Fri Mar 05 18:12:01 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.648772	107.821708	0.000000
-1.201837	91.375226	0.005005
-1.795130	54.412199	0.010010
-3.944268	30.674465	0.015014
-7.611423	4.923815	0.020019
-12.459878	4.101375	0.025024
-17.769883	9.203184	0.030029
-22.222493	4.064491	0.035034
-26.016835	8.867780	0.040038
-29.603962	10.876720	0.045043
-33.358942	8.187790	0.050048
-37.482806	15.405988	0.055053
-40.716761	7.240664	0.060058
-44.610934	8.606309	0.065062
-48.379455	3.623473	0.070067
-52.006852	4.618559	0.075072
-56.224483	5.469684	0.080077
-59.780177	4.258180	0.085082
-63.280035	9.894506	0.090086
-67.157621	8.092530	0.095091
-70.830416	4.613096	0.100096
-74.802617	10.785271	0.105101
-78.584597	7.738013	0.110106
-82.357668	12.326679	0.115110
-86.056117	8.870284	0.120115
-89.694534	-0.269671	0.125120
-93.777807	12.206113	0.130125
-97.283375	10.564035	0.135130
-101.075664	12.995327	0.140134
-104.614828	9.505662	0.145139
-108.360266	9.101956	0.150144
-112.522977	9.591172	0.155149
-115.998346	6.102386	0.160154
-120.033103	9.177953	0.165158
-123.712031	7.317565	0.170163
-127.351933	5.676464	0.175168
-131.066758	9.180407	0.180173
-134.417073	3.156406	0.185178
-138.769077	1.885993	0.190182
-142.712517	8.216114	0.195187
-146.351095	6.584293	0.200192
-150.295857	11.555278	0.205197
-154.090388	11.022279	0.210202
-157.976095	10.702535	0.215206
-161.711899	0.427036	0.220211
-165.143040	9.532939	0.225216
-169.217216	12.931851	0.230221
-172.508830	8.179048	0.235226
-176.430456	13.780330	0.240230
-179.892565	-1.121526	0.245235
-183.652739	3.033139	0.250240
-187.356733	18.378583	0.255245
-191.058265	6.725684	0.260250
-195.380362	6.073509	0.265254
-199.059388	13.660958	0.270259
-202.532746	5.598728	0.275264
-206.552945	11.518568	0.280269
-210.439217	10.665978	0.285274
-214.101248	11.617947	0.290278
-217.818735	10.475076	0.295283
-221.658450	12.291214	0.300288
-225.281206	17.050077	0.305293
-229.079343	12.879671	0.310298
-232.635822	19.804204	0.315302
-236.232400	17.389940	0.320307
-240.068695	11.128255	0.325312
-244.364508	12.484203	0.330317
-247.743238	9.459590	0.335322
-251.673377	11.588257	0.340326
-255.532223	16.758589	0.345331
-259.120446	5.084566	0.350336
-262.992238	15.412129	0.355341
-266.221872	8.957464	0.360346
-270.473498	9.931083	0.365350
-274.546277	14.843850	0.370355
-278.065431	12.628607	0.375360
-281.894798	12.478269	0.380365
-285.364317	15.419731	0.385370
-289.234604	20.924687	0.390374
-292.989669	17.073944	0.395379
-296.569852	7.067143	0.400384
-300.964454	16.755961	0.405389
-304.253773	9.757355	0.410394
-308.391325	14.615861	0.415398
-311.862656	20.117091	0.420403
-315.399809	17.113132	0.425408
-319.158733	16.532131	0.430413
-322.889085	1.146611	0.435418
-326.947661	5.439017	0.440422
-330.488425	13.439831	0.445427
-334.195154	10.765752	0.450432
-338.103984	22.641633	0.455437
-341.527690	10.104098	0.460442
-345.823738	15.539912	0.465446
-349.296260	16.938080	0.470451
-353.162481	9.249463	0.475456
-357.160673	14.554165	0.480461
-360.910862	11.147463	0.485466
-364.732914	10.912509	0.490470
-368.348328	15.362897	0.495475
-372.141476	9.819955	0.500480
-375.759755	20.148217	0.505485
-379.049301	12.608851	0.510490
-383.146228	14.830592	0.515494
-386.993100	16.246004	0.520499
-390.744637	12.467398	0.525504
-394.645526	22.213172	0.530509
-398.604420	1.866821	0.535514
-402.385296	-0.035205	0.540518
-406.001613	4.875857	0.545523
-409.509873	6.199390	0.550528
-413.496601	7.780680	0.555533
-416.994102	6.639266	0.560538
-421.009306	8.638283	0.565542
-424.753681	5.311183	0.570547
-428.410170	9.260428	0.575552
-432.719018	8.819459	0.580557
-435.987809	6.430432	0.585562
-439.500919	0.309870	0.590566
-443.459096	10.444911	0.595571
-446.809577	3.047845	0.600576
-451.102997	5.974447	0.605581
-454.676393	3.228806	0.610586
-458.540271	8.955351	0.615590
-462.245076	12.483425	0.620595
-465.774301	4.774303	0.625600
-469.896306	14.613847	0.630605
-473.439008	4.263873	0.635610
-477.462381	8.935690	0.640614
-481.144256	-1.795747	0.645619
-484.946902	4.572350	0.650624
-488.844359	18.238084	0.655629
-492.148766	6.732004	0.660634
-496.216539	10.668186	0.665638
-500.043346	6.337221	0.670643
-503.420603	7.253609	0.675648
-507.610373	8.408582	0.680653
-510.955461	5.147161	0.685658
-514.977084	2.749171	0.690662
-518.972260	12.111213	0.695667
-522.588401	11.745852	0.700672
-526.363932	12.035169	0.705677
-530.180175	5.321331	0.710682
-533.784818	16.278424	0.715686
-537.646644	18.710462	0.720691
-541.224455	10.222304	0.725696
-545.032683	14.145497	0.730701
-548.379882	0.769740	0.735706
-552.464694	6.102782	0.740710
-556.405663	7.579227	0.745715
-560.276300	13.303858	0.750720
-563.963507	5.557046	0.755725
-567.583320	4.022224	0.760730
-571.442990	7.147840	0.765734
-575.117117	4.639250	0.770739
-578.884910	-0.826970	0.775744
-582.735084	5.619833	0.780749
-586.557839	6.334688	0.785754
-590.530080	10.039720	0.790758
-594.064032	9.785920	0.795763
-597.448853	8.609425	0.800768
-601.322046	8.975964	0.805773
-605.105661	-10.700957	0.810778
-609.244947	2.423248	0.815782
-612.867978	0.280299	0.820787
-616.615950	2.057174	0.825792
-620.408825	4.453095	0.830797
-623.839932	-1.740207	0.835802
-627.747091	8.267117	0.840806
-631.499555	-0.935741	0.845811
-635.327470	7.289569	0.850816
-639.319845	10.564229	0.855821
-642.535613	0.709507	0.860826
-647.076830	7.929148	0.865830
-650.308752	8.098691	0.870835
-653.889878	1.915209	0.875840
-658.033275	18.679820	0.880845
-661.616422	7.281612	0.885850
-665.349530	9.526127	0.890854
-669.359620	2.950731	0.895859
-672.874628	12.829237	0.900864
-676.710882	15.866123	0.905869
-680.337329	10.670799	0.910874
-683.861865	8.412871	0.915878
-688.011673	6.849379	0.920883
-691.791400	-1.407568	0.925888
-695.877712	24.002417	0.930893
-699.252006	2.262215	0.935898
-703.144867	9.968145	0.940902
-706.805131	9.234796	0.945907
-710.442520	3.464099	0.950912
-714.522527	12.833697	0.955917
-717.965583	6.383820	0.960922
-721.951658	18.658979	0.965926
-725.881492	10.973280	0.970931
-729.276432	2.049346	0.975936
-733.054805	10.736828	0.980941
-736.914960	2.328803	0.985946
-740.878013	11.285510	0.990950
-744.233627	7.199774	0.995955
-747.899199	0.295068	1.000960
-752.078651	8.676086	1.005965
-755.710452	7.398940	1.010970
-759.546718	10.451729	1.015974
-763.227188	10.816117	1.020979
-766.890085	12.939181	1.025984
-770.837036	13.603217	1.030989
-774.516013	12.188559	1.035994
-778.324792	6.338127	1.040998
-782.332249	9.620165	1.046003
-785.644555	10.252179	1.051008
-789.557406	11.647242	1.056013
-793.297679	2.059502	1.061018
-797.417943	16.217050	1.066022
-800.845885	19.630425	1.071027
-804.583017	7.001794	1.076032
-808.739670	11.807424	1.081037
-812.098694	2.040504	1.086042
-815.967368	3.953681	1.091046
-819.701804	9.983381	1.096051
-823.003357	1.896229	1.101056
-827.104070	11.160508	1.106061
-831.073752	7.319715	1.111066
-834.942567	17.661862	1.116070
-838.453274	0.777123	1.121075
-841.542823	-0.302713	1.126080
-845.705289	10.192043	1.131085
-849.492799	-0.195459	1.136090
-853.695590	19.043758	1.141094
-857.569106	9.318148	1.146099
-861.275444	5.241343	1.151104
-864.970205	11.991753	1.156109
-868.273715	3.709436	1.161114
-872.359038	7.757864	1.166118
-875.831059	8.596888	1.171123
-879.834593	9.252805	1.176128
-884.075902	11.083738	1.181133
-887.481360	4.733768	1.186138
-891.524079	11.356918	1.191142
-895.058628	8.397583	1.196147
-898.061651	5.771173	1.201152
-902.182741	12.711226	1.206157
-905.760540	10.744429	1.211162
-910.076818	14.659534	1.216166
-913.764749	2.130464	1.221171
-917.201985	7.108265	1.226176
-921.198210	15.786709	1.231181
-925.004215	4.894507	1.236186
-928.995596	15.179121	1.241190
-932.642717	13.953586	1.246195
-935.964429	2.769502	1.251200
-940.087891	1.645375	1.256205
-943.655209	3.769197	1.261210
-947.728083	4.806904	1.266214
-951.311537	3.509718	1.271219
-954.926612	0.027184	1.276224
-958.792995	11.042492	1.281229
-962.571990	-6.010444	1.286234
-966.772647	-5.302357	1.291238
-970.206567	4.134652	1.296243
-973.604130	-2.167560	1.301248
-977.661401	7.290292	1.306253
-981.107593	-4.676487	1.311258
-985.303366	3.021550	1.316262
-988.987803	10.505362	1.321267
-992.294435	-2.951877	1.326272
-996.550335	-2.838881	1.331277
-1000.045566	-10.795439	1.336282
-1003.883313	-3.149897	1.341286
-1008.021327	8.806219	1.346291
-1011.656474	3.838325	1.351296
-1015.511428	9.903367	1.356301
-1019.156645	2.141132	1.361306
-1022.599130	2.161933	1.366310
-1026.459084	4.048827	1.371315
-1030.007389	5.471141	1.376320
-1034.229209	17.068545	1.381325
-1038.035650	0.863806	1.386330
-1041.552349	7.545000	1.391334
-1045.216138	4.543489	1.396339
-1048.808313	0.964400	1.401344
-1053.173928	14.609659	1.406349
-1056.787572	14.504920	1.411354
-1060.482515	9.157156	1.416358
-1064.099856	-2.178138	1.421363
-1067.157328	-4.516493	1.426368
-1071.495061	9.453919	1.431373
-1075.380286	1.648164	1.436378
-1079.670891	10.746112	1.441382
-1083.451412	7.506288	1.446387
-1086.790431	-4.620968	1.451392
-1090.348165	2.587256	1.456397
-1093.745173	0.244901	1.461402
-1098.122997	7.760941	1.466406
-1102.198436	10.273790	1.471411
-1105.251462	12.362897	1.476416
-1109.304177	10.164877	1.481421
-1113.172615	5.584552	1.486426
-1116.708453	5.199376	1.491430
-1120.402155	-3.089525	1.496435
-1124.425406	10.767592	1.501440
-1128.434388	11.760699	1.506445
-1131.969670	8.722999	1.511450
-1135.681697	4.388929	1.516454
-1139.413212	12.610634	1.521459
-1143.011029	-0.460739	1.526464
-1146.751719	9.747842	1.531469
-1150.315453	0.413169	1.536474
-1154.465299	8.044226	1.541478
-1158.279948	-1.332292	1.546483
-1161.760626	-3.878781	1.551488
-1165.974128	7.772702	1.556493
-1169.391370	-6.149111	1.561498
-1173.339048	5.634895	1.566502
-1177.306178	12.820441	1.571507
-1180.349922	5.996726	1.576512
-1184.292923	13.653090	1.581517
-1188.437217	-1.368209	1.586522
-1192.346824	9.890917	1.591526
-1195.963572	-2.822518	1.596531
-1199.157531	-1.552841	1.601536
-1203.273670	3.879347	1.606541
-1207.051066	-3.471914	1.611546
-1210.488851	5.611226	1.616550
-1214.401245	6.212130	1.621555
-1218.661936	3.921427	1.626560
-1222.272506	11.105184	1.631565
-1226.003039	0.862185	1.636570
-1229.593011	-9.396984	1.641574
-1233.520717	10.396474	1.646579
-1237.127116	8.226610	1.651584
-1241.059311	0.933291	1.656589
-1244.616167	-1.391145	1.661594
-1248.452204	12.264321	1.666598
-1252.596190	-2.512471	1.671603
-1255.902528	-8.562340	1.676608
-1259.660432	0.926911	1.681613
-1263.178622	-10.293022	1.686618
-1267.045869	6.258033	1.691622
-1271.118084	3.461022	1.696627
-1274.963884	-4.785930	1.701632
-1278.587210	0.904988	1.706637
-1282.113307	-3.654137	1.711642
-1286.004452	3.522575	1.716646
-1289.595617	0.074595	1.721651
-1293.419598	4.838856	1.726656
-1297.434596	-2.704460	1.731661
-1301.008679	0.231542	1.736666
-1305.239598	2.432156	1.741670
-1309.192285	-1.183437	1.746675
-1312.472966	-2.331400	1.751680
-1315.966974	10.682793	1.756685
-1319.546127	7.422171	1.761690
-1323.699189	7.459380	1.766694
-1327.600925	11.829287	1.771699
-1331.186408	7.658212	1.776704
-1335.094947	20.238893	1.781709
-1338.556420	4.444685	1.786714
-1342.288241	9.866060	1.791718
-1346.217778	2.239764	1.796723
-1350.056976	-6.463853	1.801728
-1353.847529	9.043725	1.806733
-1357.537889	-0.030639	1.811738
-1361.309925	7.303749	1.816742
-1365.200507	14.844781	1.821747
-1368.617369	5.997889	1.826752
-1372.392973	5.798143	1.831757
-1375.823030	-5.970305	1.836762
-1379.869448	1.389109	1.841766
-1384.140877	-0.683522	1.846771
-1387.607671	0.942328	1.851776
-1391.300743	10.900803	1.856781
-1395.241773	-5.105112	1.861786
-1399.252486	2.830518	1.866790
-1402.552614	12.685102	1.871795
-1406.066153	6.517234	1.876800
-1410.260648	6.447691	1.881805
-1413.639369	3.930996	1.886810
-1417.838369	4.961330	1.891814
-1421.716781	1.565856	1.896819
-1425.482794	-8.330487	1.901824
-1429.125286	-0.081600	1.906829
-1432.507533	-1.377134	1.911834
-1436.213260	-3.234308	1.916838
-1440.209770	1.012183	1.921843
-1443.908198	-4.236611	1.926848
-1447.945063	-1.961153	1.931853
-1451.789856	3.700831	1.936858
-1455.516730	0.558697	1.941862
-1459.327356	6.071720	1.946867
-1463.094900	1.411190	1.951872
-1466.624197	16.782492	1.956877
-1469.894004	0.435845	1.961882
-1474.015119	3.458125	1.966886
-1478.101609	4.262394	1.971891
-1481.473916	3.312272	1.976896
-1485.321783	9.070998	1.981901
-1488.940951	6.551917	1.986906
-1492.903465	9.405331	1.991910
-1496.825520	19.484215	1.996915
-1500.740244	7.974359	2.006912
-1501.405099	5.671521	2.016909
-1498.965955	8.254362	2.026906
-1496.319393	8.228677	2.036902
-1494.189252	12.364193	2.046899
-1492.069503	12.748143	2.056896
-1490.226301	4.503045	2.066893
-1488.527166	6.841231	2.076890
-1486.680542	11.819539	2.086886
-1484.158476	7.730562	2.096883
-1482.558264	6.097671	2.106880
-1480.733579	9.007875	2.116877
-1479.073964	2.982229	2.126874
-1476.915324	2.262574	2.136870
-1475.313303	5.360018	2.146867
-1473.173886	4.531338	2.156864
-1471.143798	0.748527	2.166861
-1469.362713	5.194173	2.176858
-1467.358810	9.400456	2.186854
-1465.534365	9.340651	2.196851
-1463.882634	7.004772	2.206848
-1461.847575	5.693854	2.216845
-1459.938720	0.086217	2.226842
-1458.068327	5.128637	2.236838
-1456.521481	2.957981	2.246835
-1454.234303	6.081529	2.256832
-1452.053555	7.954200	2.266829
-1450.526247	2.492925	2.276826
-1448.734589	2.359434	2.286822
-1446.953340	4.588186	2.296819
-1444.717522	5.113072	2.306816
-1442.833252	1.694691	2.316813
-1440.993174	0.486064	2.326810
-1439.270720	0.278396	2.336806
-1437.379084	2.936332	2.346803
-1435.545036	2.426584	2.356800
-1433.820935	3.502366	2.366797
-1431.625603	-0.297394	2.376794
-1429.459602	3.725071	2.386790
-1427.898207	4.489007	2.396787
-1425.966958	8.514324	2.406784
-1424.246356	4.084772	2.416781
-1422.249673	3.195304	2.426778
-1420.580197	5.393023	2.436774
-1418.568845	5.595443	2.446771
-1416.301377	4.163670	2.456768
-1414.979115	-1.763712	2.466765
-1412.774735	0.784174	2.476762
-1411.298626	-0.975645	2.486758
-1409.131743	4.680943	2.496755
-1407.350333	7.508134	2.506752
-1405.342070	11.486403	2.516749
-1403.382767	5.319666	2.526746
-1401.473678	4.355817	2.536742
-1399.706825	7.390612	2.546739
-1398.004404	5.365618	2.556736
-1396.019107	-0.882642	2.566733
-1393.779361	-2.504170	2.576730
-1391.947744	-2.047159	2.586726
-1390.470458	-4.001368	2.596723
-1388.433098	-0.902500	2.606720
-1386.688510	-0.546818	2.616717
-1384.837737	-6.944061	2.626714
-1382.731498	-5.337298	2.636710
-1381.189166	-0.504406	2.646707
-1378.939599	-0.711146	2.656704
-1376.958211	-4.255549	2.666701
-1375.421395	-0.743376	2.676698
-1373.363190	-4.401128	2.686694
-1371.736862	0.543064	2.696691
-1369.703257	2.447263	2.706688
-1367.618264	-2.515853	2.716685
-1366.124682	0.622714	2.726682
-1364.132245	3.878800	2.736678
-1362.214729	9.387456	2.746675
-1360.332438	4.703113	2.756672
-1358.427189	1.973033	2.766669
-1356.308100	-0.548111	2.776666
-1354.699731	5.024247	2.786662
-1352.658700	2.207699	2.796659
-1350.977709	4.245729	2.806656
-1349.123736	6.017645	2.816653
-1346.920735	-3.518124	2.826650
-1345.174740	-5.657425	2.836646
-1343.595078	4.474895	2.846643
-1341.502599	5.944950	2.856640
-1339.837541	-0.686226	2.866637
-1337.855783	-1.424808	2.876634
-1335.897045	4.623599	2.886630
-1333.928346	-1.928277	2.896627
-1332.100086	0.026192	2.906624
-1329.935599	1.571576	2.916621
-1328.372024	0.884147	2.926618
-1326.352011	3.630579	2.936614
-1324.422769	-0.423342	2.946611
-1322.758808	10.852900	2.956608
-1320.817071	6.302759	2.966605
-1319.191734	-2.141033	2.976602
-1317.101209	0.447276	2.986598
-1315.312978	8.353033	2.996595
-1313.552318	-0.665058	3.006592
-1311.544109	-7.821672	3.016589
-1309.797654	-6.251995	3.026586
-1307.728070	-2.294508	3.036582
-1305.789828	1.245046	3.046579
-1303.791284	1.574356	3.056576
-1302.112668	0.844848	3.066573
-1300.080845	1.014094	3.076570
-1298.495882	3.964394	3.086566
-1296.315186	8.739393	3.096563
-1294.713938	7.892795	3.106560
-1292.749074	3.215815	3.116557
-1290.681484	-4.073448	3.126554
-1288.922102	-4.522183	3.136550
-1287.291006	4.622982	3.146547
-1285.128804	-1.457709	3.156544
-1283.405840	0.756815	3.166541
-1281.289499	3.063125	3.176538
-1279.377220	7.380561	3.186534
-1277.661948	5.454651	3.196531
-1275.785917	-0.098644	3.206528
-1273.967577	5.909130	3.216525
-1271.875895	0.523435	3.226522
-1270.237927	-0.412708	3.236518
-1268.417542	5.064205	3.246515
-1266.455153	-3.818766	3.256512
-1264.867825	-0.147226	3.266509
-1262.764612	5.376011	3.276506
-1260.632549	0.294923	3.286502
-1258.838458	0.522777	3.296499
-1257.050101	-6.437556	3.306496
-1255.078449	0.287819	3.316493
-1253.169772	-0.360048	3.326490
-1251.515532	2.571305	3.336486
-1249.444242	0.477913	3.346483
-1247.693644	1.953816	3.356480
-1245.746267	1.604507	3.366477
-1243.838034	-1.833343	3.376474
-1241.842272	1.730222	3.386470
-1240.421885	0.461015	3.396467
-1238.476868	6.303281	3.406464
-1236.316463	9.092068	3.416461
-1234.302599	0.099827	3.426458
-1232.601758	2.586358	3.436454
-1230.910038	3.009041	3.446451
-1229.142733	6.493910	3.456448
-1227.026672	-2.884159	3.466445
-1224.889790	2.775834	3.476442
-1222.965943	0.642900	3.486438
-1221.475946	3.207389	3.496435
-1219.500323	3.524650	3.506432
-1217.758330	11.311573	3.516429
-1215.794286	4.766846	3.526426
-1213.907236	-3.864024	3.536422
-1212.243161	9.428652	3.546419
-1210.012336	2.939140	3.556416
-1208.076320	-2.598438	3.566413
-1206.422380	5.344689	3.576410
-1204.469351	7.179823	3.586406
-1202.577316	2.269826	3.596403
-1200.818347	5.506572	3.606400
-1198.923710	1.635132	3.616397
-1196.980157	3.302837	3.626394
-1195.126999	1.124393	3.636390
-1193.340668	5.926276	3.646387
-1191.484244	8.676900	3.656384
-1189.457285	-0.720042	3.666381
-1187.544098	3.079421	3.676378
-1185.707138	1.149896	3.686374
-1183.725813	4.687402	3.696371
-1181.868631	1.600408	3.706368
-1179.986639	-1.062650	3.716365
-1178.374716	-2.405097	3.726362
-1176.306173	1.454783	3.736358
-1174.413234	4.379582	3.746355
-1172.896833	3.319269	3.756352
-1170.513455	-0.516657	3.766349
-1168.872045	3.871054	3.776346
-1166.882297	3.616086	3.786342
-1165.082060	-1.028136	3.796339
-1163.507785	8.399386	3.806336
-1161.325307	4.162968	3.816333
-1159.394883	6.983886	3.826330
-1157.285699	2.413401	3.836326
-1155.893621	0.122433	3.846323
-1153.931068	-0.279755	3.856320
-1151.724367	3.134878	3.866317
-1149.873106	-1.307492	3.876314
-1148.253406	4.517426	3.886310
-1146.284735	6.050100	3.896307
-1144.473002	5.253617	3.906304
-1142.621145	3.741752	3.916301
-1140.645185	-0.737929	3.926298
-1138.842824	-1.918180	3.936294
-1137.306805	2.243251	3.946291
-1135.164865	-1.168743	3.956288
-1132.864390	-2.100248	3.966285
-1131.100006	2.956255	3.976282
-1129.326992	-1.348842	3.986278
-1127.727099	-1.884048	3.996275
-1125.823827	1.174930	4.006272
-1123.703527	3.880238	4.016269
-1121.845597	-0.252118	4.026266
-1119.818069	-0.273084	4.036262
-1118.327869	-1.101796	4.046259
-1116.396415	-1.314237	4.056256
-1114.436200	6.415755	4.066253
-1112.639061	0.221501	4.076250
-1110.685684	0.013453	4.086246
-1108.803965	10.373967	4.096243
-1106.899791	6.362121	4.106240
-1105.127445	8.475723	4.116237
-1103.054136	6.903201	4.126234
-1101.109945	4.899744	4.136230
-1099.355803	5.299906	4.146227
-1097.375051	5.595923	4.156224
-1096.022196	4.879196	4.166221
-1093.799675	-0.685177	4.176218
-1091.610246	-0.180950	4.186214
-1090.018404	3.611577	4.196211
-1088.117641	2.737737	4.206208
-1086.401338	-0.555602	4.216205
-1084.362755	-0.545147	4.226202
-1082.690669	-2.964548	4.236198
-1080.648502	-7.067918	4.246195
-1078.874612	-0.617072	4.256192
-1076.794645	0.621537	4.266189
-1074.914483	-1.845351	4.276186
-1073.301266	-0.702612	4.286182
-1070.881162	-5.899083	4.296179
-1069.390335	-4.368861	4.306176
-1067.591141	-2.917962	4.316173
-1065.589802	-2.424679	4.326170
-1063.744120	-6.348184	4.336166
-1061.968953	-3.930257	4.346163
-1060.068418	-5.059833	4.356160
-1058.400302	1.464793	4.366157
-1056.083827	0.437643	4.376154
-1054.369994	-5.825350	4.386150
-1052.450615	-2.228872	4.396147
-1050.668462	-2.804231	4.406144
-1048.826577	-1.878052	4.416141
-1046.796713	-1.244049	4.426138
-1044.792251	-0.088074	4.436134
-1043.005133	-3.119544	4.446131
-1041.232670	1.375199	4.456128
-1039.408191	0.673077	4.466125
-1037.327456	-0.741098	4.476122
-1035.591249	-0.058540	4.486118
-1033.893788	7.858818	4.496115
-1031.901242	5.298196	4.506112
-1030.126092	-3.857818	4.516109
-1028.369348	2.646342	4.526106
-1026.064039	0.957833	4.536102
-1024.333755	-0.193435	4.546099
-1022.445302	3.104850	4.556096
-1020.580540	1.867339	4.566093
-1018.496942	-0.973103	4.576090
-1016.705331	6.910264	4.586086
-1014.958771	0.912067	4.596083
-1013.060853	1.115611	4.606080
-1011.300703	2.812805	4.616077
-1009.441928	3.529467	4.626074
-1007.581406	-3.265389	4.636070
-1005.720410	-2.152754	4.646067
-1003.583285	0.133122	4.656064
-1001.627975	-2.955216	4.666061
-1000.108350	-0.913225	4.676058
-998.183691	-2.867683	4.686054
-995.947414	1.489765	4.696051
-994.481365	1.391326	4.706048
-992.537947	3.035542	4.716045
-990.400584	4.064519	4.726042
-988.825356	4.253369	4.736038
-986.767932	2.588749	4.746035
-984.756500	5.636868	4.756032
-983.251767	2.326906	4.766029
-981.351354	1.909535	4.776026
-979.147187	2.602568	4.786022
-977.519978	1.534134	4.796019
-975.778705	-1.788384	4.806016
-973.609913	-6.243503	4.816013
-971.616637	-3.596691	4.826010
-969.976829	-2.753402	4.836006
-968.032690	-5.323598	4.846003
-966.226800	4.070196	4.856000
-964.268141	2.898243	4.865997
-962.411197	6.185828	4.875994
-960.382752	-1.243757	4.885990
-958.844049	4.529517	4.895987
-957.084095	10.093728	4.905984
-955.351418	6.714174	4.915981
-953.047092	3.576381	4.925978
-950.903089	2.895868	4.935974
-948.885168	6.773530	4.945971
-947.574153	4.312480	4.955968
-945.680846	1.954118	4.965965
-943.490465	-0.086997	4.975962
-941.888658	-1.261874	4.985958
-940.082179	1.659578	4.995955
-937.903744	-1.777026	5.005952
-935.957004	4.712622	5.015949
-934.227151	4.810467	5.025946
-932.512083	1.571118	5.035942
-930.486963	-3.795752	5.045939
-928.753494	4.433308	5.055936
-926.958274	6.279701	5.065933
-924.739165	4.148745	5.075930
-922.898525	2.313572	5.085926
-921.257913	0.417223	5.095923
-919.330502	5.885213	5.105920
-917.646901	2.751960	5.115917
-915.364518	5.643132	5.125914
-913.552707	3.499936	5.135910
-911.613990	-0.623073	5.145907
-909.861566	-1.089359	5.155904
-908.119077	2.486576	5.165901
-905.998784	5.709998	5.175898
-904.539263	2.312572	5.185894
-902.474074	4.412671	5.195891
-900.360400	10.439863	5.205888
-898.677588	8.871527	5.215885
-896.615331	11.872126	5.225882
-894.512930	8.116126	5.235878
-893.272899	4.771167	5.245875
-891.172769	0.854478	5.255872
-889.266050	5.203141	5.265869
-887.516719	6.197932	5.275866
-885.403826	-0.956141	5.285862
-883.528517	0.774847	5.295859
-881.626979	-1.589517	5.305856
-880.137408	1.464754	5.315853
-877.911539	1.350708	5.325850
-876.249190	2.987850	5.335846
-874.194209	1.590566	5.345843
-872.073116	1.985921	5.355840
-870.493310	2.327281	5.365837
-868.858652	1.859325	5.375834
-866.472655	11.147840	5.385830
-864.661107	6.749924	5.395827
-863.125586	1.876649	5.405824
-861.101162	6.568109	5.415821
-859.286433	7.288775	5.425818
-857.281046	1.617213	5.435814
-855.344746	3.654272	5.445811
-853.525497	9.927528	5.455808
-851.864891	6.081134	5.465805
-850.062158	11.663857	5.475802
-847.827771	6.794138	5.485798
-846.029043	8.704772	5.495795
