Fri Mar 05 18:08:29 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.343223	100.298001	0.000000
0.778179	89.382139	0.005005
-0.603503	51.082110	0.010010
-2.452917	11.722147	0.015014
-6.118797	-6.987444	0.020019
-11.773226	1.641924	0.025024
-16.482170	-14.889010	0.030029
-21.392045	-5.657713	0.035034
-25.669252	-11.846209	0.040038
-29.215822	-11.674556	0.045043
-32.983893	-5.257378	0.050048
-36.014890	-12.206067	0.055053
-39.897526	-0.979706	0.060058
-43.557368	-8.778993	0.065062
-47.262315	-8.550508	0.070067
-51.059854	-1.141404	0.075072
-54.629469	-11.927692	0.080077
-58.719277	5.545091	0.085082
-62.680265	-5.412146	0.090086
-66.118071	-6.929400	0.095091
-70.167103	4.806116	0.100096
-73.642812	-6.846703	0.105101
-77.589898	-7.356995	0.110106
-81.264248	-3.955707	0.115110
-85.013968	-9.565919	0.120115
-89.133992	-6.594995	0.125120
-92.642225	-13.864867	0.130125
-96.583325	-2.862489	0.135130
-100.276086	-5.315172	0.140134
-103.711852	-4.765266	0.145139
-107.353759	-9.968434	0.150144
-111.036835	-16.778283	0.155149
-115.222577	-7.991939	0.160154
-119.180982	-6.767247	0.165158
-122.655312	-11.183403	0.170163
-126.982027	-6.534638	0.175168
-130.661085	-8.749757	0.180173
-134.677680	-3.756215	0.185178
-138.329303	-4.059660	0.190182
-141.536849	-7.487010	0.195187
-145.715557	-2.984833	0.200192
-148.859616	-9.858561	0.205197
-152.789388	0.039782	0.210202
-156.468392	0.049823	0.215206
-160.184981	-2.020487	0.220211
-164.133974	1.749612	0.225216
-167.711972	-9.028852	0.230221
-171.633288	-4.941454	0.235226
-175.700013	-7.193988	0.240230
-179.417252	-8.702756	0.245235
-183.235926	-7.990702	0.250240
-186.782488	-16.317201	0.255245
-190.883044	-6.057228	0.260250
-194.480386	-11.092325	0.265254
-197.541755	-10.862240	0.270259
-201.570462	-7.897817	0.275264
-205.273343	-12.815127	0.280269
-209.276616	-6.129908	0.285274
-212.860901	-3.085005	0.290278
-216.769803	-3.476581	0.295283
-220.557572	-2.375155	0.300288
-224.063645	-6.464390	0.305293
-228.238353	2.041258	0.310298
-231.709205	-10.745938	0.315302
-235.763939	-4.984462	0.320307
-239.613816	-5.074757	0.325312
-243.032310	-15.419650	0.330317
-247.203489	-8.898388	0.335322
-250.997991	-8.607986	0.340326
-254.584339	-17.989338	0.345331
-258.319078	-14.297447	0.350336
-261.487270	-10.155075	0.355341
-265.590700	-13.013466	0.360346
-269.752214	-17.605145	0.365350
-273.248437	-10.019879	0.370355
-276.809470	-7.574696	0.375360
-280.758241	-11.238356	0.380365
-284.984339	-4.712993	0.385370
-288.060171	-13.912432	0.390374
-291.958926	-9.095147	0.395379
-295.862357	-13.032530	0.400384
-299.595253	-10.380101	0.405389
-303.604160	-5.652448	0.410394
-307.179128	-7.959605	0.415398
-310.684175	-11.380231	0.420403
-314.672852	-3.547552	0.425408
-317.983794	-11.372134	0.430413
-321.835323	-9.053977	0.435418
-325.655131	-5.373632	0.440422
-329.568835	-5.791067	0.445427
-334.020501	-4.845251	0.450432
-337.231453	-9.527068	0.455437
-341.061840	-12.540885	0.460442
-344.959550	-9.417365	0.465446
-348.594379	-6.753709	0.470451
-352.427402	-7.739086	0.475456
-355.998812	-8.521793	0.480461
-359.701314	-5.044632	0.485466
-363.151574	-8.126990	0.490470
-366.960466	-5.645255	0.495475
-371.181511	2.294004	0.500480
-374.986016	-13.831782	0.505485
-378.605296	-0.246798	0.510490
-382.561018	-4.795443	0.515494
-386.025312	-6.637595	0.520499
-390.118523	-9.308163	0.525504
-393.802577	-2.802933	0.530509
-397.384622	-6.706308	0.535514
-401.179831	-5.007311	0.540518
-404.954370	-13.539920	0.545523
-408.880468	-2.711356	0.550528
-412.405986	-16.577648	0.555533
-416.044431	-6.865780	0.560538
-419.962524	-8.900350	0.565542
-423.363437	-4.391019	0.570547
-427.526053	3.870172	0.575552
-431.436748	-12.549224	0.580557
-435.349378	-6.174593	0.585562
-439.039623	-6.840425	0.590566
-442.263860	-8.454320	0.595571
-446.343013	0.966846	0.600576
-449.878917	-9.179207	0.605581
-453.962640	-4.781566	0.610586
-458.054839	-7.034277	0.615590
-461.312455	-0.425160	0.620595
-465.199379	-3.368244	0.625600
-468.481265	-16.303510	0.630605
-472.728176	-4.866940	0.635610
-476.401830	-5.719871	0.640614
-480.020757	-10.618610	0.645619
-484.255600	-3.377140	0.650624
-488.015307	-12.337765	0.655629
-491.481956	-7.656990	0.660634
-495.100388	-13.908833	0.665638
-498.666046	-4.047620	0.670643
-502.697248	-1.929140	0.675648
-506.566539	-7.607881	0.680653
-510.520856	-4.796758	0.685658
-514.124983	-8.567112	0.690662
-517.884891	-3.636027	0.695667
-521.649183	-9.113889	0.700672
-525.006512	-8.889730	0.705677
-529.117636	-1.261083	0.710682
-532.854025	-4.267525	0.715686
-536.422101	-15.017011	0.720691
-540.419347	-7.275650	0.725696
-543.751542	-11.215553	0.730701
-547.852567	-8.168043	0.735706
-551.675833	-10.272734	0.740710
-555.307967	-14.155246	0.745715
-559.632064	-3.236065	0.750720
-562.999769	-0.573759	0.755725
-566.902871	-1.505016	0.760730
-570.788521	-5.350161	0.765734
-574.187810	-10.939862	0.770739
-578.217831	2.722052	0.775744
-581.617064	-11.263492	0.780749
-585.668614	-0.278995	0.785754
-589.356440	-5.612842	0.790758
-593.219675	-3.087376	0.795763
-596.686668	6.305625	0.800768
-600.203173	-7.452998	0.805773
-604.163987	-0.368645	0.810778
-608.132376	-2.516293	0.815782
-612.151045	-8.167836	0.820787
-615.883448	2.333630	0.825792
-619.330863	-1.059470	0.830797
-623.624819	4.236230	0.835802
-627.122694	-8.396206	0.840806
-630.423213	-2.942249	0.845811
-634.201994	-7.381535	0.850816
-638.026665	-7.235513	0.855821
-641.700314	-3.565411	0.860826
-645.907240	-4.954202	0.865830
-649.545558	-4.117257	0.870835
-653.540608	4.273655	0.875840
-656.438539	-8.429363	0.880845
-660.781163	2.433028	0.885850
-664.531264	2.538792	0.890854
-667.987685	1.219355	0.895859
-672.131237	3.340301	0.900864
-675.974912	-4.114772	0.905869
-679.810255	-1.918481	0.910874
-683.136117	-3.952629	0.915878
-687.035336	0.784932	0.920883
-690.942486	2.980100	0.925888
-694.527902	-6.905334	0.930893
-698.344814	-6.024005	0.935898
-701.960541	-2.828276	0.940902
-705.885761	-9.413965	0.945907
-709.862093	-0.999148	0.950912
-713.084393	-1.630523	0.955917
-717.079632	1.386178	0.960922
-721.052013	-9.173818	0.965926
-724.912279	-8.954157	0.970931
-728.935991	-10.126070	0.975936
-732.318928	-6.038661	0.980941
-735.841195	-6.765569	0.985946
-739.421191	-0.897787	0.990950
-742.930888	-13.014046	0.995955
-746.953188	-1.981928	1.000960
-750.975827	-11.116133	1.005965
-755.106880	-11.676325	1.010970
-759.049753	-8.731004	1.015974
-762.335239	-8.746653	1.020979
-766.026933	-11.723590	1.025984
-769.865338	-10.703091	1.030989
-773.543438	-8.181695	1.035994
-777.330278	-8.869406	1.040998
-781.214803	-9.867931	1.046003
-785.087334	-8.003002	1.051008
-788.502161	-4.930721	1.056013
-792.346896	-8.040851	1.061018
-795.890380	-2.386985	1.066022
-799.806025	-6.927126	1.071027
-803.932783	-9.197361	1.076032
-807.481145	-11.623123	1.081037
-811.554336	-0.218485	1.086042
-815.612967	-8.227168	1.091046
-818.283672	-7.661337	1.096051
-822.311259	-4.730756	1.101056
-826.006296	-8.653249	1.106061
-830.013549	1.857774	1.111066
-834.072085	-6.649217	1.116070
-837.660117	-13.960368	1.121075
-841.172145	-2.582314	1.126080
-844.711844	-17.822328	1.131085
-848.699789	-12.390652	1.136090
-852.780562	-10.848717	1.141094
-856.276192	-5.301764	1.146099
-860.234900	-3.159580	1.151104
-864.102037	-5.906459	1.156109
-868.015555	-6.878128	1.161114
-871.605959	0.636296	1.166118
-874.992231	-9.141905	1.171123
-878.751768	-2.579733	1.176128
-882.387533	-6.815968	1.181133
-886.388834	-1.468825	1.186138
-890.578226	-10.118793	1.191142
-894.229504	-7.513189	1.196147
-897.870206	-9.741120	1.201152
-901.120177	-11.668815	1.206157
-904.942267	-3.584283	1.211162
-909.118410	-4.428735	1.216166
-912.985189	-3.058109	1.221171
-916.760936	2.760806	1.226176
-920.093330	-13.310182	1.231181
-923.969731	-1.766517	1.236186
-927.492670	-8.326257	1.241190
-931.551461	-0.790468	1.246195
-935.564993	0.871746	1.251200
-938.926536	-11.971216	1.256205
-942.803068	-12.858785	1.261210
-946.630442	-10.839962	1.266214
-950.338023	-2.647513	1.271219
-954.295627	2.170778	1.276224
-957.859977	-2.892054	1.281229
-961.419535	-5.262173	1.286234
-965.507905	0.908013	1.291238
-969.007147	-7.979911	1.296243
-973.038091	-6.357427	1.301248
-976.606484	-8.186784	1.306253
-980.689669	-7.920015	1.311258
-984.269180	-6.060619	1.316262
-987.971476	-5.466815	1.321267
-992.106081	-7.606147	1.326272
-995.393927	-12.268430	1.331277
-999.230342	-6.444418	1.336282
-1002.979551	-13.750027	1.341286
-1006.554040	-11.213304	1.346291
-1010.645660	0.819084	1.351296
-1014.398285	2.867064	1.356301
-1018.348491	-0.555409	1.361306
-1022.002073	-6.147921	1.366310
-1025.471252	-9.270419	1.371315
-1029.451173	-8.797727	1.376320
-1032.950941	-14.260277	1.381325
-1037.000952	-10.117787	1.386330
-1040.707348	-13.268551	1.391334
-1044.192945	-9.121709	1.396339
-1048.337561	-11.732430	1.401344
-1051.736470	-13.710206	1.406349
-1055.686220	-8.741620	1.411354
-1059.772769	2.862679	1.416358
-1063.403820	-4.475926	1.421363
-1067.197821	-4.755162	1.426368
-1070.449242	-17.623411	1.431373
-1074.129809	-11.923561	1.436378
-1078.309317	-7.955831	1.441382
-1082.021306	-5.726586	1.446387
-1086.088391	-1.537125	1.451392
-1089.821345	-11.275302	1.456397
-1093.407544	-11.833745	1.461402
-1096.952988	-20.127431	1.466406
-1100.365544	-19.068862	1.471411
-1104.876354	-8.814324	1.476416
-1108.431485	-9.294134	1.481421
-1112.476074	-4.876413	1.486426
-1116.022535	-9.607535	1.491430
-1119.440563	-22.745520	1.496435
-1123.314203	-3.886433	1.501440
-1126.592447	-7.003053	1.506445
-1131.009958	-8.216925	1.511450
-1134.951266	-1.339846	1.516454
-1138.589508	-11.693917	1.521459
-1142.343518	-8.018081	1.526464
-1146.180292	-7.262160	1.531469
-1149.653779	-13.466754	1.536474
-1153.514940	-13.361362	1.541478
-1156.993076	-8.550069	1.546483
-1161.349256	-8.113146	1.551488
-1164.574708	-10.216281	1.556493
-1168.404610	-5.407035	1.561498
-1172.342401	-11.907891	1.566502
-1175.839965	-7.471934	1.571507
-1179.762226	-4.125512	1.576512
-1183.177444	-16.495864	1.581517
-1187.397088	-12.401672	1.586522
-1191.203888	-7.310655	1.591526
-1194.882724	-6.335496	1.596531
-1199.049080	-5.335938	1.601536
-1202.403296	-10.277460	1.606541
-1205.942274	-14.012991	1.611546
-1209.703813	-6.950092	1.616550
-1213.703787	-7.814300	1.621555
-1217.809790	-1.935761	1.626560
-1221.393395	-4.672216	1.631565
-1225.087247	-5.312577	1.636570
-1228.883931	-5.291495	1.641574
-1232.542659	-9.908272	1.646579
-1236.584145	-3.041805	1.651584
-1240.085115	-5.460291	1.656589
-1243.565810	-9.107320	1.661594
-1247.191643	-12.795770	1.666598
-1250.740037	-8.944509	1.671603
-1255.137244	-11.203768	1.676608
-1258.957610	-13.072785	1.681613
-1262.753344	-9.298617	1.686618
-1266.381545	-13.462901	1.691622
-1269.570426	-10.728873	1.696627
-1273.826700	-10.386578	1.701632
-1277.861203	-15.789967	1.706637
-1281.643994	-2.660115	1.711642
-1285.256369	-1.875225	1.716646
-1289.094438	-9.779568	1.721651
-1292.258032	-9.052305	1.726656
-1296.238247	-10.269619	1.731661
-1300.365012	-3.140235	1.736666
-1304.064669	-8.633446	1.741670
-1307.836872	-3.038420	1.746675
-1311.516456	-6.841168	1.751680
-1314.809454	-9.625567	1.756685
-1318.796202	-9.652763	1.761690
-1322.689056	-7.559769	1.766694
-1326.258492	-7.749946	1.771699
-1330.500456	-15.223705	1.776704
-1334.009585	-1.374328	1.781709
-1337.906994	-6.337507	1.786714
-1341.988249	-7.472335	1.791718
-1345.616469	-6.965515	1.796723
-1349.076123	-5.138944	1.801728
-1352.431854	-21.353723	1.806733
-1356.322683	-12.218271	1.811738
-1360.356738	-3.343733	1.816742
-1363.864248	-15.134465	1.821747
-1367.976389	-12.186269	1.826752
-1371.656483	-18.688599	1.831757
-1375.662847	-14.388518	1.836762
-1379.607519	-5.655992	1.841766
-1382.849086	-1.858385	1.846771
-1386.809522	-1.880214	1.851776
-1390.498880	-11.837742	1.856781
-1394.050436	-11.809902	1.861786
-1398.221116	-5.395571	1.866790
-1401.929218	-12.096798	1.871795
-1405.466657	-2.442249	1.876800
-1408.818713	-15.855262	1.881805
-1412.842699	-3.840935	1.886810
-1416.668393	-2.676331	1.891814
-1420.419644	-20.108170	1.896819
-1424.706651	-13.176850	1.901824
-1428.098460	-10.761779	1.906829
-1431.940512	-15.859810	1.911834
-1435.879812	-6.514615	1.916838
-1439.093240	-13.873731	1.921843
-1443.035778	-15.158323	1.926848
-1446.527963	-3.970268	1.931853
-1450.546190	-8.637934	1.936858
-1454.386738	-6.436400	1.941862
-1457.992925	-14.916897	1.946867
-1462.281053	-10.465893	1.951872
-1465.680103	-12.644880	1.956877
-1469.281299	-11.109282	1.961882
-1473.054628	-9.809466	1.966886
-1476.881979	-15.584714	1.971891
-1480.708522	-13.866354	1.976896
-1484.382562	-9.931544	1.981901
-1488.478458	-11.033803	1.986906
-1491.944513	-16.795920	1.991910
-1495.506523	-18.586063	1.996915
-1499.791116	-9.604726	2.006912
-1500.709635	-3.373536	2.016909
-1498.313181	-12.662513	2.026906
-1495.211245	-13.083212	2.036902
-1493.041127	-14.087330	2.046899
-1491.107842	-9.339182	2.056896
-1489.489650	-4.916368	2.066893
-1487.589346	-9.990523	2.076890
-1485.485018	-10.098289	2.086886
-1483.617791	-10.179137	2.096883
-1481.595359	-4.638394	2.106880
-1479.923153	-8.548622	2.116877
-1477.872415	-4.255068	2.126874
-1476.067879	-6.946983	2.136870
-1474.152926	-9.470258	2.146867
-1472.160488	-3.473113	2.156864
-1470.684243	-3.597132	2.166861
-1468.216725	-7.262069	2.176858
-1466.310228	-9.015019	2.186854
-1464.589358	-6.910787	2.196851
-1462.833789	-2.345736	2.206848
-1460.820287	-3.548961	2.216845
-1458.992923	-7.460336	2.226842
-1457.315338	-10.514022	2.236838
-1455.551597	-8.399279	2.246835
-1453.505497	-11.148805	2.256832
-1451.229753	-9.765006	2.266829
-1449.481948	-9.046686	2.276826
-1447.631326	-13.724424	2.286822
-1445.845446	-11.946384	2.296819
-1444.124517	-8.288426	2.306816
-1441.986271	-11.017959	2.316813
-1440.114163	-13.858038	2.326810
-1438.444252	-12.241427	2.336806
-1436.730928	-7.909598	2.346803
-1434.455391	-6.978917	2.356800
-1432.410539	-14.657812	2.366797
-1430.569863	-10.002152	2.376794
-1429.010591	-15.383243	2.386790
-1426.901903	-13.287393	2.396787
-1425.048603	-8.077947	2.406784
-1423.429148	-7.958017	2.416781
-1421.230853	-5.780190	2.426778
-1419.441127	-14.155612	2.436774
-1417.678915	-13.818530	2.446771
-1415.930956	-11.410696	2.456768
-1413.777795	-6.677155	2.466765
-1412.043191	-8.405697	2.476762
-1409.916643	-8.490109	2.486758
-1408.119341	-10.986599	2.496755
-1406.342501	-8.119160	2.506752
-1404.659889	-6.731931	2.516749
-1402.613616	-2.388641	2.526746
-1400.923753	-7.020082	2.536742
-1398.550406	-12.689390	2.546739
-1396.757941	-12.503981	2.556736
-1394.974717	-4.395326	2.566733
-1393.083263	-4.925253	2.576730
-1391.569041	-12.282314	2.586726
-1389.638902	-6.535652	2.596723
-1387.460656	-2.445588	2.606720
-1385.759540	-4.255594	2.616717
-1383.804833	-7.472020	2.626714
-1381.679127	-1.895609	2.636710
-1379.758908	-7.797101	2.646707
-1378.156195	-7.120236	2.656704
-1376.621732	-5.739269	2.666701
-1374.267054	-10.565545	2.676698
-1372.340093	-8.167386	2.686694
-1370.429081	-7.243022	2.696691
-1368.727683	-5.468764	2.706688
-1367.045015	-2.188311	2.716685
-1365.130524	-3.969302	2.726682
-1363.064025	-3.620890	2.736678
-1361.165220	-12.124264	2.746675
-1359.455105	-6.244455	2.756672
-1357.690531	-9.449369	2.766669
-1355.507451	-10.630702	2.776666
-1353.582037	-5.458001	2.786662
-1351.570113	-7.764590	2.796659
-1350.133101	-9.933354	2.806656
-1348.278334	-10.141574	2.816653
-1346.255140	-7.378262	2.826650
-1343.984970	-9.318806	2.836646
-1342.732258	-9.820655	2.846643
-1340.758936	-4.762982	2.856640
-1338.816105	-9.736460	2.866637
-1336.811246	-15.667255	2.876634
-1334.870838	-13.209637	2.886630
-1333.011011	-4.841604	2.896627
-1330.893083	-5.770900	2.906624
-1329.328060	-11.901291	2.916621
-1327.541336	-8.883789	2.926618
-1325.756569	-6.532303	2.936614
-1323.664856	-12.830684	2.946611
-1321.954932	-3.450201	2.956608
-1319.777387	-11.224461	2.966605
-1318.012280	-3.393898	2.976602
-1316.304489	-11.467181	2.986598
-1314.296422	-10.711468	2.996595
-1312.499717	-9.036109	3.006592
-1310.609738	-3.030308	3.016589
-1308.449207	-10.430773	3.026586
-1306.698890	-12.993878	3.036582
-1305.026163	-6.871193	3.046579
-1302.936601	-8.171722	3.056576
-1301.285478	-8.400994	3.066573
-1299.272056	-14.176811	3.076570
-1297.170433	-12.804463	3.086566
-1295.276832	-13.165702	3.096563
-1293.898144	-20.242057	3.106560
-1292.056424	-14.129045	3.116557
-1289.959875	-3.665652	3.126554
-1287.992761	-13.665733	3.136550
-1285.981051	-12.858471	3.146547
-1284.432984	-12.049633	3.156544
-1282.301422	-5.487196	3.166541
-1280.545773	-2.122040	3.176538
-1278.405802	-5.754885	3.186534
-1276.653545	-9.409359	3.196531
-1275.134863	-10.419542	3.206528
-1273.173625	-6.275686	3.216525
-1271.001071	-13.799624	3.226522
-1269.149949	-17.758869	3.236518
-1267.532787	-11.163040	3.246515
-1265.619082	-10.717453	3.256512
-1263.790952	-12.773494	3.266509
-1261.910893	-11.454076	3.276506
-1259.658455	-13.636445	3.286502
-1257.916914	-8.011063	3.296499
-1255.985598	-9.546757	3.306496
-1254.291020	-13.487254	3.316493
-1252.558747	-10.847829	3.326490
-1250.533801	-13.336421	3.336486
-1248.506538	-10.715780	3.346483
-1246.585129	-11.716183	3.356480
-1244.820852	-15.784673	3.366477
-1243.086810	-14.407134	3.376474
-1241.300712	-13.508463	3.386470
-1239.145796	-13.079350	3.396467
-1237.219338	-9.274116	3.406464
-1235.392722	-8.422978	3.416461
-1233.542879	-8.440840	3.426458
-1231.673950	-11.624467	3.436454
-1230.102140	-10.284115	3.446451
-1227.887388	-9.621403	3.456448
-1226.008970	-12.362849	3.466445
-1224.275847	-6.756619	3.476442
-1222.311650	-8.362286	3.486438
-1220.373606	-8.258459	3.496435
-1218.539944	-9.146901	3.506432
-1216.903040	-6.999040	3.516429
-1214.969774	-3.205928	3.526426
-1212.793059	-5.744040	3.536422
-1211.174513	-3.836401	3.546419
-1209.074952	-3.270504	3.556416
-1207.312881	-1.989003	3.566413
-1205.363969	-4.534866	3.576410
-1203.711162	-7.857577	3.586406
-1201.712035	-6.798748	3.596403
-1199.669019	-6.054842	3.606400
-1197.791002	-6.337717	3.616397
-1196.198404	-7.696001	3.626394
-1194.143875	-4.665978	3.636390
-1192.571098	-5.318438	3.646387
-1190.447588	-7.506954	3.656384
-1188.395752	-7.606050	3.666381
-1186.821512	-9.142974	3.676378
-1184.668709	-6.575522	3.686374
-1182.758510	-11.189962	3.696371
-1181.158414	-5.252930	3.706368
-1179.178027	-2.215767	3.716365
-1177.485397	-4.119005	3.726362
-1175.357013	-8.413080	3.736358
-1173.303023	-6.510350	3.746355
-1171.567557	-5.824581	3.756352
-1169.658134	-6.518258	3.766349
-1168.069465	-2.619440	3.776346
-1166.259489	-8.139963	3.786342
-1164.100948	-6.392904	3.796339
-1162.358592	-7.381958	3.806336
-1160.407720	-6.964336	3.816333
-1158.472175	-11.458074	3.826330
-1156.591283	-9.058674	3.836326
-1154.533827	-10.726575	3.846323
-1153.096344	-4.135066	3.856320
-1151.340921	-3.867749	3.866317
-1149.074589	-7.005946	3.876314
-1147.253502	-15.479360	3.886310
-1145.375214	-5.209854	3.896307
-1143.336831	-4.664109	3.906304
-1141.854306	-4.863137	3.916301
-1139.941674	-2.397745	3.926298
-1137.519199	-0.422880	3.936294
-1136.001536	-8.421419	3.946291
-1134.309991	-2.917413	3.956288
-1132.190872	-4.345681	3.966285
-1130.524634	-3.312480	3.976282
-1128.452344	-7.218583	3.986278
-1126.562531	-11.542342	3.996275
-1124.640822	-6.555166	4.006272
-1122.924757	-11.016920	4.016269
-1120.998436	-0.680860	4.026266
-1118.852356	-3.411359	4.036262
-1117.360856	-9.427226	4.046259
-1115.748450	-8.649094	4.056256
-1113.604925	-4.924269	4.066253
-1111.522230	-7.025657	4.076250
-1109.684711	-6.503013	4.086246
-1107.700833	-10.761279	4.096243
-1105.910462	-6.128874	4.106240
-1103.955260	-9.747796	4.116237
-1102.208233	-6.775867	4.126234
-1100.418431	-8.519329	4.136230
-1098.615359	-11.944956	4.146227
-1096.394457	-11.033622	4.156224
-1094.629369	-3.401819	4.166221
-1093.007870	-11.066406	4.176218
-1090.743293	-6.314054	4.186214
-1089.330142	-0.997589	4.196211
-1087.334948	5.040530	4.206208
-1085.250221	-4.398733	4.216205
-1083.559598	-2.616220	4.226202
-1081.649477	0.062787	4.236198
-1079.624469	-5.792081	4.246195
-1077.716152	-8.872941	4.256192
-1076.104226	-0.487126	4.266189
-1074.156841	-3.837925	4.276186
-1071.818039	-6.839217	4.286182
-1070.316807	1.419042	4.296179
-1068.723346	3.596067	4.306176
-1066.334275	-7.988762	4.316173
-1064.759672	-1.685974	4.326170
-1063.125095	-10.208449	4.336166
-1061.153591	-6.895017	4.346163
-1059.063357	-14.231918	4.356160
-1057.007178	-0.570689	4.366157
-1055.149996	-10.270377	4.376154
-1053.049986	-8.974917	4.386150
-1051.862889	-7.523956	4.396147
-1049.780652	-4.968773	4.406144
-1047.786938	-4.343166	4.416141
-1045.737086	-6.573457	4.426138
-1043.914684	-7.474172	4.436134
-1042.188027	-15.322920	4.446131
-1040.506527	-12.349938	4.456128
-1038.820598	-14.829917	4.466125
-1036.587298	-18.880116	4.476122
-1034.716158	-12.495264	4.486118
-1032.684665	-12.346226	4.496115
-1030.890441	-13.198212	4.506112
-1028.809954	-11.157481	4.516109
-1027.320442	-11.360712	4.526106
-1025.309049	-13.695363	4.536102
-1023.391472	-8.742176	4.546099
-1021.298281	-12.275729	4.556096
-1019.502515	-15.223274	4.566093
-1017.886585	-13.026125	4.576090
-1016.001790	-13.428363	4.586086
-1014.079689	-13.893409	4.596083
-1012.328112	-4.929866	4.606080
-1010.568412	-5.785790	4.616077
-1008.399334	-14.821622	4.626074
-1006.436654	-11.590419	4.636070
-1004.614611	-13.561602	4.646067
-1002.577188	-14.321406	4.656064
-1000.885854	-10.748371	4.666061
-999.049201	-13.885604	4.676058
-997.149021	-7.742209	4.686054
-995.440415	-15.510669	4.696051
-993.476451	-16.380299	4.706048
-991.402045	-16.481253	4.716045
-989.618107	-13.147237	4.726042
-987.814660	-17.253387	4.736038
-985.885788	-21.209063	4.746035
-984.251364	-19.406438	4.756032
-982.271094	-16.508037	4.766029
-980.216563	-21.800682	4.776026
-978.472759	-19.993440	4.786022
-976.353897	-15.929796	4.796019
-974.409670	-14.674090	4.806016
-972.695326	-12.279483	4.816013
-970.946054	-11.242077	4.826010
-968.997809	-14.723983	4.836006
-967.185480	-12.223460	4.846003
-965.147404	-10.625901	4.856000
-963.331505	-4.862167	4.865997
-961.472805	-12.376706	4.875994
-959.948540	-6.392643	4.885990
-957.486068	-3.451325	4.895987
-956.010533	-14.365738	4.905984
-953.918110	-12.631594	4.915981
-952.181218	-8.404208	4.925978
-950.288221	-7.514510	4.935974
-948.234881	-9.007887	4.945971
-946.586950	-6.087887	4.955968
-944.641611	-3.385975	4.965965
-942.600629	-11.791780	4.975962
-940.914396	-15.255452	4.985958
-938.861782	-16.650806	4.995955
-936.973071	-20.017374	5.005952
-935.087314	-13.955308	5.015949
-933.552842	-14.375674	5.025946
-931.848132	-11.292633	5.035942
-929.624449	-15.159615	5.045939
-927.637890	-5.797773	5.055936
-925.721994	-12.056659	5.065933
-923.906085	-12.834661	5.075930
-922.106476	-6.060891	5.085926
-920.386869	-10.592549	5.095923
-918.250634	-10.543846	5.105920
-916.516112	-8.138211	5.115917
-914.544052	-9.643826	5.125914
-912.714522	-9.955037	5.135910
-910.737138	-14.529483	5.145907
-909.190912	-12.682700	5.155904
-907.293174	-8.204674	5.165901
-905.259589	-10.651724	5.175898
-903.242209	-9.366601	5.185894
-901.463935	-10.342258	5.195891
-899.511289	-6.637237	5.205888
-897.862800	-14.673925	5.215885
-895.648982	-6.396841	5.225882
-893.879121	-6.744287	5.235878
-892.148675	-6.262775	5.245875
-890.152756	-12.665486	5.255872
-888.117432	-11.203212	5.265869
-886.571619	-10.777442	5.275866
-884.544148	-9.609182	5.285862
-882.770740	-10.190878	5.295859
-880.850448	-9.834450	5.305856
-878.924942	-3.827634	5.315853
-877.324631	-8.458615	5.325850
-875.290012	-9.306285	5.335846
-873.022835	-1.482982	5.345843
-871.251706	-6.968662	5.355840
-869.639672	-12.027839	5.365837
-867.733174	-8.894903	5.375834
-865.816138	-10.634846	5.385830
-863.727179	-7.589500	5.395827
-861.982736	-14.199886	5.405824
-860.305490	-12.287171	5.415821
-858.356846	-12.634752	5.425818
-856.385578	-12.831207	5.435814
-854.557561	-9.611500	5.445811
-852.709895	-12.791438	5.455808
-850.871796	-6.347454	5.465805
-848.846838	-15.265375	5.475802
-847.096831	-12.811636	5.485798
-845.199366	-12.685221	5.495795
-843.131235	-13.197158	5.505792
-841.467012	-7.150120	5.515789
-839.808633	-10.637693	5.525786
-837.584547	-12.733024	5.535782
-835.579329	-9.852692	5.545779
-833.810183	-10.335773	5.555776
-832.067693	-8.468205	5.565773
-830.218829	-8.067158	5.575770
-828.637861	-5.821651	5.585766
-826.427043	-10.862835	5.595763
-824.219080	-6.608018	5.605760
-822.797019	-4.232890	5.615757
-820.823442	-5.885518	5.625754
-818.832912	-8.611412	5.635750
-816.918051	-14.565305	5.645747
-815.176184	-10.183866	5.655744
-813.341428	-11.383231	5.665741
-811.542959	-6.701353	5.675738
-809.327456	-9.802686	5.685734
-807.641452	-10.304037	5.695731
-805.583685	-10.179529	5.705728
-803.739819	-11.465608	5.715725
-802.214161	-8.467535	5.725722
-800.558551	-7.006068	5.735718
-798.037115	-10.197347	5.745715
-796.519443	-9.741755	5.755712
-794.339025	-9.670001	5.765709
-792.727516	-10.039430	5.775706
-790.968814	-7.331239	5.785702
-788.849176	-12.090965	5.795699
-786.787572	-7.501655	5.805696
-785.204377	-6.603357	5.815693
-783.109070	-9.987042	5.825690
-781.266482	-3.940043	5.835686
-779.307200	-1.413907	5.845683
-777.367196	-7.723908	5.855680
-775.865946	-7.826221	5.865677
-774.238335	-3.983871	5.875674
-772.150902	-6.230990	5.885670
-770.029521	-10.711497	5.895667
-768.080705	-8.046307	5.905664
-766.312542	-9.339205	5.915661
-764.537696	-8.433629	5.925658
-762.878330	-8.251723	5.935654
-760.727599	-5.359843	5.945651
-758.647779	-8.035221	5.955648
-756.991035	-4.994908	5.965645
-755.002594	-1.854445	5.975642
-753.156767	-8.716235	5.985638
-751.299601	-15.513516	5.995635
-749.689424	-9.372503	6.005632
-747.755167	-12.455672	6.015629
-745.406336	-6.993255	6.025626
-743.726575	-4.160301	6.035622
-742.102911	-6.022211	6.045619
-740.264620	-11.022729	6.055616
-738.101994	-7.153752	6.065613
-736.262272	-5.634819	6.075610
-734.595009	-4.582548	6.085606
-732.623651	-8.229022	6.095603
-730.583026	-11.070222	6.105600
-728.911766	-7.361135	6.115597
-726.839931	-9.463613	6.125594
-725.002717	-10.050652	6.135590
-723.475240	-8.415490	6.145587
-721.512490	-11.057915	6.155584
-719.297426	-3.808773	6.165581
-717.427600	-5.703691	6.175578
-715.783045	-6.762055	6.185574
-713.983407	-9.188927	6.195571
-712.045800	-5.484497	6.205568
-709.931552	-7.517947	6.215565
-708.056382	-7.473124	6.225562
-706.323015	-2.763386	6.235558
-704.579423	-6.135010	6.245555
-702.371210	-10.199849	6.255552
-700.778861	-11.788297	6.265549
-698.838010	-6.555905	6.275546
-696.877211	-9.371689	6.285542
-695.203317	-9.000998	6.295539
-693.323816	-11.510093	6.305536
-691.286510	-13.314908	6.315533
-689.373050	-10.631370	6.325530
-687.535280	-10.035800	6.335526
-685.641797	-13.889271	6.345523
-683.832529	-13.066506	6.355520
-681.920926	-12.323251	6.365517
-680.078041	-9.481580	6.375514
-678.165723	-13.429638	6.385510
-676.397569	-11.640266	6.395507
-674.363160	-18.494235	6.405504
-672.353736	-14.499661	6.415501
-670.763016	-13.067208	6.425498
-668.886747	-10.148754	6.435494
-666.887774	-13.558001	6.445491
-664.895148	-12.222923	6.455488
-663.030461	-11.307941	6.465485
-661.549209	-7.410543	6.475482
-659.361826	-8.334547	6.485478
-657.322320	-7.753819	6.495475
-655.610909	-9.347052	6.505472
-653.915036	-5.812373	6.515469
-651.891734	-13.760377	6.525466
-650.197802	-10.901198	6.535462
-648.295681	-14.729178	6.545459
-646.079706	-15.591419	6.555456
-644.219936	-12.970319	6.565453
-642.547100	-14.898442	6.575450
-640.747557	-9.509207	6.585446
-638.783981	-7.839455	6.595443
-636.782072	-8.853807	6.605440
-635.195764	-12.383414	6.615437
-633.308252	-10.968355	6.625434
-631.040228	-9.123023	6.635430
-629.331982	-12.782639	6.645427
-627.553005	-17.784650	6.655424
-625.515641	-10.750189	6.665421
-623.671880	-16.646787	6.675418
-621.788263	-14.001057	6.685414
-619.876411	-20.878034	6.695411
-618.401139	-14.563789	6.705408
-616.435303	-10.890630	6.715405
-614.680844	-15.388173	6.725402
-612.516418	-7.413969	6.735398
-610.474279	-14.643347	6.745395
-608.665171	-14.469466	6.755392
-607.057621	-16.451873	6.765389
-604.795764	-19.339366	6.775386
-603.262686	-15.456527	6.785382
-601.251457	-12.546949	6.795379
-599.312633	-22.927279	6.805376
-597.414367	-18.570659	6.815373
-595.522794	-18.795218	6.825370
-593.847800	-13.212358	6.835366
-591.972465	-17.058122	6.845363
-590.014162	-16.139090	6.855360
-588.031100	-19.465200	6.865357
-586.451868	-18.768247	6.875354
-584.386470	-18.788455	6.885350
-582.587791	-7.191991	6.895347
-580.482371	-16.073614	6.905344
-578.592673	-10.629256	6.915341
-576.845726	-15.288209	6.925338
-574.995063	-9.690764	6.935334
-572.928804	-11.973805	6.945331
-571.356158	-13.330066	6.955328
-569.051430	-13.787980	6.965325
-567.598144	-17.601041	6.975322
-565.694627	-18.045387	6.985318
-563.989001	-17.682830	6.995315
-561.890583	-14.277129	7.005312
-559.921379	-20.582153	7.015309
-558.346535	-20.110276	7.025306
-556.174641	-10.968752	7.035302
-554.107168	-19.566386	7.045299
-552.174683	-10.678728	7.055296
-550.552400	-15.478807	7.065293
-548.735029	-19.192117	7.075290
-546.785877	-13.281951	7.085286
-545.122403	-16.383287	7.095283
-543.168509	-13.884513	7.105280
-540.991876	-20.157918	7.115277
-539.229280	-10.845203	7.125274
-537.308145	-13.973481	7.135270
-535.606914	-12.552272	7.145267
-534.079954	-16.643933	7.155264
-531.939067	-11.617040	7.165261
-529.819362	-10.145825	7.175258
-527.878602	-7.100183	7.185254
-526.264633	-8.699867	7.195251
-524.205472	-15.076079	7.205248
-522.260660	-9.427310	7.215245
-520.960685	-11.627383	7.225242
-518.839535	-7.153131	7.235238
-516.704271	-10.468760	7.245235
-514.919320	-13.603691	7.255232
-512.946508	-13.234825	7.265229
-511.163919	-17.638891	7.275226
-509.426015	-13.403427	7.285222
-507.783097	-16.659355	7.295219
-505.478914	-17.072909	7.305216
-503.804082	-11.969970	7.315213
-501.728431	-12.018586	7.325210
-499.629878	-17.166292	7.335206
-497.919523	-20.213503	7.345203
-496.182397	-18.227980	7.355200
-494.185362	-20.889910	7.365197
-492.448232	-13.910008	7.375194
-490.593431	-18.942982	7.385190
-488.523304	-16.465885	7.395187
-486.889623	-15.185436	7.405184
-484.741339	-12.818715	7.415181
-482.879233	-9.051502	7.425178
-481.503303	-13.682715	7.435174
-479.743806	-7.088490	7.445171
-477.038953	-16.531574	7.455168
-475.254371	-14.602563	7.465165
-473.858695	-13.315673	7.475162
-471.909083	-15.047876	7.485158
-469.756245	-14.284554	7.495155
-467.705340	-11.747522	7.505152
-466.338522	-18.344705	7.515149
-464.343865	-13.025963	7.525146
-462.624963	-8.626369	7.535142
-460.272518	-5.835899	7.545139
-458.445218	-11.628696	7.555136
-456.731835	-12.299968	7.565133
-454.975959	-15.731801	7.575130
-453.407838	-10.570728	7.585126
-450.966649	-11.422965	7.595123
-449.118833	-16.078993	7.605120
-447.248016	-21.054490	7.615117
-445.688935	-10.679687	7.625114
-443.531449	-11.385554	7.635110
-441.843381	-17.756123	7.645107
-439.983899	-17.722795	7.655104
-438.006720	-9.956944	7.665101
-435.932621	-15.947037	7.675098
-434.149919	-15.257211	7.685094
-432.340108	-17.415492	7.695091
-430.429359	-14.777097	7.705088
-428.713327	-17.681479	7.715085
-426.714401	-17.970418	7.725082
-425.140748	-15.755045	7.735078
-422.971586	-7.771934	7.745075
-421.233441	-20.624393	7.755072
-419.209253	-15.896137	7.765069
-417.382038	-23.168412	7.775066
-415.428252	-17.644148	7.785062
-413.584509	-15.380315	7.795059
-411.865410	-15.207702	7.805056
-409.847239	-17.163967	7.815053
-407.755896	-11.649028	7.825050
-406.306119	-11.161816	7.835046
-404.178719	-14.602412	7.845043
-402.368096	-12.442232	7.855040
-400.493657	-13.282870	7.865037
-398.691335	-16.952615	7.875034
-396.904413	-14.506005	7.885030
-394.819507	-14.947599	7.895027
-392.883274	-10.667921	7.905024
-390.963250	-13.827490	7.915021
-388.902029	-11.516254	7.925018
-387.396008	-13.365461	7.935014
-385.617182	-8.280615	7.945011
-383.536024	-12.635948	7.955008
-381.636122	-15.912300	7.965005
-379.628709	-11.966093	7.975002
-378.258210	-4.283321	7.984998
-376.065644	-9.644893	7.994995
-373.876571	-10.891024	8.004992
-372.413387	-16.600358	8.014989
-370.668842	-13.501150	8.024986
-368.569937	-9.879025	8.034982
-366.809879	-10.486630	8.044979
-364.696229	-14.322905	8.054976
-363.161725	-18.237242	8.064973
-361.016601	-12.972434	8.074970
-359.311765	-11.114288	8.084966
-357.214108	-15.191170	8.094963
-355.472112	-11.625738	8.104960
-353.401775	-11.198097	8.114957
-351.600247	-17.629357	8.124954
-349.984542	-9.979404	8.134950
-348.132408	-14.121294	8.144947
-345.950292	-7.828128	8.154944
-344.096576	-11.817104	8.164941
-342.524167	-8.696707	8.174938
-340.445140	-11.268970	8.184934
-338.477812	-12.215972	8.194931
-336.738390	-14.242942	8.204928
-334.727279	-8.705650	8.214925
-332.857113	-17.655313	8.224922
-331.127207	-13.781605	8.234918
-329.280922	-8.664851	8.244915
-327.145426	-15.106781	8.254912
-325.388672	-13.577437	8.264909
-323.605988	-14.311785	8.274906
-321.685376	-13.149663	8.284902
-319.785177	-16.773396	8.294899
-318.203510	-19.847311	8.304896
-315.855227	-14.270671	8.314893
-314.245030	-9.945191	8.324890
-312.419602	-17.262904	8.334886
-310.159544	-14.730701	8.344883
-308.650973	-10.461628	8.354880
-306.618446	-14.534388	8.364877
-304.865162	-9.803834	8.374874
-302.930634	-14.517811	8.384870
-301.053378	-11.338679	8.394867
-299.122726	-18.730024	8.404864
-297.132937	-10.855528	8.414861
-295.472580	-9.426040	8.424858
-293.494055	-7.834176	8.434854
-291.918098	-4.251661	8.444851
-289.968072	-14.898843	8.454848
-287.765343	-13.724884	8.464845
-285.840336	-13.506100	8.474842
-284.101404	-12.515478	8.484838
-282.371738	-13.484499	8.494835
-280.318057	-16.933749	8.504832
-278.502458	-13.591594	8.514829
-276.759578	-13.503208	8.524826
-274.790883	-8.931758	8.534822
-272.930298	-8.262137	8.544819
-271.038137	-9.757633	8.554816
-269.145220	-11.123770	8.564813
-266.908330	-9.382066	8.574810
-265.170783	-2.218878	8.584807
-263.767083	-10.978772	8.594803
-261.857690	-10.013765	8.604800
-259.935362	-7.636032	8.614797
-257.721427	-11.589283	8.624794
-255.784966	-12.030747	8.634791
-254.281558	-7.642387	8.644787
-252.142639	-10.053604	8.654784
-250.399551	-7.293556	8.664781
-248.448314	-8.989524	8.674778
-246.677605	-6.060192	8.684775
-244.594442	-17.570201	8.694771
-242.882257	-14.719950	8.704768
-240.813037	-17.352145	8.714765
-239.068854	-16.027580	8.724762
-237.562010	-19.027921	8.734759
-235.537719	-12.684194	8.744755
-233.200721	-12.475860	8.754752
-231.882342	-14.838201	8.764749
-229.821336	-20.807090	8.774746
-227.643893	-18.068984	8.784743
-225.954026	-18.090526	8.794739
-223.931681	-18.401983	8.804736
-222.358506	-22.933482	8.814733
-220.432926	-18.451425	8.824730
-218.389922	-12.920699	8.834727
-216.631701	-8.975630	8.844723
-214.737004	-21.744003	8.854720
-212.838416	-18.156085	8.864717
-210.691252	-18.482715	8.874714
-208.906912	-19.405145	8.884711
-207.100248	-18.328958	8.894707
-205.285919	-22.660505	8.904704
-203.743166	-26.426056	8.914701
-201.722964	-31.622590	8.924698
-199.485329	-18.191576	8.934695
-197.940833	-20.795255	8.944691
-195.886808	-22.802859	8.954688
-194.144497	-22.690638	8.964685
-192.001572	-26.013526	8.974682
-190.442556	-17.162260	8.984679
-188.492992	-15.000403	8.994675
-186.741454	-20.081418	9.004672
-184.646030	-21.607707	9.014669
-182.778676	-18.185313	9.024666
-181.134548	-17.166854	9.034663
-179.055389	-24.774448	9.044659
-177.267524	-22.994162	9.054656
-175.482959	-23.585012	9.064653
-173.486690	-20.263712	9.074650
-171.455143	-18.504939	9.084647
-169.548299	-19.088456	9.094643
-167.936773	-19.040611	9.104640
-166.112833	-18.614543	9.114637
-163.679825	-16.373493	9.124634
-162.148091	-22.471032	9.134631
-160.320893	-19.455910	9.144627
-158.660127	-16.071583	9.154624
-156.693268	-22.129605	9.164621
-154.539049	-21.904660	9.174618
-152.872726	-23.128754	9.184615
-151.309104	-21.798996	9.194611
-148.977309	-18.888072	9.204608
-147.224711	-16.154731	9.214605
-145.254574	-20.752687	9.224602
-143.429954	-17.184488	9.234599
-141.612239	-19.168549	9.244595
-139.861001	-19.166665	9.254592
-137.612088	-21.254269	9.264589
-135.713519	-20.919036	9.274586
-134.079192	-18.994211	9.284583
-132.262529	-21.661807	9.294579
-130.310369	-22.149889	9.304576
-128.194334	-20.230870	9.314573
-126.756060	-16.233101	9.324570
-125.119574	-19.884085	9.334567
-122.862788	-21.178691	9.344563
-120.838609	-13.268469	9.354560
-118.833102	-21.476921	9.364557
-117.258101	-23.204333	9.374554
-115.299367	-19.739620	9.384551
-113.362151	-23.146465	9.394547
-111.303318	-23.067320	9.404544
-109.708201	-20.561464	9.414541
-107.895510	-20.417777	9.424538
-105.848835	-16.610232	9.434535
-104.103297	-13.441504	9.444531
-102.283574	-9.016667	9.454528
-100.131245	-16.956418	9.464525
-98.342017	-21.823905	9.474522
-96.492599	-15.341621	9.484519
-94.749428	-17.046903	9.494515
-92.637615	-15.291394	9.504512
-90.959850	-19.102107	9.514509
-89.095262	-21.862584	9.524506
-86.974835	-12.027088	9.534503
-85.314941	-19.532980	9.544499
-83.295287	-15.026341	9.554496
-81.559400	-14.082456	9.564493
-79.772635	-21.021195	9.574490
-77.725817	-10.605502	9.584487
-76.008793	-16.795717	9.594483
-73.999022	-26.749616	9.604480
-72.104189	-19.391895	9.614477
-70.347608	-23.643079	9.624474
-68.516664	-18.233129	9.634471
-66.438229	-18.401819	9.644467
-64.320515	-21.207400	9.654464
-62.819620	-23.342970	9.664461
-61.178691	-14.018341	9.674458
-59.014173	-18.430920	9.684455
-57.161384	-12.528635	9.694451
-55.260872	-14.652164	9.704448
-53.444614	-18.800749	9.714445
-51.216109	-18.664934	9.724442
-49.656338	-17.122908	9.734439
-47.917775	-18.341087	9.744435
-45.671572	-15.230082	9.754432
-43.908271	-18.021738	9.764429
-42.204794	-19.096942	9.774426
-40.386007	-19.399458	9.784423
-38.469539	-15.684769	9.794419
-36.402932	-25.649288	9.804416
-34.625806	-24.492467	9.814413
-32.804613	-27.048604	9.824410
-30.834237	-25.766287	9.834407
-28.831481	-19.131561	9.844403
-27.316520	-22.208864	9.854400
-25.026329	-16.024213	9.864397
-23.291316	-28.684876	9.874394
-21.520770	-27.181193	9.884391
-19.721324	-17.528123	9.894387
-17.623514	-18.726217	9.904384
-16.155495	-20.930730	9.914381
-14.025194	-20.603945	9.924378
-12.290085	-13.422804	9.934375
-10.205677	-22.562744	9.944371
-8.301363	-18.321862	9.954368
-6.319043	-21.000002	9.964365
-4.877772	-9.682350	9.974362
-3.705034	11.794872	9.984359
-2.324742	63.639015	9.994355
-0.990754	118.922738	10.004352
0.000000	173.793942	10.009357
0.974434	208.313977	10.014362
1.393335	251.343986	10.019367
2.170014	270.735845	10.024371
2.596215	300.241890	10.029376
3.047808	308.559759	10.034381
2.780944	321.638153	10.039386
3.095403	334.057677	10.044391
3.693069	343.249594	10.049395
3.804412	353.585163	10.054400
3.834762	348.382568	10.059405
3.907220	358.382128	10.064410
3.927921	354.221911	10.069415
4.012469	357.012518	10.074419
3.720868	365.598786	10.079424
4.225221	355.703034	10.084429
4.306026	370.339315	10.089434
4.090254	380.066306	10.094439
4.169770	378.139240	10.099443
3.959629	374.397480	10.104448
4.775612	376.230861	10.109453
4.467262	373.159235	10.114458
4.389828	381.900594	10.119463
4.507461	386.409626	10.124467
4.008426	394.510155	10.129472
4.423976	380.911483	10.134477
4.344981	390.783829	10.139482
4.289607	385.851952	10.144487
4.801777	396.211928	10.149491
4.470329	400.978689	10.154496
4.910535	400.635778	10.159501
4.688673	409.714022	10.164506
4.839422	415.894169	10.169511
5.094847	406.667328	10.174515
4.911467	406.816569	10.179520
4.994892	403.904806	10.184525
4.841758	405.134222	10.189530
4.948359	418.952688	10.194535
5.088403	424.070047	10.199539
5.068719	425.549429	10.204544
5.387640	427.512568	10.209549
5.489616	440.932802	10.214554
5.578255	422.715049	10.219559
4.900469	415.256678	10.224563
4.855456	426.721165	10.229568
5.553532	430.686590	10.234573
5.358677	444.516894	10.239578
5.750403	444.803070	10.244583
5.629061	442.300875	10.249587
5.414749	447.343872	10.254592
5.686169	441.041443	10.259597
5.498669	452.369398	10.264602
5.627782	450.596846	10.269607
5.787063	450.022764	10.274611
5.546542	450.337246	10.279616
5.669793	433.990636	10.284621
5.345609	461.079250	10.289626
5.255694	452.930964	10.294631
5.896698	458.197098	10.299635
5.983592	454.967786	10.304640
5.959139	455.030172	10.309645
5.754447	468.951959	10.314650
6.168419	481.205918	10.319655
6.250281	488.070482	10.324659
6.275339	501.996657	10.329664
6.536865	488.468188	10.334669
6.550702	477.425234	10.339674
6.419061	467.072583	10.344679
6.112998	461.762751	10.349683
5.943424	469.383390	10.354688
6.134449	483.669449	10.359693
6.792189	499.382422	10.364698
6.727490	499.936958	10.369703
6.686965	495.959941	10.374707
6.326723	502.376185	10.379712
6.525971	493.093591	10.384717
6.184580	501.809313	10.389722
6.472637	511.039684	10.394727
6.687893	503.426200	10.399731
6.599332	506.805877	10.404736
6.890606	501.287202	10.409741
6.971088	504.069023	10.414746
6.832709	507.628545	10.419751
6.980286	519.852486	10.424755
7.037745	534.065276	10.429760
7.354233	526.143878	10.434765
7.274594	536.989464	10.439770
7.162473	545.203411	10.444775
7.140436	547.777654	10.449779
7.387083	550.622871	10.454784
7.737081	547.480889	10.459789
7.414942	544.304187	10.464794
7.373729	529.024557	10.469799
7.473480	531.005324	10.474803
7.615654	547.713700	10.479808
7.668790	549.958964	10.484813
7.582153	552.890462	10.489818
7.848711	552.728223	10.494823
7.618747	539.509931	10.499827
7.552585	552.154369	10.504832
7.662544	548.544443	10.509837
7.783916	554.800303	10.514842
7.570817	548.124078	10.519847
8.046421	558.355955	10.524851
7.492900	566.282331	10.529856
7.883916	556.543304	10.534861
7.802536	563.853439	10.539866
7.695719	561.561808	10.544871
8.108341	562.292536	10.549875
7.841642	562.761016	10.554880
7.669477	570.599755	10.559885
7.940920	588.959234	10.564890
8.039768	589.839369	10.569895
8.342471	596.635640	10.574899
7.977979	595.905387	10.579904
8.181058	593.168479	10.584909
8.479618	596.366571	10.589914
8.579401	603.237793	10.594919
8.334996	604.491247	10.599923
8.414882	604.473908	10.604928
8.764741	618.829387	10.609933
8.764089	629.739719	10.614938
8.717001	620.890602	10.619943
8.825443	618.345415	10.624947
8.816971	632.463155	10.629952
9.455015	621.254288	10.634957
8.940288	619.772086	10.639962
8.773312	614.809043	10.644967
8.962007	610.412207	10.649971
9.032718	616.890655	10.654976
9.330448	633.694173	10.659981
9.167342	625.336677	10.664986
8.998938	615.130143	10.669991
9.446987	633.787960	10.674995
9.365623	628.729249	10.680000
9.307622	616.663098	10.685005
9.118850	623.738064	10.690010
9.316545	635.332746	10.695015
9.463692	638.337365	10.700019
9.500960	638.702164	10.705024
9.423469	632.712369	10.710029
9.630413	645.108307	10.715034
9.580504	645.471242	10.720039
9.901701	635.361650	10.725043
9.605930	642.840072	10.730048
9.499391	638.889317	10.735053
9.595299	636.819244	10.740058
9.884111	641.212735	10.745063
9.748877	647.408635	10.750067
9.374425	662.997829	10.755072
9.948655	648.488866	10.760077
9.731102	655.962704	10.765082
9.684395	653.943764	10.770087
9.798338	660.347522	10.775091
10.346078	673.632207	10.780096
10.631065	666.540563	10.785101
10.813733	678.686495	10.790106
10.079280	665.695226	10.795111
10.506853	651.190729	10.800115
10.077352	662.536946	10.805120
10.646053	653.939693	10.810125
10.365733	663.927921	10.815130
10.484401	664.407479	10.820135
10.785281	669.037190	10.825139
10.755733	673.115594	10.830144
10.632963	664.128702	10.835149
10.460696	663.476601	10.840154
10.590585	671.644131	10.845159
10.673681	684.050395	10.850163
10.873022	691.919832	10.855168
10.925543	685.223253	10.860173
10.497892	693.763600	10.865178
10.721390	690.955603	10.870183
10.840799	686.610800	10.875187
11.020130	701.343670	10.880192
10.705675	696.388354	10.885197
10.541706	701.680469	10.890202
10.708484	698.397358	10.895207
11.127970	712.197736	10.900211
10.834622	713.529974	10.905216
11.156970	711.557822	10.910221
11.125910	721.629341	10.915226
11.145535	720.334726	10.920231
11.526216	713.924859	10.925235
11.321081	724.801642	10.930240
11.540831	721.500614	10.935245
11.339528	725.336750	10.940250
11.563701	716.570472	10.945255
11.837217	720.690440	10.950259
11.461759	725.450131	10.955264
11.797735	726.287720	10.960269
11.486567	727.458785	10.965274
11.872759	727.514022	10.970279
11.827717	727.909301	10.975283
11.642920	728.956123	10.980288
12.215406	743.027037	10.985293
12.051078	753.797977	10.990298
12.073828	745.298795	10.995303
12.006701	734.714872	11.000307
12.253959	755.164884	11.005312
12.403587	748.243037	11.010317
12.004387	734.655716	11.015322
12.117036	747.960983	11.020327
12.375642	759.861463	11.025331
12.249303	762.452380	11.030336
12.573827	757.186946	11.035341
12.564360	761.702175	11.040346
12.659883	768.859606	11.045351
12.798547	752.625306	11.050355
12.442140	749.502913	11.055360
12.668270	741.477531	11.060365
12.234995	743.716828	11.065370
12.390594	751.203738	11.070375
12.595442	759.373554	11.075379
12.345606	760.203654	11.080384
12.846839	761.257754	11.085389
12.765714	762.004168	11.090394
12.785497	766.642476	11.095399
12.826303	761.649394	11.100403
12.962520	770.109306	11.105408
12.956392	758.454264	11.110413
12.769105	764.505540	11.115418
12.811939	758.908117	11.120423
13.221846	773.651594	11.125427
13.195351	789.152303	11.130432
13.260421	780.726780	11.135437
13.185773	796.350303	11.140442
13.413696	796.719391	11.145447
13.777333	797.626694	11.150451
13.609614	792.545428	11.155456
13.533624	792.918834	11.160461
13.426173	789.111697	11.165466
13.612526	794.445746	11.170471
13.452701	787.279904	11.175475
13.139267	786.942073	11.180480
13.388789	784.213492	11.185485
13.369528	785.049395	11.190490
13.657746	795.293983	11.195495
13.964108	789.159311	11.200499
13.477274	796.002760	11.205504
13.576897	795.715747	11.210509
13.669704	815.630619	11.215514
13.930661	825.207740	11.220519
14.289833	829.176871	11.225523
14.179244	826.420561	11.230528
14.455622	821.274756	11.235533
14.284525	825.013052	11.240538
14.398816	819.785860	11.245543
14.178782	801.380308	11.250547
14.140475	824.900805	11.255552
14.427329	818.696686	11.260557
14.527105	829.289926	11.265562
14.411572	829.084544	11.270567
14.825703	833.732517	11.275571
14.767807	827.676433	11.280576
14.962310	804.615449	11.285581
14.464102	807.700964	11.290586
14.459250	796.581895	11.295591
14.630903	804.436885	11.300595
14.526119	823.746146	11.305600
14.868603	823.376236	11.310605
14.838335	832.247547	11.315610
14.523182	828.336324	11.320615
14.770243	833.044065	11.325619
14.902564	833.830559	11.330624
15.061715	827.298271	11.335629
14.839860	838.810215	11.340634
14.989940	833.675089	11.345639
14.999727	831.238649	11.350643
14.847265	830.198573	11.355648
15.171179	825.866844	11.360653
15.229203	828.117680	11.365658
15.167990	824.618574	11.370663
15.314221	833.958514	11.375667
15.213962	858.756921	11.380672
15.464130	863.697585	11.385677
15.606124	868.347974	11.390682
15.642408	857.861016	11.395687
15.815066	860.492575	11.400691
15.762666	864.626721	11.405696
15.937245	850.769559	11.410701
15.545339	837.225137	11.415706
15.631608	838.654541	11.420711
15.934195	851.825519	11.425715
15.712981	861.129462	11.430720
15.951124	852.193703	11.435725
15.995349	855.601170	11.440730
15.824500	866.368501	11.445735
16.024133	856.524173	11.450739
16.065768	853.978562	11.455744
16.256159	869.249203	11.460749
16.225495	860.201761	11.465754
15.913338	854.216187	11.470759
16.341011	861.808002	11.475763
16.093453	862.879038	11.480768
16.072784	860.909537	11.485773
16.026808	863.952893	11.490778
15.968987	862.719508	11.495783
16.432340	861.931315	11.500787
16.078651	863.317348	11.505792
16.399140	878.994637	11.510797
16.378413	895.630041	11.515802
16.399554	900.681372	11.520807
16.733963	894.034360	11.525811
16.536705	901.606019	11.530816
17.037622	892.051107	11.535821
16.929943	897.225496	11.540826
16.508524	897.530990	11.545831
16.989309	898.725570	11.550835
16.743430	903.423644	11.555840
16.912301	899.450967	11.560845
16.896671	908.364148	11.565850
16.995146	896.239687	11.570855
17.397325	889.379999	11.575859
16.924088	899.060085	11.580864
17.272578	893.301882	11.585869
17.308454	900.718072	11.590874
17.121948	901.873998	11.595879
17.450049	889.971557	11.600883
16.987135	900.060040	11.605888
17.135021	906.895346	11.610893
17.318372	915.551269	11.615898
17.483683	918.207667	11.620903
17.545683	915.671413	11.625907
17.708544	915.866363	11.630912
17.788463	915.809592	11.635917
17.681883	910.677528	11.640922
17.977900	918.995333	11.645927
18.037156	914.443995	11.650931
17.684598	921.516842	11.655936
18.003885	915.564575	11.660941
17.897691	925.895823	11.665946
17.981531	921.132386	11.670951
18.130835	912.240726	11.675955
17.907533	913.591772	11.680960
17.941104	909.686409	11.685965
18.011666	911.460554	11.690970
18.213729	910.285068	11.695975
18.203001	911.770956	11.700979
18.102225	913.892581	11.705984
18.305486	914.604680	11.710989
18.320993	913.378520	11.715994
18.233028	914.608622	11.720999
18.348429	917.578936	11.726003
17.933816	916.206898	11.731008
18.169676	909.501475	11.736013
18.481253	925.109266	11.741018
18.557470	943.006705	11.746023
18.611259	939.331519	11.751027
18.609305	944.808422	11.756032
18.961762	934.279651	11.761037
18.920411	952.534930	11.766042
19.042040	949.775463	11.771047
19.123721	948.284044	11.776051
18.634347	942.899184	11.781056
18.845428	942.875901	11.786061
18.910851	948.733178	11.791066
18.718631	957.307882	11.796071
18.593658	946.709375	11.801075
18.709366	951.686499	11.806080
18.897082	945.088884	11.811085
18.936666	949.356629	11.816090
19.249432	965.634540	11.821095
19.554595	965.039536	11.826099
19.520466	969.882856	11.831104
19.546384	949.177906	11.836109
19.659560	951.818969	11.841114
19.525834	945.838014	11.846119
20.017841	938.688774	11.851123
19.766759	942.620435	11.856128
19.878575	936.210776	11.861133
19.790516	944.988864	11.866138
20.004932	954.730416	11.871143
19.991020	941.287255	11.876147
19.829946	945.879557	11.881152
19.813789	945.715097	11.886157
19.635785	942.624922	11.891162
19.800398	945.108744	11.896167
19.853988	936.797724	11.901171
19.579689	946.276571	11.906176
19.818385	945.155958	11.911181
19.793002	950.326701	11.916186
20.062312	968.253302	11.921191
20.173576	965.149312	11.926195
20.073821	973.130483	11.931200
20.396094	968.835247	11.936205
20.365667	971.773635	11.941210
20.374767	981.488813	11.946215
20.369109	975.292646	11.951219
20.411540	972.778429	11.956224
20.708259	961.522815	11.961229
20.871450	972.335512	11.966234
20.757978	981.346353	11.971239
20.778859	968.272968	11.976243
20.784790	970.443818	11.981248
20.952928	963.885591	11.986253
20.494109	952.935804	11.991258
20.569639	965.703882	11.996263
21.172318	961.247217	12.001267
20.559671	971.022921	12.006272
20.814831	963.476168	12.011277
20.978395	973.724995	12.016282
21.017626	977.294151	12.021287
20.845918	972.069942	12.026291
21.006802	974.032345	12.031296
20.893049	966.184068	12.036301
20.966299	974.998739	12.041306
20.673597	974.086686	12.046311
20.887241	962.777295	12.051315
20.777091	974.161920	12.056320
21.027149	965.704417	12.061325
21.137406	971.534838	12.066330
20.873307	979.136912	12.071335
20.802943	968.510753	12.076339
21.072863	969.465347	12.081344
20.920861	973.891404	12.086349
20.959564	975.789710	12.091354
20.931446	969.056973	12.096359
20.875602	966.060070	12.101363
20.789110	983.573467	12.106368
21.162620	972.020141	12.111373
20.943506	971.957446	12.116378
20.871831	965.786008	12.121383
21.008110	965.523110	12.126387
21.208683	978.957291	12.131392
21.267790	974.633060	12.136397
21.140448	961.446904	12.141402
20.993443	955.832372	12.146407
21.128117	948.125057	12.151411
21.032478	957.274189	12.156416
21.214541	943.198106	12.161421
21.202672	952.586208	12.166426
20.924256	949.780943	12.171431
21.213478	944.947676	12.176435
20.959874	948.992504	12.181440
21.109843	950.209891	12.186445
21.124878	948.464150	12.191450
21.126003	945.571715	12.196455
21.164480	941.639539	12.201459
21.225432	955.509167	12.206464
20.980827	938.511762	12.211469
20.730159	924.528376	12.216474
20.761210	931.849149	12.221479
21.215087	934.330989	12.226483
20.907398	943.778888	12.231488
20.844929	923.660557	12.236493
20.906875	937.257172	12.241498
20.991855	928.300062	12.246503
21.034232	920.929209	12.251507
20.614981	925.336372	12.256512
20.990012	927.527197	12.261517
20.902071	949.705034	12.266522
20.989012	955.060519	12.271527
21.064122	942.539164	12.276531
20.736779	936.087580	12.281536
21.091263	938.546636	12.286541
20.758456	930.496754	12.291546
20.670587	946.394596	12.296551
21.098275	942.876620	12.301555
21.042908	951.502038	12.306560
21.259607	941.737728	12.311565
20.995018	929.093145	12.316570
20.749403	924.739468	12.321575
21.061648	924.528935	12.326579
20.793924	924.041871	12.331584
20.781916	923.763198	12.336589
21.034707	937.091232	12.341594
21.015259	933.271597	12.346599
20.959044	932.071857	12.351603
20.877722	929.407061	12.356608
21.129853	917.808477	12.361613
21.008877	920.903236	12.366618
20.796618	924.034634	12.371623
21.101924	921.992628	12.376627
20.967850	931.352108	12.381632
21.090649	929.291110	12.386637
21.292727	934.271800	12.391642
21.108780	932.777804	12.396647
21.490147	917.961840	12.401651
21.203011	925.899539	12.406656
21.026232	928.358958	12.411661
21.090130	927.886024	12.416666
20.918146	931.722268	12.421671
21.341061	921.856476	12.426675
21.296077	924.628427	12.431680
21.207184	903.804646	12.436685
21.128970	902.602898	12.441690
21.160565	910.333617	12.446695
21.130204	899.590731	12.451699
20.887477	909.379148	12.456704
21.156490	906.770449	12.461709
21.117583	921.322293	12.466714
20.876507	911.324277	12.471719
21.133267	911.231413	12.476723
20.632922	911.347629	12.481728
20.846483	907.571266	12.486733
20.735076	915.920937	12.491738
20.624748	912.760833	12.496743
20.741251	901.720106	12.501747
20.612089	909.810809	12.506752
21.058739	903.488118	12.511757
21.173990	910.394870	12.516762
20.646519	914.573265	12.521767
21.131311	902.311478	12.526771
20.748437	907.159150	12.531776
20.851302	910.609320	12.536781
21.006051	913.224820	12.541786
20.624522	916.034680	12.546791
20.843019	913.421420	12.551795
20.838020	919.807992	12.556800
20.724678	911.336728	12.561805
20.962969	904.657730	12.566810
20.617581	910.734284	12.571815
20.899384	908.498892	12.576819
21.024454	925.218317	12.581824
21.076596	926.509658	12.586829
21.181238	921.094718	12.591834
20.923206	919.503722	12.596839
21.184920	916.842564	12.601843
21.064977	927.015143	12.606848
21.050649	912.967260	12.611853
21.327859	917.692300	12.616858
20.907665	916.120861	12.621863
21.010414	914.809816	12.626867
20.915273	921.970924	12.631872
21.219737	916.265470	12.636877
20.985396	921.989973	12.641882
20.955220	919.608783	12.646887
21.227732	916.636793	12.651891
20.970589	914.933682	12.656896
20.938351	916.911899	12.661901
21.303585	920.365958	12.666906
20.979621	912.499195	12.671911
21.104483	907.311290	12.676915
20.713846	909.106956	12.681920
21.050739	904.883529	12.686925
20.913416	896.944424	12.691930
20.429599	896.712621	12.696935
20.801536	912.230340	12.701939
21.167286	916.138518	12.706944
21.031038	921.385287	12.711949
20.941945	916.914386	12.716954
20.894156	921.465742	12.721959
21.105282	923.848305	12.726963
20.962490	919.256647	12.731968
20.958394	899.583240	12.736973
20.945831	892.739239	12.741978
20.963328	892.200373	12.746983
21.229460	882.845357	12.751987
20.918051	883.115955	12.756992
20.743004	887.891044	12.761997
20.711829	884.554303	12.767002
20.570820	892.077558	12.772007
21.050181	905.327631	12.777011
20.820739	917.209886	12.782016
21.026287	920.635795	12.787021
20.973417	920.540274	12.792026
21.009050	925.857409	12.797031
21.313975	921.922953	12.802035
20.905537	900.071417	12.807040
21.021827	894.291899	12.812045
20.593792	887.317034	12.817050
20.779970	896.634872	12.822055
21.002803	901.032660	12.827059
20.905364	906.736897	12.832064
21.283642	899.070394	12.837069
21.067780	896.548500	12.842074
21.051007	896.082915	12.847079
21.045083	893.992776	12.852083
20.889189	900.611583	12.857088
20.789450	896.221241	12.862093
20.775277	894.285396	12.867098
20.739567	895.351030	12.872103
21.020276	882.427893	12.877107
20.793123	890.841748	12.882112
20.803765	889.578515	12.887117
21.132743	891.175810	12.892122
20.907462	890.579466	12.897127
20.932262	887.618606	12.902131
20.756833	891.737688	12.907136
20.879417	886.297820	12.912141
20.930861	899.756504	12.917146
20.727713	901.429214	12.922151
21.303575	910.443610	12.927155
20.915195	900.175758	12.932160
20.805326	891.380649	12.937165
20.780891	892.646351	12.942170
20.966230	897.062735	12.947175
21.028790	886.271919	12.952179
21.037558	889.082602	12.957184
20.851816	891.542656	12.962189
21.037926	897.260014	12.967194
21.048733	901.920300	12.972199
21.268577	893.563072	12.977203
20.989550	901.559393	12.982208
20.889690	896.118730	12.987213
21.084906	894.210992	12.992218
21.104628	898.943977	12.997223
21.290192	894.377230	13.002227
21.076753	902.998657	13.007232
21.071377	890.203154	13.012237
21.029353	898.366692	13.017242
21.212937	905.442330	13.022247
21.042527	898.251310	13.027251
20.805133	899.959447	13.032256
20.896894	898.011435	13.037261
21.096619	897.915052	13.042266
21.081976	901.628412	13.047271
21.212191	896.972714	13.052275
20.845693	885.651041	13.057280
20.867959	870.479208	13.062285
20.996180	871.313671	13.067290
20.799966	872.356015	13.072295
21.121529	866.669932	13.077299
20.703257	878.236893	13.082304
20.834973	887.355237	13.087309
20.926208	896.081041	13.092314
21.155906	891.311696	13.097319
20.768175	875.123372	13.102323
20.761230	885.692672	13.107328
20.840468	892.841723	13.112333
21.200890	893.710119	13.117338
20.811439	896.177433	13.122343
20.824678	895.916814	13.127347
20.758546	901.101925	13.132352
20.929763	899.753149	13.137357
20.761112	908.417902	13.142362
20.229409	935.061061	13.147367
20.864198	916.517435	13.152371
20.692091	919.306508	13.157376
20.956571	907.515134	13.162381
21.122716	912.617464	13.167386
20.453921	921.048160	13.172391
21.108997	918.682258	13.177395
20.683649	916.278937	13.182400
20.838841	912.051372	13.187405
20.725396	913.611996	13.192410
20.601140	914.270672	13.197415
21.114611	920.284361	13.202419
20.822484	913.562219	13.207424
21.135388	919.760877	13.212429
21.033606	911.059091	13.217434
20.859704	919.035499	13.222439
21.207241	913.501388	13.227443
21.002896	912.048498	13.232448
20.862169	910.501875	13.237453
21.144322	911.441109	13.242458
20.880107	908.106838	13.247463
21.259266	902.808981	13.252467
20.969354	914.953214	13.257472
21.178872	908.660459	13.262477
21.513849	912.280206	13.267482
21.069754	913.587615	13.272487
21.235018	906.445560	13.277491
21.108996	901.136811	13.282496
20.781248	890.362513	13.287501
20.898582	885.469155	13.292506
20.845426	888.277098	13.297511
20.888928	874.262610	13.302515
20.971960	895.417164	13.307520
21.151649	893.579717	13.312525
20.956102	889.908041	13.317530
20.580414	882.633067	13.322535
20.961166	877.388586	13.327539
20.911647	889.500762	13.332544
20.897499	885.057344	13.337549
21.179865	893.080820	13.342554
20.931858	889.881175	13.347559
20.782573	882.782995	13.352563
20.850698	878.375346	13.357568
20.854924	883.129723	13.362573
21.086951	893.350226	13.367578
20.788920	885.696979	13.372583
20.880376	894.088404	13.377587
21.129863	901.311237	13.382592
20.979705	900.472655	13.387597
21.125909	885.172218	13.392602
20.790932	892.756377	13.397607
21.104528	884.325848	13.402611
20.981081	892.399859	13.407616
21.011455	887.167104	13.412621
20.951281	882.089154	13.417626
20.987630	887.554406	13.422631
20.986018	885.105581	13.427635
20.810086	887.516757	13.432640
21.277545	878.060240	13.437645
21.377199	877.733793	13.442650
20.852507	885.110069	13.447655
21.426667	878.183528	13.452659
21.180616	878.192944	13.457664
21.055871	885.764068	13.462669
21.251894	886.338538	13.467674
21.154172	886.299062	13.472679
20.901547	865.405250	13.477683
20.636978	857.670981	13.482688
20.993657	861.741454	13.487693
20.914485	881.743778	13.492698
20.873169	886.365060	13.497703
21.296782	871.737963	13.502707
20.665885	870.894055	13.507712
20.696736	873.579778	13.512717
20.929050	884.599811	13.517722
20.702368	887.361309	13.522727
20.787360	880.855020	13.527731
20.606400	890.884329	13.532736
20.706606	884.782500	13.537741
20.867170	887.229897	13.542746
20.539235	892.787952	13.547751
21.048416	892.954473	13.552755
20.792097	890.003756	13.557760
21.142653	886.066763	13.562765
21.283688	887.239834	13.567770
21.042259	893.826547	13.572775
21.160383	892.675491	13.577779
21.141005	899.860777	13.582784
21.237258	891.106913	13.587789
21.308569	883.106149	13.592794
21.146240	867.377086	13.597799
21.126352	861.753354	13.602803
20.579648	859.273198	13.607808
20.804482	863.106058	13.612813
20.926516	864.673276	13.617818
20.732838	861.873436	13.622823
20.908543	854.959995	13.627827
20.589077	866.205232	13.632832
20.788116	886.899686	13.637837
21.183685	887.601613	13.642842
20.736391	892.524216	13.647847
20.778799	892.514432	13.652851
20.664351	898.065247	13.657856
20.974335	895.106210	13.662861
21.330054	893.223338	13.667866
21.113911	902.239468	13.672871
21.110029	894.586611	13.677875
20.972269	882.372097	13.682880
21.026107	866.277367	13.687885
20.915378	858.786664	13.692890
20.908742	861.479940	13.697895
