Fri Mar 05 18:01:24 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.723719	92.827819	0.000000
-1.902671	91.126642	0.005005
-2.230489	60.662448	0.010010
-3.697278	17.677228	0.015014
-7.194873	-16.070694	0.020019
-12.296999	-24.545053	0.025024
-18.319301	-19.819773	0.030029
-23.041423	-24.505271	0.035034
-27.074777	-25.824931	0.040038
-31.174852	-13.502347	0.045043
-34.340036	-26.490737	0.050048
-38.280941	-20.499173	0.055053
-41.526759	-20.903630	0.060058
-45.137783	-18.283480	0.065062
-49.349046	-18.078147	0.070067
-52.851526	-20.401851	0.075072
-56.669710	-14.424317	0.080077
-60.293049	-19.676142	0.085082
-64.334339	-19.619330	0.090086
-67.940857	-19.198204	0.095091
-71.503251	-26.255147	0.100096
-75.832445	-13.923536	0.105101
-79.586306	-26.683890	0.110106
-83.402807	-19.638957	0.115110
-87.214620	-21.999990	0.120115
-89.896730	-32.071438	0.125120
-93.842649	-20.954531	0.130125
-97.939366	-30.380774	0.135130
-101.671540	-28.184348	0.140134
-105.951590	-24.695668	0.145139
-109.501167	-29.907142	0.150144
-113.593822	-16.393406	0.155149
-117.041874	-19.703441	0.160154
-120.966372	-16.399205	0.165158
-125.101277	-17.281438	0.170163
-128.196968	-21.196479	0.175168
-132.075287	-21.999791	0.180173
-135.804348	-21.847600	0.185178
-139.259682	-23.125265	0.190182
-143.567272	-20.491588	0.195187
-146.834667	-20.113422	0.200192
-150.853723	-18.968731	0.205197
-154.764629	-21.197144	0.210202
-158.461972	-23.754531	0.215206
-162.319619	-16.326009	0.220211
-165.681356	-25.211818	0.225216
-169.534945	-22.382460	0.230221
-173.250641	-19.942543	0.235226
-177.274756	-22.261664	0.240230
-181.102601	-17.247523	0.245235
-184.611376	-22.083763	0.250240
-188.749839	-26.926734	0.255245
-192.035272	-30.833482	0.260250
-195.793742	-31.673166	0.265254
-199.743819	-24.335498	0.270259
-203.335807	-28.084491	0.275264
-207.536595	-21.438521	0.280269
-211.516507	-25.071970	0.285274
-214.683515	-22.672255	0.290278
-218.611774	-24.129795	0.295283
-222.095626	-25.793883	0.300288
-226.066693	-13.824333	0.305293
-229.800339	-22.478794	0.310298
-233.137568	-21.554763	0.315302
-237.566828	-18.551407	0.320307
-241.088889	-28.121159	0.325312
-244.818356	-20.288762	0.330317
-248.549136	-16.469604	0.335322
-252.473628	-22.124079	0.340326
-256.247590	-16.629554	0.345331
-259.824666	-24.651349	0.350336
-263.833138	-14.684864	0.355341
-267.439863	-14.438453	0.360346
-271.100963	-20.368338	0.365350
-275.246046	-20.974289	0.370355
-278.745749	-23.485764	0.375360
-282.754178	-18.882621	0.380365
-286.251287	-22.561477	0.385370
-290.035065	-22.920720	0.390374
-293.797496	-24.664813	0.395379
-297.214229	-24.038670	0.400384
-301.337274	-14.922760	0.405389
-305.296035	-26.654146	0.410394
-308.833533	-23.666868	0.415398
-312.739155	-10.878133	0.420403
-316.158157	-22.090108	0.425408
-320.071969	-11.346995	0.430413
-323.808124	-23.288936	0.435418
-327.443418	-31.484256	0.440422
-331.584886	-16.435859	0.445427
-335.142907	-31.787292	0.450432
-339.387815	-18.505949	0.455437
-343.165718	-30.403338	0.460442
-346.304792	-32.344647	0.465446
-350.252177	-28.495484	0.470451
-353.851835	-25.558143	0.475456
-357.522318	-19.822938	0.480461
-361.466164	-23.293153	0.485466
-365.425683	-26.232564	0.490470
-369.548713	-22.558756	0.495475
-372.826085	-34.386197	0.500480
-376.717819	-28.716567	0.505485
-380.220516	-25.107100	0.510490
-384.059064	-25.832773	0.515494
-388.047237	-21.265811	0.520499
-391.250639	-34.918579	0.525504
-395.241175	-27.673496	0.530509
-399.189125	-28.149856	0.535514
-402.582072	-24.994710	0.540518
-406.693043	-25.534915	0.545523
-410.387876	-39.768356	0.550528
-414.359879	-22.810352	0.555533
-417.922235	-24.529426	0.560538
-421.694665	-30.247317	0.565542
-425.811546	-20.933492	0.570547
-429.282086	-21.011369	0.575552
-433.061645	-28.973741	0.580557
-436.874927	-27.516075	0.585562
-440.465197	-30.320358	0.590566
-444.629064	-20.300391	0.595571
-447.831562	-27.091728	0.600576
-451.363427	-25.658481	0.605581
-455.455342	-28.168154	0.610586
-459.091465	-23.482257	0.615590
-463.275003	-24.600569	0.620595
-467.128771	-21.993069	0.625600
-471.021419	-14.437056	0.630605
-474.904507	-21.192198	0.635610
-477.990354	-31.394231	0.640614
-481.593572	-22.728499	0.645619
-485.180965	-25.591522	0.650624
-489.325787	-21.387316	0.655629
-493.388758	-26.609241	0.660634
-497.039619	-23.841710	0.665638
-501.112830	-23.028415	0.670643
-504.068884	-29.709220	0.675648
-507.847009	-10.772945	0.680653
-511.834354	-20.260070	0.685658
-515.904097	-24.011118	0.690662
-519.669288	-22.930018	0.695667
-523.272444	-28.624317	0.700672
-526.839305	-21.528702	0.705677
-530.596615	-22.079453	0.710682
-534.723775	-25.259887	0.715686
-538.615503	-19.769777	0.720691
-542.406988	-30.738960	0.725696
-545.864658	-21.083958	0.730701
-549.694689	-24.971013	0.735706
-553.817339	-26.701302	0.740710
-557.246035	-15.005552	0.745715
-560.645504	-25.330841	0.750720
-564.636999	-18.728743	0.755725
-568.414902	-28.241335	0.760730
-572.133391	-32.953589	0.765734
-576.232974	-16.940074	0.770739
-579.642002	-30.474556	0.775744
-583.368147	-29.252934	0.780749
-587.236167	-24.321636	0.785754
-590.730221	-22.902111	0.790758
-594.831107	-21.245276	0.795763
-598.476180	-24.220337	0.800768
-602.533161	-22.354456	0.805773
-606.216517	-27.220508	0.810778
-609.591576	-29.595279	0.815782
-613.479484	-20.398160	0.820787
-617.113888	-22.778795	0.825792
-621.149802	-29.842008	0.830797
-625.042260	-32.892619	0.835802
-628.418401	-27.979925	0.840806
-632.690390	-18.409161	0.845811
-636.132350	-27.740346	0.850816
-639.827288	-24.686429	0.855821
-643.789780	-21.531406	0.860826
-647.438366	-18.352417	0.865830
-651.470164	-13.038445	0.870835
-654.846774	-26.041815	0.875840
-658.630465	-22.847528	0.880845
-662.478056	-23.400989	0.885850
-665.952029	-24.805796	0.890854
-669.993276	-22.738883	0.895859
-673.860088	-26.829593	0.900864
-677.418316	-27.861365	0.905869
-681.524090	-20.837108	0.910874
-685.086757	-25.881595	0.915878
-688.956243	-19.103248	0.920883
-692.555923	-25.485403	0.925888
-696.256662	-23.513864	0.930893
-700.237077	-27.461793	0.935898
-703.882077	-24.879394	0.940902
-707.661710	-31.828864	0.945907
-711.510383	-28.559454	0.950912
-715.215803	-22.368695	0.955917
-718.752159	-16.771087	0.960922
-722.293423	-28.148967	0.965926
-726.573483	-28.732555	0.970931
-730.201617	-24.809218	0.975936
-734.135076	-20.986890	0.980941
-737.894135	-33.227237	0.985946
-741.359405	-26.369910	0.990950
-745.320663	-11.838525	0.995955
-748.937702	-22.710657	1.000960
-752.696246	-24.036734	1.005965
-756.444011	-26.799586	1.010970
-760.217891	-24.201233	1.015974
-764.294020	-13.970828	1.020979
-767.985692	-23.889536	1.025984
-772.015962	-23.860096	1.030989
-775.205592	-14.731758	1.035994
-778.753241	-19.021548	1.040998
-782.620617	-24.744167	1.046003
-786.583806	-29.940518	1.051008
-790.483484	-29.321627	1.056013
-794.343469	-26.080239	1.061018
-797.725417	-22.937337	1.066022
-801.749224	-23.944960	1.071027
-805.361321	-19.068419	1.076032
-809.179584	-8.432872	1.081037
-812.892364	-18.797575	1.086042
-816.269342	-23.682303	1.091046
-820.914038	-14.337069	1.096051
-824.368573	-20.406321	1.101056
-828.236718	-13.096523	1.106061
-831.854279	-19.685338	1.111066
-835.125846	-13.010232	1.116070
-839.423406	-20.726682	1.121075
-842.965238	-20.138105	1.126080
-846.615257	-19.860239	1.131085
-850.645451	-32.208434	1.136090
-853.862887	-22.197177	1.141094
-858.160178	-17.114814	1.146099
-861.773300	-18.128067	1.151104
-865.622956	-18.750253	1.156109
-869.338475	-27.423887	1.161114
-873.023122	-28.748968	1.166118
-876.961562	-25.570599	1.171123
-880.680451	-27.421637	1.176128
-884.459646	-17.449832	1.181133
-888.035391	-27.385294	1.186138
-892.014375	-29.533778	1.191142
-895.937151	-25.917903	1.196147
-899.529365	-27.587311	1.201152
-903.389869	-14.981527	1.206157
-906.800394	-16.970143	1.211162
-910.515947	-25.030257	1.216166
-914.759087	-13.333115	1.221171
-918.086831	-25.047601	1.226176
-922.151886	-24.116614	1.231181
-925.899988	-30.004717	1.236186
-929.426128	-22.646950	1.241190
-933.345992	-22.956593	1.246195
-937.132193	-36.824428	1.251200
-940.885745	-19.088421	1.256205
-944.604858	-28.852626	1.261210
-948.263914	-30.165910	1.266214
-952.059649	-24.021854	1.271219
-955.530471	-27.087295	1.276224
-960.031091	-22.595145	1.281229
-964.073754	-16.829479	1.286234
-966.908550	-24.689724	1.291238
-970.993238	-13.749548	1.296243
-974.574759	-19.888148	1.301248
-978.157809	-26.012302	1.306253
-982.075372	-17.767095	1.311258
-986.052967	-17.641630	1.316262
-990.244091	-18.521240	1.321267
-993.499137	-22.256659	1.326272
-996.732286	-19.837456	1.331277
-1000.545467	-18.189665	1.336282
-1004.805412	-14.548069	1.341286
-1008.992315	-6.198232	1.346291
-1012.761309	-23.173781	1.351296
-1015.993956	-18.333963	1.356301
-1019.487577	-21.004570	1.361306
-1023.350830	-30.674620	1.366310
-1027.589969	-15.768772	1.371315
-1031.273322	-18.356973	1.376320
-1035.182967	-12.322299	1.381325
-1038.998988	-15.676182	1.386330
-1041.900459	-26.580279	1.391334
-1046.547700	-26.869577	1.396339
-1049.761425	-27.372403	1.401344
-1053.399659	-26.326533	1.406349
-1057.387910	-17.748194	1.411354
-1061.214120	-30.385677	1.416358
-1065.118139	-19.253476	1.421363
-1068.661719	-25.036862	1.426368
-1072.922665	-18.920700	1.431373
-1076.656702	-17.447876	1.436378
-1079.791267	-16.750625	1.441382
-1083.866433	-20.957124	1.446387
-1087.188339	-26.334388	1.451392
-1091.286648	-29.403319	1.456397
-1094.864429	-26.350097	1.461402
-1098.570507	-28.319529	1.466406
-1102.797946	-12.708938	1.471411
-1106.186849	-28.463033	1.476416
-1110.104884	-27.086878	1.481421
-1113.865178	-25.817955	1.486426
-1117.462253	-31.751978	1.491430
-1121.188138	-24.757802	1.496435
-1125.127515	-28.298386	1.501440
-1129.146242	-17.918875	1.506445
-1133.365092	-27.265330	1.511450
-1136.327043	-26.530965	1.516454
-1140.383234	-18.829462	1.521459
-1143.746103	-33.359188	1.526464
-1147.458293	-28.827253	1.531469
-1151.485254	-22.048212	1.536474
-1155.415030	-27.712895	1.541478
-1159.341867	-13.172193	1.546483
-1162.575545	-26.897804	1.551488
-1166.214453	-17.548850	1.556493
-1170.221025	-28.536143	1.561498
-1173.782778	-29.307966	1.566502
-1177.886612	-14.923421	1.571507
-1181.509300	-25.823886	1.576512
-1185.513399	-25.149781	1.581517
-1189.396745	-15.162425	1.586522
-1192.709709	-21.384649	1.591526
-1196.851729	-15.512806	1.596531
-1200.418532	-23.414882	1.601536
-1204.011243	-22.495913	1.606541
-1207.685046	-20.884283	1.611546
-1211.568409	-20.863400	1.616550
-1215.640192	-22.632192	1.621555
-1219.200210	-36.351215	1.626560
-1222.912304	-24.987708	1.631565
-1226.653914	-29.895465	1.636570
-1230.244971	-26.696410	1.641574
-1234.359391	-26.559662	1.646579
-1237.972983	-26.801108	1.651584
-1241.975064	-26.508858	1.656589
-1245.877528	-25.321050	1.661594
-1248.892022	-22.969614	1.666598
-1253.238623	-17.422906	1.671603
-1256.605141	-28.036231	1.676608
-1260.322056	-15.063373	1.681613
-1264.336947	-24.869582	1.686618
-1267.919150	-27.369507	1.691622
-1271.786972	-22.448186	1.696627
-1275.618512	-28.308156	1.701632
-1279.694711	-19.071974	1.706637
-1283.405203	-8.700541	1.711642
-1286.632055	-20.670304	1.716646
-1290.568058	-25.278755	1.721651
-1294.273845	-30.114861	1.726656
-1298.375885	-18.718783	1.731661
-1302.035247	-22.655548	1.736666
-1305.173877	-22.119771	1.741670
-1309.130895	-22.131090	1.746675
-1313.110400	-29.441783	1.751680
-1317.126473	-23.936831	1.756685
-1320.995752	-19.439403	1.761690
-1324.513505	-31.625886	1.766694
-1328.457639	-19.696788	1.771699
-1331.874158	-32.194359	1.776704
-1335.545784	-30.754768	1.781709
-1339.631489	-12.771048	1.786714
-1343.243386	-31.838553	1.791718
-1346.854417	-16.625867	1.796723
-1350.698540	-28.102462	1.801728
-1354.942411	-32.439157	1.806733
-1358.434990	-19.032134	1.811738
-1362.079370	-25.946953	1.816742
-1366.124134	-24.723546	1.821747
-1369.678696	-33.002621	1.826752
-1373.546632	-29.341121	1.831757
-1377.078419	-19.280445	1.836762
-1380.651174	-30.070292	1.841766
-1384.298904	-28.498829	1.846771
-1388.164100	-23.429504	1.851776
-1391.830253	-25.378043	1.856781
-1395.869687	-27.132768	1.861786
-1399.671787	-26.744528	1.866790
-1403.701239	-32.252461	1.871795
-1407.432843	-35.724890	1.876800
-1411.051095	-34.907169	1.881805
-1414.999781	-31.560683	1.886810
-1418.440631	-28.087344	1.891814
-1422.361953	-26.774793	1.896819
-1426.260520	-25.563652	1.901824
-1429.998829	-30.083660	1.906829
-1433.533043	-26.182181	1.911834
-1437.114724	-38.129574	1.916838
-1441.329579	-21.001820	1.921843
-1444.979935	-31.126264	1.926848
-1448.361161	-31.291046	1.931853
-1452.441059	-36.160021	1.936858
-1455.951674	-32.882039	1.941862
-1460.022476	-34.068646	1.946867
-1463.462243	-32.826833	1.951872
-1467.429698	-26.649738	1.956877
-1471.358430	-25.242876	1.961882
-1474.883277	-31.345582	1.966886
-1478.697442	-24.954893	1.971891
-1482.106239	-23.484619	1.976896
-1486.303582	-22.083601	1.981901
-1490.136312	-21.218791	1.986906
-1493.766587	-30.340258	1.991910
-1497.529799	-23.397873	1.996915
-1501.573875	-31.989248	2.006912
-1502.180364	-27.099353	2.016909
-1499.843445	-21.534509	2.026906
-1496.969922	-19.935188	2.036902
-1494.808474	-19.661864	2.046899
-1492.941044	-21.141504	2.056896
-1490.957437	-28.729925	2.066893
-1489.215152	-14.053784	2.076890
-1487.440970	-20.781273	2.086886
-1485.367654	-26.056620	2.096883
-1483.527117	-22.022837	2.106880
-1481.388006	-25.447085	2.116877
-1479.750926	-29.615166	2.126874
-1477.812555	-24.577017	2.136870
-1475.880736	-23.010023	2.146867
-1473.811794	-27.485689	2.156864
-1471.875480	-26.525745	2.166861
-1470.486279	-27.742461	2.176858
-1468.473241	-21.942553	2.186854
-1466.410133	-23.507193	2.196851
-1464.358914	-20.452950	2.206848
-1462.572106	-27.452449	2.216845
-1460.872154	-26.276219	2.226842
-1459.131778	-23.971164	2.236838
-1456.854998	-18.988765	2.246835
-1454.856578	-21.275690	2.256832
-1453.169246	-25.271796	2.266829
-1451.344852	-24.189699	2.276826
-1449.270985	-23.295974	2.286822
-1447.786909	-27.295845	2.296819
-1445.733772	-29.138352	2.306816
-1443.785899	-27.929176	2.316813
-1441.914799	-25.275556	2.326810
-1439.953534	-25.928575	2.336806
-1438.011604	-35.142958	2.346803
-1436.334469	-28.242363	2.356800
-1434.690389	-20.130118	2.366797
-1432.310171	-24.488220	2.376794
-1430.461373	-22.023656	2.386790
-1428.962517	-22.408406	2.396787
-1426.734700	-29.236910	2.406784
-1425.184497	-27.875617	2.416781
-1423.321300	-26.283380	2.426778
-1421.048233	-23.263040	2.436774
-1419.237333	-30.384790	2.446771
-1417.667329	-28.316115	2.456768
-1415.517979	-34.571499	2.466765
-1413.428624	-29.358517	2.476762
-1411.755883	-22.645096	2.486758
-1410.111783	-18.972967	2.496755
-1407.943590	-24.236598	2.506752
-1405.973137	-27.011649	2.516749
-1404.084175	-29.789441	2.526746
-1402.715484	-29.384363	2.536742
-1400.635087	-31.070138	2.546739
-1398.768068	-29.832187	2.556736
-1396.624530	-29.246421	2.566733
-1394.895292	-24.632622	2.576730
-1392.940188	-23.416664	2.586726
-1391.204975	-24.110820	2.596723
-1389.295509	-25.822904	2.606720
-1387.260844	-22.710674	2.616717
-1385.269521	-26.046436	2.626714
-1383.543517	-23.637965	2.636710
-1381.996123	-22.116714	2.646707
-1379.504835	-29.363159	2.656704
-1378.032023	-26.077280	2.666701
-1376.357645	-21.140462	2.676698
-1374.588984	-23.242109	2.686694
-1372.215769	-21.404631	2.696691
-1370.510678	-24.964563	2.706688
-1368.497220	-28.412804	2.716685
-1366.649051	-29.707675	2.726682
-1364.975345	-25.972357	2.736678
-1362.986438	-30.013523	2.746675
-1360.894559	-24.870368	2.756672
-1358.901986	-28.253677	2.766669
-1357.394041	-22.784921	2.776666
-1355.444309	-32.133129	2.786662
-1353.637706	-30.111762	2.796659
-1352.014529	-27.860496	2.806656
-1349.787920	-33.270797	2.816653
-1347.893214	-27.587629	2.826650
-1346.048016	-30.047306	2.836646
-1343.912270	-22.430555	2.846643
-1342.591979	-22.350860	2.856640
-1340.427792	-22.254678	2.866637
-1338.323366	-20.879413	2.876634
-1336.753908	-18.921123	2.886630
-1334.886531	-24.150745	2.896627
-1332.831946	-27.880286	2.906624
-1330.783819	-29.117136	2.916621
-1329.271482	-22.458500	2.926618
-1327.636789	-23.725483	2.936614
-1325.512359	-24.192940	2.946611
-1323.378184	-28.359964	2.956608
-1321.569980	-29.301023	2.966605
-1319.743630	-23.433196	2.976602
-1317.938279	-18.750988	2.986598
-1316.101485	-28.627424	2.996595
-1314.037103	-23.490874	3.006592
-1312.300337	-29.811184	3.016589
-1310.320370	-31.305534	3.026586
-1308.362616	-27.246156	3.036582
-1306.798875	-23.411083	3.046579
-1304.810704	-23.743022	3.056576
-1303.146489	-31.325962	3.066573
-1300.970246	-26.453630	3.076570
-1299.128464	-28.833775	3.086566
-1297.109575	-30.241184	3.096563
-1295.263476	-25.612852	3.106560
-1293.482101	-23.247913	3.116557
-1291.760810	-19.163300	3.126554
-1289.701601	-27.625799	3.136550
-1288.048288	-24.514019	3.146547
-1286.041857	-30.037448	3.156544
-1283.982956	-30.551222	3.166541
-1282.038650	-29.987146	3.176538
-1280.381499	-25.195922	3.186534
-1278.719357	-29.156296	3.196531
-1276.643462	-23.412061	3.206528
-1274.661882	-31.412107	3.216525
-1272.742593	-24.559611	3.226522
-1270.974923	-20.540829	3.236518
-1269.227363	-25.193838	3.246515
-1267.219881	-19.621806	3.256512
-1265.271429	-18.832582	3.266509
-1263.410753	-20.903083	3.276506
-1261.855627	-20.324070	3.286502
-1259.727961	-16.696064	3.296499
-1257.634856	-23.092319	3.306496
-1255.854436	-22.159348	3.316493
-1254.124283	-17.267676	3.326490
-1252.333939	-14.155693	3.336486
-1250.693103	-19.570056	3.346483
-1248.239119	-25.199824	3.356480
-1246.492705	-21.525000	3.366477
-1244.782304	-26.920489	3.376474
-1242.790819	-17.347851	3.386470
-1240.814738	-17.448846	3.396467
-1238.899306	-30.923718	3.406464
-1237.239687	-26.574976	3.416461
-1235.370237	-26.630479	3.426458
-1233.634204	-22.879771	3.436454
-1231.334563	-23.166755	3.446451
-1229.708207	-20.930118	3.456448
-1227.879619	-18.913745	3.466445
-1225.788797	-24.739590	3.476442
-1224.071100	-26.076629	3.486438
-1222.357815	-21.921205	3.496435
-1220.415574	-20.486718	3.506432
-1218.235095	-21.127262	3.516429
-1216.443011	-26.016314	3.526426
-1214.801580	-19.390885	3.536422
-1212.991072	-19.054820	3.546419
-1210.945216	-20.073301	3.556416
-1208.951064	-19.866097	3.566413
-1207.017497	-22.131383	3.576410
-1205.275803	-17.803643	3.586406
-1203.643728	-11.483030	3.596403
-1201.498210	-17.516564	3.606400
-1199.518458	-13.643769	3.616397
-1197.923010	-14.189097	3.626394
-1195.944474	-15.739968	3.636390
-1193.979136	-19.297212	3.646387
-1192.051520	-18.329322	3.656384
-1190.192836	-24.351682	3.666381
-1188.287556	-17.629501	3.676378
-1186.577218	-15.635226	3.686374
-1184.718926	-17.267902	3.696371
-1182.665653	-16.591699	3.706368
-1180.899932	-15.089456	3.716365
-1179.320166	-16.027011	3.726362
-1177.295114	-15.341551	3.736358
-1175.179518	-7.227170	3.746355
-1173.320123	-17.632939	3.756352
-1171.527246	-16.651367	3.766349
-1169.414608	-23.514901	3.776346
-1167.801430	-24.629905	3.786342
-1165.942643	-16.799702	3.796339
-1163.936741	-13.736350	3.806336
-1162.146984	-18.857106	3.816333
-1160.327299	-20.273578	3.826330
-1158.177619	-18.041675	3.836326
-1156.461336	-17.096785	3.846323
-1154.725770	-20.825660	3.856320
-1152.962975	-19.210818	3.866317
-1150.703510	-17.707025	3.876314
-1148.792313	-17.838614	3.886310
-1147.305281	-19.822397	3.896307
-1145.240752	-18.140561	3.906304
-1143.435429	-31.747755	3.916301
-1141.205313	-18.611505	3.926298
-1139.660334	-21.251946	3.936294
-1137.921328	-15.144189	3.946291
-1135.619410	-18.737869	3.956288
-1133.712094	-22.454734	3.966285
-1132.144622	-22.272358	3.976282
-1130.168054	-16.859468	3.986278
-1128.359239	-20.732681	3.996275
-1127.044577	-12.442739	4.006272
-1124.623985	-19.061814	4.016269
-1122.711020	-20.060536	4.026266
-1120.994850	-18.228203	4.036262
-1118.829353	-20.581053	4.046259
-1117.026726	-25.869629	4.056256
-1115.384025	-27.823032	4.066253
-1113.377134	-21.387051	4.076250
-1111.292823	-18.211457	4.086246
-1109.497947	-18.951267	4.096243
-1107.472829	-21.605343	4.106240
-1105.817861	-22.348030	4.116237
-1103.981483	-17.207962	4.126234
-1102.208369	-21.596513	4.136230
-1100.296959	-20.962281	4.146227
-1098.391691	-28.141538	4.156224
-1096.423566	-18.959773	4.166221
-1094.856099	-16.857306	4.176218
-1092.812703	-21.113822	4.186214
-1090.684279	-24.199687	4.196211
-1088.757213	-23.735325	4.206208
-1086.710215	-19.816345	4.216205
-1085.254515	-21.059264	4.226202
-1083.191249	-19.636125	4.236198
-1081.502807	-20.358887	4.246195
-1079.787062	-21.956045	4.256192
-1077.674620	-20.119176	4.266189
-1075.827053	-26.422314	4.276186
-1073.795557	-18.322806	4.286182
-1072.361670	-23.078663	4.296179
-1070.044936	-31.411651	4.306176
-1068.396920	-19.669621	4.316173
-1066.419368	-24.076640	4.326170
-1064.298563	-17.412509	4.336166
-1062.831316	-21.054186	4.346163
-1060.974517	-23.856566	4.356160
-1059.125095	-24.023991	4.366157
-1056.765872	-24.025061	4.376154
-1055.168887	-20.545663	4.386150
-1053.211143	-21.613072	4.396147
-1051.459413	-19.527419	4.406144
-1049.569439	-26.972624	4.416141
-1047.595116	-32.184399	4.426138
-1045.635668	-25.848140	4.436134
-1044.123705	-24.564157	4.446131
-1041.954319	-21.048411	4.456128
-1040.032842	-22.053164	4.466125
-1038.120407	-25.257597	4.476122
-1036.371298	-21.344609	4.486118
-1034.492682	-27.191615	4.496115
-1032.906379	-20.601438	4.506112
-1030.898501	-23.529018	4.516109
-1028.892079	-22.976242	4.526106
-1026.780458	-23.542435	4.536102
-1024.986547	-16.137534	4.546099
-1023.491419	-19.644695	4.556096
-1021.813759	-26.155889	4.566093
-1019.304153	-22.374002	4.576090
-1017.445045	-25.276196	4.586086
-1015.729330	-21.861551	4.596083
-1013.840467	-26.835414	4.606080
-1011.988750	-29.461674	4.616077
-1010.347612	-22.120752	4.626074
-1008.432921	-24.400228	4.636070
-1006.328765	-21.737729	4.646067
-1004.439454	-21.049355	4.656064
-1002.622795	-24.331603	4.666061
-1000.409329	-28.889988	4.676058
-998.836975	-22.614935	4.686054
-997.231965	-31.438783	4.696051
-995.205034	-21.911055	4.706048
-993.156147	-25.970990	4.716045
-991.423432	-25.743893	4.726042
-989.537063	-31.311042	4.736038
-987.645878	-24.502744	4.746035
-985.985268	-24.112527	4.756032
-983.727248	-23.355206	4.766029
-982.057097	-26.301365	4.776026
-980.005587	-24.205178	4.786022
-977.953363	-23.143351	4.796019
-976.328726	-24.503224	4.806016
-974.481385	-24.596036	4.816013
-972.738011	-21.735275	4.826010
-970.841621	-32.257343	4.836006
-968.901509	-24.315235	4.846003
-966.936696	-27.982741	4.856000
-965.003388	-26.822935	4.865997
-963.074647	-26.061884	4.875994
-961.335639	-29.851174	4.885990
-959.784376	-25.262252	4.895987
-957.658065	-29.201903	4.905984
-955.819559	-29.004330	4.915981
-953.585975	-28.473607	4.925978
-951.873046	-30.603926	4.935974
-950.141225	-24.504345	4.945971
-948.078733	-23.556242	4.955968
-946.387776	-30.333206	4.965965
-944.563345	-33.116109	4.975962
-942.749454	-27.255445	4.985958
-940.680875	-27.988368	4.995955
-938.928573	-28.146483	5.005952
-936.866555	-22.529182	5.015949
-934.816807	-31.411481	5.025946
-933.283802	-26.909625	5.035942
-931.657985	-23.074736	5.045939
-929.563211	-30.088376	5.055936
-927.402481	-35.100908	5.065933
-925.501428	-33.279046	5.075930
-923.772668	-30.602234	5.085926
-922.156829	-23.743532	5.095923
-920.187435	-25.919576	5.105920
-918.043356	-25.109234	5.115917
-916.015737	-24.566067	5.125914
-914.607742	-30.422996	5.135910
-912.857872	-26.364764	5.145907
-910.940558	-26.760831	5.155904
-908.679422	-27.521358	5.165901
-906.553526	-19.744692	5.175898
-905.010164	-24.292162	5.185894
-903.231610	-25.439747	5.195891
-901.182467	-27.693266	5.205888
-899.728140	-28.613735	5.215885
-897.758072	-27.612913	5.225882
-895.617296	-21.239192	5.235878
-893.709409	-27.839223	5.245875
-891.886782	-19.404555	5.255872
-890.115801	-22.313088	5.265869
-888.386316	-24.932342	5.275866
-886.138941	-21.439969	5.285862
-884.385233	-20.161374	5.295859
-882.504948	-22.757367	5.305856
-880.597693	-18.286888	5.315853
-878.392335	-23.379151	5.325850
-877.314907	-22.635077	5.335846
-875.255623	-23.674363	5.345843
-872.975546	-25.178438	5.355840
-870.955873	-21.357527	5.365837
-869.373462	-25.486467	5.375834
-867.836060	-26.478622	5.385830
-865.806158	-22.070374	5.395827
-863.861684	-18.357437	5.405824
-861.911208	-27.378553	5.415821
-860.142332	-33.848958	5.425818
-858.292409	-26.759204	5.435814
-856.012646	-19.968701	5.445811
-854.252911	-24.751268	5.455808
-852.644261	-25.342684	5.465805
-850.609034	-29.872439	5.475802
-848.623425	-29.186703	5.485798
-846.839453	-27.551327	5.495795
-845.154078	-23.883798	5.505792
-842.997096	-26.013977	5.515789
-841.386308	-23.493510	5.525786
-839.470366	-27.587328	5.535782
-837.344173	-25.916653	5.545779
-835.826348	-29.842607	5.555776
-833.784919	-24.946682	5.565773
-831.882965	-32.246795	5.575770
-829.796625	-25.284813	5.585766
-828.238123	-24.372879	5.595763
-826.139293	-23.962601	5.605760
-824.182037	-23.976548	5.615757
-822.409786	-21.276608	5.625754
-820.842072	-23.132558	5.635750
-818.764124	-21.615211	5.645747
-816.644676	-20.271871	5.655744
-815.218455	-21.408857	5.665741
-813.406271	-29.885177	5.675738
-811.037117	-27.114856	5.685734
-809.404539	-20.154527	5.695731
-807.663954	-22.001787	5.705728
-805.562165	-24.345750	5.715725
-803.592017	-24.998080	5.725722
-801.947440	-28.704266	5.735718
-799.779352	-24.463317	5.745715
-798.248667	-22.638987	5.755712
-796.147114	-21.938581	5.765709
-794.300117	-23.782315	5.775706
-792.574418	-22.432855	5.785702
-790.347337	-17.637620	5.795699
-788.638267	-18.047670	5.805696
-787.120485	-21.051450	5.815693
-785.189153	-20.225926	5.825690
-783.097622	-26.141520	5.835686
-781.331664	-25.351140	5.845683
-779.199332	-18.031708	5.855680
-777.395812	-23.686516	5.865677
-775.482977	-25.341804	5.875674
-773.708614	-24.840140	5.885670
-771.741131	-23.186669	5.895667
-770.080271	-17.775097	5.905664
-768.163875	-24.663776	5.915661
-766.158950	-27.994891	5.925658
-764.171892	-18.956371	5.935654
-762.276362	-26.054876	5.945651
-760.914288	-23.740922	5.955648
-758.880531	-20.195329	5.965645
-756.710890	-18.455731	5.975642
-754.796506	-24.458256	5.985638
-753.396753	-21.346606	5.995635
-751.184338	-15.445260	6.005632
-749.174609	-21.974620	6.015629
-747.456412	-16.960631	6.025626
-745.363508	-15.440871	6.035622
-743.637732	-16.917810	6.045619
-741.969198	-21.363605	6.055616
-739.999432	-19.988377	6.065613
-738.136405	-20.336152	6.075610
-735.811643	-18.310263	6.085606
-734.335910	-20.603053	6.095603
-732.683235	-11.905807	6.105600
-730.637710	-15.691822	6.115597
-728.678230	-19.372501	6.125594
-726.690153	-13.473171	6.135590
-724.937614	-20.705120	6.145587
-723.184818	-19.683636	6.155584
-720.822556	-17.520035	6.165581
-719.097737	-17.057782	6.175578
-717.453369	-16.383715	6.185574
-715.721804	-16.239918	6.195571
-713.655855	-17.374871	6.205568
-711.617046	-20.373450	6.215565
-709.803830	-20.871143	6.225562
-708.283256	-20.578353	6.235558
-706.500904	-24.655458	6.245555
-704.456075	-16.933532	6.255552
-702.374316	-18.391540	6.265549
-700.431358	-18.534157	6.275546
-698.679265	-18.410997	6.285542
-696.682828	-18.341096	6.295539
-694.771281	-13.801665	6.305536
-693.002412	-15.618626	6.315533
-691.356402	-23.087748	6.325530
-689.384485	-16.440512	6.335526
-687.420858	-20.552889	6.345523
-685.649877	-14.353556	6.355520
-683.380038	-13.787315	6.365517
-681.663183	-16.500726	6.375514
-680.242926	-22.365809	6.385510
-678.107078	-12.957809	6.395507
-676.176234	-22.488834	6.405504
-674.255341	-15.670792	6.415501
-672.700199	-19.163650	6.425498
-670.346126	-15.514420	6.435494
-668.288202	-15.710121	6.445491
-666.698201	-14.105189	6.455488
-664.671625	-17.144408	6.465485
-663.040018	-19.474697	6.475482
-661.173251	-18.915079	6.485478
-659.218401	-22.623385	6.495475
-657.323360	-20.539802	6.505472
-655.346668	-12.972735	6.515469
-653.949909	-20.938869	6.525466
-652.023249	-23.594202	6.535462
-650.058560	-22.322301	6.545459
-647.967831	-17.615666	6.555456
-645.952083	-18.575164	6.565453
-644.166703	-22.272168	6.575450
-642.101714	-16.558745	6.585446
-640.588745	-15.858890	6.595443
-638.845917	-23.864523	6.605440
-636.737709	-18.306427	6.615437
-634.569154	-16.782866	6.625434
-633.089057	-17.816243	6.635430
-631.202466	-18.354023	6.645427
-629.274501	-20.022667	6.655424
-627.425016	-18.391272	6.665421
-625.340389	-19.887569	6.675418
-623.513257	-23.674917	6.685414
-621.653150	-18.328227	6.695411
-620.024074	-18.475892	6.705408
-618.052574	-19.418822	6.715405
-616.090723	-19.229639	6.725402
-614.112713	-16.410826	6.735398
-612.521956	-22.344169	6.745395
-610.487022	-15.867989	6.755392
-608.408725	-25.825171	6.765389
-606.650907	-25.139152	6.775386
-604.811145	-21.829278	6.785382
-602.935598	-17.326652	6.795379
-601.186360	-24.449039	6.805376
-599.512670	-16.746666	6.815373
-597.263382	-20.940930	6.825370
-595.514870	-23.157214	6.835366
-593.493256	-19.483212	6.845363
-591.718963	-13.922252	6.855360
-589.915555	-25.362404	6.865357
-588.031427	-18.772107	6.875354
-586.138064	-28.592350	6.885350
-583.952062	-28.858968	6.895347
-582.692846	-20.512449	6.905344
-580.257823	-26.307485	6.915341
-578.224825	-17.372449	6.925338
-576.666993	-20.766199	6.935334
-575.143508	-20.093247	6.945331
-572.995236	-19.534321	6.955328
-571.060419	-16.759100	6.965325
-569.242784	-17.328448	6.975322
-567.147465	-18.861141	6.985318
-565.615606	-12.246124	6.995315
-563.668489	-13.170904	7.005312
-561.437390	-19.656534	7.015309
-559.718227	-30.849511	7.025306
-557.971000	-16.825445	7.035302
-555.959166	-22.080730	7.045299
-554.307985	-21.257632	7.055296
-552.303967	-20.741960	7.065293
-550.632107	-26.560321	7.075290
-548.425956	-20.765148	7.085286
-546.843428	-16.727264	7.095283
-544.979973	-20.967218	7.105280
-542.745199	-20.232602	7.115277
-541.014946	-20.776916	7.125274
-539.255704	-15.963540	7.135270
-537.287726	-15.898433	7.145267
-535.033630	-22.081384	7.155264
-533.736191	-19.228000	7.165261
-531.869362	-22.146851	7.175258
-529.583518	-20.886675	7.185254
-527.693681	-14.251444	7.195251
-526.214782	-14.119255	7.205248
-524.082327	-24.099236	7.215245
-522.341638	-25.309967	7.225242
-520.438816	-20.953741	7.235238
-518.634094	-23.068418	7.245235
-516.875927	-21.100231	7.255232
-514.817736	-22.998015	7.265229
-512.764880	-20.457925	7.275226
-510.858151	-16.887081	7.285222
-509.206263	-16.281967	7.295219
-507.368757	-19.811931	7.305216
-505.348692	-22.827873	7.315213
-503.451726	-27.701594	7.325210
-501.825931	-23.135307	7.335206
-499.800673	-32.660754	7.345203
-497.868351	-26.943379	7.355200
-496.145189	-28.171819	7.365197
-494.173556	-26.515617	7.375194
-492.273206	-22.725837	7.385190
-490.472994	-21.121203	7.395187
-488.399395	-26.037337	7.405184
-486.530409	-18.940829	7.415181
-484.874233	-21.909686	7.425178
-482.949478	-21.640255	7.435174
-480.986769	-23.409071	7.445171
-479.014314	-17.729665	7.455168
-477.167892	-13.195437	7.465165
-475.356750	-16.754327	7.475162
-473.279134	-20.008392	7.485158
-471.650685	-20.133749	7.495155
-469.774210	-16.633831	7.505152
-467.711852	-20.041777	7.515149
-466.060050	-25.883725	7.525146
-464.377863	-25.993974	7.535142
-462.446114	-26.016181	7.545139
-460.174085	-14.329093	7.555136
-458.525496	-22.551675	7.565133
-456.572543	-25.005783	7.575130
-454.537859	-25.595498	7.585126
-452.543047	-23.627161	7.595123
-451.242249	-23.406479	7.605120
-449.141892	-21.121823	7.615117
-447.308137	-22.637903	7.625114
-445.255451	-25.646374	7.635110
-443.572313	-19.407553	7.645107
-441.656706	-17.922366	7.655104
-439.648373	-21.361136	7.665101
-437.780518	-13.972286	7.675098
-436.041354	-12.389439	7.685094
-434.569467	-12.406079	7.695091
-432.166912	-21.563826	7.705088
-430.112291	-22.223023	7.715085
-428.537575	-20.223893	7.725082
-426.429207	-27.068766	7.735078
-424.788963	-20.782027	7.745075
-422.833594	-22.450147	7.755072
-421.016742	-13.824665	7.765069
-419.003147	-21.068102	7.775066
-417.004345	-21.871538	7.785062
-415.374717	-28.898908	7.795059
-413.234241	-28.622815	7.805056
-411.698064	-27.080170	7.815053
-409.887006	-18.070057	7.825050
-407.796090	-25.137928	7.835046
-405.796834	-28.838915	7.845043
-404.123075	-27.348237	7.855040
-402.243444	-27.183644	7.865037
-400.425268	-23.833842	7.875034
-398.424974	-25.242263	7.885030
-396.573534	-21.681444	7.895027
-394.432816	-21.313790	7.905024
-392.865614	-19.615027	7.915021
-391.073439	-21.045475	7.925018
-388.823012	-26.539261	7.935014
-387.073169	-25.374943	7.945011
-385.518419	-17.004435	7.955008
-383.836848	-23.266366	7.965005
-381.729311	-29.013656	7.975002
-379.498483	-26.759246	7.984998
-377.703435	-26.107424	7.994995
-376.100470	-24.059083	8.004992
-373.834833	-26.329361	8.014989
-372.016093	-26.942949	8.024986
-370.339722	-22.602544	8.034982
-368.498071	-22.109742	8.044979
-366.687090	-20.718319	8.054976
-364.625674	-20.279552	8.064973
-362.832036	-25.817226	8.074970
-360.763772	-19.636677	8.084966
-358.875600	-25.322080	8.094963
-357.261728	-20.963792	8.104960
-355.616440	-14.860968	8.114957
-353.515200	-20.255113	8.124954
-351.338768	-21.170545	8.134950
-349.799402	-23.376946	8.144947
-347.693454	-24.669558	8.154944
-345.903135	-23.601676	8.164941
-344.095966	-25.833464	8.174938
-342.280325	-22.371101	8.184934
-340.311906	-23.482267	8.194931
-338.404252	-20.025117	8.204928
-336.444596	-18.868996	8.214925
-334.586003	-29.773036	8.224922
-332.662097	-29.853889	8.234918
-330.549010	-27.989599	8.244915
-329.238745	-25.510793	8.254912
-327.652069	-26.260988	8.264909
-325.332888	-27.025496	8.274906
-323.075696	-31.223933	8.284902
-321.417546	-34.104571	8.294899
-319.768485	-28.116018	8.304896
-318.074724	-17.064382	8.314893
-315.887514	-32.200524	8.324890
-314.089328	-25.139939	8.334886
-311.960808	-27.715125	8.344883
-310.180321	-24.589770	8.354880
-308.266677	-28.321224	8.364877
-306.419787	-25.834916	8.374874
-304.504822	-30.253449	8.384870
-302.685668	-26.363703	8.394867
-301.154672	-29.839844	8.404864
-299.072448	-26.093150	8.414861
-297.008693	-20.214993	8.424858
-295.436229	-28.453744	8.434854
-293.256991	-24.784114	8.444851
-291.479511	-25.357895	8.454848
-289.838865	-28.260983	8.464845
-287.913896	-27.741944	8.474842
-285.757592	-19.975839	8.484838
-284.025999	-13.782525	8.494835
-281.908436	-18.768673	8.504832
-280.595936	-17.719204	8.514829
-278.279838	-17.508922	8.524826
-276.132843	-25.008817	8.534822
-274.696960	-33.179959	8.544819
-272.925274	-24.602413	8.554816
-270.940105	-18.703792	8.564813
-269.075932	-21.882560	8.574810
-266.938922	-27.601303	8.584807
-265.254709	-25.737968	8.594803
-263.308231	-25.197078	8.604800
-261.711408	-16.695820	8.614797
-259.592302	-22.250641	8.624794
-257.474667	-21.825493	8.634791
-255.489988	-27.174106	8.644787
-254.030454	-27.663948	8.654784
-252.390165	-19.460161	8.664781
-250.352940	-16.708913	8.674778
-248.395166	-23.084324	8.684775
-246.405824	-19.254857	8.694771
-244.501119	-20.401568	8.704768
-242.788487	-17.983780	8.714765
-240.958188	-23.538277	8.724762
-238.990462	-22.572846	8.734759
-237.163934	-18.633694	8.744755
-235.083203	-18.516860	8.754752
-233.386110	-21.989473	8.764749
-231.459852	-23.426995	8.774746
-229.536170	-15.985296	8.784743
-227.617268	-27.172065	8.794739
-225.863254	-20.489633	8.804736
-223.933283	-28.624348	8.814733
-222.097259	-17.781664	8.824730
-220.292313	-21.517810	8.834727
-218.232220	-20.587632	8.844723
-216.476518	-19.978357	8.854720
-214.575921	-16.725249	8.864717
-212.885526	-18.295644	8.874714
-210.817781	-18.914117	8.884711
-208.847893	-21.789174	8.894707
-206.967336	-25.033672	8.904704
-205.190076	-21.072421	8.914701
-203.430464	-17.488893	8.924698
-201.584695	-19.750424	8.934695
-199.533076	-21.591630	8.944691
-197.550019	-26.889412	8.954688
-195.822770	-16.085397	8.964685
-193.850003	-25.459345	8.974682
-191.866360	-30.281930	8.984679
-189.703460	-27.692801	8.994675
-188.728298	-28.901122	9.004672
-186.306214	-25.161197	9.014669
-184.678087	-26.896905	9.024666
-182.683726	-28.004190	9.034663
-180.806184	-31.065020	9.044659
-178.894612	-30.095315	9.054656
-176.721012	-27.353137	9.064653
-175.252104	-27.170188	9.074650
-173.524386	-28.986522	9.084647
-171.510451	-36.043495	9.094643
-169.541373	-28.177924	9.104640
-167.657182	-26.220113	9.114637
-165.620947	-27.424070	9.124634
-163.853732	-28.401928	9.134631
-162.316362	-23.087039	9.144627
-160.296260	-26.889058	9.154624
-158.347495	-29.973871	9.164621
-156.208816	-28.143509	9.174618
-154.268404	-29.595861	9.184615
-152.578579	-31.622459	9.194611
-151.113401	-29.090903	9.204608
-149.033309	-27.221184	9.214605
-147.121989	-31.359532	9.224602
-144.845900	-26.304630	9.234599
-143.351299	-38.592096	9.244595
-141.485390	-31.839033	9.254592
-139.457785	-24.308840	9.264589
-137.509361	-28.889700	9.274586
-136.025841	-32.907664	9.284583
-134.043100	-35.074154	9.294579
-132.018378	-31.649728	9.304576
-130.057457	-30.304158	9.314573
-128.370651	-31.002305	9.324570
-126.331777	-31.600308	9.334567
-124.544113	-29.434420	9.344563
-122.675623	-20.021893	9.354560
-120.704400	-22.964992	9.364557
-119.057096	-21.679899	9.374554
-117.029857	-27.902078	9.384551
-115.104105	-26.047176	9.394547
-113.074936	-25.222505	9.404544
-111.570532	-22.188737	9.414541
-109.446651	-35.098468	9.424538
-107.631289	-30.095545	9.434535
-105.806480	-35.662489	9.444531
-103.947927	-37.973356	9.454528
-102.290835	-33.915482	9.464525
-100.077677	-28.709174	9.474522
-98.126302	-31.958573	9.484519
-96.201987	-28.753368	9.494515
-94.612583	-38.107122	9.504512
-92.804176	-27.203870	9.514509
-90.568750	-27.087909	9.524506
-88.747187	-37.271370	9.534503
-86.962378	-31.259302	9.544499
-85.212795	-23.723383	9.554496
-82.985640	-28.180511	9.564493
-81.466158	-26.480243	9.574490
-79.698933	-25.800072	9.584487
-77.669406	-29.652479	9.594483
-75.742956	-26.768138	9.604480
-73.917454	-26.556756	9.614477
-71.866232	-26.084531	9.624474
-70.108244	-26.043961	9.634471
-68.329419	-29.123696	9.644467
-66.301219	-25.764506	9.654464
-64.706564	-17.832779	9.664461
-62.655774	-22.670718	9.674458
-60.779565	-27.357637	9.684455
-58.772924	-23.286021	9.694451
-56.926150	-22.831693	9.704448
-55.051585	-24.905069	9.714445
-53.478182	-20.405890	9.724442
-51.369361	-25.180443	9.734439
-49.259088	-28.399891	9.744435
-47.620648	-33.369405	9.754432
-45.810021	-28.579634	9.764429
-44.123543	-29.655056	9.774426
-41.902918	-20.721026	9.784423
-40.014861	-24.386616	9.794419
-38.044262	-27.026379	9.804416
-36.420240	-22.303148	9.814413
-34.476769	-27.013410	9.824410
-32.406698	-28.240025	9.834407
-30.688107	-28.286304	9.844403
-28.502160	-30.737772	9.854400
-27.003119	-28.036268	9.864397
-25.443731	-21.580008	9.874394
-23.223839	-24.663758	9.884391
-21.213582	-30.169437	9.894387
-19.602063	-30.912343	9.904384
-17.583488	-27.928961	9.914381
-15.472160	-27.003624	9.924378
-13.899602	-29.175639	9.934375
-11.715706	-28.110290	9.944371
-10.029356	-32.056325	9.954368
-8.311483	-29.348664	9.964365
-6.682719	-20.143331	9.974362
-5.335771	8.181552	9.984359
-4.138532	50.752672	9.994355
-2.599445	97.021165	10.004352
-0.993005	169.822715	10.014349
0.000000	224.449223	10.019354
0.691407	269.431203	10.024359
1.673553	302.297883	10.029363
2.010008	338.188317	10.034368
2.702759	353.990408	10.039373
2.515192	378.918941	10.044378
2.642825	396.642175	10.049383
3.264613	411.328061	10.054387
3.212469	415.020622	10.059392
3.522728	430.114213	10.064397
3.990598	449.617346	10.069402
3.787557	457.248232	10.074407
4.256231	452.076695	10.079411
3.922001	462.180828	10.084416
4.491168	460.305070	10.089421
4.451197	454.195895	10.094426
3.739843	455.446685	10.099431
4.708845	461.348252	10.104435
4.083032	473.730436	10.109440
4.630387	466.633376	10.114445
4.767910	469.374696	10.119450
4.773506	478.177181	10.124455
4.922087	482.683041	10.129459
4.654098	483.777946	10.134464
4.492296	467.196054	10.139469
4.628947	474.962008	10.144474
4.613516	482.288573	10.149479
5.027964	477.800657	10.154483
4.789145	481.612906	10.159488
4.974372	486.150771	10.164493
5.111578	489.373147	10.169498
4.636479	472.167824	10.174503
5.028583	481.779189	10.179507
5.298025	490.821886	10.184512
5.122986	480.714330	10.189517
4.762518	473.777853	10.194522
4.952102	488.997995	10.199527
5.397511	494.391703	10.204531
5.194725	504.102711	10.209536
5.347009	505.468066	10.214541
5.501358	497.531607	10.219546
5.047301	506.467361	10.224551
5.424622	503.910947	10.229555
5.308877	508.905288	10.234560
5.638881	507.670112	10.239565
5.666031	502.332431	10.244570
5.523438	510.966174	10.249575
5.645986	508.004094	10.254579
5.502754	520.074354	10.259584
5.681741	509.377258	10.264589
5.834503	514.958015	10.269594
5.660359	518.308918	10.274599
5.866784	515.423348	10.279603
5.708366	525.810160	10.284608
6.141575	520.062322	10.289613
5.880544	526.661636	10.294618
5.717592	532.806884	10.299623
5.804922	519.006553	10.304627
5.596227	529.026047	10.309632
6.081127	531.379206	10.314637
6.057098	530.744589	10.319642
6.028439	532.187699	10.324647
6.287098	542.754012	10.329651
6.352466	549.883206	10.334656
6.541112	562.826296	10.339661
6.385736	558.727319	10.344666
6.321828	574.069994	10.349671
6.819012	556.580152	10.354675
6.248903	559.858601	10.359680
6.558337	565.102127	10.364685
6.617654	564.115144	10.369690
6.389704	577.381764	10.374695
6.879037	574.257075	10.379699
6.297063	576.993332	10.384704
6.658109	567.002065	10.389709
6.586729	578.849585	10.394714
6.636416	577.638618	10.399719
6.884994	573.852116	10.404723
6.724390	575.204307	10.409728
6.924037	576.417024	10.414733
6.875523	583.250564	10.419738
6.811318	586.695916	10.424743
7.305983	602.656044	10.429747
6.927404	615.744862	10.434752
7.371474	609.594681	10.439757
6.843439	613.322203	10.444762
6.986655	622.255797	10.449767
7.422531	619.880849	10.454771
7.073952	619.613414	10.459776
7.228662	618.541820	10.464781
7.350415	622.957380	10.469786
7.474852	628.246210	10.474791
7.535589	626.342718	10.479795
7.356973	629.058800	10.484800
7.589770	623.257729	10.489805
7.321216	635.076819	10.494810
7.571487	643.542307	10.499815
8.033830	644.279430	10.504819
7.672439	652.311021	10.509824
8.095637	649.394000	10.514829
8.128753	653.536681	10.519834
8.285697	661.427241	10.524839
8.481211	650.386758	10.529843
8.124912	642.058556	10.534848
8.301066	639.362309	10.539853
8.028935	633.143425	10.544858
7.893898	635.262731	10.549863
8.119416	649.133643	10.554867
8.056494	656.808519	10.559872
8.293446	660.764133	10.564877
8.528924	660.780450	10.569882
8.524162	666.755429	10.574887
8.824043	665.493504	10.579891
8.371682	659.495762	10.584896
8.721035	674.636992	10.589901
8.592530	673.031785	10.594906
8.507019	672.954215	10.599911
8.964770	670.777635	10.604915
8.618793	682.612268	10.609920
8.796767	673.454441	10.614925
8.693684	677.778140	10.619930
8.903679	680.602564	10.624935
8.797458	679.802842	10.629939
8.403667	686.301970	10.634944
8.737993	681.000386	10.639949
9.165948	683.227026	10.644954
8.913386	691.799563	10.649959
9.037144	683.304866	10.654963
8.729291	686.759144	10.659968
8.825202	682.183196	10.664973
9.032353	697.957463	10.669978
9.154411	704.383774	10.674983
9.302058	706.609397	10.679987
9.022625	718.857679	10.684992
9.154329	725.484327	10.689997
9.479715	718.914604	10.695002
9.577900	717.066633	10.700007
9.675731	721.927622	10.705011
9.470593	716.672652	10.710016
9.795352	718.461560	10.715021
9.362326	714.029906	10.720026
9.492424	719.387258	10.725031
9.776677	715.878905	10.730035
9.381553	721.924062	10.735040
9.724972	721.366451	10.740045
10.296273	733.579971	10.745050
10.019581	741.672222	10.750055
9.726927	729.503082	10.755059
9.884875	734.641514	10.760064
9.829135	742.543966	10.765069
10.317595	750.638757	10.770074
10.122566	754.757930	10.775079
10.619744	752.112964	10.780083
10.167403	763.362183	10.785088
10.239411	760.433348	10.790093
10.647282	760.996224	10.795098
10.282465	751.984862	10.800103
10.629573	753.249772	10.805107
10.492262	760.045515	10.810112
10.610666	755.961162	10.815117
10.733012	757.014323	10.820122
10.661554	756.631710	10.825127
10.841511	742.004193	10.830131
10.383151	743.851789	10.835136
10.719177	745.858117	10.840141
10.402849	755.975367	10.845146
10.534211	753.245240	10.850151
10.826107	745.567426	10.855155
10.781548	756.283197	10.860160
10.822523	754.693527	10.865165
10.982339	759.472095	10.870170
10.584693	761.926647	10.875175
10.857743	759.344243	10.880179
10.734621	759.458768	10.885184
10.901101	770.189774	10.890189
11.237561	780.182407	10.895194
11.257858	781.526262	10.900199
11.552976	785.020008	10.905203
11.458082	788.044489	10.910208
11.318747	786.794264	10.915213
11.556666	800.404701	10.920218
11.816383	799.508748	10.925223
11.914478	785.452537	10.930227
11.467429	772.625109	10.935232
11.433477	783.320283	10.940237
11.657126	792.624385	10.945242
11.713972	807.731982	10.950247
11.979697	794.029101	10.955251
11.827843	795.695334	10.960256
11.913127	799.815541	10.965261
12.126235	788.052994	10.970266
11.544772	793.684743	10.975271
11.846004	791.619854	10.980275
11.990935	805.371295	10.985280
12.182434	794.249335	10.990285
12.172310	804.645808	10.995290
12.049220	802.238561	11.000295
12.169182	792.091616	11.005299
11.876431	810.928024	11.010304
12.277655	803.049797	11.015309
12.197646	811.918183	11.020314
11.990380	800.005045	11.025319
12.496295	796.478662	11.030323
12.248182	804.476495	11.035328
12.021487	799.776915	11.040333
12.334533	809.443692	11.045338
12.381429	826.045612	11.050343
12.643682	825.012835	11.055347
12.670231	836.639133	11.060352
12.574734	829.463868	11.065357
12.809281	834.605888	11.070362
12.603368	830.518838	11.075367
12.928422	836.809527	11.080371
12.861873	846.272717	11.085376
12.933019	837.243802	11.090381
13.000269	836.588303	11.095386
13.004745	833.506207	11.100391
13.117865	833.724986	11.105395
12.694661	848.965978	11.110400
12.921591	842.190324	11.115405
13.170058	836.120141	11.120410
12.702081	841.415232	11.125415
12.816633	840.698566	11.130419
13.202559	860.942366	11.135424
13.333587	859.957330	11.140429
13.762948	865.013874	11.145434
13.464944	869.580053	11.150439
13.471224	869.938101	11.155443
13.151592	872.705897	11.160448
13.292198	868.319899	11.165453
13.585319	863.734516	11.170458
13.366289	875.814796	11.175463
13.544093	871.863662	11.180467
13.640866	868.454571	11.185472
13.634927	865.102869	11.190477
13.738693	867.148631	11.195482
13.644501	880.219131	11.200487
13.875980	882.604889	11.205491
13.618116	896.728992	11.210496
14.196809	897.766933	11.215501
14.283625	892.160947	11.220506
13.849696	898.952026	11.225511
14.229541	897.547216	11.230515
14.155898	896.768307	11.235520
14.211315	901.694474	11.240525
14.218879	903.810785	11.245530
14.114209	901.889484	11.250535
14.460461	901.996952	11.255539
14.279619	908.071876	11.260544
14.553427	903.118154	11.265549
14.504580	894.401686	11.270554
14.616277	904.187385	11.275559
14.601767	902.709061	11.280563
14.425670	911.470610	11.285568
14.196336	914.468461	11.290573
14.473388	909.537876	11.295578
14.702313	915.795043	11.300583
14.701768	914.148107	11.305587
14.686791	935.600937	11.310592
15.094543	933.895177	11.315597
15.322786	938.718087	11.320602
14.839269	935.444128	11.325607
15.325290	933.679358	11.330611
14.984364	935.367880	11.335616
15.102067	927.411800	11.340621
15.059297	939.118629	11.345626
15.302516	938.535202	11.350631
15.447720	939.534263	11.355635
15.341571	946.025472	11.360640
15.004291	944.659350	11.365645
15.583990	942.946662	11.370650
15.501000	950.155705	11.375655
15.521006	937.123517	11.380659
15.508555	944.872503	11.385664
15.498005	939.863193	11.390669
15.547609	941.252067	11.395674
15.205506	948.425951	11.400679
15.361769	942.545491	11.405683
15.378769	948.884580	11.410688
15.382869	943.903686	11.415693
15.548080	944.219824	11.420698
15.381291	956.162514	11.425703
16.027229	970.151980	11.430707
15.830835	982.501576	11.435712
16.007061	982.180382	11.440717
16.162500	987.426548	11.445722
15.763260	977.456921	11.450727
16.230853	973.985500	11.455731
16.060426	980.326901	11.460736
16.131884	986.878904	11.465741
16.415154	978.706343	11.470746
16.311059	980.851516	11.475751
16.498425	980.938594	11.480755
16.310831	984.891049	11.485760
16.229910	980.321925	11.490765
16.463900	987.552181	11.495770
16.242120	991.445430	11.500775
16.657680	991.498473	11.505779
16.389213	989.577266	11.510784
16.428128	986.172646	11.515789
16.847799	983.701658	11.520794
16.579687	997.293641	11.525799
16.464504	991.543991	11.530803
16.844285	1008.766445	11.535808
17.023530	1017.456392	11.540813
17.240516	1013.410652	11.545818
16.796585	1005.710504	11.550823
17.133472	1007.670208	11.555827
16.896020	1010.613386	11.560832
17.156359	1014.963588	11.565837
17.422383	1016.874667	11.570842
17.234887	1016.973440	11.575847
16.979164	1005.620641	11.580851
17.203191	1018.069589	11.585856
17.679353	1007.797070	11.590861
17.646061	1018.723358	11.595866
17.348429	1011.602327	11.600871
17.451218	1002.785904	11.605875
17.286694	1016.232846	11.610880
17.644275	1017.707443	11.615885
17.685860	1010.257096	11.620890
17.271039	1011.540268	11.625895
17.647869	1015.952321	11.630899
17.633781	1020.008798	11.635904
17.312085	1022.183956	11.640909
17.341207	1016.330845	11.645914
16.983834	1020.707036	11.650919
17.425350	1025.884714	11.655923
17.342640	1047.483357	11.660928
17.847830	1048.790105	11.665933
17.483995	1043.199171	11.670938
17.278982	1048.849033	11.675943
17.831279	1057.802806	11.680947
18.259691	1069.257942	11.685952
18.357281	1074.492865	11.690957
18.534450	1072.748957	11.695962
18.084952	1079.649846	11.700967
18.514501	1068.392713	11.705971
18.651993	1077.377180	11.710976
18.551085	1072.219795	11.715981
18.505464	1061.082623	11.720986
18.387433	1065.818871	11.725991
18.754259	1071.811233	11.730995
18.509321	1068.806724	11.736000
18.726517	1065.681973	11.741005
19.029100	1060.357717	11.746010
18.578385	1061.693144	11.751015
18.702477	1053.938635	11.756019
18.847370	1056.648138	11.761024
18.936728	1078.060879	11.766029
18.809608	1080.515701	11.771034
18.945117	1087.565364	11.776039
19.104717	1081.573918	11.781043
19.242807	1087.183260	11.786048
19.399336	1071.028556	11.791053
19.149341	1054.693474	11.796058
18.689125	1059.310820	11.801063
19.040202	1068.176836	11.806067
19.149322	1078.168878	11.811072
19.050529	1082.153719	11.816077
19.019133	1082.800875	11.821082
18.998631	1080.522312	11.826087
18.905992	1077.652007	11.831091
18.726202	1090.767892	11.836096
19.033262	1105.824846	11.841101
19.208036	1113.883138	11.846106
18.757517	1124.797992	11.851111
19.287157	1123.638955	11.856115
19.495440	1116.733671	11.861120
19.671083	1139.529282	11.866125
20.016309	1147.386130	11.871130
20.115271	1143.136806	11.876135
20.114919	1122.674703	11.881139
19.607895	1127.828662	11.886144
19.812996	1125.745943	11.891149
20.146102	1122.333791	11.896154
20.290372	1140.805990	11.901159
20.474504	1127.279834	11.906163
20.154523	1119.439203	11.911168
20.367131	1117.095061	11.916173
20.403845	1118.262057	11.921178
20.164727	1116.311705	11.926183
20.481056	1107.452482	11.931187
20.326959	1121.147043	11.936192
19.888974	1124.177430	11.941197
20.259279	1111.322624	11.946202
20.229291	1130.824869	11.951207
20.664658	1141.632332	11.956211
20.671956	1155.264118	11.961216
20.719748	1144.584331	11.966221
20.894766	1146.103046	11.971226
20.370904	1143.426896	11.976231
20.876834	1139.925665	11.981235
21.036092	1140.629153	11.986240
20.912267	1135.619708	11.991245
20.702456	1128.775590	11.996250
20.582669	1138.640166	12.001255
21.148081	1140.089510	12.006259
21.112227	1149.958842	12.011264
21.133511	1146.104361	12.016269
20.989809	1146.516305	12.021274
20.852270	1156.112458	12.026279
21.285475	1141.798999	12.031283
21.222956	1141.444915	12.036288
21.031331	1151.496808	12.041293
21.530781	1151.643716	12.046298
21.346247	1136.133190	12.051303
21.475235	1123.434363	12.056307
21.253014	1118.105480	12.061312
21.234992	1118.243459	12.066317
21.029549	1112.188002	12.071322
20.553838	1126.692467	12.076327
21.161532	1117.170894	12.081331
21.291448	1124.055081	12.086336
21.096778	1123.904235	12.091341
20.901799	1122.985378	12.096346
20.824731	1126.155336	12.101351
21.143233	1118.944643	12.106355
20.965818	1129.692133	12.111360
21.181080	1129.502708	12.116365
20.973143	1128.462114	12.121370
20.855187	1138.019646	12.126375
21.179135	1123.792238	12.131379
21.288591	1127.104349	12.136384
20.938397	1132.934325	12.141389
21.218277	1131.148005	12.146394
20.610665	1133.127486	12.151399
21.306652	1125.649973	12.156403
21.007106	1127.589776	12.161408
21.300646	1126.098566	12.166413
21.054771	1123.271621	12.171418
20.624324	1133.398659	12.176423
20.904477	1127.493632	12.181427
20.895535	1145.977660	12.186432
21.175451	1157.718357	12.191437
21.385284	1158.347540	12.196442
21.123878	1151.888575	12.201447
21.322633	1132.258963	12.206451
21.293548	1141.750277	12.211456
21.120584	1135.875731	12.216461
21.250646	1128.956107	12.221466
21.534001	1130.548224	12.226471
21.561409	1132.232424	12.231475
21.202335	1134.229826	12.236480
21.365408	1135.326987	12.241485
21.184530	1131.565477	12.246490
20.953801	1137.893696	12.251495
21.184499	1120.489851	12.256499
21.172524	1138.629752	12.261504
21.307429	1128.077234	12.266509
21.451458	1127.160289	12.271514
20.929736	1116.300891	12.276519
20.864221	1111.843609	12.281523
21.085643	1115.903551	12.286528
20.832830	1123.590037	12.291533
21.062073	1129.381206	12.296538
21.080856	1131.785163	12.301543
21.194399	1140.017258	12.306547
21.215981	1144.355117	12.311552
21.003376	1131.866906	12.316557
21.302341	1134.500590	12.321562
21.084513	1124.986890	12.326567
21.082722	1112.879063	12.331571
20.856808	1106.974336	12.336576
21.106025	1114.605181	12.341581
21.047721	1112.804203	12.346586
20.850247	1129.249098	12.351591
21.169980	1133.754672	12.356595
21.150331	1142.530831	12.361600
21.140737	1137.306812	12.366605
21.331184	1117.918268	12.371610
21.067139	1115.458539	12.376615
20.940770	1110.599336	12.381619
21.161616	1118.001295	12.386624
20.952178	1111.826614	12.391629
21.074186	1108.467853	12.396634
20.953161	1117.737248	12.401639
21.449356	1116.640324	12.406643
21.085542	1114.708286	12.411648
20.966063	1114.226868	12.416653
20.789797	1114.588806	12.421658
20.841360	1129.064364	12.426663
20.842516	1137.185060	12.431667
21.245890	1145.844853	12.436672
21.386188	1145.642152	12.441677
21.054397	1133.466297	12.446682
21.023885	1137.711527	12.451687
21.289370	1131.805684	12.456691
20.987805	1134.336443	12.461696
21.221100	1133.988795	12.466701
21.437195	1126.363091	12.471706
20.995491	1118.972431	12.476711
21.224023	1117.198246	12.481715
21.334710	1122.349874	12.486720
21.256536	1116.082494	12.491725
21.111130	1115.371797	12.496730
21.199799	1115.607098	12.501735
21.209297	1116.027723	12.506739
21.338519	1130.137620	12.511744
21.472548	1119.677509	12.516749
21.516917	1117.888541	12.521754
21.250378	1126.615754	12.526759
21.505825	1102.582481	12.531763
20.983446	1097.657127	12.536768
21.002695	1091.946712	12.541773
21.090010	1088.058845	12.546778
20.676251	1091.422865	12.551783
20.959924	1102.410632	12.556787
21.347618	1117.540690	12.561792
21.229186	1106.828303	12.566797
21.063791	1095.658953	12.571802
20.870172	1090.211177	12.576807
20.944194	1100.291632	12.581811
20.939560	1115.950309	12.586816
21.188420	1121.652393	12.591821
21.355639	1117.702093	12.596826
20.809712	1120.058918	12.601831
21.164828	1116.638525	12.606835
21.202321	1112.919466	12.611840
21.244607	1113.051767	12.616845
21.175333	1094.534251	12.621850
20.977820	1098.691767	12.626855
20.778390	1087.232143	12.631859
20.607290	1100.758279	12.636864
21.068748	1110.310110	12.641869
21.293476	1113.064454	12.646874
21.239452	1123.299405	12.651879
21.252846	1116.583709	12.656883
21.169515	1114.425562	12.661888
20.993302	1104.831112	12.666893
20.987283	1096.658894	12.671898
21.058453	1114.765001	12.676903
21.037430	1110.805302	12.681907
20.995733	1108.538001	12.686912
20.959462	1123.976993	12.691917
21.041862	1120.128542	12.696922
21.260720	1135.481113	12.701927
21.166537	1128.774686	12.706931
21.003996	1120.690508	12.711936
21.173533	1120.635336	12.716941
20.962112	1113.762305	12.721946
20.811556	1128.263795	12.726951
21.245085	1123.335778	12.731955
21.176947	1131.495913	12.736960
21.291214	1129.987561	12.741965
21.218216	1109.704239	12.746970
20.859629	1104.792184	12.751975
20.775031	1103.319499	12.756979
21.070077	1111.891673	12.761984
21.168922	1130.045429	12.766989
21.302654	1131.148058	12.771994
21.278137	1120.135221	12.776999
21.007363	1098.237734	12.782003
20.924287	1104.337361	12.787008
20.859073	1109.303343	12.792013
21.090975	1116.004083	12.797018
21.288722	1131.239368	12.802023
21.289445	1115.323169	12.807027
21.020229	1108.350538	12.812032
20.929133	1101.907010	12.817037
21.095016	1102.449362	12.822042
20.957188	1105.075436	12.827047
21.309244	1113.700025	12.832051
21.207914	1111.649627	12.837056
21.016063	1105.991806	12.842061
21.179460	1104.127865	12.847066
20.871617	1112.467377	12.852071
21.370580	1104.706667	12.857075
21.623019	1108.689900	12.862080
21.684913	1106.277539	12.867085
21.617391	1108.565147	12.872090
21.287964	1107.625155	12.877095
21.477606	1098.099309	12.882099
21.387937	1095.666967	12.887104
21.222465	1074.735265	12.892109
21.263960	1074.830629	12.897114
20.696659	1078.705680	12.902119
20.892031	1072.844164	12.907123
20.865433	1063.749479	12.912128
20.902767	1071.384923	12.917133
21.182922	1085.232555	12.922138
20.921200	1086.662430	12.927143
20.934723	1095.801527	12.932147
20.890455	1098.664227	12.937152
20.889964	1101.873221	12.942157
21.267213	1105.663849	12.947162
20.882590	1111.802905	12.952167
21.057906	1107.930961	12.957171
20.888887	1114.599449	12.962176
20.765656	1112.394832	12.967181
21.057877	1109.195809	12.972186
21.015940	1114.699822	12.977191
21.232508	1095.244057	12.982195
20.842034	1121.360677	12.987200
20.971501	1107.933155	12.992205
21.157533	1110.050993	12.997210
21.062330	1114.767844	13.002215
21.214689	1114.812406	13.007219
21.410513	1116.909757	13.012224
21.152044	1112.175715	13.017229
21.268116	1111.637009	13.022234
21.114245	1112.639629	13.027239
21.363664	1111.321845	13.032243
21.402635	1110.302586	13.037248
20.939338	1101.057528	13.042253
20.804252	1097.059251	13.047258
20.871504	1111.222385	13.052263
21.172836	1110.269309	13.057267
21.298653	1125.833064	13.062272
21.099703	1113.646287	13.067277
21.443348	1121.433981	13.072282
21.042837	1104.723839	13.077287
21.192853	1088.561481	13.082291
21.182107	1086.317634	13.087296
20.828879	1093.042307	13.092301
21.099455	1083.126628	13.097306
20.775513	1084.989884	13.102311
21.155892	1103.793420	13.107315
21.162703	1104.582732	13.112320
20.956092	1097.829591	13.117325
21.268486	1099.872071	13.122330
20.941840	1092.250161	13.127335
21.139923	1089.689909	13.132339
20.941374	1100.355583	13.137344
21.138892	1109.764205	13.142349
21.336745	1085.326940	13.147354
21.404044	1089.541572	13.152359
21.055970	1084.752439	13.157363
21.332850	1086.276979	13.162368
21.400901	1088.116346	13.167373
21.125288	1078.489666	13.172378
20.769690	1092.510476	13.177383
21.332665	1074.191786	13.182387
21.408514	1088.911038	13.187392
21.279327	1087.087462	13.192397
21.311616	1082.609857	13.197402
21.084261	1090.000497	13.202407
21.083896	1083.140339	13.207411
20.791253	1094.379319	13.212416
21.008108	1094.245628	13.217421
21.158490	1089.875353	13.222426
21.219972	1085.616253	13.227431
21.214711	1084.939978	13.232435
21.050855	1088.726231	13.237440
20.922832	1088.842328	13.242445
21.343439	1083.737382	13.247450
21.036094	1093.791135	13.252455
21.103969	1088.488537	13.257459
21.032928	1089.936097	13.262464
20.892588	1088.959637	13.267469
21.133770	1085.302721	13.272474
20.835732	1101.012127	13.277479
20.949141	1087.220504	13.282483
21.210646	1091.049305	13.287488
20.942769	1091.928169	13.292493
21.087267	1097.706821	13.297498
21.134174	1097.011973	13.302503
20.976817	1097.124075	13.307507
21.037728	1102.372744	13.312512
20.933681	1090.857685	13.317517
21.085117	1096.003593	13.322522
21.104318	1097.774263	13.327527
21.103658	1092.596937	13.332531
21.025031	1100.597861	13.337536
21.010544	1100.318127	13.342541
21.086299	1095.424321	13.347546
20.822476	1101.273628	13.352551
21.071813	1100.078084	13.357555
20.671712	1103.739581	13.362560
20.745699	1099.055025	13.367565
20.816138	1099.745079	13.372570
20.750594	1115.087796	13.377575
21.086216	1115.273454	13.382579
21.215279	1133.327766	13.387584
21.294945	1123.743744	13.392589
21.204996	1113.092260	13.397594
21.062357	1110.659691	13.402599
21.140035	1092.974325	13.407603
21.188029	1101.743613	13.412608
20.847542	1110.155359	13.417613
20.918421	1101.535587	13.422618
20.771742	1106.460153	13.427623
20.933947	1121.219285	13.432627
21.313609	1138.639054	13.437632
21.338656	1134.022224	13.442637
21.366286	1116.849493	13.447642
21.089275	1124.157386	13.452647
21.179131	1104.072046	13.457651
21.133654	1102.592333	13.462656
21.227527	1103.584612	13.467661
21.200580	1102.428407	13.472666
20.929361	1108.371158	13.477671
21.156025	1104.487082	13.482675
21.304274	1100.879682	13.487680
21.140541	1104.477453	13.492685
21.375063	1098.565522	13.497690
21.051626	1110.776203	13.502695
21.284962	1104.192604	13.507699
21.343342	1107.103594	13.512704
20.865869	1108.225650	13.517709
21.512370	1106.581146	13.522714
20.941817	1107.972754	13.527719
21.288322	1105.251615	13.532723
21.210561	1107.002268	13.537728
21.235245	1109.109569	13.542733
21.254418	1108.453841	13.547738
20.799654	1107.271252	13.552743