-844.417698	8.407933	5.505792
-842.556377	7.663755	5.515789
-840.407806	7.737369	5.525786
-838.337822	0.432295	5.535782
-836.588002	6.634554	5.545779
-834.885288	-2.956608	5.555776
-832.950275	7.675119	5.565773
-831.100048	3.108409	5.575770
-829.068837	5.641912	5.585766
-827.008417	2.042687	5.595763
-825.492200	1.295264	5.605760
-824.172795	2.742519	5.615757
-821.827739	5.290600	5.625754
-819.730606	12.572655	5.635750
-817.813425	5.115171	5.645747
-816.205708	3.475210	5.655744
-814.074899	2.864826	5.665741
-812.484661	4.436170	5.675738
-810.311612	2.570057	5.685734
-808.614049	2.527889	5.695731
-806.661608	4.548199	5.705728
-804.700728	9.796199	5.715725
-802.806815	7.213634	5.725722
-801.143378	8.654862	5.735718
-799.309191	4.502856	5.745715
-797.321596	1.384255	5.755712
-795.518654	0.423650	5.765709
-793.580150	1.741968	5.775706
-791.628796	0.833436	5.785702
-789.843432	9.425384	5.795699
-787.872444	5.884696	5.805696
-786.020718	1.241988	5.815693
-784.306690	3.764646	5.825690
-782.220089	3.344519	5.835686
-780.273432	8.582182	5.845683
-778.506608	4.950971	5.855680
-776.806670	8.082220	5.865677
-774.496537	5.851587	5.875674
-772.745302	1.381270	5.885670
-771.274394	-1.035765	5.895667
-769.262072	2.037667	5.905664
-767.346039	7.270761	5.915661
-765.524865	2.661372	5.925658
-763.501296	-1.340869	5.935654
-761.517013	0.154902	5.945651
-759.825736	1.995931	5.955648
-758.040747	4.440950	5.965645
-756.139072	5.870979	5.975642
-753.923377	2.259630	5.985638
-752.281747	-2.870542	5.995635
-750.428853	7.457009	6.005632
-748.597502	3.763401	6.015629
-746.449964	6.516815	6.025626
-744.869686	-0.154119	6.035622
-743.261432	7.354562	6.045619
-741.030441	10.397811	6.055616
-739.135672	1.770777	6.065613
-737.366875	9.511182	6.075610
-735.346487	1.153032	6.085606
-733.614112	1.468523	6.095603
-731.521282	5.129139	6.105600
-729.854635	3.083491	6.115597
-727.660809	3.779993	6.125594
-725.880964	6.080593	6.135590
-724.135927	-2.765665	6.145587
-722.350213	0.549289	6.155584
-720.247320	2.758793	6.165581
-718.530836	-0.820118	6.175578
-716.970939	0.541398	6.185574
-714.698420	2.810645	6.195571
-712.461489	-2.408315	6.205568
-711.011018	2.577108	6.215565
-709.321404	6.698507	6.225562
-707.242935	6.890816	6.235558
-705.335972	3.886229	6.245555
-703.743800	4.533629	6.255552
-701.620761	4.949353	6.265549
-699.555690	-0.193185	6.275546
-697.704443	3.929236	6.285542
-695.958615	4.288396	6.295539
-694.211268	4.839952	6.305536
-692.491440	6.545413	6.315533
-690.436569	3.548784	6.325530
-688.282152	4.704791	6.335526
-686.637661	-1.057394	6.345523
-684.976962	-0.604095	6.355520
-682.867455	-5.046330	6.365517
-680.728213	2.074384	6.375514
-678.873789	-1.902341	6.385510
-676.984945	-3.882400	6.395507
-675.495191	1.207299	6.405504
-673.648982	2.410987	6.415501
-671.735032	1.857487	6.425498
-669.576539	-0.238287	6.435494
-667.562751	-3.163593	6.445491
-665.947237	-0.293518	6.455488
-664.430249	-1.841511	6.465485
-662.153237	2.380284	6.475482
-660.196906	1.820022	6.485478
-658.376244	-0.989155	6.495475
-656.208257	-1.145850	6.505472
-654.795521	-0.766599	6.515469
-653.005884	-4.423470	6.525466
-651.059203	-6.144322	6.535462
-649.120569	-5.470134	6.545459
-647.079210	-2.957040	6.555456
-645.293694	-6.359028	6.565453
-643.300624	-0.702336	6.575450
-641.610118	-0.297980	6.585446
-639.743521	0.258248	6.595443
-637.923974	-7.813518	6.605440
-636.182234	-3.744607	6.615437
-634.216616	1.891216	6.625434
-632.107861	5.974130	6.635430
-630.317621	0.641866	6.645427
-628.257024	1.514487	6.655424
-626.351881	0.543997	6.665421
-624.972774	3.155020	6.675418
-622.875512	-0.959936	6.685414
-620.874371	2.827539	6.695411
-619.127842	-1.248750	6.705408
-616.997327	-0.243600	6.715405
-615.516452	-1.582104	6.725402
-613.528484	0.187950	6.735398
-611.573322	-3.654814	6.745395
-609.751630	-0.853955	6.755392
-607.879007	1.101904	6.765389
-605.853475	0.268517	6.775386
-604.117114	-1.635020	6.785382
-602.025561	3.404382	6.795379
-600.248876	3.234457	6.805376
-598.340724	2.010869	6.815373
-596.752898	6.287565	6.825370
-594.607040	10.435643	6.835366
-592.817003	4.953430	6.845363
-590.993800	5.859271	6.855360
-588.938311	4.329514	6.865357
-586.933709	-0.035882	6.875354
-585.450821	-2.682096	6.885350
-583.454717	3.446287	6.895347
-581.514529	0.817027	6.905344
-579.676265	-1.169089	6.915341
-577.901358	0.579764	6.925338
-575.851349	-2.182301	6.935334
-573.715234	1.245750	6.945331
-572.211803	-3.994867	6.955328
-570.518146	-0.827724	6.965325
-568.644832	4.619214	6.975322
-566.373390	1.335454	6.985318
-564.549365	-0.910490	6.995315
-562.646496	-0.731058	7.005312
-560.792355	4.395254	7.015309
-558.977689	-4.477810	7.025306
-557.221454	-1.093278	7.035302
-555.486802	3.025779	7.045299
-553.342001	-2.513071	7.055296
-551.562245	-5.110365	7.065293
-549.758130	-0.266589	7.075290
-547.720657	-6.760950	7.085286
-545.761753	-3.716686	7.095283
-544.068456	-3.181650	7.105280
-542.142666	5.800193	7.115277
-540.235486	4.862604	7.125274
-538.437482	-1.726138	7.135270
-536.452508	-1.043468	7.145267
-534.425382	2.296235	7.155264
-532.700279	6.565261	7.165261
-531.392916	-0.049324	7.175258
-529.097319	2.898546	7.185254
-526.995123	-0.225509	7.195251
-524.992115	-0.752063	7.205248
-523.234014	-4.433806	7.215245
-521.647823	-6.155399	7.225242
-519.884814	-2.432437	7.235238
-517.495893	-2.685874	7.245235
-515.582020	-2.144994	7.255232
-514.055321	-2.238611	7.265229
-512.032403	-4.314170	7.275226
-510.306476	0.381068	7.285222
-508.622058	-8.335364	7.295219
-506.648491	-10.622516	7.305216
-504.315073	-6.455365	7.315213
-502.805879	-1.993936	7.325210
-500.876584	1.363001	7.335206
-498.654325	-0.750700	7.345203
-496.865080	0.629599	7.355200
-495.531412	-2.205895	7.365197
-493.470846	0.676912	7.375194
-491.207091	-0.083895	7.385190
-489.720968	0.154257	7.395187
-487.634126	2.769180	7.405184
-485.921732	1.360622	7.415181
-483.916775	0.056925	7.425178
-482.274575	-0.838300	7.435174
-480.088679	-2.802488	7.445171
-478.087376	1.564579	7.455168
-476.833569	-0.678659	7.465165
-474.811703	4.627788	7.475162
-472.409754	1.879079	7.485158
-470.935854	8.640452	7.495155
-469.198692	6.981626	7.505152
-467.023822	7.270859	7.515149
-464.954844	6.703819	7.525146
-463.460204	3.105244	7.535142
-461.422261	8.998103	7.545139
-459.411990	1.436012	7.555136
-457.746943	-0.356556	7.565133
-455.803045	0.346951	7.575130
-454.125131	2.532981	7.585126
-451.680795	1.416523	7.595123
-450.292791	-2.987672	7.605120
-448.547887	0.046637	7.615117
-446.353943	-2.180920	7.625114
-444.639714	-0.633860	7.635110
-442.736855	-8.908277	7.645107
-440.816834	-4.956108	7.655104
-438.747541	-2.916252	7.665101
-437.178214	-2.193970	7.675098
-435.295024	4.710496	7.685094
-433.252267	10.127335	7.695091
-431.204743	-0.256036	7.705088
-429.587530	0.738087	7.715085
-427.736728	-1.027279	7.725082
-425.705028	1.605979	7.735078
-423.804622	1.154316	7.745075
-422.528963	6.006788	7.755072
-420.144735	0.740880	7.765069
-418.267043	4.022440	7.775066
-416.313409	8.101903	7.785062
-414.574635	3.853301	7.795059
-412.654135	4.001615	7.805056
-410.672276	2.407973	7.815053
-408.845140	7.327140	7.825050
-406.764965	7.189429	7.835046
-405.167717	3.149753	7.845043
-403.620575	-5.040998	7.855040
-401.389227	-3.664899	7.865037
-399.588314	-1.951642	7.875034
-397.512020	-0.918689	7.885030
-395.850676	1.611092	7.895027
-394.137284	1.719856	7.905024
-391.904097	-3.147687	7.915021
-390.122746	3.752551	7.925018
-388.289952	-1.936878	7.935014
-386.220390	-3.992938	7.945011
-384.651413	3.132271	7.955008
-382.635259	-2.957493	7.965005
-380.574379	5.810290	7.975002
-378.778223	4.066317	7.984998
-376.987856	1.271657	7.994995
-375.144192	-0.893595	8.004992
-373.230114	3.686445	8.014989
-371.349535	1.134763	8.024986
-369.799274	4.838125	8.034982
-367.800995	0.287590	8.044979
-365.501425	2.748656	8.054976
-363.758031	-3.796510	8.064973
-362.290746	-1.200985	8.074970
-360.146054	8.022400	8.084966
-358.096910	0.585237	8.094963
-356.526462	1.056333	8.104960
-354.445907	4.049761	8.114957
-352.739086	3.828013	8.124954
-350.492790	8.505041	8.134950
-348.654356	2.492622	8.144947
-346.919394	1.660050	8.154944
-345.259161	1.902076	8.164941
-343.405985	2.016982	8.174938
-341.561302	2.712737	8.184934
-339.496356	2.586989	8.194931
-337.530207	9.189342	8.204928
-335.554825	5.544095	8.214925
-334.041658	8.135472	8.224922
-332.051972	8.787560	8.234918
-330.096314	8.025562	8.244915
-328.063659	5.312261	8.254912
-326.300332	9.995359	8.264909
-324.599012	11.257190	8.274906
-322.883883	8.889855	8.284902
-320.537080	2.616296	8.294899
-318.632633	5.718398	8.304896
-316.893549	5.398365	8.314893
-315.129088	3.656340	8.324890
-313.527202	1.652891	8.334886
-311.454792	1.975990	8.344883
-309.286880	1.925414	8.354880
-307.600493	0.246385	8.364877
-305.921635	-8.491143	8.374874
-303.476680	0.985953	8.384870
-301.860471	-4.008820	8.394867
-299.890415	2.449250	8.404864
-298.369282	-6.414682	8.414861
-296.514252	7.912538	8.424858
-294.604974	0.516698	8.434854
-292.375852	4.337547	8.444851
-290.453554	-0.496072	8.454848
-288.867952	1.654285	8.464845
-287.216412	-3.570337	8.474842
-285.417627	-2.455093	8.484838
-283.214878	-2.845955	8.494835
-280.878726	-0.559598	8.504832
-279.396765	2.152063	8.514829
-277.558856	2.117872	8.524826
-275.925292	-0.327992	8.534822
-273.686199	7.361414	8.544819
-271.931463	5.183589	8.554816
-270.267883	0.536548	8.564813
-268.080085	7.143058	8.574810
-266.519628	2.154045	8.584807
-264.244041	-2.036446	8.594803
-262.328144	-2.727305	8.604800
-260.467023	-0.565640	8.614797
-258.889484	2.006037	8.624794
-257.122807	4.234886	8.634791
-255.045274	1.825546	8.644787
-252.986342	0.507108	8.654784
-251.415919	-2.043929	8.664781
-249.648391	0.281108	8.674778
-247.349734	-0.185031	8.684775
-245.663350	-1.908228	8.694771
-243.943637	-2.281961	8.704768
-242.054364	-5.373372	8.714765
-239.987841	-1.851796	8.724762
-238.080425	0.964099	8.734759
-236.289263	-0.174216	8.744755
-234.404209	0.821505	8.754752
-232.316256	-10.671886	8.764749
-230.510136	0.190975	8.774746
-228.808640	-0.664594	8.784743
-226.900685	-3.359487	8.794739
-224.928071	-4.032525	8.804736
-223.413816	-6.122986	8.814733
-221.139665	-2.091354	8.824730
-219.464172	-2.854342	8.834727
-217.425123	-0.365765	8.844723
-215.793074	-5.573019	8.854720
-213.634765	-1.060245	8.864717
-211.751601	-1.652679	8.874714
-210.011583	4.892712	8.884711
-208.370038	-3.459845	8.894707
-206.353221	0.882879	8.904704
-204.463005	-4.067138	8.914701
-202.703513	-3.436630	8.924698
-200.686150	1.442872	8.934695
-198.817334	1.885405	8.944691
-197.009904	-8.295257	8.954688
-194.858053	-0.942391	8.964685
-192.867255	-5.002104	8.974682
-191.380169	1.297864	8.984679
-189.526655	-5.735303	8.994675
-187.577036	-5.293025	9.004672
-185.482625	-5.720195	9.014669
-183.778355	-4.975068	9.024666
-181.909749	-5.091456	9.034663
-180.133588	-4.580437	9.044659
-178.030958	-11.113329	9.054656
-176.363474	-1.393602	9.064653
-174.656003	-6.557601	9.074650
-172.305218	-6.285119	9.084647
-170.992575	-1.965791	9.094643
-168.795286	1.366029	9.104640
-166.895830	-0.735337	9.114637
-164.722992	-5.929378	9.124634
-162.859542	-2.770079	9.134631
-161.384892	0.656533	9.144627
-159.245987	-9.777531	9.154624
-157.450193	-5.225807	9.164621
-155.671377	-8.247419	9.174618
-153.746728	-7.497961	9.184615
-151.802940	-4.839385	9.194611
-150.006898	1.956069	9.204608
-148.360466	-4.047677	9.214605
-146.242030	-7.848236	9.224602
-144.389173	-3.064019	9.234599
-142.701447	0.080702	9.244595
-140.359885	-3.344915	9.254592
-138.639177	-1.942355	9.264589
-136.916044	0.759337	9.274586
-135.023989	5.614682	9.284583
-133.005859	-1.468400	9.294579
-131.091336	-4.641127	9.304576
-129.497554	5.267250	9.314573
-127.564028	4.249989	9.324570
-125.281956	6.156695	9.334567
-123.699300	3.390619	9.344563
-122.061217	-5.529776	9.354560
-120.082138	-0.077232	9.364557
-117.980789	11.573923	9.374554
-116.045466	6.848883	9.384551
-114.507300	6.205776	9.394547
-112.552237	0.051751	9.404544
-110.603718	3.855965	9.414541
-108.694596	-0.530138	9.424538
-106.984029	10.678095	9.434535
-104.999560	5.829955	9.444531
-102.983479	3.768452	9.454528
-101.213317	0.129288	9.464525
-99.177275	-1.213792	9.474522
-97.517354	-2.012108	9.484519
-95.581090	3.398340	9.494515
-94.029272	7.126907	9.504512
-91.844685	-0.497456	9.514509
-89.865155	3.710790	9.524506
-88.362589	4.347634	9.534503
-86.315768	6.730873	9.544499
-84.171098	1.719819	9.554496
-82.332916	5.331653	9.564493
-80.475072	0.191092	9.574490
-78.630466	5.264061	9.584487
-77.133315	5.647557	9.594483
-74.705187	2.498726	9.604480
-73.034325	4.109819	9.614477
-71.145355	1.416492	9.624474
-69.158063	4.210309	9.634471
-67.573281	5.399334	9.644467
-65.803845	-1.375592	9.654464
-63.521472	1.664850	9.664461
-61.701631	3.842732	9.674458
-60.115066	6.171518	9.684455
-58.100020	0.517983	9.694451
-56.216122	2.118788	9.704448
-54.130215	7.795938	9.714445
-52.427750	6.389265	9.724442
-50.500928	8.557985	9.734439
-48.633222	3.965367	9.744435
-46.581668	1.328230	9.754432
-44.962024	5.699718	9.764429
-43.233316	4.246232	9.774426
-41.128386	-0.060527	9.784423
-39.439269	4.178299	9.794419
-37.724590	5.551893	9.804416
-35.455737	0.142109	9.814413
-33.482144	-2.695745	9.824410
-31.688115	0.901065	9.834407
-29.947806	5.605434	9.844403
-28.311670	2.594035	9.854400
-26.142958	2.096727	9.864397
-24.280281	0.691360	9.874394
-22.352147	1.481422	9.884391
-20.312603	6.523344	9.894387
-18.513219	1.036876	9.904384
-16.832396	2.205877	9.914381
-14.860021	1.626208	9.924378
-12.965616	-1.889024	9.934375
-11.217188	-1.705048	9.944371
-9.316305	1.108918	9.954368
-7.628800	-1.492223	9.964365
-5.868637	15.623138	9.974362
-4.542792	35.774754	9.984359
-2.854461	67.854855	9.994355
-1.291301	111.639715	10.004352
0.000000	145.058135	10.009357
0.464333	175.795662	10.014362
1.066586	191.370411	10.019367
1.817651	218.488800	10.024371
1.687213	249.267732	10.029376
2.320720	252.062190	10.034381
2.680135	267.723065	10.039386
2.816071	277.579914	10.044391
2.822660	276.031919	10.049395
2.839770	289.403972	10.054400
3.301732	280.544838	10.059405
3.113505	292.719573	10.064410
3.393220	279.773495	10.069415
3.453615	274.471506	10.074419
2.869069	269.906348	10.079424
2.718526	271.892274	10.084429
3.308365	285.307018	10.089434
3.153003	289.657664	10.094439
3.581395	298.332427	10.099443
3.222737	304.563768	10.104448
3.415325	305.121386	10.109453
3.054492	303.538949	10.114458
3.132303	303.944556	10.119463
3.573889	296.331353	10.124467
3.518820	316.606512	10.129472
3.852390	309.709151	10.134477
3.893297	310.480205	10.139482
3.796855	314.436668	10.144487
3.882057	317.223973	10.149491
3.724551	314.945178	10.154496
3.775267	316.902164	10.159501
3.556194	327.667261	10.164506
3.729912	321.017752	10.169511
4.011675	317.315809	10.174515
3.932923	316.689785	10.179520
3.852795	319.382031	10.184525
3.725795	319.025488	10.189530
4.151215	326.035409	10.194535
4.433422	326.599235	10.199539
4.151053	328.338102	10.204544
4.530034	320.533014	10.209549
4.013987	334.385979	10.214554
4.006065	330.135701	10.219559
4.318952	333.591622	10.224563
3.859494	337.006724	10.229568
4.101753	333.904038	10.234573
4.309300	348.832255	10.239578
4.531035	363.250422	10.244583
4.825097	366.838669	10.249587
4.752243	369.619655	10.254592
4.774294	368.099147	10.259597
4.835555	373.831435	10.264602
4.737343	377.999518	10.269607
4.891176	365.682174	10.274611
4.904611	374.746459	10.279616
4.769492	370.642620	10.284621
5.033969	368.444750	10.289626
5.091308	382.587945	10.294631
5.063604	376.213400	10.299635
4.844999	382.564367	10.304640
5.085760	380.501172	10.309645
4.913438	389.558823	10.314650
5.124859	391.212629	10.319655
5.397664	392.445041	10.324659
5.033388	384.960328	10.329664
5.091553	384.273037	10.334669
5.112866	394.980918	10.339674
4.950069	399.482600	10.344679
4.964905	387.908109	10.349683
5.029834	394.254861	10.354688
5.256220	397.923300	10.359693
5.491030	402.408875	10.364698
5.148748	403.570652	10.369703
5.605597	412.346606	10.374707
5.524375	421.632609	10.379712
5.548297	419.747504	10.384717
5.530263	428.348464	10.389722
5.599504	420.755161	10.394727
5.942053	433.591290	10.399731
5.801243	451.688238	10.404736
6.112320	451.720735	10.409741
6.157594	452.047954	10.414746
5.815680	453.884647	10.419751
6.137434	462.431431	10.424755
6.294427	466.312816	10.429760
6.434084	460.663786	10.434765
6.145872	460.138977	10.439770
6.316454	463.183943	10.444775
6.377101	468.611998	10.449779
6.222158	472.320777	10.454784
6.091137	463.240707	10.459789
5.941940	475.527647	10.464794
6.232961	468.914557	10.469799
6.304818	473.405643	10.474803
6.475069	472.014459	10.479808
6.407902	467.412449	10.484813
6.548619	478.673811	10.489818
6.584070	475.367526	10.494823
6.552817	479.307327	10.499827
6.564164	503.882198	10.504832
6.866564	497.313014	10.509837
6.870161	502.767529	10.514842
6.677686	510.260892	10.519847
6.750190	500.192650	10.524851
6.777349	509.450384	10.529856
6.803793	502.508874	10.534861
6.710745	509.961145	10.539866
6.725799	507.932355	10.544871
7.007602	521.461110	10.549875
6.865636	525.259301	10.554880
7.353493	531.503960	10.559885
7.223384	537.087053	10.564890
7.372748	540.185885	10.569895
7.453851	549.187443	10.574899
7.002533	546.424010	10.579904
7.637055	551.421499	10.584909
7.708616	548.956311	10.589914
7.607465	539.056097	10.594919
7.848028	541.004911	10.599923
7.705172	546.150045	10.604928
8.035396	545.572327	10.609933
8.017701	543.783735	10.614938
7.701062	550.524171	10.619943
7.891886	548.826906	10.624947
7.881142	552.555286	10.629952
7.995008	545.246554	10.634957
7.549442	553.516787	10.639962
7.733637	545.815192	10.644967
8.194233	551.395541	10.649971
7.980264	560.589259	10.654976
7.969540	550.707732	10.659981
8.218640	561.942410	10.664986
8.058524	562.376511	10.669991
8.229741	570.635115	10.674995
8.336679	587.404268	10.680000
8.466735	581.490201	10.685005
8.371517	583.587201	10.690010
8.219166	590.772989	10.695015
8.540247	591.705964	10.700019
8.385627	583.810793	10.705024
8.599433	590.501337	10.710029
8.494221	589.223469	10.715034
8.349645	587.097119	10.720039
8.807013	587.696100	10.725043
8.556089	593.626510	10.730048
8.757600	579.442040	10.735053
8.618726	590.896326	10.740058
8.338496	601.726576	10.745063
8.720889	604.818218	10.750067
8.959999	621.315577	10.755072
9.175704	618.956705	10.760077
9.008606	626.264719	10.765082
9.253746	624.984587	10.770087
9.180033	622.891086	10.775091
9.087846	635.208494	10.780096
9.314653	629.608580	10.785101
9.350351	630.867792	10.790106
9.365389	630.099053	10.795111
9.635058	638.565934	10.800115
9.519727	637.803796	10.805120
9.469581	635.802735	10.810125
9.666991	636.476300	10.815130
9.457182	644.302100	10.820135
9.574396	646.735834	10.825139
9.465608	643.468288	10.830144
9.767829	634.711696	10.835149
9.186367	648.886071	10.840154
9.388976	647.854010	10.845159
9.678594	648.317314	10.850163
9.307151	647.969786	10.855168
9.746372	662.489189	10.860173
9.824667	663.400965	10.865178
9.844802	668.488604	10.870183
10.146667	678.790800	10.875187
10.019981	687.825586	10.880192
10.143629	680.512072	10.885197
9.992158	682.659062	10.890202
10.014388	684.571752	10.895207
10.372343	674.084098	10.900211
10.201214	687.496003	10.905216
10.304255	678.074094	10.910221
10.243465	684.792708	10.915226
10.079981	682.918535	10.920231
10.288679	692.415530	10.925235
10.069110	724.903447	10.930240
10.508644	714.262393	10.935245
10.626615	715.551071	10.940250
10.468291	718.203819	10.945255
10.877194	718.174980	10.950259
10.516778	715.928485	10.955264
10.838277	721.174670	10.960269
10.675093	716.376569	10.965274
10.597871	722.066423	10.970279
10.793433	724.307888	10.975283
10.534295	731.565975	10.980288
11.066788	726.988095	10.985293
10.744016	724.492726	10.990298
10.928465	748.510506	10.995303
11.406298	750.211755	11.000307
11.333984	753.404341	11.005312
11.214540	755.167737	11.010317
11.381910	760.621460	11.015322
11.177921	755.921324	11.020327
11.419698	756.038999	11.025331
11.529598	764.619753	11.030336
11.504239	758.394487	11.035341
11.201249	758.021845	11.040346
11.047905	758.065336	11.045351
11.345489	755.105136	11.050355
11.706070	766.569791	11.055360
11.634221	760.415022	11.060365
11.296672	758.086020	11.065370
11.596629	765.109858	11.070375
11.571107	761.600329	11.075379
11.489753	776.019937	11.080384
12.326052	779.021871	11.085389
12.031415	794.385485	11.090394
12.102634	782.565127	11.095399
12.265053	780.706774	11.100403
11.944774	783.071528	11.105408
11.908406	772.537880	11.110413
11.984398	795.459626	11.115418
11.749596	797.940069	11.120423
12.290573	796.563847	11.125427
11.982298	800.492722	11.130432
12.209172	802.207195	11.135437
12.500259	795.515093	11.140442
12.026833	797.828577	11.145447
12.121460	801.156985	11.150451
12.147057	807.844530	11.155456
12.224578	818.573722	11.160461
12.376512	825.195390	11.165466
12.460845	835.478772	11.170471
13.034480	834.007446	11.175475
12.397621	837.037762	11.180480
13.175449	833.581447	11.185485
12.715906	832.139281	11.190490
12.912604	830.195024	11.195495
12.930259	830.398913	11.200499
12.682235	835.625583	11.205504
13.051631	838.676768	11.210509
12.904730	842.535756	11.215514
12.973213	841.034604	11.220519
13.191693	835.715083	11.225523
13.111517	837.238818	11.230528
13.199008	832.862780	11.235533
13.066559	838.279190	11.240538
12.799672	846.161515	11.245543
13.317422	844.183397	11.250547
13.159330	846.478134	11.255552
13.621401	852.321738	11.260557
13.214312	876.337877	11.265562
13.452407	870.930051	11.270567
13.888794	866.309105	11.275571
13.732150	875.050718	11.280576
13.685325	876.657454	11.285581
13.776437	881.610835	11.290586
13.859400	872.985274	11.295591
13.603138	872.173055	11.300595
13.678701	879.697978	11.305600
14.059368	874.317879	11.310605
13.847178	874.629397	11.315610
13.916993	872.345797	11.320615
14.145553	869.040164	11.325619
13.795650	879.246169	11.330624
13.778456	884.104853	11.335629
13.717333	876.511603	11.340634
13.818959	884.052874	11.345639
13.849366	874.811170	11.350643
13.743639	884.183385	11.355648
14.129953	898.642071	11.360653
14.125810	899.775186	11.365658
13.878846	913.270362	11.370663
14.527379	899.558376	11.375667
14.132111	909.363173	11.380672
14.234054	907.782555	11.385677
14.324831	914.477101	11.390682
14.446416	912.765605	11.395687
14.523674	911.550075	11.400691
14.870205	938.141353	11.405696
15.038828	936.764579	11.410701
14.718942	923.708545	11.415706
14.575926	921.678098	11.420711
14.959563	934.023953	11.425715
14.915249	946.639943	11.430720
15.061762	947.898855	11.435725
15.042635	948.278938	11.440730
15.297066	939.111859	11.445735
15.419406	937.491711	11.450739
14.827418	933.011111	11.455744
15.352054	930.486211	11.460749
15.384896	936.075008	11.465754
15.076665	931.284199	11.470759
15.331010	935.828331	11.475763
15.351796	951.040866	11.480768
15.149952	945.550205	11.485773
15.224338	946.218174	11.490778
15.326352	953.172742	11.495783
15.717764	947.568532	11.500787
15.462576	950.063292	11.505792
15.695285	939.240580	11.510797
15.497450	949.897083	11.515802
15.204572	953.943401	11.520807
15.523349	942.343648	11.525811
15.351009	946.470095	11.530816
15.747326	951.953612	11.535821
15.626016	970.119062	11.540826
15.774766	977.865772	11.545831
15.845888	977.307286	11.550835
15.597652	974.205422	11.555840
16.327352	974.562273	11.560845
15.974609	975.482888	11.565850
15.908307	983.143254	11.570855
16.244561	980.866820	11.575859
16.212910	978.000093	11.580864
