262746
1160.297807	24.333821	68.267751
1159.829816	22.296861	68.272756
1159.339783	18.172264	68.277761
1157.970136	23.813781	68.282766
1158.180871	21.293530	68.287770
1157.570393	23.480449	68.292775
1156.690529	16.084012	68.297780
1155.797744	23.915876	68.302785
1155.110772	24.351840	68.307790
1154.837909	25.524646	68.312794
1153.439915	19.396552	68.317799
1152.979901	18.381819	68.322804
1152.489876	27.977402	68.327809
1152.079719	28.000311	68.332814
1151.316621	21.164072	68.337818
1150.258051	16.276735	68.342823
1149.656085	16.202415	68.347828
1149.180291	20.438555	68.352833
1148.740979	31.655148	68.357838
1148.092164	17.286173	68.362842
1147.004996	26.506783	68.367847
1146.080614	20.673961	68.372852
1145.919972	16.810802	68.377857
1145.511423	22.518657	68.382862
1144.836265	20.694434	68.387866
1143.912644	25.558502	68.392871
1143.366067	23.150827	68.397876
1142.955202	27.400297	68.402881
1141.733649	29.263353	68.407886
1141.020784	26.705501	68.412890
1140.441492	29.685442	68.417895
1140.146761	25.438313	68.422900
1139.979231	20.194769	68.427905
1138.178452	20.128206	68.432910
1137.789659	22.704088	68.437914
1137.236273	21.934457	68.442919
1136.943125	19.033864	68.447924
1135.927122	23.267622	68.452929
1134.921526	16.102517	68.457934
1134.657084	17.023237	68.462938
1134.226073	25.690024	68.467943
1133.675749	24.659696	68.472948
1132.748119	15.790035	68.477953
1132.046571	24.163947	68.482958
1131.660486	15.815300	68.487962
1130.834141	15.965920	68.492967
1129.893747	17.747985	68.497972
1129.430773	14.488035	68.502977
1128.808935	30.961522	68.507982
1128.404075	19.329325	68.512986
1127.124815	17.940265	68.517991
1126.578344	7.379330	68.522996
1126.281865	20.142341	68.528001
1125.479470	23.887939	68.533006
1124.610713	13.660555	68.538010
1123.550457	23.457238	68.543015
1123.377953	20.177892	68.548020
1123.206693	18.126856	68.553025
1122.574998	23.434949	68.558030
1121.567943	13.644326	68.563034
1120.732142	23.854759	68.568039
1120.353610	20.914131	68.573044
1119.561122	21.526170	68.578049
1118.535155	26.106890	68.583054
1117.951695	18.737439	68.588058
1117.346025	27.594446	68.593063
1116.883070	18.765995	68.598068
1116.429815	17.649264	68.603073
1115.272106	22.086930	68.608078
1114.888934	23.088043	68.613082
1114.436414	27.713169	68.618087
1113.796336	29.600439	68.623092
1112.723895	20.017346	68.628097
1111.812758	24.332208	68.633102
1111.363259	20.660089	68.638106
1111.065327	23.224674	68.643111
1110.614966	19.618928	68.648116
1109.986734	12.296031	68.653121
1108.949524	20.325930	68.658126
1108.742795	23.497358	68.663130
1107.325915	16.181639	68.668135
1106.612353	18.678294	68.673140
1106.295569	19.325055	68.678145
1105.687293	25.982519	68.683150
1105.293294	12.309504	68.688154
1104.098131	21.356485	68.693159
1103.431500	11.893359	68.698164
1103.192871	17.979481	68.703169
1102.483247	12.673941	68.708174
1101.507075	22.275895	68.713178
1100.635605	26.343164	68.718183
1100.007710	21.688549	68.723188
1100.163025	10.905587	68.728193
1099.434336	29.531372	68.733198
1098.595149	17.063062	68.738202
1097.659879	16.385732	68.743207
1096.966687	17.962895	68.748212
1096.039568	17.399392	68.753217
1094.857165	29.011757	68.758222
1094.741962	14.264590	68.763226
1094.293738	19.947219	68.768231
1094.184927	27.875168	68.773236
1093.722010	19.106645	68.778241
1092.488998	19.684688	68.783246
1091.969301	16.679787	68.788250
1091.230869	21.504947	68.793255
1090.346793	13.030521	68.798260
1089.508811	24.334190	68.803265
1089.052568	19.166546	68.808270
1088.707820	12.460911	68.813274
1087.887454	19.489600	68.818279
1086.968467	21.004910	68.823284
1086.338834	16.588710	68.828289
1085.812191	21.031654	68.833294
1085.471458	12.611147	68.838298
1084.871551	17.302300	68.843303
1084.016775	22.363601	68.848308
1083.599642	17.079345	68.853313
1082.466977	21.935685	68.858318
1081.817639	20.026944	68.863322
1081.215926	21.878155	68.868327
1080.558648	18.319527	68.873332
1079.660591	17.440732	68.878337
1078.573467	26.144092	68.883342
1078.264031	22.597938	68.888346
1077.681891	16.593999	68.893351
1077.298485	16.237332	68.898356
1077.448102	14.673019	68.903361
1076.131258	20.531689	68.908366
1075.287786	17.256587	68.913370
1074.698321	26.724487	68.918375
1073.586011	23.247714	68.923380
1072.875658	18.650384	68.928385
1072.167345	17.812371	68.933390
1072.281173	16.957108	68.938394
1071.752787	24.119133	68.943399
1070.548257	23.522499	68.948404
1069.996076	7.638435	68.953409
1069.090851	19.589923	68.958414
1069.097687	17.204614	68.963418
1067.830163	18.759611	68.968423
1067.099807	16.515241	68.973428
1066.339244	13.383079	68.978433
1065.576781	23.091400	68.983438
1065.790061	14.021333	68.988442
1064.915159	14.909864	68.993447
1063.935867	19.055801	68.998452
1063.753986	9.564457	69.003457
1062.776176	20.808369	69.008462
1061.701029	15.294477	69.013466
1061.066196	20.172550	69.018471
1060.384320	14.209718	69.023476
1060.319500	12.761527	69.028481
1059.556753	21.082106	69.033486
1058.798813	14.036917	69.038490
1057.910722	25.022120	69.043495
1057.353682	15.331828	69.048500
1057.398764	10.989650	69.053505
1055.706699	17.642921	69.058510
1055.141824	12.995644	69.063514
1054.623004	18.202207	69.068519
1054.121744	14.226085	69.073524
1053.799143	15.156066	69.078529
1052.301663	18.818296	69.083534
1051.993219	13.858972	69.088538
1051.665956	16.882413	69.093543
1050.960169	17.356093	69.098548
1050.959895	10.190364	69.103553
1049.535302	17.308886	69.108558
1049.121070	14.629432	69.113562
1047.705424	18.172983	69.118567
1046.777325	12.741364	69.123572
1046.282975	7.668112	69.128577
1045.724230	13.075001	69.133582
1045.460910	18.149447	69.138586
1045.384828	13.247776	69.143591
1044.873298	16.172796	69.148596
1043.954386	14.267532	69.153601
1043.100093	17.106731	69.158606
1042.364824	3.839718	69.163610
1041.284402	5.932688	69.168615
1040.779633	17.298469	69.173620
1040.524265	2.873262	69.178625
1039.625202	7.017478	69.183630
1038.729420	-0.023113	69.188634
1037.866242	20.680508	69.193639
1037.213806	15.069408	69.198644
1036.942111	11.085152	69.203649
1036.629490	18.104035	69.208654
1035.968558	12.311352	69.213658
1034.750185	15.112283	69.218663
1034.363195	8.545852	69.223668
1033.835471	17.406233	69.228673
1032.361448	14.463297	69.233678
1032.049551	7.959039	69.238682
1031.219339	13.607829	69.243687
1030.786913	13.074456	69.248692
1030.749533	11.125136	69.253697
1030.181682	15.492639	69.258702
1029.415099	9.344591	69.263706
1028.567121	17.055809	69.268711
1027.598355	19.317110	69.273716
1026.780982	8.040760	69.278721
1025.964267	17.544818	69.283726
1025.742245	6.752512	69.288730
1025.310672	7.439624	69.293735
1024.643704	11.496453	69.298740
1023.632315	15.559195	69.303745
1022.677718	18.796002	69.308750
1022.716814	14.800146	69.313754