20.928415	1098.619380	13.557747
21.304380	1106.823791	13.562752
20.920863	1113.756753	13.567757
21.213943	1108.020001	13.572762
20.889612	1110.473954	13.577767
21.254245	1107.448692	13.582771
21.438569	1105.980425	13.587776
21.325975	1100.006367	13.592781
20.866444	1085.056269	13.597786
20.565232	1087.053897	13.602791
20.901549	1091.124681	13.607795
20.793723	1106.325095	13.612800
20.815750	1113.693316	13.617805
21.417391	1110.873124	13.622810
21.425918	1116.469236	13.627815
21.154031	1116.013705	13.632819
21.361395	1114.208989	13.637824
21.014892	1104.569943	13.642829
21.222458	1092.581719	13.647834
20.965000	1091.254894	13.652839
20.979408	1094.114542	13.657843
21.169026	1090.798622	13.662848
21.183201	1094.010794	13.667853
21.275284	1084.133838	13.672858
20.719429	1087.951866	13.677863
20.998763	1089.460244	13.682867
21.260600	1094.021566	13.687872
20.923316	1095.109430	13.692877
21.201676	1090.685621	13.697882
21.022719	1093.891537	13.702887
21.372654	1089.677897	13.707891
21.162040	1086.520448	13.712896
20.686258	1097.429848	13.717901
21.323971	1086.873646	13.722906
20.958205	1090.370374	13.727911
21.120667	1083.748410	13.732915
20.981077	1091.513023	13.737920
21.022913	1089.857729	13.742925
20.961042	1086.053591	13.747930
21.178414	1095.012710	13.752935
21.376322	1097.656199	13.757939
21.408357	1100.973557	13.762944
21.226066	1091.943906	13.767949
21.522894	1085.468472	13.772954
21.261347	1095.276775	13.777959
21.415010	1084.701582	13.782963
21.282483	1091.642600	13.787968
21.291672	1091.296793	13.792973
21.553219	1075.305912	13.797978
20.841881	1082.576611	13.802983
21.091302	1073.843999	13.807987
21.226763	1088.377894	13.812992
20.755251	1073.061461	13.817997
21.361008	1081.289132	13.823002
21.176117	1070.025919	13.828007
20.963083	1063.127935	13.833011
20.969220	1074.816033	13.838016
20.857922	1081.694518	13.843021
21.229529	1081.685969	13.848026
20.834501	1087.538850	13.853031
20.858202	1091.134320	13.858035
21.095017	1092.860026	13.863040
21.184702	1087.850448	13.868045
21.399135	1090.151430	13.873050
20.967795	1090.520147	13.878055
20.678512	1096.669223	13.883059
20.961039	1094.574158	13.888064
20.771256	1099.367598	13.893069
21.097706	1093.693345	13.898074
20.797690	1101.287201	13.903079
21.074343	1103.153226	13.908083
21.140783	1095.086948	13.913088
21.101178	1092.119073	13.918093
21.209480	1095.943137	13.923098
21.170890	1098.845148	13.928103
21.052952	1099.734003	13.933107
21.143068	1108.887702	13.938112
21.123747	1103.584814	13.943117
21.543141	1092.909662	13.948122
21.045647	1103.376205	13.953127
21.159009	1104.472619	13.958131
21.241263	1107.017851	13.963136
20.851800	1097.030811	13.968141
20.962623	1095.800586	13.973146
21.218041	1105.147923	13.978151
21.158874	1097.245986	13.983155
21.255220	1093.257319	13.988160
21.086434	1098.338389	13.993165
21.224645	1091.418271	13.998170
20.734612	1083.174231	14.003175
21.271051	1090.242741	14.008179
21.266734	1096.779281	14.013184
20.666011	1079.680014	14.018189
21.007323	1088.627441	14.023207
20.657847	1094.724144	14.028224
21.180972	1095.255254	14.033242
21.050120	1106.323475	14.038259
20.860411	1115.433144	14.043277
20.994440	1098.334454	14.048295
20.707484	1109.462186	14.053312
21.040126	1103.024960	14.058330
20.828409	1099.911221	14.063347
21.097833	1105.510425	14.068365
21.132259	1102.621702	14.073383
21.078685	1103.749768	14.078400
21.235096	1124.172239	14.083418
21.400494	1127.282095	14.088435
21.500279	1131.280208	14.093453
21.440287	1126.122397	14.098471
21.048423	1122.546581	14.103488
21.442140	1128.256535	14.108506
21.562745	1132.731124	14.113523
21.350994	1138.289111	14.118541
21.076164	1133.505358	14.123559
21.138133	1143.073572	14.128576
21.319509	1134.290581	14.133594
21.341876	1138.588136	14.138611
21.183079	1142.735258	14.143629
21.506808	1135.023653	14.148647
21.636507	1134.340161	14.153664
21.438610	1138.611501	14.158682
21.518564	1140.635390	14.163699
21.374845	1136.714805	14.168717
21.514655	1136.721866	14.173735
21.279286	1147.275082	14.178752
21.558755	1145.047294	14.183770
21.675705	1132.889262	14.188787
21.513123	1135.381295	14.193805
21.746168	1149.302529	14.198823
21.905310	1164.356403	14.203840
21.911836	1160.633654	14.208858
21.733292	1142.972833	14.213875
21.885076	1143.310696	14.218893
22.247678	1140.747162	14.223911
21.901137	1149.781191	14.228928
21.952283	1136.338201	14.233946
21.857568	1143.147802	14.238963
21.390588	1137.614439	14.243981
21.542619	1141.273869	14.248999
21.493634	1157.616272	14.254016
21.591278	1168.553705	14.259034
21.915427	1165.134239	14.264051
21.702268	1176.519252	14.269069
21.775247	1169.406080	14.274087
21.933524	1179.613368	14.279104
21.759567	1175.938281	14.284122
21.964636	1178.058628	14.289139
21.953226	1179.343577	14.294157
22.372095	1176.506780	14.299175
21.845474	1175.124121	14.304192
21.993140	1174.313486	14.309210
22.273321	1174.701658	14.314227
22.095300	1183.342292	14.319245
22.365050	1171.209407	14.324263
21.948153	1179.697010	14.329280
22.088360	1182.797525	14.334298
22.239538	1179.128779	14.339315
21.754793	1186.962571	14.344333
22.094471	1177.257632	14.349351
22.093744	1206.694022	14.354368
22.238683	1210.014809	14.359386
22.634679	1203.655528	14.364403
22.575166	1208.854972	14.369421
22.178838	1186.174435	14.374439
22.290974	1199.787011	14.379456
22.515015	1203.951737	14.384474
22.861255	1192.929047	14.389491
22.073024	1191.351364	14.394509
22.453239	1184.269405	14.399527
22.680555	1195.790248	14.404544
22.460172	1192.256278	14.409562
22.431137	1186.992042	14.414579
22.815737	1183.121672	14.419597
22.747328	1178.399363	14.424615
22.430644	1177.910563	14.429632
22.510785	1177.189355	14.434650
22.653502	1174.024568	14.439667
22.214785	1187.244417	14.444685
22.502117	1186.651402	14.449703
22.670719	1202.152142	14.454720
22.516328	1200.851684	14.459738
22.980241	1206.127305	14.464755
22.714361	1207.485097	14.469773
22.933781	1208.800086	14.474791
23.031948	1209.093803	14.479808
22.734886	1199.810545	14.484826
22.991430	1178.130201	14.489843
22.608123	1178.825566	14.494861
22.790123	1180.185063	14.499879
22.867793	1185.670946	14.504896
22.786353	1190.839273	14.509914
22.755005	1196.470759	14.514931
23.003847	1198.776045	14.519949
23.111831	1203.900790	14.524967
22.795297	1200.720374	14.529984
22.954604	1208.136034	14.535002
23.222993	1204.226777	14.540019
23.010572	1212.026582	14.545037
22.881138	1203.702923	14.550055
22.819503	1199.801477	14.555072
22.861932	1206.955766	14.560090
22.999417	1205.559984	14.565107
23.075057	1207.963690	14.570125
23.063188	1211.175776	14.575143
22.829772	1205.218930	14.580160
23.067624	1208.165441	14.585178
23.244954	1200.590418	14.590195
22.939362	1204.230834	14.595213
23.115252	1198.837946	14.600231
23.326924	1203.272074	14.605248
23.206696	1208.094218	14.610266
23.316668	1202.817242	14.615283
23.534867	1208.447467	14.620301
23.305319	1206.480987	14.625319
23.390428	1201.927675	14.630336
23.230159	1203.374018	14.635354
23.469024	1192.470709	14.640371
22.939593	1206.425529	14.645389
23.022148	1204.509157	14.650407
23.405895	1198.237566	14.655424
23.308738	1206.283264	14.660442
23.342367	1198.443285	14.665459
23.543212	1214.356556	14.670477
23.527420	1212.428341	14.675495
23.518993	1220.278199	14.680512
23.580526	1235.435024	14.685530
23.877057	1227.067789	14.690547
23.709137	1208.084566	14.695565
23.496509	1202.649825	14.700583
23.659798	1197.875606	14.705600
23.543197	1200.895959	14.710618
23.754570	1203.321274	14.715635
23.509272	1211.671405	14.720653
23.596488	1226.094201	14.725671
23.869495	1226.272721	14.730688
23.854154	1239.672062	14.735706
24.069258	1220.434233	14.740723
23.826557	1211.300394	14.745741
23.586613	1210.306967	14.750759
23.855833	1214.992269	14.755776
23.826108	1225.552852	14.760794
24.062183	1237.353132	14.765811
23.797522	1228.237730	14.770829
24.075949	1225.131513	14.775847
23.735358	1216.524547	14.780864
23.623294	1239.764975	14.785882
23.930823	1234.439170	14.790899
23.749573	1241.810851	14.795917
24.051888	1236.996352	14.800935
24.228054	1233.650029	14.805952
23.934667	1236.037094	14.810970
24.003852	1229.747237	14.815987
23.960006	1235.840866	14.821005
24.049471	1230.845592	14.826023
24.349009	1226.544375	14.831040
24.251421	1238.936671	14.836058
24.464631	1233.653441	14.841075
23.966195	1235.123840	14.846093
24.124555	1242.745747	14.851111
24.211953	1235.955877	14.856128
24.019681	1241.553271	14.861146
24.188540	1234.498710	14.866163
24.140786	1239.122890	14.871181
24.400946	1236.599277	14.876199
24.459828	1229.909919	14.881216
24.570085	1236.519332	14.886234
24.566796	1230.425875	14.891251
24.547048	1239.418057	14.896269
24.336674	1230.566142	14.901287
24.591284	1233.989784	14.906304
24.330116	1230.666028	14.911322
24.461780	1223.313794	14.916339
24.484600	1229.388135	14.921357
24.534920	1229.514870	14.926375
24.721927	1226.984837	14.931392
24.437224	1235.919387	14.936410
24.632559	1228.162143	14.941427
24.649620	1238.036474	14.946445
24.330213	1236.740312	14.951463
24.437839	1239.945928	14.956480
24.486386	1240.293968	14.961498
24.349663	1236.854400	14.966515
24.727689	1241.719780	14.971533
24.798222	1256.788671	14.976551
25.040933	1247.451531	14.981568
24.891541	1248.426569	14.986586
25.201398	1238.344865	14.991603
24.860137	1235.674928	14.996621
24.623995	1241.232912	15.001639
24.645186	1236.229649	15.006656
24.730879	1230.792145	15.011674
24.727317	1243.587108	15.016691
24.628906	1263.383421	15.021709
24.907558	1273.485839	15.026727
25.126739	1269.011013	15.031744
25.090225	1273.847355	15.036762
24.905594	1266.632860	15.041779
25.052959	1261.356191	15.046797
24.777367	1266.338424	15.051815
24.889810	1269.634520	15.056832
25.210505	1270.229390	15.061850
25.133402	1270.056321	15.066867
24.963286	1267.945064	15.071885
24.866089	1273.585509	15.076903
25.200874	1266.379403	15.081920
25.098369	1272.672752	15.086938
25.331655	1266.531318	15.091955
25.377424	1269.857713	15.096973
25.259099	1268.098438	15.101991
25.590341	1260.102409	15.107008
25.239016	1261.595751	15.112026
25.234367	1264.952211	15.117043
25.242528	1266.142805	15.122061
25.178906	1265.250245	15.127079
25.218947	1271.096900	15.132096
25.186776	1281.668926	15.137114
25.489344	1296.181716	15.142131
25.693414	1296.128974	15.147149
25.698186	1297.526976	15.152167
25.622513	1281.639789	15.157184
25.304065	1271.498614	15.162202
25.637673	1283.317982	15.167219
25.675577	1287.477028	15.172237
25.513631	1287.765832	15.177255
25.548500	1291.595795	15.182272
25.400956	1295.928366	15.187290
25.581929	1296.385853	15.192307
25.501312	1299.073277	15.197325
25.640323	1306.454470	15.202343
25.466292	1301.653009	15.207360
25.455888	1298.950734	15.212378
25.281386	1302.254067	15.217395
25.687994	1299.533254	15.222413
25.429877	1302.669015	15.227431
26.182959	1304.585555	15.232448
25.760823	1311.141490	15.237466
25.729567	1300.620195	15.242483
26.143424	1316.477576	15.247501
25.834916	1313.443727	15.252519
26.139605	1321.049413	15.257536
26.229677	1305.283635	15.262554
26.150749	1298.022375	15.267571
26.117009	1297.422366	15.272589
25.990752	1301.523440	15.277607
26.076958	1294.077742	15.282624
26.166742	1297.223293	15.287642
25.857000	1303.446672	15.292659
26.009061	1299.678649	15.297677
26.157994	1317.890778	15.302695
26.440564	1315.904731	15.307712
26.725137	1321.968821	15.312730
26.467226	1305.082641	15.317747
26.248311	1295.620105	15.322765
26.028221	1299.022736	15.327783
26.536868	1291.960354	15.332800
26.342272	1294.915298	15.337818
26.194489	1295.913679	15.342835
26.527059	1290.835559	15.347853
26.268022	1290.435092	15.352871
26.594379	1289.844501	15.357888
26.238633	1299.262357	15.362906
26.674309	1296.843667	15.367923
26.625843	1284.070061	15.372941
26.146335	1302.421742	15.377959
26.605861	1318.057895	15.382976
26.514038	1331.564694	15.387994
26.546396	1324.421744	15.393011
26.914722	1321.823445	15.398029
26.731906	1308.160411	15.403047
26.756175	1299.724871	15.408064
26.584412	1302.569989	15.413082
26.564261	1301.088437	15.418099
26.812681	1312.664213	15.423117
26.655116	1328.482186	15.428135
26.979202	1315.323491	15.433152
26.939555	1300.272943	15.438170
26.761984	1299.601489	15.443187
26.909778	1299.834593	15.448205
26.624943	1306.499194	15.453223
26.811032	1321.375889	15.458240
26.655487	1316.891605	15.463258
26.706813	1326.578834	15.468275
26.967722	1319.231893	15.473293
26.613339	1333.973789	15.478311
26.876225	1319.938396	15.483328
26.885199	1330.981337	15.488346
26.921993	1329.432493	15.493363
26.851003	1321.228441	15.498381
26.832091	1322.794615	15.503399
27.079613	1323.416891	15.508416
26.646220	1327.317624	15.513434
27.021316	1348.948295	15.518451
27.298592	1353.753488	15.523469
27.402337	1369.001253	15.528487
27.630874	1362.671761	15.533504
27.371371	1345.731516	15.538522
27.153530	1334.639811	15.543539
27.353939	1320.430328	15.548557
27.112984	1336.970304	15.553575
27.451383	1341.538426	15.558592
27.454866	1360.901740	15.563610
27.546876	1347.126400	15.568627
27.569141	1325.716817	15.573645
27.287552	1328.691937	15.578663
27.561257	1331.519489	15.583680
27.680183	1349.630257	15.588698
27.394251	1348.101428	15.593715
27.550733	1337.635896	15.598733
27.906687	1351.324560	15.603751
27.537648	1330.381681	15.608768
27.600707	1333.375763	15.613786
27.520810	1339.899143	15.618803
27.814044	1343.927810	15.623821
27.556366	1350.086272	15.628839
28.122522	1348.270505	15.633856
27.621631	1336.198271	15.638874
27.531654	1348.140318	15.643891
27.886723	1344.695428	15.648909
27.870060	1350.244401	15.653927
27.848182	1353.841171	15.658944
27.795585	1364.569108	15.663962
27.944377	1363.293425	15.668979
28.093917	1355.957151	15.673997
27.990135	1348.171259	15.679015
27.968392	1354.027017	15.684032
28.145850	1356.119545	15.689050
27.771106	1356.135534	15.694067
28.139761	1354.276546	15.699085
28.087339	1358.582163	15.704103
28.049870	1353.778566	15.709120
28.096165	1350.150891	15.714138
28.185824	1355.950338	15.719155
28.476303	1355.535366	15.724173
28.111225	1356.916859	15.729191
28.296905	1360.099040	15.734208
28.366862	1361.264840	15.739226
28.066171	1345.146831	15.744243
28.493569	1345.425791	15.749261
28.076264	1356.966211	15.754279
28.372034	1343.607500	15.759296
28.288865	1352.623239	15.764314
28.119836	1358.713291	15.769331
28.517266	1347.741312	15.774349
28.642096	1360.602420	15.779367
28.244063	1365.113402	15.784384
28.476671	1353.849151	15.789402
28.238607	1358.615417	15.794419
28.331304	1354.885952	15.799437
27.974226	1353.999295	15.804455
28.365161	1352.868257	15.809472
28.536271	1346.105098	15.814490
27.979638	1355.676951	15.819507
28.741564	1367.616056	15.824525
28.706595	1372.572528	15.829543
28.645699	1368.778678	15.834560
29.017927	1379.983951	15.839578
28.831978	1374.758048	15.844595
28.870020	1375.014953	15.849613
28.606847	1368.558599	15.854631
28.563589	1376.221388	15.859648
28.672660	1372.315477	15.864666
28.812081	1379.080762	15.869683
28.968424	1372.522880	15.874701
28.652556	1384.324798	15.879719
29.097484	1366.667295	15.884736
28.752466	1370.906323	15.889754
28.922859	1370.156551	15.894771
29.179941	1371.079345	15.899789
28.866368	1378.172521	15.904807
29.278630	1380.448623	15.909824
28.945538	1367.850129	15.914842
28.712504	1379.773333	15.919859
29.140185	1367.309120	15.924877
28.941688	1371.243974	15.929895
28.999241	1378.886752	15.934912
29.247512	1391.927198	15.939930
29.395291	1398.346643	15.944947
29.631347	1394.176634	15.949965
29.660571	1379.466614	15.954983
29.349148	1364.825104	15.960000
29.679791	1370.067771	15.965018
28.958320	1375.666253	15.970035
29.216696	1362.311130	15.975053
29.332393	1373.000431	15.980071
29.563970	1386.701889	15.985088
29.699990	1388.768783	15.990106
29.472873	1388.029717	15.995123
29.531616	1380.323284	16.000141
29.571817	1393.319837	16.005159
29.748532	1394.076902	16.010176
30.131541	1380.329837	16.015194
29.437008	1380.827872	16.020211
29.279870	1366.436261	16.025229
29.610167	1382.056129	16.030247
29.699533	1391.995328	16.035264
29.907277	1382.690422	16.040282
29.735209	1390.917282	16.045299
30.126172	1392.215151	16.050317
29.993461	1401.162526	16.055335
29.986559	1391.921742	16.060352
29.773945	1377.829998	16.065370
29.451421	1389.860299	16.070387
30.103638	1395.606210	16.075405
30.243565	1386.826534	16.080423
30.302942	1389.243089	16.085440
30.243459	1379.612699	16.090458
29.701424	1378.140448	16.095475
30.213841	1378.932845	16.100493
29.829518	1392.224431	16.105511
29.902107	1390.634476	16.110528
30.124014	1390.661478	16.115546
30.186501	1394.524819	16.120563
30.003311	1397.433129	16.125581
29.695378	1402.136617	16.130599
30.090606	1394.508646	16.135616
30.208645	1396.723137	16.140634
29.805151	1398.415950	16.145651
29.962207	1408.021870	16.150669
30.233664	1427.811322	16.155687
30.330545	1428.829678	16.160704
30.848848	1431.792852	16.165722
30.670744	1433.151607	16.170739
30.535115	1424.349790	16.175757
30.955132	1428.432981	16.180775
30.552583	1408.983519	16.185792
30.363278	1392.828812	16.190810
30.542659	1398.171128	16.195827
30.669646	1411.462188	16.200845
30.419631	1423.245768	16.205863
30.352641	1427.452262	16.210880
31.192385	1418.807134	16.215898
31.041706	1424.184016	16.220915
31.108794	1416.149807	16.225933
30.734488	1401.943036	16.230951
30.422876	1399.901523	16.235968
30.546226	1402.690147	16.240986
30.735267	1410.640753	16.246003
30.598592	1416.971077	16.251021
30.750977	1416.412951	16.256039
30.749786	1424.382896	16.261056
31.026792	1416.060356	16.266074
31.024924	1415.203556	16.271091
31.008924	1414.821738	16.276109
31.050049	1410.405947	16.281127
31.102552	1414.616974	16.286144
31.356347	1414.367525	16.291162
31.073434	1411.947813	16.296179
31.175448	1415.043458	16.301197
31.223537	1412.393184	16.306215
31.154077	1415.416287	16.311232
31.383774	1408.569817	16.316250
31.164949	1413.738900	16.321267
31.309561	1417.569482	16.326285
31.426351	1413.055886	16.331303
31.235020	1411.053391	16.336320
31.302687	1407.069125	16.341338
31.210689	1413.448168	16.346355
31.086862	1413.859103	16.351373
31.613955	1413.361553	16.356391
31.182112	1418.588213	16.361408
31.415958	1430.089324	16.366426
31.513165	1445.394058	16.371443
31.641871	1449.923299	16.376461
31.805779	1450.384300	16.381479
31.658745	1447.774583	16.386496
31.895978	1438.133007	16.391514
31.795549	1447.431575	16.396531
31.841689	1451.430468	16.401549
31.840296	1436.306033	16.406567
31.688234	1436.388755	16.411584
31.906404	1434.692198	16.416602
31.958763	1426.805847	16.421619
31.592411	1428.871864	16.426637
31.885778	1435.176074	16.431655
31.998538	1450.317087	16.436672
32.198771	1445.006748	16.441690
31.819945	1447.497144	16.446707
32.179773	1445.479093	16.451725
32.168897	1452.111859	16.456743
32.072430	1446.785921	16.461760
32.331256	1437.684420	16.466778
32.001158	1440.244125	16.471795
32.063568	1442.993711	16.476813
31.958869	1440.287573	16.481831
31.772753	1448.858864	16.486848
32.211162	1444.787134	16.491866
31.904545	1454.878421	16.496883
31.849231	1450.015499	16.501901
32.251320	1445.549200	16.506919
31.853928	1450.304727	16.511936
32.203491	1449.059151	16.516954
32.498489	1468.904683	16.521971
32.333540	1471.268152	16.526989
32.446426	1478.829792	16.532007
32.044528	1486.717385	16.537024
32.419675	1479.964094	16.542042
32.584689	1483.675814	16.547059
32.449230	1483.235177	16.552077
32.674552	1474.399352	16.557095
32.659144	1475.581925	16.562112
33.064707	1472.014899	16.567130
32.864301	1481.295614	16.572147
32.774887	1475.136349	16.577165
33.077186	1472.837227	16.582183
32.958217	1483.128280	16.587200
33.134909	1476.538003	16.592218
32.935835	1475.179362	16.597235
32.849824	1472.485182	16.602253
33.029521	1457.647254	16.607271
32.645026	1466.259637	16.612288
33.030574	1468.384275	16.617306
33.051060	1470.608045	16.622323
32.799769	1470.770307	16.627341
32.961356	1468.589592	16.632359
32.847816	1478.046012	16.637376
32.892706	1481.476423	16.642394
33.100354	1472.324071	16.647411
33.339592	1475.658981	16.652429
33.206088	1468.559722	16.657447
32.937802	1475.997317	16.662464
33.061458	1473.398690	16.667482
33.011100	1478.268771	16.672499
32.922718	1474.240947	16.677517
33.419637	1476.363553	16.682535
33.318501	1497.817134	16.687552
33.660204	1494.938314	16.692570
33.351504	1495.864054	16.697587
33.385308	1502.542416	16.702605
33.429753	1490.636343	16.707623
33.363531	1510.920250	16.712640
33.377475	1502.117338	16.717658
33.400106	1508.481284	16.722675
33.465030	1511.118788	16.727693
33.755830	1500.378438	16.732711
33.589605	1505.904919	16.737728
33.715162	1504.124018	16.742746
33.592448	1501.612666	16.747763
33.221334	1507.193853	16.752781
33.837283	1498.941480	16.757799
33.469347	1503.401295	16.762816
33.884983	1506.744257	16.767834
34.147328	1512.023041	16.772851
33.726410	1514.233063	16.777869
34.050372	1506.211318	16.782887
33.882675	1527.515886	16.787904
34.038912	1527.286717	16.792922
34.297935	1524.049030	16.797939
33.960071	1527.284081	16.802957
34.603128	1508.756318	16.807975
34.142204	1496.446322	16.812992
34.010748	1496.096289	16.818010
33.981732	1503.117391	16.823027
34.146853	1515.291825	16.828045
34.509181	1520.580621	16.833063
34.451365	1524.433296	16.838080
34.481617	1513.091080	16.843098
34.375583	1492.698303	16.848115
34.432176	1503.031371	16.853133
34.588899	1487.285441	16.858151
34.290138	1497.782948	16.863168
34.088163	1497.121669	16.868186
34.466284	1512.967662	16.873203
34.552835	1525.945929	16.878221
34.648741	1543.226057	16.883239
34.687830	1532.043665	16.888256
34.317485	1531.528800	16.893274
34.436018	1532.999135	16.898291
34.496665	1539.653569	16.903309
34.814508	1531.052295	16.908327
34.730492	1531.493066	16.913344
34.626508	1535.089605	16.918362
34.763001	1532.750850	16.923379
34.621367	1535.504683	16.928397
34.723323	1522.678558	16.933415
34.734789	1531.179839	16.938432
34.896064	1527.011496	16.943450
34.858082	1526.678802	16.948467
34.847505	1535.322037	16.953485
35.177827	1550.923992	16.958503
35.102129	1565.858427	16.963520
34.873965	1572.852335	16.968538
35.049004	1574.927977	16.973555
34.995988	1571.507226	16.978573
35.365677	1558.256089	16.983591
34.914306	1570.881290	16.988608
34.994985	1565.660770	16.993626
35.473180	1559.212715	16.998643
35.207463	1566.445436	17.003661
35.391587	1559.683249	17.008679
35.786906	1558.100005	17.013696
35.331929	1563.869996	17.018714
35.448300	1557.533142	17.023731
35.461670	1563.149770	17.028749
35.664654	1561.069413	17.033767
35.164692	1567.256386	17.038784
35.441682	1558.970736	17.043802
35.541156	1558.527233	17.048819
35.448704	1565.590733	17.053837
35.738398	1557.763991	17.058855
35.704416	1559.992530	17.063872
35.450546	1546.810976	17.068890
35.829392	1554.174491	17.073907
35.740446	1575.630962	17.078925
35.872854	1570.862335	17.083943
35.896060	1575.125277	17.088960
35.719529	1581.481693	17.093978
35.967068	1584.565174	17.098995
35.723347	1594.187950	17.104013
36.160216	1587.541965	17.109031
36.227767	1589.894324	17.114048
36.029898	1589.167887	17.119066
36.258361	1589.128559	17.124083
36.244597	1587.821366	17.129101
36.507680	1582.134408	17.134119
35.977900	1578.069201	17.139136
35.971350	1585.537467	17.144154
36.292224	1580.970815	17.149171
36.218294	1594.456911	17.154189
36.279327	1588.210675	17.159207
36.606398	1584.109473	17.164224
36.507404	1593.692646	17.169242
36.247898	1589.048666	17.174259
36.534929	1590.186152	17.179277
36.597152	1575.978798	17.184295
36.642775	1580.763598	17.189312
36.373597	1580.919275	17.194330
36.839436	1582.113976	17.199347
36.337931	1589.400837	17.204365
36.534667	1580.776377	17.209383
36.696156	1588.605623	17.214400
36.409026	1590.095836	17.219418
36.533112	1590.546676	17.224435
36.820655	1594.605424	17.229453
36.750837	1589.542619	17.234471
36.702026	1588.372374	17.239488
36.376898	1584.618255	17.244506
36.652692	1600.319417	17.249523
36.773198	1617.279505	17.254541
36.914007	1608.405166	17.259559
36.916479	1615.753235	17.264576
36.815795	1618.042764	17.269594
37.153243	1611.769732	17.274611
37.063020	1619.148320	17.279629
37.186729	1621.403630	17.284647
37.239158	1608.485435	17.289664
37.279729	1613.535341	17.294682
37.258213	1604.265291	17.299699
37.107142	1610.227517	17.304717
37.146979	1620.083528	17.309735
37.594764	1604.294979	17.314752
37.455068	1609.033837	17.319770
37.358850	1608.252642	17.324787
37.182505	1621.714984	17.329805
37.469477	1604.469386	17.334823
37.300277	1614.497175	17.339840
37.348510	1633.804159	17.344858
37.793995	1635.050093	17.349875
37.755787	1649.838623	17.354893
37.725861	1640.991497	17.359911
37.850409	1632.122883	17.364928
37.661736	1632.238189	17.369946
38.164956	1627.302635	17.374963
37.818730	1621.021450	17.379981
37.709781	1617.357906	17.384999
37.776649	1609.661854	17.390016
37.800677	1636.080213	17.395034
38.277648	1626.574894	17.400051
37.826795	1634.706348	17.405069
38.188387	1637.430273	17.410087
38.333200	1634.807793	17.415104
38.211803	1617.978918	17.420122
38.307344	1602.559614	17.425139
38.068932	1599.205398	17.430157
38.299452	1600.983520	17.435175
38.185112	1600.559963	17.440192
37.927221	1604.549973	17.445210
38.333537	1613.413071	17.450227
38.055564	1624.426494	17.455245
38.219309	1627.607513	17.460263
38.658341	1630.012319	17.465280
38.572056	1630.191524	17.470298
38.628837	1625.461686	17.475315
38.166596	1624.981926	17.480333
38.379527	1622.615232	17.485351
38.523809	1635.578882	17.490368
38.434286	1627.115682	17.495386
38.746934	1620.240938	17.500403
38.340070	1629.465008	17.505421
38.635955	1623.354343	17.510439
38.694589	1631.829281	17.515456
38.725215	1632.239969	17.520474
38.850250	1625.096248	17.525491
38.613504	1636.461783	17.530509
38.761345	1626.789507	17.535527
39.156727	1627.588790	17.540544
38.449662	1639.616133	17.545562
39.273785	1639.930930	17.550579
39.085309	1655.758121	17.555597
39.355219	1649.588662	17.560615
39.225085	1623.824851	17.565632
39.032784	1618.350528	17.570650
39.431033	1612.342313	17.575667
39.010851	1618.340388	17.580685
39.265424	1631.713554	17.585703
39.589202	1625.222455	17.590720
39.504139	1628.475411	17.595738
39.723954	1614.450539	17.600755
39.656265	1604.929070	17.605773
39.340601	1616.386621	17.610791
39.494861	1609.306678	17.615808
39.580423	1613.935669	17.620826
39.516003	1606.851279	17.625843
39.584817	1618.378864	17.630861
39.450549	1614.890832	17.635879
40.048918	1609.913364	17.640896
39.745632	1611.237829	17.645914
39.523217	1610.740266	17.650931
39.643064	1615.154559	17.655949
39.447048	1607.916539	17.660967
39.615930	1620.561621	17.665984
39.640792	1634.632155	17.671002
39.610632	1638.457638	17.676019
39.716599	1635.573131	17.681037
39.990370	1639.568803	17.686055
39.912678	1651.361262	17.691072
39.665373	1640.539100	17.696090
39.912159	1643.540910	17.701107
39.805505	1643.787076	17.706125
39.915004	1638.013688	17.711143
39.808035	1647.360621	17.716160
40.041778	1662.734262	17.721178
40.077125	1663.383319	17.726195
40.140264	1668.728545	17.731213
40.123755	1669.114503	17.736231
40.161435	1663.764728	17.741248
40.174095	1675.384692	17.746266
40.594693	1671.241017	17.751283
40.487332	1675.021403	17.756301
40.607546	1669.026837	17.761319
40.599822	1663.493166	17.766336
40.549028	1671.482956	17.771354
40.301089	1671.472423	17.776371
40.425670	1671.178295	17.781389
40.553664	1680.494064	17.786407
41.108748	1681.983667	17.791424
40.589179	1699.373165	17.796442
40.957511	1705.443720	17.801459
40.962170	1698.391530	17.806477
40.647419	1702.303325	17.811495
41.037376	1705.170617	17.816512
41.083768	1705.097404	17.821530
41.297571	1702.649541	17.826547
41.543336	1698.580154	17.831565
41.260502	1686.156639	17.836583
41.344015	1665.559551	17.841600
41.086322	1674.167560	17.846618
40.997973	1666.386115	17.851635
41.336301	1668.648889	17.856653
41.202167	1671.113662	17.861671
41.315910	1661.375223	17.866688
41.607877	1678.453552	17.871706
41.278193	1671.731581	17.876723
41.467666	1672.889355	17.881741
41.257457	1680.992676	17.886759
41.430796	1681.961099	17.891776
41.589394	1701.569921	17.896794
41.756560	1698.342915	17.901811
41.820589	1698.646022	17.906829
41.788065	1687.576402	17.911847
41.660920	1665.901476	17.916864
41.359095	1673.629262	17.921882
41.591376	1686.294965	17.926899
41.784887	1688.726358	17.931917
41.684388	1701.817208	17.936935
41.623314	1695.820085	17.941952
41.582319	1706.208192	17.946970
41.654978	1698.361720	17.951987
42.004589	1702.007869	17.957005
41.867197	1694.626736	17.962023
41.607986	1691.983739	17.967040
41.729443	1708.742418	17.972058
41.927483	1719.093194	17.977075
42.003305	1733.554493	17.982093
41.847421	1733.251612	17.987111
42.086357	1724.750909	17.992128
42.078121	1736.005347	17.997146
42.261211	1724.664546	18.002163
42.393314	1731.453187	18.007181
42.316792	1737.775628	18.012199
42.613602	1729.043875	18.017216
42.146062	1729.180064	18.022234
42.634284	1723.590074	18.027251
42.791746	1730.140268	18.032269
42.254883	1730.611587	18.037287
42.591508	1736.691146	18.042304
42.812643	1762.552857	18.047322
43.056594	1766.163962	18.052339
43.176976	1757.454827	18.057357
42.734999	1749.651085	18.062375
42.972329	1736.195150	18.067392
43.003167	1727.663925	18.072410
42.514914	1723.460692	18.077427
42.814210	1745.450929	18.082445
42.850386	1760.857760	18.087463
42.998386	1754.646350	18.092480
42.774931	1756.949976	18.097498
42.913752	1762.181695	18.102515
43.138248	1754.622462	18.107533
43.087255	1759.216645	18.112551
43.239016	1754.698939	18.117568
43.113152	1752.021290	18.122586
43.291648	1755.034016	18.127603
43.363441	1754.660209	18.132621
43.196881	1765.604051	18.137639
43.607626	1752.998269	18.142656
43.401857	1760.528292	18.147674
43.080106	1779.964490	18.152691
43.656025	1778.232069	18.157709
43.321730	1787.110363	18.162727
43.691546	1778.625723	18.167744
43.524698	1782.613844	18.172762
43.659193	1780.852723	18.177779
43.873151	1776.943346	18.182797
43.723965	1780.039807	18.187815
43.908418	1770.331706	18.192832
43.828745	1775.268702	18.197850
43.715972	1773.695687	18.202867
43.889859	1773.839687	18.207885
43.808481	1781.359318	18.212903
43.682648	1777.403456	18.217920
43.752977	1791.565213	18.222938
44.137043	1795.981465	18.227955
44.399667	1795.939049	18.232973
44.126146	1801.421401	18.237991
44.559381	1794.161578	18.243008
44.190201	1781.985369	18.248026
44.602962	1784.807351	18.253043
44.271653	1774.376049	18.258061
44.079715	1789.280485	18.263079
44.654310	1792.023953	18.268096
44.469118	1799.168432	18.273114
44.844729	1801.617207	18.278131
44.754774	1802.423909	18.283149
44.555362	1797.856800	18.288167
44.843801	1795.655805	18.293184
44.622059	1805.212286	18.298202
44.532598	1804.039855	18.303219
44.917224	1806.378644	18.308237
44.545307	1793.420994	18.313255
44.728690	1797.654519	18.318272
44.751032	1794.605551	18.323290
44.625555	1796.265859	18.328307
44.786133	1785.782048	18.333325
44.792237	1792.553846	18.338343
44.686309	1794.158335	18.343360
44.797320	1807.039346	18.348378
45.196874	1822.483460	18.353395
45.133114	1815.627761	18.358413
45.473889	1822.819717	18.363431
45.677815	1811.943545	18.368448
45.616501	1819.856436	18.373466
45.782894	1817.808624	18.378483
46.006528	1789.389205	18.383501
45.670823	1794.235685	18.388519
46.054016	1786.434024	18.393536
46.076959	1787.400486	18.398554
45.535414	1787.556344	18.403571
45.986512	1781.568736	18.408589
45.738818	1782.404529	18.413607
45.443252	1785.562096	18.418624
45.791768	1784.723327	18.423642
45.492713	1787.006766	18.428659
46.043022	1769.893593	18.433677
45.614049	1787.949928	18.438695
45.510425	1786.061604	18.443712
45.732599	1784.489437	18.448730
45.280499	1792.012357	18.453747
45.777833	1805.889708	18.458765
45.709765	1817.877412	18.463783
45.968732	1809.831260	18.468800
45.968508	1810.178441	18.473818
45.884096	1818.598432	18.478835
45.992992	1811.282572	18.483853
45.769728	1824.375021	18.488871
45.857291	1834.598769	18.493888
46.747122	1838.895034	18.498906
46.710167	1844.390797	18.503923
46.894167	1842.765718	18.508941
46.481705	1853.045637	18.513959
46.921528	1840.742699	18.518976
46.614577	1830.352307	18.523994
46.164762	1819.626026	18.529011
46.879139	1826.155867	18.534029
46.826854	1841.329118	18.539047
46.568191	1841.537393	18.544064
46.870499	1845.429461	18.549082
47.163211	1842.919434	18.554099
46.977141	1839.073060	18.559117
46.660657	1838.197198	18.564135
46.860909	1839.048857	18.569152
47.026297	1837.293814	18.574170
46.788440	1841.698371	18.579187
47.072802	1839.522403	18.584205
47.094609	1837.285271	18.589223
47.198940	1833.191212	18.594240
47.554463	1831.596197	18.599258
47.281572	1838.577701	18.604275
47.274365	1834.723250	18.609293
47.006493	1832.868984	18.614311
47.351535	1837.300126	18.619328
47.538119	1831.762142	18.624346
47.062961	1847.111398	18.629363
47.607525	1851.029327	18.634381
47.621881	1858.849151	18.639399
47.448875	1863.538342	18.644416
47.682811	1868.786392	18.649434
47.610437	1865.124030	18.654451
48.027737	1864.779277	18.659469
47.965171	1853.647462	18.664487
48.294643	1850.878289	18.669504
48.517611	1848.109585	18.674522
48.217756	1850.364844	18.679539
48.108343	1828.914957	18.684557
48.168431	1829.033847	18.689575
48.253690	1825.506816	18.694592
48.584814	1819.002662	18.699610
48.428780	1812.756343	18.704627
48.521528	1810.200344	18.709645
48.368165	1823.313107	18.714663
48.481999	1820.834762	18.719680
48.457929	1821.589266	18.724698
48.034688	1814.935638	18.729715
48.176053	1808.930562	18.734733
48.472997	1818.490845	18.739751
48.374787	1821.948094	18.744768
48.570572	1819.716252	18.749786
48.620381	1819.395505	18.754803
48.976265	1830.809823	18.759821
48.655203	1825.777570	18.764839
48.400819	1817.033785	18.769856
48.796221	1830.161281	18.774874
48.969584	1844.658261	18.779891
48.789739	1842.461158	18.784909
48.744095	1845.108493	18.789927
48.788925	1857.259925	18.794944
48.958964	1848.461011	18.799962
48.646505	1850.103167	18.804979
48.957463	1843.359949	18.809997
48.868206	1840.641047	18.815015
48.732954	1841.093932	18.820032
48.986573	1862.099743	18.825050
49.089980	1879.116352	18.830067
49.289685	1877.106482	18.835085
49.495671	1880.361052	18.840103
49.339358	1878.233344	18.845120
49.803392	1877.301418	18.850138
49.632319	1883.985103	18.855155
50.068009	1869.335611	18.860173
49.819951	1878.102667	18.865191
49.544659	1877.628473	18.870208
49.950234	1871.652810	18.875226
49.337480	1878.667303	18.880243
49.702189	1874.248528	18.885261
50.102562	1874.924324	18.890279
49.945361	1876.603073	18.895296
49.988690	1875.015374	18.900314
49.902327	1870.374362	18.905331
50.155129	1866.753738	18.910349
50.011242	1871.664825	18.915367
49.966260	1868.380376	18.920384
50.154219	1866.923780	18.925402
49.839089	1877.535864	18.930419
50.375651	1886.202947	18.935437
50.437742	1895.608025	18.940455
50.643518	1889.329921	18.945472
50.598887	1890.440102	18.950490
50.347870	1893.834430	18.955507
50.593284	1892.785561	18.960525
50.726303	1896.966581	18.965543
50.103230	1903.596515	18.970560
50.736204	1901.689798	18.975578
50.488365	1903.964299	18.980595
50.294461	1902.124183	18.985613
50.551363	1902.146394	18.990631
50.218605	1906.208207	18.995648
50.482544	1910.349470	19.000666
50.315702	1926.636020	19.005683
50.796803	1933.108727	19.010701
50.784912	1936.351654	19.015719
50.998417	1944.231003	19.020736
51.319158	1930.063877	19.025754
51.244149	1931.623332	19.030771
51.119915	1935.088692	19.035789
51.263591	1931.745820	19.040807
51.115907	1935.016698	19.045824
50.934627	1931.294603	19.050842
51.117230	1953.969228	19.055859
51.325074	1963.036464	19.060877
51.477254	1962.822882	19.065895
51.218802	1963.929416	19.070912
51.555007	1964.518700	19.075930
51.655423	1974.985128	19.080947
51.792659	1967.850306	19.085965
51.788906	1967.385500	19.090983
51.891456	1957.372554	19.096000
52.118288	1956.149662	19.101018
51.925712	1959.684922	19.106035
51.928830	1952.505426	19.111053
52.082462	1959.948335	19.116071
51.862078	1961.270617	19.121088
52.165463	1951.229575	19.126106
52.275874	1957.638711	19.131123
52.284078	1958.765641	19.136141
52.339200	1956.558574	19.141159
52.001546	1958.175656	19.146176
52.296177	1949.079927	19.151194
52.105070	1970.100193	19.156211
52.696560	1973.163508	19.161229
52.520702	1977.237285	19.166247
52.288712	1985.057925	19.171264
52.558660	1989.955747	19.176282
52.250189	1985.544415	19.181299
52.295086	1982.814314	19.186317
52.554118	1984.542315	19.191335
52.488987	1993.307007	19.196352
52.620910	1985.600381	19.201370
52.735869	2010.988633	19.206387
52.664615	2009.322443	19.211405
53.029818	2009.095334	19.216423
53.058717	2023.214368	19.221440
53.604742	2002.781374	19.226458
53.632215	2003.047055	19.231475
53.536326	1999.284579	19.236493
53.785148	1980.761683	19.241511
53.497357	1979.504455	19.246528
53.536101	1965.155734	19.251546
53.492493	1972.106235	19.256563
53.521607	1967.421603	19.261581
53.570885	1961.750511	19.266599
53.308778	1973.316214	19.271616
53.637221	1954.878189	19.276634
53.284270	1959.958732	19.281651
53.607667	1968.875393	19.286669
53.802457	1974.321655	19.291687
53.972391	1984.167389	19.296704
53.877345	1972.969870	19.301722
53.987940	1966.783215	19.306739
53.787535	1973.554211	19.311757
54.117790	1989.328128	19.316775
54.081448	1993.892518	19.321792
54.237927	1992.097975	19.326810
53.937957	1987.118936	19.331827
53.891395	1996.081250	19.336845
54.097465	1995.523981	19.341863
54.140902	2001.165873	19.346880
54.239887	1992.861176	19.351898
54.189584	1997.637029	19.356915
54.258812	1990.071763	19.361933
54.285535	1995.168060	19.366951
54.442432	1996.437248	19.371968
54.541151	1989.767146	19.376986
54.382738	2001.898414	19.382003
54.452812	2018.919717	19.387021
54.801655	2027.474453	19.392039
54.635479	2029.193194	19.397056
54.956736	2027.806567	19.402074
55.038886	2020.372160	19.407091
54.873908	2021.507052	19.412109
54.880018	2018.416576	19.417127
54.684366	2021.680965	19.422144
55.106271	2010.694365	19.427162
55.531740	2016.485351	19.432179
55.488130	2008.654897	19.437197
55.343155	2009.046409	19.442215
55.217708	2013.112155	19.447232
55.393345	2010.624706	19.452250
55.218644	2021.562958	19.457267
55.286385	2017.484123	19.462285
55.450837	2009.769937	19.467303
55.587189	2021.226500	19.472320
55.736259	2031.891297	19.477338
55.758635	2043.576079	19.482355
55.806491	2048.683183	19.487373
56.305572	2042.726361	19.492391
55.798028	2023.332148	19.497408
56.031462	2005.956177	19.502426
56.019503	2010.533202	19.507443
56.118456	2012.134139	19.512461
56.007868	2013.393291	19.517479
56.186063	2030.439052	19.522496
56.204643	2034.323725	19.527514
56.197323	2033.102777	19.532531
56.106771	2042.194058	19.537549
56.320643	2033.516257	19.542567
56.094840	2039.344269	19.547584
56.232182	2036.982488	19.552602
56.236930	2047.042609	19.557619
56.070165	2037.332143	19.562637
56.194029	2038.146443	19.567655
56.188387	2045.470852	19.572672
56.498585	2052.221011	19.577690
56.703987	2062.537821	19.582707
56.840838	2063.385449	19.587725
56.843858	2064.975735	19.592743
56.820129	2083.689897	19.597760
56.684625	2064.802643	19.602778
56.581000	2071.526784	19.607795
56.476955	2072.727475	19.612813
56.971094	2061.943272	19.617831
56.678522	2091.324952	19.622848
57.113669	2097.242643	19.627866
57.218320	2100.065849	19.632883
56.937488	2101.804460	19.637901
57.387969	2099.271586	19.642919
56.933056	2102.374401	19.647936
57.307687	2091.576200	19.652954
57.228099	2108.693060	19.657971
57.173450	2122.515594	19.662989
57.723797	2126.355592	19.668007
57.872521	2136.316509	19.673024
57.874879	2130.287851	19.678042
58.046215	2133.090202	19.683059
57.772337	2134.144933	19.688077
58.006015	2131.187256	19.693095
57.744132	2137.473359	19.698112
57.898669	2141.090955	19.703130
58.201132	2123.843063	19.708147
58.032845	2132.450452	19.713165
58.122624	2128.243001	19.718183
57.860796	2130.750242	19.723200
57.958564	2130.452517	19.728218
58.371956	2138.540006	19.733235
58.283999	2151.088859	19.738253
58.334175	2155.145511	19.743271
58.392222	2150.973006	19.748288
58.501025	2151.202119	19.753306
58.759908	2147.014887	19.758323
58.377682	2160.706427	19.763341
58.641118	2150.851754	19.768359
58.650999	2146.974830	19.773376
58.360970	2155.252397	19.778394
58.746163	2166.645786	19.783411
58.551563	2172.003202	19.788429
58.667316	2180.181450	19.793447
58.915021	2179.379192	19.798464
59.212189	2184.939781	19.803482
59.014098	2177.106345	19.808499
59.044264	2185.612104	19.813517
59.543710	2179.121062	19.818535
59.537911	2181.755024	19.823552
59.217058	2172.671585	19.828570
59.404507	2186.789874	19.833587
59.371359	2202.528379	19.838605
59.659739	2202.927077	19.843623
59.594835	2210.111564	19.848640
59.586136	2210.980055	19.853658
59.948882	2203.417420	19.858675
59.631632	2207.352557	19.863693
59.908802	2205.027442	19.868711
60.123436	2203.826927	19.873728
59.670857	2203.380211	19.878746
60.153550	2200.100411	19.883763
59.889738	2206.838364	19.888781
59.900952	2200.942775	19.893799
59.789833	2209.162731	19.898816
59.796841	2210.870389	19.903834
60.637323	2216.157906	19.908851
60.247276	2226.908835	19.913869
60.494408	2233.138963	19.918887
60.570098	2219.482610	19.923904
60.789176	2228.798362	19.928922
61.025164	2229.739526	19.933939
60.797640	2214.755757	19.938957
60.586610	2204.349010	19.943975
60.787109	2213.480503	19.948992
60.595812	2223.682926	19.954010
60.947383	2219.504489	19.959027
60.844605	2233.564494	19.964045
61.072383	2228.466586	19.969063
61.119692	2235.637908	19.974080
61.087518	2228.956324	19.979098
61.499978	2218.760046	19.984115
61.011575	2225.770599	19.989133
61.371693	2220.963870	19.994151
61.446428	2228.465123	19.999168
61.223626	2233.429034	20.004186
61.484059	2230.596862	20.009203
61.377477	2233.172966	20.014221
61.644370	2224.247466	20.019239
61.476172	2230.249645	20.024256
61.522614	2231.342179	20.029274
61.618082	2243.157053	20.034291
61.768547	2251.719964	20.039309
61.851428	2240.720405	20.044327
62.008169	2247.164755	20.049344
61.611667	2259.066762	20.054362
62.038620	2245.392117	20.059379
61.649259	2261.255934	20.064397
61.950898	2264.979103	20.069415
62.265748	2252.383471	20.074432
62.227226	2254.088956	20.079450
62.531895	2271.701640	20.084467
62.271356	2283.330264	20.089485
62.894726	2287.437121	20.094503
62.782897	2264.698506	20.099520
62.293685	2260.607749	20.104538
62.726593	2255.161682	20.109555
62.564391	2275.483985	20.114573
62.573997	2280.647614	20.119591
62.676681	2281.530595	20.124608
62.796275	2285.127055	20.129626
63.112933	2282.113637	20.134643
62.920241	2285.802383	20.139661
62.764911	2276.000259	20.144679
63.012913	2278.454527	20.149696
62.914026	2289.080400	20.154714
63.171528	2274.677605	20.159731
62.894318	2281.997463	20.164749
63.139710	2292.102751	20.169767
63.558563	2305.492027	20.174784
63.457958	2310.096657	20.179802
63.739808	2306.850441	20.184819
63.446268	2309.343891	20.189837
63.511626	2297.793307	20.194855
63.815926	2308.578286	20.199872
63.806082	2306.254097	20.204890
63.854816	2291.554991	20.209907
63.828692	2302.809572	20.214925
64.024965	2301.103039	20.219943
64.239266	2302.881478	20.224960
63.766219	2301.394185	20.229978
64.073448	2296.655650	20.234995
64.041315	2298.535536	20.240013
63.775467	2292.332484	20.245031
63.990422	2306.670687	20.250048
63.869357	2334.882549	20.255066
64.356024	2332.995184	20.260083
64.289440	2336.563142	20.265101
64.283207	2333.694034	20.270119
64.630397	2328.776846	20.275136
64.122963	2341.198473	20.280154
64.378871	2350.157598	20.285171
64.684673	2362.366940	20.290189
64.435329	2366.882824	20.295207
64.888138	2368.251946	20.300224
64.863552	2368.551896	20.305242
65.151047	2362.917383	20.310259
65.256969	2358.897653	20.315277
65.212886	2359.170820	20.320295
65.249341	2370.469749	20.325312
65.354512	2383.602347	20.330330
65.497312	2387.769362	20.335347
65.475517	2386.304481	20.340365
65.643348	2387.040207	20.345383
65.720172	2383.989505	20.350400
65.563931	2391.578813	20.355418
66.064674	2376.996317	20.360435
65.849713	2391.013010	20.365453
66.030256	2393.432433	20.370471
66.113952	2377.506046	20.375488
65.564677	2365.844986	20.380506
66.005001	2368.889236	20.385523
65.913141	2384.879579	20.390541
66.380820	2377.278094	20.395559
66.456940	2372.830473	20.400576
66.398816	2375.897588	20.405594
66.431046	2376.350520	20.410611
66.399491	2376.122187	20.415629
66.339713	2366.912032	20.420647
66.640742	2375.270866	20.425664
66.461731	2370.542998	20.430682
66.911589	2370.233949	20.435699
66.864632	2363.772553	20.440717
66.788499	2363.327145	20.445735
67.008606	2360.009744	20.450752
66.911605	2376.398927	20.455770
66.705802	2371.609255	20.460787
66.822548	2368.437343	20.465805
66.549793	2368.995555	20.470823
66.919013	2371.362856	20.475840
66.653874	2371.469907	20.480858
67.010642	2370.528319	20.485875
67.445264	2382.219203	20.490893
67.931500	2373.611821	20.495911
68.194652	2371.605924	20.500928
67.552723	2359.870758	20.505946
68.024952	2350.310670	20.510963
67.879232	2350.579597	20.515981
67.681791	2349.133294	20.520999
67.785759	2339.451814	20.526016
68.012056	2337.846681	20.531034
67.815741	2339.623754	20.536051
67.687889	2343.618392	20.541069
67.780665	2354.591320	20.546087
68.391319	2359.521455	20.551104
67.914586	2373.454024	20.556122
68.058690	2367.024296	20.561139
68.400362	2371.714154	20.566157
68.051891	2374.877136	20.571175
68.376236	2373.787328	20.576192
68.169776	2378.613383	20.581210
68.537761	2374.233270	20.586227
68.685541	2370.859754	20.591245
68.503884	2376.296987	20.596263
68.634792	2375.078349	20.601280
68.819903	2392.759019	20.606298
68.934050	2402.152188	20.611315
69.188632	2406.975514	20.616333
69.229698	2408.824861	20.621351
69.106557	2401.985436	20.626368
69.009534	2406.083728	20.631386
69.304493	2403.937455	20.636403
69.433589	2405.465193	20.641421
68.952390	2412.606837	20.646439
69.519966	2403.967585	20.651456
69.321919	2412.059928	20.656474
69.441363	2393.716044	20.661491
69.309024	2400.811480	20.666509
69.044308	2403.965828	20.671527
69.259421	2409.453851	20.676544
69.623656	2431.705367	20.681562
69.823043	2431.452786	20.686579
69.898276	2434.512016	20.691597
69.616911	2437.018491	20.696615
70.267698	2421.811042	20.701632
70.185099	2433.622219	20.706650
69.952170	2432.965043	20.711667
69.901057	2427.870644	20.716685
69.933198	2434.620494	20.721703
70.071108	2448.666703	20.726720
70.014465	2460.575236	20.731738
70.164611	2465.939130	20.736755
70.426363	2458.669364	20.741773
70.429483	2462.573922	20.746791
70.482111	2465.386619	20.751808
70.767532	2487.553249	20.756826
71.066552	2486.651544	20.761843
71.185522	2493.667611	20.766861
71.222649	2489.167177	20.771879
71.326610	2483.196898	20.776896
71.134896	2485.386232	20.781914
71.407208	2479.367077	20.786931
71.441034	2487.260434	20.791949
71.342029	2483.271781	20.796967
71.548262	2478.810456	20.801984
71.403311	2472.979781	20.807002
71.471622	2477.904423	20.812019
71.567155	2479.774984	20.817037
71.728644	2485.203152	20.822055
71.750460	2480.493561	20.827072
71.619846	2483.740598	20.832090
71.779864	2479.076615	20.837107
71.692973	2482.606942	20.842125
71.662768	2475.401039	20.847143
71.949654	2500.279734	20.852160
71.671554	2506.456879	20.857178
71.695028	2516.482085	20.862195
72.215219	2510.660157	20.867213
72.164205	2515.271887	20.872231
72.408586	2509.686672	20.877248
72.366161	2530.853153	20.882266
72.614017	2528.626273	20.887283
72.554906	2531.953952	20.892301
72.443849	2537.600240	20.897319
72.469959	2528.848260	20.902336
72.390005	2530.490376	20.907354
72.364001	2537.864690	20.912371
72.782253	2547.279460	20.917389
72.877702	2562.831863	20.922407
73.240037	2554.711395	20.927424
73.188274	2556.761210	20.932442
73.332617	2561.066477	20.937459
73.671009	2557.192900	20.942477
73.333746	2559.370847	20.947495
73.670544	2554.216107	20.952512
73.468932	2552.916762	20.957530
73.641741	2552.285330	20.962547
73.760024	2549.258661	20.967565
73.887876	2553.910312	20.972583
73.883844	2552.633731	20.977600
73.970384	2555.813111	20.982618
73.936269	2552.067384	20.987635
73.670096	2553.719538	20.992653
74.068535	2564.822436	20.997671
73.837784	2562.086634	21.002688
74.151531	2572.147391	21.007706
74.225041	2577.819321	21.012723
74.131861	2581.018718	21.017741
74.166609	2586.283854	21.022759
74.594073	2580.518379	21.027776
74.556802	2590.178102	21.032794
74.485937	2586.671856	21.037811
74.867077	2571.010897	21.042829
74.852073	2587.591761	21.047847
75.205208	2577.401553	21.052864
75.060053	2571.873723	21.057882
75.177638	2577.299489	21.062899
75.303110	2574.469898	21.067917
75.082609	2573.448883	21.072935
75.284875	2573.775587	21.077952
75.494655	2589.823453	21.082970
75.435529	2593.170027	21.087987
75.724887	2595.835650	21.093005
75.463745	2612.036525	21.098023
75.931348	2598.437666	21.103040
75.880725	2603.687319	21.108058
75.573574	2600.890538	21.113075
75.747750	2596.959759	21.118093
75.799435	2602.436162	21.123111
76.111593	2597.662134	21.128128
75.755938	2600.591892	21.133146
75.694195	2607.903505	21.138163
76.264321	2595.442284	21.143181
75.474247	2610.980220	21.148199
75.970914	2616.180346	21.153216
76.197157	2619.606487	21.158234
76.208382	2627.247083	21.163251
76.343742	2626.687698	21.168269
76.220082	2626.783984	21.173287
76.365755	2643.863182	21.178304
76.725742	2654.099119	21.183322
76.721917	2657.437675	21.188339
76.960848	2651.498505	21.193357
77.056685	2657.843410	21.198375
76.743093	2652.480862	21.203392
77.166901	2655.961244	21.208410
76.735046	2659.758237	21.213427
77.239664	2667.704039	21.218445
77.400828	2681.027779	21.223463
77.693819	2685.586270	21.228480
77.567884	2685.431983	21.233498
77.600494	2698.865919	21.238515
77.657392	2686.588740	21.243533
77.919384	2691.296918	21.248551
77.661717	2675.121797	21.253568
78.147136	2686.288793	21.258586
78.135893	2683.617074	21.263603
78.137478	2678.758826	21.268621
77.891663	2686.515178	21.273639
78.004639	2682.909578	21.278656
78.309904	2682.426142	21.283674
78.188744	2682.428420	21.288691
78.556187	2671.519241	21.293709
78.108632	2684.311549	21.298727
77.960644	2684.303946	21.303744
78.455503	2698.417754	21.308762
78.478825	2709.907832	21.313779
78.367170	2716.454195	21.318797
78.473387	2721.858229	21.323815
78.534104	2711.187519	21.328832
78.972902	2730.159912	21.333850
78.630917	2738.240779	21.338867
78.840713	2743.182276	21.343885
78.916715	2742.619768	21.348903
78.779666	2738.357070	21.353920
79.085142	2751.110358	21.358938
79.678894	2760.780466	21.363955
79.851169	2760.970363	21.368973
79.872850	2766.322604	21.373991
80.668212	2741.593890	21.379008
80.470513	2738.045692	21.384026
80.145681	2731.219401	21.389043
80.577529	2710.213659	21.394061
80.650852	2716.175942	21.399079
80.483193	2713.933496	21.404096
80.729589	2711.477125	21.409114
80.588706	2715.484955	21.414131
80.406989	2709.899973	21.419149
80.298595	2706.573530	21.424167
80.427920	2711.468067	21.429184
80.728394	2718.251556	21.434202
80.423887	2724.985223	21.439219
80.586560	2716.314399	21.444237
80.846613	2719.041358	21.449255
80.712657	2719.944803	21.454272
80.746574	2714.151581	21.459290
80.838633	2713.902741	21.464307
80.799510	2715.278775	21.469325
80.410546	2735.390090	21.474343
80.762739	2737.739717	21.479360
81.183183	2743.871627	21.484378
80.765819	2746.639768	21.489395
81.033831	2748.396325	21.494413
81.243299	2771.091535	21.499431
81.318494	2779.146006	21.504448
81.199062	2785.150073	21.509466
81.076574	2780.999889	21.514483
81.865481	2788.238066	21.519501
81.838947	2806.270795	21.524519
81.579095	2809.411079	21.529536
81.914712	2806.076730	21.534554
81.859574	2807.073019	21.539571
82.138297	2811.087110	21.544589
82.072226	2810.167311	21.549607
82.073308	2829.480249	21.554624
82.541665	2838.184746	21.559642
82.500344	2833.032792	21.564659
82.697565	2831.162426	21.569677
83.357910	2826.207717	21.574695
83.264431	2833.548103	21.579712
83.132753	2823.604175	21.584730
83.037227	2830.347824	21.589747
83.005644	2825.226572	21.594765
83.205257	2828.358872	21.599783
82.890473	2823.547100	21.604800
83.690821	2820.860766	21.609818
83.308894	2829.066048	21.614835
83.257839	2826.341655	21.619853
83.222681	2824.172456	21.624871
83.281829	2831.898339	21.629888
83.816480	2836.269660	21.634906
83.370932	2848.460795	21.639923
83.738869	2851.609519	21.644941
83.902246	2861.592196	21.649959
83.676797	2854.492763	21.654976
84.315811	2857.223813	21.659994
83.995628	2860.589271	21.665011
84.252601	2849.509571	21.670029
83.968742	2853.286155	21.675047
84.214109	2879.505480	21.680064
84.691748	2877.853912	21.685082
84.286273	2884.768949	21.690099
84.728994	2889.202147	21.695117
84.602719	2882.159255	21.700135
85.019256	2876.980674	21.705152
85.555314	2871.836525	21.710170
85.451377	2875.305160	21.715187
85.352045	2868.099862	21.720205
85.396959	2866.592041	21.725223
85.331616	2868.263330	21.730240
85.628751	2856.711525	21.735258
85.328052	2862.587204	21.740275
85.450541	2863.059582	21.745293
85.616984	2867.167900	21.750311
85.716247	2867.099624	21.755328
85.744627	2857.374006	21.760346
85.588253	2866.363805	21.765363
85.983342	2854.255956	21.770381
85.878889	2860.969577	21.775399
85.770291	2862.874317	21.780416
86.057355	2872.745237	21.785434
86.252955	2889.357359	21.790451
86.342984	2887.261009	21.795469
86.455754	2898.765289	21.800487
86.286742	2901.025794	21.805504
86.307590	2900.247882	21.810522
86.313392	2900.089887	21.815539
86.599184	2898.335185	21.820557
86.433109	2897.376264	21.825575
86.375373	2912.165250	21.830592
86.721124	2910.743962	21.835610
86.482436	2918.768332	21.840627
86.764986	2918.229514	21.845645
86.722615	2924.524207	21.850663
86.874967	2935.198582	21.855680
87.155728	2942.300766	21.860698
86.942211	2941.758466	21.865715
86.953527	2950.494231	21.870733
87.317383	2966.002682	21.875751
87.372594	2976.000328	21.880768
87.820794	2969.682315	21.885786
87.478696	2977.900207	21.890803
87.812982	2982.765293	21.895821
88.196062	2998.721464	21.900839
88.247291	3013.522280	21.905856
88.761729	3005.422934	21.910874
88.725445	3001.259726	21.915891
88.670398	2984.864723	21.920909
88.893409	2969.808322	21.925927
88.727191	2967.829921	21.930944
88.692201	2961.707758	21.935962
88.901594	2958.659395	21.940979
88.660188	2988.047295	21.945997
89.013077	2979.515897	21.951015
89.126036	2995.665396	21.956032
89.212283	2989.445221	21.961050
89.488106	2992.946929	21.966067
89.369877	2989.725042	21.971085
89.492771	2989.589277	21.976103
89.276912	2997.518798	21.981120
89.522555	2980.208167	21.986138
89.315346	2986.120903	21.991155
89.407017	2992.631816	21.996173
89.707012	2982.920221	22.001191
89.608349	3009.197794	22.006208
89.799724	3011.271827	22.011226
89.402297	3012.132350	22.016243
89.766190	3012.806948	22.021261
89.657215	3014.046259	22.026279
89.668915	3045.613055	22.031296
90.169682	3031.126671	22.036314
90.225656	3047.364767	22.041331
90.193078	3047.444955	22.046349
90.131563	3043.311718	22.051367
90.410251	3063.423197	22.056384
91.018845	3071.629543	22.061402
90.876407	3077.977233	22.066419
90.784109	3079.821975	22.071437
91.093862	3073.815489	22.076455
91.097606	3075.541861	22.081472
91.257565	3072.234682	22.086490
91.333839	3068.806333	22.091507
91.026710	3074.547029	22.096525
91.395478	3085.093387	22.101543
91.196825	3101.449244	22.106560
91.729503	3103.929840	22.111578
91.650117	3107.157830	22.116595
92.210508	3102.152893	22.121613
92.500090	3094.673847	22.126631
92.396954	3095.688036	22.131648
92.360457	3084.454367	22.136666
92.412902	3091.253202	22.141683
92.184617	3090.894969	22.146701
92.334148	3095.995663	22.151719
92.546542	3088.408572	22.156736
92.558796	3085.867550	22.161754
92.358371	3090.119401	22.166771
92.248371	3094.140500	22.171789
92.748049	3104.731287	22.176807
92.579817	3113.191347	22.181824
93.175816	3109.690327	22.186842
93.040071	3112.054116	22.191859
92.705090	3111.933163	22.196877
93.107936	3121.373577	22.201895
93.235980	3136.852954	22.206912
93.711029	3142.869340	22.211930
93.378720	3142.393963	22.216947
93.521210	3138.449215	22.221965
93.826152	3137.276706	22.226983
93.491480	3147.774818	22.232000
93.954338	3142.690238	22.237018
94.203976	3141.519469	22.242035
93.938658	3167.692531	22.247053
94.091607	3167.618052	22.252071
94.563942	3170.358441	22.257088
94.640982	3170.699626	22.262106
94.437440	3166.115435	22.267123
94.319460	3173.599923	22.272141
94.980484	3167.701789	22.277159
94.806884	3163.344102	22.282176
95.207784	3158.490450	22.287194
94.827064	3166.051450	22.292211
94.677200	3176.251071	22.297229
95.027144	3164.812537	22.302247
95.045198	3174.431567	22.307264
95.279069	3187.296564	22.312282
95.274518	3204.055817	22.317299
95.258779	3214.355219	22.322317
95.482143	3206.172387	22.327335
95.463429	3204.960237	22.332352
95.425869	3203.960346	22.337370
95.689240	3195.542220	22.342387
95.877471	3206.089926	22.347405
95.761242	3217.080313	22.352423
96.200902	3224.975424	22.357440
96.302829	3220.881364	22.362458
96.448967	3216.343655	22.367475
96.150560	3231.032106	22.372493
96.225934	3224.042636	22.377511
96.142553	3228.390712	22.382528
96.366626	3230.226710	22.387546
96.414325	3247.916957	22.392563
96.524323	3253.775277	22.397581
96.707750	3250.654689	22.402599
96.486839	3260.059367	22.407616
97.159374	3270.008320	22.412634
97.407683	3283.183405	22.417651
97.046168	3293.674889	22.422669
97.895677	3267.151715	22.427687
97.867122	3270.989953	22.432704
97.875533	3264.414703	22.437722
98.180349	3264.678656	22.442739
98.117098	3265.636150	22.447757
98.327195	3259.078296	22.452775
98.232445	3268.328339	22.457792
98.255885	3268.555354	22.462810
98.425383	3263.130480	22.467827
98.063488	3268.031172	22.472845
98.596624	3259.999507	22.477863
98.767277	3266.380731	22.482880
98.498304	3263.574583	22.487898
98.714549	3263.722076	22.492915
98.587785	3266.025458	22.497933
98.681064	3265.178549	22.502951
98.743759	3272.472219	22.507968
98.687183	3291.657295	22.512986
98.932150	3290.184393	22.518003
98.680999	3301.039814	22.523021
99.050552	3295.642023	22.528039
98.969690	3306.028969	22.533056
99.070326	3329.772938	22.538074
99.361635	3328.325682	22.543091
99.385470	3332.884037	22.548109
99.345668	3336.512472	22.553127
99.515655	3359.922109	22.558144
99.516098	3367.883412	22.563162
99.761959	3352.735656	22.568179
99.730781	3376.568377	22.573197
100.003337	3380.124194	22.578215
100.102212	3394.212937	22.583232
100.294922	3389.358586	22.588250
100.764732	3382.401323	22.593267
100.706976	3382.424167	22.598285
101.134636	3367.861007	22.603303
100.998713	3364.320896	22.608320
100.891098	3373.344135	22.613338
101.423102	3370.740627	22.618355
101.327060	3372.087253	22.623373
101.392930	3369.642259	22.628391
101.444215	3379.437845	22.633408
101.681764	3385.513451	22.638426
102.023669	3396.139840	22.643443
102.069362	3372.509827	22.648461
101.951129	3364.348345	22.653479
102.049478	3358.288139	22.658496
101.792161	3367.387170	22.663514
102.493275	3368.579130	22.668531
102.110100	3385.990551	22.673549
102.244435	3393.182389	22.678567
102.266728	3385.291127	22.683584
102.777835	3390.943932	22.688602
102.581439	3393.997911	22.693619
102.856839	3395.717184	22.698637
102.993059	3388.964160	22.703655
103.072830	3388.873031	22.708672
102.793576	3393.004592	22.713690
103.107283	3385.977035	22.718707
102.832858	3390.186492	22.723725
103.279513	3381.356707	22.728743
102.988088	3395.303950	22.733760
103.013417	3416.083299	22.738778
103.365604	3411.136640	22.743795
103.391062	3424.328513	22.748813
103.220264	3420.635829	22.753831
103.254115	3438.363127	22.758848
103.506310	3451.828815	22.763866
104.014207	3445.100665	22.768883
103.650822	3457.166700	22.773901
103.903742	3475.697703	22.778919
104.168358	3487.598315	22.783936
104.230780	3491.612478	22.788954
104.428904	3481.027858	22.793971
104.216857	3500.398483	22.798989
104.688604	3509.011590	22.804007
104.777322	3515.082665	22.809024
105.181544	3522.494276	22.814042
105.026628	3515.684570	22.819059
105.025408	3518.771955	22.824077
105.025785	3514.510712	22.829095
105.161887	3530.122167	22.834112
104.992383	3542.950326	22.839130
105.187231	3550.886231	22.844147
105.558456	3547.910274	22.849165
105.652459	3550.903812	22.854183
105.826284	3557.421540	22.859200
105.621287	3574.733966	22.864218
106.005509	3571.784252	22.869235
106.085154	3568.190046	22.874253
106.195390	3572.466438	22.879271
106.191427	3571.084342	22.884288
106.240747	3566.606808	22.889306
106.713872	3573.143680	22.894323
106.401740	3598.736535	22.899341
106.535420	3593.373106	22.904359
106.755745	3595.983060	22.909376
106.942316	3599.211223	22.914394
107.162556	3592.093846	22.919411
106.764721	3597.190755	22.924429
106.635814	3610.124206	22.929447
107.184436	3626.741440	22.934464
107.020998	3626.678083	22.939482
107.371750	3632.548507	22.944499
107.395880	3650.217037	22.949517
107.776006	3659.644118	22.954535
107.885253	3667.887960	22.959552
107.763694	3672.149426	22.964570
107.928059	3662.196263	22.969587
107.790113	3678.963957	22.974605
108.153274	3686.984804	22.979623
108.529931	3696.742085	22.984640
108.305224	3692.151663	22.989658
108.842276	3688.105297	22.994675
108.725090	3691.903499	22.999693
108.806820	3702.404038	23.004711
109.064716	3717.108883	23.009728
109.151447	3715.103412	23.014746
109.486616	3708.852677	23.019763
109.488358	3724.705253	23.024781
109.521606	3721.165610	23.029799
109.623763	3714.274693	23.034816
109.298301	3703.364335	23.039834
109.537639	3709.217158	23.044851
109.752466	3726.327498	23.049869
109.684614	3740.410122	23.054887
109.701264	3739.835802	23.059904
109.531886	3747.536464	23.064922
110.062040	3744.090642	23.069939
110.086663	3761.015016	23.074957
110.139985	3770.193771	23.079975
110.233111	3767.126024	23.084992
110.790215	3763.520135	23.090010
110.958995	3773.994256	23.095027
111.211332	3790.965738	23.100045