16.190743	973.108445	11.585869
16.094044	982.379138	11.590874
16.024610	986.142223	11.595879
16.552123	975.563438	11.600883
16.200918	990.201354	11.605888
16.590997	1000.201890	11.610893
16.951688	1010.285975	11.615898
16.519435	999.575586	11.620903
16.561380	988.903123	11.625907
16.428255	991.635487	11.630912
16.789346	1009.754798	11.635917
16.853785	1011.913923	11.640922
17.068547	1007.300682	11.645927
17.077278	1002.508185	11.650931
16.904108	996.777944	11.655936
17.008862	983.533479	11.660941
17.012268	983.105652	11.665946
16.929539	987.258034	11.670951
17.149873	996.423760	11.675955
17.130864	1004.031647	11.680960
17.062154	1009.165905	11.685965
17.049326	1017.285369	11.690970
17.132277	1012.384828	11.695975
17.360000	1005.417284	11.700979
17.347532	1020.398631	11.705984
17.209496	1013.287552	11.710989
17.228546	1018.785531	11.715994
17.217622	1017.847433	11.720999
17.453413	1017.174364	11.726003
17.463164	1014.539956	11.731008
17.610296	1004.989367	11.736013
17.367992	1012.648644	11.741018
17.221272	1012.522329	11.746023
17.631865	1016.136313	11.751027
17.249252	1035.148628	11.756032
17.901530	1034.305042	11.761037
18.038576	1042.506281	11.766042
18.044720	1042.868142	11.771047
17.955328	1042.299770	11.776051
17.933050	1046.218579	11.781056
18.063241	1040.114265	11.786061
18.028687	1045.348754	11.791066
17.971762	1051.144318	11.796071
18.217065	1039.765961	11.801075
18.245404	1047.239362	11.806080
18.179733	1039.127099	11.811085
18.281208	1050.604918	11.816090
18.215089	1043.170876	11.821095
18.394445	1039.117623	11.826099
18.337273	1046.522654	11.831104
18.728760	1044.522067	11.836109
18.151648	1050.813798	11.841114
18.385617	1038.088831	11.846119
18.606103	1044.559303	11.851123
18.278089	1056.152152	11.856128
18.297574	1048.645313	11.861133
18.454239	1050.577614	11.866138
18.521888	1067.629580	11.871143
18.792867	1081.546975	11.876147
18.682322	1078.460188	11.881152
18.781203	1071.646427	11.886157
18.818496	1086.543417	11.891162
18.753526	1081.070301	11.896167
19.272142	1074.110738	11.901171
19.184833	1080.262853	11.906176
19.347673	1075.310122	11.911181
19.163216	1082.972826	11.916186
19.094701	1080.402145	11.921191
19.198615	1079.544295	11.926195
18.884685	1080.906623	11.931200
19.413219	1077.439548	11.936205
19.371963	1087.888234	11.941210
19.177496	1084.791963	11.946215
19.662968	1082.372643	11.951219
19.625165	1088.825190	11.956224
19.527651	1079.574583	11.961229
19.654072	1084.121817	11.966234
19.474064	1076.401542	11.971239
19.486238	1096.022815	11.976243
19.612092	1107.603245	11.981248
19.578703	1104.898423	11.986253
19.709466	1107.806360	11.991258
19.888439	1110.510258	11.996263
20.033157	1112.028906	12.001267
19.879232	1114.172406	12.006272
20.043054	1110.201255	12.011277
20.038352	1109.712422	12.016282
20.123353	1107.881359	12.021287
20.408170	1114.418092	12.026291
20.352318	1117.352641	12.031296
20.320131	1107.888938	12.036301
20.207758	1097.692060	12.041306
20.008715	1095.355104	12.046311
20.110544	1089.013996	12.051315
19.775839	1087.282207	12.056320
19.862863	1081.150853	12.061325
19.847906	1097.432998	12.066330
19.857006	1088.377502	12.071335
19.951284	1110.762190	12.076339
19.641738	1123.999434	12.081344
20.124518	1109.610300	12.086349
19.945101	1114.575366	12.091354
19.942792	1112.928555	12.096359
20.264735	1108.895123	12.101363
20.136053	1117.235779	12.106368
20.098174	1108.988144	12.111373
20.126712	1114.927813	12.116378
19.865397	1098.296441	12.121383
20.071116	1091.341829	12.126387
19.956489	1093.202276	12.131392
20.071411	1086.777860	12.136397
19.765439	1092.128992	12.141402
19.795862	1105.088835	12.146407
20.212701	1117.770996	12.151411
20.217926	1115.820967	12.156416
20.260942	1097.353407	12.161421
19.853806	1099.188751	12.166426
19.813518	1093.356845	12.171431
19.859967	1096.849139	12.176435
19.941607	1114.925624	12.181440
20.117271	1115.236793	12.186445
20.155321	1125.281734	12.191450
20.071998	1101.935825	12.196455
20.083153	1093.469834	12.201459
20.008344	1096.732286	12.206464
20.088408	1088.800986	12.211469
20.176219	1095.057653	12.216474
20.080658	1093.957202	12.221479
20.122393	1089.777637	12.226483
19.984125	1095.359090	12.231488
20.047089	1088.644099	12.236493
19.980714	1093.942034	12.241498
20.256030	1091.417446	12.246503
20.318959	1092.163739	12.251507
20.007237	1086.472120	12.256512
20.065811	1088.879008	12.261517
20.206619	1095.085430	12.266522
20.083028	1094.479140	12.271527
20.073253	1091.799730	12.276531
19.953391	1089.247489	12.281536
19.912952	1094.754985	12.286541
19.933726	1096.407739	12.291546
20.074376	1091.743209	12.296551
20.240085	1092.322495	12.301555
20.101794	1099.172733	12.306560
20.081182	1095.628432	12.311565
20.035050	1104.824110	12.316570
20.056846	1099.990070	12.321575
20.246183	1103.041643	12.326579
20.145233	1113.809769	12.331584
20.126566	1097.442502	12.336589
19.755729	1085.021347	12.341594
19.955601	1094.332338	12.346599
20.216103	1092.029330	12.351603
19.954265	1098.414313	12.356608
20.197588	1082.632176	12.361613
19.694060	1091.006580	12.366618
19.944688	1095.022237	12.371623
20.384127	1088.277165	12.376627
20.073139	1083.943316	12.381632
19.809952	1071.382778	12.386637
20.005321	1076.405548	12.391642
19.750361	1077.307419	12.396647
20.112799	1077.350655	12.401651
19.847166	1090.719650	12.406656
20.216661	1086.242571	12.411661
20.233715	1070.074660	12.416666
19.727251	1071.785481	12.421671
20.192875	1075.984483	12.426675
20.055927	1074.626469	12.431680
20.058846	1071.232977	12.436685
20.280370	1077.368953	12.441690
19.811515	1077.653596	12.446695
20.126632	1074.084930	12.451699
20.065305	1081.611289	12.456704
20.281811	1071.892670	12.461709
19.891796	1078.651359	12.466714
19.823987	1076.245373	12.471719
20.212833	1069.611680	12.476723
19.960936	1076.983122	12.481728
19.911508	1083.763980	12.486733
20.137697	1086.536833	12.491738
20.092398	1080.889464	12.496743
20.202097	1073.736477	12.501747
19.999549	1087.820875	12.506752
20.300151	1077.847542	12.511757
19.992516	1077.076623	12.516762
20.017600	1085.779126	12.521767
20.300010	1078.678234	12.526771
20.057916	1074.901156	12.531776
20.403432	1078.361517	12.536781
20.312146	1085.598527	12.541786
19.968417	1082.723989	12.546791
20.069850	1080.687651	12.551795
20.064392	1077.639302	12.556800
20.098962	1063.326432	12.561805
19.887418	1061.410984	12.566810
19.733028	1060.556484	12.571815
20.313372	1072.423187	12.576819
19.769097	1069.692612	12.581824
20.039997	1071.389057	12.586829
20.199827	1075.937268	12.591834
20.066144	1072.102684	12.596839
19.820501	1063.825917	12.601843
19.557438	1067.128638	12.606848
19.797079	1079.147468	12.611853
20.018664	1081.488139	12.616858
19.925884	1093.459066	12.621863
20.024543	1093.155617	12.626867
20.384455	1095.792804	12.631872
20.253417	1094.123156	12.636877
20.143170	1084.409331	12.641882
19.933874	1069.211957	12.646887
20.027652	1068.896670	12.651891
19.787946	1071.378729	12.656896
19.964469	1074.090108	12.661901
20.258314	1086.701175	12.666906
20.148282	1085.304960	12.671911
20.079637	1070.585093	12.676915
20.042922	1066.746084	12.681920
19.880141	1066.258020	12.686925
19.962375	1069.854209	12.691930
19.951878	1063.329947	12.696935
19.976538	1066.501615	12.701939
19.835286	1074.136132	12.706944
19.869968	1065.826481	12.711949
20.138504	1076.042805	12.716954
19.833335	1077.708116	12.721959
20.173545	1079.331211	12.726963
19.877628	1079.324106	12.731968
19.880385	1082.347869	12.736973
20.282501	1088.940794	12.741978
19.999331	1088.139950	12.746983
20.281020	1075.957748	12.751987
20.010738	1081.555519	12.756992
20.105413	1073.708638	12.761997
20.039637	1070.691202	12.767002
20.097477	1076.679015	12.772007
19.997058	1066.890298	12.777011
20.077859	1066.483244	12.782016
20.001288	1068.710604	12.787021
19.785114	1079.983619	12.792026
19.699840	1078.112690	12.797031
20.058604	1075.079586	12.802035
19.809073	1076.398523	12.807040
19.685613	1071.890463	12.812045
20.202163	1080.410487	12.817050
20.026128	1091.361689	12.822055
20.098508	1081.491781	12.827059
19.982807	1093.624073	12.832064
19.832396	1079.332017	12.837069
20.006326	1089.676991	12.842074
20.037597	1093.943697	12.847079
20.126573	1083.619300	12.852083
19.795591	1076.247200	12.857088
20.065907	1083.765612	12.862093
20.174190	1086.165360	12.867098
20.085309	1074.944366	12.872103
20.267627	1076.284320	12.877107
19.892537	1080.183709	12.882112
20.461872	1081.570756	12.887117
19.965354	1074.384346	12.892122
20.041626	1078.371032	12.897127
20.250966	1070.868597	12.902131
19.975501	1075.677065	12.907136
20.197923	1081.685943	12.912141
19.954743	1077.085790	12.917146
19.969104	1079.812783	12.922151
20.009668	1076.172778	12.927155
20.157453	1079.216780	12.932160
20.332439	1075.616053	12.937165
20.187538	1078.901509	12.942170
19.920324	1073.677504	12.947175
20.406610	1071.261998	12.952179
20.139737	1076.632122	12.957184
20.120557	1069.684213	12.962189
19.927329	1080.758008	12.967194
19.950554	1082.401696	12.972199
20.453612	1080.500804	12.977203
19.903530	1070.518851	12.982208
19.974538	1047.912519	12.987213
20.238864	1049.692806	12.992218
19.870794	1044.190769	12.997223
20.190387	1046.185401	13.002227
19.839114	1052.272363	13.007232
19.951772	1048.042070	13.012237
19.980138	1044.364591	13.017242
20.064133	1050.231516	13.022247
19.881272	1043.129149	13.027251
19.872136	1053.060918	13.032256
20.308045	1050.430292	13.037261
20.212230	1049.714697	13.042266
20.054599	1055.004305	13.047271
20.507774	1043.497376	13.052275
20.039364	1045.575897	13.057280
19.903564	1048.653294	13.062285
20.027123	1047.660625	13.067290
19.899392	1045.920275	13.072295
20.281618	1048.079975	13.077299
19.988245	1055.330277	13.082304
20.273141	1048.165919	13.087309
19.953403	1050.917017	13.092314
19.999632	1051.039863	13.097319
20.233720	1044.312582	13.102323
19.974351	1048.191140	13.107328
19.898005	1048.842938	13.112333
19.981091	1052.382211	13.117338
20.029605	1050.277039	13.122343
20.008478	1049.980868	13.127347
19.775840	1052.866323	13.132352
19.923830	1049.426042	13.137357
19.900388	1056.341528	13.142362
19.769739	1062.726073	13.147367
20.049119	1057.746875	13.152371
19.788735	1060.693532	13.157376
19.889154	1060.193454	13.162381
19.990720	1060.424179	13.167386
19.938509	1062.780129	13.172391
20.051673	1049.143142	13.177395
19.909606	1055.542122	13.182400
20.128979	1052.591185	13.187405
20.106746	1060.144416	13.192410
19.839671	1063.353151	13.197415
19.997835	1049.436937	13.202419
19.672671	1057.940584	13.207424
19.759274	1054.916196	13.212429
19.656033	1058.045177	13.217434
20.135699	1079.239935	13.222439
20.337418	1078.345983	13.227443
19.941734	1072.706400	13.232448
20.156644	1060.467046	13.237453
19.792318	1056.701583	13.242458
19.900822	1062.469978	13.247463
19.970947	1056.015659	13.252467
19.824631	1062.680273	13.257472
20.062111	1064.393875	13.262477
20.206237	1064.340242	13.267482
20.164338	1067.121154	13.272487
20.456094	1056.972611	13.277491
20.041769	1058.587514	13.282496
20.015627	1052.310992	13.287501
20.347032	1056.162353	13.292506
19.924109	1062.164544	13.297511
20.306844	1059.849142	13.302515
19.644160	1055.042279	13.307520
19.799821	1058.499008	13.312525
19.912967	1053.529765	13.317530
19.976327	1062.264788	13.322535
20.140846	1054.769510	13.327539
19.895718	1060.528068	13.332544
19.813942	1057.060559	13.337549
19.777411	1062.822122	13.342554
19.665540	1058.038590	13.347559
19.775582	1065.180395	13.352563
19.926674	1069.386190	13.357568
20.337046	1073.347976	13.362573
20.222894	1069.551282	13.367578
20.060207	1062.747702	13.372583
20.112896	1056.785853	13.377587
19.798511	1073.649577	13.382592
20.074665	1056.273301	13.387597
19.955328	1055.394284	13.392602
19.928467	1058.849372	13.397607
20.088830	1063.823312	13.402611
20.167385	1056.943407	13.407616
20.229563	1063.764809	13.412621
20.023427	1067.236663	13.417626
19.929091	1065.515429	13.422631
20.159268	1057.305502	13.427635
19.929829	1061.516001	13.432640
19.963494	1052.278396	13.437645
20.019253	1061.418368	13.442650
20.092068	1054.593002	13.447655
19.979165	1058.782547	13.452659
20.018103	1076.123769	13.457664
19.989146	1067.939395	13.462669
19.949239	1070.172736	13.467674
19.665365	1065.500222	13.472679
20.000008	1063.209051	13.477683
19.670316	1079.808693	13.482688
20.264333	1074.661023	13.487693
20.113777	1070.465609	13.492698
19.957833	1062.087795	13.497703
20.075401	1072.642038	13.502707
20.061074	1073.155412	13.507712
20.152436	1067.858447	13.512717
19.911864	1071.652792	13.517722
19.656454	1072.002749	13.522727
19.983267	1065.526410	13.527731
19.874652	1076.798039	13.532736
20.072465	1073.179479	13.537741
19.918182	1068.457119	13.542746
19.945027	1069.553762	13.547751
20.264394	1070.656583	13.552755
19.824796	1075.997479	13.557760
20.088358	1072.760342	13.562765
19.898112	1075.613806	13.567770
19.971603	1071.468609	13.572775
20.179472	1073.601712	13.577779
20.330811	1079.902651	13.582784
20.120169	1074.150756	13.587789
20.214565	1072.899361	13.592794
20.268988	1077.890991	13.597799
20.175114	1074.235366	13.602803
20.067383	1080.464074	13.607808
20.278365	1077.881146	13.612813
20.286554	1072.674723	13.617818
20.281244	1078.045710	13.622823
20.301217	1064.861218	13.627827
20.083886	1056.899302	13.632832
19.980997	1045.914763	13.637837
19.700400	1039.980845	13.642842
19.659473	1043.759900	13.647847
20.041765	1053.227079	13.652851
19.864718	1073.119797	13.657856
20.140183	1065.429394	13.662861
20.307407	1071.119823	13.667866
20.004420	1060.835879	13.672871
19.942291	1053.528153	13.677875
19.591847	1049.717896	13.682880
19.936386	1063.297081	13.687885
19.956343	1067.422856	13.692890
20.058905	1077.256395	13.697895
19.952133	1074.624001	13.702899
19.929544	1081.481799	13.707904
20.510383	1070.376363	13.712909
20.206691	1062.395887	13.717914
20.008119	1046.998111	13.722919
19.642102	1044.560838	13.727923
19.654980	1056.942276	13.732928
19.767373	1066.694596	13.737933
20.114065	1070.840018	13.742938
20.055459	1076.713139	13.747943
19.983588	1068.116100	13.752947
20.068628	1083.509355	13.757952
19.907741	1075.212754	13.762957
20.183512	1079.405764	13.767962
19.802794	1084.425794	13.772967
19.928243	1078.100638	13.777971
20.064132	1083.117915	13.782976
19.988726	1073.703709	13.787981
20.092785	1080.035057	13.792986
20.041515	1084.668985	13.797991
20.435101	1080.729800	13.802995
20.117941	1078.339927	13.808000
20.076060	1051.464242	13.813005
20.279179	1050.917820	13.818010
19.966213	1053.284604	13.823015
20.341324	1050.175562	13.828019
19.961602	1058.624039	13.833024
19.603801	1051.145832	13.838029
19.797975	1056.743639	13.843034
19.975703	1053.925511	13.848039
20.195362	1046.837797	13.853043
19.519634	1059.325912	13.858048
20.187105	1053.997784	13.863053
20.159738	1058.218634	13.868058
20.265837	1060.223662	13.873063
20.331130	1046.277316	13.878067
20.127482	1055.854511	13.883072
20.097684	1051.412739	13.888077
19.991459	1061.533481	13.893082
19.960616	1058.675282	13.898087
20.096103	1050.721758	13.903091
20.015801	1059.836117	13.908096
20.038582	1041.163679	13.913101
20.181939	1048.447621	13.918106
19.844171	1059.997870	13.923111
19.914738	1046.702024	13.928115
19.905459	1055.616590	13.933120
20.159123	1053.796483	13.938125
19.884474	1056.135865	13.943130
20.105799	1057.633614	13.948135
20.264034	1052.251865	13.953139
20.095375	1053.262195	13.958144
20.112687	1050.283556	13.963149
20.214628	1054.884364	13.968154
20.094099	1054.577236	13.973159
20.444657	1054.101135	13.978163
20.176137	1048.387658	13.983168
20.335925	1027.071459	13.988173
19.917245	1029.113658	13.993178
20.047963	1024.682567	13.998183
20.170936	1013.467257	14.003187
19.856288	1015.914735	14.008192
19.964670	1018.843204	14.013210
19.772828	1008.840857	14.018227
19.654087	1024.767599	14.023245
19.998490	1031.035747	14.028263
20.097627	1051.799579	14.033280
20.379452	1048.211384	14.038298
20.226898	1053.798222	14.043315
20.010091	1043.444317	14.048333
20.508482	1040.522388	14.053351
19.868525	1029.720014	14.058368
19.910095	1039.189692	14.063386
20.019794	1053.802695	14.068403
20.263594	1059.799814	14.073421
20.384639	1051.064199	14.078439
20.612607	1060.117971	14.083456
20.479153	1047.846559	14.088474
20.003641	1034.174619	14.093491
20.116141	1050.700817	14.098509
20.390819	1048.088283	14.103527
20.385258	1060.008479	14.108544
20.087984	1065.669528	14.113562
20.529492	1057.807766	14.118579
20.255294	1061.753626	14.123597
20.355602	1054.882266	14.128615
20.377061	1065.270700	14.133632
20.482799	1053.866439	14.138650
20.445155	1060.213624	14.143667
20.121814	1064.731270	14.148685
20.316201	1060.627678	14.153703
20.105488	1068.132726	14.158720
20.095477	1058.471016	14.163738
20.234309	1058.497747	14.168755
20.108965	1070.884597	14.173773
20.301875	1082.563937	14.178791
20.291170	1098.583645	14.183808
20.385326	1091.182335	14.188826
20.576637	1094.203707	14.193843
20.072942	1097.370537	14.198861
20.460874	1094.334076	14.203879
20.414008	1094.951228	14.208896
20.203208	1103.819383	14.213914
21.117901	1111.726998	14.218931
21.046107	1111.936765	14.223949
20.752119	1105.228161	14.228967
20.620640	1097.354730	14.233984
20.625321	1101.145218	14.239002
21.085108	1122.237034	14.244019
20.966079	1121.360256	14.249037
20.738729	1107.275060	14.254055
20.715980	1116.913929	14.259072
20.671867	1119.515874	14.264090
21.280691	1126.605512	14.269107
21.166265	1119.984670	14.274125
20.857371	1100.148710	14.279143
20.870495	1112.081699	14.284160
21.096052	1124.787808	14.289178
21.557922	1123.023972	14.294195
20.931579	1110.057163	14.299213
21.198119	1097.611796	14.304231
20.888608	1095.950544	14.309248
20.802792	1091.546343	14.314266
21.024962	1110.616092	14.319283
20.941286	1126.366673	14.324301
21.246178	1126.005896	14.329319
21.362668	1134.024314	14.334336
21.275859	1115.114067	14.339354
21.021137	1108.020872	14.344371
21.103305	1124.942116	14.349389
21.120246	1132.323582	14.354407
21.436833	1129.020057	14.359424
21.118081	1131.508499	14.364442
21.134727	1122.096549	14.369459
21.253656	1136.270845	14.374477
21.575445	1122.625033	14.379495
21.149598	1127.286467	14.384512
21.168769	1134.983768	14.389530
21.412308	1129.065629	14.394547
21.457918	1141.035934	14.399565
21.660131	1128.772266	14.404583
21.453533	1133.733801	14.409600
21.356295	1131.856997	14.414618
21.414279	1127.541538	14.419635
21.531791	1127.854825	14.424653
21.585684	1132.200636	14.429671
21.640813	1139.599611	14.434688
21.436979	1137.909701	14.439706
21.719197	1125.111012	14.444723
21.623652	1131.750618	14.449741
21.563081	1133.428644	14.454759
21.487919	1146.130037	14.459776
21.307748	1135.680557	14.464794
21.490576	1131.852505	14.469811
21.256486	1140.292585	14.474829
21.523438	1128.456697	14.479847
21.632435	1134.281858	14.484864
21.370325	1138.381545	14.489882
21.765084	1138.553082	14.494899
21.909331	1151.312296	14.499917
21.766427	1148.432065	14.504935
21.551150	1141.914605	14.509952
21.412937	1151.630117	14.514970
21.444288	1143.335845	14.519987
21.623227	1152.789980	14.525005
21.590676	1148.956162	14.530023
21.624968	1158.371234	14.535040
21.748931	1152.605083	14.540058
21.954352	1156.415480	14.545075
21.473498	1166.839269	14.550093
21.906472	1174.376206	14.555111
22.200704	1190.170406	14.560128
22.219743	1185.753385	14.565146
22.388244	1183.931722	14.570163
22.451788	1176.118382	14.575181
22.331536	1156.157086	14.580199
22.140562	1149.757660	14.585216
22.018519	1149.751277	14.590234
22.315898	1143.536670	14.595251
22.089528	1142.741507	14.600269
22.364394	1152.166185	14.605287
22.410440	1147.467218	14.610304
22.370007	1143.261050	14.615322
22.761435	1147.252572	14.620339
22.142994	1150.628057	14.625357
22.564925	1150.272209	14.630375
22.375449	1147.760430	14.635392
22.228809	1154.235156	14.640410
22.631859	1150.467933	14.645427
22.343205	1151.681311	14.650445
22.271791	1152.546996	14.655463
22.343946	1142.769088	14.660480
22.022543	1141.882113	14.665498
22.555845	1136.566653	14.670515
22.591157	1150.594631	14.675533
22.677479	1141.519207	14.680551
22.658583	1141.625367	14.685568
22.574937	1145.013873	14.690586
22.535544	1145.389940	14.695603
22.507724	1149.165960	14.700621
22.682718	1139.969425	14.705639
22.599984	1144.439282	14.710656
22.693869	1144.839711	14.715674
22.635019	1141.445834	14.720691
22.662825	1149.605826	14.725709
22.669664	1147.662868	14.730727
22.759609	1152.802850	14.735744
22.460446	1157.623421	14.740762
22.704760	1139.451592	14.745779
22.667577	1142.636051	14.750797
22.784865	1148.215281	14.755815
22.796801	1155.791833	14.760832
22.741262	1149.844305	14.765850
22.686466	1145.232998	14.770867
22.562816	1152.586558	14.775885
22.761882	1157.407892	14.780903
23.162263	1170.001997	14.785920
22.821586	1178.610115	14.790938
23.081870	1179.344244	14.795955
22.783018	1177.535771	14.800973
22.949778	1177.121516	14.805991
23.197612	1179.478699	14.811008
23.038955	1177.066610	14.816026
23.324150	1184.389586	14.821043
23.297563	1173.983225	14.826061
23.336947	1157.211074	14.831079
23.117849	1161.404585	14.836096
22.758206	1151.953527	14.841114
22.844439	1155.329098	14.846131
22.951124	1175.742679	14.851149
23.133981	1181.725186	14.856167
23.114727	1181.142389	14.861184
23.030494	1182.957121	14.866202
23.353918	1179.154612	14.871219
23.045694	1190.314619	14.876237
23.285603	1186.206877	14.881255
23.827799	1184.663827	14.886272
23.457654	1181.270038	14.891290
23.708249	1173.287647	14.896307
23.385401	1181.973938	14.901325
23.456774	1175.846490	14.906343
23.264842	1175.822152	14.911360
23.086882	1180.490473	14.916378
23.263741	1178.321398	14.921395
23.415200	1180.156742	14.926413
23.307818	1176.405640	14.931431
23.383441	1173.690333	14.936448
23.524895	1182.064248	14.941466
23.658680	1179.891031	14.946483
23.501276	1173.116564	14.951501
23.591647	1172.683817	14.956519
23.599859	1183.440192	14.961536
23.521572	1173.782216	14.966554
23.569264	1169.053091	14.971571
23.569902	1186.357872	14.976589
23.630491	1196.568692	14.981607
24.036030	1192.732632	14.986624
23.528590	1197.860152	14.991642
23.822222	1196.096399	14.996659
23.733029	1202.963909	15.001677
24.040392	1211.183172	15.006695
24.130015	1200.802304	15.011712
24.191414	1197.471823	15.016730
24.049094	1177.694135	15.021747
23.922570	1182.010532	15.026765
23.693564	1176.585397	15.031783
23.779799	1168.874626	15.036800
23.338786	1192.811211	15.041818
23.947370	1192.893586	15.046835
24.069061	1212.739299	15.051853
24.122948	1204.781973	15.056871
24.391882	1209.654318	15.061888
23.987122	1213.140461	15.066906
24.518843	1205.305133	15.071923
24.215246	1215.607086	15.076941
24.150558	1214.900181	15.081959
24.554509	1206.082384	15.086976
24.208788	1218.635075	15.091994
24.566980	1201.565050	15.097011
24.102582	1193.197228	15.102029
23.921592	1186.445394	15.107047
24.017871	1199.230392	15.112064
24.227820	1207.269340	15.117082
24.556132	1202.222516	15.122099
24.471285	1209.891613	15.127117
24.580562	1210.371390	15.132135
24.931922	1201.191521	15.137152
24.330082	1197.872435	15.142170
24.552543	1190.649607	15.147187
24.714781	1183.542571	15.152205
24.161942	1176.175193	15.157223
24.433012	1176.580399	15.162240
24.318874	1200.305980	15.167258
24.878135	1200.006882	15.172275
24.460320	1197.410384	15.177293
24.376993	1210.165047	15.182311
24.846306	1208.223042	15.187328
24.655750	1219.659259	15.192346
24.453825	1217.532501	15.197363
24.677699	1219.253263	15.202381
24.614591	1216.151857	15.207399
24.694277	1208.512112	15.212416
24.652457	1211.332368	15.217434
24.921715	1207.094092	15.222451