1022.017639	11.073154	69.318759
1021.019246	5.425641	69.323764
1020.264517	10.004236	69.328769
1019.554449	14.714506	69.333774
1019.159635	5.760125	69.338778
1018.511389	3.885926	69.343783
1017.468050	6.045549	69.348788
1016.895754	7.277049	69.353793
1016.633798	9.744449	69.358798
1016.544836	3.236265	69.363802
1015.219393	15.519565	69.368807
1014.712509	15.923758	69.373812
1013.968559	11.062123	69.378817
1012.585493	14.289834	69.383822
1012.205972	7.693834	69.388826
1011.445544	14.758736	69.393831
1011.194630	21.034484	69.398836
1010.687223	14.168656	69.403841
1010.163617	18.789333	69.408846
1009.350932	10.516484	69.413850
1008.754988	25.861431	69.418855
1007.940532	14.064201	69.423860
1007.308789	16.492666	69.428865
1005.893047	18.331487	69.433870
1005.681522	9.718545	69.438874
1005.177019	15.274513	69.443879
1004.837339	18.620072	69.448884
1004.162110	21.657884	69.453889
1002.903655	20.306581	69.458894
1002.404202	10.764849	69.463898
1002.052143	18.572215	69.468903
1001.457103	15.181913	69.473908
1000.785225	16.276292	69.478913
1000.149067	17.980028	69.483918
999.621418	16.348430	69.488922
998.516263	17.855545	69.493927
997.491890	7.050562	69.498932
996.900121	16.766425	69.503937
996.335880	17.115090	69.508942
996.499944	14.056606	69.513946
995.740379	16.831859	69.518951
994.822998	15.582414	69.523956
994.320953	16.230280	69.528961
993.423772	20.454643	69.533966
993.118493	19.602986	69.538970
991.893753	23.284933	69.543975
991.279547	16.663195	69.548980
990.781512	16.228583	69.553985
989.203342	20.039313	69.558990
989.175922	16.699047	69.563994
988.628015	17.218587	69.568999
988.057959	18.344078	69.574004
988.249387	9.876764	69.579009
986.922339	21.263006	69.584014
986.217637	13.744149	69.589018
985.341132	20.299226	69.594023
984.360306	22.008925	69.599028
983.624686	11.610604	69.604033
982.698279	26.020920	69.609038
982.799134	14.868141	69.614042
982.209965	17.007549	69.619047
981.681129	20.386365	69.624052
981.215738	12.824698	69.629057
980.384980	14.780189	69.634062
980.098293	8.185193	69.639066
978.977599	9.220104	69.644071
977.731399	12.648413	69.649076
977.475569	14.026693	69.654081
976.788826	12.947144	69.659086
976.422275	8.610546	69.664090
975.344109	16.757395	69.669095
974.342731	18.623340	69.674100
974.307820	14.822197	69.679105
973.287196	20.990185	69.684110
973.544544	4.013778	69.689114
972.104341	17.936542	69.694119
971.500068	5.101321	69.699124
971.238108	7.081423	69.704129
970.266993	13.500163	69.709134
969.330792	7.443788	69.714138
968.907180	12.496433	69.719143
967.944983	6.671288	69.724148
967.765988	16.630566	69.729153
966.624855	24.533541	69.734158
966.160964	7.315496	69.739162
965.426933	19.525206	69.744167
964.922677	5.652156	69.749172
964.725378	8.533491	69.754177
963.713315	10.538340	69.759182
963.232497	5.305254	69.764186
962.123998	17.907306	69.769191
961.454037	6.435632	69.774196
960.707689	3.149851	69.779201
960.114083	16.504213	69.784206
959.754131	8.454243	69.789210
958.987807	14.310516	69.794215
958.261519	11.114586	69.799220
957.670853	10.704184	69.804225
956.647689	13.442543	69.809230
956.412390	11.748661	69.814234
955.798365	20.009323	69.819239
955.322953	13.464864	69.824244
954.509793	14.477654	69.829249
953.628261	14.026804	69.834254
953.270242	8.045590	69.839258
952.162516	15.244626	69.844263
951.200358	9.534604	69.849268
951.157534	20.842651	69.854273
950.300069	20.015793	69.859278
950.249847	11.448156	69.864282
949.261549	11.175156	69.869287
948.231672	8.634699	69.874292
948.146889	0.837427	69.879297
947.202455	18.669605	69.884302
946.527006	9.405071	69.889306
945.828606	8.190185	69.894311
945.608075	11.499439	69.899316
944.396372	11.596323	69.904321
943.324563	12.967261	69.909326
942.934442	14.639741	69.914330
942.292249	17.803202	69.919335
941.956960	15.967531	69.924340
941.618509	18.924952	69.929345
940.095242	21.197256	69.934350
939.692112	15.242145	69.939354
939.079009	18.486137	69.944359
938.925271	14.473661	69.949364
938.068580	16.318170	69.954369
936.723816	16.098750	69.959374
936.401930	2.679261	69.964378
935.982042	8.456747	69.969383
935.224516	11.124453	69.974388
934.357105	8.110270	69.979393
933.514039	19.810611	69.984398
933.128187	11.324778	69.989402
932.643671	16.827111	69.994407
932.122213	17.389766	69.999412
931.262214	17.470109	70.004417
930.081091	14.310302	70.009422
930.129436	10.562149	70.014426
929.579362	16.581142	70.019431
928.567839	7.584576	70.024436
928.286876	8.643569	70.029441
927.325137	10.006458	70.034446
926.950872	10.719161	70.039450
925.796384	12.010220	70.044455
925.092891	9.966635	70.049460
924.792713	12.799687	70.054465
924.088117	13.678509	70.059470
923.578647	12.285320	70.064474
922.378088	11.945182	70.069479
921.886946	13.868719	70.074484
921.552702	-3.770495	70.079489
920.707970	11.191396	70.084494
919.779518	8.813013	70.089498
919.197517	11.058531	70.094503
918.615424	13.447574	70.099508
918.494719	8.519900	70.104513
917.206026	17.479327	70.109518
916.397278	5.305905	70.114522
915.893164	13.862904	70.119527
915.477177	16.307517	70.124532
915.239101	9.603866	70.129537
913.742584	21.499680	70.134542
913.468110	8.419592	70.139546
912.909623	10.503666	70.144551
912.592436	11.180477	70.149556
911.375278	5.679801	70.154561
910.358104	13.526791	70.159566
910.121715	4.280708	70.164570
909.669258	16.639584	70.169575
908.622165	14.524526	70.174580
908.283751	11.333115	70.179585
907.078773	17.265524	70.184590
906.825948	7.451172	70.189594
906.405932	16.661871	70.194599
905.611397	9.772385	70.199604
904.813336	12.580597	70.204609
904.044252	20.586813	70.209614
904.018426	9.887889	70.214618
902.810321	13.776970	70.219623
901.908966	14.647688	70.224628
901.474238	0.184832	70.229633
901.027985	16.857463	70.234638
900.249241	9.702101	70.239642
899.530526	3.573295	70.244647
898.876181	5.565391	70.249652
898.701269	0.144855	70.254657
897.532926	15.323848	70.259662
896.936578	3.405226	70.264666
896.314379	10.150093	70.269671
895.919504	8.036895	70.274676
894.725227	4.753040	70.279681
893.860082	22.299787	70.284686
893.453668	2.882135	70.289690
893.103641	5.535457	70.294695
892.442993	7.180035	70.299700
891.390108	11.550640	70.304705
890.801567	15.183412	70.309710
890.682708	3.769139	70.314714
890.111154	10.874971	70.319719
889.065217	11.581040	70.324724
888.528392	8.331322	70.329729
887.805855	14.298919	70.334734
886.659619	7.302986	70.339738
885.514859	12.377377	70.344743
885.274094	10.449396	70.349748
885.048695	3.258012	70.354753
884.469027	17.100617	70.359758
884.425243	8.140862	70.364762
883.365347	14.526450	70.369767
882.402194	7.315289	70.374772
882.033077	6.623625	70.379777
880.658932	8.242993	70.384782
880.140841	3.375423	70.389786
879.592503	8.302842	70.394791
879.266056	-0.487331	70.399796
878.837572	-6.903605	70.404801