21.026120	856.520347	13.702899
20.671705	863.927804	13.707904
20.467047	861.716391	13.712909
21.032844	878.570485	13.717914
20.824448	884.491126	13.722919
20.946395	887.424116	13.727923
21.061004	903.944896	13.732928
20.856823	896.070075	13.737933
21.083793	891.730134	13.742938
20.782030	894.670781	13.747943
21.120097	889.903076	13.752947
21.158734	891.903104	13.757952
20.952990	881.459465	13.762957
21.118794	862.386689	13.767962
20.977898	867.269873	13.772967
20.859993	862.008734	13.777971
20.574033	861.992975	13.782976
20.525207	864.413838	13.787981
20.902531	870.535961	13.792986
20.807983	895.317750	13.797991
21.313364	893.835242	13.802995
21.044270	895.425423	13.808000
21.102068	894.318685	13.813005
20.986029	870.181090	13.818010
20.777701	877.232486	13.823015
20.985861	856.948067	13.828019
20.640734	863.863569	13.833024
21.037452	881.342351	13.838029
21.286615	882.882984	13.843034
20.939324	878.260874	13.848039
20.962566	857.906593	13.853043
20.928450	862.730163	13.858048
20.999226	862.947686	13.863053
20.901364	856.948430	13.868058
20.737696	864.235568	13.873063
20.882514	859.675331	13.878067
20.744988	868.093802	13.883072
20.896662	875.368496	13.888077
21.038914	868.525045	13.893082
21.108870	882.330873	13.898087
21.025892	861.187639	13.903091
20.823228	869.532915	13.908096
21.015222	866.335638	13.913101
20.897683	871.631449	13.918106
20.806663	871.314914	13.923111
21.302896	865.173581	13.928115
20.819278	863.404089	13.933120
21.026392	868.160795	13.938125
21.030995	863.701776	13.943130
20.575287	873.967302	13.948135
20.756071	870.469012	13.953139
20.761667	871.912865	13.958144
21.055687	874.622848	13.963149
20.960769	866.632836	13.968154
20.607395	877.402480	13.973159
20.916305	879.774170	13.978163
20.998453	894.860236	13.983168
21.084075	887.398128	13.988173
21.169138	877.080009	13.993178
20.860394	877.017417	13.998183
20.642009	869.677932	14.003187
20.885334	878.828935	14.008192
20.688565	874.008271	14.013210
21.137450	889.684746	14.018227
20.940773	897.117523	14.023245
21.214567	887.468853	14.028263
20.826975	881.236983	14.033280
21.012159	895.017511	14.038298
21.155539	889.632199	14.043315
20.921508	884.701927	14.048333
21.338084	886.531158	14.053351
21.129684	882.170967	14.058368
20.748634	878.341695	14.063386
21.143549	889.592315	14.068403
20.983244	902.254452	14.073421
21.309842	900.031662	14.078439
20.979684	908.984867	14.083456
21.281833	903.169947	14.088474
21.140396	895.863730	14.093491
21.110143	913.431973	14.098509
21.189809	904.838323	14.103527
21.136293	903.470562	14.108544
21.345404	911.784033	14.113562
21.122349	907.462352	14.118579
21.015609	911.621397	14.123597
21.461640	903.301228	14.128615
21.339827	905.667807	14.133632
21.208551	911.290572	14.138650
21.544070	909.096246	14.143667
21.400973	909.232467	14.148685
21.580265	903.618045	14.153703
21.713851	906.916043	14.158720
21.474273	911.620107	14.163738
21.787937	908.062273	14.168755
21.446043	916.325205	14.173773
21.639841	904.740253	14.178791
21.497911	915.422127	14.183808
21.277161	914.996564	14.188826
21.357880	915.889911	14.193843
21.526631	915.164687	14.198861
21.596439	906.731489	14.203879
21.628829	916.816108	14.208896
21.816461	912.112732	14.213914
21.730693	917.742398	14.218931
21.336528	920.235794	14.223949
21.700130	916.128857	14.228967
21.714405	915.488050	14.233984
21.081713	925.966631	14.239002
21.511448	917.710403	14.244019
21.349111	922.367543	14.249037
21.732304	934.142325	14.254055
21.670308	949.316744	14.259072
21.783657	947.565276	14.264090
21.908406	944.550387	14.269107
21.464384	954.855745	14.274125
21.483100	951.178200	14.279143
21.757693	946.478247	14.284160
21.393764	951.184855	14.289178
21.881464	948.692536	14.294195
22.267807	954.463995	14.299213
22.069035	944.134017	14.304231
22.171438	952.810608	14.309248
22.205138	954.754403	14.314266
22.271888	950.954363	14.319283
21.857619	948.193767	14.324301
22.047377	951.352250	14.329319
22.416016	947.006967	14.334336
22.081094	950.861064	14.339354
21.972090	951.059489	14.344371
22.054898	954.946059	14.349389
22.285700	950.098928	14.354407
22.327185	948.867024	14.359424
22.204603	958.556382	14.364442
22.698084	949.770854	14.369459
21.925969	962.146800	14.374477
22.095730	963.586747	14.379495
22.357095	962.922257	14.384512
21.992341	962.719442	14.389530
22.687566	951.193691	14.394547
22.036417	951.456567	14.399565
21.761435	950.693578	14.404583
22.028984	955.436321	14.409600
22.089178	964.031559	14.414618
22.252658	960.210581	14.419635
22.269601	978.924437	14.424653
22.749725	979.295530	14.429671
22.608874	985.876279	14.434688
22.534236	991.882522	14.439706
22.576093	985.160523	14.444723
22.393087	979.264864	14.449741
22.404186	971.121786	14.454759
22.649539	981.173268	14.459776
22.359934	992.712482	14.464794
22.554213	989.021082	14.469811
22.479689	998.549426	14.474829
22.571441	993.810193	14.479847
23.016740	985.376046	14.484864
22.930535	997.823520	14.489882
23.015331	992.541112	14.494899
22.737825	978.359409	14.499917
22.718338	973.458595	14.504935
22.619588	970.434517	14.509952
22.634019	984.332818	14.514970
22.949391	984.347932	14.519987
22.599681	982.282557	14.525005
22.623656	996.498681	14.530023
22.899559	986.122849	14.535040
22.442172	987.117762	14.540058
22.376262	983.593711	14.545075
22.731482	986.034443	14.550093
22.651911	987.200334	14.555111
22.598595	984.296425	14.560128
22.458963	1001.345803	14.565146
22.828226	996.056560	14.570163
22.814889	1002.770353	14.575181
23.015166	1008.464543	14.580199
23.104717	1004.598715	14.585216
23.214178	1005.045448	14.590234
23.091669	1006.001892	14.595251
22.906667	1009.286232	14.600269
22.927174	1013.979520	14.605287
23.173119	1010.821012	14.610304
22.901830	1014.311033	14.615322
23.039340	1004.276597	14.620339
23.081040	1012.571210	14.625357
22.979766	1008.444799	14.630375
23.401189	1005.401453	14.635392
22.994368	1013.517488	14.640410
23.209396	1014.103118	14.645427
23.272307	1012.425756	14.650445
23.094042	1011.659135	14.655463
23.169773	1015.185829	14.660480
23.005362	1022.983983	14.665498
23.314937	1029.319867	14.670515
23.716524	1036.630546	14.675533
23.378828	1048.376470	14.680551
23.654328	1041.076038	14.685568
23.664297	1035.875552	14.690586
23.816365	1021.026731	14.695603
23.853722	1018.661290	14.700621
23.395770	1009.424209	14.705639
23.596293	1008.590877	14.710656
23.636132	1008.621625	14.715674
23.848796	1000.474695	14.720691
23.738354	1005.312353	14.725709
23.370387	1016.129458	14.730727
23.922219	1007.605945	14.735744
23.747479	1010.117054	14.740762
23.772070	1004.927618	14.745779
23.720005	1002.591387	14.750797
23.495593	1008.941648	14.755815
24.024633	1005.395056	14.760832
23.488361	1013.847141	14.765850
23.865824	1007.219471	14.770867
23.903853	1008.761448	14.775885
23.735633	1010.016202	14.780903
24.009550	1011.272009	14.785920
23.636268	1007.974737	14.790938
23.794368	1008.613493	14.795955
23.776583	1014.678319	14.800973
23.756306	1010.973945	14.805991
23.807328	1012.532727	14.811008
23.705269	1030.530217	14.816026
23.781960	1038.760273	14.821043
23.933785	1039.056313	14.826061
23.930457	1046.614060	14.831079
24.192395	1043.855704	14.836096
24.212542	1036.780055	14.841114
24.147414	1040.688671	14.846131
24.336853	1041.873009	14.851149
24.106794	1039.536060	14.856167
24.325141	1038.788763	14.861184
24.169824	1037.731392	14.866202
23.995998	1042.552430	14.871219
24.506829	1035.813809	14.876237
24.359683	1044.542057	14.881255
24.603337	1038.700233	14.886272
24.116513	1027.642185	14.891290
24.164381	1020.434703	14.896307
24.392721	1027.944477	14.901325
24.123076	1040.021684	14.906343
24.668131	1033.150185	14.911360
24.669810	1031.890015	14.916378
24.379792	1023.114581	14.921395
24.012671	1012.943545	14.926413
23.907526	1033.154064	14.931431
24.551037	1033.499885	14.936448
24.253699	1038.278485	14.941466
24.122570	1039.978800	14.946483
24.483411	1047.455651	14.951501
24.312596	1044.020680	14.956519
24.598622	1039.246512	14.961536
24.438966	1048.457333	14.966554
24.700170	1045.580326	14.971571
24.835878	1043.204699	14.976589
24.407592	1043.199213	14.981607
24.581144	1042.593559	14.986624
24.435013	1044.857856	14.991642
24.466517	1056.287698	14.996659
24.882563	1060.166764	15.001677
24.767540	1065.786995	15.006695
25.065647	1064.876744	15.011712
24.673257	1064.665751	15.016730
24.711419	1059.849311	15.021747
24.985531	1064.506883	15.026765
24.983863	1074.476703	15.031783
25.221466	1056.870744	15.036800
24.879192	1042.297386	15.041818
24.904816	1039.238511	15.046835
24.928021	1036.150921	15.051853
24.972987	1040.728627	15.056871
25.193261	1046.915950	15.061888
25.089990	1039.654698	15.066906
24.855519	1040.306520	15.071923
25.124971	1047.101074	15.076941
24.964299	1056.618813	15.081959
25.233809	1057.167439	15.086976
25.271763	1066.212254	15.091994
25.178012	1056.842330	15.097011
25.222795	1048.151909	15.102029
25.092331	1066.084758	15.107047
25.348078	1065.321269	15.112064
25.179718	1072.939960	15.117082
25.451033	1069.524128	15.122099
25.375900	1050.416998	15.127117
25.103554	1050.575408	15.132135
25.271543	1051.012021	15.137152
25.579037	1066.665622	15.142170
25.388988	1056.657441	15.147187
25.494834	1063.816311	15.152205
25.290143	1055.057922	15.157223
25.668975	1051.289877	15.162240
25.366320	1045.649237	15.167258
25.322342	1038.448531	15.172275
25.732378	1050.206542	15.177293
25.477430	1059.714938	15.182311
25.760871	1055.166914	15.187328
25.446307	1054.024041	15.192346
25.453619	1065.163582	15.197363
25.676962	1054.387083	15.202381
26.008045	1067.551453	15.207399
25.857127	1045.049119	15.212416
25.432737	1039.135306	15.217434
25.529683	1043.770791	15.222451
25.888762	1050.227782	15.227469
25.678472	1059.804564	15.232487
25.861020	1054.191139	15.237504
25.534983	1060.580441	15.242522
25.736021	1067.590417	15.247539
25.819451	1048.370693	15.252557
25.881970	1063.298846	15.257575
25.777544	1060.250486	15.262592
25.661110	1071.701577	15.267610
25.312368	1066.928757	15.272627
25.898432	1064.427808	15.277645
25.540565	1069.784743	15.282663
25.703607	1064.170493	15.287680
25.567946	1077.661799	15.292698
25.852372	1090.092707	15.297715
25.926659	1097.042688	15.302733
26.238141	1098.036097	15.307751
26.337964	1095.850237	15.312768
26.560918	1099.211105	15.317786
26.335236	1096.393657	15.322803
26.556929	1086.888452	15.327821
25.969072	1074.966342	15.332839
26.206047	1063.239879	15.337856
26.213003	1074.919839	15.342874
26.534174	1077.242531	15.347891
26.154274	1067.953636	15.352909
25.785302	1077.820804	15.357927
26.308354	1090.749286	15.362944
26.492494	1092.577866	15.367962
26.006723	1099.617178	15.372979
26.425889	1095.082102	15.377997
26.422625	1096.386060	15.383015
26.524669	1092.065954	15.388032
26.768551	1098.199195	15.393050
26.646281	1100.020017	15.398067
26.806982	1090.567012	15.403085
26.439681	1100.361566	15.408103
26.586661	1089.530366	15.413120
27.001675	1093.752538	15.418138
26.557630	1097.910379	15.423155
26.897133	1090.931635	15.428173
26.671828	1092.467645	15.433191
26.679029	1087.767824	15.438208
26.755260	1091.771102	15.443226
26.767302	1087.124780	15.448243
26.853109	1079.082987	15.453261
26.684272	1083.728631	15.458279
26.558273	1076.421433	15.463296
27.167964	1089.852068	15.468314
26.916067	1084.883676	15.473331
27.044179	1081.706982	15.478349
26.804128	1071.103488	15.483367
26.834949	1071.254442	15.488384
27.113538	1082.682649	15.493402
27.124621	1077.024989	15.498419
27.138230	1073.699026	15.503437
26.489021	1070.990824	15.508455
26.954836	1081.980951	15.513472
27.215154	1089.073508	15.518490
26.978149	1096.022801	15.523507
27.584750	1101.823685	15.528525
27.358430	1096.275460	15.533543
26.979750	1082.671383	15.538560
27.026439	1090.797711	15.543578
26.976937	1096.890441	15.548595
27.404846	1091.428210	15.553613
27.171434	1092.931691	15.558631
27.251314	1090.175623	15.563648
27.152578	1089.589015	15.568666
27.144728	1096.608727	15.573683
27.005725	1095.458298	15.578701
27.226020	1101.618112	15.583719
27.432849	1096.164399	15.588736
27.340216	1088.792096	15.593754
27.026071	1096.861146	15.598771
27.138133	1085.982033	15.603789
27.145702	1096.733005	15.608807
27.344439	1110.928446	15.613824
27.340302	1113.553939	15.618842
27.401949	1116.258606	15.623859
27.626099	1121.504636	15.628877
27.661734	1116.823866	15.633895
27.506227	1114.816374	15.638912
27.490787	1123.485907	15.643930
27.458619	1125.481132	15.648947
27.555592	1116.531438	15.653965
27.650858	1123.714048	15.658983
27.761364	1125.047055	15.664000
27.933589	1114.143380	15.669018
27.653279	1123.898906	15.674035
27.786178	1114.699654	15.679053
27.569083	1117.341811	15.684071
27.505421	1112.871157	15.689088
27.857613	1128.540505	15.694106
28.079287	1148.621975	15.699123
28.195469	1135.197691	15.704141
28.016747	1130.187723	15.709159
27.977592	1134.149640	15.714176
28.338953	1118.688440	15.719194
27.906462	1126.268275	15.724211
28.313026	1113.743121	15.729229
28.004204	1116.205632	15.734247
27.584549	1114.190721	15.739264
28.194779	1128.044466	15.744282
28.177992	1148.606010	15.749299
28.400710	1130.161518	15.754317
28.509903	1147.030586	15.759335
28.277025	1147.723845	15.764352
28.569019	1142.538901	15.769370
28.307992	1129.232993	15.774387
27.975387	1125.860776	15.779405
28.264198	1135.350920	15.784423
28.154027	1138.540766	15.789440
28.732224	1143.052330	15.794458
28.711039	1143.184051	15.799475
28.816319	1133.964023	15.804493
28.538785	1122.269239	15.809511
28.347975	1122.027665	15.814528
28.426836	1118.353856	15.819546
28.613807	1130.674497	15.824563
28.510762	1129.225734	15.829581
28.798191	1134.653593	15.834599
28.698437	1135.607201	15.839616
29.081236	1120.916540	15.844634
28.555740	1109.315589	15.849651
28.573369	1103.593951	15.854669
28.498912	1114.246331	15.859687
28.841149	1130.225594	15.864704
29.159260	1124.879182	15.869722
28.693500	1123.752553	15.874739
28.663354	1131.304396	15.879757
28.759541	1137.091535	15.884775
28.834283	1132.270023	15.889792
28.977376	1135.952750	15.894810
28.678962	1143.578852	15.899827
29.153767	1142.191296	15.904845
29.069182	1141.095893	15.909863
28.887657	1142.794818	15.914880
29.012466	1139.698079	15.919898
29.161733	1145.110224	15.924915
28.779680	1142.766040	15.929933
28.579268	1141.063022	15.934951
28.854748	1135.040684	15.939968
28.991462	1134.840467	15.944986
28.816897	1146.929339	15.950003
29.288277	1151.963692	15.955021
29.039461	1158.329708	15.960039
28.912924	1170.306328	15.965056
29.419688	1168.525905	15.970074
29.489209	1164.225909	15.975091
29.131731	1166.516070	15.980109
29.377869	1172.934500	15.985127
29.460367	1168.675693	15.990144
29.688025	1169.844507	15.995162
29.651911	1175.355449	16.000179
29.816031	1168.115193	16.005197
29.700919	1151.697220	16.010215
29.421758	1153.547792	16.015232
29.594489	1141.881853	16.020250
29.515481	1152.040248	16.025267
29.423309	1163.671594	16.030285
29.829868	1167.169940	16.035303
29.947012	1165.835497	16.040320
29.842852	1153.759875	16.045338
29.481050	1153.979747	16.050355
29.886990	1155.953863	16.055373
30.215927	1152.680624	16.060391
29.697319	1140.490213	16.065408
29.972568	1134.820284	16.070426
29.994152	1135.419470	16.075443
29.824085	1132.071665	16.080461
29.718788	1129.107589	16.085479
29.628261	1137.013573	16.090496
30.220432	1146.224093	16.095514
29.878900	1151.443953	16.100531
30.201857	1156.000952	16.105549
30.451180	1141.584827	16.110567
29.934571	1144.835569	16.115584
30.205631	1134.430516	16.120602
29.820575	1146.484532	16.125619
30.052833	1159.155853	16.130637
30.334922	1154.206089	16.135655
30.137807	1161.050732	16.140672
30.416708	1157.238037	16.145690
30.321563	1169.679218	16.150707
30.333994	1160.749274	16.155725
30.304691	1151.013489	16.160743
30.285807	1180.910148	16.165760
30.526111	1164.150741	16.170778
30.763062	1162.323687	16.175795
30.332644	1145.816794	16.180813
30.310851	1145.638713	16.185831
30.513304	1155.441532	16.190848
30.382117	1151.062650	16.195866
30.296217	1159.348597	16.200883
30.244183	1163.119086	16.205901
30.266442	1159.001244	16.210919
30.464322	1162.186007	16.215936
30.537167	1162.703083	16.220954
30.508320	1160.897974	16.225971
30.558722	1164.632461	16.230989
30.499860	1156.580666	16.236007
30.265265	1164.795947	16.241024
30.498722	1155.947161	16.246042
30.436720	1188.366089	16.251059
30.659949	1191.321863	16.256077
31.137826	1187.751927	16.261095
31.206920	1195.184151	16.266112
31.085562	1191.922162	16.271130
31.144323	1190.380728	16.276147
30.910716	1174.929419	16.281165
30.992342	1181.846808	16.286183
30.663583	1186.183708	16.291200
30.926027	1191.297022	16.296218
31.066495	1190.340332	16.301235
31.016816	1191.772831	16.306253
31.142621	1188.401417	16.311271
31.079203	1189.715764	16.316288
31.002649	1188.766161	16.321306
31.074448	1189.636565	16.326323
31.215272	1197.991769	16.331341
31.177991	1195.417970	16.336359
31.118431	1192.117808	16.341376
31.174357	1192.409485	16.346394
31.085598	1191.478346	16.351411
31.185766	1192.468500	16.356429
31.508376	1185.241497	16.361447
31.297491	1192.012056	16.366464
31.107392	1188.224606	16.371482
31.765683	1205.634612	16.376499
31.986434	1204.958500	16.381517
32.001607	1190.641811	16.386535
31.620824	1188.824404	16.391552
31.511865	1181.555336	16.396570
31.794073	1191.208599	16.401587
31.430500	1184.251500	16.406605
31.647040	1180.101877	16.411623
31.786786	1186.397277	16.416640
31.679049	1188.358944	16.421658
31.759761	1179.419670	16.426675
31.762294	1190.413772	16.431693
31.649083	1188.353117	16.436711
31.782517	1199.285446	16.441728
32.056939	1207.191464	16.446746
31.832621	1209.682985	16.451763
32.051215	1214.737231	16.456781
32.382119	1203.566709	16.461799
32.166801	1192.421182	16.466816
31.537121	1187.181087	16.471834
31.713187	1187.706083	16.476851
31.922242	1205.981371	16.481869
32.168143	1212.765602	16.486887
32.003968	1211.568839	16.491904
32.286711	1203.173081	16.496922
32.533329	1205.175762	16.501939
32.054411	1210.420701	16.506957
32.380286	1210.564710	16.511975
32.205737	1209.076219	16.516992
32.312639	1206.022435	16.522010
32.377679	1206.050738	16.527027
32.291348	1211.293624	16.532045
32.411000	1204.931153	16.537063
32.236872	1215.120495	16.542080
32.415898	1207.468050	16.547098
32.559753	1211.233263	16.552115
32.372209	1212.192227	16.557133
32.473405	1206.701050	16.562151
32.446416	1209.468638	16.567168
32.344138	1214.241352	16.572186
32.171609	1207.230174	16.577203
32.164970	1217.341677	16.582221
32.427012	1229.226478	16.587239
32.559681	1242.550076	16.592256
32.780084	1236.246244	16.597274
32.780920	1237.494502	16.602291
32.593551	1240.651064	16.607309
32.664823	1243.553217	16.612327
32.954895	1244.990521	16.617344
32.747725	1236.275678	16.622362
32.619746	1243.044834	16.627379
32.777857	1237.525691	16.632397
33.259926	1237.467026	16.637415
33.017511	1241.513305	16.642432
33.162927	1239.219473	16.647450
33.197846	1227.005984	16.652467
32.869260	1240.924633	16.657485
33.023640	1242.290767	16.662503
32.946440	1239.854682	16.667520
33.063965	1260.114948	16.672538
33.156315	1265.564533	16.677555
33.312479	1271.615879	16.682573
33.446717	1264.091677	16.687591
33.287003	1269.680574	16.692608
33.366440	1270.065248	16.697626
33.600159	1258.364318	16.702643
33.381375	1264.782222	16.707661
33.467939	1264.219536	16.712679
33.439785	1255.205554	16.717696
33.248270	1264.642614	16.722714
33.529563	1264.604962	16.727731
33.432620	1266.219621	16.732749
33.734119	1256.503366	16.737767
33.594635	1264.691734	16.742784
33.721035	1262.885448	16.747802
33.805096	1261.189740	16.752819
33.525471	1276.046050	16.757837
33.711241	1255.715633	16.762855
33.712782	1266.979738	16.767872
33.964186	1267.894649	16.772890
34.145252	1255.922107	16.777907
33.640213	1269.946797	16.782925
33.963347	1269.323568	16.787943
33.636801	1270.295268	16.792960
33.582152	1271.868573	16.797978
33.768380	1265.622092	16.802995
33.778993	1274.225422	16.808013
33.934554	1270.108310	16.813031
34.126030	1278.077936	16.818048
34.127325	1286.020481	16.823066
34.300579	1282.190782	16.828083
34.013616	1284.764671	16.833101
34.363567	1285.383065	16.838119
34.297105	1287.611883	16.843136
34.228993	1289.877931	16.848154
34.222688	1282.242423	16.853171
34.466512	1304.495396	16.858189
34.583381	1301.120662	16.863207
34.449856	1280.575283	16.868224
34.107894	1271.651458	16.873242
34.064833	1279.066218	16.878259
34.397569	1288.526647	16.883277
34.455447	1287.093101	16.888295
34.555383	1290.901521	16.893312
34.706441	1303.461644	16.898330
35.070310	1290.383123	16.903347
34.837598	1298.196250	16.908365
34.908828	1299.932748	16.913383
34.816727	1301.598551	16.918400
34.758248	1300.352672	16.923418
34.723695	1296.107779	16.928435
34.357220	1298.461533	16.933453
34.666685	1300.077444	16.938471
34.704980	1297.526968	16.943488
34.731200	1296.030041	16.948506
34.822946	1297.469881	16.953523
34.649102	1303.530617	16.958541
34.830863	1292.969013	16.963559
35.093757	1296.181977	16.968576
34.965471	1293.560539	16.973594
34.888153	1296.226840	16.978611
34.645986	1299.893189	16.983629
35.131880	1303.903548	16.988647
35.423682	1321.199894	16.993664
35.167281	1321.799379	16.998682
35.561727	1309.193404	17.003699
35.458197	1307.240519	17.008717
35.299875	1303.327627	17.013735
35.407341	1293.264749	17.018752
35.251713	1298.816824	17.023770
35.478665	1299.837889	17.028787
35.518335	1311.214717	17.033805
35.699605	1308.789306	17.038823
35.577158	1298.549940	17.043840
35.111118	1302.739661	17.048858
35.798986	1296.303825	17.053875
35.530696	1303.832391	17.058893
35.692241	1309.124656	17.063911
35.569915	1309.787704	17.068928
35.806514	1318.358948	17.073946
36.112047	1303.770095	17.078963
35.780850	1298.234587	17.083981
35.361968	1290.086762	17.088999
35.689752	1298.432654	17.094016
35.543686	1314.128190	17.099034
35.921055	1299.073255	17.104051
35.660821	1310.405890	17.109069
35.923286	1306.881297	17.114087
35.980269	1312.962638	17.119104
35.845018	1317.197922	17.124122
35.922221	1306.190491	17.129139
36.036675	1312.633919	17.134157
35.787297	1316.140179	17.139175
36.047936	1310.456782	17.144192
35.712700	1311.041312	17.149210
35.887540	1324.515570	17.154227
36.218586	1331.616629	17.159245
36.171208	1344.339006	17.164263
36.656158	1338.703197	17.169280
36.207032	1343.123052	17.174298
36.316671	1340.853002	17.179315
36.509026	1347.497177	17.184333
36.297814	1343.667433	17.189351
36.206421	1340.565021	17.194368
36.383636	1343.052299	17.199386
36.651636	1340.996890	17.204403
36.760329	1343.855340	17.209421
36.555881	1342.093162	17.214439
36.833573	1335.204391	17.219456
36.954257	1338.369257	17.224474
37.168735	1331.199545	17.229491
37.120135	1335.920477	17.234509
36.980282	1333.578530	17.239527
36.917610	1331.295063	17.244544
36.680108	1340.204649	17.249562
36.962775	1328.241799	17.254579
36.817767	1332.479430	17.259597
36.514477	1338.847133	17.264615
37.091590	1330.275356	17.269632
36.986015	1337.576628	17.274650
37.067968	1336.615104	17.279667
36.944484	1335.333971	17.284685
36.802754	1333.374590	17.289703
36.813072	1328.877912	17.294720
36.847213	1337.547530	17.299738
36.920838	1333.193344	17.304755
36.886744	1347.957079	17.309773
37.419123	1356.672303	17.314791
37.369554	1362.861900	17.319808
37.265417	1369.213583	17.324826
37.540348	1359.123164	17.329843
37.494173	1368.791167	17.334861
37.797454	1360.082141	17.339879
38.061146	1343.620835	17.344896
37.958463	1328.065106	17.349914
38.003576	1318.879727	17.354931
37.817823	1318.345529	17.359949
37.931108	1320.405675	17.364967
37.963098	1318.789056	17.369984
37.746739	1323.985864	17.375002
38.113391	1312.861471	17.380019
37.734471	1316.815491	17.385037
37.543112	1313.692848	17.390055
37.868978	1317.563559	17.395072
37.718526	1321.426868	17.400090
37.822031	1316.138214	17.405107
37.608445	1312.207391	17.410125
37.640915	1309.863133	17.415143
38.094496	1318.510673	17.420160
37.682552	1320.775722	17.425178
38.008510	1308.498439	17.430195
37.900144	1310.173130	17.435213
38.140770	1315.112993	17.440231
38.028951	1308.473561	17.445248
38.279836	1324.965500	17.450266
38.136604	1332.666840	17.455283
38.401076	1339.657393	17.460301
38.380159	1346.770551	17.465319
38.384051	1339.694988	17.470336
38.314440	1351.618630	17.475354
38.802422	1338.937145	17.480371
38.523486	1336.724353	17.485389
38.126345	1325.179837	17.490407
38.528929	1329.813859	17.495424
38.323702	1336.615830	17.500442
38.290210	1336.919412	17.505459
38.482391	1340.135800	17.510477
38.538183	1345.560571	17.515495
38.352409	1342.594342	17.520512
38.467907	1353.617742	17.525530
38.662187	1338.875916	17.530547
38.739194	1344.177746	17.535565
38.618222	1347.709939	17.540583
38.913521	1353.562153	17.545600
39.060280	1377.569799	17.550618
39.059626	1369.991548	17.555635
39.118183	1374.921930	17.560653
39.071706	1376.425513	17.565671
39.306565	1366.706442	17.570688
38.990193	1362.097469	17.575706
38.947889	1365.900280	17.580723
38.917438	1371.448147	17.585741
38.770314	1385.046964	17.590759
39.299710	1373.661386	17.595776
39.147589	1377.588688	17.600794
39.216712	1375.130028	17.605811
39.373564	1376.455666	17.610829
39.405795	1373.242289	17.615847
39.468785	1368.993615	17.620864
39.281840	1381.346579	17.625882
39.520209	1366.310599	17.630899
39.187918	1373.504109	17.635917
39.108964	1379.878523	17.640935
39.459338	1371.254006	17.645952
39.608201	1371.137584	17.650970
39.532491	1379.985993	17.655987
39.378379	1395.549185	17.661005
39.534555	1391.741846	17.666023
39.930704	1396.279382	17.671040
39.378472	1406.651082	17.676058
39.793335	1400.075476	17.681075
40.169461	1391.847199	17.686093
39.647401	1403.301108	17.691111
39.798100	1400.403904	17.696128
39.857731	1401.243226	17.701146
39.862001	1405.910914	17.706163
39.963972	1399.253073	17.711181
39.960603	1404.410432	17.716199
40.203768	1401.814676	17.721216
40.134783	1412.788891	17.726234
40.304723	1413.990528	17.731251
40.587044	1416.111822	17.736269
40.202867	1407.083740	17.741287
40.522660	1397.998441	17.746304
40.415146	1392.221140	17.751322
40.481475	1389.072325	17.756339
40.591728	1385.877176	17.761357
40.305238	1397.568017	17.766375
40.587255	1391.528014	17.771392
40.417184	1399.249401	17.776410
40.705843	1416.399276	17.781427
40.991344	1419.861149	17.786445
40.602726	1402.782543	17.791463
40.646861	1395.079938	17.796480
40.967219	1412.234977	17.801498
40.989890	1417.348860	17.806515
41.070560	1397.396040	17.811533
40.782179	1388.550117	17.816551
40.867330	1386.441277	17.821568
40.625703	1400.358007	17.826586
40.711227	1412.463033	17.831603
40.887739	1412.329616	17.836621
40.892898	1427.966546	17.841639
41.191805	1416.043508	17.846656
41.071105	1422.854848	17.851674
41.181056	1409.033306	17.856691
41.453881	1411.996947	17.861709
41.372638	1416.911886	17.866727
41.609972	1410.838101	17.871744
41.273737	1410.452964	17.876762
41.418010	1414.830894	17.881779
41.644289	1400.875181	17.886797
41.040107	1411.125387	17.891815
41.562550	1410.287883	17.896832
41.358162	1409.653614	17.901850
41.375528	1412.952960	17.906867
41.506493	1421.482908	17.911885
41.174433	1422.162896	17.916903
41.497281	1418.303796	17.921920
41.446777	1413.591836	17.926938
41.310317	1418.418049	17.931955
41.588484	1423.141163	17.936973
41.477883	1442.978718	17.941991
41.794357	1441.389074	17.947008
41.642613	1447.204083	17.952026
41.559908	1454.331868	17.957043
41.819256	1454.315808	17.962061
41.657987	1447.467108	17.967079
42.041290	1448.077832	17.972096
42.028841	1448.518855	17.977114
41.920792	1446.014504	17.982131
42.072969	1448.269825	17.987149
41.604030	1446.965124	17.992167
42.148061	1468.844832	17.997184
42.214029	1473.633270	18.002202
42.123728	1477.490959	18.007219
41.981040	1473.279779	18.012237
41.993491	1485.256513	18.017255
42.542471	1473.776493	18.022272
42.552521	1475.844475	18.027290
42.234705	1483.264620	18.032307
42.561001	1475.417075	18.037325
42.501490	1481.887539	18.042343
42.544113	1485.099498	18.047360
42.714991	1479.958924	18.052378
42.725433	1487.590214	18.057395
42.953241	1491.026697	18.062413
42.571992	1489.869252	18.067431
42.916863	1495.753732	18.072448
43.048555	1493.333053	18.077466
42.967285	1494.591283	18.082483
43.331783	1483.055731	18.087501
42.854828	1472.953014	18.092519
42.792217	1466.877493	18.097536
43.068396	1480.776208	18.102554
43.164666	1485.223168	18.107571
43.101192	1484.149541	18.112589
42.973127	1491.033665	18.117607
42.925240	1487.281659	18.122624
43.360413	1485.667573	18.127642
43.287042	1490.969057	18.132659
43.470188	1493.106181	18.137677
43.214005	1492.120709	18.142695
43.622049	1492.200491	18.147712
43.487899	1489.828506	18.152730
43.277639	1488.234774	18.157747
43.613575	1483.027759	18.162765
43.397989	1491.966976	18.167783
43.194480	1488.765216	18.172800
43.646384	1488.898568	18.177818
43.232864	1489.831452	18.182835
43.540683	1490.277241	18.187853
43.349636	1513.763225	18.192871
43.686152	1521.225327	18.197888
43.951293	1518.597730	18.202906
43.884953	1519.402878	18.207923
44.175306	1515.523766	18.212941
44.002169	1514.335485	18.217959
44.024637	1514.831506	18.222976
44.303906	1510.503461	18.227994
43.971443	1521.636192	18.233011
44.418544	1516.733140	18.238029
44.443000	1510.521796	18.243047
44.281906	1519.414584	18.248064
43.942703	1517.357677	18.253082
43.915314	1523.192210	18.258099
44.195455	1520.005331	18.263117
44.192732	1519.257876	18.268135
44.191011	1516.991402	18.273152
44.181938	1516.011350	18.278170
44.096494	1524.823644	18.283187
44.301460	1530.850798	18.288205
44.843405	1542.359282	18.293223
44.475698	1547.772231	18.298240
45.023077	1549.815873	18.303258
44.846707	1547.368023	18.308275
45.039690	1546.920498	18.313293
44.709275	1550.019710	18.318311
45.253382	1549.634167	18.323328
45.201566	1538.286103	18.328346
44.745115	1531.592204	18.333363
44.693338	1528.806712	18.338381
44.948688	1545.941602	18.343399
45.233406	1548.139617	18.348416
45.121371	1538.122592	18.353434
45.025310	1547.010530	18.358451
45.121125	1549.685445	18.363469
45.130749	1548.704769	18.368487
45.042108	1551.276174	18.373504
45.016913	1546.394955	18.378522
44.889722	1556.879090	18.383539
45.313278	1544.548289	18.388557
44.801662	1550.002283	18.393575
45.239849	1564.767994	18.398592
45.476675	1566.864317	18.403610
45.710110	1567.941002	18.408627
46.002538	1564.617651	18.413645
45.875886	1566.893866	18.418663
45.871154	1567.957410	18.423680
46.268481	1562.116826	18.428698
45.848397	1552.045884	18.433715
45.787867	1532.961747	18.438733
45.669255	1534.140986	18.443751
45.735748	1535.673761	18.448768
45.716040	1536.027062	18.453786
45.966889	1564.911651	18.458803
46.153265	1553.538170	18.463821
46.106807	1564.863648	18.468839
45.937169	1564.529018	18.473856
46.324929	1563.329929	18.478874
45.946529	1562.767455	18.483891
46.155631	1564.995624	18.488909
46.088288	1558.699007	18.493927
46.276217	1564.678552	18.498944
46.338178	1557.067407	18.503962
46.100979	1567.955301	18.508979
46.257390	1574.888480	18.513997
46.168775	1565.102886	18.519015
46.155644	1564.112465	18.524032
46.701768	1569.301014	18.529050
46.607699	1587.484333	18.534067
47.235230	1578.949207	18.539085
47.636157	1562.734774	18.544103
47.238923	1546.362924	18.549120
47.656877	1542.530312	18.554138
47.470133	1543.478156	18.559155
47.159425	1526.562381	18.564173
46.874117	1515.504064	18.569191
47.037386	1512.046371	18.574208
46.955110	1504.972672	18.579226
46.929523	1513.001431	18.584243
47.242179	1523.374489	18.589261
47.251015	1534.672247	18.594279
47.180753	1540.186413	18.599296
47.167972	1544.824616	18.604314
47.002570	1545.459148	18.609331
47.130780	1539.697678	18.614349
47.231127	1545.360826	18.619367
47.284930	1542.719738	18.624384
47.638628	1540.175547	18.629402
47.492816	1545.615243	18.634419
47.453774	1540.774776	18.639437
47.570092	1539.483693	18.644455
47.698764	1542.876222	18.649472
47.334745	1542.689007	18.654490
47.321199	1544.791438	18.659507
47.449365	1545.254871	18.664525
47.755790	1562.606593	18.669543
47.628497	1564.619409	18.674560
47.704381	1569.167181	18.679578
47.822541	1573.707425	18.684595
48.078826	1569.729119	18.689613
47.924244	1567.516907	18.694631
47.684228	1569.121382	18.699648
47.848995	1559.700461	18.704666
47.682534	1570.561344	18.709683
48.233618	1585.486049	18.714701
48.293079	1586.590483	18.719719
47.998933	1601.234705	18.724736
48.458717	1596.842448	18.729754
48.509150	1599.308303	18.734771
48.329009	1593.944443	18.739789
48.563931	1596.470542	18.744807
48.437494	1592.257522	18.749824
48.883887	1588.449465	18.754842
48.673049	1590.183006	18.759859
48.626204	1589.775304	18.764877
49.005507	1590.317455	18.769895
48.595317	1592.338426	18.774912
48.841933	1585.768337	18.779930
48.602865	1589.629332	18.784947
48.262292	1598.252683	18.789965
48.823503	1586.753321	18.794983
48.367506	1592.901652	18.800000
48.433587	1596.291592	18.805018
48.649363	1621.669065	18.810035
48.924244	1615.382339	18.815053
49.237477	1615.033618	18.820071
49.005428	1625.500705	18.825088
49.126408	1620.843130	18.830106
49.313290	1619.795635	18.835123
49.330820	1620.384476	18.840141
49.310627	1621.472514	18.845159
49.176251	1618.202279	18.850176
49.542436	1613.990126	18.855194
49.245250	1641.857930	18.860211
49.540032	1648.528383	18.865229
49.992266	1644.498354	18.870247
49.607102	1652.937712	18.875264
50.149238	1655.567418	18.880282
50.238845	1657.799716	18.885299
49.812776	1630.911949	18.890317
49.916258	1623.206837	18.895335
49.708558	1623.878009	18.900352
49.898664	1629.031334	18.905370
49.937005	1647.356430	18.910387
50.189208	1650.800074	18.915405
50.212468	1648.865461	18.920423
49.890720	1653.594665	18.925440
49.970823	1651.752455	18.930458
50.089574	1649.240999	18.935475
50.148709	1653.303793	18.940493
50.314799	1654.200089	18.945511
50.084757	1654.233768	18.950528
50.267199	1641.439508	18.955546
49.931695	1648.535342	18.960563
50.138729	1671.149491	18.965581
50.713365	1665.186985	18.970599
50.387704	1683.232742	18.975616
50.521183	1678.114583	18.980634
50.544963	1675.392523	18.985651
50.471227	1681.240804	18.990669
50.758153	1677.647723	18.995687
50.756800	1677.287036	19.000704
50.853609	1667.377410	19.005722
50.593449	1679.787925	19.010739
50.603160	1676.211528	19.015757
51.110077	1687.868873	19.020775
50.990470	1710.255945	19.025792
51.292425	1703.600679	19.030810
51.393744	1713.954879	19.035827
51.758389	1702.230354	19.040845
51.510100	1692.956244	19.045863
51.213471	1675.633750	19.050880
51.259710	1670.907063	19.055898
51.302362	1676.541709	19.060915
51.289166	1692.893701	19.065933
51.663173	1696.544462	19.070951
51.807485	1704.575332	19.075968
51.617252	1698.483887	19.080986
51.754335	1700.223302	19.086003
51.783221	1697.154330	19.091021
51.710099	1695.913112	19.096039
51.436876	1693.626987	19.101056
51.855958	1685.641040	19.106074
51.798055	1695.827911	19.111091
51.729028	1700.699308	19.116109
52.052326	1693.733091	19.121127
51.896098	1697.702821	19.126144
52.040598	1700.522595	19.131162
52.168652	1701.162244	19.136179
51.947722	1693.543446	19.141197
52.135296	1705.001607	19.146215
51.977572	1697.689716	19.151232
52.359372	1711.706312	19.156250
52.315991	1719.597226	19.161267
52.606586	1724.000681	19.166285
52.928600	1721.446568	19.171303
52.882779	1725.644109	19.176320
52.748383	1708.850237	19.181338
52.541876	1707.707377	19.186355
52.777208	1717.012936	19.191373
52.709807	1716.956176	19.196391
52.667406	1720.899892	19.201408
52.718583	1717.313725	19.206426
52.870472	1720.024564	19.211443
52.682474	1729.018519	19.216461
53.005747	1719.630421	19.221479
53.063952	1717.713037	19.226496
52.735315	1716.857878	19.231514
52.785340	1718.713435	19.236531
52.942086	1717.759623	19.241549
52.979379	1720.429745	19.246567
52.632963	1744.049428	19.251584
52.942216	1746.048490	19.256602
53.575573	1741.047226	19.261619
53.156802	1762.208622	19.266637
53.622954	1755.582992	19.271655
53.550441	1760.808139	19.276672
53.397466	1763.541652	19.281690
53.648115	1754.570204	19.286707
53.499406	1759.461408	19.291725
53.835072	1753.469335	19.296743
53.712709	1755.394080	19.301760
53.832964	1748.146377	19.306778
54.153498	1747.838964	19.311795
54.148581	1754.110490	19.316813
54.216416	1736.370327	19.321831
54.299032	1745.505191	19.326848
53.752700	1745.617632	19.331866
54.274435	1747.158053	19.336883
54.213087	1741.624168	19.341901
54.553258	1736.199293	19.346919
54.260006	1748.238372	19.351936
54.397274	1734.921082	19.356954
54.440372	1733.723464	19.361971
54.143880	1744.512399	19.366989
54.611563	1744.194889	19.372007
54.480517	1751.885853	19.377024
54.535109	1755.443630	19.382042
54.487807	1756.957609	19.387059
54.646891	1757.391734	19.392077
54.761152	1748.140782	19.397095
54.711235	1758.542732	19.402112
54.533168	1759.877776	19.407130
54.896497	1760.014248	19.412147
54.607451	1763.215454	19.417165
54.906961	1754.118226	19.422183
54.845922	1764.127878	19.427200
55.144566	1766.197067	19.432218
55.012937	1767.379188	19.437235
55.397371	1786.040190	19.442253
55.370830	1779.500208	19.447271
55.146731	1786.530359	19.452288
55.310711	1790.632317	19.457306
56.006929	1784.015602	19.462323
55.400588	1793.745699	19.467341
55.694895	1788.840184	19.472359
55.479857	1787.065480	19.477376
55.797619	1788.499999	19.482394
55.871008	1784.518557	19.487411
55.830473	1790.559805	19.492429
55.853235	1773.367953	19.497447
55.811111	1781.817173	19.502464
55.258985	1794.393910	19.507482
55.836669	1777.686180	19.512499
55.717132	1785.180254	19.517517
55.768726	1785.891095	19.522535
55.907696	1786.009863	19.527552
55.973058	1796.653813	19.532570
56.036598	1808.827176	19.537587
56.494751	1810.642036	19.542605
56.453255	1809.515325	19.547623
56.548544	1817.926917	19.552640
56.584389	1810.474762	19.557658
56.509893	1811.311116	19.562675
56.510567	1811.573862	19.567693
56.448514	1816.961757	19.572711
56.711318	1811.752132	19.577728
57.006444	1810.535550	19.582746
56.999155	1806.850925	19.587763
57.007190	1816.900724	19.592781
57.071108	1802.635440	19.597799
56.971879	1810.151459	19.602816
56.695517	1810.140611	19.607834
56.910159	1804.000278	19.612851
56.632067	1812.768746	19.617869
56.968045	1810.011026	19.622887
57.206758	1804.352175	19.627904
56.869832	1797.565148	19.632922
57.191805	1806.174194	19.637939
57.066987	1808.118216	19.642957
57.202357	1806.303354	19.647975
57.391551	1820.245373	19.652992
57.201453	1834.876379	19.658010
57.411665	1824.363342	19.663027
57.316452	1835.648824	19.668045
57.320389	1835.894532	19.673063
57.508788	1831.333113	19.678080
57.424551	1835.842793	19.683098
57.842606	1833.135693	19.688115
57.807359	1842.250086	19.693133
57.955943	1845.049572	19.698151
58.200611	1848.846855	19.703168
58.140459	1848.889621	19.708186
58.383104	1849.593592	19.713203
58.343252	1855.829830	19.718221
58.511159	1844.134210	19.723239
58.331097	1825.080553	19.728256
58.230407	1834.810261	19.733274
58.596161	1837.446110	19.738291
58.420066	1845.638283	19.743309
58.779295	1840.916683	19.748327
58.559335	1847.825069	19.753344
58.493104	1845.991228	19.758362
58.812450	1840.108698	19.763379
58.755792	1842.247939	19.768397
58.757284	1840.038322	19.773415
59.149877	1846.355037	19.778432
58.668701	1843.793713	19.783450
58.890522	1839.097962	19.788467
58.600207	1847.904583	19.793485
58.672099	1847.424448	19.798503
59.012877	1847.256177	19.803520
58.645725	1850.537505	19.808538
58.713129	1851.930156	19.813555
59.063261	1873.309671	19.818573
59.080455	1873.178064	19.823591
59.231257	1877.547227	19.828608
59.181294	1879.395155	19.833626
59.308677	1871.207857	19.838643
59.001992	1877.717131	19.843661
59.223214	1887.478911	19.848679
59.502874	1888.764560	19.853696
59.485274	1906.861356	19.858714
59.935929	1901.578477	19.863731
60.170115	1901.553848	19.868749
60.123218	1893.829315	19.873767
59.852492	1896.355096	19.878784
59.764171	1902.122413	19.883802
60.258054	1900.323513	19.888819
60.261122	1898.190722	19.893837
60.151864	1895.031259	19.898855
60.478694	1892.597485	19.903872
60.168245	1896.184413	19.908890
60.560975	1892.443833	19.913907
60.430419	1895.688222	19.918925
60.217842	1891.405475	19.923943
60.274589	1899.093309	19.928960
60.042473	1899.780185	19.933978
60.622087	1898.655089	19.938995
60.520448	1908.587150	19.944013
60.464111	1915.164276	19.949031
60.970311	1923.037654	19.954048
60.696069	1934.583810	19.959066
61.075229	1925.540633	19.964083
61.179535	1920.294108	19.969101
61.087738	1923.936628	19.974119
61.366503	1925.352997	19.979136
61.189670	1924.803980	19.984154
61.469993	1917.699779	19.989171
61.106242	1923.208983	19.994189
61.296972	1931.136613	19.999207
61.283548	1917.039297	20.004224
61.275792	1920.220844	20.009242
61.358706	1919.055404	20.014259
61.208318	1921.550983	20.019277
61.372651	1918.971645	20.024295
61.710312	1921.073178	20.029312
61.373192	1924.416591	20.034330
61.916751	1940.974249	20.039347
61.975362	1950.765939	20.044365
62.027253	1951.029958	20.049383
62.253009	1940.380638	20.054400
61.875217	1936.366497	20.059418
62.317999	1935.632132	20.064435
62.551789	1933.752003	20.069453
62.337460	1940.740553	20.074471
62.375314	1933.942456	20.079488
62.290995	1947.194333	20.084506
62.428163	1935.272285	20.089523
62.130324	1943.148056	20.094541
62.038545	1943.066865	20.099559
62.238073	1933.972100	20.104576
62.278551	1941.673564	20.109594
62.583939	1923.696279	20.114611
62.295312	1933.628290	20.119629
62.555197	1939.018372	20.124647
62.859618	1958.228025	20.129664
62.690130	1967.488187	20.134682
62.941005	1959.431383	20.139699
63.030097	1964.921080	20.144717
62.898606	1960.955748	20.149735
63.355099	1959.161232	20.154752
62.933358	1969.994691	20.159770
63.165236	1963.621859	20.164787
63.093166	1959.545579	20.169805
63.401997	1954.831195	20.174823
63.260945	1961.655470	20.179840
63.136450	1965.565149	20.184858
63.782889	1976.536594	20.189875
63.692571	1985.326345	20.194893
63.745864	1994.553354	20.199911
64.040841	1983.732498	20.204928
63.932849	1990.968407	20.209946
63.772960	1988.146581	20.214963
63.947866	1983.102727	20.219981
63.809299	1987.392221	20.224999
64.038225	1979.334973	20.230016
63.847105	1986.878323	20.235034
64.327163	1982.644759	20.240051
64.260029	1984.637025	20.245069
64.367706	1987.837146	20.250087
64.604334	1976.735350	20.255104
64.215435	1982.147115	20.260122
63.972630	1983.006390	20.265139
64.448064	1978.388135	20.270157
64.571198	1991.427622	20.275175
64.627321	2011.148901	20.280192
64.383174	2017.736361	20.285210
64.861243	2012.821916	20.290227
65.117776	2008.517018	20.295245
64.690834	2011.209319	20.300263
65.088427	2008.743788	20.305280
65.192866	2010.691389	20.310298
65.207104	2001.490053	20.315315
65.125441	2005.787782	20.320333
65.268852	2007.814118	20.325351
65.409152	2007.164176	20.330368
65.300422	2016.748982	20.335386
65.561559	2010.395847	20.340403
65.406555	2012.487869	20.345421
65.215727	2018.354960	20.350439
65.570543	2006.796158	20.355456
65.295110	2013.973045	20.360474
65.607954	2022.895167	20.365491
65.588937	2030.819334	20.370509
65.839537	2039.199991	20.375527
65.657391	2034.375103	20.380544
65.579872	2048.407075	20.385562
65.559685	2031.003883	20.390579
65.587824	2033.998813	20.395597
65.856809	2058.870650	20.400615
66.583764	2057.501798	20.405632
66.774640	2066.452053	20.410650
66.774762	2060.160190	20.415667
66.684652	2034.139983	20.420685
66.620521	2032.814710	20.425703
66.496833	2020.714736	20.430720
66.317874	2019.682299	20.435738
66.552651	2026.171356	20.440755
66.727902	2027.999902	20.445773
66.651396	2054.046155	20.450791
67.141309	2053.372703	20.455808
67.161120	2050.508832	20.460826
66.819796	2055.274322	20.465843
67.245378	2049.828632	20.470861
67.051859	2046.219270	20.475879
67.230252	2037.129386	20.480896
67.425075	2052.418166	20.485914
67.312658	2054.036951	20.490931
67.492703	2041.212834	20.495949
67.377319	2052.254711	20.500967
67.561516	2055.312068	20.505984
67.738254	2056.122526	20.511002
67.458569	2052.489935	20.516019
67.493583	2059.850164	20.521037
67.351997	2057.623218	20.526055
67.397093	2057.098581	20.531072
67.440799	2066.072307	20.536090
67.295390	2079.492938	20.541107
67.473219	2077.417201	20.546125
67.687733	2083.813551	20.551143
67.694128	2088.959370	20.556160
68.486435	2100.685591	20.561178
68.240694	2108.443803	20.566195
68.530652	2111.400926	20.571213
68.855647	2104.387050	20.576231
69.183621	2102.716059	20.581248
68.883235	2084.865868	20.586266
68.787375	2071.250361	20.591283
69.047718	2064.879238	20.596301
68.757979	2070.316124	20.601319
68.788936	2070.274352	20.606336
68.637729	2070.303322	20.611354
68.793916	2070.225059	20.616371
68.934358	2081.683169	20.621389
68.860935	2105.521046	20.626407
69.216732	2097.417542	20.631424
69.039270	2102.734275	20.636442
68.959630	2105.194218	20.641459
69.233542	2104.133597	20.646477
69.071809	2111.486687	20.651495
69.531281	2100.283969	20.656512
69.405607	2101.043549	20.661530
68.996341	2101.570689	20.666547
69.602581	2111.900494	20.671565
69.361829	2121.952424	20.676583
69.315278	2121.088432	20.681600
69.851419	2116.907242	20.686618
69.385440	2120.827374	20.691635
70.073623	2114.175614	20.696653
69.690856	2117.664791	20.701671
69.787181	2126.984919	20.706688
70.094119	2141.175911	20.711706
70.320732	2142.797271	20.716723
70.567577	2148.258732	20.721741
70.469701	2148.783407	20.726759
70.420400	2138.534928	20.731776
70.528655	2142.099187	20.736794
70.237723	2145.643732	20.741811
70.626289	2140.866230	20.746829
70.584712	2146.015000	20.751847
70.512178	2145.099302	20.756864
70.846182	2141.688173	20.761882
70.913743	2136.693637	20.766899
70.854941	2126.058102	20.771917
70.939188	2146.287941	20.776935
71.319617	2151.379635	20.781952
71.551772	2161.854089	20.786970
71.292533	2156.795250	20.791987
71.876838	2148.636396	20.797005
71.852141	2147.919944	20.802023
71.709957	2133.040622	20.807040
71.472643	2121.863275	20.812058
71.504834	2127.343231	20.817075
71.643917	2121.156609	20.822093
71.439343	2137.981690	20.827111
71.681444	2144.474353	20.832128
72.200545	2147.647437	20.837146
71.758080	2149.188294	20.842163
72.243920	2146.089614	20.847181
72.187770	2157.304614	20.852199
72.268300	2151.139116	20.857216
72.219674	2148.489871	20.862234
72.235344	2149.437720	20.867251
72.348307	2143.407854	20.872269
72.542349	2146.340952	20.877287
72.420173	2143.029321	20.882304
72.624637	2141.260035	20.887322
72.183939	2145.048712	20.892339
72.589306	2151.781210	20.897357
72.706715	2164.883121	20.902375
72.950474	2171.331482	20.907392
72.866176	2179.613818	20.912410
73.077498	2184.701030	20.917427
72.823106	2172.294549	20.922445
72.695180	2181.390111	20.927463
72.889078	2175.920757	20.932480
73.393808	2170.077753	20.937498
72.921570	2173.606383	20.942515
73.226014	2169.411787	20.947533
73.290963	2179.464559	20.952551
73.238004	2195.698387	20.957568
73.750203	2200.714808	20.962586
73.624741	2201.148705	20.967603
74.047923	2195.677388	20.972621
73.808450	2195.156440	20.977639
73.921158	2194.440884	20.982656
74.309180	2195.431610	20.987674
73.893458	2194.630423	20.992691
74.089882	2196.423364	20.997709
73.957578	2180.121027	21.002727
73.670992	2188.157173	21.007744
73.817907	2199.671765	21.012762
73.915829	2212.735924	21.017779
74.361092	2214.462436	21.022797
74.723080	2219.175593	21.027815
74.981513	2215.713572	21.032832
75.074686	2223.656134	21.037850
74.678185	2223.295525	21.042867
74.554087	2224.124081	21.047885
74.977774	2210.500313	21.052903
74.598972	2220.280924	21.057920
74.745252	2213.048505	21.062938
74.716278	2222.507454	21.067955
75.053543	2235.114201	21.072973
75.001402	2248.876445	21.077991
75.146963	2247.661658	21.083008
75.509483	2235.556332	21.088026
75.312428	2249.604414	21.093043
75.401035	2238.596034	21.098061
75.744827	2237.619439	21.103079
75.741351	2231.851955	21.108096
75.861587	2227.124299	21.113114
75.792861	2229.057070	21.118131
76.030097	2224.454705	21.123149
76.056144	2223.229876	21.128167
76.034591	2233.763723	21.133184
76.478528	2244.901394	21.138202
76.409543	2244.763863	21.143219
76.407955	2237.366230	21.148237
76.674085	2243.190423	21.153255
76.372935	2231.399394	21.158272
76.388766	2233.335985	21.163290
76.564509	2246.756681	21.168307
76.879616	2242.434508	21.173325
76.789793	2245.534821	21.178343
76.834008	2256.205291	21.183360
77.249324	2242.955680	21.188378
77.220812	2252.946320	21.193395
77.344543	2242.925032	21.198413
77.121490	2229.835450	21.203431
76.897785	2222.662819	21.208448
77.272837	2237.158472	21.213466
76.964041	2244.340791	21.218483
77.351994	2247.911598	21.223501
77.205361	2243.459334	21.228519
77.214885	2254.951832	21.233536
77.718056	2247.800134	21.238554
77.597447	2245.803434	21.243571
77.368734	2247.448654	21.248589
77.520994	2253.335061	21.253607
77.520146	2275.615174	21.258624
77.922317	2277.357220	21.263642
77.670859	2282.666154	21.268659
77.745791	2281.291148	21.273677
77.914225	2281.151936	21.278695
78.010236	2278.636921	21.283712
78.430062	2293.054695	21.288730
77.898645	2311.073469	21.293747
78.533798	2313.383265	21.298765
78.738579	2316.074769	21.303783
78.696529	2319.474256	21.308800
78.905751	2314.206140	21.313818
78.394465	2320.199185	21.318835
78.453912	2311.488368	21.323853
78.873715	2314.855887	21.328871
78.400464	2324.817605	21.333888
78.775848	2327.729685	21.338906
79.336465	2334.565727	21.343923
79.248637	2343.263262	21.348941
79.328350	2343.270350	21.353959
79.287552	2334.916109	21.358976
79.806646	2324.592582	21.363994
79.728401	2336.017334	21.369011
79.718765	2324.799587	21.374029
79.945870	2329.395849	21.379047
79.713763	2332.481901	21.384064
80.035843	2322.533545	21.389082
79.796532	2330.375016	21.394099
80.035974	2331.063005	21.399117
80.126415	2334.526320	21.404135
79.892381	2330.676352	21.409152
79.909959	2338.590130	21.414170
80.144269	2355.678203	21.419187
80.129606	2358.235591	21.424205
80.256296	2357.287320	21.429223
80.332309	2362.900392	21.434240
80.519283	2359.313650	21.439258
80.481069	2372.914894	21.444275
80.823862	2384.560437	21.449293
80.885230	2385.260310	21.454311
80.535631	2388.959004	21.459328
80.717136	2382.572000	21.464346
80.981609	2389.687349	21.469363
80.949657	2390.105552	21.474381
81.168389	2388.912908	21.479399
81.058739	2391.249467	21.484416
81.456152	2402.681793	21.489434
81.173463	2419.572359	21.494451
81.330347	2422.155889	21.499469
81.382580	2413.288839	21.504487
81.447961	2416.531985	21.509504
81.403781	2420.693278	21.514522
81.630298	2426.186405	21.519539
82.129847	2429.475159	21.524557
82.630066	2429.286179	21.529575
82.561330	2422.606328	21.534592
82.646239	2409.813580	21.539610
82.449259	2406.485500	21.544627
82.577784	2391.672080	21.549645
82.622899	2394.823273	21.554663
82.540249	2394.440136	21.559680
82.441249	2389.263625	21.564698
82.486765	2399.198509	21.569715
82.478561	2399.361209	21.574733
82.609133	2414.710174	21.579751
82.797562	2433.562167	21.584768
82.898778	2433.023847	21.589786
83.174561	2429.169635	21.594803
83.151938	2430.235309	21.599821
82.929552	2433.367816	21.604839
82.968435	2432.409158	21.609856
83.358711	2428.792337	21.614874
83.252785	2453.819034	21.619891
83.521877	2450.249066	21.624909
83.880460	2457.693978	21.629927
83.612153	2467.570403	21.634944
83.772534	2456.234980	21.639962
83.824536	2456.344028	21.644979
83.762736	2457.633845	21.649997
83.578446	2452.322243	21.655015
83.870836	2461.501190	21.660032
83.862018	2462.592983	21.665050
84.503961	2469.441292	21.670067
84.446871	2477.145226	21.675085
84.345130	2481.046693	21.680103
84.330459	2476.223267	21.685120
84.589105	2472.467744	21.690138
84.691543	2477.470951	21.695155
84.471622	2475.633221	21.700173
84.798447	2474.527953	21.705191
84.643379	2495.163006	21.710208
85.278491	2491.422955	21.715226
85.383441	2502.477229	21.720243
85.355228	2499.690938	21.725261
85.390881	2492.539741	21.730279
85.256003	2498.600260	21.735296
85.151094	2504.836138	21.740314
85.323290	2502.706177	21.745331
85.338679	2500.385691	21.750349
85.326466	2495.534335	21.755367
85.268359	2498.618631	21.760384
85.704973	2512.275644	21.765402
85.497995	2530.248451	21.770419
85.653324	2526.571534	21.775437
85.716898	2528.860036	21.780455
85.827595	2529.974465	21.785472
85.907373	2532.352418	21.790490
86.355113	2543.938874	21.795507
86.683972	2549.613955	21.800525
86.561070	2557.239539	21.805543
86.553499	2560.138012	21.810560
86.587107	2552.389278	21.815578
86.803042	2556.680611	21.820595
86.776180	2559.240766	21.825613
87.255069	2553.203506	21.830631
86.880132	2550.915369	21.835648
86.858969	2555.928875	21.840666
87.119525	2550.517975	21.845683
86.676508	2552.820408	21.850701
87.203754	2553.596237	21.855719
87.116746	2575.829977	21.860736
87.233348	2575.391460	21.865754
87.543522	2572.420611	21.870771
87.501566	2581.833092	21.875789
87.955649	2577.656996	21.880807
87.742260	2570.841248	21.885824
87.852484	2573.906580	21.890842
88.216521	2573.106874	21.895859
87.868733	2569.104286	21.900877
88.370411	2585.217842	21.905895
88.294773	2590.222741	21.910912
89.014072	2585.851742	21.915930
88.955560	2578.459081	21.920947
88.089564	2574.812879	21.925965
88.828095	2579.495210	21.930983
88.896958	2584.860935	21.936000
88.898827	2590.705388	21.941018
88.767887	2592.025121	21.946035
88.813758	2596.497766	21.951053
89.186053	2594.276098	21.956071
88.815776	2605.864053	21.961088
88.889633	2598.735030	21.966106
89.115734	2595.020852	21.971123
88.760017	2601.797062	21.976141
89.034823	2605.602326	21.981159
89.092786	2621.322576	21.986176
89.206315	2629.239301	21.991194
89.696756	2632.818247	21.996211
89.739150	2649.952218	22.001229
90.057632	2654.115526	22.006247
90.422855	2657.686129	22.011264
90.748559	2643.515936	22.016282
90.557360	2626.483062	22.021299
90.280418	2614.924635	22.026317
90.612143	2611.345427	22.031335
90.520178	2610.284125	22.036352
90.310508	2606.451436	22.041370
90.571423	2601.738983	22.046387
90.547399	2606.157488	22.051405
90.961064	2617.649537	22.056423
90.605608	2633.880175	22.061440
90.696909	2634.819141	22.066458
91.121935	2632.794367	22.071475
90.883337	2641.990460	22.076493
91.046982	2640.506878	22.081511
90.911204	2647.922173	22.086528
90.987767	2640.389945	22.091546
91.072620	2648.636131	22.096563
91.364873	2659.279139	22.101581
91.395555	2664.588838	22.106599
91.354708	2663.695585	22.111616
91.810686	2661.595863	22.116634
91.872427	2656.809748	22.121651
92.103172	2674.404566	22.126669
92.161963	2677.783335	22.131687
92.375612	2684.320109	22.136704
92.453727	2687.991571	22.141722
92.383699	2686.955871	22.146739
92.226366	2683.905377	22.151757
92.913908	2672.241076	22.156775
92.779936	2685.540870	22.161792
92.762182	2680.458280	22.166810
92.959640	2680.725844	22.171827
92.799198	2692.242646	22.176845
92.762978	2676.945475	22.181863
92.953487	2681.581510	22.186880
93.001183	2677.131160	22.191898
92.971042	2676.031675	22.196915
93.146678	2689.650240	22.201933
93.404817	2690.383252	22.206951
93.424601	2708.511264	22.211968
93.556938	2706.418310	22.216986
94.088839	2702.646685	22.222003
93.797788	2702.597266	22.227021
93.567484	2699.219369	22.232039
93.657402	2698.561701	22.237056
93.901106	2711.311218	22.242074
94.467847	2721.285913	22.247091
93.966389	2735.710243	22.252109
94.535725	2722.040750	22.257127
94.451230	2725.674437	22.262144
94.902884	2732.605925	22.267162
95.032043	2719.311845	22.272179
94.944884	2728.214026	22.277197
94.819023	2731.685972	22.282215
94.857598	2729.967459	22.287232
94.736303	2727.753691	22.292250
95.226333	2715.969034	22.297267
94.848925	2719.855529	22.302285
95.388344	2720.717531	22.307303
95.201124	2722.286173	22.312320
94.977666	2723.315459	22.317338
95.592641	2727.982147	22.322355
95.346287	2750.148742	22.327373
95.451683	2749.451632	22.332391
95.237120	2748.092071	22.337408
95.271705	2741.331093	22.342426
95.981123	2744.595106	22.347443
95.884711	2773.676709	22.352461
96.131944	2777.388087	22.357479
96.423534	2771.803032	22.362496
95.860369	2774.982876	22.367514
96.422457	2778.468624	22.372531
96.174161	2777.701269	22.377549
96.262778	2785.176817	22.382567
96.542490	2792.660439	22.387584
96.345077	2807.207051	22.392602
96.781184	2795.811662	22.397619
96.686013	2805.762179	22.402637
96.740427	2803.456661	22.407655
96.910637	2820.376149	22.412672
97.110094	2833.641783	22.417690
97.500016	2831.854641	22.422707
97.366916	2831.505496	22.427725
97.519288	2838.488696	22.432743
97.845242	2827.663068	22.437760
98.252043	2832.340177	22.442778
98.416645	2819.563468	22.447795
97.800906	2829.692201	22.452813
98.348186	2816.197626	22.457831
98.269712	2810.705397	22.462848
98.152455	2818.386067	22.467866
98.434925	2814.304139	22.472883
98.494496	2820.203199	22.477901
98.571978	2826.071086	22.482919
98.569653	2832.109816	22.487936
98.436191	2838.468384	22.492954
98.857345	2830.026031	22.497971
98.755867	2839.673934	22.502989
98.328222	2835.876732	22.508007
98.949217	2843.766138	22.513024
98.688551	2859.270787	22.518042
99.087896	2865.391790	22.523059
99.241701	2865.279293	22.528077
99.486814	2867.284814	22.533095
99.496172	2863.014368	22.538112
99.488363	2884.756098	22.543130
99.656931	2884.454813	22.548147
99.532399	2895.763880	22.553165
99.742494	2891.684820	22.558183
100.401861	2899.355744	22.563200
99.748940	2902.967634	22.568218
100.274292	2898.066602	22.573235
100.115319	2901.184373	22.578253
100.395257	2918.194246	22.583271
100.466843	2925.604144	22.588288
100.589886	2922.817251	22.593306
100.453509	2926.197309	22.598323
100.352336	2939.076755	22.603341
100.628026	2924.329007	22.608359
100.834749	2927.825838	22.613376
100.604544	2951.387237	22.618394
101.211299	2942.670575	22.623411
101.481362	2943.844579	22.628429
101.401067	2941.107416	22.633447
101.675322	2950.715926	22.638464
101.843858	2949.233894	22.643482
101.909848	2951.570062	22.648499
102.100554	2950.998575	22.653517
102.073304	2941.820570	22.658535
102.144543	2936.204515	22.663552
102.002972	2944.986495	22.668570
102.041624	2943.153881	22.673587
102.358502	2951.023406	22.678605
102.234164	2966.963467	22.683623
102.413800	2968.380808	22.688640
102.091976	2979.198283	22.693658
102.224420	2980.652257	22.698675
102.374912	2980.635472	22.703693
102.868785	2998.801517	22.708711
103.020614	2994.295918	22.713728
102.971249	3003.839648	22.718746
103.146074	2997.759449	22.723763
103.263904	3005.339795	22.728781
103.122452	3006.547963	22.733799
103.300767	3025.985240	22.738816
103.331130	3034.247413	22.743834
103.532217	3033.970046	22.748851
103.489009	3030.485929	22.753869
103.583759	3038.535668	22.758887
104.189387	3038.941104	22.763904
103.877369	3063.234725	22.768922
104.080384	3058.803542	22.773939
104.375408	3057.899182	22.778957
104.608108	3061.475288	22.783975
104.962817	3058.858314	22.788992
104.548625	3062.988331	22.794010
104.924449	3048.092333	22.799027
104.786651	3054.852090	22.804045
104.784537	3063.034500	22.809063
105.121150	3047.174818	22.814080
105.136480	3064.660502	22.819098
105.200899	3080.469894	22.824115
105.044062	3084.038114	22.829133
104.941158	3088.446530	22.834151
105.500756	3088.367652	22.839168
105.350683	3079.222521	22.844186
105.840336	3081.620946	22.849203
106.004847	3097.335729	22.854221
105.935571	3109.937270	22.859239
106.137544	3107.088983	22.864256
106.372325	3109.981956	22.869274
106.477314	3107.448849	22.874291
106.453421	3111.665315	22.879309
106.507255	3111.476722	22.884327
106.767215	3107.025431	22.889344
106.484420	3111.677297	22.894362
106.714409	3102.116763	22.899379
106.548940	3103.974610	22.904397
106.500972	3107.700897	22.909415
107.068940	3113.434829	22.914432
106.888393	3133.207951	22.919450
106.925014	3133.223486	22.924467
106.859081	3137.061990	22.929485
106.930427	3136.216108	22.934503
107.337850	3151.082746	22.939520
107.315391	3156.821959	22.944538
107.790121	3160.893632	22.949555
108.001065	3156.780537	22.954573
107.812197	3165.747975	22.959591
107.942369	3157.098536	22.964608
108.220452	3179.409488	22.969626
108.338163	3187.177172	22.974643
108.534681	3175.349279	22.979661
108.529067	3180.210267	22.984679
108.801023	3181.000889	22.989696
108.851950	3181.520748	22.994714
109.473983	3165.731848	22.999731
109.864149	3156.236201	23.004749
109.560979	3158.479448	23.009767
110.077607	3149.602402	23.014784
109.711317	3153.831789	23.019802
109.678411	3134.735645	23.024819
109.947908	3126.934045	23.029837
109.740940	3120.194105	23.034855
109.717528	3118.752107	23.039872
109.980054	3146.157492	23.044890
110.150613	3150.252495	23.049907
110.273475	3146.519244	23.054925
110.219245	3154.805202	23.059943
110.559883	3143.954976	23.064960
110.350279	3158.458253	23.069978
110.082071	3154.551367	23.074995
110.543868	3154.821628	23.080013
110.304070	3146.068357	23.085031
110.629223	3166.074754	23.090048
110.600639	3178.629746	23.095066
110.316348	3184.303739	23.100083
110.371711	3195.354645	23.105101
110.697666	3207.984495	23.110119
111.062475	3208.572300	23.115136
111.161001	3221.998342	23.120154
110.973901	3222.119566	23.125171
111.425155	3229.742043	23.130189
111.414910	3241.619211	23.135207
111.468697	3236.575366	23.140224
111.447302	3246.863693	23.145242
111.698528	3260.589522	23.150259
112.292416	3266.515261	23.155277
112.135263	3275.479281	23.160295
112.375599	3269.971439	23.165312
112.557208	3273.348067	23.170330
112.320973	3270.280138	23.175347
112.303628	3274.431887	23.180365
112.334576	3286.741479	23.185383
112.653746	3291.175474	23.190400
112.803278	3298.792610	23.195418
112.818252	3300.802639	23.200435
113.192414	3309.407407	23.205453
113.079502	3319.112515	23.210471
113.641070	3311.172988	23.215488
113.919734	3310.441929	23.220506
113.747062	3310.876304	23.225523
114.085392	3304.769905	23.230541
113.843631	3311.303280	23.235559
114.158317	3301.589084	23.240576
113.862723	3313.287616	23.245594
114.350182	3323.985728	23.250611
114.672900	3331.676743	23.255629