24.929653	1215.803153	15.227469
24.723415	1214.053053	15.232487
25.147062	1204.952105	15.237504
24.899303	1213.158443	15.242522
24.784927	1211.382680	15.247539
25.160536	1213.491391	15.252557
24.816717	1214.538959	15.257575
24.971665	1208.625478	15.262592
24.629782	1217.824509	15.267610
24.695241	1208.342580	15.272627
24.681657	1217.640265	15.277645
24.157789	1215.638005	15.282663
24.854431	1219.000395	15.287680
24.973402	1236.811777	15.292698
25.082160	1241.772603	15.297715
25.104497	1249.599241	15.302733
25.018074	1238.721796	15.307751
25.139299	1239.570132	15.312768
25.470570	1254.674199	15.317786
25.349186	1241.348295	15.322803
25.462952	1243.649003	15.327821
25.365022	1247.741412	15.332839
25.466232	1239.509880	15.337856
25.426908	1244.705120	15.342874
25.098153	1245.093519	15.347891
25.533719	1233.944839	15.352909
25.169183	1235.592702	15.357927
25.332807	1244.858995	15.362944
25.235915	1246.148766	15.367962
25.397328	1241.524968	15.372979
25.721513	1239.040577	15.377997
25.247951	1250.709941	15.383015
25.751132	1240.560401	15.388032
25.571422	1246.643236	15.393050
25.404365	1249.565275	15.398067
25.808401	1251.707212	15.403085
25.434127	1249.636253	15.408103
25.643755	1238.461468	15.413120
25.726737	1243.069313	15.418138
25.675473	1246.651675	15.423155
25.504860	1240.183677	15.428173
25.278670	1248.959989	15.433191
25.671120	1231.711424	15.438208
25.477077	1247.196581	15.443226
25.493309	1238.412288	15.448243
25.920330	1246.367870	15.453261
25.807780	1261.528571	15.458279
25.855239	1273.162834	15.463296
25.948336	1277.223997	15.468314
26.020175	1267.928211	15.473331
26.113144	1266.025772	15.478349
26.028428	1259.949926	15.483367
25.710349	1244.161243	15.488384
25.750101	1252.694571	15.493402
25.940834	1255.370775	15.498419
25.927310	1270.734353	15.503437
25.875809	1274.676999	15.508455
26.480763	1265.497543	15.513472
26.114094	1269.142013	15.518490
26.370754	1269.218382	15.523507
26.266930	1263.769316	15.528525
26.312033	1272.816206	15.533543
26.633944	1267.623295	15.538560
26.591224	1270.573487	15.543578
26.501432	1262.336223	15.548595
26.508472	1249.005561	15.553613
26.359373	1239.495695	15.558631
26.393097	1230.069939	15.563648
26.048148	1243.907747	15.568666
25.978405	1244.700022	15.573683
26.455477	1250.715074	15.578701
26.233234	1268.285960	15.583719
26.362594	1262.968811	15.588736
26.477349	1260.077352	15.593754
26.657549	1261.473948	15.598771
26.783175	1271.666581	15.603789
26.552650	1269.766971	15.608807
26.776476	1267.868831	15.613824
26.618318	1270.852379	15.618842
26.609929	1272.279840	15.623859
26.989916	1267.762752	15.628877
26.576092	1273.886870	15.633895
26.595576	1263.869518	15.638912
26.749887	1262.620358	15.643930
26.498873	1265.901872	15.648947
26.610697	1264.987479	15.653965
26.601165	1273.073267	15.658983
26.784890	1265.433417	15.664000
26.776950	1277.263717	15.669018
26.411370	1265.710295	15.674035
27.024726	1264.740294	15.679053
26.554019	1273.308642	15.684071
26.890677	1270.403026	15.689088
26.707294	1275.891827	15.694106
26.866530	1296.736091	15.699123
27.225285	1292.369466	15.704141
27.012312	1306.977555	15.709159
27.167534	1298.190722	15.714176
27.109551	1308.259288	15.719194
27.132403	1305.453267	15.724211
27.198492	1301.176579	15.729229
26.969556	1306.719850	15.734247
27.370977	1299.284372	15.739264
27.280059	1307.530245	15.744282
26.845428	1311.927283	15.749299
27.347540	1303.406033	15.754317
27.162523	1306.444211	15.759335
26.978903	1297.513210	15.764352
26.909146	1302.021946	15.769370
26.695216	1298.375900	15.774387
27.644627	1299.313958	15.779405
27.183847	1305.152195	15.784423
27.226442	1303.222391	15.789440
27.528070	1322.605378	15.794458
27.880662	1328.812572	15.799475
27.688249	1314.729467	15.804493
27.294246	1310.523010	15.809511
27.535416	1311.905954	15.814528
27.485999	1308.995050	15.819546
27.621295	1334.093713	15.824563
27.646962	1331.950302	15.829581
27.939285	1335.878242	15.834599
28.091177	1332.137660	15.839616
27.743730	1323.891903	15.844634
27.572237	1306.438237	15.849651
27.709385	1322.574616	15.854669
27.435202	1324.013013	15.859687
27.852293	1337.171704	15.864704
28.294988	1328.781045	15.869722
27.765929	1335.853274	15.874739
28.042205	1320.991445	15.879757
27.822135	1327.878315	15.884775
28.180966	1340.642013	15.889792
28.113816	1328.883633	15.894810
27.838532	1333.220654	15.899827
28.313860	1334.499397	15.904845
27.827336	1338.700215	15.909863
27.770424	1342.218217	15.914880
28.126740	1328.005894	15.919898
27.812112	1340.231243	15.924915
28.002789	1325.755102	15.929933
27.958967	1327.912636	15.934951
27.750932	1332.573216	15.939968
28.169103	1328.087774	15.944986
28.123344	1339.338175	15.950003
27.959013	1327.041562	15.955021
28.126532	1353.812051	15.960039
28.216776	1353.577531	15.965056
28.502705	1364.731789	15.970074
28.122599	1371.484532	15.975091
28.616475	1363.134458	15.980109
28.402017	1370.136863	15.985127
28.883309	1369.769970	15.990144
28.682534	1364.661176	15.995162
28.745414	1371.403832	16.000179
29.059422	1352.332603	16.005197
28.609948	1343.496673	16.010215
28.329749	1336.806999	16.015232
28.576187	1335.136491	16.020250
28.537949	1338.684548	16.025267
28.697607	1351.504405	16.030285
28.867193	1352.976639	16.035303
28.904249	1356.975186	16.040320
28.690114	1340.088308	16.045338
28.642367	1343.266630	16.050355
28.503339	1362.828497	16.055373
28.791120	1367.483160	16.060391
28.624733	1374.311150	16.065408
28.813536	1362.676310	16.070426
28.750989	1367.342013	16.075443
29.088015	1358.960326	16.080461
28.648754	1371.597283	16.085479
28.761924	1362.488337	16.090496
28.951690	1364.173656	16.095514
28.503500	1371.866180	16.100531
28.854445	1359.636017	16.105549
29.176063	1378.294620	16.110567
29.111546	1387.176583	16.115584
29.529420	1388.074362	16.120602
29.579168	1381.463398	16.125619
29.482304	1367.926603	16.130637
29.320913	1356.099857	16.135655
29.333750	1361.080742	16.140672
29.137456	1360.263465	16.145690
29.244040	1357.440934	16.150707
29.505422	1351.603234	16.155725
29.179095	1366.771398	16.160743
29.098954	1363.612112	16.165760
29.631398	1359.638573	16.170778
29.420012	1377.993627	16.175795
29.036479	1376.388194	16.180813
29.542919	1377.332412	16.185831
29.564053	1395.603996	16.190848
29.689892	1389.467771	16.195866
29.530354	1399.463716	16.200883
29.764659	1384.160181	16.205901
29.561393	1388.979689	16.210919
29.364909	1398.303515	16.215936
29.624032	1386.036848	16.220954
29.313900	1382.823785	16.225971
29.619198	1389.265863	16.230989
29.386028	1391.365511	16.236007
29.185968	1397.487048	16.241024
29.720678	1403.627474	16.246042
29.665801	1418.840492	16.251059
29.809996	1425.533235	16.256077
29.866786	1421.801507	16.261095
29.450275	1429.520471	16.266112
30.185992	1414.361102	16.271130
29.671852	1419.754050	16.276147
29.977054	1411.563822	16.281165
30.021637	1421.400591	16.286183
29.889530	1423.084553	16.291200
30.105735	1419.196831	16.296218
30.264358	1416.345538	16.301235
30.416319	1417.431243	16.306253
30.419890	1416.746477	16.311271
30.222954	1418.131661	16.316288
30.394825	1414.914079	16.321306
30.181753	1421.043208	16.326323
30.382316	1402.677458	16.331341
30.239489	1419.371433	16.336359
30.282978	1408.698884	16.341376
30.782172	1415.700753	16.346394
30.449542	1410.857592	16.351411
30.850143	1408.374358	16.356429
30.725356	1410.050072	16.361447
30.504764	1411.563304	16.366464
30.667340	1411.345564	16.371482
30.506732	1409.412759	16.376499
30.781378	1408.112932	16.381517
30.758416	1413.146738	16.386535
30.863636	1416.086736	16.391552
31.095466	1406.998952	16.396570
30.948687	1417.364916	16.401587
31.142872	1407.432080	16.406605
30.907450	1396.930658	16.411623
30.540547	1386.131659	16.416640
30.759079	1372.561861	16.421658
30.718090	1395.056145	16.426675
30.866479	1400.322968	16.431693
30.956812	1406.114247	16.436711
30.856030	1409.596788	16.441728
31.012318	1404.127420	16.446746
31.034381	1412.371851	16.451763
31.310015	1412.039331	16.456781
31.162482	1417.388752	16.461799
31.206824	1411.581712	16.466816
31.314128	1399.049008	16.471834
30.942184	1392.192245	16.476851
31.044747	1406.546391	16.481869
30.984402	1410.337892	16.486887
30.797284	1404.237416	16.491904
30.888891	1414.254667	16.496922
30.910510	1409.624796	16.501939
31.317696	1413.175768	16.506957
31.020120	1406.943462	16.511975
31.023385	1416.575234	16.516992
31.186464	1411.900777	16.522010
31.734560	1419.938611	16.527027
31.646269	1414.347790	16.532045
31.447233	1409.060154	16.537063
31.420034	1415.586736	16.542080
31.809317	1395.772732	16.547098
31.553094	1416.785682	16.552115
31.643048	1409.605118	16.557133
31.593210	1408.559974	16.562151
31.510949	1407.379209	16.567168
31.520397	1403.947634	16.572186
31.445648	1422.173980	16.577203
31.646727	1433.818478	16.582221
31.866323	1442.037713	16.587239
32.129195	1433.949398	16.592256
32.075690	1432.303120	16.597274
31.948911	1424.679674	16.602291
31.934188	1408.609608	16.607309
32.016001	1398.984153	16.612327
31.647980	1405.886004	16.617344
31.950971	1415.831002	16.622362
31.849295	1428.056282	16.627379
32.138696	1431.498621	16.632397
32.166735	1426.993569	16.637415
32.261728	1430.651756	16.642432
32.449538	1430.381224	16.647450
32.166354	1426.970359	16.652467
32.020984	1425.347386	16.657485
32.086917	1426.235229	16.662503
32.108939	1432.078314	16.667520
32.410515	1425.696169	16.672538
32.202641	1422.712980	16.677555
32.272233	1420.521651	16.682573
32.105043	1423.633305	16.687591
31.983784	1426.120187	16.692608
32.449608	1420.883033	16.697626
32.081900	1432.235192	16.702643
31.998688	1427.567763	16.707661
32.625535	1436.984469	16.712679
32.531690	1449.659216	16.717696
32.345415	1437.351065	16.722714
32.454583	1446.626172	16.727731
32.515044	1466.891008	16.732749
32.916552	1463.042938	16.737767
32.812517	1462.831537	16.742784
33.134191	1461.715339	16.747802
32.968929	1456.976824	16.752819
32.419633	1445.421096	16.757837
32.851255	1443.977460	16.762855
32.792031	1455.922270	16.767872
32.917477	1463.933937	16.772890
32.800590	1465.952124	16.777907
33.024582	1455.198839	16.782925
32.835506	1459.448211	16.787943
32.867855	1463.191120	16.792960
32.943248	1454.674130	16.797978
32.880761	1461.709759	16.802995
33.031535	1463.367487	16.808013
33.045659	1447.925171	16.813031
32.761333	1458.557722	16.818048
32.762438	1455.451528	16.823066
32.682027	1456.392602	16.828083
33.222703	1468.292871	16.833101
33.212116	1479.207414	16.838119
33.440182	1484.449762	16.843136
33.658795	1479.384944	16.848154
33.805419	1471.319868	16.853171
33.347791	1462.500110	16.858189
33.486364	1449.392119	16.863207
33.131646	1461.994433	16.868224
33.103512	1458.852788	16.873242
33.358242	1474.189528	16.878259
33.675969	1479.054969	16.883277
33.899222	1482.970368	16.888295
33.765505	1479.699258	16.893312
33.859903	1474.407272	16.898330
33.985384	1479.904307	16.903347
33.215146	1460.728207	16.908365
34.031728	1469.632512	16.913383
33.700884	1480.544648	16.918400
33.977038	1489.285032	16.923418
33.822540	1485.479226	16.928435
33.731157	1474.718020	16.933453
34.074496	1482.652472	16.938471
33.612568	1488.966046	16.943488
33.846748	1482.483720	16.948506
33.796435	1482.157564	16.953523
33.648083	1487.511860	16.958541
34.043555	1478.035329	16.963559
33.796231	1492.948762	16.968576
33.972165	1481.118453	16.973594
34.020458	1481.641002	16.978611
33.808184	1485.321465	16.983629
34.213060	1487.460159	16.988647
34.172762	1510.138565	16.993664
34.340389	1504.737356	16.998682
34.205067	1523.601166	17.003699
34.387316	1516.981593	17.008717
34.606952	1506.674946	17.013735
34.552157	1511.907357	17.018752
34.647588	1514.903996	17.023770
34.803892	1511.880011	17.028787
34.571439	1493.174982	17.033805
34.530523	1473.684332	17.038823
34.247950	1479.193747	17.043840
34.532786	1500.644375	17.048858
34.692130	1495.477312	17.053875
34.548385	1512.324133	17.058893
34.926054	1500.268140	17.063911
34.825854	1504.095911	17.068928
34.786773	1499.066680	17.073946
34.917135	1500.864529	17.078963
34.897311	1514.690853	17.083981
34.945504	1505.513526	17.088999
34.772009	1499.697932	17.094016
34.914543	1492.906154	17.099034
34.855128	1500.213462	17.104051
34.909036	1508.238923	17.109069
34.789306	1496.089220	17.114087
34.792496	1500.908873	17.119104
35.043509	1491.092767	17.124122
35.178766	1503.947327	17.129139
34.750924	1501.716549	17.134157
35.087244	1496.890159	17.139175
35.134468	1503.958650	17.144192
34.944125	1497.808309	17.149210
35.040987	1493.710712	17.154227
35.129179	1500.288146	17.159245
35.315202	1521.204757	17.164263
35.254984	1530.958421	17.169280
35.451130	1531.612344	17.174298
35.593240	1536.548288	17.179315
35.411849	1536.537998	17.184333
35.786765	1529.888477	17.189351
35.747626	1537.262574	17.194368
35.728806	1527.397452	17.199386
35.744693	1511.747134	17.204403
35.587501	1523.103544	17.209421
35.774752	1517.530089	17.214439
35.822486	1520.131615	17.219456
35.877900	1516.024104	17.224474
35.948435	1503.785843	17.229491
35.775359	1497.334641	17.234509
35.731104	1492.754578	17.239527
35.844893	1514.738266	17.244544
36.293847	1517.838981	17.249562
36.060149	1507.175172	17.254579
35.701547	1496.094749	17.259597
36.122724	1509.260026	17.264615
36.046746	1518.259521	17.269632
35.946464	1523.443346	17.274650
36.155600	1522.888608	17.279667
36.046420	1520.616443	17.284685
36.446166	1526.843733	17.289703
35.944843	1527.560913	17.294720
35.999303	1527.361201	17.299738
36.375181	1516.793659	17.304755
36.200671	1528.524879	17.309773
36.315172	1522.335347	17.314791
36.594792	1523.369238	17.319808
36.351919	1527.836436	17.324826
36.299188	1518.856892	17.329843
36.208093	1527.361697	17.334861
36.628479	1522.023209	17.339879
36.508990	1530.442875	17.344896
36.455716	1522.285376	17.349914
36.400712	1521.675231	17.354931
36.392532	1526.480188	17.359949
36.712532	1519.290410	17.364967
36.426303	1529.101356	17.369984
36.636293	1548.192501	17.375002
36.967799	1559.287727	17.380019
36.586345	1556.963020	17.385037
36.912184	1560.634763	17.390055
36.973703	1554.667613	17.395072
36.991746	1559.151413	17.400090
37.042591	1559.502873	17.405107
36.830166	1564.637739	17.410125
36.859993	1556.192455	17.415143
37.034889	1554.561650	17.420160
37.107514	1550.240585	17.425178
36.875979	1553.539506	17.430195
36.622187	1559.771148	17.435213
36.813347	1548.275007	17.440231
36.969828	1558.535285	17.445248
37.192984	1572.458201	17.450266
37.552969	1573.659402	17.455283
37.448096	1578.406647	17.460301
37.430392	1575.470967	17.465319
37.464595	1583.796934	17.470336
37.305738	1580.431489	17.475354
37.653511	1569.344539	17.480371
37.246339	1585.048102	17.485389
37.582564	1576.679790	17.490407
37.712881	1592.097063	17.495424
37.581273	1585.624263	17.500442
37.619697	1581.397526	17.505459
37.681290	1590.097467	17.510477
37.794753	1576.861224	17.515495
37.807793	1581.535391	17.520512
37.668720	1566.666406	17.525530
37.802677	1575.338279	17.530547
37.637680	1577.580461	17.535565
37.824588	1566.370507	17.540583
37.696333	1570.828090	17.545600
37.539825	1574.987352	17.550618
37.911256	1579.785270	17.555635
37.799106	1605.410751	17.560653
37.745390	1609.006964	17.565671
38.000032	1607.247022	17.570688
37.816735	1608.888829	17.575706
38.455404	1604.129808	17.580723
37.941091	1618.359161	17.585741
38.087488	1604.487599	17.590759
38.022124	1607.258200	17.595776
38.122837	1602.256192	17.600794
38.126830	1604.626379	17.605811
38.258446	1634.087667	17.610829
38.478147	1638.470111	17.615847
38.438341	1639.463713	17.620864
38.610913	1637.661797	17.625882
38.795811	1627.037326	17.630899
38.171398	1640.584214	17.635917
38.815440	1633.844530	17.640935
38.943103	1629.885925	17.645952
38.454933	1641.449381	17.650970
38.805535	1633.471242	17.655987
39.058694	1632.730928	17.661005
39.128780	1635.955020	17.666023
38.852892	1632.550808	17.671040
38.778242	1639.537335	17.676058
38.713307	1628.110292	17.681075
38.965853	1633.224512	17.686093
39.184425	1634.392426	17.691111
39.235544	1628.172843	17.696128
39.303086	1620.470321	17.701146
39.485053	1611.825336	17.706163
39.322321	1614.326729	17.711181
39.226922	1596.096820	17.716199
39.502054	1586.697618	17.721216
39.223570	1581.068634	17.726234
39.589402	1577.113746	17.731251
39.442803	1582.266436	17.736269
39.420464	1582.658672	17.741287
39.750388	1572.761495	17.746304
39.269005	1582.660234	17.751322
39.607567	1573.221821	17.756339
39.715721	1581.579254	17.761357
39.369385	1582.689385	17.766375
39.335174	1580.132315	17.771392
39.317074	1586.417620	17.776410
40.003327	1592.091122	17.781427
39.915316	1597.151884	17.786445
39.541286	1592.188625	17.791463
39.937085	1597.021991	17.796480
39.484067	1618.132689	17.801498
40.060874	1612.280763	17.806515
39.974319	1610.208696	17.811533
39.873717	1613.407305	17.816551
40.092982	1612.296418	17.821568
40.094391	1618.581771	17.826586
39.985088	1610.332477	17.831603
39.792009	1616.939092	17.836621
39.964821	1618.469832	17.841639
40.292842	1613.920812	17.846656
40.094723	1626.930904	17.851674
40.080682	1613.518321	17.856691
39.967026	1620.485103	17.861709
39.804301	1615.585671	17.866727
40.125744	1613.612927	17.871744
39.996594	1614.496499	17.876762
40.389214	1629.075183	17.881779
40.336174	1642.729948	17.886797
40.512406	1642.776675	17.891815
40.472395	1641.616681	17.896832
40.340467	1655.331234	17.901850
40.400608	1639.137280	17.906867
40.481839	1648.875543	17.911885
40.402382	1653.290759	17.916903
40.636543	1653.012832	17.921920
40.376908	1657.001360	17.926938
41.057732	1647.509100	17.931955
40.525134	1647.552462	17.936973
40.836043	1650.458130	17.941991
40.781223	1645.871838	17.947008
40.919135	1659.640107	17.952026
40.816664	1674.291504	17.957043
41.010916	1680.290492	17.962061
40.856942	1669.518674	17.967079
41.087675	1675.667583	17.972096
40.723036	1682.334624	17.977114
41.277372	1666.197901	17.982131
41.056452	1671.876893	17.987149
41.386076	1667.364571	17.992167
41.289089	1672.475557	17.997184
41.200061	1675.381303	18.002202
41.234087	1671.660220	18.007219
41.056761	1672.869253	18.012237
41.229210	1665.099636	18.017255
41.330810	1674.769382	18.022272
41.478531	1695.845734	18.027290
41.814289	1696.822704	18.032307
41.778764	1699.950387	18.037325
41.783871	1704.327748	18.042343
42.259289	1694.459199	18.047360
41.737158	1677.404741	18.052378
41.656121	1666.970529	18.057395
41.512586	1676.098883	18.062413
42.017958	1687.352109	18.067431
42.248085	1685.799791	18.072448
41.528658	1691.790335	18.077466
41.732989	1692.371382	18.082483
41.838599	1695.965803	18.087501
41.891356	1702.044786	18.092519
42.243220	1704.485361	18.097536
42.067653	1705.490395	18.102554
42.044731	1698.144419	18.107571
41.974522	1697.168576	18.112589
41.761299	1703.499208	18.117607
41.791085	1698.812883	18.122624
41.969391	1722.815167	18.127642
42.283004	1720.397670	18.132659
42.461760	1724.012682	18.137677
42.472294	1730.021327	18.142695
42.832060	1720.490555	18.147712
42.737525	1725.580718	18.152730
42.860773	1727.083979	18.157747
42.460530	1733.496365	18.162765
42.321410	1732.238904	18.167783
42.736068	1723.291667	18.172800
42.437200	1727.598741	18.177818
42.703913	1724.806448	18.182835
42.504139	1728.002021	18.187853
42.379719	1727.874883	18.192871
42.502860	1720.917766	18.197888
42.376593	1735.904955	18.202906
42.770548	1744.776155	18.207923
42.917867	1752.916638	18.212941
42.920251	1758.957271	18.217959
42.957121	1749.695859	18.222976
42.698056	1757.742269	18.227994
43.157278	1751.477998	18.233011
43.075141	1762.415176	18.238029
43.136981	1753.502166	18.243047
43.032284	1744.428516	18.248064
43.043623	1749.217848	18.253082
43.326943	1765.605922	18.258099
43.492377	1783.250101	18.263117
43.459411	1787.426689	18.268135
43.739144	1783.384796	18.273152
43.771985	1791.313091	18.278170
43.559154	1777.339768	18.283187
43.756570	1788.403855	18.288205
43.676610	1787.420909	18.293223
43.474378	1778.326610	18.298240
43.645420	1785.009733	18.303258
43.780515	1783.345135	18.308275
43.921434	1780.246465	18.313293
44.181883	1777.096482	18.318311
44.108734	1770.718890	18.323328
43.990772	1784.205589	18.328346
43.893222	1777.849191	18.333363
44.046608	1778.030920	18.338381
43.974997	1784.104602	18.343399
44.271594	1780.377798	18.348416
43.814841	1789.884178	18.353434
43.918262	1778.320833	18.358451
44.235538	1785.139522	18.363469
44.138484	1791.580664	18.368487
44.408942	1778.192561	18.373504
44.258666	1781.520262	18.378522
44.337896	1785.671876	18.383539
44.450291	1777.756821	18.388557
44.064015	1791.328793	18.393575
44.604184	1801.605136	18.398592
44.895631	1811.842495	18.403610
44.724024	1809.304938	18.408627
45.018692	1803.578165	18.413645
44.958586	1811.925597	18.418663
44.982101	1782.254579	18.423680
44.621962	1785.781718	18.428698
44.435204	1776.641691	18.433715
45.116645	1785.950813	18.438733
44.895276	1805.849688	18.443751
45.249598	1795.954763	18.448768
44.923454	1787.387564	18.453786
44.919235	1792.348506	18.458803
45.101329	1806.923190	18.463821
44.760698	1810.454303	18.468839
45.512748	1802.695217	18.473856
45.389096	1800.167318	18.478874
45.156311	1811.495891	18.483891
45.231120	1805.105700	18.488909
44.772150	1813.037718	18.493927
45.223828	1813.289075	18.498944
45.341674	1806.969104	18.503962
45.401793	1811.749891	18.508979
45.462740	1805.423264	18.513997
45.498206	1814.302913	18.519015
45.521899	1804.068996	18.524032
45.412075	1810.149570	18.529050
45.350557	1803.392552	18.534067
45.608893	1824.386949	18.539085
45.632860	1834.676422	18.544103
45.862317	1839.075464	18.549120
45.678383	1841.665227	18.554138
45.925353	1836.772745	18.559155
46.245419	1833.214446	18.564173
45.759340	1844.034408	18.569191
45.902829	1841.970455	18.574208
45.942638	1829.489049	18.579226
45.725733	1836.463748	18.584243
45.729479	1837.977427	18.589261
46.005297	1847.265541	18.594279
46.051907	1865.124629	18.599296
46.283132	1863.151296	18.604314
46.090256	1870.666494	18.609331
46.168919	1867.058590	18.614349
46.155023	1869.437966	18.619367
46.398435	1860.082977	18.624384
46.633125	1866.409891	18.629402
46.453084	1863.099672	18.634419
47.022239	1856.569265	18.639437
46.801132	1862.516585	18.644455
47.035759	1854.158813	18.649472
46.930907	1853.935737	18.654490
46.822127	1855.969989	18.659507
47.016053	1850.158583	18.664525
46.737080	1866.186522	18.669543
46.978514	1847.514795	18.674560
47.309462	1844.713809	18.679578
46.933913	1848.178920	18.684595
47.069859	1851.387050	18.689613
46.915314	1855.019068	18.694631
47.128351	1854.739788	18.699648
46.985917	1842.484080	18.704666
47.051816	1852.058169	18.709683
47.268851	1846.953362	18.714701
47.099934	1872.359470	18.719719
47.618248	1871.427407	18.724736
47.681428	1878.961552	18.729754
47.338340	1878.815013	18.734771
47.673015	1871.600698	18.739789
47.404957	1883.405329	18.744807
47.475680	1881.974376	18.749824
47.868083	1878.439926	18.754842
47.676492	1876.615041	18.759859
47.996302	1872.219064	18.764877
47.730693	1876.616053	18.769895
48.044329	1874.183584	18.774912
47.953727	1875.771307	18.779930
47.959911	1876.055172	18.784947
48.099486	1863.912574	18.789965
47.750192	1874.399256	18.794983
48.232481	1867.699424	18.800000
48.212065	1873.797229	18.805018
48.135946	1881.770481	18.810035
47.979708	1868.258421	18.815053
48.007772	1876.037287	18.820071
48.117657	1873.159856	18.825088
48.174891	1867.534639	18.830106
48.149129	1876.806370	18.835123
48.241030	1866.691318	18.840141
48.060650	1881.135891	18.845159
48.118494	1881.974711	18.850176
48.193242	1901.544107	18.855194
48.146014	1903.925659	18.860211
48.712948	1903.234400	18.865229
48.558031	1911.121912	18.870247