111.280817	3789.212390	23.105063
111.575971	3790.606803	23.110080
111.386889	3801.045184	23.115098
111.535467	3791.601870	23.120115
111.511952	3796.426743	23.125133
111.368771	3794.008725	23.130151
111.883035	3792.466867	23.135168
111.873603	3787.046736	23.140186
111.822450	3790.613371	23.145203
111.964192	3790.295229	23.150221
111.778999	3791.143972	23.155239
111.893096	3789.578609	23.160256
111.731937	3821.793766	23.165274
112.175940	3823.188832	23.170291
112.249846	3818.435104	23.175309
112.206821	3829.404833	23.180327
112.406093	3844.211198	23.185344
112.700919	3851.035454	23.190362
112.639870	3851.109959	23.195379
112.740057	3853.367797	23.200397
112.913325	3857.046557	23.205415
113.311231	3865.437216	23.210432
113.233824	3882.901942	23.215450
113.590581	3874.768271	23.220467
113.371513	3875.177935	23.225485
113.191226	3878.449719	23.230503
113.524709	3889.557697	23.235520
113.600796	3904.915577	23.240538
114.120866	3895.822037	23.245555
114.484691	3899.166752	23.250573
114.593143	3891.368470	23.255591
114.698564	3889.396183	23.260608
114.584577	3894.500634	23.265626
114.884157	3889.198752	23.270643
115.143272	3882.355888	23.275661
115.163178	3881.779470	23.280679
115.219569	3877.684623	23.285696
115.232548	3891.302149	23.290714
115.510647	3886.505608	23.295731
115.330070	3895.142732	23.300749
115.630311	3911.025002	23.305767
115.768072	3903.188998	23.310784
116.021369	3908.860307	23.315802
116.539979	3905.689276	23.320819
116.318146	3905.352017	23.325837
116.092091	3896.622129	23.330855
116.171194	3891.391595	23.335872
116.245729	3900.477365	23.340890
116.303712	3903.829948	23.345907
116.690641	3906.685587	23.350925
116.404597	3903.808872	23.355943
116.640789	3908.285552	23.360960
116.428471	3910.784404	23.365978
116.391279	3907.984435	23.370995
116.726729	3925.984411	23.376013
116.452593	3934.643558	23.381031
116.594263	3941.836856	23.386048
116.650740	3965.959433	23.391066
116.811246	3964.332368	23.396083
116.687434	3981.856534	23.401101
116.912490	4001.973922	23.406119
117.574601	3999.526570	23.411136
117.912858	4009.578906	23.416154
118.350354	4023.328677	23.421171
118.467530	4022.037360	23.426189
118.346382	4025.663203	23.431207
118.575578	4016.095177	23.436224
118.790698	4024.157126	23.441242
118.917565	4011.879484	23.446259
119.005207	4017.130405	23.451277
118.810325	4020.319582	23.456295
119.238479	4000.162242	23.461312
119.026825	4012.741064	23.466330
119.047865	4017.843692	23.471347
119.287334	4012.430986	23.476365
119.128033	4009.775557	23.481383
119.368577	4007.664487	23.486400
119.090026	4031.633696	23.491418
119.518315	4040.851947	23.496435
119.698056	4043.363035	23.501453
119.792175	4040.033100	23.506471
120.548522	4041.488518	23.511488
120.475477	4044.943846	23.516506
120.480350	4044.962210	23.521523
121.057856	4049.946213	23.526541
120.815757	4063.048373	23.531559
121.128434	4050.247800	23.536576
121.236804	4059.837273	23.541594
121.422251	4045.078423	23.546611
121.022208	4033.738369	23.551629
120.926088	4046.273620	23.556647
121.190800	4042.058968	23.561664
121.199844	4051.779134	23.566682
121.268461	4057.511422	23.571699
121.390530	4053.738830	23.576717
121.395972	4076.312044	23.581735
121.551465	4077.359792	23.586752
121.470656	4079.020309	23.591770
121.409603	4086.489887	23.596787
121.694054	4102.901192	23.601805
121.721299	4119.554145	23.606823
122.282304	4126.130749	23.611840
122.218640	4152.344990	23.616858
122.577302	4153.685257	23.621875
122.710321	4151.811594	23.626893
122.644700	4158.806762	23.631911
123.195490	4164.844541	23.636928
123.206967	4174.576201	23.641946
123.259036	4173.337736	23.646963
123.572232	4179.478708	23.651981
123.389594	4182.594376	23.656999
123.575372	4174.734050	23.662016
123.762808	4191.476399	23.667034
123.654031	4201.001466	23.672051
124.384633	4204.522204	23.677069
124.069973	4204.305947	23.682087
124.140612	4204.512076	23.687104
124.329135	4214.678904	23.692122
124.137144	4204.849077	23.697139
124.762110	4210.665779	23.702157
125.091670	4221.599985	23.707175
125.431205	4217.421341	23.712192
125.211959	4220.536562	23.717210
125.268915	4231.613374	23.722227
125.848985	4214.256620	23.727245
125.486074	4218.122464	23.732263
125.760236	4213.160449	23.737280
125.617075	4218.083998	23.742298
125.796227	4216.568794	23.747315
125.864892	4213.604769	23.752333
125.860436	4224.059635	23.757351
126.019424	4213.656171	23.762368
126.029338	4223.292133	23.767386
125.794813	4224.904801	23.772403
126.090155	4239.619147	23.777421
126.254529	4251.869935	23.782439
126.312397	4248.008406	23.787456
126.453023	4267.892593	23.792474
126.402265	4275.783880	23.797491
127.030432	4273.069695	23.802509
127.033403	4280.899707	23.807527
126.875197	4299.989015	23.812544
127.246484	4305.636156	23.817562
126.852381	4314.850413	23.822579
127.414393	4319.934534	23.827597
127.436981	4337.482979	23.832615
127.713286	4341.605663	23.837632
127.604026	4349.392244	23.842650
127.801129	4374.915461	23.847667
128.335155	4368.176439	23.852685
128.348992	4379.264172	23.857703
128.383512	4379.966980	23.862720
128.541323	4383.676660	23.867738
128.531858	4401.721210	23.872755
128.670841	4399.446908	23.877773
129.025162	4399.994870	23.882791
129.299942	4405.201926	23.887808
129.353086	4426.988423	23.892826
129.177748	4433.821057	23.897843
130.011450	4419.222798	23.902861
130.516798	4430.065401	23.907879
130.657267	4419.380737	23.912896
130.338764	4417.568817	23.917914
130.038477	4423.902919	23.922931
130.660432	4423.230471	23.927949
130.534467	4429.208711	23.932967
130.798410	4421.257117	23.937984
130.735134	4408.669601	23.943002
130.853327	4407.085426	23.948019
131.311219	4403.555001	23.953037
131.091429	4409.943918	23.958055
131.174958	4407.880647	23.963072
131.589097	4400.388163	23.968090
131.223544	4405.766564	23.973107
131.611586	4400.837465	23.978125
131.398863	4429.798830	23.983143
131.600346	4425.276316	23.988160
131.451533	4438.754149	23.993178
131.219804	4444.744540	23.998195
132.067543	4449.569939	24.003213
131.889262	4475.648833	24.008231
132.232111	4471.404293	24.013248
132.169148	4476.830447	24.018266
131.952375	4486.042492	24.023283
132.467471	4491.987760	24.028301
132.519554	4512.919376	24.033319
132.586001	4503.458810	24.038336
132.669461	4521.221985	24.043354
133.288530	4523.710302	24.048371
134.047726	4506.172804	24.053389
134.247295	4509.486426	24.058407
134.199264	4513.239979	24.063424
134.157447	4517.440193	24.068442
134.385515	4508.388914	24.073459
134.634409	4505.994007	24.078477
134.926774	4507.992362	24.083495
134.785742	4502.279834	24.088512
134.837166	4506.955310	24.093530
134.610845	4501.045539	24.098547
134.826369	4507.302141	24.103565
134.848256	4502.496697	24.108583
134.636675	4505.067909	24.113600
134.678555	4515.575384	24.118618
134.699022	4525.246050	24.123635
135.048494	4538.096160	24.128653
134.966927	4551.985849	24.133671
135.272463	4563.613321	24.138688
135.158474	4573.624875	24.143706
135.205684	4593.313553	24.148723
135.741091	4591.921663	24.153741
135.894635	4594.715530	24.158759
135.693504	4609.801298	24.163776
135.866526	4624.989484	24.168794
136.246884	4626.793660	24.173811
137.159345	4631.598574	24.178829
137.399135	4633.760318	24.183847
137.987192	4637.043487	24.188864
137.767916	4616.136516	24.193882
137.608219	4611.582640	24.198899
138.125985	4598.722142	24.203917
137.843940	4595.879266	24.208935
138.068494	4587.847324	24.213952
138.302228	4593.024016	24.218970
137.982698	4602.601831	24.223987
138.230853	4593.323864	24.229005
138.163852	4616.574250	24.234023
138.045665	4624.314408	24.239040
138.577118	4624.000191	24.244058
138.505830	4627.860545	24.249075
139.177260	4618.849428	24.254093
139.150749	4623.276959	24.259111
139.061805	4626.769574	24.264128
139.214137	4612.297879	24.269146
139.330760	4612.487241	24.274163
139.596183	4609.714407	24.279181
139.203905	4626.585886	24.284199
139.594343	4639.016515	24.289216
139.927295	4639.319287	24.294234
139.448121	4651.027119	24.299251
139.747494	4652.900072	24.304269
139.885360	4665.895755	24.309287
140.016447	4682.382517	24.314304
139.994633	4681.541295	24.319322
139.989305	4698.249660	24.324339
140.375798	4709.880074	24.329357
140.503240	4715.866010	24.334375
140.721141	4738.874470	24.339392
141.083971	4738.904987	24.344410
141.062216	4753.999275	24.349427
141.055843	4758.731253	24.354445
141.223783	4769.304562	24.359463
141.144750	4774.420262	24.364480
141.719450	4775.162829	24.369498
141.895183	4802.280997	24.374515
142.677657	4788.992617	24.379533
142.318530	4798.765692	24.384551
142.867712	4782.708190	24.389568
143.013002	4789.391515	24.394586
142.768021	4792.625822	24.399603
142.943217	4788.510992	24.404621
143.169714	4776.314385	24.409639
143.177863	4786.777867	24.414656
143.757812	4804.849291	24.419674
143.650890	4814.005472	24.424691
143.637252	4810.021452	24.429709
144.008218	4810.679284	24.434727
143.658601	4806.654431	24.439744
144.273475	4811.259037	24.444762
143.779833	4825.141525	24.449779
144.106143	4832.441925	24.454797
144.026834	4844.136496	24.459815
144.164206	4849.875437	24.464832
144.392048	4841.190618	24.469850
144.555066	4874.020392	24.474867
144.694842	4874.268219	24.479885
144.840050	4882.927134	24.484903
144.692600	4901.098148	24.489920
145.467628	4896.650037	24.494938
145.152736	4911.501705	24.499955
145.585571	4925.053233	24.504973
145.606158	4929.614961	24.509991
145.775370	4946.283186	24.515008
146.082321	4939.778382	24.520026
145.800753	4957.144759	24.525043
146.275053	4958.415526	24.530061
146.450865	4971.864894	24.535079
146.637679	4976.039795	24.540096
146.524575	4962.508562	24.545114
146.920676	4961.461426	24.550131
146.917308	4976.431061	24.555149
147.452196	4982.676278	24.560167
147.466513	4990.575665	24.565184
148.120115	4984.604059	24.570202
148.398163	4975.056737	24.575219
148.497532	4975.512419	24.580237
148.786655	4968.908954	24.585255
148.254622	4973.133969	24.590272
148.532370	4970.820931	24.595290
148.458526	4973.614940	24.600307
148.557284	4983.009858	24.605325
148.583707	4970.717541	24.610343
148.418740	4978.440953	24.615360
148.858777	4980.481914	24.620378
148.722317	4991.856064	24.625395
148.885354	4988.917747	24.630413
149.125329	5003.158619	24.635431
149.131353	5025.470414	24.640448
149.532396	5020.644466	24.645466
149.528326	5029.898459	24.650483
149.572738	5051.987027	24.655501
149.690579	5056.507323	24.660519
149.708427	5070.767945	24.665536
150.396899	5092.109512	24.670554
150.453101	5103.113930	24.675571
150.557974	5095.849798	24.680589
150.942125	5110.460378	24.685607
150.748490	5122.167891	24.690624
151.173959	5127.800420	24.695642
151.201383	5120.772067	24.700659
151.275365	5141.822245	24.705677
151.380867	5153.328663	24.710695
151.790010	5156.579903	24.715712
151.650881	5151.039121	24.720730
151.807261	5164.970904	24.725747
151.948938	5181.457321	24.730765
152.216252	5178.939783	24.735783
152.372688	5184.159695	24.740800
152.865822	5210.554526	24.745818
152.829323	5210.385943	24.750835
153.064289	5214.352607	24.755853
153.125925	5210.962289	24.760871
153.054281	5214.733947	24.765888
153.273469	5238.908188	24.770906
153.093347	5256.641109	24.775923
153.511336	5255.127055	24.780941
153.550692	5262.689003	24.785959
153.630427	5281.805362	24.790976
153.724557	5280.958206	24.795994
153.894505	5288.514291	24.801011
153.936746	5315.745167	24.806029
154.035045	5314.130238	24.811047
154.070771	5324.110557	24.816064
154.518916	5342.863766	24.821082
154.641285	5352.242565	24.826099
154.983338	5373.330576	24.831117
155.683731	5369.254576	24.836135
155.469329	5380.366079	24.841152
156.117537	5378.312552	24.846170
156.294712	5369.991915	24.851187
156.123425	5371.251583	24.856205
156.254620	5376.504699	24.861223
156.235946	5375.834454	24.866240
156.430642	5384.731247	24.871258
156.707622	5402.099558	24.876275
156.785062	5404.354182	24.881293
157.007880	5396.532939	24.886311
156.999532	5406.721757	24.891328
156.910680	5405.741695	24.896346
156.960636	5427.449137	24.901363
156.633573	5434.197060	24.906381
157.241969	5449.323752	24.911399
157.289076	5466.100941	24.916416
158.093401	5459.290008	24.921434
157.864567	5482.399187	24.926451
157.757223	5489.712416	24.931469
158.023439	5496.272136	24.936487
158.023571	5523.200115	24.941504
158.727510	5518.707300	24.946522
158.986926	5516.463193	24.951539
159.159061	5541.058494	24.956557
159.707534	5531.110494	24.961575
160.210395	5519.385342	24.966592
160.413918	5513.685142	24.971610
160.699018	5518.145865	24.976627
160.656359	5502.651675	24.981645
160.921825	5483.851081	24.986663
160.682676	5490.527576	24.991680
161.108058	5477.231014	24.996698
161.042868	5474.916723	25.001715
160.585824	5479.485545	25.006733
161.017596	5477.466519	25.011751
160.915117	5492.814400	25.016768
161.132883	5503.136388	25.021786
161.393438	5511.503478	25.026803
161.082966	5518.986799	25.031821
161.358533	5516.936813	25.036839
161.313740	5547.207973	25.041856
161.402089	5545.882570	25.046874
161.684022	5565.624808	25.051891
161.801165	5576.150934	25.056909
161.942879	5577.804458	25.061927
162.200662	5590.989547	25.066944
162.943184	5595.876966	25.071962
163.112892	5597.651128	25.076979
163.267323	5597.915516	25.081997
163.360303	5593.889106	25.087015
163.158001	5606.991788	25.092032
163.337396	5603.951607	25.097050
163.616765	5620.187602	25.102067
163.701538	5623.665339	25.107085
163.877863	5626.510847	25.112103
163.940963	5641.868672	25.117120
163.846797	5650.167303	25.122138
164.051401	5662.562340	25.127155
163.964123	5677.068479	25.132173
164.361787	5683.592375	25.137191
164.425361	5691.451236	25.142208
164.684445	5716.851232	25.147226
164.960592	5723.796575	25.152243
165.139407	5714.241000	25.157261
166.479283	5716.550080	25.162279
166.314305	5722.409171	25.167296
166.546614	5711.325763	25.172314
166.639177	5705.470876	25.177331
166.452694	5712.474246	25.182349
166.818539	5717.288015	25.187367
166.807465	5733.455575	25.192384
166.730212	5737.083488	25.197402
167.079999	5736.639295	25.202419
167.032971	5744.404882	25.207437
167.276624	5740.794227	25.212455
166.737341	5762.058734	25.217472
167.164241	5761.284377	25.222490
167.569902	5765.570952	25.227507
167.439293	5797.025488	25.232525
167.906070	5795.632640	25.237543
167.997304	5809.669049	25.242560
168.161915	5828.422453	25.247578
168.353269	5833.779439	25.252595
168.280522	5844.140907	25.257613
168.732763	5848.132896	25.262631
168.909369	5871.521864	25.267648
168.921671	5864.601002	25.272666
169.619595	5879.170181	25.277683
169.578760	5900.976195	25.282701
169.767184	5891.049962	25.287719
169.779030	5898.998222	25.292736
169.826759	5900.662835	25.297754
170.198900	5908.896698	25.302771
170.106343	5910.435762	25.307789
170.331684	5914.851845	25.312807
170.437604	5938.695948	25.317824
170.604455	5941.730288	25.322842
170.820995	5945.305112	25.327859
170.991092	5973.627783	25.332877
171.500752	5980.023800	25.337895
171.679738	5983.167941	25.342912
171.968904	5969.175879	25.347930
172.987050	5953.545116	25.352947
172.858245	5945.889019	25.357965
173.086240	5943.824531	25.362983
173.219870	5941.715294	25.368000
173.424982	5942.883518	25.373018
173.709256	5935.077372	25.378035
173.710319	5918.058810	25.383053
173.924822	5906.849846	25.388071
173.619210	5893.980262	25.393088
173.818437	5897.900096	25.398106
173.813697	5893.373829	25.403123
173.640083	5899.974751	25.408141
173.970786	5918.608157	25.413159
174.217037	5930.808733	25.418176
174.081269	5933.700130	25.423194
174.445890	5927.453219	25.428211
174.303393	5947.937940	25.433229
174.529703	5960.143293	25.438247
174.966643	5958.991232	25.443264
174.531086	5969.772571	25.448282
174.470589	5983.145666	25.453299
174.962420	6000.544941	25.458317
175.327293	6022.896223	25.463335
175.452544	6031.020028	25.468352
175.465805	6046.073067	25.473370
175.571710	6055.767303	25.478387
175.696775	6075.886156	25.483405
175.945707	6096.974313	25.488423
176.393242	6104.435413	25.493440
176.246402	6122.867474	25.498458
176.689803	6124.880528	25.503475
176.864539	6154.818931	25.508493
177.238427	6149.339173	25.513511
177.218451	6166.047594	25.518528
177.224809	6181.079053	25.523546
177.833044	6183.031212	25.528563
177.593785	6208.325823	25.533581
177.980072	6224.135498	25.538599
178.039918	6222.857070	25.543616
178.460904	6241.579560	25.548634
178.502476	6248.261200	25.553651
178.696881	6265.048065	25.558669
178.912274	6276.545703	25.563687
178.898441	6291.344445	25.568704
178.854041	6297.588964	25.573722
179.523722	6313.724144	25.578739
179.439991	6325.924943	25.583757
179.992576	6328.364388	25.588775
180.168144	6354.583720	25.593792
180.145625	6360.966406	25.598810
180.396843	6360.109093	25.603827
180.128101	6373.347360	25.608845
180.500588	6378.019446	25.613863
180.771194	6380.462159	25.618880
180.738542	6402.813665	25.623898
181.327596	6406.110465	25.628915
181.306182	6418.831729	25.633933
181.469470	6437.150208	25.638951
181.613208	6440.083688	25.643968
181.705324	6441.085064	25.648986
181.992010	6461.708208	25.654003
181.767115	6481.257088	25.659021
182.283448	6480.070301	25.664039
183.792446	6466.840854	25.669056
183.991951	6464.197794	25.674074
184.426533	6458.650808	25.679092
184.281516	6450.261343	25.684109
184.325627	6444.468183	25.689127
184.552633	6428.519301	25.694144
184.406435	6437.949480	25.699162
184.541608	6430.437521	25.704180
184.480833	6433.128217	25.709197
184.815730	6438.667900	25.714215
184.735145	6452.878664	25.719232
184.643952	6474.530674	25.724250
185.186477	6458.336316	25.729268
185.190716	6474.730423	25.734285
185.300021	6497.164872	25.739303
185.406827	6497.491164	25.744320
185.403742	6504.020312	25.749338
185.882891	6526.517008	25.754356
185.597872	6539.740708	25.759373
185.902784	6535.844702	25.764391
186.075008	6556.661695	25.769408
186.327720	6571.437887	25.774426
186.487379	6575.534562	25.779444
187.026972	6590.922044	25.784461
187.085946	6596.519944	25.789479
187.343035	6607.133860	25.794496
187.505489	6619.328693	25.799514
187.960440	6618.696180	25.804532
187.988884	6635.408423	25.809549
188.225875	6648.113861	25.814567
188.497600	6648.269081	25.819584
188.349057	6663.713640	25.824602
188.570191	6659.136963	25.829620
188.693758	6673.530982	25.834637
188.631362	6689.156970	25.839655
188.910194	6709.372550	25.844672
189.272398	6720.414357	25.849690
189.503768	6722.527400	25.854708
189.412487	6744.307285	25.859725
189.310562	6756.320918	25.864743
189.388002	6766.618165	25.869760
189.441914	6794.068635	25.874778
189.629941	6807.597196	25.879796
190.180244	6824.656852	25.884813
190.705063	6851.970971	25.889831
191.000996	6851.215875	25.894848
191.110470	6857.988467	25.899866
191.073663	6872.451527	25.904884
191.297775	6886.182923	25.909901
191.483721	6891.770919	25.914919
192.101995	6905.123169	25.919936
192.098869	6926.511571	25.924954
192.454810	6916.843579	25.929972
192.490836	6927.002757	25.934989
192.590205	6933.057017	25.940007
192.891496	6948.237367	25.945024
193.355476	6952.448898	25.950042
193.148241	6963.093038	25.955060
193.415889	6976.838822	25.960077
193.613377	6985.906096	25.965095
193.930057	6987.021209	25.970112
194.082994	7013.648972	25.975130
194.107944	7004.213104	25.980148
194.367178	7020.229588	25.985165
194.680905	7038.768750	25.990183
194.910167	7041.623404	25.995200
194.686064	7053.157882	26.000218
195.267400	7071.324719	26.005236
195.354526	7081.134354	26.010253
195.389499	7078.710204	26.015271
195.826069	7097.952199	26.020288
195.502189	7113.299279	26.025306
195.930500	7120.391771	26.030324
196.291316	7137.264824	26.035341
196.262843	7140.332129	26.040359
196.823357	7154.912679	26.045376
196.846639	7172.668167	26.050394
197.358903	7162.936536	26.055412
197.556112	7184.767063	26.060429
198.148503	7191.752381	26.065447
198.643456	7184.825557	26.070464
198.716281	7188.559727	26.075482
199.161521	7186.050474	26.080500
198.932733	7191.724381	26.085517
198.764409	7190.878048	26.090535
199.017453	7179.907492	26.095552
198.971376	7182.516504	26.100570
199.334144	7201.378537	26.105588
199.617824	7212.433232	26.110605
199.211964	7220.643155	26.115623
199.669711	7229.399971	26.120640
199.991472	7248.119095	26.125658
200.122684	7255.879082	26.130676
200.481082	7258.551879	26.135693
200.557964	7280.804614	26.140711
200.458163	7288.971284	26.145728
200.497942	7305.163130	26.150746
200.561197	7316.616585	26.155764
200.754557	7323.938635	26.160781
200.868096	7349.228498	26.165799
201.263845	7347.107962	26.170816
201.204324	7373.784406	26.175834
201.502684	7384.803052	26.180852
201.838036	7404.517188	26.185869
201.797757	7419.304740	26.190887
202.351220	7438.436867	26.195904
202.245382	7455.132093	26.200922
202.683055	7460.406725	26.205940
203.050927	7471.549303	26.210957
203.235798	7484.339307	26.215975
203.706504	7493.215001	26.220992
203.564972	7511.576714	26.226010
203.881494	7513.583442	26.231028
204.689456	7515.866704	26.236045
204.778670	7526.221222	26.241063
205.191357	7521.269084	26.246080
204.977090	7524.042284	26.251098
205.321172	7531.775950	26.256116
205.442775	7544.855441	26.261133
205.333934	7556.846819	26.266151
205.839607	7560.849255	26.271168
205.857816	7578.896004	26.276186
205.796447	7591.721426	26.281204
205.862835	7595.349313	26.286221
206.309521	7616.583181	26.291239
206.699182	7618.776561	26.296256
206.447067	7637.576262	26.301274
206.977751	7652.405604	26.306292
207.417948	7664.360680	26.311309
207.442512	7689.427661	26.316327
207.824112	7687.808230	26.321344
207.748642	7704.732602	26.326362
208.038412	7723.238665	26.331380
208.146386	7728.605305	26.336397
207.969052	7747.558470	26.341415
208.229727	7751.567757	26.346432
208.354522	7790.647072	26.351450
208.704474	7793.816672	26.356468
209.242314	7810.765743	26.361485
209.159998	7831.279253	26.366503
210.029907	7837.798850	26.371520
210.102087	7852.386337	26.376538
210.047971	7859.770928	26.381556
210.035195	7876.050068	26.386573
210.529514	7887.416348	26.391591
211.061428	7896.707458	26.396608
210.970878	7924.143691	26.401626
211.165251	7910.221590	26.406644
211.707404	7919.417833	26.411661
211.876619	7939.300023	26.416679
212.435888	7942.917480	26.421696
212.379170	7951.158694	26.426714
212.190292	7946.278722	26.431732
212.640349	7965.522444	26.436749
212.450963	7978.060529	26.441767
212.769465	7982.033117	26.446784
212.849491	7997.684192	26.451802
213.193086	8009.271325	26.456820
213.420119	8004.452897	26.461837
213.659515	8035.785088	26.466855
213.879651	8040.183752	26.471872
213.972324	8055.791559	26.476890
213.952221	8063.439561	26.481908
214.180422	8076.585934	26.486925
214.077507	8098.088712	26.491943
214.787868	8113.911686	26.496960
214.764096	8128.967222	26.501978
214.992739	8148.229955	26.506996
215.482830	8150.614365	26.512013
215.678210	8182.043196	26.517031
215.820134	8179.147366	26.522048
215.941946	8209.192368	26.527066
215.984163	8225.400559	26.532084
216.718797	8235.295006	26.537101
217.038980	8245.370430	26.542119
217.497532	8228.950694	26.547136
217.838165	8248.126845	26.552154
218.327863	8254.206760	26.557172
218.510756	8250.909346	26.562189
218.834437	8254.457420	26.567207
219.198953	8254.103678	26.572224
219.224281	8252.734576	26.577242
219.408555	8255.979874	26.582260
219.581343	8244.562558	26.587277
219.525549	8250.782559	26.592295
219.590072	8244.913444	26.597312
219.924709	8257.765222	26.602330
220.106194	8275.722252	26.607348
220.243399	8270.117358	26.612365
220.185852	8280.844408	26.617383
220.319631	8300.780337	26.622400
220.836726	8303.598397	26.627418
220.781540	8311.364650	26.632436
221.026346	8310.470090	26.637453
220.907679	8326.231487	26.642471
221.347627	8335.551701	26.647488
221.490205	8357.576009	26.652506
221.397026	8368.019209	26.657524
221.974511	8382.949630	26.662541
222.004447	8409.134410	26.667559
222.170744	8428.524698	26.672576
222.418705	8438.271809	26.677594
222.098156	8462.044322	26.682612
222.587771	8481.839558	26.687629
222.441213	8507.172059	26.692647
223.262298	8518.112928	26.697664
223.654515	8548.578223	26.702682
223.603913	8569.748327	26.707700
224.243694	8580.963281	26.712717
224.820118	8586.418836	26.717735
225.131332	8590.995160	26.722752
225.820217	8588.259545	26.727770
225.799425	8580.913815	26.732788
226.315841	8581.091042	26.737805
226.308208	8584.643227	26.742823
226.253809	8578.262932	26.747840
226.667646	8585.235280	26.752858
226.749126	8609.182376	26.757876
227.311630	8609.842918	26.762893
226.960922	8615.153945	26.767911
226.999314	8610.027799	26.772928
227.318426	8618.678089	26.777946
227.093098	8637.539692	26.782964
227.730596	8634.969259	26.787981
227.648160	8661.199937	26.792999
228.057561	8670.583466	26.798016
228.216297	8671.838004	26.803034
228.213775	8690.465052	26.808052
228.531088	8706.164029	26.813069
229.011871	8729.511740	26.818087
228.995630	8738.704656	26.823104
229.454693	8746.857780	26.828122
229.872013	8771.387059	26.833140
230.180067	8773.367377	26.838157
230.216973	8780.361350	26.843175
230.520031	8796.696982	26.848192
230.932565	8805.663009	26.853210
230.673831	8810.990132	26.858228
231.310945	8816.428228	26.863245
231.350054	8829.336664	26.868263
231.235915	8836.990214	26.873280
231.652182	8859.424128	26.878298
231.275822	8870.896527	26.883316
231.916156	8888.730379	26.888333
232.269451	8904.198361	26.893351
232.291495	8920.759145	26.898368
232.836695	8936.572735	26.903386
232.874317	8967.154044	26.908404
233.051767	8971.516507	26.913421
233.388516	8991.706666	26.918439
233.648489	9004.255809	26.923456
234.002242	9023.355708	26.928474
233.780759	9041.307464	26.933492
234.237878	9061.066546	26.938509
234.337759	9071.944950	26.943527
234.828375	9092.761934	26.948544
235.433449	9104.837474	26.953562
234.955376	9129.164211	26.958580
235.628935	9131.840230	26.963597
235.931418	9142.898475	26.968615
235.840014	9158.657184	26.973632
236.524911	9162.664935	26.978650
237.494391	9170.935237	26.983668
237.927119	9174.626693	26.988685
237.905891	9180.889573	26.993703
238.210036	9178.335998	26.998720
238.591015	9170.388027	27.003738
238.777814	9175.400678	27.008756
239.312917	9163.377561	27.013773
239.141049	9152.402878	27.018791
238.934704	9148.023059	27.023808
239.263818	9147.732003	27.028826
239.426137	9158.998333	27.033844
239.658924	9155.395291	27.038861
239.351370	9153.866693	27.043879
239.414973	9169.139925	27.048896
239.918306	9173.801487	27.053914
239.717871	9194.389990	27.058932
240.029867	9210.169042	27.063949
240.326115	9224.521069	27.068967
240.507575	9249.346075	27.073984
240.844361	9259.639894	27.079002
240.570125	9285.341119	27.084020
240.907679	9295.705668	27.089037
241.021234	9322.264331	27.094055
241.269280	9351.057894	27.099072
241.943204	9368.031509	27.104090
241.976986	9391.483782	27.109108
242.270255	9407.272715	27.114125
242.984616	9419.117026	27.119143
242.666740	9441.232857	27.124160
243.454479	9443.057702	27.129178
243.850915	9461.057434	27.134196
244.290643	9476.995444	27.139213
244.382269	9491.758105	27.144231
244.756045	9496.599397	27.149248
245.592007	9491.993892	27.154266
245.439110	9500.373271	27.159284
245.678324	9502.468153	27.164301
246.287429	9496.174899	27.169319
246.019905	9504.905060	27.174336
246.273781	9518.712046	27.179354
246.607124	9529.311167	27.184372
246.933339	9529.122484	27.189389
247.097011	9526.632957	27.194407
247.443258	9549.759427	27.199424
247.497639	9549.405132	27.204442
247.703433	9560.198536	27.209460
247.928423	9548.693212	27.214477
248.083979	9569.604807	27.219495
248.217496	9579.499189	27.224512
248.850791	9577.899255	27.229530
248.990408	9601.374333	27.234548
249.040421	9607.021616	27.239565
249.194630	9614.557228	27.244583
249.280003	9632.012963	27.249600
249.817295	9638.942911	27.254618
249.621437	9648.256703	27.259636
250.124295	9663.565870	27.264653
250.282745	9677.013207	27.269671
250.417635	9696.549835	27.274688
250.888514	9699.249617	27.279706
250.830919	9717.431827	27.284724
251.094858	9714.772818	27.289741
251.568722	9733.926487	27.294759
251.254481	9759.141047	27.299776
251.534058	9763.015650	27.304794
251.822154	9787.290559	27.309812
252.197844	9795.433547	27.314829
252.684387	9820.055819	27.319847
252.457799	9837.064133	27.324864
253.055481	9861.077707	27.329882
252.816187	9872.661425	27.334900
253.145102	9899.864394	27.339917
253.848303	9913.901934	27.344935
253.776500	9936.956343	27.349952
254.142916	9947.437550	27.354970
254.431941	9971.549302	27.359988
254.466894	9988.916291	27.365005
254.994107	10004.363587	27.370023
255.022627	10041.963256	27.375040
255.399701	10056.659716	27.380058
255.265387	10079.428779	27.385076
255.695659	10101.733641	27.390093
256.093359	10122.809667	27.395111
256.294222	10140.479360	27.400128
256.926411	10157.885522	27.405146
257.227575	10182.737452	27.410164
257.361470	10200.709092	27.415181
257.588095	10216.359570	27.420199
257.628583	10238.295478	27.425216
258.079537	10253.334517	27.430234
258.530271	10268.708884	27.435252
258.766334	10272.530742	27.440269
259.548539	10299.539787	27.445287
259.569925	10314.640285	27.450304
259.904475	10312.974965	27.455322
260.231294	10328.576926	27.460340
260.502574	10335.796735	27.465357
260.874242	10330.948613	27.470375
261.032209	10351.933710	27.475392
261.206282	10353.451967	27.480410
261.163921	10365.821025	27.485428
261.621913	10377.617640	27.490445
262.094359	10380.470773	27.495463
262.353107	10394.346653	27.500480
262.352103	10410.059199	27.505498
262.558147	10408.172733	27.510516
262.878782	10431.920110	27.515533
263.218234	10451.834368	27.520551
263.129246	10471.308127	27.525568
263.227438	10485.397790	27.530586
263.706495	10501.684397	27.535604
264.048667	10524.884243	27.540621
263.845800	10526.279225	27.545639
264.083398	10557.400521	27.550656
264.380488	10572.411676	27.555674
264.601855	10588.644617	27.560692
264.838484	10607.664459	27.565709
265.183811	10629.789242	27.570727
265.436624	10649.582593	27.575744
265.858117	10662.416294	27.580762
265.754842	10686.878608	27.585780
266.219758	10701.780498	27.590797
266.537999	10719.915411	27.595815
266.284045	10748.122667	27.600832
266.907367	10766.082678	27.605850
267.288444	10793.891278	27.610868
267.363773	10809.311088	27.615885
268.205736	10836.544149	27.620903
268.633971	10847.813035	27.625920
269.032305	10859.969194	27.630938
269.149681	10859.186698	27.635956
269.275745	10871.153691	27.640973
270.119043	10887.127445	27.645991
269.775952	10907.255002	27.651008
270.151023	10913.944982	27.656026
270.489948	10919.264537	27.661044
270.345770	10942.768837	27.666061
271.092380	10957.804150	27.671079
271.316325	10968.298550	27.676096
271.782718	10972.973066	27.681114
271.841599	10982.471973	27.686132
271.987593	10996.943109	27.691149
272.909363	11006.330844	27.696167
272.650302	11019.432130	27.701184
272.929205	11031.798529	27.706202
273.306573	11046.744232	27.711220
273.343651	11062.752048	27.716237
273.501869	11077.829330	27.721255
273.574502	11098.575430	27.726272
274.038307	11116.435553	27.731290
274.435432	11137.853307	27.736308
274.476892	11152.156488	27.741325
274.935995	11159.255845	27.746343
275.194854	11182.873166	27.751360
275.206416	11204.226542	27.756378
275.696069	11221.185393	27.761396
275.928149	11249.596894	27.766413
275.979097	11266.800659	27.771431
276.191142	11292.253427	27.776448
277.897424	11288.963206	27.781466
278.891517	11281.378229	27.786484
279.227767	11272.274359	27.791501
279.673671	11247.570463	27.796519
279.762153	11236.904193	27.801536
279.823545	11239.520779	27.806554
280.048040	11232.545516	27.811572
280.202376	11240.561848	27.816589
280.315403	11229.725397	27.821607
280.270987	11205.095402	27.826624
280.337066	11206.779918	27.831642
280.619072	11227.426312	27.836660
280.624229	11232.573684	27.841677
281.029590	11234.754489	27.846695
280.846712	11243.459164	27.851712
280.913983	11253.209362	27.856730
281.012574	11266.099185	27.861748
280.971804	11289.004109	27.866765
281.228111	11309.721417	27.871783
281.230787	11330.349510	27.876800
281.502897	11357.355386	27.881818
281.745281	11383.744638	27.886836
281.940750	11413.348630	27.891853
282.093044	11432.483112	27.896871
282.232230	11472.710974	27.901888
282.750610	11504.179073	27.906906
283.421460	11538.475585	27.911924
283.532205	11570.587714	27.916941
283.768303	11589.231067	27.921959
283.975456	11627.669452	27.926976
284.526477	11662.138044	27.931994
285.081529	11675.077650	27.937012
285.487262	11711.267701	27.942029
285.714710	11722.661538	27.947047
286.007009	11730.198825	27.952064
286.427805	11757.762010	27.957082
287.068910	11772.987140	27.962100
286.858584	11787.482182	27.967117
287.580599	11808.456130	27.972135
287.668603	11827.521662	27.977152
287.900656	11847.987955	27.982170
288.340755	11858.654154	27.987188
288.308301	11886.233740	27.992205
288.763590	11896.716506	27.997223
289.084886	11917.711780	28.002240
289.554650	11932.181395	28.007258
289.843769	11946.401965	28.012276
290.181668	11974.329224	28.017293
290.529209	11982.098101	28.022311
290.850918	12001.857247	28.027328
291.025406	12013.911879	28.032346
291.111594	12032.030258	28.037364
291.326314	12056.553891	28.042381
291.506885	12061.244596	28.047399
292.171384	12082.402836	28.052416
292.538307	12104.620396	28.057434
293.138030	12111.014561	28.062452
293.673278	12115.142229	28.067469
294.219464	12117.508128	28.072487
294.247640	12125.418310	28.077504
294.681215	12136.129037	28.082522
294.950030	12132.382399	28.087540
294.445143	12144.572978	28.092557
295.033627	12161.838087	28.097575
295.164252	12168.167335	28.102592
295.041288	12190.344252	28.107610
295.495791	12198.351814	28.112628
295.805826	12214.221303	28.117645
296.234438	12233.075426	28.122663
296.268216	12249.159009	28.127680
296.109171	12276.639442	28.132698
296.395174	12288.814660	28.137716
296.577177	12317.879827	28.142733
296.981741	12349.726563	28.147751
297.048611	12374.907534	28.152768
297.214130	12396.244733	28.157786
298.556033	12397.501581	28.162804
299.095265	12414.753872	28.167821
299.524663	12418.859533	28.172839
300.095597	12432.514055	28.177856
300.315822	12443.783938	28.182874
300.912048	12435.783732	28.187892
300.946812	12449.756632	28.192909
300.868500	12441.297393	28.197927
301.302468	12462.553818	28.202944
301.814539	12467.291089	28.207962
302.168415	12476.613242	28.212980
302.322041	12498.702735	28.217997
302.949326	12501.044849	28.223015
303.024493	12497.616005	28.228032
303.181608	12502.695111	28.233050
303.515381	12519.650356	28.238068
303.450649	12537.511396	28.243085
303.974697	12550.649550	28.248103
303.955104	12563.676991	28.253120
304.269531	12577.858796	28.258138
304.808752	12597.632262	28.263156
304.801634	12614.590687	28.268173
304.922929	12634.453053	28.273191
305.268546	12659.387469	28.278208
305.518333	12672.162089	28.283226
305.692266	12690.641265	28.288244
305.472908	12718.160247	28.293261
305.916365	12744.809906	28.298279
306.384888	12773.592648	28.303296
306.813431	12804.948179	28.308314
307.375129	12820.918894	28.313332
307.624982	12845.325338	28.318349
307.676419	12862.426333	28.323367
308.097789	12882.440444	28.328384
308.313170	12920.200864	28.333402
308.718490	12939.234133	28.338420
308.907510	12963.249004	28.343437
309.159515	12989.952511	28.348455
309.459372	13013.269574	28.353472
309.781974	13046.558282	28.358490
310.256137	13061.881284	28.363508
310.502273	13092.545325	28.368525
311.032549	13109.249495	28.373543
311.363550	13126.732189	28.378560
311.366797	13147.735382	28.383578
311.973602	13165.743785	28.388596
312.069890	13194.502525	28.393613
312.163811	13216.355789	28.398631
312.791243	13234.591239	28.403648
312.783570	13255.477357	28.408666
313.301660	13269.675757	28.413684
313.507398	13312.187510	28.418701
314.069045	13325.193801	28.423719
314.613679	13342.382917	28.428736
314.581271	13371.122157	28.433754
315.202011	13379.767358	28.438772
315.576134	13401.667737	28.443789
315.410292	13421.519035	28.448807
315.650636	13445.545573	28.453824
315.654871	13474.307504	28.458842
316.450303	13492.287312	28.463860
316.597297	13518.281499	28.468877
317.104190	13533.422835	28.473895
317.553932	13560.484504	28.478912
317.727217	13587.377617	28.483930
318.007202	13601.338854	28.488948
318.173567	13631.310762	28.493965
318.435942	13657.142734	28.498983
319.065066	13683.353098	28.504000
319.029446	13716.341688	28.509018
319.527268	13736.601268	28.514036
320.212384	13767.472317	28.519053
320.859856	13773.917838	28.524071
321.350907	13776.058699	28.529088
321.326354	13804.004377	28.534106
322.128502	13813.711899	28.539124
322.337896	13840.216054	28.544141
322.452797	13841.402742	28.549159
322.995084	13856.029132	28.554176
323.344937	13865.361834	28.559194
323.192550	13881.477298	28.564212
323.696695	13903.289971	28.569229
323.954804	13916.470221	28.574247
324.317267	13934.475086	28.579264
324.321693	13956.161428	28.584282
324.866363	13975.211862	28.589300
324.707757	13985.935037	28.594317
324.885656	14023.132920	28.599335
325.766368	14034.806371	28.604352
326.234599	14057.971547	28.609370
326.465336	14067.576650	28.614388
326.826741	14090.281052	28.619405
327.276093	14109.345272	28.624423
327.906836	14118.354580	28.629440
327.843573	14137.060377	28.634458
328.366171	14150.075175	28.639476
328.504500	14157.125328	28.644493
328.324132	14182.297510	28.649511
329.206273	14196.777953	28.654528
329.228697	14220.822040	28.659546
329.607559	14241.775523	28.664564
329.651933	14259.719190	28.669581
329.996729	14275.507940	28.674599
330.336657	14299.290661	28.679616
330.449687	14321.839955	28.684634
330.759124	14339.359949	28.689652
331.096043	14378.815476	28.694669
331.198374	14403.379882	28.699687
331.335206	14436.156839	28.704704
331.760778	14459.796459	28.709722
332.138328	14482.133387	28.714740
332.393133	14524.417790	28.719757
332.696832	14554.959957	28.724775
333.149638	14573.141985	28.729792
333.818156	14612.605191	28.734810
334.883682	14604.200985	28.739828
335.857451	14619.413944	28.744845
336.097360	14637.985627	28.749863
336.869565	14632.707924	28.754880
336.619832	14635.812892	28.759898
337.276227	14635.651162	28.764916
337.458914	14656.982581	28.769933
337.447537	14672.988028	28.774951
337.819095	14663.690344	28.779968
337.904960	14687.287921	28.784986
338.189291	14696.581880	28.790004
338.210533	14711.308572	28.795021
338.342287	14745.003177	28.800039
338.532739	14766.299362	28.805056
338.922265	14792.742011	28.810074
339.032004	14823.993367	28.815092
339.290005	14849.729146	28.820109
339.507002	14880.187468	28.825127
340.185088	14899.649120	28.830144
340.639137	14936.357341	28.835162
341.004745	14965.099697	28.840180
341.845612	14977.432488	28.845197
342.408842	14984.522174	28.850215
343.163120	14992.881409	28.855232
343.452411	15000.850657	28.860250
343.987616	15018.313696	28.865268
344.179980	15030.554054	28.870285
344.242959	15035.748797	28.875303
344.682310	15045.982976	28.880320
344.506846	15064.929009	28.885338
344.971003	15073.999979	28.890356
345.299800	15088.783215	28.895373
345.447500	15102.031780	28.900391
345.701172	15131.877365	28.905408
346.093477	15159.080032	28.910426
346.437308	15168.990394	28.915444
346.710089	15194.577960	28.920461
346.573382	15222.080965	28.925479
347.286480	15244.723251	28.930496
347.521992	15260.730800	28.935514
347.581288	15290.026649	28.940532
347.928691	15309.962140	28.945549
348.057274	15333.045503	28.950567
348.586029	15368.336540	28.955584
348.687814	15390.664911	28.960602
349.066650	15424.708285	28.965620
349.677274	15447.075900	28.970637
349.457354	15479.664823	28.975655
350.210472	15502.807348	28.980672
350.652843	15536.893200	28.985690
351.097167	15572.342632	28.990708
351.901776	15601.437422	28.995725
351.696197	15622.787281	29.000743
352.247525	15647.355923	29.005760
352.543607	15675.314124	29.010778
352.991548	15697.268710	29.015796
353.364236	15727.685195	29.020813
353.438907	15762.087010	29.025831
353.945492	15777.296068	29.030848
354.008121	15812.041807	29.035866
354.462812	15845.384131	29.040884
355.155736	15870.879483	29.045901
355.493184	15909.633211	29.050919
356.373390	15911.272151	29.055936
356.946718	15921.059227	29.060954
357.672420	15933.332417	29.065972
357.903382	15951.324686	29.070989
358.098659	15967.208293	29.076007
358.819708	15976.664016	29.081024
359.022855	15985.563760	29.086042
359.472155	15983.268994	29.091060
359.814487	16007.233586	29.096077
359.724798	16023.979523	29.101095
360.075981	16032.064039	29.106112
360.281917	16064.521958	29.111130
360.693238	16080.883804	29.116148
360.738168	16099.239332	29.121165
360.800816	16135.815957	29.126183
361.128600	16149.726233	29.131200
361.320418	16184.438835	29.136218
361.839592	16200.992855	29.141236
362.304044	16232.550937	29.146253
362.557021	16262.885005	29.151271
362.698791	16283.915476	29.156288
362.858762	16322.435748	29.161306
363.301151	16366.439085	29.166324
363.658668	16398.280279	29.171341
363.966987	16436.136878	29.176359
364.451204	16461.220436	29.181376
364.876293	16506.132187	29.186394
365.121961	16537.053750	29.191412
365.630610	16565.256047	29.196429
366.065224	16599.446658	29.201447
366.392835	16622.281734	29.206464
366.587299	16649.911848	29.211482
367.086123	16679.427667	29.216500
367.678751	16697.086210	29.221517
367.983226	16720.408955	29.226535
368.453425	16743.295497	29.231552
369.443772	16756.609804	29.236570
369.609276	16770.708700	29.241588
370.766204	16782.305605	29.246605
371.022675	16791.319753	29.251623
370.920229	16819.357710	29.256640
371.331295	16826.897689	29.261658
371.474742	16839.845875	29.266676
371.765242	16854.102874	29.271693
371.947645	16894.464433	29.276711
372.247527	16903.152840	29.281728
372.879637	16931.409751	29.286746
372.776707	16961.414517	29.291764
373.212715	16980.564841	29.296781
373.319817	17018.949014	29.301799
373.897029	17039.631987	29.306816
374.208153	17080.687279	29.311834
374.129881	17112.227745	29.316852
374.797100	17145.957698	29.321869
374.802063	17187.833312	29.326887
375.260551	17219.239635	29.331904
375.732682	17250.352511	29.336922
375.931565	17296.624637	29.341940
376.749660	17327.747493	29.346957
376.779938	17367.077835	29.351975
377.135331	17391.082449	29.356992
377.671131	17425.143007	29.362010
378.058123	17468.574245	29.367028
378.499138	17496.835475	29.372045
378.646467	17542.812610	29.377063
379.119568	17576.797272	29.382080
379.630619	17610.089731	29.387098
380.654199	17631.837809	29.392116
381.707446	17638.285672	29.397133
382.087616	17659.346551	29.402151
382.801420	17671.953352	29.407168
383.832338	17662.860820	29.412186
383.884781	17671.699725	29.417204
384.417724	17676.790342	29.422221
384.443480	17695.808895	29.427239
384.664459	17701.214988	29.432256
385.096082	17703.606353	29.437274
385.535284	17722.919688	29.442292
385.370560	17736.013012	29.447309
385.517931	17763.415599	29.452327
385.910001	17778.812802	29.457344
386.226416	17795.225645	29.462362
386.182627	17822.056423	29.467380
386.495531	17843.171973	29.472397
386.748692	17888.121423	29.477415
386.929796	17903.934271	29.482432
387.577030	17931.615775	29.487450
387.523669	17974.801269	29.492468
387.803373	17991.886336	29.497485
388.011668	18027.016982	29.502503
388.605386	18062.928841	29.507520
388.945206	18097.610715	29.512538
389.052943	18144.935761	29.517556
389.697988	18170.391160	29.522573
389.558059	18219.390233	29.527591
390.254881	18252.849750	29.532608
390.657517	18288.691000	29.537626
391.130231	18334.444985	29.542644
391.863540	18364.503843	29.547661
391.599138	18417.462592	29.552679
392.561442	18446.364176	29.557696
393.432810	18479.675886	29.562714
393.598881	18511.488137	29.567732
394.136209	18542.723535	29.572749
394.269440	18574.276560	29.577767
394.809812	18614.489461	29.582784
395.179560	18642.137703	29.587802
395.348373	18675.974816	29.592820
396.554950	18686.174989	29.597837
397.553277	18701.924562	29.602855
398.261702	18712.311628	29.607872
398.860399	18729.634884	29.612890
398.912432	18747.750060	29.617908
399.378436	18740.729004	29.622925
399.731520	18766.474054	29.627943
399.790601	18780.087357	29.632960
400.549168	18796.651683	29.637978
400.522845	18814.304183	29.642996
401.142952	18824.524280	29.648013
401.306783	18850.484684	29.653031
401.596135	18871.523484	29.658048
402.097012	18883.932116	29.663066
402.170930	18917.676204	29.668084
402.220156	18936.342099	29.673101
402.563532	18965.692923	29.678119
402.904909	18993.749500	29.683136
403.466851	19016.773611	29.688154
403.721713	19062.289615	29.693172
404.266016	19086.107668	29.698189
404.687192	19111.217565	29.703207
404.658345	19148.132808	29.708224
405.135289	19186.940204	29.713242
405.465635	19224.928439	29.718260
405.728680	19264.845829	29.723277
405.839990	19304.312640	29.728295
405.843702	19353.034856	29.733312
406.900184	19390.087991	29.738330
406.609905	19438.369463	29.743348
407.592022	19473.237902	29.748365
407.629533	19522.625819	29.753383
408.460173	19558.514786	29.758400
409.054483	19579.469323	29.763418
409.248969	19635.578404	29.768436
409.648751	19658.545825	29.773453
410.190629	19694.104292	29.778471
410.341186	19737.725998	29.783488
410.785401	19771.807855	29.788506
411.105623	19815.278705	29.793524
411.723906	19848.102091	29.798541
412.472909	19890.381024	29.803559
412.725002	19919.122097	29.808576
413.316948	19946.777402	29.813594
413.285615	19993.017017	29.818612
414.442674	20008.705614	29.823629
415.163678	20043.405483	29.828647
415.207967	20072.030317	29.833664
415.779761	20099.354400	29.838682
416.028427	20130.829161	29.843700
416.674018	20151.341179	29.848717
416.999702	20182.852598	29.853735
417.160062	20211.634025	29.858752
417.881215	20235.014156	29.863770
418.043414	20272.746631	29.868788
418.608046	20302.294664	29.873805
418.685741	20328.481908	29.878823
419.442101	20359.675402	29.883840
420.340766	20374.755817	29.888858
420.368677	20420.788785	29.893876
420.788084	20435.073018	29.898893
421.128052	20473.988118	29.903911
421.317792	20510.762257	29.908928
421.928614	20533.346868	29.913946
422.422870	20560.230476	29.918964
422.872031	20597.383248	29.923981
423.031725	20624.714847	29.928999
423.353885	20667.150522	29.934016
424.003521	20701.971117	29.939034
424.197174	20742.088396	29.944052
424.774174	20761.586728	29.949069
425.232764	20805.465917	29.954087
425.452658	20833.004867	29.959104
426.075269	20876.051641	29.964122
426.409127	20908.804432	29.969140
426.509448	20950.131867	29.974157
427.197110	20985.421941	29.979175
427.491209	21017.270849	29.984192
428.055000	21051.245855	29.989210
428.541319	21092.045118	29.994228
428.934636	21126.750766	29.999245
429.367952	21165.711770	30.004263
429.556628	21202.883061	30.009280
430.267661	21232.436294	30.014298
430.393766	21282.261780	30.019316
430.779292	21319.517755	30.024333
431.989941	21335.778829	30.029351
432.137807	21367.462721	30.034368
432.684589	21385.854551	30.039386
433.084257	21422.077546	30.044404
433.581417	21435.360283	30.049421
433.685090	21464.206585	30.054439
433.984628	21508.840035	30.059456
434.075622	21530.954435	30.064474
434.791379	21578.713151	30.069492
435.434025	21603.827976	30.074509
436.145092	21629.672295	30.079527
436.241723	21656.837728	30.084544
436.819028	21679.043395	30.089562
437.432854	21710.160680	30.094580
437.668369	21756.068367	30.099597
437.974275	21778.097674	30.104615
438.070429	21815.870351	30.109632
438.626963	21851.647170	30.114650
439.332057	21895.215229	30.119668
439.477534	21929.914876	30.124685
439.737863	21962.322410	30.129703
439.832873	22005.539034	30.134720
440.338493	22054.225058	30.139738
440.498982	22102.009245	30.144756
441.312785	22143.964915	30.149773
441.979548	22186.332433	30.154791
442.219481	22234.208329	30.159808
442.947691	22267.492620	30.164826
443.863912	22308.109951	30.169844
443.608973	22355.242760	30.174861
444.829833	22367.333466	30.179879
446.012083	22401.492451	30.184896
446.797744	22407.685283	30.189914
447.294483	22434.659122	30.194932
447.525623	22449.541507	30.199949
448.465625	22475.179814	30.204967
448.265250	22492.136366	30.209984
448.862104	22500.866431	30.215002
449.176392	22523.827238	30.220020
449.580172	22552.046411	30.225037
449.908733	22563.267305	30.230055
450.192897	22579.364600	30.235072
450.821707	22615.674329	30.240090
450.958454	22637.675861	30.245108
451.225622	22657.906452	30.250125
451.682630	22692.592787	30.255143
451.965344	22734.985159	30.260160
452.213654	22755.990007	30.265178
452.598385	22793.934065	30.270196
452.572923	22836.220639	30.275213
453.428084	22883.584575	30.280231
453.727204	22923.983592	30.285248
454.066830	22960.465428	30.290266
454.549893	23011.292597	30.295284
455.443617	23037.315703	30.300301
456.461232	23064.681020	30.305319
456.454443	23084.234285	30.310336
457.467792	23112.515655	30.315354
457.985988	23129.281199	30.320372
458.169297	23161.680612	30.325389
458.348786	23175.771615	30.330407
458.855881	23214.923616	30.335424
459.004751	23247.609109	30.340442
459.195609	23274.750481	30.345460
459.722829	23318.630429	30.350477
460.228944	23337.651720	30.355495
460.636424	23395.534184	30.360512
460.957035	23426.257298	30.365530
461.154486	23457.623956	30.370548
461.315086	23508.991682	30.375565
462.062556	23554.652851	30.380583
462.306605	23598.826817	30.385600
462.768141	23642.777989	30.390618
463.129181	23690.099387	30.395636
463.775258	23752.244482	30.400653
464.625668	23784.679872	30.405671
464.418012	23831.168303	30.410688
465.264682	23870.512005	30.415706
465.842795	23917.639583	30.420724
466.243660	23972.598789	30.425741
466.739491	24023.924211	30.430759
466.887276	24068.154198	30.435776
467.582457	24114.624854	30.440794
468.197284	24162.366466	30.445812
468.547029	24203.349887	30.450829
469.529535	24243.907259	30.455847
469.748073	24296.480620	30.460864
470.117053	24336.747622	30.465882
471.004927	24374.271033	30.470900
471.184370	24423.679563	30.475917
471.954192	24453.481522	30.480935
472.389702	24487.489846	30.485952
472.892771	24535.918397	30.490970
473.665671	24578.990665	30.495988
474.213179	24605.819090	30.501005
475.120314	24629.029579	30.506023
475.469109	24666.537946	30.511040
475.995905	24690.157313	30.516058
476.600122	24718.817111	30.521076
476.977784	24748.432382	30.526093
477.691122	24769.947167	30.531111
478.298506	24798.765734	30.536128
478.911414	24817.363716	30.541146
479.087837	24849.121675	30.546164
479.207756	24878.132277	30.551181
480.286450	24887.386395	30.556199
480.515131	24917.826883	30.561216
481.485941	24918.776145	30.566234
482.295751	24928.864055	30.571252
482.736447	24945.800632	30.576269
483.226381	24958.579367	30.581287
483.059454	24987.192349	30.586304
483.326156	24990.309901	30.591322
483.902666	25001.063676	30.596340
483.964862	25033.501147	30.601357
484.410037	25053.546499	30.606375
484.590711	25088.763410	30.611392
485.028976	25116.809896	30.616410
485.243755	25149.170509	30.621428
485.428882	25183.203661	30.626445
486.125487	25224.580325	30.631463
486.212601	25281.677720	30.636480
486.194957	25317.062228	30.641498
486.798886	25369.094788	30.646516
487.323630	25427.408664	30.651533
487.850818	25469.662989	30.656551
488.288704	25532.287761	30.661568
488.415524	25586.080579	30.666586
488.810168	25644.398637	30.671604
489.263016	25708.459467	30.676621
489.717389	25755.382129	30.681639
490.075431	25824.053861	30.686656
490.865295	25880.512002	30.691674
491.364731	25938.266892	30.696692
491.983399	26004.466640	30.701709
492.838296	26052.632578	30.706727
492.919532	26115.556728	30.711744
493.681213	26166.542549	30.716762
494.373401	26207.884633	30.721780
495.110545	26260.218715	30.726797
496.174260	26298.547435	30.731815
496.499186	26345.119789	30.736832
496.932949	26388.702386	30.741850
497.701365	26430.756931	30.746868
498.068798	26472.875468	30.751885
498.518169	26513.830795	30.756903
499.190196	26554.240222	30.761920
499.351968	26595.265210	30.766938
499.965096	26640.256965	30.771956
500.358204	26692.926164	30.776973
500.868366	26728.924574	30.781991
501.155541	26780.184900	30.787008
501.471697	26819.053892	30.792026
502.285560	26867.069655	30.797044
502.377903	26932.336768	30.802061
503.084412	26976.154830	30.807079
503.329554	27033.015002	30.812096
503.954603	27078.515048	30.817114
504.508302	27139.420269	30.822132
504.826862	27187.021099	30.827149
505.512971	27237.046941	30.832167
506.050410	27299.115125	30.837184
506.325625	27343.176230	30.842202
506.842245	27392.295110	30.847220
507.115977	27461.473363	30.852237
507.722021	27507.984581	30.857255
508.366540	27554.919999	30.862272
508.581759	27610.163878	30.867290
509.489197	27653.679150	30.872308
509.928183	27705.487088	30.877325
510.742533	27750.377387	30.882343
511.091537	27797.611143	30.887360
511.725209	27842.465871	30.892378
512.888804	27866.265018	30.897396
513.379328	27916.026282	30.902413
514.384833	27940.181651	30.907431
515.131927	27954.132057	30.912448
515.377981	27984.926189	30.917466
516.030961	28007.357107	30.922484
516.395448	28044.752645	30.927501
516.762626	28078.690404	30.932519
517.388441	28117.568335	30.937536
517.350587	28152.051409	30.942554
517.758733	28183.875926	30.947572
517.945567	28237.033704	30.952589
518.461091	28277.997137	30.957607
519.193695	28320.735206	30.962624
519.304222	28373.929225	30.967642
519.777570	28420.703735	30.972660
520.439245	28468.316699	30.977677
520.960001	28510.639885	30.982695
521.571553	28569.305052	30.987712
522.057845	28626.767477	30.992730
522.784642	28672.154929	30.997748
523.191845	28727.067866	31.002765
523.642619	28771.598139	31.007783
524.784082	28802.512780	31.012800
526.220123	28824.128252	31.017818
526.961977	28854.772555	31.022836
527.363504	28884.309665	31.027853
528.072037	28906.110485	31.032871
528.338758	28932.209968	31.037888
528.750710	28962.648575	31.042906
529.269960	28983.816179	31.047924
529.807153	29022.924724	31.052941
529.920099	29048.363352	31.057959
531.343028	29066.438498	31.062976
531.443350	29098.643218	31.067994
531.859192	29122.585404	31.073012
532.199490	29150.957085	31.078029
532.862676	29181.543619	31.083047
533.084465	29212.066568	31.088064
533.372636	29257.609056	31.093082
533.792955	29288.376317	31.098100
533.878938	29333.037157	31.103117
534.482192	29375.317930	31.108135
535.334746	29423.757467	31.113152
535.614359	29473.620133	31.118170
536.400621	29501.352447	31.123188
536.966723	29550.485727	31.128205
537.635818	29592.556423	31.133223
538.543516	29619.295623	31.138240
539.052781	29647.614459	31.143258
539.683607	29667.319978	31.148276
539.834952	29700.739166	31.153293
539.992842	29740.314890	31.158311
540.694943	29768.254917	31.163328
541.109850	29796.749798	31.168346
541.751980	29824.070640	31.173364
542.774317	29860.147283	31.178381
543.641045	29876.685478	31.183399
544.243018	29901.811129	31.188416
544.129063	29945.881381	31.193434
544.719970	29970.466743	31.198452
545.415863	30006.614624	31.203469
545.350528	30042.548147	31.208487
545.839501	30076.305179	31.213504
546.288954	30122.960720	31.218522
546.877752	30164.976336	31.223540
546.808119	30216.075790	31.228557
547.511753	30260.913431	31.233575
548.299253	30320.264522	31.238592
548.669658	30378.511240	31.243610
549.169814	30430.584452	31.248628
549.652473	30478.877998	31.253645
550.037360	30541.774034	31.258663
550.744433	30591.939242	31.263680
551.040363	30641.864331	31.268698
551.673631	30699.997816	31.273716
552.023622	30770.025890	31.278733
552.491411	30828.502988	31.283751
553.264613	30893.489924	31.288768
553.898906	30956.270587	31.293786
554.485292	31015.597910	31.298804
554.753835	31064.989605	31.303821
555.469671	31125.412617	31.308839
555.724366	31191.462115	31.313856
556.060756	31253.676663	31.318874
556.907680	31312.722402	31.323892
557.284951	31385.957833	31.328909
558.571182	31431.684676	31.333927
559.562322	31486.173390	31.338944
560.494034	31545.392450	31.343962
561.717409	31581.910573	31.348980
562.164473	31613.724535	31.353997
562.725956	31646.540136	31.359015
563.567743	31671.390721	31.364032
563.705200	31714.771531	31.369050
564.260918	31746.437617	31.374068
564.682968	31796.379216	31.379085
565.026265	31835.181745	31.384103
565.861852	31875.015612	31.389120
566.087743	31920.438272	31.394138
567.222159	31943.425265	31.399156
567.763781	31976.068149	31.404173
568.062345	32023.301644	31.409191
569.125276	32043.327378	31.414208
569.615719	32077.471315	31.419226
570.188035	32095.776767	31.424244
570.679361	32124.260364	31.429261
571.096829	32152.115816	31.434279
571.759962	32188.032554	31.439296
571.803144	32222.774503	31.444314
572.340011	32249.047453	31.449332
572.643542	32285.680559	31.454349
573.003706	32332.351857	31.459367
573.864420	32362.635448	31.464384
574.164448	32416.330970	31.469402
574.921697	32459.933420	31.474420
574.812857	32524.047429	31.479437
575.242536	32577.943503	31.484455
576.023644	32621.889364	31.489472
576.281241	32694.742974	31.494490
576.911287	32745.585906	31.499508
577.531881	32813.847184	31.504525
577.962837	32866.441957	31.509543
578.736464	32937.207783	31.514560
578.943031	33000.196761	31.519578
579.697228	33050.322538	31.524596
580.126816	33125.407956	31.529613
580.547764	33194.416682	31.534631
581.173497	33262.341647	31.539648
581.516074	33332.605598	31.544666
582.600640	33393.607144	31.549684
583.057785	33465.297362	31.554701
584.055782	33513.396320	31.559719
585.165040	33561.753564	31.564736
586.159808	33612.295144	31.569754
586.692011	33664.898388	31.574772
587.309477	33721.277883	31.579789
587.421604	33762.265649	31.584807
588.485382	33808.456995	31.589824
589.186149	33857.991535	31.594842
590.077309	33906.627291	31.599860
590.896079	33941.266639	31.604877
591.236521	33991.927782	31.609895
591.932576	34017.084144	31.614912
592.518062	34071.863541	31.619930
593.152776	34108.955533	31.624948
593.530689	34150.471013	31.629965
593.674643	34203.235537	31.634983
594.387062	34241.343290	31.640000
594.423518	34293.713768	31.645018
594.970038	34358.693668	31.650036
595.765069	34408.320454	31.655053
596.180564	34472.069952	31.660071
596.913895	34524.281288	31.665088
597.241771	34583.492305	31.670106
597.638126	34640.996324	31.675124
598.475291	34704.737879	31.680141
598.452914	34765.852977	31.685159
599.641321	34818.172471	31.690176
599.932649	34875.872171	31.695194
600.752194	34929.843039	31.700212
601.255689	34982.745091	31.705229
601.590929	35044.423818	31.710247
602.369022	35103.080974	31.715264
602.801090	35167.730681	31.720282
603.556770	35217.061867	31.725300
604.339775	35275.717269	31.730317
604.624253	35340.102640	31.735335
605.751876	35385.644961	31.740352
606.875185	35426.606609	31.745370
607.642850	35467.093699	31.750388
608.394702	35501.239296	31.755405
608.964150	35553.839407	31.760423
609.436926	35589.628278	31.765440
610.090193	35645.127262	31.770458
610.765004	35684.688448	31.775476
611.610987	35726.541628	31.780493
611.346779	35788.518791	31.785511
612.440189	35819.805879	31.790528
612.863867	35889.180038	31.795546
613.281827	35939.386974	31.800564
614.047261	35975.891561	31.805581
614.887374	36031.001019	31.810599
615.746217	36076.915969	31.815616
615.986649	36119.628083	31.820634
616.576764	36168.802400	31.825652
617.521115	36216.928740	31.830669
617.943078	36274.084269	31.835687
619.057397	36317.073938	31.840704
619.266646	36364.980377	31.845722
619.467347	36421.509454	31.850740
620.844624	36446.518418	31.855757
622.077997	36489.785981	31.860775
622.659981	36519.774678	31.865792
623.015296	36560.407339	31.870810
623.567765	36598.626349	31.875828
624.382628	36637.035428	31.880845
624.617688	36689.149975	31.885863
624.905086	36724.442602	31.890880
625.617491	36781.392776	31.895898
625.729363	36837.056025	31.900916
626.575434	36887.585476	31.905933
626.688657	36952.336975	31.910951
627.467000	37008.993609	31.915968
627.784983	37082.704969	31.920986
628.163973	37146.875649	31.926004
629.220830	37200.354048	31.931021
629.699440	37259.586752	31.936039
630.410887	37311.844939	31.941056
631.116621	37367.815848	31.946074
631.940612	37420.923657	31.951092
632.949200	37478.298884	31.956109
633.508420	37528.625235	31.961127
634.508079	37565.521697	31.966144
634.966184	37614.404328	31.971162
635.266579	37654.168533	31.976180
636.124695	37696.444108	31.981197
636.372907	37747.845545	31.986215
636.528479	37802.271968	31.991232
637.570570	37854.718848	31.996250
638.186515	37917.495524	32.001268
638.866528	37963.630162	32.006285
638.666146	38022.248342	32.011303
639.554296	38080.917276	32.016320
640.367331	38150.708608	32.021338
641.064823	38209.972852	32.026356
641.735886	38266.598752	32.031373
642.239605	38340.448416	32.036391
642.880741	38384.272447	32.041408
643.735976	38441.506642	32.046426
644.546713	38509.253076	32.051444
645.316227	38559.036523	32.056461
645.884222	38614.095260	32.061479
646.867810	38660.019455	32.066496
647.623186	38712.066823	32.071514
648.044640	38763.964112	32.076532
648.838953	38821.371709	32.081549
649.418881	38875.696145	32.086567
650.166666	38934.317848	32.091584
651.425721	38964.464826	32.096602
651.745196	39025.498311	32.101620
652.787349	39065.045196	32.106637
653.021954	39116.080790	32.111655
653.744971	39162.763758	32.116672
654.118327	39223.221684	32.121690
654.435884	39271.084396	32.126708
655.291255	39325.137750	32.131725
655.586773	39389.073160	32.136743
656.090451	39447.603042	32.141760
656.626054	39517.165049	32.146778
657.040549	39595.123373	32.151796
657.751594	39654.410992	32.156813
658.119940	39726.192451	32.161831
658.499680	39799.893143	32.166848
659.504622	39871.154360	32.171866
659.787169	39953.522471	32.176884
661.295831	40014.002677	32.181901
661.535446	40087.174975	32.186919
662.184935	40153.141657	32.191936
663.194352	40226.330737	32.196954
663.641765	40295.906801	32.201972
664.613624	40372.805315	32.206989
665.448058	40431.460943	32.212007
666.395707	40498.034363	32.217024
667.007147	40555.480071	32.222042
667.364132	40633.379736	32.227060
668.613430	40675.471111	32.232077