114.267101	3340.297348	23.260647
114.344044	3340.834305	23.265664
114.722800	3332.627348	23.270682
114.568561	3333.474930	23.275699
114.841023	3333.518149	23.280717
114.936208	3344.617884	23.285735
115.377226	3349.284986	23.290752
115.607550	3355.258512	23.295770
115.389048	3364.748421	23.300787
115.800511	3356.281356	23.305805
115.748062	3360.632247	23.310823
115.854824	3349.262994	23.315840
115.858296	3363.771041	23.320858
115.957283	3360.484436	23.325875
115.935036	3360.971131	23.330893
116.059687	3361.930787	23.335911
116.121749	3376.390956	23.340928
116.261697	3382.514999	23.345946
116.026996	3379.578175	23.350963
116.365745	3371.612789	23.355981
116.662662	3392.527092	23.360999
116.767354	3412.637423	23.366016
117.031668	3422.568791	23.371034
116.929810	3414.286604	23.376051
117.031327	3415.795114	23.381069
116.953291	3417.015229	23.386087
117.413317	3426.164908	23.391104
117.669274	3431.507403	23.396122
117.729380	3448.932125	23.401139
117.955379	3445.445887	23.406157
118.132580	3444.421840	23.411175
118.154135	3440.157148	23.416192
118.089190	3446.187237	23.421210
118.139980	3438.294482	23.426227
118.115364	3433.745301	23.431245
117.928729	3441.771693	23.436263
118.458768	3447.128700	23.441280
118.408397	3464.349217	23.446298
118.720537	3473.296735	23.451315
118.908408	3456.107258	23.456333
118.705107	3459.808844	23.461351
118.929041	3458.221169	23.466368
119.684730	3474.134726	23.471386
119.291487	3487.120227	23.476403
119.610196	3482.421095	23.481421
119.635979	3482.841921	23.486439
119.936343	3483.756259	23.491456
120.174271	3490.543620	23.496474
119.919423	3486.082270	23.501491
119.982938	3482.323784	23.506509
120.006401	3480.097043	23.511527
120.120766	3489.253110	23.516544
120.203124	3501.309243	23.521562
120.363487	3506.084085	23.526579
120.565536	3505.618543	23.531597
120.878552	3515.709770	23.536615
120.799268	3507.726799	23.541632
121.030770	3523.020714	23.546650
121.114113	3537.281767	23.551667
121.415656	3531.485585	23.556685
121.590029	3532.288642	23.561703
120.968591	3542.266150	23.566720
121.490189	3543.178253	23.571738
121.309119	3548.929538	23.576755
121.638802	3563.345643	23.581773
121.517432	3577.229520	23.586791
121.690086	3581.869478	23.591808
122.158600	3584.345310	23.596826
122.106638	3600.277662	23.601843
122.250320	3595.825101	23.606861
122.501953	3596.643376	23.611879
122.547616	3600.216401	23.616896
122.720789	3611.466744	23.621914
122.725982	3629.530567	23.626931
122.928239	3631.219705	23.631949
122.729024	3637.347591	23.636967
123.037636	3629.472622	23.641984
123.393138	3642.980792	23.647002
123.165706	3656.123297	23.652019
123.795263	3647.519020	23.657037
123.910093	3649.812899	23.662055
123.775797	3652.468257	23.667072
124.038920	3650.668988	23.672090
123.880638	3655.161925	23.677107
124.474334	3666.390880	23.682125
124.350387	3692.800829	23.687143
124.385532	3679.038638	23.692160
124.560899	3684.503426	23.697178
124.715067	3681.420355	23.702195
124.822304	3680.431837	23.707213
124.869150	3673.588233	23.712231
124.656382	3680.528580	23.717248
125.654731	3683.749104	23.722266
125.781730	3693.488576	23.727283
126.020512	3679.280117	23.732301
126.153940	3674.350078	23.737319
126.483371	3663.286495	23.742336
126.097887	3662.023329	23.747354
126.037515	3659.887024	23.752371
126.405289	3652.347962	23.757389
126.123806	3657.414368	23.762407
126.049789	3669.789794	23.767424
126.302823	3675.890421	23.772442
126.282440	3689.571857	23.777459
126.484108	3684.767815	23.782477
126.544478	3694.404630	23.787495
126.696265	3709.720892	23.792512
127.469348	3710.438715	23.797530
127.375185	3718.830480	23.802547
127.504813	3714.730199	23.807565
127.598405	3711.003834	23.812583
127.743984	3708.614409	23.817600
127.900504	3711.833084	23.822618
127.724025	3720.473195	23.827635
127.588116	3715.708027	23.832653
127.683262	3725.648484	23.837671
127.925792	3736.576337	23.842688
127.745851	3735.674517	23.847706
127.851582	3752.993202	23.852723
128.094874	3768.928217	23.857741
128.385119	3763.019677	23.862759
128.579309	3775.712726	23.867776
129.057883	3786.399224	23.872794
129.193992	3794.664630	23.877811
129.434470	3791.452130	23.882829
129.703249	3792.192161	23.887847
129.398857	3791.288155	23.892864
129.751017	3784.004829	23.897882
129.600120	3789.622380	23.902899
129.840641	3788.810060	23.907917
129.854919	3811.595935	23.912935
129.967005	3818.055800	23.917952
130.078527	3814.278561	23.922970
130.169324	3820.951868	23.927987
130.083629	3822.673572	23.933005
130.314770	3838.539012	23.938023
130.326010	3851.139362	23.943040
130.576969	3843.141309	23.948058
130.382375	3860.737725	23.953075
130.797948	3874.457592	23.958093
130.695626	3873.024955	23.963111
131.052548	3881.947490	23.968128
131.334572	3877.413782	23.973146
131.400673	3900.554197	23.978163
131.770987	3900.281301	23.983181
131.688481	3907.028697	23.988199
131.732342	3910.872708	23.993216
132.119216	3906.461518	23.998234
131.768405	3916.724959	24.003251
132.042125	3933.401087	24.008269
132.137380	3930.857592	24.013287
132.301992	3939.076053	24.018304
132.851985	3948.795446	24.023322
133.044829	3968.468452	24.028339
133.617632	3965.814974	24.033357
133.722276	3956.442229	24.038375
133.512305	3968.983551	24.043392
133.973987	3955.992492	24.048410
133.671637	3960.607618	24.053427
133.664011	3954.959696	24.058445
133.798326	3949.928727	24.063463
133.852611	3956.467099	24.068480
133.796839	3948.587916	24.073498
133.847986	3948.789157	24.078515
134.233863	3971.777995	24.083533
134.653109	3962.697294	24.088551
134.498221	3976.818182	24.093568
134.898708	3960.419460	24.098586
134.814428	3973.548861	24.103603
135.327627	3967.549619	24.108621
135.262462	3962.808491	24.113639
135.582833	3992.620611	24.118656
135.842228	3985.413343	24.123674
135.551449	3995.907209	24.128691
135.564166	3990.247375	24.133709
135.945411	3991.916669	24.138727
135.678384	3997.234203	24.143744
136.206704	3997.907684	24.148762
135.942113	3997.068907	24.153779
136.310916	4016.358332	24.158797
136.349973	4026.250507	24.163815
136.458048	4031.401249	24.168832
136.661165	4029.355040	24.173850
136.434460	4037.665063	24.178867
136.679590	4036.050347	24.183885
136.851019	4038.879660	24.188903
136.784120	4049.090053	24.193920
137.326917	4052.484793	24.198938
137.342389	4070.998299	24.203955
137.245452	4082.351865	24.208973
137.394870	4080.324440	24.213991
137.372000	4091.610346	24.219008
137.600720	4097.608034	24.224026
137.497120	4106.730800	24.229043
138.041181	4116.842244	24.234061
138.565070	4125.477118	24.239079
138.286947	4142.667874	24.244096
138.764858	4135.926035	24.249114
138.798255	4142.070533	24.254131
138.757063	4144.142343	24.259149
139.188263	4151.479784	24.264167
139.302911	4161.466203	24.269184
139.421861	4168.630805	24.274202
139.289703	4163.093918	24.279219
139.407809	4162.909225	24.284237
139.550182	4170.328133	24.289255
139.705925	4190.767314	24.294272
140.219398	4188.077630	24.299290
140.580038	4188.940709	24.304307
140.415955	4189.867790	24.309325
140.442908	4184.824753	24.314343
140.300150	4195.346293	24.319360
140.819673	4206.911620	24.324378
141.031907	4208.316020	24.329395
141.186431	4208.419749	24.334413
141.359593	4201.237140	24.339431
141.069340	4213.380021	24.344448
141.381907	4205.738556	24.349466
141.886566	4223.808431	24.354483
141.471966	4237.012765	24.359501
141.804259	4232.762018	24.364519
142.101004	4234.304780	24.369536
142.305757	4226.094397	24.374554
142.208607	4241.462709	24.379571
142.261122	4254.385668	24.384589
142.857135	4249.904054	24.389607
142.553816	4265.818203	24.394624
142.619557	4251.307155	24.399642
142.827705	4263.836338	24.404659
142.832069	4288.090179	24.409677
143.372751	4287.331458	24.414695
143.382838	4288.122206	24.419712
143.918399	4272.941465	24.424730
143.730641	4277.686318	24.429747
143.690091	4287.410418	24.434765
144.233291	4291.471499	24.439783
144.479040	4304.963955	24.444800
144.538587	4299.837796	24.449818
145.021054	4301.015811	24.454835
144.873635	4311.197528	24.459853
145.189794	4299.359887	24.464871
145.271697	4303.501607	24.469888
145.357398	4301.888684	24.474906
145.260163	4309.987043	24.479923
145.088473	4301.477901	24.484941
145.551297	4295.444080	24.489959
145.704540	4302.426268	24.494976
145.745159	4319.817368	24.499994
145.770482	4330.803114	24.505011
145.680699	4336.238835	24.510029
145.767670	4337.632540	24.515047
145.661646	4341.790863	24.520064
145.927662	4347.999842	24.525082
146.336353	4361.128866	24.530099
145.713232	4369.786291	24.535117
146.217164	4382.819115	24.540135
146.226328	4402.265520	24.545152
146.466463	4407.013776	24.550170
146.923409	4428.383154	24.555187
146.977331	4429.316398	24.560205
147.259221	4436.128659	24.565223
147.333787	4457.552757	24.570240
147.596106	4459.506983	24.575258
147.912101	4466.415308	24.580275
147.524456	4465.865970	24.585293
148.567813	4460.316184	24.590311
148.787136	4473.185989	24.595328
148.614948	4482.679456	24.600346
148.846412	4475.920117	24.605363
148.612148	4469.769229	24.610381
149.163300	4477.834311	24.615399
149.119874	4500.541553	24.620416
149.160911	4502.511401	24.625434
149.386158	4507.638906	24.630451
149.509607	4503.070504	24.635469
149.643677	4502.131152	24.640487
149.492528	4522.888003	24.645504
149.866867	4532.615341	24.650522
150.513816	4527.431631	24.655539
150.317587	4535.136799	24.660557
150.404098	4534.767539	24.665575
150.710787	4558.250614	24.670592
150.747407	4560.749857	24.675610
151.129125	4561.767732	24.680627
150.830197	4563.605342	24.685645
151.307979	4555.891724	24.690663
151.238194	4569.233333	24.695680
151.494097	4578.454839	24.700698
151.587600	4588.446492	24.705715
151.658926	4585.200217	24.710733
151.839543	4583.998537	24.715751
151.890045	4606.141039	24.720768
152.214338	4618.982434	24.725786
152.238198	4614.931026	24.730803
152.130263	4624.442661	24.735821
152.365294	4641.870800	24.740839
152.692621	4648.266814	24.745856
152.850504	4647.616321	24.750874
152.609475	4660.946767	24.755891
152.832152	4680.455475	24.760909
153.576767	4685.707140	24.765927
153.644803	4694.843811	24.770944
153.886093	4697.245929	24.775962
153.943326	4701.180850	24.780979
154.102953	4713.913265	24.785997
154.139771	4706.869376	24.791015
154.662791	4698.427034	24.796032
154.337215	4708.579214	24.801050
154.617989	4703.545878	24.806067
154.550027	4710.425067	24.811085
154.867473	4722.554859	24.816103
155.130118	4735.132400	24.821120
155.261335	4726.198651	24.826138
155.257096	4724.043013	24.831155
155.390097	4738.292592	24.836173
155.532149	4754.236165	24.841191
155.814990	4757.169799	24.846208
155.548904	4762.234910	24.851226
155.907451	4765.715846	24.856243
156.538925	4786.487530	24.861261
156.535072	4787.445744	24.866279
156.666301	4788.974049	24.871296
156.606951	4791.430414	24.876314
156.865886	4788.678150	24.881331
156.834020	4810.508382	24.886349
157.214731	4810.613029	24.891367
157.828130	4807.008845	24.896384
157.966080	4797.739615	24.901402
158.255402	4798.256138	24.906419
158.545346	4795.368330	24.911437
158.830624	4784.141018	24.916455
158.926349	4786.459365	24.921472
158.709040	4789.106919	24.926490
158.735501	4779.266207	24.931507
158.893537	4791.952525	24.936525
158.971316	4791.262874	24.941543
159.196559	4784.093708	24.946560
158.946451	4776.651028	24.951578
159.566791	4794.590659	24.956595
159.704244	4815.044638	24.961613
159.594598	4809.265534	24.966631
159.979185	4813.987744	24.971648
159.909662	4818.296156	24.976666
160.062578	4813.471989	24.981683
160.027856	4834.698494	24.986701
160.094772	4837.525745	24.991719
160.218522	4844.225733	24.996736
160.161312	4852.066248	25.001754
160.469770	4871.673250	25.006771
160.329499	4874.697975	25.011789
160.836805	4882.088952	25.016807
160.999412	4904.494109	25.021824
161.107291	4907.507596	25.026842
161.591687	4921.263104	25.031859
161.430963	4933.702192	25.036877
161.778944	4929.178894	25.041895
162.395412	4928.969016	25.046912
162.591361	4935.376664	25.051930
162.929597	4941.307672	25.056947
163.669427	4934.787276	25.061965
163.887717	4904.882120	25.066983
164.066370	4897.435526	25.072000
163.621314	4898.744177	25.077018
163.766322	4891.731728	25.082035
164.008247	4882.722014	25.087053
164.160773	4879.728648	25.092071
164.188018	4869.934955	25.097088
164.195856	4863.040374	25.102106
164.076659	4865.564513	25.107123
164.025308	4885.481450	25.112141
164.514475	4872.916349	25.117159
164.691974	4876.463944	25.122176
164.323891	4875.788735	25.127194
164.735781	4877.376936	25.132211
164.529246	4899.434198	25.137229
164.590757	4908.604298	25.142247
164.810921	4920.239954	25.147264
164.829667	4935.651088	25.152282
165.312288	4940.404914	25.157299
165.168101	4963.531750	25.162317
165.430738	4961.358701	25.167335
165.756441	4986.906225	25.172352
165.754689	5006.870490	25.177370
166.112260	5005.091409	25.182387
166.319370	5023.566901	25.187405
166.406210	5041.821633	25.192423
166.620427	5033.503083	25.197440
166.733599	5053.158774	25.202458
166.784516	5062.357409	25.207475
166.838690	5081.412021	25.212493
167.556706	5091.950369	25.217511
167.741197	5092.308172	25.222528
167.402594	5104.275388	25.227546
167.945246	5116.091873	25.232563
167.984726	5123.511934	25.237581
168.119320	5128.586450	25.242599
168.509795	5139.217968	25.247616
168.469000	5148.687764	25.252634
169.053619	5152.400247	25.257651
168.703844	5157.867495	25.262669
168.959013	5179.347242	25.267687
169.332768	5183.263295	25.272704
169.219475	5197.175729	25.277722
169.694095	5199.282670	25.282739
169.646151	5222.048387	25.287757
169.837190	5218.653070	25.292775
169.941497	5232.020231	25.297792
170.597189	5246.404109	25.302810
170.872678	5242.033893	25.307827
170.642766	5258.815432	25.312845
170.793156	5254.139438	25.317863
170.976256	5268.937785	25.322880
171.179961	5276.557541	25.327898
171.609858	5275.552878	25.332915
171.886244	5275.373621	25.337933
171.739044	5270.387092	25.342951
171.970604	5285.116361	25.347968
171.683532	5300.970807	25.352986
172.103852	5294.753754	25.358003
172.311111	5304.387871	25.363021
172.518647	5309.904786	25.368039
172.697172	5317.463276	25.373056
172.582909	5330.991259	25.378074
172.896473	5322.565442	25.383091
172.668716	5338.541861	25.388109
173.056387	5349.742814	25.393127
173.280292	5355.117091	25.398144
173.323397	5381.085646	25.403162
173.595977	5377.433392	25.408179
174.026732	5384.385223	25.413197
174.351429	5408.409658	25.418215
174.560405	5416.063263	25.423232
174.591472	5418.974233	25.428250
174.858079	5411.429960	25.433267
175.145763	5423.731875	25.438285
174.981945	5443.916902	25.443303
175.067120	5438.815375	25.448320
175.204018	5445.959642	25.453338
175.469128	5458.561799	25.458355
176.009297	5476.040621	25.463373
175.593869	5481.094381	25.468391
176.207401	5471.868492	25.473408
176.143715	5501.223268	25.478426
176.081206	5499.206626	25.483443
176.465600	5503.677323	25.488461
176.873146	5526.699758	25.493479
177.421861	5520.760331	25.498496
177.324230	5530.657212	25.503514
177.303082	5518.984893	25.508531
177.442455	5538.408098	25.513549
177.511170	5547.768634	25.518567
178.167508	5545.203855	25.523584
177.898050	5559.626185	25.528602
178.208968	5579.885194	25.533619
178.712898	5577.084284	25.538637
179.207487	5584.740433	25.543655
179.393817	5580.485043	25.548672
179.168333	5581.905869	25.553690
179.425330	5569.210403	25.558707
179.544386	5579.970489	25.563725
179.615381	5604.370076	25.568743
179.960512	5600.537829	25.573760
179.935648	5608.672565	25.578778
180.097237	5597.522584	25.583795
180.220580	5611.033395	25.588813
180.323937	5632.634781	25.593831
180.622863	5640.867399	25.598848
180.512118	5645.972556	25.603866
180.738188	5644.385889	25.608883
180.567409	5662.781597	25.613901
180.737736	5674.763326	25.618919
181.515618	5673.615824	25.623936
181.330445	5702.105230	25.628954
181.356279	5708.013975	25.633971
181.875191	5707.806276	25.638989
182.031677	5724.733658	25.644007
182.063790	5740.240274	25.649024
182.201789	5740.178280	25.654042
182.346499	5758.921922	25.659059
182.470462	5763.482216	25.664077
182.748710	5775.927552	25.669095
182.857767	5788.897128	25.674112
183.105344	5793.566757	25.679130
183.283278	5801.425358	25.684148
183.505031	5826.114417	25.689165
183.595220	5830.683264	25.694183
183.757786	5842.718296	25.699200
183.881163	5858.032667	25.704218
184.087878	5853.724382	25.709236
184.295942	5875.115087	25.714253
184.392155	5886.585583	25.719271
184.843949	5903.016823	25.724288
185.273718	5920.149486	25.729306
185.397709	5911.726812	25.734324
185.595171	5914.660919	25.739341
185.837347	5938.619118	25.744359
185.943908	5943.044552	25.749376
186.141982	5941.970593	25.754394
186.219106	5941.063050	25.759412
186.894020	5957.886012	25.764429
186.621188	5968.763151	25.769447
186.934887	5962.031730	25.774464
187.052852	5975.686929	25.779482
187.328715	5985.596951	25.784500
188.084111	5989.602655	25.789517
187.840288	5999.676584	25.794535
188.114333	5993.232361	25.799552
188.166797	5998.867103	25.804570
188.245849	5996.888406	25.809588
188.727849	6009.495008	25.814605
188.808058	6024.876231	25.819623
188.800673	6017.005539	25.824640
188.990910	6017.331767	25.829658
188.946223	6025.291286	25.834676
189.518205	6038.424889	25.839693
189.312399	6044.527276	25.844711
189.629168	6049.182021	25.849728
189.606960	6070.552285	25.854746
189.792438	6080.557036	25.859764
190.309463	6079.557318	25.864781
189.943500	6105.151747	25.869799
190.466033	6105.673630	25.874816
190.497017	6116.112178	25.879834
190.862560	6130.097062	25.884852
191.040991	6137.218519	25.889869
191.126628	6150.543851	25.894887
191.432206	6157.364940	25.899904
191.807975	6170.655048	25.904922
191.729902	6174.947905	25.909940
192.056579	6176.312224	25.914957
191.886157	6185.514586	25.919975
192.304117	6182.351177	25.924992
192.903100	6187.887054	25.930010
192.910301	6196.755820	25.935028
193.387035	6209.968495	25.940045
193.409944	6229.560669	25.945063
193.961461	6225.025778	25.950080
193.793065	6229.306300	25.955098
193.728428	6230.500902	25.960116
194.192795	6219.915900	25.965133
194.130605	6239.597191	25.970151
194.089399	6250.295978	25.975168
194.217967	6252.828844	25.980186
194.380109	6269.224843	25.985204
194.584884	6271.580330	25.990221
194.663864	6289.446015	25.995239
195.043462	6296.332476	26.000256
195.435642	6303.269652	26.005274
195.388131	6328.451753	26.010292
196.006954	6336.007447	26.015309
195.745690	6342.892244	26.020327
196.209436	6357.919965	26.025344
196.437980	6363.106607	26.030362
196.269829	6373.792676	26.035380
196.891588	6384.919329	26.040397
196.514298	6391.275015	26.045415
197.186660	6409.578922	26.050432
197.249013	6426.747147	26.055450
197.401728	6432.154413	26.060468
197.789992	6449.967834	26.065485
198.010202	6464.086361	26.070503
197.931887	6471.205637	26.075520
198.290269	6481.275938	26.080538
198.303360	6490.469687	26.085556
198.424836	6502.520461	26.090573
198.753847	6524.418425	26.095591
199.585314	6519.924579	26.100608
199.355950	6525.321980	26.105626
200.016776	6543.248638	26.110644
200.425718	6543.923199	26.115661
200.304818	6549.593658	26.120679
200.072531	6549.553717	26.125696
200.735003	6555.744488	26.130714
201.115646	6572.788174	26.135732
201.182791	6569.134553	26.140749
201.089495	6580.453253	26.145767
201.329316	6580.279818	26.150784
201.207048	6583.089569	26.155802
201.154511	6601.705995	26.160820
201.527999	6605.547727	26.165837
201.596145	6621.339073	26.170855
202.433970	6626.967655	26.175872
202.995293	6624.896251	26.180890
203.295654	6631.648363	26.185908
203.293472	6626.373089	26.190925
203.274030	6626.905080	26.195943
203.442809	6622.782023	26.200960
203.501081	6624.558205	26.205978
203.442410	6647.533969	26.210996
203.812420	6654.188435	26.216013
203.621427	6657.544996	26.221031
204.020432	6682.539662	26.226048
204.487147	6679.550533	26.231066
204.372138	6693.553945	26.236084
204.540193	6698.544984	26.241101
204.560976	6714.581607	26.246119
204.693629	6723.271743	26.251136
205.051697	6737.544805	26.256154
205.009538	6750.915442	26.261172
205.715526	6763.963022	26.266189
205.713343	6774.719698	26.271207
205.780707	6791.699489	26.276224
206.353103	6801.849982	26.281242
206.429095	6809.457844	26.286260
206.899165	6822.976641	26.291277
206.721901	6841.901240	26.296295
206.699104	6838.265826	26.301312
207.190889	6866.360757	26.306330
207.375372	6879.761473	26.311348
207.486411	6895.925535	26.316365
207.701250	6905.258910	26.321383
207.751132	6924.066353	26.326400
208.261292	6942.207148	26.331418
208.688979	6946.581686	26.336436
209.006007	6955.846082	26.341453
209.146784	6970.114668	26.346471
209.400099	6973.565704	26.351488
209.891782	6979.632809	26.356506
209.499248	7000.398553	26.361524
210.024811	7005.693867	26.366541
210.089540	7010.639322	26.371559
210.382248	7022.846557	26.376576
210.348058	7030.306070	26.381594
210.709070	7036.443603	26.386612
211.161108	7048.328025	26.391629
211.312883	7061.968603	26.396647
211.271684	7067.716254	26.401664
211.640469	7064.546341	26.406682
211.567366	7087.803632	26.411700
212.187543	7092.188443	26.416717
212.496100	7097.037613	26.421735
212.560885	7110.531585	26.426752
212.876929	7119.453168	26.431770
212.981539	7115.767473	26.436788
213.284927	7108.103964	26.441805
213.336979	7118.077967	26.446823
213.384389	7137.551761	26.451840
213.771028	7143.101399	26.456858
213.241401	7152.674795	26.461876
213.893536	7167.227152	26.466893
214.101718	7172.481849	26.471911
214.085838	7187.344524	26.476928
214.654958	7192.647912	26.481946
214.604148	7203.706940	26.486964
214.972516	7214.748721	26.491981
215.058285	7237.147621	26.496999
215.130409	7239.525199	26.502016
215.593156	7260.487010	26.507034
215.560892	7267.493095	26.512052
215.882355	7281.780386	26.517069
216.272109	7291.870632	26.522087
216.135536	7302.768719	26.527104
217.065996	7320.483371	26.532122
217.067571	7326.165286	26.537140
217.511992	7328.658211	26.542157
217.916694	7338.305456	26.547175
218.009715	7354.653083	26.552192
218.581117	7353.440822	26.557210
218.384464	7356.090250	26.562228
218.437916	7359.014557	26.567245
218.631245	7362.735704	26.572263
218.752797	7374.702191	26.577280
219.201090	7380.586742	26.582298
218.851923	7399.733810	26.587316
219.137428	7409.934396	26.592333
219.669702	7425.468471	26.597351
219.570504	7437.695249	26.602368
219.728251	7446.002530	26.607386
219.749997	7470.450800	26.612404
220.166074	7478.905767	26.617421
220.491708	7491.823417	26.622439
220.748045	7514.158557	26.627456
221.113924	7528.997694	26.632474
221.163038	7541.578224	26.637492
221.455038	7553.045548	26.642509
221.723714	7577.039149	26.647527
221.210067	7587.018667	26.652544
222.350668	7599.643993	26.657562
221.944014	7622.633060	26.662580
222.367776	7634.254131	26.667597
222.937133	7639.253117	26.672615
222.887082	7657.175243	26.677632
223.260754	7668.848392	26.682650
223.216031	7688.563431	26.687668
223.533765	7693.112315	26.692685
224.179162	7712.401820	26.697703
223.814545	7722.256553	26.702720
224.195108	7733.975081	26.707738
224.538666	7740.100346	26.712756
224.555695	7750.114192	26.717773
225.233639	7769.430058	26.722791
225.361759	7767.138384	26.727808
225.429143	7782.872064	26.732826
225.415419	7801.250481	26.737844
225.886741	7806.810083	26.742861
226.103712	7820.977237	26.747879
226.136205	7830.378822	26.752896
226.433275	7836.031921	26.757914
226.729142	7861.391642	26.762932
226.706288	7873.252497	26.767949
227.188642	7879.987971	26.772967
227.365154	7891.943356	26.777984
227.890489	7899.541125	26.783002
228.071812	7919.626082	26.788020
228.266090	7928.098174	26.793037
228.592213	7926.738084	26.798055
228.748012	7944.796923	26.803072
229.005785	7946.482835	26.808090
228.827556	7958.193046	26.813108
229.260884	7976.321781	26.818125
229.569687	7992.574328	26.823143
229.439668	8009.556281	26.828160
229.548178	8027.732533	26.833178
229.730937	8041.328148	26.838196
230.166009	8058.051670	26.843213
230.664730	8074.540794	26.848231
230.403196	8097.149798	26.853248
230.549138	8111.030702	26.858266
230.924496	8128.199774	26.863284
231.135980	8146.375885	26.868301
231.464443	8171.081727	26.873319
231.461685	8191.962463	26.878336
232.052604	8199.501928	26.883354
232.256533	8224.194660	26.888372
232.404847	8240.034351	26.893389
232.929331	8258.820537	26.898407
232.617471	8268.255259	26.903424
233.351903	8284.066480	26.908442
233.581784	8296.575547	26.913460
233.418188	8328.041102	26.918477
233.943450	8336.404789	26.923495
234.235648	8351.933251	26.928512
234.501042	8356.889657	26.933530
234.408708	8379.051104	26.938548
234.857264	8389.553731	26.943565
235.218029	8405.417175	26.948583
235.277521	8421.401455	26.953600
235.402937	8446.038212	26.958618
235.943149	8461.980919	26.963636
235.926310	8477.060646	26.968653
236.288771	8496.527692	26.973671
236.109169	8511.536608	26.978688
236.826607	8526.608714	26.983706
236.944542	8547.166551	26.988724
237.063885	8572.374622	26.993741
237.495661	8565.761328	26.998759
237.641030	8587.922175	27.003776
237.799674	8602.921329	27.008794
237.912983	8623.087716	27.013812
238.202721	8638.658183	27.018829
238.893856	8654.130051	27.023847
238.773250	8661.770197	27.028864
239.174014	8665.768267	27.033882
239.422427	8687.834534	27.038900
239.717537	8690.951940	27.043917
240.207059	8693.683835	27.048935
240.284479	8725.678010	27.053952
240.513652	8728.794919	27.058970
240.650374	8730.759519	27.063988
240.740167	8747.708051	27.069005
241.266306	8756.019504	27.074023
241.233161	8769.902811	27.079040
241.765979	8781.666752	27.084058
242.329010	8777.260305	27.089076
242.927025	8785.840865	27.094093
243.359171	8794.729995	27.099111
243.836393	8796.999175	27.104128
244.071267	8789.019938	27.109146
244.215446	8780.925710	27.114164
243.975760	8776.561449	27.119181
244.150453	8781.439990	27.124199
244.353354	8787.985130	27.129216
244.511077	8786.506620	27.134234
244.712813	8783.099750	27.139252
244.614955	8790.802045	27.144269
245.125065	8806.772743	27.149287
244.860625	8824.492779	27.154304
245.252151	8835.729600	27.159322
245.817868	8842.693821	27.164340
245.694199	8850.647759	27.169357
245.814847	8868.341479	27.174375
246.113510	8889.534774	27.179392
246.461369	8905.264269	27.184410
246.204979	8920.651376	27.189428
246.243774	8948.883435	27.194445
246.705907	8953.678043	27.199463
247.119729	8979.865266	27.204480
247.346165	9008.732902	27.209498
247.515819	9029.888726	27.214516
247.580990	9043.444188	27.219533
248.088260	9062.501700	27.224551
248.173593	9091.766585	27.229568
248.643897	9106.394297	27.234586
248.881248	9122.428487	27.239604
248.808742	9148.458227	27.244621
249.501375	9159.895187	27.249639
249.272592	9195.738678	27.254656
249.631570	9207.587330	27.259674
250.210189	9228.952894	27.264692
250.370446	9239.064521	27.269709
251.003350	9239.864066	27.274727
251.103489	9258.417744	27.279744
251.100105	9254.344238	27.284762
251.792805	9278.650722	27.289780
251.849648	9282.008096	27.294797
252.126153	9295.470680	27.299815
252.518992	9302.902205	27.304832
252.503641	9305.241330	27.309850
252.789270	9319.684632	27.314868
252.777156	9342.407631	27.319885
253.067462	9366.419540	27.324903
253.593511	9373.093249	27.329920
253.766311	9398.129311	27.334938
254.014171	9407.507784	27.339956
254.107564	9428.884877	27.344973
254.536728	9440.498628	27.349991
254.711352	9452.904931	27.355008
255.105282	9478.432371	27.360026
255.356264	9478.150105	27.365044
255.625120	9504.448709	27.370061
255.701608	9511.350362	27.375079
255.850030	9523.983618	27.380096
256.473042	9537.343177	27.385114
257.010351	9558.433267	27.390132
256.897340	9571.811810	27.395149
257.471076	9588.289469	27.400167
257.403824	9609.435866	27.405184
257.670526	9614.332279	27.410202
258.018378	9623.336471	27.415220
258.114295	9647.061869	27.420237
258.354982	9653.751681	27.425255
258.597100	9668.759056	27.430272
259.047349	9686.691207	27.435290
259.336817	9701.508089	27.440308
259.495216	9713.219518	27.445325
259.985415	9724.287813	27.450343
260.107682	9735.232182	27.455360
260.061005	9751.725890	27.460378
260.420717	9760.657050	27.465396
260.559675	9774.685416	27.470413
261.256342	9779.488947	27.475431
261.229156	9813.944974	27.480448
261.558820	9820.914231	27.485466
261.871231	9828.735029	27.490484
261.939379	9858.148165	27.495501
262.441043	9867.279878	27.500519
262.596380	9881.784234	27.505536
263.007191	9891.641508	27.510554
263.133314	9908.466719	27.515572
263.239131	9932.619909	27.520589
263.937586	9935.969202	27.525607
264.093731	9957.889525	27.530624
263.776839	9974.221336	27.535642
264.382336	9985.184874	27.540660
264.322961	10003.645271	27.545677
264.736446	10012.542432	27.550695
264.781706	10027.289956	27.555712
264.716044	10042.321974	27.560730
265.194082	10058.892141	27.565748
265.521155	10096.942144	27.570765
266.086227	10101.932033	27.575783
266.765110	10125.705740	27.580800
266.870568	10125.117686	27.585818
267.605578	10121.223344	27.590836
267.271464	10147.600298	27.595853
267.692837	10153.813323	27.600871
268.122875	10164.787253	27.605888
268.551786	10182.405834	27.610906
268.815203	10184.294554	27.615924
268.613138	10185.162326	27.620941
269.137117	10198.149866	27.625959
269.276990	10213.891852	27.630976
269.499566	10222.762511	27.635994
269.826014	10240.186569	27.641012
269.629502	10259.162605	27.646029
269.779360	10272.113434	27.651047
270.474286	10278.394664	27.656064
270.336954	10302.698570	27.661082
270.773445	10320.564806	27.666100
270.761598	10344.116836	27.671117
271.190105	10366.062416	27.676135
271.525814	10386.733655	27.681152
271.664068	10411.101237	27.686170
272.210710	10427.399578	27.691188
272.666487	10454.300463	27.696205
272.734304	10464.484317	27.701223
273.164953	10484.429466	27.706240
273.059219	10502.184408	27.711258
273.852473	10520.514642	27.716276
273.915116	10535.456258	27.721293
274.348957	10546.868640	27.726311
274.636920	10570.187096	27.731328
274.657045	10582.926692	27.736346
275.164251	10596.074661	27.741364
275.402033	10616.467075	27.746381
275.595045	10617.095597	27.751399
276.389775	10630.127716	27.756416
276.288486	10644.846077	27.761434
276.605744	10655.248057	27.766452
277.056684	10677.162182	27.771469
277.161947	10679.966330	27.776487
277.497152	10703.892936	27.781504
277.545615	10717.495855	27.786522
277.916307	10728.371832	27.791540
277.975650	10744.614001	27.796557
278.224669	10764.644747	27.801575
278.707056	10783.955943	27.806592
278.796847	10802.184180	27.811610
278.918735	10799.542017	27.816628
279.286229	10829.456727	27.821645
279.513610	10843.411389	27.826663
279.690937	10861.027972	27.831680
279.773976	10875.917088	27.836698
280.344505	10895.556749	27.841716
280.416154	10919.065865	27.846733
280.800141	10932.635368	27.851751
281.520946	10950.381476	27.856768
281.710954	10967.295673	27.861786
281.843167	10973.690900	27.866804
281.935072	11005.992592	27.871821
282.344571	11014.845729	27.876839
282.683312	11030.967323	27.881856
282.877553	11045.173414	27.886874
283.519375	11060.457495	27.891892
283.678779	11077.477242	27.896909
284.101750	11093.687010	27.901927
284.347243	11101.188175	27.906944
284.373852	11113.976574	27.911962
285.006241	11131.843047	27.916980
284.993071	11151.230162	27.921997
285.095270	11167.323098	27.927015
285.426875	11186.248383	27.932032
285.612830	11196.975283	27.937050
286.193011	11216.218317	27.942068
286.381416	11241.125672	27.947085
286.330193	11263.262758	27.952103
286.960404	11277.039682	27.957120
287.101235	11299.380562	27.962138
288.065984	11303.543485	27.967156
288.391981	11305.065235	27.972173
289.129478	11310.540246	27.977191
289.521414	11304.701499	27.982208
289.481728	11318.611213	27.987226
290.011499	11334.055306	27.992244
290.133653	11346.448312	27.997261
290.158926	11339.053879	28.002279
290.600108	11336.957538	28.007296
290.482697	11353.261590	28.012314
291.068717	11366.775867	28.017332
291.077077	11376.986735	28.022349
291.486263	11394.993585	28.027367
291.768649	11404.611799	28.032384
291.690840	11409.650688	28.037402
292.228440	11415.713876	28.042420
292.227854	11443.181394	28.047437
292.542476	11454.551093	28.052455
292.841432	11472.381390	28.057472
292.817500	11494.502854	28.062490
293.145281	11518.635005	28.067508
293.351643	11541.646241	28.072525
293.586237	11557.048670	28.077543
293.733511	11583.212857	28.082560
293.808475	11627.008834	28.087578
294.094426	11637.401528	28.092596
294.736509	11664.096595	28.097613
294.899275	11684.682851	28.102631
295.488899	11698.936139	28.107648
295.724003	11724.062152	28.112666
296.209279	11740.328408	28.117684
296.468477	11756.096270	28.122701
296.645638	11775.851728	28.127719
297.267286	11785.403122	28.132736
297.309817	11807.390872	28.137754
297.562458	11810.886240	28.142772
297.773068	11835.492717	28.147789
297.954956	11857.961292	28.152807
298.329869	11868.698692	28.157824
298.311853	11896.663524	28.162842
298.638223	11924.805517	28.167860
298.990354	11937.980951	28.172877
299.127955	11962.153172	28.177895
299.814118	11985.648050	28.182912
299.673851	12018.060923	28.187930
300.337544	12043.521764	28.192948
300.633645	12060.154815	28.197965
300.720505	12091.487327	28.202983
301.342040	12109.876783	28.208000
301.789864	12132.943310	28.213018
302.204311	12141.180199	28.218036
302.654257	12173.376536	28.223053
302.761491	12183.096366	28.228071
303.350673	12203.010253	28.233088
303.272839	12222.268537	28.238106
303.657618	12240.294452	28.243124
304.423393	12255.500169	28.248141
304.235220	12274.107830	28.253159
304.465494	12289.300542	28.258176
304.708319	12313.241661	28.263194
305.173644	12333.873258	28.268212
305.201392	12364.690536	28.273229
305.360115	12382.167412	28.278247
306.087393	12390.312660	28.283264
306.002716	12424.872333	28.288282
306.289808	12450.238423	28.293300
306.835308	12472.807281	28.298317
307.193760	12499.886714	28.303335
307.282831	12513.068467	28.308352
307.656390	12541.324809	28.313370
308.492151	12564.063021	28.318388
308.587525	12585.591451	28.323405
308.866227	12604.549669	28.328423
309.562661	12624.285944	28.333440
309.576429	12640.497948	28.338458
309.821350	12666.215204	28.343476
310.412146	12681.266030	28.348493
310.245815	12707.492367	28.353511
310.453132	12714.291584	28.358528
310.888311	12747.308658	28.363546
311.294807	12752.211368	28.368564
311.621335	12773.994667	28.373581
311.681928	12794.541246	28.378599
312.259290	12802.807829	28.383616
312.306708	12826.039984	28.388634
312.159201	12852.744058	28.393652
312.687624	12871.606820	28.398669
312.900976	12901.972008	28.403687
313.467157	12927.803905	28.408704
313.761579	12955.048539	28.413722
314.058798	12962.012521	28.418740
314.847592	12975.137758	28.423757
314.722621	12997.312044	28.428775
315.210914	13006.030503	28.433792
315.895446	13023.489153	28.438810
315.947502	13048.334513	28.443828
316.595219	13062.956591	28.448845
316.596374	13083.471116	28.453863
317.034857	13098.556375	28.458880
317.538108	13108.072969	28.463898
318.527539	13105.415333	28.468916
318.988281	13110.851191	28.473933
319.131569	13123.972680	28.478951
319.999768	13094.587563	28.483968
320.869524	13077.044222	28.488986
321.506110	13073.392343	28.494004
321.841585	13061.914051	28.499021
321.995278	13034.590102	28.504039
322.291509	13022.097524	28.509056
322.144111	13024.554696	28.514074
322.267889	13021.574940	28.519092
322.637681	13012.409045	28.524109
322.380929	13030.596398	28.529127
322.563398	13033.110217	28.534144
322.684671	13025.905315	28.539162
322.788150	13031.467554	28.544180
322.873680	13046.945436	28.549197
322.941547	13070.057219	28.554215
323.225044	13092.287767	28.559232
323.607687	13111.787964	28.564250
323.790491	13129.841420	28.569268
324.058569	13148.901294	28.574285
324.009467	13185.704613	28.579303
324.192085	13206.508403	28.584320
324.568865	13239.832917	28.589338
324.581164	13275.554817	28.594356
325.094050	13305.074863	28.599373
325.517305	13334.018270	28.604391
325.946270	13365.421775	28.609408
326.072691	13396.089225	28.614426
326.634264	13427.755801	28.619444
327.411141	13442.389249	28.624461
327.275826	13477.752274	28.629479
327.933912	13500.197560	28.634496
328.246796	13523.588317	28.639514
328.920078	13543.383306	28.644532
329.493347	13547.473974	28.649549
329.111118	13558.275879	28.654567
329.755185	13577.291616	28.659584
330.095404	13609.878172	28.664602
330.169579	13622.821882	28.669620
330.681912	13640.253093	28.674637
330.518274	13667.919753	28.679655
330.947545	13690.862771	28.684672
331.469086	13708.541055	28.689690
331.634260	13737.277798	28.694708
331.974259	13764.034645	28.699725
332.421465	13794.987908	28.704743
332.829678	13812.817217	28.709760
333.033177	13840.266855	28.714778
333.407510	13869.316983	28.719796
333.914789	13875.911569	28.724813
334.202927	13896.086534	28.729831
334.514363	13932.802992	28.734848
334.959823	13943.580019	28.739866
335.038011	13965.260048	28.744884
335.595154	13982.714620	28.749901
335.642243	14008.931016	28.754919
336.147844	14024.869590	28.759936
336.503028	14053.939554	28.764954
336.924536	14080.035585	28.769972
337.141751	14092.267481	28.774989
337.175118	14131.250878	28.780007
337.452054	14157.918781	28.785024
337.831834	14186.758551	28.790042
337.970788	14220.056978	28.795060
338.325608	14249.071280	28.800077
338.909592	14282.043260	28.805095
339.392314	14304.275898	28.810112
339.593855	14344.584132	28.815130
339.820683	14370.031803	28.820148
340.289085	14391.131746	28.825165
340.808939	14433.026750	28.830183
341.153859	14456.684836	28.835200
341.487482	14480.180422	28.840218
342.126195	14510.488196	28.845236
342.441664	14521.991627	28.850253
342.622147	14550.392773	28.855271
343.065051	14564.469131	28.860288
343.364598	14592.694225	28.865306
343.622159	14626.518327	28.870324
344.307259	14642.107444	28.875341
344.543127	14660.661438	28.880359
345.113871	14681.026017	28.885376
345.291693	14693.713309	28.890394
345.694043	14719.870658	28.895412
346.388023	14720.788355	28.900429
346.575988	14744.033690	28.905447
347.096427	14756.072837	28.910464
347.663568	14773.272239	28.915482
347.609900	14789.828505	28.920500
348.061252	14786.190898	28.925517
348.300248	14804.954276	28.930535
348.276813	14815.822197	28.935552
349.033821	14833.597701	28.940570
349.156447	14850.301102	28.945588
349.674837	14858.670716	28.950605
349.885252	14891.114669	28.955623
350.046901	14899.924264	28.960640
350.402629	14915.268959	28.965658
350.420583	14938.729645	28.970676
350.974613	14952.977892	28.975693
351.045122	14989.395075	28.980711
351.194658	15005.450268	28.985728
351.984216	15025.782501	28.990746
352.289037	15044.196266	28.995764
353.262823	15042.797315	29.000781
353.612042	15071.721069	29.005799
353.704272	15080.168366	29.010816
354.701156	15093.785627	29.015834
354.839495	15110.762847	29.020852
354.983565	15113.502784	29.025869
355.444597	15136.593796	29.030887
355.228344	15148.262248	29.035904
355.933389	15167.056013	29.040922
355.900563	15189.682978	29.045940
356.406127	15203.327661	29.050957
356.703984	15237.248147	29.055975
356.898517	15258.591132	29.060992
357.178828	15274.654698	29.066010
357.341613	15308.300650	29.071028
358.012961	15338.662335	29.076045
358.243110	15368.387403	29.081063
358.417118	15393.673459	29.086080
358.911913	15418.712398	29.091098
359.144475	15449.723089	29.096116
359.426508	15476.765059	29.101133
359.690331	15511.647551	29.106151
360.360918	15540.711104	29.111168
360.485061	15576.739286	29.116186
360.927863	15607.111549	29.121204
361.645203	15628.928157	29.126221
361.716093	15657.989286	29.131239
361.996921	15683.780583	29.136256
362.738693	15701.921787	29.141274
362.866046	15739.263462	29.146292
363.334549	15759.101441	29.151309
363.764952	15790.373578	29.156327
364.025169	15825.795680	29.161344
364.376304	15850.626352	29.166362
364.509087	15879.125533	29.171380
365.043722	15904.332321	29.176397
365.115506	15935.747721	29.181415
365.412778	15963.178036	29.186432
366.122157	15989.070429	29.191450
366.214663	16016.868479	29.196468
366.473752	16051.536627	29.201485
367.168850	16080.556944	29.206503
367.329699	16106.044671	29.211520
367.660948	16121.512277	29.216538
367.962241	16155.208073	29.221556
368.404629	16175.134600	29.226573
369.021363	16200.056371	29.231591
369.112503	16230.544756	29.236608
369.654317	16255.398444	29.241626
370.033968	16279.642435	29.246644
370.686345	16303.661913	29.251661
371.023944	16326.190371	29.256679
371.070813	16355.851673	29.261696
372.163498	16378.233501	29.266714
372.035629	16408.429800	29.271732
372.445293	16420.547651	29.276749
373.152149	16442.296225	29.281767
372.831026	16469.593129	29.286784
373.555833	16491.927258	29.291802
374.105150	16529.517750	29.296820
374.254466	16547.182750	29.301837
374.667697	16571.810210	29.306855
375.274374	16607.076141	29.311872
375.485516	16624.287308	29.316890
375.413558	16652.491820	29.321908
376.093826	16679.359251	29.326925
376.575475	16708.986981	29.331943
376.935978	16733.260718	29.336960
377.362939	16755.618483	29.341978
377.672764	16789.385754	29.346996
377.976794	16802.302987	29.352013
378.465738	16826.443809	29.357031
378.446357	16852.771491	29.362048
379.481114	16883.377510	29.367066
379.462579	16922.623559	29.372084
379.985168	16947.655632	29.377101
380.479195	16973.985559	29.382119
380.347806	17011.355786	29.387136
380.981315	17030.705146	29.392154
381.343415	17064.924121	29.397172
381.573389	17096.218243	29.402189
381.756204	17131.052533	29.407207
382.121122	17171.502247	29.412224
382.782776	17195.758640	29.417242
383.783112	17214.978910	29.422260
385.019849	17216.830352	29.427277
385.891732	17225.105567	29.432295
386.076046	17243.480337	29.437312
386.570715	17238.619050	29.442330
386.489651	17244.185945	29.447348
387.112342	17241.690830	29.452365
387.692917	17249.296743	29.457383
387.949293	17254.189014	29.462400
388.655526	17254.164009	29.467418
388.696091	17250.170737	29.472436
388.957706	17250.213828	29.477453
389.238960	17245.816067	29.482471
389.479445	17250.709294	29.487488
389.617508	17260.139244	29.492506
389.831923	17281.071033	29.497524
389.881854	17290.053635	29.502541
390.441679	17309.978467	29.507559
389.905239	17330.663443	29.512576
390.664583	17350.823459	29.517594
390.400118	17381.740259	29.522612
390.471183	17416.740243	29.527629
391.173565	17452.825132	29.532647
391.271404	17490.478486	29.537664
391.680554	17528.781536	29.542682
392.111738	17574.451672	29.547700
392.399294	17620.407823	29.552717
393.166897	17655.242624	29.557735
393.124742	17691.996717	29.562752
393.638452	17735.506512	29.567770
394.294515	17778.200818	29.572788
394.599223	17803.116236	29.577805
395.014501	17852.526801	29.582823
394.972781	17890.473051	29.587840
395.514938	17934.730070	29.592858
396.195309	17982.597583	29.597876
396.702581	18014.887195	29.602893
397.386099	18054.290769	29.607911
397.505700	18099.732559	29.612928
398.291834	18119.506223	29.617946
398.559233	18163.915948	29.622964
398.709327	18198.353889	29.627981
399.635638	18228.035718	29.632999
400.034761	18264.901954	29.638016
400.360546	18293.716957	29.643034
400.926512	18327.252258	29.648052
401.261359	18361.481976	29.653069
402.269651	18379.976411	29.658087
401.976629	18413.376318	29.663104
402.773250	18433.972777	29.668122
402.985149	18460.604925	29.673140
403.306718	18484.703343	29.678157
403.980317	18500.288471	29.683175
404.775186	18534.054689	29.688192
404.972795	18552.087132	29.693210
405.290446	18578.425052	29.698228
405.782068	18603.607264	29.703245
406.167595	18618.495842	29.708263
406.343048	18653.429207	29.713280
406.916964	18672.490095	29.718298
407.286342	18692.708882	29.723316
407.505721	18734.572177	29.728333
407.762546	18749.957411	29.733351
408.036226	18779.326540	29.738368
408.444937	18799.853396	29.743386
409.026498	18837.602228	29.748404
409.480539	18859.848466	29.753421
410.254082	18877.195367	29.758439
410.389781	18914.324031	29.763456
410.882027	18927.475273	29.768474
411.362856	18949.282685	29.773492
411.309013	18960.514486	29.778509
411.571716	18996.028864	29.783527
411.901335	19023.401554	29.788544
412.220378	19045.806195	29.793562
413.037722	19085.117820	29.798580
413.252985	19112.856561	29.803597
413.610661	19138.481889	29.808615
413.744210	19181.962588	29.813632
414.243968	19214.628758	29.818650
414.829340	19257.141510	29.823668
414.624247	19286.959182	29.828685
415.313845	19327.176518	29.833703
415.574206	19372.428691	29.838720
416.221117	19401.374513	29.843738
416.024854	19451.775093	29.848756
416.384100	19497.884028	29.853773
417.281806	19534.047357	29.858791
417.581796	19576.693075	29.863808
418.139091	19604.339599	29.868826
418.963006	19649.194466	29.873844
419.316722	19687.638438	29.878861
420.119406	19720.825192	29.883879
419.953959	19768.373837	29.888896
420.160821	19802.065603	29.893914
421.065447	19843.841970	29.898932
421.124754	19878.779248	29.903949
421.832077	19913.811411	29.908967
422.279173	19959.002446	29.913984
422.807097	19995.361218	29.919002
423.247333	20028.101178	29.924020
423.422616	20068.270456	29.929037
424.197076	20107.205594	29.934055
424.409288	20134.656029	29.939072
425.179284	20169.247209	29.944090
425.596650	20200.830347	29.949108
425.659456	20241.587379	29.954125
426.290200	20269.168246	29.959143
427.010306	20300.932521	29.964160
427.197447	20336.114667	29.969178
427.710049	20368.546902	29.974196
428.106360	20405.487541	29.979213
428.459947	20433.049853	29.984231
428.882636	20474.495955	29.989248
429.466309	20499.925265	29.994266
429.849383	20530.372578	29.999284
430.347843	20562.631844	30.004301
431.024023	20584.400959	30.009319
431.263847	20623.148495	30.014336
431.391898	20645.962702	30.019354
431.901076	20675.580594	30.024372
432.447193	20700.494060	30.029389
433.122731	20733.135782	30.034407
433.327789	20759.095226	30.039424
433.728149	20771.400281	30.044442
434.201881	20791.120406	30.049460
434.503382	20824.130639	30.054477
435.605357	20839.422250	30.059495
435.924438	20864.948653	30.064512
436.133344	20888.174042	30.069530
436.643012	20917.075621	30.074548
436.785118	20948.252053	30.079565
437.504589	20965.008979	30.084583
437.506916	21005.384622	30.089600
437.838901	21031.747221	30.094618
438.002905	21056.922969	30.099636
438.229812	21095.496519	30.104653
439.580778	21120.229646	30.109671
439.706224	21158.740758	30.114688
439.814466	21185.641743	30.119706
440.731042	21221.258592	30.124724
441.111902	21247.082930	30.129741
441.712854	21284.093837	30.134759
442.038716	21312.337861	30.139776
442.696309	21336.420992	30.144794
443.070433	21363.813907	30.149812
443.087932	21399.116028	30.154829
443.633667	21427.769431	30.159847
444.062565	21461.737323	30.164864
444.484403	21500.228034	30.169882
445.006498	21530.119563	30.174900
445.092775	21571.777309	30.179917
445.854883	21604.303082	30.184935
446.176654	21642.468262	30.189952
446.654807	21685.209841	30.194970
447.023561	21711.491320	30.199988
447.504184	21743.083226	30.205005
448.311998	21782.354300	30.210023
449.294522	21805.236460	30.215040
449.635735	21826.929925	30.220058
450.551414	21850.420604	30.225076
450.807611	21873.685590	30.230093
451.378604	21895.621358	30.235111
451.474935	21918.349519	30.240128
451.720616	21935.310566	30.245146
452.368553	21951.860200	30.250164
452.877314	21991.501581	30.255181
453.161701	22009.123660	30.260199
453.848560	22040.219391	30.265216
454.262369	22060.040444	30.270234
454.212546	22084.925032	30.275252
454.437052	22122.242048	30.280269
454.977744	22153.666892	30.285287
455.228506	22191.975459	30.290304
455.355707	22233.413401	30.295322
455.984776	22257.575737	30.300340
456.345479	22304.127823	30.305357
456.355686	22342.453814	30.310375
457.007198	22386.979675	30.315392
457.228829	22420.013057	30.320410
457.505782	22453.854486	30.325428
457.711310	22506.963078	30.330445
458.250062	22546.292310	30.335463
458.788174	22599.566404	30.340480
458.937065	22656.332156	30.345498
459.915512	22697.251307	30.350516
460.094611	22757.670507	30.355533
460.506377	22799.767184	30.360551
461.490991	22846.805907	30.365568
461.724210	22906.153697	30.370586
462.302517	22947.971390	30.375604
462.729316	23001.280320	30.380621
463.608483	23041.314287	30.385639
463.976540	23069.962743	30.390656
464.124055	23109.056383	30.395674
464.729803	23158.117718	30.400692
465.355248	23206.374989	30.405709
465.825578	23249.342585	30.410727
466.240258	23297.557306	30.415744
466.600393	23348.722898	30.420762
467.157982	23375.631625	30.425780
467.692016	23428.349096	30.430797
468.390692	23461.429156	30.435815
468.850319	23507.658653	30.440832
469.314086	23547.000734	30.445850
470.293867	23569.338440	30.450868
470.806222	23609.206210	30.455885
471.108056	23640.612188	30.460903
471.645784	23680.343759	30.465920
472.163373	23727.116843	30.470938
472.743476	23757.018299	30.475956
472.766617	23788.111347	30.480973
473.068042	23824.468542	30.485991
473.589844	23863.631225	30.491008
474.110582	23908.116803	30.496026
474.650276	23947.978702	30.501044
475.202270	23987.125850	30.506061
475.451401	24033.529835	30.511079
476.132734	24068.857369	30.516096
476.403988	24100.896946	30.521114
476.923462	24148.550860	30.526132
477.625613	24182.003676	30.531149
477.893869	24221.679485	30.536167
478.608343	24269.216043	30.541184
478.350305	24313.005996	30.546202
479.151882	24347.197187	30.551220
479.734722	24391.535576	30.556237
479.952099	24432.931784	30.561255
480.721077	24476.987889	30.566272
480.777925	24528.682957	30.571290
481.596730	24560.272280	30.576308
481.900575	24605.354447	30.581325
482.268355	24642.537165	30.586343
482.949200	24685.455398	30.591360
482.958633	24732.380129	30.596378
483.776264	24769.476508	30.601396
484.302184	24816.061603	30.606413
484.434823	24858.580008	30.611431
485.099584	24900.555271	30.616448
485.476659	24959.504915	30.621466
485.688072	25002.538960	30.626484
486.731869	25041.761594	30.631501
487.350411	25079.638011	30.636519
488.494073	25104.123678	30.641536
489.229047	25125.632869	30.646554
490.378943	25146.256696	30.651572
490.719249	25175.055153	30.656589
491.171451	25199.911882	30.661607
491.923496	25223.384797	30.666624
492.060583	25238.169531	30.671642
492.792528	25263.680559	30.676660
493.161053	25274.449342	30.681677
493.732136	25295.299497	30.686695
494.242199	25312.833351	30.691712
494.513883	25337.484290	30.696730
495.129939	25352.613507	30.701748
495.088860	25387.713994	30.706765
495.275178	25410.712462	30.711783
496.250326	25445.928488	30.716800
496.250083	25482.184676	30.721818
496.635578	25517.925722	30.726836
496.920990	25548.356464	30.731853
497.160090	25584.074498	30.736871
497.719537	25632.470150	30.741888
498.045817	25681.314329	30.746906
498.495018	25720.025954	30.751924
499.031540	25771.650183	30.756941
499.445133	25816.737966	30.761959
500.076247	25858.522572	30.766976
500.656283	25906.638457	30.771994
501.133196	25947.251949	30.777012
501.247150	26006.371040	30.782029
501.797434	26050.139368	30.787047
502.400976	26093.551111	30.792064
503.092063	26147.687943	30.797082
503.810254	26197.840505	30.802100
504.693008	26234.105832	30.807117
504.575591	26287.231147	30.812135
505.421556	26320.537896	30.817152
505.405515	26374.552575	30.822170
506.065473	26421.499141	30.827188
506.552755	26463.117571	30.832205
506.845386	26517.870615	30.837223
507.827121	26562.398058	30.842240
508.617700	26601.173234	30.847258
509.370315	26637.531109	30.852276
510.044470	26664.852249	30.857293
510.239844	26698.885042	30.862311
510.809443	26725.806952	30.867328
511.263919	26749.799073	30.872346
511.868567	26782.950623	30.877364
511.831168	26814.945513	30.882381
512.587818	26855.724729	30.887399
513.324462	26894.687262	30.892416
513.129974	26936.651881	30.897434
513.688972	26977.183985	30.902452
514.325694	27019.232283	30.907469
514.725975	27069.116748	30.912487
515.380069	27109.572581	30.917504
515.611991	27157.459292	30.922522
515.978298	27203.823033	30.927540
516.390245	27251.492253	30.932557
516.903604	27296.304338	30.937575
517.819590	27345.393678	30.942592
518.150933	27397.155858	30.947610
519.178503	27442.824027	30.952628
519.630136	27482.911221	30.957645
519.832807	27528.778797	30.962663
520.390397	27567.780932	30.967680
520.919720	27622.422796	30.972698
521.579487	27673.490613	30.977716
522.063989	27715.087498	30.982733
522.176031	27764.780498	30.987751
523.150319	27802.846968	30.992768
523.432110	27865.433411	30.997786
524.156299	27911.003103	31.002804
524.740419	27950.011388	31.007821
525.200783	27992.351897	31.012839
526.261724	28040.079215	31.017856
526.618492	28086.111345	31.022874
527.367588	28120.547433	31.027892
527.794036	28162.372182	31.032909
528.114402	28208.558588	31.037927
529.034695	28241.973295	31.042944
529.311042	28288.724797	31.047962
529.677731	28326.537869	31.052980
530.334255	28378.263986	31.057997
530.649167	28420.360882	31.063015
531.024951	28469.741395	31.068032
531.761441	28521.463109	31.073050
531.952489	28557.158330	31.078068
532.440862	28600.986762	31.083085
532.991913	28658.635470	31.088103
533.828641	28696.333554	31.093120
534.142675	28749.666103	31.098138
534.259493	28807.595680	31.103156
535.127251	28866.282059	31.108173
535.500732	28916.083489	31.113191
536.021897	28965.259539	31.118208
536.679680	29022.545828	31.123226
537.150701	29067.350635	31.128244
537.560615	29120.062382	31.133261
537.622783	29166.228018	31.138279
538.831818	29208.543844	31.143296
539.219951	29262.123145	31.148314
539.440468	29320.564395	31.153332
540.326929	29363.948508	31.158349
540.712762	29419.166128	31.163367
541.048692	29464.075494	31.168384
541.707660	29522.696632	31.173402
542.474269	29575.857350	31.178420
542.949822	29624.955974	31.183437
543.113299	29681.437601	31.188455
543.821359	29734.308721	31.193472
544.642675	29788.049267	31.198490
544.850308	29844.392037	31.203508
545.656087	29887.067001	31.208525
545.987703	29952.132600	31.213543
546.872655	30002.820402	31.218560
547.305972	30062.157113	31.223578
548.004166	30115.177607	31.228596
548.511432	30165.711733	31.233613
549.154737	30223.398551	31.238631
549.665653	30272.737775	31.243648
550.358672	30332.382406	31.248666
550.866833	30385.284319	31.253684
551.534304	30424.920410	31.258701
551.733762	30478.831625	31.263719
552.530093	30532.797673	31.268736
552.853973	30583.032893	31.273754
553.871882	30628.311227	31.278772
554.707383	30674.258637	31.283789
554.543677	30731.941819	31.288807
555.600936	30773.255110	31.293824
556.315832	30811.548043	31.298842
556.813122	30863.649412	31.303860
557.713727	30905.571154	31.308877
558.110492	30957.293225	31.313895
558.816409	30998.083032	31.318912
559.644079	31045.437063	31.323930
560.025113	31087.618555	31.328948
560.751393	31119.210228	31.333965
560.978031	31167.821961	31.338983
561.378554	31206.448019	31.344000
561.894402	31255.190474	31.349018
562.382219	31296.948846	31.354036
563.222494	31328.948329	31.359053
564.061812	31378.479722	31.364071
564.474612	31422.010939	31.369088
565.022226	31467.156869	31.374106
565.219344	31513.521969	31.379124
565.881900	31561.338812	31.384141
565.900394	31610.645425	31.389159
566.609241	31664.375361	31.394176
567.110960	31709.828742	31.399194
567.484014	31754.243534	31.404212
567.882380	31798.023931	31.409229
568.461145	31855.964769	31.414247
569.092255	31904.463811	31.419264
569.640716	31955.777106	31.424282
569.713139	32018.589302	31.429300
570.542126	32064.674042	31.434317
571.058173	32121.211920	31.439335
571.649573	32179.817054	31.444352
571.903177	32241.395411	31.449370
572.379817	32311.276864	31.454388
572.991316	32362.934465	31.459405
573.685175	32423.358911	31.464423
575.086095	32472.236686	31.469440
575.969571	32523.613454	31.474458
576.658812	32571.274499	31.479476
577.285109	32614.762247	31.484493
577.835940	32665.013376	31.489511
578.056089	32711.141722	31.494528
578.879479	32750.331409	31.499546
579.199830	32799.839388	31.504564
579.767176	32847.957281	31.509581
580.714364	32885.704166	31.514599
581.641932	32918.564538	31.519616
582.558735	32955.994856	31.524634
582.998736	32991.179280	31.529652
583.482437	33033.116096	31.534669
584.011583	33075.452472	31.539687
584.742800	33110.283383	31.544704
585.797363	33144.310957	31.549722
585.913045	33187.976118	31.554740
586.371553	33232.237822	31.559757
586.960468	33274.930901	31.564775
587.494009	33311.250264	31.569792
587.696732	33354.747518	31.574810
588.134550	33403.158786	31.579828
589.061134	33449.956972	31.584845
589.516719	33510.413878	31.589863
589.700651	33555.178897	31.594880
590.604982	33597.371727	31.599898
590.896766	33655.582111	31.604916
591.592728	33709.259265	31.609933
591.685258	33765.751978	31.614951
592.016029	33817.455671	31.619968
592.693067	33888.066946	31.624986
593.286505	33959.201015	31.630004
594.037608	34023.347237	31.635021
594.702028	34080.319020	31.640039
595.319329	34138.810297	31.645056
596.162733	34189.895940	31.650074
596.594377	34251.418712	31.655092
597.146624	34303.362940	31.660109
597.564998	34359.643394	31.665127
598.455070	34424.763770	31.670144
599.446725	34472.648534	31.675162
599.596794	34522.983298	31.680180
600.080203	34575.973500	31.685197
600.662427	34628.903992	31.690215
600.958127	34676.890725	31.695232
601.661545	34733.581069	31.700250
601.969528	34802.538199	31.705268
602.458825	34849.714232	31.710285
603.282255	34913.819254	31.715303
603.663463	34973.878690	31.720320
604.660130	35038.349150	31.725338
605.197176	35109.052524	31.730356
605.625468	35160.243511	31.735373
605.831578	35225.868493	31.740391
606.854380	35287.255209	31.745408
607.858528	35358.366088	31.750426
608.216219	35428.721005	31.755444
608.829158	35490.214731	31.760461
609.506630	35548.559470	31.765479
610.114798	35603.685065	31.770496
610.896218	35656.684831	31.775514
611.891190	35714.533415	31.780532
612.256841	35765.427217	31.785549
613.028547	35825.124809	31.790567
613.093740	35894.618569	31.795584
614.098495	35949.423579	31.800602
614.339019	36014.883775	31.805620
615.545063	36072.725206	31.810637
616.027216	36142.557199	31.815655
616.761466	36194.101499	31.820672
617.620655	36240.661263	31.825690
617.519285	36304.617751	31.830708
618.485595	36363.297716	31.835725
619.210475	36432.770624	31.840743
619.538724	36490.267682	31.845760
620.552089	36543.856089	31.850778
620.662058	36611.698072	31.855796
621.363410	36671.069315	31.860813
621.917572	36741.311717	31.865831
622.749528	36795.167892	31.870848
623.377208	36856.085628	31.875866
623.715305	36927.131058	31.880884
624.345308	36993.195238	31.885901
624.939579	37063.301727	31.890919
625.690263	37129.612108	31.895936
626.531400	37189.388627	31.900954
627.064737	37262.767872	31.905972
627.838293	37312.379429	31.910989
628.410442	37380.155625	31.916007
628.675941	37448.644733	31.921024
629.616975	37501.834602	31.926042
630.713252	37559.200377	31.931060
631.191738	37614.269640	31.936077
631.687751	37678.044738	31.941095
632.120668	37747.730385	31.946112
633.003576	37802.429963	31.951130
633.583449	37867.199976	31.956148
633.791397	37920.224086	31.961165
634.978803	37966.996522	31.966183
635.432508	38015.101637	31.971200
636.255062	38058.595938	31.976218
636.794616	38113.959846	31.981236
637.488437	38157.042858	31.986253
638.129879	38205.881792	31.991271
638.398899	38272.164557	31.996288
639.467035	38322.794943	32.001306
639.860918	38382.383576	32.006324
640.337636	38439.567173	32.011341
640.565438	38499.026555	32.016359
641.476417	38562.626943	32.021376
642.605153	38617.364120	32.026394
643.030092	38681.258380	32.031412
643.826774	38738.664827	32.036429
644.599489	38791.562300	32.041447
645.005880	38852.639148	32.046464
645.817843	38896.190901	32.051482
646.170060	38963.264164	32.056500
646.547515	39022.412975	32.061517
647.446210	39087.988393	32.066535
648.125741	39155.905966	32.071552
648.751364	39216.422524	32.076570
649.040345	39302.609807	32.081588
649.562010	39356.706468	32.086605
650.534554	39417.449187	32.091623
650.862442	39480.575016	32.096640
652.038412	39549.865878	32.101658
652.789088	39622.003316	32.106676
653.697814	39675.542616	32.111693
654.068474	39738.836053	32.116711
654.734716	39800.341695	32.121728
655.643019	39858.872709	32.126746
656.157666	39924.881513	32.131764
656.694347	39989.060927	32.136781
657.551889	40045.332975	32.141799
658.087212	40109.724373	32.146816
658.817310	40175.356053	32.151834
659.627047	40236.644869	32.156852
660.107422	40301.398987	32.161869
660.902225	40350.680138	32.166887
661.495014	40418.971374	32.171904
662.152307	40475.535356	32.176922
662.892987	40541.876416	32.181940
663.418838	40605.186193	32.186957
664.665270	40654.513005	32.191975
665.414905	40694.933095	32.196992
666.420872	40749.767646	32.202010
667.273897	40803.702576	32.207028
667.686435	40840.114209	32.212045
668.533725	40889.757587	32.217063
668.743922	40952.466008	32.222080
669.509198	40995.830273	32.227098
669.871758	41043.627261	32.232116
670.407665	41095.459326	32.237133
671.060221	41130.808257	32.242151
671.277408	41203.351150	32.247168
671.828062	41251.408948	32.252186
672.381850	41311.430226	32.257204
672.934815	41367.751966	32.262221
673.643737	41434.662984	32.267239
674.158089	41492.571542	32.272256
674.942909	41552.162594	32.277274
675.541934	41621.009612	32.282292
675.617588	41697.008941	32.287309
676.814070	41767.745442	32.292327
677.037422	41843.958470	32.297344
677.840724	41920.745047	32.302362
678.525489	41996.456293	32.307380
679.044306	42073.620053	32.312397
679.833277	42148.006324	32.317415
680.396616	42240.020706	32.322432
680.894279	42302.839675	32.327450
681.575424	42390.867901	32.332468
682.166973	42479.137959	32.337485
683.334644	42554.017700	32.342503
684.090575	42633.335369	32.347520
684.661706	42704.910271	32.352538
685.778928	42778.294347	32.357556
686.295411	42855.947755	32.362573
686.717038	42936.234840	32.367591
687.343332	43020.167859	32.372608