48.449607	1907.687780	18.875264
48.630501	1913.004667	18.880282
48.451998	1908.592188	18.885299
48.967031	1922.490915	18.890317
48.875967	1932.167961	18.895335
49.359161	1938.883964	18.900352
49.291006	1938.484344	18.905370
49.247759	1920.053786	18.910387
49.273749	1913.729540	18.915405
49.104370	1911.503884	18.920423
48.923313	1898.643113	18.925440
49.394740	1915.798166	18.930458
49.414271	1929.115192	18.935475
49.401406	1929.931468	18.940493
49.260959	1941.759842	18.945511
49.215810	1933.600816	18.950528
49.430861	1936.432946	18.955546
49.490018	1929.125679	18.960563
49.478094	1932.211891	18.965581
49.345316	1933.652176	18.970599
49.306632	1932.941088	18.975616
49.365846	1942.791607	18.980634
49.780941	1938.140505	18.985651
49.896123	1949.411330	18.990669
49.276219	1956.049198	18.995687
49.898351	1961.646551	19.000704
50.065498	1953.305778	19.005722
49.638020	1962.768271	19.010739
49.871315	1958.898920	19.015757
49.919809	1962.820298	19.020775
49.878566	1963.523900	19.025792
50.025744	1963.267706	19.030810
50.010284	1960.624988	19.035827
50.247556	1948.267732	19.040845
50.328307	1959.975106	19.045863
50.351791	1963.607862	19.050880
50.787970	1975.053264	19.055898
50.635388	1976.936415	19.060915
50.791508	1963.132968	19.065933
50.650423	1959.913265	19.070951
50.376074	1956.606266	19.075968
50.687491	1957.544663	19.080986
50.988794	1978.735370	19.086003
51.116672	1976.931102	19.091021
51.206957	1972.962635	19.096039
50.890467	1957.135951	19.101056
50.763716	1948.210423	19.106074
50.562223	1952.760819	19.111091
51.071567	1958.047365	19.116109
51.249364	1966.830469	19.121127
51.079952	1974.504015	19.126144
51.575116	1972.948728	19.131162
51.269080	1974.539357	19.136179
51.419708	1973.985282	19.141197
51.460008	1976.774497	19.146215
51.305742	1970.121864	19.151232
51.597951	1968.141938	19.156250
51.294799	1982.606192	19.161267
51.434739	1973.612158	19.166285
51.570837	1972.901511	19.171303
51.387757	1971.722618	19.176320
51.630407	1968.464525	19.181338
51.400619	1972.773239	19.186355
51.487266	1974.316973	19.191373
51.217425	1970.335146	19.196391
51.564810	1985.756761	19.201408
51.807329	1993.783086	19.206426
52.075166	2005.328513	19.211443
52.006179	2007.419367	19.216461
51.791513	1994.974470	19.221479
51.877041	2005.604279	19.226496
52.060481	1999.678857	19.231514
52.377064	1992.796164	19.236531
52.290669	1992.932759	19.241549
51.982515	1997.729077	19.246567
52.299226	1998.042867	19.251584
52.420793	1988.556990	19.256602
52.132691	1996.228238	19.261619
52.461248	2006.923118	19.266637
52.559200	2027.060833	19.271655
52.707391	2020.346569	19.276672
52.978186	2024.950667	19.281690
52.741573	2026.046476	19.286707
52.745089	2013.128637	19.291725
52.485834	2022.666596	19.296743
52.351550	2021.457106	19.301760
52.610983	2016.175575	19.306778
52.462908	2026.006508	19.311795
52.607887	2019.232976	19.316813
52.789376	2026.119844	19.321831
53.074495	2050.899305	19.326848
53.451414	2046.215715	19.331866
53.237578	2054.680619	19.336883
53.451189	2051.081825	19.341901
53.284411	2054.760679	19.346919
53.187898	2052.981963	19.351936
53.231699	2041.845598	19.356954
53.193332	2057.896728	19.361971
53.409741	2058.681953	19.366989
53.389165	2051.473865	19.372007
53.332363	2059.735959	19.377024
53.364856	2054.647139	19.382042
53.420179	2056.845603	19.387059
54.096871	2064.798792	19.392077
54.069592	2067.745109	19.397095
54.084519	2057.245757	19.402112
54.298040	2047.627188	19.407130
54.305072	2046.625631	19.412147
54.197055	2046.263042	19.417165
54.281256	2029.343514	19.422183
54.089290	2035.464026	19.427200
54.478184	2037.275773	19.432218
53.937491	2048.272138	19.437235
53.935102	2041.836734	19.442253
54.022613	2042.074595	19.447271
54.240084	2062.192511	19.452288
54.316639	2063.015772	19.457306
54.360572	2076.315669	19.462323
54.450817	2073.641913	19.467341
54.658600	2066.560224	19.472359
54.489156	2066.886261	19.477376
54.657196	2058.431229	19.482394
54.716372	2069.575786	19.487411
54.653673	2069.527686	19.492429
54.392290	2062.574309	19.497447
54.457612	2085.346102	19.502464
54.678038	2089.901619	19.507482
54.887607	2097.359043	19.512499
54.915517	2094.286982	19.517517
55.146766	2097.226685	19.522535
55.025134	2097.783435	19.527552
55.234766	2097.755618	19.532570
54.969689	2096.397076	19.537587
55.074715	2103.355170	19.542605
55.554066	2117.159877	19.547623
55.528646	2128.375391	19.552640
55.749635	2130.849499	19.557658
55.774826	2130.664672	19.562675
55.636597	2108.329415	19.567693
55.649320	2097.474059	19.572711
55.566122	2111.238689	19.577728
56.040372	2121.689386	19.582746
56.276836	2127.815549	19.587763
56.286404	2093.410815	19.592781
56.244214	2089.385570	19.597799
55.989082	2088.970929	19.602816
56.021669	2086.203322	19.607834
56.145301	2079.752523	19.612851
56.017504	2069.940596	19.617869
56.280116	2079.561336	19.622887
56.238622	2075.714540	19.627904
56.572411	2074.803243	19.632922
56.019997	2078.911729	19.637939
56.455947	2089.499086	19.642957
56.531974	2099.748980	19.647975
56.331326	2107.933358	19.652992
56.864595	2104.102655	19.658010
56.787709	2109.535452	19.663027
56.674084	2104.117523	19.668045
56.733969	2099.406604	19.673063
56.697782	2107.227304	19.678080
57.048359	2103.052891	19.683098
56.705666	2112.125965	19.688115
56.929511	2104.115873	19.693133
57.229979	2098.262994	19.698151
56.780919	2107.131995	19.703168
57.166686	2105.071057	19.708186
57.228097	2104.207130	19.713203
57.119028	2104.204181	19.718221
57.097912	2102.739085	19.723239
56.958006	2100.186981	19.728256
57.354009	2106.020250	19.733274
57.279252	2124.240394	19.738291
57.401855	2131.669229	19.743309
57.525209	2130.568095	19.748327
57.245580	2145.093258	19.753344
57.609046	2132.478957	19.758362
57.438835	2138.888655	19.763379
57.398629	2141.711979	19.768397
57.939661	2142.140239	19.773415
57.895887	2141.746950	19.778432
57.573886	2137.940940	19.783450
57.532840	2148.196168	19.788467
57.891112	2160.697170	19.793485
58.167008	2160.052318	19.798503
57.941781	2167.288078	19.803520
58.279233	2160.833035	19.808538
58.058328	2167.677953	19.813555
57.872689	2161.740533	19.818573
58.387813	2157.080490	19.823591
58.178776	2165.654031	19.828608
58.460807	2191.435563	19.833626
58.459318	2191.026878	19.838643
58.560324	2205.311265	19.843661
58.869980	2188.007135	19.848679
58.295596	2201.983119	19.853696
58.694157	2194.093782	19.858714
58.606270	2189.094121	19.863731
58.878226	2189.492927	19.868749
58.667352	2186.065628	19.873767
58.703730	2192.336999	19.878784
58.883721	2194.115222	19.883802
58.802924	2201.776328	19.888819
58.899822	2216.125882	19.893837
59.345082	2211.392012	19.898855
58.941933	2218.438283	19.903872
59.135943	2221.148756	19.908890
59.050867	2221.742158	19.913907
59.071496	2222.313195	19.918925
59.688025	2227.847047	19.923943
59.610306	2241.930285	19.928960
59.954458	2245.039224	19.933978
60.039348	2243.093899	19.938995
59.477105	2236.204152	19.944013
59.969772	2236.016353	19.949031
59.944012	2244.050205	19.954048
60.181681	2244.667650	19.959066
59.940506	2246.497315	19.964083
59.986892	2254.851613	19.969101
60.066944	2242.991146	19.974119
60.272586	2241.629101	19.979136
60.577450	2242.677114	19.984154
60.393466	2249.008037	19.989171
60.379721	2247.461517	19.994189
60.706196	2240.401718	19.999207
60.329358	2239.602955	20.004224
60.208714	2239.888962	20.009242
60.421812	2246.938440	20.014259
60.310624	2245.213956	20.019277
60.592609	2246.436311	20.024295
60.619827	2248.109115	20.029312
60.664878	2254.791310	20.034330
60.596123	2245.437091	20.039347
60.965024	2265.251894	20.044365
61.350511	2257.473160	20.049383
61.093833	2266.776458	20.054400
61.070367	2266.407459	20.059418
61.301384	2259.860795	20.064435
61.135729	2267.982259	20.069453
61.233617	2266.053736	20.074471
61.273480	2269.510117	20.079488
61.366217	2269.226417	20.084506
61.275188	2276.375541	20.089523
61.745856	2276.269911	20.094541
62.006810	2268.711616	20.099559
61.853421	2271.796862	20.104576
61.364390	2273.456034	20.109594
62.082934	2269.793180	20.114611
61.758297	2266.270734	20.119629
62.238723	2261.237050	20.124647
61.938785	2270.796603	20.129664
61.931774	2276.292259	20.134682
61.994574	2259.776259	20.139699
61.711866	2269.099442	20.144717
62.052531	2262.717783	20.149735
61.840326	2262.532271	20.154752
61.977687	2266.084013	20.159770
62.300821	2270.250358	20.164787
61.771406	2273.967434	20.169805
62.146656	2287.862061	20.174823
62.225534	2302.419092	20.179840
62.487617	2296.845994	20.184858
62.354397	2300.169518	20.189875
62.258103	2301.743249	20.194893
62.817206	2308.079975	20.199911
62.740635	2322.885213	20.204928
62.908381	2330.905558	20.209946
62.961919	2322.266478	20.214963
62.973783	2326.262230	20.219981
63.355260	2322.105640	20.224999
63.161942	2327.791495	20.230016
62.713542	2323.313379	20.235034
63.425509	2324.699218	20.240051
62.895813	2330.066653	20.245069
63.067421	2323.613602	20.250087
63.286326	2323.104476	20.255104
63.009103	2332.734388	20.260122
63.290130	2339.111542	20.265139
63.500757	2354.841684	20.270157
63.741479	2360.696674	20.275175
63.407925	2358.359473	20.280192
63.724260	2358.052699	20.285210
63.914656	2355.161549	20.290227
63.783946	2363.301877	20.295245
64.128858	2360.347540	20.300263
64.332655	2358.095338	20.305280
64.197807	2356.490245	20.310298
63.947863	2355.583138	20.315315
64.315484	2351.482239	20.320333
64.239373	2348.343333	20.325351
64.462964	2364.141426	20.330368
64.523675	2363.112408	20.335386
64.413116	2364.124421	20.340403
64.435072	2378.699258	20.345421
64.687758	2372.588804	20.350439
64.687638	2377.498161	20.355456
64.378428	2381.388597	20.360474
64.536570	2364.543417	20.365491
64.691229	2375.151458	20.370509
64.906166	2373.266397	20.375527
64.634508	2371.996191	20.380544
64.617619	2373.979675	20.385562
64.834591	2387.490603	20.390579
64.470604	2407.855901	20.395597
64.754543	2413.521526	20.400615
65.240267	2401.707933	20.405632
64.931233	2413.952160	20.410650
65.298920	2403.596102	20.415667
65.321622	2417.042072	20.420685
65.522013	2418.720317	20.425703
65.419590	2430.809683	20.430720
65.776523	2423.199818	20.435738
65.762300	2414.984461	20.440755
65.945008	2413.891933	20.445773
66.217703	2420.583523	20.450791
66.418925	2422.238038	20.455808
66.581627	2415.733664	20.460826
66.606578	2392.511394	20.465843
66.566657	2391.202657	20.470861
66.402603	2382.108184	20.475879
66.642179	2379.851846	20.480896
66.564273	2376.966508	20.485914
66.648358	2376.248405	20.490931
66.366961	2374.945928	20.495949
66.565018	2372.772513	20.500967
66.745915	2374.425544	20.505984
66.189676	2373.178697	20.511002
66.300662	2371.119854	20.516019
66.178678	2383.280736	20.521037
66.584982	2394.492107	20.526055
66.618124	2400.741271	20.531072
66.602503	2405.731772	20.536090
66.777980	2400.814322	20.541107
66.830932	2414.005322	20.546125
66.908232	2416.175164	20.551143
67.125528	2426.737069	20.556160
67.127770	2435.458780	20.561178
67.576028	2432.381755	20.566195
67.353041	2431.272117	20.571213
67.374462	2435.572367	20.576231
67.188041	2440.653833	20.581248
67.707900	2441.192461	20.586266
67.632328	2434.770915	20.591283
67.429987	2449.190445	20.596301
67.650050	2442.010651	20.601319
67.637119	2446.619228	20.606336
67.559614	2467.763293	20.611354
67.694680	2471.106213	20.616371
67.525852	2465.546709	20.621389
67.836921	2462.144659	20.626407
67.842785	2467.841280	20.631424
67.903503	2491.441172	20.636442
68.518765	2489.101307	20.641459
68.493183	2505.487561	20.646477
68.668229	2504.923282	20.651495
68.810190	2501.515941	20.656512
68.500233	2506.522737	20.661530
68.600162	2497.814799	20.666547
68.792152	2502.374195	20.671565
68.729250	2491.536900	20.676583
68.312942	2497.536056	20.681600
68.744272	2499.171189	20.686618
69.124581	2489.417180	20.691635
68.984316	2492.316311	20.696653
68.877358	2498.955210	20.701671
69.208499	2486.088538	20.706688
68.945074	2488.345765	20.711706
69.103884	2496.367628	20.716723
69.291078	2525.441132	20.721741
69.405913	2521.249921	20.726759
69.644223	2518.456505	20.731776
69.356235	2534.523582	20.736794
69.281825	2522.643470	20.741811
69.320966	2521.038143	20.746829
69.602245	2531.981657	20.751847
70.117667	2534.328645	20.756864
70.044928	2543.322748	20.761882
70.073276	2542.055026	20.766899
69.967237	2539.908845	20.771917
70.140864	2556.279119	20.776935
70.201477	2543.082683	20.781952
70.078931	2557.322831	20.786970
70.441375	2543.843847	20.791987
70.153817	2546.937174	20.797005
70.237331	2553.246807	20.802023
70.227021	2544.029387	20.807040
70.354706	2540.079974	20.812058
70.395852	2555.147496	20.817075
70.822480	2573.772012	20.822093
71.058592	2563.226798	20.827111
71.293372	2564.554250	20.832128
71.128908	2572.085727	20.837146
71.268145	2560.490094	20.842163
71.307825	2560.532645	20.847181
71.342749	2561.620585	20.852199
71.200055	2552.181993	20.857216
71.151375	2553.056719	20.862234
71.366039	2551.601174	20.867251
71.326825	2557.843066	20.872269
71.302909	2559.385616	20.877287
71.550887	2559.195934	20.882304
71.440839	2569.279964	20.887322
71.741309	2564.705159	20.892339
71.593628	2560.358360	20.897357
71.750968	2564.451331	20.902375
72.133313	2556.552589	20.907392
71.713074	2561.100298	20.912410
71.986472	2576.601990	20.917427
71.916703	2592.182023	20.922445
71.973194	2588.926737	20.927463
72.693173	2590.567766	20.932480
71.999534	2600.357081	20.937498
72.456745	2587.436391	20.942515
72.414273	2587.526655	20.947533
72.483998	2585.163648	20.952551
72.497747	2587.537159	20.957568
72.256836	2591.399451	20.962586
72.517268	2593.285249	20.967603
72.646760	2600.153151	20.972621
72.745054	2614.867868	20.977639
72.740178	2618.358998	20.982656
72.619092	2620.529043	20.987674
72.716387	2621.974394	20.992691
72.684246	2616.267961	20.997709
72.687491	2628.397275	21.002727
73.238928	2637.792189	21.007744
73.274432	2647.858568	21.012762
73.456904	2652.066336	21.017779
73.209371	2662.262817	21.022797
73.140146	2651.145586	21.027815
73.441405	2652.772375	21.032832
73.215289	2673.636799	21.037850
73.630847	2681.945842	21.042867
73.783301	2671.270726	21.047885
73.666482	2686.684518	21.052903
74.025802	2665.635432	21.057920
74.073115	2676.287556	21.062938
74.417207	2668.456999	21.067955
74.126918	2669.515001	21.072973
74.084487	2670.774970	21.077991
74.564934	2687.950738	21.083008
74.264624	2691.872873	21.088026
74.884079	2698.008999	21.093043
74.784541	2699.556543	21.098061
75.033187	2699.597236	21.103079
75.044559	2695.716674	21.108096
74.962968	2697.176401	21.113114
75.042257	2686.484623	21.118131
75.257570	2691.446259	21.123149
75.207131	2702.375938	21.128167
75.518296	2690.232038	21.133184
75.355867	2678.656887	21.138202
74.943379	2671.445702	21.143219
75.530066	2671.796694	21.148237
75.412888	2692.679957	21.153255
75.498133	2686.514266	21.158272
75.496939	2697.979648	21.163290
75.409070	2696.630544	21.168307
75.475676	2696.531929	21.173325
75.548974	2693.685346	21.178343
75.663509	2688.724815	21.183360
75.517095	2698.467044	21.188378
75.587094	2715.403089	21.193395
76.112212	2722.805795	21.198413
75.738746	2730.384841	21.203431
75.714519	2725.005915	21.208448
75.540659	2731.981252	21.213466
75.963941	2743.382910	21.218483
76.056368	2757.136657	21.223501
76.067729	2758.200838	21.228519
76.487054	2754.656385	21.233536
76.458396	2765.846158	21.238554
76.639996	2767.685554	21.243571
76.647862	2772.814814	21.248589
76.989171	2785.225451	21.253607
76.904278	2778.134243	21.258624
76.646365	2785.569030	21.263642
77.088384	2774.744613	21.268659
77.365165	2774.049252	21.273677
77.182580	2769.602549	21.278695
77.239155	2772.384601	21.283712
77.413722	2773.794046	21.288730
77.533301	2772.282059	21.293747
77.633095	2765.019026	21.298765
77.879024	2770.415533	21.303783
77.737833	2764.848360	21.308800
77.757219	2769.771258	21.313818
77.747466	2772.027406	21.318835
77.947022	2772.535320	21.323853
77.833283	2795.597149	21.328871
77.971768	2790.078975	21.333888
78.309864	2793.812013	21.338906
78.418366	2781.979611	21.343923
78.329867	2781.581638	21.348941
78.780640	2789.535076	21.353959
78.878255	2774.487093	21.358976
78.657258	2786.350232	21.363994
78.987276	2772.757429	21.369011
79.129891	2778.230198	21.374029
78.946361	2785.067869	21.379047
78.976110	2785.376313	21.384064
78.625675	2790.079725	21.389082
78.554980	2786.114685	21.394099
79.113641	2784.599540	21.399117
79.015135	2780.884365	21.404135
79.249876	2774.900107	21.409152
79.053781	2783.527006	21.414170
79.384266	2776.619707	21.419187
79.263006	2799.987169	21.424205
79.241581	2811.305618	21.429223
79.887241	2806.106169	21.434240
79.682052	2814.958727	21.439258
79.672972	2811.268615	21.444275
79.546036	2811.203223	21.449293
79.648578	2809.634953	21.454311
80.077836	2809.537502	21.459328
79.992076	2816.076408	21.464346
79.888097	2831.739240	21.469363
80.575078	2839.090235	21.474381
80.430689	2850.683980	21.479399
80.484302	2840.708089	21.484416
80.494995	2842.786354	21.489434
80.423519	2840.002162	21.494451
80.749117	2836.808530	21.499469
80.548310	2842.716034	21.504487
80.551504	2837.675666	21.509504
80.218166	2844.803923	21.514522
80.372599	2844.692874	21.519539
80.622373	2854.128170	21.524557
80.501391	2875.841414	21.529575
80.827769	2867.768932	21.534592
80.940378	2865.733362	21.539610
81.153769	2883.478995	21.544627
81.074582	2896.073993	21.549645
81.029121	2908.081511	21.554663
81.326936	2897.704786	21.559680
81.341784	2903.342719	21.564698
81.559781	2906.718139	21.569715
82.052667	2908.784809	21.574733
81.795521	2921.203682	21.579751
81.848465	2927.025129	21.584768
82.088521	2925.315348	21.589786
82.269047	2926.330538	21.594803
82.422858	2919.774655	21.599821
82.506688	2919.456179	21.604839
82.600594	2908.800454	21.609856
82.815515	2921.767064	21.614874
82.604524	2919.692628	21.619891
82.936008	2918.676242	21.624909
82.548171	2925.825029	21.629927
82.907292	2914.967318	21.634944
83.039772	2912.394445	21.639962
82.931149	2916.611738	21.644979
83.231784	2910.592532	21.649997
83.236435	2908.272103	21.655015
83.370771	2909.049227	21.660032
83.315467	2918.720435	21.665050
83.062617	2913.536798	21.670067
83.590045	2905.165565	21.675085
83.367817	2905.329334	21.680103
83.528056	2909.979666	21.685120
83.778095	2904.237562	21.690138
83.632269	2913.075206	21.695155
84.267890	2920.654692	21.700173
84.145787	2931.741498	21.705191
84.281359	2922.022300	21.710208
84.064309	2919.268386	21.715226
84.158259	2931.954587	21.720243
84.438780	2928.079815	21.725261
84.072988	2937.548037	21.730279
84.316811	2932.602206	21.735296
84.371118	2933.895542	21.740314
84.230499	2931.147531	21.745331
84.452534	2922.251529	21.750349
84.156626	2934.255741	21.755367
84.425376	2945.750640	21.760384
84.487280	2955.247426	21.765402
84.472692	2961.132361	21.770419
84.702066	2957.134368	21.775437
84.433000	2969.124889	21.780455
84.973637	2980.172123	21.785472
84.963695	3006.123587	21.790490
85.275894	2997.375209	21.795507
85.278883	2993.876640	21.800525
85.455677	3005.481434	21.805543
85.395315	2996.942717	21.810560
85.400877	3011.722966	21.815578
85.470918	3026.140531	21.820595
85.854605	3022.427064	21.825613
85.477596	3024.244657	21.830631
85.610808	3026.727412	21.835648
86.004118	3040.468057	21.840666
86.122277	3050.973854	21.845683
86.389817	3050.755876	21.850701
86.239018	3067.125754	21.855719
86.533283	3048.591965	21.860736
86.816173	3052.222171	21.865754
86.567605	3063.950694	21.870771
86.775020	3055.034917	21.875789
86.840785	3053.755678	21.880807
86.783356	3049.395914	21.885824
87.169120	3051.164243	21.890842
86.919917	3052.765584	21.895859
87.002475	3045.754527	21.900877
87.087317	3061.156220	21.905895
87.323470	3071.535444	21.910912
87.599201	3068.765851	21.915930
87.456526	3067.896654	21.920947
87.816747	3073.872114	21.925965
87.869556	3071.278093	21.930983
87.606991	3069.712166	21.936000
87.724041	3072.044896	21.941018
87.784703	3074.801969	21.946035
87.898268	3072.558543	21.951053
87.837876	3082.544542	21.956071
87.967787	3098.656510	21.961088
88.248180	3096.218921	21.966106
88.118068	3100.953375	21.971123
88.233365	3099.782658	21.976141
88.315908	3096.492426	21.981159
88.469141	3103.142024	21.986176
88.563713	3116.124066	21.991194
88.838442	3125.965403	21.996211
89.317622	3132.822631	22.001229
88.951591	3132.778058	22.006247
89.043347	3130.313119	22.011264
89.048152	3132.689719	22.016282
88.934083	3132.828375	22.021299
89.350213	3123.098130	22.026317
89.056197	3129.753770	22.031335
89.118941	3133.052523	22.036352
89.273929	3132.116975	22.041370
89.367877	3150.974638	22.046387
89.547275	3150.016317	22.051405
89.248687	3158.671579	22.056423
89.573862	3163.542700	22.061440
89.892599	3159.689306	22.066458
89.768541	3179.890759	22.071475
90.267183	3186.835375	22.076493
90.064879	3176.509100	22.081511
89.773891	3183.504115	22.086528
90.264659	3178.968788	22.091546
90.088507	3188.157559	22.096563
90.437612	3194.970268	22.101581
90.603208	3212.462754	22.106599
90.637764	3215.348307	22.111616
90.727290	3217.497440	22.116634
90.692675	3216.762826	22.121651
91.061508	3210.935581	22.126669
90.947403	3216.056126	22.131687
90.803116	3218.855348	22.136704
91.223581	3233.366701	22.141722
91.363462	3240.539257	22.146739
91.245378	3233.205324	22.151757
91.029797	3246.688480	22.156775
91.351312	3246.024513	22.161792
92.099967	3253.659309	22.166810
91.784213	3259.977065	22.171827
92.308808	3267.037939	22.176845
92.145584	3270.187893	22.181863
92.193849	3267.087955	22.186880
92.103261	3271.073556	22.191898
91.957939	3270.511565	22.196915
92.437893	3258.962528	22.201933
92.330879	3270.586043	22.206951
92.215128	3270.806781	22.211968
92.678646	3279.235172	22.216986
92.280306	3294.860479	22.222003
92.646918	3291.174055	22.227021
92.974663	3295.860733	22.232039
92.835257	3297.421777	22.237056
92.919835	3299.676336	22.242074
92.997118	3316.681141	22.247091
93.211908	3311.392110	22.252109
93.233403	3326.674384	22.257127
93.049649	3326.430037	22.262144
93.683306	3321.037235	22.267162
93.370278	3323.218323	22.272179
93.600474	3338.943259	22.277197
94.044777	3348.153549	22.282215
93.940707	3354.082804	22.287232
94.059457	3351.384606	22.292250
93.925594	3360.561234	22.297267
94.239177	3346.050917	22.302285
94.395508	3341.856790	22.307303
94.106566	3353.130210	22.312320
94.514020	3352.872612	22.317338
94.373838	3345.749039	22.322355
94.547288	3350.118141	22.327373
94.871621	3369.837715	22.332391
94.866722	3374.596343	22.337408
95.247532	3375.282269	22.342426
94.836376	3379.512537	22.347443
95.290032	3368.397127	22.352461
95.057339	3372.065578	22.357479
94.840518	3380.026680	22.362496
95.366266	3369.341092	22.367514
95.176154	3377.493813	22.372531
95.555114	3393.306005	22.377549
95.579073	3407.320654	22.382567
95.626882	3412.306888	22.387584
96.034032	3397.730466	22.392602
95.763181	3412.390784	22.397619
96.067524	3405.725721	22.402637
96.035757	3399.443085	22.407655
95.777030	3410.519785	22.412672
96.164867	3423.973746	22.417690
96.291729	3437.326162	22.422707
96.437071	3447.322082	22.427725
96.517176	3441.571468	22.432743
96.499823	3440.555611	22.437760
96.554448	3445.073489	22.442778
96.822052	3458.342121	22.447795
96.911052	3460.061853	22.452813
96.906077	3471.096561	22.457831
96.689458	3475.048820	22.462848
97.054137	3466.915626	22.467866
96.919238	3491.213843	22.472883
97.218924	3499.000605	22.477901
97.465749	3503.094517	22.482919
97.464296	3505.095360	22.487936
97.782814	3496.672935	22.492954
97.679769	3512.134956	22.497971
98.377264	3522.178186	22.502989
98.260613	3524.985645	22.508007
98.188259	3525.981417	22.513024