669.613285	40727.954082	32.237095
671.096473	40751.711448	32.242112
671.719102	40776.766599	32.247130
672.570776	40815.559355	32.252148
673.148882	40844.346713	32.257165
673.775914	40881.929513	32.262183
674.361654	40905.965635	32.267200
674.624150	40956.270514	32.272218
675.009764	40989.589738	32.277236
675.697240	41030.285849	32.282253
676.102282	41089.251825	32.287271
676.366325	41143.405094	32.292288
677.132575	41181.098856	32.297306
677.567987	41229.329931	32.302324
678.231557	41284.609156	32.307341
678.500408	41363.664836	32.312359
679.036203	41414.520528	32.317376
679.813778	41476.541735	32.322394
680.473169	41554.880020	32.327412
681.411513	41607.873854	32.332429
681.991566	41687.613253	32.337447
682.519695	41751.962027	32.342464
683.542980	41814.285988	32.347482
683.963095	41877.065814	32.352500
684.614142	41944.562666	32.357517
685.367630	42014.046476	32.362535
685.904840	42080.129916	32.367552
686.861827	42145.784012	32.372570
687.457069	42221.735070	32.377588
687.885628	42292.782690	32.382605
688.889160	42374.580735	32.387623
689.219857	42434.238190	32.392640
690.037429	42500.739139	32.397658
690.856460	42578.034613	32.402676
691.191478	42649.720018	32.407693
691.927957	42722.136719	32.412711
692.450112	42808.600068	32.417728
693.458940	42877.478883	32.422746
693.872705	42967.881326	32.427764
694.689929	43040.526244	32.432781
695.951611	43108.198540	32.437799
696.416320	43184.556306	32.442816
697.012302	43256.981841	32.447834
697.911103	43318.703294	32.452852
699.077698	43383.805055	32.457869
700.201183	43445.538503	32.462887
701.241479	43492.209534	32.467904
702.635474	43544.572086	32.472922
703.217505	43600.423765	32.477940
703.992356	43645.137442	32.482957
704.334141	43692.390277	32.487975
704.673758	43732.406811	32.492992
706.358483	43765.846311	32.498010
707.162055	43809.161478	32.503028
707.992303	43844.872898	32.508045
708.398291	43878.427896	32.513063
709.132233	43913.987595	32.518080
709.569176	43937.786649	32.523098
709.748540	43975.513718	32.528116
710.520332	44021.825130	32.533133
710.901895	44058.974420	32.538151
711.304212	44113.581861	32.543168
712.217070	44155.394618	32.548186
712.704471	44217.273108	32.553204
713.068869	44266.202223	32.558221
713.457177	44329.046466	32.563239
713.806649	44396.263325	32.568256
714.762800	44451.121199	32.573274
715.225482	44531.898743	32.578292
715.846333	44600.827246	32.583309
716.416841	44680.421028	32.588327
716.545823	44758.596391	32.593344
717.407444	44836.623900	32.598362
718.053730	44933.886570	32.603380
718.439639	45005.343268	32.608397
719.375280	45105.570578	32.613415
719.829932	45202.874719	32.618432
721.264913	45273.919394	32.623450
721.610747	45370.825343	32.628468
722.581549	45453.100553	32.633485
724.101949	45524.151575	32.638503
724.718555	45591.532408	32.643520
725.964283	45672.064336	32.648538
726.324530	45755.201688	32.653556
727.432035	45822.319102	32.658573
728.020516	45892.718623	32.663591
728.380775	45972.134051	32.668608
729.365052	46032.835577	32.673626
729.967944	46121.034615	32.678644
730.667344	46186.833319	32.683661
731.600437	46262.584131	32.688679
732.357174	46338.719878	32.693696
733.315114	46407.797434	32.698714
734.333394	46475.231289	32.703732
735.159957	46535.984907	32.708749
735.085380	46614.305056	32.713767
735.886766	46685.973784	32.718784
736.583555	46753.920550	32.723802
737.428860	46838.926237	32.728820
737.894065	46927.160698	32.733837
738.850859	46996.799223	32.738855
739.370494	47075.011030	32.743872
740.151533	47144.734916	32.748890
740.435754	47240.976273	32.753908
741.354620	47314.865948	32.758925
741.940553	47402.850070	32.763943
742.253752	47494.197457	32.768960
743.265727	47582.439639	32.773978
744.247045	47667.613823	32.778996
744.718789	47743.504400	32.784013
746.391465	47816.421050	32.789031
747.772258	47875.907772	32.794048
748.782514	47929.672985	32.799066
749.342132	47990.710767	32.804084
750.197869	48040.846947	32.809101
750.985559	48099.359162	32.814119
751.519161	48152.771802	32.819136
752.305936	48204.014364	32.824154
752.482337	48264.905841	32.829172
753.281887	48333.953042	32.834189
753.998126	48397.964993	32.839207
754.696512	48467.363301	32.844224
755.127855	48527.748075	32.849242
755.438275	48617.788995	32.854260
756.005273	48691.841412	32.859277
756.959551	48770.455366	32.864295
757.415685	48853.355348	32.869312
758.373463	48940.306511	32.874330
759.107233	49027.341097	32.879348
759.523632	49119.680734	32.884365
760.572737	49201.418178	32.889383
761.257364	49291.099982	32.894400
762.080532	49375.225149	32.899418
763.057678	49466.325491	32.904436
763.989922	49550.541413	32.909453
765.064377	49629.222072	32.914471
765.352227	49715.109746	32.919488
766.511267	49787.024393	32.924506
767.462930	49872.819767	32.929524
767.793157	49960.150359	32.934541
768.516322	50031.138159	32.939559
769.441409	50119.447789	32.944576
770.472227	50202.388773	32.949594
770.943690	50295.584096	32.954612
771.713768	50372.927924	32.959629
772.673821	50456.600883	32.964647
773.507466	50536.734539	32.969664
774.491095	50621.243973	32.974682
775.029182	50697.123933	32.979700
775.682189	50784.675404	32.984717
776.555056	50871.059322	32.989735
776.916710	50955.404249	32.994752
778.183197	51040.568089	32.999770
779.053092	51127.764795	33.004788
779.627619	51201.725411	33.009805
780.844230	51283.843355	33.014823
781.335315	51375.860813	33.019840
782.403365	51457.040614	33.024858
782.870317	51540.421553	33.029876
783.525368	51632.373188	33.034893
784.087985	51712.643602	33.039911
784.770856	51792.800545	33.044928
785.921191	51878.176208	33.049946
786.060165	51977.278267	33.054964
786.640688	52068.836850	33.059981
787.514476	52157.660170	33.064999
787.924828	52263.036048	33.070016
788.902256	52350.303607	33.075034
790.097456	52448.277464	33.080052
790.671983	52526.652719	33.085069
791.578025	52606.910307	33.090087
792.177978	52704.992938	33.095104
792.867476	52793.141716	33.100122
793.690622	52891.868423	33.105140
794.351814	52974.606419	33.110157
795.475157	53065.708030	33.115175
795.889987	53177.350621	33.120192
796.635848	53261.894491	33.125210
797.780000	53362.999886	33.130228
797.843416	53453.969163	33.135245
798.750275	53556.606373	33.140263
799.493296	53670.876367	33.145280
800.661138	53768.956405	33.150298
801.539567	53868.863278	33.155316
802.780894	53955.979761	33.160333
804.362381	54030.703850	33.165351
805.244543	54126.233512	33.170368
806.069823	54214.421225	33.175386
806.843726	54283.826782	33.180404
807.674244	54374.624876	33.185421
809.135768	54447.842013	33.190439
809.908477	54527.138148	33.195456
810.855101	54588.244027	33.200474
811.633957	54669.392708	33.205492
812.047206	54751.928876	33.210509
813.056885	54816.636631	33.215527
813.626699	54901.080394	33.220544
814.173696	54976.115083	33.225562
814.868673	55056.770616	33.230580
815.693431	55145.228062	33.235597
816.509674	55221.815015	33.240615
817.258828	55319.524941	33.245632
818.440231	55398.548296	33.250650
819.052414	55490.696718	33.255668
819.160824	55581.669409	33.260685
819.945311	55676.051559	33.265703
820.866547	55773.259836	33.270720
821.716245	55864.257980	33.275738
823.237467	55953.826982	33.280756
824.109084	56036.422234	33.285773
825.923798	56100.157195	33.290791
826.358530	56176.859369	33.295808
827.022844	56250.179051	33.300826
827.759302	56332.528814	33.305844
828.902382	56403.474697	33.310861
830.314317	56466.075428	33.315879
830.811466	56544.881160	33.320896
831.834045	56610.717051	33.325914
832.610042	56679.670434	33.330932
833.299634	56747.577095	33.335949
834.144473	56813.849249	33.340967
834.808538	56869.640887	33.345984
835.770781	56925.950330	33.351002
836.665926	56984.180598	33.356020
837.350025	57046.813920	33.361037
837.814796	57112.762491	33.366055
838.517069	57189.382090	33.371072
838.611774	57256.545545	33.376090
839.371878	57340.348273	33.381108
840.123753	57421.756485	33.386125
841.036231	57499.622516	33.391143
841.385261	57589.152426	33.396160
842.208070	57682.689486	33.401178
842.998812	57772.153128	33.406196
843.852008	57865.518946	33.411213
845.229855	57957.090551	33.416231
846.113803	58062.749557	33.421248
846.378089	58150.581320	33.426266
847.384913	58237.379722	33.431284
847.944766	58332.824655	33.436301
848.975242	58433.998152	33.441319
849.705979	58546.282897	33.446336
850.330234	58647.648501	33.451354
851.523544	58743.180989	33.456372
852.072821	58854.059906	33.461389
853.378120	58944.770195	33.466407
853.829743	59056.142611	33.471424
854.354147	59170.642512	33.476442
855.376199	59279.083845	33.481460
856.208850	59391.935252	33.486477
857.098386	59494.207286	33.491495
858.323764	59602.602347	33.496512
858.809854	59713.215403	33.501530
859.451116	59827.306039	33.506548
860.298404	59944.670461	33.511565
861.595766	60058.073941	33.516583
862.070191	60172.748951	33.521600
863.115112	60285.682466	33.526618
864.064214	60393.216700	33.531636
864.911988	60510.515114	33.536653
866.110953	60619.384419	33.541671
867.327400	60732.151226	33.546688
868.306507	60828.978866	33.551706
869.169583	60926.854865	33.556724
870.572501	61025.485391	33.561741
871.623377	61110.913371	33.566759
872.675124	61206.809352	33.571776
873.299427	61284.733864	33.576794
874.952484	61380.636074	33.581812
875.175667	61468.875158	33.586829
876.059796	61559.096734	33.591847
877.046020	61647.104686	33.596864
877.927172	61743.096857	33.601882
878.686832	61818.646323	33.606900
879.680758	61912.369895	33.611917
880.416293	61991.640636	33.616935
881.113564	62083.647047	33.621952
881.620693	62171.828426	33.626970
882.658645	62259.622577	33.631988
883.286994	62339.552880	33.637005
884.101982	62418.095920	33.642023
885.041802	62515.146877	33.647040
885.960220	62594.432085	33.652058
887.073926	62685.269865	33.657076
887.644830	62788.428388	33.662093
888.504686	62869.694631	33.667111
889.487921	62967.959969	33.672128
890.144079	63069.031648	33.677146
891.120263	63152.585929	33.682164
891.751709	63261.361809	33.687181
892.879075	63347.697221	33.692199
893.520313	63449.089095	33.697216
894.944634	63549.175758	33.702234
896.283021	63628.240535	33.707252
897.258123	63724.663586	33.712269
898.370747	63803.035494	33.717287
899.308068	63895.978854	33.722304
899.951289	63987.598831	33.727322
900.867059	64076.020861	33.732340
901.075435	64179.339344	33.737357
902.445787	64257.182581	33.742375
903.462802	64345.965572	33.747392
904.280253	64438.955912	33.752410
905.753935	64520.848422	33.757428
906.462804	64614.100078	33.762445
906.852890	64698.765043	33.767463
907.763660	64799.799037	33.772480
908.389946	64892.348255	33.777498
909.622416	64989.523138	33.782516
910.226243	65096.898917	33.787533
911.293726	65195.484450	33.792551
911.626280	65307.209409	33.797568
912.233630	65417.943768	33.802586
913.526583	65526.447204	33.807604
913.948117	65645.954918	33.812621
914.988867	65762.774903	33.817639
916.244933	65867.075920	33.822656
916.920712	65987.619165	33.827674
917.551238	66105.438259	33.832692
918.366009	66221.851635	33.837709
919.207896	66335.627173	33.842727
920.392794	66463.505459	33.847744
921.188768	66589.829288	33.852762
922.564169	66701.273164	33.857780
923.302633	66827.955143	33.862797
924.066964	66946.452955	33.867815
925.138162	67067.492757	33.872832
926.164982	67184.484632	33.877850
926.767198	67302.492391	33.882868
927.634944	67424.918717	33.887885
928.722939	67537.297572	33.892903
929.845894	67637.023868	33.897920
930.469314	67756.414536	33.902938
931.615472	67861.931478	33.907956
932.127462	67977.177948	33.912973
933.095516	68085.952745	33.917991
934.122507	68202.167320	33.923008
935.166469	68324.305912	33.928026
935.978116	68441.295351	33.933044
936.661381	68562.450397	33.938061
937.547305	68674.185634	33.943079
938.457591	68805.446191	33.948096
939.302900	68931.613085	33.953114
940.425302	69037.285468	33.958132
941.320891	69174.104314	33.963149
941.737530	69299.950075	33.968167
943.274555	69428.537309	33.973184
943.717339	69565.007619	33.978202
945.051885	69678.585262	33.983220
945.928599	69811.191016	33.988237
947.004277	69940.619515	33.993255
948.480456	70061.657637	33.998272
949.414062	70179.415174	34.003290
951.338359	70287.550872	34.008308
952.905270	70369.175221	34.013325
954.178014	70469.252249	34.018343
955.783384	70548.470227	34.023360
956.898418	70638.242563	34.028378
958.020070	70707.460198	34.033396
959.229801	70801.382094	34.038413
960.236690	70855.359289	34.043431
961.466495	70923.859117	34.048448
962.429848	71001.032763	34.053466
963.049939	71066.812016	34.058484
964.360974	71137.555403	34.063501
965.011990	71215.411448	34.068519
965.520439	71289.733069	34.073536
966.232935	71376.779958	34.078554
967.130603	71454.919951	34.083572
967.908304	71550.481194	34.088589
968.519205	71640.148732	34.093607
968.971870	71730.170432	34.098624
969.940058	71843.521842	34.103642
970.638667	71941.726193	34.108660
971.533212	72048.215544	34.113677
972.212377	72157.286271	34.118695
973.190760	72272.597377	34.123712
973.924090	72387.689062	34.128730
974.648608	72505.594794	34.133748
975.813031	72629.952539	34.138765
976.908983	72748.906450	34.143783
977.702460	72869.040331	34.148800
978.107144	73000.181676	34.153818
979.162894	73116.193095	34.158836
980.177137	73239.902369	34.163853
980.878058	73378.733872	34.168871
981.691111	73497.781483	34.173888
982.841908	73623.038599	34.178906
984.139912	73726.243476	34.183924
985.080811	73850.732841	34.188941
985.801673	73980.484234	34.193959
987.095775	74090.889547	34.198976
988.071252	74212.026281	34.203994
989.105429	74329.217272	34.209012
990.342981	74452.159086	34.214029
990.869156	74572.983978	34.219047
991.993252	74697.885495	34.224064
992.929451	74824.005800	34.229082
994.427605	74939.862561	34.234100
995.472310	75050.489771	34.239117
997.387983	75141.109271	34.244135
999.287628	75226.277643	34.249152
1000.707725	75324.655518	34.254170
1001.924319	75404.460247	34.259188
1002.806493	75479.167703	34.264205
1003.898746	75571.209427	34.269223
1004.835396	75652.115118	34.274240
1005.655885	75737.804949	34.279258
1006.674929	75811.765048	34.284276
1007.653143	75901.690225	34.289293
1008.120925	76001.297325	34.294311
1009.175648	76077.685979	34.299328
1009.878286	76181.295192	34.304346
1010.650297	76279.066630	34.309364
1011.754943	76386.556762	34.314381
1012.118212	76489.437822	34.319399
1013.340088	76602.352228	34.324416
1014.169039	76718.736458	34.329434
1015.040913	76824.692161	34.334452
1015.882556	76946.681877	34.339469
1016.445748	77081.085820	34.344487
1017.535817	77199.573895	34.349504
1018.231286	77334.596832	34.354522
1019.153419	77470.545331	34.359540
1019.924997	77611.252854	34.364557
1020.994558	77754.037691	34.369575
1022.220284	77879.245982	34.374592
1022.905124	78024.830789	34.379610
1023.742352	78162.902206	34.384628
1025.225572	78299.462223	34.389645
1025.560698	78454.978908	34.394663
1027.107559	78591.322149	34.399680
1027.863589	78743.879053	34.404698
1029.083191	78895.225546	34.409716
1029.948571	79034.764812	34.414733
1031.063755	79178.677432	34.419751
1032.190929	79321.192166	34.424768
1033.220913	79465.777741	34.429786
1034.450862	79607.114991	34.434804
1035.528658	79756.233659	34.439821
1036.533585	79901.597464	34.444839
1037.742731	80032.927904	34.449856
1038.345957	80161.447709	34.454874
1039.428931	80283.538908	34.459892
1040.742543	80412.389756	34.464909
1041.708101	80539.899711	34.469927
1042.575344	80676.756755	34.474944
1043.422436	80819.332660	34.479962
1044.323454	80951.577665	34.484980
1045.417873	81089.298955	34.489997
1046.412085	81231.784736	34.495015
1047.586921	81375.532402	34.500032
1048.428027	81525.991053	34.505050
1049.406385	81662.748379	34.510068
1050.758488	81802.329942	34.515085
1051.728184	81955.344249	34.520103
1053.309880	82085.951905	34.525120
1054.231015	82233.134421	34.530138
1055.835733	82368.007565	34.535156
1056.668861	82502.093932	34.540173
1057.865315	82646.750947	34.545191
1059.002573	82774.367330	34.550208
1059.770811	82916.192417	34.555226
1060.653615	83068.773449	34.560244
1061.814110	83203.425468	34.565261
1062.765534	83353.228451	34.570279
1064.388898	83491.671663	34.575296
1065.522556	83635.384441	34.580314
1066.372717	83769.836540	34.585332
1067.664811	83906.899957	34.590349
1068.602063	84044.109226	34.595367
1069.919975	84182.434841	34.600384
1071.034660	84325.801254	34.605402
1071.926431	84461.199521	34.610420
1073.532673	84595.972855	34.615437
1073.732012	84735.257706	34.620455
1075.006400	84868.852611	34.625472
1076.141901	85021.717325	34.630490
1077.300799	85150.944284	34.635508
1078.800458	85297.714653	34.640525
1079.870733	85439.590767	34.645543
1080.952904	85567.801804	34.650560
1082.094263	85707.531198	34.655578
1083.175158	85840.189210	34.660596
1084.174076	85969.813314	34.665613
1085.424722	86111.608286	34.670631
1086.348813	86239.171909	34.675648
1087.797640	86378.079011	34.680666
1088.511694	86507.309047	34.685684
1089.918056	86642.930162	34.690701
1091.150112	86783.183305	34.695719
1091.809831	86904.754075	34.700736
1093.034342	87046.534085	34.705754
1094.174252	87178.078044	34.710772
1095.197263	87306.100203	34.715789
1095.844952	87445.932080	34.720807
1097.198056	87586.013104	34.725824
1098.209479	87710.523557	34.730842
1098.741167	87843.616440	34.735860
1099.919303	87966.988876	34.740877
1101.040022	88102.253563	34.745895
1102.315098	88240.820881	34.750912
1103.301387	88368.089984	34.755930
1104.099997	88507.177462	34.760948
1105.443089	88637.110673	34.765965
1106.748859	88780.773665	34.770983
1107.680649	88903.128180	34.776000
1108.726434	89039.036701	34.781018
1109.837137	89187.735748	34.786036
1111.200163	89326.055682	34.791053
1111.525624	89474.299758	34.796071
1112.739779	89621.518093	34.801088
1113.672853	89774.904032	34.806106
1114.769319	89931.585332	34.811124
1116.286686	90079.536416	34.816141
1116.926292	90246.076435	34.821159
1117.946882	90397.308835	34.826176
1119.032044	90556.273204	34.831194
1120.258279	90715.108768	34.836212
1121.897952	90871.583892	34.841229
1122.915907	91025.629158	34.846247
1124.318564	91176.774529	34.851264
1125.802628	91326.307834	34.856282
1126.615946	91479.357888	34.861300
1128.155764	91629.529508	34.866317
1128.944874	91783.888434	34.871335
1130.495332	91924.193585	34.876352
1131.960881	92075.809478	34.881370
1132.542034	92220.514712	34.886388
1133.864821	92359.328187	34.891405
1135.049651	92519.644399	34.896423
1136.142301	92656.320510	34.901440
1137.469330	92809.879962	34.906458
1138.509444	92964.087001	34.911476
1140.051514	93106.102443	34.916493
1140.767118	93255.201716	34.921511
1142.329024	93392.048075	34.926528
1143.700768	93531.367106	34.931546
1144.964519	93658.578402	34.936564
1146.676203	93787.800249	34.941581
1147.443046	93924.535956	34.946599
1148.745459	94067.133298	34.951616
1149.978749	94192.752125	34.956634
1150.650789	94334.040824	34.961652
1151.768942	94463.341992	34.966669
1152.722433	94624.766495	34.971687
1153.509919	94764.445473	34.976704
1154.751028	94910.587669	34.981722
1155.312724	95061.969079	34.986740
1156.710100	95211.738357	34.991757
1157.566359	95365.889956	34.996775
1158.316043	95514.448469	35.001792
1159.492714	95663.888945	35.006810
1160.155596	95821.623267	35.011828
1161.531390	95966.289575	35.016845
1162.430477	96129.517437	35.021863
1163.419516	96294.357984	35.026880
1164.610470	96452.670633	35.031898
1165.225929	96628.264255	35.036916
1166.644295	96782.430990	35.041933
1167.464665	96963.118886	35.046951
1168.867121	97128.386858	35.051968
1170.480152	97300.119765	35.056986
1171.917295	97470.654605	35.062004
1173.216619	97625.162297	35.067021
1174.317422	97788.521808	35.072039
1175.991848	97955.549259	35.077056
1177.034529	98111.967398	35.082074
1178.297456	98275.734813	35.087092
1179.328128	98426.773004	35.092109
1180.605209	98604.541555	35.097127
1181.633837	98762.434171	35.102144
1183.292670	98925.282811	35.107162
1184.390547	99095.700211	35.112180
1185.832128	99251.683055	35.117197
1187.547983	99422.029902	35.122215
1189.249196	99555.575962	35.127232
1190.912087	99677.638937	35.132250
1192.312822	99819.826466	35.137268
1194.191194	99937.908439	35.142285
1195.518992	100070.131215	35.147303
1196.444792	100185.822410	35.152320
1197.995525	100302.756180	35.157338
1199.386881	100421.373628	35.162356
1200.817918	100532.082577	35.167373
1202.183932	100644.409535	35.172391
1203.525005	100759.752827	35.177408
1204.379737	100873.237846	35.182426
1205.026304	100996.437477	35.187444
1205.955365	101112.885733	35.192461
1207.094060	101242.272587	35.197479
1208.046119	101366.773350	35.202496
1208.839062	101498.121187	35.207514
1209.826700	101639.569285	35.212532
1210.650491	101777.633695	35.217549
1211.562653	101942.121897	35.222567
1212.441789	102097.631138	35.227584
1213.602065	102248.471109	35.232602
1214.408505	102413.485646	35.237620
1215.777785	102585.714182	35.242637
1216.554237	102758.905167	35.247655
1217.675242	102922.082453	35.252672
1219.694436	103084.004320	35.257690
1220.865399	103246.720293	35.262708
1221.969883	103403.297072	35.267725
1222.972962	103579.305671	35.272743
1223.827193	103740.986972	35.277760
1225.195810	103896.360630	35.282778
1226.050084	104059.866620	35.287796
1227.730045	104206.516780	35.292813
1229.160014	104364.699838	35.297831
1229.968897	104523.071302	35.302848
1230.973725	104689.076371	35.307866
1231.962858	104856.502665	35.312884
1233.221513	105028.228632	35.317901
1234.248113	105200.442059	35.322919
1235.626481	105384.099853	35.327936
1237.141005	105541.093822	35.332954
1238.323094	105727.608033	35.337972
1239.882591	105887.982974	35.342989
1241.042244	106069.377139	35.348007
1242.374017	106236.739618	35.353024
1243.962841	106406.207877	35.358042
1244.692081	106584.098550	35.363060
1245.972650	106752.656264	35.368077
1247.317272	106932.331359	35.373095
1248.192683	107116.886145	35.378112
1249.877512	107284.585834	35.383130
1250.316671	107478.776009	35.388148
1251.903326	107661.633244	35.393165
1253.555131	107836.557289	35.398183
1254.965696	108028.951812	35.403200
1256.375819	108205.879023	35.408218
1257.660857	108394.581076	35.413236
1258.968722	108559.906369	35.418253
1260.388230	108743.197068	35.423271
1261.367809	108924.229823	35.428288
1262.950120	109097.724516	35.433306
1263.896241	109294.051236	35.438324
1264.940467	109475.394269	35.443341
1266.621031	109656.118432	35.448359
1268.040919	109837.727230	35.453376
1268.954054	110015.094682	35.458394
1270.379969	110197.559701	35.463412
1271.714748	110371.425574	35.468429
1273.060361	110558.115410	35.473447
1274.134853	110737.861453	35.478464
1275.705479	110922.473682	35.483482
1276.687117	111114.257963	35.488500
1277.998331	111295.958069	35.493517
1279.660269	111477.198614	35.498535
1280.708928	111663.849044	35.503552
1281.882953	111843.967093	35.508570
1283.018847	112037.734342	35.513588
1284.975219	112217.490159	35.518605
1285.994868	112408.999842	35.523623
1286.973459	112593.098219	35.528640
1288.598816	112776.481067	35.533658
1290.030340	112962.611882	35.538676
1291.148728	113151.313441	35.543693
1292.310548	113333.913099	35.548711
1293.290748	113505.084406	35.553728
1294.645571	113671.347978	35.558746
1295.617872	113852.652077	35.563764
1297.383826	114021.530519	35.568781
1298.716276	114195.644994	35.573799
1299.695116	114376.420022	35.578816
1301.105510	114545.643387	35.583834
1302.244865	114726.363741	35.588852
1303.520199	114905.645612	35.593869
1305.068345	115081.365296	35.598887
1305.986542	115264.562107	35.603904
1307.257945	115451.103927	35.608922
1308.469731	115642.803875	35.613940
1309.864219	115830.063323	35.618957
1311.470980	116012.858479	35.623975
1312.354946	116219.392162	35.628992
1313.958962	116405.774116	35.634010
1315.484766	116595.025348	35.639028
1316.700437	116789.050582	35.644045
1318.084826	116971.856274	35.649063
1319.158216	117163.842868	35.654080
1320.718628	117354.860710	35.659098
1321.615117	117558.699552	35.664116
1322.941369	117755.671389	35.669133
1324.404863	117953.059804	35.674151
1325.380581	118161.278730	35.679168
1327.038738	118359.798027	35.684186
1328.747446	118568.828161	35.689204
1329.576769	118778.753275	35.694221
1330.955902	118975.966588	35.699239
1332.580068	119181.323503	35.704256
1333.936904	119377.542928	35.709274
1335.038381	119591.255928	35.714292
1336.484892	119794.075031	35.719309
1338.023705	119995.766549	35.724327
1338.948293	120211.349088	35.729344
1340.238594	120411.462224	35.734362
1341.557198	120625.313772	35.739380
1342.612506	120832.585125	35.744397
1344.499020	121045.602575	35.749415
1346.192280	121265.972939	35.754432
1347.624296	121462.968556	35.759450
1348.805268	121672.746911	35.764468
1350.675788	121870.955061	35.769485
1352.542111	122052.548140	35.774503
1353.952755	122249.692317	35.779520
1355.953074	122432.989226	35.784538
1357.500480	122610.216464	35.789556
1358.659132	122794.865567	35.794573
1360.172841	122970.947958	35.799591
1361.837322	123142.561751	35.804608
1363.455930	123299.731855	35.809626
1364.892801	123477.235735	35.814644
1366.392125	123641.633893	35.819661
1367.486755	123797.750233	35.824679
1368.556383	123961.281333	35.829696
1369.514830	124109.137261	35.834714
1371.145451	124266.298446	35.839732
1371.761315	124430.575847	35.844749
1373.191915	124595.332751	35.849767
1374.490143	124772.170529	35.854784
1375.794271	124951.288571	35.859802
1376.878654	125111.239546	35.864820
1377.818731	125289.518328	35.869837
1379.058320	125464.444544	35.874855
1380.248753	125662.852112	35.879872
1382.099287	125841.040466	35.884890
1382.973187	126037.524967	35.889908
1384.095029	126235.390234	35.894925
1385.107923	126449.020096	35.899943
1386.411839	126658.501026	35.904960
1387.880974	126866.551169	35.909978
1389.066825	127073.279778	35.914996
1390.460578	127290.440668	35.920013
1392.003155	127496.178323	35.925031
1393.465394	127702.335663	35.930048
1394.816460	127922.650026	35.935066
1396.148903	128140.093378	35.940084
1398.100603	128348.926785	35.945101
1400.065481	128555.263960	35.950119
1401.196772	128770.172496	35.955136
1403.070283	128975.007067	35.960154
1404.441490	129177.414541	35.965172
1406.212596	129383.155207	35.970189
1407.799179	129577.904641	35.975207
1409.204648	129780.754456	35.980224
1410.670908	129977.400825	35.985242
1412.150991	130168.687253	35.990260
1413.488593	130364.292556	35.995277
1415.005110	130557.058156	36.000295
1416.074571	130759.448988	36.005312
1417.754771	130951.950552	36.010330
1419.300287	131154.382583	36.015348
1420.919910	131342.892795	36.020365
1422.939815	131519.925045	36.025383
1424.503589	131709.105406	36.030400
1426.070407	131886.858125	36.035418
1427.694117	132067.441031	36.040436
1429.158243	132250.850568	36.045453
1430.426865	132413.703081	36.050471
1431.879253	132603.743330	36.055488
1433.089239	132777.681170	36.060506
1434.519376	132960.403789	36.065524
1435.828655	133147.011326	36.070541
1437.119222	133321.535180	36.075559
1438.520485	133519.445474	36.080576
1440.488452	133702.150697	36.085594
1441.626142	133877.449801	36.090612
1443.093378	134050.796944	36.095629
1444.467626	134215.670259	36.100647
1445.619152	134394.961705	36.105664
1447.708428	134548.407918	36.110682
1448.942736	134711.253552	36.115700
1450.209941	134872.827731	36.120717
1451.607771	135028.857292	36.125735
1453.222552	135194.838385	36.130752
1454.284166	135367.307493	36.135770
1455.597095	135530.031173	36.140788
1456.487195	135711.526467	36.145805
1457.926098	135891.339025	36.150823
1459.353566	136072.941245	36.155840
1460.572868	136266.793477	36.160858
1462.242345	136460.892255	36.165876
1463.210998	136667.877231	36.170893
1464.651981	136857.110802	36.175911
1465.525085	137071.932580	36.180928
1466.463448	137285.009424	36.185946
1468.070667	137500.097830	36.190964
1468.894509	137730.456068	36.195981
1470.508581	137952.022376	36.200999
1471.683831	138187.891644	36.206016
1473.093070	138429.111590	36.211034
1474.402193	138665.153454	36.216052
1475.667478	138923.432818	36.221069
1477.363895	139167.933453	36.226087
1478.919141	139410.937712	36.231104
1480.688129	139661.361957	36.236122
1482.127249	139909.774913	36.241140
1483.582101	140161.153049	36.246157
1485.172310	140401.118058	36.251175
1486.475038	140669.469405	36.256192
1487.808544	140917.362436	36.261210
1489.511965	141169.571266	36.266228
1490.728544	141434.026757	36.271245
1492.017977	141702.693503	36.276263
1493.822699	141958.428883	36.281280
1494.908867	142229.375916	36.286298
1497.012756	142500.176303	36.291316
1498.159712	142762.512303	36.296333
1500.103677	143021.010167	36.301351
1501.494085	143291.905525	36.306368
1503.084537	143546.813569	36.311386
1504.778462	143801.910068	36.316404
1506.109164	144076.168002	36.321421
1508.418050	144327.495273	36.326439
1510.436522	144574.244167	36.331456
1512.048622	144828.918433	36.336474
1513.887275	145054.873725	36.341492
1515.607674	145298.113821	36.346509
1517.420311	145528.690636	36.351527
1519.017352	145772.068080	36.356544
1520.687748	145991.528718	36.361562
1522.690160	146209.974744	36.366580
1524.463279	146427.089677	36.371597
1526.274789	146638.394251	36.376615
1527.726171	146829.830176	36.381632
1529.204173	147015.216356	36.386650
1530.792453	147204.832731	36.391668
1532.149060	147399.177385	36.396685
1533.443520	147588.044091	36.401703
1534.900328	147788.206462	36.406720
1536.186368	147986.761901	36.411738
1537.654482	148181.055552	36.416756
1538.724225	148401.528277	36.421773
1539.887570	148606.648368	36.426791
1541.268871	148820.418990	36.431808
1542.885198	149040.035929	36.436826
1545.194589	149236.192606	36.441844
1547.107344	149448.425050	36.446861
1548.881336	149642.945121	36.451879
1550.583202	149852.095046	36.456896
1551.822534	150061.243731	36.461914
1553.493590	150257.330499	36.466932
1554.585985	150473.604692	36.471949
1555.937630	150683.969262	36.476967
1557.304057	150911.207213	36.481984
1558.402988	151126.977551	36.487002
1559.967236	151362.922377	36.492020
1560.756741	151605.216985	36.497037
1562.793411	151831.302502	36.502055
1564.092048	152084.118814	36.507072
1565.303127	152323.207446	36.512090
1567.298544	152558.952826	36.517108
1568.344619	152826.915126	36.522125
1570.257991	153071.780477	36.527143
1571.865287	153314.388686	36.532160
1572.928187	153573.745321	36.537178
1574.639362	153821.640509	36.542196
1575.730140	154096.744167	36.547213
1577.475844	154362.794446	36.552231
1579.244036	154621.603317	36.557248
1580.569684	154894.837637	36.562266
1582.312592	155169.592816	36.567284
1583.513431	155443.802338	36.572301
1585.181331	155711.384413	36.577319
1586.923462	155989.912211	36.582336
1588.567444	156258.909829	36.587354
1590.590022	156533.847091	36.592372
1591.886730	156820.592993	36.597389
1593.889590	157086.230527	36.602407
1595.767189	157364.101215	36.607424
1596.847506	157629.192036	36.612442
1599.087770	157886.111847	36.617460
1600.966917	158139.324756	36.622477
1603.092848	158395.087176	36.627495
1605.376593	158636.776006	36.632512
1607.381376	158872.411282	36.637530
1609.154906	159111.331216	36.642548
1610.523095	159351.788165	36.647565
1611.913067	159578.585643	36.652583
1613.453644	159797.853337	36.657600
1614.833330	160016.602646	36.662618
1616.687201	160219.971500	36.667636
1618.019820	160442.776282	36.672653
1619.483739	160662.999921	36.677671
1620.918808	160890.813132	36.682688
1622.430931	161123.447298	36.687706
1623.735365	161351.030549	36.692724
1625.276665	161586.884266	36.697741
1627.434001	161806.294596	36.702759
1629.190318	162048.673767	36.707776
1630.601215	162273.392466	36.712794
1632.518158	162493.758269	36.717812
1633.892910	162727.794278	36.722829
1635.281920	162966.433232	36.727847
1636.996240	163208.408298	36.732864
1638.782955	163443.588300	36.737882
1640.697747	163677.379746	36.742900
1641.905674	163914.341489	36.747917
1643.335087	164164.218718	36.752935
1644.846071	164410.850547	36.757952
1646.118726	164667.630206	36.762970
1647.543400	164921.026486	36.767988
1649.241856	165184.185085	36.773005
1650.585403	165460.808102	36.778023
1652.108808	165726.167165	36.783040
1653.410261	166003.650668	36.788058
1655.429877	166277.229786	36.793076
1656.709106	166557.270295	36.798093
1658.349255	166836.025240	36.803111
1660.456925	167116.597873	36.808128
1661.583386	167419.943817	36.813146
1663.841569	167691.402439	36.818164
1665.848949	167970.690858	36.823181
1667.734415	168243.950330	36.828199
1669.454132	168522.096151	36.833216
1671.165497	168796.097528	36.838234
1673.048760	169074.690694	36.843252
1674.437792	169353.275572	36.848269
1676.368094	169624.279874	36.853287
1678.444469	169892.256592	36.858304
1679.810777	170169.201922	36.863322
1681.703307	170447.055067	36.868340
1683.400537	170715.300613	36.873357
1685.193473	170984.496860	36.878375
1687.278721	171241.128279	36.883392
1688.878556	171511.132590	36.888410
1691.070846	171766.570700	36.893428
1692.732700	172027.498682	36.898445
1694.683044	172289.777965	36.903463
1696.326185	172538.597632	36.908480
1698.014419	172806.440164	36.913498
1699.577435	173058.231547	36.918516
1701.343745	173314.495689	36.923533
1703.018458	173561.769026	36.928551
1704.376917	173807.381497	36.933568
1705.820253	174043.543565	36.938586
1707.474607	174278.722039	36.943604
1709.103756	174530.918061	36.948621
1710.369667	174780.889799	36.953639
1712.412018	175028.316674	36.958656
1713.597025	175282.414703	36.963674
1715.046866	175535.711058	36.968692
1716.660816	175801.111286	36.973709
1718.245051	176070.400061	36.978727
1720.079917	176329.869304	36.983744
1721.331376	176616.265465	36.988762
1723.190502	176889.575693	36.993780
1724.588476	177177.348004	36.998797
1726.163369	177451.595133	37.003815
1728.464083	177731.526835	37.008832
1729.936490	178025.141926	37.013850
1731.597734	178313.387698	37.018868
1733.288224	178611.006803	37.023885
1735.066571	178893.452452	37.028903
1737.207976	179184.190768	37.033920
1738.520493	179476.927774	37.038938
1740.338272	179771.489715	37.043956
1742.009309	180073.816575	37.048973
1743.429026	180375.779446	37.053991
1745.642731	180683.848177	37.059008
1747.191158	180981.151000	37.064026
1748.892301	181291.043697	37.069044
1750.870286	181595.793930	37.074061
1752.476945	181899.184141	37.079079
1754.217548	182203.062716	37.084096
1756.356402	182510.661342	37.089114
1758.371935	182819.855082	37.094132
1760.160063	183125.483476	37.099149
1762.164645	183423.910403	37.104167
1764.522000	183707.031229	37.109184
1765.901238	184007.096694	37.114202
1767.896530	184312.256177	37.119220
1769.844738	184603.314840	37.124237
1771.797861	184901.328303	37.129255
1773.897245	185199.307807	37.134272
1775.493609	185498.803030	37.139290
1777.630267	185785.334586	37.144308
1778.937194	186077.253155	37.149325
1780.418456	186370.897066	37.154343
1782.084497	186661.683691	37.159360
1783.967302	186959.201394	37.164378
1785.567164	187261.093179	37.169396
1787.356757	187556.383381	37.174413
1789.178121	187865.362975	37.179431
1790.847670	188167.249531	37.184448
1792.265248	188488.962087	37.189466
1794.236249	188783.533214	37.194484
1796.085671	189093.227032	37.199501
1797.876515	189391.231546	37.204519
1799.554639	189675.943426	37.209536
1801.280433	189960.865166	37.214554
1803.099631	190246.611346	37.219572
1805.020769	190525.248890	37.224589
1806.913178	190823.741076	37.229607
1808.766246	191100.742916	37.234624
1810.373154	191388.725043	37.239642
1812.358548	191669.427555	37.244660
1814.889228	191948.572928	37.249677
1816.031823	192246.672481	37.254695
1817.582185	192525.596010	37.259712
1819.686789	192810.004619	37.264730
1821.180179	193107.279464	37.269748
1823.264697	193395.996992	37.274765
1825.336033	193686.012814	37.279783
1827.417266	193968.578736	37.284800
1829.040136	194278.328523	37.289818
1830.972049	194558.116563	37.294836
1832.802707	194855.893899	37.299853
1834.413015	195158.568963	37.304871
1836.358496	195446.647548	37.309888
1838.100206	195745.091452	37.314906
1839.881501	196049.775336	37.319924
1841.916642	196362.594509	37.324941
1843.852668	196660.187825	37.329959
1845.790757	196954.076329	37.334976
1847.660404	197254.310876	37.339994
1849.791143	197541.115070	37.345012
1852.066901	197841.770802	37.350029
1853.806189	198143.604965	37.355047
1855.587147	198436.663538	37.360064
1857.621043	198745.524185	37.365082
1859.274111	199045.739742	37.370100
1861.121933	199341.267739	37.375117
1862.542599	199638.375621	37.380135
1864.569638	199935.325403	37.385152
1866.505271	200245.301794	37.390170
1868.463109	200555.403342	37.395188
1870.344351	200868.577878	37.400205
1871.783269	201171.923568	37.405223
1873.493821	201471.521309	37.410240
1875.419203	201796.625899	37.415258
1877.411762	202111.795326	37.420276
1879.372354	202421.741805	37.425293
1881.059723	202749.136449	37.430311
1883.642647	203043.056917	37.435328
1885.873826	203355.377361	37.440346
1887.250267	203659.990331	37.445364
1889.570458	203963.706165	37.450381
1890.923092	204281.972243	37.455399
1892.666650	204601.929803	37.460416
1894.802105	204910.884510	37.465434
1896.491664	205220.305143	37.470452
1898.295069	205544.650567	37.475469
1899.719448	205863.675500	37.480487
1901.907898	206163.107549	37.485504
1903.343528	206460.781799	37.490522
1904.953141	206764.091702	37.495540
1906.939726	207069.691811	37.500557
1908.663523	207385.592512	37.505575
1910.304465	207703.386835	37.510592
1912.420607	208021.462843	37.515610
1914.273898	208338.680880	37.520628
1916.356601	208648.805724	37.525645
1917.830941	208978.680621	37.530663
1920.074345	209292.172752	37.535680
1921.865607	209626.088597	37.540698
1923.583347	209955.244468	37.545716
1925.588565	210281.182597	37.550733
1926.962602	210617.645484	37.555751
1928.931980	210957.989330	37.560768
1931.203425	211307.402421	37.565786
1932.991473	211646.445656	37.570804
1934.780447	212005.993996	37.575821
1936.819893	212364.704732	37.580839
1938.808560	212711.059782	37.585856
1940.582704	213066.972591	37.590874
1942.269920	213431.547030	37.595892
1944.019440	213782.985906	37.600909
1946.168534	214161.380431	37.605927
1948.297279	214521.929535	37.610944
1950.174756	214900.828352	37.615962
1952.340859	215269.869239	37.620980
1954.474447	215626.995399	37.625997
1956.563494	215990.427884	37.631015
1959.087839	216340.512674	37.636032
1961.553573	216697.616999	37.641050
1963.515202	217054.320662	37.646068
1965.852011	217396.301934	37.651085
1967.721813	217750.382748	37.656103
1969.759480	218103.270561	37.661120
1972.142314	218440.069207	37.666138
1974.294687	218768.640304	37.671156
1977.015943	219098.417688	37.676173
1978.615239	219448.880272	37.681191
1980.750598	219824.653597	37.686208
1982.513282	220153.889453	37.691226
1984.549587	220487.971750	37.696244
1986.656974	220818.158887	37.701261
1988.562895	221164.263753	37.706279
1990.378578	221488.379981	37.711296
1992.058896	221829.495492	37.716314
1993.780108	222184.319281	37.721332
1995.666274	222523.652920	37.726349
1997.322934	222882.604114	37.731367
1999.394077	223231.167983	37.736384
2001.280207	223588.194006	37.741402
2002.916629	223942.924855	37.746420
2005.046716	224301.096219	37.751437
2006.724921	224663.239109	37.756455
2008.388886	225015.113241	37.761472
2010.238897	225356.445432	37.766490
2012.387559	225705.426637	37.771508
2014.575320	226042.111357	37.776525
2016.088019	226405.164264	37.781543
2017.981897	226752.107738	37.786560
2019.764156	227108.797175	37.791578
2021.924585	227469.593120	37.796596
2024.707951	227806.901386	37.801613
2026.873211	228163.635973	37.806631
2029.283562	228504.206102	37.811648
2031.837999	228847.243579	37.816666
2034.002312	229190.598244	37.821684
2036.524349	229517.846455	37.826701
2038.511877	229852.190296	37.831719
2040.989856	230181.301881	37.836736
2043.145254	230510.897582	37.841754
2044.978063	230851.593558	37.846772
2047.489620	231170.671305	37.851789
2049.583488	231501.118380	37.856807
2051.126979	231830.714210	37.861824
2053.327996	232164.626080	37.866842
2055.210993	232494.551288	37.871860
2057.521718	232819.939697	37.876877
2059.235749	233170.212433	37.881895
2061.067097	233510.994260	37.886912
2063.717402	233849.234479	37.891930
2065.072586	234192.380019	37.896948
2067.015623	234535.433454	37.901965
2068.915872	234895.207084	37.906983
2071.111683	235238.121169	37.912000
2073.210560	235598.500694	37.917018
2075.429529	235948.347290	37.922036
2077.693590	236301.235757	37.927053
2079.356909	236661.865792	37.932071
2081.376347	237022.110344	37.937088
2083.412482	237384.004383	37.942106
2085.069766	237765.161544	37.947124
2087.210716	238120.335961	37.952141
2089.576042	238505.904398	37.957159
2091.437133	238874.892069	37.962176
2093.480410	239248.119153	37.967194
2095.123593	239636.472908	37.972212
2097.429549	240010.270350	37.977229
2099.464050	240404.457295	37.982247
2101.282924	240785.725790	37.987264
2103.604636	241166.483913	37.992282
2105.483885	241567.100061	37.997300
2108.192192	241950.288482	38.002317
2110.279136	242330.985822	38.007335
2112.675686	242709.349161	38.012352
2115.525807	243077.481515	38.017370
2117.648980	243448.524278	38.022388
2120.162715	243809.091923	38.027405
2122.033205	244173.953679	38.032423
2124.722238	244499.925195	38.037440
2127.404147	244830.521551	38.042458
2129.269231	245166.201421	38.047476
2131.288696	245470.741608	38.052493
2133.608962	245799.492572	38.057511
2135.244521	246126.422437	38.062528
2137.060010	246457.337859	38.067546
2138.968757	246796.545381	38.072564
2141.380759	247120.433191	38.077581
2143.389237	247455.689229	38.082599
2145.266655	247803.718211	38.087616
2147.703244	248146.858446	38.092634
2149.383598	248501.956416	38.097652
2151.234562	248849.534715	38.102669
2153.018917	249209.215424	38.107687
2155.455066	249567.650478	38.112704
2157.458914	249937.814202	38.117722
2159.332838	250321.513015	38.122740
2161.270355	250688.386705	38.127757
2163.314383	251079.807752	38.132775
2165.261814	251458.671114	38.137792
2167.243945	251853.228116	38.142810
2169.116775	252250.089486	38.147828
2171.298599	252647.613955	38.152845
2173.447468	253060.080872	38.157863
2175.648427	253464.411761	38.162880
2178.011029	253876.135267	38.167898
2179.944890	254290.950486	38.172916
2181.997496	254696.780739	38.177933
2184.220093	255129.282603	38.182951
2186.204230	255560.095816	38.187968
2188.826075	255976.837444	38.192986
2191.015873	256409.778913	38.198004
2193.016737	256829.821323	38.203021
2195.103451	257261.942469	38.208039
2197.430309	257697.735086	38.213056
2199.554388	258126.574929	38.218074
2201.580952	258562.365892	38.223092
2204.282440	258992.919211	38.228109
2206.816616	259427.894437	38.233127
2208.768903	259854.960776	38.238144
2211.335146	260287.823844	38.243162
2213.420515	260726.860506	38.248180
2215.826858	261154.212395	38.253197
2218.561654	261579.861601	38.258215
2220.770423	262003.054507	38.263232
2223.735960	262411.114787	38.268250
2226.229856	262830.097437	38.273268
2228.701162	263225.154516	38.278285
2231.561090	263630.082989	38.283303
2233.705968	264029.587422	38.288320
2236.248019	264426.641384	38.293338
2238.487291	264807.866792	38.298356
2240.781955	265198.533732	38.303373
2243.043149	265569.214027	38.308391
2245.545245	265926.900790	38.313408
2248.160471	266277.329965	38.318426
2250.241756	266629.596881	38.323444
2252.083906	266971.613641	38.328461
2254.575668	267316.423574	38.333479
2256.275499	267674.391178	38.338496
2258.660935	268017.592574	38.343514
2260.541298	268373.931547	38.348532
2262.676086	268737.521115	38.353549
2265.058296	269092.688535	38.358567
2267.417533	269447.656538	38.363584
2269.270929	269805.600888	38.368602
2271.178026	270195.595911	38.373620
2273.077627	270567.555886	38.378637
2275.603399	270945.411899	38.383655
2277.782814	271335.745213	38.388672
2280.065245	271721.642117	38.393690
2282.479888	272115.875875	38.398708
2284.771118	272498.596144	38.403725
2286.923844	272888.273576	38.408743
2288.787241	273287.904273	38.413760
2291.269966	273682.610165	38.418778
2293.279249	274113.768847	38.423796
2295.428097	274521.458061	38.428813
2297.857835	274934.005592	38.433831
2299.647761	275360.016747	38.438848
2302.296948	275769.735048	38.443866
2304.372016	276203.626755	38.448884
2306.779507	276623.214364	38.453901
2308.406229	277059.260056	38.458919
2310.810790	277492.184697	38.463936
2313.008754	277931.823042	38.468954
2315.309376	278380.767980	38.473972
2317.674562	278831.582335	38.478989
2320.302004	279273.590738	38.484007
2322.011684	279740.258630	38.489024
2324.583146	280183.266139	38.494042
2327.142931	280634.023228	38.499060
2329.453124	281092.694596	38.504077
2332.190944	281525.767549	38.509095
2334.697969	281990.910251	38.514112
2337.205828	282432.935495	38.519130
2339.486937	282887.088226	38.524148
2342.078248	283324.399855	38.529165
2344.718523	283782.864124	38.534183
2346.972682	284237.959706	38.539200
2349.283222	284680.395114	38.544218
2351.843947	285121.748842	38.549236
2353.796956	285569.549162	38.554253
2356.584475	286010.256215	38.559271
2358.848282	286464.864956	38.564288
2361.419186	286910.533378	38.569306
2364.032876	287354.136776	38.574324
2366.221569	287794.275930	38.579341
2368.677447	288226.421010	38.584359
2370.892412	288652.583190	38.589376
2373.103498	289049.583000	38.594394
2375.414731	289462.900313	38.599412
2377.439052	289880.352309	38.604429
2379.629798	290308.979824	38.609447
2381.687433	290741.260294	38.614464
2384.026334	291157.415622	38.619482
2386.126794	291600.153649	38.624500
2388.255242	292047.560464	38.629517
2390.755403	292486.016652	38.634535
2393.140409	292928.503816	38.639552
2395.568684	293382.617485	38.644570
2397.498872	293837.266393	38.649588
2399.577008	294298.520835	38.654605
2402.081589	294773.271379	38.659623
2404.105352	295243.677058	38.664640
2406.911831	295714.465577	38.669658
2409.268555	296199.041279	38.674676
2411.698067	296681.876864	38.679693
2414.358521	297157.231843	38.684711
2416.429101	297646.065780	38.689728
2418.899207	298139.102509	38.694746
2421.487206	298632.931990	38.699764
2423.541586	299126.438183	38.704781
2426.145967	299623.818348	38.709799
2428.591312	300128.969609	38.714816
2431.184861	300618.473987	38.719834
2433.402279	301127.976384	38.724852
2435.795723	301632.978587	38.729869
2438.581880	302137.561232	38.734887
2440.876256	302655.479383	38.739904
2443.590201	303160.527153	38.744922
2445.767835	303668.579219	38.749940
2449.358884	304161.317423	38.754957
2452.751379	304654.618743	38.759975
2455.332312	305142.077776	38.764992
2458.901570	305603.012781	38.770010
2462.446447	306050.233868	38.775028
2465.340666	306487.980649	38.780045
2468.111369	306915.382250	38.785063
2470.609493	307365.076031	38.790080
2473.328146	307794.362475	38.795098
2475.774819	308219.296341	38.800116
2478.214799	308644.407572	38.805133
2480.956208	309055.779091	38.810151
2483.069084	309488.584439	38.815168
2485.770308	309901.407134	38.820186
2488.194118	310321.206349	38.825204
2490.536931	310742.718605	38.830221
2492.967400	311160.100716	38.835239
2494.982530	311586.360574	38.840256
2497.233701	312012.657569	38.845274
2500.001511	312449.919542	38.850292
2501.858076	312880.695055	38.855309
2504.360478	313310.528314	38.860327
2505.843299	313732.317639	38.865344
2508.313838	314144.043311	38.870362
2510.231087	314567.157300	38.875380
2512.034816	315001.056393	38.880397
2514.090077	315442.304624	38.885415
2516.244444	315897.224748	38.890432
2518.377147	316358.673473	38.895450
2520.579893	316821.988349	38.900468
2522.615774	317312.909330	38.905485
2525.271698	317790.675179	38.910503
2527.588294	318288.149983	38.915520
2529.652803	318794.246355	38.920538
2532.023622	319300.697759	38.925556
2534.405418	319816.947846	38.930573
2537.343767	320336.636939	38.935591
2539.299554	320867.145305	38.940608
2541.708257	321399.965974	38.945626
2544.474311	321927.418905	38.950644
2546.877274	322477.884323	38.955661
2549.526933	323021.196186	38.960679
2552.129899	323573.832225	38.965696
2554.619658	324114.800490	38.970714
2557.743691	324669.632247	38.975732
2560.171854	325226.271964	38.980749
2562.788722	325774.522900	38.985767
2565.857510	326321.733438	38.990784
2568.389527	326881.976590	38.995802
2571.096277	327433.680808	39.000820
2573.806106	327978.930384	39.005837
2576.492704	328527.455603	39.010855
2579.351378	329092.836655	39.015872
2582.338467	329638.284243	39.020890
2585.458926	330187.693491	39.025908
2588.424099	330725.137462	39.030925
2591.445159	331251.471693	39.035943
2594.044542	331783.937844	39.040960
2596.690510	332303.670741	39.045978
2599.855924	332837.639046	39.050996
2602.352579	333353.985185	39.056013
2605.527763	333862.069007	39.061031
2608.126744	334381.793818	39.066048
2611.202069	334890.698363	39.071066
2614.234703	335387.163828	39.076084
2616.793959	335901.423980	39.081101
2620.118666	336386.358702	39.086119
2622.664840	336876.669183	39.091136
2625.045672	337362.609521	39.096154
2627.632107	337851.738285	39.101172
2629.945067	338345.832449	39.106189
2633.196100	338823.600427	39.111207
2635.283419	339315.564606	39.116224
2637.730257	339807.391810	39.121242
2640.515631	340302.639923	39.126260
2642.918933	340804.063518	39.131277
2645.242987	341281.172437	39.136295
2647.891636	341748.298986	39.141312
2650.265488	342214.170620	39.146330
2652.913428	342678.141836	39.151348
2654.955431	343152.614808	39.156365
2657.774064	343620.055285	39.161383
2659.854397	344105.050774	39.166400
2662.219858	344590.276346	39.171418
2664.949590	345073.942278	39.176436
2667.223340	345575.777789	39.181453
2669.559063	346086.180041	39.186471
2672.021440	346604.529232	39.191488
2674.260967	347116.333743	39.196506
2677.106107	347641.670328	39.201524
2679.596601	348182.366184	39.206541
2682.527842	348711.258495	39.211559
2684.684795	349249.838874	39.216576
2687.031352	349803.412250	39.221594
2689.625622	350353.691383	39.226612
2691.928184	350923.811541	39.231629
2694.341829	351501.625021	39.236647
2696.893357	352094.920365	39.241664
2699.406214	352677.147550	39.246682
2701.865923	353269.606425	39.251700
2704.305737	353876.581178	39.256717
2707.037270	354485.279388	39.261735
2710.013780	355111.877408	39.266752
2712.703249	355712.241880	39.271770
2716.139519	356320.527146	39.276788
2718.728735	356936.629950	39.281805
2721.549245	357556.825687	39.286823
2724.529128	358176.353797	39.291840
2727.625977	358787.835015	39.296858
2730.186039	359410.789549	39.301876
2732.841736	360022.172668	39.306893
2735.899261	360638.255788	39.311911
2738.901232	361258.806546	39.316928
2741.220044	361885.624537	39.321946
2744.105369	362510.263275	39.326964
2747.365749	363120.520467	39.331981
2750.737891	363737.578690	39.336999
2753.882741	364348.396137	39.342016
2756.896938	364951.739558	39.347034
2759.935863	365552.304819	39.352052
2762.543158	366160.721174	39.357069
2765.420823	366755.002211	39.362087
2767.902599	367355.123787	39.367104
2770.357223	367961.890008	39.372122
2773.296861	368550.579503	39.377140
2775.893579	369167.304450	39.382157
2778.799026	369774.684369	39.387175
2781.443905	370373.951619	39.392192
2783.946941	370997.084798	39.397210
2786.818679	371617.486112	39.402228
2789.716465	372233.738214	39.407245
2792.703286	372829.008780	39.412263
2795.462691	373414.944192	39.417280
2797.996815	373984.516263	39.422298
2800.610689	374563.506232	39.427316
2803.040007	375153.071863	39.432333
2805.428533	375734.719460	39.437351
2807.800877	376330.898837	39.442368
2810.615922	376929.916850	39.447386
2813.714752	377532.990884	39.452404
2815.663405	378149.404821	39.457421
2818.327559	378771.048754	39.462439
2821.047415	379394.551275	39.467456
2823.771565	380022.964621	39.472474
2826.789085	380656.673978	39.477492
2829.462292	381302.096587	39.482509
2831.908093	381953.150465	39.487527
2834.804888	382606.556967	39.492544
2837.547169	383271.518359	39.497562
2840.389464	383930.973018	39.502580
2842.961745	384608.392223	39.507597
2845.652317	385278.399016	39.512615
2848.831484	385958.665015	39.517632
2851.111521	386650.144847	39.522650
2854.092531	387335.210308	39.527668
2856.584161	388037.790132	39.532685
2859.699662	388737.594313	39.537703
2862.618979	389448.524450	39.542720
2865.471092	390161.987109	39.547738
2868.555359	390866.065612	39.552756
2871.251656	391583.049216	39.557773
2873.951261	392307.701617	39.562791
2877.460687	393032.996740	39.567808
2880.007147	393756.476327	39.572826
2883.149269	394476.676440	39.577844
2886.027538	395212.320673	39.582861
2888.925092	395942.138930	39.587879
2891.857608	396674.471425	39.592896
2894.925766	397407.172025	39.597914
2898.019522	398128.898649	39.602932
2901.084520	398859.082615	39.607949
2904.281627	399581.166578	39.612967
2907.887688	400299.239867	39.617984
2910.868066	401018.942802	39.623002
2913.976723	401733.209124	39.628020
2916.873707	402442.929549	39.633037
2920.292054	403155.847314	39.638055
2923.541202	403865.961778	39.643072
2926.518318	404566.039029	39.648090
2930.233160	405248.086629	39.653108
2933.478526	405946.087736	39.658125
2936.322318	406627.609108	39.663143
2939.495653	407300.292650	39.668160
2942.095433	407987.906031	39.673178
2945.276827	408655.539530	39.678196
2948.756536	409325.823183	39.683213
2951.487367	409982.016595	39.688231
2954.810505	410611.539654	39.693248
2957.468528	411239.127095	39.698266
2960.540751	411851.809126	39.703284
2962.905935	412481.317446	39.708301
2965.446459	413105.259660	39.713319
2968.270626	413737.734953	39.718336
2970.751502	414366.601553	39.723354
2973.564786	415005.057162	39.728372
2976.518990	415659.922852	39.733389
2979.458274	416304.132890	39.738407
2982.153825	416962.608160	39.743424
2984.593752	417640.746807	39.748442
2987.494035	418305.316065	39.753460
2990.428505	418989.982889	39.758477
2992.991075	419682.825280	39.763495
2996.104590	420369.102348	39.768512
2998.608051	421070.458201	39.773530
3001.843063	421771.883191	39.778548
3004.803378	422487.217443	39.783565
3007.259988	423207.578301	39.788583
3010.237268	423925.760364	39.793600
3013.434099	424660.329866	39.798618
3016.723457	425390.254247	39.803636
3019.714019	426123.321893	39.808653
3022.285647	426872.723592	39.813671
3025.744404	427609.653270	39.818688
3028.251696	428370.446841	39.823706
3031.221158	429127.751244	39.828724
3034.101278	429896.445564	39.833741
3036.832838	430657.263937	39.838759
3039.897418	431430.797255	39.843776
3042.986665	432218.739235	39.848794
3046.214785	433005.546104	39.853812
3048.859973	433796.878083	39.858829
3052.247354	434586.447300	39.863847
3055.658149	435372.189780	39.868864
3058.864388	436135.352968	39.873882
3063.109582	436921.041582	39.878900
3066.801177	437692.613654	39.883917
3069.813680	438463.712170	39.888935
3073.470093	439224.633179	39.893952
3076.265320	439985.565637	39.898970
3079.696582	440744.500326	39.903988
3082.928670	441504.151746	39.909005
3085.849272	442260.740151	39.914023
3089.038529	443016.857297	39.919040
3091.623597	443779.172246	39.924058
3094.577695	444543.328318	39.929076
3097.440726	445316.384240	39.934093
3100.288206	446089.164295	39.939111
3103.747316	446870.630398	39.944128
3106.403252	447656.550875	39.949146
3109.259696	448428.695713	39.954164
3112.582016	449210.459566	39.959181
3115.521861	449981.274165	39.964199
3118.906995	450738.731940	39.969216
3122.012505	451471.206944	39.974234
3125.027692	452203.875210	39.979252
3127.893121	452927.181083	39.984269
3131.219388	453677.920920	39.989287
3134.242570	454416.487980	39.994304
3136.777076	455172.515575	39.999322
3140.028048	455921.724902	40.004340
3142.991194	456680.366132	40.009357
3145.653160	457457.294947	40.014375
3148.893569	458226.667306	40.019392
3151.739812	459007.054109	40.024410
3154.733201	459795.990578	40.029428
3157.457146	460598.600636	40.034445
3160.318521	461399.894582	40.039463
3163.965975	462203.867353	40.044480
3166.742060	463025.551538	40.049498
3169.845196	463838.603957	40.054516
3172.740216	464675.785520	40.059533
3175.408873	465521.214302	40.064551
3178.640433	466362.018893	40.069568
3181.814464	467223.281892	40.074586
3185.329905	468076.313258	40.079604
3188.737078	468940.300750	40.084621
3191.616048	469813.893347	40.089639
3195.258149	470675.394614	40.094656
3198.355985	471556.312099	40.099674
3201.760069	472414.845313	40.104692
3204.926243	473295.929848	40.109709
3208.118474	474179.297701	40.114727
3211.412995	475061.094105	40.119744
3214.946361	475932.804503	40.124762
3218.207054	476814.428155	40.129780
3221.784706	477685.903447	40.134797
3225.108504	478566.832903	40.139815
3229.142275	479438.310610	40.144832
3232.318752	480311.249972	40.149850
3235.948363	481178.468834	40.154868
3239.106606	482053.456002	40.159885
3242.199253	482925.129337	40.164903
3245.452023	483801.639805	40.169920
3248.705474	484662.748870	40.174938
3252.140101	485532.784740	40.179956
3255.866826	486404.604262	40.184973
3258.917879	487273.105575	40.189991
3262.058881	488129.124489	40.195008
3265.376852	489004.880207	40.200026
3268.848708	489881.732655	40.205044
3271.971816	490743.192165	40.210061
3274.932348	491613.830816	40.215079
3278.588427	492484.621675	40.220096
3282.046372	493351.917803	40.225114
3285.382215	494219.141861	40.230132
3288.529612	495092.768552	40.235149
3291.842514	495941.077028	40.240167
3295.357483	496765.175841	40.245184
3298.384811	497586.032040	40.250202
3301.489610	498409.868264	40.255220
3304.954173	499227.146952	40.260237
3307.642023	500049.257135	40.265255
3310.663262	500880.465289	40.270272
3313.663582	501714.767907	40.275290
3316.825812	502557.638012	40.280308
3320.047469	503409.393303	40.285325
3322.735786	504275.224239	40.290343
3325.996807	505138.297120	40.295360
3328.842083	506022.843579	40.300378
3331.929163	506914.877151	40.305396
3335.120266	507808.210880	40.310413
3337.936511	508716.898634	40.315431
3341.168910	509642.629318	40.320448
3344.332985	510564.687658	40.325466
3347.514977	511495.724814	40.330484
3350.664976	512436.856958	40.335501
3353.785270	513401.350206	40.340519
3356.970789	514352.712000	40.345536
3360.866556	515317.981419	40.350554
3364.030192	516303.436829	40.355572
3367.682814	517256.677644	40.360589
3371.375836	518230.031326	40.365607
3375.149242	519195.447311	40.370624
3378.546476	520178.717994	40.375642
3382.090855	521164.982246	40.380660
3385.304137	522133.288334	40.385677
3388.685629	523127.930230	40.390695
3392.754611	524110.604495	40.395712
3396.090835	525081.638429	40.400730
3399.129332	526076.303326	40.405748
3402.768862	527053.924488	40.410765
3406.259952	528045.017409	40.415783
3409.634362	529033.344970	40.420800
3413.227157	530039.013846	40.425818
3416.900891	531028.982929	40.430836
3420.526178	532014.512825	40.435853
3423.578248	533025.013380	40.440871
3427.372256	534008.576044	40.445888
3430.869331	535008.497227	40.450906
3433.962020	536006.855556	40.455924
3437.762011	537008.412161	40.460941
3441.072301	538006.555084	40.465959
3444.732332	539001.907582	40.470976
3448.066788	540003.239604	40.475994
3451.406305	541015.382592	40.481012
3455.171741	542009.512570	40.486029
3458.476049	543028.877540	40.491047
3461.844345	544022.533375	40.496064
3465.311014	545037.606079	40.501082
3468.474216	546053.512920	40.506100
3471.794455	547083.470905	40.511117
3475.163592	548083.515206	40.516122
3478.707030	549035.036856	40.521127
3482.292436	549945.313833	40.526132
3485.726269	550785.371103	40.531136
3488.668352	551566.828698	40.536141
3491.504374	552284.135723	40.541146
3494.581939	552927.711631	40.546151
3497.227226	553514.068425	40.551156
3499.412095	554041.754583	40.556160
3501.669888	554509.078038	40.561165
3503.885597	554923.932004	40.566170
3506.115049	555276.829140	40.571175
3508.141503	555558.678495	40.576180
3509.532402	555803.751066	40.581184
3511.367614	555997.704619	40.586189
3513.083907	556148.145659	40.591194
3514.613331	556241.720113	40.596199
3515.508067	556322.179457	40.601204
3516.121663	556358.650394	40.606208
3517.439551	556343.058726	40.611213
3518.100813	556333.623407	40.616218
3518.986115	556275.025770	40.621223
3519.397301	556181.498401	40.626228
3519.856254	556086.903646	40.631232
3520.561924	555945.864952	40.636237
3520.654544	555818.137042	40.641242
3521.395926	555647.077904	40.646247
3521.798133	555464.166184	40.651252
3521.715428	555290.559622	40.656256
3522.379438	555071.939030	40.661261
3522.607281	554863.876253	40.666266
3522.823719	554628.723721	40.671271
3522.693884	554395.639846	40.676276
3522.867856	554141.165529	40.681280
3522.995348	553893.100776	40.686285
3523.015404	553639.852590	40.691290
3522.981904	553373.945785	40.696295
3522.990519	553107.926491	40.701300
3522.766929	552844.814645	40.706304
3522.945724	552552.927486	40.711309
3522.836907	552279.444580	40.716314
3522.922885	551996.036808	40.721319
3522.811986	551718.103663	40.726324
3522.469036	551433.339897	40.731328
3522.761509	551127.984749	40.736333
3522.155148	550852.535163	40.741338
3521.911792	550570.261522	40.746343
3522.067033	550276.666917	40.751348
3521.893247	550001.485988	40.756352
3521.671072	549705.820146	40.761357
3521.305424	549442.466928	40.766362
3521.201855	549144.247799	40.771367
3520.892462	548865.382967	40.776372
3520.944676	548590.038686	40.781376
3520.931405	548309.652930	40.786381
3520.505098	548034.272868	40.791386
3520.335248	547762.329391	40.796391
3520.225958	547497.184621	40.801396
3519.713700	547223.064608	40.806400
3519.482800	546961.866041	40.811405
3519.296602	546712.163339	40.816410
3519.215780	546434.629273	40.821415
3518.949791	546195.226843	40.826420
3518.541702	545938.530251	40.831424
3518.425905	545681.984890	40.836429
3518.059364	545455.508019	40.841434
3518.089919	545196.508235	40.846439
3518.218419	544957.376707	40.851444
3517.805905	544711.512209	40.856448
3517.809356	544482.488502	40.861453
3517.148325	544253.818685	40.866458
3517.305943	544014.616860	40.871463