877.519924	14.790191	70.409806
876.779956	-0.589212	70.414810
876.342707	5.665727	70.419815
875.706506	7.667557	70.424820
875.595247	9.612641	70.429825
874.385196	13.714943	70.434830
873.838794	12.636741	70.439834
873.233633	6.769002	70.444839
872.614655	4.443886	70.449844
871.551085	11.560224	70.454849
870.735516	-1.058385	70.459854
870.486250	1.854880	70.464858
869.777836	7.067990	70.469863
869.190522	2.145205	70.474868
868.278380	2.911991	70.479873
867.195987	5.049502	70.484878
866.982543	3.399463	70.489882
866.946524	8.157023	70.494887
866.191954	0.699773	70.499892
865.873172	6.439094	70.504897
865.118829	9.207242	70.509902
863.961770	5.846512	70.514906
862.999231	10.956565	70.519911
862.472055	12.499477	70.524916
862.310867	3.131042	70.529921
860.888590	10.252439	70.534926
860.015325	4.383224	70.539930
859.347536	12.113111	70.544935
858.850487	6.548304	70.549940
858.678639	7.124712	70.554945
858.430987	11.352962	70.559950
857.983884	4.666826	70.564954
856.760704	15.847339	70.569959
856.156497	10.510910	70.574964
855.454705	9.528413	70.579969
854.473310	12.854702	70.584974
853.859997	12.634018	70.589978
853.390811	5.262237	70.594983
852.872550	8.262480	70.599988
852.029058	-3.504811	70.604993
851.344254	6.456119	70.609998
850.916846	4.132056	70.615002
849.713724	9.863908	70.620007
848.512602	15.063987	70.625012
848.384149	3.335844	70.630017
847.600375	14.187782	70.635022
847.515196	2.742924	70.640026
847.251722	14.199623	70.645031
846.609008	5.150701	70.650036
845.864791	2.673634	70.655041
844.850233	6.653360	70.660046
844.115140	9.002114	70.665050
843.147941	4.606607	70.670055
842.534012	10.984298	70.675060
842.229633	5.543375	70.680065
841.488184	20.026778	70.685070
840.642776	2.573036	70.690074
839.853991	6.795958	70.695079
839.173541	10.870743	70.700084
838.835706	5.816786	70.705089
838.392606	8.691521	70.710094
837.340898	11.894961	70.715098
836.464738	2.559915	70.720103
835.843290	16.648882	70.725108
836.007751	10.846306	70.730113
835.250296	17.332008	70.735118
834.238901	7.318288	70.740122
833.523259	6.369544	70.745127
832.885033	2.418437	70.750132
832.107184	2.561434	70.755137
831.255193	12.560024	70.760142
830.681485	-0.929737	70.765146
830.188018	9.973764	70.770151
829.779702	11.119275	70.775156
829.196800	-3.337314	70.780161
827.916743	3.715723	70.785166
827.433821	4.868379	70.790170
827.118300	8.905575	70.795175
825.828103	7.748660	70.800180
825.191535	8.171958	70.805185
824.495658	13.990239	70.810190
824.705650	11.230382	70.815194
824.002926	15.005929	70.820199
822.966704	11.056676	70.825204
822.270896	4.365984	70.830209
821.816245	8.672921	70.835214
821.513512	-2.918654	70.840218
820.076851	8.612834	70.845223
819.005346	16.555240	70.850228
818.876033	3.690203	70.855233
818.192039	15.773690	70.860238
818.104411	9.930817	70.865242
817.213513	11.932204	70.870247
816.526713	10.269211	70.875252
816.178476	6.775014	70.880257
814.531350	10.596822	70.885262
813.884740	5.197769	70.890266
813.440781	10.734662	70.895271
812.867663	15.096733	70.900276
812.700449	8.739804	70.905281
811.886452	16.000946	70.910286
810.912219	-3.480821	70.915290
810.383616	7.354153	70.920295
809.635841	8.698794	70.925300
809.710280	4.481268	70.930305
808.406332	6.395442	70.935310
808.070902	7.127212	70.940314
807.184313	1.454115	70.945319
805.949888	7.364441	70.950324
805.448793	5.736546	70.955329
804.588472	8.728171	70.960334
804.503119	-0.546664	70.965338
804.263269	1.940887	70.970343
803.214343	6.285661	70.975348
802.507123	1.511302	70.980353
801.878215	1.666869	70.985358
801.412819	-1.244097	70.990362
800.513400	8.861401	70.995367
799.718583	10.147298	71.000372
799.024264	0.135165	71.005377
798.432398	6.911491	71.010382
798.043039	1.209703	71.015386
796.799121	6.722557	71.020391
796.461076	7.112530	71.025396
796.048054	9.328018	71.030401
795.262331	13.019009	71.035406
794.602924	-2.040427	71.040410
793.883611	10.952317	71.045415
792.960783	8.784411	71.050420
793.033548	2.124342	71.055425
791.762798	9.860344	71.060430
790.992758	-2.101548	71.065434
790.503231	5.525848	71.070439
790.155155	8.716637	71.075444
789.447566	3.360418	71.080449
788.372818	8.500975	71.085454
788.034842	-0.498663	71.090458
787.200187	6.614376	71.095463
786.665771	9.625087	71.100468
785.940589	-0.095109	71.105473
785.181567	8.554526	71.110478
784.748697	-4.434064	71.115482
784.272277	-1.110875	71.120487
783.241075	3.308358	71.125492
782.590399	-5.644645	71.130497
781.802512	2.060215	71.135502
781.617225	-3.554203	71.140506
780.385061	2.997621	71.145511
779.493363	1.608546	71.150516
779.531761	1.684687	71.155521
778.743536	6.823787	71.160526
778.273600	-0.886911	71.165530
777.378396	9.886580	71.170535
776.522976	10.682216	71.175540
776.169299	2.544558	71.180545
775.391005	8.188303	71.185550
774.679622	6.210678	71.190554
773.871864	6.837870	71.195559
773.438558	3.257874	71.200564
773.191376	-7.900963	71.205569
772.233197	15.762107	71.210574
771.566894	-0.477414	71.215578
770.559031	-5.202318	71.220583
770.261697	2.515911	71.225588
769.245983	4.732736	71.230593
768.571367	7.319474	71.235598
768.112573	-0.457654	71.240602
767.767963	3.155227	71.245607
766.556076	7.729396	71.250612
766.091559	2.424375	71.255617
765.090937	6.034465	71.260622
764.879963	3.365286	71.265626
764.347456	6.096564	71.270631
763.485730	9.739737	71.275636
763.164105	5.859673	71.280641
762.495231	9.103118	71.285646
761.842608	-1.718343	71.290650
760.662262	-2.638811	71.295655
760.003262	8.010339	71.300660
759.785999	6.190600	71.305665
759.162667	17.436501	71.310670
757.979503	4.677762	71.315674
757.358032	6.286172	71.320679
756.761038	11.785934	71.325684
756.647426	-1.184093	71.330689
755.291532	3.827766	71.335694
754.706563	2.916589	71.340698
754.298381	4.815907	71.345703
753.679674	7.849506	71.350708
752.964502	8.056669	71.355713
751.548423	11.196726	71.360718
751.344966	3.997139	71.365722
750.933091	3.436889	71.370727
750.344526	7.380363	71.375732
750.116513	-0.476084	71.380737
748.821770	6.336465	71.385742
748.444378	-11.696376	71.390746
747.868849	1.688230	71.395751
746.842792	-2.524389	71.400756
746.143982	6.467343	71.405761
745.265649	2.541876	71.410766
744.688484	-2.059197	71.415770
744.172539	6.733100	71.420775
743.853133	2.663445	71.425780
743.547027	6.998782	71.430785
742.328232	11.184538	71.435790
741.619250	5.205632	71.440794
741.465261	5.635695	71.445799
740.072556	-1.013392	71.450804
739.800785	-5.237292	71.455809
738.932379	6.894486	71.460814
738.644637	-4.164843	71.465818
737.832990	0.810831	71.470823
736.718058	-0.840741	71.475828
736.331910	0.030006	71.480833
735.781083	8.338982	71.485838
735.105250	-1.261312	71.490842
734.249802	-4.375095	71.495847
733.185450	5.520126	71.500852
733.146912	-3.235426	71.505857
732.393260	1.436111	71.510862