98.354726	3521.223154	22.518042
98.225634	3514.540626	22.523059
98.426199	3516.030960	22.528077
98.649563	3519.942964	22.533095
98.351989	3525.798517	22.538112
98.777097	3516.061864	22.543130
98.467602	3521.496087	22.548147
98.874483	3539.376076	22.553165
99.153945	3548.240684	22.558183
98.883605	3549.797459	22.563200
98.987640	3544.757288	22.568218
99.082137	3552.936309	22.573235
99.210567	3541.738109	22.578253
99.556387	3546.171824	22.583271
99.290434	3554.633312	22.588288
99.821766	3566.317322	22.593306
99.797559	3573.221205	22.598323
100.026555	3577.229088	22.603341
100.329342	3565.542076	22.608359
100.098456	3568.924724	22.613376
100.019749	3573.384450	22.618394
99.796717	3572.260567	22.623411
100.069973	3567.118670	22.628429
100.274231	3585.197801	22.633447
100.657384	3599.608480	22.638464
100.761996	3597.392364	22.643482
100.730817	3607.466888	22.648499
100.439418	3608.886999	22.653517
101.049602	3604.610986	22.658535
100.621437	3612.406099	22.663552
100.815318	3614.171272	22.668570
100.928949	3625.398798	22.673587
101.142146	3627.470843	22.678605
101.242385	3634.345470	22.683623
101.252830	3634.336832	22.688640
101.744198	3642.510831	22.693658
101.545729	3657.151196	22.698675
101.778696	3665.003753	22.703693
101.883444	3655.189866	22.708711
101.939606	3653.683970	22.713728
101.888350	3649.819436	22.718746
101.756014	3662.832638	22.723763
102.433815	3673.174905	22.728781
102.839398	3675.788981	22.733799
102.818785	3673.550341	22.738816
103.006060	3682.864764	22.743834
102.896182	3682.798220	22.748851
102.635521	3690.624090	22.753869
103.235906	3664.243931	22.758887
103.227122	3674.887633	22.763904
103.298468	3672.557234	22.768922
103.417711	3666.658690	22.773939
103.239504	3677.703869	22.778957
103.420083	3672.520073	22.783975
103.307900	3677.177118	22.788992
104.000241	3681.518644	22.794010
103.890397	3697.417764	22.799027
104.029047	3702.779805	22.804045
104.142999	3686.416100	22.809063
104.035440	3693.923341	22.814080
104.111359	3694.521807	22.819098
104.030911	3686.829213	22.824115
104.093864	3692.286709	22.829133
104.522801	3701.419433	22.834151
104.505088	3723.128474	22.839168
104.747626	3727.577928	22.844186
104.775378	3721.063032	22.849203
105.187362	3721.382919	22.854221
105.355656	3707.708844	22.859239
105.213699	3715.579520	22.864256
105.515340	3716.735938	22.869274
105.340588	3720.078202	22.874291
105.317504	3716.653634	22.879309
105.277483	3709.317241	22.884327
105.314935	3716.447363	22.889344
105.672435	3704.439992	22.894362
105.773386	3726.259131	22.899379
105.858614	3746.025994	22.904397
106.205175	3737.040417	22.909415
106.086626	3745.177995	22.914432
106.283561	3750.953996	22.919450
106.108596	3741.061931	22.924467
106.362984	3747.275604	22.929485
106.294865	3741.848236	22.934503
106.133619	3760.460236	22.939520
106.441044	3772.573459	22.944538
106.371619	3777.749222	22.949555
106.314097	3788.304016	22.954573
106.846085	3795.341944	22.959591
106.753133	3805.358012	22.964608
106.654071	3808.615065	22.969626
106.855853	3814.440665	22.974643
107.076967	3830.409877	22.979661
107.394997	3836.315285	22.984679
107.581661	3837.940033	22.989696
108.062130	3833.089119	22.994714
108.162226	3837.724951	22.999731
107.953289	3862.049746	23.004749
108.381986	3858.011075	23.009767
108.555561	3864.682950	23.014784
108.404053	3863.606640	23.019802
108.492784	3862.049115	23.024819
108.611653	3864.118142	23.029837
108.708238	3856.820468	23.034855
108.868932	3863.293791	23.039872
108.558591	3862.581871	23.044890
109.038608	3852.260387	23.049907
108.561618	3877.309222	23.054925
108.917616	3872.520624	23.059943
108.794085	3882.041286	23.064960
108.566404	3895.332651	23.069978
109.155922	3912.566422	23.074995
109.446314	3923.386804	23.080013
109.504892	3919.458271	23.085031
109.462265	3933.320407	23.090048
109.855073	3943.001862	23.095066
110.113492	3940.655752	23.100083
110.253377	3944.155582	23.105101
110.458770	3940.822759	23.110119
110.559278	3946.069034	23.115136
110.754043	3941.587761	23.120154
110.947740	3939.957635	23.125171
110.654215	3945.798546	23.130189
110.933966	3934.546025	23.135207
110.935392	3945.739767	23.140224
110.657852	3938.452935	23.145242
110.894274	3953.417593	23.150259
110.982387	3971.282072	23.155277
111.270594	3963.239470	23.160295
111.411725	3975.945012	23.165312
111.306881	3970.704355	23.170330
111.450819	3969.297715	23.175347
111.700005	3993.268825	23.180365
112.047171	3994.479370	23.185383
111.642231	4002.768174	23.190400
111.644778	3995.011049	23.195418
111.805424	4012.653178	23.200435
111.694744	4016.253555	23.205453
112.183912	4027.820362	23.210471
112.316197	4034.212541	23.215488
112.567810	4031.095751	23.220506
112.358582	4032.438288	23.225523
112.501411	4049.966085	23.230541
112.819344	4049.876948	23.235559
112.657832	4060.254990	23.240576
113.106100	4061.090684	23.245594
113.617819	4075.464812	23.250611
113.820588	4077.348204	23.255629
114.131768	4077.637761	23.260647
114.103664	4081.816586	23.265664
114.066829	4075.810601	23.270682
114.266238	4067.997658	23.275699
114.225505	4070.362003	23.280717
114.548558	4071.147647	23.285735
114.307476	4077.619835	23.290752
114.177947	4074.039082	23.295770
114.685696	4064.860038	23.300787
114.467979	4077.827431	23.305805
114.526046	4068.514760	23.310823
114.452561	4071.210808	23.315840
114.626864	4066.933368	23.320858
114.906635	4080.309976	23.325875
114.696096	4100.886004	23.330893
115.524533	4091.354501	23.335911
115.362961	4090.726624	23.340928
115.146669	4091.676156	23.345946
115.632224	4107.502806	23.350963
115.982623	4127.245205	23.355981
116.073746	4104.817621	23.360999
116.230641	4121.989245	23.366016
116.426066	4118.986028	23.371034
116.748521	4107.129460	23.376051
116.357055	4113.468302	23.381069
116.556326	4108.333297	23.386087
116.664498	4109.367978	23.391104
116.570658	4113.327576	23.396122
116.889827	4107.684123	23.401139
116.449883	4109.834424	23.406157
116.549919	4107.176835	23.411175
116.742468	4120.854535	23.416192
116.978191	4129.500687	23.421210
116.984256	4139.828463	23.426227
116.756946	4141.446879	23.431245
117.055460	4147.380700	23.436263
117.136697	4165.812153	23.441280
117.247487	4180.133883	23.446298
117.687934	4168.196301	23.451315
117.552411	4194.642697	23.456333
117.854182	4203.039988	23.461351
118.266982	4193.558963	23.466368
118.152439	4207.933957	23.471386
118.528499	4197.432920	23.476403
118.136996	4214.910015	23.481421
118.232864	4218.568764	23.486439
118.613026	4241.288983	23.491456
118.587288	4236.951347	23.496474
119.068135	4237.750389	23.501491
118.879395	4240.076211	23.506509
119.272622	4263.953205	23.511527
119.249250	4268.354753	23.516544
119.382668	4263.182992	23.521562
119.583952	4266.096450	23.526579
119.807456	4274.779252	23.531597
119.655241	4272.290876	23.536615
119.816511	4276.678719	23.541632
119.554264	4293.020526	23.546650
119.899808	4299.185284	23.551667
120.022915	4298.545047	23.556685
120.211294	4318.549552	23.561703
120.511181	4331.042062	23.566720
120.452422	4324.978108	23.571738
120.704138	4320.494719	23.576755
120.867250	4336.882823	23.581773
121.222308	4339.728506	23.586791
121.158229	4358.975593	23.591808
120.994519	4362.809511	23.596826
121.230567	4358.652736	23.601843
121.199113	4360.511363	23.606861
121.678712	4378.002372	23.611879
121.489258	4380.173347	23.616896
121.631227	4382.999520	23.621914
121.926007	4385.980699	23.626931
121.905085	4389.134946	23.631949
122.082508	4393.701194	23.636967
122.284323	4408.140800	23.641984
122.488509	4416.523092	23.647002
122.680880	4411.998790	23.652019
122.517559	4425.097848	23.657037
122.892002	4402.276906	23.662055
123.173591	4406.764398	23.667072
122.977278	4398.373206	23.672090
123.300716	4418.326416	23.677107
123.287191	4436.152596	23.682125
123.747882	4441.635850	23.687143
123.810076	4427.307741	23.692160
123.590038	4435.143260	23.697178
124.271375	4432.902717	23.702195
123.771676	4429.426531	23.707213
123.827094	4426.597414	23.712231
124.054995	4426.165464	23.717248
124.022811	4430.360772	23.722266
124.457744	4444.064635	23.727283
124.508186	4452.473037	23.732301
124.567231	4458.937657	23.737319
124.555273	4454.670924	23.742336
124.648694	4468.206622	23.747354
124.925981	4457.034345	23.752371
125.102441	4471.692044	23.757389
125.104364	4485.830816	23.762407
125.042598	4488.016061	23.767424
125.063225	4487.372489	23.772442
125.525624	4490.276612	23.777459
125.300232	4516.078639	23.782477
125.573277	4512.568904	23.787495
125.618793	4519.813778	23.792512
125.758772	4533.055745	23.797530
126.176446	4539.643376	23.802547
126.329532	4555.210407	23.807565
126.033746	4548.404508	23.812583
126.353182	4554.715149	23.817600
126.228771	4577.870370	23.822618
126.782539	4570.515967	23.827635
126.649166	4582.600232	23.832653
126.574379	4590.957088	23.837671
127.049001	4607.392590	23.842688
126.978327	4608.283530	23.847706
127.120440	4610.899668	23.852723
127.238097	4628.387324	23.857741
127.405172	4641.248223	23.862759
127.780521	4645.420308	23.867776
127.628958	4656.718442	23.872794
128.192083	4667.239413	23.877811
128.272552	4672.057227	23.882829
128.129674	4677.589606	23.887847
128.349136	4676.397437	23.892864
128.238288	4688.859763	23.897882
128.476625	4704.669833	23.902899
128.727808	4709.644535	23.907917
128.815449	4706.061255	23.912935
128.915959	4710.093872	23.917952
129.164741	4724.869316	23.922970
129.582790	4728.440631	23.927987
129.903770	4734.888782	23.933005
129.713136	4737.596549	23.938023
129.979701	4720.500876	23.943040
129.634706	4729.083417	23.948058
130.040687	4731.221652	23.953075
130.327152	4735.739151	23.958093
130.446906	4746.356836	23.963111
130.935305	4754.265233	23.968128
130.763383	4770.522357	23.973146
130.763313	4754.405378	23.978163
131.037042	4758.502437	23.983181
131.263699	4762.437854	23.988199
131.397459	4757.998319	23.993216
131.186207	4762.363099	23.998234
131.311348	4757.425360	24.003251
131.460439	4759.336283	24.008269
131.683633	4750.032257	24.013287
131.668503	4755.501025	24.018304
131.436893	4761.131763	24.023322
131.781634	4762.397048	24.028339
131.880051	4773.300594	24.033357
131.848160	4784.446000	24.038375
131.612233	4784.291762	24.043392
131.879553	4804.264672	24.048410
131.953977	4820.709152	24.053427
132.104868	4822.359385	24.058445
132.790183	4831.411816	24.063463
132.701374	4832.662055	24.068480
132.843709	4847.276005	24.073498
133.442158	4852.377122	24.078515
133.660913	4862.129424	24.083533
134.079065	4866.797477	24.088551
134.164037	4864.797511	24.093568
133.975264	4865.908704	24.098586
134.194910	4866.917011	24.103603
134.164935	4860.368333	24.108621
134.369076	4855.290513	24.113639
134.621351	4849.999681	24.118656
134.513141	4852.294661	24.123674
134.833253	4844.054533	24.128691
135.123809	4852.248647	24.133709
135.013069	4855.912175	24.138727
134.870533	4849.822812	24.143744
135.177074	4876.935545	24.148762
135.188814	4872.503631	24.153779
135.310851	4885.832957	24.158797
135.273648	4889.000921	24.163815
135.491436	4879.271261	24.168832
135.532705	4896.653404	24.173850
135.546890	4908.238427	24.178867
135.683879	4911.237007	24.183885
135.645127	4914.288785	24.188903
135.988332	4920.362131	24.193920
135.874480	4936.134983	24.198938
135.870551	4950.514304	24.203955
136.460796	4960.670833	24.208973
136.209178	4971.952905	24.213991
136.656299	4978.344074	24.219008
136.516544	5000.083894	24.224026
136.793908	4997.460025	24.229043
137.483239	5007.859629	24.234061
137.364235	5030.204342	24.239079
137.438700	5030.570218	24.244096
137.706348	5036.506964	24.249114
138.068165	5032.877529	24.254131
137.771858	5039.147303	24.259149
137.709475	5042.257948	24.264167
138.084251	5053.503932	24.269184
138.338438	5062.583552	24.274202
138.352765	5057.930092	24.279219
138.492546	5067.795827	24.284237
138.636050	5095.439266	24.289255
138.682358	5085.469317	24.294272
138.573484	5092.463725	24.299290
139.035523	5104.613191	24.304307
139.313547	5115.785746	24.309325
139.299842	5116.629082	24.314343
139.699675	5121.964160	24.319360
139.482952	5135.831581	24.324378
139.800441	5142.676208	24.329395
140.555384	5132.572782	24.334413
140.495028	5130.144354	24.339431
140.892188	5127.209476	24.344448
141.062442	5127.885799	24.349466
141.247202	5131.234782	24.354483
140.907015	5123.862148	24.359501
141.064106	5129.690679	24.364519
141.622769	5121.174762	24.369536
141.355359	5123.090774	24.374554
141.411911	5127.182441	24.379571
141.476352	5130.413713	24.384589
141.663599	5153.413929	24.389607
141.703106	5159.912656	24.394624
142.239927	5151.213742	24.399642
141.807469	5164.082574	24.404659
142.244861	5150.731677	24.409677
141.734481	5171.964377	24.414695
142.442089	5178.130787	24.419712
142.221090	5186.143875	24.424730
142.205589	5204.499211	24.429747
142.507109	5204.734478	24.434765
142.415975	5218.124843	24.439783
142.716024	5232.915440	24.444800
142.867802	5249.263093	24.449818
142.983691	5254.662376	24.454835
143.420777	5262.734223	24.459853
143.085489	5294.767416	24.464871
143.632389	5289.296489	24.469888
143.918518	5306.692785	24.474906
143.681186	5314.798237	24.479923
144.225666	5311.764305	24.484941
144.199707	5322.545683	24.489959
144.559708	5336.485770	24.494976
144.675716	5345.403493	24.499994
144.761439	5348.439447	24.505011
144.891623	5345.740640	24.510029
144.926563	5354.229130	24.515047
145.506226	5360.759048	24.520064
145.883661	5369.243292	24.525082
146.111871	5370.866311	24.530099
146.337352	5359.365666	24.535117
146.307461	5368.708705	24.540135
146.173222	5375.914210	24.545152
146.176649	5368.054730	24.550170
146.221694	5366.164131	24.555187
146.557354	5368.921848	24.560205
146.528000	5363.891313	24.565223
146.514395	5364.582014	24.570240
146.584522	5377.691111	24.575258
146.752751	5391.307781	24.580275
146.869159	5390.994290	24.585293
146.857464	5401.116497	24.590311
147.438895	5417.306927	24.595328
147.380618	5420.353268	24.600346
147.634710	5423.439496	24.605363
148.007036	5431.661809	24.610381
147.759868	5447.879745	24.615399
148.244683	5448.372964	24.620416
148.508041	5448.516761	24.625434
147.975067	5453.409036	24.630451
148.430846	5465.849333	24.635469
148.555468	5478.977368	24.640487
148.845314	5475.351436	24.645504
148.934227	5486.500925	24.650522
148.947395	5507.025927	24.655539
149.516243	5505.931410	24.660557
149.190754	5513.851185	24.665575
149.438004	5518.065189	24.670592
149.463966	5532.146841	24.675610
149.498775	5555.012271	24.680627
149.633789	5557.945210	24.685645
149.911935	5571.433584	24.690663
149.871264	5584.780829	24.695680
150.259904	5597.262626	24.700698
150.284567	5608.383111	24.705715
150.804756	5603.982420	24.710733
150.711569	5624.174424	24.715751
151.130715	5631.731633	24.720768
151.147178	5638.636290	24.725786
151.191119	5655.062168	24.730803
151.477586	5653.483159	24.735821
151.065685	5673.987258	24.740839
151.630947	5680.189167	24.745856
152.052344	5691.122147	24.750874
151.916925	5705.654559	24.755891
152.679518	5698.854830	24.760909
152.568821	5703.664121	24.765927
152.718107	5699.151807	24.770944
152.945347	5702.877313	24.775962
152.988892	5703.879927	24.780979
153.398015	5703.213700	24.785997
153.552043	5722.336516	24.791015
153.596753	5733.283953	24.796032
153.477748	5736.502906	24.801050
153.470237	5745.833959	24.806067
153.792995	5734.268734	24.811085
153.446584	5740.590062	24.816103
154.040969	5747.058012	24.821120
154.334947	5756.296942	24.826138
154.383587	5764.988049	24.831155
154.641740	5755.778531	24.836173
154.637039	5755.920224	24.841191
155.200616	5767.164191	24.846208
155.600657	5783.968531	24.851226
155.613990	5772.194544	24.856243
155.995445	5768.468175	24.861261
155.808081	5778.491976	24.866279
155.906331	5782.898187	24.871296
156.123773	5770.660496	24.876314
155.965108	5777.879532	24.881331
156.048437	5767.296606	24.886349
156.000495	5779.947302	24.891367
156.637635	5788.834919	24.896384
156.503913	5798.941449	24.901402
156.517943	5808.915850	24.906419
156.849066	5798.247760	24.911437
156.844159	5825.203391	24.916455
156.728006	5836.424392	24.921472
157.166357	5840.800786	24.926490
157.438743	5843.934542	24.931507
157.337364	5858.040741	24.936525
157.425920	5866.041817	24.941543
157.295472	5868.719734	24.946560
157.646310	5891.667478	24.951578
157.749375	5903.573497	24.956595
158.298986	5915.041681	24.961613
158.512329	5923.195989	24.966631
158.564052	5928.450749	24.971648
159.158598	5947.654687	24.976666
158.957759	5952.200690	24.981683
159.179921	5953.775172	24.986701
159.319152	5965.742353	24.991719
159.361686	5967.046490	24.996736
159.846824	5986.837567	25.001754
159.877960	5993.084644	25.006771
160.028359	5991.830214	25.011789
159.899235	5997.429340	25.016807
160.043127	6011.579980	25.021824
160.483952	6013.457930	25.026842
160.223260	6019.930151	25.031859
160.931432	6037.102658	25.036877
160.803013	6049.028391	25.041895
161.146227	6043.477943	25.046912
161.426654	6049.851313	25.051930
161.087037	6059.409397	25.056947
161.716315	6067.918410	25.061965
161.467922	6077.942700	25.066983
161.568322	6076.632504	25.072000
162.208542	6076.580107	25.077018
161.975386	6094.951577	25.082035
162.459787	6096.766728	25.087053
162.491304	6095.039488	25.092071
162.726429	6097.938477	25.097088
162.918811	6108.277261	25.102106
162.922432	6130.942408	25.107123
163.356796	6129.678886	25.112141
163.296627	6141.746453	25.117159
162.946627	6141.140656	25.122176
163.747684	6153.823114	25.127194
163.625524	6161.192303	25.132211
164.078452	6157.077562	25.137229
163.912443	6162.465472	25.142247
164.227199	6189.566715	25.147264
164.587373	6189.152186	25.152282
164.215328	6197.905111	25.157299
164.956803	6205.949407	25.162317
164.893561	6222.054671	25.167335
164.944090	6221.111201	25.172352
165.492866	6216.014954	25.177370
165.396981	6231.650198	25.182387
165.923073	6235.037071	25.187405
165.857049	6257.822882	25.192423
165.755571	6252.344831	25.197440
165.851201	6257.650932	25.202458
165.818135	6273.646795	25.207475
166.049491	6288.429731	25.212493
166.350679	6302.194420	25.217511
166.711407	6320.675269	25.222528
167.170753	6313.630919	25.227546
166.936426	6321.435872	25.232563
167.073405	6332.513815	25.237581
167.102311	6340.908627	25.242599
167.057623	6344.310993	25.247616
167.524253	6357.669322	25.252634
167.532955	6381.267210	25.257651
168.149243	6380.534882	25.262669
168.161972	6391.867939	25.267687
168.218271	6411.153575	25.272704
168.836382	6410.129830	25.277722
168.818980	6431.363618	25.282739
168.974521	6435.894650	25.287757
168.730718	6445.724108	25.292775
169.111092	6449.240486	25.297792
169.457564	6459.127701	25.302810
169.197524	6478.763641	25.307827
169.610906	6472.954784	25.312845
169.756445	6492.024082	25.317863
169.923428	6498.946056	25.322880
170.385924	6495.160167	25.327898
170.513615	6496.275312	25.332915
170.647822	6504.778534	25.337933
170.843613	6526.611865	25.342951
170.710320	6532.347979	25.347968
171.175602	6528.659991	25.352986
171.043264	6536.031775	25.358003
171.007462	6541.377030	25.363021
171.172809	6552.013135	25.368039
171.184882	6564.957074	25.373056
171.689071	6573.826238	25.378074
171.703767	6587.110476	25.383091
172.005335	6600.936756	25.388109
172.887956	6604.776744	25.393127
172.734097	6612.698060	25.398144
173.186656	6609.805212	25.403162
173.313870	6610.415293	25.408179
173.324840	6613.933954	25.413197
173.672094	6609.708472	25.418215
173.906714	6617.102049	25.423232
174.217991	6632.251054	25.428250
174.084290	6634.902086	25.433267
174.093161	6639.753202	25.438285
174.220841	6637.807565	25.443303
173.984775	6644.530276	25.448320
174.154078	6651.643940	25.453338
173.963299	6669.885041	25.458355
174.309413	6684.033982	25.463373
174.735119	6708.274061	25.468391
174.760875	6714.048620	25.473408
175.111518	6726.268332	25.478426
175.211930	6744.065351	25.483443
175.544675	6748.885325	25.488461
175.431651	6771.985497	25.493479
175.370689	6789.561623	25.498496
175.843666	6795.814917	25.503514
175.834137	6813.132653	25.508531
176.197684	6825.532939	25.513549
176.567966	6835.127050	25.518567
176.558768	6851.327455	25.523584
176.791812	6869.129837	25.528602
177.088689	6878.985111	25.533619
177.292772	6895.052417	25.538637
177.517789	6902.211612	25.543655
177.335066	6916.254668	25.548672
177.517855	6925.749687	25.553690
177.554312	6941.201696	25.558707
177.784228	6960.047265	25.563725
178.293844	6976.762314	25.568743
178.062378	6993.147811	25.573760
178.679262	7005.765160	25.578778
178.783616	7028.689438	25.583795
179.081271	7041.688978	25.588813
179.552288	7046.001514	25.593831
179.497258	7055.202476	25.598848
180.162438	7066.781392	25.603866
180.184686	7082.187815	25.608883
180.177219	7079.737258	25.613901
180.032110	7079.320646	25.618919
180.153118	7084.410545	25.623936
180.712662	7105.015098	25.628954
180.674303	7107.451150	25.633971
180.943488	7108.110223	25.638989
180.800361	7122.567345	25.644007
181.038938	7144.943992	25.649024
181.276167	7142.240387	25.654042
181.384999	7150.985656	25.659059
181.260521	7178.488426	25.664077
181.773077	7181.522018	25.669095
181.807153	7203.666183	25.674112
182.173621	7217.831273	25.679130
182.050849	7227.952760	25.684148
182.338304	7238.539988	25.689165
182.878096	7249.629935	25.694183
182.689456	7272.628053	25.699200
183.145801	7280.696368	25.704218
183.291095	7295.229639	25.709236
183.266965	7310.627953	25.714253
183.565379	7316.327802	25.719271
184.128422	7335.352077	25.724288
184.640174	7343.935652	25.729306
184.818639	7353.834513	25.734324
184.915128	7347.995582	25.739341
185.041858	7333.327044	25.744359
185.070219	7352.419273	25.749376
185.594091	7346.959938	25.754394
185.845406	7354.982294	25.759412
185.838412	7361.679034	25.764429
185.908058	7363.838240	25.769447
185.923292	7358.433238	25.774464
186.276106	7376.041659	25.779482
186.475047	7385.743705	25.784500
186.158192	7385.376498	25.789517
186.434214	7385.558434	25.794535
186.412848	7416.496442	25.799552
186.672141	7429.079097	25.804570
186.742036	7447.507783	25.809588
186.901553	7449.128612	25.814605
187.175390	7464.337943	25.819623
187.532323	7486.807185	25.824640
187.887763	7501.059286	25.829658
187.980696	7511.093068	25.834676
188.274590	7522.423864	25.839693
188.533043	7524.572665	25.844711
188.590660	7543.726572	25.849728
188.858660	7547.438968	25.854746
188.944422	7559.707891	25.859764
189.068111	7574.929469	25.864781
189.270724	7590.170742	25.869799
189.333259	7604.339803	25.874816
189.650399	7614.363483	25.879834
189.673484	7631.587264	25.884852
189.304976	7636.107390	25.889869
190.334634	7641.134455	25.894887
190.326218	7658.000138	25.899904
190.468838	7671.049339	25.904922
190.658761	7688.258784	25.909940
190.988219	7690.104352	25.914957
191.190619	7689.644124	25.919975
191.296509	7709.025828	25.924992
191.960357	7711.616393	25.930010
192.245306	7710.620900	25.935028
192.268915	7717.803942	25.940045
192.587457	7719.548959	25.945063
192.749102	7736.452145	25.950080
192.813113	7737.907640	25.955098
192.966881	7735.920325	25.960116
193.012788	7751.243009	25.965133
193.444603	7758.924017	25.970151
193.656809	7772.588190	25.975168
193.700039	7773.471780	25.980186
193.895794	7785.551023	25.985204
193.624172	7798.620735	25.990221
194.100201	7794.800894	25.995239
194.178295	7810.061851	26.000256
194.162818	7835.160213	26.005274
194.517876	7846.320190	26.010292
194.502050	7851.601351	26.015309
194.948477	7854.413099	26.020327
194.973634	7878.980588	26.025344
195.018688	7888.815301	26.030362
194.978522	7909.395788	26.035380
195.295694	7939.120223	26.040397
195.411427	7941.127768	26.045415
195.658557	7962.303462	26.050432