688.473242	43094.784667	32.377626
689.246421	43171.531125	32.382644
689.885178	43249.595843	32.387661
690.483230	43313.840968	32.392679
691.082755	43395.663358	32.397696
691.519860	43476.660257	32.402714
692.297848	43551.719927	32.407732
693.278031	43641.615425	32.412749
694.218734	43702.226941	32.417767
694.598146	43792.679453	32.422784
695.250685	43870.946666	32.427802
696.211970	43949.284950	32.432820
696.662231	44022.755251	32.437837
697.582165	44101.258538	32.442855
698.347749	44172.890552	32.447872
698.834685	44245.885903	32.452890
699.580836	44329.026941	32.457908
700.193578	44402.649639	32.462925
700.865800	44481.465388	32.467943
701.519885	44571.057966	32.472960
702.334436	44643.422337	32.477978
703.328186	44725.260766	32.482996
703.909065	44804.486870	32.488013
705.000930	44865.800825	32.493031
705.701370	44941.512955	32.498048
706.627276	45001.784318	32.503066
707.021637	45072.744051	32.508084
707.620463	45143.371802	32.513101
708.770961	45197.594869	32.518119
709.245980	45259.620471	32.523136
710.020759	45331.047552	32.528154
710.382229	45384.396716	32.533172
710.678549	45460.330025	32.538189
711.921629	45524.720374	32.543207
712.162220	45590.400052	32.548224
713.091383	45655.093259	32.553242
713.771019	45734.544472	32.558260
714.394466	45807.530916	32.563277
715.160101	45878.005715	32.568295
715.564701	45951.447219	32.573312
716.449442	46024.683228	32.578330
717.200933	46100.515285	32.583348
718.528330	46158.568650	32.588365
720.046924	46209.824123	32.593383
720.901375	46268.341227	32.598400
721.586218	46317.685262	32.603418
722.174246	46378.163449	32.608436
722.724031	46447.072105	32.613453
723.581990	46494.111076	32.618471
724.146087	46567.962015	32.623488
724.355698	46632.337978	32.628506
725.196577	46694.130555	32.633524
725.755047	46763.518651	32.638541
726.846596	46820.024703	32.643559
727.257592	46893.118893	32.648576
727.687144	46966.576436	32.653594
728.487113	47036.532958	32.658612
728.864145	47122.099807	32.663629
729.809442	47196.580530	32.668647
730.131953	47279.954456	32.673664
730.727904	47361.919002	32.678682
731.384539	47451.607906	32.683700
732.201833	47532.493598	32.688717
733.174189	47605.633885	32.693735
733.748817	47690.215959	32.698752
734.383105	47781.598202	32.703770
735.297152	47871.301892	32.708788
735.730970	47957.529522	32.713805
736.882440	48030.475814	32.718823
737.831559	48126.498643	32.723840
738.158207	48209.210487	32.728858
739.054762	48279.648798	32.733876
739.406452	48374.569012	32.738893
740.066869	48464.789403	32.743911
740.406795	48562.681801	32.748928
741.310422	48654.003567	32.753946
742.326605	48744.424335	32.758964
743.205842	48846.101112	32.763981
743.606657	48926.661868	32.768999
744.461237	49031.660126	32.774016
745.185014	49109.503827	32.779034
746.075448	49205.390358	32.784052
746.487051	49291.908842	32.789069
747.294166	49367.941697	32.794087
748.394802	49462.969371	32.799104
748.951667	49540.525961	32.804122
749.777112	49624.099044	32.809140
750.338768	49723.505644	32.814157
751.119228	49799.099626	32.819175
752.018922	49889.071389	32.824192
752.211977	49983.567838	32.829210
753.029028	50066.891868	32.834228
753.777242	50161.032632	32.839245
754.969139	50250.372720	32.844263
755.720852	50337.372290	32.849280
756.471962	50420.339233	32.854298
757.860861	50509.665033	32.859316
758.682947	50590.989898	32.864333
759.705991	50660.088864	32.869351
760.459543	50736.915567	32.874368
761.397605	50820.249085	32.879386
762.490383	50885.269869	32.884404
763.251965	50964.816663	32.889421
763.996830	51022.641025	32.894439
764.938198	51091.716787	32.899456
765.864210	51153.110509	32.904474
766.967161	51217.016825	32.909492
767.371856	51290.584515	32.914509
768.132218	51342.922353	32.919527
769.111919	51415.266016	32.924544
769.335928	51482.727991	32.929562
770.174300	51545.064872	32.934580
771.056359	51619.858195	32.939597
771.873700	51675.066235	32.944615
772.690174	51760.080392	32.949632
773.469919	51822.730550	32.954650
774.271361	51889.666588	32.959668
774.759675	51966.616514	32.964685
775.614023	52027.715333	32.969703
776.374904	52091.107956	32.974720
777.091852	52168.435798	32.979738
778.372854	52238.282491	32.984756
778.828911	52301.588663	32.989773
779.881504	52368.890487	32.994791
780.431642	52433.946443	32.999808
781.217162	52505.258607	33.004826
781.929082	52576.623798	33.009844
782.202689	52662.486109	33.014861
782.747475	52731.950069	33.019879
783.424606	52812.070797	33.024896
784.018518	52905.578195	33.029914
784.805662	52988.087258	33.034932
785.390152	53077.301352	33.039949
786.226328	53170.377013	33.044967
786.635363	53265.957827	33.049984
787.328513	53354.663600	33.055002
788.792154	53439.636288	33.060020
789.267360	53522.913930	33.065037
789.954239	53616.189241	33.070055
790.648102	53682.167397	33.075072
791.371757	53768.660857	33.080090
792.656867	53840.555277	33.085108
793.049273	53934.115824	33.090125
793.894321	54011.352221	33.095143
794.743451	54104.089703	33.100160
795.348125	54201.194109	33.105178
796.259716	54285.396907	33.110196
796.639258	54378.649287	33.115213
797.480151	54472.128575	33.120231
798.706925	54551.370869	33.125248
799.149535	54652.509127	33.130266
800.350515	54736.794206	33.135284
801.409006	54831.358124	33.140301
802.441767	54912.274296	33.145319
803.434478	54997.521773	33.150336
803.970918	55078.539781	33.155354
805.173478	55161.737530	33.160372
805.727111	55236.538057	33.165389
806.503048	55323.232584	33.170407
807.165329	55405.614632	33.175424
807.720056	55502.307739	33.180442
808.849531	55590.377244	33.185460
809.557152	55678.410148	33.190477
810.040257	55772.145586	33.195495
810.702782	55861.000985	33.200512
811.158682	55955.082616	33.205530
812.740313	56051.864544	33.210548
813.388892	56143.290008	33.215565
813.911983	56243.982270	33.220583
815.033938	56331.762940	33.225600
815.715402	56441.519647	33.230618
816.480592	56534.683711	33.235636
817.471392	56631.670068	33.240653
818.409367	56725.082242	33.245671
819.129252	56820.016519	33.250688
819.759454	56926.949344	33.255706
820.908354	57008.673916	33.260724
821.617260	57115.929947	33.265741
822.071853	57216.392167	33.270759
823.212573	57300.013531	33.275776
823.784163	57412.776875	33.280794
824.714518	57513.471213	33.285812
825.400010	57609.156920	33.290829
826.154727	57708.989983	33.295847
827.285692	57814.263370	33.300864
827.564505	57923.385764	33.305882
828.601977	58021.656928	33.310900
829.306674	58125.446615	33.315917
830.218325	58239.057483	33.320935
831.681520	58335.996523	33.325952
832.846609	58424.335927	33.330970
833.960323	58505.659111	33.335988
834.875262	58573.450815	33.341005
835.601514	58652.692552	33.346023
836.426724	58730.071880	33.351040
836.840727	58814.062002	33.356058
837.536081	58894.910425	33.361076
838.270755	58973.186054	33.366093
839.113179	59069.738342	33.371111
840.260422	59149.906584	33.376128
840.367523	59246.649441	33.381146
841.093009	59332.057325	33.386164
841.987860	59429.746094	33.391181
842.677198	59533.385039	33.396199
843.717500	59636.233021	33.401216
844.409092	59742.048218	33.406234
845.444704	59834.677442	33.411252
846.422211	59940.388263	33.416269
847.231112	60033.913385	33.421287
848.431830	60119.296587	33.426304
849.023969	60217.842807	33.431322
850.196143	60315.520477	33.436340
850.857328	60398.066951	33.441357
851.851826	60501.024853	33.446375
852.893138	60596.883959	33.451392
853.399704	60699.339612	33.456410
853.961236	60787.912553	33.461428
854.881285	60889.700330	33.466445
855.768202	60995.226261	33.471463
856.581480	61101.424453	33.476480
857.594654	61206.517819	33.481498
858.794316	61297.988231	33.486516
859.988240	61388.256914	33.491533
860.950290	61467.990889	33.496551
862.439291	61548.680229	33.501568
863.438583	61629.643634	33.506586
864.512894	61710.352300	33.511604
865.273996	61783.532507	33.516621
865.805729	61881.399174	33.521639
866.766282	61949.836863	33.526656
867.596434	62027.478468	33.531674
868.308980	62106.711706	33.536692
869.076926	62198.681498	33.541709
869.727154	62288.690495	33.546727
870.528311	62368.157037	33.551744
870.856793	62479.041139	33.556762
872.019053	62571.600510	33.561780
872.817271	62667.316187	33.566797
873.461065	62767.724349	33.571815
874.204661	62863.174965	33.576832
874.869754	62966.647159	33.581850
875.782603	63059.131754	33.586868
876.517360	63171.714233	33.591885
877.432904	63279.345253	33.596903
878.506366	63381.974682	33.601920
878.844741	63503.935258	33.606938
879.832814	63596.521024	33.611956
880.815040	63696.738110	33.616973
881.445205	63806.707137	33.621991
882.377236	63905.527951	33.627008
883.175190	64010.424767	33.632026
883.873886	64117.599196	33.637044
884.829652	64217.671635	33.642061
885.733191	64319.417276	33.647079
886.618732	64418.693445	33.652096
887.186328	64542.320117	33.657114
887.921668	64653.508979	33.662132
888.907916	64778.100134	33.667149
889.763461	64893.730732	33.672167
890.685997	65006.414141	33.677184
891.401227	65130.750675	33.682202
891.879445	65257.200763	33.687220
893.020513	65382.791345	33.692237
893.953812	65510.816186	33.697255
894.918046	65632.889673	33.702272
896.025881	65748.134673	33.707290
897.329981	65855.478287	33.712308
898.916439	65953.412732	33.717325
899.867014	66072.067405	33.722343
901.469871	66158.838225	33.727360
902.757910	66259.610666	33.732378
904.092517	66341.292420	33.737396
905.106901	66429.652088	33.742413
906.308054	66498.481553	33.747431
907.685765	66558.300226	33.752448
908.723471	66639.259802	33.757466
909.557092	66708.976050	33.762484
910.335342	66772.712668	33.767501
910.898990	66853.527477	33.772519
911.643861	66934.996045	33.777536
912.286500	67018.256377	33.782554
913.366671	67093.203375	33.787572
914.123625	67176.844185	33.792589
914.366838	67273.309196	33.797607
915.483225	67356.021787	33.802624
915.991733	67454.087995	33.807642
916.581721	67556.406003	33.812660
917.303088	67660.523075	33.817677
918.153366	67765.839470	33.822695
919.115923	67870.904818	33.827712
919.847134	67991.125512	33.832730
920.618511	68094.510423	33.837748
921.689719	68207.324645	33.842765
922.233057	68330.774059	33.847783
923.193101	68434.737248	33.852800
924.322882	68558.650742	33.857818
925.064565	68668.632846	33.862836
926.138484	68778.019367	33.867853
926.931801	68895.961324	33.872871
928.032920	68997.017787	33.877888
928.530063	69124.169211	33.882906
929.579630	69225.860533	33.887924
930.767416	69331.415968	33.892941
931.640936	69443.820197	33.897959
932.528202	69542.228328	33.902976
933.470782	69653.555013	33.907994
933.920464	69764.613261	33.913012
934.764924	69875.824136	33.918029
936.151661	69988.156132	33.923047
937.108007	70090.448041	33.928064
937.915368	70208.300868	33.933082
938.354330	70319.509269	33.938100
939.802344	70441.362145	33.943117
939.993289	70567.510126	33.948135
940.792013	70676.780407	33.953152
942.000936	70818.677859	33.958170
942.844989	70952.913139	33.963188
944.155489	71062.464276	33.968205
945.156386	71199.658636	33.973223
946.023217	71324.219018	33.978240
947.002694	71450.487261	33.983258
947.820209	71569.799882	33.988276
949.038281	71696.082273	33.993293
949.804318	71825.205031	33.998311
951.260681	71947.634546	34.003328
952.549600	72067.077349	34.008346
953.201862	72188.176627	34.013364
954.282379	72313.985636	34.018381
954.698870	72440.735203	34.023399
955.782020	72558.855111	34.028416
957.201873	72679.039037	34.033434
958.845719	72782.322329	34.038452
960.081147	72888.053459	34.043469
961.101290	73003.108600	34.048487
962.245040	73101.430409	34.053504
963.145596	73216.006585	34.058522
964.027222	73318.345976	34.063540
964.527799	73423.792428	34.068557
965.565250	73539.966421	34.073575
966.679944	73654.466798	34.078592
967.116076	73768.273227	34.083610
967.965476	73890.956582	34.088628
969.384774	74002.269707	34.093645
969.910781	74121.315337	34.098663
971.059491	74246.354663	34.103680
971.931781	74372.228698	34.108698
972.662864	74496.862056	34.113716
974.021768	74615.417868	34.118733
974.699322	74738.689865	34.123751
975.740952	74853.625797	34.128768
976.973782	74969.751685	34.133786
977.796850	75100.188351	34.138804
978.587281	75211.241664	34.143821
979.078681	75346.194518	34.148839
980.207678	75464.640219	34.153856
981.631161	75573.547136	34.158874
982.279279	75701.171515	34.163892
983.264435	75814.320684	34.168909
983.923612	75933.886688	34.173927
984.513460	76055.543751	34.178944
985.941696	76170.969186	34.183962
986.656294	76299.623257	34.188980
988.211092	76412.501844	34.193997
988.846052	76541.511408	34.199015
989.577380	76673.375885	34.204032
990.784544	76787.664413	34.209050
991.541781	76924.329870	34.214068
992.957109	77047.650203	34.219085
993.763053	77167.604609	34.224103
994.588287	77304.862239	34.229120
995.438708	77434.361449	34.234138
996.289885	77572.027581	34.239156
997.588275	77700.787223	34.244173
998.126927	77844.914046	34.249191
999.383124	77981.184824	34.254208
1000.358221	78121.571809	34.259226
1001.141171	78264.657709	34.264244
1002.218565	78409.492886	34.269261
1003.450325	78548.735804	34.274279
1004.820261	78683.349711	34.279296
1006.048241	78810.370291	34.284314
1007.096787	78953.696851	34.289332
1008.058251	79076.374676	34.294349
1009.123998	79218.480373	34.299367
1010.039440	79353.841003	34.304384
1011.319923	79475.212536	34.309402
1012.077249	79615.669631	34.314420
1013.268840	79737.758504	34.319437
1014.338198	79878.806192	34.324455
1015.422760	80008.619372	34.329472
1016.072980	80145.133607	34.334490
1016.617263	80283.347093	34.339508
1018.043353	80421.819469	34.344525
1018.810938	80574.715777	34.349543
1019.792254	80717.711235	34.354560
1020.970686	80856.131079	34.359578
1021.914746	81006.587628	34.364596
1022.830106	81148.427029	34.369613
1024.136249	81286.962173	34.374631
1025.310033	81425.664695	34.379648
1026.965278	81556.465128	34.384666
1028.081420	81688.237203	34.389684
1029.581054	81802.342612	34.394701
1030.685774	81927.258755	34.399719
1031.634124	82048.375725	34.404736
1033.222718	82171.085843	34.409754
1034.064938	82289.230779	34.414772
1035.182399	82399.866221	34.419789
1036.013091	82519.986778	34.424807
1036.956474	82636.903732	34.429824
1038.162118	82739.308144	34.434842
1038.658043	82849.191331	34.439860
1040.040231	82949.703632	34.444877
1040.754680	83069.156692	34.449895
1041.349500	83184.342932	34.454912
1042.425914	83296.462720	34.459930
1043.204476	83428.008586	34.464948
1043.987658	83544.494527	34.469965
1044.850216	83680.340494	34.474983
1045.906101	83819.267250	34.480000
1047.198821	83937.558408	34.485018
1047.635499	84077.698127	34.490036
1048.687657	84203.072389	34.495053
1049.634046	84345.371001	34.500071
1050.501889	84487.543962	34.505088
1052.017697	84623.475418	34.510106
1052.701459	84777.123763	34.515124
1053.892186	84912.293139	34.520141
1054.949818	85051.796741	34.525159
1055.973877	85194.398501	34.530176
1057.428836	85338.848526	34.535194
1058.161411	85492.437357	34.540212
1059.536534	85625.703996	34.545229
1060.896570	85768.199240	34.550247
1061.570948	85910.703331	34.555264
1063.169804	86037.683385	34.560282
1064.420424	86185.282634	34.565300
1065.535929	86325.367083	34.570317
1066.295961	86462.878505	34.575335
1067.475731	86605.540785	34.580352
1068.719233	86737.924727	34.585370
1069.509355	86881.390652	34.590388
1070.616463	87015.650759	34.595405
1071.930617	87168.267477	34.600423
1072.939772	87311.948047	34.605440
1073.970058	87447.209534	34.610458
1074.592420	87587.956092	34.615476
1075.779576	87740.653974	34.620493
1076.591731	87880.600761	34.625511
1077.797787	88032.001336	34.630528
1078.924890	88177.667204	34.635546
1079.661837	88335.392419	34.640564
1080.881931	88486.673785	34.645581
1082.545685	88633.635963	34.650599
1083.218785	88780.130637	34.655616
1084.759016	88915.048252	34.660634
1085.963129	89062.067468	34.665652
1087.379001	89194.274609	34.670669
1088.355045	89343.007881	34.675687
1089.341230	89481.976039	34.680704
1090.899134	89611.955991	34.685722
1091.914041	89755.854204	34.690740
1092.949898	89886.646115	34.695757
1094.591107	90020.833550	34.700775
1095.331762	90154.469366	34.705792
1096.782374	90278.898593	34.710810
1097.087427	90398.400591	34.715828
1098.351133	90526.080084	34.720845
1099.249411	90654.963179	34.725863
1100.121783	90786.482160	34.730880
1101.123904	90912.624372	34.735898
1102.032223	91043.709102	34.740916
1103.352758	91165.444461	34.745933
1104.473966	91293.087830	34.750951
1105.404960	91428.965361	34.755968
1106.677541	91568.160500	34.760986
1107.480775	91705.805691	34.766004
1108.496430	91847.541753	34.771021
1109.519325	91982.668067	34.776039
1110.733440	92123.596373	34.781056
1112.445544	92253.162639	34.786074
1113.367082	92404.701957	34.791092
1114.079981	92547.667104	34.796109
1115.414187	92679.927188	34.801127
1116.109206	92840.689531	34.806144
1117.296036	92986.428433	34.811162
1118.307917	93147.667587	34.816180
1119.150539	93302.122521	34.821197
1120.325690	93457.531362	34.826215
1121.169499	93610.830714	34.831232
1122.933156	93765.572497	34.836250
1124.219970	93923.218661	34.841268
1125.333239	94066.907904	34.846285
1127.073609	94206.108429	34.851303
1128.008642	94372.144407	34.856320
1129.261858	94515.580227	34.861338
1130.044569	94659.718031	34.866356
1131.356351	94813.798828	34.871373
1132.711527	94958.037272	34.876391
1133.152919	95115.775666	34.881408
1134.687593	95266.262705	34.886426
1135.634780	95422.050362	34.891444
1136.762629	95578.582121	34.896461
1137.953690	95728.772644	34.901479
1138.608163	95885.356509	34.906496
1139.861795	96051.303586	34.911514
1141.007903	96217.490392	34.916532
1142.637801	96372.265065	34.921549
1144.719173	96500.652164	34.926567
1145.975512	96642.721911	34.931584
1148.039909	96774.554715	34.936602
1148.861910	96902.821736	34.941620
1149.960484	97041.173913	34.946637
1151.360217	97161.063051	34.951655
1152.174986	97304.048556	34.956672
1153.598199	97422.556186	34.961690
1154.571265	97560.475975	34.966708
1155.376394	97686.428281	34.971725
1156.376770	97819.012059	34.976743
1157.292592	97973.518940	34.981760
1158.382624	98092.633444	34.986778
1159.524010	98227.114122	34.991796
1160.571429	98356.789608	34.996813
1161.380211	98483.479611	35.001831
1162.734854	98620.952851	35.006848
1163.830811	98744.827514	35.011866
1164.780229	98895.722673	35.016884
1166.108968	99024.053865	35.021901
1167.090023	99165.550384	35.026919
1167.330022	99313.745626	35.031936
1168.728858	99465.104508	35.036954
1169.601417	99624.437864	35.041972
1170.589837	99788.359995	35.046989
1171.844443	99931.595611	35.052007
1172.961239	100106.008899	35.057024
1174.304531	100260.874409	35.062042
1175.547504	100428.626507	35.067060
1177.021249	100593.964061	35.072077
1177.843654	100733.103677	35.077095
1178.868496	100912.757687	35.082112
1180.319922	101071.597650	35.087130
1181.602619	101231.433628	35.092148
1182.931282	101393.079385	35.097165
1184.603021	101544.927291	35.102183
1185.894724	101702.366925	35.107200
1187.130987	101846.920735	35.112218
1188.334214	102014.836104	35.117236
1189.498230	102167.635680	35.122253
1190.783324	102320.258805	35.127271
1192.054982	102479.592519	35.132288
1193.618910	102634.078012	35.137306
1194.866297	102778.047304	35.142324
1196.237012	102929.623001	35.147341
1197.327867	103066.031776	35.152359
1198.575411	103217.274545	35.157376
1199.737374	103357.179404	35.162394
1200.764823	103504.592585	35.167412
1201.968182	103661.951814	35.172429
1203.441094	103819.092040	35.177447
1204.185182	103977.146550	35.182464
1205.837917	104114.731345	35.187482
1207.349881	104259.990199	35.192500
1208.497784	104410.762834	35.197517
1209.635406	104550.412823	35.202535
1210.642066	104705.842137	35.207552
1211.638764	104839.099243	35.212570
1212.581015	105005.159847	35.217588
1213.879681	105168.652517	35.222605
1215.200920	105320.333638	35.227623
1216.038870	105489.135467	35.232640
1217.039120	105645.660437	35.237658
1218.236913	105811.698668	35.242676
1219.038625	105984.490488	35.247693
1220.680167	106146.789822	35.252711
1221.734389	106322.258965	35.257728
1222.952493	106486.798706	35.262746
1224.234050	106653.392704	35.267764
1225.228733	106801.059296	35.272781
1226.554072	106945.471755	35.277799
1227.491623	107120.699445	35.282816
1228.349112	107275.567867	35.287834
1229.676322	107437.704359	35.292852
1230.887691	107601.385680	35.297869
1231.972855	107772.366745	35.302887
1233.344032	107954.322747	35.307904
1234.353720	108112.305289	35.312922
1235.660391	108298.824882	35.317940
1236.341994	108481.027379	35.322957
1238.309995	108650.545084	35.327975
1239.391304	108830.578944	35.332992
1240.544469	109003.671889	35.338010
1241.726633	109177.590620	35.343028
1243.022982	109371.171178	35.348045
1244.455668	109543.400649	35.353063
1245.735912	109723.517052	35.358080
1246.884649	109897.819661	35.363098
1248.261009	110089.582858	35.368116
1249.052406	110277.079291	35.373133
1250.544174	110463.066892	35.378151
1251.921272	110647.561274	35.383168
1253.059827	110843.596542	35.388186
1254.537803	111029.426023	35.393204
1255.627965	111222.996947	35.398221
1256.985475	111399.967256	35.403239
1258.281307	111595.204861	35.408256
1259.793213	111790.010843	35.413274
1261.120554	111980.441823	35.418292
1262.213215	112161.618654	35.423309
1263.571960	112356.719294	35.428327
1264.779967	112553.985106	35.433344
1266.298243	112733.047363	35.438362
1267.723660	112917.329347	35.443380
1268.876187	113104.238939	35.448397
1270.269568	113286.135776	35.453415
1271.626987	113467.222995	35.458432
1272.881232	113657.336505	35.463450
1274.065095	113858.383182	35.468468
1275.277872	114038.016107	35.473485
1277.048019	114218.574638	35.478503
1278.330517	114402.022899	35.483520
1279.659377	114575.544552	35.488538
1281.574583	114748.391731	35.493556
1283.109035	114913.830024	35.498573
1284.781697	115072.549171	35.503591
1286.293475	115234.479427	35.508608
1287.436970	115392.448993	35.513626
1289.189520	115534.032616	35.518644
1290.590611	115698.382938	35.523661
1292.200588	115844.676051	35.528679
1293.361704	115975.409431	35.533696
1294.534712	116124.198492	35.538714
1296.137864	116239.876740	35.543732
1296.865418	116379.747597	35.548749
1298.200608	116509.164434	35.553767
1299.265334	116643.031605	35.558784
1300.348596	116778.669342	35.563802
1301.541694	116917.639705	35.568820
1302.720849	117062.830614	35.573837
1303.871297	117196.820009	35.578855
1304.949408	117356.489968	35.583872
1305.597785	117518.793551	35.588890
1307.525036	117662.798873	35.593908
1308.520156	117818.312299	35.598925
1309.603881	117984.462614	35.603943
1310.654600	118152.759396	35.608960
1311.937288	118314.694875	35.613978
1313.091043	118486.086382	35.618996
1314.333185	118662.859781	35.624013
1315.473585	118840.840968	35.629031
1316.851385	119022.280913	35.634048
1318.269872	119194.952073	35.639066
1319.306460	119384.775449	35.644084
1320.700609	119574.467382	35.649101
1322.088448	119757.576203	35.654119
1323.543455	119938.434013	35.659136
1324.513413	120126.677638	35.664154
1326.063257	120313.133369	35.669172
1327.475483	120504.158951	35.674189
1329.197786	120671.896630	35.679207
1330.617722	120858.136246	35.684224
1331.719668	121052.330700	35.689242
1333.310909	121234.036992	35.694260
1334.694529	121418.158594	35.699277
1335.948754	121593.752975	35.704295
1337.307140	121780.705469	35.709312
1338.790740	121963.915732	35.714330
1340.390751	122148.020676	35.719348
1341.522559	122338.154167	35.724365
1342.819814	122514.583731	35.729383
1344.091251	122695.945567	35.734400
1345.235141	122886.486355	35.739418
1346.637077	123074.783603	35.744436
1348.125977	123244.537885	35.749453
1349.881225	123436.809334	35.754471
1351.561699	123603.710890	35.759488
1352.757039	123781.089645	35.764506
1354.309144	123963.416096	35.769524
1354.920937	124144.259262	35.774541
1356.607182	124328.023509	35.779559
1358.290197	124499.920857	35.784576
1359.396653	124697.624440	35.789594
1360.739786	124878.229612	35.794612
1362.145770	125059.421344	35.799629
1363.339112	125240.610085	35.804647
1364.972876	125428.798272	35.809664
1365.857315	125612.153993	35.814682
1367.709067	125774.291550	35.819700
1368.881537	125944.265110	35.824717
1369.796116	126124.921348	35.829735
1371.199907	126291.554110	35.834752
1372.361671	126464.116777	35.839770
1373.761984	126634.818476	35.844788
1374.728531	126810.821953	35.849805
1376.153698	127008.605660	35.854823
1377.572260	127188.428740	35.859840
1378.689482	127383.781179	35.864858
1380.438031	127552.647049	35.869876
1381.929795	127739.834918	35.874893
1383.440055	127932.620482	35.879911
1385.514208	128097.865496	35.884928
1387.043499	128278.058133	35.889946
1388.451815	128453.064420	35.894964
1389.775451	128640.677829	35.899981
1391.039970	128815.848610	35.904999
1392.358813	129003.300535	35.910016
1393.254181	129197.788878	35.915034
1394.576737	129369.698030	35.920052
1395.915824	129568.223159	35.925069
1396.702684	129761.035020	35.930087
1398.328234	129957.363639	35.935104
1399.391963	130174.953259	35.940122
1400.965204	130381.529930	35.945140
1402.105622	130587.492753	35.950157
1403.621686	130797.375620	35.955175
1405.127467	131001.712381	35.960192
1406.431666	131214.077258	35.965210
1407.915682	131420.954455	35.970228
1409.086394	131647.077888	35.975245
1410.551151	131852.073472	35.980263
1411.821341	132070.633136	35.985280
1413.446424	132295.979995	35.990298
1415.186539	132506.372055	35.995316
1416.546810	132728.533485	36.000333
1418.093635	132949.336592	36.005351
1419.416802	133161.180816	36.010368
1420.683082	133379.586394	36.015386
1422.432311	133581.926348	36.020404
1424.221359	133800.518135	36.025421
1425.889000	134008.309862	36.030439
1427.767822	134199.863242	36.035456
1428.741949	134407.996133	36.040474
1430.846558	134606.029296	36.045492
1432.383748	134811.211908	36.050509
1433.940605	134993.470272	36.055527
1435.298187	135184.555455	36.060544
1436.486473	135383.221051	36.065562
1438.246322	135575.410660	36.070580
1439.620607	135771.134861	36.075597
1440.760287	135978.783826	36.080615
1442.250294	136164.152057	36.085632
1443.292018	136361.542384	36.090650
1444.550296	136553.868811	36.095668
1445.981563	136738.679761	36.100685
1447.068481	136938.601210	36.105703
1448.643079	137129.119688	36.110720
1449.633216	137326.955542	36.115738
1451.062876	137525.495899	36.120756
1452.115294	137731.701080	36.125773
1453.358323	137939.803651	36.130791
1454.818122	138150.635896	36.135808
1455.882220	138368.451890	36.140826
1457.358276	138596.405737	36.145844
1458.767914	138814.841750	36.150861
1460.536740	139043.715640	36.155879
1461.662120	139257.777129	36.160896
1462.982761	139487.878892	36.165914
1464.954918	139718.778704	36.170932
1466.132230	139948.843401	36.175949
1467.582199	140181.654723	36.180967
1469.278394	140413.072627	36.185984
1470.549778	140647.588844	36.191002
1472.161241	140881.076946	36.196020
1473.556711	141125.602204	36.201037
1475.286167	141359.049883	36.206055
1476.698701	141590.851363	36.211072
1477.858258	141835.546543	36.216090
1479.614301	142081.099482	36.221108
1481.639844	142310.590995	36.226125
1483.249155	142537.602766	36.231143
1485.244344	142762.121361	36.236160
1486.901843	142984.058896	36.241178
1488.539786	143205.151918	36.246196
1490.931152	143416.050223	36.251213
1492.438363	143618.623520	36.256231
1494.312107	143807.577527	36.261248
1495.845872	144026.018516	36.266266
1497.561914	144219.246279	36.271284
1499.455676	144402.268692	36.276301
1500.970257	144588.229749	36.281319
1502.803190	144777.563722	36.286336
1503.950795	144969.149902	36.291354
1505.907619	145141.455760	36.296372
1507.708265	145329.378528	36.301389
1509.065601	145520.846026	36.306407
1510.984439	145686.062460	36.311424
1512.481794	145854.743879	36.316442
1514.246072	146017.578180	36.321460
1515.826447	146180.721414	36.326477
1517.047376	146360.414260	36.331495
1518.538156	146538.544108	36.336512
1519.805340	146711.094884	36.341530
1520.998664	146885.965430	36.346548
1521.989085	147074.331540	36.351565
1522.806896	147258.935911	36.356583
1524.288936	147447.302178	36.361600
1525.231200	147658.852183	36.366618
1526.904176	147848.191935	36.371636
1528.310624	148027.852036	36.376653
1529.230077	148236.645933	36.381671
1530.611839	148424.476093	36.386688
1531.718102	148623.050540	36.391706
1533.126156	148837.107740	36.396724
1534.386880	149056.425453	36.401741
1535.835147	149276.247303	36.406759
1537.063832	149496.815462	36.411776
1538.511704	149727.251403	36.416794
1540.061085	149949.660629	36.421812
1541.917167	150170.818273	36.426829
1543.576400	150412.470555	36.431847
1545.143633	150635.959228	36.436864
1546.402068	150868.905496	36.441882
1547.993753	151100.874979	36.446900
1549.831814	151338.930478	36.451917
1550.802259	151585.340995	36.456935
1553.030224	151816.377673	36.461952
1554.039440	152059.527244	36.466970
1555.442101	152304.581256	36.471988
1557.314575	152552.339046	36.477005
1558.763432	152805.326187	36.482023
1560.534636	153055.221138	36.487040
1561.998593	153307.816645	36.492058
1563.371943	153556.307792	36.497076
1564.766465	153814.484197	36.502093
1566.231542	154074.185550	36.507111
1567.917082	154328.820226	36.512128
1569.323370	154595.419749	36.517146
1570.973419	154860.283603	36.522164
1572.770857	155121.170098	36.527181
1574.534838	155384.815387	36.532199
1575.945145	155651.676147	36.537216
1577.629490	155915.807337	36.542234
1579.011201	156181.814545	36.547252
1580.975806	156450.038985	36.552269
1582.163140	156727.746911	36.557287
1584.103664	156983.311891	36.562304
1585.774046	157249.459009	36.567322
1587.302757	157532.774592	36.572340
1588.932895	157791.425457	36.577357
1590.348361	158068.803556	36.582375
1592.412405	158331.206366	36.587392
1593.852153	158595.536347	36.592410
1595.642368	158860.408654	36.597428
1597.573235	159115.356764	36.602445
1598.996941	159379.162587	36.607463
1601.086201	159634.114653	36.612480
1602.560111	159888.595644	36.617498
1603.857135	160153.746216	36.622516
1605.869011	160418.265281	36.627533
1607.566422	160664.486065	36.632551
1609.173057	160919.283067	36.637568
1610.763526	161169.316124	36.642586
1612.434171	161397.614261	36.647604
1614.739882	161619.116946	36.652621
1616.604039	161845.966824	36.657639
1618.444711	162057.337097	36.662656
1619.868186	162270.144539	36.667674
1621.444760	162490.335310	36.672692
1623.012965	162700.801455	36.677709
1624.161035	162932.705282	36.682727
1625.629755	163155.593186	36.687744
1627.420861	163384.303243	36.692762
1628.892900	163610.325972	36.697780
1630.498413	163844.813590	36.702797
1631.955461	164076.777056	36.707815
1633.654236	164305.279233	36.712832
1635.456546	164542.745869	36.717850
1637.107778	164781.024371	36.722868
1638.593072	165020.801996	36.727885
1640.271328	165261.831520	36.732903
1641.807017	165501.984740	36.737920
1643.121568	165740.614582	36.742938
1644.854813	165986.941681	36.747956
1646.761062	166228.004651	36.752973
1648.434338	166473.012705	36.757991
1649.686666	166715.641268	36.763008
1651.451645	166967.639339	36.768026
1653.047602	167227.035223	36.773044
1655.358421	167464.376229	36.778061
1657.271405	167714.808333	36.783079
1659.029079	167952.481234	36.788096
1660.773242	168200.064063	36.793114
1662.352989	168434.330823	36.798132
1664.203368	168676.914978	36.803149
1665.503617	168932.602191	36.808167
1667.402797	169171.769623	36.813184
1669.108637	169416.499695	36.818202
1670.647576	169662.259906	36.823220
1672.121612	169908.501315	36.828237
1673.839675	170172.223197	36.833255
1675.157392	170419.063476	36.838272
1676.914870	170674.258272	36.843290
1678.538953	170934.575294	36.848308
1680.389260	171182.629678	36.853325
1681.825501	171440.176472	36.858343
1683.585190	171704.016214	36.863360
1685.114584	171963.898403	36.868378
1686.727043	172222.665471	36.873396
1688.498148	172474.305143	36.878413
1689.811044	172759.255434	36.883431
1691.541605	173023.755526	36.888448
1693.267400	173287.408175	36.893466
1694.552187	173563.894556	36.898484
1697.024038	173830.311978	36.903501
1698.208536	174098.546717	36.908519
1700.147721	174361.436711	36.913536
1702.294386	174624.942455	36.918554
1703.550982	174881.930956	36.923572
1705.071952	175126.903182	36.928589
1706.434946	175389.865934	36.933607
1708.126025	175627.861981	36.938624
1709.776215	175894.169650	36.943642
1711.093343	176151.245292	36.948660
1712.845835	176417.908006	36.953677
1714.189867	176692.274765	36.958695
1715.925376	176968.522266	36.963712
1717.841412	177244.463817	36.968730
1719.561269	177524.548954	36.973748
1721.168324	177799.693193	36.978765
1722.919606	178086.501283	36.983783
1724.252823	178367.452722	36.988800
1726.041148	178660.577117	36.993818
1727.745827	178956.977507	36.998836
1729.562779	179241.740298	37.003853
1730.753196	179545.179234	37.008871
1732.451729	179841.015788	37.013888
1734.441940	180140.956994	37.018906
1735.942774	180450.722334	37.023924
1737.735751	180753.909165	37.028941
1739.648906	181069.678342	37.033959
1741.518709	181376.321174	37.038976
1743.836616	181666.565163	37.043994
1745.696011	181973.480288	37.049012
1747.896044	182265.891296	37.054029
1749.903443	182570.122501	37.059047
1751.678956	182866.398769	37.064064
1753.821050	183141.948873	37.069082
1755.624627	183421.995512	37.074100
1757.837488	183702.727568	37.079117
1760.010763	183977.364279	37.084135
1762.278686	184248.409333	37.089152
1764.387659	184520.762857	37.094170
1765.984574	184795.965566	37.099188
1768.038228	185053.649688	37.104205
1769.654687	185320.528317	37.109223
1771.181861	185576.091040	37.114240
1773.247165	185837.470360	37.119258
1774.764425	186105.003789	37.124276
1777.222693	186351.375353	37.129293
1779.566041	186585.990451	37.134311
1781.138945	186841.717911	37.139328
1782.965501	187086.937404	37.144346
1784.267960	187339.398496	37.149364
1785.978644	187578.662035	37.154381
1787.666001	187837.079746	37.159399
1789.135883	188098.046045	37.164416
1790.934244	188358.707837	37.169434
1792.022576	188633.696858	37.174452
1793.717363	188899.707974	37.179469
1795.312283	189171.662842	37.184487
1797.098069	189441.533106	37.189504
1798.956500	189708.715658	37.194522
1800.344029	189967.357543	37.199540
1802.121636	190222.271289	37.204557
1803.676380	190489.112975	37.209575
1804.915554	190761.044476	37.214592
1806.990280	191023.986623	37.219610
1808.199410	191304.669939	37.224628
1810.080625	191569.422476	37.229645
1811.790115	191851.615867	37.234663
1813.549875	192134.450144	37.239680
1815.506907	192422.394671	37.244698
1816.730236	192716.028828	37.249716
1818.841501	193005.056392	37.254733
1820.818428	193304.805850	37.259751
1822.286481	193606.617761	37.264768
1824.542376	193900.120330	37.269786
1826.460072	194190.505374	37.274804
1828.732387	194477.345557	37.279821
1830.735128	194764.445914	37.284839
1832.435335	195054.908495	37.289856
1834.671502	195347.369125	37.294874
1836.206694	195653.840475	37.299892
1838.029093	195935.949966	37.304909
1839.951737	196232.894930	37.309927
1841.464829	196546.736532	37.314944
1843.514787	196838.778220	37.319962
1845.157587	197142.829716	37.324980
1847.132129	197453.087698	37.329997
1848.722747	197762.608814	37.335015
1850.284297	198069.382050	37.340032
1852.386801	198390.045844	37.345050
1853.853836	198718.973886	37.350068
1855.631774	199030.770010	37.355085
1857.607201	199351.815116	37.360103
1859.515800	199685.502269	37.365120
1861.761062	200001.151936	37.370138
1863.582421	200322.887267	37.375156
1865.650279	200647.695198	37.380173
1867.589040	200965.848857	37.385191
1869.286724	201289.031106	37.390208
1871.349529	201604.160408	37.395226
1873.144405	201938.145808	37.400244
1874.892972	202261.160587	37.405261
1876.712915	202587.847051	37.410279
1878.407462	202917.855674	37.415296
1880.518188	203241.795981	37.420314
1882.542784	203578.889966	37.425332
1884.614365	203894.804951	37.430349
1886.764008	204204.908107	37.435367
1888.735168	204538.817292	37.440384
1891.122944	204845.445974	37.445402
1892.703001	205164.378234	37.450420
1894.896674	205477.934005	37.455437
1896.960849	205782.905216	37.460455
1898.861818	206107.250215	37.465472
1900.467216	206407.930565	37.470490
1902.425218	206699.035543	37.475508
1903.835299	206987.182186	37.480525
1905.906534	207284.187716	37.485543
1907.626894	207583.218076	37.490560
1909.338057	207870.610228	37.495578
1910.834626	208175.874077	37.500596
1912.610228	208481.882242	37.505613
1914.873589	208785.338990	37.510631
1916.743426	209092.947488	37.515648
1918.702320	209392.469278	37.520666
1920.599672	209715.323314	37.525684
1922.345935	210011.657232	37.530701
1924.405779	210323.900768	37.535719
1926.179077	210645.573193	37.540736
1928.620620	210949.304108	37.545754
1930.434167	211266.936126	37.550772
1932.209927	211583.763192	37.555789
1934.560178	211896.679256	37.560807
1936.067304	212222.667525	37.565824
1938.206185	212536.712033	37.570842
1940.143776	212853.418017	37.575860
1942.272645	213165.245346	37.580877
1944.485472	213487.369903	37.585895
1946.784246	213808.035033	37.590912
1949.219534	214107.490344	37.595930
1951.105110	214414.550310	37.600948
1953.245863	214723.031229	37.605965
1955.392103	215018.879948	37.610983
1957.237630	215322.408121	37.616000
1959.179291	215631.534150	37.621018
1961.326781	215937.518285	37.626036
1963.291964	216246.719501	37.631053
1965.191911	216547.959044	37.636071
1967.028834	216852.879179	37.641088
1969.092570	217159.745307	37.646106
1970.817059	217472.011885	37.651124
1972.591671	217793.984855	37.656141
1974.514942	218123.223622	37.661159
1976.181387	218486.062358	37.666176
1978.127271	218805.498683	37.671194
1979.955254	219128.015074	37.676212
1981.603361	219456.262375	37.681229
1984.252157	219794.484590	37.686247
1985.302678	220128.936972	37.691264
1986.954091	220468.539426	37.696282
1988.910552	220813.465931	37.701300
1991.008296	221154.371941	37.706317
1993.475716	221493.341608	37.711335
1994.977801	221845.620450	37.716352
1997.153690	222192.664206	37.721370
1999.175266	222536.064414	37.726388
2001.210304	222876.619736	37.731405
2003.871007	223223.070529	37.736423
2005.336190	223572.086994	37.741440
2007.618894	223903.211140	37.746458
2009.605928	224231.082140	37.751476
2011.503259	224551.146836	37.756493
2013.572767	224871.045793	37.761511
2015.709941	225187.240163	37.766528
2017.523798	225502.026777	37.771546
2019.544472	225827.308430	37.776564
2021.758231	226138.897585	37.781581
2024.379523	226462.588032	37.786599
2025.390792	226790.827147	37.791616
2027.660137	227111.502948	37.796634
2029.368776	227437.195834	37.801652
2031.221147	227768.962331	37.806669
2033.496500	228100.078855	37.811687
2035.445438	228444.429367	37.816704
2037.325669	228779.141291	37.821722
2039.664766	229113.883258	37.826740
2041.805338	229455.007248	37.831757
2044.117369	229790.873498	37.836775
2045.813029	230139.715207	37.841792
2048.276974	230474.366194	37.846810
2050.478098	230814.012598	37.851828
2052.110052	231155.096612	37.856845
2054.422363	231495.210402	37.861863
2056.360288	231843.004138	37.866880
2058.730191	232195.403812	37.871898
2060.610900	232539.323279	37.876916
2062.589521	232898.772027	37.881933
2064.664123	233236.034304	37.886951
2066.419362	233596.359178	37.891968
2068.503231	233957.826940	37.896986
2070.534037	234315.951832	37.902004
2072.084605	234679.462459	37.907021
2074.431411	235048.562738	37.912039
2076.132688	235423.329054	37.917056
2078.007844	235804.850600	37.922074
2079.821938	236187.627758	37.927092
2081.869756	236577.811106	37.932109
2084.342847	236959.749917	37.937127
2086.094387	237352.395972	37.942144
2088.630438	237733.514732	37.947162
2091.294350	238103.616624	37.952180
2093.410590	238491.129000	37.957197
2095.459152	238874.284730	37.962215
2097.744799	239247.295112	37.967232
2100.496437	239620.512173	37.972250
2102.746623	239984.843875	37.977268
2104.837891	240347.322327	37.982285
2107.301366	240710.758832	37.987303
2109.503741	241073.907652	37.992320
2111.727626	241427.046535	37.997338
2114.028455	241785.025644	38.002356
2115.980909	242149.182482	38.007373
2118.020709	242499.280188	38.012391
2120.341582	242861.475617	38.017408
2122.426812	243199.782293	38.022426
2124.950336	243522.195854	38.027444
2126.940321	243844.771039	38.032461
2129.343963	244145.005108	38.037479
2131.089600	244476.917182	38.042496
2132.882446	244798.027292	38.047514
2134.812301	245123.688554	38.052532
2136.533809	245459.747153	38.057549
2138.771943	245800.804782	38.062567
2140.747495	246142.463701	38.067584
2142.144367	246485.612274	38.072602
2144.086230	246847.116366	38.077620
2145.869699	247202.753413	38.082637
2147.967294	247579.932470	38.087655
2149.755782	247962.470352	38.092672
2151.531133	248343.055371	38.097690
2153.463176	248727.807689	38.102708
2155.631889	249133.225558	38.107725
2157.295933	249528.030473	38.112743
2159.449017	249937.212253	38.117760
2161.644731	250351.951233	38.122778
2164.062828	250760.229339	38.127796
2165.778165	251178.882176	38.132813
2168.566009	251588.424483	38.137831
2170.567170	252014.070264	38.142848
2172.776221	252430.818809	38.147866
2175.499983	252850.077661	38.152884
2177.763510	253275.176700	38.157901
2180.108561	253688.223169	38.162919
2182.203369	254096.204371	38.167936
2184.495784	254515.281220	38.172954
2186.970179	254935.346159	38.177972
2189.084161	255360.778182	38.182989
2191.584538	255774.794934	38.188007
2193.480592	256199.424901	38.193024
2195.602354	256611.369475	38.198042
2198.077893	257030.676209	38.203060
2200.545289	257461.771756	38.208077
2202.862828	257863.348672	38.213095
2205.316401	258286.115844	38.218112
2207.565042	258698.323326	38.223130
2210.282829	259105.909989	38.228148
2212.637481	259505.375194	38.233165
2215.554936	259893.574524	38.238183
2217.919428	260294.563482	38.243200
2220.113839	260683.488229	38.248218
2222.860362	261066.737308	38.253236
2224.722027	261455.334786	38.258253
2227.086229	261844.513531	38.263271
2229.521694	262229.718588	38.268288
2231.621047	262611.471782	38.273306
2234.384500	262986.362893	38.278324
2236.187073	263382.745322	38.283341
2238.439133	263749.944997	38.288359
2240.598245	264132.808068	38.293376
2242.375889	264500.109092	38.298394
2244.574681	264863.660213	38.303412
2246.294759	265229.980291	38.308429
2249.066764	265588.030260	38.313447
2250.796110	265958.566392	38.318464
2253.089294	266315.219463	38.323482
2255.436951	266668.307703	38.328500
2257.439316	267041.138449	38.333517
2259.871635	267404.476665	38.338535
2261.852669	267772.789503	38.343552
2263.900786	268146.604444	38.348570
2265.960082	268522.323079	38.353588
2267.739373	268919.018656	38.358605
2269.871235	269312.025869	38.363623
2272.047010	269711.834413	38.368640
2273.865516	270112.512703	38.373658
2276.538886	270519.482672	38.378676
2278.307689	270936.071691	38.383693
2280.569479	271348.594365	38.388711
2283.243171	271769.079335	38.393728
2285.150963	272198.221406	38.398746
2287.752356	272623.798746	38.403764
2290.043464	273049.171334	38.408781
2292.306584	273476.301262	38.413799
2294.813868	273910.022816	38.418816
2296.909800	274330.015565	38.423834
2298.973648	274766.728858	38.428852
2301.106117	275200.382850	38.433869
2303.951226	275634.965365	38.438887
2306.321902	276084.966709	38.443904
2308.392770	276533.846953	38.448922
2310.884823	276966.097307	38.453940
2313.393415	277415.339796	38.458957
2315.994466	277847.369396	38.463975
2318.440866	278291.388352	38.468992
2320.843166	278733.381850	38.474010
2323.527956	279155.312523	38.479028
2325.555475	279603.919089	38.484045
2328.094426	280040.835005	38.489063
2330.412528	280479.741732	38.494080
2332.336244	280927.906693	38.499098
2335.127467	281365.035807	38.504116
2337.407280	281807.021489	38.509133
2339.731975	282241.226320	38.514151
2342.591084	282680.401313	38.519168
2345.004508	283115.048600	38.524186
2347.026324	283549.046284	38.529204
2349.441660	283989.077921	38.534221
2351.955981	284430.236558	38.539239
2354.468246	284868.321277	38.544256
2356.709313	285318.184713	38.549274
2359.282298	285757.173311	38.554292
2361.244697	286194.454559	38.559309
2363.892260	286625.885578	38.564327
2366.267049	287060.179013	38.569344
2368.879985	287482.189924	38.574362
2371.767507	287868.694353	38.579380
2373.593382	288276.222306	38.584397
2376.026210	288673.009719	38.589415
2378.696008	289061.833363	38.594432
2380.675335	289460.164928	38.599450
2383.432897	289845.290169	38.604468
2385.693649	290242.331240	38.609485
2388.093739	290653.981519	38.614503
2390.225171	291054.649002	38.619520
2392.325173	291455.981283	38.624538
2394.802748	291858.878807	38.629556
2397.186435	292270.579767	38.634573
2399.498242	292681.554716	38.639591
2401.608401	293100.969053	38.644608
2403.890131	293531.938839	38.649626
2405.680981	293960.064310	38.654644
2408.020841	294398.999427	38.659661
2410.491680	294836.414121	38.664679
2413.192757	295272.394256	38.669696
2415.358920	295718.923842	38.674714
2418.141214	296149.884944	38.679732
2420.945780	296595.473028	38.684749
2423.066047	297044.038907	38.689767
2425.899851	297479.357867	38.694784
2427.953783	297934.511096	38.699802
2430.221464	298388.155964	38.704820
2432.459517	298852.269775	38.709837
2434.815705	299304.882099	38.714855
2437.212943	299774.378627	38.719872
2439.122683	300250.148987	38.724890
2441.979036	300707.682181	38.729908
2443.972127	301197.127756	38.734925
2446.420158	301668.337863	38.739943
2449.370897	302160.600487	38.744960
2451.325653	302646.237266	38.749978
2453.812246	303134.506026	38.754996
2455.994813	303628.180863	38.760013
2458.287643	304115.410114	38.765031
2460.823207	304625.662918	38.770048
2462.931163	305143.525519	38.775066
2465.810703	305638.911475	38.780084
2467.769086	306160.248254	38.785101
2470.388045	306664.256906	38.790119
2473.160241	307175.783103	38.795136
2475.590691	307693.990764	38.800154
2477.949012	308213.045871	38.805172
2480.592319	308733.196581	38.810189
2483.125263	309247.520592	38.815207
2485.819789	309756.736838	38.820224
2488.735283	310279.402930	38.825242
2491.596622	310776.955283	38.830260
2494.160874	311289.995237	38.835277
2496.762542	311797.870877	38.840295
2499.419248	312286.432219	38.845312
2502.021332	312790.086932	38.850330
2504.241213	313268.121706	38.855348
2506.881811	313728.638786	38.860365
2509.325306	314182.962425	38.865383
2512.017630	314638.057378	38.870400
2515.038290	315098.965274	38.875418
2518.267646	315534.287423	38.880436
2520.777339	315972.109123	38.885453
2523.297364	316423.845319	38.890471
2526.012094	316866.786315	38.895488
2528.576420	317313.685755	38.900506
2530.848456	317767.410575	38.905524
2533.112244	318218.010631	38.910541
2535.252135	318676.298145	38.915559
2537.703393	319130.394304	38.920576
2539.557138	319612.570482	38.925594
2542.137899	320077.054203	38.930612
2544.780490	320552.116196	38.935629
2547.050242	321032.364849	38.940647
2549.752255	321502.282179	38.945664
2551.808191	322007.270184	38.950682
2554.097773	322495.964602	38.955700
2556.654918	323014.276466	38.960717
2558.794419	323515.229695	38.965735
2561.459047	324030.267560	38.970752
2563.552435	324553.519316	38.975770
2566.164185	325087.326285	38.980788
2568.794018	325608.886327	38.985805
2571.259690	326152.664313	38.990823
2573.883937	326683.487405	38.995840
2576.233284	327226.032046	39.000858
2578.785469	327754.472143	39.005876
2581.752914	328302.904397	39.010893
2584.464350	328850.128931	39.015911
2587.234691	329386.039794	39.020928
2589.840029	329937.260042	39.025946
2592.849355	330470.992103	39.030964
2595.963389	331013.185093	39.035981
2598.602338	331553.951075	39.040999
2601.519539	332083.191205	39.046016
2604.129226	332616.996040	39.051034
2606.593191	333146.274606	39.056052
2609.687156	333681.111876	39.061069
2611.939775	334212.447180	39.066087
2614.900511	334737.749809	39.071104
2617.410984	335269.112191	39.076122
2620.195391	335799.309738	39.081140
2622.637789	336324.098062	39.086157
2625.196117	336867.348734	39.091175
2628.298077	337392.049438	39.096192
2630.754623	337924.541586	39.101210
2633.422802	338457.986040	39.106228
2636.085114	338983.454350	39.111245
2638.635673	339521.961210	39.116263
2641.547417	340039.586389	39.121280
2643.742970	340562.855700	39.126298
2646.498921	341068.639911	39.131316
2649.110630	341560.681726	39.136333
2651.558447	342049.901930	39.141351
2654.336457	342550.795594	39.146368
2656.685469	343049.188758	39.151386
2659.151742	343552.763834	39.156404
2661.109676	344067.230585	39.161421
2664.119082	344574.011380	39.166439
2666.904776	345089.455092	39.171456
2669.187098	345619.546473	39.176474
2671.816702	346139.245253	39.181492
2674.178543	346658.930929	39.186509
2676.798397	347208.019858	39.191527
2679.180338	347748.915798	39.196544
2681.675901	348306.822814	39.201562
2684.085505	348856.842699	39.206580
2686.876581	349410.071437	39.211597
2689.374046	349977.912452	39.216615
2692.344989	350545.291726	39.221632
2694.677467	351124.544834	39.226650
2697.189338	351708.510198	39.231668
2700.203201	352289.064217	39.236685
2702.830562	352877.922923	39.241703
2705.894341	353456.577619	39.246720
2708.458419	354042.234735	39.251738
2711.241406	354626.809768	39.256756
2714.287464	355225.728669	39.261773
2717.012944	355812.812067	39.266791
2720.047498	356408.647387	39.271808
2722.451758	356998.128307	39.276826
2725.493573	357586.942822	39.281844
2728.517546	358179.027328	39.286861
2730.864105	358781.415214	39.291879
2734.208912	359361.454502	39.296896
2737.218989	359952.301217	39.301914
2740.050369	360539.996365	39.306932
2743.067431	361134.938897	39.311949
2745.376491	361729.224637	39.316967
2748.465454	362310.968771	39.321984
2751.127036	362904.295410	39.327002
2753.789297	363500.456730	39.332020
2756.366143	364087.842872	39.337037
2758.951044	364684.483169	39.342055
2762.242623	365286.003103	39.347072
2764.950629	365877.354904	39.352090
2767.663368	366471.058184	39.357108
2771.001257	367061.863071	39.362125
2773.492975	367650.560896	39.367143
2776.218708	368246.877319	39.372160
2779.578811	368842.729847	39.377178
2782.322642	369424.410776	39.382196
2785.324605	370009.899953	39.387213
2787.766792	370592.374021	39.392231
2790.438667	371177.112783	39.397248
2793.228031	371763.118900	39.402266
2795.901333	372328.278066	39.407284
2798.934277	372873.632185	39.412301
2800.960557	373442.836870	39.417319
2803.644722	373996.832811	39.422336
2806.562517	374561.009288	39.427354
2808.711613	375134.864871	39.432372
2811.573728	375701.216299	39.437389
2813.826756	376296.959919	39.442407
2816.247042	376875.796601	39.447424
2818.879166	377471.437288	39.452442
2821.594201	378077.381484	39.457460
2824.073163	378688.935042	39.462477
2826.734985	379312.170669	39.467495
2829.880043	379932.224790	39.472512
2832.763113	380560.682015	39.477530
2834.871215	381198.028979	39.482548
2837.642171	381841.196364	39.487565
2840.392230	382492.854141	39.492583
2843.215870	383143.195303	39.497600
2846.169889	383801.773934	39.502618
2849.003747	384464.519934	39.507636
2851.959615	385130.582977	39.512653
2854.387529	385809.780456	39.517671
2857.349559	386483.072316	39.522688
2860.063831	387160.728160	39.527706
2863.370786	387825.570374	39.532724
2867.191351	388500.590974	39.537741
2870.097705	389178.203702	39.542759
2873.642377	389848.169921	39.547776
2876.798379	390507.000510	39.552794
2880.153089	391149.885878	39.557812
2883.554643	391799.320375	39.562829
2886.790396	392445.928626	39.567847
2889.746388	393096.880183	39.572864
2892.675734	393737.350270	39.577882
2895.521666	394391.058775	39.582900
2898.446419	395021.716960	39.587917
2901.653808	395664.718551	39.592935
2904.086552	396309.250457	39.597952
2906.653961	396961.888123	39.602970
2909.461376	397616.579541	39.607988
2912.359002	398268.099594	39.613005
2915.161474	398932.375473	39.618023
2917.751601	399594.389540	39.623040
2920.805858	400261.894582	39.628058
2923.473054	400926.277903	39.633076
2926.674677	401588.483949	39.638093
2929.591336	402259.645515	39.643111
2932.508416	402932.795675	39.648128
2935.617558	403593.250701	39.653146
2938.453424	404266.943006	39.658164
2941.375468	404930.390948	39.663181
2943.597954	405630.414012	39.668199
2946.664546	406295.356284	39.673216
2950.293517	406949.928940	39.678234
2953.036901	407596.845881	39.683252
2955.834130	408231.522985	39.688269
2958.975554	408857.843815	39.693287
2961.880042	409497.673615	39.698304
2964.930385	410132.549576	39.703322
2967.449285	410782.044573	39.708340
2970.130637	411414.645252	39.713357
2972.982667	412064.490388	39.718375
2975.380071	412727.090493	39.723392
2978.505394	413386.772685	39.728410
2981.134914	414057.998750	39.733428
2984.238547	414726.219949	39.738445
2987.051300	415405.875492	39.743463
2990.057018	416087.942548	39.748480
2992.787375	416783.720778	39.753498
2995.410497	417490.952592	39.758516
2998.464540	418199.618947	39.763533
3001.201394	418909.787361	39.768551
3003.885121	419633.172601	39.773568
3006.487129	420345.707758	39.778586
3009.401266	421097.396213	39.783604
3012.637206	421833.938528	39.788621
3015.383139	422589.438713	39.793639
3018.071293	423338.745621	39.798656
3021.381888	424095.432228	39.803674
3024.400559	424873.220994	39.808692
3027.623699	425627.902616	39.813709
3030.698020	426392.795203	39.818727
3033.605463	427169.420479	39.823744
3037.118922	427938.125496	39.828762
3041.287844	428687.682089	39.833780
3044.895210	429446.095227	39.838797
3049.315815	430185.741688	39.843815
3052.701755	430904.559932	39.848832
3056.164281	431628.436765	39.853850
3058.906634	432363.221372	39.858868
3061.914436	433078.316025	39.863885
3064.757731	433805.268524	39.868903
3067.458450	434554.938125	39.873920
3070.348860	435274.978400	39.878938
3073.594175	436018.137067	39.883956
3076.535235	436754.915559	39.888973
3079.597789	437498.641605	39.893991
3082.314967	438249.742829	39.899008
3085.126161	438987.665765	39.904026
3088.117744	439755.464365	39.909044
3091.006992	440515.862398	39.914061
3094.021169	441272.976435	39.919079
3096.785327	442034.713950	39.924096
3099.769752	442810.670385	39.929114
3102.831957	443581.070978	39.934132
3105.608101	444364.047573	39.939149
3108.455367	445158.479175	39.944167
3111.086304	445954.335883	39.949184
3114.595116	446738.636956	39.954202
3116.782863	447516.084658	39.959220
3120.244301	448282.928220	39.964237
3122.697772	449041.149279	39.969255
3125.763565	449822.177423	39.974272
3129.344185	450592.266402	39.979290
3132.236088	451368.511972	39.984308
3135.494980	452154.238478	39.989325
3138.744193	452927.034282	39.994343
3141.829494	453706.256741	39.999360
3145.149624	454499.837567	40.004378
3148.147576	455296.932967	40.009396
3151.154628	456103.056174	40.014413
3154.135292	456895.694943	40.019431
3156.725819	457719.737635	40.024448
3159.721036	458535.944422	40.029466
3163.063928	459366.434551	40.034484
3165.863044	460206.389268	40.039501
3169.181218	461038.033926	40.044519
3172.191788	461885.074083	40.049536
3175.492761	462741.798149	40.054554
3178.025742	463617.224404	40.059572
3181.304788	464475.905978	40.064589
3184.476990	465357.887075	40.069607
3187.425506	466240.928965	40.074624
3190.677553	467131.472185	40.079642
3193.534458	468035.644335	40.084660
3197.027087	468934.012824	40.089677
3200.489562	469830.931324	40.094695
3204.057938	470726.479452	40.099712
3207.766391	471621.865345	40.104730
3211.138214	472517.872112	40.109748
3214.731360	473400.355533	40.114765
3218.130525	474290.566646	40.119783
3220.884062	475194.743480	40.124800
3224.705759	476082.735880	40.129818
3228.530759	476973.165395	40.134836
3231.835130	477856.863940	40.139853
3234.986455	478748.028260	40.144871
3237.730786	479637.144453	40.149888
3241.303352	480519.266304	40.154906
3243.995859	481428.475858	40.159924
3247.631968	482332.591670	40.164941
3250.670498	483230.038728	40.169959
3253.726605	484139.468122	40.174976
3257.583722	485026.545058	40.179994
3261.418688	485908.885320	40.185012
3264.992972	486799.613255	40.190029
3268.513202	487688.489133	40.195047
3271.764477	488579.942340	40.200064
3275.227531	489456.063273	40.205082
3278.348703	490343.007802	40.210100
3281.483989	491221.320645	40.215117
3285.330782	492096.398300	40.220135
3288.136557	492987.711592	40.225152
3291.169357	493840.914486	40.230170
3294.619146	494690.375509	40.235188
3298.317156	495507.537590	40.240205
3301.241894	496345.641692	40.245223
3304.646752	497164.543184	40.250240
3308.033795	497982.501504	40.255258
3311.013884	498796.447620	40.260276
3314.485753	499631.333611	40.265293
3317.891523	500469.321340	40.270311
3320.685031	501302.822752	40.275328
3324.121810	502141.130678	40.280346
3327.121645	502992.391068	40.285364
3329.948152	503843.789164	40.290381
3332.962337	504708.896225	40.295399
3335.736056	505588.736746	40.300416
3338.909006	506462.261764	40.305434
3342.312497	507366.037788	40.310452
3345.308494	508258.577120	40.315469
3349.176027	509158.451341	40.320487
3351.947699	510073.892439	40.325504
3355.275122	510987.127815	40.330522
3358.366015	511916.042998	40.335540
3361.625358	512860.419824	40.340557
3365.140495	513785.179470	40.345575
3368.018152	514735.767118	40.350592
3371.905534	515674.286877	40.355610
3375.086780	516633.394761	40.360628
3378.400603	517605.842679	40.365645
3382.131167	518557.993580	40.370663
3385.467516	519516.203534	40.375680
3389.363815	520466.099460	40.380698
3392.843340	521434.108912	40.385716
3396.316007	522395.305142	40.390733
3399.705658	523376.020364	40.395751
3402.566081	524369.565481	40.400768
3406.424645	525327.299277	40.405786
3409.509763	526309.748831	40.410804
3412.914607	527299.950839	40.415821
3416.362919	528286.354262	40.420839
3419.853266	529278.082404	40.425856
3423.116461	530266.709691	40.430874
3426.647084	531282.697532	40.435892
3430.107196	532262.600454	40.440909
3433.887038	533260.782849	40.445927
3437.281191	534268.938129	40.450944
3440.849135	535267.276366	40.455962
3444.496584	536268.207230	40.460980
3447.884315	537253.094353	40.465997
3451.824225	538255.108152	40.471015
3454.985948	539258.941732	40.476032
3458.320684	540266.156545	40.481050
3462.201181	541257.001214	40.486068
3465.500240	542253.512522	40.491085
3469.030683	543242.720026	40.496103
3472.208582	544257.546640	40.501120
3475.649567	545235.731556	40.506125
3478.833306	546190.378852	40.511130
3481.623217	547076.285214	40.516135
3485.179956	547921.289229	40.521140
3488.078194	548710.786282	40.526144
3491.006802	549429.032903	40.531149
3493.444200	550088.182046	40.536154
3495.872658	550678.578350	40.541159
3499.061745	551208.080678	40.546164
3500.740993	551681.343198	40.551168
3502.983919	552086.994382	40.556173
3505.057599	552438.626532	40.561178
3506.819164	552754.025023	40.566183
3508.826360	553016.051888	40.571188
3510.157583	553229.749312	40.576192
3511.442283	553392.598422	40.581197
3512.896826	553523.737203	40.586202
3513.919290	553612.768435	40.591207
3515.430417	553663.280538	40.596212
3516.222354	553693.172050	40.601216
3516.935575	553672.174008	40.606221
3517.687984	553619.690116	40.611226
3518.341620	553558.746316	40.616231
3518.978159	553475.859801	40.621236
3519.275910	553365.380289	40.626240
3519.954226	553238.847293	40.631245
3520.489102	553092.307206	40.636250
3520.721906	552935.420550	40.641255
3521.450464	552745.761460	40.646260
3521.394666	552553.045364	40.651264
3522.019223	552334.639668	40.656269
3521.987753	552132.630801	40.661274
3522.227427	551890.868815	40.666279
3522.384800	551659.408618	40.671284
3521.990484	551417.133433	40.676288
3522.351477	551163.937061	40.681293
3522.269000	550922.916181	40.686298
3522.388864	550642.451195	40.691303
3522.101109	550394.944809	40.696308
3522.215685	550133.897698	40.701312
3522.439128	549853.350622	40.706317
3522.468020	549572.879342	40.711322
3521.922334	549318.179255	40.716327
3521.931679	549034.370113	40.721332
3521.870620	548752.030062	40.726336
3521.738327	548462.277283	40.731341
3521.519898	548205.436921	40.736346
3521.151662	547928.731344	40.741351
3521.357080	547646.025001	40.746356
3520.946443	547380.015175	40.751360
3521.214465	547100.367079	40.756365
3520.921710	546817.673036	40.761370
3520.874934	546547.603345	40.766375
3520.500278	546266.375358	40.771380
3520.276236	546007.276562	40.776384
3520.251261	545738.399979	40.781389
3519.861464	545458.572288	40.786394
3519.586358	545214.105809	40.791399
3519.798392	544916.303754	40.796404
3518.762874	544679.772767	40.801408
3518.886148	544407.769332	40.806413
3518.868794	544157.136580	40.811418
3518.394319	543912.781102	40.816423
3518.743117	543660.618134	40.821428
3518.528801	543416.263861	40.826432
3518.098442	543159.571075	40.831437
3518.054887	542919.169919	40.836442
3517.635087	542683.872947	40.841447
3517.776855	542443.737760	40.846452
3517.200934	542210.830887	40.851456
3516.844301	541978.693541	40.856461
3516.776082	541756.655312	40.861466
3516.445670	541516.478899	40.866471
3516.353129	541307.211784	40.871476
3515.898000	541099.160358	40.876480
3515.901169	540870.988299	40.881485
3515.750869	540674.142527	40.886490
3515.262856	540479.165317	40.891495
3515.575984	540253.156609	40.896500
3515.322474	540046.977545	40.901504
3515.153796	539859.920025	40.906509
3515.107466	539658.903940	40.911514
3514.647883	539463.000170	40.916519
3514.621758	539267.176845	40.921524
3514.212493	539084.389532	40.926528
3514.509634	538889.570688	40.931533
3513.987564	538711.038584	40.936538
3513.808669	538530.278645	40.941543
3513.896607	538346.040350	40.946548
3513.672258	538182.504098	40.951552
3513.433678	537997.757676	40.956557
3513.504021	537830.989465	40.961562
3513.338673	537657.590319	40.966567
3513.237077	537486.451772	40.971572
3512.623625	537314.584141	40.976576
3512.942101	537153.021695	40.981581
3512.694079	536998.112717	40.986586