732.574269	-7.893737	71.515866
731.076913	-2.947657	71.520871
730.190719	0.216851	71.525876
730.247711	-11.141801	71.530881
729.164264	-0.199554	71.535886
728.414962	-2.087544	71.540890
727.749598	-3.910047	71.545895
727.023180	-0.116515	71.550900
727.065838	-8.378768	71.555905
725.578905	1.345609	71.560910
725.121579	-4.712783	71.565914
724.569290	5.878376	71.570919
723.871412	4.314951	71.575924
723.100850	2.409846	71.580929
722.202657	4.590629	71.585934
721.767491	0.971515	71.590938
721.397121	2.204043	71.595943
720.950681	3.877635	71.600948
719.822180	-4.317987	71.605953
719.328061	6.919953	71.610958
718.698061	-1.250965	71.615962
717.998488	6.006168	71.620967
717.261169	5.292732	71.625972
716.772450	6.499950	71.630977
716.071773	4.273046	71.635982
715.215631	1.148340	71.640986
714.082253	2.895046	71.645991
713.787287	10.310114	71.650996
713.815694	6.257622	71.656001
712.759380	7.933708	71.661006
711.784493	4.160830	71.666010
711.103308	2.847074	71.671015
710.617310	-0.035359	71.676020
710.599727	4.154684	71.681025
709.271244	9.274171	71.686030
708.420050	1.818175	71.691034
708.045733	-3.326143	71.696039
707.626516	2.468605	71.701044
706.766437	-2.678790	71.706049
705.764762	5.653093	71.711054
705.112621	1.336794	71.716058
705.097584	0.429496	71.721063
704.315667	3.473325	71.726068
703.418469	-2.494518	71.731073
702.502676	-3.859225	71.736078
702.072835	-1.180557	71.741082
701.031893	3.401113	71.746087
700.016238	2.571148	71.751092
699.674589	2.573760	71.756097
698.934380	5.145728	71.761102
698.850537	7.961697	71.766106
698.595820	3.465414	71.771111
698.020579	3.069966	71.776116
697.147260	-6.748031	71.781121
696.247730	-2.906424	71.786126
695.609845	4.132722	71.791130
694.567516	5.306672	71.796135
693.797088	5.305021	71.801140
693.801387	-3.799561	71.806145
693.262696	-1.215527	71.811150
692.251912	-4.995294	71.816154
691.134710	1.069884	71.821159
690.624312	4.239220	71.826164
690.648011	-8.199119	71.831169
689.145790	3.560492	71.836174
688.411836	-1.398813	71.841178
688.101950	-4.181547	71.846183
687.331783	2.301476	71.851188
687.373406	-6.269706	71.856193
686.368409	2.343419	71.861198
685.600259	-5.382843	71.866202
685.340763	-3.221753	71.871207
683.928534	2.571852	71.876212
683.434030	-3.409644	71.881217
682.558458	0.253103	71.886222
682.327664	-4.456729	71.891226
681.809229	4.112033	71.896231
681.081698	8.094999	71.901236
680.326761	-0.372992	71.906241
679.461191	7.401039	71.911246
678.786395	4.092918	71.916250
678.524270	0.329557	71.921255
677.472758	3.821621	71.926260
676.997567	3.358202	71.931265
676.301070	0.066156	71.936270
675.785109	0.577522	71.941274
675.001870	7.737597	71.946279
673.849397	7.891414	71.951284
673.749728	-3.136347	71.956289
672.957112	2.736794	71.961294
672.613100	0.836320	71.966298
671.715489	3.871773	71.971303
670.728151	8.235176	71.976308
670.400742	-0.819735	71.981313
669.673564	8.302690	71.986318
669.267466	0.597625	71.991322
668.318280	6.740141	71.996327
667.708381	14.378840	72.001332
667.130940	14.409545	72.006337
666.209147	10.710234	72.011342
665.318657	11.084120	72.016346
664.953601	11.938903	72.021351
664.471071	6.531114	72.026356
664.247502	1.465302	72.031361
663.141442	6.500501	72.036366
662.675867	0.847153	72.041370
661.880479	11.636317	72.046375
660.928033	13.489856	72.051380
659.838513	10.873865	72.056385
659.120589	15.982879	72.061390
658.774839	8.083690	72.066394
658.841240	1.043002	72.071399
657.971495	15.343423	72.076404
657.757980	5.608023	72.081409
656.452873	10.192356	72.086414
655.840659	2.807137	72.091418
655.559011	8.838615	72.096423
654.070892	7.248092	72.101428
653.440620	0.564371	72.106433
652.788530	7.711449	72.111438
652.662872	6.309237	72.116442
652.322512	6.396810	72.121447
651.502944	-0.677828	72.126452
650.624113	7.607700	72.131457
649.833961	10.567697	72.136462
649.441450	5.319049	72.141466
648.597076	12.282279	72.146471
647.392790	6.290821	72.151476
647.514359	-11.148062	72.156481
646.959642	10.408518	72.161486
645.985466	10.603342	72.166490
644.910979	5.859140	72.171495
644.599782	15.134530	72.176500
644.094758	16.002145	72.181505
643.355091	13.240553	72.186510
642.517183	6.121526	72.191514
641.860720	9.427680	72.196519
641.397521	8.347320	72.201524
641.145060	2.455023	72.206529
639.683862	7.452170	72.211534
639.052312	6.526362	72.216538
638.654059	-1.142096	72.221543
638.397309	1.953735	72.226548
637.240283	-2.936595	72.231553
636.390471	10.518521	72.236558
635.915681	10.901908	72.241562
635.790497	11.284810	72.246567
634.692984	14.257493	72.251572
634.108109	5.912250	72.256577
632.949247	10.060122	72.261582
632.855123	6.184850	72.266586
632.083056	7.948167	72.271591
630.867689	7.799772	72.276596
630.460385	1.477956	72.281601
629.617954	13.115172	72.286606
629.520419	6.348185	72.291610
628.890699	2.720651	72.296615
628.459023	6.043048	72.301620
627.517823	6.090695	72.306625
626.741213	6.097935	72.311630
626.457109	6.637041	72.316634
625.523528	3.843260	72.321639
624.624732	6.035212	72.326644
624.379407	2.403229	72.331649
623.553571	9.420285	72.336654
622.720266	6.673614	72.341658
621.961975	2.533527	72.346663
621.339547	3.413537	72.351668
621.697943	5.436794	72.356673
620.176855	8.458022	72.361678
619.643755	5.485335	72.366682
619.160070	-7.854667	72.371687
617.895024	3.561261	72.376692
617.249726	-4.911548	72.381697
616.515037	-1.353224	72.386702
616.318423	0.613345	72.391706
615.936701	4.590135	72.396711
614.619436	2.765834	72.401716
614.089537	5.518802	72.406721
613.524291	9.737722	72.411726
613.371931	4.816700	72.416730
612.334304	11.585206	72.421735
611.169181	11.853036	72.426740
610.730262	-6.013838	72.431745
610.493096	5.315651	72.436750
609.941562	3.044524	72.441754
608.837947	-2.412563	72.446759
607.790041	9.440317	72.451764
607.872608	0.197112	72.456769
606.982335	2.051806	72.461774
606.103324	4.213803	72.466778
605.331915	3.966321	72.471783
604.861747	10.530899	72.476788
604.379232	1.078066	72.481793
604.040651	1.130667	72.486798
603.084252	-2.206695	72.491802
602.649615	4.484691	72.496807
601.892877	8.700997	72.501812
600.890509	-0.615414	72.506817
599.773043	8.823091	72.511822
599.077141	7.081184	72.516826
598.708895	8.073684	72.521831
598.539346	5.038365	72.526836
598.400419	-2.848013	72.531841
597.137537	2.475551	72.536846
596.354589	-2.537422	72.541850
596.135473	5.043770	72.546855
594.976746	10.708732	72.551860
594.145671	-5.075509	72.556865
593.411944	7.750816	72.561870
593.008657	5.432423	72.566874
592.578977	13.961832	72.571879
591.682470	11.149542	72.576884
590.984264	1.179111	72.581889
590.216712	6.996240	72.586894
589.896753	10.509015	72.591898
589.602128	7.261797	72.596903
588.436165	14.672100	72.601908
587.645889	5.337680	72.606913
586.968962	17.101517	72.611918
586.807221	3.497337	72.616922
585.576893	3.679367	72.621927