3517.083368	543785.820050	40.876468
3516.642620	543563.415004	40.881472
3516.717925	543338.653317	40.886477
3516.362945	543128.899528	40.891482
3516.286871	542899.005762	40.896487
3515.936915	542700.654715	40.901492
3515.946211	542479.575950	40.906496
3515.861540	542269.363461	40.911501
3515.477046	542067.576354	40.916506
3515.353702	541860.191533	40.921511
3515.080046	541658.734813	40.926516
3514.667093	541469.970304	40.931520
3514.866418	541265.808083	40.936525
3514.861183	541085.759609	40.941530
3514.325480	540886.202097	40.946535
3514.372383	540700.990629	40.951540
3514.122858	540516.530634	40.956544
3513.950944	540341.548877	40.961549
3513.726503	540171.370320	40.966554
3513.492882	539981.195433	40.971559
3513.670438	539812.868086	40.976564
3513.227342	539650.141000	40.981568
3513.311050	539464.302572	40.986573
3513.172314	539300.210704	40.991578
3513.101272	539139.388691	40.996583
3512.881686	538978.335957	41.001588
3512.251405	538824.820204	41.006592
3512.786882	538661.422822	41.011597
3512.039105	538512.921884	41.016602
3512.173608	538369.582538	41.021607
3511.851344	538208.840859	41.026612
3511.584203	538078.338881	41.031616
3512.140739	537920.737813	41.036621
3511.694165	537792.130294	41.041626
3511.590417	537651.397432	41.046631
3511.420857	537511.835238	41.051636
3511.142871	537371.783870	41.056640
3511.240860	537224.197225	41.061645
3510.945642	537110.256623	41.066650
3511.056431	536975.594616	41.071655
3510.598392	536847.890020	41.076660
3510.438834	536736.904986	41.081664
3510.523672	536601.637719	41.086669
3510.341050	536487.573662	41.091674
3510.454381	536357.299847	41.096679
3510.213905	536248.192802	41.101684
3509.946620	536140.099365	41.106688
3510.186675	536024.096270	41.111693
3509.760506	535920.673112	41.116698
3509.612269	535804.578206	41.121703
3509.776889	535688.483479	41.126708
3509.675650	535598.139088	41.131712
3509.690616	535487.622505	41.136717
3509.221289	535389.708126	41.141722
3509.312120	535279.582133	41.146727
3509.388254	535183.802674	41.151732
3509.068966	535082.579437	41.156736
3509.045578	534972.822877	41.161741
3508.734671	534890.589261	41.166746
3508.827090	534792.632798	41.171751
3508.924365	534706.646318	41.176756
3508.717509	534628.991459	41.181760
3508.667238	534523.529496	41.186765
3508.482522	534440.212762	41.191770
3508.630492	534355.681187	41.196775
3508.291750	534268.094242	41.201780
3508.049318	534187.310941	41.206784
3508.035817	534092.044001	41.211789
3507.965813	534028.205347	41.216794
3507.991584	533944.094948	41.221799
3508.066868	533882.556399	41.226804
3507.687350	533796.236091	41.231808
3508.186329	533729.932060	41.236813
3507.651871	533648.333339	41.241818
3507.970754	533569.731285	41.246823
3507.790377	533504.240891	41.251828
3507.691939	533415.045128	41.256832
3507.645744	533353.473159	41.261837
3507.508071	533285.701846	41.266842
3507.338665	533227.988127	41.271847
3507.654762	533159.942471	41.276852
3507.343047	533099.219736	41.281856
3507.510179	533025.892715	41.286861
3507.223423	532969.813145	41.291866
3507.395017	532890.675234	41.296871
3507.027135	532826.019899	41.301876
3507.225835	532765.063622	41.306880
3507.302010	532697.104379	41.311885
3507.009211	532642.893773	41.316890
3507.078461	532578.774539	41.321895
3507.058379	532513.759814	41.326900
3506.969427	532458.354400	41.331904
3506.855787	532402.649573	41.336909
3506.707985	532341.039127	41.341914
3506.886518	532295.745335	41.346919
3506.812955	532242.054397	41.351924
3506.559378	532184.501661	41.356928
3506.727827	532115.514884	41.361933
3506.749256	532060.797894	41.366938
3506.516871	532014.860947	41.371943
3506.560217	531970.345390	41.376948
3506.487662	531914.177630	41.381952
3506.468191	531870.732663	41.386957
3506.641338	531832.966056	41.391962
3506.594924	531768.558637	41.396967
3506.406673	531727.362903	41.401972
3506.336134	531674.477878	41.406976
3506.394107	531609.699649	41.411981
3506.153166	531578.313152	41.416986
3506.336436	531525.842205	41.421991
3506.238971	531481.751690	41.426996
3506.171926	531445.436745	41.432000
3506.258876	531383.330700	41.437005
3506.194815	531353.583048	41.442010
3506.225552	531296.487323	41.447015
3506.027104	531262.819929	41.452020
3505.808284	531216.929008	41.457024
3505.960719	531168.402565	41.462029
3505.920039	531141.884326	41.467034
3505.930863	531098.482944	41.472039
3505.927585	531060.287640	41.477044
3505.708197	531013.992021	41.482048
3505.656021	530986.515377	41.487053
3505.549555	530949.093976	41.492058
3505.653898	530912.599128	41.497063
3506.136365	530871.295116	41.502068
3505.802681	530834.364077	41.507072
3505.715406	530789.411077	41.512077
3506.087422	530770.658325	41.517082
3505.684257	530723.986697	41.522087
3505.685131	530678.867871	41.527092
3505.431911	530650.563486	41.532096
3505.559414	530612.245366	41.537101
3505.393511	530589.788018	41.542106
3505.466030	530545.112211	41.547111
3505.650784	530516.687831	41.552116
3505.355022	530486.621473	41.557120
3505.572397	530452.179245	41.562125
3505.266156	530442.425873	41.567130
3505.231062	530410.297127	41.572135
3505.244776	530379.625860	41.577140
3505.491213	530356.597739	41.582144
3505.594571	530320.960614	41.587149
3505.136143	530295.921712	41.592154
3505.070988	530262.130041	41.597159
3505.485739	530230.586668	41.602164
3505.159380	530213.611020	41.607168
3505.442716	530181.886214	41.612173
3505.255637	530157.612628	41.617178
3505.443616	530127.469118	41.622183
3505.622847	530105.512318	41.627188
3505.177132	530063.746570	41.632192
3505.408751	530039.406619	41.637197
3505.157401	530008.271251	41.642202
3505.395920	529975.694147	41.647207
3505.354495	529943.969667	41.652212
3504.861355	529931.921250	41.657216
3505.275952	529895.223410	41.662221
3505.184127	529864.769930	41.667226
3504.894503	529847.585967	41.672231
3505.001757	529818.717822	41.677236
3505.105983	529793.488123	41.682240
3505.248769	529754.508629	41.687245
3505.183507	529744.009336	41.692250
3504.807318	529723.958812	41.697255
3504.860536	529693.633658	41.702260
3504.963816	529679.974921	41.707264
3505.096909	529653.780395	41.712269
3504.806992	529636.090962	41.717274
3505.137115	529608.248302	41.722279
3504.957488	529597.716460	41.727284
3504.584427	529569.125893	41.732288
3505.070494	529542.319572	41.737293
3504.897668	529520.215488	41.742298
3505.080233	529493.204412	41.747303
3504.979749	529480.941994	41.752308
3505.438019	529461.719288	41.757312
3505.091128	529427.060829	41.762317
3505.362386	529404.128449	41.767322
3505.288396	529373.266962	41.772327
3505.232990	529343.716245	41.777332
3505.286265	529316.472655	41.782336
3505.543828	529285.457530	41.787341
3505.090226	529261.982633	41.792346
3504.797097	529240.604588	41.797351
3505.098729	529213.473152	41.802356
3504.997540	529192.772122	41.807360
3505.098532	529157.233794	41.812365
3505.044367	529144.812202	41.817370
3505.312923	529114.249775	41.822375
3505.341729	529087.009655	41.827380
3505.218821	529064.998102	41.832384
3505.185774	529050.046578	41.837389
3504.859996	529025.540513	41.842394
3505.146096	528991.842182	41.847399
3505.001167	528960.738447	41.852404
3504.464831	528959.964458	41.857408
3504.750757	528927.478754	41.862413
3504.886661	528920.787458	41.867418
3504.911186	528890.212638	41.872423
3505.063471	528879.931036	41.877428
3505.011337	528846.690106	41.882432
3505.028675	528827.637387	41.887437
3504.787747	528805.745189	41.892442
3504.794176	528790.231335	41.897447
3505.028882	528758.359755	41.902452
3504.658420	528743.259148	41.907456
3505.046145	528710.201061	41.912461
3505.257099	528708.298307	41.917466
3505.033660	528673.214422	41.922471
3504.827760	528644.191497	41.927476
3504.798839	528629.643176	41.932480
3504.919681	528601.730758	41.937485
3504.871241	528586.023249	41.942490
3504.954762	528564.281558	41.947495
3504.903784	528535.941394	41.952500
3504.659736	528521.629106	41.957504
3504.587856	528498.345392	41.962509
3504.642531	528487.674706	41.967514
3504.749700	528465.272222	41.972519
3504.937947	528442.957955	41.977524
3504.496187	528435.448180	41.982528
3504.824589	528413.061184	41.987533
3504.837028	528399.213568	41.992538
3504.644098	528383.174968	41.997543
3505.151979	528366.722382	42.002548
3504.588359	528335.683595	42.007552
3504.761918	528322.315771	42.012557
3504.712889	528309.084185	42.017562
3504.821980	528285.670487	42.022567
3505.069481	528271.482406	42.027572
3504.746228	528245.054476	42.032576
3504.835775	528229.072136	42.037581
3504.790635	528215.334526	42.042586
3504.871542	528187.730888	42.047591
3504.845794	528166.157521	42.052596
3504.681184	528143.645941	42.057600
3504.902800	528128.754357	42.062605
3504.904397	528118.344479	42.067610
3505.064089	528089.869149	42.072615
3504.803564	528065.351277	42.077620
3504.758890	528046.155817	42.082624
3504.866825	528014.353310	42.087629
3504.831168	528003.039637	42.092634
3504.892006	527979.228842	42.097639
3504.811608	527962.515087	42.102644
3504.636938	527925.147805	42.107648
3504.823626	527917.235240	42.112653
3505.057953	527896.075203	42.117658
3504.945268	527881.387831	42.122663
3504.818934	527848.409200	42.127668
3504.633651	527836.310510	42.132672
3504.643290	527811.496869	42.137677
3504.785159	527796.718648	42.142682
3504.531504	527780.486897	42.147687
3504.756444	527750.737281	42.152692
3504.437111	527745.936692	42.157696
3504.701498	527726.439319	42.162701
3504.666644	527718.662743	42.167706
3504.814960	527699.183683	42.172711
3504.703516	527681.665983	42.177716
3504.468920	527678.064814	42.182720
3504.821457	527647.941093	42.187725
3504.522358	527637.831103	42.192730
3504.364476	527631.741585	42.197735
3504.538920	527601.191111	42.202740
3504.511288	527594.828314	42.207744
3504.698164	527568.571295	42.212749
3504.807699	527557.790241	42.217754
3504.618729	527542.407120	42.222759
3504.832849	527519.228363	42.227764
3504.644840	527511.576965	42.232768
3504.482004	527492.399511	42.237773
3504.099090	527465.120606	42.242778
3504.353267	527459.824992	42.247783
3504.416431	527460.371156	42.252788
3504.491021	527436.001480	42.257792
3504.673140	527423.288509	42.262797
3504.541173	527416.588383	42.267802
3504.360744	527393.016987	42.272807
3504.665632	527379.324395	42.277812
3504.520046	527368.229788	42.282816
3504.352142	527349.760464	42.287821
3504.540857	527331.487429	42.292826
3504.562737	527323.297404	42.297831
3504.656723	527313.579897	42.302836
3504.288033	527299.286203	42.307840
3504.712561	527276.680267	42.312845
3504.424923	527258.078154	42.317850
3504.130206	527262.875395	42.322855
3504.431327	527244.432884	42.327860
3504.436357	527227.553241	42.332864
3504.590291	527214.137050	42.337869
3504.719744	527199.158090	42.342874
3504.490079	527180.799404	42.347879
3504.597060	527168.502397	42.352884
3504.437425	527151.446556	42.357888
3504.880641	527132.526626	42.362893
3504.686437	527126.341581	42.367898
3504.666205	527097.993984	42.372903
3504.777376	527081.249019	42.377908
3504.383981	527066.049358	42.382912
3504.520664	527048.036905	42.387917
3504.477824	527046.022460	42.392922
3504.328001	527036.596007	42.397927
3504.510351	527018.778450	42.402932
3504.286375	527020.633440	42.407936
3504.473470	526991.191605	42.412941
3504.438853	526972.599700	42.417946
3504.434454	526963.352364	42.422951
3504.581084	526957.517676	42.427956
3504.413016	526932.326452	42.432960
3504.295166	526923.248638	42.437965
3504.078604	526925.911062	42.442970
3504.230729	526899.708968	42.447975
3504.605493	526873.926476	42.452980
3504.279532	526882.973910	42.457984
3504.267570	526877.265334	42.462989
3504.441924	526843.681175	42.467994
3504.418754	526846.717344	42.472999
3504.650587	526829.649816	42.478004
3504.260308	526816.066623	42.483008
3504.321414	526808.324971	42.488013
3504.358840	526797.807487	42.493018
3504.475681	526784.194646	42.498023
3504.588666	526771.037243	42.503028
3504.423635	526757.721622	42.508032
3504.400108	526741.654582	42.513037
3504.559088	526729.146865	42.518042
3504.607379	526721.811499	42.523047
3504.952954	526707.303293	42.528052
3504.416363	526689.497933	42.533056
3504.780455	526672.914712	42.538061
3504.674019	526657.315533	42.543066
3504.377967	526642.908689	42.548071
3504.334021	526623.559778	42.553076
3504.253550	526603.155314	42.558080
3504.633368	526590.309352	42.563085
3504.456765	526567.595276	42.568090
3503.931515	526559.541878	42.573095
3504.588361	526534.725017	42.578100
3504.399041	526552.190962	42.583104
3504.387159	526536.222951	42.588109
3504.159204	526519.076152	42.593114
3504.516255	526508.406879	42.598119
3504.582722	526503.949237	42.603124
3504.317492	526479.278039	42.608128
3504.327558	526469.977592	42.613133
3504.200728	526458.980461	42.618138
3504.068713	526456.474650	42.623143
3504.282654	526431.980332	42.628148
3504.604080	526427.128596	42.633152
3504.655254	526418.276470	42.638157
3504.435649	526393.547389	42.643162
3504.016759	526398.920444	42.648167
3504.274027	526392.107821	42.653172
3504.067259	526381.830818	42.658176
3504.372928	526358.079972	42.663181
3504.464805	526355.993606	42.668186
3504.446587	526359.130162	42.673191
3504.684428	526325.989728	42.678196
3504.505034	526320.812810	42.683200
3504.619777	526316.398023	42.688205
3504.271797	526291.638536	42.693210
3504.272480	526279.761960	42.698215
3504.629006	526270.204475	42.703220
3504.335617	526260.951871	42.708224
3504.273473	526243.829106	42.713229
3504.394665	526234.713114	42.718234
3504.238917	526232.362637	42.723239
3504.401011	526208.482644	42.728244
3504.418560	526189.426722	42.733248
3504.858365	526180.108718	42.738253
3504.678785	526161.589319	42.743258
3504.394226	526150.364209	42.748263
3504.615113	526143.860470	42.753268
3504.340792	526111.103783	42.758272
3504.622794	526099.132064	42.763277
3504.509244	526093.995204	42.768282
3504.181803	526069.484825	42.773287
3504.232680	526058.863648	42.778292
3504.257153	526054.665218	42.783296
3504.616473	526045.309317	42.788301
3504.774767	526028.454717	42.793306
3504.501070	526019.148320	42.798311
3504.606390	525983.703277	42.803316
3504.316169	525973.135960	42.808321
3504.574767	525966.525107	42.813325
3504.701681	525949.372143	42.818330
3504.652611	525931.135088	42.823335
3504.711957	525913.386281	42.828340
3504.191868	525900.682010	42.833345
3504.309453	525891.010447	42.838349
3504.341718	525885.142903	42.843354
3504.065749	525860.270282	42.848359
3504.255147	525848.565717	42.853364
3504.176287	525850.751687	42.858369
3504.330906	525841.680727	42.863373
3504.310733	525808.175676	42.868378
3504.361401	525805.792508	42.873383
3504.290211	525803.327519	42.878388
3504.205558	525799.398975	42.883393
3504.526630	525768.468023	42.888397
3504.304314	525767.492603	42.893402
3504.519964	525752.448118	42.898407
3504.307599	525733.225830	42.903412
3504.048234	525724.068618	42.908417
3504.145814	525721.576940	42.913421
3504.280719	525717.664212	42.918426
3504.000220	525711.694420	42.923431
3504.312815	525695.825901	42.928436
3504.192133	525684.069147	42.933441
3504.447216	525689.436987	42.938445
3504.159884	525688.118051	42.943450
3504.347444	525656.702575	42.948455
3504.392005	525645.829416	42.953460
3503.935543	525640.645530	42.958465
3504.355766	525637.546885	42.963469
3504.109544	525616.712486	42.968474
3503.975489	525610.011929	42.973479
3504.137088	525594.167176	42.978484
3504.137742	525609.582465	42.983489
3504.308069	525582.415044	42.988493
3504.329573	525574.476887	42.993498
3504.185398	525556.810394	42.998503
3504.597211	525552.196816	43.003508
3504.164839	525537.759976	43.008513
3504.356196	525531.007948	43.013517
3504.336831	525529.545558	43.018522
3504.392481	525516.446725	43.023527
3504.342392	525490.880782	43.028532
3503.999382	525490.278214	43.033537
3504.235324	525474.269967	43.038541
3504.133336	525481.715992	43.043546
3504.070884	525456.505741	43.048551
3504.012533	525453.280540	43.053556
3503.942222	525438.078794	43.058561
3504.060468	525433.107249	43.063565
3504.173444	525449.111441	43.068570
3503.962385	525442.170275	43.073575
3504.031950	525422.246003	43.078580
3504.335524	525405.468867	43.083585
3504.564615	525393.504986	43.088589
3504.433862	525403.027819	43.093594
3504.392653	525379.532518	43.098599
3504.576834	525361.156859	43.103604
3504.342881	525363.872832	43.108609
3504.366419	525335.110845	43.113613
3504.080534	525324.946749	43.118618
3504.282457	525314.857168	43.123623
3504.360968	525318.130267	43.128628
3504.341636	525295.389519	43.133633
3504.443332	525275.257816	43.138637
3504.155167	525279.953528	43.143642
3504.191908	525269.839486	43.148647
3504.402861	525231.495157	43.153652
3504.367169	525235.443378	43.158657
3504.362721	525217.400626	43.163661
3504.406560	525222.195504	43.168666
3503.885378	525200.696428	43.173671
3504.129784	525192.773390	43.178676
3504.069455	525182.725180	43.183681
3504.495536	525185.640109	43.188685
3504.506429	525163.046024	43.193690
3504.285723	525163.434967	43.198695
3504.495292	525149.047934	43.203700
3504.529556	525134.132626	43.208705
3504.620640	525107.583440	43.213709
3504.290093	525114.711962	43.218714
3504.714259	525096.449695	43.223719
3504.896180	525077.063208	43.228724
3504.251273	525059.576402	43.233729
3504.041383	525042.627332	43.238733
3504.261636	525041.834627	43.243738
3503.871744	525035.275353	43.248743
3504.169381	525032.246514	43.253748
3504.539723	525030.267590	43.258753
3504.158042	525000.810905	43.263757
3504.016935	524998.457930	43.268762
3504.296065	524994.320055	43.273767
3504.347715	524985.062714	43.278772
3504.030872	524971.112533	43.283777
3504.159171	524960.731107	43.288781
3504.117610	524961.849889	43.293786
3504.195742	524951.122582	43.298791
3504.417540	524944.820387	43.303796
3504.208454	524932.672706	43.308801
3504.366386	524910.661546	43.313805
3504.456250	524914.792173	43.318810
3504.399459	524900.649195	43.323815
3504.352612	524872.706200	43.328820
3504.276943	524876.711372	43.333825
3504.610138	524854.975694	43.338829
3504.517433	524835.682868	43.343834
3504.199019	524822.844771	43.348839
3504.343264	524817.767839	43.353844
3504.148678	524806.780279	43.358849
3504.393841	524787.888886	43.363853
3503.898652	524796.711525	43.368858
3504.286706	524787.855791	43.373863
3504.273743	524770.673129	43.378868
3504.250320	524755.716044	43.383873
3504.556142	524741.869416	43.388877
3504.374644	524733.861842	43.393882
3504.430461	524720.509612	43.398887
3504.506966	524707.811175	43.403892
3504.304570	524707.388526	43.408897
3504.589375	524674.692148	43.413901
3504.432130	524675.879780	43.418906
3504.327840	524652.595561	43.423911
3504.521710	524635.380062	43.428916
3504.315607	524621.563705	43.433921
3504.396905	524621.247845	43.438925
3504.341688	524612.007180	43.443930
3504.275313	524586.088555	43.448935
3504.186749	524566.542028	43.453940
3504.388910	524571.615343	43.458945
3504.234272	524553.646129	43.463949
3504.303843	524545.750409	43.468954
3504.199611	524535.051649	43.473959
3504.319378	524524.924014	43.478964
3504.205401	524522.971039	43.483969
3504.530775	524489.004249	43.488973
3504.631008	524486.613051	43.493978
3504.150289	524481.432619	43.498983
3504.392795	524451.674080	43.503988
3504.164897	524452.822352	43.508993
3504.265468	524426.472720	43.513997
3504.348645	524437.883025	43.519002
3504.288719	524420.252506	43.524007
3504.458301	524400.867153	43.529012
3504.245743	524405.702803	43.534017
3504.324651	524389.364481	43.539021
3504.454053	524360.836738	43.544026
3504.451905	524364.021691	43.549031
3504.187550	524360.525560	43.554036
3503.838377	524347.085399	43.559041
3504.090118	524325.513517	43.564045
3504.439772	524324.144323	43.569050
3504.078525	524322.028227	43.574055
3504.542244	524314.171183	43.579060
3504.081704	524292.358026	43.584065
3504.320373	524289.641643	43.589069
3504.321401	524274.073697	43.594074
3504.154547	524259.088274	43.599079
3504.349009	524240.659163	43.604084
3504.207922	524235.424966	43.609089
3504.634807	524234.902835	43.614093
3504.189908	524216.322030	43.619098
3503.939285	524202.158528	43.624103
3504.454316	524197.983162	43.629108
3504.307912	524194.468351	43.634113
3504.071294	524176.511673	43.639117
3504.286091	524162.122930	43.644122
3504.090101	524147.243101	43.649127
3503.994206	524152.110932	43.654132
3503.983979	524152.011714	43.659137
3504.157724	524140.257832	43.664141
3504.174182	524113.668253	43.669146
3503.965103	524108.798585	43.674151
3504.229761	524113.912713	43.679156
3503.782133	524119.745981	43.684161
3504.107900	524099.122471	43.689165
3504.162075	524089.207114	43.694170
3504.029713	524074.873168	43.699175
3503.911952	524071.050525	43.704180
3503.958893	524066.393107	43.709185
3504.288652	524064.117204	43.714189
3504.357904	524051.318303	43.719194
3503.970677	524041.674873	43.724199
3504.146108	524027.999882	43.729204
3504.083145	524031.447245	43.734209
3503.942002	524023.129659	43.739213
3504.341677	524024.229307	43.744218
3504.136960	524004.194992	43.749223
3504.397731	523988.585712	43.754228
3504.323062	523991.074551	43.759233
3504.235282	523982.697962	43.764237
3504.293738	523958.376081	43.769242
3503.985214	523949.882727	43.774247
3504.221803	523940.494458	43.779252
3504.199662	523952.427222	43.784257
3504.426000	523914.532238	43.789261
3504.312374	523920.919344	43.794266
3504.142728	523906.995516	43.799271
3504.342248	523895.793396	43.804276
3504.337632	523881.489632	43.809281
3504.333600	523857.430210	43.814285
3504.329005	523854.499472	43.819290
3504.337459	523863.799025	43.824295
3504.506796	523830.209339	43.829300
3504.282718	523824.937579	43.834305
3504.307889	523818.413290	43.839309
3504.104705	523794.789631	43.844314
3504.329501	523773.170721	43.849319
3504.180307	523775.469184	43.854324
3504.153461	523776.787912	43.859329
3504.353340	523761.238585	43.864333
3504.349590	523749.108096	43.869338
3504.034482	523731.264422	43.874343
3504.382621	523725.851633	43.879348
3504.201877	523730.328625	43.884353
3504.013906	523700.131268	43.889357
3504.171054	523705.919637	43.894362
3504.541245	523704.799884	43.899367
3504.346569	523699.017961	43.904372
3503.721201	523676.016882	43.909377
3504.018887	523665.304561	43.914381
3504.227865	523656.880894	43.919386
3504.110237	523657.607410	43.924391
3504.186362	523655.624280	43.929396
3503.920531	523649.297563	43.934401
3504.129920	523628.843490	43.939405
3504.166138	523624.592020	43.944410
3504.084230	523625.060153	43.949415
3504.143921	523621.360996	43.954420
3504.097759	523617.729118	43.959425
3503.780621	523592.505648	43.964429
3504.229879	523582.476982	43.969434
3503.983805	523579.483268	43.974439
3504.178133	523578.997878	43.979444
3504.399417	523575.374264	43.984449
3504.355809	523560.267613	43.989453
3504.308430	523541.370451	43.994458
3503.961958	523535.561915	43.999463
3504.197798	523540.933522	44.004468
3504.032717	523534.034807	44.009473
3504.142120	523502.223088	44.014477
3504.326775	523504.671011	44.019482
3504.177367	523491.451296	44.024487
3504.232693	523496.901999	44.029492
3504.207786	523480.073683	44.034497
3504.566494	523458.332089	44.039501
3504.108791	523466.441851	44.044506
3504.395697	523448.300511	44.049511
3504.542351	523420.880437	44.054516
3504.110163	523420.746816	44.059521
3504.256897	523409.047220	44.064525
3503.999654	523418.540673	44.069530
3504.349975	523394.930032	44.074535
3504.430840	523374.041016	44.079540
3503.918225	523380.440855	44.084545
3504.221608	523360.780359	44.089549
3504.083464	523345.385159	44.094554
3504.029376	523335.385355	44.099559
3504.292854	523322.959563	44.104564
3504.258082	523335.653009	44.109569
3504.422793	523315.407795	44.114573
3504.437941	523298.724605	44.119578
3504.519677	523287.287938	44.124583
3504.487677	523279.306556	44.129588
3503.977187	523254.921899	44.134593
3504.087769	523235.898313	44.139597
3504.226653	523240.527113	44.144602
3504.053415	523241.869023	44.149607
3504.358852	523246.976983	44.154612
3503.947052	523215.954769	44.159617
3504.237959	523203.474001	44.164621
3504.101588	523200.917816	44.169626
3504.055406	523200.167139	44.174631
3504.431814	523182.971784	44.179636
3503.709482	523175.402764	44.184641
3504.422621	523156.839879	44.189645
3504.495729	523156.575835	44.194650
3504.214910	523151.413921	44.199655
3503.849337	523120.687511	44.204660
3504.021654	523119.649546	44.209665
3503.893037	523116.434982	44.214669
3503.998026	523126.477940	44.219674
3504.043207	523115.299676	44.224679
3504.265045	523117.489034	44.229684
3503.897560	523097.580417	44.234689
3504.161355	523085.306041	44.239693
3504.027052	523070.112168	44.244698
3503.985075	523072.494882	44.249703
3504.093218	523068.889038	44.254708
3504.158804	523077.169027	44.259713
3504.094038	523051.348774	44.264717
3504.013662	523038.724370	44.269722
3504.211093	523038.289024	44.274727
3504.503038	523035.007966	44.279732
3504.019335	523024.216535	44.284737
3504.275283	523007.040035	44.289741
3504.319056	522985.954182	44.294746
3503.924360	523001.889411	44.299751
3504.479455	522987.698580	44.304756
3504.115977	522972.490291	44.309761
3504.452148	522964.298908	44.314765
3504.323097	522948.750243	44.319770
3504.400328	522952.377875	44.324775
3504.360367	522919.072125	44.329780
3503.996783	522922.718893	44.334785
3504.579603	522905.490617	44.339789
3504.204445	522893.721493	44.344794
3504.161412	522881.546012	44.349799
3504.050112	522869.836263	44.354804
3503.953448	522874.603500	44.359809
3504.044194	522863.771709	44.364813
3503.882140	522877.951585	44.369818
3504.191734	522851.414690	44.374823
3504.122518	522830.750895	44.379828
3503.986697	522826.728609	44.384833
3504.177317	522821.087668	44.389837
3504.049943	522834.048896	44.394842
3503.893603	522817.392315	44.399847
3504.319936	522787.601651	44.404852
3503.960639	522788.871908	44.409857
3504.062777	522786.126305	44.414861
3504.119468	522788.240713	44.419866
3504.250365	522771.387031	44.424871
3504.439471	522747.447076	44.429876
3503.981569	522751.108791	44.434881
3504.132878	522739.761840	44.439885
3504.351073	522740.182562	44.444890
3504.100481	522726.927664	44.449895
3504.245813	522699.607676	44.454900
3503.913532	522698.598895	44.459905
3504.131317	522699.322985	44.464909
3504.034045	522696.457237	44.469914
3504.055778	522680.884479	44.474919
3504.274572	522661.388158	44.479924
3504.148180	522667.474472	44.484929
3504.168059	522644.572128	44.489933
3504.152309	522656.959796	44.494938
3504.137561	522650.087490	44.499943
3504.213482	522619.896950	44.504948
3503.576182	522615.296719	44.509953
3504.121403	522613.845922	44.514957
3503.893540	522610.191987	44.519962
3503.829492	522619.402616	44.524967
3504.334295	522614.874609	44.529972
3503.991030	522595.972560	44.534977
3503.930346	522578.542350	44.539981
3503.940718	522571.312184	44.544986
3503.896277	522562.220292	44.549991
3504.278876	522568.276740	44.554996
3503.724765	522589.393768	44.560001
3504.061506	522568.614919	44.565005
3504.295240	522567.668313	44.570010
3504.277374	522543.659671	44.575015
3504.482527	522539.128457	44.580020
3504.149321	522531.598725	44.585025
3504.103814	522511.132978	44.590029
3504.075750	522500.673583	44.595034
3503.718280	522498.859951	44.600039
3504.142189	522488.581862	44.605044
3503.865470	522487.665386	44.610049
3503.846614	522493.987524	44.615053
3504.079356	522494.860913	44.620058
3504.131698	522479.485329	44.625063
3504.215869	522450.101988	44.630068
3504.385576	522444.464221	44.635073
3504.045869	522449.320552	44.640077
3504.186474	522448.489763	44.645082
3504.161944	522421.903876	44.650087
3504.238423	522413.045544	44.655092
3504.060936	522409.737461	44.660097
3504.747794	522401.844222	44.665101
3504.310655	522396.858428	44.670106
3504.266809	522387.816897	44.675111
3504.409507	522378.745873	44.680116
3504.067666	522356.102503	44.685121
3504.241159	522339.342742	44.690125
3503.869922	522338.744508	44.695130
3503.851594	522327.474635	44.700135
3504.405854	522328.802729	44.705140
3504.052155	522321.276138	44.710145
3504.134737	522297.150149	44.715149
3503.785498	522299.025475	44.720154
3503.844753	522294.719462	44.725159
3504.188490	522293.755453	44.730164
3503.852311	522292.949468	44.735169
3503.851864	522288.804546	44.740173
3504.105470	522285.630503	44.745178
3504.146232	522264.038667	44.750183
3504.081216	522252.220051	44.755188
3503.863833	522246.946714	44.760193
3504.237336	522238.900721	44.765197
3504.493657	522233.198639	44.770202
3504.422953	522225.880030	44.775207
3504.398916	522212.487794	44.780212
3504.150921	522215.257063	44.785217
3504.458621	522187.152266	44.790221
3504.215570	522184.966647	44.795226
3504.231265	522160.800476	44.800231
3504.214296	522156.658132	44.805236
3503.975468	522148.708884	44.810241
3504.148679	522120.018602	44.815245
3504.046475	522118.922863	44.820250
3504.166636	522118.651364	44.825255
3504.464099	522109.859041	44.830260
3504.049673	522081.868207	44.835265
3503.971929	522080.465284	44.840269
3503.995349	522077.226480	44.845274
3504.070511	522061.493025	44.850279
3504.252660	522071.221127	44.855284
3503.518444	522076.594900	44.860289
3504.003259	522062.111057	44.865293
3504.209325	522044.789765	44.870298
3503.868188	522044.843945	44.875303
3503.745787	522037.280660	44.880308
3504.087147	522036.114801	44.885313
3503.930992	522032.803268	44.890317
3504.008547	522040.374159	44.895322
3503.854181	522036.253502	44.900327
3503.735895	522019.286769	44.905332
3503.801239	522005.121943	44.910337
3503.656410	521992.254146	44.915341
3504.210841	521987.617017	44.920346
3503.958289	521985.887848	44.925351
3504.035745	521985.370334	44.930356
3503.746192	521982.989827	44.935361
3503.789961	521986.622965	44.940365
3503.663003	521993.569019	44.945370
3503.713973	521991.994084	44.950375
3504.108303	521991.679246	44.955380
3503.978192	521972.035036	44.960385
3503.757007	521964.285120	44.965389
3504.087709	521958.672290	44.970394
3503.762803	521954.730228	44.975399
3503.775542	521947.398304	44.980404
3503.595458	521960.065245	44.985409
3504.166101	521946.073261	44.990413
3503.741414	521964.996867	44.995418
3504.165304	521954.111810	45.000423
3503.951756	521946.512336	45.005428
3503.848116	521933.334664	45.010433
3504.186118	521916.346251	45.015437
3503.980755	521915.671228	45.020442
3503.756104	521915.706995	45.025447
3503.917021	521920.534903	45.030452
3503.962581	521919.870770	45.035457
3504.035882	521902.519759	45.040461
3503.739043	521895.337852	45.045466
3503.986201	521883.874047	45.050471
3503.982904	521876.443519	45.055476
3503.729747	521882.600718	45.060481
3503.953818	521876.650843	45.065485
3504.216859	521873.121357	45.070490
3503.975370	521869.519960	45.075495
3504.005794	521872.144171	45.080500
3503.931468	521855.423083	45.085505
3504.009564	521833.976433	45.090509
3503.891059	521829.698396	45.095514
3504.073586	521835.685638	45.100519
3504.433363	521832.595831	45.105524
3504.145035	521828.041317	45.110529
3503.973744	521804.258045	45.115533
3504.094149	521795.695753	45.120538
3503.729900	521795.601926	45.125543
3504.473898	521788.255448	45.130548
3504.167346	521794.522227	45.135553
3504.300761	521768.466390	45.140557
3504.257152	521752.094214	45.145562
3503.880324	521753.316766	45.150567
3504.173888	521735.223011	45.155572
3504.033821	521751.574198	45.160577
3503.692776	521736.917288	45.165581
3503.883359	521715.806576	45.170586
3503.874905	521720.307440	45.175591
3503.756338	521718.658170	45.180596
3503.752026	521727.657649	45.185601
3503.937160	521704.980623	45.190605
3503.957006	521718.879991	45.195610
3503.631960	521716.100625	45.200615
3504.087888	521710.215148	45.205620
3504.032572	521709.364737	45.210625
3504.105667	521707.533509	45.215629
3503.913439	521684.107246	45.220634
3503.924436	521675.612738	45.225639
3503.930145	521666.259649	45.230644
3503.762316	521683.171384	45.235649
3504.058400	521676.148425	45.240653
3503.634336	521678.288417	45.245658
3503.660656	521672.875264	45.250663
3503.903571	521679.560771	45.255668
3503.582196	521680.724009	45.260673
3503.782317	521669.874133	45.265677
3504.069147	521675.288856	45.270682
3503.812340	521642.621403	45.275687
3504.147992	521635.844942	45.280692
3503.711772	521637.076891	45.285697
3503.980881	521631.322023	45.290701
3504.098105	521625.995593	45.295706
3504.046355	521636.215913	45.300711
3503.926656	521623.293297	45.305716
3503.614413	521609.036149	45.310721
3504.221866	521597.565746	45.315725
3503.760565	521593.392385	45.320730
3503.792498	521602.285095	45.325735
3504.161329	521601.317080	45.330740
3504.116700	521598.847247	45.335745
3504.397851	521594.809298	45.340749
3503.809474	521571.849923	45.345754
3503.822887	521567.298194	45.350759
3503.903803	521564.707403	45.355764
3503.764679	521560.938094	45.360769
3504.058826	521555.583675	45.365773
3504.227632	521560.814876	45.370778
3504.408798	521550.170133	45.375783
3504.178646	521519.570939	45.380788
3503.764780	521522.417097	45.385793
3503.784772	521510.432840	45.390797
3504.058807	521513.372482	45.395802
3503.929045	521510.309441	45.400807
3504.103395	521514.427587	45.405812
3503.938487	521486.042403	45.410817
3504.048431	521474.953880	45.415821
3504.211872	521464.867980	45.420826
3503.966616	521477.747816	45.425831
3503.926697	521456.420431	45.430836
3503.795754	521466.552268	45.435841
3504.122229	521459.423303	45.440845
3504.043487	521438.304249	45.445850
3503.830430	521437.883194	45.450855
3503.914290	521421.642199	45.455860
3503.837067	521430.855585	45.460865
3503.933594	521429.323949	45.465869
3503.794955	521434.957670	45.470874
3503.823744	521425.803011	45.475879
3504.287648	521426.842139	45.480884
3503.668143	521429.821927	45.485889
3503.861290	521402.289981	45.490893
3503.747151	521397.101156	45.495898
3503.879371	521390.912850	45.500903
3504.068295	521386.889429	45.505908
3503.815313	521396.585607	45.510913
3503.859628	521383.232438	45.515917
3503.754498	521401.145649	45.520922
3503.561125	521387.375062	45.525927
3504.091834	521384.460371	45.530932
3503.690944	521397.112098	45.535937
3503.874875	521389.247316	45.540941
3503.925457	521372.101549	45.545946
3503.584344	521361.033691	45.550951
3503.978082	521348.939683	45.555956
3503.757056	521340.633341	45.560961
3503.787249	521354.379720	45.565965
3503.860082	521345.976376	45.570970
3503.662534	521359.758749	45.575975
3503.917753	521342.732269	45.580980
3503.404249	521362.530045	45.585985
3503.537602	521358.110963	45.590989
3503.401680	521357.728267	45.595994
3503.425726	521367.481783	45.600999
3503.301925	521357.289557	45.606004
3503.824708	521352.758362	45.611009
3503.818524	521353.821246	45.616013
3503.877674	521356.643218	45.621018
3503.955186	521359.209515	45.626023
3504.246011	521353.501671	45.631028
3503.827259	521369.138973	45.636033
3503.795824	521340.024670	45.641037
3504.046505	521315.617879	45.646042
3503.948911	521329.081149	45.651047
3504.179841	521322.877215	45.656052
3504.036393	521323.759579	45.661057
3503.986805	521317.397764	45.666061
3503.820491	521330.113573	45.671066
3504.073957	521315.109534	45.676071
3504.064961	521278.610563	45.681076
3503.900618	521289.607223	45.686081
3503.793819	521281.535569	45.691085
3503.914195	521275.551312	45.696090
3503.845427	521265.299774	45.701095
3503.899038	521271.762598	45.706100
3503.865510	521282.890250	45.711105
3503.879312	521271.412345	45.716109
3503.861879	521269.241493	45.721114
3503.633729	521239.096449	45.726119
3503.903458	521229.549709	45.731124
3503.678176	521241.314361	45.736129
3503.757607	521232.101034	45.741133
3503.786830	521236.545522	45.746138
3503.763631	521227.904521	45.751143
3503.777232	521234.474794	45.756148
3503.913254	521230.763027	45.761153
3504.132824	521229.414143	45.766157
3503.911887	521228.893217	45.771162
3504.071278	521245.854794	45.776167
3504.074891	521224.469669	45.781172
3503.923110	521201.541868	45.786177
3504.084484	521200.606623	45.791181
3503.883817	521200.739709	45.796186
3503.844419	521199.532869	45.801191
3504.162437	521197.612314	45.806196
3503.805954	521203.179439	45.811201
3503.820744	521177.849179	45.816205
3503.957078	521170.497368	45.821210
3503.693855	521169.730347	45.826215
3504.231522	521156.905673	45.831220
3504.109919	521159.857362	45.836225
3503.812584	521168.954022	45.841229
3503.981160	521172.314838	45.846234
3503.778804	521163.601011	45.851239
3503.864922	521142.354403	45.856244
3503.735025	521128.725230	45.861249
3504.140427	521109.096439	45.866253
3503.794511	521116.077477	45.871258
3504.023221	521122.108238	45.876263
3504.107702	521111.579603	45.881268
3503.714499	521123.674216	45.886273
3503.968541	521112.866001	45.891277
3504.018288	521124.233376	45.896282
3504.059538	521103.802697	45.901287
3504.074702	521095.964450	45.906292
3503.964650	521107.710984	45.911297
3504.135628	521088.422557	45.916301
3503.752971	521094.044411	45.921306
3503.680751	521099.162193	45.926311
3503.989714	521090.367504	45.931316
3503.793599	521095.959871	45.936321
3504.127793	521069.213955	45.941325
3503.850235	521056.265285	45.946330
3503.946795	521049.930820	45.951335
3504.228484	521044.123202	45.956340
3504.242468	521049.480152	45.961345
3504.210382	521034.975993	45.966349
3504.453922	521021.388813	45.971354
3503.898337	521020.667998	45.976359
3504.169067	521009.604299	45.981364
3504.017129	521015.745824	45.986369
3503.923800	520990.432363	45.991373
3504.003080	520971.309959	45.996378
3503.961413	520964.036748	46.001383
3504.239778	520961.364094	46.006388
3503.977321	520958.170256	46.011393
3504.209741	520962.380476	46.016397
3503.833452	520951.065118	46.021402
3503.795020	520932.871284	46.026407
3504.051525	520928.786511	46.031412
3503.753929	520927.822687	46.036417
3504.025549	520923.331076	46.041421
3503.992272	520920.454897	46.046426
3503.953893	520932.594676	46.051431
3504.235919	520922.793034	46.056436
3503.853866	520911.023555	46.061441
3503.941833	520880.322317	46.066445
3504.005375	520878.391394	46.071450
3503.771204	520891.269940	46.076455
3503.938920	520881.991903	46.081460
3503.934229	520875.723932	46.086465
3503.930216	520879.516539	46.091469
3503.807656	520875.997234	46.096474
3503.935250	520883.156305	46.101479
3504.135403	520857.998473	46.106484
3503.928992	520850.043463	46.111489
3503.696220	520854.782250	46.116493
3504.254432	520842.510201	46.121498
3504.330609	520847.099042	46.126503
3504.061832	520832.884898	46.131508
3504.148919	520824.428475	46.136513
3504.064794	520805.129480	46.141517
3503.933921	520806.919900	46.146522
3503.934918	520805.656088	46.151527
3504.369943	520796.588533	46.156532
3504.057557	520795.222587	46.161537
3504.188418	520777.153488	46.166541
3504.525471	520758.748437	46.171546
3503.910619	520767.036048	46.176551
3503.972250	520762.931481	46.181556
3503.896684	520744.288297	46.186561
3503.679296	520720.965735	46.191565
3503.659850	520720.261273	46.196570
3503.948853	520711.924545	46.201575
3504.004838	520703.068523	46.206580
3503.825596	520718.264133	46.211585
3503.810953	520718.519488	46.216589
3504.002739	520711.108149	46.221594
3504.095853	520719.182763	46.226599
3504.108335	520707.805783	46.231604
3504.061430	520700.229941	46.236609
3504.023899	520675.918307	46.241613
3503.902020	520688.475922	46.246618
3503.853570	520681.658668	46.251623
3503.996687	520673.850549	46.256628
3503.671263	520673.548348	46.261633
3504.120069	520676.864972	46.266637
3503.972906	520658.030778	46.271642
3504.181411	520649.049504	46.276647
3503.959307	520640.793530	46.281652
3503.623620	520636.397837	46.286657
3504.192726	520630.746869	46.291661
3504.287268	520637.607930	46.296666
3503.996011	520630.525693	46.301671
3504.203664	520603.192332	46.306676
3503.735261	520596.795323	46.311681
3503.666534	520599.789312	46.316685
3503.872263	520591.212901	46.321690
3504.024906	520592.099058	46.326695
3504.312725	520594.430004	46.331700
3504.014375	520597.460289	46.336705
3503.927307	520569.313987	46.341709
3504.202932	520558.754781	46.346714
3503.753866	520565.196228	46.351719
3504.059569	520553.418892	46.356724
3503.814717	520557.451873	46.361729
3503.918818	520549.194847	46.366733
3504.043221	520554.534506	46.371738
3504.017890	520537.399861	46.376743
3504.164525	520522.361423	46.381748
3503.987045	520516.828428	46.386753
3503.934332	520516.786460	46.391757
3503.778715	520513.929547	46.396762
3503.876227	520516.290586	46.401767
3504.147132	520514.781858	46.406772
3503.659145	520497.821418	46.411777
3503.852459	520479.539888	46.416781
3503.906454	520471.796318	46.421786
3503.944554	520477.048530	46.426791
3504.208400	520461.839836	46.431796
3503.755168	520472.377136	46.436801
3503.939679	520466.483559	46.441805
3504.050088	520458.174934	46.446810
3503.878041	520469.122806	46.451815
3503.810733	520446.837837	46.456820
3503.678483	520431.388380	46.461825
3503.789795	520422.978478	46.466829
3503.946421	520438.424604	46.471834
3504.085658	520445.683142	46.476839
3504.088698	520430.869548	46.481844
3504.082594	520444.167414	46.486849
3504.290200	520428.310331	46.491853
3504.354477	520406.257295	46.496858
3503.899938	520397.229016	46.501863
3504.196197	520380.751181	46.506868
3504.005444	520390.893138	46.511873
3503.846739	520387.328883	46.516877
3503.895035	520377.766091	46.521882
3503.832520	520350.121108	46.526887
3504.046662	520355.092742	46.531892
3503.813472	520355.079302	46.536897
3503.753244	520353.117323	46.541901
3503.697989	520348.373877	46.546906
3503.552121	520347.537707	46.551911
3503.792947	520351.999546	46.556916
3503.768257	520356.705585	46.561921
3503.698965	520352.318263	46.566925
3503.986453	520362.435201	46.571930
3503.764543	520354.836304	46.576935
3503.941937	520340.399530	46.581940
3503.932026	520339.187965	46.586945
3503.593533	520317.501822	46.591949
3503.864691	520308.004877	46.596954
3503.539265	520311.191169	46.601959
3503.640535	520305.007345	46.606964
3503.999853	520310.208835	46.611969
3503.963323	520312.894439	46.616973
3503.773258	520304.886021	46.621978
3503.824548	520314.231396	46.626983
3504.135622	520312.059048	46.631988
3503.981793	520317.897786	46.636993
3503.732154	520301.303929	46.641997
3503.977930	520280.839890	46.647002
3503.839453	520282.429336	46.652007
3504.258084	520275.386407	46.657012
3503.979209	520268.554845	46.662017
3504.116424	520272.224154	46.667021
3504.125228	520272.121903	46.672026
3503.788324	520260.698723	46.677031
3503.983904	520226.945758	46.682036
3503.943749	520233.221582	46.687041
3504.334398	520225.171890	46.692045
3504.244204	520222.355142	46.697050
3503.902678	520226.807951	46.702055
3504.107552	520212.872304	46.707060
3504.027018	520204.290382	46.712065
3503.872599	520182.827755	46.717069
3503.748494	520189.571891	46.722074
3504.015058	520198.124929	46.727079
3504.198586	520175.344916	46.732084
3503.854936	520185.865077	46.737089
3503.792542	520174.196211	46.742093
3504.008587	520143.018317	46.747098
3503.929223	520148.188084	46.752103
3503.936879	520142.221230	46.757108
3503.840339	520140.467199	46.762113
3503.994435	520130.280837	46.767117
3504.003377	520137.256757	46.772122
3503.710546	520138.263913	46.777127
3504.229636	520137.423740	46.782132
3503.949264	520116.385403	46.787137
3503.822042	520105.990701	46.792141
3503.903635	520094.450694	46.797146
3503.492675	520105.891602	46.802151
3503.704127	520094.027716	46.807156
3503.714134	520107.626661	46.812161
3503.928622	520099.402519	46.817165
3503.934495	520107.541785	46.822170
3503.768193	520102.815820	46.827175
3503.986389	520096.259524	46.832180
3503.842599	520102.096752	46.837185
3503.879446	520089.603201	46.842189
3503.950083	520083.575811	46.847194
3503.474583	520073.994520	46.852199
3503.808247	520061.352913	46.857204
3503.660591	520066.078472	46.862209
3503.965241	520055.261561	46.867213
3503.895077	520059.165933	46.872218
3503.465077	520070.306523	46.877223
3504.020178	520050.703359	46.882228
3503.762919	520072.585658	46.887233
3503.881210	520051.383104	46.892237
3504.048419	520058.081246	46.897242
3503.850483	520064.533752	46.902247
3503.972149	520040.752154	46.907252
3503.896971	520023.422614	46.912257
3503.903966	520017.506377	46.917261
3503.849404	520017.414141	46.922266
3503.520673	520024.342367	46.927271
3504.067941	520007.420009	46.932276
3503.650860	520015.777853	46.937281
3503.911437	520021.045603	46.942285
3503.737684	520027.292065	46.947290
3503.620830	520023.367203	46.952295
3504.164374	520019.691863	46.957300
3503.716395	520020.369638	46.962305
3504.007281	519993.022101	46.967309
3503.938327	519990.656987	46.972314
3503.907499	519986.920753	46.977319
3504.057197	519987.200702	46.982324
3503.909781	519981.106624	46.987329
3504.110890	519986.181549	46.992333
3503.866324	519980.911771	46.997338
3503.722679	519978.609020	47.002343
3503.737793	519960.708992	47.007348
3503.821417	519953.061612	47.012353
3504.176180	519940.770490	47.017357
3504.128221	519947.148775	47.022362
3504.059710	519944.429671	47.027367
3503.980311	519948.386088	47.032372
3504.087761	519941.392204	47.037377
3504.154040	519925.809770	47.042381
3503.980089	519905.108252	47.047386
3503.968234	519911.278608	47.052391
3503.931898	519900.363816	47.057396
3503.813789	519901.191691	47.062401
3503.899542	519905.526487	47.067405
3504.013259	519899.492220	47.072410
3503.687338	519891.707310	47.077415
3503.937016	519864.062716	47.082420
3503.976177	519868.657684	47.087425
3503.629079	519857.791985	47.092429
3503.852398	519858.363655	47.097434
3503.790319	519864.592527	47.102439
3503.736988	519860.101431	47.107444
3504.019674	519861.017632	47.112449
3504.004319	519856.014939	47.117453
3504.012489	519861.625995	47.122458
3504.208571	519847.388070	47.127463
3504.028645	519820.215785	47.132468
3504.163214	519827.576455	47.137473
3504.171649	519812.508650	47.142477
3503.959228	519815.879412	47.147482
3503.911245	519817.859075	47.152487
3504.516188	519799.410601	47.157492
3503.830560	519796.131744	47.162497
3504.015906	519799.742992	47.167501
3504.133764	519788.702634	47.172506
3503.834397	519792.643299	47.177511
3503.876910	519786.771924	47.182516
3504.131793	519759.480249	47.187521
3503.830517	519757.758539	47.192525
3504.036599	519750.546745	47.197530
3503.994995	519735.891257	47.202535
3504.230833	519734.286883	47.207540
3503.803545	519746.387899	47.212545
3504.241072	519734.791377	47.217549
3504.233578	519718.512570	47.222554
3504.030501	519707.725125	47.227559
3504.219729	519696.268944	47.232564
3503.948848	519701.721925	47.237569
3503.957908	519685.389908	47.242573
3503.816215	519674.744419	47.247578
3503.998000	519665.058990	47.252583
3504.011186	519664.652683	47.257588
3503.943946	519656.523412	47.262593
3503.715105	519654.992482	47.267597
3504.030459	519657.420331	47.272602
3503.863704	519656.233507	47.277607
3504.288414	519648.532069	47.282612
3504.005533	519636.998793	47.287617
3504.028930	519624.608133	47.292621
3503.839201	519622.110376	47.297626
3503.840886	519616.953235	47.302631
3503.839632	519614.981846	47.307636
3503.849906	519623.424018	47.312641
3503.478715	519611.045160	47.317645
3503.880318	519611.740338	47.322650
3503.690380	519623.500565	47.327655
3503.655855	519619.663712	47.332660
3503.650774	519620.322054	47.337665
3503.919338	519600.814206	47.342669
3504.112096	519580.205993	47.347674
3503.572956	519584.993573	47.352679
3503.366058	519579.363789	47.357684
3503.307370	519582.356376	47.362689
3503.900814	519581.959467	47.367693
3503.849910	519582.978975	47.372698
3503.427058	519571.568897	47.377703
3503.831079	519567.966073	47.382708
3503.814496	519582.884224	47.387713
3503.896486	519568.209050	47.392717
3503.905941	519577.258098	47.397722
3503.434665	519580.922626	47.402727
3503.844579	519575.043661	47.407732
3503.721389	519573.748824	47.412737
3503.792706	519579.046633	47.417741
3503.762147	519576.169787	47.422746
3503.707969	519579.616705	47.427751
3504.007665	519578.204463	47.432756
3503.941541	519591.512509	47.437761
3503.961505	519563.094756	47.442765
3503.959542	519552.376540	47.447770
3503.810022	519548.203924	47.452775
3503.908706	519537.065306	47.457780
3503.953951	519534.024789	47.462785
3503.885481	519539.799751	47.467789
3503.960680	519540.799329	47.472794
3503.783664	519546.288084	47.477799
3504.155739	519527.724434	47.482804
3503.913137	519526.448469	47.487809
3503.838087	519505.124088	47.492813
3503.987464	519499.235718	47.497818
3503.496563	519507.605489	47.502823
3503.962212	519491.099985	47.507828
3503.922725	519501.117461	47.512833
3504.014886	519500.496424	47.517837
3503.981097	519496.811107	47.522842
3503.728431	519494.626642	47.527847
3504.035910	519480.471912	47.532852
3503.818106	519471.405697	47.537857
3503.834170	519456.184678	47.542861
3503.972681	519455.354071	47.547866
3503.726128	519457.213482	47.552871
3504.120454	519462.915317	47.557876
3503.837596	519459.269362	47.562881
3503.762534	519455.388317	47.567885
3503.994807	519453.481116	47.572890
3503.917478	519444.797167	47.577895
3503.928120	519424.166985	47.582900
3503.655058	519425.322740	47.587905
3503.760852	519418.935624	47.592909
3503.755003	519420.756992	47.597914
3503.575448	519408.549932	47.602919
3503.597848	519400.204121	47.607924
3503.519991	519405.626688	47.612929
3503.486804	519416.553313	47.617933
3503.473917	519420.802709	47.622938
3503.330613	519417.033563	47.627943
3503.638144	519414.204369	47.632948
3503.310683	519419.211339	47.637953
3503.525738	519416.143959	47.642957
3504.136787	519413.469030	47.647962
3503.706030	519421.323730	47.652967
3503.878232	519418.869852	47.657972
3503.834218	519418.320899	47.662977
3503.877766	519425.139969	47.667981
3503.687916	519414.906409	47.672986
3503.783006	519420.301633	47.677991
3503.890663	519407.290762	47.682996
3503.344507	519422.393890	47.688001
3503.632456	519410.264615	47.693005
3503.759596	519417.474962	47.698010
3503.605557	519426.802740	47.703015
3503.722194	519421.728489	47.708020
3503.793907	519419.138814	47.713025
3503.546656	519428.076839	47.718029
3503.893252	519424.988668	47.723034
3503.781074	519430.770577	47.728039
3504.080969	519413.532786	47.733044
3503.746154	519409.086060	47.738049
3503.848006	519391.879550	47.743053
3504.026935	519379.868608	47.748058
3503.652689	519385.742518	47.753063
3504.034267	519382.244323	47.758068
3503.862372	519388.844659	47.763073
3503.768404	519384.460978	47.768077
3503.585273	519379.889146	47.773082
3503.606964	519392.576742	47.778087
3504.045362	519377.440574	47.783092
3503.625827	519387.619315	47.788097
3503.703237	519380.832184	47.793101
3504.033733	519379.010570	47.798106
3503.487783	519353.563876	47.803111
3504.046819	519347.003966	47.808116
3503.912534	519339.390744	47.813121
3503.777771	519340.423523	47.818125
3503.918727	519340.957670	47.823130
3503.777908	519347.047501	47.828135
3504.198650	519343.138619	47.833140
3504.096459	519348.362808	47.838145
3504.282914	519335.086619	47.843149
3504.491139	519309.419522	47.848154
3504.042159	519305.597547	47.853159
3504.096161	519301.645503	47.858164
3504.180302	519292.582023	47.863169
3504.160660	519255.422922	47.868173
3504.330733	519264.750121	47.873178
3503.946369	519258.389860	47.878183
3504.066114	519255.893689	47.883188
3503.680255	519265.106519	47.888193
3503.849284	519231.659069	47.893197
3503.843053	519229.941226	47.898202
3504.026213	519221.974404	47.903207
3503.838236	519216.189820	47.908212
3504.295573	519220.516623	47.913217
3504.061442	519212.110143	47.918221
3503.900311	519217.293129	47.923226
3504.026980	519208.425125	47.928231
3504.309814	519178.701120	47.933236
3504.100221	519177.470470	47.938241
3504.036071	519180.817924	47.943245
3504.058933	519178.741548	47.948250
3503.968018	519173.851713	47.953255
3503.947663	519155.197989	47.958260
3503.956803	519146.348530	47.963265
3504.358676	519133.644866	47.968269
3504.247107	519134.067252	47.973274
3504.047294	519147.801283	47.978279
3503.622228	519117.885695	47.983284
3503.722847	519118.072294	47.988289
3503.776732	519104.159573	47.993293
3503.855082	519084.226124	47.998298
3503.411318	519091.830227	48.003303
3503.908268	519089.678901	48.008308
3503.484524	519094.195571	48.013313
3503.818925	519092.474433	48.018317
3503.848535	519098.234046	48.023322
3503.912826	519094.533135	48.028327
3504.206573	519087.560002	48.033332
3503.983123	519083.247269	48.038337
3503.956589	519080.925879	48.043341
3504.062129	519082.527430	48.048346
3504.130168	519059.207942	48.053351
3504.228981	519054.844262	48.058356
3503.507583	519058.245069	48.063361
3504.211103	519043.774553	48.068365
3504.097592	519052.843328	48.073370
3504.175270	519045.651521	48.078375
3504.049434	519013.514283	48.083380
3503.951039	519007.917713	48.088385
3504.025095	519005.580413	48.093389
3504.009587	519003.661765	48.098394
3504.078917	519006.583659	48.103399
3504.193410	518994.936555	48.108404
3503.864744	518975.471807	48.113409
3504.217144	518971.826452	48.118413
3504.167017	518962.480640	48.123418
3504.389793	518963.558051	48.128423
3504.725779	518933.774639	48.133428
3504.384197	518924.373752	48.138433
3504.099012	518915.065069	48.143437
3504.114595	518916.731418	48.148442
3504.148673	518894.175498	48.153447
3504.343573	518883.627977	48.158452
3504.223652	518876.113394	48.163457
3504.474045	518870.512207	48.168461
3504.650482	518834.079595	48.173466
3504.100446	518835.734234	48.178471
3504.168871	518827.987607	48.183476
3504.239063	518821.049699	48.188481
3503.972957	518800.260228	48.193485
3504.104061	518797.661067	48.198490
3503.953134	518787.067023	48.203495
3504.199053	518782.224953	48.208500
3503.860194	518794.363251	48.213505
3503.894621	518780.149956	48.218509
3504.087408	518756.962009	48.223514
3503.958453	518744.443079	48.228519
3504.321437	518747.571416	48.233524
3504.189128	518750.272415	48.238529
3504.188433	518742.384985	48.243533
3503.821188	518723.077725	48.248538
3503.623787	518713.198860	48.253543
3504.179612	518702.948112	48.258548
3503.698150	518712.226924	48.263553
3503.940169	518701.570712	48.268557
3503.868960	518700.722656	48.273562
3503.685469	518705.252018	48.278567
3503.842751	518705.126288	48.283572
3503.603596	518702.433950	48.288577
3503.761574	518703.471057	48.293581
3504.006830	518702.168474	48.298586
3504.047800	518684.060714	48.303591
3504.271638	518665.468962	48.308596
3503.894069	518664.972707	48.313601
3503.597258	518659.660197	48.318605
3504.008308	518648.572728	48.323610
3503.943664	518651.718115	48.328615
3504.065734	518648.867544	48.333620
3503.756173	518648.613354	48.338625
3504.156842	518626.959821	48.343629
3504.072435	518607.456027	48.348634
3503.636267	518614.958021	48.353639
3504.126241	518609.116622	48.358644
3503.998270	518619.502565	48.363649
3503.930067	518615.367420	48.368653
3503.936891	518616.681242	48.373658
3503.960201	518602.520113	48.378663
3504.126481	518575.139351	48.383668
3504.172316	518569.620960	48.388673
3504.255097	518567.686725	48.393677
3503.946206	518562.932289	48.398682
3503.938464	518567.939542	48.403687
3504.392368	518551.485519	48.408692
3504.178621	518541.659697	48.413697
3504.108381	518529.839211	48.418701
3504.294715	518524.349160	48.423706
3504.061197	518516.599551	48.428711
3503.892780	518491.951421	48.433716
3503.854591	518492.716168	48.438721
3504.136674	518479.019665	48.443725
3504.110378	518478.872388	48.448730
3503.801763	518488.275695	48.453735
3504.111471	518482.462746	48.458740
3504.126073	518473.258116	48.463745
3503.894496	518455.597696	48.468749
3503.772392	518458.044311	48.473754
3503.737494	518446.218178	48.478759
3503.813769	518455.408973	48.483764
3503.877373	518455.601431	48.488769
3504.320356	518451.891080	48.493773
3503.952657	518450.381984	48.498778
3503.842976	518428.303224	48.503783
3503.761311	518407.180718	48.508788
3503.884609	518398.666758	48.513793
3503.867669	518410.956708	48.518797
3504.318760	518398.446955	48.523802
3503.997744	518400.975584	48.528807
3504.112936	518396.508012	48.533812
3504.087085	518392.517809	48.538817
3504.187928	518371.770920	48.543821
3504.129565	518369.201641	48.548826
3503.978021	518369.680928	48.553831
3504.059917	518363.701693	48.558836
3503.860014	518368.385433	48.563841
3503.765726	518342.309571	48.568845
3503.942774	518331.562262	48.573850
3503.653340	518321.090939	48.578855
3503.676408	518306.980159	48.583860
3503.716837	518329.930133	48.588865
3504.005798	518313.097432	48.593869
3503.796392	518307.467606	48.598874
3503.525504	518322.123714	48.603879
3504.050442	518301.006315	48.608884
3504.077595	518313.339932	48.613889
3504.047502	518308.490789	48.618893
3504.141247	518300.082578	48.623898
3504.082255	518286.743214	48.628903
3504.101345	518279.610899	48.633908
3503.827899	518285.469265	48.638913
3503.843395	518275.859869	48.643917
3503.812742	518270.909675	48.648922
3503.666556	518284.180870	48.653927
3503.712417	518268.802349	48.658932
3503.857758	518276.313706	48.663937
3503.826940	518268.127425	48.668941
3503.871961	518245.467759	48.673946
3503.999672	518240.088008	48.678951
3504.022853	518228.657053	48.683956
3503.531242	518235.257824	48.688961
3503.901276	518238.789659	48.693965
3503.875174	518219.023367	48.698970
3503.593369	518238.181508	48.703975
3503.796619	518224.800641	48.708980
3503.746848	518232.342860	48.713985
3503.579573	518214.520323	48.718989
3503.923704	518229.736635	48.723994
3503.631589	518226.496381	48.728999
3504.104975	518220.758597	48.734004
3503.762497	518209.233735	48.739009
3503.979317	518196.204652	48.744013
3503.732703	518180.417199	48.749018
3503.780049	518197.955857	48.754023
3503.981817	518188.721482	48.759028
3504.099161	518191.130287	48.764033
3504.086549	518175.002453	48.769037
3503.761405	518184.105158	48.774042
3503.585718	518193.285363	48.779047
3504.039526	518180.775016	48.784052
3504.047479	518167.071021	48.789057
3504.349463	518143.814387	48.794061
3504.341602	518137.596434	48.799066
3503.871276	518142.676936	48.804071
3503.960700	518136.696428	48.809076
3503.893328	518128.768680	48.814081
3503.634230	518110.353769	48.819085
3503.800515	518096.270734	48.824090
3503.818417	518104.560786	48.829095
3504.024190	518098.764132	48.834100
3503.696324	518095.832892	48.839105
3503.720738	518096.790021	48.844109
3503.827032	518089.643839	48.849114
3503.828206	518108.706835	48.854119
3503.762713	518104.267745	48.859124
3503.777543	518106.439943	48.864129
3503.418058	518098.507790	48.869133
3503.815230	518102.743272	48.874138
3504.103281	518107.248826	48.879143
3504.026971	518082.130441	48.884148
3503.969164	518066.363599	48.889153
3503.488397	518069.524308	48.894157
3503.633270	518062.220322	48.899162
3503.521094	518053.743405	48.904167
3503.452107	518065.687885	48.909172
3503.787069	518060.578705	48.914177
3503.761217	518055.324298	48.919181
3503.708420	518059.529789	48.924186
3503.419916	518059.373390	48.929191
3503.716581	518062.866297	48.934196
3503.733501	518074.544366	48.939201
3503.557037	518069.060946	48.944205
3503.995641	518063.429736	48.949210
3503.774591	518062.453636	48.954215
3503.666596	518068.235362	48.959220
3503.689462	518063.933989	48.964225
3503.943769	518063.489529	48.969229
3503.649205	518065.862332	48.974234
3503.372562	518075.614774	48.979239
3503.749123	518065.139144	48.984244
3503.835371	518070.940730	48.989249
3503.767240	518064.479451	48.994253
3504.270926	518060.354899	48.999258
3503.960544	518037.902821	49.004263
3504.149290	518019.568713	49.009268
3503.645013	518030.469593	49.014273
3503.824852	518023.412887	49.019277
3503.983144	518022.073433	49.024282
3503.897177	518019.508462	49.029287
3504.023081	518023.837410	49.034292
3504.014051	518008.619018	49.039297
3503.490002	517990.549244	49.044301
3504.091182	517986.662088	49.049306
3503.791665	517988.934555	49.054311
3504.047064	517986.517881	49.059316
3503.540534	517979.923606	49.064321
3503.611705	517979.103571	49.069325
3503.654175	517987.238103	49.074330
3503.561531	517988.769958	49.079335
3503.896194	517979.362765	49.084340
3503.778830	517990.151947	49.089345
3503.698175	517988.091783	49.094349
3503.966038	517980.414364	49.099354
3504.080741	517984.290006	49.104359
3503.689725	517969.637609	49.109364
3503.702371	517955.477611	49.114369
3503.952314	517941.684612	49.119373
3504.087923	517941.764564	49.124378
3503.806317	517945.096077	49.129383
3504.117608	517941.001907	49.134388
3503.950238	517941.382577	49.139393
3503.964871	517935.616080	49.144397
3504.184430	517939.980811	49.149402
3503.788406	517906.619988	49.154407
3503.985941	517901.583048	49.159412
3503.767764	517892.768847	49.164417
3503.848221	517892.452994	49.169421
3504.111568	517900.805481	49.174426
3503.617533	517907.912418	49.179431
3503.744075	517893.532101	49.184436
3503.909436	517902.709123	49.189441
3503.735080	517902.585244	49.194445
3503.955510	517892.639839	49.199450
3503.904238	517867.921693	49.204455
3503.712035	517854.603036	49.209460
3503.666123	517859.464841	49.214465
3503.976114	517847.836590	49.219469
3504.123491	517847.510158	49.224474
3503.741838	517853.840870	49.229479
3504.155568	517855.798351	49.234484
3504.060939	517840.694465	49.239489
3504.086306	517836.089244	49.244493
3504.170696	517810.489953	49.249498
3503.895661	517821.607563	49.254503
3504.292680	517803.897647	49.259508
3503.778122	517814.850860	49.264513
3504.010694	517812.488334	49.269517
3504.442402	517799.880062	49.274522
3504.188698	517790.717462	49.279527
3504.050900	517777.339577	49.284532
3504.010707	517775.121293	49.289537
3503.646841	517773.510396	49.294541
3503.881637	517770.945250	49.299546
3503.873654	517777.267491	49.304551
3504.122923	517749.922808	49.309556
3503.635793	517739.280100	49.314561
3503.611674	517730.131742	49.319565
3503.788022	517726.463377	49.324570
3503.552358	517729.888803	49.329575
3503.597069	517727.657092	49.334580
3503.656214	517723.198198	49.339585
3503.799631	517725.704082	49.344589
3503.959344	517724.111550	49.349594
3503.838872	517726.305185	49.354599