3512.464925	536837.744597	40.991591
3512.527563	536674.096292	40.996596
3512.404528	536519.920300	41.001600
3512.049694	536372.547330	41.006605
3512.072468	536230.012482	41.011610
3511.768533	536072.375559	41.016615
3511.808454	535925.087414	41.021620
3511.427324	535790.946215	41.026624
3511.475762	535646.280509	41.031629
3511.512616	535509.343278	41.036634
3511.049679	535376.221580	41.041639
3511.289736	535234.299774	41.046644
3511.006431	535100.541168	41.051648
3510.933753	534971.142618	41.056653
3510.614631	534848.247469	41.061658
3510.199484	534725.417029	41.066663
3510.654579	534595.426781	41.071668
3510.310603	534478.190044	41.076672
3510.628534	534349.128639	41.081677
3510.518120	534228.115077	41.086682
3509.892784	534112.940595	41.091687
3510.078156	533989.554750	41.096692
3509.562763	533886.181661	41.101696
3509.739678	533780.677838	41.106701
3509.611725	533666.280176	41.111706
3509.512429	533561.374189	41.116711
3509.268636	533458.056343	41.121716
3509.375296	533364.583722	41.126720
3509.327563	533255.373579	41.131725
3509.487108	533147.039222	41.136730
3509.016395	533044.411211	41.141735
3508.789084	532951.291993	41.146740
3508.531801	532854.792212	41.151744
3508.681432	532756.408838	41.156749
3508.966771	532679.575056	41.161754
3508.469145	532584.778714	41.166759
3508.704682	532495.322040	41.171764
3508.442795	532418.472420	41.176768
3508.254265	532327.111527	41.181773
3508.492195	532233.712392	41.186778
3507.973373	532152.658343	41.191783
3508.077126	532066.756489	41.196788
3508.020383	531987.043133	41.201792
3507.994066	531911.922025	41.206797
3507.859971	531831.866450	41.211802
3507.633444	531749.602101	41.216807
3507.823794	531678.234778	41.221812
3507.577308	531606.885651	41.226816
3507.659497	531528.310009	41.231821
3507.612912	531452.533095	41.236826
3507.487429	531388.893872	41.241831
3507.755106	531313.470798	41.246836
3507.630242	531246.041632	41.251840
3507.223349	531177.898891	41.256845
3507.412651	531101.779848	41.261850
3507.258153	531038.699551	41.266855
3507.287682	530966.091284	41.271860
3507.214686	530915.123515	41.276864
3507.066813	530828.698848	41.281869
3507.421412	530776.500967	41.286874
3507.123584	530711.976774	41.291879
3507.282698	530635.658134	41.296884
3507.014260	530591.238015	41.301888
3507.130678	530530.184408	41.306893
3507.123549	530467.179567	41.311898
3506.830224	530402.804968	41.316903
3507.102305	530328.942776	41.321908
3506.699535	530277.368207	41.326912
3506.669330	530218.913432	41.331917
3506.664537	530160.606005	41.336922
3506.534513	530098.781235	41.341927
3506.294703	530054.708762	41.346932
3506.366011	529998.005584	41.351936
3506.400649	529942.369085	41.356941
3506.051406	529904.427366	41.361946
3506.068453	529852.633461	41.366951
3506.125503	529801.692045	41.371956
3505.837630	529765.811954	41.376960
3505.752910	529722.471963	41.381965
3506.002481	529683.980306	41.386970
3506.120328	529636.919462	41.391975
3506.246318	529600.013529	41.396980
3506.015406	529553.866554	41.401984
3505.964796	529508.903649	41.406989
3505.696465	529460.842200	41.411994
3505.714331	529428.399549	41.416999
3506.228549	529368.794441	41.422004
3505.584183	529345.551646	41.427008
3505.471166	529302.316030	41.432013
3505.786159	529263.863537	41.437018
3505.888058	529226.707886	41.442023
3505.906496	529187.695717	41.447028
3505.722205	529153.920133	41.452032
3505.631037	529110.528945	41.457037
3505.516222	529083.008022	41.462042
3505.359745	529049.227817	41.467047
3505.790390	528994.586522	41.472052
3505.643979	528966.464017	41.477056
3505.339614	528930.230910	41.482061
3505.133070	528886.453092	41.487066
3505.145797	528872.251905	41.492071
3505.262882	528840.600863	41.497076
3505.445170	528808.686794	41.502080
3505.641810	528775.304974	41.507085
3505.651256	528731.543119	41.512090
3505.307124	528707.089694	41.517095
3505.632697	528668.128758	41.522100
3505.247976	528638.325246	41.527104
3505.514138	528605.740593	41.532109
3505.270004	528570.760445	41.537114
3505.457744	528541.674785	41.542119
3505.254054	528502.443369	41.547124
3505.009622	528472.667902	41.552128
3505.477435	528439.646773	41.557133
3505.820959	528412.456499	41.562138
3505.139730	528395.332597	41.567143
3505.579186	528358.071017	41.572148
3505.560532	528321.083889	41.577152
3505.211153	528283.037217	41.582157
3505.293013	528250.582029	41.587162
3505.043356	528222.070250	41.592167
3505.282328	528191.712514	41.597172
3505.247782	528167.714655	41.602176
3504.889580	528137.653337	41.607181
3505.342614	528105.796124	41.612186
3505.047704	528081.536084	41.617191
3505.295893	528042.282637	41.622196
3504.783640	528026.394976	41.627200
3504.952592	527997.260752	41.632205
3505.054567	527980.265279	41.637210
3505.295981	527953.494630	41.642215
3505.400351	527917.346197	41.647220
3505.237706	527892.913359	41.652224
3504.844644	527840.268048	41.657229
3505.507894	527832.381009	41.662234
3505.117385	527817.686728	41.667239
3505.583156	527763.995794	41.672244
3504.951241	527738.373516	41.677248
3505.107472	527713.940536	41.682253
3505.351429	527687.118501	41.687258
3505.040713	527656.391805	41.692263
3504.953377	527631.592914	41.697268
3505.057122	527613.181778	41.702272
3504.748655	527577.148357	41.707277
3505.008223	527543.147567	41.712282
3504.745924	527537.276491	41.717287
3505.016525	527499.231012	41.722292
3505.087598	527485.019359	41.727296
3504.677636	527454.813317	41.732301
3504.651390	527430.914102	41.737306
3504.342202	527414.033546	41.742311
3504.787044	527385.713705	41.747316
3504.516915	527370.797837	41.752320
3504.336004	527363.903109	41.757325
3504.657472	527351.117309	41.762330
3504.657589	527330.043803	41.767335
3504.705858	527307.294959	41.772340
3504.558767	527287.811293	41.777344
3504.671707	527262.121049	41.782349
3504.548714	527246.676444	41.787354
3504.425733	527241.035920	41.792359
3504.883799	527208.519137	41.797364
3504.675850	527191.268585	41.802368
3504.729180	527164.020966	41.807373
3504.450507	527151.279325	41.812378
3504.572884	527134.734553	41.817383
3504.685562	527107.224772	41.822388
3504.668433	527091.055764	41.827392
3504.544002	527071.770399	41.832397
3504.513052	527063.234650	41.837402
3504.388140	527050.064327	41.842407
3504.645944	527037.743173	41.847412
3504.902181	527024.310436	41.852416
3504.316380	526999.791493	41.857421
3504.710534	526985.225103	41.862426
3504.679142	526960.567933	41.867431
3504.870292	526938.351890	41.872436
3504.866050	526920.715083	41.877440
3504.863478	526901.814552	41.882445
3504.672666	526874.756639	41.887450
3504.650713	526863.995700	41.892455
3504.741291	526828.150194	41.897460
3504.661966	526810.221905	41.902464
3504.690868	526785.453858	41.907469
3505.035836	526762.404649	41.912474
3504.686909	526749.977018	41.917479
3504.807379	526729.035308	41.922484
3504.731640	526709.792346	41.927488
3504.887529	526685.559993	41.932493
3504.818555	526657.016840	41.937498
3504.755387	526645.655806	41.942503
3504.619210	526612.170424	41.947508
3504.508622	526604.859942	41.952512
3504.341825	526573.097629	41.957517
3504.554072	526555.982126	41.962522
3504.445710	526553.219756	41.967527
3504.577970	526525.503719	41.972532
3504.520098	526518.791332	41.977536
3504.583733	526491.136621	41.982541
3504.559218	526475.069232	41.987546
3504.429673	526461.949694	41.992551
3504.309412	526439.832716	41.997556
3504.620651	526437.155621	42.002560
3504.571924	526406.132401	42.007565
3504.498773	526396.592179	42.012570
3504.385457	526384.228101	42.017575
3504.641493	526366.347384	42.022580
3504.497442	526361.265810	42.027584
3504.439252	526341.413156	42.032589
3504.425888	526321.755550	42.037594
3504.174560	526324.928857	42.042599
3504.747945	526281.475425	42.047604
3504.530482	526283.076658	42.052608
3504.568491	526252.746985	42.057613
3504.606173	526234.951173	42.062618
3504.586012	526229.395117	42.067623
3504.384176	526193.695483	42.072628
3504.396793	526194.552800	42.077632
3504.404103	526172.718527	42.082637
3504.804219	526153.551300	42.087642
3504.424636	526145.120703	42.092647
3504.599557	526122.147987	42.097652
3504.237827	526106.942169	42.102656
3504.429721	526088.666959	42.107661
3504.757854	526071.482080	42.112666
3504.261547	526061.856920	42.117671
3504.432863	526034.841423	42.122676
3504.214265	526020.421546	42.127680
3504.489700	526016.233827	42.132685
3504.778680	525983.286410	42.137690
3504.362220	525985.424531	42.142695
3504.713456	525946.857195	42.147700
3504.657737	525945.754241	42.152704
3504.305552	525917.355608	42.157709
3504.534024	525911.456899	42.162714
3504.489642	525890.641226	42.167719
3504.205440	525872.339937	42.172724
3504.379502	525859.222456	42.177728
3504.295539	525860.044516	42.182733
3504.439128	525825.300278	42.187738
3503.724056	525813.536280	42.192743
3504.328109	525801.867021	42.197748
3504.484494	525792.087993	42.202752
3504.327986	525790.040676	42.207757
3504.593238	525779.739022	42.212762
3504.461311	525759.139180	42.217767
3504.516766	525735.325589	42.222772
3504.315346	525727.826896	42.227776
3504.169670	525712.536010	42.232781
3504.264934	525711.409175	42.237786
3504.022187	525705.382705	42.242791
3504.350242	525665.504277	42.247796
3504.441887	525665.742633	42.252800
3504.064878	525664.185026	42.257805
3504.478052	525645.823792	42.262810
3504.102618	525619.702678	42.267815
3504.396060	525610.407294	42.272820
3503.945794	525600.724035	42.277824
3504.256078	525584.602833	42.282829
3504.327589	525567.508516	42.287834
3503.756756	525579.880548	42.292839
3504.376642	525563.862014	42.297844
3504.562827	525548.215267	42.302848
3504.146332	525539.638556	42.307853
3504.412304	525517.156000	42.312858
3504.108776	525505.326725	42.317863
3504.408388	525490.167414	42.322868
3504.438421	525491.881232	42.327872
3504.293753	525456.373081	42.332877
3504.706598	525454.033561	42.337882
3504.509312	525439.003282	42.342887
3504.734805	525419.559524	42.347892
3504.563078	525402.554020	42.352896
3504.282005	525383.948422	42.357901
3504.381927	525377.665495	42.362906
3504.396963	525349.511065	42.367911
3504.754905	525326.760992	42.372916
3504.299572	525317.785960	42.377920
3504.528705	525295.359458	42.382925
3504.505886	525290.662723	42.387930
3504.618486	525265.171489	42.392935
3504.555654	525249.816524	42.397940
3504.623947	525238.231538	42.402944
3504.321226	525201.736945	42.407949
3504.504420	525218.185145	42.412954
3504.227863	525194.322141	42.417959
3504.541703	525161.722906	42.422964
3504.514836	525161.575656	42.427968
3504.361994	525138.451162	42.432973
3504.179737	525121.244850	42.437978
3504.013476	525127.639716	42.442983
3504.129985	525095.273708	42.447988
3504.180482	525081.821317	42.452992
3504.392438	525091.441739	42.457997
3504.145409	525080.816260	42.463002
3504.253673	525063.159618	42.468007
3504.439614	525046.299377	42.473012
3504.543648	525047.091763	42.478016
3504.119820	525030.934407	42.483021
3504.543040	524999.884405	42.488026
3504.591472	524995.580670	42.493031
3504.273919	524966.669437	42.498036
3504.373076	524967.563686	42.503040
3504.162184	524953.192170	42.508045
3504.238443	524930.486058	42.513050
3504.034052	524934.460921	42.518055
3504.112685	524923.682776	42.523060
3504.093842	524902.507974	42.528064
3504.059663	524893.162870	42.533069
3504.084436	524886.689454	42.538074
3503.689065	524882.860188	42.543079
3503.987054	524885.997497	42.548084
3504.035371	524851.771646	42.553088
3503.875967	524843.659366	42.558093
3504.434819	524847.564157	42.563098
3504.178817	524842.297617	42.568103
3504.243189	524792.299314	42.573108
3504.125381	524796.563791	42.578112
3503.995357	524807.299867	42.583117
3504.319706	524807.248735	42.588122
3504.370985	524782.474046	42.593127
3504.123021	524763.761405	42.598132
3503.940212	524772.736792	42.603136
3504.060725	524756.796387	42.608141
3504.257915	524734.930140	42.613146
3504.019092	524728.346690	42.618151
3504.012634	524714.700815	42.623156
3504.062275	524717.119242	42.628160
3503.775912	524699.878387	42.633165
3504.075123	524685.324916	42.638170
3504.258175	524680.443828	42.643175
3504.161335	524674.798263	42.648180
3504.008525	524663.348899	42.653184
3504.230555	524639.962254	42.658189
3504.148875	524644.928688	42.663194
3503.955331	524643.240890	42.668199
3504.222001	524623.183122	42.673204
3504.058095	524613.656181	42.678208
3504.210793	524600.591592	42.683213
3504.106774	524606.774648	42.688218
3504.106888	524583.170272	42.693223
3504.353408	524567.664667	42.698228
3504.401244	524557.295505	42.703232
3504.087310	524552.998382	42.708237
3504.395552	524527.929960	42.713242
3504.015402	524527.333093	42.718247
3504.186955	524510.727289	42.723252
3504.139915	524494.257109	42.728256
3504.124055	524489.154677	42.733261
3504.418234	524476.522533	42.738266
3504.059911	524464.397875	42.743271
3504.103407	524441.595160	42.748276
3503.908347	524452.341753	42.753280
3504.006196	524438.426430	42.758285
3504.408908	524440.030911	42.763290
3503.928367	524435.355727	42.768295
3504.306116	524417.756872	42.773300
3504.280931	524400.171141	42.778304
3503.950465	524402.548603	42.783309
3503.836272	524385.179105	42.788314
3503.844377	524376.079746	42.793319
3503.880293	524365.712343	42.798324
3503.837615	524364.809400	42.803329
3503.764271	524380.591369	42.808333
3503.910213	524368.892392	42.813338
3503.737816	524345.618208	42.818343
3503.674438	524341.230880	42.823348
3503.628398	524349.224516	42.828353
3503.687538	524336.932687	42.833357
3504.045184	524331.417348	42.838362
3503.632102	524334.464974	42.843367
3503.886817	524340.439793	42.848372
3503.793092	524331.659778	42.853377
3503.598415	524313.949104	42.858381
3504.028216	524305.237964	42.863386
3503.427489	524311.904008	42.868391
3503.506089	524305.927308	42.873396
3503.605481	524307.731383	42.878401
3503.573166	524301.266754	42.883405
3503.976168	524306.864326	42.888410
3503.771483	524300.831308	42.893415
3504.214634	524305.158888	42.898420
3503.758109	524300.530414	42.903425
3503.978883	524277.143441	42.908429
3504.151658	524273.578049	42.913434
3503.797435	524275.201095	42.918439
3504.072282	524266.514426	42.923444
3504.335237	524255.251785	42.928449
3503.840517	524231.826198	42.933453
3503.942548	524230.900376	42.938458
3503.724616	524230.682225	42.943463
3503.746660	524219.154360	42.948468
3503.849575	524225.759769	42.953473
3503.651680	524223.061692	42.958477
3503.827134	524194.526057	42.963482
3503.848945	524201.093749	42.968487
3504.171911	524195.533299	42.973492
3503.999335	524196.925457	42.978497
3503.873944	524185.117595	42.983501
3504.154348	524178.148572	42.988506
3503.847058	524179.309293	42.993511
3504.312435	524157.248233	42.998516
3504.171506	524151.558906	43.003521
3504.086217	524149.955037	43.008525
3504.213795	524118.242414	43.013530
3504.098900	524127.915077	43.018535
3504.039501	524117.815312	43.023540
3504.027902	524105.938859	43.028545
3504.121152	524083.784877	43.033549
3504.563224	524078.660481	43.038554
3504.088519	524076.865422	43.043559
3503.935569	524048.836355	43.048564
3504.097955	524049.922849	43.053569
3504.070051	524045.327646	43.058573
3504.410818	524031.171390	43.063578
3504.203531	524003.100285	43.068583
3504.091655	523989.824285	43.073588
3503.672645	523989.182991	43.078593
3503.957609	523983.224100	43.083597
3504.043949	523983.261134	43.088602
3503.897994	523969.030113	43.093607
3504.318764	523948.340585	43.098612
3503.691213	523960.166804	43.103617
3503.857636	523955.136485	43.108621
3504.052113	523950.051182	43.113626
3503.869986	523930.114035	43.118631
3503.946450	523913.118268	43.123636
3503.763042	523914.764898	43.128641
3503.791508	523905.864243	43.133645
3503.933025	523916.709634	43.138650
3503.797963	523922.089105	43.143655
3503.947389	523894.972372	43.148660
3504.039332	523885.252917	43.153665
3503.636744	523899.014963	43.158669
3504.244820	523863.182120	43.163674
3503.989987	523873.887998	43.168679
3504.110154	523865.124467	43.173684
3504.066415	523855.375894	43.178689
3504.007979	523841.282568	43.183693
3504.033024	523841.683121	43.188698
3503.978856	523837.597484	43.193703
3504.317264	523819.094343	43.198708
3504.355789	523808.574527	43.203713
3504.018979	523813.278259	43.208717
3504.872853	523773.160383	43.213722
3504.165806	523778.074286	43.218727
3504.548471	523754.610419	43.223732
3504.436740	523752.201928	43.228737
3504.360402	523732.601648	43.233741
3504.568109	523716.343145	43.238746
3504.020207	523693.026273	43.243751
3504.098709	523678.961709	43.248756
3504.226452	523682.479999	43.253761
3504.458720	523676.529325	43.258765
3504.371578	523645.102449	43.263770
3504.429690	523646.407643	43.268775
3504.187102	523620.818300	43.273780
3504.127757	523612.537938	43.278785
3504.115738	523594.645957	43.283789
3504.004446	523589.356131	43.288794
3503.996066	523571.969030	43.293799
3504.345978	523554.727473	43.298804
3504.281927	523566.566008	43.303809
3504.047099	523544.109303	43.308813
3504.195219	523529.427026	43.313818
3504.298429	523533.050323	43.318823
3504.600717	523504.645065	43.323828
3504.293716	523494.280755	43.328833
3504.133716	523488.341465	43.333837
3504.393017	523468.991104	43.338842
3504.352294	523448.020039	43.343847
3504.065255	523434.973462	43.348852
3504.098022	523436.029937	43.353857
3504.048075	523421.429416	43.358861
3504.022440	523403.893216	43.363866
3503.838860	523393.762077	43.368871
3504.094414	523392.761392	43.373876
3504.420439	523385.734269	43.378881
3504.441949	523360.759903	43.383885
3504.579880	523350.426272	43.388890
3504.286886	523342.283799	43.393895
3504.294746	523317.715915	43.398900
3504.336476	523321.348978	43.403905
3503.908593	523303.421307	43.408909
3503.939652	523280.770562	43.413914
3503.966586	523280.210398	43.418919
3504.160630	523267.542587	43.423924
3504.112832	523270.279928	43.428929
3504.094883	523256.937929	43.433933
3503.981877	523243.156000	43.438938
3503.959063	523236.234499	43.443943
3503.988744	523228.344262	43.448948
3503.957379	523224.558160	43.453953
3504.080543	523194.461994	43.458957
3504.139733	523186.213227	43.463962
3504.008113	523184.161640	43.468967
3504.038906	523180.921746	43.473972
3503.879378	523172.050400	43.478977
3503.860646	523165.279871	43.483981
3504.554875	523160.165881	43.488986
3504.290346	523165.919913	43.493991
3504.236437	523138.631850	43.498996
3504.251841	523113.405319	43.504001
3504.259667	523106.630568	43.509005
3504.274825	523102.685435	43.514010
3504.080099	523098.672376	43.519015
3504.169732	523069.642820	43.524020
3504.461059	523076.218921	43.529025
3504.078424	523059.749768	43.534029
3504.211351	523039.256223	43.539034
3503.998066	523037.065876	43.544039
3504.484643	523022.481292	43.549044
3504.231452	522997.751983	43.554049
3504.572106	522999.922472	43.559053
3504.574202	522979.651730	43.564058
3504.288854	522962.459401	43.569063
3504.337622	522944.658192	43.574068
3504.461112	522928.007806	43.579073
3504.150707	522916.784309	43.584077
3504.301585	522905.841745	43.589082
3504.305232	522887.339901	43.594087
3504.228658	522875.068409	43.599092
3504.308864	522864.440290	43.604097
3504.347000	522846.590103	43.609101
3504.149465	522825.289162	43.614106
3504.270132	522833.509953	43.619111
3504.045615	522817.925469	43.624116
3504.328802	522796.599059	43.629121
3504.005425	522776.834462	43.634125
3504.124415	522769.536493	43.639130
3503.895297	522771.695969	43.644135
3504.169908	522753.858854	43.649140
3504.289016	522737.512270	43.654145
3504.229441	522735.600890	43.659149
3504.088383	522718.385494	43.664154
3503.954273	522703.949281	43.669159
3504.279771	522688.530492	43.674164
3504.136196	522694.771082	43.679169
3503.618504	522690.000154	43.684173
3504.296518	522656.226172	43.689178
3503.788419	522664.799185	43.694183
3503.851187	522664.435541	43.699188
3503.847007	522665.396804	43.704193
3504.196695	522654.827055	43.709197
3504.358046	522625.482061	43.714202
3503.923904	522623.377117	43.719207
3504.390443	522616.024145	43.724212
3504.186595	522600.486736	43.729217
3504.236154	522576.416647	43.734221
3504.451678	522572.389164	43.739226
3504.173902	522560.199786	43.744231
3504.188920	522538.409909	43.749236
3504.054570	522534.791577	43.754241
3503.968145	522524.139021	43.759245
3504.233492	522521.923502	43.764250
3503.882601	522505.196008	43.769255
3504.053283	522496.878716	43.774260
3503.934882	522505.845182	43.779265
3503.813178	522500.809401	43.784269
3504.107668	522490.551579	43.789274
3503.719845	522476.559676	43.794279
3503.693198	522458.972060	43.799284
3504.114699	522454.911991	43.804289
3504.142059	522449.903185	43.809293
3504.180826	522447.571815	43.814298
3504.078114	522427.064188	43.819303
3503.909962	522422.389587	43.824308
3504.059869	522397.393439	43.829313
3503.761637	522410.179769	43.834317
3503.898991	522405.153564	43.839322
3503.887530	522384.833668	43.844327
3503.860080	522371.947408	43.849332
3503.684208	522367.880634	43.854337
3503.763696	522371.962909	43.859341
3503.926647	522367.438166	43.864346
3503.884488	522380.639011	43.869351
3503.968981	522362.882068	43.874356
3504.297077	522340.991889	43.879361
3503.821375	522335.961458	43.884365
3503.897248	522334.433038	43.889370
3503.782940	522335.613936	43.894375
3503.995911	522326.582144	43.899380
3503.587367	522305.971048	43.904385
3503.687912	522293.671119	43.909389
3503.842565	522289.046561	43.914394
3503.974267	522289.733609	43.919399
3504.005430	522296.705015	43.924404
3504.209915	522294.195772	43.929409
3504.197018	522280.801617	43.934413
3504.263707	522256.121719	43.939418
3504.216187	522250.518060	43.944423
3504.145642	522232.279956	43.949428
3503.785002	522221.771647	43.954433
3503.721057	522213.491295	43.959437
3504.287200	522210.773219	43.964442
3504.103756	522205.191029	43.969447
3504.221204	522191.675093	43.974452
3504.246547	522166.597173	43.979457
3503.864146	522172.269081	43.984461
3504.169568	522171.108784	43.989466
3504.118987	522160.955849	43.994471
3504.138209	522132.795137	43.999476
3504.073793	522122.694918	44.004481
3504.275606	522122.966469	44.009485
3504.336593	522095.203512	44.014490
3504.109809	522092.560194	44.019495
3504.142219	522086.236105	44.024500
3504.243987	522078.738337	44.029505
3503.999031	522060.224289	44.034509
3504.143188	522037.604482	44.039514
3503.879934	522039.213367	44.044519
3504.382110	522025.383718	44.049524
3504.391821	522010.368071	44.054529
3504.093236	522004.045714	44.059533
3504.380043	521986.104722	44.064538
3504.164786	521979.617526	44.069543
3504.086453	521956.072262	44.074548
3504.244156	521954.429766	44.079553
3504.139721	521942.869716	44.084557
3503.945966	521924.397974	44.089562
3503.733829	521917.303620	44.094567
3503.895176	521913.941731	44.099572
3504.037831	521912.604930	44.104577
3503.882589	521914.348414	44.109581
3504.144766	521884.935591	44.114586
3503.743096	521877.668963	44.119591
3503.552125	521872.087847	44.124596
3503.864391	521867.842686	44.129601
3504.138366	521873.461504	44.134605
3504.069663	521865.737815	44.139610
3503.811617	521860.723385	44.144615
3504.097037	521849.000541	44.149620
3504.056873	521841.120668	44.154625
3503.657709	521840.830018	44.159629
3503.902472	521840.336483	44.164634
3503.655907	521842.953820	44.169639
3503.987141	521831.830365	44.174644
3503.818150	521811.635758	44.179649
3503.530557	521804.502727	44.184653
3503.809977	521791.415841	44.189658
3503.505346	521798.693305	44.194663
3503.686980	521797.855870	44.199668
3503.758333	521794.305966	44.204673
3503.612879	521801.811038	44.209677
3504.164038	521793.281588	44.214682
3503.929060	521788.162382	44.219687
3503.626963	521761.821195	44.224692
3503.835831	521769.775815	44.229697
3503.800823	521762.956719	44.234701
3504.013640	521752.256358	44.239706
3503.827175	521760.121808	44.244711
3503.985959	521745.436230	44.249716
3503.955687	521725.421805	44.254721
3503.814913	521726.151944	44.259725
3504.039337	521708.321614	44.264730
3503.954287	521713.643357	44.269735
3504.234729	521719.918409	44.274740
3503.686627	521696.598682	44.279745
3503.627290	521692.108886	44.284749
3503.840341	521681.054562	44.289754
3503.573003	521686.000695	44.294759
3503.826697	521665.637989	44.299764
3504.044400	521674.147355	44.304769
3503.732158	521686.936467	44.309773
3504.038741	521670.710839	44.314778
3503.713901	521654.433335	44.319783
3503.690429	521634.569385	44.324788
3503.840984	521635.202927	44.329793
3503.755619	521632.132747	44.334797
3503.863788	521626.655926	44.339802
3503.480731	521638.394630	44.344807
3503.796011	521640.670424	44.349812
3503.928847	521639.638477	44.354817
3503.585904	521626.397058	44.359821
3503.980449	521615.971208	44.364826
3503.843634	521603.101623	44.369831
3503.995343	521594.382434	44.374836
3503.971355	521590.190349	44.379841
3503.830106	521600.829218	44.384845
3503.801124	521591.531936	44.389850
3503.704149	521574.055585	44.394855
3503.868065	521552.544176	44.399860
3503.869306	521558.913975	44.404865
3503.660515	521566.075285	44.409869
3504.284352	521551.973234	44.414874
3503.605679	521566.185329	44.419879
3503.771047	521562.114970	44.424884
3503.429192	521544.373966	44.429889
3503.502484	521526.162888	44.434893
3503.887610	521520.187266	44.439898
3503.950952	521527.507798	44.444903
3503.995288	521524.973197	44.449908
3503.980081	521529.020098	44.454913
3503.580363	521522.915755	44.459917
3503.811682	521526.317036	44.464922
3503.605132	521513.610066	44.469927
3503.895466	521490.005856	44.474932
3503.852353	521483.744025	44.479937
3503.718116	521481.540970	44.484941
3503.622053	521473.770863	44.489946
3503.726069	521489.477064	44.494951
3504.046795	521477.798927	44.499956
3503.981990	521484.128640	44.504961
3503.495575	521464.287100	44.509965
3503.743839	521442.964434	44.514970
3503.723527	521445.242744	44.519975
3503.948090	521440.505787	44.524980
3503.678523	521438.374671	44.529985
3503.716604	521445.952007	44.534989
3504.376194	521434.068614	44.539994
3504.313311	521434.634790	44.544999
3504.053154	521413.493556	44.550004
3504.156538	521398.159207	44.555009
3504.139307	521402.105350	44.560013
3504.373912	521385.638040	44.565018
3504.049713	521372.191230	44.570023
3503.811484	521358.376935	44.575028
3503.965309	521363.559927	44.580033
3503.859738	521357.206809	44.585037
3503.917583	521330.403589	44.590042
3503.748811	521329.520406	44.595047
3503.751628	521318.296845	44.600052
3503.648984	521326.199811	44.605057
3503.212273	521320.707901	44.610061
3503.767171	521318.547565	44.615066
3503.665006	521322.557707	44.620071
3503.704034	521326.798306	44.625076
3504.169750	521314.035477	44.630081
3503.811772	521303.930593	44.635085
3504.375544	521285.793387	44.640090
3503.829514	521289.115364	44.645095
3503.916498	521285.006771	44.650100
3504.032024	521286.758080	44.655105
3503.716625	521258.395967	44.660109
3503.954720	521248.045167	44.665114
3503.710596	521239.995018	44.670119
3503.865721	521227.685657	44.675124
3504.444313	521237.149321	44.680129
3504.014967	521230.948440	44.685133
3504.313123	521222.104794	44.690138
3503.864391	521212.014197	44.695143
3503.946539	521202.244128	44.700148
3504.268340	521202.243953	44.705153
3503.993296	521182.115882	44.710157
3504.254528	521162.054689	44.715162
3503.979735	521165.940487	44.720167
3504.141663	521155.045555	44.725172
3504.056970	521139.235133	44.730177
3503.859566	521118.690266	44.735181
3504.393294	521115.977136	44.740186
3503.847813	521122.585188	44.745191
3504.018421	521110.576626	44.750196
3503.948789	521083.034811	44.755201
3503.780860	521081.190918	44.760205
3504.047878	521074.222683	44.765210
3503.687452	521074.482009	44.770215
3503.846513	521070.463081	44.775220
3503.917861	521059.632958	44.780225
3503.623459	521052.045667	44.785229
3503.665700	521046.983522	44.790234
3503.485241	521039.732108	44.795239
3503.283911	521040.977409	44.800244
3503.648289	521042.992747	44.805249
3503.690512	521037.323929	44.810253
3503.812998	521039.933617	44.815258
3503.699973	521042.024414	44.820263
3504.047697	521028.723896	44.825268
3504.194803	521047.254853	44.830273
3503.471660	521029.371328	44.835277
3503.787688	521004.852345	44.840282
3503.764737	521005.108887	44.845287
3504.011681	521008.912256	44.850292
3503.704168	521003.450374	44.855297
3503.760412	520999.346567	44.860301
3503.860879	521009.340942	44.865306
3503.589303	521005.187840	44.870311
3503.537812	521000.848281	44.875316
3503.653884	520974.844172	44.880321
3503.572804	520977.637715	44.885325
3503.942411	520960.643076	44.890330
3503.636387	520975.100120	44.895335
3503.886531	520962.017196	44.900340
3503.787084	520961.274704	44.905345
3503.757802	520971.441279	44.910349
3504.020810	520968.012571	44.915354
3503.815170	520968.500215	44.920359
3504.002810	520933.536264	44.925364
3503.739312	520929.179640	44.930369
3503.710388	520938.486720	44.935373
3503.904283	520917.171960	44.940378
3503.725351	520913.307530	44.945383
3503.722748	520921.700443	44.950388
3503.911085	520931.933759	44.955393
3503.742793	520903.396107	44.960397
3504.067143	520883.375151	44.965402
3503.530560	520892.661385	44.970407
3504.009850	520885.305623	44.975412
3504.047900	520879.940749	44.980417
3504.170249	520880.224883	44.985421
3504.433570	520849.394427	44.990426
3503.875670	520842.505923	44.995431
3504.113105	520836.957850	45.000436
3503.824438	520841.907608	45.005441
3504.015630	520819.935912	45.010445
3504.025637	520806.688593	45.015450
3504.081162	520817.296870	45.020455
3504.348953	520792.684080	45.025460
3504.307381	520792.640227	45.030465
3503.757294	520765.679384	45.035469
3503.890932	520755.193112	45.040474
3503.899335	520752.613513	45.045479
3503.969254	520747.749128	45.050484
3503.829098	520737.407234	45.055489
3503.659317	520728.232827	45.060493
3504.216645	520718.589590	45.065498
3504.030710	520718.366327	45.070503
3504.022452	520726.456892	45.075508
3504.200895	520708.278838	45.080513
3503.647104	520696.435027	45.085517
3503.711115	520675.494381	45.090522
3503.701029	520680.652941	45.095527
3503.560365	520676.782405	45.100532
3503.748012	520680.140210	45.105537
3503.552857	520682.800163	45.110541
3503.583074	520670.611239	45.115546
3503.760018	520680.998186	45.120551
3503.751576	520669.725401	45.125556
3503.655505	520666.403944	45.130561
3503.440772	520651.523633	45.135565
3503.596143	520641.691097	45.140570
3503.578616	520634.363192	45.145575
3503.648786	520644.008678	45.150580
3503.699300	520644.152500	45.155585
3503.593740	520644.118761	45.160589
3504.181260	520632.448409	45.165594
3503.607457	520643.004600	45.170599
3503.705758	520638.540154	45.175604
3503.973184	520640.773097	45.180609
3503.970528	520633.088940	45.185613
3503.830268	520620.370794	45.190618
3503.921755	520608.172139	45.195623
3503.782395	520598.841179	45.200628
3503.760076	520592.120702	45.205633
3503.800993	520600.153000	45.210637
3504.044615	520608.355484	45.215642
3503.587696	520598.316356	45.220647
3503.529905	520572.794104	45.225652
3503.978515	520571.054933	45.230657
3503.680272	520566.754260	45.235661
3503.529338	520577.496442	45.240666
3503.714535	520581.714132	45.245671
3503.771437	520565.526871	45.250676
3503.550565	520570.718782	45.255681
3503.357383	520587.180633	45.260685
3503.890154	520574.507745	45.265690
3503.679560	520573.631130	45.270695
3503.412869	520579.184183	45.275700
3504.017283	520581.515543	45.280705
3503.730071	520551.631019	45.285709
3504.026311	520533.333036	45.290714
3503.609072	520536.988709	45.295719
3503.875193	520535.177263	45.300724
3504.232233	520530.570776	45.305729
3504.083924	520526.246394	45.310733
3504.003635	520502.497106	45.315738
3503.618826	520502.001928	45.320743
3503.573442	520497.914059	45.325748
3504.238656	520488.910885	45.330753
3503.842196	520498.781886	45.335757
3503.823261	520480.280871	45.340762
3503.698847	520469.531857	45.345767
3503.517850	520460.561304	45.350772
3503.853253	520443.116513	45.355777
3503.364727	520448.654116	45.360781
3504.100028	520440.853227	45.365786
3504.077136	520446.721696	45.370791
3503.880043	520451.050402	45.375796
3504.264426	520445.883434	45.380801
3503.685664	520432.273850	45.385805
3504.159247	520403.785543	45.390810
3503.619210	520412.920919	45.395815
3503.826442	520409.096447	45.400820
3503.798583	520410.769398	45.405825
3503.468389	520406.726523	45.410829
3503.843380	520403.431672	45.415834
3503.867173	520400.344005	45.420839
3503.661316	520386.270978	45.425844
3503.734183	520373.771743	45.430849
3503.837607	520376.435110	45.435853
3503.842980	520367.991187	45.440858
3503.395698	520377.566945	45.445863
3503.401287	520372.914849	45.450868
3503.469137	520371.185282	45.455873
3503.349810	520371.103160	45.460877
3503.803193	520377.654746	45.465882
3503.455760	520374.069610	45.470887
3503.630718	520372.575904	45.475892
3503.564756	520377.490601	45.480897
3503.531588	520379.922767	45.485901
3503.818449	520375.832910	45.490906
3503.418509	520379.890349	45.495911
3503.518628	520367.285686	45.500916
3503.633569	520355.032577	45.505921
3503.232466	520363.387648	45.510925
3503.695781	520367.561434	45.515930
3503.493965	520343.881682	45.520935
3503.562905	520343.668686	45.525940
3503.394228	520338.841892	45.530945
3503.354101	520336.927155	45.535949
3503.585817	520338.457969	45.540954
3503.594249	520353.573674	45.545959
3503.474225	520341.559926	45.550964
3503.694390	520343.800380	45.555969
3503.565019	520344.680452	45.560973
3503.810594	520345.804609	45.565978
3503.878644	520353.276599	45.570983
3503.830448	520357.885145	45.575988
3503.305324	520356.148185	45.580993
3503.533285	520348.478001	45.585997
3503.499845	520353.539240	45.591002
3503.716325	520347.741522	45.596007
3503.872382	520353.025600	45.601012
3503.803186	520345.099034	45.606017
3503.471841	520332.663657	45.611021
3503.795669	520316.282284	45.616026
3503.673699	520321.155293	45.621031
3503.867642	520313.389352	45.626036
3503.827199	520307.834464	45.631041
3503.935087	520309.435411	45.636045
3503.945878	520319.393825	45.641050
3503.794256	520324.524310	45.646055
3504.016266	520285.003294	45.651060
3503.949660	520284.558930	45.656065
3503.734123	520283.885313	45.661069
3504.229499	520277.183997	45.666074
3503.923189	520285.423007	45.671079
3503.908675	520264.342571	45.676084
3503.911398	520236.787891	45.681089
3503.514639	520242.361617	45.686093
3504.109641	520224.420535	45.691098
3503.813246	520243.932559	45.696103
3503.675918	520233.741574	45.701108
3504.138583	520233.516903	45.706113
3503.836314	520222.644162	45.711117
3503.882321	520193.818603	45.716122
3503.762620	520190.500784	45.721127
3504.246227	520193.710793	45.726132
3503.812011	520188.875366	45.731137
3504.035972	520180.295679	45.736141
3504.237985	520161.253794	45.741146
3503.679672	520155.629031	45.746151
3504.030048	520143.692463	45.751156
3503.891523	520147.354728	45.756161
3503.848223	520144.227058	45.761165
3503.657591	520125.146074	45.766170
3503.660953	520114.679983	45.771175
3503.762593	520106.422945	45.776180
3504.126821	520109.297927	45.781185
3503.590912	520110.596181	45.786189
3503.825853	520115.160042	45.791194
3503.665395	520113.719329	45.796199
3503.836126	520115.462039	45.801204
3504.026468	520095.410743	45.806209
3503.562822	520078.142421	45.811213
3503.759027	520067.898614	45.816218
3503.793391	520068.752821	45.821223
3503.921083	520058.722074	45.826228
3504.047666	520075.083338	45.831233
3503.586900	520064.538898	45.836237
3503.922329	520057.508859	45.841242
3503.604231	520039.256868	45.846247
3503.385466	520028.269680	45.851252
3503.866921	520025.867992	45.856257
3503.537781	520031.633337	45.861261
3503.896671	520018.835827	45.866266
3503.543258	520039.519969	45.871271
3503.824615	520035.532017	45.876276
3504.124291	520031.035576	45.881281
3503.824854	520022.841891	45.886285
3503.981142	520006.233894	45.891290
3504.116523	519987.404575	45.896295
3503.842683	519984.464992	45.901300
3503.538112	519991.338773	45.906305
3503.604585	519986.626384	45.911309
3503.634312	519986.267904	45.916314
3503.803895	519991.651079	45.921319
3503.742570	519983.520856	45.926324
3503.874392	519962.164104	45.931329
3503.839655	519966.972870	45.936333
3503.652536	519958.407483	45.941338
3503.374031	519961.586320	45.946343
3503.425613	519950.606908	45.951348
3503.863572	519952.964671	45.956353
3503.653439	519961.845914	45.961357
3503.783783	519951.915802	45.966362
3503.492993	519956.916720	45.971367
3503.776942	519952.169947	45.976372
3503.968922	519960.684277	45.981377
3503.745138	519944.945242	45.986381
3503.918089	519914.177867	45.991386
3503.690704	519925.438156	45.996391
3503.987578	519926.453115	46.001396
3503.836366	519917.022519	46.006401
3503.709040	519919.874112	46.011405
3504.074073	519914.558357	46.016410
3503.959868	519901.329937	46.021415
3503.762012	519884.322756	46.026420
3503.959361	519872.662977	46.031425
3503.559813	519875.810403	46.036429
3504.078593	519869.762497	46.041434
3503.775694	519876.636062	46.046439
3503.656484	519856.734521	46.051444
3504.006832	519837.871053	46.056449
3503.500526	519844.372303	46.061453
3503.898048	519829.748388	46.066458
3503.733256	519842.161716	46.071463
3503.904054	519839.050707	46.076468
3504.116327	519833.607392	46.081473
3504.188229	519828.590741	46.086477
3503.921928	519812.959419	46.091482
3503.592498	519809.978031	46.096487
3503.894794	519797.391533	46.101492
3503.876809	519811.349036	46.106497
3503.645800	519805.925218	46.111501
3503.757740	519789.981290	46.116506
3503.865699	519773.734616	46.121511
3503.412437	519768.295354	46.126516
3503.595253	519749.508824	46.131521
3503.114776	519754.893706	46.136525
3503.584914	519763.616973	46.141530
3503.832899	519755.387187	46.146535
3503.571177	519766.400211	46.151540
3503.732572	519757.577393	46.156545
3503.628372	519759.919758	46.161549
3503.862904	519760.034501	46.166554
3503.564584	519759.020027	46.171559
3503.887514	519760.789279	46.176564
3503.881095	519753.105303	46.181569
3503.692814	519764.359521	46.186573
3503.639769	519730.695042	46.191578
3503.778447	519717.325383	46.196583
3503.633597	519720.432580	46.201588
3503.896504	519732.677268	46.206593
3503.607131	519724.127920	46.211597
3503.805472	519710.647705	46.216602
3503.717147	519727.902807	46.221607
3503.837092	519731.827671	46.226612
3503.886426	519711.899314	46.231617
3503.372181	519701.919253	46.236621
3503.499896	519685.517688	46.241626
3503.539447	519682.629636	46.246631
3503.311753	519678.519818	46.251636
3503.248661	519688.591414	46.256641
3503.189333	519714.184385	46.261645
3503.665217	519722.755085	46.266650
3503.731072	519723.098731	46.271655
3503.597936	519713.210119	46.276660
3503.676128	519688.524517	46.281665
3503.556719	519684.448144	46.286669
3503.731142	519683.763425	46.291674
3503.479933	519688.353687	46.296679
3503.722604	519689.124428	46.301684
3503.678433	519684.783363	46.306689
3503.277716	519693.189272	46.311693
3503.863314	519685.057769	46.316698
3503.738256	519689.223609	46.321703
3503.721414	519686.243351	46.326708
3503.889796	519679.188994	46.331713
3503.664428	519696.263550	46.336717
3503.584004	519676.203979	46.341722
3503.662125	519674.118793	46.346727
3503.674640	519654.853470	46.351732
3503.703981	519653.180475	46.356737
3503.529966	519662.460654	46.361741
3503.745728	519647.612504	46.366746
3503.786920	519650.791430	46.371751
3503.923844	519648.949748	46.376756
3504.180651	519644.459979	46.381761
3503.728514	519646.503432	46.386765
3504.044662	519614.196049	46.391770
3503.905288	519610.274495	46.396775
3503.808090	519598.206033	46.401780
3503.619274	519599.500024	46.406785
3503.324538	519614.917132	46.411789
3503.618290	519601.017262	46.416794
3503.632402	519611.329505	46.421799
3503.827596	519616.557075	46.426804
3503.441762	519611.916070	46.431809
3503.522947	519631.166901	46.436813
3503.705899	519603.936592	46.441818
3503.406251	519593.214698	46.446823
3503.602373	519578.976317	46.451828
3503.644458	519575.733922	46.456833
3503.295195	519571.441049	46.461837
3504.086980	519570.557624	46.466842
3503.816855	519577.830618	46.471847
3503.535928	519573.274142	46.476852
3503.792047	519572.677627	46.481857
3503.551792	519570.491069	46.486861
3503.657033	519569.766720	46.491866
3503.622943	519571.693544	46.496871
3503.598760	519570.332364	46.501876
3503.717775	519568.695747	46.506881
3503.492688	519583.444588	46.511885
3503.664894	519572.496417	46.516890
3503.594191	519567.805590	46.521895
3503.547652	519548.043870	46.526900
3503.501304	519537.180781	46.531905
3503.577620	519541.314830	46.536909
3503.673191	519540.035840	46.541914
3503.628837	519536.604857	46.546919
3503.603144	519527.710365	46.551924
3503.712925	519526.125763	46.556929
3503.596899	519538.784416	46.561933
3503.525107	519538.593654	46.566938
3503.792482	519541.534607	46.571943
3503.513114	519539.050863	46.576948
3503.771017	519539.869764	46.581953
3503.361901	519542.310916	46.586957
3503.875016	519541.673779	46.591962
3503.626037	519539.084110	46.596967
3503.574519	519548.092188	46.601972
3503.828780	519526.867199	46.606977
3503.446274	519506.096755	46.611981
3503.503112	519502.043040	46.616986
3503.461052	519504.325058	46.621991
3503.400731	519495.941630	46.626996
3503.761277	519508.828344	46.632001
3503.594570	519511.787353	46.637005
3503.604862	519508.246604	46.642010
3503.532316	519507.297550	46.647015
3503.515757	519503.255436	46.652020
3503.726497	519512.171521	46.657025
3503.488249	519514.231743	46.662029
3503.766724	519497.502797	46.667034
3503.777982	519502.001064	46.672039
3503.553808	519507.446637	46.677044
3503.917346	519498.692850	46.682049
3503.693954	519516.576254	46.687053
3504.228749	519484.992469	46.692058
3503.858991	519474.686067	46.697063
3503.724921	519461.460431	46.702068
3504.216030	519455.517870	46.707073
3504.073832	519458.725820	46.712077
3504.371526	519440.123022	46.717082
3504.216424	519425.181607	46.722087
3504.106317	519420.952016	46.727092
3503.905308	519393.832608	46.732097
3503.900580	519382.002177	46.737101
3504.326904	519384.564107	46.742106
3504.195836	519381.045675	46.747111
3503.936538	519380.783426	46.752116
3503.902248	519357.985869	46.757121
3503.974899	519355.952069	46.762125
3503.977606	519363.586523	46.767130
3504.018736	519364.641942	46.772135
3503.756706	519350.779147	46.777140
3503.534435	519328.314628	46.782145
3503.705935	519320.652889	46.787149
3504.145737	519305.010598	46.792154
3503.852105	519310.517775	46.797159
3503.599866	519314.451006	46.802164
3504.028417	519303.816068	46.807169
3504.143863	519318.359638	46.812173
3504.132496	519292.828053	46.817178
3503.761568	519273.521766	46.822183
3504.000169	519270.956110	46.827188
3504.002399	519274.242390	46.832193
3503.817285	519278.165019	46.837197
3503.963598	519254.175857	46.842202
3503.909712	519236.993563	46.847207
3503.977929	519229.954846	46.852212
3503.934781	519211.709034	46.857217
3503.770368	519220.381204	46.862221
3503.797825	519212.691621	46.867226
3503.818061	519203.587447	46.872231
3503.904455	519197.203146	46.877236
3504.066869	519182.716941	46.882241
3503.734790	519185.651585	46.887245
3504.134593	519179.925605	46.892250
3503.697643	519190.006037	46.897255
3503.680966	519169.986332	46.902260
3503.755001	519155.716320	46.907265
3503.702729	519153.196622	46.912269
3503.706838	519144.448897	46.917274
3503.451971	519141.910657	46.922279
3503.747261	519147.223680	46.927284
3503.996862	519140.661875	46.932289
3503.765200	519149.850331	46.937293
3503.803462	519136.243261	46.942298
3503.588888	519135.063824	46.947303
3503.684342	519134.593812	46.952308
3503.929261	519103.762981	46.957313
3503.532329	519104.533723	46.962317
3503.664016	519097.636603	46.967322
3503.222250	519107.414475	46.972327
3503.749627	519097.522215	46.977332
3503.729946	519102.328854	46.982337
3503.408315	519100.205657	46.987341
3503.522020	519089.822595	46.992346
3503.618782	519100.678278	46.997351
3503.393554	519105.820777	47.002356
3503.752052	519095.196778	47.007361
3503.449720	519109.452633	47.012365
3503.744860	519095.349869	47.017370
3503.704908	519107.744018	47.022375
3503.656840	519103.605663	47.027380
3503.705951	519105.873325	47.032385
3503.959791	519092.889452	47.037389
3503.647565	519067.961253	47.042394
3503.756598	519074.163296	47.047399
3503.769884	519065.768014	47.052404
3504.128992	519064.042836	47.057409
3503.919539	519074.744688	47.062413
3503.799498	519062.123259	47.067418
3503.664431	519042.172673	47.072423
3503.876989	519027.425595	47.077428
3504.059929	519033.160911	47.082433
3503.628676	519037.779811	47.087437
3503.929665	519024.636744	47.092442
3503.972472	519028.220034	47.097447
3504.034809	519010.766321	47.102452
3504.097180	518988.509159	47.107457
3504.066329	518991.547912	47.112461
3504.180387	518981.265851	47.117466
3503.780687	518971.975111	47.122471
3503.602785	518956.733499	47.127476
3503.995979	518940.744292	47.132481
3503.721712	518947.006968	47.137485
3503.848485	518937.734119	47.142490
3503.691488	518934.219689	47.147495
3503.385925	518936.897373	47.152500
3503.769192	518942.601057	47.157505
3504.032424	518944.531523	47.162509
3504.055583	518917.375896	47.167514
3503.742586	518906.605100	47.172519
3503.721273	518896.142131	47.177524
3503.948870	518896.308542	47.182529
3503.628307	518903.336991	47.187533
3503.774687	518904.274679	47.192538
3503.819474	518906.441927	47.197543
3503.577273	518905.620778	47.202548
3503.744115	518898.364080	47.207553
3503.806576	518889.910373	47.212557
3504.064385	518864.891766	47.217562
3503.699083	518862.724878	47.222567
3503.720481	518863.581196	47.227572
3504.011181	518854.939707	47.232577
3503.584161	518864.867080	47.237581
3503.768713	518843.449976	47.242586
3503.719737	518841.637588	47.247591
3503.524676	518818.814132	47.252596
3503.700316	518821.668589	47.257601
3503.721831	518816.962972	47.262605
3503.507763	518812.800218	47.267610
3503.610187	518808.739127	47.272615
3503.521271	518806.933049	47.277620
3503.664038	518808.275816	47.282625
3503.610156	518809.144036	47.287629
3503.707592	518813.274930	47.292634
3503.731578	518810.844252	47.297639
3503.775352	518817.714025	47.302644
3503.938294	518798.626173	47.307649
3503.659052	518815.912409	47.312653
3503.977133	518763.883499	47.317658
3503.651675	518800.188766	47.322663
3503.686358	518766.660133	47.327668
3503.805711	518782.568762	47.332673
3503.879550	518760.360041	47.337677
3503.838892	518786.811078	47.342682
3503.869449	518771.890287	47.347687
3503.790038	518756.632921	47.352692
3503.711278	518735.004480	47.357697
3503.943282	518740.529891	47.362701
3504.163366	518724.517273	47.367706
3504.031649	518727.369765	47.372711
3503.627623	518732.237262	47.377716
3504.086306	518713.962141	47.382721
3503.697875	518695.517515	47.387725
3503.636345	518699.420747	47.392730
3503.812114	518693.527757	47.397735
3503.933041	518700.082005	47.402740
3503.633465	518696.539496	47.407745
3503.815268	518702.730178	47.412749
3503.827721	518686.093018	47.417754
3503.784659	518674.369263	47.422759
3503.145263	518670.273701	47.427764
3503.737579	518650.055978	47.432769
3503.683645	518659.873940	47.437773
3503.923697	518660.493455	47.442778
3503.555132	518662.321563	47.447783
3503.711116	518665.179155	47.452788
3503.955047	518654.219038	47.457793
3503.677153	518667.561270	47.462797
3503.532098	518651.656858	47.467802
3503.653127	518659.323501	47.472807
3503.682020	518655.476249	47.477812
3503.556681	518624.905298	47.482817
3503.485848	518627.697621	47.487821
3503.710830	518625.487963	47.492826
3503.617449	518624.744403	47.497831
3503.730645	518619.569166	47.502836
3504.019866	518627.108113	47.507841
3503.674296	518625.140327	47.512845
3504.050656	518611.529947	47.517850
3503.676783	518626.151472	47.522855
3503.441586	518626.441598	47.527860
3503.731383	518608.395308	47.532865
3503.895608	518596.234225	47.537869
3504.118924	518582.294066	47.542874
3503.882086	518571.763830	47.547879
3503.722715	518574.064519	47.552884
3503.905997	518574.844702	47.557889
3503.903363	518575.047506	47.562893
3504.159982	518558.169370	47.567898
3503.946523	518553.399689	47.572903
3504.023720	518538.774697	47.577908
3504.276270	518535.347139	47.582913
3503.960871	518528.217066	47.587917
3503.879899	518504.869502	47.592922
3503.938535	518500.309618	47.597927
3503.886528	518491.368160	47.602932
3504.063647	518492.301013	47.607937
3503.617643	518488.225400	47.612941
3503.805790	518461.042943	47.617946
3503.703235	518456.457960	47.622951
3503.587549	518456.880891	47.627956
3503.985862	518446.755823	47.632961
3504.085412	518449.268425	47.637965
3503.886571	518442.625531	47.642970
3503.523724	518457.649974	47.647975
3503.715250	518441.186519	47.652980
3503.953591	518408.282299	47.657985
3503.712037	518403.314759	47.662989
3503.632070	518406.007434	47.667994
3503.695882	518405.643532	47.672999
3503.600283	518408.894884	47.678004
3503.627948	518405.957922	47.683009
3503.295632	518411.471513	47.688013
3503.674047	518412.170297	47.693018
3503.317829	518409.546833	47.698023
3503.537842	518401.877000	47.703028
3503.759651	518407.960341	47.708033
3503.502379	518428.075105	47.713037
3503.762804	518422.219201	47.718042
3503.870240	518419.117941	47.723047
3503.444323	518396.330387	47.728052
3503.739638	518371.507361	47.733057
3503.263569	518390.493775	47.738061
3503.562780	518370.220910	47.743066
3503.542941	518375.583994	47.748071
3503.561121	518367.693225	47.753076
3504.123232	518371.700219	47.758081
3503.770360	518379.846412	47.763085
3503.714300	518372.928101	47.768090
3503.899365	518369.106661	47.773095
3503.599312	518375.474757	47.778100
3503.921775	518369.710158	47.783105
3504.022619	518344.917830	47.788109
3504.278239	518336.837823	47.793114
3503.957221	518325.865655	47.798119
3503.851599	518327.197159	47.803124
3504.079208	518314.671899	47.808129
3503.866621	518300.345320	47.813133
3503.652001	518285.614534	47.818138
3503.888695	518284.667094	47.823143
3503.957401	518284.808062	47.828148
3503.908091	518288.254379	47.833153
3503.729961	518286.664602	47.838157
3503.876918	518257.263479	47.843162
3503.827450	518256.512962	47.848167
3503.620912	518247.595797	47.853172
3504.066752	518243.075770	47.858177
3503.868931	518235.522467	47.863181
3504.018440	518237.420428	47.868186
3504.020209	518229.683881	47.873191
3504.021331	518214.059330	47.878196
3504.110480	518204.134675	47.883201
3504.014332	518204.099441	47.888205
3503.829765	518194.521432	47.893210
3503.972757	518174.930363	47.898215
3503.735402	518170.568867	47.903220
3503.807436	518154.579098	47.908225
3503.431989	518161.768231	47.913229
3503.490094	518160.545622	47.918234
3503.743604	518156.612186	47.923239
3503.749579	518158.027193	47.928244
3503.837629	518151.035446	47.933249
3503.573709	518161.898194	47.938253
3503.623199	518149.653787	47.943258
3503.754822	518160.909101	47.948263
3503.482295	518145.529998	47.953268
3503.992503	518112.228262	47.958273
3503.645840	518110.968497	47.963277
3503.976148	518114.860498	47.968282
3503.873980	518111.590050	47.973287
3503.723026	518109.692570	47.978292
3503.834308	518105.832167	47.983297
3503.644613	518121.132938	47.988301
3503.781540	518101.542741	47.993306
3503.701020	518082.897063	47.998311
3503.693310	518072.734813	48.003316
3503.946874	518076.638953	48.008321
3503.307932	518078.509860	48.013325
3503.536691	518074.378055	48.018330
3503.768787	518069.942331	48.023335
3504.095145	518072.216880	48.028340
3503.910934	518076.038520	48.033345
3503.685398	518065.809564	48.038349
3503.903911	518050.908977	48.043354
3504.071799	518049.669007	48.048359
3503.648390	518041.139966	48.053364
3503.934327	518041.297166	48.058369
3503.865091	518043.887073	48.063373
3503.670560	518042.754952	48.068378
3503.574797	518038.017084	48.073383
3503.804725	518032.115298	48.078388
3503.925374	518006.459720	48.083393
3503.906461	518005.350404	48.088397
3504.033906	518008.364318	48.093402
3504.231729	518005.804913	48.098407
3503.591964	517985.477731	48.103412
3503.835853	517969.511184	48.108417
3503.557062	517965.206748	48.113421
3503.690972	517962.859701	48.118426
3504.005969	517959.219892	48.123431
3503.741396	517964.419530	48.128436
3503.906177	517965.354363	48.133441
3503.668229	517960.942340	48.138445
3503.599400	517966.717824	48.143450
3503.743422	517958.554141	48.148455
3503.797524	517943.123222	48.153460
3503.584819	517933.094418	48.158465
3503.788560	517923.151482	48.163469
3503.900770	517918.835798	48.168474
3503.722489	517927.611970	48.173479
3503.708369	517921.141931	48.178484
3503.937818	517919.133737	48.183489
3503.574684	517921.921814	48.188493
3503.911940	517914.334354	48.193498
3503.944494	517892.586082	48.198503
3503.639108	517879.790778	48.203508
3503.915605	517871.757811	48.208513
3503.777939	517873.802336	48.213517
3503.682029	517875.941394	48.218522
3503.637964	517879.993756	48.223527
3503.751088	517877.144325	48.228532
3503.947869	517866.342836	48.233537
3503.460381	517858.278920	48.238541
3503.315687	517842.778198	48.243546
3503.654666	517840.499852	48.248551
3503.713261	517841.704306	48.253556
3503.629622	517828.418819	48.258561
3503.956532	517836.508398	48.263565
3503.845043	517836.273324	48.268570
3503.903500	517839.904964	48.273575
3503.679890	517846.716273	48.278580
3503.692993	517833.213236	48.283585
3503.621702	517837.017083	48.288589
3503.447328	517819.599524	48.293594
3503.864681	517817.055958	48.298599
3503.525831	517800.473432	48.303604
3503.466298	517786.779573	48.308609
3503.695431	517791.901229	48.313613
3503.822698	517798.353702	48.318618
3503.703237	517792.456490	48.323623
3503.668252	517788.770830	48.328628
3503.834582	517780.704666	48.333633
3503.565125	517796.473439	48.338637
3503.670817	517790.945166	48.343642
3503.952952	517793.378443	48.348647
3503.565282	517788.990038	48.353652
3503.382510	517765.606952	48.358657
3503.484574	517756.387913	48.363661
3503.429246	517751.845835	48.368666
3503.573255	517762.391536	48.373671
3503.450540	517760.792949	48.378676
3503.270291	517746.258513	48.383681
3503.297730	517764.255868	48.388685
3503.585591	517786.206763	48.393690
3503.412770	517793.364028	48.398695
3503.486016	517792.644660	48.403700
3503.698053	517787.554672	48.408705
3503.505034	517768.926421	48.413709
3503.549868	517764.368515	48.418714
3503.592712	517759.659225	48.423719
3503.685593	517766.572240	48.428724
3503.989961	517748.623841	48.433729
3503.828386	517763.768800	48.438733
3503.787632	517761.853861	48.443738
3503.925699	517753.842717	48.448743
3503.795177	517755.835562	48.453748
3503.572503	517730.183255	48.458753
3503.374284	517729.253960	48.463757
3503.877069	517721.134587	48.468762
3503.890974	517712.435120	48.473767
3503.698965	517714.134291	48.478772
3503.665261	517716.111837	48.483777
3503.621649	517726.130988	48.488781
3503.866897	517718.557982	48.493786
3504.143342	517703.951323	48.498791
3504.009938	517708.725777	48.503796
3503.741864	517689.451938	48.508801
3503.778085	517675.136056	48.513805
3503.873331	517675.930197	48.518810
3503.757851	517679.842198	48.523815
3503.268005	517681.689581	48.528820
3503.783921	517667.297871	48.533825
3503.671592	517680.058498	48.538829
3503.350948	517681.828571	48.543834
3503.642350	517679.406024	48.548839
3503.893714	517672.388261	48.553844
3504.150095	517659.352294	48.558849
3503.763317	517647.277605	48.563853
3503.619877	517631.776486	48.568858
3503.730650	517628.371151	48.573863
3503.787734	517631.547955	48.578868
3503.887337	517631.127813	48.583873
3503.907298	517628.141364	48.588877
3503.698599	517612.043743	48.593882
3504.195540	517599.475371	48.598887
3503.588973	517588.092745	48.603892
3503.755073	517582.908822	48.608897
3503.744427	517589.231475	48.613901
3503.911358	517569.484205	48.618906
3504.158385	517581.075641	48.623911
3503.509500	517568.233255	48.628916
3503.981158	517546.769090	48.633921
3503.781929	517542.300266	48.638925
3503.881773	517535.812063	48.643930
3503.986350	517544.644863	48.648935
3503.554057	517539.757777	48.653940
3503.922281	517540.053676	48.658945
3503.544021	517545.170281	48.663949
3503.837627	517519.132641	48.668954
3504.044352	517502.766984	48.673959
3503.554854	517508.204583	48.678964
3503.618200	517488.271321	48.683969
3503.541781	517507.448413	48.688973
3503.272356	517495.607898	48.693978
3503.616677	517497.272885	48.698983
3503.392985	517504.842852	48.703988
3503.831863	517488.693321	48.708993
3503.663571	517498.176079	48.713997
3503.788675	517502.201795	48.719002
3504.043976	517493.969728	48.724007
3503.639301	517472.896816	48.729012
3503.818447	517460.934808	48.734017
3503.605451	517456.417570	48.739021
3503.481309	517457.296966	48.744026
3503.699790	517454.481377	48.749031
3503.394625	517458.777380	48.754036
3503.535632	517453.597383	48.759041
3503.576901	517458.243166	48.764045
3503.599562	517459.402761	48.769050
3503.821715	517451.024210	48.774055
3503.330896	517461.316475	48.779060
3503.734018	517452.454218	48.784065
3503.683346	517461.766705	48.789069
3503.648353	517453.024264	48.794074
3503.719274	517463.430007	48.799079
3503.779435	517450.222621	48.804084
3503.776697	517426.507196	48.809089
3503.886593	517424.113302	48.814093
3503.445098	517413.210135	48.819098
3503.876870	517410.360825	48.824103
3503.730493	517414.834011	48.829108
3503.896183	517399.182678	48.834113
3503.789699	517416.392504	48.839117
3503.918435	517405.095797	48.844122
3503.754261	517400.419126	48.849127
3503.350941	517394.718339	48.854132
3503.652689	517381.371579	48.859137
3503.723951	517390.310862	48.864141
3503.648926	517386.783143	48.869146
3504.037641	517379.794114	48.874151
3503.627375	517388.101567	48.879156
3503.640824	517387.695036	48.884161
3503.218844	517387.458464	48.889165
3503.414864	517382.876557	48.894170
3503.597798	517381.330757	48.899175
3503.607191	517391.190030	48.904180
3503.807180	517384.079131	48.909185
3503.685188	517390.571161	48.914189
3503.760390	517367.247871	48.919194
3503.750444	517350.966878	48.924199
3503.659644	517352.650088	48.929204
3503.706707	517344.400294	48.934209
3503.580301	517341.740333	48.939213
3503.813949	517340.338215	48.944218
3503.885431	517340.074213	48.949223
3503.520676	517343.418883	48.954228
3504.065183	517324.673558	48.959233
3504.057838	517334.232106	48.964237
3503.895819	517317.418874	48.969242
3503.973897	517304.309675	48.974247
3503.891556	517302.047284	48.979252
3503.934034	517299.158352	48.984257
3503.731781	517302.123373	48.989261
3503.688898	517291.713364	48.994266
3503.792282	517270.357618	48.999271
3503.663660	517262.186119	49.004276
3503.606057	517263.307847	49.009281
3503.862223	517257.249936	49.014285
3503.671501	517252.880825	49.019290
3503.708541	517248.728551	49.024295
3503.589634	517259.417265	49.029300
3503.776334	517263.888413	49.034305
3503.630880	517259.360445	49.039309
3503.836752	517254.422972	49.044314
3503.777784	517232.587162	49.049319
3503.676989	517219.000491	49.054324
3503.745497	517220.709102	49.059329
3503.667122	517214.653485	49.064333
3503.499906	517216.803898	49.069338
3503.781753	517217.770839	49.074343
3503.544851	517218.111824	49.079348
3503.713224	517216.770581	49.084353
3503.730988	517220.914468	49.089357
3504.128374	517212.508100	49.094362
3503.906881	517203.441030	49.099367
3503.498209	517187.475739	49.104372
3503.721461	517171.410549	49.109377
3503.682903	517171.871889	49.114381
3503.473517	517181.209620	49.119386
3503.359343	517164.135831	49.124391
3503.473813	517171.601931	49.129396
3504.056964	517164.632647	49.134401
3503.608912	517175.070033	49.139405
3503.764032	517166.246823	49.144410
3503.752391	517167.108452	49.149415
3503.576222	517177.755702	49.154420
3503.990916	517160.547748	49.159425
3503.797353	517147.177953	49.164429
3503.547384	517135.637513	49.169434
3503.809112	517135.090597	49.174439
3503.473091	517144.954045	49.179444
3503.673422	517131.623114	49.184449
3503.420852	517136.062592	49.189453
3503.629453	517132.692261	49.194458
3503.632759	517133.399825	49.199463
3503.467096	517133.830688	49.204468
3503.642228	517138.404834	49.209473
3503.485734	517134.131418	49.214477
3503.648117	517132.993387	49.219482
3503.656263	517137.138815	49.224487
3503.568108	517139.883558	49.229492
3503.903884	517132.953361	49.234497
3503.610866	517106.805525	49.239501
3503.666120	517095.014540	49.244506
3503.796927	517098.634908	49.249511
3503.343370	517107.910137	49.254516
3503.481552	517099.089569	49.259521
3503.592233	517096.139253	49.264525
3503.626586	517090.672592	49.269530
3503.853307	517094.378936	49.274535
3503.752694	517100.159746	49.279540
3504.062492	517093.941594	49.284545
3503.776723	517092.924964	49.289549
3503.978813	517081.363602	49.294554
3503.789967	517056.412858	49.299559
3503.672251	517052.942384	49.304564
3504.049853	517043.780533	49.309569
3503.708107	517050.914251	49.314573
3503.686442	517049.855874	49.319578
3503.715775	517049.143414	49.324583
3503.412269	517055.360856	49.329588
3503.482783	517045.792430	49.334593
3503.397800	517060.521378	49.339597
3503.868219	517050.434630	49.344602
3504.005514	517019.515785	49.349607
3503.528764	517003.105959	49.354612
3503.458841	517009.589909	49.359617
3503.454716	517024.407245	49.364621
3503.725231	517010.862850	49.369626
3503.758586	517009.441795	49.374631
3503.810805	517009.534811	49.379636
3503.476943	517008.525778	49.384641
3503.469753	517016.264020	49.389645
3503.634426	517013.557998	49.394650
3503.975188	517012.695176	49.399655
3503.878532	516997.590615	49.404660
3503.733477	516980.420380	49.409665
3503.829128	516983.136096	49.414669
3503.691989	516973.297039	49.419674
3503.702679	516967.884646	49.424679
3503.361886	516969.455703	49.429684
3503.738214	516958.422969	49.434689
3503.294714	516969.567725	49.439693
3503.729421	516973.038948	49.444698
3503.975871	516963.644940	49.449703
3503.507053	516964.679979	49.454708