584.843720	5.814986	72.626932
584.566742	9.327223	72.631937
583.940173	14.877462	72.636942
583.393216	10.173844	72.641946
582.336939	8.337951	72.646951
581.553545	12.809255	72.651956
581.368276	2.623076	72.656961
580.939868	11.139665	72.661966
580.259735	5.488972	72.666970
579.523860	7.421588	72.671975
578.683440	12.758299	72.676980
577.892553	3.813505	72.681985
576.796610	8.202125	72.686990
576.400755	6.477089	72.691994
575.854114	7.539011	72.696999
575.225336	7.816045	72.702004
574.477978	4.248268	72.707009
573.590015	10.988215	72.712014
573.188029	12.366156	72.717018
572.934808	0.378807	72.722023
572.143795	4.695200	72.727028
571.218466	7.935383	72.732033
570.590746	8.500845	72.737038
570.234043	3.899396	72.742042
569.762431	1.052552	72.747047
568.622873	11.484956	72.752052
568.171929	1.509842	72.757057
567.385597	8.694091	72.762062
566.290648	12.943780	72.767066
565.269338	0.482671	72.772071
564.670397	3.979960	72.777076
564.293089	-2.854417	72.782081
564.019288	11.404705	72.787086
563.844016	0.366925	72.792090
563.193962	0.108010	72.797095
562.060798	12.712532	72.802100
561.617450	3.040573	72.807105
560.843363	15.285111	72.812110
560.185689	7.993898	72.817114
559.402612	5.975718	72.822119
558.785714	16.261791	72.827124
558.284444	7.578387	72.832129
556.871735	12.340765	72.837134
556.153985	9.935272	72.842138
556.238993	10.589059	72.847143
555.675691	13.459329	72.852148
555.183198	1.412324	72.857153
554.147648	1.974944	72.862158
553.372305	2.548155	72.867162
552.721053	10.376392	72.872167
551.812368	5.952767	72.877172
551.271087	9.579653	72.882177
550.276203	11.178207	72.887182
549.791711	11.214634	72.892186
549.492873	8.281920	72.897191
549.272113	13.505734	72.902196
548.827791	5.373105	72.907201
547.674655	21.142745	72.912206
547.147903	10.837493	72.917210
546.369812	10.056484	72.922215
545.248872	16.125473	72.927220
544.852772	7.471053	72.932225
544.384430	6.620200	72.937230
543.097391	10.862650	72.942234
542.410747	20.940633	72.947239
541.866112	8.010916	72.952244
541.346186	-2.065167	72.957249
540.811200	12.539927	72.962254
540.721056	-0.365986	72.967258
539.841588	2.508918	72.972263
538.672516	5.347953	72.977268
538.723852	-3.120683	72.982273
538.046189	1.441023	72.987278
536.915717	4.081513	72.992282
535.964038	-3.840967	72.997287
535.497798	0.226569	73.002292
535.421178	-2.793583	73.007297
534.558674	9.138596	73.012302
533.802651	4.159204	73.017306
533.451315	-4.090735	73.022311
532.108237	5.878916	73.027316
531.295291	2.255368	73.032321
530.843572	4.798769	73.037326
530.363059	5.105813	73.042330
530.019263	8.377952	73.047335
528.505507	8.015358	73.052340
528.004519	-2.166245	73.057345
527.617939	10.158493	73.062350
527.302536	8.848021	73.067354
526.691847	0.645706	73.072359
525.602049	6.255556	73.077364
525.070216	-4.897304	73.082369
524.285563	3.212394	73.087374
523.897705	0.136166	73.092378
523.019719	-1.551476	73.097383
522.157139	6.274160	73.102388
521.658683	-2.750311	73.107393
521.152958	9.158149	73.112398
520.361162	1.475142	73.117402
519.385659	0.695629	73.122407
518.298769	1.987141	73.127412
518.589166	6.855118	73.132417
517.922838	8.027587	73.137422
517.620351	4.532464	73.142426
516.840021	3.677702	73.147431
515.809270	9.800144	73.152436
515.545312	-3.726226	73.157441
514.114530	3.052903	73.162446
513.568495	-0.766131	73.167450
512.656000	9.030849	73.172455
512.618326	8.992944	73.177460
512.625431	1.840280	73.182465
511.100102	10.006483	73.187470
510.792968	15.434879	73.192474
510.237569	-1.443538	73.197479
508.590810	-0.118022	73.202484
508.125722	-6.331248	73.207489
507.373942	6.029591	73.212494
506.856254	-4.138304	73.217498
506.693652	0.445434	73.222503
506.255955	3.554332	73.227508
505.762340	-2.802590	73.232513
504.280887	7.163888	73.237518
504.037775	-5.689257	73.242522
503.729751	2.970587	73.247527
502.332533	2.458549	73.252532
501.711909	-6.631608	73.257537
501.083110	7.203075	73.262542
500.957198	-5.995184	73.267546
499.974249	-5.817830	73.272551
498.695881	5.742200	73.277556
498.537967	-5.437107	73.282561
497.830296	7.091755	73.287566
497.531630	5.930015	73.292570
497.191902	-1.175274	73.297575
495.706032	8.807683	73.302580
495.408540	0.298426	73.307585
494.687072	0.915113	73.312590
494.025177	8.557390	73.317594
493.167317	5.168102	73.322599
492.372180	5.891149	73.327604
492.111511	-0.155940	73.332609
491.630905	15.989129	73.337614
490.882914	4.154745	73.342618
489.771990	-9.845398	73.347623
489.356535	5.496039	73.352628
489.136599	-3.396171	73.357633
487.912548	2.848542	73.362638
487.254475	5.987824	73.367642
486.819329	0.367520	73.372647
486.353588	2.072611	73.377652
485.177557	2.510979	73.382657
484.551882	3.050904	73.387662
483.984023	-0.360929	73.392666
483.780566	-1.988863	73.397671
482.894539	10.754510	73.402676
481.953652	-1.178448	73.407681
481.494813	4.343505	73.412686
481.079092	3.395968	73.417690
480.167309	-1.191141	73.422695
479.132257	1.330087	73.427700
478.776546	-1.314420	73.432705
478.283112	-0.978499	73.437710
478.063942	-1.709759	73.442714
477.016065	-3.275695	73.447719
476.130285	2.964015	73.452724
475.924641	-4.626275	73.457729
474.326969	2.247276	73.462734
473.773168	1.141961	73.467738
473.648173	3.324218	73.472743
472.860908	7.159050	73.477748
472.592223	8.979410	73.482753
471.257153	-0.963619	73.487758
470.610848	8.008758	73.492762
470.560931	4.236848	73.497767
469.757340	12.390584	73.502772
469.080073	0.757841	73.507777
468.204348	4.229862	73.512782
467.632480	8.853580	73.517786
467.264792	-5.335943	73.522791
466.046250	2.767205	73.527796
465.288705	0.667717	73.532801
464.614126	5.438692	73.537806
464.073932	2.361515	73.542810
464.060818	3.540310	73.547815
462.748833	0.873124	73.552820
462.234042	-1.656143	73.557825
461.605311	8.628668	73.562830
461.230003	6.630709	73.567834
460.307693	15.096690	73.572839
459.301124	11.857270	73.577844
458.758377	-3.427196	73.582849
458.188871	7.587800	73.587854
457.790466	2.813238	73.592858
457.448840	3.071357	73.597863
456.161998	4.527225	73.602868
456.071758	-0.086695	73.607873
454.943040	-0.944274	73.612878
454.083080	1.077536	73.617882
453.437761	-2.473339	73.622887
452.658831	6.252079	73.627892
452.640351	-1.161441	73.632897
452.289945	5.606429	73.637902
451.291725	3.433326	73.642906
450.697280	-0.370093	73.647911
449.903749	3.866306	73.652916
448.748969	-6.360909	73.657921
447.705136	2.390948	73.662926
447.458281	3.419322	73.667930
447.299720	-1.111167	73.672935
446.686332	8.947266	73.677940
446.559792	-4.457473	73.682945
445.239043	-0.405159	73.687950
444.735621	3.477497	73.692954
443.911369	7.239381	73.697959
442.989226	6.956041	73.702964
442.453940	5.861976	73.707969
441.937424	4.205078	73.712974
440.997444	-1.859918	73.717978
440.163910	1.753628	73.722983
439.248505	7.403535	73.727988