195.949646	7979.144973	26.055450
196.364101	7985.399056	26.060468
196.366661	7999.814518	26.065485
196.926672	8017.968651	26.070503
197.273083	8037.925439	26.075520
197.405281	8051.980339	26.080538
197.683352	8071.905575	26.085556
197.556801	8074.168558	26.090573
198.030991	8093.503062	26.095591
198.253122	8095.223755	26.100608
198.522101	8111.664074	26.105626
198.490227	8128.312510	26.110644
198.572777	8134.976042	26.115661
198.984657	8135.279551	26.120679
199.081978	8160.873152	26.125696
199.103013	8168.875215	26.130714
199.507560	8179.676588	26.135732
199.361309	8192.671965	26.140749
199.807776	8203.463918	26.145767
199.836907	8230.027369	26.150784
200.158924	8244.415352	26.155802
200.515111	8240.941472	26.160820
200.800171	8257.686287	26.165837
201.223681	8255.794401	26.170855
201.064479	8272.377915	26.175872
201.601630	8282.039612	26.180890
201.506546	8289.027808	26.185908
201.148683	8313.744811	26.190925
201.693318	8310.834215	26.195943
201.801918	8338.455013	26.200960
201.816732	8346.020631	26.205978
202.197873	8366.400803	26.210996
202.584083	8380.952989	26.216013
202.979101	8381.546029	26.221031
202.923083	8404.561725	26.226048
203.113180	8404.890369	26.231066
203.824176	8429.237286	26.236084
203.747718	8438.213910	26.241101
203.898018	8431.018360	26.246119
204.018160	8457.801817	26.251136
204.034332	8463.309449	26.256154
204.474659	8475.413216	26.261172
204.512719	8489.684202	26.266189
204.586947	8497.864464	26.271207
204.814853	8521.064467	26.276224
204.854686	8524.017498	26.281242
205.334618	8551.341050	26.286260
205.252125	8570.692913	26.291277
205.568586	8588.587138	26.296295
206.092362	8596.344812	26.301312
206.465750	8615.543790	26.306330
206.376570	8632.694546	26.311348
206.361490	8647.325523	26.316365
206.979298	8652.581893	26.321383
207.252733	8666.614067	26.326400
207.492662	8687.020336	26.331418
207.914003	8681.663436	26.336436
207.836511	8702.684568	26.341453
208.281399	8720.846500	26.346471
208.748207	8724.295350	26.351488
208.497883	8734.647514	26.356506
208.794361	8745.835211	26.361524
208.658596	8765.124598	26.366541
209.045697	8772.806572	26.371559
209.159015	8778.491636	26.376576
209.310277	8800.678109	26.381594
209.623462	8803.203586	26.386612
209.406175	8830.705687	26.391629
209.845151	8843.033855	26.396647
210.041986	8860.914424	26.401664
210.102430	8871.487459	26.406682
210.548757	8899.196708	26.411700
210.648428	8910.760983	26.416717
210.792858	8915.554239	26.421735
210.920550	8950.024757	26.426752
211.506106	8957.933705	26.431770
211.917933	8959.613637	26.436788
212.336127	8962.129484	26.441805
212.912474	8947.004840	26.446823
213.186463	8936.168931	26.451840
213.404305	8940.727391	26.456858
213.996287	8933.983337	26.461876
213.708801	8940.813636	26.466893
213.939527	8940.035256	26.471911
213.883032	8941.571462	26.476928
213.901405	8962.860194	26.481946
214.331854	8962.849917	26.486964
214.081390	8979.564441	26.491981
213.932222	8976.607720	26.496999
213.937233	9000.261480	26.502016
214.344314	9013.458958	26.507034
214.849512	9032.153084	26.512052
214.604576	9058.371357	26.517069
215.369779	9072.212588	26.522087
215.280299	9079.328138	26.527104
215.387955	9100.382874	26.532122
215.977234	9100.213494	26.537140
215.878970	9124.337206	26.542157
216.591395	9134.293388	26.547175
216.484907	9146.827989	26.552192
216.461359	9168.739103	26.557210
216.932184	9170.462382	26.562228
217.107482	9201.260576	26.567245
217.438736	9210.350521	26.572263
217.360856	9228.870273	26.577280
217.149534	9251.017234	26.582298
217.891593	9267.881169	26.587316
217.738001	9282.721358	26.592333
218.355149	9314.340597	26.597351
218.224899	9331.425900	26.602368
218.527084	9351.266362	26.607386
218.656009	9366.616023	26.612404
219.092308	9400.932136	26.617421
219.365801	9403.815825	26.622439
219.488417	9425.026027	26.627456
219.810518	9436.277837	26.632474
220.514850	9455.445991	26.637492
220.267634	9482.022654	26.642509
220.334693	9488.746314	26.647527
220.583212	9502.958742	26.652544
220.771551	9525.721171	26.657562
221.133192	9532.567880	26.662580
221.308266	9550.148175	26.667597
221.942027	9571.421906	26.672615
222.064268	9587.038074	26.677632
222.237378	9603.278497	26.682650
222.685547	9622.094597	26.687668
222.530475	9628.067523	26.692685
222.890201	9644.607205	26.697703
223.050470	9651.939379	26.702720
223.269969	9662.029189	26.707738
223.724202	9683.995137	26.712756
223.861430	9691.090182	26.717773
223.916098	9700.557415	26.722791
224.213324	9718.683105	26.727808
224.377964	9715.076913	26.732826
224.834043	9732.404071	26.737844
224.973001	9738.111776	26.742861
225.157289	9745.438199	26.747879
225.898946	9759.283037	26.752896
225.704101	9782.961228	26.757914
226.298461	9777.631849	26.762932
226.035921	9786.708981	26.767949
226.433013	9800.299492	26.772967
226.448666	9823.248874	26.777984
226.632169	9825.601992	26.783002
227.196026	9839.360344	26.788020
227.084252	9852.491742	26.793037
227.205135	9868.939889	26.798055
227.583080	9882.561072	26.803072
227.535478	9901.449077	26.808090
228.078627	9912.671124	26.813108
228.084998	9926.867857	26.818125
228.471426	9950.457979	26.823143
228.760828	9961.336057	26.828160
228.867400	9980.967313	26.833178
228.994963	9981.130068	26.838196
229.173145	10005.117465	26.843213
229.344435	10015.497736	26.848231
229.626073	10043.693197	26.853248
229.650130	10058.226437	26.858266
229.971069	10079.294977	26.863284
230.166370	10091.531194	26.868301
230.401736	10115.834297	26.873319
231.070952	10125.391537	26.878336
231.128107	10145.897001	26.883354
231.171111	10161.326492	26.888372
231.622493	10185.805014	26.893389
231.627153	10202.593944	26.898407
231.841669	10215.323024	26.903424
232.404416	10241.898226	26.908442
232.341029	10256.331477	26.913460
232.628661	10281.005861	26.918477
232.690724	10294.693512	26.923495
233.408166	10311.372483	26.928512
233.596256	10335.775952	26.933530
234.324606	10328.536152	26.938548
234.486646	10346.156443	26.943565
234.475439	10355.535030	26.948583
234.846791	10361.910714	26.953600
234.847644	10367.816575	26.958618
235.301104	10381.148350	26.963636
235.447621	10384.671867	26.968653
235.908279	10407.454002	26.973671
236.096394	10418.257261	26.978688
236.170002	10420.622088	26.983706
236.271070	10414.067794	26.988724
236.733275	10426.493127	26.993741
236.493814	10449.293270	26.998759
236.918497	10455.046998	27.003776
237.031736	10473.841214	27.008794
237.413891	10487.911280	27.013812
237.320616	10501.372028	27.018829
237.161567	10511.494418	27.023847
237.493838	10520.356362	27.028864
237.511155	10547.572337	27.033882
237.752683	10573.661779	27.038900
238.343696	10589.519865	27.043917
238.546944	10612.554270	27.048935
238.942173	10629.642276	27.053952
238.976981	10649.475913	27.058970
239.437840	10667.039895	27.063988
239.686023	10696.619046	27.069005
240.065880	10701.848757	27.074023
240.697356	10716.240156	27.079040
240.419086	10742.324204	27.084058
240.583357	10754.727252	27.089076
241.041005	10763.596114	27.094093
241.082833	10783.896317	27.099111
241.590033	10797.866068	27.104128
241.642293	10821.479733	27.109146
241.880445	10836.660791	27.114164
242.129170	10856.175685	27.119181
242.276303	10873.579379	27.124199
242.787220	10891.792838	27.129216
242.849146	10907.545129	27.134234
243.085169	10925.339262	27.139252
243.449209	10934.195599	27.144269
243.970758	10951.110555	27.149287
244.830480	10957.691399	27.154304
245.182469	10963.228073	27.159322
245.054345	10953.002423	27.164340
245.704442	10966.972575	27.169357
245.682227	10987.476287	27.174375
245.845797	10983.682449	27.179392
245.592150	11001.432141	27.184410
245.665917	10999.247207	27.189428
246.244635	11018.368911	27.194445
245.995552	11025.502354	27.199463
246.600908	11045.590299	27.204480
246.378933	11062.840933	27.209498
246.974624	11077.840098	27.214516
247.355669	11089.936542	27.219533
247.157804	11111.979398	27.224551
247.480838	11117.604764	27.229568
247.508996	11151.836247	27.234586
247.842796	11167.056306	27.239604
248.342268	11191.541980	27.244621
248.174517	11206.812707	27.249639
249.011105	11216.415004	27.254656
248.857378	11241.891520	27.259674
249.477827	11258.252695	27.264692
249.763769	11255.325140	27.269709
249.772064	11272.160525	27.274727
250.350004	11290.639654	27.279744
250.443478	11302.391716	27.284762
250.571793	11316.865076	27.289780
251.066073	11328.262836	27.294797
250.685483	11341.577292	27.299815
250.959215	11355.303000	27.304832
251.083198	11383.743524	27.309850
251.473545	11397.800935	27.314868
251.882955	11424.304081	27.319885
251.882119	11435.854240	27.324903
252.761814	11438.774717	27.329920
253.076936	11463.194388	27.334938
253.341387	11468.167283	27.339956
253.697944	11476.069606	27.344973
253.771747	11494.191722	27.349991
254.144661	11500.750642	27.355008
254.226751	11534.689662	27.360026
254.274863	11543.009939	27.365044
254.522436	11560.605812	27.370061
254.772844	11571.440109	27.375079
254.966960	11578.128705	27.380096
255.318293	11600.120737	27.385114
255.205620	11631.851927	27.390132
255.574009	11642.806786	27.395149
255.749735	11674.275445	27.400167
255.879430	11686.050366	27.405184
256.359202	11707.123408	27.410202
256.948359	11726.541084	27.415220
257.050876	11743.720694	27.420237
257.192260	11771.094809	27.425255
257.572001	11780.279137	27.430272
257.764417	11798.185145	27.435290
258.148313	11822.664683	27.440308
258.770410	11831.045145	27.445325
258.817813	11841.059358	27.450343
259.293509	11854.754902	27.455360
259.489721	11871.848096	27.460378
259.760948	11893.097893	27.465396
260.143612	11895.397750	27.470413
260.382737	11913.474731	27.475431
260.118453	11923.859625	27.480448
260.493471	11938.361554	27.485466
261.092618	11960.559992	27.490484
261.546393	11972.321456	27.495501
261.438628	11981.804202	27.500519
261.584380	11995.783680	27.505536
261.795518	12011.857304	27.510554
261.844681	12032.159385	27.515572
262.398445	12038.002756	27.520589
262.390380	12069.142603	27.525607
262.550121	12085.368344	27.530624
262.884399	12106.092431	27.535642
263.035867	12115.114796	27.540660
263.055418	12132.787822	27.545677
263.122311	12153.985347	27.550695
263.430648	12157.883150	27.555712
263.913437	12192.933374	27.560730
264.129262	12216.715590	27.565748
264.549141	12242.840087	27.570765
264.746535	12269.257681	27.575783
264.977198	12287.215433	27.580800
265.786912	12294.518972	27.585818
266.279763	12305.702420	27.590836
266.703108	12320.416819	27.595853
267.106499	12322.802780	27.600871
267.478985	12320.198321	27.605888
267.581602	12336.623134	27.610906
267.971848	12350.909324	27.615924
268.895862	12350.381966	27.620941
268.483772	12351.510194	27.625959
269.084652	12350.164950	27.630976
269.276392	12350.614649	27.635994
269.689083	12361.129257	27.641012
269.825049	12368.976100	27.646029
269.687155	12385.237007	27.651047
270.252709	12375.117672	27.656064
270.053083	12389.909985	27.661082
269.950242	12404.259470	27.666100
270.460322	12407.250869	27.671117
270.591661	12426.429137	27.676135
270.753334	12440.360636	27.681152
271.015857	12469.283305	27.686170
271.137473	12482.218409	27.691188
271.531746	12494.121612	27.696205
272.287754	12505.745192	27.701223
272.813252	12518.703720	27.706240
272.699734	12542.441531	27.711258
272.854417	12552.162432	27.716276
273.250950	12565.584226	27.721293
273.482841	12575.536851	27.726311
273.521266	12600.395341	27.731328
273.751699	12615.025162	27.736346
274.024104	12623.431895	27.741364
275.145867	12621.933257	27.746381
274.994391	12635.321337	27.751399
275.500197	12645.435598	27.756416
275.725023	12656.843073	27.761434
276.184906	12662.511557	27.766452
276.351192	12673.783342	27.771469
276.272595	12695.194023	27.776487
276.617751	12692.704553	27.781504
276.770639	12712.555910	27.786522
277.075207	12728.997959	27.791540
277.289915	12735.382404	27.796557
277.110806	12769.043075	27.801575
277.368360	12783.922004	27.806592
277.651400	12801.522126	27.811610
277.311504	12817.223943	27.816628
278.079991	12841.455498	27.821645
278.377248	12867.128319	27.826663
278.310993	12894.514920	27.831680
278.794725	12917.117613	27.836698
279.077121	12936.931696	27.841716
279.396041	12953.228731	27.846733
279.411715	12988.503229	27.851751
279.861907	13016.278853	27.856768
280.217322	13029.106509	27.861786
280.379601	13056.944332	27.866804
281.156605	13081.871462	27.871821
281.333104	13107.291868	27.876839
281.624990	13123.222634	27.881856
282.264976	13135.514811	27.886874
282.252508	13157.905571	27.891892
282.523780	13168.673923	27.896909
282.921479	13185.309338	27.901927
283.117574	13198.933670	27.906944
283.254752	13222.240466	27.911962
283.528682	13240.090114	27.916980
284.294486	13256.103708	27.921997
284.323360	13279.399317	27.927015
284.596403	13285.639891	27.932032
284.814036	13305.503740	27.937050
285.182176	13309.560474	27.942068
286.516679	13312.861384	27.947085
286.649054	13324.324535	27.952103
287.188709	13321.472562	27.957120
287.637381	13323.828838	27.962138
287.320014	13330.655326	27.967156
287.528461	13328.043195	27.972173
287.726972	13342.953729	27.977191
288.170709	13350.321041	27.982208
288.514745	13354.511023	27.987226
288.560671	13374.800845	27.992244
288.754538	13377.007144	27.997261
288.592636	13396.916354	28.002279
289.030755	13407.865217	28.007296
289.456980	13417.711653	28.012314
289.584467	13456.947084	28.017332
289.619075	13467.856393	28.022349
289.966388	13490.531938	28.027367
289.945571	13504.593864	28.032384
290.346175	13533.521145	28.037402
290.239109	13554.868785	28.042420
290.727214	13581.403104	28.047437
290.949140	13616.372627	28.052455
291.491387	13636.150336	28.057472
291.760720	13665.310546	28.062490
291.923956	13683.701945	28.067508
292.144986	13709.544396	28.072525
292.352431	13732.524610	28.077543
292.995377	13758.303317	28.082560
293.257216	13777.846149	28.087578
293.503743	13804.546788	28.092596
294.016133	13819.601809	28.097613
293.934995	13843.615739	28.102631
294.159421	13858.764813	28.107648
295.002576	13877.989093	28.112666
294.964599	13907.563027	28.117684
295.462398	13921.904699	28.122701
295.856165	13941.474930	28.127719
296.107262	13960.024271	28.132736
296.430923	13973.522001	28.137754
296.901407	13990.387977	28.142772
297.197177	14006.658635	28.147789
297.203315	14019.985607	28.152807
297.355934	14050.772855	28.157824
297.880427	14062.321275	28.162842
297.730899	14089.379661	28.167860
298.325894	14094.067034	28.172877
298.604399	14125.396348	28.177895
299.008403	14147.979011	28.182912
299.196350	14165.966254	28.187930
299.305410	14193.649309	28.192948
299.830343	14214.416043	28.197965
300.333404	14233.154937	28.202983
300.369095	14252.918434	28.208000
300.945941	14272.780413	28.213018
301.029912	14290.968488	28.218036
301.586597	14314.233507	28.223053
302.173540	14311.401473	28.228071
302.550594	14331.642838	28.233088
302.918143	14343.456888	28.238106
302.910266	14360.126441	28.243124
303.362674	14372.945775	28.248141
303.570356	14389.425229	28.253159
303.760482	14422.631355	28.258176
304.287357	14417.035916	28.263194
304.647346	14444.014016	28.268212
305.123761	14449.471528	28.273229
305.111422	14472.899314	28.278247
305.447490	14478.739664	28.283264
305.626767	14496.303368	28.288282
305.579942	14517.064905	28.293300
306.256515	14538.891360	28.298317
306.356061	14557.551291	28.303335
306.808387	14574.833523	28.308352
307.662347	14570.406728	28.313370
307.675764	14593.069125	28.318388
308.010601	14607.571740	28.323405
308.323629	14625.501012	28.328423
308.403165	14637.457828	28.333440
309.278581	14648.052315	28.338458
309.420560	14667.215363	28.343476
309.672401	14678.509731	28.348493
309.423707	14689.810173	28.353511
309.470441	14705.188170	28.358528
310.076344	14721.812942	28.363546
310.172097	14743.139158	28.368564
310.657870	14757.278354	28.373581
311.070759	14767.075439	28.378599
310.813032	14793.909635	28.383616
311.231543	14804.445479	28.388634
311.467693	14839.518262	28.393652
311.741407	14864.574579	28.398669
312.086225	14878.781227	28.403687
312.160118	14915.953602	28.408704
312.861925	14929.835928	28.413722
313.166737	14957.145816	28.418740
313.219947	14977.523884	28.423757
313.712314	15013.162230	28.428775
313.989360	15034.412327	28.433792
314.461616	15060.416000	28.438810
314.331253	15087.415023	28.443828
314.642096	15106.209044	28.448845
315.352929	15136.057080	28.453863
315.549467	15176.857112	28.458880
316.036914	15188.491512	28.463898
316.368919	15219.659341	28.468916
316.518072	15237.222788	28.473933
316.759438	15268.729719	28.478951
317.098868	15287.417059	28.483968
317.581670	15310.418735	28.488986
317.833827	15342.856049	28.494004
318.145684	15357.659253	28.499021
318.713620	15388.058234	28.504039
318.787634	15416.414829	28.509056
319.174912	15436.050694	28.514074
319.310489	15448.887472	28.519092
320.021956	15480.282717	28.524109
320.635650	15495.669952	28.529127
321.120757	15509.026393	28.534144
321.918824	15528.330803	28.539162
322.058566	15531.157676	28.544180
322.652379	15526.077387	28.549197
323.104164	15546.118019	28.554215
323.198349	15569.835279	28.559232
323.594489	15563.722248	28.564250
323.835720	15576.939489	28.569268
323.901154	15583.742076	28.574285
324.219967	15599.136849	28.579303
324.378625	15604.780640	28.584320
324.746589	15612.357953	28.589338
324.622049	15637.308449	28.594356
324.987830	15656.217601	28.599373
325.249337	15676.362930	28.604391
325.378613	15702.459748	28.609408
325.851404	15731.417857	28.614426
325.924947	15745.683697	28.619444
326.234836	15770.905292	28.624461
326.636149	15791.526662	28.629479
326.990854	15825.374667	28.634496
327.501141	15840.113647	28.639514
327.819328	15862.025579	28.644532
327.861919	15874.435454	28.649549
328.478638	15882.826315	28.654567
328.730902	15915.135500	28.659584
329.007674	15939.938089	28.664602
329.383110	15959.048218	28.669620
329.692041	15973.389145	28.674637
329.772177	16002.356606	28.679655
329.899553	16020.847158	28.684672
330.869183	16036.414018	28.689690
330.810002	16074.653694	28.694708
330.982074	16092.079437	28.699725
331.566329	16110.181568	28.704743
331.447131	16144.311683	28.709760
331.967330	16157.637903	28.714778
332.484930	16191.568616	28.719796
332.669791	16219.862766	28.724813
332.986734	16241.827007	28.729831
333.147688	16269.931373	28.734848
334.074747	16290.786333	28.739866
334.291983	16313.851122	28.744884
335.420055	16320.849816	28.749901
336.409545	16331.076250	28.754919
336.365939	16343.246124	28.759936
337.060212	16331.093040	28.764954
337.325100	16339.981527	28.769972
337.727893	16339.280488	28.774989
337.764427	16335.567981	28.780007
337.842389	16354.876784	28.785024
338.280977	16364.750123	28.790042
338.610228	16369.320436	28.795060
338.636992	16387.817818	28.800077
339.195658	16383.639443	28.805095
339.147357	16408.477662	28.810112
339.167796	16421.744396	28.815130
339.441990	16444.314907	28.820148
339.534318	16464.077823	28.825165
339.921941	16483.903737	28.830183
340.278765	16516.449272	28.835200
340.774072	16538.534517	28.840218
341.210847	16568.451452	28.845236
341.217359	16588.624634	28.850253
341.638008	16611.500573	28.855271
341.836125	16635.159601	28.860288
341.842067	16670.394093	28.865306
342.494847	16696.462309	28.870324
342.820620	16725.452604	28.875341
343.221537	16758.481950	28.880359
343.417836	16788.604750	28.885376
343.924415	16805.974054	28.890394
344.224711	16845.179161	28.895412
344.577148	16869.577108	28.900429
345.436187	16884.981364	28.905447
345.549589	16921.584281	28.910464
346.264388	16928.398540	28.915482
346.810121	16929.051021	28.920500
347.235999	16934.154705	28.925517
347.577302	16945.188953	28.930535
347.664228	16977.468836	28.935552
348.065351	16971.938694	28.940570
348.182429	16983.840167	28.945588
348.306561	17006.041331	28.950605
348.797542	17024.233811	28.955623
349.008537	17050.620657	28.960640
349.223751	17072.468437	28.965658
349.412270	17084.764889	28.970676
349.925675	17104.790447	28.975693
350.614231	17118.069808	28.980711
350.866561	17157.755778	28.985728
351.626504	17159.793389	28.990746
351.818857	17174.927811	28.995764
351.783609	17204.674943	29.000781
352.332855	17214.235336	29.005799
352.455329	17241.423998	29.010816
353.106991	17263.711541	29.015834
353.177441	17276.517109	29.020852
353.105930	17319.849127	29.025869
353.682556	17331.760311	29.030887
353.824554	17370.110489	29.035904
354.417634	17392.897706	29.040922
354.800934	17413.785727	29.045940
354.933135	17449.079424	29.050957
355.471793	17467.914036	29.055975
355.903111	17492.596063	29.060992
356.234689	17523.338887	29.066010
356.274980	17554.680946	29.071028
356.844171	17578.495863	29.076045
357.551845	17601.755284	29.081063
357.776601	17625.216499	29.086080
358.079841	17658.162146	29.091098
358.743834	17676.625070	29.096116
358.560773	17706.865617	29.101133
359.151811	17732.781641	29.106151
359.355241	17756.460233	29.111168
359.651884	17791.381254	29.116186
360.155689	17811.815563	29.121204
360.112567	17849.786574	29.126221
360.524946	17879.731386	29.131239
361.262845	17909.696432	29.136256
361.961199	17932.916103	29.141274
362.260607	17948.223987	29.146292
362.620384	17982.566859	29.151309
362.949259	17996.442104	29.156327
363.287757	18017.346739	29.161344
363.811995	18041.414027	29.166362
364.264329	18059.606403	29.171380
364.635320	18084.991133	29.176397
364.919622	18099.738170	29.181415
365.081669	18131.807682	29.186432
365.181803	18157.059307	29.191450
365.418939	18174.749081	29.196468
365.995307	18203.185257	29.201485
366.641308	18213.782078	29.206503
366.614116	18240.579388	29.211520
367.115993	18260.272437	29.216538
367.562485	18275.604847	29.221556
367.781128	18304.653355	29.226573
368.192262	18320.470205	29.231591
368.009663	18352.463588	29.236608
368.720197	18380.742482	29.241626
369.786446	18398.517333	29.246644
369.683965	18430.735918	29.251661
370.170186	18440.830374	29.256679
370.446203	18465.062289	29.261696
370.542212	18494.720097	29.266714
371.161111	18510.608372	29.271732
371.655525	18543.488026	29.276749
372.212405	18553.956754	29.281767
372.619971	18583.227268	29.286784
373.251734	18597.542220	29.291802
373.562490	18613.600576	29.296820
373.713275	18642.995983	29.301837
373.954524	18658.799696	29.306855
374.573347	18677.295817	29.311872
375.026759	18688.974123	29.316890
375.259128	18715.766324	29.321908
375.456097	18729.518351	29.326925
375.960243	18749.529794	29.331943
376.157686	18774.911806	29.336960
376.420897	18806.219283	29.341978
377.001749	18825.466966	29.346996
376.983004	18865.395381	29.352013
377.483018	18887.355066	29.357031
377.580553	18917.795783	29.362048
377.969422	18950.109599	29.367066
378.414760	18974.655907	29.372084
378.301981	19020.615993	29.377101
379.189072	19036.455772	29.382119
379.295090	19081.829153	29.387136
379.777795	19112.123432	29.392154
380.072596	19150.528057	29.397172
380.294383	19181.020754	29.402189
380.644093	19215.876266	29.407207
381.426957	19257.534838	29.412224
381.476540	19292.103267	29.417242
382.188528	19318.293246	29.422260
382.398232	19362.776411	29.427277
383.079264	19392.039910	29.432295
383.468720	19428.429112	29.437312
383.760145	19454.673734	29.442330
384.182913	19489.986382	29.447348
384.819272	19510.390384	29.452365
385.231294	19536.675777	29.457383
385.721079	19561.834901	29.462400
386.428145	19572.054769	29.467418
387.415288	19595.064747	29.472436
387.108321	19619.114539	29.477453
387.713410	19620.852725	29.482471
387.926684	19644.505839	29.487488
387.911262	19665.199357	29.492506
388.562020	19676.163011	29.497524
388.661504	19697.491501	29.502541
388.953860	19725.433510	29.507559