3503.730815	516969.701603	49.459713
3503.452298	516962.767294	49.464717
3503.726617	516958.981992	49.469722
3503.688578	516943.766980	49.474727
3503.458851	516931.970355	49.479732
3503.954618	516929.414261	49.484737
3503.723829	516918.275187	49.489741
3503.654761	516931.383535	49.494746
3503.710134	516926.065202	49.499751
3503.678223	516935.779569	49.504756
3503.546829	516925.787869	49.509761
3503.576495	516929.323123	49.514765
3503.675568	516927.487124	49.519770
3503.623122	516920.163084	49.524775
3503.699299	516921.971651	49.529780
3503.701195	516908.975318	49.534785
3503.604372	516894.123533	49.539789
3503.761023	516891.216484	49.544794
3503.671258	516891.331944	49.549799
3503.560266	516892.563273	49.554804
3503.674327	516884.808348	49.559809
3503.772020	516877.460557	49.564813
3503.632565	516889.821530	49.569818
3503.658161	516890.019893	49.574823
3503.613458	516892.504964	49.579828
3503.887340	516882.095198	49.584833
3503.776782	516882.669064	49.589837
3503.441443	516878.828401	49.594842
3504.034654	516854.714548	49.599847
3503.809783	516840.944903	49.604852
3504.002369	516844.100441	49.609857
3503.733729	516847.227742	49.614861
3503.830471	516835.935705	49.619866
3503.931275	516844.466061	49.624871
3503.800293	516824.663855	49.629876
3504.014517	516795.350641	49.634881
3503.889995	516804.725739	49.639885
3503.988651	516808.907512	49.644890
3504.150079	516795.279046	49.649895
3504.273709	516786.966303	49.654900
3504.104912	516762.365931	49.659905
3503.835807	516778.236754	49.664909
3504.118972	516761.049176	49.669914
3503.883014	516749.506252	49.674919
3503.747705	516739.110504	49.679924
3503.742635	516721.462752	49.684929
3503.820766	516720.944843	49.689933
3503.721994	516727.736878	49.694938
3503.983001	516726.380954	49.699943
3503.648413	516726.787958	49.704948
3503.732882	516714.132407	49.709953
3503.816217	516730.756678	49.714957
3503.735930	516704.473443	49.719962
3503.852968	516691.256463	49.724967
3503.615241	516687.147478	49.729972
3504.240165	516671.372303	49.734977
3503.969077	516670.606173	49.739981
3503.660232	516680.162184	49.744986
3503.917366	516657.112556	49.749991
3503.749209	516650.868645	49.754996
3503.960607	516644.210753	49.760001
3503.909024	516637.796704	49.765005
3503.891968	516637.040990	49.770010
3504.035685	516637.574673	49.775015
3503.626135	516626.109670	49.780020
3503.343775	516599.655930	49.785025
3503.562977	516598.913441	49.790029
3503.870753	516595.122768	49.795034
3504.142687	516584.814264	49.800039
3504.011931	516591.914829	49.805044
3503.826423	516583.448567	49.810049
3504.069211	516581.185256	49.815053
3503.956134	516564.666944	49.820058
3503.897667	516552.842979	49.825063
3503.571308	516552.186719	49.830068
3503.670213	516544.585741	49.835073
3503.821281	516549.821262	49.840077
3503.402103	516548.825685	49.845082
3503.891695	516556.890178	49.850087
3503.717602	516557.423527	49.855092
3503.717411	516536.184348	49.860097
3503.541427	516525.643186	49.865101
3503.480440	516512.251923	49.870106
3503.971437	516497.913712	49.875111
3503.713658	516508.978849	49.880116
3503.777526	516502.192509	49.885121
3503.549506	516511.887551	49.890125
3503.458469	516500.624967	49.895130
3503.713964	516505.085447	49.900135
3503.627204	516506.666963	49.905140
3503.798217	516503.858717	49.910145
3503.563369	516501.721461	49.915149
3503.728757	516506.803022	49.920154
3503.805928	516480.494545	49.925159
3503.582034	516459.543477	49.930164
3503.734509	516471.201206	49.935169
3503.798081	516456.627098	49.940173
3503.707483	516470.042633	49.945178
3503.668789	516469.442041	49.950183
3503.455244	516460.373307	49.955188
3503.813013	516461.935136	49.960193
3503.759986	516463.410184	49.965197
3503.759095	516470.793694	49.970202
3504.011126	516447.238881	49.975207
3503.632703	516432.330052	49.980212
3503.749166	516425.687078	49.985217
3503.959231	516422.316373	49.990221
3503.806081	516427.549448	49.995226
3503.873357	516422.886486	50.000231
3503.502225	516428.609147	50.005236
3503.807117	516420.318141	50.010241
3503.564480	516405.590107	50.015245
3503.641607	516388.535852	50.020250
3503.903586	516383.488112	50.025255
3503.827468	516386.686209	50.030260
3503.849168	516382.333862	50.035265
3504.018850	516379.323524	50.040269
3503.734301	516381.846582	50.045274
3504.010627	516377.555128	50.050279
3503.722720	516361.721661	50.055284
3503.873071	516341.115854	50.060289
3503.759730	516332.284064	50.065293
3503.647665	516331.341071	50.070298
3503.889088	516333.679859	50.075303
3503.515002	516332.474858	50.080308
3504.030694	516332.039488	50.085313
3503.637060	516341.760805	50.090317
3503.396944	516317.828463	50.095322
3503.748056	516303.815619	50.100327
3503.462766	516291.622755	50.105332
3503.799717	516283.225472	50.110337
3503.700822	516296.541317	50.115341
3503.393877	516289.914643	50.120346
3503.782945	516280.801132	50.125351
3503.788140	516297.337047	50.130356
3503.902103	516280.226288	50.135361
3503.725627	516292.290132	50.140365
3503.457955	516287.932928	50.145370
3503.834132	516288.531021	50.150375
3503.409030	516301.898422	50.155380
3503.663754	516283.450582	50.160385
3503.483181	516263.706115	50.165389
3503.113278	516262.500448	50.170394
3503.471522	516263.657654	50.175399
3503.499173	516284.185119	50.180404
3503.706621	516292.698903	50.185409
3503.766038	516268.264010	50.190413
3503.516861	516243.169866	50.195418
3503.618006	516256.251841	50.200423
3503.300248	516256.504483	50.205428
3503.705112	516250.068708	50.210433
3503.606972	516248.617802	50.215437
3503.569420	516256.108343	50.220442
3503.724193	516244.958445	50.225447
3503.526708	516258.441616	50.230452
3503.574915	516254.793036	50.235457
3503.408080	516248.447624	50.240461
3503.324411	516247.247283	50.245466
3503.661225	516247.295322	50.250471
3503.045111	516251.337359	50.255476
3503.360915	516242.033124	50.260481
3503.441785	516255.421729	50.265485
3503.342094	516250.936823	50.270490
3503.466023	516242.168624	50.275495
3503.339543	516256.095710	50.280500
3503.442246	516254.461347	50.285505
3503.127468	516250.516144	50.290509
3503.589234	516249.735300	50.295514
3503.876065	516245.998430	50.300519
3503.607518	516248.670691	50.305524
3503.691680	516243.448732	50.310529
3503.480511	516251.371284	50.315533
3503.442069	516245.005576	50.320538
3503.694330	516241.375311	50.325543
3503.537651	516252.272927	50.330548
3503.814463	516249.144491	50.335553
3503.578764	516258.436327	50.340557
3503.442033	516253.047003	50.345562
3503.792341	516243.737315	50.350567
3503.452304	516252.084802	50.355572
3503.918605	516251.404383	50.360577
3503.803446	516245.961075	50.365581
3503.760476	516221.744580	50.370586
3503.665774	516225.855920	50.375591
3503.755914	516208.091432	50.380596
3503.784391	516216.279547	50.385601
3503.791341	516215.267165	50.390605
3503.768194	516224.373712	50.395610
3503.710430	516212.751677	50.400615
3503.305540	516228.442203	50.405620
3503.623348	516222.121319	50.410625
3503.704315	516222.058084	50.415629
3503.581958	516213.581652	50.420634
3503.472557	516188.010194	50.425639
3503.376731	516178.619274	50.430644
3503.338015	516168.865324	50.435649
3503.390415	516194.344947	50.440653
3503.591119	516207.057228	50.445658
3503.578436	516182.886459	50.450663
3503.539085	516184.865081	50.455668
3503.720588	516177.250879	50.460673
3503.635259	516174.129098	50.465677
3503.511302	516180.116202	50.470682
3503.493559	516189.272484	50.475687
3503.521895	516171.062587	50.480692
3503.325724	516173.369422	50.485697
3503.144776	516170.667323	50.490701
3503.406519	516175.480901	50.495706
3503.636607	516177.568648	50.500711
3503.728024	516190.500500	50.505716
3503.736168	516171.838656	50.510721
3503.608620	516176.612624	50.515725
3503.765714	516184.123003	50.520730
3503.481198	516169.805947	50.525735
3503.341150	516143.784125	50.530740
3503.490758	516102.443980	50.535745
3503.442041	516072.361913	50.540749
3503.316043	516022.518579	50.545754
3503.166588	515948.657270	50.550759
3503.187936	515883.062428	50.555764
3503.078972	515802.973730	50.560769
3502.970302	515700.582172	50.565773
3503.059790	515599.220692	50.570778
3503.009338	515492.570543	50.575783
3502.660670	515375.245288	50.580788
3502.618107	515229.397762	50.585793
3502.113937	515079.677130	50.590797
3502.139957	514940.795499	50.595802
3502.096184	514777.141901	50.600807
3502.032735	514622.391139	50.605812
3501.733853	514442.944396	50.610817
3501.612193	514252.846592	50.615821
3501.147097	514069.274822	50.620826
3501.033369	513854.489477	50.625831
3500.949687	513645.816654	50.630836
3500.778206	513428.253166	50.635841
3500.499435	513212.322383	50.640845
3500.099936	512967.071146	50.645850
3499.940298	512724.914476	50.650855
3499.217403	512489.419039	50.655860
3498.917728	512229.775985	50.660865
3498.882796	511967.203831	50.665869
3498.492236	511692.897637	50.670874
3498.290994	511422.553320	50.675879
3497.400353	511152.971288	50.680884
3497.427704	510851.471272	50.685889
3496.989147	510576.092304	50.690893
3496.586551	510273.790029	50.695898
3496.545443	509974.966531	50.700903
3496.321030	509667.515808	50.705908
3495.631922	509339.694069	50.710913
3495.437898	509033.087206	50.715917
3494.992871	508697.524563	50.720922
3494.768086	508353.268917	50.725927
3493.704657	508038.281867	50.730932
3493.742703	507690.176772	50.735937
3492.958779	507349.885378	50.740941
3492.453652	506995.173286	50.745946
3492.572196	506640.405943	50.750951
3491.908281	506295.369104	50.755956
3491.510188	505912.484098	50.760961
3491.027787	505547.112491	50.765965
3490.365473	505170.527650	50.770970
3490.018284	504784.016938	50.775975
3489.491804	504412.910211	50.780980
3489.252592	504027.833299	50.785985
3488.603970	503640.029204	50.790989
3487.952628	503246.852403	50.795994
3487.603307	502851.240392	50.800999
3487.030820	502445.026365	50.806004
3486.495638	502044.060820	50.811009
3486.055506	501648.588071	50.816013
3485.691594	501233.607695	50.821018
3485.551282	500803.549272	50.826023
3484.456266	500388.361039	50.831028
3483.834197	499966.406724	50.836033
3483.303545	499547.212081	50.841037
3483.011697	499115.871460	50.846042
3482.628169	498682.813804	50.851047
3481.969245	498244.828150	50.856052
3481.415362	497800.993401	50.861057
3480.953390	497363.917080	50.866061
3480.109123	496922.992335	50.871066
3479.761997	496471.548823	50.876071
3478.985741	496028.313297	50.881076
3478.827236	495558.084307	50.886081
3477.918200	495120.315813	50.891085
3477.417574	494659.180900	50.896090
3476.651206	494201.317003	50.901095
3476.026053	493741.697734	50.906100
3475.576783	493265.480790	50.911105
3474.897109	492820.076198	50.916109
3474.241993	492344.121204	50.921114
3473.981060	491885.967961	50.926119
3472.944262	491412.885280	50.931124
3472.568473	490944.446567	50.936129
3471.757518	490476.621963	50.941133
3470.834479	489998.117012	50.946138
3470.777722	489528.326192	50.951143
3469.984702	489054.891992	50.956148
3469.076875	488574.271715	50.961153
3468.745575	488110.668177	50.966157
3468.036095	487631.664021	50.971162
3467.263810	487151.239364	50.976167
3466.493757	486672.828392	50.981172
3465.880500	486193.418126	50.986177
3465.195744	485710.562384	50.991181
3464.227385	485240.353346	50.996186
3463.842913	484756.970131	51.001191
3462.966030	484287.837792	51.006196
3462.727742	483804.964799	51.011201
3461.781508	483330.095209	51.016205
3461.350957	482854.169791	51.021210
3460.592740	482366.783199	51.026215
3459.525240	481890.124155	51.031220
3458.958925	481409.979388	51.036225
3458.223954	480928.886734	51.041229
3457.743069	480449.464908	51.046234
3457.440569	479965.442618	51.051239
3456.497695	479495.394298	51.056244
3455.771844	479008.121582	51.061249
3455.343546	478522.512801	51.066253
3454.620171	478043.222782	51.071258
3454.057264	477550.060488	51.076263
3453.032405	477070.034468	51.081268
3452.418177	476581.822962	51.086273
3452.157085	476105.403425	51.091277
3451.269063	475613.765175	51.096282
3450.451673	475132.595523	51.101287
3449.547925	474648.032049	51.106292
3449.078361	474157.255122	51.111297
3448.193092	473677.328698	51.116301
3447.817821	473201.061342	51.121306
3447.222515	472702.614941	51.126311
3446.212343	472228.959776	51.131316
3445.550512	471754.072615	51.136321
3444.757888	471267.129805	51.141325
3443.673101	470790.056629	51.146330
3443.370369	470302.709363	51.151335
3442.626584	469832.353514	51.156340
3441.593766	469353.515182	51.161345
3441.004116	468883.620423	51.166349
3440.295387	468405.773717	51.171354
3439.806508	467933.914936	51.176359
3438.865464	467466.781750	51.181364
3438.063797	466977.812933	51.186369
3437.844527	466518.555930	51.191373
3436.810846	466031.934290	51.196378
3436.145673	465556.855427	51.201383
3435.333368	465096.393538	51.206388
3434.744203	464622.042348	51.211393
3434.153357	464165.125727	51.216397
3433.376441	463695.398362	51.221402
3432.937835	463211.711532	51.226407
3431.886654	462755.496849	51.231412
3430.880748	462284.202589	51.236417
3430.199920	461816.143254	51.241421
3429.558906	461350.451249	51.246426
3429.396777	460891.419220	51.251431
3427.966685	460428.469582	51.256436
3427.672169	459962.997357	51.261441
3426.826634	459506.478809	51.266445
3425.856859	459043.528448	51.271450
3425.559915	458579.853237	51.276455
3424.632124	458119.159369	51.281460
3424.127207	457657.526654	51.286465
3423.256213	457203.551388	51.291469
3422.469431	456742.603614	51.296474
3422.051811	456291.175911	51.301479
3421.057847	455836.786309	51.306484
3420.371156	455375.845150	51.311489
3419.791721	454923.654397	51.316493
3418.729316	454472.342641	51.321498
3418.613722	454010.928013	51.326503
3417.645198	453567.751675	51.331508
3416.888138	453115.349761	51.336513
3416.129248	452665.729717	51.341517
3415.587113	452215.000982	51.346522
3414.812651	451760.190097	51.351527
3413.939202	451318.629300	51.356532
3413.431055	450862.642156	51.361537
3412.472030	450414.024287	51.366541
3411.698925	449971.762063	51.371546
3411.265285	449519.390127	51.376551
3410.355257	449082.663776	51.381556
3409.781959	448636.487730	51.386561
3408.955720	448193.743248	51.391565
3408.095439	447757.643883	51.396570
3407.427533	447318.105711	51.401575
3406.643696	446890.910128	51.406580
3406.173865	446452.593208	51.411585
3405.365941	446014.118581	51.416589
3404.378317	445579.216997	51.421594
3404.035161	445146.489492	51.426599
3403.479122	444713.483230	51.431604
3402.371217	444280.454837	51.436609
3401.754991	443843.077214	51.441613
3401.166827	443406.550054	51.446618
3400.840213	442961.446022	51.451623
3399.728519	442549.401327	51.456628
3399.281166	442105.265013	51.461633
3398.826352	441676.553407	51.466637
3397.449326	441248.487668	51.471642
3396.738512	440805.739811	51.476647
3396.043364	440385.470247	51.481652
3395.459132	439961.723854	51.486657
3394.664880	439541.303166	51.491661
3393.929612	439117.921447	51.496666
3393.249993	438691.249097	51.501671
3392.168886	438283.950517	51.506676
3391.767635	437865.926813	51.511681
3391.300067	437447.119609	51.516685
3390.397679	437021.291460	51.521690
3390.073673	436604.605196	51.526695
3389.176209	436180.513591	51.531700
3388.384354	435757.185118	51.536705
3387.290444	435349.434461	51.541709
3386.728656	434932.605733	51.546714
3386.331883	434511.961172	51.551719
3385.363930	434110.238435	51.556724
3384.911495	433689.766773	51.561729
3383.964237	433287.723108	51.566733
3382.852650	432872.343953	51.571738
3382.518398	432465.544061	51.576743
3381.911125	432065.788765	51.581748
3381.190207	431646.468603	51.586753
3380.308330	431246.997946	51.591757
3379.599817	430839.596793	51.596762
3379.490866	430423.714940	51.601767
3378.243826	430033.602365	51.606772
3377.909847	429614.086611	51.611777
3377.026092	429211.182305	51.616781
3376.173598	428807.124138	51.621786
3375.532149	428407.648168	51.626791
3374.702975	428008.779909	51.631796
3374.306555	427592.771660	51.636801
3373.283578	427207.533777	51.641805
3372.836432	426810.491744	51.646810
3372.501214	426409.667446	51.651815
3371.808117	426004.957243	51.656820
3370.634643	425608.266166	51.661825
3370.048527	425203.171392	51.666829
3369.373560	424812.154961	51.671834
3368.857468	424414.250241	51.676839
3367.848657	424010.804508	51.681844
3367.379154	423610.035982	51.686849
3366.488159	423212.884110	51.691853
3365.711938	422819.975454	51.696858
3365.175317	422421.257464	51.701863
3364.529553	422041.423432	51.706868
3363.636957	421654.333178	51.711873
3363.211871	421252.430927	51.716877
3362.554470	420862.726880	51.721882
3361.790793	420467.318754	51.726887
3361.014980	420079.552985	51.731892
3360.666113	419678.936835	51.736897
3359.738800	419300.532343	51.741901
3358.503979	418913.178628	51.746906
3358.582423	418507.702369	51.751911
3357.540259	418122.695254	51.756916
3356.657720	417734.710755	51.761921
3356.055497	417345.635028	51.766925
3355.538178	416958.268091	51.771930
3354.704947	416568.684775	51.776935
3353.949472	416197.020260	51.781940
3353.459425	415809.481013	51.786945
3352.821041	415427.778054	51.791949
3352.093082	415036.277225	51.796954
3351.613649	414642.165681	51.801959
3350.698910	414260.033679	51.806964
3350.090877	413879.829951	51.811969
3349.273562	413499.425688	51.816973
3348.936383	413113.147437	51.821978
3347.929875	412730.908294	51.826983
3347.209590	412349.355778	51.831988
3346.351389	411965.457063	51.836993
3345.591955	411588.830322	51.841997
3344.602093	411217.800026	51.847002
3344.373941	410833.075527	51.852007
3343.728985	410461.752570	51.857012
3343.054579	410081.281710	51.862017
3342.443727	409702.905108	51.867021
3342.099320	409330.478745	51.872026
3341.437752	408939.750530	51.877031
3340.052094	408569.359926	51.882036
3339.657842	408187.067409	51.887041
3338.985241	407812.768336	51.892045
3338.291966	407436.587362	51.897050
3337.769757	407061.238765	51.902055
3337.157414	406689.610245	51.907060
3336.051629	406307.101784	51.912065
3335.724689	405930.717358	51.917069
3335.006528	405563.183721	51.922074
3334.192985	405183.919066	51.927079
3333.591366	404814.426597	51.932084
3332.793426	404429.253926	51.937089
3332.249990	404057.023823	51.942093
3331.406719	403695.638631	51.947098
3330.547706	403311.936047	51.952103
3329.775390	402939.220588	51.957108
3329.297871	402574.053850	51.962113
3328.303986	402212.548434	51.967117
3327.619769	401844.915101	51.972122
3327.316870	401469.490148	51.977127
3326.348935	401119.304690	51.982132
3325.642611	400746.604000	51.987137
3325.465780	400381.339251	51.992141
3324.430161	400021.137512	51.997146
3323.770248	399651.517988	52.002151
3322.971993	399280.873928	52.007156
3322.325827	398910.684580	52.012161
3321.690429	398555.182285	52.017165
3321.197615	398194.289840	52.022170
3320.533108	397821.549036	52.027175
3319.663267	397472.122280	52.032180
3319.096917	397102.484639	52.037185
3318.758518	396723.349947	52.042189
3317.578009	396372.791345	52.047194
3317.024331	396001.054862	52.052199
3316.525244	395647.813237	52.057204
3315.990132	395276.421699	52.062209
3315.271909	394920.613965	52.067213
3314.525740	394554.027396	52.072218
3313.813248	394187.024756	52.077223
3312.932958	393816.841277	52.082228
3312.197014	393451.868334	52.087233
3311.792686	393096.780013	52.092237
3310.706856	392745.838331	52.097242
3310.407604	392383.352850	52.102247
3309.443993	392019.290570	52.107252
3308.907278	391654.826412	52.112257
3308.268521	391300.138069	52.117261
3307.260935	390942.021080	52.122266
3306.952034	390572.042966	52.127271
3305.673190	390230.285281	52.132276
3305.173920	389869.839405	52.137281
3304.623355	389520.077329	52.142285
3303.628095	389166.110339	52.147290
3302.938791	388813.439089	52.152295
3302.557426	388461.580186	52.157300
3301.811688	388116.005325	52.162305
3301.264308	387762.716406	52.167309
3300.329638	387415.028695	52.172314
3299.939295	387072.998448	52.177319
3299.160612	386721.719355	52.182324
3298.419748	386363.742970	52.187329
3297.870644	386016.896307	52.192333
3297.048216	385662.358922	52.197338
3296.815564	385314.158620	52.202343
3295.942723	384960.131020	52.207348
3295.258206	384605.358177	52.212353
3294.536121	384257.555900	52.217357
3293.682496	383902.269021	52.222362
3293.403704	383548.744312	52.227367
3292.799969	383206.304913	52.232372
3291.680674	382855.169985	52.237377
3291.263929	382497.562666	52.242381
3290.659452	382149.315264	52.247386
3290.135751	381798.839257	52.252391
3288.978180	381441.873211	52.257396
3288.446445	381091.569981	52.262401
3287.886289	380739.436848	52.267405
3287.079749	380393.214558	52.272410
3286.593621	380040.859841	52.277415
3285.926583	379697.025418	52.282420
3285.365660	379342.285382	52.287425
3284.346246	378991.709545	52.292429
3283.536298	378648.168217	52.297434
3283.196566	378292.824081	52.302439
3282.310482	377952.417164	52.307444
3281.921275	377592.369053	52.312449
3281.404670	377246.403597	52.317453
3280.621165	376904.572475	52.322458
3280.158554	376543.203791	52.327463
3279.058904	376207.419554	52.332468
3278.438089	375850.546380	52.337473
3278.097291	375496.856184	52.342477
3276.960541	375147.765653	52.347482
3276.989697	374788.083973	52.352487
3275.708230	374450.253463	52.357492
3275.054178	374097.618094	52.362497
3274.503679	373751.856900	52.367501
3274.196889	373401.678936	52.372506
3273.486865	373048.509210	52.377511
3272.604842	372697.347857	52.382516
3272.071510	372343.304704	52.387521
3271.223432	371990.682016	52.392525
3270.542369	371637.928177	52.397530
3269.969737	371280.855006	52.402535
3268.937661	370944.024876	52.407540
3268.557959	370589.917177	52.412545
3267.747064	370229.056869	52.417549
3266.922883	369891.498617	52.422554
3266.065228	369544.606448	52.427559
3265.542420	369212.617445	52.432564
3264.802493	368863.131671	52.437569
3264.494543	368516.042493	52.442573
3263.793775	368170.462806	52.447578
3262.995985	367823.318367	52.452583
3261.929644	367487.306089	52.457588
3261.668022	367135.161190	52.462593
3261.187678	366797.041049	52.467597
3260.136705	366456.108196	52.472602
3259.360621	366105.206788	52.477607
3258.542985	365766.063561	52.482612
3257.692557	365431.095523	52.487617
3257.071969	365096.241281	52.492621
3256.418993	364764.315606	52.497626
3256.139307	364430.725525	52.502631
3255.187454	364096.476014	52.507636
3254.399536	363754.717725	52.512641
3254.122278	363414.300946	52.517645
3253.372133	363088.026905	52.522650
3252.785799	362737.985330	52.527655
3251.946393	362402.204471	52.532660
3251.375605	362062.129468	52.537665
3250.689413	361728.126054	52.542669
3249.976835	361399.340610	52.547674
3249.384036	361058.498437	52.552679
3248.635060	360731.775121	52.557684
3248.050597	360388.433162	52.562689
3247.329356	360050.046786	52.567693
3246.317504	359717.073021	52.572698
3245.794072	359371.678422	52.577703
3245.334278	359048.078546	52.582708
3244.557375	358708.724551	52.587713
3243.971506	358378.931253	52.592717
3243.054328	358042.266656	52.597722
3242.593702	357695.297915	52.602727
3241.805038	357369.372333	52.607732
3240.947135	357028.263622	52.612737
3240.498325	356705.129961	52.617741
3239.508334	356373.274988	52.622746
3239.181879	356031.642742	52.627751
3238.166733	355712.638398	52.632756
3237.845287	355380.492940	52.637761
3237.022297	355038.372626	52.642765
3236.378635	354716.580261	52.647770
3235.768346	354381.521936	52.652775
3234.920998	354062.429745	52.657780
3234.193944	353729.217917	52.662785
3233.705395	353399.350909	52.667789
3232.519506	353077.455880	52.672794
3231.958990	352756.147053	52.677799
3231.748478	352427.884084	52.682804
3230.998216	352097.006786	52.687809
3230.535956	351776.007239	52.692813
3229.601277	351443.933422	52.697818
3228.990725	351114.402152	52.702823
3227.936463	350793.515752	52.707828
3227.264262	350460.707118	52.712833
3227.306768	350130.862868	52.717837
3226.523836	349809.724057	52.722842
3226.112403	349478.115184	52.727847
3225.465041	349151.937220	52.732852
3224.308552	348815.351984	52.737857
3223.878827	348488.092136	52.742861
3223.101566	348156.507677	52.747866
3222.678615	347808.881581	52.752871
3221.666496	347493.135748	52.757876
3220.897329	347166.379932	52.762881
3220.316343	346840.177839	52.767885
3219.544066	346506.775700	52.772890
3218.859716	346181.095196	52.777895
3218.149886	345856.740386	52.782900
3217.615488	345532.025097	52.787905
3216.983716	345199.382113	52.792909
3216.042997	344887.402941	52.797914
3215.926669	344554.929232	52.802919
3214.725958	344233.060984	52.807924
3214.230959	343902.399732	52.812929
3213.541024	343579.556221	52.817933
3212.703670	343258.261483	52.822938
3212.269323	342931.148698	52.827943
3211.745428	342611.429912	52.832948
3210.972125	342295.490617	52.837953
3210.389495	341960.505239	52.842957
3209.196972	341637.705286	52.847962
3208.978403	341307.240472	52.852967
3208.040644	340984.574931	52.857972
3207.351638	340657.235580	52.862977
3206.935732	340333.822239	52.867981
3206.075973	340020.023044	52.872986
3205.640644	339691.925717	52.877991
3204.895705	339377.952396	52.882996
3204.024460	339048.724272	52.888001
3203.357056	338726.615175	52.893005
3202.598494	338415.617517	52.898010
3202.087339	338084.901908	52.903015
3201.277274	337769.174484	52.908020
3200.371354	337445.772966	52.913025
3199.972168	337124.886188	52.918029
3199.131452	336810.762676	52.923034
3198.715224	336500.541691	52.928039
3197.514624	336190.188774	52.933044
3197.349250	335863.862059	52.938049
3196.565613	335547.330574	52.943053
3195.926401	335236.298877	52.948058
3195.269188	334915.900420	52.953063
3194.513003	334608.982903	52.958068
3193.577103	334290.662143	52.963073
3193.181004	333979.051600	52.968077
3192.580967	333659.249151	52.973082
3191.922214	333342.483958	52.978087
3190.998038	333031.079965	52.983092
3190.474483	332719.891231	52.988097
3189.701289	332403.419909	52.993101
3189.180312	332088.969359	52.998106
3188.774953	331773.098923	53.003111
3188.008228	331464.539857	53.008116
3187.085667	331148.850320	53.013121
3186.600620	330835.585106	53.018125
3186.086329	330519.879139	53.023130
3185.311111	330199.579605	53.028135
3184.734093	329886.681279	53.033140
3184.118460	329560.269054	53.038145
3183.353513	329241.491260	53.043149
3182.524775	328941.663781	53.048154
3181.824439	328614.726170	53.053159
3180.944437	328304.771485	53.058164
3180.061660	327990.818839	53.063169
3179.724733	327685.689376	53.068173
3179.016923	327370.739037	53.073178
3178.325231	327059.807502	53.078183
3177.563906	326751.406262	53.083188
3177.177005	326445.566936	53.088193
3176.529882	326134.726502	53.093197
3175.895706	325824.493838	53.098202
3175.184049	325508.467285	53.103207
3174.491917	325198.877862	53.108212
3173.558642	324883.189433	53.113217
3173.496011	324573.778074	53.118221
3172.647223	324263.395119	53.123226
3172.298715	323941.118050	53.128231
3171.370253	323632.069275	53.133236
3170.675178	323310.557487	53.138241
3170.023817	322994.206134	53.143245
3169.239125	322684.672806	53.148250
3168.580984	322372.292127	53.153255
3167.632572	322061.305680	53.158260
3166.955991	321756.665905	53.163265
3166.239760	321440.726425	53.168269
3165.745369	321134.222405	53.173274
3165.316335	320826.612117	53.178279
3164.510525	320526.393355	53.183284
3164.127274	320203.751214	53.188289
3163.442064	319893.275567	53.193293
3162.639889	319586.942202	53.198298
3161.962799	319266.074601	53.203303
3161.177133	318956.222722	53.208308
3160.307742	318638.056875	53.213313
3159.466393	318326.683948	53.218317
3158.943937	318018.544179	53.223322
3158.215853	317715.604828	53.228327
3157.404684	317409.698523	53.233332
3157.015828	317112.025252	53.238337
3156.390940	316803.719496	53.243341
3155.383047	316500.285837	53.248346
3154.949294	316195.487236	53.253351
3154.276740	315893.730107	53.258356
3153.723606	315584.747099	53.263361
3152.959257	315282.493366	53.268365
3151.993401	314981.110890	53.273370
3151.767220	314668.814019	53.278375
3150.644255	314378.734863	53.283380
3150.206641	314074.770696	53.288385
3149.800365	313761.226374	53.293389
3148.926682	313459.824827	53.298394
3148.203596	313151.956264	53.303399
3147.639502	312855.214781	53.308404
3147.137137	312538.218937	53.313409
3146.399270	312234.449735	53.318413
3145.707518	311927.769485	53.323418
3145.202870	311612.986655	53.328423
3144.553335	311319.412015	53.333428
3143.744137	311015.115964	53.338433
3143.311938	310694.793324	53.343437
3142.511978	310389.781113	53.348442
3141.752954	310083.386527	53.353447
3141.147947	309768.487074	53.358452
3140.377901	309467.440133	53.363457
3139.653696	309164.526243	53.368461
3138.801884	308861.071541	53.373466
3138.386239	308550.442377	53.378471
3137.692016	308253.913069	53.383476
3136.842999	307939.301996	53.388481
3136.249291	307638.910081	53.393485
3135.378255	307341.260607	53.398490
3134.974885	307043.638275	53.403495
3134.137651	306750.998660	53.408500
3133.316200	306442.032683	53.413505
3133.096449	306140.304737	53.418509
3132.183983	305841.053973	53.423514
3131.433228	305529.833672	53.428519
3130.762072	305239.481688	53.433524
3129.894873	304941.775101	53.438529
3129.710666	304634.206471	53.443533
3128.466975	304331.643259	53.448538
3128.137862	304049.128913	53.453543
3127.526065	303741.498606	53.458548
3126.927607	303443.975414	53.463553
3126.165412	303135.629067	53.468557
3125.223192	302853.769576	53.473562
3124.659550	302552.775652	53.478567
3123.960519	302249.790716	53.483572
3123.121392	301962.056006	53.488577
3122.844266	301659.537880	53.493581
3122.074476	301371.587328	53.498586
3121.586349	301061.665284	53.503591
3120.689848	300772.485809	53.508596
3119.885454	300480.158868	53.513601
3119.459862	300182.856438	53.518605
3118.618154	299892.775347	53.523610
3118.014972	299583.556177	53.528615
3117.114204	299303.415273	53.533620
3116.576688	299003.327068	53.538625
3116.218327	298707.743017	53.543629
3115.442445	298407.003865	53.548634
3114.883677	298108.190756	53.553639
3114.128833	297819.161895	53.558644
3113.323686	297516.694087	53.563649
3112.795266	297225.591080	53.568653
3111.884254	296934.522678	53.573658
3111.362353	296632.925357	53.578663
3110.691392	296344.390177	53.583668
3110.036182	296060.410638	53.588673
3109.335668	295766.785860	53.593677
3108.494067	295467.834887	53.598682
3107.960364	295175.940033	53.603687
3106.943165	294886.082226	53.608692
3106.516330	294597.709532	53.613697
3106.052436	294300.454254	53.618701
3104.845322	294018.036200	53.623706
3104.525537	293720.910086	53.628711
3103.995213	293434.665927	53.633716
3103.158736	293137.493431	53.638721
3102.915333	292842.085789	53.643725
3102.045727	292556.607255	53.648730
3101.256060	292262.405858	53.653735
3100.514028	291976.855470	53.658740
3099.876998	291680.591782	53.663745
3099.273115	291392.828618	53.668749
3098.456567	291104.665817	53.673754
3097.854004	290802.920075	53.678759
3097.453728	290519.835158	53.683764
3096.482014	290235.719785	53.688769
3096.193016	289936.826694	53.693773
3095.422398	289655.505771	53.698778
3094.917454	289359.931534	53.703783
3094.112803	289076.527043	53.708788
3093.292598	288782.606546	53.713793
3092.936739	288489.707372	53.718797
3091.932000	288199.508309	53.723802
3091.347419	287897.731012	53.728807
3090.553073	287606.963252	53.733812
3089.631170	287325.129162	53.738817
3088.745242	287034.884722	53.743821
3088.143875	286757.940174	53.748826
3087.941494	286469.904633	53.753831
3086.982292	286194.748070	53.758836
3086.608840	285911.501641	53.763841
3086.400918	285619.875285	53.768845
3085.143252	285334.221538	53.773850
3084.419601	285033.635193	53.778855
3083.695581	284749.399164	53.783860
3083.101361	284464.200068	53.788865
3082.982984	284176.429590	53.793869
3081.804873	283888.979440	53.798874
3081.462241	283598.213355	53.803879
3080.726240	283317.645658	53.808884
3079.935946	283024.657919	53.813889
3079.446598	282725.790158	53.818893
3078.529928	282433.025806	53.823898
3078.161029	282144.835273	53.828903
3077.439848	281847.531779	53.833908
3076.521869	281556.779136	53.838913
3075.881817	281265.345653	53.843917
3074.849012	280981.945751	53.848922
3074.780786	280688.918863	53.853927
3073.841468	280406.548106	53.858932
3072.922166	280128.580079	53.863937
3072.588788	279829.533332	53.868941
3071.867779	279553.494761	53.873946
3071.550872	279266.109673	53.878951
3070.779896	278977.421061	53.883956
3069.774474	278694.270622	53.888961
3069.100354	278411.602498	53.893965
3068.089021	278127.332224	53.898970
3067.877316	277835.218407	53.903975
3067.017692	277564.116588	53.908980
3066.428838	277286.732108	53.913985
3065.536759	276992.866592	53.918989
3064.959124	276719.325954	53.923994
3064.375319	276435.573430	53.928999
3063.657472	276162.411459	53.934004
3062.767877	275875.549179	53.939009
3062.512434	275599.868996	53.944013
3061.271007	275325.389049	53.949018
3061.012560	275045.430611	53.954023
3060.590361	274764.275596	53.959028
3059.505388	274491.986600	53.964033
3059.028197	274203.276166	53.969037
3058.596145	273933.277860	53.974042
3057.485679	273646.628736	53.979047
3057.157928	273371.978697	53.984052
3056.342711	273096.845525	53.989057
3056.043602	272809.100244	53.994061
3055.085211	272535.696169	53.999066
3054.628463	272243.187852	54.004071
3053.690112	271961.528928	54.009076
3052.931312	271683.636419	54.014081
3052.591277	271401.118843	54.019085
3051.615061	271129.526071	54.024090
3050.964246	270844.561905	54.029095
3050.484794	270574.495138	54.034100
3049.731683	270291.177280	54.039105
3049.277162	270001.648905	54.044109
3048.393002	269730.729562	54.049114
3048.030038	269448.903775	54.054119
3047.383845	269178.430841	54.059124
3046.552455	268887.536269	54.064129
3045.983244	268601.413821	54.069133
3045.426660	268322.038582	54.074138
3044.752006	268043.599006	54.079143
3043.928858	267751.608473	54.084148
3043.065697	267473.555541	54.089153
3042.793382	267194.517832	54.094157
3041.661214	266918.290521	54.099162
3041.274214	266631.910931	54.104167
3040.208896	266357.914530	54.109172
3039.723724	266081.457908	54.114177
3039.297485	265805.323201	54.119181
3038.221428	265524.910986	54.124186
3037.870977	265245.020795	54.129191
3037.082943	264983.842702	54.134196
3036.130363	264695.592751	54.139201
3035.463628	264418.503710	54.144205
3034.802757	264150.837112	54.149210
3034.278375	263871.994083	54.154215
3033.648210	263594.415932	54.159220
3032.714138	263334.331677	54.164225
3032.308208	263052.719956	54.169229
3031.533685	262793.222064	54.174234
3030.655158	262502.644453	54.179239
3030.205458	262240.039403	54.184244
3029.346442	261967.872476	54.189249
3029.110341	261689.571285	54.194253
3028.433902	261436.094803	54.199258
3027.503336	261146.163323	54.204263
3027.086453	260889.386316	54.209268
3026.169484	260612.314443	54.214273
3025.907578	260327.065853	54.219277
3024.912034	260064.319825	54.224282
3024.389092	259790.955591	54.229287
3023.729556	259515.703167	54.234292
3023.254799	259245.056888	54.239297
3022.397319	258962.450729	54.244301
3021.284313	258696.643017	54.249306
3020.977078	258422.685735	54.254311
3020.294608	258153.194033	54.259316
3019.667454	257885.705800	54.264321
3019.091903	257608.812173	54.269325
3018.297103	257330.349115	54.274330
3017.897631	257057.986927	54.279335
3016.950214	256793.734029	54.284340
3016.383460	256513.631389	54.289345
3015.738216	256230.689170	54.294349
3014.716133	255970.447421	54.299354
3013.982120	255702.774857	54.304359
3013.697628	255429.734272	54.309364
3013.243269	255166.118333	54.314369
3012.433926	254887.049382	54.319373
3011.286898	254625.632076	54.324378
3011.055796	254353.730452	54.329383
3010.476769	254087.232359	54.334388
3009.648652	253814.560081	54.339393
3009.023851	253535.412833	54.344397
3008.339298	253271.097237	54.349402
3007.495821	252993.335133	54.354407
3006.871037	252727.431871	54.359412
3006.275187	252453.655133	54.364417
3005.750086	252184.986435	54.369421
3004.834050	251919.410566	54.374426
3004.394729	251649.481202	54.379431
3003.546116	251389.014263	54.384436
3002.620257	251111.853773	54.389441
3002.085534	250842.653804	54.394445
3001.581516	250581.191247	54.399450
3000.869355	250320.933500	54.404455
3000.386779	250062.320601	54.409460
2999.656210	249790.224640	54.414465
2999.066234	249518.972728	54.419469
2998.038533	249252.349047	54.424474
2997.598371	248978.069279	54.429479
2996.970943	248718.793831	54.434484
2996.338302	248449.129380	54.439489
2995.557100	248176.203762	54.444493
2994.748108	247911.330343	54.449498
2994.428032	247653.204915	54.454503
2993.462093	247382.016178	54.459508
2993.045278	247114.662775	54.464513
2992.421174	246852.919725	54.469517
2991.629135	246583.844050	54.474522
2991.213361	246313.665200	54.479527
2990.111285	246050.089299	54.484532
2989.381876	245782.660474	54.489537
2989.117564	245505.048601	54.494541
2987.975552	245252.812773	54.499546
2987.289139	244985.862496	54.504551
2986.542463	244732.011618	54.509556
2986.175560	244464.145934	54.514561
2985.856562	244198.132177	54.519565
2984.655120	243936.333121	54.524570
2984.038328	243663.593738	54.529575
2983.635963	243406.584052	54.534580
2982.716676	243153.170920	54.539585
2982.372726	242878.938440	54.544589
2981.483446	242622.338427	54.549594
2980.832260	242358.851095	54.554599
2979.983207	242099.979358	54.559604
2979.211786	241837.658072	54.564609
2978.609325	241574.164660	54.569613
2977.853689	241322.002510	54.574618
2977.382791	241059.125988	54.579623
2976.856376	240801.530049	54.584628
2975.985633	240540.882458	54.589633
2975.927939	240274.478999	54.594637
2974.852946	240012.999085	54.599642
2974.201631	239752.929623	54.604647
2973.457876	239491.016453	54.609652
2973.274264	239221.146646	54.614657
2972.400959	238959.382501	54.619661
2971.348037	238702.358306	54.624666
2970.578983	238433.397887	54.629671
2970.119428	238172.945114	54.634676
2969.173130	237916.491496	54.639681
2968.831887	237659.688034	54.644685
2967.850288	237407.544622	54.649690
2967.316520	237148.557444	54.654695
2966.499547	236891.703761	54.659700
2965.883692	236641.057513	54.664705
2965.577544	236376.510454	54.669709
2964.740851	236128.115719	54.674714
2964.155660	235869.496235	54.679719
2963.531916	235612.538626	54.684724
2962.881066	235355.662325	54.689729
2962.265243	235089.868855	54.694733
2961.382239	234835.373240	54.699738
2960.680627	234582.275488	54.704743
2960.122695	234327.169468	54.709748
2959.187231	234066.420070	54.714753
2958.993687	233797.787587	54.719757
2958.127897	233548.155943	54.724762
2957.412587	233286.838982	54.729767
2956.624363	233029.430102	54.734772
2955.911398	232772.773867	54.739777
2955.238332	232516.213838	54.744781
2954.385823	232269.206006	54.749786
2954.018962	232006.538680	54.754791
2953.595460	231746.452772	54.759796
2952.776171	231498.321296	54.764801
2952.046418	231241.289844	54.769805
2951.277757	230992.769734	54.774810
2951.053105	230730.949134	54.779815
2950.260940	230480.218869	54.784820
2949.174841	230231.547340	54.789825
2948.708801	229969.105080	54.794829
2948.060429	229711.148318	54.799834
2947.668256	229461.019511	54.804839
2946.793893	229203.711054	54.809844
2945.744419	228952.567388	54.814849
2945.491773	228699.770553	54.819853
2944.389630	228462.869798	54.824858
2943.720603	228207.874177	54.829863
2943.288152	227961.422422	54.834868
2942.801609	227707.392361	54.839873
2942.394366	227461.218096	54.844877
2941.562211	227204.341604	54.849882
2940.899404	226939.953414	54.854887
2939.970638	226682.559081	54.859892
2939.390118	226441.685648	54.864897
2938.906102	226185.750071	54.869901
2938.073634	225932.543849	54.874906
2937.596706	225672.815001	54.879911
2936.906303	225419.384144	54.884916
2935.763434	225171.181518	54.889921
2934.991704	224916.148306	54.894925
2934.910997	224668.339153	54.899930
2934.037620	224411.592271	54.904935
2933.177759	224164.009848	54.909940
2932.569574	223916.566555	54.914945
2932.050571	223658.212855	54.919949
2931.033752	223418.970379	54.924954
2930.375200	223169.678753	54.929959
2929.920630	222924.683834	54.934964
2929.337173	222682.676177	54.939969
2928.628161	222429.155765	54.944973
2927.937497	222186.300966	54.949978
2927.583253	221932.433199	54.954983
2926.852917	221674.043054	54.959988
2925.986234	221438.780000	54.964993
2925.660309	221174.802744	54.969997
2924.879607	220933.480973	54.975002
2924.100415	220677.902453	54.980007
2923.647861	220424.857196	54.985012
2922.958579	220174.918105	54.990017
2922.160455	219917.155657	54.995021
2921.604450	219675.865966	55.000026
2921.000374	219410.958727	55.005031
2920.180080	219159.070703	55.010036
2919.358365	218914.388606	55.015041
2918.885173	218665.540554	55.020045
2918.051823	218417.068606	55.025050
2917.424494	218168.513966	55.030055
2916.850166	217915.942077	55.035060
2916.177847	217675.046521	55.040065
2915.994540	217415.056999	55.045069
2914.639563	217170.210632	55.050074
2914.096021	216907.581425	55.055079
2913.578051	216659.167440	55.060084
2912.397435	216408.644411	55.065089
2911.937735	216156.429737	55.070093
2911.166223	215918.992649	55.075098
2910.640247	215670.125188	55.080103
2909.954742	215418.381714	55.085108
2909.346764	215173.996818	55.090113
2908.649997	214931.765268	55.095117
2907.960839	214691.251735	55.100122
2907.596540	214431.314676	55.105127
2906.737581	214187.113055	55.110132
2905.852301	213943.718377	55.115137
2905.703834	213691.501639	55.120141
2904.676514	213447.749390	55.125146
2903.832666	213196.446511	55.130151
2903.134634	212953.038504	55.135156
2902.286366	212711.602603	55.140161
2902.082754	212464.159608	55.145165
2901.151324	212228.975471	55.150170
2900.518303	211986.057131	55.155175
2900.167522	211745.398786	55.160180
2899.313588	211511.325029	55.165185
2898.588951	211255.326767	55.170189
2897.954810	211014.130512	55.175194
2897.151236	210768.074478	55.180199
2896.658452	210527.023130	55.185204
2896.295774	210289.286772	55.190209
2895.638761	210041.797540	55.195213
2894.846554	209796.825310	55.200218
2893.919475	209543.169674	55.205223
2893.479294	209299.340032	55.210228
2892.825376	209061.056213	55.215233
2892.169995	208806.087779	55.220237
2891.550126	208560.978539	55.225242
2890.798110	208308.102026	55.230247
2890.236771	208078.321944	55.235252
2889.398337	207832.232017	55.240257
2889.246939	207584.519742	55.245261
2888.287230	207340.041903	55.250266
2887.579932	207091.299664	55.255271
2887.093561	206838.718061	55.260276
2886.160451	206588.002767	55.265281
2885.619388	206340.777265	55.270285
2884.650666	206101.180302	55.275290
2884.189095	205856.425965	55.280295
2883.837442	205603.955494	55.285300
2882.802259	205366.764655	55.290305
2882.111395	205116.500802	55.295309
2881.266657	204875.018329	55.300314
2880.798676	204635.589807	55.305319
2880.195222	204389.667715	55.310324
2879.324544	204152.850254	55.315329
2878.680896	203901.667811	55.320333
2877.805973	203665.629326	55.325338
2877.520606	203417.382956	55.330343
2876.615341	203178.806000	55.335348
2875.998152	202936.086567	55.340353
2875.815773	202686.210821	55.345357
2874.798743	202445.580258	55.350362
2874.179877	202197.226562	55.355367
2873.594639	201952.126494	55.360372
2872.872225	201708.169101	55.365377
2872.481854	201466.539932	55.370381
2871.498538	201229.701546	55.375386
2870.858460	200983.901747	55.380391
2870.233444	200740.493090	55.385396
2869.629435	200491.101100	55.390401
2869.118023	200237.534289	55.395405
2867.964349	200006.161959	55.400410
2867.333460	199755.924942	55.405415
2866.746939	199517.873041	55.410420
2866.182972	199274.639364	55.415425
2865.764139	199037.110203	55.420429
2865.051809	198788.672080	55.425434
2864.131010	198540.395366	55.430439
2863.657359	198303.387123	55.435444
2862.667259	198064.349343	55.440449
2862.501481	197813.322327	55.445453
2861.558644	197580.196386	55.450458
2860.950957	197331.417602	55.455463
2860.483839	197092.097769	55.460468
2859.215075	196851.875262	55.465473
2858.877808	196607.383508	55.470477
2858.142041	196369.954596	55.475482
2857.310447	196130.276949	55.480487
2856.728029	195890.510044	55.485492
2856.001171	195648.425803	55.490497
2855.513080	195407.526432	55.495501
2854.635873	195173.980901	55.500506
2854.041083	194932.820706	55.505511
2853.837414	194690.721726	55.510516
2852.810946	194453.996583	55.515521
2851.971066	194212.445971	55.520525
2851.491424	193978.308518	55.525530
2850.740979	193744.927580	55.530535
2850.096053	193509.825990	55.535540
2849.320901	193271.679648	55.540545
2848.987534	193021.338603	55.545549
2847.895863	192784.555259	55.550554
2847.229298	192555.174563	55.555559
2846.715946	192318.594487	55.560564
2846.029651	192082.577319	55.565569
2845.389851	191846.057692	55.570573
2844.707120	191619.775711	55.575578
2843.977327	191374.709662	55.580583
2843.442569	191138.456711	55.585588
2842.768541	190916.019059	55.590593
2842.081639	190666.471142	55.595597
2841.404661	190442.216689	55.600602
2840.804954	190201.067399	55.605607
2840.430044	189960.799770	55.610612
2839.621652	189725.245894	55.615617
2839.068066	189494.245809	55.620621
2838.238639	189245.847412	55.625626
2837.735136	189001.978908	55.630631
2837.053837	188771.715011	55.635636
2836.135935	188538.321743	55.640641
2835.849223	188289.193516	55.645645
2834.991767	188059.991503	55.650650
2834.251015	187818.405823	55.655655
2833.705139	187579.551293	55.660660
2832.918689	187346.741049	55.665665
2832.308092	187096.970688	55.670669
2831.522411	186867.419624	55.675674
2831.020313	186620.217251	55.680679
2830.474281	186389.816367	55.685684
2829.685912	186161.210654	55.690689
2829.124394	185907.037078	55.695693
2828.244803	185674.288131	55.700698
2827.818538	185436.316206	55.705703
2827.278168	185195.475739	55.710708
2826.382857	184950.659964	55.715713
2826.158086	184711.680324	55.720717
2824.820724	184486.541154	55.725722
2824.313702	184242.443713	55.730727
2823.581489	183994.337828	55.735732
2822.754666	183766.119120	55.740737
2822.513892	183516.754939	55.745741
2821.730568	183288.786194	55.750746
2821.050886	183053.716484	55.755751
2820.534263	182799.629535	55.760756
2819.948354	182570.526453	55.765761
2819.146521	182329.055778	55.770765
2818.181827	182099.391794	55.775770
2817.507767	181860.880136	55.780775
2817.176554	181623.218644	55.785780
2816.199616	181390.087520	55.790785
2815.500233	181153.428217	55.795789
2814.664207	180919.094263	55.800794
2814.392998	180676.200245	55.805799
2813.402528	180439.043940	55.810804
2812.568060	180218.120868	55.815809
2812.057713	179976.642442	55.820813
2811.156635	179757.767523	55.825818
2810.652328	179516.596001	55.830823
2810.170159	179289.757885	55.835828
2809.315746	179075.789012	55.840833
2808.757486	178835.125950	55.845837
2807.986299	178613.488787	55.850842
2807.538203	178374.095590	55.855847
2806.827856	178144.692136	55.860852
2806.107343	177920.621089	55.865857
2805.552886	177681.782878	55.870861
2804.624324	177464.323254	55.875866
2804.160759	177228.869339	55.880871
2803.516319	176996.637968	55.885876
2802.804586	176776.934385	55.890881
2802.459524	176539.557673	55.895885
2801.925982	176309.373082	55.900890
2801.050092	176068.839735	55.905895
2800.130038	175834.140110	55.910900
2799.384024	175609.729355	55.915905
2799.000275	175371.157155	55.920909
2798.349904	175142.294893	55.925914
2797.581370	174912.346088	55.930919
2797.203399	174685.185704	55.935924
2796.114895	174451.321934	55.940929
2795.590540	174217.344711	55.945933
2794.815694	173983.764628	55.950938
2794.574345	173753.675262	55.955943
2793.947511	173523.203119	55.960948
2792.945630	173297.955315	55.965953
2792.754392	173054.927505	55.970957
2791.558358	172826.609851	55.975962
2790.745822	172596.019812	55.980967
2790.250711	172365.012001	55.985972
2789.464998	172134.102428	55.990977
2788.898569	171899.064317	55.995981
2788.446994	171678.940052	56.000986
2787.733565	171439.921847	56.005991
2787.274207	171211.445893	56.010996
2786.358370	170980.614515	56.016001
2785.881517	170737.722392	56.021005
2784.812134	170512.844416	56.026010
2784.458708	170281.953491	56.031015
2783.839540	170046.260754	56.036020
2783.160143	169810.515394	56.041025
2782.431741	169584.164429	56.046029
2781.876359	169358.270623	56.051034
2781.431832	169117.443610	56.056039
2780.825589	168884.235671	56.061044
2779.798122	168660.786048	56.066049
2779.263617	168419.023883	56.071053
2778.274611	168187.699278	56.076058
2777.598116	167950.133610	56.081063
2777.187862	167718.491265	56.086068
2776.103105	167491.217159	56.091073
2775.496333	167253.822806	56.096077
2774.858506	167043.965510	56.101082
2774.322357	166810.403047	56.106087
2773.726932	166583.540076	56.111092
2772.656963	166358.470296	56.116097
2772.652480	166131.669025	56.121101
2771.934454	165905.452634	56.126106
2771.009933	165664.049526	56.131111
2770.608424	165430.537869	56.136116
2769.685943	165212.508812	56.141121
2769.059515	164975.360813	56.146125
2768.291178	164754.258291	56.151130
2767.495134	164520.992844	56.156135
2766.944277	164290.258520	56.161140
2766.339376	164076.559890	56.166145
2765.839919	163852.330358	56.171149
2764.929951	163624.848581	56.176154
2764.064376	163397.488330	56.181159
2764.043089	163159.645802	56.186164
2762.749335	162943.227453	56.191169
2762.471906	162708.772434	56.196173
2761.319430	162492.397953	56.201178
2760.904072	162261.044617	56.206183
2760.431740	162041.093996	56.211188
2759.653694	161820.315839	56.216193
2759.326088	161580.052833	56.221197
2758.468424	161362.811963	56.226202
2757.758940	161135.135992	56.231207
2757.390784	160914.768873	56.236212
2756.499017	160618.265384	56.241217
2756.250175	160385.232166	56.246221
2755.307332	160159.837011	56.251226
2754.709212	159924.637203	56.256231
2754.104206	159686.655742	56.261236
2753.257255	159464.580790	56.266241
2752.777853	159222.031076	56.271245
2751.936625	159003.263630	56.276250
2751.511665	158779.600519	56.281255
2750.637921	158542.749964	56.286260
2749.682508	158315.067446	56.291265
2749.441606	158075.704284	56.296269
2748.784047	157857.588669	56.301274
2747.991635	157618.417707	56.306279
2747.282362	157387.384159	56.311284
2746.480048	157170.160251	56.316289
2746.235649	156928.555352	56.321293
2745.424840	156695.254208	56.326298
2744.835262	156476.793248	56.331303
2744.108311	156234.176363	56.336308
2743.463242	156006.002160	56.341313
2743.096974	155767.755324	56.346317
2742.151621	155555.153367	56.351322
2741.459541	155320.164727	56.356327
2741.063788	155081.279018	56.361332
2740.133412	154852.305993	56.366337
2739.465666	154616.352238	56.371341
2738.803029	154387.772128	56.376346
2737.979932	154154.922435	56.381351
2737.531143	153921.506583	56.386356
2736.700345	153695.932294	56.391361
2736.047470	153459.513920	56.396365
2735.800137	153243.180403	56.401370
2734.741947	153015.307815	56.406375
2734.373094	152769.074366	56.411380
2733.384571	152543.939556	56.416385
2732.929057	152313.192553	56.421389
2732.021972	152077.993611	56.426394
2731.426946	151843.357013	56.431399
2731.026741	151607.509114	56.436404
2730.057582	151393.996601	56.441409
2729.592740	151144.676274	56.446413
2728.759426	150925.527217	56.451418
2728.257372	150694.201464	56.456423
2727.586594	150449.113438	56.461428
2726.586602	150236.414057	56.466433
2725.891005	150004.399344	56.471437
2725.420675	149769.719622	56.476442
2724.829514	149548.800131	56.481447
2724.074296	149320.905020	56.486452
2723.038160	149095.038727	56.491457
2722.370613	148870.284899	56.496461
2721.707398	148654.708240	56.501466
2721.342801	148420.364664	56.506471
2720.600522	148189.895434	56.511476
2719.766399	147973.969114	56.516481
2719.060469	147761.455418	56.521485
2718.308611	147531.678716	56.526490
2717.910737	147303.715807	56.531495
2717.331511	147082.404604	56.536500
2716.577627	146865.786752	56.541505
2716.105319	146631.028490	56.546509
2715.308928	146414.001054	56.551514
2714.499840	146184.751460	56.556519
2714.053172	145952.701072	56.561524
2713.272660	145737.442227	56.566529
2712.570126	145509.781895	56.571533
2711.722047	145285.513940	56.576538
2711.010373	145059.129131	56.581543
2710.413661	144836.679936	56.586548
2709.826894	144630.636700	56.591553
2709.450080	144404.178145	56.596557
2708.643374	144178.310354	56.601562
2707.784551	143948.970552	56.606567
2707.282731	143733.821075	56.611572
2706.677021	143509.934081	56.616577
2706.069935	143290.026334	56.621581
2705.038628	143060.250239	56.626586
2704.628519	142845.880238	56.631591
2704.340030	142624.084196	56.636596
2703.056225	142405.598785	56.641601
2702.640590	142176.328954	56.646605
2701.860077	141956.165920	56.651610
2701.191879	141742.047797	56.656615
2700.826150	141520.246535	56.661620
2699.787602	141305.923297	56.666625
2699.513509	141080.590981	56.671629
2698.859480	140855.727129	56.676634
2697.962521	140634.575548	56.681639
2697.177293	140410.282147	56.686644
2696.656495	140193.762771	56.691649
2696.026365	139963.552460	56.696653
2695.409854	139749.211452	56.701658
2694.726081	139525.404064	56.706663
2694.261080	139300.509098	56.711668
2693.419167	139082.854223	56.716673
2693.204572	138848.584308	56.721677
2692.108763	138622.333223	56.726682
2691.627977	138406.900313	56.731687
2690.939738	138184.234407	56.736692
2689.937919	137966.003133	56.741697
2689.733005	137733.442913	56.746701
2688.940281	137521.229389	56.751706
2688.281339	137291.958920	56.756711
2687.623889	137066.094872	56.761716
2686.948469	136838.520261	56.766721
2686.269983	136613.082261	56.771725
2685.603656	136393.767628	56.776730
2684.852867	136165.257313	56.781735
2684.406686	135944.640705	56.786740
2683.390752	135722.718564	56.791745
2682.821722	135486.892512	56.796749
2682.134378	135271.769244	56.801754
2681.381931	135055.247740	56.806759
2680.672361	134832.915398	56.811764
2679.952573	134615.375681	56.816769
2679.472561	134385.019741	56.821773
2678.686261	134179.549577	56.826778
2677.946662	133953.036557	56.831783
2677.393578	133745.322122	56.836788
2676.792664	133527.657403	56.841793
2676.284184	133303.335927	56.846797
2675.634054	133077.196698	56.851802
2674.755839	132865.691090	56.856807
2674.208109	132649.891917	56.861812
2673.486554	132428.177013	56.866817
2673.011971	132199.082550	56.871821
2672.001474	131991.732724	56.876826
2671.520351	131768.155673	56.881831
2670.968818	131538.011700	56.886836
2670.139966	131327.271801	56.891841
2669.704133	131104.924907	56.896845
2668.880559	130877.395233	56.901850
2668.291396	130664.653458	56.906855
2667.536072	130448.865755	56.911860
2666.495561	130221.007385	56.916865
2666.100300	130003.273473	56.921869
2665.580840	129789.384104	56.926874
2664.994487	129566.120560	56.931879
2664.293003	129347.436833	56.936884
2663.505801	129131.549980	56.941889
2663.192706	128906.990962	56.946893
2662.115182	128679.913048	56.951898
2661.645073	128465.517932	56.956903
2660.787963	128251.147685	56.961908
2660.016256	128026.922446	56.966913
2659.826895	127803.013165	56.971917
2658.850756	127589.086016	56.976922
2658.122440	127375.260959	56.981927
2657.774020	127139.456491	56.986932
2656.753730	126936.463724	56.991937
2656.068284	126716.210637	56.996941
2655.538953	126502.259220	57.001946
2654.927847	126292.056224	57.006951
2654.503414	126072.046343	57.011956
2653.814381	125844.041192	57.016961
2653.140235	125619.908986	57.021965
2652.317607	125406.241201	57.026970
2651.600046	125183.110030	57.031975
2651.276734	124955.854419	57.036980
2650.287402	124746.307428	57.041985
2649.504498	124507.711749	57.046989
2648.965774	124293.575954	57.051994
2648.265602	124086.909029	57.056999
2647.847734	123865.176197	57.062004
2646.977232	123651.136164	57.067009
2646.238859	123423.108376	57.072013
2645.636794	123211.873798	57.077018
2644.448655	122992.251187	57.082023
2644.186944	122783.670817	57.087028
2643.441482	122564.527594	57.092033
2642.776215	122349.690828	57.097037
2642.469549	122129.973711	57.102042
2641.539576	121921.188512	57.107047
2640.981035	121701.921171	57.112052
2640.119649	121489.877844	57.117057
2639.746350	121267.346812	57.122061
2638.934321	121054.130966	57.127066
2638.141137	120843.821560	57.132071
2637.569926	120624.907963	57.137076
2637.049621	120411.270154	57.142081
2636.511418	120190.158314	57.147085
2635.439770	119978.477859	57.152090
2634.928340	119759.587372	57.157095
2634.207991	119537.087836	57.162100
2633.458146	119334.757207	57.167105
2633.069063	119114.798890	57.172109
2632.578442	118898.362742	57.177114
2631.515456	118678.019730	57.182119
2631.231681	118463.934979	57.187124
2630.569020	118254.076371	57.192129
2629.594460	118029.979464	57.197133
2629.201563	117821.484518	57.202138
2628.434927	117605.655138	57.207143
2627.947711	117385.352464	57.212148
2627.139582	117175.798597	57.217153
2626.613335	116948.605752	57.222157
2625.878958	116738.643841	57.227162
2625.138581	116522.057635	57.232167
2624.389893	116297.317899	57.237172
2623.442457	116087.553761	57.242177
2622.984092	115868.230673	57.247181
2622.488664	115650.978256	57.252186
2621.770038	115440.465900	57.257191
2621.185273	115229.654785	57.262196
2620.226506	115022.636886	57.267201
2619.838856	114795.561768	57.272205
2618.899101	114587.427286	57.277210
2618.249409	114372.501549	57.282215
2617.469149	114161.082868	57.287220
2616.919511	113943.625126	57.292225
2616.044167	113732.269525	57.297229
2615.469008	113524.562026	57.302234
2614.765221	113316.165774	57.307239
2614.705412	113103.055063	57.312244
2613.539567	112901.094973	57.317249
2613.032818	112685.348566	57.322253
2612.277363	112474.136855	57.327258
2611.536321	112266.878568	57.332263
2611.012189	112048.557336	57.337268
2610.398893	111839.562435	57.342273
2609.345506	111631.413293	57.347277
2608.810302	111409.761180	57.352282
2608.224694	111202.226903	57.357287
2607.620681	111001.202205	57.362292
2606.781310	110800.857402	57.367297
2606.598691	110575.755278	57.372301
2605.645277	110371.510091	57.377306
2604.711211	110160.600165	57.382311
2604.173518	109942.128250	57.387316
2603.702688	109743.719907	57.392321
2603.175635	109531.773579	57.397325
2602.399712	109322.755877	57.402330
2601.702416	109107.172294	57.407335
2601.358805	108896.496916	57.412340
2600.296208	108686.083243	57.417345
2599.635773	108479.440403	57.422349
2599.133339	108264.182369	57.427354
2598.465685	108050.881453	57.432359
2598.220793	107841.563806	57.437364
2596.937093	107635.452037	57.442369
2596.299618	107415.432124	57.447373
2595.736369	107208.714862	57.452378
2594.796821	107006.240511	57.457383
2594.553445	106799.044572	57.462388
2593.504080	106593.202752	57.467393
2593.186805	106374.740519	57.472397
2592.487963	106174.170238	57.477402
2591.678925	105963.885911	57.482407
2591.322016	105747.009199	57.487412
2590.281639	105541.428738	57.492417
2589.648538	105341.882845	57.497421
2588.777306	105135.320993	57.502426
2588.136256	104924.568670	57.507431
2587.920953	104708.820948	57.512436
2587.239979	104522.099297	57.517441
2586.548883	104300.422350	57.522445
2585.758748	104091.743943	57.527450
2585.244436	103887.046012	57.532455
2584.635206	103665.209740	57.537460
2583.991592	103461.525687	57.542465
2583.322131	103256.140877	57.547469
2582.780869	103038.854863	57.552474
2581.858786	102827.061776	57.557479
2581.441012	102606.898957	57.562484
2580.571138	102403.412134	57.567489
2579.876634	102197.653512	57.572493
2579.301688	101977.990932	57.577498
2578.293827	101778.014191	57.582503
2577.578158	101562.222175	57.587508
2576.782083	101352.585624	57.592513
2576.265758	101149.751441	57.597517
2575.747040	100952.432005	57.602522
2575.184601	100744.032604	57.607527
2574.639301	100537.960417	57.612532
2573.680228	100333.909416	57.617537
2573.093721	100132.446355	57.622541
2572.373926	99924.846774	57.627546
2571.769930	99714.687038	57.632551
2571.072035	99502.209778	57.637556
2570.442374	99300.773463	57.642561
2569.569061	99093.199320	57.647565
2569.199309	98897.802029	57.652570
2568.504578	98689.987542	57.657575
2568.196389	98479.272021	57.662580
2567.030806	98279.534325	57.667585
2566.358308	98066.343168	57.672589
2565.852182	97869.511020	57.677594
2564.819458	97660.871413	57.682599
2564.466655	97466.853618	57.687604
2563.605699	97261.374446	57.692609
2563.453121	97055.677024	57.697613
2562.649403	96854.010663	57.702618
2561.704028	96647.592677	57.707623
2561.426186	96434.937675	57.712628
2560.711661	96233.934958	57.717633
2559.822008	96026.720983	57.722637
2558.976287	95810.787738	57.727642
2558.485553	95617.720824	57.732647
2558.023715	95407.907833	57.737652
2557.216395	95203.586673	57.742657
2556.525529	94993.179627	57.747661
2555.841666	94799.826865	57.752666
2555.240721	94589.593247	57.757671
2554.757408	94379.025856	57.762676
2553.910012	94186.433589	57.767681
2553.315566	93974.543149	57.772685
2552.778447	93769.456538	57.777690
2551.686032	93566.584247	57.782695
2551.137942	93364.933873	57.787700
2550.552089	93168.332767	57.792705
2550.304796	92949.675048	57.797709
2549.654177	92748.128930	57.802714
2548.896903	92545.390353	57.807719
2548.199712	92332.707393	57.812724
2547.260159	92124.573454	57.817729
2546.750536	91914.331483	57.822733
2545.992231	91713.813704	57.827738
2545.389453	91504.560565	57.832743
2544.844941	91296.283013	57.837748
2543.974724	91108.844436	57.842753
2543.510168	90896.341297	57.847757
2542.619710	90683.020006	57.852762
2541.698762	90479.451263	57.857767
2541.340482	90273.125809	57.862772
2540.268323	90079.958018	57.867777
2539.687595	89867.514929	57.872781
2539.333086	89670.572170	57.877786
2538.516825	89470.584891	57.882791
2538.019871	89268.868636	57.887796
2537.029718	89077.827042	57.892801
2536.703520	88870.685469	57.897805
2536.001771	88670.059684	57.902810
2535.207440	88468.936874	57.907815
2534.775373	88268.234004	57.912820
2533.781452	88070.373605	57.917825
2533.182900	87859.854881	57.922829
2532.799796	87671.081533	57.927834
2531.739852	87460.157994	57.932839