3503.804776	517724.035365	49.359604
3503.881865	517730.091347	49.364609
3503.729262	517737.245519	49.369613
3503.898464	517721.594162	49.374618
3503.410960	517732.745416	49.379623
3503.842389	517718.974111	49.384628
3503.843081	517720.390105	49.389633
3504.166959	517699.758814	49.394637
3504.214541	517693.177968	49.399642
3503.975726	517693.772201	49.404647
3503.882247	517685.797800	49.409652
3503.824588	517683.430567	49.414657
3503.691784	517684.665401	49.419661
3504.078181	517679.244578	49.424666
3503.958621	517661.363335	49.429671
3503.889923	517635.484575	49.434676
3503.894296	517647.164930	49.439681
3503.739099	517638.290071	49.444685
3504.091257	517637.223338	49.449690
3503.812079	517641.313021	49.454695
3503.982527	517640.881806	49.459700
3504.060186	517642.589038	49.464705
3504.211861	517625.929037	49.469709
3504.116966	517606.476282	49.474714
3503.736339	517606.182741	49.479719
3503.876391	517597.311756	49.484724
3504.314073	517595.928105	49.489729
3503.980404	517588.800685	49.494733
3503.889703	517581.685423	49.499738
3503.863265	517570.666387	49.504743
3504.155479	517559.040743	49.509748
3503.914352	517556.803625	49.514753
3503.925512	517555.032293	49.519757
3504.313655	517553.302503	49.524762
3504.228425	517546.135794	49.529767
3504.302920	517515.885494	49.534772
3504.209636	517519.339023	49.539777
3504.279642	517501.275943	49.544781
3504.227406	517500.829357	49.549786
3504.030984	517480.280037	49.554791
3503.900477	517453.955662	49.559796
3503.558275	517461.342190	49.564801
3503.383661	517455.908839	49.569805
3503.792431	517453.973512	49.574810
3503.447928	517466.113676	49.579815
3503.830198	517459.024732	49.584820
3503.823212	517466.054870	49.589825
3503.750241	517456.155581	49.594829
3503.854332	517467.870867	49.599834
3503.417640	517475.221757	49.604839
3503.715740	517467.033654	49.609844
3503.908702	517464.171673	49.614849
3503.784587	517469.349355	49.619853
3503.929469	517467.101775	49.624858
3503.692695	517467.139459	49.629863
3503.696794	517464.661299	49.634868
3503.488902	517473.846992	49.639873
3503.757484	517471.731560	49.644877
3503.845505	517461.857393	49.649882
3503.838134	517448.559758	49.654887
3503.876841	517431.664585	49.659892
3503.676571	517436.904881	49.664897
3503.824170	517428.639415	49.669901
3504.146885	517433.847611	49.674906
3503.917974	517428.625102	49.679911
3503.970093	517424.672907	49.684916
3503.894887	517428.932667	49.689921
3503.938812	517416.486534	49.694925
3503.770728	517399.573448	49.699930
3503.718707	517392.148588	49.704935
3503.954786	517376.233499	49.709940
3503.780923	517385.818398	49.714945
3503.555494	517386.410526	49.719949
3503.833049	517377.669389	49.724954
3503.589157	517388.175563	49.729959
3503.922182	517381.246070	49.734964
3503.834762	517389.755397	49.739969
3504.048167	517381.580639	49.744973
3504.063967	517388.303806	49.749978
3503.486434	517385.057934	49.754983
3503.932422	517379.324192	49.759988
3503.711359	517364.745527	49.764993
3503.687260	517357.467939	49.769997
3503.844752	517343.082251	49.775002
3503.719582	517357.463344	49.780007
3504.190510	517344.039454	49.785012
3504.066492	517357.307888	49.790017
3503.956614	517336.795276	49.795021
3504.088118	517338.342327	49.800026
3504.017433	517335.117462	49.805031
3504.218663	517303.885966	49.810036
3504.026624	517303.309772	49.815041
3503.867031	517296.660382	49.820045
3504.094250	517300.821803	49.825050
3503.950020	517286.736596	49.830055
3503.858844	517290.796646	49.835060
3503.867394	517283.159894	49.840065
3503.761855	517271.596922	49.845069
3503.803950	517254.953869	49.850074
3504.068404	517260.677003	49.855079
3503.809015	517263.297197	49.860084
3503.947281	517256.499573	49.865089
3503.663194	517260.741826	49.870093
3503.919047	517250.031926	49.875098
3503.954112	517257.662314	49.880103
3504.039147	517248.193031	49.885108
3503.896173	517229.354241	49.890113
3503.699182	517213.153478	49.895117
3504.013323	517213.609754	49.900122
3503.727542	517205.210410	49.905127
3504.132265	517209.090959	49.910132
3504.251625	517212.561507	49.915137
3503.958481	517202.646301	49.920141
3503.666622	517196.169480	49.925146
3503.821748	517192.656055	49.930151
3503.907865	517164.122572	49.935156
3503.881387	517164.885529	49.940161
3503.788376	517166.973762	49.945165
3503.786199	517167.985716	49.950170
3503.807710	517168.589385	49.955175
3504.019907	517173.966836	49.960180
3503.892993	517170.396853	49.965185
3503.723295	517168.603500	49.970189
3503.849235	517180.163833	49.975194
3503.842376	517167.674973	49.980199
3504.091661	517150.442821	49.985204
3503.834022	517132.987374	49.990209
3503.777743	517136.131727	49.995213
3503.660074	517128.059745	50.000218
3503.489388	517125.862001	50.005223
3504.056540	517134.874803	50.010228
3504.146792	517113.066086	50.015233
3503.807894	517115.446032	50.020237
3503.936217	517126.247509	50.025242
3503.919304	517119.170952	50.030247
3504.023649	517101.354846	50.035252
3503.593882	517097.579880	50.040257
3503.625606	517102.985882	50.045261
3503.838668	517084.242352	50.050266
3503.781184	517086.678954	50.055271
3504.214080	517090.959620	50.060276
3504.100181	517092.697189	50.065281
3503.853760	517090.561980	50.070285
3504.044145	517087.801477	50.075290
3503.927920	517068.351461	50.080295
3503.890691	517047.068488	50.085300
3503.850127	517047.631405	50.090305
3503.632894	517042.457495	50.095309
3503.960318	517043.063380	50.100314
3503.895608	517051.063611	50.105319
3503.729788	517042.442950	50.110324
3503.735569	517055.792245	50.115329
3504.008903	517033.802780	50.120333
3504.230458	517052.882725	50.125338
3503.777514	517024.029667	50.130343
3504.185421	517000.906388	50.135348
3503.901668	516999.889567	50.140353
3503.746641	516996.779104	50.145357
3503.990252	516994.161877	50.150362
3503.922095	517002.314381	50.155367
3504.024835	517001.185898	50.160372
3504.311264	516996.741451	50.165377
3504.139401	516969.714889	50.170381
3504.336313	516957.699343	50.175386
3503.874266	516959.744798	50.180391
3504.001153	516951.178959	50.185396
3503.867857	516953.475859	50.190401
3503.690018	516945.008752	50.195405
3503.742834	516921.941493	50.200410
3503.747407	516917.794420	50.205415
3503.921571	516919.334767	50.210420
3503.884682	516916.863004	50.215425
3503.605670	516908.664713	50.220429
3503.786161	516907.271092	50.225434
3503.688079	516923.064196	50.230439
3503.730521	516919.517957	50.235444
3503.783769	516910.053505	50.240449
3503.782186	516921.887019	50.245453
3503.753946	516919.616163	50.250458
3503.741751	516922.500746	50.255463
3503.976340	516911.692852	50.260468
3503.876374	516921.468612	50.265473
3503.648682	516909.014465	50.270477
3503.707874	516876.287562	50.275482
3503.579622	516889.000787	50.280487
3503.756389	516875.825291	50.285492
3503.908984	516879.948046	50.290497
3503.728226	516871.784775	50.295501
3503.698028	516858.540843	50.300506
3503.709553	516870.473458	50.305511
3503.394130	516862.634880	50.310516
3503.621803	516874.027641	50.315521
3503.648344	516871.444707	50.320525
3503.533558	516866.608529	50.325530
3503.509401	516875.259825	50.330535
3503.531958	516860.338794	50.335540
3503.978082	516867.702111	50.340545
3503.841625	516859.582399	50.345549
3503.580661	516870.293873	50.350554
3503.566756	516876.718531	50.355559
3503.699469	516865.977280	50.360564
3503.424624	516873.960244	50.365569
3503.524752	516871.719658	50.370573
3503.768593	516866.219968	50.375578
3503.772032	516880.581145	50.380583
3504.156804	516874.452359	50.385588
3504.004177	516881.960882	50.390593
3503.784405	516868.595219	50.395597
3503.853743	516871.820903	50.400602
3503.797350	516855.496428	50.405607
3503.831316	516835.011026	50.410612
3503.774968	516830.974697	50.415617
3503.947506	516825.789677	50.420621
3503.976862	516840.804185	50.425626
3503.680057	516832.001845	50.430631
3503.850873	516827.525058	50.435636
3504.042488	516829.871754	50.440641
3503.936527	516820.533555	50.445645
3503.765833	516828.803489	50.450650
3503.596640	516833.533376	50.455655
3503.628519	516815.576712	50.460660
3503.986068	516812.992015	50.465665
3503.742921	516802.411273	50.470669
3503.919464	516785.139671	50.475674
3503.697356	516786.085275	50.480679
3503.984500	516769.150156	50.485684
3504.291406	516785.637907	50.490689
3504.005874	516780.980399	50.495693
3504.218721	516784.739672	50.500698
3504.067688	516763.221479	50.505703
3504.296868	516754.588799	50.510708
3503.819320	516749.708790	50.515713
3504.039037	516750.028299	50.520717
3504.604141	516739.016342	50.525722
3503.840874	516725.079077	50.530727
3503.833240	516697.924973	50.535732
3503.753814	516673.411769	50.540737
3503.703076	516631.093620	50.545741
3503.804503	516582.531273	50.550746
3503.349984	516529.454831	50.555751
3503.600291	516461.247586	50.560756
3503.320954	516400.001301	50.565761
3503.045457	516317.413560	50.570765
3503.264345	516222.357489	50.575770
3502.977415	516124.144298	50.580775
3503.040925	515995.532437	50.585780
3502.831673	515876.571298	50.590785
3502.360279	515752.441837	50.595789
3502.528241	515606.868853	50.600794
3502.106590	515468.518566	50.605799
3502.280478	515302.561136	50.610804
3501.878424	515150.044577	50.615809
3501.495496	514966.015825	50.620813
3501.861843	514789.149389	50.625818
3501.344331	514593.606739	50.630823
3501.132197	514390.629427	50.635828
3500.997367	514183.945339	50.640833
3500.615939	513964.703929	50.645837
3500.522282	513745.060119	50.650842
3500.107311	513503.462492	50.655847
3499.853684	513258.497644	50.660852
3499.570817	513012.218769	50.665857
3498.968924	512761.434438	50.670861
3499.029598	512494.557813	50.675866
3498.408090	512236.434424	50.680871
3498.010108	511970.380761	50.685876
3497.878841	511688.296164	50.690881
3497.236750	511413.217767	50.695885
3497.145536	511121.455675	50.700890
3496.620434	510828.796013	50.705895
3496.499441	510522.914654	50.710900
3496.275822	510222.052293	50.715905
3495.559803	509914.230530	50.720909
3495.433185	509586.782158	50.725914
3494.701631	509264.178734	50.730919
3494.689363	508943.732187	50.735924
3494.317352	508611.750661	50.740929
3493.824139	508268.904107	50.745933
3493.772608	507907.210030	50.750938
3492.497423	507562.499801	50.755943
3492.528017	507196.122963	50.760948
3491.984830	506841.264327	50.765953
3491.419450	506475.371226	50.770957
3491.254668	506103.132600	50.775962
3490.815852	505732.700379	50.780967
3490.429430	505349.095257	50.785972
3490.022231	504963.713839	50.790977
3489.198773	504582.134491	50.795981
3488.788844	504176.190472	50.800986
3488.056360	503799.336662	50.805991
3487.991018	503389.220762	50.810996
3487.406712	502983.630988	50.816001
3486.565337	502576.655408	50.821005
3486.134446	502161.001509	50.826010
3485.283866	501756.589701	50.831015
3485.175597	501331.704338	50.836020
3484.487639	500926.083746	50.841025
3483.965578	500501.294551	50.846029
3483.603164	500074.090945	50.851034
3482.601432	499664.340550	50.856039
3482.421236	499232.836016	50.861044
3481.858063	498796.876315	50.866049
3481.276429	498361.972025	50.871053
3480.809211	497912.408784	50.876058
3480.189883	497478.248471	50.881063
3479.375494	497032.717592	50.886068
3478.813658	496593.818684	50.891073
3478.341823	496149.376368	50.896077
3477.775612	495697.799238	50.901082
3476.938190	495255.215560	50.906087
3476.489751	494790.230615	50.911092
3475.894593	494340.092817	50.916097
3475.358075	493886.947212	50.921101
3474.947795	493418.326327	50.926106
3474.132856	492969.911334	50.931111
3473.356551	492504.464613	50.936116
3472.344054	492051.349108	50.941121
3472.122907	491588.526162	50.946125
3471.724166	491116.705329	50.951130
3470.801902	490670.378636	50.956135
3470.486598	490195.989090	50.961140
3470.014927	489732.703835	50.966145
3469.264176	489255.523074	50.971149
3468.516452	488781.368654	50.976154
3467.650364	488312.691245	50.981159
3466.880554	487838.769840	50.986164
3466.437476	487370.204764	50.991169
3465.726946	486902.126269	50.996173
3464.976992	486408.917343	51.001178
3464.199174	485954.452478	51.006183
3464.000230	485472.935227	51.011188
3463.273366	485004.306105	51.016193
3462.301706	484528.459770	51.021197
3461.689616	484043.982958	51.026202
3460.794538	483567.087486	51.031207
3460.532563	483092.106708	51.036212
3459.582555	482623.404234	51.041217
3458.746914	482141.042990	51.046221
3458.543452	481674.327575	51.051226
3457.465705	481193.045128	51.056231
3456.699708	480710.333423	51.061236
3456.106316	480239.085003	51.066241
3455.401491	479764.093082	51.071245
3454.617594	479295.233758	51.076250
3453.982344	478828.214765	51.081255
3453.359498	478351.908963	51.086260
3452.982343	477870.687795	51.091265
3452.101572	477408.995312	51.096269
3451.469362	476925.054906	51.101274
3450.542154	476459.648105	51.106279
3449.804784	475989.081515	51.111284
3449.540495	475517.060620	51.116289
3448.610516	475040.369494	51.121293
3448.078884	474556.710786	51.126298
3447.262813	474085.098365	51.131303
3446.721882	473608.261220	51.136308
3446.037765	473138.126548	51.141313
3445.126132	472658.081559	51.146317
3444.598775	472179.383887	51.151322
3443.713810	471715.635361	51.156327
3442.917866	471245.576153	51.161332
3442.121288	470785.037048	51.166337
3441.613085	470308.067010	51.171341
3441.130074	469829.662422	51.176346
3440.091123	469371.310089	51.181351
3439.649318	468893.181547	51.186356
3438.866822	468427.821909	51.191361
3438.040836	467962.509454	51.196365
3437.429824	467501.411745	51.201370
3436.586329	467034.154667	51.206375
3435.754840	466562.017528	51.211380
3435.283137	466097.571076	51.216385
3434.441354	465622.372091	51.221389
3433.624191	465168.456401	51.226394
3432.889558	464712.033139	51.231399
3432.373408	464245.626102	51.236404
3431.694893	463797.592441	51.241409
3430.523619	463347.091614	51.246413
3430.299849	462869.552750	51.251418
3429.938781	462415.151352	51.256423
3428.864065	461952.941373	51.261428
3428.274022	461509.258315	51.266433
3427.614511	461035.652972	51.271437
3426.845497	460569.358285	51.276442
3425.736099	460123.345133	51.281447
3425.319828	459658.598231	51.286452
3424.608402	459204.489265	51.291457
3424.129887	458749.218121	51.296461
3423.214376	458286.499282	51.301466
3422.334038	457848.063086	51.306471
3421.653712	457389.295600	51.311476
3420.976756	456940.308655	51.316481
3420.360127	456491.100163	51.321485
3419.685891	456037.376688	51.326490
3418.782910	455600.066420	51.331495
3418.212723	455140.981461	51.336500
3417.443931	454690.949068	51.341505
3416.675048	454251.511189	51.346509
3416.307845	453794.497459	51.351514
3415.207738	453356.768781	51.356519
3414.371131	452906.965173	51.361524
3413.633010	452471.293125	51.366529
3412.696386	452021.741491	51.371533
3412.366736	451593.649732	51.376538
3411.709587	451158.142748	51.381543
3411.061776	450715.775784	51.386548
3410.471986	450281.104122	51.391553
3409.632745	449842.962339	51.396557
3408.841202	449399.983893	51.401562
3408.054451	448971.915616	51.406567
3407.635847	448526.070453	51.411572
3406.974133	448100.706704	51.416577
3406.186194	447655.157013	51.421581
3405.528241	447215.566788	51.426586
3404.667073	446797.112870	51.431591
3404.135146	446350.178370	51.436596
3403.625182	445915.869390	51.441601
3402.413658	445493.996531	51.446605
3401.967655	445054.586246	51.451610
3400.988748	444624.032821	51.456615
3400.520031	444180.752550	51.461620
3399.901697	443752.105869	51.466625
3399.119510	443324.847896	51.471629
3398.581576	442894.041299	51.476634
3397.830129	442473.717351	51.481639
3397.026630	442038.267502	51.486644
3396.384210	441602.479768	51.491649
3395.581578	441183.461296	51.496653
3394.678469	440750.846792	51.501658
3393.724631	440329.908508	51.506663
3393.315003	439901.617441	51.511668
3392.619279	439488.086394	51.516673
3392.079043	439064.319572	51.521677
3391.463515	438637.536656	51.526682
3390.481071	438233.726599	51.531687
3389.907965	437806.618015	51.536692
3389.702811	437384.724054	51.541697
3388.544827	436964.928317	51.546701
3387.837904	436551.654605	51.551706
3387.427058	436129.695788	51.556711
3386.713216	435703.817400	51.561716
3385.866729	435291.890510	51.566721
3385.131342	434876.207298	51.571725
3384.585693	434450.915844	51.576730
3383.730008	434038.081382	51.581735
3382.958770	433611.872155	51.586740
3382.352672	433200.025582	51.591745
3381.939675	432790.553883	51.596749
3381.268764	432365.526716	51.601754
3380.325421	431952.647019	51.606759
3379.917844	431527.386621	51.611764
3378.944354	431105.458843	51.616769
3378.112524	430704.983464	51.621773
3377.613357	430284.973295	51.626778
3376.525675	429879.142449	51.631783
3375.969416	429461.159461	51.636788
3375.637829	429058.141918	51.641793
3374.637207	428648.596139	51.646797
3373.958394	428237.850345	51.651802
3373.029804	427835.010051	51.656807
3372.427899	427417.560500	51.661812
3371.474914	427021.644586	51.666817
3370.601511	426623.195989	51.671821
3370.515030	426216.540951	51.676826
3369.624034	425821.664063	51.681831
3369.124823	425425.855898	51.686836
3368.140812	425023.845390	51.691841
3367.567543	424622.551263	51.696845
3367.209422	424219.617063	51.701850
3365.906727	423823.963262	51.706855
3365.327311	423426.944767	51.711860
3364.677299	423035.011522	51.716865
3364.143311	422635.307389	51.721869
3363.613629	422230.669122	51.726874
3362.602053	421841.087379	51.731879
3362.275202	421432.265014	51.736884
3361.465009	421052.089388	51.741889
3360.678586	420657.425902	51.746893
3360.000870	420250.572096	51.751898
3359.065614	419861.534672	51.756903
3358.302040	419462.024192	51.761908
3357.612028	419078.576473	51.766913
3356.836285	418689.929390	51.771917
3356.562955	418289.283153	51.776922
3355.333404	417904.202712	51.781927
3354.888763	417514.445514	51.786932
3354.333316	417143.245944	51.791937
3353.821075	416747.086921	51.796941
3353.111570	416359.693062	51.801946
3352.369819	415980.352686	51.806951
3351.978658	415584.260039	51.811956
3351.248316	415192.077362	51.816961
3350.434414	414798.378160	51.821965
3349.788698	414404.545375	51.826970
3349.272667	414016.073123	51.831975
3348.269819	413620.787153	51.836980
3347.853063	413248.956507	51.841985
3347.205140	412843.313584	51.846989
3346.185196	412456.246940	51.851994
3345.379020	412077.170696	51.856999
3345.005128	411685.977114	51.862004
3344.189907	411300.692421	51.867009
3343.364515	410918.174042	51.872013
3343.065519	410523.294229	51.877018
3342.211042	410141.837729	51.882023
3341.709536	409752.316033	51.887028
3340.989630	409367.550360	51.892033
3340.158296	408982.060450	51.897037
3339.805685	408584.292084	51.902042
3338.694557	408216.879281	51.907047
3338.380249	407812.335023	51.912052
3337.794549	407424.829689	51.917057
3336.873853	407048.249366	51.922061
3336.484598	406657.628224	51.927066
3335.661797	406266.867372	51.932071
3334.636045	405869.500509	51.937076
3334.079469	405491.369515	51.942081
3333.242982	405108.093516	51.947085
3332.826564	404722.281071	51.952090
3331.514828	404349.262442	51.957095
3330.891582	403964.312062	51.962100
3330.414943	403588.153212	51.967105
3329.632610	403221.569421	51.972109
3329.315055	402841.309850	51.977114
3328.414768	402472.524760	51.982119
3327.666603	402082.665677	51.987124
3327.094675	401706.677465	51.992129
3326.277958	401329.605147	51.997133
3325.704681	400957.573559	52.002138
3325.236875	400578.835878	52.007143
3324.469371	400202.505109	52.012148
3323.966444	399827.017786	52.017153
3322.854143	399453.757734	52.022157
3322.359051	399077.167460	52.027162
3321.785128	398701.729213	52.032167
3320.976262	398326.120453	52.037172
3320.531158	397945.924975	52.042177
3319.734646	397578.186131	52.047181
3319.044776	397196.902205	52.052186
3318.246546	396834.315880	52.057191
3317.762674	396453.422993	52.062196
3317.295816	396070.794357	52.067201
3316.146485	395689.870898	52.072205
3315.807194	395317.026528	52.077210
3315.267057	394954.989142	52.082215
3314.561377	394579.372608	52.087220
3313.692288	394192.006646	52.092225
3312.954773	393822.895196	52.097229
3312.538639	393444.423689	52.102234
3311.419906	393076.686516	52.107239
3310.856132	392709.391538	52.112244
3310.075162	392335.313108	52.117249
3309.324034	391964.734580	52.122253
3308.887525	391591.864879	52.127258
3308.385440	391229.171847	52.132263
3307.674008	390850.337201	52.137268
3306.815383	390473.784670	52.142273
3306.127163	390100.913419	52.147277
3305.565430	389724.890708	52.152282
3304.708912	389366.048483	52.157287
3304.144750	388991.823680	52.162292
3303.824808	388613.157323	52.167297
3302.917153	388252.760851	52.172301
3302.263053	387873.147808	52.177306
3301.099555	387496.255876	52.182311
3300.419454	387142.143927	52.187316
3299.781438	386764.754369	52.192321
3299.300380	386398.118036	52.197325
3298.738533	386033.092838	52.202330
3298.059164	385673.473673	52.207335
3297.177802	385317.595695	52.212340
3296.606538	384944.092943	52.217345
3295.912171	384582.558193	52.222349
3295.360469	384210.418161	52.227354
3294.416362	383843.397225	52.232359
3293.670119	383468.152516	52.237364
3293.032593	383120.454552	52.242369
3292.091915	382750.802884	52.247373
3291.983137	382391.265073	52.252378
3290.850321	382049.027108	52.257383
3290.507375	381672.429059	52.262388
3290.062757	381306.321622	52.267393
3289.079483	380953.826184	52.272397
3288.600393	380593.795828	52.277402
3287.701981	380235.430722	52.282407
3286.724399	379859.169519	52.287412
3286.178378	379512.034480	52.292417
3285.263023	379151.550978	52.297421
3285.277249	378795.393536	52.302426
3284.436488	378440.792420	52.307431
3283.720386	378075.027928	52.312436
3283.108203	377720.663924	52.317441
3281.980589	377361.214904	52.322445
3281.821082	376997.641543	52.327450
3280.752994	376651.733790	52.332455
3280.374730	376286.357155	52.337460
3279.602721	375930.730651	52.342465
3279.008695	375572.300270	52.347469
3278.396841	375209.901402	52.352474
3277.516683	374858.810254	52.357479
3276.899136	374500.628452	52.362484
3276.511970	374131.697946	52.367489
3275.724751	373779.565289	52.372493
3275.149613	373415.007872	52.377498
3274.034112	373058.214970	52.382503
3273.618096	372691.285684	52.387508
3272.789540	372334.797284	52.392513
3271.957166	371987.896799	52.397517
3271.932231	371630.410337	52.402522
3271.027461	371280.030307	52.407527
3270.386684	370919.811473	52.412532
3269.786687	370562.941128	52.417537
3268.950318	370201.271621	52.422541
3268.639878	369837.556966	52.427546
3267.633871	369481.276005	52.432551
3267.020112	369119.994601	52.437556
3266.404937	368764.027465	52.442561
3265.561027	368407.508439	52.447565
3265.147336	368041.556139	52.452570
3264.368244	367686.114897	52.457575
3263.521356	367324.651873	52.462580
3263.198883	366970.989811	52.467585
3262.388911	366611.779383	52.472589
3261.718528	366251.628039	52.477594
3260.606775	365895.716116	52.482599
3260.122180	365537.972052	52.487604
3259.154592	365178.622315	52.492609
3258.362134	364838.451338	52.497613
3257.971323	364476.460464	52.502618
3256.973426	364135.248078	52.507623
3256.350380	363789.419456	52.512628
3255.627378	363445.206970	52.517633
3254.834402	363098.280476	52.522637
3254.637205	362748.331053	52.527642
3253.947792	362403.825565	52.532647
3253.474290	362058.418248	52.537652
3252.453671	361716.300931	52.542657
3251.756227	361361.229489	52.547661
3251.125758	361006.475545	52.552666
3250.702970	360662.016798	52.557671
3250.005243	360315.614298	52.562676
3249.282413	359966.795916	52.567681
3248.708185	359616.628294	52.572685
3248.137508	359261.088464	52.577690
3247.098168	358922.134641	52.582695
3246.191837	358571.324887	52.587700
3245.732616	358227.108825	52.592705
3244.715128	357886.693846	52.597709
3244.295078	357541.932365	52.602714
3243.504234	357202.672769	52.607719
3242.957662	356861.234630	52.612724
3242.285363	356520.017601	52.617729
3241.452720	356183.429586	52.622733
3241.175029	355824.026741	52.627738
3240.434988	355490.015064	52.632743
3239.915823	355143.114980	52.637748
3239.359762	354804.081837	52.642753
3238.149487	354463.190400	52.647757
3237.421408	354109.826962	52.652762
3236.982294	353775.680035	52.657767
3236.233481	353430.356977	52.662772
3235.635253	353085.084132	52.667777
3234.853399	352757.601578	52.672781
3234.292695	352406.057775	52.677786
3233.613091	352076.009825	52.682791
3232.744874	351725.171787	52.687796
3232.338231	351381.689752	52.692801
3231.408471	351048.264659	52.697805
3230.989170	350712.593452	52.702810
3230.107342	350371.037928	52.707815
3229.664991	350026.687496	52.712820
3228.774866	349693.298592	52.717825
3228.281729	349355.747245	52.722829
3227.611479	349010.332018	52.727834
3227.166293	348685.468975	52.732839
3226.007941	348329.971669	52.737844
3225.891158	347998.664336	52.742849
3224.929056	347659.980532	52.747853
3224.543952	347316.163930	52.752858
3223.705035	346979.212674	52.757863
3222.990307	346629.819134	52.762868
3222.186092	346287.080622	52.767873
3220.992616	345953.920814	52.772877
3221.353095	345611.197580	52.777882
3220.331657	345276.530354	52.782887
3219.628915	344937.458324	52.787892
3219.140415	344591.070856	52.792897
3218.133110	344247.665060	52.797901
3217.316804	343911.303037	52.802906
3216.737265	343582.155852	52.807911
3216.241886	343234.208777	52.812916
3215.423556	342899.673956	52.817921
3214.400324	342571.609498	52.822925
3214.434163	342228.918126	52.827930
3213.300090	341898.169394	52.832935
3212.724499	341556.130605	52.837940
3211.926838	341220.030451	52.842945
3211.349916	340890.766254	52.847949
3211.217326	340553.768123	52.852954
3209.921138	340219.701369	52.857959
3209.510564	339886.154526	52.862964
3208.483650	339547.332380	52.867969
3207.815408	339223.750257	52.872973
3207.508713	338887.661585	52.877978
3206.741064	338550.396736	52.882983
3206.106013	338222.680442	52.887988
3205.457907	337886.945961	52.892993
3204.626961	337545.129232	52.897997
3204.034279	337209.484272	52.903002
3203.083172	336894.921089	52.908007
3202.841489	336549.467475	52.913012
3202.189092	336217.110721	52.918017
3201.538027	335886.534040	52.923021
3200.901079	335542.792367	52.928026
3200.254312	335223.412654	52.933031
3199.524799	334874.590826	52.938036
3198.655764	334542.540025	52.943041
3198.090889	334212.221476	52.948045
3197.625474	333878.448852	52.953050
3196.462648	333542.901095	52.958055
3195.914447	333211.353127	52.963060
3195.717303	332879.977147	52.968065
3194.647164	332544.944505	52.973069
3194.085863	332213.673899	52.978074
3193.667300	331878.458613	52.983079
3192.634980	331542.396899	52.988084
3191.907969	331216.417696	52.993089
3191.181043	330887.789323	52.998093
3190.807623	330546.756136	53.003098
3189.998594	330231.961754	53.008103
3189.716366	329892.413133	53.013108
3188.789726	329554.263306	53.018113
3187.896565	329226.061099	53.023117
3187.530673	328888.812412	53.028122
3186.881367	328549.417556	53.033127
3186.154977	328220.038882	53.038132
3185.483190	327888.817056	53.043137
3184.502050	327560.010475	53.048141
3184.543784	327223.122686	53.053146
3183.354825	326887.599304	53.058151
3182.756929	326549.969619	53.063156
3181.935218	326224.798362	53.068161
3181.256262	325896.904404	53.073165
3180.514213	325563.519667	53.078170
3180.153537	325233.586713	53.083175
3179.434126	324902.563445	53.088180
3178.433417	324581.385625	53.093185
3177.641490	324253.477358	53.098189
3177.532848	323911.940022	53.103194
3176.479834	323607.494339	53.108199
3175.653748	323268.817630	53.113204
3174.945356	322933.787310	53.118209
3174.301791	322616.160796	53.123213
3173.993945	322287.098808	53.128218
3172.929264	321961.847192	53.133223
3172.436447	321643.913122	53.138228
3171.926878	321317.247238	53.143233
3170.868885	320993.900526	53.148237
3170.550455	320663.841019	53.153242
3169.557979	320351.175480	53.158247
3169.144556	320022.274387	53.163252
3168.798217	319694.710953	53.168257
3167.813035	319375.446195	53.173261
3167.401832	319045.089841	53.178266
3166.512599	318714.400537	53.183271
3165.775696	318380.350375	53.188276
3164.666442	318069.070405	53.193281
3164.349315	317752.240540	53.198285
3163.953825	317422.741638	53.203290
3163.097589	317098.330644	53.208295
3162.426148	316778.217975	53.213300
3161.675750	316455.188507	53.218305
3160.952667	316138.162892	53.223309
3160.523044	315811.133771	53.228314
3159.548708	315495.775468	53.233319
3159.065176	315164.525863	53.238324
3158.549754	314840.537237	53.243329
3157.807672	314519.486256	53.248333
3157.078011	314200.469369	53.253338
3156.216580	313871.388791	53.258343
3155.489900	313552.929619	53.263348
3154.693649	313229.973413	53.268353
3153.972130	312932.137097	53.273357
3153.599383	312609.952277	53.278362
3152.837965	312295.518082	53.283367
3152.056346	311973.166871	53.288372
3151.027640	311656.303105	53.293377
3150.536916	311349.920895	53.298381
3150.050014	311027.647579	53.303386
3149.454026	310718.428290	53.308391
3148.360661	310407.351567	53.313396
3148.272377	310095.732974	53.318401
3147.031546	309788.293834	53.323405
3146.444119	309469.291437	53.328410
3145.912188	309165.379889	53.333415
3145.291669	308849.156673	53.338420
3144.717219	308545.250251	53.343425
3143.621868	308232.207229	53.348429
3143.358943	307917.401913	53.353434
3142.711500	307612.944462	53.358439
3142.133538	307292.279524	53.363444
3141.561681	306988.266937	53.368449
3140.579673	306674.081537	53.373453
3139.929570	306352.839906	53.378458
3139.535506	306044.111315	53.383463
3138.738030	305725.743539	53.388468
3138.066386	305419.476587	53.393473
3137.308342	305117.806370	53.398477
3136.874535	304793.521735	53.403482
3136.059820	304482.360419	53.408487
3135.302429	304174.041464	53.413492
3135.016756	303860.910551	53.418497
3134.395710	303537.391055	53.423501
3133.445010	303223.880098	53.428506
3132.548399	302922.532555	53.433511
3132.102435	302616.707460	53.438516
3131.604915	302291.739487	53.443521
3130.618035	301992.034105	53.448525
3130.203739	301675.506306	53.453530
3129.453587	301360.711749	53.458535
3129.164994	301043.831665	53.463540
3128.262318	300737.209122	53.468545
3127.747685	300421.152978	53.473549
3126.909634	300105.682169	53.478554
3126.217323	299796.757988	53.483559
3125.520043	299476.425046	53.488564
3124.879091	299162.958502	53.493569
3124.022032	298855.484722	53.498573
3123.607398	298534.468550	53.503578
3122.807836	298228.308780	53.508583
3121.951287	297916.300150	53.513588
3121.368330	297604.043925	53.518593
3120.854240	297294.806788	53.523597
3120.418450	296973.663732	53.528602
3119.348824	296658.044847	53.533607
3118.693013	296357.054313	53.538612
3118.261290	296041.766354	53.543617
3117.417101	295730.668789	53.548621
3116.945625	295414.367397	53.553626
3116.110211	295113.989049	53.558631
3115.286538	294798.990281	53.563636
3114.829683	294491.496696	53.568641
3113.799565	294182.412536	53.573645
3113.149689	293873.751610	53.578650
3112.576317	293567.268301	53.583655
3111.909578	293249.440924	53.588660
3111.354353	292946.417401	53.593665
3110.315292	292648.410695	53.598669
3109.814883	292341.277425	53.603674
3109.360944	292040.146691	53.608679
3108.269396	291734.557801	53.613684
3107.721777	291435.198361	53.618689
3106.863116	291132.908074	53.623693
3106.616989	290825.707104	53.628698
3105.738388	290531.543374	53.633703
3105.128450	290226.232908	53.638708
3104.706464	289919.033195	53.643713
3103.921835	289610.693534	53.648717
3103.261558	289303.378011	53.653722
3102.280106	289004.084366	53.658727
3102.241136	288696.848108	53.663732
3101.602451	288388.407574	53.668737
3100.691096	288083.957374	53.673741
3100.046384	287778.980772	53.678746
3099.113486	287474.991784	53.683751
3098.607478	287168.235340	53.688756
3097.792629	286862.826341	53.693761
3097.203144	286577.119026	53.698765
3096.782548	286261.561775	53.703770
3095.909252	285956.339470	53.708775
3095.133426	285652.451276	53.713780
3094.774209	285348.089400	53.718785
3093.676717	285055.533945	53.723789
3092.953296	284746.772317	53.728794
3092.467586	284450.987006	53.733799
3091.735480	284144.034516	53.738804
3090.996529	283839.884373	53.743809
3090.201653	283542.823003	53.748813
3089.821367	283227.486095	53.753818
3088.884036	282932.255106	53.758823
3088.236353	282634.431272	53.763828
3087.765647	282334.261640	53.768833
3086.985180	282043.818775	53.773837
3086.376902	281745.657095	53.778842
3085.688689	281443.611265	53.783847
3084.938606	281141.880686	53.788852
3084.387855	280845.594080	53.793857
3083.399224	280555.565427	53.798861
3083.155585	280258.618702	53.803866
3082.134332	279968.161996	53.808871
3081.557767	279668.084178	53.813876
3081.139159	279372.998497	53.818881
3080.147670	279075.354675	53.823885
3079.575188	278774.791977	53.828890
3078.590693	278481.094438	53.833895
3077.982496	278190.469857	53.838900
3077.788474	277900.441819	53.843905
3077.148151	277600.424343	53.848909
3076.336050	277307.539656	53.853914
3075.581415	277016.606874	53.858919
3075.130045	276725.753377	53.863924
3074.677284	276437.013925	53.868929
3073.998514	276128.368459	53.873933
3073.567200	275823.554977	53.878938
3072.463333	275526.488426	53.883943
3071.691306	275224.708610	53.888948
3071.207903	274928.766288	53.893953
3070.461215	274639.742090	53.898957
3069.951482	274335.730433	53.903962
3069.493796	274044.393796	53.908967
3068.711886	273732.377212	53.913972
3068.231123	273432.461396	53.918977
3067.224552	273137.034856	53.923981
3066.915771	272823.364402	53.928986
3065.696983	272528.837434	53.933991
3064.841894	272224.855104	53.938996
3064.629698	271932.129957	53.944001
3063.597928	271645.901676	53.949005
3063.170283	271350.129061	53.954010
3062.283773	271048.342201	53.959015
3061.764981	270757.499539	53.964020
3061.025963	270460.120973	53.969025
3060.381532	270164.612176	53.974029
3059.858762	269865.926136	53.979034
3058.866638	269576.508549	53.984039
3058.389785	269281.482874	53.989044
3057.638499	268986.322466	53.994049
3056.998843	268701.917590	53.999053
3056.237851	268406.962691	54.004058
3055.754295	268115.173006	54.009063
3055.080935	267820.000745	54.014068
3054.441924	267525.179740	54.019073
3053.458055	267241.008252	54.024077
3053.174897	266944.144686	54.029082
3052.507412	266656.510668	54.034087
3051.364007	266362.890706	54.039092
3050.852993	266063.516874	54.044097
3050.103150	265779.512863	54.049101
3049.617365	265489.889697	54.054106
3049.116390	265202.459374	54.059111
3048.046312	264908.242926	54.064116
3047.810865	264617.383693	54.069121
3046.688704	264330.154144	54.074125
3046.361325	264031.542106	54.079130
3045.654339	263741.980598	54.084135
3044.850291	263456.229408	54.089140
3044.476560	263160.961686	54.094145
3043.356229	262880.481944	54.099149
3042.935718	262584.789140	54.104154
3042.112674	262311.444756	54.109159
3041.487659	262008.806599	54.114164
3041.177113	261718.801952	54.119169
3040.207220	261431.321383	54.124173
3039.718052	261148.170917	54.129178
3039.022685	260851.810075	54.134183
3037.865516	260566.652054	54.139188
3037.657545	260287.227111	54.144193
3036.827493	259994.275657	54.149197
3036.519525	259705.444034	54.154202
3035.663888	259427.293968	54.159207
3034.881572	259137.137299	54.164212
3034.298463	258842.390699	54.169217
3033.295792	258557.974294	54.174221
3032.900193	258270.049445	54.179226
3032.322563	257989.106380	54.184231
3031.303402	257698.785067	54.189236
3031.009367	257418.536313	54.194241
3030.274327	257133.162328	54.199245
3029.805015	256848.408773	54.204250
3028.561803	256558.735522	54.209255
3028.227805	256279.105662	54.214260
3027.665138	255985.632636	54.219265
3026.842888	255708.754845	54.224269
3026.209681	255424.996777	54.229274
3025.140086	255136.724054	54.234279
3024.678140	254844.637316	54.239284
3024.130387	254562.675038	54.244289
3023.333471	254285.947885	54.249293
3023.178881	253996.385868	54.254298
3022.111552	253721.765126	54.259303
3021.744522	253437.330963	54.264308
3021.460843	253141.449332	54.269313
3020.179081	252862.381547	54.274317
3019.586059	252565.760296	54.279322
3018.908064	252291.258222	54.284327
3018.059438	252001.452520	54.289332
3017.422341	251723.048389	54.294337
3016.426315	251446.484178	54.299341
3016.180278	251152.280559	54.304346
3015.365890	250882.564488	54.309351
3014.720169	250597.694943	54.314356
3014.325510	250314.161320	54.319361
3013.315839	250040.020824	54.324365
3012.677318	249751.204235	54.329370
3012.032404	249476.497587	54.334375
3011.408038	249192.747560	54.339380
3010.718957	248911.784107	54.344385
3009.576600	248643.778874	54.349389
3009.369705	248354.030575	54.354394
3008.407556	248088.085989	54.359399
3008.003053	247806.264524	54.364404
3007.560341	247526.817976	54.369409
3006.630285	247256.438629	54.374413
3005.999760	246971.980541	54.379418
3005.370356	246698.447740	54.384423
3004.661244	246411.940415	54.389428
3004.091380	246147.261371	54.394433
3003.151466	245872.938890	54.399437
3003.038045	245581.653175	54.404442
3002.099301	245311.253324	54.409447
3001.130212	245035.740182	54.414452
3000.934057	244758.781004	54.419457
2999.764620	244482.129256	54.424461
2999.022880	244201.590519	54.429466
2998.614196	243929.326862	54.434471
2998.166095	243653.071915	54.439476
2997.545587	243381.912453	54.444481
2996.525505	243106.131177	54.449485
2996.267910	242827.657772	54.454490
2995.358495	242545.086388	54.459495
2994.590499	242265.268943	54.464500
2994.279700	241982.884145	54.469505
2993.455814	241719.629095	54.474509
2992.533993	241440.754568	54.479514
2991.996980	241172.464108	54.484519
2991.015259	240891.002873	54.489524
2990.669639	240609.670765	54.494529
2989.793677	240338.940235	54.499533
2989.640679	240060.991191	54.504538
2988.552046	239788.895012	54.509543
2988.019139	239522.619271	54.514548
2987.724994	239241.536880	54.519553
2986.847061	238973.203452	54.524557
2986.135117	238691.195421	54.529562
2985.486992	238415.951506	54.534567
2984.835777	238128.995155	54.539572
2984.302620	237860.609753	54.544577
2983.273115	237599.306230	54.549581
2982.764944	237309.477336	54.554586
2982.125317	237031.485344	54.559591
2981.203236	236772.713176	54.564596
2980.903338	236496.604023	54.569601
2980.154965	236211.195868	54.574605
2979.438099	235943.659083	54.579610
2979.004545	235666.962091	54.584615
2978.086764	235392.888854	54.589620
2977.669052	235105.445152	54.594625
2976.821125	234837.193479	54.599629
2976.470716	234552.490713	54.604634
2975.676382	234285.683406	54.609639
2974.564115	234003.572735	54.614644
2974.113454	233728.233185	54.619649
2973.590200	233464.491639	54.624653
2972.682110	233173.286065	54.629658
2971.910990	232911.087550	54.634663
2971.593557	232637.003071	54.639668
2970.968116	232354.030636	54.644673
2969.448767	232097.172659	54.649677
2969.419146	231810.237120	54.654682
2968.707770	231547.116155	54.659687
2967.982614	231275.238948	54.664692
2966.996330	231001.672409	54.669697
2966.457672	230741.148974	54.674701
2965.846180	230472.413432	54.679706
2965.348568	230202.056506	54.684711
2964.591518	229929.347991	54.689716
2964.196686	229662.210079	54.694721
2963.554237	229401.299446	54.699725
2963.309806	229112.521988	54.704730
2962.173069	228841.200865	54.709735
2961.274261	228572.669160	54.714740
2960.546293	228297.567527	54.719745
2959.595933	228022.654727	54.724749
2959.292907	227760.243810	54.729754
2958.484408	227499.339557	54.734759
2957.701801	227233.899837	54.739764
2957.413736	226960.184047	54.744769
2956.471437	226700.219991	54.749773
2955.921476	226423.492012	54.754778
2955.213526	226159.113157	54.759783
2954.520794	225887.450840	54.764788
2953.945686	225626.769936	54.769793
2953.114703	225363.418763	54.774797
2952.625734	225092.057749	54.779802
2951.871793	224826.137260	54.784807
2950.973731	224566.070947	54.789812
2950.510998	224301.009900	54.794817
2949.935195	224045.833573	54.799821
2949.217668	223765.130921	54.804826
2948.833012	223499.079898	54.809831
2948.037401	223240.847479	54.814836
2947.385319	222972.625499	54.819841
2946.730631	222707.727380	54.824845
2946.034550	222434.294862	54.829850
2945.394433	222175.710307	54.834855
2944.630170	221901.552099	54.839860
2944.286639	221631.236312	54.844865
2943.589231	221371.823320	54.849869
2943.227160	221096.815023	54.854874
2942.373768	220822.152830	54.859879
2941.426787	220546.793580	54.864884
2940.875367	220276.197235	54.869889
2940.219235	220014.185467	54.874893
2939.821695	219727.361928	54.879898
2939.057653	219466.807597	54.884903
2938.337298	219189.253412	54.889908
2937.695883	218917.581490	54.894913
2937.026029	218652.432514	54.899917
2936.092343	218377.180993	54.904922
2935.204422	218111.419308	54.909927
2934.762622	217845.664332	54.914932
2934.055785	217567.223105	54.919937
2933.320201	217309.014115	54.924941
2932.939506	217043.379713	54.929946
2931.948331	216778.364856	54.934951
2931.325273	216505.426176	54.939956
2930.723512	216236.163845	54.944961
2929.935511	215976.707832	54.949965
2929.330101	215709.204688	54.954970
2928.654668	215443.139285	54.959975
2927.940783	215185.532886	54.964980
2926.939364	214920.348479	54.969985
2926.349987	214663.258922	54.974989
2926.040246	214396.719605	54.979994
2925.370123	214136.513576	54.984999
2924.432302	213876.516403	54.990004
2923.886054	213607.064619	54.995009
2923.038769	213346.724212	55.000013
2922.508783	213085.430861	55.005018
2921.909816	212829.673544	55.010023
2921.080052	212564.878503	55.015028
2920.594185	212307.997930	55.020033
2919.956395	212049.296831	55.025037
2919.437711	211780.993619	55.030042
2918.811312	211525.220253	55.035047
2917.821225	211269.480026	55.040052
2917.335578	210994.008954	55.045057
2916.557851	210736.798948	55.050061
2916.118464	210482.031055	55.055066
2915.335784	210231.709631	55.060071
2914.430149	209953.343954	55.065076
2914.214804	209698.938274	55.070081
2913.418909	209440.921801	55.075085
2912.780894	209171.286542	55.080090
2911.798585	208907.001620	55.085095
2911.331041	208647.650933	55.090100
2910.548538	208383.247500	55.095105
2909.733007	208128.548691	55.100109
2909.295156	207861.420162	55.105114
2908.650093	207610.069245	55.110119
2907.942427	207343.889331	55.115124
2907.335397	207080.316439	55.120129
2906.678128	206829.199761	55.125133
2905.817845	206564.816497	55.130138
2905.259061	206313.266375	55.135143
2904.579661	206059.140110	55.140148
2903.981414	205792.376991	55.145153
2903.431698	205535.928847	55.150157
2902.696172	205277.347681	55.155162
2901.861137	205023.301392	55.160167
2901.324354	204753.580614	55.165172
2900.660611	204498.465879	55.170177
2899.464193	204254.928695	55.175181
2899.129519	203979.681604	55.180186
2898.410343	203731.044070	55.185191
2897.929874	203475.624815	55.190196
2897.500165	203223.354785	55.195201
2896.424503	202972.142625	55.200205
2896.080768	202696.775828	55.205210
2895.601045	202452.852786	55.210215
2894.864160	202192.007614	55.215220
2894.022483	201933.623639	55.220225
2893.175815	201674.618065	55.225229
2892.801094	201412.815597	55.230234
2891.956978	201166.347007	55.235239
2890.872618	200908.858816	55.240244
2890.675494	200645.237483	55.245249
2890.041687	200390.887234	55.250253
2889.591591	200127.333879	55.255258
2888.541786	199873.624548	55.260263
2887.848257	199617.760260	55.265268
2887.679369	199352.969894	55.270273
2886.806802	199107.443971	55.275277
2886.214398	198845.866315	55.280282
2885.616077	198585.067103	55.285287
2884.610383	198328.240306	55.290292
2883.914185	198075.832253	55.295297
2883.220091	197822.763352	55.300301
2883.015294	197557.567556	55.305306
2881.693116	197301.928339	55.310311
2881.347222	197050.729438	55.315316
2880.829663	196795.550588	55.320321
2880.029713	196537.147427	55.325325
2879.343626	196273.879386	55.330330
2878.864777	196027.503647	55.335335
2878.067427	195775.898803	55.340340
2877.443792	195506.262447	55.345345
2876.701630	195250.465039	55.350349
2876.277831	194995.700055	55.355354
2875.600128	194741.829073	55.360359
2874.723973	194485.509540	55.365364
2873.791999	194223.652374	55.370369
2873.292598	193973.167061	55.375373
2872.558707	193718.750202	55.380378
2871.718950	193464.669488	55.385383
2871.465443	193205.267659	55.390388
2870.589683	192959.745694	55.395393
2870.120095	192706.971638	55.400397
2869.363248	192453.340965	55.405402
2868.737420	192197.196986	55.410407
2867.907446	191942.206338	55.415412
2867.441592	191684.423768	55.420417
2866.364993	191442.656378	55.425421
2866.350456	191174.740698	55.430426
2865.499806	190921.488990	55.435431
2864.762754	190680.142345	55.440436
2864.085164	190422.438103	55.445441
2863.401726	190164.150886	55.450445
2863.045499	189902.886907	55.455450
2862.258747	189646.756294	55.460455
2861.478356	189398.641509	55.465460
2861.210553	189132.596583	55.470465
2860.162247	188889.018051	55.475469
2859.601433	188629.612760	55.480474
2859.056832	188375.893362	55.485479
2858.300070	188119.740729	55.490484
2857.494545	187856.192672	55.495489
2856.754651	187604.747508	55.500493
2856.203487	187349.024506	55.505498
2855.316121	187096.078728	55.510503
2854.766921	186838.653404	55.515508
2854.406706	186583.489569	55.520513
2853.389138	186335.657424	55.525517
2853.131038	186080.162127	55.530522
2852.252264	185824.321271	55.535527
2851.253536	185568.767994	55.540532
2850.720178	185315.101601	55.545537
2849.812988	185070.210252	55.550541
2849.759969	184808.341359	55.555546
2848.700469	184564.252873	55.560551
2848.217586	184314.782192	55.565556
2847.633863	184053.650499	55.570561
2846.894886	183804.706606	55.575565
2846.193514	183548.570554	55.580570
2845.199118	183295.993451	55.585575
2844.705703	183044.864974	55.590580
2844.514674	182784.823366	55.595585
2843.355672	182532.798215	55.600589
2842.814771	182273.616435	55.605594
2842.200812	182027.473984	55.610599
2841.276926	181778.379865	55.615604
2841.098491	181515.023562	55.620609
2840.038312	181267.683948	55.625613
2839.620768	181017.572610	55.630618
2839.058620	180762.893477	55.635623
2838.178307	180503.267068	55.640628
2837.574621	180256.725875	55.645633
2836.712646	180008.395261	55.650637
2836.225368	179754.969496	55.655642
2835.642057	179500.886259	55.660647
2834.776893	179246.073236	55.665652
2834.160984	178993.511857	55.670657
2833.435019	178748.944829	55.675661
2832.688261	178502.499949	55.680666
2832.076779	178253.961737	55.685671
2831.648352	178003.386263	55.690676
2830.818352	177748.894616	55.695681
2830.050578	177503.451007	55.700685
2829.535150	177249.891956	55.705690
2828.746989	176999.443021	55.710695
2827.982337	176756.852437	55.715700
2827.642729	176510.329269	55.720705
2826.759817	176260.459419	55.725709
2826.383690	176001.238539	55.730714
2825.653974	175749.210683	55.735719
2824.758896	175489.451967	55.740724
2824.313545	175246.934099	55.745729
2823.585921	174996.169684	55.750733
2822.981083	174740.172659	55.755738
2822.274529	174497.815057	55.760743
2821.570213	174250.816245	55.765748
2820.984499	173983.501371	55.770753
2820.037639	173748.715657	55.775757
2819.432196	173492.408605	55.780762
2818.800364	173247.744596	55.785767
2818.031247	173001.323266	55.790772
2817.792123	172746.870660	55.795777
2816.830747	172503.255390	55.800781
2816.448400	172254.157463	55.805786
2815.758884	172000.544017	55.810791
2814.846832	171750.884521	55.815796
2814.425636	171498.300071	55.820801
2813.770202	171259.209617	55.825805
2813.125954	170994.988894	55.830810
2812.395556	170746.031863	55.835815
2811.899100	170497.891417	55.840820
2811.272210	170241.405193	55.845825
2810.407042	169988.799001	55.850829
2809.970608	169728.470796	55.855834
2808.917373	169474.231775	55.860839
2807.926476	169244.604667	55.865844
2807.529546	168992.464886	55.870849
2806.780942	168744.070337	55.875853
2806.347553	168497.420519	55.880858
2805.506345	168257.703888	55.885863
2804.857107	168001.757393	55.890868
2804.715059	167742.006328	55.895873
2803.910204	167500.139585	55.900877
2803.163095	167244.480705	55.905882
2802.400304	167003.144540	55.910887
2801.505869	166753.425363	55.915892
2801.229771	166497.760481	55.920897
2800.402881	166251.530844	55.925901
2799.988286	165999.756940	55.930906
2798.992161	165752.985153	55.935911
2798.450098	165507.923270	55.940916
2798.053788	165254.282251	55.945921
2796.768744	165014.491142	55.950925
2796.182269	164755.492223	55.955930
2795.710722	164508.162374	55.960935
2794.803621	164262.607021	55.965940
2794.164617	164029.052178	55.970945
2793.385385	163779.347321	55.975949
2792.808161	163524.627843	55.980954
2792.562575	163289.540415	55.985959
2791.659047	163042.390536	55.990964
2791.164914	162787.752013	55.995969
2790.220407	162543.510979	56.000973
2789.525954	162297.655353	56.005978
2788.846370	162051.951608	56.010983
2788.085798	161803.007448	56.015988
2788.016627	161567.674313	56.020993
2787.075447	161331.031411	56.025997
2786.779365	161009.369595	56.031002
2785.917167	160762.025276	56.036007
2784.964054	160512.001690	56.041012
2784.910283	160261.532252	56.046017
2783.916174	160015.701518	56.051021
2783.109540	159757.256157	56.056026
2782.265126	159508.201347	56.061031
2781.558798	159267.199537	56.066036
2780.793542	159021.657271	56.071041
2780.146172	158770.059168	56.076045
2779.883290	158522.826187	56.081050
2779.405074	158285.100410	56.086055
2778.376982	158040.458407	56.091060
2778.153962	157777.549057	56.096065
2777.256968	157537.695335	56.101069
2776.487856	157289.229104	56.106074
2775.850163	157046.312025	56.111079
2775.236840	156792.294607	56.116084
2774.768220	156541.955493	56.121089
2774.076925	156292.111116	56.126093
2773.186582	156047.270633	56.131098
2772.656516	155797.480574	56.136103
2771.769262	155546.719224	56.141108
2771.453804	155298.589523	56.146113
2770.499094	155055.596859	56.151117
2769.870309	154794.833832	56.156122
2769.404864	154552.949453	56.161127
2768.775376	154305.855532	56.166132
2768.072380	154041.690572	56.171137
2767.297370	153802.898668	56.176141
2766.546334	153533.457271	56.181146
2765.980550	153300.063580	56.186151
2765.436031	153055.863536	56.191156
2764.746550	152810.925561	56.196161
2764.098569	152552.229383	56.201165
2763.294558	152308.940245	56.206170
2762.493963	152061.114543	56.211175
2761.725891	151811.874631	56.216180
2761.664691	151565.168437	56.221185
2760.363382	151321.711088	56.226189
2759.671569	151070.913966	56.231194
2759.100333	150831.361100	56.236199
2758.514729	150583.359866	56.241204
2758.262229	150340.658748	56.246209
2757.187388	150099.792861	56.251213
2756.534786	149845.656094	56.256218
2755.928855	149600.143976	56.261223
2755.667654	149349.863728	56.266228
2754.983686	149089.751465	56.271233
2753.703431	148842.216647	56.276237
2753.369500	148595.741208	56.281242
2752.664625	148349.072222	56.286247
2751.640048	148101.388179	56.291252
2751.309781	147853.151219	56.296257
2750.300304	147610.310798	56.301261
2750.123060	147365.065440	56.306266
2749.166164	147124.419039	56.311271
2748.457896	146873.491688	56.316276
2747.825023	146627.955603	56.321281
2747.067781	146396.471521	56.326285
2746.191718	146153.011019	56.331290
2745.694652	145910.115058	56.336295
2744.902600	145663.404334	56.341300
2744.798035	145423.271191	56.346305
2743.875089	145180.994757	56.351309
2743.067773	144939.807473	56.356314
2742.056201	144695.223233	56.361319
2741.306549	144466.153906	56.366324
2740.940381	144221.382155	56.371329
2740.159306	143993.350600	56.376333
2740.204099	143748.530150	56.381338
2739.567067	143503.082606	56.386343
2738.635303	143265.422524	56.391348
2737.787457	143018.347534	56.396353
2737.102582	142778.682430	56.401357
2736.832220	142536.717054	56.406362
2736.144787	142293.383754	56.411367
2735.350824	142047.794712	56.416372
2734.489569	141794.009675	56.421377
2733.991754	141566.192550	56.426381
2733.177514	141311.692478	56.431386
2732.700023	141078.272138	56.436391
2732.000479	140836.337329	56.441396
2731.288166	140592.983354	56.446401
2730.575718	140350.469959	56.451405
2730.046837	140106.175970	56.456410
2729.380429	139864.421534	56.461415
2728.628131	139633.838446	56.466420
2728.064769	139384.524197	56.471425
2727.278408	139140.100928	56.476429
2726.868087	138891.821086	56.481434
2726.274208	138650.992400	56.486439
2725.029786	138399.405588	56.491444
2724.446702	138159.862387	56.496449
2723.659388	137929.513923	56.501453
2723.141198	137679.152164	56.506458
2722.526084	137447.242828	56.511463
2721.648964	137211.362063	56.516468
2721.441250	136970.231668	56.521473
2720.470596	136737.609218	56.526477
2720.052658	136494.623006	56.531482
2719.298238	136256.659563	56.536487
2718.357175	136012.591394	56.541492
2718.022061	135772.532729	56.546497
2717.063482	135543.690971	56.551501
2716.498838	135292.645367	56.556506
2716.070156	135057.155448	56.561511
2715.140596	134832.837272	56.566516
2715.062508	134575.343396	56.571521
2713.814451	134347.712922	56.576525
2713.367245	134098.767801	56.581530
2712.649060	133860.106734	56.586535
2712.282574	133624.186647	56.591540
2711.550945	133386.395446	56.596545
2710.738374	133143.486962	56.601549
2710.181760	132897.326105	56.606554
2709.522327	132659.681903	56.611559
2708.282550	132422.118919	56.616564
2708.107069	132175.637104	56.621569
2707.162828	131946.605572	56.626573
2706.529930	131715.989544	56.631578
2706.012739	131476.846439	56.636583
2705.259076	131239.152766	56.641588
2704.591145	130996.811200	56.646593
2703.849970	130781.119578	56.651597
2703.143141	130539.829655	56.656602
2702.843232	130304.421792	56.661607
2701.858532	130074.459139	56.666612
2701.437766	129823.933928	56.671617
2700.668835	129601.244408	56.676621
2700.082251	129357.786289	56.681626
2699.610970	129119.621174	56.686631
2698.763690	128884.134115	56.691636
2698.102349	128643.831256	56.696641
2697.278348	128407.074421	56.701645
2696.742078	128168.597488	56.706650
2695.847591	127932.300393	56.711655
2695.210152	127699.863693	56.716660
2694.776843	127458.950709	56.721665
2693.947167	127232.720874	56.726669
2693.436118	126989.411209	56.731674
2692.758384	126756.379207	56.736679
2692.052200	126530.592774	56.741684
2691.396833	126278.790451	56.746689
2690.639922	126047.440711	56.751693
2690.245541	125800.440100	56.756698
2689.367426	125564.592510	56.761703
2688.889327	125327.400914	56.766708
2688.140861	125087.688926	56.771713
2687.584597	124865.740421	56.776717
2686.739421	124628.473386	56.781722
2686.039404	124383.337344	56.786727
2685.083406	124147.247704	56.791732
2684.640467	123917.225113	56.796737
2683.741677	123690.121251	56.801741
2683.224502	123444.850458	56.806746
2682.723544	123210.881086	56.811751
2682.003503	122968.440475	56.816756
2681.386193	122732.068298	56.821761
2680.905063	122503.308287	56.826765
2680.136048	122262.100861	56.831770
2679.328535	122029.523684	56.836775
2678.759281	121794.612457	56.841780
2678.418484	121551.451611	56.846785
2676.986674	121315.944815	56.851789
2676.770895	121082.202850	56.856794
2676.208561	120847.527457	56.861799
2675.165490	120615.774532	56.866804
2674.601349	120391.401041	56.871809
2673.893377	120155.929546	56.876813
2673.370251	119924.163793	56.881818
2672.483702	119694.387603	56.886823
2672.089492	119465.500366	56.891828
2671.267751	119235.070392	56.896833
2670.696492	119008.932292	56.901837
2670.196041	118763.600548	56.906842
2669.523084	118533.007176	56.911847
2668.777302	118305.804588	56.916852
2668.269432	118072.357870	56.921857
2667.415480	117847.994965	56.926861
2666.914335	117592.415982	56.931866
2666.202885	117366.073150	56.936871
2665.229721	117134.244802	56.941876
2665.028100	116898.608213	56.946881
2663.875931	116673.775886	56.951885
2663.157629	116435.825964	56.956890
2662.672769	116202.792386	56.961895
2662.020275	115987.827236	56.966900
2661.610828	115746.864100	56.971905
2660.966749	115515.385400	56.976909
2660.106688	115283.384452	56.981914
2659.493869	115055.516626	56.986919
2658.767294	114827.002401	56.991924
2658.227604	114589.003271	56.996929
2657.374294	114354.356585	57.001933
2656.474858	114129.842992	57.006938
2655.838845	113896.257813	57.011943
2655.392813	113670.508590	57.016948
2654.772447	113444.052766	57.021953
2653.905257	113213.493588	57.026957
2653.174362	112985.923307	57.031962
2652.707439	112752.842357	57.036967
2651.818004	112540.914234	57.041972
2651.440792	112300.879981	57.046977
2650.538546	112076.924598	57.051981
2650.114701	111848.421113	57.056986
2649.478050	111620.899064	57.061991
2648.515501	111398.380931	57.066996
2648.135884	111163.270107	57.072001
2647.302195	110936.762871	57.077005
2646.851991	110709.847886	57.082010
2646.077943	110495.526334	57.087015
2645.275792	110257.114889	57.092020
2644.721357	110029.619774	57.097025
2643.989954	109805.435679	57.102029
2643.506518	109574.170336	57.107034
2642.722277	109350.170097	57.112039
2642.079750	109125.330830	57.117044
2641.272408	108887.282482	57.122049
2640.662931	108675.285922	57.127053
2640.018266	108440.496864	57.132058
2639.197234	108207.489392	57.137063
2638.405839	107991.231632	57.142068
2637.938084	107765.184206	57.147073
2637.115748	107541.726888	57.152077
2636.647482	107316.464195	57.157082
2635.687305	107104.993729	57.162087
2634.910461	106888.115290	57.167092
2634.560465	106658.531547	57.172097
2633.953238	106441.300281	57.177101
2633.128192	106220.108098	57.182106
2632.365973	105994.307857	57.187111
2631.861017	105786.932760	57.192116
2631.274988	105557.105034	57.197121
2630.307458	105334.205072	57.202125
2629.657447	105111.390102	57.207130
2629.243132	104909.477410	57.212135
2628.254138	104687.678157	57.217140
2627.865239	104461.731659	57.222145
2626.917926	104250.385763	57.227149
2626.727115	104026.213847	57.232154
2625.882019	103808.441401	57.237159
2625.134666	103601.079257	57.242164
2625.057409	103372.162608	57.247169
2624.099289	103147.670135	57.252173
2623.601463	102926.412165	57.257178
2622.873456	102704.228435	57.262183
2621.927537	102485.177239	57.267188
2621.593789	102253.698301	57.272193
2620.785065	102033.709675	57.277197
2620.134632	101803.452639	57.282202
2619.449376	101586.341444	57.287207
2618.798362	101373.959285	57.292212
2618.203512	101137.489423	57.297217
2617.529129	100923.421283	57.302221
2617.148725	100694.737287	57.307226
2616.155443	100473.314504	57.312231
2615.356720	100251.444321	57.317236
2614.840397	100021.805228	57.322241
2614.198833	99809.613419	57.327245
2613.718523	99575.729327	57.332250
2613.028403	99353.476253	57.337255
2612.258782	99134.085990	57.342260
2611.774792	98904.535295	57.347265
2610.918821	98677.640137	57.352269
2610.276351	98452.394261	57.357274
2609.643106	98242.733666	57.362279
2608.724869	98017.764094	57.367284
2608.187315	97793.935177	57.372289
2607.144980	97579.042900	57.377293
2606.696593	97347.783208	57.382298
2606.058485	97134.835317	57.387303
2605.381214	96916.460049	57.392308
2604.746785	96696.063168	57.397313
2604.087885	96479.420670	57.402317
2603.470901	96257.128882	57.407322
2603.070208	96047.958929	57.412327
2602.588044	95810.054412	57.417332
2601.957924	95590.073464	57.422337
2600.786313	95364.263277	57.427341
2600.394036	95150.533941	57.432346
2599.372732	94924.640901	57.437351
2598.854959	94702.361321	57.442356
2598.369936	94473.223180	57.447361
2597.703575	94256.000652	57.452365
2597.126763	94028.238735	57.457370
2596.246620	93812.994944	57.462375
2595.530586	93584.910798	57.467380
2595.030749	93352.463428	57.472385
2594.421502	93141.799799	57.477389
2593.708576	92922.232196	57.482394
2593.064989	92697.589012	57.487399
2592.125085	92479.253921	57.492404
2591.837567	92248.331671	57.497409
2590.947364	92032.047651	57.502413
2590.221574	91806.855781	57.507418
2589.664209	91596.851677	57.512423
2588.959594	91374.171902	57.517428
2588.624205	91147.891268	57.522433
2587.435429	90928.184183	57.527437
2587.051541	90710.634398	57.532442
2586.528056	90489.564414	57.537447
2585.464501	90264.384727	57.542452
2584.936132	90041.925066	57.547457
2584.542561	89820.828530	57.552461
2584.111687	89600.925802	57.557466
2583.070855	89387.880840	57.562471
2582.492271	89167.333793	57.567476
2582.296660	88931.758855	57.572481
2581.281362	88711.488518	57.577485
2580.701217	88479.491891	57.582490
2580.012428	88259.332876	57.587495
2578.889756	88035.802228	57.592500
2578.516441	87803.545445	57.597505
2577.947842	87586.772411	57.602509
2576.998568	87367.120202	57.607514
2576.265900	87150.612112	57.612519
2575.646596	86928.325434	57.617524
2574.835151	86700.422886	57.622529
2574.267459	86491.109760	57.627533
2573.631303	86264.825982	57.632538
2572.888585	86042.206651	57.637543
2572.214751	85834.045160	57.642548
2571.584292	85614.867424	57.647553
2570.868899	85394.874950	57.652557
2570.417077	85186.690892	57.657562
2569.557924	84969.527496	57.662567
2568.555906	84751.317652	57.667572
2568.306152	84537.485147	57.672577
2567.574852	84321.512488	57.677581
2566.855323	84110.345014	57.682586
2566.489084	83887.561665	57.687591
2565.707309	83676.421045	57.692596
2565.102196	83454.732329	57.697601
2564.203989	83237.085711	57.702605
2563.627782	83014.991345	57.707610
2563.106540	82802.030677	57.712615
2562.356506	82594.381979	57.717620
2562.169001	82372.384877	57.722625
2561.186892	82152.404872	57.727629
2560.329155	81931.951101	57.732634
2559.838915	81710.389257	57.737639
2558.931148	81497.864318	57.742644
2558.432936	81282.107605	57.747649
2557.435085	81069.056224	57.752653
2556.934920	80849.983186	57.757658
2556.497257	80636.790371	57.762663
2555.772632	80424.659260	57.767668
2555.203483	80208.918529	57.772673
2554.459400	79989.196043	57.777677
2553.866304	79773.919923	57.782682
2553.092585	79546.943966	57.787687
2552.174738	79346.635871	57.792692
2551.804800	79116.976917	57.797697
2551.007630	78906.070566	57.802701
2550.315581	78682.354838	57.807706
2549.678358	78470.489666	57.812711
2548.888517	78269.873860	57.817716
2548.647178	78038.356070	57.822721
2547.601450	77832.614069	57.827725
2547.175039	77618.151433	57.832730
2546.789108	77397.043618	57.837735
2546.168777	77183.503415	57.842740
2545.392509	76957.963104	57.847745