439.054783	4.753723	73.732993
438.535227	11.438159	73.737998
438.418776	1.341971	73.743002
437.630966	-4.840314	73.748007
436.703173	10.314675	73.753012
436.194535	-0.769312	73.758017
434.973810	6.102548	73.763022
433.997491	0.666267	73.768026
433.526924	15.527621	73.773031
433.357170	6.922322	73.778036
432.934787	-2.289293	73.783041
431.811754	5.251426	73.788046
431.181030	7.616778	73.793050
430.982868	7.995548	73.798055
429.937721	13.986269	73.803060
428.964860	12.034646	73.808065
428.042799	5.586736	73.813070
427.394060	-3.743355	73.818074
427.526920	6.658230	73.823079
426.818362	5.596510	73.828084
426.555178	3.552304	73.833089
425.347581	9.242468	73.838094
424.657155	6.116697	73.843098
424.311539	1.398389	73.848103
422.956499	4.468968	73.853108
422.541358	4.150578	73.858113
421.837706	8.699107	73.863118
421.359087	1.142861	73.868122
421.009194	-0.179446	73.873127
419.536254	10.033310	73.878132
419.395445	-2.765153	73.883137
418.986740	-3.529286	73.888142
418.300421	6.368876	73.893146
417.479169	3.967305	73.898151
416.637552	5.800117	73.903156
416.123398	-4.242150	73.908161
415.466377	4.635744	73.913166
414.448644	-2.864551	73.918170
413.799058	-4.000321	73.923175
413.062763	3.630169	73.928180
412.651139	2.983201	73.933185
412.494161	1.690080	73.938190
411.710901	4.942372	73.943194
410.940428	2.449129	73.948199
410.134102	12.177178	73.953204
409.751609	3.941691	73.958209
408.376055	5.492147	73.963214
407.717851	7.549634	73.968218
407.457276	0.990015	73.973223
406.514723	11.567707	73.978228
406.538607	-2.431877	73.983233
405.736253	-2.398387	73.988238
404.899992	1.955225	73.993242
404.710218	-2.267498	73.998247
403.376282	3.177868	74.003252
402.973426	-10.709546	74.008257
402.037022	-1.971642	74.013262
401.772261	3.401116	74.018266
400.910294	-1.558189	74.023271
399.827647	5.868870	74.028276
399.195863	-1.702386	74.033281
398.742864	5.914503	74.038286
398.471705	3.652365	74.043290
398.178969	-1.828177	74.048295
397.150883	4.696018	74.053300
396.688865	2.457989	74.058305
395.352214	4.705603	74.063310
394.209136	0.977015	74.068314
393.990097	3.967500	74.073319
393.327638	7.623187	74.078324
393.182299	7.922577	74.083329
392.759661	6.097759	74.088334
391.506501	8.210639	74.093338
391.231314	1.549267	74.098343
390.497675	9.053181	74.103348
389.878207	-7.824431	74.108353
388.427779	14.601901	74.113358
387.919662	4.861462	74.118362
387.651963	1.725108	74.123367
387.170742	12.533649	74.128372
386.790029	9.129864	74.133377
385.649135	1.581397	74.138382
385.077723	3.557245	74.143386
384.513548	11.288054	74.148391
383.559776	5.669998	74.153396
382.770474	4.086550	74.158401
382.063805	2.370081	74.163406
381.567288	4.810254	74.168410
381.393386	0.115053	74.173415
380.088023	-1.480770	74.178420
379.850890	-2.616029	74.183425
379.077519	-1.063751	74.188430
378.734469	3.507745	74.193434
377.697758	3.509205	74.198439
377.075702	7.976929	74.203444
376.727963	2.325374	74.208449
376.149401	6.522803	74.213454
374.950451	-2.694349	74.218458
374.485984	6.941373	74.223463
373.861217	7.490643	74.228468
373.273970	0.103116	74.233473
371.747241	2.822599	74.238478
371.084001	-0.225481	74.243482
371.142453	-4.079312	74.248487
370.374681	13.827316	74.253492
370.412888	-10.737398	74.258497
369.542376	2.503434	74.263502
368.607339	-4.103233	74.268506
367.833128	-1.183546	74.273511
367.504405	2.152441	74.278516
366.588862	-5.495007	74.283521
365.560324	2.073254	74.288526
364.866376	1.028149	74.293530
364.512283	1.337155	74.298535
363.944250	6.993226	74.303540
363.321086	2.710264	74.308545
362.982881	3.713779	74.313550
362.175811	2.614161	74.318554
361.302094	-0.258441	74.323559
360.060114	2.683760	74.328564
359.591217	-4.415104	74.333569
358.915423	9.791376	74.338574
358.716714	1.873555	74.343578
358.207475	-1.044518	74.348583
356.983127	11.746496	74.353588
356.478321	-4.687313	74.358593
356.285762	1.604379	74.363598
355.365746	3.944889	74.368602
354.542845	-3.431881	74.373607
353.693444	3.352444	74.378612
353.661674	-8.657524	74.383617
352.949481	1.320466	74.388622
351.958464	4.806168	74.393626
351.652988	-4.121269	74.398631
350.984614	9.424837	74.403636
350.048936	-8.397456	74.408641
349.090579	2.580171	74.413646
348.630958	4.386817	74.418650
348.444787	2.253073	74.423655
347.181524	0.480240	74.428660
346.353067	2.216356	74.433665
345.867403	5.120025	74.438670
345.337620	4.930312	74.443674
345.140598	-3.656427	74.448679
343.754758	-0.393235	74.453684
343.365476	-6.722583	74.458689
342.772770	-5.637500	74.463694
342.158969	-4.772991	74.468698
341.626256	-4.214731	74.473703
340.488593	6.196946	74.478708
339.841666	-3.387302	74.483713
339.623996	5.707596	74.488718
338.877256	-0.563203	74.493722
338.280686	0.834747	74.498727
337.461129	2.164154	74.503732
336.891209	-3.385743	74.508737
336.267157	1.292048	74.513742
335.226655	-5.471265	74.518746
334.721569	4.637730	74.523751
333.924838	5.455701	74.528756
333.620721	-4.850260	74.533761
333.260479	-3.147766	74.538766
331.912940	-4.508172	74.543770
331.543399	0.151131	74.548775
330.873039	-5.426911	74.553780
330.296782	-6.903942	74.558785
329.259836	-0.419315	74.563790
328.674263	-1.385485	74.568794
328.346398	-4.158988	74.573799
327.434105	2.854573	74.578804
327.164929	-10.858574	74.583809
325.828340	2.224734	74.588814
325.091303	3.028462	74.593818
325.058428	-5.436196	74.598823
324.301187	-3.719310	74.603828
324.051771	-7.137699	74.608833
322.894538	-3.365287	74.613838
322.136886	-0.388300	74.618842
321.703687	-2.585172	74.623847
321.284958	-1.332265	74.628852
320.361823	-10.618575	74.633857
319.643331	2.976520	74.638862
319.109427	2.377445	74.643866
318.392661	-0.867099	74.648871
317.539570	5.659194	74.653876
317.223540	-10.673790	74.658881
316.610502	-3.364139	74.663886
315.207494	-2.734964	74.668890
314.799215	-1.813317	74.673895
314.076067	2.788807	74.678900
313.641957	-7.270914	74.683905
313.703875	-3.416849	74.688910
312.278658	-2.506578	74.693914
311.616309	-9.558820	74.698919
311.039640	-2.862115	74.703924
310.795137	-2.548492	74.708929
309.268604	-8.970957	74.713934
308.789015	-3.934552	74.718938
308.283443	-15.217677	74.723943
307.912623	3.232821	74.728948
307.457277	-9.892383	74.733953
306.581974	-0.547578	74.738958
306.088927	-4.807105	74.743962
305.276259	-11.765995	74.748967
303.987457	-6.412937	74.753972
303.439033	-2.862145	74.758977
302.872144	-8.456670	74.763982
302.151571	2.859974	74.768986
302.150534	-9.902389	74.773991
300.895357	-7.808070	74.778996
300.279690	-8.780474	74.784001
299.607022	-4.440295	74.789006
299.102083	-1.161372	74.794010
299.044790	-12.837663	74.799015
298.197141	-3.855249	74.804020
297.506346	-9.776964	74.809025
296.510248	-0.458635	74.814030
295.587847	-5.651122	74.819034
294.564950	-6.443490	74.824039
294.176732	5.630764	74.829044