2531.125706	87256.944733	57.937844
2530.574653	87067.493217	57.942849
2530.323658	86862.710910	57.947853
2529.266565	86660.701928	57.952858
2528.443838	86465.599474	57.957863
2528.067307	86258.725401	57.962868
2527.257005	86053.608358	57.967873
2526.367219	85854.553610	57.972877
2525.809693	85659.866528	57.977882
2525.459783	85462.948590	57.982887
2524.960258	85253.916663	57.987892
2523.952582	85061.322234	57.992897
2523.555378	84854.376241	57.997901
2523.051851	84656.450476	58.002906
2522.202879	84455.937971	58.007911
2521.615842	84248.184874	58.012916
2520.664285	84042.874981	58.017921
2520.540099	83837.670455	58.022925
2519.533613	83638.933782	58.027930
2518.793207	83441.754130	58.032935
2518.338659	83228.095089	58.037940
2517.448738	83022.443026	58.042945
2516.886788	82811.283578	58.047949
2515.972907	82615.558941	58.052954
2515.213811	82426.625286	58.057959
2514.551898	82223.042860	58.062964
2513.964706	82024.388021	58.067969
2513.307333	81827.134239	58.072973
2512.637129	81628.591373	58.077978
2511.984964	81433.514429	58.082983
2511.440627	81228.389206	58.087988
2510.523828	81045.323909	58.092993
2509.778608	80831.652891	58.097997
2509.427677	80628.207777	58.103002
2508.578391	80439.642230	58.108007
2507.996506	80246.194023	58.113012
2507.313533	80049.455406	58.118017
2507.127101	79838.069921	58.123021
2506.270261	79644.011795	58.128026
2505.362025	79443.638882	58.133031
2504.693519	79248.882832	58.138036
2503.843825	79055.336073	58.143041
2503.412324	78847.706852	58.148045
2502.509030	78644.280008	58.153050
2501.906265	78456.130679	58.158055
2501.486551	78254.532155	58.163060
2500.703068	78072.542910	58.168065
2500.236172	77868.927798	58.173069
2499.240216	77672.736674	58.178074
2498.610004	77476.565488	58.183079
2498.274447	77273.138236	58.188084
2497.361097	77085.012666	58.193089
2496.724897	76878.455970	58.198093
2496.152928	76682.650675	58.203098
2495.449501	76482.464219	58.208103
2495.169476	76279.735054	58.213108
2494.202886	76095.036048	58.218113
2493.262664	75886.104411	58.223117
2492.755994	75707.621646	58.228122
2492.092220	75508.959173	58.233127
2491.386400	75301.757849	58.238132
2490.743663	75117.098758	58.243137
2489.772843	74916.247788	58.248141
2489.490622	74724.413434	58.253146
2488.854292	74534.461775	58.258151
2487.916654	74339.902821	58.263156
2487.333377	74153.139602	58.268161
2486.574592	73942.678655	58.273165
2485.908960	73755.057849	58.278170
2485.474528	73568.954361	58.283175
2484.816153	73370.977281	58.288180
2484.242959	73179.013686	58.293185
2483.670945	72984.010739	58.298189
2483.109657	72777.788077	58.303194
2482.125461	72584.742293	58.308199
2481.454987	72391.306535	58.313204
2480.421931	72194.414112	58.318209
2480.238684	72005.320460	58.323213
2479.681523	71807.950956	58.328218
2478.604235	71610.254090	58.333223
2478.006462	71421.662467	58.338228
2477.521434	71232.490954	58.343233
2477.046683	71033.405652	58.348237
2476.510098	70840.065083	58.353242
2475.660456	70637.350035	58.358247
2475.161351	70434.974234	58.363252
2474.145341	70241.867536	58.368257
2473.568240	70052.145436	58.373261
2472.998309	69852.821038	58.378266
2472.152952	69654.961212	58.383271
2471.452855	69458.765265	58.388276
2470.941339	69273.341241	58.393281
2470.184746	69078.583242	58.398285
2469.761258	68886.054641	58.403290
2469.184595	68688.795341	58.408295
2468.374191	68488.275076	58.413300
2467.559581	68290.994161	58.418305
2467.252890	68091.747220	58.423309
2466.693501	67899.116842	58.428314
2465.632826	67708.474288	58.433319
2465.137968	67504.139180	58.438324
2464.420222	67308.999930	58.443329
2463.933317	67113.351021	58.448333
2463.148550	66915.502918	58.453338
2462.174907	66721.809820	58.458343
2461.661018	66518.697748	58.463348
2461.034710	66333.915133	58.468353
2460.413598	66130.589791	58.473357
2459.834664	65943.760921	58.478362
2458.827582	65747.388100	58.483367
2458.453130	65553.497684	58.488372
2457.465927	65364.082437	58.493377
2456.864700	65164.576541	58.498381
2456.509925	64974.802034	58.503386
2455.824216	64788.995517	58.508391
2455.368839	64584.583599	58.513396
2453.984492	64400.262633	58.518401
2453.477740	64198.332700	58.523405
2453.350150	64000.381755	58.528410
2452.363513	63815.829205	58.533415
2451.774223	63620.893637	58.538420
2450.676227	63437.394572	58.543425
2450.506453	63237.419187	58.548429
2449.840942	63034.257076	58.553434
2448.891426	62845.009524	58.558439
2448.533542	62644.918196	58.563444
2447.623846	62465.694929	58.568449
2447.016007	62275.667515	58.573453
2446.418281	62080.369105	58.578458
2445.626067	61892.112859	58.583463
2445.229491	61680.953962	58.588468
2444.185580	61506.668129	58.593473
2443.681428	61314.693232	58.598477
2443.350329	61117.383832	58.603482
2442.571448	60920.264618	58.608487
2442.203390	60723.066496	58.613492
2440.937418	60536.101822	58.618497
2440.461272	60340.026498	58.623501
2439.786716	60148.780580	58.628506
2439.225721	59956.926635	58.633511
2438.892604	59760.188892	58.638516
2437.860943	59565.548743	58.643521
2437.150550	59362.686393	58.648525
2436.367730	59186.047667	58.653530
2435.557026	58985.725004	58.658535
2435.295530	58794.785081	58.663540
2434.554822	58603.970566	58.668545
2433.744854	58405.065755	58.673549
2432.931425	58215.811415	58.678554
2432.464123	58034.024771	58.683559
2432.001590	57841.876188	58.688564
2431.267176	57642.188891	58.693569
2430.762706	57448.908380	58.698573
2430.236930	57251.493270	58.703578
2429.268969	57060.933164	58.708583
2428.768943	56859.052199	58.713588
2427.775042	56672.019752	58.718593
2427.476824	56470.819985	58.723597
2426.879684	56276.063020	58.728602
2426.012446	56079.246256	58.733607
2425.262331	55880.805255	58.738612
2424.449015	55700.894004	58.743617
2424.043144	55500.187114	58.748621
2423.047933	55309.551283	58.753626
2422.384231	55113.332864	58.758631
2422.116691	54921.563461	58.763636
2420.944279	54735.715102	58.768641
2420.516680	54550.370804	58.773645
2419.756010	54357.305694	58.778650
2419.132400	54165.673437	58.783655
2418.785920	53973.597346	58.788660
2417.943627	53779.896205	58.793665
2417.088906	53594.360329	58.798669
2416.810798	53412.978460	58.803674
2415.899756	53211.072977	58.808679
2415.407609	53023.099442	58.813684
2414.692842	52837.140877	58.818689
2413.988829	52639.290943	58.823693
2413.350840	52445.011517	58.828698
2412.645699	52260.813509	58.833703
2412.241033	52063.381206	58.838708
2411.239633	51872.864519	58.843713
2410.708723	51674.592644	58.848717
2410.003136	51483.561691	58.853722
2409.439743	51299.983809	58.858727
2408.960535	51099.988769	58.863732
2407.862191	50906.972718	58.868737
2407.420112	50708.494866	58.873741
2406.614843	50524.754406	58.878746
2405.827892	50347.799549	58.883751
2405.288787	50147.546156	58.888756
2404.580687	49961.005495	58.893761
2404.038963	49769.125158	58.898765
2403.412701	49584.166845	58.903770
2402.455849	49389.682988	58.908775
2401.892904	49196.072083	58.913780
2401.181929	49013.920341	58.918785
2400.652245	48817.638102	58.923789
2400.131250	48638.329506	58.928794
2399.244209	48448.609250	58.933799
2398.765320	48260.762395	58.938804
2397.929816	48081.493455	58.943809
2397.476058	47888.850627	58.948813
2396.948741	47703.450062	58.953818
2395.912404	47508.948712	58.958823
2395.622451	47302.297594	58.963828
2394.572839	47120.392915	58.968833
2393.907124	46930.634794	58.973837
2393.485489	46745.850659	58.978842
2392.745035	46555.716162	58.983847
2392.104463	46369.313132	58.988852
2391.329319	46177.138443	58.993857
2390.800895	45992.834617	58.998861
2390.325850	45792.319573	59.003866
2389.462187	45614.380132	59.008871
2388.814229	45411.578299	59.013876
2388.407066	45226.871045	59.018881
2387.593584	45026.282391	59.023885
2387.134868	44843.108743	59.028890
2386.031847	44656.246840	59.033895
2385.831714	44459.192116	59.038900
2385.013955	44278.295325	59.043905
2384.379871	44071.461507	59.048909
2383.528981	43881.145742	59.053914
2382.569801	43691.706328	59.058919
2382.468247	43500.352368	59.063924
2381.423078	43318.179578	59.068929
2380.468639	43122.211518	59.073933
2380.075835	42938.399048	59.078938
2379.492932	42761.402386	59.083943
2378.809532	42566.570924	59.088948
2377.784664	42378.171407	59.093953
2377.278387	42177.993728	59.098957
2376.775353	41999.897955	59.103962
2375.914872	41824.830194	59.108967
2375.616229	41628.310143	59.113972
2375.165411	41449.572956	59.118977
2374.381090	41262.700145	59.123981
2373.701329	41067.426450	59.128986
2372.868572	40874.241001	59.133991
2372.398260	40684.260465	59.138996
2371.424385	40509.072253	59.144001
2371.114256	40306.753865	59.149005
2370.528749	40128.130798	59.154010
2369.626507	39929.793797	59.159015
2369.218433	39740.313430	59.164020
2368.229911	39545.934430	59.169025
2367.335671	39364.373879	59.174029
2366.969058	39169.203324	59.179034
2366.303459	38990.830892	59.184039
2365.700108	38795.977223	59.189044
2364.826906	38615.836216	59.194049
2364.233193	38423.339245	59.199053
2363.328047	38235.756595	59.204058
2362.801206	38061.826769	59.209063
2362.272204	37864.815670	59.214068
2361.517321	37675.530196	59.219073
2360.784252	37490.859314	59.224077
2360.422073	37305.956156	59.229082
2359.447738	37126.599418	59.234087
2358.982001	36934.176476	59.239092
2358.122808	36760.505542	59.244097
2357.532271	36567.019020	59.249101
2356.931019	36379.103630	59.254106
2356.054746	36189.286546	59.259111
2355.697934	36006.320426	59.264116
2354.760064	35829.514959	59.269121
2354.148751	35639.922848	59.274125
2353.730169	35459.559948	59.279130
2352.673932	35285.145149	59.284135
2352.816311	35086.390838	59.289140
2351.851897	34909.676699	59.294145
2351.053302	34715.188628	59.299149
2350.132665	34520.489830	59.304154
2349.279913	34344.693287	59.309159
2348.862738	34159.719567	59.314164
2348.289715	33973.664697	59.319169
2348.006939	33787.134402	59.324173
2346.991251	33605.334138	59.329178
2346.032220	33426.186718	59.334183
2345.980884	33244.817459	59.339188
2344.783454	33054.135398	59.344193
2343.731665	32869.342998	59.349197
2343.541592	32681.060907	59.354202
2343.010955	32502.367522	59.359207
2342.232561	32322.552239	59.364212
2341.338398	32139.310635	59.369217
2340.751324	31958.919008	59.374221
2340.155739	31771.349978	59.379226
2339.755966	31596.463514	59.384231
2339.147992	31411.985161	59.389236
2338.267157	31232.431833	59.394241
2337.622917	31055.225868	59.399245
2337.320865	30864.695628	59.404250
2336.321255	30681.897742	59.409255
2335.501442	30494.004277	59.414260
2335.334795	30314.183343	59.419265
2334.603093	30127.082794	59.424269
2333.622016	29943.222023	59.429274
2332.470415	29756.712135	59.434279
2332.208300	29572.839450	59.439284
2331.572213	29402.158228	59.444289
2331.123224	29224.716649	59.449293
2330.447253	29035.415581	59.454298
2329.807214	28856.308212	59.459303
2329.299046	28668.150807	59.464308
2328.612893	28486.765432	59.469313
2327.776829	28302.876378	59.474317
2327.426055	28125.984119	59.479322
2326.461861	27941.108323	59.484327
2326.021445	27750.712038	59.489332
2325.361522	27566.635890	59.494337
2324.373384	27383.557045	59.499341
2324.180372	27196.036499	59.504346
2323.063309	27012.557311	59.509351
2322.754557	26818.451159	59.514356
2321.933458	26642.073015	59.519361
2321.225380	26457.587381	59.524365
2320.769386	26271.379873	59.529370
2319.821676	26086.085794	59.534375
2319.305950	25901.926686	59.539380
2318.598545	25722.722355	59.544385
2317.439882	25539.615579	59.549389
2316.665222	25360.064992	59.554394
2315.997347	25174.322344	59.559399
2315.657035	24998.582506	59.564404
2314.816722	24831.318627	59.569409
2314.373498	24657.803943	59.574413
2313.657483	24472.244470	59.579418
2312.727017	24304.830569	59.584423
2312.406521	24121.670970	59.589428
2311.478704	23950.885696	59.594433
2310.667647	23759.416925	59.599437
2310.270807	23594.073124	59.604442
2309.738092	23420.041897	59.609447
2309.245295	23240.741976	59.614452
2308.382099	23067.445374	59.619457
2307.810305	22878.611311	59.624461
2307.339093	22701.126386	59.629466
2306.176435	22532.400916	59.634471
2305.709649	22353.237930	59.639476
2305.201958	22179.596888	59.644481
2304.303572	22002.576807	59.649485
2303.869616	21819.481348	59.654490
2303.040576	21644.681851	59.659495
2302.360970	21455.511434	59.664500
2301.791905	21285.805667	59.669505
2301.202642	21106.559303	59.674509
2300.717867	20928.340669	59.679514
2299.857745	20750.485991	59.684519
2299.302978	20561.019046	59.689524
2298.430395	20385.122309	59.694529
2297.434038	20199.799211	59.699533
2297.077616	20034.771850	59.704538
2296.222891	19866.972610	59.709543
2295.844285	19676.596939	59.714548
2295.032168	19506.983966	59.719553
2294.420441	19336.112935	59.724557
2293.790474	19159.635180	59.729562
2292.852070	18991.323263	59.734567
2292.277624	18808.519867	59.739572
2291.699150	18629.315748	59.744577
2291.390758	18455.528109	59.749581
2290.526633	18286.983417	59.754586
2289.575776	18113.117932	59.759591
2289.275771	17939.805205	59.764596
2288.409990	17771.286069	59.769601
2287.883679	17590.858375	59.774605
2287.492324	17409.814553	59.779610
2286.346045	17234.764654	59.784615
2285.743811	17053.975502	59.789620
2285.049814	16879.251378	59.794625
2284.261216	16718.028987	59.799629
2283.959562	16534.070233	59.804634
2283.323390	16365.207422	59.809639
2282.646662	16186.294209	59.814644
2281.763875	16004.730555	59.819649
2281.403318	15845.426659	59.824653
2281.123079	15654.124733	59.829658
2279.745881	15484.080139	59.834663
2279.158745	15300.543001	59.839668
2278.840814	15126.846905	59.844673
2278.034208	14955.971911	59.849677
2277.197251	14767.744327	59.854682
2276.402889	14609.696233	59.859687
2276.145361	14427.283747	59.864692
2275.177564	14257.316083	59.869697
2274.548419	14087.293125	59.874701
2273.785582	13900.950595	59.879706
2272.786998	13728.738874	59.884711
2272.617654	13557.610789	59.889716
2271.865251	13395.618907	59.894721
2271.199531	13223.340643	59.899725
2270.439943	13041.518571	59.904730
2269.535693	12885.094501	59.909735
2269.221625	12701.204891	59.914740
2268.203690	12540.186606	59.919745
2267.672075	12366.069839	59.924750
2267.128564	12191.794770	59.929754
2266.233482	12023.400894	59.934759
2265.614963	11856.798282	59.939764
2265.057429	11684.343494	59.944769
2264.312253	11525.903117	59.949774
2263.950082	11349.074237	59.954778
2262.768545	11200.833781	59.959783
2262.215692	11020.683676	59.964788
2261.651727	10858.628735	59.969793
2261.186364	10698.317166	59.974798
2260.532312	10524.765006	59.979802
2259.319571	10360.517161	59.984807
2258.958973	10192.619889	59.989812
2258.314961	10040.875865	59.994817
2258.029226	9865.537905	59.999822
2257.325413	9693.411789	60.004826
2256.442824	9525.648308	60.009831
2255.419590	9356.524087	60.014836
2254.823316	9192.055033	60.019841
2254.468349	9039.481863	60.024846
2253.939775	8865.253253	60.029850
2252.926736	8702.665977	60.034855
2252.561881	8537.492378	60.039860
2251.786487	8368.527304	60.044865
2251.075044	8206.767764	60.049870
2250.030316	8038.929983	60.054874
2249.284223	7882.658246	60.059879
2248.864035	7707.283470	60.064884
2247.958337	7553.312587	60.069889
2247.401222	7393.532893	60.074894
2246.723988	7234.536824	60.079898
2246.238673	7074.458431	60.084903
2245.431307	6916.379016	60.089908
2244.507560	6753.425548	60.094913
2243.927689	6599.308263	60.099918
2243.501251	6447.231882	60.104922
2242.516656	6295.609650	60.109927
2242.036871	6125.929172	60.114932
2241.472707	5980.638198	60.119937
2240.660507	5826.169757	60.124942
2240.166642	5662.786099	60.129946
2239.302652	5514.069341	60.134951
2238.788288	5365.452423	60.139956
2237.619099	5202.644766	60.144961
2236.906206	5056.386219	60.149966
2236.547080	4896.416880	60.154970
2235.301165	4767.757393	60.159975
2234.954093	4605.208423	60.164980
2233.744465	4472.380293	60.169985
2233.053795	4335.121084	60.174990
2232.361957	4199.010950	60.179994
2231.457185	4064.520412	60.184999
2230.824960	3927.758921	60.190004
2230.137880	3805.149917	60.195009
2229.082122	3671.860521	60.200014
2228.779239	3543.958841	60.205018
2227.738920	3431.810427	60.210023
2226.491876	3312.518553	60.215028
2225.203191	3227.498785	60.220033
2223.273957	3146.276902	60.225038
2222.098167	3066.417080	60.230042
2221.207871	3009.160025	60.235047
2220.097011	2934.393361	60.240052
2219.137359	2872.530165	60.245057
2218.606544	2809.159092	60.250062
2218.125933	2754.987178	60.255066
2217.118394	2709.279366	60.260071
2216.482487	2651.558261	60.265076
2216.258439	2601.112052	60.270081
2215.126201	2561.305487	60.275086
2214.744888	2514.681889	60.280090
2214.108448	2477.219629	60.285095
2213.950460	2416.335282	60.290100
2213.066365	2368.571880	60.295105
2212.255930	2307.006798	60.300110
2211.827801	2259.863049	60.305114
2211.211697	2220.446344	60.310119
2210.725561	2172.179600	60.315124
2209.892972	2102.200251	60.320129
2209.668490	2059.952974	60.325134
2208.952867	2003.334584	60.330138
2208.313450	1949.738144	60.335143
2207.744673	1902.580005	60.340148
2207.008708	1840.438843	60.345153
2206.261091	1790.318226	60.350158
2206.074560	1734.460750	60.355162
2205.361520	1685.868060	60.360167
2204.472409	1622.595237	60.365172
2203.749149	1574.456409	60.370177
2203.080331	1511.533953	60.375182
2202.438300	1465.074926	60.380186
2201.874858	1418.021599	60.385191
2201.341217	1353.398678	60.390196
2200.621925	1316.197790	60.395201
2199.828692	1263.158990	60.400206
2199.502478	1212.100540	60.405210
2198.850014	1166.430334	60.410215
2198.096624	1100.678667	60.415220
2197.413340	1043.421699	60.420225
2196.726047	984.722513	60.425230
2196.115296	941.061187	60.430234
2194.976467	895.823060	60.435239
2194.706217	842.101933	60.440244
2193.730579	804.734055	60.445249
2193.159834	760.652141	60.450254
2192.704540	712.138510	60.455258
2191.945138	664.323844	60.460263
2191.292303	614.257683	60.465268
2190.608305	567.536916	60.470273
2190.114174	526.483399	60.475278
2189.372216	474.197917	60.480282
2188.511224	441.815286	60.485287
2187.786379	380.538089	60.490292
2187.148589	347.194515	60.495297
2186.192325	301.236157	60.500302
2185.815416	258.095695	60.505306
2184.930340	239.046633	60.510311
2184.299056	187.090001	60.515316
2183.437678	154.712805	60.520321
2182.732292	132.937049	60.525326
2182.016983	86.087963	60.530330
2181.129502	56.930710	60.535335
2180.546403	22.246613	60.540340
2179.628131	-8.503155	60.545345
2179.102865	-14.857110	60.550350
2178.221303	-43.553029	60.555354
2177.444757	-57.750640	60.560359
2176.363556	-70.993111	60.565364
2175.019814	-69.992839	60.570369
2172.736935	-44.883847	60.575374
2170.960212	8.671751	60.580378
2170.478735	25.639859	60.585383
2171.033338	37.687263	60.590388
2171.295393	33.611768	60.595393
2171.119831	42.062693	60.600398
2171.069567	29.880336	60.605402
2170.509705	32.749609	60.610407
2170.096245	23.121328	60.615412
2169.723731	17.886473	60.620417
2168.744507	17.548367	60.625422
2167.312453	21.478590	60.630426
2165.851840	36.111934	60.635431
2165.060253	39.164642	60.640436
2164.485523	48.300256	60.645441
2163.892847	48.910119	60.650446
2164.165680	42.271807	60.655450
2163.427846	52.254938	60.660455
2163.108917	45.445577	60.665460
2162.399339	43.957610	60.670465
2161.717014	46.931478	60.675470
2161.052520	44.826046	60.680474
2160.209241	46.650563	60.685479
2159.283802	47.634942	60.690484
2159.040725	48.736566	60.695489
2158.339625	56.993328	60.700494
2157.696145	50.017832	60.705498
2156.654420	56.141295	60.710503
2156.611394	53.680196	60.715508
2155.837932	51.904306	60.720513
2155.005210	55.324687	60.725518
2154.394598	55.596759	60.730522
2154.288057	62.894971	60.735527
2153.640526	57.699011	60.740532
2152.510724	58.827789	60.745537
2151.636935	59.956948	60.750542
2150.763047	56.856514	60.755546
2150.216880	58.517191	60.760551
2150.123159	61.435519	60.765556
2149.559077	62.045580	60.770561
2148.432846	59.691698	60.775566
2147.665006	58.862717	60.780570
2147.477181	62.124000	60.785575
2147.205937	60.815654	60.790580
2146.465045	58.641917	60.795585
2145.465193	64.727202	60.800590
2145.079336	69.152221	60.805594
2143.929073	58.773465	60.810599
2143.259032	55.795239	60.815604
2142.327315	58.933272	60.820609
2141.645653	68.560557	60.825614
2141.401869	69.525095	60.830618
2141.167132	67.433477	60.835623
2140.422060	65.372374	60.840628
2139.679691	67.366978	60.845633
2138.550937	73.963181	60.850638
2138.083195	62.130913	60.855642
2137.278678	73.092944	60.860647
2137.194779	72.420380	60.865652
2136.496489	69.057107	60.870657
2135.721005	66.745351	60.875662
2135.247404	57.538205	60.880666
2134.262928	71.143515	60.885671
2133.607202	69.724282	60.890676
2133.025478	69.591208	60.895681
2132.065687	82.156498	60.900686
2131.198340	67.443310	60.905690
2130.403249	71.698290	60.910695
2130.248059	71.283057	60.915700
2129.938168	69.059856	60.920705
2129.355575	70.265824	60.925710
2128.976782	64.677123	60.930714
2127.995242	65.124761	60.935719
2127.143079	59.393547	60.940724
2126.575364	63.134604	60.945729
2125.673154	64.328209	60.950734
2125.195249	71.716893	60.955738
2124.337233	71.119858	60.960743
2123.329492	67.457169	60.965748
2122.884781	65.911410	60.970753
2122.147879	69.781824	60.975758
2122.425405	72.205981	60.980762
2121.611501	78.099337	60.985767
2120.541076	66.693885	60.990772
2119.847022	70.816134	60.995777
2119.144621	75.685647	61.000782
2119.215738	66.319519	61.005786
2117.741717	71.913903	61.010791
2117.358758	67.671077	61.015796
2116.984264	70.651308	61.020801
2115.794071	73.494461	61.025806
2115.436889	70.925510	61.030810
2114.780090	77.524105	61.035815
2114.200995	70.388577	61.040820
2112.847687	74.834652	61.045825
2112.802556	75.584732	61.050830
2112.146250	68.299023	61.055834
2111.469320	85.375491	61.060839
2110.768995	69.618616	61.065844
2110.183287	66.262719	61.070849
2109.525775	70.218313	61.075854
2108.988701	58.332402	61.080858
2107.970917	65.034011	61.085863
2107.602242	64.245782	61.090868
2106.954808	57.960089	61.095873
2105.590526	65.353807	61.100878
2105.324552	59.310371	61.105882
2104.446897	64.841663	61.110887
2104.099602	66.751503	61.115892
2103.726737	57.919485	61.120897
2102.910115	67.457799	61.125902
2102.629523	66.658747	61.130906
2101.698864	67.954651	61.135911
2101.001193	68.920253	61.140916
2100.059032	66.362131	61.145921
2099.541423	77.029470	61.150926
2099.092295	67.878372	61.155930
2098.045695	76.374497	61.160935
2097.702752	68.583301	61.165940
2096.912735	72.939992	61.170945
2095.901771	66.929620	61.175950
2095.615673	67.601239	61.180954
2094.815642	70.861903	61.185959
2094.404042	69.391323	61.190964
2093.880233	78.832714	61.195969
2092.769229	79.108512	61.200974
2092.386361	68.563840	61.205978
2091.654654	76.693011	61.210983
2091.223188	71.510087	61.215988
2089.949285	66.833038	61.220993
2089.392956	70.450864	61.225998
2089.232003	65.679200	61.231002
2088.563608	68.102070	61.236007
2087.383086	64.156141	61.241012
2087.250957	65.197585	61.246017
2086.150350	70.466206	61.251022
2086.015246	64.742642	61.256026
2084.757273	68.568018	61.261031
2084.380616	66.808028	61.266036
2083.641816	70.085787	61.271041
2083.240735	74.645701	61.276046
2082.315619	70.861100	61.281050
2081.788408	72.368965	61.286055
2081.440432	74.766221	61.291060
2080.508274	71.648247	61.296065
2079.490129	86.083715	61.301070
2079.140874	72.889018	61.306074
2078.261323	72.759064	61.311079
2077.952568	69.606816	61.316084
2077.616603	62.587268	61.321089
2076.576156	74.517203	61.326094
2076.629477	64.529397	61.331098
2075.779318	64.983013	61.336103
2074.776419	68.894075	61.341108
2073.715448	66.231810	61.346113
2072.580089	77.334675	61.351118
2072.830110	67.432351	61.356122
2071.895090	76.874345	61.361127
2070.917773	64.610430	61.366132
2070.586802	73.847742	61.371137
2069.860597	61.279037	61.376142
2069.348420	68.258405	61.381146
2068.773604	67.438238	61.386151
2067.865585	73.584674	61.391156
2067.448279	66.469220	61.396161
2066.917400	76.747562	61.401166
2066.375990	66.034084	61.406170
2065.604329	64.125465	61.411175
2065.016138	69.189761	61.416180
2064.228669	71.830242	61.421185
2062.590450	75.287022	61.426190
2062.728636	69.474352	61.431194
2062.099583	75.721604	61.436199
2061.359014	76.211452	61.441204
2060.986228	73.061483	61.446209
2059.853280	70.640894	61.451214
2059.459384	68.169247	61.456218
2058.672560	74.887840	61.461223
2058.177669	75.773959	61.466228
2057.881281	70.230543	61.471233
2056.895498	74.067929	61.476238
2056.628780	63.025417	61.481242
2055.436007	72.394773	61.486247
2054.473861	69.248452	61.491252
2053.988056	64.529927	61.496257
2053.292456	67.710945	61.501262
2053.151590	68.260166	61.506266
2052.187794	72.646026	61.511271
2051.277899	68.639814	61.516276
2050.876261	69.167341	61.521281
2050.132468	74.002434	61.526286
2049.767234	68.846858	61.531290
2049.357591	68.986128	61.536295
2048.779181	66.215745	61.541300
2047.368204	62.516158	61.546305
2046.495863	68.656935	61.551310
2046.021852	62.389469	61.556314
2045.204396	68.038964	61.561319
2045.170407	70.723874	61.566324
2044.606404	71.196742	61.571329
2043.806402	72.954502	61.576334
2043.469190	64.187802	61.581338
2042.630327	67.229127	61.586343
2041.654152	72.943241	61.591348
2040.592613	72.129364	61.596353
2040.009338	71.774195	61.601358
2040.026632	63.758673	61.606362
2038.887063	76.622186	61.611367
2038.178844	68.975714	61.616372
2037.498065	72.979174	61.621377
2036.640543	59.887249	61.626382
2036.640680	64.716238	61.631386
2036.112771	71.286502	61.636391
2035.668827	66.476176	61.641396
2034.992970	63.039985	61.646401
2033.566626	75.311893	61.651406
2033.008132	63.747963	61.656410
2032.280458	65.585713	61.661415
2032.100911	62.160641	61.666420
2031.199659	61.527920	61.671425
2030.488254	61.268787	61.676430
2030.046384	71.498307	61.681434
2028.954986	71.599123	61.686439
2027.920682	81.001692	61.691444
2027.870557	68.696294	61.696449
2027.312805	66.059840	61.701454
2026.760887	56.464590	61.706458
2025.667378	71.071297	61.711463
2025.092897	66.873081	61.716468
2024.757520	66.035422	61.721473
2024.285147	63.655090	61.726478
2023.498433	62.351300	61.731482
2022.066141	65.646100	61.736487
2021.255072	62.445851	61.741492
2020.725335	67.486683	61.746497
2020.783364	67.242629	61.751502
2020.607161	63.782332	61.756506
2019.367597	69.986134	61.761511
2018.772100	64.485472	61.766516
2018.444146	59.935876	61.771521
2017.102073	69.977102	61.776526
2016.464082	63.139552	61.781530
2015.752693	62.339499	61.786535
2015.246989	64.176716	61.791540
2014.661103	62.295399	61.796545
2014.025623	64.191063	61.801550
2013.994164	59.922431	61.806554
2012.766343	62.817331	61.811559
2011.447237	60.049403	61.816564
2010.865170	68.055480	61.821569
2010.635496	65.497849	61.826574
2010.296989	62.566389	61.831578
2009.318027	64.690048	61.836583
2008.892681	63.751548	61.841588
2008.359129	61.492900	61.846593
2007.467396	61.055806	61.851598
2007.019408	60.001046	61.856602
2005.540697	62.505243	61.861607
2005.202960	60.303829	61.866612
2004.801965	53.788233	61.871617
2003.950271	60.327884	61.876622
2003.759118	59.516224	61.881626
2003.391156	61.801535	61.886631
2002.350758	64.431713	61.891636
2001.519339	56.547760	61.896641
2000.186878	72.917678	61.901646
2000.036909	62.296640	61.906650
1999.282347	71.317323	61.911655
1998.842670	64.593387	61.916660
1998.691179	61.290028	61.921665
1997.921086	59.423761	61.926670
1997.205964	53.148850	61.931674
1995.914026	69.523373	61.936679
1995.109347	63.119163	61.941684
1994.702371	66.333232	61.946689
1993.859979	65.752685	61.951694
1993.906529	66.611222	61.956698
1993.224901	65.953114	61.961703
1992.297519	63.332761	61.966708
1991.457283	63.888914	61.971713
1990.296751	74.655158	61.976718
1989.855859	67.310065	61.981722
1989.407073	67.545448	61.986727
1989.101980	65.389318	61.991732
1988.344552	61.310044	61.996737
1988.043772	70.148305	62.001742
1987.514796	58.568670	62.006746
1986.165822	71.982701	62.011751
1985.125165	67.052629	62.016756
1984.940250	64.965737	62.021761
1984.143297	67.603013	62.026766
1984.006421	58.452852	62.031770
1983.337063	58.049856	62.036775
1982.599412	54.721267	62.041780
1981.346205	55.794008	62.046785
1980.340956	67.369851	62.051790
1980.301682	58.055956	62.056794
1979.658673	64.698114	62.061799
1978.859857	62.065244	62.066804
1978.761985	58.292882	62.071809
1978.145121	62.887056	62.076814
1977.562899	63.815438	62.081818
1976.041491	64.492340	62.086823
1975.610282	65.073460	62.091828
1974.935404	64.956785	62.096833
1974.052239	66.866543	62.101838
1974.005219	54.896581	62.106842
1973.544298	56.067496	62.111847
1972.653262	63.032892	62.116852
1971.893997	52.478622	62.121857
1970.782515	61.134895	62.126862
1970.532036	55.148951	62.131866
1970.146569	69.061351	62.136871
1969.668868	57.497239	62.141876
1968.697989	52.164999	62.146881
1967.324251	62.053562	62.151886
1967.033302	54.183182	62.156890
1966.298477	62.344405	62.161895
1965.848048	52.662099	62.166900
1965.520332	58.572929	62.171905
1964.859120	62.854007	62.176910
1964.054328	57.506441	62.181914
1962.922396	61.565762	62.186919
1962.321174	58.830564	62.191924
1962.011832	50.682395	62.196929
1961.144821	63.906372	62.201934
1960.933810	52.591682	62.206938
1960.001981	62.652961	62.211943
1958.848216	56.657439	62.216948
1958.276934	59.900748	62.221953
1957.604699	65.287501	62.226958
1957.336429	53.750077	62.231962
1956.672759	54.927947	62.236967
1956.240654	63.835941	62.241972
1955.564620	61.850671	62.246977
1954.122014	71.764373	62.251982
1953.759555	62.769879	62.256986
1953.025238	52.113881	62.261991
1952.706626	56.163946	62.266996
1952.659194	55.468253	62.272001
1951.596333	61.390127	62.277006
1950.925674	53.796082	62.282010
1949.659915	63.659627	62.287015
1949.188503	67.700834	62.292020
1949.096937	58.158690	62.297025
1948.045863	68.161631	62.302030
1947.828320	57.385745	62.307034
1946.454229	59.345059	62.312039
1945.838704	63.992646	62.317044
1945.265784	56.028253	62.322049
1944.429849	59.860809	62.327054
1944.237565	54.625760	62.332058
1943.670791	63.014211	62.337063
1943.080278	67.326651	62.342068
1941.949654	60.261389	62.347073
1940.957011	58.775840	62.352078
1940.535629	58.390262	62.357082
1939.974042	64.571623	62.362087
1939.783463	63.644754	62.367092
1939.177884	66.404633	62.372097
1938.642043	61.118463	62.377102
1937.777876	65.860720	62.382106
1936.876371	66.489697	62.387111
1936.362308	57.628094	62.392116
1935.254607	56.581881	62.397121
1934.508362	63.514839	62.402126
1933.873111	57.454360	62.407130
1933.598987	59.860406	62.412135
1932.845690	61.221254	62.417140
1932.596176	60.754773	62.422145
1931.805717	60.241699	62.427150
1930.923169	50.974953	62.432154
1929.927235	66.476136	62.437159
1929.514139	56.086132	62.442164
1928.817005	62.482989	62.447169
1928.260699	69.491457	62.452174
1927.931272	58.099370	62.457178
1927.000347	68.357647	62.462183
1926.195615	59.483841	62.467188
1925.768500	64.719716	62.472193
1924.554644	63.841755	62.477198
1924.573532	57.150700	62.482202
1924.058460	64.274052	62.487207
1922.709439	61.745898	62.492212
1922.092199	59.131531	62.497217
1921.003999	58.109038	62.502222
1920.787933	54.543113	62.507226
1920.555854	56.470952	62.512231
1919.612257	55.969578	62.517236
1919.599518	64.039827	62.522241
1918.182160	61.259160	62.527246
1917.439044	56.073717	62.532250
1916.947247	55.497461	62.537255
1916.607335	61.282492	62.542260
1916.395661	56.703416	62.547265
1914.876839	63.809498	62.552270
1914.076957	54.570636	62.557274
1913.331978	62.876990	62.562279
1912.935985	67.936030	62.567284
1912.246157	57.750822	62.572289
1911.710788	60.658839	62.577294
1911.353612	57.585273	62.582298
1910.666999	60.682890	62.587303
1909.831551	62.201874	62.592308
1909.449320	51.428492	62.597313
1908.560123	65.578565	62.602318
1907.966043	62.998373	62.607322
1906.981218	60.026033	62.612327
1906.430940	59.902210	62.617332
1905.939681	66.073989	62.622337
1905.053867	68.875213	62.627342
1904.849722	58.543507	62.632346
1903.595913	59.034455	62.637351
1902.541643	60.608684	62.642356
1902.232658	52.739604	62.647361
1901.517434	58.592107	62.652366
1901.313233	52.732875	62.657370
1900.539770	58.001661	62.662375
1900.130755	65.953466	62.667380
1899.819521	51.491177	62.672385
1898.515091	64.939164	62.677390
1898.107827	48.352093	62.682394
1897.594539	62.295819	62.687399
1896.420515	62.097556	62.692404
1895.060530	57.803306	62.697409
1894.664030	70.585150	62.702414
1894.519706	59.717220	62.707418
1893.539655	61.533571	62.712423
1893.204357	64.162232	62.717428
1892.777101	48.489861	62.722433
1892.419558	65.435183	62.727438
1891.632478	52.625476	62.732442
1890.438503	58.333209	62.737447
1890.027606	55.417994	62.742452
1889.521360	58.108491	62.747457
1888.800952	59.397894	62.752462
1888.438383	53.322523	62.757466
1887.261891	65.733017	62.762471
1886.493603	60.146282	62.767476
1886.377570	57.715711	62.772481
1885.632684	57.335771	62.777486
1884.598886	56.862925	62.782490
1883.716791	64.232222	62.787495
1882.885937	57.772286	62.792500
1882.683209	45.342919	62.797505
1882.036210	58.052557	62.802510
1882.046438	55.720216	62.807514
1880.932748	59.369797	62.812519
1879.896086	59.532951	62.817524
1879.817918	52.904622	62.822529
1878.914847	60.201551	62.827534
1877.764940	56.839099	62.832538
1876.819850	60.895596	62.837543
1876.334114	56.973505	62.842548
1875.921820	45.602483	62.847553
1875.177208	61.775009	62.852558
1875.072484	47.227899	62.857562
1874.383041	59.250385	62.862567
1873.729146	57.444559	62.867572
1873.118950	51.353314	62.872577
1872.187785	57.497164	62.877582
1872.022875	53.462631	62.882586
1870.742498	51.480299	62.887591
1869.692133	66.886053	62.892596
1869.558232	53.398606	62.897601
1868.717513	65.134441	62.902606
1868.340246	58.891087	62.907610
1867.467688	50.081698	62.912615
1866.940207	54.420412	62.917620
1866.212203	59.882271	62.922625
1865.144046	57.891477	62.927630
1864.705463	56.381066	62.932634
1864.153085	57.180148	62.937639
1863.721004	58.956813	62.942644
1863.281018	57.077600	62.947649
1862.221456	61.483454	62.952654
1861.738717	60.598250	62.957658
1860.998187	54.434657	62.962663
1860.565249	54.396296	62.967668
1859.418858	64.064295	62.972673
1858.239006	61.905148	62.977678
1858.230569	60.334323	62.982682
1857.425296	54.734549	62.987687
1856.927577	62.812410	62.992692
1856.799675	57.764278	62.997697
1856.144071	64.922568	63.002702
1855.095788	61.698538	63.007706
1854.480653	59.456034	63.012711
1854.078097	62.817659	63.017716
1853.152227	54.869913	63.022721
1851.714135	58.219338	63.027726
1851.563905	58.241749	63.032730
1850.885429	56.941329	63.037735
1850.336489	56.987625	63.042740
1849.999200	60.906617	63.047745
1848.947988	57.809218	63.052750
1848.147623	51.104748	63.057754
1847.449145	53.869932	63.062759
1846.983119	59.003177	63.067764
1846.639233	52.918540	63.072769
1846.210163	58.966902	63.077774
1845.486945	49.204940	63.082778
1844.458143	67.855957	63.087783
1843.778374	59.184704	63.092788
1843.262517	47.915294	63.097793
1841.985083	55.613891	63.102798
1841.257573	45.508822	63.107802
1840.653376	54.295903	63.112807
1840.170739	55.866122	63.117812
1839.766703	51.524194	63.122817
1839.243329	53.542450	63.127822
1839.019208	53.612867	63.132826
1838.246243	58.001606	63.137831
1837.509022	53.884481	63.142836
1836.874092	48.607768	63.147841
1835.500941	56.349954	63.152846
1834.879086	53.786809	63.157850
1833.845806	51.197528	63.162855
1833.383774	50.343737	63.167860
1833.334369	52.698335	63.172865
1832.649327	53.972674	63.177870
1832.378044	51.733925	63.182874
1831.844056	59.245085	63.187879
1830.770301	49.236002	63.192884
1830.241360	56.610734	63.197889
1829.371808	58.601958	63.202894
1828.132241	53.501688	63.207898
1827.190623	57.161814	63.212903
1826.495194	54.208212	63.217908
1826.434567	47.935091	63.222913
1825.740812	52.454763	63.227918
1825.591094	52.994360	63.232922
1825.049666	54.931903	63.237927
1824.254080	59.944011	63.242932
1823.662013	52.960456	63.247937
1822.737113	55.091364	63.252942
1822.372244	46.499437	63.257946
1821.175486	56.031931	63.262951
1820.138688	52.668893	63.267956
1819.936586	50.058021	63.272961
1818.924703	55.224330	63.277966
1819.034728	48.603974	63.282970
1818.479494	57.118343	63.287975
1817.065056	52.654582	63.292980
1816.734924	49.597241	63.297985
1815.820544	57.112034	63.302990
1815.629842	55.994375	63.307994
1815.171795	46.690235	63.312999
1813.772756	52.703385	63.318004
1813.627949	52.696552	63.323009
1812.687192	53.317611	63.328014
1812.068288	53.307213	63.333018
1811.378827	54.550718	63.338023
1810.740896	53.994536	63.343028
1809.832111	54.339270	63.348033
1808.990508	64.807326	63.353038
1808.608482	59.134047	63.358042
1808.520837	59.424080	63.363047
1807.544192	65.709223	63.368052
1806.738395	55.703329	63.373057
1805.776764	53.009637	63.378062
1805.442200	44.829237	63.383066
1805.005830	57.743565	63.388071
1804.538720	57.221761	63.393076
1803.565637	54.398995	63.398081
1802.856626	62.819513	63.403086
1802.440766	55.297024	63.408090
1801.838330	52.905854	63.413095
1800.591136	52.217760	63.418100
1799.951852	50.657228	63.423105
1799.273264	59.268465	63.428110
1798.895542	51.487597	63.433114
1798.291373	52.995118	63.438119
1797.530644	52.299160	63.443124
1796.668607	60.702977	63.448129
1796.087621	58.354135	63.453134
1795.658946	47.774251	63.458138
1795.113514	58.449172	63.463143
1794.320432	50.537140	63.468148
1793.740578	54.614510	63.473153
1792.437248	62.198966	63.478158
1792.264518	47.648480	63.483162
1791.713006	56.927120	63.488167
1791.420035	58.913526	63.493172
1790.494369	55.638512	63.498177
1789.376824	57.435732	63.503182
1789.097982	48.647214	63.508186
1788.730503	44.766293	63.513191
1787.585584	55.555342	63.518196
1786.783380	47.151153	63.523201
1785.618263	56.063595	63.528206
1785.574683	54.616630	63.533210
1785.047799	52.246583	63.538215
1784.467177	58.793705	63.543220
1783.939727	55.411295	63.548225
1782.480735	55.209453	63.553230
1782.153346	57.491499	63.558234
1781.701811	59.108831	63.563239
1781.436187	57.818561	63.568244
1780.746771	50.462532	63.573249
1779.668103	55.972213	63.578254
1778.852385	50.610683	63.583258
1778.429305	63.508713	63.588263
1777.954703	51.341748	63.593268
1777.528636	46.892940	63.598273
1776.126407	58.287436	63.603278
1775.858773	55.056163	63.608282
1775.317919	55.780890	63.613287
1774.291916	61.559769	63.618292
1773.697002	56.699361	63.623297
1772.411627	59.849523	63.628302
1772.153003	58.603875	63.633306
1772.026287	63.751055	63.638311
1771.333917	60.314411	63.643316
1770.897400	52.353644	63.648321
1769.577682	66.952182	63.653326
1769.039673	58.401951	63.658330
1768.289645	60.473564	63.663335
1767.960692	60.798768	63.668340
1767.501852	54.801792	63.673345
1766.523536	64.033101	63.678350
1766.005405	51.631768	63.683354
1764.928430	62.241296	63.688359
1764.648840	54.659325	63.693364
1764.249971	54.058879	63.698369
1763.279324	61.079553	63.703374
1762.682109	58.523552	63.708378
1762.433676	54.363516	63.713383
1761.179300	60.694357	63.718388
1760.427628	52.818340	63.723393
1759.627778	59.824504	63.728398
1759.151078	56.555471	63.733402
1758.879592	62.958879	63.738407
1757.765556	64.807598	63.743412
1756.931036	53.748102	63.748417
1756.217963	59.915699	63.753422
1755.790857	57.764789	63.758426
1755.386778	57.595700	63.763431
1754.956903	52.769014	63.768436
1754.596693	48.005385	63.773441
1753.293949	60.230954	63.778446
1752.931406	53.384440	63.783450
1751.921349	53.363638	63.788455
1750.808331	59.373973	63.793460
1750.284947	46.268552	63.798465
1749.257265	56.733052	63.803470
1749.094028	49.753956	63.808474
1748.597847	51.058246	63.813479
1748.002709	48.572887	63.818484
1747.891503	51.497145	63.823489
1747.192967	51.329091	63.828494
1746.281356	47.810579	63.833498
1745.615726	43.414022	63.838503
1744.874312	54.487520	63.843508
1743.992232	52.487726	63.848513
1742.981785	48.153820	63.853518
1742.925828	49.233643	63.858522
1742.422416	49.652794	63.863527
1741.789378	54.014600	63.868532
1740.680711	52.301544	63.873537
1739.890843	53.720294	63.878542
1739.385472	50.875310	63.883546
1738.842022	58.864246	63.888551
1738.109985	60.781615	63.893556
1737.392832	58.273057	63.898561
1736.909703	53.609381	63.903566
1736.229344	57.847813	63.908570
1736.024505	55.188495	63.913575
1734.658243	57.056782	63.918580
1734.165521	61.317454	63.923585
1733.464343	67.751265	63.928590
1733.059187	53.688733	63.933594
1731.714900	57.919072	63.938599
1730.986333	60.881461	63.943604
1730.345711	49.942578	63.948609
1729.823190	60.011443	63.953614
1729.743044	57.135192	63.958618
1729.267214	55.197040	63.963623
1728.689740	57.933571	63.968628
1728.201507	52.300837	63.973633
1726.819805	60.802981	63.978638
1726.572321	57.172680	63.983642
1725.190276	54.971594	63.988647
1724.308060	63.356556	63.993652
1724.214331	50.450991	63.998657
1723.098384	56.846595	64.003662
1722.961969	46.138306	64.008666
1722.949207	58.632098	64.013671
1721.455239	51.747672	64.018676
1720.864021	41.617852	64.023681
1720.073394	59.970842	64.028686
1719.781907	51.178037	64.033690
1719.278236	57.735023	64.038695
1718.368127	54.080658	64.043700
1718.004710	49.942048	64.048705
1716.796492	56.891653	64.053710
1716.735870	47.560686	64.058714
1715.530023	53.432805	64.063719
1714.745606	56.796749	64.068724
1714.050789	47.487666	64.073729
1713.596578	50.982094	64.078734
1713.265212	50.153304	64.083738
1712.890891	45.686830	64.088743
1711.831448	55.941908	64.093748
1711.581458	54.273830	64.098753
1710.284628	53.122133	64.103758
1709.413939	54.175243	64.108762
1708.839138	51.732397	64.113767
1708.171325	55.902606	64.118772
1707.908025	44.424385	64.123777
1707.338629	56.292197	64.128782
1706.512572	45.348085	64.133786
1705.666888	53.528539	64.138791
1704.941941	55.577260	64.143796
1704.608176	48.418667	64.148801
1704.016363	58.662552	64.153806
1703.073786	45.623733	64.158810
1702.047243	41.748164	64.163815
1701.687334	49.222221	64.168820
1701.385887	42.460640	64.173825
1700.884814	45.177153	64.178830
1699.850593	50.459018	64.183834
1699.156946	46.981599	64.188839
1698.612690	53.294286	64.193844
1698.022553	47.291376	64.198849
1696.569735	50.912890	64.203854
1696.224705	45.859843	64.208858
1695.678046	44.584262	64.213863
1695.244029	51.926582	64.218868
1695.089050	50.021054	64.223873
1693.915381	54.262157	64.228878
1693.274664	46.841651	64.233882
1692.589566	48.574948	64.238887
1691.699341	48.155071	64.243892
1691.607860	43.121677	64.248897
1690.313539	51.557910	64.253902
1689.755144	43.113457	64.258906
1689.046594	42.926508	64.263911
1688.567508	39.254156	64.268916
1688.634856	42.809246	64.273921
1687.487027	47.330109	64.278926
1686.831479	50.555311	64.283930
1686.262600	49.270644	64.288935
1685.055948	48.000552	64.293940
1684.109096	37.881505	64.298945
1683.285013	58.504420	64.303950
1682.735848	45.485124	64.308954
1682.531660	48.201791	64.313959
1681.928434	49.638221	64.318964
1681.958872	36.657756	64.323969
1681.092170	46.918491	64.328974
1680.032285	48.824872	64.333978
1679.499934	45.326569	64.338983
1678.894972	45.665665	64.343988
1677.809665	43.641407	64.348993
1676.790504	48.214378	64.353998
1676.202297	44.420583	64.359002
1675.754029	49.707150	64.364007
1675.424473	51.265695	64.369012
1675.457536	39.926495	64.374017
1674.672346	52.285924	64.379022
1673.517908	45.751316	64.384026
1673.147353	49.475322	64.389031
1671.993266	48.673147	64.394036
1671.009904	52.157018	64.399041
1670.353880	57.465553	64.404046
1669.816232	53.928666	64.409050
1669.181555	53.133871	64.414055
1668.817595	51.879737	64.419060
1668.860544	50.543616	64.424065
1667.960650	57.501035	64.429070
1666.832024	53.159124	64.434074
1666.495076	48.459629	64.439079
1665.270801	54.780994	64.444084
1664.542922	42.217472	64.449089
1663.790030	50.070941	64.454094
1663.487136	37.502992	64.459098
1663.110589	42.227783	64.464103
1662.213615	54.182330	64.469108
1661.410132	52.521757	64.474113
1661.028403	52.614073	64.479118
1660.673200	48.740687	64.484122
1659.850605	51.694374	64.489127
1658.799464	56.824394	64.494132
1658.540362	43.497242	64.499137
1657.623894	58.176836	64.504142
1656.580461	52.901990	64.509146
1655.939146	49.138715	64.514151
1655.235440	58.100910	64.519156
1654.899658	42.932936	64.524161
1654.060748	47.549823	64.529166
1654.153705	45.376243	64.534170
1653.238459	43.883246	64.539175
1652.077540	41.183428	64.544180
1651.824514	43.024721	64.549185
1651.001587	45.308227	64.554190
1650.478753	54.407275	64.559194
1649.615732	48.132326	64.564199
1648.817318	48.265607	64.569204
1648.605609	46.839049	64.574209
1647.538500	51.932182	64.579214
1646.552106	52.142638	64.584218
1646.046636	57.436722	64.589223
1645.471215	56.317114	64.594228
1645.190815	54.065645	64.599233
1644.665470	60.755401	64.604238
1644.080162	55.265847	64.609242
1642.939323	52.226935	64.614247
1642.206457	54.261161	64.619252
1641.971179	54.839593	64.624257
1641.021746	54.681463	64.629262
1640.249450	57.775407	64.634266
1639.742411	52.366466	64.639271
1639.172376	59.984305	64.644276
1638.599596	51.157354	64.649281
1637.238568	58.974977	64.654286
1636.657558	52.014956	64.659290
1636.224041	48.250214	64.664295
1635.639475	57.299146	64.669300
1635.582711	52.170348	64.674305
1634.733881	57.626220	64.679310
1633.483780	53.529139	64.684314
1632.926985	51.737917	64.689319
1632.362937	54.071769	64.694324
1632.047710	50.926930	64.699329
1631.417332	58.855568	64.704334
1630.266140	49.801954	64.709338
1629.663209	46.751712	64.714343
1629.062048	47.266842	64.719348
1629.030302	46.071904	64.724353
1627.886205	51.897975	64.729358
1626.611023	51.551896	64.734362
1626.454517	48.328223	64.739367
1625.800148	51.434974	64.744372
1625.598353	46.275602	64.749377
1624.727653	54.360696	64.754382
1623.827974	53.915535	64.759386
1623.517243	53.977653	64.764391
1622.887764	54.355351	64.769396
1621.826894	50.907911	64.774401
1620.582365	57.894864	64.779406
1620.155072	51.016087	64.784410
1619.772170	56.798503	64.789415
1618.882336	52.719890	64.794420
1618.974355	59.426688	64.799425
1618.286173	55.752873	64.804430
1617.362173	55.380967	64.809434
1616.750846	57.641905	64.814439
1616.068553	60.045012	64.819444
1615.535244	43.998487	64.824449
1614.332499	55.184727	64.829454
1614.172165	49.041013	64.834458
1613.546910	48.075994	64.839463
1612.164858	60.634352	64.844468
1611.935340	53.184811	64.849473
1611.239801	52.592098	64.854478
1610.767026	47.242381	64.859482
1610.558058	51.735541	64.864487
1609.484333	50.422287	64.869492
1608.595970	42.963884	64.874497
1607.981007	52.038146	64.879502
1607.439314	47.492623	64.884506
1606.747669	47.900703	64.889511
1605.538201	55.025600	64.894516
1605.355575	46.463119	64.899521
1604.617086	42.947121	64.904526
1604.462087	50.585755	64.909530
1603.514983	52.892159	64.914535
1602.421658	51.389625	64.919540
1601.798223	43.999523	64.924545
1601.337322	49.422153	64.929550
1600.890786	49.937955	64.934554
1600.715739	36.769365	64.939559
1599.567883	43.633722	64.944564
1598.988416	44.555438	64.949569
1598.283128	49.466516	64.954574
1597.231761	46.252555	64.959578
1596.781405	47.581132	64.964583
1595.910510	48.733664	64.969588
1595.665494	41.707660	64.974593
1594.891342	48.604113	64.979598
1594.112094	45.750636	64.984602
1593.443318	52.180897	64.989607
1592.514529	49.942564	64.994612
1592.458855	43.815343	64.999617
1591.630187	44.697804	65.004622
1590.567733	44.623886	65.009626
1590.010158	46.762743	65.014631
1589.241421	52.992835	65.019636
1589.201085	47.973401	65.024641
1588.647309	49.982338	65.029646
1587.727960	44.724084	65.034650
1586.873861	44.230691	65.039655
1586.333729	49.924544	65.044660
1585.931395	49.703162	65.049665
1584.480922	48.355159	65.054670
1584.064113	46.978542	65.059674
1583.366369	45.561404	65.064679
1583.018491	48.359257	65.069684
1582.609600	41.233132	65.074689
1581.443143	50.284632	65.079694
1580.695531	53.287932	65.084698
1580.476615	52.321439	65.089703
1579.671493	51.962199	65.094708
1579.427462	44.734180	65.099713
1578.270219	42.984759	65.104718
1577.788008	40.238641	65.109722
1577.041457	41.661594	65.114727
1575.902511	45.922457	65.119732
1575.469301	40.722589	65.124737
1574.625202	45.160541	65.129742
1574.166320	48.903323	65.134746
1573.989667	41.339735	65.139751
1573.363774	47.223841	65.144756
1572.522237	42.806400	65.149761
1571.473144	52.660886	65.154766
1571.080687	46.274927	65.159770
1570.552937	44.532725	65.164775
1569.674457	52.423517	65.169780
1569.079545	48.843713	65.174785
1568.061682	47.617800	65.179790
1567.933340	41.137836	65.184794
1567.513655	50.433398	65.189799
1566.190124	52.380139	65.194804
1565.344460	44.916545	65.199809
1564.782893	53.875093	65.204814
1564.640040	51.287951	65.209818
1564.167340	49.179017	65.214823
1563.274438	50.271976	65.219828
1562.693688	47.117298	65.224833
1562.200061	56.129709	65.229838
1561.369592	46.899011	65.234842
1560.098653	42.264364	65.239847
1559.009068	46.205140	65.244852
1559.194278	45.209129	65.249857
1558.401404	48.315825	65.254862
1558.075676	48.224208	65.259866
1557.133234	48.919745	65.264871
1556.409600	50.731742	65.269876
1556.230083	43.797843	65.274881
1555.417336	62.062900	65.279886
1554.563172	48.227902	65.284890
1553.431927	43.585254	65.289895
1552.872742	47.134232	65.294900
1552.616618	40.201469	65.299905
1551.866181	43.966925	65.304910
1551.740953	49.642165	65.309914
1550.871575	55.148634	65.314919
1550.106130	52.960058	65.319924
1549.507547	43.832875	65.324929
1548.223355	52.573499	65.329934
1547.591759	41.682142	65.334938
1547.320586	40.716072	65.339943
1546.394200	53.386555	65.344948
1546.519583	51.278785	65.349953
1545.520459	43.743387	65.354958
1544.348886	43.525971	65.359962
1543.996173	48.176021	65.364967
1543.577760	48.159061	65.369972
1542.499982	36.895467	65.374977
1541.795259	46.983831	65.379982
1541.046286	51.111774	65.384986
1540.848979	44.953445	65.389991
1540.168088	44.527166	65.394996
1539.426703	51.524087	65.400001
1538.649219	47.702055	65.405006
1538.061677	46.877726	65.410010
1537.766598	46.593575	65.415015
1536.703159	40.501917	65.420020
1535.630198	37.619437	65.425025
1535.209541	45.407520	65.430030
1534.651457	48.017998	65.435034
1534.698392	44.952826	65.440039
1533.128950	49.305772	65.445044
1532.591017	44.483692	65.450049
1531.663139	53.317519	65.455054
1531.210664	43.815447	65.460058
1530.882555	46.176483	65.465063
1530.602712	47.164146	65.470068
1529.705518	46.340138	65.475073
1529.085341	51.964714	65.480078
1528.162239	44.237462	65.485082
1527.208524	47.336608	65.490087
1526.437696	37.896170	65.495092
1526.504398	42.313984	65.500097
1525.517638	46.205315	65.505102
1525.092963	43.904246	65.510106
1524.164098	38.707460	65.515111
1523.260701	41.727643	65.520116
1523.065938	40.486071	65.525121
1522.183683	46.423541	65.530126
1521.132686	47.861773	65.535130
1520.253001	44.306736	65.540135
1519.767012	50.075576	65.545140
1519.840057	43.629850	65.550145
1519.032152	52.993418	65.555150
1518.613367	48.035707	65.560154
1517.612310	49.339842	65.565159
1516.801820	46.417236	65.570164
1516.592720	42.580586	65.575169
1515.678478	42.762278	65.580174
1514.433817	43.223571	65.585178
1514.315126	39.042957	65.590183
1513.891300	42.991496	65.595188
1513.284050	36.620765	65.600193
1512.090722	46.055042	65.605198
1511.555977	44.634100	65.610202
1511.183096	45.649167	65.615207
1510.201557	48.651810	65.620212
1509.492119	39.917591	65.625217
1508.646176	44.616063	65.630222
1508.150651	43.056419	65.635226
1507.849619	43.151703	65.640231
1507.225033	44.369204	65.645236
1506.525712	35.302206	65.650241
1505.600740	45.600626	65.655246
1504.909749	41.392685	65.660250
1504.701740	30.315761	65.665255
1503.440198	48.387189	65.670260
1502.863439	38.307189	65.675265
1502.175608	38.064958	65.680270
1501.715019	38.504158	65.685274
1501.678451	35.302442	65.690279
1500.340436	40.773005	65.695284
1499.670965	25.831598	65.700289
1498.833973	41.383283	65.705294
1498.671106	36.782319	65.710298
1497.723000	31.678494	65.715303
1496.831134	39.935717	65.720308
1496.145737	33.553756	65.725313
1495.978219	44.113440	65.730318
1495.460221	33.005351	65.735322
1494.409626	30.387431	65.740327
1493.463390	41.830993	65.745332
1493.196434	27.147331	65.750337
1492.668536	34.796329	65.755342
1491.365117	37.255594	65.760346
1490.652579	32.112757	65.765351
1490.104790	35.606314	65.770356
1489.875189	25.463270	65.775361
1489.231345	36.642720	65.780366
1488.807835	32.114722	65.785370
1488.177551	33.359942	65.790375
1486.935771	37.925776	65.795380
1486.694848	34.341781	65.800385
1485.951987	37.752796	65.805390
1485.062273	39.741022	65.810394
1484.325410	29.710134	65.815399
1483.421751	32.258841	65.820404
1483.399188	22.816210	65.825409
1482.964851	34.096410	65.830414
1482.122684	32.684908	65.835418
1481.213525	25.497966	65.840423
1480.392557	39.388080	65.845428
1480.022616	26.089644	65.850433
1479.086533	32.273806	65.855438
1478.161985	33.463288	65.860442
1478.097041	27.731813	65.865447
1477.352334	29.017298	65.870452
1477.076373	42.369771	65.875457
1475.703367	33.217458	65.880462
1475.036295	42.262166	65.885466
1474.685625	29.102598	65.890471
1474.055377	41.612475	65.895476
1473.652861	31.541068	65.900481
1472.465246	37.183289	65.905486
1471.783257	34.547797	65.910490
1471.202185	33.690916	65.915495
1470.760229	39.730316	65.920500
1470.439359	34.451116	65.925505
1469.042081	39.718214	65.930510
1468.713077	33.046221	65.935514
1468.412767	41.527993	65.940519
1467.473992	40.054575	65.945524
1466.906539	34.182181	65.950529
1466.027153	45.025322	65.955534
1465.524769	43.479393	65.960538
1464.499032	39.704730	65.965543
1463.730699	45.086346	65.970548
1463.420222	32.814561	65.975553
1462.708894	42.266868	65.980558
1462.578536	34.624976	65.985562
1461.310997	32.402688	65.990567
1460.449445	36.857636	65.995572
1460.330883	35.044116	66.000577
1459.664596	36.146825	66.005582
1458.236303	37.424264	66.010586
1457.637367	40.643670	66.015591
1457.086338	39.258446	66.020596
1456.867608	35.801821	66.025601
1456.483366	36.159506	66.030606
1455.817574	39.033131	66.035610
1455.217913	43.990531	66.040615
1453.903413	46.915221	66.045620
1453.781950	35.163776	66.050625
1452.837785	35.142079	66.055630
1451.677325	35.446510	66.060634
1451.485288	32.096036	66.065639
1450.782577	46.665986	66.070644
1450.811669	35.048314	66.075649
1449.597948	39.996075	66.080654
1448.810092	39.533203	66.085658
1448.324985	34.975577	66.090663
1447.686984	40.699195	66.095668
1446.877730	30.891148	66.100673
1445.974676	36.622198	66.105678
1445.019109	37.116425	66.110682
1444.585187	33.599384	66.115687
1444.092902	39.940112	66.120692
1444.238741	34.768094	66.125697
1443.230408	36.033987	66.130702
1442.139644	43.100649	66.135706
1441.793389	38.342750	66.140711
1440.906212	45.009609	66.145716
1440.028993	37.218334	66.150721
1439.297175	46.711753	66.155726
1439.019725	41.226951	66.160730
1438.915467	41.464439	66.165735
1437.295116	49.085233	66.170740
1436.909340	35.634769	66.175745
1436.168242	44.246531	66.180750
1435.997252	47.699134	66.185754
1435.371695	29.661385	66.190759
1433.770229	48.636878	66.195764
1433.110624	36.683953	66.200769
1432.943730	40.170597	66.205774
1432.615072	44.326379	66.210778
1432.281601	34.575181	66.215783
1431.031761	41.485773	66.220788
1430.853569	38.399615	66.225793
1429.994547	46.156454	66.230798
1428.722460	41.287085	66.235802
1427.840793	42.220601	66.240807
1427.076753	38.899543	66.245812
1426.958093	46.631747	66.250817
1426.638362	46.635392	66.255822
1426.448328	48.406763	66.260826
1425.374036	45.672783	66.265831
1424.363440	40.593112	66.270836
1424.174511	41.941666	66.275841
1422.995084	40.161149	66.280846
1422.139837	44.763349	66.285850
1421.874106	35.912903	66.290855
1421.006340	37.670570	66.295860
1420.933141	39.502221	66.300865
1419.798610	40.814991	66.305870
1419.199265	38.038639	66.310874
1418.524906	37.321183	66.315879
1417.544109	44.523345	66.320884
1416.734484	36.161494	66.325889
1415.911440	40.034723	66.330894
1415.631314	45.532722	66.335898
1415.419205	42.740551	66.340903
1414.604172	45.708875	66.345908
1414.259147	48.540987	66.350913
1413.060822	48.711099	66.355918
1412.542147	48.440427	66.360922
1412.266352	45.514869	66.365927
1411.324751	49.504722	66.370932
1410.299133	44.892665	66.375937
1409.874689	50.864634	66.380942
1409.260892	46.981934	66.385946
1408.830398	46.539543	66.390951
1407.696947	51.349981	66.395956
1407.208331	44.217645	66.400961
1406.484075	48.739101	66.405966
1405.974873	43.504040	66.410970
1405.664634	50.393028	66.415975
1404.248601	42.015604	66.420980
1403.961949	46.838100	66.425985
1403.112099	49.043953	66.430990
1402.848055	52.031935	66.435994
1402.339299	51.127303	66.440999
1401.264878	50.735229	66.446004
1400.663253	47.167578	66.451009
1400.217863	40.659182	66.456014
1399.510392	46.608329	66.461018
1398.532173	39.504936	66.466023
1397.742310	48.118151	66.471028
1397.150726	36.840432	66.476033
1396.869199	50.125981	66.481038
1396.201434	48.305144	66.486042
1395.471921	38.433973	66.491047
1394.895812	45.489808	66.496052
1394.264325	38.585201	66.501057
1393.063393	41.711073	66.506062
1391.983716	44.401337	66.511066
1391.771825	40.087309	66.516071
1391.290887	47.586930	66.521076
1391.270796	34.426872	66.526081
1390.640859	41.406103	66.531086
1389.538798	40.636790	66.536090
1389.179367	41.701777	66.541095
1387.834172	40.315074	66.546100
1387.091439	38.696978	66.551105
1386.518073	42.270317	66.556110
1385.978493	47.640821	66.561114
1385.445124	37.992375	66.566119
1384.775374	56.712550	66.571124
1384.412173	48.546256	66.576129
1383.427188	53.098127	66.581134
1382.673398	57.671597	66.586138
1382.348273	41.065345	66.591143
1381.743252	52.114065	66.596148
1380.901459	44.806056	66.601153
1380.235922	39.099094	66.606158
1379.635218	44.867261	66.611162
1378.954901	46.603029	66.616167
1377.747235	48.283851	66.621172
1377.252960	42.403001	66.626177
1376.323048	46.484050	66.631182
1376.064631	47.253848	66.636186
1376.082916	43.892023	66.641191
1374.932687	50.206464	66.646196
1374.427995	45.166244	66.651201
1373.923698	45.762232	66.656206
1373.256295	54.149398	66.661210
1372.254244	33.566286	66.666215
1371.564936	50.225245	66.671220
1371.168381	45.278226	66.676225
1370.792390	42.209325	66.681230
1369.592393	42.348183	66.686234
1368.865703	36.510592	66.691239
1368.137262	50.783436	66.696244
1367.646350	42.352011	66.701249
1366.301402	40.897468	66.706254
1365.758672	51.155661	66.711258
1365.553773	41.917068	66.716263
1364.907698	48.588199	66.721268
1364.750459	37.564730	66.726273
1364.120715	41.311046	66.731278
1363.033293	31.138808	66.736282
1362.404677	35.679761	66.741287
1361.615355	41.905287	66.746292
1361.071598	36.918595	66.751297
1360.048245	36.278714	66.756302
1359.531110	44.561561	66.761306
1359.323131	37.510788	66.766311
1358.478750	43.051180	66.771316
1358.046503	31.785996	66.776321
1356.907204	41.080844	66.781326
1356.059345	48.172002	66.786330
1355.670691	41.291883	66.791335
1355.123762	45.509181	66.796340
1354.845716	39.931444	66.801345
1353.637651	41.902511	66.806350
1352.897484	37.913758	66.811354
1352.785403	41.375921	66.816359
1351.300468	45.961548	66.821364
1350.971596	36.390994	66.826369
1350.674103	42.842698	66.831374
1349.962254	38.346375	66.836378
1349.519420	36.308436	66.841383
1348.348321	48.394940	66.846388
1347.705866	46.582709	66.851393
1347.244030	40.318225	66.856398
1346.514147	45.725297	66.861402
1345.641453	43.178509	66.866407
1344.622365	37.489918	66.871412
1344.445660	38.547939	66.876417
1343.585084	44.456779	66.881422
1343.412253	40.270595	66.886426
1343.354119	38.029566	66.891431
1342.044441	46.422645	66.896436
1341.513702	41.142138	66.901441
1340.126172	49.121802	66.906446
1339.165628	50.129391	66.911450
1338.830867	43.917248	66.916455
1338.220089	50.879253	66.921460
1338.096805	38.306487	66.926465
1337.688660	41.093445	66.931470
1337.052889	46.050299	66.936474
1336.258149	43.249837	66.941479
1335.308883	43.410352	66.946484
1334.928054	37.222884	66.951489
1333.540707	45.644085	66.956494
1332.624670	46.579943	66.961498
1332.517995	38.136330	66.966503
1331.843121	50.658056	66.971508
1331.503804	38.289956	66.976513
1331.183470	43.893703	66.981518
1330.083622	46.699167	66.986522
1329.649975	42.051381	66.991527
1328.342382	47.474609	66.996532
1327.491147	40.622308	67.001537
1326.639396	41.413900	67.006542
1326.423117	45.766299	67.011546
1326.067389	38.344766	67.016551
1325.537103	42.439568	67.021556
1325.559706	48.726839	67.026561
1324.617656	50.523158	67.031566
1323.918587	46.176202	67.036570
1322.761272	42.679575	67.041575
1322.031005	46.364609	67.046580
1321.657893	38.507430	67.051585
1320.918387	47.476946	67.056590
1319.634691	47.965039	67.061594
1319.576896	45.850118	67.066599
1318.842686	50.548227	67.071604
1318.147938	42.813149	67.076609
1317.073164	48.278217	67.081614
1316.083527	50.611983	67.086618
1315.752506	40.685370	67.091623
1315.016992	43.029196	67.096628
1314.979030	43.886957	67.101633
1314.613375	44.074543	67.106638
1313.965896	49.482715	67.111642
1312.840298	39.171482	67.116647
1312.420778	43.726513	67.121652
1311.646028	35.143109	67.126657
1310.418455	39.191076	67.131662
1309.771049	46.387575	67.136666
1309.317451	42.157722	67.141671
1308.839814	48.187045	67.146676
1308.789232	37.641812	67.151681
1307.919690	47.491481	67.156686
1306.691760	40.915132	67.161690
1306.370104	47.982565	67.166695
1305.349570	48.026684	67.171700
1304.497281	39.242712	67.176705
1303.761370	39.784072	67.181710
1303.180284	42.478678	67.186714
1303.046112	40.222931	67.191719
1302.268727	51.284871	67.196724
1302.266070	41.640380	67.201729
1301.101751	42.169429	67.206734
1300.503743	49.962075	67.211738
1299.950477	37.933943	67.216743
1298.556569	44.974735	67.221748
1297.950554	43.735491	67.226753
1297.263584	45.551187	67.231758