2544.478136	76741.806366	57.852749
2543.932739	76521.601390	57.857754
2543.398197	76310.724383	57.862759
2542.556407	76089.582555	57.867764
2542.002358	75868.049014	57.872769
2540.989367	75651.767381	57.877773
2540.542468	75437.596981	57.882778
2539.896730	75227.414119	57.887783
2539.284972	75011.633278	57.892788
2538.335059	74792.208101	57.897793
2537.504224	74581.554395	57.902797
2537.157003	74363.451244	57.907802
2536.664046	74151.215174	57.912807
2536.027668	73950.142330	57.917812
2535.322498	73726.977168	57.922817
2534.885233	73505.793072	57.927821
2534.115856	73286.279619	57.932826
2533.131354	73061.512540	57.937831
2532.379828	72853.937026	57.942836
2532.150698	72636.682801	57.947841
2531.046872	72431.220165	57.952845
2530.590405	72209.622597	57.957850
2530.466394	71991.478115	57.962855
2529.318477	71790.628366	57.967860
2528.757866	71565.323097	57.972865
2527.864297	71343.627055	57.977869
2527.134043	71125.246066	57.982874
2526.663160	70907.295135	57.987879
2525.403948	70702.939196	57.992884
2525.294722	70486.291187	57.997889
2524.823975	70281.972962	58.002893
2524.048422	70061.875181	58.007898
2523.032030	69842.831542	58.012903
2522.153666	69638.388217	58.017908
2521.689751	69423.112962	58.022913
2521.329601	69211.497474	58.027917
2520.241095	68998.067798	58.032922
2519.608509	68791.402674	58.037927
2519.185665	68588.069854	58.042932
2518.776008	68376.072159	58.047937
2517.851666	68169.079799	58.052941
2517.088733	67956.958958	58.057946
2516.855570	67736.459183	58.062951
2515.436619	67524.200018	58.067956
2514.759899	67313.440575	58.072961
2514.218495	67121.998358	58.077965
2513.776198	66901.047154	58.082970
2513.446421	66695.616536	58.087975
2512.637320	66489.402738	58.092980
2512.056796	66274.934265	58.097985
2511.165046	66065.774085	58.102989
2510.305018	65863.229291	58.107994
2509.815485	65643.500018	58.112999
2508.933579	65424.478246	58.118004
2508.883210	65224.268997	58.123009
2508.168695	65010.519734	58.128013
2507.676935	64798.580376	58.133018
2506.944032	64588.828381	58.138023
2505.879903	64378.893707	58.143028
2505.632880	64161.853251	58.148033
2504.785851	63957.274651	58.153037
2503.932045	63740.981068	58.158042
2503.389146	63520.477086	58.163047
2502.927717	63312.883837	58.168052
2502.038322	63093.987956	58.173057
2501.098471	62888.719946	58.178061
2500.682781	62674.673882	58.183066
2499.947010	62464.942431	58.188071
2499.357217	62254.575945	58.193076
2498.992620	62039.154881	58.198081
2498.167674	61828.213031	58.203085
2497.518748	61615.099150	58.208090
2496.803322	61400.336137	58.213095
2495.530341	61195.360832	58.218100
2495.193244	60983.531092	58.223105
2494.672684	60771.976572	58.228109
2494.072542	60570.428007	58.233114
2493.493867	60367.143401	58.238119
2492.583601	60159.883699	58.243124
2492.284317	59940.414652	58.248129
2491.425739	59732.132141	58.253133
2490.735124	59523.818978	58.258138
2489.966752	59311.443295	58.263143
2489.456089	59101.270305	58.268148
2488.634935	58894.747985	58.273153
2488.168822	58684.936625	58.278157
2487.409963	58479.535890	58.283162
2486.927055	58271.308181	58.288167
2486.125844	58057.844070	58.293172
2485.577892	57845.772941	58.298177
2484.836924	57635.282615	58.303181
2484.062904	57419.593197	58.308186
2483.515429	57211.843349	58.313191
2482.573546	57007.383598	58.318196
2482.326172	56787.845213	58.323201
2481.497606	56585.097114	58.328205
2480.807084	56369.833939	58.333210
2480.261910	56166.792292	58.338215
2479.404803	55953.915102	58.343220
2478.727836	55749.544347	58.348225
2478.301803	55537.502444	58.353229
2477.518952	55328.985027	58.358234
2477.175102	55119.327508	58.363239
2475.957915	54914.959887	58.368244
2475.547261	54696.595741	58.373249
2474.272928	54499.688365	58.378253
2474.139735	54291.244286	58.383258
2473.598636	54078.943142	58.388263
2472.688155	53882.313835	58.393268
2472.246877	53672.681968	58.398273
2471.160451	53465.632595	58.403277
2470.596925	53250.901634	58.408282
2470.048710	53046.898167	58.413287
2469.301359	52850.013624	58.418292
2468.665390	52637.646190	58.423297
2468.030258	52441.605815	58.428301
2467.187209	52230.190463	58.433306
2466.942854	52019.340814	58.438311
2465.965996	51818.469431	58.443316
2465.411445	51613.426221	58.448321
2464.767124	51409.981636	58.453325
2464.361418	51206.808425	58.458330
2463.416577	50992.636092	58.463335
2462.740139	50786.995100	58.468340
2462.237889	50582.505841	58.473345
2461.516095	50384.669549	58.478349
2460.879035	50168.376331	58.483354
2460.348001	49957.893614	58.488359
2459.367679	49764.243503	58.493364
2459.201705	49554.640966	58.498369
2458.378284	49352.535702	58.503373
2457.891118	49140.929312	58.508378
2457.255835	48932.028565	58.513383
2456.295965	48714.342445	58.518388
2455.626522	48501.314080	58.523393
2454.819685	48309.294137	58.528397
2454.298755	48094.858263	58.533402
2453.580453	47885.533709	58.538407
2452.430037	47689.041616	58.543412
2452.625619	47465.515431	58.548417
2451.684949	47275.954225	58.553421
2450.905621	47071.191599	58.558426
2450.288936	46864.324076	58.563431
2449.600741	46660.924631	58.568436
2449.178823	46449.757455	58.573441
2448.402636	46245.288581	58.578445
2447.705844	46036.093174	58.583450
2447.334575	45828.588365	58.588455
2446.337543	45620.865746	58.593460
2445.914287	45404.840096	58.598465
2445.016499	45203.777588	58.603469
2444.537922	44996.843641	58.608474
2444.123113	44787.501333	58.613479
2443.003357	44577.362378	58.618484
2442.382964	44367.393470	58.623489
2441.476241	44165.468164	58.628493
2441.055189	43953.672949	58.633498
2440.517061	43736.515824	58.638503
2439.629422	43544.636474	58.643508
2439.114760	43330.244916	58.648513
2438.509784	43132.749441	58.653517
2438.075996	42923.315449	58.658522
2437.147897	42713.013582	58.663527
2436.099932	42509.757289	58.668532
2435.640819	42298.519538	58.673537
2435.040656	42101.926842	58.678541
2434.453012	41902.070753	58.683546
2433.801425	41686.067240	58.688551
2432.634966	41489.074802	58.693556
2432.471255	41280.538070	58.698561
2431.813620	41073.717077	58.703565
2430.793972	40872.847240	58.708570
2430.371358	40670.398833	58.713575
2429.548614	40465.091241	58.718580
2429.102226	40254.088328	58.723585
2428.294377	40064.533769	58.728589
2427.459711	39859.731748	58.733594
2427.009278	39652.360594	58.738599
2426.201371	39461.661727	58.743604
2425.638602	39247.426471	58.748609
2424.844389	39043.530528	58.753613
2423.947456	38847.714511	58.758618
2423.311894	38648.974113	58.763623
2422.593259	38457.431242	58.768628
2422.104622	38254.606058	58.773633
2421.547530	38062.572484	58.778637
2420.840263	37858.847646	58.783642
2420.399785	37658.416910	58.788647
2419.696878	37451.864993	58.793652
2419.193548	37259.394080	58.798657
2418.554643	37053.834337	58.803661
2417.694941	36855.058755	58.808666
2417.155601	36645.583715	58.813671
2416.243673	36441.818245	58.818676
2416.032713	36244.654133	58.823681
2415.197750	36043.587414	58.828685
2414.490824	35838.783497	58.833690
2414.087323	35625.695660	58.838695
2413.157734	35429.265159	58.843700
2412.854424	35220.721906	58.848705
2411.870290	35015.281241	58.853709
2411.244971	34807.413765	58.858714
2410.840167	34613.274103	58.863719
2409.937868	34411.325598	58.868724
2409.335097	34194.426287	58.873729
2408.640759	33986.306510	58.878733
2407.937361	33786.268517	58.883738
2407.604659	33590.267492	58.888743
2406.564530	33387.493443	58.893748
2406.075198	33175.171029	58.898753
2404.891661	32977.494659	58.903757
2404.585133	32770.731925	58.908762
2403.724623	32568.955535	58.913767
2402.653604	32374.113124	58.918772
2402.516778	32172.040311	58.923777
2401.764520	31975.780314	58.928781
2400.977285	31777.903664	58.933786
2400.416862	31579.794298	58.938791
2399.554131	31390.221118	58.943796
2399.285633	31190.529384	58.948801
2398.290640	30987.916547	58.953805
2397.729235	30788.176572	58.958810
2397.080892	30583.936702	58.963815
2396.120679	30411.523913	58.968820
2395.562593	30196.101339	58.973825
2394.959876	30004.361783	58.978829
2394.249510	29812.510387	58.983834
2393.840785	29616.887594	58.988839
2392.742052	29415.843225	58.993844
2392.270324	29229.685313	58.998849
2391.462964	29038.551981	59.003853
2391.006624	28844.781923	59.008858
2390.650518	28639.137395	59.013863
2389.489538	28448.962875	59.018868
2389.027344	28253.404343	59.023873
2388.489276	28066.721947	59.028877
2387.560435	27868.230711	59.033882
2387.261310	27669.804755	59.038887
2386.420287	27479.514968	59.043892
2385.949565	27279.323102	59.048897
2385.287753	27083.675980	59.053901
2384.553089	26886.052214	59.058906
2384.051738	26688.341721	59.063911
2382.875003	26500.799118	59.068916
2382.341554	26295.866333	59.073921
2381.935860	26099.496957	59.078925
2381.198390	25914.948252	59.083930
2380.518578	25725.275101	59.088935
2379.472271	25527.226062	59.093940
2378.957052	25324.829380	59.098945
2378.163906	25134.907863	59.103949
2377.642139	24940.560537	59.108954
2377.165994	24752.416920	59.113959
2376.247572	24569.042519	59.118964
2375.414391	24366.371072	59.123969
2374.706268	24183.243356	59.128973
2374.045539	23992.966829	59.133978
2373.178172	23796.923821	59.138983
2372.480728	23627.767505	59.143988
2372.290496	23431.390976	59.148993
2371.620881	23250.834441	59.153997
2371.054626	23059.923819	59.159002
2370.616656	22871.103646	59.164007
2369.315499	22680.854267	59.169012
2368.935717	22498.030968	59.174017
2368.403962	22317.633699	59.179021
2367.583957	22116.430629	59.184026
2366.857479	21932.321635	59.189031
2366.218622	21752.285735	59.194036
2365.743566	21558.182142	59.199041
2365.062420	21378.841010	59.204045
2364.222024	21191.624626	59.209050
2363.642539	21001.364598	59.214055
2362.928433	20815.495500	59.219060
2362.486203	20618.122937	59.224065
2361.549390	20440.830647	59.229069
2360.744881	20250.744827	59.234074
2360.263696	20072.871181	59.239079
2359.396274	19887.747922	59.244084
2358.870601	19698.838076	59.249089
2357.968043	19521.779652	59.254093
2357.249990	19341.321483	59.259098
2356.546956	19153.804297	59.264103
2355.725742	18982.181209	59.269108
2355.098895	18808.524623	59.274113
2354.176357	18629.150788	59.279117
2353.865266	18450.284010	59.284122
2353.145369	18277.681494	59.289127
2352.338880	18106.378682	59.294132
2352.064914	17925.868726	59.299137
2351.357458	17762.046332	59.304141
2350.523182	17587.053860	59.309146
2350.088918	17402.170688	59.314151
2349.018544	17231.601388	59.319156
2348.548738	17053.513867	59.324161
2347.735201	16884.782091	59.329165
2347.173888	16716.075687	59.334170
2346.693784	16536.660048	59.339175
2345.528631	16373.568584	59.344180
2344.956617	16188.461959	59.349185
2344.242113	16025.347277	59.354189
2343.383205	15855.123431	59.359194
2343.063538	15679.264467	59.364199
2342.294324	15523.759402	59.369204
2341.654409	15354.963037	59.374209
2340.951850	15188.840821	59.379213
2340.036402	15014.588146	59.384218
2339.552844	14854.261284	59.389223
2338.470770	14695.920783	59.394228
2337.955033	14512.197259	59.399233
2337.746113	14364.976868	59.404237
2336.437808	14212.470806	59.409242
2335.923577	14053.464358	59.414247
2335.237703	13892.237010	59.419252
2334.544298	13727.995264	59.424257
2333.657066	13575.069531	59.429261
2332.990031	13418.575835	59.434266
2332.409310	13264.960760	59.439271
2331.406353	13123.005000	59.444276
2330.733085	12974.092783	59.449281
2329.811780	12825.777936	59.454285
2328.876671	12679.564781	59.459290
2328.020643	12542.797657	59.464295
2327.354944	12408.171681	59.469300
2326.598096	12266.717200	59.474305
2325.503318	12141.604169	59.479309
2325.025602	12017.073357	59.484314
2324.188744	11895.223366	59.489319
2323.299922	11774.941544	59.494324
2322.850011	11650.960626	59.499329
2322.083099	11536.091015	59.504333
2321.446599	11408.723934	59.509338
2320.957618	11291.247823	59.514343
2319.852793	11177.669092	59.519348
2319.483565	11061.964676	59.524353
2318.702567	10948.391925	59.529357
2317.930453	10828.267152	59.534362
2317.320582	10705.132670	59.539367
2316.404296	10604.579653	59.544372
2315.695799	10494.745759	59.549377
2315.158741	10396.194845	59.554381
2314.159686	10293.085634	59.559386
2313.725439	10182.441949	59.564391
2312.935439	10075.036186	59.569396
2312.452173	9969.031621	59.574401
2311.634446	9860.985936	59.579405
2310.662603	9754.331691	59.584410
2309.938107	9656.240222	59.589415
2309.183155	9559.759500	59.594420
2308.381120	9459.966847	59.599425
2308.105271	9360.301860	59.604429
2307.481976	9270.757695	59.609434
2306.607490	9175.988060	59.614439
2305.948669	9086.329512	59.619444
2305.306859	8987.213037	59.624449
2304.705809	8900.371838	59.629453
2303.827969	8807.576354	59.634458
2303.646556	8707.250178	59.639463
2302.422281	8624.953381	59.644468
2302.072506	8529.419747	59.649473
2301.097024	8444.700189	59.654477
2300.295486	8354.269807	59.659482
2299.771757	8268.874839	59.664487
2299.094730	8184.899550	59.669492
2298.478423	8097.382563	59.674497
2297.895888	8020.175437	59.679501
2296.875611	7947.544597	59.684506
2296.118186	7863.710878	59.689511
2294.968485	7793.986862	59.694516
2294.524175	7723.163139	59.699521
2293.830473	7648.186942	59.704525
2292.829433	7585.346207	59.709530
2291.928331	7512.236265	59.714535
2291.164016	7458.331713	59.719540
2290.828611	7390.004601	59.724545
2290.071136	7332.645151	59.729549
2289.136832	7269.724157	59.734554
2288.744038	7204.930656	59.739559
2287.765744	7148.456593	59.744564
2287.273182	7085.545585	59.749569
2286.885957	7033.023279	59.754573
2285.733600	6978.107539	59.759578
2285.281872	6913.554217	59.764583
2284.280284	6859.795176	59.769588
2284.091677	6789.866983	59.774593
2283.599935	6744.551370	59.779597
2282.924804	6688.568581	59.784602
2282.330710	6628.354242	59.789607
2281.277079	6570.059793	59.794612
2281.108893	6517.495876	59.799617
2280.280770	6457.496847	59.804621
2279.547229	6403.479994	59.809626
2279.296104	6348.003148	59.814631
2278.074973	6291.388236	59.819636
2277.780702	6231.039588	59.824641
2277.179690	6168.799665	59.829645
2276.460182	6110.480834	59.834650
2275.559877	6048.249057	59.839655
2274.832583	5990.451781	59.844660
2274.639260	5933.338352	59.849665
2273.740246	5879.830842	59.854669
2272.783264	5815.065037	59.859674
2272.678571	5767.298471	59.864679
2271.680020	5719.740906	59.869684
2271.356150	5656.595790	59.874689
2270.444284	5603.151267	59.879693
2269.293058	5544.225549	59.884698
2269.438931	5495.638387	59.889703
2268.110221	5450.377454	59.894708
2267.496180	5390.383480	59.899713
2266.873265	5339.449025	59.904718
2266.252011	5286.002928	59.909722
2265.932947	5235.039559	59.914727
2264.985487	5181.017704	59.919732
2264.580858	5129.253444	59.924737
2264.157230	5079.936060	59.929742
2263.233436	5019.551790	59.934746
2262.742353	4970.218653	59.939751
2261.882323	4917.971281	59.944756
2261.336967	4862.450423	59.949761
2260.471470	4808.465041	59.954766
2259.565503	4765.007763	59.959770
2258.983418	4712.471714	59.964775
2258.223373	4670.568323	59.969780
2257.799932	4610.964529	59.974785
2257.385895	4570.352958	59.979790
2256.690826	4514.051038	59.984794
2256.148241	4453.109319	59.989799
2255.440917	4415.384238	59.994804
2254.633999	4357.988509	59.999809
2254.010048	4306.834554	60.004814
2253.502044	4253.716538	60.009818
2253.008065	4192.523670	60.014823
2252.133588	4150.343342	60.019828
2251.648884	4088.272351	60.024833
2250.909318	4038.605514	60.029838
2250.237825	3988.022576	60.034842
2249.786423	3929.435546	60.039847
2248.708363	3880.945306	60.044852
2248.178053	3827.793713	60.049857
2247.555490	3777.089371	60.054862
2246.608068	3725.712696	60.059866
2246.327574	3669.059557	60.064871
2245.134672	3630.947389	60.069876
2244.521301	3575.743447	60.074881
2244.188647	3534.794498	60.079886
2243.030173	3485.930273	60.084890
2242.972142	3437.740276	60.089895
2242.162387	3394.162149	60.094900
2241.620234	3334.538173	60.099905
2240.682632	3294.681206	60.104910
2239.967574	3248.104056	60.109914
2239.468130	3192.131851	60.114919
2238.665138	3148.371193	60.119924
2238.091031	3092.037376	60.124929
2237.787443	3049.712849	60.129934
2237.165438	2998.863617	60.134938
2236.545959	2944.192219	60.139943
2235.894503	2897.218061	60.144948
2235.130128	2841.379921	60.149953
2234.526038	2790.995461	60.154958
2233.903988	2736.475881	60.159962
2233.192235	2678.047914	60.164967
2232.222742	2636.436708	60.169972
2231.525712	2580.168520	60.174977
2231.136340	2533.660265	60.179982
2230.046824	2484.567616	60.184986
2229.465007	2444.360771	60.189991
2228.401614	2399.597120	60.194996
2228.157910	2353.726426	60.200001
2227.696413	2313.686182	60.205006
2226.783303	2273.231106	60.210010
2226.748314	2218.358483	60.215015
2225.682260	2178.285189	60.220020
2225.027376	2125.298317	60.225025
2224.483619	2073.855499	60.230030
2223.774372	2024.246657	60.235034
2223.354196	1971.779876	60.240039
2222.452492	1925.998354	60.245044
2222.006679	1871.002939	60.250049
2220.998446	1837.423595	60.255054
2220.395566	1773.390650	60.260058
2219.570856	1730.103749	60.265063
2218.743449	1691.538037	60.270068
2218.524059	1645.220136	60.275073
2217.689685	1607.189640	60.280078
2216.771428	1557.077715	60.285082
2216.314847	1515.292906	60.290087
2215.431330	1466.475398	60.295092
2214.951872	1420.488887	60.300097
2214.310448	1372.891884	60.305102
2213.491677	1339.470527	60.310106
2213.075520	1294.758987	60.315111
2211.995987	1267.117745	60.320116
2211.313670	1214.420844	60.325121
2210.816777	1179.198125	60.330126
2210.204961	1136.925661	60.335130
2209.850997	1089.527645	60.340135
2209.159450	1050.203965	60.345140
2208.461503	1011.179488	60.350145
2207.643813	963.633868	60.355150
2206.854753	922.244173	60.360154
2206.380427	874.170435	60.365159
2205.437163	840.120988	60.370164
2205.004672	790.731079	60.375169
2204.309425	757.677858	60.380174
2203.597790	725.012130	60.385178
2202.683065	678.468538	60.390183
2201.872568	643.272428	60.395188
2201.405319	607.070947	60.400193
2200.725972	573.775113	60.405198
2200.226141	540.556539	60.410202
2199.850048	489.116361	60.415207
2198.980643	470.482421	60.420212
2198.456555	425.129872	60.425217
2197.677175	379.182407	60.430222
2196.943833	351.249059	60.435226
2196.252416	313.081776	60.440231
2195.527577	279.170103	60.445236
2195.004929	234.792551	60.450241
2194.051571	213.019708	60.455246
2193.079731	184.783878	60.460250
2192.557613	150.898692	60.465255
2191.608032	122.802964	60.470260
2191.366357	92.770319	60.475265
2190.551099	59.873358	60.480270
2189.455402	35.674214	60.485274
2189.163512	14.034853	60.490279
2188.345973	-14.759687	60.495284
2187.507116	-36.320071	60.500289
2186.732095	-52.422970	60.505294
2185.792426	-66.645133	60.510298
2185.363312	-94.728397	60.515303
2183.865999	-89.529218	60.520308
2180.605199	-27.985041	60.525313
2178.006485	44.011082	60.530318
2178.401105	42.131968	60.535322
2179.771052	44.214185	60.540327
2180.197881	38.669637	60.545332
2180.334979	32.731068	60.550337
2180.011836	19.611128	60.555342
2179.526631	24.517283	60.560346
2178.486875	7.822355	60.565351
2176.746648	29.554415	60.570356
2175.948726	28.179936	60.575361
2175.546125	26.408398	60.580366
2174.706378	40.153376	60.585370
2174.391446	29.028666	60.590375
2173.810837	43.131520	60.595380
2172.893594	42.690661	60.600385
2172.472396	42.156898	60.605390
2172.366493	53.405685	60.610394
2172.011678	43.801257	60.615399
2170.601838	47.034227	60.620404
2169.992958	40.692022	60.625409
2169.389695	49.034377	60.630414
2168.161253	53.851884	60.635418
2167.836688	47.942407	60.640423
2167.434532	57.438795	60.645428
2166.786681	48.117421	60.650433
2166.237789	51.186971	60.655438
2165.174323	54.264052	60.660442
2164.597925	41.986999	60.665447
2163.800074	52.511324	60.670452
2163.936747	53.461356	60.675457
2163.245297	61.965955	60.680462
2161.742018	58.993883	60.685466
2161.626976	52.764136	60.690471
2160.780457	58.087204	60.695476
2160.235075	52.739500	60.700481
2159.486656	52.327053	60.705486
2158.506697	52.411844	60.710490
2158.202359	48.476776	60.715495
2157.464135	64.594895	60.720500
2157.260929	55.332281	60.725505
2156.993794	55.196722	60.730510
2155.537786	59.660817	60.735514
2154.811862	46.508573	60.740519
2154.620652	59.811597	60.745524
2154.205226	49.358874	60.750529
2152.826141	45.731554	60.755534
2152.390041	57.837032	60.760538
2152.156472	46.336682	60.765543
2151.318058	58.889224	60.770548
2150.515951	56.543953	60.775553
2149.361575	51.523139	60.780558
2148.707188	55.987772	60.785562
2148.405887	55.627386	60.790567
2147.537395	56.132913	60.795572
2146.963002	57.216281	60.800577
2146.579688	59.554621	60.805582
2145.467975	60.123977	60.810586
2144.899973	55.921647	60.815591
2144.642508	56.834869	60.820596
2144.289250	62.519665	60.825601
2143.184824	54.581274	60.830606
2141.996964	58.397237	60.835610
2142.528771	61.569707	60.840615
2141.590106	58.788765	60.845620
2140.542664	56.655905	60.850625
2139.580675	63.542810	60.855630
2139.330355	60.535936	60.860634
2139.091898	55.219960	60.865639
2137.752197	57.927701	60.870644
2136.847751	56.607985	60.875649
2137.143753	59.865184	60.880654
2136.081168	54.405583	60.885658
2135.175280	42.754871	60.890663
2135.138772	66.071245	60.895668
2134.379607	56.444247	60.900673
2132.986162	52.297213	60.905678
2131.915159	53.372654	60.910682
2132.550426	53.872956	60.915687
2131.764923	59.107496	60.920692
2130.404975	53.119466	60.925697
2130.163977	51.049457	60.930702
2129.651633	55.341734	60.935706
2128.351453	50.304642	60.940711
2128.036321	54.048351	60.945716
2127.812298	50.701396	60.950721
2126.481784	58.441615	60.955726
2126.177982	60.686911	60.960730
2125.953850	56.884206	60.965735
2124.447073	61.668628	60.970740
2124.100826	51.791595	60.975745
2123.730328	53.599593	60.980750
2122.496413	56.006685	60.985754
2121.957499	43.580186	60.990759
2121.757426	57.215790	60.995764
2121.074679	46.565790	61.000769
2120.198560	55.110738	61.005774
2119.267616	67.163859	61.010778
2118.964403	59.140909	61.015783
2117.992658	60.973357	61.020788
2117.586205	55.255088	61.025793
2117.021790	55.180904	61.030798
2116.347572	49.184991	61.035802
2116.019432	49.494383	61.040807
2115.282832	57.201859	61.045812
2114.694322	56.683618	61.050817
2114.281605	49.193747	61.055822
2113.243446	56.469658	61.060826
2112.102865	53.545720	61.065831
2111.481349	62.960225	61.070836
2111.083374	50.689563	61.075841
2110.172672	54.084640	61.080846
2109.836445	54.138257	61.085850
2109.087876	44.944859	61.090855
2107.915160	48.157577	61.095860
2107.651058	51.079433	61.100865
2107.352883	53.003695	61.105870
2105.968287	55.885743	61.110874
2105.735246	46.206808	61.115879
2105.106016	55.445904	61.120884
2104.331989	58.549618	61.125889
2103.928128	49.588536	61.130894
2102.958349	59.868911	61.135898
2102.756904	53.693886	61.140903
2102.145603	57.714849	61.145908
2101.256984	52.793816	61.150913
2101.139413	49.217069	61.155918
2100.021702	51.250893	61.160922
2098.896849	45.324928	61.165927
2098.715774	53.400008	61.170932
2097.957197	59.456655	61.175937
2097.056214	55.140017	61.180942
2096.223788	47.814537	61.185946
2095.988823	47.339546	61.190951
2095.041881	51.286035	61.195956
2094.537675	50.949974	61.200961
2093.898629	48.824864	61.205966
2093.207744	51.328724	61.210970
2092.880828	47.983910	61.215975
2092.401418	48.926051	61.220980
2091.869948	46.063160	61.225985
2090.757585	48.244381	61.230990
2089.562927	51.723955	61.235994
2089.177534	46.163212	61.240999
2088.436035	49.594523	61.246004
2087.595271	51.844611	61.251009
2087.143535	40.323708	61.256014
2086.477448	42.262205	61.261018
2086.193791	41.671933	61.266023
2085.497357	50.759259	61.271028
2084.952168	51.181954	61.276033
2084.349011	48.612732	61.281038
2083.628233	46.366548	61.286042
2083.522240	42.810046	61.291047
2082.045632	48.266250	61.296052
2081.043527	51.995982	61.301057
2080.176959	52.065960	61.306062
2079.518323	55.916234	61.311066
2079.519949	49.653787	61.316071
2078.774417	45.489116	61.321076
2078.189717	48.815114	61.326081
2077.747923	47.956611	61.331086
2076.827809	50.892694	61.336090
2076.535029	42.232557	61.341095
2075.789890	55.659758	61.346100
2074.996405	47.766678	61.351105
2074.034971	44.437414	61.356110
2072.900536	55.210731	61.361114
2072.513729	47.475471	61.366119
2072.435919	60.104440	61.371124
2071.914598	54.500612	61.376129
2071.384020	42.881832	61.381134
2070.389466	56.575715	61.386138
2069.920758	44.546545	61.391143
2068.679616	49.818719	61.396148
2067.622982	51.125307	61.401153
2067.722886	55.041282	61.406158
2066.919569	52.716734	61.411162
2066.335327	49.158862	61.416167
2065.289789	49.337680	61.421172
2064.461023	48.639951	61.426177
2064.576787	51.695496	61.431182
2063.739503	57.647941	61.436186
2063.227493	54.893936	61.441191
2062.743363	58.123548	61.446196
2062.112319	50.974287	61.451201
2061.113350	46.398811	61.456206
2060.093899	60.968758	61.461210
2059.839247	42.813491	61.466215
2059.112799	59.361855	61.471220
2058.802430	55.486109	61.476225
2057.863598	52.517559	61.481230
2056.412665	56.413161	61.486234
2055.893318	56.672479	61.491239
2055.825698	50.116655	61.496244
2055.298345	55.620917	61.501249
2054.585750	48.708544	61.506254
2053.666114	53.645828	61.511258
2053.331454	54.027229	61.516263
2052.571796	56.437930	61.521268
2051.990016	58.629576	61.526273
2050.596621	47.450540	61.531278
2050.225272	57.090285	61.536282
2049.953109	42.322141	61.541287
2048.761501	55.460644	61.546292
2048.484728	50.187038	61.551297
2047.879875	54.172291	61.556302
2047.344699	49.654101	61.561306
2047.091435	49.470618	61.566311
2046.375832	52.186582	61.571316
2045.243183	54.314268	61.576321
2044.343232	51.431021	61.581326
2043.323177	53.313742	61.586330
2042.681770	46.964120	61.591335
2042.115167	49.388337	61.596340
2041.984238	52.976651	61.601345
2041.641408	48.869505	61.606350
2040.708591	54.487015	61.611354
2040.464909	47.317282	61.616359
2039.306183	52.704128	61.621364
2038.239137	55.706127	61.626369
2037.934120	53.807149	61.631374
2036.854663	57.468745	61.636378
2036.680390	57.230145	61.641383
2036.277823	62.249377	61.646388
2035.829407	62.223035	61.651393
2034.484432	56.811457	61.656398
2033.480819	59.558947	61.661402
2032.979165	52.545285	61.666407
2032.249517	56.608701	61.671412
2031.641687	52.056312	61.676417
2031.282380	52.914742	61.681422
2030.632830	57.730311	61.686426
2030.590881	53.624296	61.691431
2029.982693	59.016807	61.696436
2028.905222	53.496538	61.701441
2028.127555	56.460492	61.706446
2026.945356	53.730869	61.711450
2026.415107	55.013847	61.716455
2026.069012	57.161780	61.721460
2025.572476	55.581803	61.726465
2025.123700	55.523978	61.731470
2024.157935	60.504867	61.736474
2023.560431	51.628162	61.741479
2022.727268	55.446222	61.746484
2021.938252	58.751045	61.751489
2021.527436	52.536722	61.756494
2020.907620	59.325188	61.761498
2020.814068	54.520847	61.766503
2019.222250	53.292935	61.771508
2018.440781	58.339194	61.776513
2017.927116	54.576154	61.781518
2017.101612	55.604786	61.786522
2017.013285	45.390358	61.791527
2016.545843	53.619709	61.796532
2016.118705	54.627687	61.801537
2015.307106	50.255891	61.806542
2013.858707	50.946557	61.811546
2013.156774	47.596627	61.816551
2013.039291	50.884745	61.821556
2012.446444	55.055768	61.826561
2011.882044	54.319246	61.831566
2010.686770	46.556206	61.836570
2009.785963	50.299846	61.841575
2009.092075	56.076569	61.846580
2008.345731	49.929704	61.851585
2007.914026	53.512144	61.856590
2007.313238	61.608116	61.861594
2007.255638	52.428080	61.866599
2006.620101	53.076457	61.871604
2006.156208	59.108426	61.876609
2005.736933	46.997306	61.881614
2004.097060	57.477119	61.886618
2003.421196	51.008390	61.891623
2002.805774	53.758928	61.896628
2002.518646	56.170331	61.901633
2002.220797	50.411194	61.906638
2000.781843	55.768418	61.911642
2000.080695	55.706503	61.916647
1999.470362	62.036125	61.921652
1998.495494	59.153747	61.926657
1998.622659	53.620473	61.931662
1997.935374	61.991967	61.936666
1997.681721	55.014642	61.941671
1996.257791	57.709012	61.946676
1995.404617	56.398556	61.951681
1995.149516	58.508391	61.956686
1994.135814	60.673991	61.961690
1994.412152	56.981102	61.966695
1993.526300	56.997396	61.971700
1992.344890	67.267242	61.976705
1991.299164	53.506623	61.981710
1990.569037	57.983311	61.986714
1990.266148	53.638007	61.991719
1989.755257	54.586740	61.996724
1989.345830	52.040409	62.001729
1988.921584	50.038933	62.006734
1988.082700	57.816291	62.011738
1987.266176	51.751540	62.016743
1986.612916	51.841307	62.021748
1985.657993	59.558235	62.026753
1985.640872	56.665758	62.031758
1984.405677	61.515957	62.036762
1983.801788	49.416800	62.041767
1983.256242	50.952965	62.046772
1982.562653	49.579331	62.051777
1982.178010	52.703268	62.056782
1981.250174	56.979519	62.061786
1980.354558	47.498835	62.066791
1979.706836	58.649108	62.071796
1978.886796	53.602112	62.076801
1978.405177	45.311036	62.081806
1977.713910	54.851750	62.086810
1977.568956	48.478532	62.091815
1977.243048	57.770425	62.096820
1975.852313	56.162091	62.101825
1975.144900	52.628526	62.106830
1974.432144	57.821592	62.111834
1974.013729	48.304582	62.116839
1973.348687	51.313752	62.121844
1972.899059	54.667216	62.126849
1971.781070	47.335077	62.131854
1970.611819	50.712891	62.136858
1970.175116	44.510577	62.141863
1969.734994	48.498080	62.146868
1969.289242	52.880738	62.151873
1969.001700	47.257175	62.156878
1968.570772	54.217522	62.161882
1967.820656	50.346944	62.166887
1966.503387	54.603016	62.171892
1966.011921	50.029018	62.176897
1965.627272	48.846054	62.181902
1964.697434	44.422082	62.186906
1964.436706	44.500004	62.191911
1963.315981	50.798684	62.196916
1962.437395	51.356338	62.201921
1962.041347	49.309388	62.206926
1961.397966	53.378049	62.211930
1961.112528	43.338435	62.216935
1960.560015	51.803658	62.221940
1959.004310	56.308910	62.226945
1958.537028	52.055946	62.231950
1957.634739	56.028509	62.236954
1957.399933	51.270256	62.241959
1956.758781	53.244252	62.246964
1956.435376	57.560178	62.251969
1956.066626	46.720034	62.256974
1954.812352	57.700083	62.261978
1954.020344	52.948284	62.266983
1953.353007	53.940786	62.271988
1953.002100	51.124959	62.276993
1952.638657	50.405434	62.281998
1951.267471	47.694813	62.287002
1950.448762	40.873447	62.292007
1949.802540	56.207376	62.297012
1949.358416	53.209217	62.302017
1949.038101	49.114283	62.307022
1948.997579	51.647397	62.312026
1948.058452	49.568390	62.317031
1946.881104	49.230410	62.322036
1945.976929	48.659816	62.327041
1945.605928	48.780479	62.332046
1944.749250	54.478974	62.337050
1944.537562	46.015735	62.342055
1943.111577	52.605752	62.347060
1942.292109	42.624116	62.352065
1941.974594	46.199473	62.357070
1941.118847	58.655450	62.362074
1940.995469	50.312237	62.367079
1940.547779	57.138046	62.372084
1940.242824	52.327851	62.377089
1939.764031	53.093292	62.382094
1938.802838	54.499902	62.387098
1937.964620	51.062814	62.392103
1936.992976	51.428659	62.397108
1935.879726	56.104965	62.402113
1935.085405	48.131643	62.407118
1934.293113	53.985508	62.412122
1934.497558	52.674326	62.417127
1933.679719	46.556187	62.422132
1933.234546	50.227511	62.427137
1933.153632	47.638496	62.432142
1931.994323	50.186800	62.437146
1931.031238	52.035284	62.442151
1930.310531	48.325640	62.447156
1929.687381	48.858520	62.452161
1929.222218	42.163968	62.457166
1927.918970	47.602187	62.462170
1927.422209	51.874671	62.467175
1926.497046	55.130167	62.472180
1926.061026	48.719584	62.477185
1925.931328	42.465385	62.482190
1925.298122	50.128092	62.487194
1925.116185	43.558893	62.492199
1924.410572	47.057090	62.497204
1922.810688	50.881784	62.502209
1922.653619	39.799876	62.507214
1921.673439	49.498436	62.512218
1921.632917	50.165909	62.517223
1920.677220	52.186699	62.522228
1919.779002	52.846838	62.527233
1919.629087	55.332662	62.532238
1918.662490	51.990085	62.537242
1917.438380	40.900964	62.542247
1916.939988	49.575229	62.547252
1915.994997	47.935584	62.552257
1915.982987	47.324280	62.557262
1915.325130	45.478187	62.562266
1914.979235	45.217956	62.567271
1914.268125	45.857851	62.572276
1913.193727	47.613622	62.577281
1912.700471	43.522499	62.582286
1911.924687	58.332924	62.587290
1911.818363	42.333625	62.592295
1910.712221	45.915920	62.597300
1909.458308	44.421525	62.602305
1909.406692	43.135228	62.607310
1908.582935	54.329227	62.612314
1908.182415	44.891401	62.617319
1906.754783	44.503286	62.622324
1906.145659	56.469076	62.627329
1905.875104	46.570620	62.632334
1905.328945	46.973003	62.637338
1904.739716	43.193604	62.642343
1904.414617	50.876784	62.647348
1903.533178	44.409191	62.652353
1902.923249	41.349056	62.657358
1901.766795	56.200998	62.662362
1901.283685	44.929570	62.667367
1900.438747	52.001393	62.672372
1900.291619	43.412788	62.677377
1899.432620	42.395043	62.682382
1897.974630	54.978189	62.687386
1897.759272	45.299642	62.692391
1897.184458	47.876586	62.697396
1896.694042	48.949826	62.702401
1896.649345	50.948985	62.707406
1895.909773	51.683296	62.712410
1895.053095	55.945120	62.717415
1894.221881	60.418957	62.722420
1893.666919	54.208625	62.727425
1892.550562	53.458839	62.732430
1891.356015	55.460791	62.737434
1891.121607	54.017427	62.742439
1890.586040	44.713018	62.747444
1889.969797	52.552822	62.752449
1889.917155	51.580519	62.757454
1889.349642	54.402325	62.762458
1888.880871	51.494829	62.767463
1887.587761	48.997363	62.772468
1887.010912	55.969848	62.777473
1886.528457	50.662692	62.782478
1884.889894	56.171523	62.787482
1884.242963	52.369748	62.792487
1883.867936	60.081363	62.797492
1883.470312	55.741656	62.802497
1882.909132	45.879889	62.807502
1882.419439	56.563508	62.812506
1881.940192	40.789022	62.817511
1880.784694	50.064398	62.822516
1880.082436	51.931412	62.827521
1879.756328	46.837566	62.832526
1879.280250	53.172696	62.837530
1878.637057	50.627232	62.842535
1877.277036	55.197657	62.847540
1876.623259	58.693944	62.852545
1876.162489	43.101037	62.857550
1875.593492	50.129049	62.862554
1875.447366	50.696589	62.867559
1874.144468	51.950888	62.872564
1873.556544	48.888842	62.877569
1872.958492	43.661552	62.882574
1872.570078	51.682812	62.887578
1871.785141	38.775045	62.892583
1870.388328	47.273411	62.897588
1869.788573	46.522034	62.902593
1869.431411	42.231105	62.907598
1868.898387	54.214777	62.912602
1868.829933	41.559112	62.917607
1868.433077	38.621280	62.922612
1867.166084	39.985003	62.927617
1866.555661	39.156469	62.932622
1865.481630	47.767595	62.937626
1865.131581	44.599967	62.942631
1864.857628	47.472938	62.947636
1863.344430	43.529592	62.952641
1862.671156	45.388853	62.957646
1862.001944	55.484356	62.962650
1861.956818	38.134870	62.967655
1861.581742	44.755175	62.972660
1860.270473	52.001987	62.977665
1859.482085	41.296322	62.982670
1858.461431	46.664464	62.987674
1858.550891	37.416947	62.992679
1858.071032	42.079436	62.997684
1857.439303	42.320366	63.002689
1856.620028	45.289394	63.007694
1855.991576	46.829285	63.012698
1855.483669	38.965068	63.017703
1854.642443	45.817101	63.022708
1853.526003	46.270628	63.027713
1853.001772	40.640515	63.032718
1852.245073	47.647870	63.037722
1851.480453	39.144715	63.042727
1850.884101	48.366004	63.047732
1850.687596	47.754034	63.052737
1850.620590	44.177166	63.057742
1849.438407	54.858782	63.062746
1848.634178	42.603826	63.067751
1847.786542	51.097002	63.072756
1847.047905	54.542112	63.077761
1846.451913	42.608924	63.082766
1845.114733	53.048634	63.087770
1844.885898	38.898176	63.092775
1844.462524	48.096728	63.097780
1844.118397	55.420216	63.102785
1843.784059	46.036554	63.107790
1843.203229	48.045153	63.112794
1842.304226	36.235788	63.117799
1841.526485	41.439196	63.122804
1840.631028	49.911581	63.127809
1839.538352	47.040092	63.132814
1838.623496	48.027771	63.137818
1838.257093	44.097880	63.142823
1837.772416	43.656260	63.147828
1837.275467	42.424915	63.152833
1837.096249	46.288995	63.157838
1836.552226	47.599429	63.162842
1835.844568	47.965969	63.167847
1835.098853	45.343753	63.172852
1833.943181	52.316696	63.177857
1832.718320	37.196832	63.182862
1832.174284	54.183047	63.187866
1832.145818	46.002985	63.192871
1831.162519	49.463295	63.197876
1830.804043	40.430423	63.202881
1830.606280	44.893569	63.207886
1829.349395	41.444157	63.212890
1828.460735	47.860582	63.217895
1827.827105	48.049779	63.222900
1827.539279	48.912652	63.227905
1827.297400	42.062812	63.232910
1826.302314	44.048885	63.237914
1825.349435	45.873707	63.242919
1824.568885	46.717052	63.247924
1824.137314	46.539829	63.252929
1823.884051	48.819705	63.257934
1822.830207	48.578868	63.262938
1821.877800	47.847234	63.267943
1821.551668	39.864268	63.272948
1820.739083	48.635750	63.277953
1820.581916	33.500888	63.282958
1819.646150	43.842158	63.287962
1818.610536	41.663401	63.292967
1818.092900	49.366121	63.297972
1817.511951	46.083775	63.302977
1817.354924	39.496444	63.307982
1815.678572	47.791633	63.312986
1815.007935	41.613893	63.317991
1814.778580	42.081107	63.322996
1814.364874	47.392300	63.328001
1814.173477	45.994156	63.333006
1813.047040	43.933910	63.338010
1812.113995	42.722939	63.343015
1811.714281	39.974815	63.348020
1810.963457	40.280405	63.353025
1810.771707	40.049327	63.358030
1809.313867	56.243908	63.363034
1808.810569	48.524054	63.368039
1808.447268	45.011592	63.373044
1807.768659	46.586269	63.378049
1806.809680	46.584277	63.383054
1805.637829	53.402096	63.388058
1805.399178	47.344996	63.393063
1804.716266	54.211328	63.398068
1804.294538	49.837617	63.403073
1803.801375	43.669543	63.408078
1803.359047	45.504757	63.413082
1803.093227	44.984229	63.418087
1802.112146	47.256685	63.423092
1800.879028	48.809037	63.428097
1799.672772	43.433919	63.433102
1798.884890	53.095666	63.438106
1798.838227	47.490650	63.443111
1798.578154	52.654439	63.448116
1797.588443	50.544097	63.453121
1797.419436	41.512681	63.458126
1796.858892	51.201404	63.463130
1795.846120	47.790513	63.468135
1795.222092	46.150404	63.473140
1794.466147	45.592594	63.478145
1793.933814	40.059984	63.483150
1792.408672	49.706350	63.488154
1792.133567	50.781684	63.493159
1791.612383	55.250466	63.498164
1790.930314	46.559167	63.503169
1790.614132	41.736591	63.508174
1790.404872	48.698018	63.513178
1789.206002	42.268270	63.518183
1788.569009	47.812059	63.523188
1787.876152	42.360140	63.528193
1787.387886	38.859645	63.533198
1786.152797	45.461994	63.538202
1785.623941	41.583148	63.543207
1785.087090	43.572156	63.548212
1784.421814	44.488673	63.553217
1784.037010	38.019530	63.558222
1783.295304	40.979412	63.563226
1782.552629	42.911219	63.568231
1781.864655	42.607559	63.573236
1781.296139	39.460451	63.578241
1780.873976	39.601880	63.583246
1779.509361	38.762257	63.588250
1779.121044	38.885694	63.593255
1778.585043	37.747301	63.598260
1777.636189	37.071893	63.603265
1777.831953	32.959685	63.608270
1776.569873	39.325036	63.613274
1775.712806	39.614391	63.618279
1775.326074	41.101715	63.623284
1774.577809	44.065796	63.628289
1774.408940	32.992103	63.633294
1772.703833	44.351334	63.638298
1771.962924	40.564521	63.643303
1771.961900	37.081265	63.648308
1771.555318	43.657691	63.653313
1771.177376	34.344062	63.658318
1769.449487	39.025002	63.663322
1768.938963	38.092310	63.668327
1768.683615	46.176022	63.673332
1768.223465	43.926387	63.678337
1768.016291	39.649505	63.683342
1766.987762	47.919103	63.688346
1766.066266	52.159716	63.693351
1765.509633	40.478942	63.698356
1764.468483	46.022269	63.703361
1763.757494	48.218722	63.708366
1762.665133	49.497986	63.713370
1762.243801	44.712616	63.718375
1761.903894	35.932294	63.723380
1761.434573	40.110548	63.728385
1761.684067	35.180784	63.733390
1760.185935	42.540897	63.738394
1759.312145	37.688616	63.743399
1758.797250	36.556337	63.748404
1758.505244	43.961436	63.753409
1757.816407	47.012281	63.758414
1756.795109	38.185636	63.763418
1756.437549	36.798121	63.768423
1755.296306	35.978228	63.773428
1754.121304	41.948115	63.778433
1753.744515	42.833011	63.783438
1753.260722	48.978558	63.788442
1752.999210	43.319358	63.793447
1752.755436	42.035201	63.798452
1751.543060	47.167312	63.803457
1750.586760	34.919214	63.808462
1749.975968	46.017906	63.813466
1749.542332	48.056763	63.818471
1748.945457	43.699846	63.823476
1748.499423	45.780098	63.828481
1747.903319	42.760389	63.833486
1746.879013	45.473416	63.838490
1746.185855	42.030706	63.843495
1745.403126	44.945072	63.848500
1744.377444	49.143890	63.853505
1743.794055	42.509166	63.858510
1743.288890	44.217168	63.863514
1742.886286	48.637156	63.868519
1742.367189	43.335857	63.873524
1742.096512	51.593904	63.878529
1741.493130	39.021653	63.883534
1740.345488	44.949352	63.888538
1739.992944	43.523192	63.893543
1738.803332	42.447624	63.898548
1737.893661	43.414012	63.903553
1737.431569	41.131574	63.908558
1736.539166	44.692601	63.913562
1736.450128	42.712049	63.918567
1736.219700	44.994612	63.923572
1734.844433	46.560110	63.928577
1734.302316	44.938547	63.933582
1733.652172	45.152468	63.938586
1732.984898	35.706600	63.943591
1732.449096	47.648138	63.948596
1731.212216	47.672968	63.953601
1730.790540	38.549230	63.958606
1730.105579	52.173507	63.963610
1729.844459	44.110842	63.968615
1729.369316	41.019882	63.973620
1728.555335	45.185076	63.978625
1727.731669	35.286210	63.983630
1726.891165	55.282774	63.988634
1726.875429	42.222921	63.993639
1725.726594	39.511802	63.998644
1724.799146	41.920853	64.003649
1724.674011	44.030564	64.008654
1723.824326	46.722170	64.013658
1723.311416	37.775361	64.018663
1722.004059	42.228673	64.023668
1721.391027	43.780339	64.028673
1721.389956	40.995719	64.033678
1720.597000	47.111526	64.038682
1719.989009	47.284060	64.043687
1719.134519	46.674113	64.048692
1717.955007	51.797865	64.053697
1717.815890	49.484627	64.058702
1717.348760	45.559720	64.063706
1716.588550	42.708020	64.068711
1715.497191	40.508198	64.073716
1714.847558	48.823286	64.078721
1714.653096	41.648948	64.083726
1714.075646	46.817419	64.088730
1713.528649	43.335731	64.093735
1712.780631	52.656831	64.098740
1711.911549	47.354360	64.103745
1711.309488	42.969892	64.108750
1710.527906	46.931238	64.113754
1709.657067	39.313959	64.118759
1709.128535	41.618644	64.123764
1708.360612	43.645950	64.128769
1708.152408	39.187880	64.133774
1707.514743	41.290693	64.138778
1706.485987	38.681940	64.143783
1705.772468	45.766049	64.148788
1705.143026	44.797064	64.153793
1705.080403	41.558573	64.158798
1703.950280	51.367749	64.163802
1702.972206	48.225791	64.168807
1702.350331	47.055321	64.173812
1702.026858	49.828932	64.178817
1701.645377	46.156942	64.183822
1700.631226	51.470486	64.188826
1699.568379	43.738623	64.193831
1699.232854	44.790446	64.198836
1698.373736	50.129828	64.203841
1698.569829	40.985235	64.208846
1697.645903	42.069025	64.213850
1696.800020	34.241198	64.218855
1695.834595	43.245151	64.223860
1695.323271	45.791547	64.228865
1695.158581	47.275150	64.233870
1693.985181	47.805606	64.238874
1693.008491	43.919071	64.243879
1692.646911	45.115391	64.248884
1692.105109	46.379766	64.253889
1691.497911	43.658317	64.258894
1690.367579	53.943797	64.263898
1689.968771	32.219062	64.268903
1689.395577	37.334816	64.273908
1688.962060	40.092790	64.278913
1688.423209	37.532382	64.283918
1687.395842	42.395418	64.288922
1686.836446	37.863824	64.293927
1686.382053	40.405907	64.298932
1685.304174	39.992317	64.303937
1684.464721	36.899315	64.308942
1683.590630	34.448938	64.313946
1683.254753	46.710398	64.318951
1682.936164	39.024323	64.323956
1682.342894	42.742860	64.328961
1682.162931	35.531532	64.333966
1681.013013	39.373194	64.338970
1680.360596	36.523308	64.343975
1679.620239	37.617367	64.348980
1678.283421	37.959313	64.353985
1677.995796	37.719821	64.358990
1676.869646	41.204453	64.363994
1676.449157	41.145349	64.368999
1676.469565	38.298968	64.374004
1676.198872	34.896406	64.379009
1675.447299	31.779984	64.384014
1674.308673	47.326198	64.389018
1673.851091	41.016881	64.394023
1672.684901	40.256185	64.399028
1671.887955	41.578444	64.404033
1671.510529	35.008802	64.409038
1670.858786	44.943847	64.414042
1670.591726	39.176728	64.419047
1669.822927	39.718615	64.424052
1668.580862	46.536597	64.429057
1668.524284	42.284690	64.434062
1667.528367	47.180586	64.439066
1667.079316	44.842472	64.444071
1666.253814	40.760033	64.449076
1665.147438	47.524920	64.454081
1664.893281	34.715862	64.459086
1664.342933	39.094669	64.464090
1664.058253	35.683290	64.469095
1663.303123	43.672928	64.474100
1661.788061	44.495810	64.479105
1661.839985	39.488613	64.484110
1661.102538	49.434124	64.489114
1660.627739	47.415508	64.494119
1659.612430	42.426466	64.499124
1658.349637	37.689644	64.504129
1658.242650	35.499049	64.509134
1657.704412	47.174460	64.514138
1657.490422	45.975472	64.519143
1656.688130	44.906221	64.524148
1655.458233	41.578776	64.529153
1655.244903	37.511055	64.534158
1654.732825	46.414611	64.539162
1653.879817	33.527223	64.544167
1653.047052	36.817011	64.549172
1652.071694	40.700341	64.554177
1651.953784	35.083006	64.559182
1651.148535	44.162455	64.564186
1650.159536	39.380561	64.569191
1649.552523	39.769010	64.574196
1648.825582	50.127615	64.579201
1648.577791	42.081773	64.584206
1648.149229	44.387934	64.589210
1647.519949	42.930057	64.594215
1646.657849	39.512642	64.599220
1645.798789	42.112715	64.604225
1645.441338	31.611509	64.609230
1643.960877	50.859727	64.614234
1643.472935	48.857396	64.619239
1643.041486	41.821652	64.624244
1642.291714	48.728598	64.629249
1642.238065	35.059744	64.634254
1641.642147	46.163969	64.639258
1640.629363	45.672244	64.644263
1639.688419	39.379804	64.649268
1639.108897	43.143476	64.654273
1638.937443	39.985362	64.659278
1637.423335	40.998928	64.664282
1636.981849	39.206849	64.669287
1636.511777	38.264604	64.674292
1636.123015	50.261641	64.679297
1635.973676	36.707343	64.684302
1634.608394	40.198444	64.689306
1634.020444	34.908116	64.694311
1633.460691	38.102492	64.699316
1632.660341	42.412210	64.704321
1631.740187	34.048978	64.709326
1631.076243	40.885514	64.714330
1630.698749	39.576882	64.719335
1630.341723	44.101608	64.724340
1628.939081	33.719156	64.729345
1628.223697	39.212345	64.734350
1627.494623	42.348464	64.739354
1627.270883	36.009893	64.744359
1627.024087	40.250586	64.749364
1626.392857	44.385194	64.754369
1625.659754	32.410798	64.759374
1624.933639	36.079485	64.764378
1624.364426	43.668988	64.769383
1623.115759	37.978988	64.774388
1622.394469	39.975252	64.779393
1621.893665	27.601234	64.784398
1621.366079	40.822021	64.789402
1621.052500	38.869267	64.794407
1620.340032	33.759585	64.799412
1619.085097	42.614006	64.804417
1618.567119	35.674025	64.809422
1618.155530	36.124476	64.814426
1617.946989	39.871787	64.819431
1617.017982	43.191072	64.824436
1615.972783	41.499651	64.829441
1615.850977	33.090009	64.834446
1614.513027	30.423185	64.839450
1613.370199	36.200345	64.844455
1613.122624	33.541634	64.849460
1612.558759	36.222553	64.854465
1612.771572	27.174667	64.859470
1611.997075	36.816966	64.864474
1611.137278	33.979549	64.869479
1610.611611	35.610401	64.874484
1609.728051	41.317983	64.879489
1608.601826	35.108618	64.884494
1607.636413	42.485093	64.889498
1607.585167	40.181560	64.894503
1607.032494	34.052960	64.899508
1606.427817	41.167103	64.904513
1605.414609	35.447587	64.909518
1604.267255	36.330354	64.914522
1603.917541	32.371048	64.919527
1603.574393	33.447749	64.924532
1603.165190	37.840410	64.929537
1602.766972	30.584924	64.934542
1601.494176	41.760430	64.939546
1600.878756	35.219156	64.944551
1600.612554	38.341662	64.949556
1599.377132	42.862452	64.954561
1598.650428	32.016209	64.959566
1597.896724	40.234301	64.964570
1597.355333	23.935195	64.969575
1597.213215	31.343285	64.974580
1596.591128	30.562405	64.979585
1596.171266	34.278635	64.984590
1594.831809	41.039577	64.989594
1594.482390	33.547667	64.994599
1594.090100	32.329706	64.999604
1592.324401	40.066748	65.004609
1592.013129	27.224209	65.009614
1591.457948	36.222928	65.014618
1591.254050	34.866218	65.019623
1590.932921	34.464894	65.024628
1589.669177	34.579221	65.029633
1589.278807	28.599890	65.034638
1588.525488	41.303009	65.039642
1587.676885	32.330733	65.044647
1586.729695	29.786347	65.049652
1585.887181	38.445928	65.054657
1585.542366	32.126603	65.059662
1585.390659	37.850371	65.064666
1584.534749	36.855899	65.069671
1583.771827	28.563907	65.074676
1582.731856	41.165912	65.079681
1582.700176	30.456831	65.084686
1582.208300	38.475617	65.089690
1581.142174	32.046971	65.094695
1580.277592	36.739088	65.099700
1579.224764	39.521366	65.104705
1579.409577	26.010192	65.109710
1578.793056	40.631325	65.114714
1577.814953	42.569056	65.119719
1577.010968	37.872919	65.124724
1576.097669	38.390484	65.129729
1575.730793	36.819963	65.134734
1575.190032	42.791644	65.139738
1574.380207	36.355390	65.144743
1573.550936	29.427041	65.149748
1572.935419	31.330811	65.154753
1572.815184	36.204287	65.159758
1572.046816	33.137879	65.164762
1571.391626	40.233244	65.169767
1570.723338	41.587132	65.174772
1569.848044	36.388216	65.179777
1569.570469	41.849697	65.184782
1568.324715	27.474539	65.189786
1567.449555	33.955119	65.194791
1567.097756	31.418636	65.199796
1566.490856	32.791155	65.204801
1566.134197	30.756942	65.209806
1565.514327	34.933912	65.214810
1564.696745	28.475243	65.219815
1564.020157	33.713107	65.224820
1563.514791	31.060672	65.229825
1562.738394	31.498136	65.234830
1561.451069	41.502652	65.239834
1560.878037	34.661327	65.244839
1560.795651	32.757004	65.249844
1560.337318	33.755814	65.254849
1559.466000	29.496186	65.259854
1558.557471	39.806380	65.264858
1557.847269	35.480145	65.269863
1557.915610	30.512926	65.274868
1556.634325	35.176645	65.279873
1555.887441	39.009507	65.284878
1555.104381	37.121906	65.289882
1554.667179	32.343838	65.294887
1554.272938	31.127772	65.299892
1553.302371	37.500509	65.304897
1552.766045	27.518213	65.309902
1552.131810	38.568604	65.314906
1551.538932	29.401158	65.319911
1550.598261	31.071161	65.324916
1549.460899	34.325800	65.329921
1549.209622	31.828542	65.334926
1548.546186	39.716893	65.339930
1548.400416	31.511352	65.344935
1548.143220	37.985204	65.349940
1546.850385	44.054327	65.354945
1546.343020	34.537381	65.359950
1545.775201	31.122129	65.364954
1544.712288	40.206273	65.369959
1543.875340	31.443486	65.374964
1543.235815	36.839477	65.379969
1542.748917	31.902144	65.384974
1542.250816	37.701460	65.389978
1541.430870	35.026478	65.394983
1540.544281	35.356874	65.399988
1540.180708	42.648766	65.404993
1539.578453	31.538329	65.409998
1539.084805	35.599047	65.415002
1537.951692	34.426282	65.420007
1537.218287	32.336821	65.425012
1536.905479	38.232855	65.430017
1536.566682	31.712300	65.435022
1535.778949	39.560478	65.440026
1534.638163	36.324596	65.445031
1534.445984	32.936387	65.450036
1533.734899	41.360619	65.455041
1532.995764	29.888719	65.460046
1532.166474	32.714341	65.465050
1531.171959	38.158865	65.470055
1530.841692	33.086250	65.475060
1530.238187	35.786100	65.480065
1529.873836	35.560395	65.485070
1528.751861	36.341386	65.490074
1528.018901	31.152987	65.495079
1527.308151	37.246310	65.500084
1526.926904	48.280162	65.505089
1526.700286	32.815766	65.510094
1525.899143	36.729802	65.515098
1525.138090	26.081449	65.520103
1524.527729	37.333063	65.525108
1523.363983	43.438454	65.530113
1522.586194	30.089722	65.535118
1522.009581	30.782468	65.540122
1521.478141	37.287287	65.545127
1521.255528	41.975175	65.550132
1520.683306	36.023179	65.555137
1519.308747	33.389035	65.560142
1518.531368	36.299457	65.565146
1518.123986	33.306591	65.570151
1517.848702	29.830661	65.575156
1517.266765	34.875288	65.580161
1517.010235	35.432006	65.585166
1515.741653	39.494453	65.590170
1515.158975	23.212981	65.595175
1514.959678	28.777143	65.600180
1513.649014	34.234066	65.605185
1512.777100	27.564845	65.610190
1512.365966	34.648240	65.615194
1511.836262	30.465232	65.620199
1511.103227	25.522870	65.625204
1510.426551	27.532572	65.630209
1509.883295	30.790582	65.635214
1509.666542	23.507858	65.640218
1508.871343	29.165149	65.645223
1507.721323	31.510291	65.650228
1506.838354	36.654805	65.655233
1506.610681	27.206972	65.660238
1505.751158	31.150791	65.665242
1504.519904	32.461695	65.670247
1504.223914	23.589300	65.675252
1503.273320	30.782086	65.680257
1503.259359	27.572148	65.685262
1502.981577	31.667952	65.690266
1502.381894	30.001973	65.695271
1501.490638	29.035226	65.700276
1500.682854	37.608879	65.705281
1499.770519	29.291778	65.710286
1498.553429	40.412734	65.715290
1498.409380	27.808583	65.720295
1498.053343	29.456653	65.725300
1497.177813	27.785630	65.730305
1496.710847	30.320275	65.735310
1495.697314	35.629053	65.740314
1494.982345	40.245375	65.745319
1494.532903	30.586771	65.750324
1493.849149	34.706096	65.755329
1493.651233	26.368499	65.760334
1492.276304	30.925697	65.765338
1492.076199	36.513646	65.770343
1491.857064	31.634699	65.775348
1490.653026	33.061138	65.780353
1489.631514	31.186226	65.785358
1488.849434	32.730114	65.790362
1488.341461	28.191981	65.795367
1488.104186	22.733995	65.800372
1487.408170	30.506097	65.805377
1487.269189	24.589342	65.810382
1486.134335	24.803089	65.815386
1485.390204	28.763268	65.820391
1484.961300	28.579370	65.825396
1483.572825	37.568612	65.830401
1482.874412	27.172108	65.835406
1482.470658	22.579564	65.840410
1481.995589	30.601993	65.845415
1481.774757	23.326231	65.850420
1481.005941	35.404165	65.855425
1480.093584	31.054891	65.860430
1479.519347	29.654546	65.865434
1478.866057	31.387713	65.870439
1478.020973	28.677324	65.875444
1476.846284	29.476177	65.880449
1476.651697	22.994222	65.885454
1475.825379	28.670660	65.890458
1475.816237	36.254743	65.895463
1475.220767	22.140588	65.900468
1473.839790	22.406076	65.905473
1474.061667	19.286396	65.910478
1473.020781	23.866206	65.915482
1471.991825	25.974489	65.920487
1471.044876	24.224936	65.925492
1470.355241	26.195705	65.930497
1470.347111	20.395358	65.935502
1469.561396	24.486734	65.940506
1469.243460	30.889811	65.945511
1468.108867	24.688159	65.950516
1467.135789	32.627312	65.955521
1466.839561	26.729244	65.960526
1466.641533	25.482006	65.965530
1465.256067	23.942511	65.970535
1465.056541	33.075533	65.975540
1464.180277	27.209733	65.980545
1464.144045	24.695654	65.985550
1462.919477	34.504139	65.990554
1461.921494	26.593352	65.995559
1461.600347	28.530785	66.000564
1461.069257	34.841581	66.005569
1460.066438	26.169857	66.010574
1459.047147	37.475438	66.015578
1458.866192	36.572433	66.020583
1458.593316	33.364224	66.025588
1457.661612	33.597735	66.030593
1456.983392	27.725691	66.035598
1456.218037	40.372392	66.040602
1455.529247	39.300935	66.045607
1455.719350	28.148169	66.050612
1454.274345	32.159833	66.055617
1453.206836	33.638709	66.060622
1452.619482	35.437099	66.065626
1452.061383	29.709974	66.070631
1451.943683	29.022431	66.075636
1450.988600	32.938876	66.080641
1450.636042	26.376372	66.085646
1450.086498	29.526577	66.090650
1448.982874	31.514267	66.095655
1447.911748	25.436585	66.100660
1447.175883	31.514990	66.105665
1446.718133	32.805478	66.110670
1446.437711	28.593902	66.115674
1445.850147	30.753467	66.120679
1445.898947	33.491581	66.125684
1444.217351	30.053110	66.130689
1444.286054	24.461335	66.135694
1443.246850	26.820429	66.140698
1442.150246	30.723100	66.145703
1441.393746	21.341995	66.150708
1440.370681	36.694842	66.155713
1440.291670	32.903858	66.160718
1440.005850	36.267625	66.165722
1439.624024	31.687372	66.170727
1438.750550	29.938767	66.175732
1437.811577	28.908662	66.180737
1437.405993	26.659886	66.185742
1435.994330	22.214949	66.190746
1435.308333	33.894930	66.195751
1434.925433	27.843479	66.200756
1434.192459	29.642942	66.205761
1434.341880	30.827455	66.210766
1433.830895	32.396079	66.215770
1432.649291	29.256627	66.220775
1432.128957	32.528355	66.225780
1431.058978	29.268652	66.230785
1430.061081	22.813468	66.235790
1429.198691	25.560798	66.240794
1428.832282	18.241952	66.245799
1428.420948	25.992466	66.250804
1428.003970	17.352222	66.255809
1427.921445	24.507969	66.260814
1426.789095	28.501487	66.265818
1426.005181	27.107676	66.270823
1425.438419	30.301625	66.275828
1424.014383	34.805160	66.280833
1423.609125	32.121073	66.285838
1422.565877	36.469456	66.290842
1422.274940	35.169178	66.295847
1421.937080	31.387803	66.300852
1421.619822	35.674400	66.305857
1421.578866	19.757888	66.310862
1420.465195	29.195502	66.315866
1419.526415	33.669212	66.320871
1418.624335	31.179226	66.325876
1417.530542	32.979278	66.330881
1417.031963	27.066074	66.335886
1416.588204	32.243301	66.340890
1416.090431	33.218442	66.345895
1415.828184	31.489382	66.350900
1414.678542	35.017277	66.355905
1414.381217	28.455463	66.360910
1413.796693	32.443907	66.365914
1412.796325	33.032142	66.370919
1412.227526	26.920358	66.375924
1411.220933	33.841363	66.380929
1410.612266	32.031748	66.385934
1409.377574	31.062856	66.390938
1408.763975	31.125963	66.395943
1408.504677	31.184788	66.400948
1408.097054	27.788263	66.405953
1407.601031	33.014803	66.410958
1407.216675	32.401192	66.415962
1406.296365	29.593972	66.420967
1405.583409	26.848411	66.425972
1404.651742	34.407245	66.430977
1404.448584	34.206398	66.435982
1403.362919	33.832015	66.440986
1402.606465	33.422644	66.445991
1402.451671	30.395955	66.450996
1401.474632	37.529897	66.456001
1400.782525	29.415963	66.461006
1400.093090	32.219390	66.466010
1399.433894	29.736534	66.471015
1399.067087	29.374037	66.476020
1397.738273	34.633616	66.481025
1397.235768	23.553113	66.486030
1396.442547	32.766321	66.491034
1396.011822	32.631616	66.496039
1395.670793	29.382210	66.501044
1395.174497	35.088212	66.506049
1394.337896	25.262519	66.511054
1393.752083	25.717046	66.516058
1393.328477	24.158729	66.521063
1392.236800	24.293109	66.526068
1391.296681	25.464738	66.531073
1390.799311	22.222841	66.536078
1390.294056	27.190638	66.541082
1389.493895	22.042937	66.546087
1388.970119	22.662653	66.551092
1387.935612	25.371122	66.556097
1387.203383	30.147912	66.561102
1386.666109	29.413528	66.566106
1386.457356	30.248105	66.571111
1386.237617	18.430340	66.576116
1384.975984	28.678426	66.581121
1384.143105	24.526302	66.586126
1383.787523	24.046900	66.591130
1383.145582	21.714279	66.596135
1382.088056	20.092732	66.601140
1381.418349	26.804060	66.606145
1381.163510	17.688599	66.611150
1380.571662	27.368134	66.616154
1379.691591	25.566982	66.621159
1379.394640	26.030785	66.626164
1378.655901	42.607959	66.631169
1377.320739	27.852880	66.636174
1376.616588	27.569250	66.641178
1375.695087	34.347422	66.646183
1375.322605	30.208843	66.651188
1375.185005	32.967125	66.656193
1374.764192	27.885281	66.661198
1374.440764	29.835703	66.666202
1373.113258	27.227280	66.671207
1372.650043	22.820839	66.676212
1371.670128	33.372669	66.681217
1370.648592	23.473881	66.686222
1370.467481	29.834709	66.691226
1369.481222	35.061918	66.696231
1369.186389	31.103393	66.701236
1368.791383	30.576641	66.706241
1368.166488	27.451221	66.711246
1367.214369	32.086348	66.716250
1366.786836	29.118794	66.721255
1365.512085	22.105230	66.726260
1364.561226	29.219246	66.731265
1364.301679	27.284750	66.736270
1363.881070	28.175089	66.741274
1363.418188	24.555535	66.746279
1362.951601	29.670162	66.751284
1361.542121	28.019419	66.756289
1361.181607	30.735867	66.761294
1360.814043	22.944109	66.766298
1359.892638	19.758596	66.771303
1359.384151	24.802608	66.776308
1358.439901	28.821444	66.781313
1358.173620	24.017826	66.786318
1357.278006	31.017401	66.791322
1356.241718	30.540566	66.796327
1355.970939	33.181244	66.801332
1355.034054	33.554394	66.806337
1354.844617	24.513695	66.811342
1353.603969	28.937642	66.816346
1352.739253	29.674653	66.821351
1352.291641	24.787896	66.826356
1351.874088	32.320200	66.831361
1351.738459	24.024768	66.836366
1350.808192	28.123388	66.841370
1349.902442	32.476745	66.846375
1349.369536	25.338934	66.851380
1348.877608	35.264380	66.856385
1348.152592	24.429014	66.861390
1347.339987	31.017983	66.866394
1346.659493	36.245475	66.871399
1346.089679	34.568478	66.876404
1344.867019	31.172232	66.881409
1344.399827	23.583985	66.886414
1343.975267	31.172599	66.891418
1343.362695	35.092973	66.896423
1343.164605	28.592669	66.901428
1342.124881	34.099637	66.906433
1341.225599	28.114537	66.911438
1340.663341	31.847130	66.916442
1340.250772	31.255364	66.921447
1339.204460	30.573538	66.926452
1338.069054	35.275665	66.931457
1337.927031	25.472033	66.936462
1337.591795	24.875856	66.941466
1337.004251	32.045663	66.946471
1336.302486	22.840410	66.951476
1335.261670	32.570837	66.956481
1334.968564	27.348842	66.961486
1334.274327	29.187907	66.966490
1333.304339	39.429075	66.971495
1332.577904	27.125723	66.976500
1331.948364	32.528051	66.981505
1331.424255	40.205042	66.986510
1331.080793	34.647259	66.991514
1330.101552	28.406782	66.996519
1329.328392	30.843475	67.001524
1328.424146	35.619244	67.006529
1328.283057	30.022978	67.011534
1327.824690	32.203028	67.016538
1326.858651	35.280700	67.021543
1326.237571	27.901435	67.026548
1325.555959	36.223241	67.031553
1325.159755	25.856022	67.036558
1324.003149	28.579199	67.041562
1323.273930	28.668594	67.046567
1323.068681	29.319683	67.051572
1322.172051	33.207952	67.056577
1321.493034	28.902070	67.061582
1320.528236	34.526448	67.066586
1320.021168	35.763295	67.071591
1320.272765	23.395911	67.076596
1319.295724	29.512691	67.081601
1318.256885	15.249893	67.086606
1317.508457	29.534024	67.091610
1317.142716	24.761997	67.096615
1316.370005	17.902038	67.101620
1315.137783	28.758938	67.106625
1314.634698	25.235678	67.111630
1313.749480	33.096248	67.116634
1313.523936	30.874063	67.121639
1313.550965	29.146331	67.126644
1312.398419	40.190853	67.131649
1311.721665	29.412483	67.136654
1311.158941	30.289156	67.141658
1310.357573	30.139279	67.146663
1309.376787	23.342369	67.151668
1308.597500	30.872266	67.156673
1308.438604	33.596088	67.161678
1308.016127	34.452038	67.166682
1307.102535	27.423658	67.171687
1306.428139	28.688690	67.176692