293.615794	-5.209860	74.834049
293.159529	-8.205749	74.839054
293.003597	-7.160315	74.844058
292.476246	-3.917244	74.849063
291.130793	0.214781	74.854068
290.487453	-5.783886	74.859073
290.118571	-6.902864	74.864078
289.204695	-3.292238	74.869082
288.611149	-9.240491	74.874087
288.067043	-0.383732	74.879092
287.301735	-10.881099	74.884097
286.514119	1.293089	74.889102
285.624281	0.072645	74.894106
285.354016	-10.005300	74.899111
284.613356	-4.618180	74.904116
283.952566	-0.833421	74.909121
283.103708	-1.014837	74.914126
282.334019	-7.305608	74.919130
282.315264	-6.832419	74.924135
281.406881	-2.803179	74.929140
280.802908	1.530787	74.934145
279.789508	-8.532777	74.939150
279.289337	5.573169	74.944154
279.382456	-5.081542	74.949159
277.722916	-4.318408	74.954164
276.884412	-2.187992	74.959169
276.533705	-4.188262	74.964174
276.216479	0.000642	74.969178
275.679647	-0.851855	74.974183
274.472109	-0.044074	74.979188
274.100521	-11.845309	74.984193
273.515738	-3.751649	74.989198
272.797138	-6.945420	74.994202
271.960832	-6.244128	74.999207
271.081051	1.568544	75.004212
271.026440	-9.201391	75.009217
270.375147	-11.664694	75.014222
269.169174	-5.115254	75.019226
268.385809	-7.267333	75.024231
267.820218	-0.996603	75.029236
267.714223	-8.142253	75.034241
267.451540	-2.433917	75.039246
265.945024	-1.330880	75.044250
265.503447	-9.738261	75.049255
264.928911	-3.505531	75.054260
264.057577	-5.331336	75.059265
263.055550	-3.982279	75.064270
262.610663	-12.308702	75.069274
262.387355	-11.809212	75.074279
261.509520	-1.904153	75.079284
261.179652	-6.963995	75.084289
260.286226	-3.115336	75.089294
259.790279	-3.961731	75.094298
259.151740	-12.060155	75.099303
257.817980	-2.260616	75.104308
257.271510	-16.235474	75.109313
256.856167	-0.637009	75.114318
256.180602	-8.901426	75.119322
256.227371	-15.536817	75.124327
254.840130	-5.690904	75.129332
254.235861	-11.246337	75.134337
253.857449	-5.199419	75.139342
252.693308	-3.048622	75.144346
252.132831	-7.521321	75.149351
251.395254	1.508218	75.154356
251.305364	-7.131853	75.159361
250.453633	-0.176812	75.164366
249.368616	1.505615	75.169370
248.903874	-1.408486	75.174375
248.370210	-1.331044	75.179380
247.702733	1.716748	75.184385
246.687891	2.254116	75.189390
245.720252	-0.680740	75.194394
245.625320	-3.532367	75.199399
245.286835	3.287234	75.204404
244.876350	-3.883991	75.209409
243.769030	1.353429	75.214414
242.887891	4.075726	75.219418
242.426137	-7.662242	75.224423
241.484425	4.591720	75.229428
240.866509	-8.646322	75.234433
240.289811	1.638105	75.239438
239.617827	-6.980129	75.244442
239.579127	-2.252132	75.249447
238.292756	-0.261621	75.254452
237.378473	-3.548769	75.259457
236.839204	-2.331827	75.264462
236.390739	-4.486822	75.269466
236.242010	-0.649643	75.274471
234.946372	6.152240	75.279476
234.333991	-4.911983	75.284481
233.893047	6.287552	75.289486
233.229108	-7.668578	75.294490
232.075838	-7.498657	75.299495
231.502333	1.714471	75.304500
231.292612	-5.927168	75.309505
230.568555	5.050987	75.314510
229.842441	-11.150355	75.319514
229.276258	-8.688012	75.324519
228.391795	3.541055	75.329524
227.740507	-6.660642	75.334529
227.556436	4.357583	75.339534
226.002033	-0.472331	75.344538
225.853736	-14.589511	75.349543
225.008040	-2.932776	75.354548
224.854304	-6.951477	75.359553
223.901989	-8.133551	75.364558
223.072071	3.134305	75.369562
222.400424	-4.627659	75.374567
222.010440	-6.268407	75.379572
221.351447	-1.655989	75.384577
220.576995	-3.290635	75.389582
220.068965	-2.925526	75.394586
219.823474	-1.484172	75.399591
218.332619	2.041844	75.404596
217.389420	0.102930	75.409601
216.858332	-1.061141	75.414606
216.437370	-4.592519	75.419610
216.348301	-11.966372	75.424615
215.346841	-4.140596	75.429620
214.879621	-14.873120	75.434625
214.137520	-4.250073	75.439630
213.398456	-2.550246	75.444634
212.382600	-1.325125	75.449639
211.808353	-1.376827	75.454644
211.541956	-7.810895	75.459649
211.006664	-3.189811	75.464654
209.962750	-2.091107	75.469658
209.365084	-8.689985	75.474663
208.809606	1.177885	75.479668
208.168632	-12.140046	75.484673
206.980189	-4.729173	75.489678
206.422260	2.683681	75.494682
206.039461	-7.300608	75.499687
205.385576	-1.654481	75.504692
205.066043	1.331537	75.509697
203.876047	-3.703124	75.514702
203.070573	3.481107	75.519706
202.947717	-4.005637	75.524711
201.952137	7.425840	75.529716
201.106891	-2.399559	75.534721
200.367884	1.795098	75.539726
199.779046	-3.277061	75.544730
199.731353	3.964552	75.549735
199.136790	-0.466428	75.554740
198.340377	-8.821946	75.559745
197.272406	0.432176	75.564750
196.688917	-0.356091	75.569754
196.831865	-0.646726	75.574759
195.054744	-4.450742	75.579764
194.809856	2.327130	75.584769
194.258073	-5.061260	75.589774
193.398061	4.468803	75.594778
192.531897	-3.875594	75.599783
191.798654	0.311838	75.604788
191.332015	-2.521521	75.609793
190.992064	7.958567	75.614798
190.305079	4.512188	75.619802
189.540614	-0.855254	75.624807
188.513845	2.336576	75.629812
188.360729	-8.739352	75.634817
188.055310	-1.729472	75.639822
186.887124	4.310914	75.644826
186.244929	6.604032	75.649831
185.449686	5.863724	75.654836
185.001325	-6.701139	75.659841
184.008331	-3.317568	75.664846
183.070025	0.675474	75.669850
183.067618	-3.197036	75.674855
182.323356	-6.967026	75.679860
182.052136	-5.385944	75.684865
180.885836	13.330177	75.689870
180.184882	1.453737	75.694874
179.851405	-7.108059	75.699879
179.065368	-8.138425	75.704884
178.099566	-1.379650	75.709889
177.454239	-0.461187	75.714894
176.704944	5.914549	75.719898
176.816880	-8.001261	75.724903
175.382274	2.503552	75.729908
174.968354	-7.792746	75.734913
174.061476	-4.960664	75.739918
173.974871	3.760081	75.744922
173.257747	-5.197874	75.749927
172.165767	-1.921522	75.754932
171.842308	-8.322829	75.759937
171.293623	-2.953676	75.764942
170.336645	-3.299168	75.769946
169.822216	-6.552271	75.774951
169.284352	-3.966692	75.779956
168.666513	-6.925751	75.784961
167.285135	-4.615693	75.789966
166.888346	4.913056	75.794970
166.769712	-12.008041	75.799975
165.783361	-3.653206	75.804980
164.857651	-12.992647	75.809985
164.127398	-1.365346	75.814990
163.548158	2.132038	75.819994
163.317441	-4.440181	75.824999
162.453730	-1.372118	75.830004
161.600638	-10.059217	75.835009
160.746951	0.706220	75.840014
160.225199	-6.231191	75.845018
160.202717	-9.354570	75.850023
158.990145	-5.546454	75.855028
158.234751	-5.846812	75.860033
157.805111	5.283111	75.865038
157.155175	0.969787	75.870042
157.087998	-6.749764	75.875047
155.918330	1.938673	75.880052
155.160801	-8.698657	75.885057
154.620066	8.214540	75.890062
153.837300	4.302457	75.895066
153.042149	-12.357788	75.900071
152.314211	-2.907130	75.905076
152.001181	-2.785999	75.910081
151.686440	-2.543164	75.915086
150.451017	-8.499411	75.920090