1296.967543	42.494819	67.236762
1296.841380	34.965828	67.241767
1295.913230	39.038736	67.246772
1295.240625	34.055202	67.251777
1294.636905	39.948445	67.256782
1293.234723	30.949129	67.261786
1292.598893	38.787210	67.266791
1291.823864	38.891651	67.271796
1291.415461	35.416317	67.276801
1291.135668	41.398412	67.281806
1290.726240	38.856835	67.286810
1289.943518	43.157368	67.291815
1288.756722	45.505145	67.296820
1288.633957	40.935676	67.301825
1288.069461	36.027997	67.306830
1287.069635	44.761355	67.311834
1286.362443	40.546598	67.316839
1285.583439	42.985659	67.321844
1285.313161	39.551444	67.326849
1284.096355	48.185259	67.331854
1283.322937	47.786378	67.336858
1282.972441	36.963971	67.341863
1282.486725	44.155265	67.346868
1281.869260	37.943931	67.351873
1281.223712	46.256668	67.356878
1280.285386	34.756570	67.361882
1279.871897	26.582539	67.366887
1279.276045	48.681545	67.371892
1278.768036	37.349575	67.376897
1277.999522	41.398683	67.381902
1277.376468	39.947679	67.386906
1276.950244	36.754314	67.391911
1275.603214	39.753650	67.396916
1274.804272	40.104759	67.401921
1274.406240	40.299077	67.406926
1273.933083	34.735033	67.411930
1273.259642	34.290294	67.416935
1272.084804	39.283988	67.421940
1271.927955	41.535812	67.426945
1271.113448	42.455547	67.431950
1270.652915	42.694498	67.436954
1270.467710	34.971463	67.441959
1269.095844	35.210240	67.446964
1268.544285	34.487491	67.451969
1268.163743	31.253748	67.456974
1267.122984	34.953470	67.461978
1266.197519	36.496424	67.466983
1265.772713	51.758677	67.471988
1265.431172	38.645018	67.476993
1264.907162	47.272760	67.481998
1263.450233	45.687840	67.487002
1263.075329	35.178416	67.492007
1262.407648	41.031372	67.497012
1262.542088	36.042524	67.502017
1261.668458	43.792264	67.507022
1260.291015	45.135845	67.512026
1260.126398	38.002495	67.517031
1259.118724	47.090362	67.522036
1259.163724	42.467409	67.527041
1257.786720	38.201470	67.532046
1257.197110	38.525606	67.537050
1256.650069	43.482559	67.542055
1256.318524	45.150280	67.547060
1254.847641	37.440871	67.552065
1254.218816	38.660681	67.557070
1253.894484	43.109115	67.562074
1253.811188	40.438411	67.567079
1253.172105	42.262273	67.572084
1252.237850	36.087131	67.577089
1251.180558	43.216348	67.582094
1250.593406	44.216635	67.587098
1250.585273	44.120288	67.592103
1249.109157	50.656916	67.597108
1248.416970	38.316565	67.602113
1247.819955	42.445647	67.607118
1247.275418	41.794329	67.612122
1247.160759	41.814273	67.617127
1246.079036	37.446190	67.622132
1245.138268	41.210449	67.627137
1245.003260	40.927688	67.632142
1244.175882	36.050786	67.637146
1243.792926	41.555681	67.642151
1242.447576	51.826398	67.647156
1242.254244	45.888263	67.652161
1241.809145	46.547405	67.657166
1241.038539	42.860008	67.662170
1240.354716	41.568493	67.667175
1239.567974	37.434214	67.672180
1238.808183	40.417458	67.677185
1237.642006	36.455486	67.682190
1236.689381	42.702281	67.687194
1236.658206	40.157336	67.692199
1235.887047	46.690679	67.697204
1235.734005	32.649736	67.702209
1235.452813	39.046810	67.707214
1234.522453	41.470529	67.712218
1234.133558	40.445943	67.717223
1233.183514	50.912430	67.722228
1232.169294	40.939935	67.727233
1231.317894	39.574144	67.732238
1230.576381	44.196159	67.737242
1230.620678	45.606988	67.742247
1229.551258	38.355745	67.747252
1228.347526	29.145133	67.752257
1228.014159	39.278570	67.757262
1227.456982	54.781082	67.762266
1227.343486	35.006119	67.767271
1226.549856	45.152828	67.772276
1225.709068	37.098798	67.777281
1225.095838	35.431772	67.782286
1224.599287	38.789489	67.787290
1223.770509	36.838183	67.792295
1222.545722	46.529891	67.797300
1222.114373	33.919407	67.802305
1221.541553	36.423471	67.807310
1221.279422	36.397480	67.812314
1220.511893	39.424539	67.817319
1219.237735	38.042401	67.822324
1218.847420	37.987908	67.827329
1218.480976	32.274439	67.832334
1217.893201	39.404694	67.837338
1217.445480	30.455498	67.842343
1216.330084	40.716457	67.847348
1216.035186	35.564066	67.852353
1215.067666	33.469241	67.857358
1213.852817	40.667683	67.862362
1213.401566	37.706978	67.867367
1212.856412	38.191217	67.872372
1212.841735	34.317380	67.877377
1212.354846	34.931131	67.882382
1211.139026	39.276905	67.887386
1210.488720	34.737724	67.892391
1210.033944	47.096721	67.897396
1209.199640	40.572949	67.902401
1208.056157	39.326160	67.907406
1207.415053	47.013703	67.912410
1207.269790	28.705701	67.917415
1206.409770	42.494838	67.922420
1205.835220	34.642914	67.927425
1204.974655	33.083040	67.932430
1204.167669	32.528666	67.937434
1204.202408	32.222066	67.942439
1203.418733	34.950486	67.947444
1202.482085	29.788193	67.952449
1201.695724	38.468699	67.957454
1201.132691	38.719232	67.962458
1200.886548	32.579764	67.967463
1199.589856	41.328818	67.972468
1198.979013	38.707323	67.977473
1198.421033	36.298204	67.982478
1198.005159	37.706519	67.987482
1197.758763	40.051438	67.992487
1196.651844	38.324157	67.997492
1195.960655	36.693191	68.002497
1195.311076	33.024413	68.007502
1194.449534	35.533398	68.012506
1193.669327	33.090235	68.017511
1192.707485	39.429975	68.022516
1192.635674	27.506676	68.027521
1192.117796	44.676141	68.032526
1191.305564	37.240506	68.037530
1190.619265	36.331038	68.042535
1189.488722	37.493457	68.047540
1189.291706	30.401546	68.052545
1188.753398	37.460857	68.057550
1188.247545	43.901550	68.062554
1187.886761	29.734381	68.067559
1186.819098	35.871746	68.072564
1185.978477	30.413478	68.077569
1185.052325	34.421445	68.082574
1184.263998	36.267482	68.087578
1183.934957	33.153301	68.092583
1183.550407	43.184491	68.097588
1183.259340	37.933720	68.102593
1182.419491	29.471117	68.107598
1181.397988	35.446594	68.112602
1181.155183	36.750112	68.117607
1179.623062	38.359619	68.122612
1178.749784	40.121395	68.127617
1178.183818	31.260403	68.132622
1177.711284	38.313986	68.137626
1177.477882	35.339142	68.142631
1177.044162	39.604697	68.147636
1176.301732	39.820688	68.152641
1175.757029	42.951097	68.157646
1174.962742	35.231906	68.162650
1174.227622	34.347555	68.167655
1173.352249	38.711741	68.172660
1172.444852	38.078726	68.177665
1171.976126	34.411153	68.182670
1171.474297	40.447491	68.187674
1171.437164	35.750871	68.192679
1169.926737	39.501674	68.197684
1169.512358	37.527057	68.202689
1169.169795	31.302001	68.207694
1167.954972	44.034205	68.212698
1167.440270	35.363764	68.217703
1166.901236	38.046977	68.222708
1166.438265	33.779224	68.227713
1165.749436	37.508168	68.232718
1164.391595	41.681001	68.237722
1164.002358	36.488428	68.242727
1163.450084	41.826288	68.247732
1163.142377	35.089466	68.252737
1162.691398	40.054809	68.257742
1161.554644	49.097002	68.262746
1161.253572	41.026542	68.267751
1160.065061	40.755224	68.272756
1159.218354	36.048593	68.277761
1158.584828	33.829702	68.282766
1157.856318	39.239750	68.287770
1157.598695	30.695590	68.292775
1156.902459	43.223883	68.297780
1156.763315	35.022012	68.302785
1155.941679	40.278132	68.307790
1155.220091	40.199066	68.312794
1154.320583	27.166312	68.317799
1153.086934	41.855434	68.322804
1152.398846	37.092035	68.327809
1151.914685	29.531695	68.332814
1151.361847	36.416696	68.337818
1151.217263	31.488001	68.342823
1150.544810	42.877061	68.347828
1150.310322	36.637970	68.352833
1149.091216	38.678698	68.357838
1148.553770	36.572266	68.362842
1147.980450	35.928702	68.367847
1146.749965	38.438037	68.372852
1146.193075	41.535695	68.377857
1145.647536	33.040486	68.382862
1144.888537	33.718032	68.387866
1144.666391	26.841447	68.392871
1143.252658	36.355065	68.397876
1142.818398	26.039632	68.402881
1142.534527	33.039552	68.407886
1142.040280	36.455265	68.412890
1141.323942	34.752620	68.417895
1140.329213	34.210782	68.422900
1139.968517	28.811819	68.427905
1139.658605	33.584407	68.432910
1138.299548	36.245088	68.437914
1137.980620	34.772556	68.442919
1137.210674	35.298875	68.447924
1136.510869	31.606563	68.452929
1135.687357	29.925698	68.457934
1134.730578	37.278670	68.462938
1134.357004	25.901717	68.467943
1134.147296	35.048774	68.472948
1133.418673	31.487208	68.477953
1132.260723	28.198946	68.482958
1131.540725	37.094423	68.487962
1131.605215	30.885055	68.492967
1130.637277	35.899513	68.497972
1129.569429	33.014827	68.502977
1129.108304	32.981074	68.507982
1128.131002	36.653406	68.512986
1128.249458	28.940445	68.517991
1127.285746	36.917442	68.522996
1126.566739	31.906649	68.528001
1126.008051	29.759445	68.533006
1125.330457	41.029473	68.538010
1125.090893	31.969915	68.543015
1123.664833	39.301341	68.548020
1123.305273	32.867677	68.553025
1122.744141	25.734346	68.558030
1121.388353	40.487061	68.563034
1120.728665	38.969383	68.568039
1120.051449	39.127706	68.573044
1119.766998	37.119814	68.578049
1119.358583	33.797488	68.583054
1118.791391	36.491496	68.588058
1118.760404	31.216716	68.593063
1117.636250	26.677243	68.598068
1116.955936	32.795595	68.603073
1115.924054	29.701761	68.608078
1114.758323	37.799210	68.613082
1114.390009	29.111812	68.618087
1113.637199	39.332473	68.623092
1113.651508	26.398815	68.628097
1113.337326	37.727732	68.633102
1111.955177	40.297480	68.638106
1111.573098	26.346621	68.643111
1110.891350	35.926749	68.648116
1109.894151	40.075358	68.653121
1109.131932	29.747444	68.658126
1108.691092	34.540861	68.663130
1108.468338	29.917931	68.668135
1107.525347	45.275222	68.673140
1106.566788	30.728485	68.678145
1106.051853	43.284717	68.683150
1105.650588	38.521440	68.688154
1105.073695	28.624536	68.693159
1103.554221	37.202478	68.698164
1103.261918	40.299057	68.703169
1102.784907	35.227697	68.708174
1101.967799	40.938868	68.713178
1101.789571	34.809112	68.718183
1100.830962	33.461999	68.723188
1100.080761	35.483352	68.728193
1099.704381	36.585766	68.733198
1098.588117	36.498534	68.738202
1097.943604	37.654642	68.743207
1097.108393	35.379539	68.748212
1096.673929	38.033514	68.753217
1096.517076	33.742312	68.758222
1095.718457	41.354000	68.763226
1094.858871	29.997597	68.768231
1094.210909	35.784367	68.773236
1093.562267	27.053256	68.778241
1093.145008	25.427633	68.783246
1092.367499	37.163005	68.788250
1091.778768	29.734438	68.793255
1091.341653	36.429144	68.798260
1090.342461	40.073432	68.803265
1089.482084	37.430160	68.808270
1088.797763	39.873139	68.813274
1088.496476	37.965704	68.818279
1087.211624	40.904778	68.823284
1086.323348	38.264368	68.828289
1086.139270	38.541377	68.833294
1085.246387	41.025420	68.838298
1085.384314	24.285691	68.843303
1084.468375	33.097223	68.848308
1083.536789	35.147436	68.853313
1082.969802	25.308893	68.858318
1082.442668	41.547814	68.863322
1082.159011	32.233495	68.868327
1080.576757	31.810380	68.873332
1080.021616	32.031298	68.878337
1079.833226	34.499465	68.883342
1079.216589	42.064860	68.888346
1078.008290	28.038860	68.893351
1077.233727	32.325532	68.898356
1076.734332	30.203602	68.903361
1076.418601	29.074359	68.908366
1075.797341	34.959390	68.913370
1075.413137	33.087227	68.918375
1074.392812	30.981937	68.923380
1073.584281	35.762888	68.928385
1073.344079	33.404175	68.933390
1072.242985	41.745258	68.938394
1071.606480	23.488640	68.943399
1070.613758	39.309600	68.948404
1070.478032	32.283653	68.953409
1070.212301	29.430666	68.958414
1069.003932	38.640402	68.963418
1068.638321	37.856576	68.968423
1067.991712	44.262905	68.973428
1067.332275	38.391065	68.978433
1066.373149	33.828515	68.983438
1065.489273	34.671037	68.988442
1065.136426	31.976995	68.993447
1064.543825	41.781080	68.998452
1063.836001	31.507611	69.003457
1063.100075	28.989636	69.008462
1062.327468	36.655540	69.013466
1061.983535	28.550925	69.018471
1061.506668	34.047119	69.023476
1060.711065	30.546698	69.028481
1059.874999	31.767983	69.033486
1059.514781	34.665626	69.038490
1058.497545	34.272487	69.043495
1057.463031	40.169651	69.048500
1056.779547	40.956639	69.053505
1056.646546	38.530408	69.058510
1056.182877	31.518788	69.063514
1055.529810	36.601453	69.068519
1054.410007	39.917999	69.073524
1053.971892	33.376995	69.078529
1053.324792	30.677728	69.083534
1052.246723	35.462141	69.088538
1051.527016	33.337420	69.093543
1050.813901	33.045715	69.098548
1050.724304	32.646927	69.103553
1050.539646	35.117656	69.108558
1049.361702	35.172729	69.113562
1048.740668	25.349103	69.118567
1048.151189	22.441968	69.123572
1047.353290	28.131169	69.128577
1046.424564	29.950695	69.133582
1045.603990	35.187749	69.138586
1045.421122	32.468244	69.143591
1044.949694	33.538477	69.148596
1044.412595	33.374895	69.153601
1043.462111	33.988315	69.158606
1042.517925	36.262906	69.163610
1042.323788	30.725495	69.168615
1041.118636	39.152531	69.173620
1040.068011	34.208720	69.178625
1039.608626	30.117052	69.183630
1039.145566	30.353292	69.188634
1038.691036	31.968061	69.193639
1038.670417	37.751229	69.198644
1037.382210	36.513352	69.203649
1036.575782	34.697333	69.208654
1035.921149	41.046594	69.213658
1035.835021	29.188677	69.218663
1034.725553	39.467676	69.223668
1034.055331	39.604408	69.228673
1033.415037	38.545733	69.233678
1032.794623	42.814202	69.238682
1032.425676	30.439865	69.243687
1031.056487	35.093979	69.248692
1030.565420	34.904153	69.253697
1030.426622	35.080918	69.258702
1029.474882	38.362849	69.263706
1028.881276	30.640177	69.268711
1027.923263	40.955007	69.273716
1027.451807	35.937977	69.278721
1026.915771	26.804183	69.283726
1026.148389	31.826190	69.288730
1025.462963	33.299495	69.293735
1024.689714	31.057140	69.298740
1024.384609	36.388811	69.303745
1023.611338	24.239668	69.308750
1022.537666	34.519280	69.313754
1022.160294	28.113706	69.318759
1021.760989	32.559891	69.323764
1021.076792	35.310382	69.328769
1019.918262	34.302627	69.333774
1018.783099	32.721853	69.338778
1018.915632	24.063605	69.343783
1018.535619	37.839479	69.348788
1018.223450	33.377449	69.353793
1016.972217	30.490453	69.358798
1016.012128	40.964895	69.363802
1015.908349	31.002205	69.368807
1015.239131	32.241114	69.373812
1013.953559	34.795545	69.378817
1013.268202	30.036490	69.383822
1012.847626	35.041169	69.388826
1012.624258	29.095236	69.393831
1011.495123	38.984695	69.398836
1010.514736	37.374566	69.403841
1010.175167	32.178855	69.408846
1009.358230	39.063320	69.413850
1009.369279	33.550037	69.418855
1008.368407	33.780388	69.423860
1007.524321	36.433317	69.428865
1007.036569	31.346344	69.433870
1006.555476	37.929780	69.438874
1005.875865	32.602088	69.443879
1004.965275	37.195863	69.448884
1004.404110	37.671655	69.453889
1003.902834	30.088846	69.458894
1003.295668	34.374134	69.463898
1002.532751	17.284157	69.468903
1001.702086	29.493215	69.473908
1001.151751	30.986034	69.478913
1000.736006	36.185495	69.483918
999.746726	31.999948	69.488922
999.616957	19.164934	69.493927
997.928753	30.863868	69.498932
996.895073	28.710272	69.503937
997.020274	33.620224	69.508942
996.353032	32.621043	69.513946
995.968922	28.451173	69.518951
995.615783	35.168797	69.523956
994.900495	27.408726	69.528961
993.741069	31.816585	69.533966
992.993908	36.310238	69.538970
992.584626	25.538272	69.543975
991.397142	40.163327	69.548980
990.952844	37.075401	69.553985
990.335845	27.749489	69.558990
989.785927	26.189150	69.563994
989.576578	22.679052	69.568999
988.714002	27.411851	69.574004
987.311743	32.467078	69.579009
986.891636	33.770438	69.584014
986.769610	37.814524	69.589018
986.443533	19.724604	69.594023
985.018515	38.785739	69.599028
984.421690	36.226730	69.604033
983.925982	32.749581	69.609038
983.375654	41.794715	69.614042
982.432644	37.925099	69.619047
981.670734	36.266024	69.624052
981.213036	39.232807	69.629057
980.834122	22.903354	69.634062
980.136634	19.366850	69.639066
979.301282	25.203957	69.644071
978.332573	30.480369	69.649076
978.193716	30.202967	69.654081
977.620982	26.615071	69.659086
976.349560	26.276606	69.664090
975.780529	31.383761	69.669095
975.242721	34.560418	69.674100
974.998063	25.536399	69.679105
973.837943	25.648596	69.684110
972.959965	24.651416	69.689114
972.843456	30.300020	69.694119
971.882679	32.947872	69.699124
971.729052	26.468858	69.704129
970.586403	31.227307	69.709134
969.737440	39.127742	69.714138
969.390007	32.947657	69.719143
968.865383	32.965040	69.724148
967.952275	38.008675	69.729153
967.267129	32.028993	69.734158
966.245618	38.504459	69.739162
966.281267	33.004611	69.744167
965.625267	34.460634	69.749172
964.912602	29.797407	69.754177
964.166647	25.238831	69.759182
963.717357	30.467287	69.764186
962.877015	30.962281	69.769191
961.765325	35.531297	69.774196
960.952799	21.863461	69.779201
961.008195	23.110080	69.784206
960.435865	37.037987	69.789210
959.623079	25.641086	69.794215
958.421965	42.070845	69.799220
957.978416	45.464328	69.804225
957.945342	29.740609	69.809230
956.674877	38.165454	69.814234
956.007802	29.125076	69.819239
955.167035	32.196977	69.824244
955.035784	28.510445	69.829249
954.766246	26.165878	69.834254
953.053930	32.954710	69.839258
952.892755	23.652474	69.844263
952.584395	30.421322	69.849268
951.841058	29.453187	69.854273
950.810424	33.141952	69.859278
950.057117	34.865785	69.864282
949.632603	24.373810	69.869287
948.800083	32.407253	69.874292
948.188901	32.572460	69.879297
947.401768	26.534898	69.884302
946.525229	23.608814	69.889306
946.724728	20.271788	69.894311
945.338924	38.312678	69.899316
944.149228	32.033238	69.904321
943.571830	31.374601	69.909326
943.341954	31.729874	69.914330
942.801173	30.276905	69.919335
942.538083	28.141056	69.924340
942.250089	32.049121	69.929345
941.367763	27.997973	69.934350
940.322331	36.204080	69.939354
940.139469	31.201072	69.944359
939.101105	24.984290	69.949364
937.880640	29.365613	69.954369
937.631627	29.526805	69.959374
936.880053	34.325538	69.964378
936.640280	22.974659	69.969383
935.312594	33.263181	69.974388
934.513330	31.425557	69.979393
934.624548	21.395553	69.984398
933.710064	38.803180	69.989402
933.270706	27.887776	69.994407
932.199856	34.930942	69.999412
931.475849	32.799056	70.004417
931.250942	35.597907	70.009422
930.344509	32.761743	70.014426
929.567236	27.471699	70.019431
928.985694	40.637804	70.024436
928.365621	25.824404	70.029441
928.125668	29.059326	70.034446
927.311671	40.907773	70.039450
926.495921	33.051745	70.044455
926.031418	32.312066	70.049460
925.261687	33.026078	70.054465
924.078720	32.965310	70.059470
922.890129	27.770690	70.064474
922.620297	32.180510	70.069479
922.131129	29.687967	70.074484
922.056392	36.101082	70.079489
921.911350	30.991129	70.084494
920.357248	37.243853	70.089498
920.092528	23.351652	70.094503
919.402950	37.492194	70.099508
918.405174	37.110208	70.104513
917.810846	32.442356	70.109518
917.121378	31.520854	70.114522
916.944329	31.424581	70.119527
916.024780	33.070799	70.124532
914.878533	30.919382	70.129537
914.671987	30.788380	70.134542
914.079238	36.798217	70.139546
913.292174	27.221845	70.144551
912.462391	30.812423	70.149556
911.715794	28.893882	70.154561
911.206644	28.779499	70.159566
910.870644	35.940695	70.164570
909.791592	31.443034	70.169575
909.074737	30.453350	70.174580
908.505860	30.771112	70.179585
908.132342	32.041837	70.184590
907.438304	36.875577	70.189594
906.751760	31.601062	70.194599
905.992814	34.152159	70.199604
905.671160	41.337884	70.204609
904.694917	34.570312	70.209614
903.346591	46.770325	70.214618
903.469321	29.203525	70.219623
903.166420	41.530473	70.224628
901.949966	29.125473	70.229633
901.566562	31.115312	70.234638
900.760340	41.353977	70.239642
900.002938	32.296453	70.244647
899.057157	31.614453	70.249652
898.329288	33.731659	70.254657
897.949235	25.688026	70.259662
897.380563	38.807928	70.264666
896.974053	32.963702	70.269671
895.694544	36.047101	70.274676
895.237766	34.938755	70.279681
894.680169	38.747803	70.284686
894.144905	33.570645	70.289690
893.820438	25.803605	70.294695
892.588321	29.180670	70.299700
892.025406	34.851437	70.304705
891.366197	30.515630	70.309710
890.790572	38.060332	70.314714
890.303236	30.476914	70.319719
889.145915	34.865557	70.324724
888.653603	26.134870	70.329729
888.524355	28.827030	70.334734
887.602519	36.083046	70.339738
886.689865	27.573808	70.344743
885.948886	37.849400	70.349748
885.405927	38.792270	70.354753
885.177115	23.394626	70.359758
883.805595	31.267858	70.364762
883.465669	22.736857	70.369767
883.011022	32.746091	70.374772
882.176876	30.797338	70.379777
881.367064	32.979631	70.384782
880.495464	36.862315	70.389786
880.007351	31.132011	70.394791
879.556268	28.305398	70.399796
878.880060	31.180812	70.404801
878.682429	25.699177	70.409806
877.320520	37.738922	70.414810
877.235305	37.703733	70.419815
876.753287	35.799863	70.424820
875.125472	38.973404	70.429825
874.894311	34.615204	70.434830
874.150811	37.004573	70.439834
874.097299	30.549060	70.444839
872.739146	38.208855	70.449844
871.866626	34.872135	70.454849
871.842335	28.240079	70.459854
871.221063	29.917686	70.464858
870.359935	29.829371	70.469863
869.141579	31.922148	70.474868
868.998624	30.566730	70.479873
868.580209	29.223617	70.484878
867.303025	34.766794	70.489882
866.564878	34.696754	70.494887
866.142422	32.034327	70.499892
865.796190	34.986538	70.504897
865.341827	33.472521	70.509902
864.466678	34.810480	70.514906
863.406010	22.252976	70.519911
862.792439	34.676678	70.524916
862.478341	27.458370	70.529921
862.466481	30.562370	70.534926
861.234470	36.680277	70.539930
860.810354	27.863046	70.544935
859.756818	30.626631	70.549940
858.620347	32.372053	70.554945
858.315168	25.937679	70.559950
857.383066	29.798458	70.564954
857.110219	25.924731	70.569959
856.816862	28.906374	70.574964
855.726607	24.628152	70.579969
855.049714	28.096636	70.584974
854.335405	36.716859	70.589978
853.984315	23.477112	70.594983
852.950140	33.621175	70.599988
852.135746	21.888678	70.604993
851.594979	19.708728	70.609998
850.741991	33.551999	70.615002
850.857885	28.141891	70.620007
849.895809	40.234705	70.625012
848.895786	33.453598	70.630017
848.325298	26.646702	70.635022
847.754003	27.896875	70.640026
847.548007	23.979392	70.645031
846.216942	37.556555	70.650036
845.738360	38.061816	70.655041
845.664437	22.188504	70.660046
844.656872	33.090028	70.665050
843.665601	24.281077	70.670055
842.836356	25.198560	70.675060
842.389872	30.488088	70.680065
842.038528	28.856749	70.685070
841.483622	25.184047	70.690074
840.780958	27.442340	70.695079
839.695445	27.345597	70.700084
839.131498	32.418849	70.705089
838.842967	37.459301	70.710094
837.811632	30.430864	70.715098
837.463164	25.700246	70.720103
836.824102	30.969965	70.725108
836.080003	23.395898	70.730113
835.269516	28.867951	70.735118
834.039078	29.240574	70.740122
834.056381	22.311733	70.745127
833.470603	23.240927	70.750132
832.927170	23.969409	70.755137
832.218425	31.159978	70.760142
831.144806	26.182081	70.765146
830.821917	21.217151	70.770151
829.812299	26.697249	70.775156
828.829536	20.061649	70.780161
828.447910	27.110256	70.785166
827.805560	39.286225	70.790170
827.418063	29.157409	70.795175
827.014057	27.903476	70.800180
826.254355	30.391633	70.805185
825.718171	28.870148	70.810190
824.727889	37.395532	70.815194
823.523533	33.157564	70.820199
823.130444	27.796939	70.825204
822.344133	27.173165	70.830209
822.072780	19.899178	70.835214
821.285342	29.685414	70.840218
821.266892	29.740527	70.845223
820.293213	32.403103	70.850228
819.247199	27.955422	70.855233
819.131501	34.427095	70.860238
818.107875	30.838474	70.865242
817.390940	27.581092	70.870247
816.748803	25.231200	70.875252
816.119084	28.903502	70.880257
815.852447	29.401838	70.885262
814.786631	39.487872	70.890266
814.289802	36.141833	70.895271
813.842993	40.819539	70.900276
812.444939	36.565100	70.905281
812.011256	31.917439	70.910286
811.039954	38.525317	70.915290
810.881723	26.262588	70.920295
810.523858	37.115894	70.925300
809.629658	33.695914	70.930305
808.964966	31.430040	70.935310
808.230677	30.328040	70.940314
807.771610	19.464705	70.945319
806.595801	38.000512	70.950324
805.745680	36.117408	70.955329
805.407241	29.972198	70.960334
804.756841	38.363053	70.965338
804.850716	28.392587	70.970343
803.418691	33.534650	70.975348
802.691422	33.633214	70.980353
802.247811	26.072826	70.985358
801.650077	29.801543	70.990362
801.453757	23.744103	70.995367
800.225740	42.005943	71.000372
799.509285	25.124711	71.005377
798.852208	21.947697	71.010382
798.334120	30.413683	71.015386
797.783789	20.074253	71.020391
796.862504	32.367167	71.025396
796.504576	32.195617	71.030401
795.917771	23.126752	71.035406
794.753233	28.459632	71.040410
794.100025	27.524507	71.045415
793.217753	32.262076	71.050420
792.928379	25.066658	71.055425
792.974236	27.010251	71.060430
791.827797	31.647944	71.065434
791.193902	26.300432	71.070439
790.546404	26.048820	71.075444
789.201044	21.139438	71.080449
788.795750	22.624979	71.085454
787.980469	33.913815	71.090458
787.621071	21.727276	71.095463
787.384908	28.274895	71.100468
786.705574	28.493571	71.105473
785.675404	28.354924	71.110478
784.990029	28.429477	71.115482
784.691966	31.944905	71.120487
783.868811	32.233788	71.125492
782.865991	28.550405	71.130497
782.518822	30.130776	71.135502
781.718095	30.595868	71.140506
781.479610	26.399704	71.145511
780.439435	24.100575	71.150516
779.359364	23.919411	71.155521
779.171305	25.255247	71.160526
778.781788	33.912087	71.165530
777.831660	18.719203	71.170535
777.173465	27.943958	71.175540
776.075495	26.991334	71.180545
776.004504	22.255978	71.185550
775.099664	26.604470	71.190554
774.505226	24.895146	71.195559
773.922556	31.425390	71.200564
773.623528	29.610685	71.205569
772.816817	19.980732	71.210574
771.900130	26.174631	71.215578
771.328879	24.108367	71.220583
770.531440	19.067607	71.225588
769.587449	25.073459	71.230593
768.801423	28.821121	71.235598
768.417124	30.237089	71.240602
768.126401	23.925015	71.245607
767.733316	34.312401	71.250612
766.921669	26.006342	71.255617
765.653529	24.839534	71.260622
765.025515	28.760743	71.265626
764.895413	20.507034	71.270631
763.718151	25.031369	71.275636
762.769032	27.704248	71.280641
762.550112	26.807226	71.285646
761.940945	32.600497	71.290650
761.797624	33.829861	71.295655
760.663104	33.209504	71.300660
759.894400	32.508827	71.305665
759.524389	22.862968	71.310670
758.683177	29.018047	71.315674
758.094153	32.243898	71.320679
757.108667	26.780479	71.325684
756.533909	35.704943	71.330689
756.376721	22.581015	71.335694
755.050813	29.656964	71.340698
754.399354	22.011407	71.345703
753.537008	34.171943	71.350708
753.155546	38.178486	71.355713
753.072251	32.867903	71.360718
752.321915	36.668238	71.365722
751.569735	28.376371	71.370727
750.758567	33.140481	71.375732
749.925173	35.596237	71.380737
749.805255	23.105065	71.385742
748.758045	38.029568	71.390746
748.469901	24.149026	71.395751
747.724031	29.908870	71.400756
746.614451	29.525830	71.405761
746.001372	28.320969	71.410766
745.036309	36.720931	71.415770
744.560560	32.218760	71.420775
744.267626	41.743353	71.425780
743.602136	34.956343	71.430785
742.940077	34.145647	71.435790
742.136293	32.141645	71.440794
741.793024	21.762956	71.445799
740.819970	33.005955	71.450804
739.804737	27.504701	71.455809
739.399436	29.838681	71.460814
738.849446	26.786564	71.465818
738.330232	21.781944	71.470823
737.414595	31.071352	71.475828
736.551615	29.458413	71.480833
736.019868	31.667442	71.485838
735.280245	28.681790	71.490842
735.386173	20.239112	71.495847
734.448074	30.085626	71.500852
733.156357	30.346625	71.505857
733.069639	27.138742	71.510862
732.467126	24.285807	71.515866
731.635447	27.413100	71.520871
730.745529	28.822843	71.525876
730.158912	29.200242	71.530881
729.688417	25.501513	71.535886
728.955852	29.246982	71.540890
728.250795	23.581226	71.545895
727.701113	33.779075	71.550900
727.086148	30.595374	71.555905
726.345335	29.486553	71.560910
725.376236	32.418102	71.565914
724.531840	31.300542	71.570919
724.535717	30.429552	71.575924
723.881839	36.594240	71.580929
723.434494	31.354242	71.585934
722.420371	36.152254	71.590938
722.120223	23.795443	71.595943
720.936017	33.804156	71.600948
720.267023	38.081998	71.605953
719.826413	28.858985	71.610958
719.073957	34.282407	71.615962
718.148336	30.351785	71.620967
717.447102	34.488098	71.625972
716.677421	33.148902	71.630977
716.541862	27.029757	71.635982
715.911097	31.112270	71.640986
715.164396	26.605940	71.645991
714.123557	31.029725	71.650996
713.623365	35.187646	71.656001
713.399638	24.939743	71.661006
712.535479	34.025414	71.666010
711.525402	32.193046	71.671015
711.111784	27.401861	71.676020
710.606371	24.598128	71.681025
710.253512	18.324348	71.686030
708.690329	31.974789	71.691034
708.103073	22.295725	71.696039
707.618920	30.720047	71.701044
707.168701	36.119001	71.706049
707.127044	29.797239	71.711054
705.843077	34.209278	71.716058
705.409205	35.319324	71.721063
704.784067	37.153709	71.726068
703.370175	32.506031	71.731073
702.788466	23.762826	71.736078
702.321675	28.861632	71.741082
701.738822	26.199547	71.746087
701.382705	21.795038	71.751092
700.666945	23.875673	71.756097
699.951172	17.916735	71.761102
699.003886	29.016863	71.766106
698.717921	28.125791	71.771111
698.381969	18.613304	71.776116
697.016192	29.245467	71.781121
696.575538	23.923985	71.786126
695.934655	23.624036	71.791130
695.400636	20.826440	71.796135
694.054333	19.364599	71.801140
693.463149	23.175875	71.806145
693.297597	20.359030	71.811150
692.543997	25.872526	71.816154
692.545999	20.398555	71.821159
691.651381	20.004966	71.826164
690.907122	29.366447	71.831169
690.359393	27.521968	71.836174
689.065254	25.870468	71.841178
688.393743	23.028533	71.846183
687.969602	26.844750	71.851188
687.325425	26.633640	71.856193
686.946571	20.761408	71.861198
685.626066	25.614525	71.866202
685.195593	21.049966	71.871207
684.863863	29.998816	71.876212
684.254043	29.233437	71.881217
683.159864	21.169532	71.886222
682.124420	31.427391	71.891226
682.042837	22.349078	71.896231
681.571539	25.698127	71.901236
681.035158	28.425161	71.906241
679.965337	16.365980	71.911246
679.219241	34.806579	71.916250
678.808272	21.808240	71.921255
678.311230	26.967060	71.926260
677.078584	29.066933	71.931265
676.573881	25.376817	71.936270
676.017225	31.562302	71.941274
675.755694	26.592358	71.946279
674.871217	36.427200	71.951284
674.022203	32.850262	71.956289
673.514278	24.754506	71.961294
672.563791	39.737746	71.966298
672.430886	29.666203	71.971303
671.606147	17.239981	71.976308
670.424552	28.904148	71.981313
670.441542	23.047733	71.986318
669.543732	35.770618	71.991322
668.773083	27.618925	71.996327
667.930488	23.675105	72.001332
667.226666	31.495726	72.006337
667.147971	21.776691	72.011342
666.413105	22.685508	72.016346
665.551392	23.545138	72.021351
664.731085	26.792069	72.026356
664.116721	31.184227	72.031361
663.805294	26.812032	72.036366
662.607193	39.401388	72.041370
661.900214	27.238692	72.046375
661.270651	30.494674	72.051380
660.488386	31.951955	72.056385
661.108449	29.522529	72.061390
660.020391	28.587303	72.066394
658.913785	24.761226	72.071399
658.284633	31.756223	72.076404
657.418532	31.899017	72.081409
656.862491	35.408229	72.086414
656.260842	36.092401	72.091418
655.491205	33.961561	72.096423
655.571424	25.937731	72.101428
654.260130	32.169278	72.106433
653.547794	28.190525	72.111438
652.913442	44.960641	72.116442
652.564032	34.305390	72.121447
651.699320	26.197071	72.126452
650.732811	32.195510	72.131457
650.410652	23.046700	72.136462
649.691223	35.424203	72.141466
648.983319	32.826202	72.146471
648.240362	33.739468	72.151476
647.288000	33.840808	72.156481
646.943707	16.695378	72.161486
646.637458	34.919270	72.166490
645.923297	27.564440	72.171495
644.993531	31.276679	72.176500
644.265782	33.982157	72.181505
644.006333	23.468713	72.186510
643.217998	36.751354	72.191514
642.390767	29.606927	72.196519
641.570045	34.309508	72.201524
641.089418	29.680401	72.206529
640.754913	28.730833	72.211534
639.300840	27.052789	72.216538
638.928948	30.054843	72.221543
638.609688	27.716660	72.226548
637.861600	34.628098	72.231553
637.448174	22.442321	72.236558
636.464708	27.002081	72.241562
635.807765	32.235262	72.246567
635.484360	23.168658	72.251572
634.243199	33.787313	72.256577
633.719263	24.134460	72.261582
632.668286	37.402159	72.266586
632.486572	27.565487	72.271591
632.127162	20.982095	72.276596
630.896395	28.918184	72.281601
630.602154	15.360363	72.286606
629.869756	29.562946	72.291610
629.291517	24.094653	72.296615
629.149834	24.910586	72.301620
627.942580	28.260157	72.306625
627.485999	26.327058	72.311630
626.217591	33.699848	72.316634
625.478818	26.598113	72.321639
624.850979	34.312022	72.326644
624.037204	28.026505	72.331649
624.190862	24.639993	72.336654
623.489423	31.044093	72.341658
623.022367	24.547234	72.346663
622.019129	15.202547	72.351668
621.196972	19.162589	72.356673
621.167354	23.161992	72.361678
619.553803	30.329548	72.366682
619.067336	30.944920	72.371687
618.543126	26.754860	72.376692
618.021630	31.476025	72.381697
617.611629	21.011799	72.386702
616.812672	35.114599	72.391706
616.022236	20.195999	72.396711
615.683257	28.598785	72.401716
614.460445	29.661028	72.406721
613.661998	18.842344	72.411726
613.153558	29.226027	72.416730
612.944169	26.025075	72.421735
612.200030	27.160896	72.426740
610.839830	36.204169	72.431745
610.459154	21.635060	72.436750
609.846845	22.658419	72.441754
609.362482	30.057732	72.446759
609.160002	26.314766	72.451764
608.300892	26.249876	72.456769
607.692416	23.341154	72.461774
606.643275	35.364310	72.466778
606.219293	23.199147	72.471783
604.837842	22.998249	72.476788
603.900844	30.647856	72.481793
603.833106	27.323415	72.486798
603.509400	34.324968	72.491802
602.811525	26.808283	72.496807
602.686725	21.300896	72.501812
601.757201	23.846126	72.506817
601.187193	19.723294	72.511822
600.205398	33.298535	72.516826
599.115447	29.138662	72.521831
598.495607	21.194801	72.526836
597.994542	29.164495	72.531841
597.775893	28.251676	72.536846
597.295882	26.640870	72.541850
596.027764	30.892734	72.546855
595.414543	28.435793	72.551860
595.275667	25.669903	72.556865
594.525799	26.333542	72.561870
593.124338	22.537114	72.566874
592.523334	21.424991	72.571879
592.018609	21.956540	72.576884
591.495362	27.621035	72.581889
591.511750	18.326852	72.586894
590.022237	30.844365	72.591898
589.772304	29.006097	72.596903
589.163329	24.496799	72.601908
587.756916	28.904739	72.606913
587.348218	30.860800	72.611918
586.930986	31.493536	72.616922
586.604044	24.863979	72.621927
586.363563	27.307349	72.626932
585.260027	32.740989	72.631937
584.744755	30.698971	72.636942
583.742777	32.885154	72.641946
582.129025	28.621058	72.646951
581.684624	19.621052	72.651956
581.170501	30.114458	72.656961
581.328574	26.785590	72.661966
580.763935	27.050709	72.666970
580.108158	21.001829	72.671975
579.373162	22.188245	72.676980
578.429334	25.573151	72.681985
577.352789	23.054393	72.686990
576.472702	21.606670	72.691994
575.728054	23.192029	72.696999
575.679421	26.886945	72.702004
574.798482	32.944321	72.707009
574.673036	24.115866	72.712014
573.833331	30.920481	72.717018
573.184623	40.859726	72.722023
572.485135	26.724619	72.727028
571.894060	28.676614	72.732033
571.275900	28.289496	72.737038
569.762107	32.683011	72.742042
569.534227	26.614861	72.747047
569.345047	18.304358	72.752052
569.007392	24.871301	72.757057
567.985804	21.618373	72.762062
566.744986	27.053384	72.767066
566.371192	27.655549	72.772071
566.207080	29.086936	72.777076
565.102200	27.504706	72.782081
564.385815	19.205640	72.787086
563.910412	31.858106	72.792090
563.384308	22.181967	72.797095
562.300487	17.232638	72.802100
561.451044	24.032496	72.807105
561.266689	20.203069	72.812110
560.678660	30.626246	72.817114
560.056386	24.773890	72.822119
559.127197	31.584878	72.827124
558.247343	29.340737	72.832129
558.253471	19.477315	72.837134
557.201723	25.481474	72.842138
556.344476	25.562967	72.847143
555.734237	28.771737	72.852148
555.045451	37.596116	72.857153
554.891228	27.163702	72.862158
553.872373	29.843032	72.867162
553.082236	21.841155	72.872167
552.525247	25.563430	72.877172
551.770913	34.584336	72.882177
551.581298	33.788326	72.887182
550.243810	39.062123	72.892186
549.936689	30.417155	72.897191
549.500482	22.794152	72.902196
548.884959	24.139747	72.907201
548.067338	23.125221	72.912206
547.161498	30.618489	72.917210
546.541140	25.054424	72.922215
546.460464	25.267690	72.927220
545.021484	20.814928	72.932225
544.717116	20.409371	72.937230
543.668792	20.762587	72.942234
543.429807	21.053112	72.947239
543.023178	31.844799	72.952244
541.630698	25.148439	72.957249
541.141120	24.698267	72.962254
540.423460	37.728386	72.967258
540.112155	32.977710	72.972263
539.640514	27.044592	72.977268
538.619752	33.403382	72.982273
538.348614	33.476672	72.987278
537.934337	32.954578	72.992282
536.765633	37.961790	72.997287
535.706373	31.431552	73.002292
535.112954	39.032759	73.007297
535.084156	27.566354	73.012302
534.214147	33.562075	73.017306
533.450005	27.237147	73.022311
532.692304	27.886282	73.027316
532.200157	35.714213	73.032321
531.830243	29.339100	73.037326
530.571837	35.895028	73.042330
530.054233	32.121844	73.047335
529.730290	29.208817	73.052340
528.616507	26.691283	73.057345
528.288221	24.788231	73.062350
527.283199	31.587654	73.067354
526.813875	31.503277	73.072359
526.518868	26.267446	73.077364
525.126300	35.446804	73.082369
524.531362	25.592401	73.087374
524.125455	30.418171	73.092378
523.719587	25.274121	73.097383
523.109590	23.378101	73.102388
522.012095	38.389523	73.107393
521.587346	21.594425	73.112398
520.854326	32.649428	73.117402
520.533784	23.997147	73.122407
519.162453	20.293739	73.127412
518.680965	27.531748	73.132417
518.347917	17.392773	73.137422
517.346437	33.183704	73.142426
517.168361	25.506969	73.147431
516.086016	18.253426	73.152436
515.488928	27.824891	73.157441
515.074209	29.315128	73.162446
514.592350	25.365939	73.167450
513.698672	24.675788	73.172455
512.930601	20.761158	73.177460
512.350772	25.262964	73.182465
511.982998	16.966731	73.187470
510.840434	24.204396	73.192474
510.100693	18.892761	73.197479
509.506002	22.392385	73.202484
509.049491	29.003500	73.207489
508.571665	13.401202	73.212494
507.673602	16.316778	73.217498
507.059749	19.131881	73.222503
506.722439	22.308218	73.227508
505.397002	32.900922	73.232513
504.983495	21.453236	73.237518
504.288176	33.744915	73.242522
503.958054	26.658549	73.247527
503.016146	18.624101	73.252532
502.055778	21.224743	73.257537
501.670873	15.389789	73.262542
501.097812	26.433500	73.267546
500.570811	16.626637	73.272551
499.748000	23.291377	73.277556
498.732416	21.631873	73.282561
498.508808	20.421800	73.287566
497.783978	25.446620	73.292570
497.304014	20.576165	73.297575
496.124919	29.461318	73.302580
495.475556	27.934286	73.307585
495.561921	17.282205	73.312590
495.081087	28.607701	73.317594
493.754009	26.371755	73.322599
493.036631	21.383001	73.327604
492.486888	29.977071	73.332609
492.406242	23.379260	73.337614
490.760325	26.738853	73.342618
490.287076	24.739050	73.347623
489.835345	28.539188	73.352628
489.042129	27.001960	73.357633
488.305419	19.135106	73.362638
487.578501	27.404154	73.367642
487.195289	13.491529	73.372647
486.712652	25.115364	73.377652
485.962239	28.119393	73.382657
485.204693	22.738060	73.387662
484.285150	33.037440	73.392666
484.080425	28.025360	73.397671
483.756960	18.979304	73.402676
482.506689	31.834078	73.407681
481.800247	15.318856	73.412686
481.080591	17.590986	73.417690
480.954309	20.076093	73.422695
479.722465	27.345344	73.427700
478.944179	31.143894	73.432705
478.760837	26.569969	73.437710
478.263718	28.595328	73.442714
477.242212	26.859502	73.447719
476.477115	22.463425	73.452724
475.717431	27.832859	73.457729
475.522329	26.219265	73.462734
474.848424	26.725752	73.467738
473.719582	23.548303	73.472743
473.231883	26.810108	73.477748
472.444195	34.382348	73.482753
472.269421	22.414072	73.487758
471.894695	30.388884	73.492762
470.490273	18.730072	73.497767
470.081826	23.308662	73.502772
469.441345	30.185644	73.507777
468.394272	23.938939	73.512782
467.408918	30.705285	73.517786
466.969795	21.089438	73.522791
466.580018	19.070033	73.527796
466.325281	31.045505	73.532801
466.106188	26.789525	73.537806
464.849256	27.685384	73.542810
463.840312	29.360195	73.547815
463.827868	29.061105	73.552820
462.650709	33.587131	73.557825
461.888459	23.144378	73.562830
461.012034	27.174617	73.567834
460.595949	23.554017	73.572839
460.519762	15.804291	73.577844
459.293715	21.997109	73.582849
458.804107	23.895114	73.587854
458.017245	22.910412	73.592858
457.410927	23.932852	73.597863
457.045789	18.679825	73.602868
455.875006	28.495676	73.607873
455.524252	23.126811	73.612878
454.879269	25.782879	73.617882
454.354197	23.233082	73.622887
453.881647	27.175318	73.627892
452.498260	28.507660	73.632897
452.329901	29.149651	73.637902
451.809867	25.793204	73.642906
450.802922	28.300360	73.647911
449.971679	25.278937	73.652916
449.452700	24.052852	73.657921
449.135278	22.695302	73.662926
448.431952	27.727746	73.667930
447.506458	23.267347	73.672935
447.193861	22.035188	73.677940
446.294490	30.016324	73.682945
445.191144	17.046379	73.687950
444.743514	24.763140	73.692954
444.122099	22.124615	73.697959
443.408583	24.061453	73.702964
442.923592	31.432499	73.707969
442.542374	25.218486	73.712974
441.378366	19.381525	73.717978
440.983322	24.834795	73.722983
440.770819	16.848163	73.727988
439.874292	34.823883	73.732993
439.026049	22.991310	73.737998
438.137301	18.671722	73.743002
437.461443	24.892005	73.748007
436.571330	22.657430	73.753012
435.777917	23.124620	73.758017
435.388636	21.726480	73.763022
434.723608	25.798740	73.768026
434.454650	29.069853	73.773031
434.319553	28.878619	73.778036
433.492428	24.104498	73.783041
432.561940	15.599896	73.788046
432.029891	19.417569	73.793050
431.030082	21.857359	73.798055
430.498477	23.153338	73.803060
429.611367	25.723410	73.808065
429.334154	14.897451	73.813070
427.960135	17.269133	73.818074
427.067744	13.626665	73.823079
426.611642	18.173427	73.828084
426.326746	24.569541	73.833089
426.158033	18.367406	73.838094
425.556560	21.547996	73.843098
424.665243	22.492851	73.848103
424.069682	22.297718	73.853108
423.377028	30.547128	73.858113
422.533832	14.936846	73.863118
421.424926	23.683103	73.868122
420.694429	24.288510	73.873127
420.879296	20.327724	73.878132
419.927067	23.228306	73.883137
419.133748	21.840934	73.888142
418.373685	19.596682	73.893146
417.756310	21.543440	73.898151
417.417869	18.096563	73.903156
416.626933	24.264222	73.908161
415.929161	14.944295	73.913166
415.299089	15.715845	73.918170
414.441904	19.520674	73.923175
413.693461	16.422993	73.928180
412.829123	16.844721	73.933185
412.433326	9.324923	73.938190
411.921011	18.024210	73.943194
411.597657	15.883053	73.948199
410.699536	14.894019	73.953204
409.916475	20.329483	73.958209
409.765589	13.147560	73.963214
408.553057	19.356381	73.968218
407.592288	20.470010	73.973223
407.162724	20.186926	73.978228
406.698495	24.768104	73.983233
406.284340	17.236248	73.988238
405.168975	18.014957	73.993242
404.638707	13.104445	73.998247
404.006188	10.235884	74.003252
403.163861	12.062368	74.008257
402.503713	13.307871	74.013262
401.671322	18.043125	74.018266
401.283323	17.326840	74.023271
401.176990	18.167902	74.028276
399.943161	20.861045	74.033281
399.401063	15.955573	74.038286
398.554238	18.450635	74.043290
398.137701	12.708269	74.048295
397.638540	12.699636	74.053300
396.539780	19.374470	74.058305
396.045364	15.279864	74.063310
395.373621	20.528854	74.068314
394.892760	20.041051	74.073319
393.818034	11.377312	74.078324
393.132975	20.108862	74.083329
392.497455	8.251097	74.088334
392.101948	12.141636	74.093338
391.526023	10.262301	74.098343
391.055013	13.436299	74.103348
389.950133	18.323004	74.108353
389.839513	12.058002	74.113358
389.317678	14.265514	74.118362
387.857050	20.356180	74.123367
387.503913	12.058436	74.128372
386.623402	16.810036	74.133377
386.500226	8.531631	74.138382
385.116727	12.920250	74.143386
384.346960	15.143619	74.148391
384.247649	9.080249	74.153396
383.307865	8.362801	74.158401
383.226954	0.413566	74.163406
382.164404	18.619166	74.168410
381.355030	20.229088	74.173415
380.964519	5.459779	74.178420
379.966709	6.672364	74.183425
379.628308	4.547016	74.188430
378.395243	13.801937	74.193434
378.136718	15.048099	74.198439
377.812054	11.299406	74.203444
377.012273	8.935340	74.208449
376.268954	7.667752	74.213454
375.488769	13.374797	74.218458
374.910042	7.801004	74.223463
374.606499	16.620781	74.228468
373.182700	25.318676	74.233473
372.967468	7.396609	74.238478
372.325531	14.070401	74.243482
371.703716	4.493169	74.248487
371.106282	10.579532	74.253492
369.936853	20.068754	74.258497
369.574688	8.811638	74.263502
369.400091	15.347872	74.268506
368.243560	12.122850	74.273511
367.389403	17.974155	74.278516
366.535480	12.338562	74.283521
366.591260	5.219122	74.288526
365.655225	13.855837	74.293530
364.630106	12.062290	74.298535
364.204842	17.225482	74.303540
363.629612	15.090569	74.308545
363.365608	8.591388	74.313550
362.554279	8.381770	74.318554
361.507479	19.053124	74.323559
360.995248	11.823926	74.328564
360.303381	18.122469	74.333569
360.241256	6.483215	74.338574
358.917455	3.737456	74.343578
358.301089	20.030021	74.348583
357.491632	5.273871	74.353588
357.123168	11.656492	74.358593
356.690033	13.931878	74.363598
355.876862	17.810137	74.368602
355.482223	14.976219	74.373607
354.623617	12.219401	74.378612
353.583510	16.553310	74.383617
353.026471	12.911043	74.388622
352.591059	16.798486	74.393626
351.974996	12.875459	74.398631
350.933932	11.264236	74.403636
350.108466	15.880914	74.408641
349.589366	12.937521	74.413646
349.450391	14.418528	74.418650
348.764965	18.470401	74.423655
347.680856	14.057405	74.428660
347.151953	16.081543	74.433665
346.621049	0.722750	74.438670
345.971280	12.023128	74.443674
344.955562	12.913719	74.448679
344.492188	7.236393	74.453684
343.801465	15.021864	74.458689
343.243818	14.834901	74.463694
342.117612	8.072583	74.468698
341.675111	6.048991	74.473703
341.348388	7.408529	74.478708
340.719814	14.474447	74.483713
340.385912	5.680840	74.488718
339.127578	8.592387	74.493722
338.500322	13.677385	74.498727
338.083356	12.576998	74.503732
337.160521	15.119675	74.508737
336.607477	7.382890	74.513742
335.666804	13.459310	74.518746
335.234197	16.273948	74.523751
335.182315	12.024456	74.528756
333.700371	16.023505	74.533761
333.181382	15.481866	74.538766
332.566645	15.248810	74.543770
331.954759	15.032646	74.548775
331.585609	18.228268	74.553780
330.273565	20.979643	74.558785
329.859311	13.334280	74.563790
329.358654	19.063020	74.568794
328.834971	19.471484	74.573799
327.971544	16.851065	74.578804
327.281082	18.180269	74.583809
326.690375	11.272681	74.588814
326.324080	15.731023	74.593818
325.241451	14.295175	74.598823
324.875373	7.914775	74.603828
323.951301	11.848566	74.608833
323.732953	8.051398	74.613838
322.363594	17.340683	74.618842
321.383037	20.278932	74.623847
321.134322	13.629081	74.628852
320.423484	16.809777	74.633857
320.385261	6.721640	74.638862
319.923425	16.161176	74.643866
318.718454	20.158667	74.648871
317.993366	14.638180	74.653876
317.455925	27.917150	74.658881
317.259160	15.559743	74.663886
315.900300	12.130446	74.668890
315.169031	16.617000	74.673895
315.323303	11.787432	74.678900
314.314085	28.536876	74.683905
313.286821	7.690396	74.688910
312.857541	19.179573	74.693914
312.121980	15.966329	74.698919
311.636034	13.732041	74.703924
310.562514	20.320092	74.708929
310.166345	11.963779	74.713934
309.469970	21.770296	74.718938
309.119760	17.390155	74.723943
308.432956	20.125464	74.728948
307.100643	24.234724	74.733953
306.708438	8.650398	74.738958
306.274727	16.369679	74.743962
305.927995	14.155781	74.748967
304.946649	22.798164	74.753972
304.044525	19.658782	74.758977
303.474017	14.465331	74.763982
302.801399	27.912509	74.768986
302.101766	14.878302	74.773991
301.470271	18.601459	74.778996
300.460058	24.641668	74.784001
300.367863	14.696176	74.789006
299.790945	24.185603	74.794010
299.146285	29.935728	74.799015
298.654315	25.146085	74.804020
297.864887	23.261379	74.809025
297.232912	15.991358	74.814030
296.090736	23.487671	74.819034
295.087709	35.400275	74.824039
294.904729	24.471795	74.829044
294.167744	22.326411	74.834049
294.034564	16.348873	74.839054
292.795531	21.588172	74.844058
292.410772	21.998154	74.849063
291.943508	22.487521	74.854068
291.119306	23.252986	74.859073
290.241552	20.437740	74.864078
289.678577	21.852292	74.869082
289.310057	23.647444	74.874087
288.796462	15.806608	74.879092
287.460093	21.405209	74.884097
286.959468	19.898684	74.889102
286.359425	28.022967	74.894106
285.977122	11.752648	74.899111
285.248500	16.798621	74.904116
284.105052	23.900893	74.909121
283.759264	16.632568	74.914126
283.260036	24.162020	74.919130
282.245134	18.339225	74.924135
281.460343	21.321979	74.929140
280.875067	26.280449	74.934145
280.620895	17.500949	74.939150
280.118309	23.950693	74.944154
279.108771	21.785680	74.949159
278.670017	24.290640	74.954164
277.888273	33.202427	74.959169
277.420559	17.133384	74.964174
276.188073	26.903940	74.969178
275.651644	20.342537	74.974183
275.274096	16.703218	74.979188
274.584799	15.434935	74.984193
273.730739	20.166584	74.989198
272.998489	20.915821	74.994202
272.401988	20.673565	74.999207
272.283800	12.421187	75.004212
271.227960	25.464241	75.009217
270.542801	19.812822	75.014222
269.700437	26.649479	75.019226
269.195951	19.961557	75.024231
268.844659	9.959601	75.029236
267.674760	17.154404	75.034241
266.858045	16.691780	75.039246
266.378306	11.482295	75.044250
265.997283	17.475833	75.049255
265.886983	13.975269	75.054260
264.972004	28.851999	75.059265
264.246493	15.750967	75.064270
263.080815	17.845091	75.069274
262.105656	27.472127	75.074279
261.529461	17.559639	75.079284
261.138313	27.784303	75.084289
261.381636	12.843020	75.089294
260.393028	15.657991	75.094298
259.155015	11.157607	75.099303
258.845496	12.101240	75.104308
257.900302	20.890842	75.109313
257.513290	9.405899	75.114318
256.130653	21.886021	75.119322
255.991053	20.747740	75.124327
255.695726	11.328239	75.129332
254.896654	12.067633	75.134337
254.033676	5.149857	75.139342
253.212395	12.349014	75.144346
252.449157	19.409608	75.149351
252.452920	11.896329	75.154356
251.157941	20.859969	75.159361
250.529972	12.796098	75.164366
250.037015	17.189482	75.169370
249.382638	19.470192	75.174375
249.344378	11.946265	75.179380
247.950538	11.848471	75.184385
247.277734	7.439345	75.189390
246.715005	11.842274	75.194394
246.154584	13.371548	75.199399
245.313092	16.642479	75.204404
244.477685	21.830069	75.209409
243.953425	12.478607	75.214414
243.525646	15.836553	75.219418
243.123251	19.069025	75.224423
241.945363	13.352662	75.229428
241.132792	19.829749	75.234433
240.937971	12.739224	75.239438
240.468141	14.910088	75.244442
239.792227	12.179384	75.249447
238.728357	6.856444	75.254452
237.781158	24.458629	75.259457
237.931498	19.894621	75.264462
236.715017	12.135894	75.269466
235.793110	17.401932	75.274471
235.410903	14.190731	75.279476
234.983664	23.571146	75.284481
234.874397	9.272722	75.289486
233.384584	15.717426	75.294490
232.651076	20.554451	75.299495
232.480414	12.116474	75.304500
231.611870	25.593317	75.309505
230.783600	17.003126	75.314510
230.044788	15.681247	75.319514
229.383609	23.466766	75.324519
229.595465	21.501304	75.329524
228.428014	24.259643	75.334529
227.560992	11.359393	75.339534
226.866387	22.827796	75.344538
226.300681	18.269132	75.349543
226.129213	20.955420	75.354548
224.800382	21.006552	75.359553
224.412937	10.324378	75.364558
223.695834	15.106748	75.369562
222.880982	12.841335	75.374567
222.183594	17.434477	75.379572
221.441388	20.088751	75.384577
221.149753	14.464500	75.389582
220.941215	17.074694	75.394586
219.974241	20.318329	75.399591
219.381499	10.406921	75.404596
218.224489	20.348395	75.409601
217.227349	18.640339	75.414606
216.322352	19.502291	75.419610
215.750987	18.022830	75.424615
215.684282	10.963925	75.429620
215.242229	16.921463	75.434625
215.074394	12.887591	75.439630
213.902592	10.064062	75.444634
213.288397	8.591431	75.449639
212.556905	4.975440	75.454644
211.636731	17.754018	75.459649
210.897759	8.796356	75.464654
209.754659	16.933106	75.469658
209.483315	9.652932	75.474663
209.369416	9.206013	75.479668
208.740390	14.783342	75.484673
208.158582	11.249145	75.489678
207.251288	17.537911	75.494682
206.767315	14.119007	75.499687
206.161476	14.868609	75.504692
204.803431	24.249191	75.509697
204.562419	13.674565	75.514702
203.963516	11.966102	75.519706
202.794315	23.888657	75.524711
202.484392	13.277708	75.529716
201.727201	23.966020	75.534721
201.324666	17.089971	75.539726
200.875530	16.545109	75.544730
199.612102	20.471546	75.549735
198.929998	20.629321	75.554740
198.102038	24.853770	75.559745
198.352270	17.821605	75.564750
197.654773	6.083401	75.569754
196.371409	18.631299	75.574759
196.000056	19.539066	75.579764
195.070037	28.860874	75.584769
194.582670	17.672648	75.589774
193.620985	12.568408	75.594778
193.108466	16.010837	75.599783
193.010986	10.483374	75.604788
192.297043	9.491866	75.609793
191.217108	10.534687	75.614798
190.492735	19.180288	75.619802
190.244415	15.392645	75.624807
189.662671	13.736645	75.629812
188.281916	21.931799	75.634817
187.531914	10.723953	75.639822
187.074846	18.557360	75.644826
186.624868	19.360967	75.649831
186.357667	10.201934	75.654836
185.167592	10.103228	75.659841
184.584001	2.010232	75.664846
184.027943	20.180856	75.669850
183.493332	20.690443	75.674855
182.958489	12.903491	75.679860
181.406938	20.438310	75.684865
181.355715	17.139651	75.689870
180.902780	16.888719	75.694874
180.160810	15.819680	75.699879
179.469892	15.267640	75.704884
178.431283	15.646270	75.709889
178.178345	22.597132	75.714894
177.746020	25.123161	75.719898
177.110856	19.828088	75.724903
176.188106	22.039640	75.729908
175.309927	19.140926	75.734913
175.135822	19.121511	75.739918
174.247586	17.877093	75.744922
173.420932	22.820451	75.749927
173.093582	20.799031	75.754932
171.633367	26.057882	75.759937
171.391057	10.127992	75.764942
170.537288	13.545987	75.769946
170.022221	12.948563	75.774951
169.884781	3.729423	75.779956
168.693977	12.370546	75.784961
168.247210	5.310747	75.789966
167.499626	14.087786	75.794970
167.007739	16.697431	75.799975
166.411394	10.746453	75.804980
165.029774	18.755669	75.809985
164.848995	12.803085	75.814990
164.190883	18.273095	75.819994
163.844668	17.063684	75.824999
163.125187	16.044681	75.830004
162.048455	15.058989	75.835009
161.677698	9.026309	75.840014
161.095050	19.431322	75.845018
159.871620	19.541378	75.850023
159.396525	18.992778	75.855028
158.492998	21.300622	75.860033
158.409551	21.118515	75.865038
158.236115	9.615315	75.870042
156.952929	13.186943	75.875047
156.603472	10.738532	75.880052
155.519979	25.635844	75.885057
154.819779	6.591866	75.890062
154.061115	12.498967	75.895066
153.004066	15.162461	75.900071
153.157918	15.641125	75.905076
152.705504	19.069246	75.910081
151.801238	2.175720	75.915086
151.032642	12.652958	75.920090
150.480452	12.810532	75.925095
150.045528	5.815082	75.930100
148.678479	14.859643	75.935105
148.065620	9.956852	75.940110
147.525501	6.671499	75.945114
147.141308	6.849594	75.950119
146.864752	8.278429	75.955124
145.529226	15.326221	75.960129
144.555824	9.969977	75.965134
144.141405	17.653080	75.970138
143.769048	15.973165	75.975143
143.649393	-4.087486	75.980148
142.401912	16.640882	75.985153
141.555919	6.082319	75.990158
141.161182	16.082042	75.995162
140.202937	13.755943	76.000167
139.484281	11.678653	76.005172
138.769882	17.982413	76.010177
138.434557	7.167371	76.015182
138.005054	9.316051	76.020186
137.270673	15.019007	76.025191
136.691774	7.545035	76.030196
135.717754	15.577578	76.035201
135.164606	12.340037	76.040206
134.716248	8.477067	76.045210
133.706594	16.160470	76.050215
133.479574	13.000238	76.055220
132.714826	19.037631	76.060225
132.366361	14.565781	76.065230
131.136838	13.181832	76.070234
130.300311	11.861375	76.075239
130.078627	4.332020	76.080244
128.785245	16.960389	76.085249
127.916346	7.879974	76.090254
127.508897	16.199073	76.095258
126.964470	7.210422	76.100263
126.815792	5.204675	76.105268
126.493020	12.478914	76.110273
125.553529	11.545472	76.115278
125.022683	4.229426	76.120282
124.131806	2.543892	76.125287
123.266014	7.332647	76.130292
122.325523	12.890274	76.135297
122.021647	13.785713	76.140302
121.283147	13.507790	76.145306
120.053084	16.801300	76.150311
119.527017	12.160651	76.155316
118.956778	20.095694	76.160321
119.089829	13.736668	76.165326
118.404355	14.674038	76.170330
117.177958	9.981064	76.175335
116.494741	11.219280	76.180340
115.983359	22.645866	76.185345
115.606801	15.097050	76.190350
114.799454	8.004877	76.195354
113.442989	18.843965	76.200359
113.245716	18.842442	76.205364
112.690347	24.050070	76.210369
112.487094	15.816010	76.215374
111.232181	16.118774	76.220378
109.950901	4.505245	76.225383
109.992044	6.447983	76.230388
109.241628	16.911294	76.235393
108.777217	14.033357	76.240398
108.232116	14.830069	76.245402
107.397957	18.782711	76.250407
106.710818	18.627493	76.255412
106.289660	16.930134	76.260417
105.606345	12.224677	76.265422
104.651621	16.062503	76.270426
104.069946	17.948444	76.275431
103.630224	12.276867	76.280436
102.768407	8.770009	76.285441
101.785140	10.182239	76.290446
101.098540	9.254209	76.295450
100.641000	13.299759	76.300455
100.705281	8.590200	76.305460
99.730344	15.932178	76.310465
98.909894	17.722154	76.315470
98.222140	17.327333	76.320474
97.495041	14.794074	76.325479
96.839910	11.918169	76.330484
95.601412	17.212664	76.335489
95.304482	17.558205	76.340494
95.024525	16.890186	76.345498
94.561619	16.746520	76.350503
93.412089	2.139359	76.355508
92.542438	16.777065	76.360513
91.956834	11.109833	76.365518
91.706530	21.103875	76.370522
91.081701	25.467853	76.375527
90.259037	17.105493	76.380532
89.387310	15.158289	76.385537
89.107894	7.513564	76.390542
88.444782	13.086891	76.395546
87.578346	19.197284	76.400551
87.102553	22.562911	76.405556
86.401143	23.189009	76.410561
85.870244	10.014446	76.415566
84.624964	15.855667	76.420570
83.741913	13.831422	76.425575
83.575204	12.047755	76.430580
83.006632	16.448493	76.435585
82.407433	16.621464	76.440590
82.042649	7.432285	76.445594
81.100814	20.398858	76.450599
80.803865	10.940231	76.455604
79.531343	17.372441	76.460609
78.511689	9.953011	76.465614
78.187000	22.773850	76.470618
77.961682	19.648046	76.475623
77.436762	12.285333	76.480628
76.294780	21.043293	76.485633
75.924560	13.941343	76.490638
75.371189	10.178715	76.495642
74.151022	13.929573	76.500647
73.623660	11.523743	76.505652
72.726517	21.080039	76.510657
72.594276	9.081418	76.515662
71.832004	16.827891	76.520666
70.609566	19.128279	76.525671
70.238393	14.727873	76.530676
69.648390	15.872385	76.535681
69.137269	18.524539	76.540686
69.207939	15.226947	76.545690
67.603308	16.243117	76.550695
67.369143	8.025038	76.555700
66.368832	17.127844	76.560705
65.358652	12.794662	76.565710
65.009734	21.621687	76.570714
64.057108	16.539715	76.575719
63.785063	11.391776	76.580724
63.450872	17.669605	76.585729
62.973614	7.329818	76.590734
62.027857	22.733477	76.595738
61.418794	24.410902	76.600743
60.534546	10.846415	76.605748
59.371327	22.362777	76.610753
58.496977	18.518878	76.615758
58.287461	11.257258	76.620762
58.029649	19.136170	76.625767
57.945958	17.567929	76.630772
56.352783	18.714746	76.635777
55.623472	11.231671	76.640782
55.244497	15.012378	76.645786
54.715240	22.999244	76.650791
54.028983	9.565613	76.655796
52.808848	18.498476	76.660801
52.656848	11.773322	76.665806
52.182233	17.244051	76.670810
51.278826	13.045237	76.675815
50.223030	10.088169	76.680820
49.724552	13.451110	76.685825
49.229893	13.498602	76.690830
49.060302	17.381535	76.695834
47.907611	19.268676	76.700839
47.283908	18.529331	76.705844
46.508630	22.737536	76.710849
46.107595	8.122981	76.715854
45.732635	19.441077	76.720858
44.499532	22.208392	76.725863
44.114513	6.794902	76.730868
43.605223	21.635349	76.735873
42.274320	10.871890	76.740878
41.784479	14.774364	76.745882
41.019638	14.327197	76.750887
41.173595	14.455744	76.755892
40.219365	18.233589	76.760897
39.185857	11.268984	76.765902
38.734755	12.050718	76.770906
38.150272	9.978868	76.775911
37.952376	6.148513	76.780916
36.514216	19.705207	76.785921
36.273213	14.525512	76.790926
35.734528	17.155259	76.795930
34.663390	15.403890	76.800935
34.017248	14.187145	76.805940
33.015793	13.052305	76.810945
32.572681	12.869223	76.815950
32.349747	12.420780	76.820954
31.245612	10.089612	76.825959
30.738905	12.446170	76.830964
29.926517	18.705659	76.835969
29.521277	8.070535	76.840974
29.526012	8.349042	76.845978
28.332269	10.961848	76.850983
27.488209	12.145316	76.855988
26.894320	16.993238	76.860993
26.399848	10.712233	76.865998
25.520588	10.928312	76.871002
24.767854	12.030981	76.876007
24.266933	6.892749	76.881012
23.288735	17.539071	76.886017
22.378205	13.317750	76.891022
22.077824	14.196874	76.896026
21.428642	22.616045	76.901031
21.302409	11.471204	76.906036
20.119476	8.925524	76.911041
19.301394	6.626006	76.916046
19.015543	10.190007	76.921050
18.316695	16.112834	76.926055
17.781830	11.830016	76.931060
16.754464	18.040218	76.936065
16.449397	7.523164	76.941070
16.049437	14.872803	76.946074
14.844846	24.227416	76.951079
14.419972	10.081885	76.956084
13.485629	17.343297	76.961089
13.045195	8.263976	76.966094
12.103175	11.125226	76.971098
11.057240	15.911213	76.976103
10.773705	14.758061	76.981108
9.915824	23.470729	76.986113
9.884169	9.760806	76.991118
9.197863	16.503248	76.996122
8.344746	10.607471	77.001127
7.814095	12.341787	77.006132
6.980184	13.154627	77.011137
6.469604	9.173876	77.016142
5.375151	22.119081	77.021147
4.536381	16.739846	77.026151
4.394135	12.602565	77.031156
3.610551	22.361544	77.036161