1305.575641	30.661741	67.181697
1305.251909	30.196210	67.186702
1304.782819	25.060554	67.191706
1303.572104	35.254845	67.196711
1303.257723	24.365243	67.201716
1302.212698	34.607308	67.206721
1301.788125	20.598519	67.211726
1300.774487	20.058178	67.216730
1299.955627	25.317139	67.221735
1299.824098	18.364694	67.226740
1299.066138	31.038622	67.231745
1298.807895	22.950361	67.236750
1297.395038	26.133784	67.241754
1296.664574	28.316102	67.246759
1296.666676	21.366063	67.251764
1296.102732	26.674382	67.256769
1295.764803	20.339833	67.261774
1294.668555	20.435557	67.266778
1293.738924	29.118516	67.271783
1293.302399	25.160456	67.276788
1291.960138	31.106651	67.281793
1291.056950	25.292514	67.286798
1290.727174	31.541357	67.291802
1290.459905	30.298837	67.296807
1290.130464	22.338599	67.301812
1289.535617	25.295753	67.306817
1288.634785	24.032548	67.311822
1287.970207	24.882841	67.316826
1287.352196	27.441537	67.321831
1286.783596	23.662184	67.326836
1285.439770	33.317802	67.331841
1285.161997	16.235705	67.336846
1284.704327	24.422548	67.341850
1284.209632	31.399393	67.346855
1282.943057	23.712762	67.351860
1282.060927	29.683568	67.356865
1281.725923	32.673525	67.361870
1281.568502	30.718069	67.366874
1281.099579	28.562976	67.371879
1280.415927	25.973651	67.376884
1279.256429	33.628675	67.381889
1278.785103	27.028321	67.386894
1277.866441	33.575823	67.391898
1276.892487	36.702082	67.396903
1276.671220	23.728617	67.401908
1275.779707	31.517654	67.406913
1275.761893	26.713962	67.411918
1274.963937	21.696846	67.416922
1273.796412	26.632773	67.421927
1273.496477	28.839679	67.426932
1272.562092	36.837397	67.431937
1271.784887	24.075346	67.436942
1270.983297	35.187078	67.441946
1270.177518	30.229555	67.446951
1269.830397	28.575515	67.451956
1269.269165	33.049161	67.456961
1269.515493	32.270622	67.461966
1268.456138	26.604336	67.466970
1267.559567	30.300214	67.471975
1267.270215	25.834609	67.476980
1265.687793	32.911888	67.481985
1265.261653	19.578329	67.486990
1264.713034	24.277059	67.491994
1264.230422	32.359060	67.496999
1263.446462	23.674708	67.502004
1261.983694	36.993764	67.507009
1262.118738	27.925134	67.512014
1261.418920	25.677447	67.517018
1261.008885	29.070441	67.522023
1260.671162	18.194028	67.527028
1259.526282	31.347405	67.532033
1258.662987	22.702481	67.537038
1258.437165	22.281313	67.542042
1257.181956	27.617562	67.547047
1256.504239	17.457570	67.552052
1255.779556	32.375055	67.557057
1255.550656	17.316406	67.562062
1255.130909	23.617405	67.567066
1254.403643	25.020173	67.572071
1253.575843	20.562926	67.577076
1252.598456	30.387373	67.582081
1252.151936	28.687639	67.587086
1252.070488	24.397141	67.592090
1250.545485	32.542407	67.597095
1250.321692	24.707308	67.602100
1249.650735	30.510494	67.607105
1249.070664	25.036092	67.612110
1248.035787	33.581255	67.617114
1247.306659	24.782527	67.622119
1246.799977	25.830082	67.627124
1246.199634	31.159969	67.632129
1245.960252	14.571698	67.637134
1244.844637	28.401699	67.642138
1243.977264	29.809405	67.647143
1243.724115	22.876306	67.652148
1243.201912	29.400192	67.657153
1242.524246	22.378480	67.662158
1241.604361	24.281839	67.667162
1240.836255	26.017551	67.672167
1240.916675	21.218742	67.677172
1239.493270	25.687573	67.682177
1238.986071	21.956818	67.687182
1238.499266	30.296543	67.692186
1237.435711	25.118242	67.697191
1236.401696	21.898645	67.702196
1235.791959	27.829297	67.707201
1235.475104	29.639910	67.712206
1235.092348	35.403574	67.717210
1234.725997	42.467257	67.722215
1234.564475	30.613447	67.727220
1233.374160	36.333647	67.732225
1232.324961	30.011295	67.737230
1231.785045	29.810401	67.742234
1230.296026	27.352328	67.747239
1230.056116	21.569934	67.752244
1229.266939	25.437987	67.757249
1229.038252	11.369690	67.762254
1229.056768	28.122913	67.767258
1228.323249	26.126612	67.772263
1227.913540	15.471402	67.777268
1226.695653	28.180636	67.782273
1225.408782	37.082867	67.787278
1224.630558	26.260743	67.792282
1224.196990	26.241643	67.797287
1223.820265	24.158636	67.802292
1223.239982	35.356611	67.807297
1223.025806	21.735452	67.812302
1222.070542	31.980610	67.817306
1221.280593	27.123096	67.822311
1220.541841	21.285992	67.827316
1219.119244	29.821859	67.832321
1218.597558	29.472982	67.837326
1218.196561	33.055364	67.842330
1217.568108	28.235247	67.847335
1217.621478	27.667173	67.852340
1216.974672	29.489261	67.857345
1216.088393	24.309586	67.862350
1215.254556	19.999977	67.867354
1214.588492	29.849041	67.872359
1214.184372	18.879115	67.877364
1212.418293	31.790667	67.882369
1211.806302	26.349739	67.887374
1211.544999	28.747635	67.892378
1211.255381	26.728050	67.897383
1211.048222	15.578562	67.902388
1210.378554	25.313074	67.907393
1209.599280	21.190340	67.912398
1208.787557	17.675191	67.917402
1208.113419	29.840615	67.922407
1207.193789	13.019910	67.927412
1206.531531	20.892351	67.932417
1206.177672	24.082442	67.937422
1205.613203	28.236476	67.942426
1204.090765	25.157655	67.947431
1204.042060	24.840792	67.952436
1203.289182	28.092770	67.957441
1203.121099	26.238369	67.962446
1202.113684	27.920686	67.967450
1200.965577	28.622391	67.972455
1200.610155	24.861197	67.977460
1199.919371	26.821177	67.982465
1199.784385	28.364736	67.987470
1198.701631	20.967478	67.992474
1197.710605	28.371797	67.997479
1197.394298	25.746149	68.002484
1197.159281	26.953941	68.007489
1196.143469	32.707904	68.012494
1195.404192	25.998795	68.017498
1194.839188	22.936442	68.022503
1194.400562	15.778954	68.027508
1192.876487	29.058896	68.032513
1192.585314	32.568618	68.037518
1191.938116	36.401485	68.042522
1191.412843	28.567035	68.047527
1191.168473	26.530794	68.052532
1189.740714	23.413269	68.057537
1188.853972	26.043115	68.062542
1188.568517	25.257683	68.067546
1188.089106	28.880927	68.072551
1188.339501	27.953493	68.077556
1186.970229	32.128301	68.082561
1186.258422	36.160689	68.087566
1185.685436	19.726420	68.092570
1184.888948	30.064610	68.097575
1183.909888	27.575919	68.102580
1183.181255	32.848949	68.107585
1183.096450	31.839206	68.112590
1182.509198	19.609986	68.117594
1181.408373	27.344024	68.122599
1180.748836	25.052106	68.127604
1180.410105	22.846363	68.132609
1180.123126	31.867127	68.137614
1178.658675	25.377452	68.142618
1177.852918	22.430671	68.147623
1177.643588	15.269834	68.152628
1177.051298	20.667838	68.157633
1176.237729	20.234504	68.162638
1175.074847	24.344947	68.167642
1174.332739	29.561771	68.172647
1174.181932	23.992304	68.177652
1173.815883	30.212229	68.182657
1173.429410	20.696679	68.187662
1172.364743	14.834161	68.192666
1171.261571	20.641448	68.197671
1171.250433	20.687635	68.202676
1170.544325	23.673549	68.207681
1169.422198	17.143627	68.212686
1168.870936	22.049383	68.217690
1168.099499	29.429822	68.222695
1167.714786	22.249570	68.227700
1167.471466	23.042350	68.232705
1166.453510	21.786780	68.237710
1165.896920	21.713138	68.242714
1164.993412	24.452895	68.247719
1163.856113	20.437591	68.252724
1163.094525	24.761764	68.257729
1162.733597	25.133261	68.262734
1162.539811	17.484230	68.267738
1162.120987	24.045299	68.272743
1161.642963	18.232981	68.277748
1160.302924	18.339154	68.282753
1159.834894	21.044339	68.287758
1159.309684	22.631045	68.292762
1158.140158	27.682460	68.297767
1157.926382	25.436343	68.302772
1157.072519	23.363009	68.307777
1156.428822	21.514877	68.312782
1155.631071	19.700713	68.317786
1154.463541	20.528536	68.322791
1154.157729	21.443227	68.327796
1153.635810	19.943172	68.332801
1153.305492	18.160316	68.337806
1153.250930	13.053385	68.342810
1151.814823	26.276771	68.347815
1151.407599	14.687588	68.352820
1150.595719	21.877333	68.357825
1149.770001	22.034170	68.362830
1148.966601	12.655918	68.367834
1148.169577	14.159701	68.372839
1148.012012	10.783382	68.377844
1147.686888	24.176989	68.382849
1146.718594	18.213993	68.387854
1145.623841	21.525097	68.392858
1145.221599	21.707618	68.397863
1145.006657	26.236590	68.402868
1143.119470	16.095561	68.407873
1142.760230	13.986133	68.412878
1142.158768	19.188473	68.417882
1141.915300	22.140227	68.422887
1141.737268	16.180841	68.427892
1140.877424	22.072442	68.432897
1139.956897	16.615961	68.437902
1139.344890	16.032298	68.442906
1138.517515	21.912426	68.447911
1137.905622	14.322025	68.452916
1136.749282	17.707587	68.457921
1136.798896	15.939993	68.462926
1136.496210	16.532475	68.467930
1135.546055	19.295432	68.472935
1134.717254	18.035019	68.477940
1133.932723	21.889741	68.482945
1133.519594	15.594000	68.487950
1132.445413	15.892874	68.492954
1131.570055	21.730171	68.497959
1131.146162	9.351984	68.502964
1130.646619	20.748435	68.507969
1130.435116	10.766657	68.512974
1129.839650	14.430446	68.517978
1128.518354	17.085280	68.522983
1128.044706	14.773270	68.527988
1127.387417	20.031805	68.532993
1126.486252	23.950817	68.537998
1125.952027	19.473726	68.543002
1125.078367	19.067315	68.548007
1125.018748	16.662633	68.553012
1124.449535	24.761574	68.558017
1123.324940	20.660686	68.563022
1122.393626	20.522079	68.568026
1122.097754	17.680295	68.573031
1121.856255	11.478687	68.578036
1120.617989	19.729792	68.583041
1120.152464	13.238954	68.588046
1119.576745	19.403920	68.593050
1118.821221	20.500546	68.598055
1117.915123	9.577392	68.603060
1117.253766	22.316402	68.608065
1116.767418	27.481513	68.613070
1116.527356	19.115995	68.618074
1115.657866	18.701038	68.623079
1114.656976	11.442199	68.628084
1113.833783	19.291370	68.633089
1113.881194	19.605799	68.638094
1113.148454	23.559526	68.643098
1111.796152	27.389456	68.648103
1111.235099	14.493747	68.653108
1110.893427	15.754784	68.658113
1110.401490	13.868330	68.663118
1109.540358	13.912537	68.668122
1108.475253	15.045800	68.673127
1108.324198	19.916285	68.678132
1107.556770	17.988498	68.683137
1107.316858	17.508082	68.688142
1106.184538	20.342609	68.693146
1105.245515	17.125306	68.698151
1105.245728	13.667117	68.703156
1104.414765	24.663692	68.708161
1103.174996	19.246974	68.713166
1102.790259	20.464399	68.718170
1102.171418	19.282563	68.723175
1101.910444	15.268234	68.728180
1100.981583	29.667835	68.733185
1099.887817	21.446018	68.738190
1099.477131	20.932844	68.743194
1098.945966	21.307778	68.748199
1098.892003	15.328660	68.753204
1097.916094	27.012225	68.758209
1096.859078	19.133086	68.763214
1096.493616	22.899071	68.768218
1095.485652	19.722703	68.773223
1094.485874	14.728302	68.778228
1094.059809	23.233423	68.783233
1093.494950	23.679953	68.788238
1093.243082	22.065983	68.793242
1092.869341	22.838516	68.798247
1091.988042	15.653704	68.803252
1091.092117	26.905057	68.808257
1090.687103	15.348658	68.813262
1089.561920	18.147361	68.818266
1088.574741	20.876799	68.823271
1088.430032	23.008562	68.828276
1087.605744	22.173243	68.833281
1087.240349	25.251636	68.838286
1086.913479	24.701474	68.843290
1085.925594	29.151561	68.848295
1085.426215	21.254677	68.853300
1083.983256	21.019280	68.858305
1083.089011	21.715344	68.863310
1082.652050	19.410123	68.868314
1081.821853	31.933145	68.873319
1081.981523	17.030351	68.878324
1081.606928	19.763262	68.883329
1081.212892	17.120037	68.888334
1080.216485	25.212829	68.893338
1078.905867	22.344828	68.898343
1078.771326	20.280088	68.903348
1077.156907	26.774328	68.908353
1076.708813	32.657215	68.913358
1076.258189	21.849273	68.918362
1075.910367	27.580580	68.923367
1075.616355	22.071759	68.928372
1074.960813	27.539773	68.933377
1073.763751	25.609384	68.938382
1073.237298	17.748354	68.943386
1072.748565	22.402893	68.948391
1071.821914	13.217755	68.953396
1070.807236	21.725058	68.958401
1070.559631	25.533798	68.963406
1069.911919	25.394246	68.968410
1069.519209	24.523387	68.973415
1068.852479	20.863789	68.978420
1067.882576	19.406642	68.983425
1067.199562	31.723315	68.988430
1067.052723	20.321394	68.993434
1065.636397	21.067410	68.998439
1065.469000	21.535869	69.003444
1064.343219	29.275497	69.008449
1063.894710	24.032542	69.013454
1063.874135	24.707887	69.018458
1062.499059	23.953900	69.023463
1062.091911	23.222540	69.028468
1061.241859	21.851987	69.033473
1060.485954	20.269327	69.038478
1059.843603	15.809458	69.043482
1059.210228	25.118731	69.048487
1058.798688	20.483359	69.053492
1058.311025	21.105281	69.058497
1057.231501	17.307929	69.063502
1056.284735	18.231564	69.068506
1055.625853	19.568310	69.073511
1055.389110	21.263688	69.078516
1054.904665	33.197095	69.083521
1054.437137	23.232402	69.088526
1053.252620	19.350827	69.093530
1052.721914	26.136299	69.098535
1052.302829	20.522797	69.103540
1050.989097	25.254985	69.108545
1050.351685	15.866133	69.113550
1049.967368	19.773899	69.118554
1049.205344	21.335225	69.123559
1048.911866	20.077980	69.128564
1048.436269	19.259738	69.133569
1047.637558	23.559884	69.138574
1046.834296	15.484273	69.143578
1046.251789	27.409622	69.148583
1045.626348	23.546333	69.153588
1044.446390	24.685280	69.158593
1044.002710	19.063078	69.163598
1043.543155	16.974358	69.168602
1043.022972	26.527410	69.173607
1042.436720	21.142368	69.178612
1041.478138	28.926366	69.183617
1040.954334	17.858833	69.188622
1040.677610	16.117932	69.193626
1039.443542	21.572341	69.198631
1038.819653	12.294890	69.203636
1037.999376	27.588744	69.208641
1037.560260	18.813346	69.213646
1036.528513	6.295355	69.218650
1035.982739	19.839187	69.223655
1035.474167	16.815208	69.228660
1035.044503	16.117399	69.233665
1034.593634	13.970527	69.238670
1033.670254	18.867701	69.243674
1032.583867	17.050617	69.248679
1032.320024	15.716116	69.253684
1031.738372	18.975587	69.258689
1030.718826	20.992650	69.263694
1029.904572	21.013655	69.268698
1029.122657	24.275029	69.273703
1028.907642	17.365867	69.278708
1028.532384	25.670513	69.283713
1028.170423	22.533316	69.288718
1026.776864	21.088400	69.293722
1026.212236	23.460454	69.298727
1026.115144	11.367781	69.303732
1024.827462	19.282996	69.308737
1024.061773	15.412068	69.313742
1023.459241	9.942889	69.318746
1022.953162	21.865537	69.323751
1022.910905	13.741390	69.328756
1022.041150	20.823675	69.333761
1021.535564	23.922805	69.338766
1020.590601	23.101979	69.343770
1019.397377	20.410882	69.348775
1018.618801	6.887477	69.353780
1018.114723	15.804000	69.358785
1017.739478	11.695898	69.363790
1017.746903	12.237471	69.368794
1016.385974	14.359325	69.373799
1015.783644	8.634639	69.378804
1015.190979	17.492716	69.383809
1014.321262	18.992336	69.388814
1013.730116	11.258321	69.393818
1012.723420	8.304149	69.398823
1012.312061	3.602529	69.403828
1012.098497	16.295525	69.408833
1010.944528	13.923054	69.413838
1010.391132	16.780622	69.418842
1009.256370	15.791298	69.423847
1009.329849	9.508048	69.428852
1008.876731	11.516992	69.433857
1007.719147	10.930287	69.438862
1006.987041	22.220246	69.443866
1006.839587	19.932053	69.448871
1006.339759	9.417412	69.453876
1004.986929	25.546674	69.458881
1004.163504	29.120603	69.463886
1003.766669	12.398179	69.468890
1002.871356	26.675759	69.473895
1002.912696	18.725975	69.478900
1001.894541	22.062796	69.483905
1000.952224	24.892366	69.488910
1000.669869	22.477399	69.493914
1000.008169	27.236748	69.498919
999.452311	15.860503	69.503924
998.381217	17.384289	69.508929
997.875872	15.274478	69.513934
997.403981	15.944366	69.518938
996.671234	27.040458	69.523943
995.829104	19.242300	69.528948
995.442140	20.548407	69.533953
995.098845	17.857698	69.538958
993.927992	17.033403	69.543962
992.725335	24.006238	69.548967
992.410840	13.121470	69.553972
992.031017	17.299775	69.558977
991.673200	21.081900	69.563982
990.479432	17.102478	69.568986
989.389566	21.685524	69.573991
989.357025	19.372738	69.578996
988.886713	20.800924	69.584001
988.547420	21.394517	69.589006
987.516211	14.829720	69.594010
986.434140	21.311838	69.599015
985.951800	11.762711	69.604020
985.543170	17.344419	69.609025
984.660974	18.759298	69.614030
984.111984	20.072267	69.619034
983.303000	26.192372	69.624039
983.019669	19.095383	69.629044
981.443536	22.697632	69.634049
980.954816	16.003930	69.639054
980.751209	14.924789	69.644058
980.158657	26.941634	69.649063
979.702274	16.013211	69.654068
978.855421	19.877891	69.659073
977.813885	25.339538	69.664078
977.834309	22.343358	69.669082
977.047358	15.646652	69.674087
976.015751	12.300627	69.679092
974.803069	23.504637	69.684097
974.624555	21.092073	69.689102
974.147826	17.399115	69.694106
973.814345	32.861533	69.699111
973.246417	21.908279	69.704116
972.093322	21.803444	69.709121
971.599090	22.890072	69.714126
971.132177	18.637286	69.719130
969.794480	21.048794	69.724135
968.950357	11.544630	69.729140
968.646586	14.329363	69.734145
968.357237	17.638527	69.739150
968.215111	10.449684	69.744154
966.731722	19.843775	69.749159
966.626257	18.641780	69.754164
965.818789	20.752856	69.759169
964.488040	20.794574	69.764174
963.619148	10.333949	69.769178
963.166937	19.893534	69.774183
962.790416	12.972239	69.779188
962.296125	13.576309	69.784193
961.966479	13.323086	69.789198
961.020605	15.113977	69.794202
960.232019	16.010897	69.799207
960.060739	15.095355	69.804212
959.080620	15.343061	69.809217
957.727967	18.215868	69.814222
957.484156	22.790443	69.819226
956.885679	17.208668	69.824231
956.590255	17.951409	69.829236
955.692177	19.468178	69.834241
954.836294	10.511542	69.839246
954.481287	7.694967	69.844250
953.938478	20.949739	69.849255
952.914641	14.789081	69.854260
952.169545	15.737433	69.859265
951.590265	15.284233	69.864270
951.227586	9.188675	69.869274
950.656348	20.170753	69.874279
949.902831	14.009656	69.879284
949.295218	15.483355	69.884289
948.638052	13.738354	69.889294
947.707214	3.446879	69.894298
946.557486	17.824879	69.899303
946.615734	2.878328	69.904308
946.012254	10.541173	69.909313
945.045657	1.633707	69.914318
944.489995	3.348307	69.919322
943.760337	19.501414	69.924327
943.436598	-2.063023	69.929332
942.146660	7.309746	69.934337
941.225226	8.312974	69.939342
940.746088	9.066030	69.944346
940.497614	13.294401	69.949351
940.029622	12.697330	69.954356
938.998731	16.758476	69.959361
938.268361	8.556190	69.964366
937.991635	10.234284	69.969370
936.855298	13.763409	69.974375
936.886684	8.442536	69.979380
935.799287	18.614169	69.984385
935.106232	15.417717	69.989390
934.616695	14.559137	69.994394
933.911868	16.780049	69.999399
933.366099	12.270153	70.004404
932.084877	19.140392	70.009409
931.675955	12.350422	70.014414
931.714845	6.843845	70.019418
930.549763	8.642824	70.024423
929.994897	4.266849	70.029428
929.106839	13.230298	70.034433
928.695461	14.526107	70.039438
927.964583	7.796844	70.044442
927.003816	14.480456	70.049447
926.545841	3.746286	70.054452
926.068207	13.481812	70.059457
925.265136	10.528387	70.064462
924.369310	10.180770	70.069466
923.271725	18.538879	70.074471
923.089309	12.818353	70.079476
922.707399	12.363710	70.084481
922.154894	14.399525	70.089486
921.968922	-0.221131	70.094490
920.349347	8.732583	70.099495
919.974563	11.161177	70.104500
919.672572	10.788436	70.109505
918.464762	12.862315	70.114510
918.059260	6.544913	70.119514
917.206468	8.787801	70.124519
916.935993	14.726011	70.129524
915.722528	12.355171	70.134529
914.760146	17.263321	70.139534
914.395133	21.065524	70.144538
913.863503	20.721448	70.149543
914.116333	15.374791	70.154548
913.223573	12.974986	70.159553
912.057982	20.749387	70.164558
911.456442	20.104188	70.169562
910.992208	21.417875	70.174567
909.989813	16.796151	70.179572
909.320519	14.447516	70.184577
908.669360	19.418101	70.189582
908.501494	22.745784	70.194586
907.178960	19.865581	70.199591
906.610288	9.212113	70.204596
905.940751	11.605617	70.209601
905.746518	11.400238	70.214606
905.231105	7.659837	70.219610
903.617434	16.035436	70.224615
903.488585	16.169749	70.229620
902.978525	16.132915	70.234625
902.370077	19.801971	70.239630
901.516624	25.055504	70.244634
900.558470	22.462676	70.249639
900.092116	22.693288	70.254644
899.778832	19.617756	70.259649
898.560712	24.527193	70.264654
898.018143	17.864162	70.269658
897.266684	22.062205	70.274663
896.950711	22.448662	70.279668
896.509516	24.337451	70.284673
895.268282	27.659356	70.289678
894.976164	11.164740	70.294682
894.034160	19.580101	70.299687
893.754887	17.174122	70.304692
892.592416	25.435335	70.309697
891.739338	25.240204	70.314702
891.654452	21.521166	70.319706
891.128200	15.024282	70.324711
890.846513	19.390413	70.329716
889.721794	15.835311	70.334721
888.894212	9.960428	70.339726
888.628382	15.776470	70.344730
887.770142	20.333725	70.349735
886.916688	18.269886	70.354740
886.404487	11.009068	70.359745
885.547502	21.140890	70.364750
884.630607	9.620299	70.369754
883.513250	25.423529	70.374759
883.227025	15.570389	70.379764
882.798104	15.697271	70.384769
882.648130	21.157391	70.389774
882.423027	14.355521	70.394778
880.925340	20.697242	70.399783
880.409213	13.829727	70.404788
879.880921	13.593942	70.409793
879.040539	20.370378	70.414798
878.443434	15.084889	70.419802
877.171564	20.345103	70.424807
877.022385	12.187528	70.429812
876.881281	14.777635	70.434817
875.978791	13.817636	70.439822
875.030392	12.860213	70.444826
874.252156	16.201470	70.449831
873.863991	19.217275	70.454836
872.611118	15.633692	70.459841
871.684680	19.324984	70.464846
871.491177	10.010625	70.469850
870.736142	22.949088	70.474855
870.781435	16.414851	70.479860
870.132751	17.286375	70.484865
869.378791	23.016110	70.489870
868.648944	20.789094	70.494874
867.840984	25.745224	70.499879
867.274273	20.442282	70.504884
866.061208	16.256252	70.509889
865.270430	20.667151	70.514894
865.252069	9.959215	70.519898
864.400031	20.243224	70.524903
864.253864	9.407393	70.529908
863.483555	17.598303	70.534913
862.584872	17.213314	70.539918
862.235454	12.497133	70.544922
860.955292	17.503196	70.549927
860.202317	12.499579	70.554932
859.694697	17.081456	70.559937
859.086630	24.804980	70.564942
858.836636	18.511720	70.569946
857.952842	27.906621	70.574951
857.645772	19.908225	70.579956
857.030915	23.649276	70.584961
855.885630	22.478763	70.589966
854.787640	18.599287	70.594970
854.115642	26.339297	70.599975
854.154364	16.090645	70.604980
853.586515	18.807036	70.609985
852.842100	19.526640	70.614990
851.834334	15.604417	70.619994
851.236700	19.371113	70.624999
850.643952	20.708422	70.630004
849.495246	19.212014	70.635009
848.888684	17.891089	70.640014
848.677305	12.115257	70.645018
848.370635	19.686717	70.650023
847.706121	14.892959	70.655028
846.803111	18.733500	70.660033
846.015134	22.789130	70.665038
845.691740	11.618798	70.670042
844.384939	17.474392	70.675047
843.547833	24.576761	70.680052
842.810808	23.494234	70.685057
842.495797	18.263200	70.690062
842.185808	12.876820	70.695066
841.594823	22.155721	70.700071
841.026267	9.255003	70.705076
840.249254	17.240395	70.710081
839.388174	17.857145	70.715086
838.984332	16.828817	70.720090
837.588838	18.066828	70.725095
836.928923	9.487496	70.730100
836.572696	17.049497	70.735105
836.436597	15.842924	70.740110
835.714636	14.969323	70.745114
834.191748	27.963798	70.750119
833.737950	19.443116	70.755124
833.688898	16.128404	70.760129
832.839426	25.297063	70.765134
832.540557	17.997565	70.770138
831.260504	25.113679	70.775143
830.576903	21.422145	70.780148
829.944489	23.382388	70.785153
829.617547	27.580681	70.790158
829.304750	15.937134	70.795162
827.952369	19.057555	70.800167
827.905607	19.106261	70.805172
827.238011	15.404297	70.810177
825.910152	21.761591	70.815182
825.206457	19.372723	70.820186
824.489098	24.651924	70.825191
824.394931	15.190863	70.830196
823.760488	20.888966	70.835201
823.093409	25.748560	70.840206
822.450802	14.643243	70.845210
821.580323	19.733921	70.850215
821.178641	13.027984	70.855220
819.968517	16.792841	70.860225
819.132854	15.099949	70.865230
819.037634	20.278528	70.870234
818.343054	12.824404	70.875239
817.669298	11.695542	70.880244
816.813211	14.273315	70.885249
816.201330	14.397795	70.890254
815.721283	14.695261	70.895258
814.675217	18.922878	70.900263
814.176131	13.927745	70.905268
813.503929	19.789563	70.910273
813.044526	19.243191	70.915278
812.694169	19.245609	70.920282
811.754083	30.557678	70.925287
811.113462	24.594706	70.930292
810.875092	21.931479	70.935297
809.618777	27.528309	70.940302
809.044836	20.502852	70.945306
808.098009	21.579559	70.950311
807.967644	17.315812	70.955316
807.135557	20.869097	70.960321
805.820025	24.357418	70.965326
805.503834	11.110592	70.970330
805.077513	25.045452	70.975335
804.836986	9.525135	70.980340
803.718355	18.285621	70.985345
802.494134	29.981987	70.990350
802.221588	13.318695	70.995354
801.973149	23.451428	71.000359
801.474168	15.264394	71.005364
800.427567	32.259655	71.010369
799.548866	27.667171	71.015374
799.156234	26.589755	71.020378
798.842729	27.920466	71.025383
797.841421	18.532866	71.030388
797.002972	23.124846	71.035393
796.136705	21.454181	71.040398
796.428610	25.490869	71.045402
794.761943	31.641915	71.050407
794.278907	24.784921	71.055412
793.715735	18.301827	71.060417
793.110131	19.623847	71.065422
792.672568	13.403043	71.070426
791.674762	21.743736	71.075431
790.890369	15.876208	71.080436
790.369569	22.806800	71.085441
790.007231	23.665872	71.090446
789.846517	12.028089	71.095450
788.570933	22.277044	71.100455
788.023902	14.960293	71.105460
787.419706	20.393379	71.110465
786.366148	19.534738	71.115470
785.820533	21.258811	71.120474
784.630907	20.502263	71.125479
784.640515	12.134909	71.130484
784.277119	25.173467	71.135489
783.265272	16.394705	71.140494
782.559012	19.461166	71.145498
781.821906	21.475937	71.150503
781.547153	15.047856	71.155508
780.346224	15.333942	71.160513
779.179168	22.659177	71.165518
779.244344	12.029417	71.170522
778.494917	22.185142	71.175527
778.201728	14.529922	71.180532
777.845939	17.928530	71.185537
776.648877	20.473870	71.190542
776.050771	10.547407	71.195546
775.428845	19.957402	71.200551
775.025000	20.457217	71.205556
774.090936	16.822928	71.210561
773.054259	20.952869	71.215566
772.992326	19.188842	71.220570
771.773145	21.174710	71.225575
770.968149	19.385485	71.230580
770.391240	18.963491	71.235585
770.018231	19.313311	71.240590
770.168778	2.216808	71.245594
768.338932	15.894137	71.250599
767.905570	18.322615	71.255604
767.474202	13.387678	71.260609
766.843928	12.540502	71.265614
766.547181	15.278402	71.270618
765.372978	25.539613	71.275623
765.021250	19.111173	71.280628
764.306911	17.181354	71.285633
763.090850	22.002209	71.290638
762.524561	10.504705	71.295642
762.032299	10.351521	71.300647
761.842989	15.406301	71.305652
760.817575	12.538801	71.310657
759.805516	22.961860	71.315662
759.124578	17.010058	71.320666
758.620788	17.585716	71.325671
758.358200	11.415912	71.330676
757.959683	7.021397	71.335681
756.786820	19.084924	71.340686
756.366118	9.212226	71.345690
755.723414	24.171906	71.350695
754.968823	19.383056	71.355700
754.175134	18.606059	71.360705
753.117542	18.035092	71.365710
752.919317	13.654418	71.370714
752.380058	32.011878	71.375719
751.542434	17.772560	71.380724
750.751838	30.336649	71.385729
750.198559	25.268153	71.390734
749.646575	23.825017	71.395738
748.831609	21.822912	71.400743
747.862687	13.559329	71.405748
747.603969	20.793561	71.410753
746.950927	21.071275	71.415758
746.553974	16.838943	71.420762
745.051150	29.448628	71.425767
744.507316	19.412598	71.430772
744.368883	18.778861	71.435777
743.999376	23.237837	71.440782
743.486978	16.461233	71.445786
742.221121	21.301064	71.450791
741.914914	14.250346	71.455796
740.981321	20.169570	71.460801
739.566319	15.843868	71.465806
739.029792	22.693389	71.470810
738.382536	22.331491	71.475815
738.191828	17.142187	71.480820
737.839937	20.995937	71.485825
737.522899	22.303562	71.490830
737.022854	19.806597	71.495834
735.954480	21.498798	71.500839
735.291186	20.639541	71.505844
734.352967	14.399119	71.510849
733.336358	14.630645	71.515854
733.297087	12.066620	71.520858
732.303324	25.473646	71.525863
731.890457	14.393285	71.530868
731.088775	15.380674	71.535873
730.056085	20.159727	71.540878
730.069689	14.422207	71.545882
729.320013	19.771231	71.550887
728.359648	13.641576	71.555892
727.889594	19.733006	71.560897
727.295682	23.010260	71.565902
726.303973	11.033285	71.570906
725.066169	23.862559	71.575911
724.950757	21.261768	71.580916
724.529216	18.394322	71.585921
724.079408	17.408029	71.590926
723.749979	19.545563	71.595930
722.352328	18.358527	71.600935
722.000026	24.136307	71.605940
721.715256	21.901544	71.610945
720.050179	24.516705	71.615950
719.543515	14.151480	71.620954
718.639229	19.943036	71.625959
718.449696	23.562769	71.630964
718.111592	20.872856	71.635969
717.194885	21.301378	71.640974
716.464905	19.869248	71.645978
715.713084	24.236136	71.650983
715.385760	13.287245	71.655988
714.936955	22.614487	71.660993
713.843966	19.052840	71.665998
713.438840	12.459446	71.671002
712.697910	18.341689	71.676007
711.793008	16.448540	71.681012
710.983355	14.177510	71.686017
710.097650	19.198103	71.691022
709.934309	18.513138	71.696026
709.484201	18.673387	71.701031
709.184859	16.843086	71.706036
708.153679	30.126766	71.711041
707.258999	32.642910	71.716046
706.509726	17.716158	71.721050
705.319588	24.349634	71.726055
704.957370	19.782182	71.731060
704.266991	23.582601	71.736065
703.831569	18.889606	71.741070
703.607904	12.839775	71.746074
703.024691	18.053482	71.751079
702.431151	20.305619	71.756084
701.464495	22.751221	71.761089
700.946697	16.333472	71.766094
700.052866	17.633602	71.771098
698.878671	22.526668	71.776103
698.785303	18.197113	71.781108
698.466824	16.861891	71.786113
697.372425	19.975990	71.791118
696.631044	23.570060	71.796122
695.880688	16.574310	71.801127
695.866640	19.853848	71.806132
694.833451	22.064032	71.811137
693.522943	17.068832	71.816142
693.228530	10.924609	71.821146
692.455855	16.684174	71.826151
692.347366	21.005390	71.831156
691.990184	6.998696	71.836161
690.656294	22.584136	71.841166
690.164660	13.183239	71.846170
689.392019	20.158680	71.851175
688.780114	22.412169	71.856180
688.142399	18.495745	71.861185
686.983332	25.431799	71.866190
686.967359	16.742083	71.871194
686.284256	17.097143	71.876199
685.763055	19.023937	71.881204
684.877734	14.402596	71.886209
683.934628	17.327020	71.891214
684.174997	10.391129	71.896218
682.576340	20.978593	71.901223
682.128127	24.606406	71.906228
681.582821	24.622542	71.911233
680.739938	22.107644	71.916238
680.654095	18.182186	71.921242
679.115027	16.695985	71.926247
678.544635	26.208182	71.931252
678.302578	13.354877	71.936257
677.641105	14.496579	71.941262
677.415204	11.899197	71.946266
676.306990	27.513365	71.951271
675.540159	15.877507	71.956276
675.227230	19.240915	71.961281
674.211360	25.214266	71.966286
673.802862	16.464057	71.971290
672.972727	28.819981	71.976295
672.067698	17.589348	71.981300
671.407747	12.129420	71.986305
670.173297	17.514659	71.991310
669.948003	17.738464	71.996314
669.553938	21.871761	72.001319
669.281067	16.037937	72.006324
668.962240	6.030765	72.011329
667.574293	11.445180	72.016334
667.172233	11.577283	72.021338
666.510217	25.406173	72.026343
665.810175	12.509111	72.031348
664.734804	15.091893	72.036353
664.240977	12.876241	72.041358
663.850702	8.811606	72.046362
663.184283	16.311050	72.051367
662.070493	20.079560	72.056372
661.645425	16.646540	72.061377
661.212234	23.042781	72.066382
660.646704	16.616875	72.071386
659.393525	20.136339	72.076391
658.380780	17.829861	72.081396
658.323461	24.659846	72.086401
657.999279	18.465172	72.091406
657.542531	11.578803	72.096410
656.161724	23.091989	72.101415
655.691634	22.167288	72.106420
655.175637	12.041701	72.111425
654.659386	18.429091	72.116430
654.153866	12.279071	72.121434
653.233192	22.462094	72.126439
652.341706	18.816342	72.131444
652.376578	17.434312	72.136449
650.851160	23.029913	72.141454
650.569249	15.445466	72.146458
649.723639	33.474814	72.151463
649.317852	21.969126	72.156468
648.368856	18.061289	72.161473
647.619922	26.054873	72.166478
647.085121	13.462674	72.171482
646.366118	17.042152	72.176487
645.821574	18.598919	72.181492
645.587458	19.227846	72.186497
644.183246	25.458609	72.191502
643.839665	15.220404	72.196506
643.161158	16.997212	72.201511
642.920720	14.190829	72.206516
641.779742	14.133105	72.211521
640.989565	15.840963	72.216526
640.838411	11.697244	72.221530
640.135644	12.429201	72.226535
639.402700	14.865987	72.231540
638.838040	20.899954	72.236545
637.836365	9.489187	72.241550
637.271937	13.941368	72.246554
636.349208	17.485484	72.251559
635.873673	19.952239	72.256564
635.531093	16.911380	72.261569
634.448369	24.171198	72.266574
633.719679	19.586433	72.271578
633.212372	21.842198	72.276583
632.530170	13.176598	72.281588
631.943294	19.430154	72.286593
631.455898	21.290071	72.291598
630.821207	15.054971	72.296602
629.849105	24.648503	72.301607
629.419356	12.958979	72.306612
628.930367	7.944940	72.311617
628.233880	19.715008	72.316622
627.759667	18.360444	72.321626
626.756694	25.161269	72.326631
626.247467	13.624759	72.331636
625.494421	18.108563	72.336641
624.628016	11.453038	72.341646
624.252425	5.771209	72.346650
623.397653	19.321705	72.351655
622.247049	16.734414	72.356660
621.665236	12.903729	72.361665
621.183289	13.382891	72.366670
620.848831	6.152190	72.371674
620.297610	16.117092	72.376679
619.461082	5.162601	72.381684
618.703584	18.308081	72.386689
617.955277	14.434527	72.391694
617.934705	14.589456	72.396698
616.881952	17.564485	72.401703
615.972733	16.345447	72.406708
615.624108	14.478853	72.411713
615.050851	17.566751	72.416718
614.138506	13.662554	72.421722
612.949983	22.768569	72.426727
612.797015	18.940544	72.431732
612.389512	20.743582	72.436737
611.765135	25.052349	72.441742
611.173057	23.204032	72.446746
610.363192	21.529182	72.451751
609.460587	19.653054	72.456756
608.730995	20.356175	72.461761
607.719042	16.792711	72.466766
607.285801	17.939080	72.471770
606.759862	12.617105	72.476775
606.463601	18.237726	72.481780
606.133726	9.695797	72.486785
604.694743	19.002563	72.491790
604.232697	12.974947	72.496794
603.705546	15.706982	72.501799
602.790577	20.230778	72.506804
602.274160	22.823904	72.511809
601.382509	18.067980	72.516814
601.105363	17.680283	72.521818
600.334314	19.892906	72.526823
599.485309	13.770804	72.531828
598.842353	16.562288	72.536833
598.126441	18.939601	72.541838
597.829419	7.143791	72.546842
597.204137	18.501958	72.551847
596.497098	13.645666	72.556852
595.670692	11.751098	72.561857
594.875093	18.353311	72.566862
594.595386	11.326789	72.571866
593.526173	19.055996	72.576871
592.495000	19.370327	72.581876
592.496425	19.054956	72.586881
591.624339	15.745198	72.591886
591.544384	16.002630	72.596890
590.473089	15.143746	72.601895
589.848985	17.949577	72.606900
589.325483	5.317758	72.611905
588.456015	17.285701	72.616910
587.605241	12.095903	72.621914
586.900709	11.574429	72.626919
586.419251	17.694501	72.631924
586.025669	12.159052	72.636929
584.878666	18.224286	72.641934
584.171766	12.014897	72.646938
583.791960	22.185900	72.651943
583.401131	19.928626	72.656948
582.721464	22.054155	72.661953
581.767958	23.816435	72.666958
581.386512	17.887952	72.671962
580.631449	18.979930	72.676967
579.475599	22.403500	72.681972
578.913723	17.771680	72.686977
578.282434	28.443236	72.691982
578.111076	19.070202	72.696986
577.257452	21.393760	72.701991
576.050850	23.044966	72.706996
575.881484	17.475377	72.712001
574.873014	28.834670	72.717006
574.971661	11.989309	72.722010
574.114381	17.402821	72.727015
573.208721	16.176924	72.732020
573.062082	12.125537	72.737025
571.574639	17.286182	72.742030
570.862372	11.875623	72.747034
569.860603	26.771091	72.752039
569.798460	9.976579	72.757044
569.447865	12.513331	72.762049
568.829128	17.866767	72.767054
568.582421	12.981310	72.772058
567.716209	18.353668	72.777063
566.716169	13.312240	72.782068
565.659677	16.346234	72.787073
564.659236	16.893810	72.792078
564.390055	9.506059	72.797082
563.936418	17.592970	72.802087
563.619988	11.149492	72.807092
563.025248	18.605997	72.812097
561.895833	20.003630	72.817102
561.517754	13.394924	72.822106
560.672567	15.486899	72.827111
559.752954	7.027890	72.832116
559.003206	7.683771	72.837121
558.265866	14.953249	72.842126
558.153679	10.782831	72.847130
557.520512	20.104759	72.852135
556.988624	17.269119	72.857140
555.773309	5.744193	72.862145
555.079593	17.587948	72.867150
555.079027	7.276203	72.872154
554.558361	8.523243	72.877159
553.262163	11.754706	72.882164
552.475447	8.366708	72.887169
551.802512	14.156150	72.892174
551.793684	7.067562	72.897178
550.983807	9.661712	72.902183
550.149962	13.254777	72.907188
549.504426	11.629468	72.912193
548.707787	17.112177	72.917198
548.057445	10.385993	72.922202
547.127318	14.888565	72.927207
546.642016	17.128223	72.932212
546.590925	12.110678	72.937217
545.299035	14.505642	72.942222
544.654460	6.501161	72.947226
543.859133	7.560138	72.952231
543.445331	11.780173	72.957236
543.220961	15.255644	72.962241
542.142490	16.545818	72.967246
541.184522	13.722866	72.972250
540.644507	15.242661	72.977255
540.337157	16.808972	72.982260
539.985926	2.454438	72.987265
538.763552	9.908426	72.992270
538.398176	11.414592	72.997274
537.807276	17.555260	73.002279
536.877451	15.508448	73.007284
536.309958	14.695487	73.012289
535.532624	15.207531	73.017294
535.048114	8.874419	73.022298
534.222866	8.883144	73.027303
533.061261	14.179564	73.032308
532.722158	14.935618	73.037313
531.912985	21.588898	73.042318
531.996747	8.048188	73.047322
531.347203	18.820426	73.052327
530.146300	8.108535	73.057332
529.615676	2.900876	73.062337
528.910851	13.806502	73.067342
528.640632	13.056574	73.072346
527.658172	17.125926	73.077351
526.645875	14.989751	73.082356
526.758851	13.562161	73.087361
525.599037	15.620690	73.092366
524.883867	11.254593	73.097370
524.210802	10.009006	73.102375
523.861966	17.490998	73.107380
523.288051	11.621580	73.112385
521.710894	23.421582	73.117390
521.443541	16.494033	73.122394
520.922179	15.889777	73.127399
520.334853	11.771406	73.132404
520.093665	17.244479	73.137409
518.928374	10.959906	73.142414
518.432922	18.816931	73.147418
517.775556	16.756682	73.152423
517.142451	16.351586	73.157428
516.329466	12.190317	73.162433
515.233425	16.880188	73.167438
515.114046	18.085381	73.172442
514.660979	13.161845	73.177447
514.063533	21.940328	73.182452
513.202539	18.067416	73.187457
512.179860	23.769084	73.192462
512.101431	17.448550	73.197466
511.187679	20.429862	73.202471
510.274319	12.914508	73.207476
509.620102	18.530661	73.212481
508.854746	12.895184	73.217486
508.895467	12.512049	73.222490
507.875596	14.627140	73.227495
506.864944	13.936834	73.232500
506.327262	12.745378	73.237505
505.881748	22.441133	73.242510
505.557849	12.032667	73.247514
504.503315	15.288732	73.252519
503.865054	21.550498	73.257524
503.170194	11.360414	73.262529
502.691488	14.991531	73.267534
501.487368	9.536355	73.272538
501.084700	19.378252	73.277543
500.899742	15.897548	73.282548
500.449005	12.471807	73.287553
499.125961	7.595420	73.292558
498.471715	10.858675	73.297562
497.684736	11.443233	73.302567
497.317451	17.247070	73.307572
497.134073	20.670280	73.312577
495.782995	17.436876	73.317582
494.959737	7.353992	73.322586
494.517665	14.366696	73.327591
494.166473	12.524187	73.332596
493.128534	5.635844	73.337601
492.376770	16.709812	73.342606
491.991295	14.789184	73.347610
491.619650	19.787863	73.352615
490.584639	20.880316	73.357620
490.424042	4.667662	73.362625
489.730523	16.706944	73.367630
488.597467	10.286359	73.372634
487.804835	22.618992	73.377639
487.202300	20.083219	73.382644
486.680593	9.050238	73.387649
486.270427	16.072054	73.392654
485.353068	6.198140	73.397658
484.432431	16.163568	73.402663
483.787992	15.203602	73.407668
483.361272	15.112573	73.412673
482.654115	15.662340	73.417678
482.314975	11.709446	73.422682
481.524922	27.001726	73.427687
480.823207	24.894934	73.432692
480.400003	21.969452	73.437697
478.882216	18.259553	73.442702
478.578379	15.953744	73.447706
478.086801	16.300422	73.452711
477.792319	12.829287	73.457716
477.268023	10.109157	73.462721
475.847240	21.743911	73.467726
475.544577	11.474000	73.472730
474.941000	15.553966	73.477735
473.691213	20.205271	73.482740
473.072960	14.946928	73.487745
472.446342	25.463205	73.492750
472.379933	12.734933	73.497754
471.651489	18.993726	73.502759
470.913960	17.346825	73.507764
469.878339	17.742343	73.512769
469.144055	24.817386	73.517774
469.158478	15.339075	73.522778
468.693490	12.607919	73.527783
468.006002	14.436667	73.532788
467.139444	2.711143	73.537793
465.811220	9.887126	73.542798
465.179092	7.747175	73.547802
464.394867	12.499348	73.552807
463.445349	11.939672	73.557812
463.726500	4.574643	73.562817
463.042554	14.697910	73.567822
462.816586	8.407203	73.572826
461.894513	14.584882	73.577831
461.151079	6.482638	73.582836
460.560563	12.542829	73.587841
458.972400	13.619352	73.592846
458.612315	8.669975	73.597850
458.270978	3.181429	73.602855
457.645920	0.909463	73.607860
457.341058	11.374461	73.612865
456.391283	16.231867	73.617870
455.862343	2.714683	73.622874
455.312850	17.246353	73.627879
454.092602	12.088674	73.632884
453.011292	8.832812	73.637889
452.509970	12.937489	73.642894
452.045225	13.021266	73.647898
451.721670	18.389192	73.652903
451.504948	17.933534	73.657908
450.818098	6.542092	73.662913
449.756278	9.089683	73.667918
449.169972	11.941562	73.672922
448.533722	13.686453	73.677927
447.333754	7.615612	73.682932
447.230906	9.870039	73.687937
446.059030	15.743741	73.692942
446.101711	9.268296	73.697946
445.099523	17.496247	73.702951
444.214329	8.842565	73.707956
444.081489	8.245804	73.712961
443.400020	16.621352	73.717966
442.603798	9.399614	73.722970
441.321713	7.705452	73.727975
440.813326	17.007512	73.732980
440.863123	8.416160	73.737985
439.482141	17.278507	73.742990
438.521580	6.468447	73.747994
438.113876	9.977868	73.752999
437.781396	-1.421146	73.758004
437.453999	-0.088182	73.763009
436.958655	17.333406	73.768014
435.868057	11.019628	73.773018
435.379743	14.084562	73.778023
434.543388	13.256121	73.783028
433.583438	3.430024	73.788033
432.885756	20.352407	73.793038
432.370025	17.299749	73.798042
432.231379	14.374667	73.803047
431.491341	22.423650	73.808052
430.540319	12.725441	73.813057
429.685142	16.312479	73.818062
429.430821	10.967771	73.823066
428.844244	18.074477	73.828071
427.622176	7.366021	73.833076
427.234112	14.598792	73.838081
426.308263	9.523530	73.843086
426.261711	11.322692	73.848090
425.352149	16.250974	73.853095
424.396700	13.943352	73.858100
424.041073	12.284495	73.863105
423.487837	14.104476	73.868110
422.387070	14.693329	73.873114
421.457456	23.420677	73.878119
420.712279	15.818635	73.883124
420.712716	18.859304	73.888129
420.221234	21.853781	73.893134
419.829474	14.286886	73.898138
418.607188	14.556049	73.903143
417.973686	11.113718	73.908148
417.515237	16.693961	73.913153
416.656288	16.216069	73.918158
416.160949	13.313136	73.923162
415.116169	13.973498	73.928167
414.566014	13.037950	73.933172
414.378962	11.052598	73.938177
413.055774	14.466634	73.943182
412.741301	16.735864	73.948186
411.967904	13.582343	73.953191
411.309228	13.044150	73.958196
410.483459	11.256784	73.963201
409.638225	12.350566	73.968206
409.485229	10.154775	73.973210
409.210893	15.383968	73.978215
408.458630	14.288235	73.983220
407.662693	11.895274	73.988225
406.789105	19.454592	73.993230
406.100780	7.546143	73.998234
405.248426	15.753381	74.003239
404.512977	23.260724	74.008244
403.944265	7.174632	74.013249
403.577060	15.709846	74.018254
403.023028	13.909140	74.023258
402.107896	14.510997	74.028263
400.939067	12.636376	74.033268
400.960830	15.553792	74.038273
400.420029	24.052019	74.043278
400.170255	17.471787	74.048282
399.070879	13.763073	74.053287
398.240408	15.496349	74.058292
397.261237	6.091240	74.063297
396.118397	12.564329	74.068302
395.949179	8.973893	74.073306
395.541893	16.373740	74.078311
394.950588	12.913652	74.083316
394.856483	8.171067	74.088321
393.737669	8.600376	74.093326
393.082366	10.512326	74.098330
392.269141	10.930783	74.103335
390.979189	18.778820	74.108340
390.574175	12.854138	74.113345
390.022238	17.862635	74.118350
389.450140	16.903781	74.123354
389.109308	23.294793	74.128359
388.788321	10.140315	74.133364
387.962370	11.929647	74.138369
386.906352	22.517521	74.143374
386.635673	14.227990	74.148378
385.356606	20.517786	74.153383
384.535153	11.809815	74.158388
384.277958	12.185391	74.163393
383.302177	22.553891	74.168398
383.209289	6.076572	74.173402
382.529833	12.477391	74.178407
381.629835	13.255046	74.183412
381.237462	7.407204	74.188417
380.718633	16.772438	74.193422
379.651802	16.597359	74.198426
378.940314	15.238084	74.203431
378.263124	8.334882	74.208436
377.994114	6.206472	74.213441
376.520077	19.627046	74.218446
376.267746	0.897942	74.223450
375.627805	5.034184	74.228455
375.040840	5.031795	74.233460
374.801882	11.223633	74.238465
373.288286	14.081388	74.243470
372.551537	5.251112	74.248474
372.055791	11.871822	74.253479
371.820605	8.023811	74.258484
371.623589	8.228941	74.263489
370.616604	13.409318	74.268494
369.978161	7.890867	74.273498
369.310664	10.503381	74.278503
368.252038	9.789239	74.283508
367.598052	10.510342	74.288513
367.085484	6.753852	74.293518
366.465460	-3.749303	74.298522
365.944877	10.832955	74.303527
365.215951	12.486977	74.308532
364.560708	6.471293	74.313537
363.612157	9.210608	74.318542
363.349580	10.375549	74.323546
362.341303	6.464670	74.328551
361.196101	9.531807	74.333556
361.066207	3.358274	74.338561
360.399582	9.667163	74.343566
359.964558	4.799140	74.348570
359.841400	9.460169	74.353575
358.702242	11.446092	74.358580
358.206431	2.771394	74.363585
357.408131	6.261074	74.368590
356.400381	13.996334	74.373594
355.698639	12.905182	74.378599
355.032877	8.045549	74.383604
355.278457	12.168396	74.388609
353.631646	10.521375	74.393614
353.100786	11.046232	74.398618
352.509063	7.881125	74.403623
351.900529	11.009390	74.408628
351.548016	5.538416	74.413633
350.178787	22.085280	74.418638
349.967196	11.627411	74.423642
349.321005	9.333611	74.428647
348.769603	4.501487	74.433652
347.882643	5.043678	74.438657
346.927936	24.710036	74.443662
346.593441	12.377766	74.448666
345.898594	11.435334	74.453671
345.637821	11.155448	74.458676
344.996809	13.421536	74.463681
343.687675	15.737344	74.468686
342.996248	13.968014	74.473690
342.544639	12.655641	74.478695
342.338406	12.042198	74.483700
341.324765	10.926645	74.488705
340.552023	19.152752	74.493710
340.504469	2.717108	74.498714
339.633702	6.647291	74.503719
338.414138	15.017160	74.508724
337.781617	10.035535	74.513729
337.098554	11.724833	74.518734
337.043560	14.607171	74.523738
336.258879	15.591974	74.528743
335.404491	23.208180	74.533748
334.713158	11.459514	74.538753
333.943040	10.816099	74.543758
333.668466	7.971042	74.548762
332.699614	10.242078	74.553767
331.638364	10.840443	74.558772
331.558226	12.227051	74.563777
330.883920	9.355820	74.568782
330.484265	7.959472	74.573786
329.333584	10.453465	74.578791
328.672584	11.566795	74.583796
328.531888	14.383942	74.588801
327.587493	13.061808	74.593806
327.088934	9.962284	74.598810
326.243255	7.563088	74.603815
325.573997	18.735905	74.608820
324.603247	8.503135	74.613825
323.586502	10.434867	74.618830
323.251646	12.967561	74.623834
322.899515	19.404534	74.628839
322.359523	11.676782	74.633844
322.098444	8.835883	74.638849
320.665774	12.453503	74.643854
320.420847	-2.482473	74.648858
319.923976	8.604509	74.653863
318.851733	9.925324	74.658868
317.930066	13.858898	74.663873
317.207383	15.723258	74.668878
317.102988	18.615048	74.673882
316.564010	12.478339	74.678887
315.552642	10.066133	74.683892
314.995467	9.860306	74.688897
314.321525	20.171248	74.693902
313.931455	15.461653	74.698906
312.625871	9.139629	74.703911
311.785317	13.957594	74.708916
311.715938	8.958753	74.713921
311.091972	23.989606	74.718926
311.125066	13.428083	74.723930
309.897065	14.551373	74.728935
308.944998	16.389220	74.733940
308.662005	3.490497	74.738945
307.544192	20.175500	74.743950
307.072849	13.066036	74.748954
306.532409	12.299283	74.753959
305.362955	18.180542	74.758964
304.744721	10.962027	74.763969
303.906638	15.202415	74.768974
303.530255	12.687416	74.773978
302.937560	21.219158	74.778983
302.579842	13.312540	74.783988
302.295954	5.502970	74.788993
301.124885	9.556733	74.793998
300.623391	10.433324	74.799002
300.188033	8.217897	74.804007
298.858166	12.910432	74.809012
298.571848	10.032558	74.814017
297.567975	10.074568	74.819022
297.254683	4.772401	74.824026
296.313827	11.404148	74.829031
295.615648	8.478385	74.834036
295.265617	10.603478	74.839041
294.587239	15.412943	74.844046
294.046005	7.264339	74.849050
292.798965	9.016744	74.854055
292.023273	11.611831	74.859060
292.005908	11.318381	74.864065
291.376532	22.311376	74.869070
290.684545	13.133359	74.874074
289.689986	20.180542	74.879079
289.039460	15.611823	74.884084
288.953001	9.297327	74.889089
287.755248	13.134569	74.894094
286.894745	14.394835	74.899098
286.462552	17.345188	74.904103
286.082382	16.929795	74.909108
285.799122	15.026026	74.914113
284.355357	24.280093	74.919118
284.044075	9.794678	74.924122
283.316492	12.550838	74.929127
282.172659	14.548579	74.934132
281.566947	15.112193	74.939137
280.916313	13.240182	74.944142
280.216796	13.697320	74.949146
279.874859	15.988289	74.954151
279.495588	15.476556	74.959156
279.134498	9.063911	74.964161
278.144096	12.413924	74.969166
277.546853	8.831809	74.974170
276.906173	5.512096	74.979175
275.593536	14.746835	74.984180
275.411329	8.187398	74.989185
274.595908	14.851198	74.994190
274.076655	11.862223	74.999194
272.982681	11.406079	75.004199
272.035267	10.913955	75.009204
272.240652	12.013764	75.014209
271.586212	9.792266	75.019214
270.886122	11.190973	75.024218
270.077052	8.891622	75.029223
269.372381	13.533389	75.034228
269.096444	6.769692	75.039233
268.058676	25.104118	75.044238
267.115049	13.977616	75.049242
266.341066	10.496223	75.054247
265.996214	11.690059	75.059252
265.797814	10.515536	75.064257
264.882313	11.216854	75.069262
264.035790	11.301605	75.074266
263.172090	8.356506	75.079271
262.667567	7.850551	75.084276
262.698533	8.538180	75.089281
261.568112	10.265701	75.094286
260.897034	12.924546	75.099290
260.438312	13.529389	75.104295
259.410229	19.143694	75.109300
258.400477	9.363469	75.114305
257.773139	12.554679	75.119310
257.474554	9.844352	75.124314
256.993092	9.057169	75.129319
256.111525	3.571208	75.134324
255.318330	2.086222	75.139329
254.640433	6.468247	75.144334
254.127455	7.073856	75.149338
254.039623	2.874353	75.154343
253.092384	9.735797	75.159348
252.330585	-0.956034	75.164353
251.634838	15.035618	75.169358
250.511132	7.345755	75.174362
249.606070	0.423737	75.179367
249.031905	10.292983	75.184372
249.080255	0.713096	75.189377
248.566110	9.919892	75.194382
248.031584	7.964722	75.199386
247.136318	9.720993	75.204391
246.136857	4.890944	75.209396
245.697939	0.914579	75.214401
244.900101	14.594844	75.219406
243.799854	10.397473	75.224410
243.377637	15.134569	75.229415
243.065676	11.718300	75.234420
242.738430	7.347225	75.239425
241.297129	9.231555	75.244430
240.665548	4.751301	75.249434
240.395390	5.397049	75.254439
239.802260	13.146670	75.259444
239.448389	0.905842	75.264449
238.030150	11.177754	75.269454
237.562255	2.922857	75.274458
237.518724	10.136982	75.279463
236.833202	3.329781	75.284468
235.618995	0.025825	75.289473
234.902538	9.810522	75.294478
234.121395	2.618008	75.299482
233.874022	2.764944	75.304487
232.775668	6.963266	75.309492
232.149932	-3.840137	75.314497
231.484320	10.541315	75.319502
231.149280	0.713463	75.324506
231.072559	0.722800	75.329511
229.777304	5.925530	75.334516
229.225262	8.984887	75.339521
228.440236	10.816632	75.344526
227.712128	4.927734	75.349530
226.628596	11.473438	75.354535
225.959646	11.168754	75.359540
225.959477	13.272769	75.364545
225.280208	13.772429	75.369550
224.585471	9.893626	75.374554
223.599577	3.306214	75.379559
223.154063	13.145492	75.384564
222.758056	3.612799	75.389569
221.912596	4.339236	75.394574
220.918545	-2.223216	75.399578
220.498683	10.799100	75.404583
220.037461	7.980665	75.409588
219.390038	4.163710	75.414593
218.098717	9.756917	75.419598
217.859958	7.404501	75.424602
217.464456	5.785153	75.429607
216.566747	8.458065	75.434612
215.969819	1.718751	75.439617
215.263090	11.139191	75.444622
214.796407	11.059313	75.449626
214.245899	4.468720	75.454631
213.184975	7.210236	75.459636
212.859898	5.227988	75.464641
212.174563	7.600525	75.469646
211.178125	8.470891	75.474650
210.356693	5.662582	75.479655
209.638075	8.414178	75.484660
209.474728	6.795663	75.489665
208.813064	10.416571	75.494670
207.748061	10.749073	75.499674
206.990418	10.220408	75.504679
206.328564	10.439743	75.509684
206.331087	2.899928	75.514689
205.410266	11.032974	75.519694
204.286985	6.372502	75.524698
203.896211	0.740498	75.529703
203.312689	11.478596	75.534708
203.267996	7.488268	75.539713
201.595344	13.170672	75.544718
201.224027	7.120811	75.549722
200.636477	10.999572	75.554727
200.104602	10.259863	75.559732
199.666125	-5.280751	75.564737
198.879362	11.184323	75.569742
198.277122	5.814702	75.574746
197.696256	7.621788	75.579751
196.226573	8.731627	75.584756
195.730904	3.223586	75.589761
194.936892	11.547734	75.594766
194.702519	11.265232	75.599770
194.514560	9.882463	75.604775
193.611010	6.183629	75.609780
193.032523	0.089532	75.614785
192.227133	12.078882	75.619790
191.502304	2.754753	75.624794
190.412095	6.256333	75.629799
189.908889	4.166869	75.634804
189.538800	-4.931534	75.639809
188.888130	10.608216	75.644814
187.995951	3.334074	75.649818
187.053404	4.400867	75.654823
186.607843	12.637916	75.659828
186.333861	6.261867	75.664833
185.721406	20.163332	75.669838
185.237733	2.718587	75.674842
184.422363	1.470558	75.679847
183.429512	5.868127	75.684852
183.244068	-2.390789	75.689857
182.073323	8.904586	75.694862
181.590573	8.004079	75.699866
180.998704	8.049829	75.704871
179.797305	13.907847	75.709876
179.450676	-1.647410	75.714881
178.296681	7.803352	75.719886
178.022401	8.703662	75.724890
177.672776	12.525565	75.729895
177.071383	12.197507	75.734900
176.976829	14.554699	75.739905
175.735399	9.435248	75.744910
175.119110	11.913483	75.749914
174.039940	10.012063	75.754919
172.891834	7.517641	75.759924
172.700854	4.578851	75.764929
172.022949	11.449414	75.769934
171.710007	7.298429	75.774938
171.444894	8.542643	75.779943
170.527634	12.256360	75.784948
170.011504	-1.655433	75.789953
169.225355	6.722660	75.794958
168.244333	11.903698	75.799962
167.125004	6.667007	75.804967
166.616910	14.587590	75.809972
166.175964	9.752095	75.814977
165.904593	13.697144	75.819982
165.298900	9.458797	75.824986
164.454705	9.429666	75.829991
163.615459	11.180186	75.834996
163.309299	1.726227	75.840001
162.173162	5.952680	75.845006
161.357184	2.746114	75.850010
160.901320	9.418840	75.855015
160.424912	11.382747	75.860020
160.127663	6.357177	75.865025
159.299414	18.055282	75.870030
158.389345	9.143915	75.875034
158.016423	11.886132	75.880039
157.161383	17.236327	75.885044
156.638317	5.262204	75.890049
155.561520	6.785671	75.895054
154.920878	7.375387	75.900058
154.741723	15.599920	75.905063
153.617375	18.137103	75.910068
153.250485	3.728411	75.915073
152.704524	12.874058	75.920078
151.833418	1.220379	75.925082
150.902663	2.102373	75.930087
149.654403	18.197917	75.935092
149.416597	5.318838	75.940097
148.912853	11.073498	75.945102
148.827571	8.679268	75.950106
148.538616	2.248844	75.955111
147.188292	3.112589	75.960116
146.846843	5.171674	75.965121
146.018362	15.489938	75.970126
144.831347	4.348701	75.975130
144.113036	5.307209	75.980135
143.716268	14.583613	75.985140
143.228691	7.612408	75.990145
142.485911	8.590589	75.995150
141.979070	7.335952	76.000154
141.112277	6.553470	76.005159
140.591450	11.670591	76.010164
140.174995	5.072836	76.015169
139.762542	7.241020	76.020174
138.486968	4.331690	76.025178
137.850677	5.865343	76.030183
137.261715	13.535465	76.035188
136.639007	0.676773	76.040193
135.569575	8.579639	76.045198
134.969747	4.310405	76.050202
134.778808	3.245095	76.055207
133.821700	2.841307	76.060212
133.763063	0.247282	76.065217
132.785527	4.860053	76.070222
131.891424	-3.259029	76.075226
131.538964	1.951092	76.080231
130.623504	6.434112	76.085236
129.913515	1.076967	76.090241
129.289306	-0.808676	76.095246
128.690975	2.579791	76.100250
128.446376	6.230402	76.105255
127.223297	1.163249	76.110260
126.641897	-1.319020	76.115265
125.898334	3.453565	76.120270
125.764566	1.035530	76.125274
124.954521	7.706394	76.130279
123.691843	10.797101	76.135284
123.553532	0.437990	76.140289
123.066459	18.142124	76.145294
121.904594	10.590885	76.150298
121.237440	4.644995	76.155303
120.774601	9.115760	76.160308
120.576946	2.196102	76.165313
119.251906	18.297593	76.170318
118.669965	5.569602	76.175322
118.159694	5.324801	76.180327
117.547359	5.298134	76.185332
117.084911	1.782882	76.190337
115.906631	9.297824	76.195342
115.053392	12.321660	76.200346
115.110510	-0.102955	76.205351
114.024778	11.752918	76.210356
113.075411	3.549611	76.215361
112.242822	13.609907	76.220366
111.698572	9.293965	76.225370
111.738067	8.743859	76.230375
111.587301	14.806520	76.235380
110.800452	3.756030	76.240385
109.732685	10.680898	76.245390
109.350644	10.147556	76.250394
108.091493	5.644426	76.255399
107.032295	10.735448	76.260404
106.874432	5.323370	76.265409
106.460788	3.273259	76.270414
105.733867	0.293793	76.275418
105.001034	0.100260	76.280423
104.245316	14.822541	76.285428
103.963855	-7.139415	76.290433
102.504730	2.367921	76.295438
101.870763	14.225868	76.300442
101.412130	1.307903	76.305447
101.042226	9.597549	76.310452
100.796122	6.956150	76.315457
99.596563	14.808821	76.320462
98.626732	9.355926	76.325466
98.136271	11.326816	76.330471
97.474418	7.411271	76.335476
97.306310	10.127137	76.340481
96.258569	20.221756	76.345486
95.469771	11.024561	76.350490
95.083790	12.817934	76.355495
94.521768	8.359747	76.360500
94.087254	2.168599	76.365505
92.842528	9.375593	76.370510
92.112445	5.122415	76.375514
91.881640	11.439121	76.380519
90.598953	11.965670	76.385524
90.312614	3.615623	76.390529
89.385634	11.153577	76.395534
89.086581	4.779968	76.400538
89.049037	11.018541	76.405543
87.627866	8.963543	76.410548
87.153276	-4.404467	76.415553
86.359348	0.428201	76.420558
86.066772	2.777551	76.425562
85.027282	5.443158	76.430567
84.330993	10.570926	76.435572
83.843972	-1.237021	76.440577
83.165024	9.738668	76.445582
82.394040	5.782185	76.450586
81.478308	0.065198	76.455591
80.927156	11.335907	76.460596
80.509079	-7.341426	76.465601
80.031068	4.272437	76.470606
79.325088	4.361644	76.475610
79.032849	6.223648	76.480615
77.935817	13.407094	76.485620
77.009379	4.197171	76.490625
75.982603	6.229952	76.495630
75.505226	9.496634	76.500634
75.109292	-1.948934	76.505639
74.635422	10.829680	76.510644
74.554705	4.681455	76.515649
73.294463	1.088452	76.520654
72.535722	-1.572104	76.525658
72.414126	3.582276	76.530663
70.698885	6.462908	76.535668
70.451763	0.508390	76.540673
69.778835	1.229438	76.545678
69.559570	2.469502	76.550682
68.719949	5.063810	76.555687
67.448515	9.866990	76.560692
67.202563	4.618783	76.565697
66.373245	3.973859	76.570702
65.911056	4.039954	76.575706
65.785925	5.916307	76.580711
64.371588	2.522934	76.585716
64.267655	-4.253961	76.590721
63.664199	2.396580	76.595726
62.442838	1.795266	76.600730
61.620306	0.791281	76.605735
60.945845	7.606121	76.610740
60.729130	1.299813	76.615745
59.951047	4.589229	76.620750
59.313333	5.134346	76.625754
58.668384	1.829574	76.630759
57.959220	1.972913	76.635764
57.862343	1.800961	76.640769
56.636567	9.203652	76.645774
56.021178	-3.060065	76.650778
55.615236	-0.489195	76.655783
54.670008	6.657426	76.660788
54.112281	2.122872	76.665793
53.174460	7.940476	76.670798
52.394822	5.007283	76.675802
52.058528	-0.381056	76.680807
51.673214	7.999362	76.685812
50.835512	1.678565	76.690817
49.773466	5.592039	76.695822
49.372138	6.140455	76.700826
49.139291	-1.625159	76.705831
47.972578	6.545575	76.710836
47.229734	-10.107105	76.715841
46.637363	2.087990	76.720846
46.214504	-5.473841	76.725850
45.898202	4.557728	76.730855
44.456324	3.698275	76.735860
44.020170	2.708360	76.740865
43.848970	4.036956	76.745870
43.187534	4.833451	76.750874
42.168123	-1.433123	76.755879
41.410036	12.466347	76.760884
40.722722	-4.307162	76.765889
40.623386	7.910221	76.770894
39.131434	-3.422008	76.775898
38.397748	-3.008237	76.780903
37.705581	2.410627	76.785908
37.291197	-4.367207	76.790913
36.791090	10.088793	76.795918
36.533207	5.719308	76.800922
35.908169	2.042347	76.805927
34.705624	6.648467	76.810932
34.620506	-2.670403	76.815937
33.373187	3.120879	76.820942
32.648794	16.664885	76.825946
32.459522	4.653330	76.830951
31.736292	15.207150	76.835956
31.545440	4.356523	76.840961
30.153347	4.845361	76.845966
29.532473	1.079426	76.850970
29.195353	5.672079	76.855975
28.661131	6.427784	76.860980
27.814541	8.854478	76.865985
27.159417	10.083647	76.870990
26.167812	7.550141	76.875994
25.237416	1.177908	76.880999
24.052681	9.807282	76.886004
24.075813	1.914101	76.891009
23.702585	4.448217	76.896014
22.964697	-2.224391	76.901018
23.244378	1.167543	76.906023
21.869970	9.559084	76.911028
21.052853	-0.507213	76.916033
20.389821	4.110621	76.921038
19.666581	7.370800	76.926042
18.608537	0.653067	76.931047
18.247595	4.345898	76.936052
17.930712	1.775729	76.941057
17.418407	6.426292	76.946062
16.339241	8.282945	76.951066
15.689039	4.608427	76.956071
15.101884	15.282473	76.961076
14.734651	3.830762	76.966081
13.606712	12.958877	76.971086
12.756473	0.071875	76.976090
12.109111	0.762050	76.981095
11.808434	10.691780	76.986100
11.669190	-1.770883	76.991105
10.394878	6.973713	76.996110
9.729512	2.863208	77.001114
9.612077	11.673998	77.006119
8.466112	9.911047	77.011124
7.880452	7.257595	77.016129
6.959636	5.077093	77.021134
6.647272	5.575053	77.026139
6.077171	0.343874	77.031143
4.799235	4.783832	77.036148
4.261977	0.411612	77.041153
3.787300	1.206709	77.046158