149.938835	-7.006062	75.925095
149.236165	-9.238778	75.930100
148.675438	0.298764	75.935105
147.490433	3.285598	75.940110
146.850450	1.273128	75.945114
146.610768	-3.414706	75.950119
146.116798	6.351900	75.955124
145.512122	-3.410906	75.960129
144.487380	2.158751	75.965134
143.830946	-2.099914	75.970138
143.503486	6.317027	75.975143
142.770697	3.417307	75.980148
141.724425	-3.475882	75.985153
141.007664	-2.216422	75.990158
140.504822	4.336071	75.995162
140.472043	2.606835	76.000167
139.289397	-0.344154	76.005172
138.549762	-5.196698	76.010177
138.061825	-3.290882	76.015182
137.440231	0.892953	76.020186
137.104852	-3.388521	76.025191
135.827280	5.899051	76.030196
135.246453	-2.848806	76.035201
134.754701	-3.796772	76.040206
134.047062	-0.234751	76.045210
133.145652	-8.980367	76.050215
132.540230	-1.455848	76.055220
132.007576	4.582565	76.060225
132.009292	-6.150601	76.065230
130.463401	-0.586145	76.070234
129.973533	-3.127192	76.075239
129.100198	6.810305	76.080244
129.189416	-8.581114	76.085249
128.063005	-4.509171	76.090254
126.964921	-1.938327	76.095258
126.595909	-20.724506	76.100263
126.048100	-2.193758	76.105268
125.460785	-6.608523	76.110273
125.173613	0.775357	76.115278
124.030757	-2.317592	76.120282
123.910431	-6.726401	76.125287
122.686339	-13.398822	76.130292
121.891660	-8.247486	76.135297
121.385977	-12.113851	76.140302
120.670872	-11.346678	76.145306
120.391988	-10.325784	76.150311
119.517980	-7.308107	76.155316
118.548847	-4.749940	76.160321
117.811997	-8.087411	76.165326
117.153097	-3.470255	76.170330
117.128897	-2.124109	76.175335
116.703942	2.102490	76.180340
115.570924	-7.139213	76.185345
114.764370	-11.738214	76.190350
113.923603	-4.657149	76.195354
114.071555	-6.479864	76.200359
112.758496	3.146124	76.205364
111.948501	-13.516462	76.210369
111.526396	-9.257202	76.215374
110.963585	1.818263	76.220378
110.547320	-10.182391	76.225383
109.391498	-6.419575	76.230388
109.051309	-7.631411	76.235393
108.734325	-11.251889	76.240398
107.345696	-1.973409	76.245402
106.548955	-10.245254	76.250407
106.291357	1.201020	76.255412
105.644115	-5.582315	76.260417
105.270643	-1.453815	76.265422
104.025495	-3.770320	76.270426
103.460624	-8.062497	76.275431
102.726459	3.191691	76.280436
102.658463	-3.860649	76.285441
102.082298	-7.714192	76.290446
100.780910	-6.329944	76.295450
100.400892	-13.887624	76.300455
99.966596	-0.370942	76.305460
98.690230	-7.211641	76.310465
98.037204	-8.882958	76.315470
97.297208	-1.723338	76.320474
97.141891	-8.682898	76.325479
96.581641	-1.397397	76.330484
96.018582	-5.298763	76.335489
95.189777	-6.279701	76.340494
94.422279	-5.617709	76.345498
94.013879	-10.303857	76.350503
92.831915	-3.786558	76.355508
92.379527	-1.742895	76.360513
91.944493	-8.694115	76.365518
91.113912	1.701787	76.370522
89.991687	-4.412833	76.375527
89.478428	-1.561495	76.380532
89.024620	-5.999119	76.385537
88.734040	-5.690741	76.390542
87.943393	1.065361	76.395546
87.161963	-7.372929	76.400551
86.116250	-9.516220	76.405556
85.603143	-10.579044	76.410561
85.452196	-9.310459	76.415566
84.590786	-1.565326	76.420570
83.879617	-3.995370	76.425575
83.148316	-4.334241	76.430580
82.838505	-6.993884	76.435585
81.999898	-6.591793	76.440590
81.152500	-7.688036	76.445594
80.865137	-3.581153	76.450599
80.246189	-7.334823	76.455604
79.210301	-6.986424	76.460609
78.531666	-4.305834	76.465614
78.059220	3.490812	76.470618
77.506847	-9.689806	76.475623
76.171582	-4.182568	76.480628
75.704783	1.247661	76.485633
75.264709	-12.810335	76.490638
74.759751	-2.682417	76.495642
73.829219	-3.765399	76.500647
72.870439	-7.748727	76.505652
72.564454	-5.050297	76.510657
71.976735	-15.292031	76.515662
71.332063	-10.893186	76.520666
70.246510	-11.787431	76.525671
69.703498	-2.038233	76.530676
69.188486	-7.532150	76.535681
68.737335	-7.243893	76.540686
68.395105	0.970393	76.545690
67.505238	-6.067556	76.550695
66.739172	9.340845	76.555700
66.410163	-2.468706	76.560705
65.425342	0.964071	76.565710
63.840434	3.174180	76.570714
63.794810	-5.624320	76.575719
63.009305	4.679243	76.580724
62.742436	6.206025	76.585729
62.587807	3.209385	76.590734
61.582451	1.972756	76.595738
60.986842	-6.124564	76.600743
60.088035	1.694354	76.605748
59.127042	-2.495206	76.610753
58.487010	-1.326812	76.615758
57.704084	10.056597	76.620762
57.384430	-6.012373	76.625767
57.076470	-0.266842	76.630772
56.409389	-3.807817	76.635777
55.550991	-5.287087	76.640782
54.821287	-4.107544	76.645786
54.085043	2.046934	76.650791
53.014213	-3.651649	76.655796
52.621744	-5.725648	76.660801
52.412436	-8.618943	76.665806
51.692838	3.214847	76.670810
50.722133	-0.990507	76.675815
49.803087	3.008970	76.680820
49.466999	0.754084	76.685825
49.167995	-0.868028	76.690830
48.262757	1.989069	76.695834
47.663615	-0.665422	76.700839
46.761500	-0.052909	76.705844
46.230184	-6.648125	76.710849
45.585124	0.994700	76.715854
44.341731	1.177508	76.720858
44.248282	-0.611437	76.725863
43.672672	3.103019	76.730868
43.107426	3.467829	76.735873
42.198540	2.034465	76.740878
41.399036	6.563678	76.745882
41.053205	0.575985	76.750887
40.369682	1.071630	76.755892
39.347857	-2.133625	76.760897
38.569485	0.047202	76.765902
37.861161	-0.150235	76.770906
37.811968	-12.171567	76.775911
37.317439	-0.343715	76.780916
36.245416	-7.737384	76.785921
35.245003	-5.049612	76.790926
34.920106	-5.678806	76.795930
35.103880	-6.327635	76.800935
33.569115	-2.977443	76.805940
33.067225	-8.381976	76.810945
32.712205	-4.119212	76.815950
31.835975	-1.818691	76.820954
30.850321	-7.857289	76.825959
29.860795	-1.843762	76.830964
29.691355	-0.867124	76.835969
29.235940	-8.737627	76.840974
28.355477	-8.634781	76.845978
27.240252	-15.917467	76.850983
26.839670	-4.350616	76.855988
26.675696	-9.179822	76.860993
26.203088	-10.745851	76.865998
24.648684	1.517583	76.871002
24.163081	-7.516669	76.876007
23.899180	-7.900115	76.881012
23.240166	0.050879	76.886017
22.323191	1.197224	76.891022
21.314973	-0.187170	76.896026
21.211618	-0.526837	76.901031
20.490642	-2.409652	76.906036
20.055049	-5.687909	76.911041
19.058169	0.473457	76.916046
17.810025	-2.888081	76.921050
17.686292	-6.925739	76.926055
17.178841	-1.343933	76.931060
16.669445	1.014776	76.936065
15.955601	-2.993407	76.941070
15.059888	-1.880414	76.946074
15.031865	-0.270298	76.951079
13.640191	2.725909	76.956084
12.765945	-15.079169	76.961089
12.216600	-8.971847	76.966094
11.818500	2.605653	76.971098
11.875797	-5.272515	76.976103
10.468499	0.452835	76.981108
9.928305	-3.586200	76.986113
9.454129	3.488459	76.991118
8.301528	3.678881	76.996122
7.339890	-6.380182	77.001127
6.704235	4.580756	77.006132
6.399781	5.187835	77.011137
5.886282	-2.228683	77.016142
5.741276	7.460192	77.021147
4.647465	-1.112745	77.026151
4.006093	-1.227810	77.031156
3.544409	-4.405704	77.036161