389.355553	19741.456488	29.512576
389.750507	19774.483341	29.517594
390.842583	19766.972183	29.522612
391.349176	19791.394250	29.527629
391.568180	19800.200487	29.532647
392.084288	19812.063771	29.537664
392.080622	19845.199965	29.542682
392.725273	19850.010671	29.547700
392.738723	19871.415320	29.552717
393.209596	19890.075849	29.557735
393.532897	19914.369417	29.562752
393.803980	19940.598802	29.567770
393.956662	19970.864248	29.572788
394.039274	19999.856465	29.577805
394.604307	20033.312741	29.582823
395.361430	20047.414144	29.587840
395.518370	20086.050542	29.592858
395.999756	20109.175339	29.597876
396.338417	20145.402226	29.602893
397.120244	20170.253549	29.607911
397.237137	20200.411735	29.612928
397.626981	20224.548306	29.617946
398.219331	20254.922227	29.622964
398.735578	20267.231976	29.627981
398.726766	20295.817186	29.632999
399.239911	20328.267222	29.638016
399.156304	20367.673477	29.643034
399.770017	20392.860658	29.648052
400.209676	20416.248508	29.653069
400.555894	20452.157518	29.658087
400.998526	20490.187079	29.663104
401.037055	20521.143552	29.668122
401.741396	20551.672677	29.673140
401.872297	20602.604241	29.678157
402.309225	20640.639013	29.683175
402.862523	20667.848467	29.688192
402.992035	20716.565222	29.693210
403.516764	20733.959262	29.698228
403.820169	20789.056128	29.703245
404.262723	20819.810989	29.708263
404.588770	20865.305675	29.713280
405.019427	20891.859325	29.718298
405.799101	20934.255306	29.723316
406.060394	20970.419238	29.728333
406.994038	20996.906312	29.733351
407.424273	21026.582201	29.738368
407.633022	21057.143231	29.743386
408.321534	21081.452478	29.748404
408.815949	21103.436251	29.753421
408.960056	21125.108857	29.758439
409.373272	21146.616541	29.763456
409.403577	21175.836629	29.768474
410.244999	21202.526190	29.773492
410.029232	21230.351396	29.778509
410.568920	21262.176937	29.783527
411.424225	21284.517733	29.788544
412.071129	21320.643082	29.793562
411.940633	21338.452500	29.798580
412.369119	21365.864196	29.803597
412.949344	21394.952178	29.808615
413.105207	21421.671008	29.813632
413.357600	21458.992881	29.818650
414.115587	21476.892446	29.823668
414.394416	21521.713701	29.828685
414.860693	21544.988726	29.833703
415.341757	21570.564378	29.838720
415.514401	21608.298625	29.843738
416.182924	21634.550206	29.848756
416.622435	21664.423508	29.853773
417.036234	21699.288889	29.858791
417.449391	21730.807104	29.863808
417.647919	21766.383489	29.868826
418.097671	21798.657630	29.873844
418.576761	21831.565132	29.878861
418.939399	21860.584675	29.883879
419.370177	21892.588728	29.888896
419.607637	21930.322080	29.893914
420.296127	21968.965824	29.898932
420.375468	22011.592068	29.903949
421.071046	22037.649406	29.908967
421.795253	22062.950829	29.913984
421.696253	22095.402797	29.919002
422.685322	22125.784859	29.924020
423.103405	22157.278724	29.929037
423.790755	22185.943891	29.934055
424.166222	22204.194294	29.939072
424.364802	22244.032057	29.944090
424.789286	22263.365594	29.949108
425.401350	22290.620475	29.954125
425.698605	22328.562637	29.959143
426.401030	22349.231154	29.964160
426.303618	22384.831662	29.969178
426.738000	22407.089105	29.974196
427.019852	22444.904825	29.979213
427.420265	22484.665352	29.984231
427.947057	22506.497058	29.989248
428.467160	22553.908029	29.994266
428.666082	22585.825976	29.999284
428.910883	22622.965129	30.004301
429.153558	22654.060232	30.009319
429.966055	22694.507054	30.014336
430.146802	22738.526639	30.019354
430.808956	22761.572971	30.024372
431.219019	22799.700715	30.029389
431.826298	22831.164201	30.034407
432.469980	22853.181768	30.039424
432.611666	22879.802132	30.044442
433.120154	22910.252821	30.049460
433.804724	22931.476315	30.054477
434.083085	22955.459966	30.059495
434.513541	22984.322682	30.064512
434.593645	23024.575115	30.069530
435.069732	23042.981380	30.074548
435.802460	23080.197462	30.079565
436.048872	23113.681895	30.084583
436.593922	23134.463947	30.089600
436.772230	23176.634873	30.094618
437.511143	23203.259876	30.099636
437.710706	23242.259527	30.104653
438.131100	23279.593579	30.109671
438.616973	23310.370015	30.114688
438.655001	23350.140032	30.119706
439.449899	23377.812702	30.124724
440.193319	23413.073597	30.129741
440.219712	23455.032368	30.134759
440.676692	23486.361197	30.139776
440.776963	23530.037391	30.144794
441.528272	23565.094140	30.149812
442.007968	23611.426101	30.154829
442.308689	23646.649342	30.159847
443.121950	23681.742165	30.164864
443.365388	23722.844695	30.169882
444.371423	23758.657663	30.174900
445.296890	23764.597759	30.179917
445.584922	23797.439741	30.184935
446.352171	23820.123490	30.189952
446.611522	23833.418282	30.194970
447.201829	23853.027461	30.199988
447.456763	23881.046193	30.205005
447.608888	23911.027018	30.210023
448.384237	23930.103460	30.215040
448.780509	23959.564971	30.220058
449.233230	23978.860656	30.225076
449.975190	23996.652210	30.230093
450.631876	24013.929595	30.235111
451.117282	24022.629976	30.240128
451.532035	24042.016074	30.245146
451.837751	24060.439636	30.250164
452.374555	24083.314082	30.255181
452.439156	24100.747333	30.260199
452.826790	24121.693610	30.265216
452.986683	24152.887543	30.270234
453.403184	24183.842934	30.275252
453.851875	24212.975169	30.280269
453.838047	24248.549191	30.285287
454.143230	24279.526441	30.290304
454.887139	24322.206605	30.295322
455.573150	24345.127767	30.300340
456.177341	24369.706799	30.305357
456.447180	24392.468249	30.310375
457.163302	24417.347771	30.315392
457.224988	24445.996968	30.320410
457.453926	24474.515588	30.325428
457.783607	24493.717276	30.330445
458.177489	24536.727915	30.335463
458.741010	24568.584661	30.340480
458.981422	24608.142022	30.345498
459.434103	24652.263788	30.350516
459.728949	24689.658169	30.355533
460.105820	24731.888224	30.360551
460.669149	24759.723086	30.365568
460.860816	24808.893870	30.370586
461.330727	24855.955746	30.375604
461.971978	24892.381607	30.380621
462.511492	24945.193596	30.385639
462.932353	24971.444473	30.390656
463.551156	25023.979399	30.395674
464.299686	25051.708851	30.400692
464.963687	25083.343431	30.405709
465.137843	25125.694262	30.410727
466.207045	25157.492105	30.415744
466.151230	25193.665747	30.420762
466.756233	25236.862060	30.425780
467.101286	25266.788693	30.430797
467.292001	25306.296610	30.435815
468.058109	25353.144962	30.440832
468.098386	25404.976058	30.445850
468.769691	25441.636294	30.450868
469.200209	25485.412530	30.455885
469.685407	25524.807108	30.460903
470.170922	25563.105903	30.465920
470.193174	25613.209746	30.470938
470.686024	25651.519400	30.475956
471.653792	25701.769106	30.480973
471.746135	25740.823442	30.485991
472.585959	25792.174686	30.491008
473.038044	25843.453936	30.496026
473.671288	25880.364673	30.501044
473.990340	25928.708718	30.506061
474.191524	25972.760735	30.511079
475.153302	26006.178229	30.516096
475.596843	26044.467527	30.521114
476.117784	26087.822906	30.526132
476.993274	26128.429914	30.531149
476.934166	26169.589280	30.536167
477.256362	26201.444386	30.541184
477.704526	26254.984282	30.546202
478.151080	26293.666033	30.551220
478.835132	26335.808040	30.556237
479.216143	26392.244938	30.561255
479.829653	26421.411657	30.566272
480.032598	26466.518875	30.571290
480.160877	26522.808196	30.576308
480.954758	26554.265054	30.581325
481.043022	26603.835175	30.586343
481.907105	26642.623790	30.591360
482.241477	26685.708751	30.596378
482.733560	26728.959365	30.601396
483.654687	26765.985422	30.606413
484.267182	26799.811595	30.611431
486.143749	26789.990693	30.616448
486.773123	26810.619138	30.621466
486.987727	26824.484499	30.626484
487.765699	26845.505308	30.631501
487.986810	26856.312756	30.636519
488.456998	26876.541197	30.641536
489.046891	26893.361202	30.646554
489.240996	26924.080770	30.651572
489.801562	26928.491872	30.656589
490.038404	26958.104835	30.661607
490.454673	26973.531269	30.666624
490.540237	27001.871579	30.671642
490.997433	27028.822812	30.676660
491.515878	27069.876710	30.681677
491.928971	27099.392523	30.686695
492.278591	27137.334594	30.691712
492.640776	27166.746761	30.696730
493.020985	27218.284501	30.701748
493.703631	27249.084439	30.706765
493.763513	27295.949315	30.711783
494.094390	27329.547279	30.716800
494.434051	27373.937973	30.721818
494.839021	27423.808403	30.726836
495.318690	27474.820563	30.731853
495.549176	27533.855534	30.736871
496.262610	27576.113500	30.741888
496.676188	27641.377180	30.746906
496.840000	27681.554671	30.751924
497.981407	27744.008198	30.756941
498.577772	27788.165310	30.761959
499.267409	27840.552378	30.766976
500.310057	27873.461338	30.771994
500.850325	27915.497220	30.777012
501.868881	27937.963988	30.782029
502.061144	27961.618219	30.787047
502.485724	28007.769934	30.792064
503.218355	28037.687248	30.797082
503.689753	28074.088278	30.802100
504.234581	28101.203835	30.807117
504.331893	28139.569798	30.812135
504.646123	28190.400976	30.817152
505.371507	28210.922945	30.822170
505.708812	28268.818411	30.827188
505.975167	28293.931603	30.832205
506.227645	28341.307762	30.837223
507.079447	28389.690128	30.842240
507.489704	28420.491563	30.847258
507.999460	28471.104943	30.852276
508.599332	28489.626978	30.857293
509.174335	28539.651829	30.862311
509.586069	28557.100788	30.867328
510.213464	28595.115488	30.872346
510.349172	28634.024913	30.877364
511.028937	28668.712602	30.882381
511.605303	28704.947040	30.887399
511.979947	28752.029151	30.892416
511.911055	28791.932848	30.897434
512.385093	28837.981336	30.902452
513.415289	28887.446215	30.907469
513.634666	28936.792979	30.912487
513.802307	28984.803863	30.917504
514.450972	29025.232083	30.922522
515.016566	29077.193758	30.927540
515.689400	29125.510690	30.932557
516.004136	29169.440629	30.937575
516.768068	29218.797637	30.942592
517.178483	29273.511057	30.947610
517.399142	29332.669164	30.952628
518.333576	29367.834696	30.957645
519.015123	29423.989995	30.962663
519.568160	29468.434371	30.967680
520.327757	29500.906326	30.972698
520.997751	29557.896045	30.977716
521.309872	29590.975291	30.982733
522.024092	29632.262947	30.987751
522.804850	29675.960843	30.992768
523.215145	29725.323706	30.997786
523.484797	29765.894512	31.002804
524.205944	29793.616787	31.007821
524.373130	29845.430032	31.012839
525.016415	29886.676046	31.017856
526.192838	29924.272282	31.022874
526.571112	29968.394403	31.027892
527.099210	29999.991708	31.032909
527.623876	30031.846514	31.037927
528.359561	30065.390378	31.042944
529.180657	30112.928547	31.047962
529.679993	30144.234417	31.052980
530.224044	30149.824777	31.057997
530.922511	30189.095864	31.063015
531.188988	30222.142682	31.068032
532.221165	30241.020241	31.073050
532.854847	30261.642946	31.078068
533.278050	30290.263018	31.083085
533.431158	30321.395847	31.088103
533.915656	30347.393148	31.093120
534.343128	30374.494938	31.098138
534.615945	30407.835845	31.103156
535.401154	30431.924046	31.108173
535.685503	30471.903235	31.113191
535.832181	30507.220344	31.118208
536.383266	30548.552063	31.123226
536.760063	30586.305563	31.128244
537.406135	30615.387172	31.133261
537.884050	30650.763733	31.138279
538.374310	30692.781648	31.143296
538.834461	30723.554268	31.148314
538.741256	30782.974074	31.153332
539.405665	30818.902876	31.158349
539.732560	30875.411228	31.163367
540.362621	30932.483021	31.168384
540.972457	30968.898408	31.173402
541.381107	31021.463392	31.178420
542.333179	31075.292734	31.183437
542.864222	31117.979826	31.188455
543.428973	31168.324858	31.193472
544.031284	31207.508102	31.198490
544.219321	31265.483660	31.203508
544.760423	31308.398186	31.208525
545.613844	31354.719596	31.213543
545.738833	31414.880821	31.218560
546.549987	31455.399504	31.223578
547.000772	31520.188869	31.228596
547.784656	31569.891824	31.233613
548.250848	31616.909273	31.238631
548.657777	31659.136800	31.243648
549.521883	31701.055191	31.248666
549.562947	31756.707358	31.253684
550.664318	31803.881094	31.258701
550.923494	31849.909225	31.263719
551.557548	31905.963953	31.268736
552.347373	31966.491010	31.273754
553.093128	31999.829171	31.278772
553.381000	32059.263807	31.283789
553.934924	32109.392768	31.288807
554.421320	32167.872504	31.293824
555.016432	32215.570975	31.298842
555.320278	32268.736686	31.303860
556.198733	32322.367465	31.308877
556.516613	32383.330603	31.313895
557.243232	32414.789024	31.318912
558.372881	32464.349760	31.323930
559.079358	32491.719553	31.328948
559.717232	32539.576082	31.333965
560.396344	32574.417174	31.338983
560.566983	32621.082606	31.344000
561.598615	32644.849508	31.349018
561.676776	32709.840024	31.354036
562.230876	32735.029262	31.359053
563.072807	32784.099269	31.364071
563.432153	32824.305510	31.369088
564.128123	32860.219557	31.374106
564.488293	32906.600246	31.379124
565.403988	32939.144004	31.384141
565.561433	32987.264349	31.389159
565.997282	33040.788255	31.394176
566.621586	33085.145941	31.399194
566.841401	33130.272786	31.404212
567.399180	33158.578487	31.409229
568.279020	33195.397165	31.414247
569.165295	33236.078506	31.419264
569.263644	33282.856622	31.424282
569.793287	33317.329001	31.429300
570.534092	33360.176070	31.434317
571.293344	33398.574993	31.439335
571.618899	33441.169983	31.444352
572.259793	33474.655510	31.449370
572.629371	33521.659083	31.454388
573.015647	33562.531204	31.459405
573.696461	33618.395123	31.464423
574.406345	33657.425177	31.469440
574.937514	33700.746324	31.474458
574.980246	33759.458398	31.479476
575.682031	33810.771746	31.484493
576.351363	33865.504898	31.489511
576.861009	33924.136886	31.494528
577.542040	33961.154453	31.499546
578.007058	34013.212364	31.504564
578.968275	34061.639745	31.509581
579.750049	34094.435687	31.514599
580.494857	34141.198386	31.519616
581.095575	34173.788432	31.524634
581.549715	34229.982146	31.529652
582.206689	34269.477655	31.534669
582.921000	34326.606074	31.539687
583.357657	34364.776427	31.544704
583.899855	34418.653567	31.549722
584.303291	34458.312865	31.554740
584.610985	34512.565016	31.559757
585.385864	34552.767591	31.564775
585.871425	34620.122129	31.569792
586.824232	34664.067551	31.574810
586.857242	34717.115545	31.579828
587.522619	34753.815768	31.584845
588.303554	34799.709075	31.589863
588.857234	34862.812996	31.594880
590.068896	34902.316257	31.599898
590.560259	34955.962024	31.604916
591.086814	35008.233951	31.609933
591.883546	35047.540361	31.614951
591.925445	35108.768690	31.619968
593.003289	35149.471507	31.624986
593.054935	35208.917183	31.630004
593.219716	35255.877856	31.635021
593.897096	35315.255788	31.640039
593.718796	35376.181206	31.645056
594.917725	35426.389297	31.650074
595.341989	35488.349544	31.655092
596.018440	35563.995367	31.660109
596.514001	35602.040924	31.665127
597.066094	35678.736563	31.670144
597.933979	35732.742646	31.675162
598.542731	35800.903711	31.680180
599.094732	35847.451219	31.685197
600.070797	35893.414203	31.690215
600.569792	35936.793574	31.695232
601.347398	35988.472042	31.700250
601.950942	36032.391550	31.705268
602.378295	36087.853190	31.710285
603.196491	36122.578667	31.715303
603.420291	36186.511069	31.720320
604.188790	36234.079929	31.725338
604.756959	36291.419644	31.730356
605.584369	36319.009828	31.735373
606.496767	36378.019852	31.740391
606.715565	36432.842620	31.745408
607.482535	36475.955250	31.750426
607.757921	36532.866268	31.755444
608.488757	36581.876862	31.760461
609.100509	36640.007034	31.765479
609.210604	36698.116389	31.770496
609.949146	36752.163695	31.775514
610.706635	36816.475463	31.780532
611.013074	36878.918411	31.785549
611.813296	36924.879113	31.790567
612.075704	37009.508803	31.795584
613.086601	37053.563196	31.800602
613.888105	37113.682958	31.805620
614.740929	37165.944332	31.810637
615.702379	37192.792478	31.815655
616.595771	37259.063065	31.820672
617.181629	37297.727192	31.825690
617.826108	37342.829298	31.830708
618.566845	37394.245185	31.835725
619.311955	37439.042981	31.840743
619.276724	37488.506166	31.845760
619.971126	37532.825075	31.850778
620.734395	37585.377941	31.855796
621.264557	37636.709843	31.860813
622.054159	37673.499164	31.865831
622.311690	37742.668494	31.870848
623.000430	37786.932207	31.875866
623.740039	37846.908339	31.880884
624.331205	37886.239943	31.885901
624.715023	37944.691573	31.890919
624.985784	38003.103066	31.895936
625.441718	38060.537622	31.900954
626.478018	38109.562355	31.905972
626.473166	38187.223753	31.910989
627.611079	38232.613899	31.916007
628.230757	38303.620017	31.921024
629.138367	38357.762224	31.926042
629.962525	38414.022954	31.931060
630.408144	38462.371703	31.936077
631.549312	38489.891836	31.941095
631.982230	38564.296896	31.946112
632.551321	38605.587389	31.951130
633.413158	38645.618772	31.956148
633.986418	38689.881160	31.961165
634.487365	38736.693913	31.966183
634.475817	38796.668447	31.971200
635.232114	38835.174915	31.976218
635.827592	38892.180080	31.981236
636.060740	38943.905417	31.986253
636.738280	38999.685260	31.991271
637.276915	39062.408346	31.996288
638.063107	39119.361828	32.001306
638.616456	39174.028235	32.006324
639.051016	39243.511362	32.011341
639.664141	39304.738040	32.016359
640.100172	39371.379869	32.021376
640.930324	39440.319848	32.026394
641.659248	39503.036333	32.031412
641.610900	39582.890328	32.036429
642.684222	39633.553582	32.041447
643.255271	39722.061599	32.046464
643.960594	39785.295386	32.051482
644.907379	39852.017035	32.056500
646.116677	39911.370575	32.061517
646.903953	39972.951969	32.066535
647.497920	40029.240504	32.071552
648.494378	40082.604496	32.076570
649.003298	40138.462225	32.081588
649.715993	40197.381740	32.086605
650.319111	40241.681254	32.091623
650.599470	40309.151065	32.096640
651.024629	40361.392608	32.101658
652.015839	40429.557129	32.106676
652.187651	40490.743208	32.111693
653.127842	40555.793865	32.116711
653.445260	40628.374889	32.121728
654.005285	40702.109829	32.126746
654.929397	40764.322022	32.131764
655.519509	40825.890569	32.136781
656.594622	40882.679343	32.141799
656.884201	40949.197663	32.146816
657.724614	41017.609325	32.151834
658.515070	41082.528118	32.156852
658.976643	41149.552877	32.161869
659.923360	41205.410611	32.166887
660.283494	41270.840218	32.171904
661.077543	41342.714379	32.176922
661.773708	41397.086005	32.181940
662.083293	41474.765880	32.186957
663.092971	41529.311954	32.191975
663.557948	41595.536737	32.196992
664.274126	41664.775087	32.202010
665.444285	41729.878745	32.207028
665.727305	41772.337472	32.212045
667.677501	41813.272294	32.217063
668.325972	41856.430066	32.222080
669.217863	41899.555497	32.227098
669.569694	41944.814165	32.232116
670.487083	41977.163808	32.237133
671.143137	42009.473111	32.242151
671.485157	42052.897818	32.247168
672.012040	42091.583793	32.252186
673.174152	42121.339741	32.257204
673.320081	42163.628846	32.262221
674.251239	42208.572009	32.267239
674.440210	42256.188487	32.272256
674.665649	42298.055196	32.277274
675.784101	42351.920993	32.282292
675.930028	42407.213021	32.287309
676.486974	42465.969547	32.292327
676.986123	42526.287443	32.297344
677.629525	42588.954701	32.302362
678.265866	42640.667990	32.307380
678.601838	42719.276667	32.312397
679.070127	42775.622598	32.317415
679.880671	42869.095870	32.322432
680.309197	42934.334782	32.327450
681.062791	43008.909947	32.332468
681.490815	43077.392294	32.337485
682.158595	43154.521124	32.342503
682.712811	43239.116230	32.347520
683.375923	43315.284385	32.352538
684.196701	43408.765247	32.357556
684.809526	43487.497361	32.362573
685.808345	43566.815068	32.367591
686.316705	43660.268160	32.372608
687.185891	43733.654521	32.377626
688.229987	43802.571617	32.382644
688.471403	43896.390252	32.387661
689.654721	43957.985935	32.392679
690.395732	44043.668813	32.397696
691.102258	44115.388621	32.402714
691.938449	44196.116848	32.407732
692.658846	44256.736776	32.412749
693.252952	44333.570252	32.417767
693.980247	44395.508243	32.422784
695.198938	44474.138897	32.427802
695.998420	44535.024821	32.432820
696.365162	44614.747645	32.437837
696.989816	44676.267616	32.442855
697.967190	44749.855564	32.447872
698.676254	44802.942366	32.452890
699.345720	44868.377316	32.457908
700.095577	44945.696617	32.462925
701.142333	44995.272534	32.467943
701.746152	45068.593196	32.472960
702.273374	45129.240604	32.477978
703.290622	45176.515521	32.482996
703.908654	45240.076588	32.488013
704.330067	45300.750900	32.493031
704.977377	45371.330604	32.498048
705.697503	45442.996915	32.503066
706.604184	45494.439032	32.508084
707.090361	45562.839858	32.513101
707.578288	45612.500189	32.518119
708.381538	45670.890745	32.523136
708.933824	45719.600951	32.528154
710.156560	45771.895891	32.533172
710.294873	45851.174845	32.538189
710.866056	45899.119030	32.543207
711.664665	45959.003607	32.548224
712.483874	46026.678046	32.553242
713.257710	46095.022531	32.558260
713.824159	46163.775750	32.563277
714.541031	46222.500557	32.568295
715.061627	46305.030365	32.573312
715.565687	46368.670459	32.578330
716.252093	46435.812321	32.583348
717.048054	46522.044424	32.588365
717.862394	46584.771398	32.593383
718.763288	46666.778554	32.598400
719.053802	46737.688741	32.603418
720.014215	46814.951211	32.608436
720.561739	46885.811613	32.613453
721.077990	46968.774328	32.618471
721.994153	47038.825718	32.623488
722.647559	47128.166129	32.628506
723.609025	47192.733434	32.633524
724.218958	47279.863398	32.638541
724.923610	47351.621990	32.643559
725.627612	47433.039311	32.648576
726.222810	47521.463323	32.653594
726.805942	47601.556503	32.658612
727.386890	47682.486555	32.663629
728.853599	47768.390783	32.668647
729.380975	47834.553575	32.673664
730.050418	47924.419246	32.678682
731.171001	47991.273874	32.683700
731.977947	48082.677220	32.688717
732.795295	48153.995147	32.693735
733.628293	48223.275619	32.698752
733.974484	48307.697938	32.703770
734.831769	48376.097927	32.708788
735.598490	48452.338159	32.713805
736.435920	48534.124267	32.718823
737.438260	48604.401646	32.723840
737.921617	48679.741315	32.728858
738.925095	48748.311953	32.733876
739.625469	48834.109840	32.738893
740.192788	48890.589027	32.743911
740.971598	48972.089861	32.748928
741.556924	49040.917528	32.753946
742.367497	49113.310127	32.758964
743.133132	49188.790039	32.763981
743.946522	49263.120337	32.768999
744.930255	49330.105934	32.774016
745.510892	49409.163152	32.779034
746.166633	49474.109316	32.784052
746.732423	49532.332700	32.789069
747.377141	49604.084697	32.794087
748.063553	49672.106636	32.799104
748.742515	49742.752404	32.804122
749.336848	49802.944439	32.809140
749.654652	49899.493583	32.814157
750.258656	49970.423576	32.819175
751.060166	50051.679583	32.824192
751.828551	50144.746956	32.829210
752.881960	50224.515152	32.834228
753.838346	50298.369409	32.839245
754.350194	50382.033562	32.844263
755.458811	50457.438991	32.849280
756.479856	50533.041718	32.854298
757.444719	50593.474078	32.859316
758.136674	50672.995695	32.864333
758.707365	50753.597342	32.869351
759.584864	50818.872859	32.874368
760.623983	50891.289933	32.879386
761.512071	50962.213347	32.884404
762.381573	51030.347007	32.889421
762.995047	51104.360164	32.894439
764.142200	51167.934005	32.899456
764.340808	51236.475058	32.904474
765.251849	51294.952189	32.909492
766.397764	51355.478226	32.914509
767.108782	51426.008758	32.919527
768.041687	51488.541647	32.924544
768.340509	51568.110870	32.929562
769.209655	51625.090325	32.934580
770.201038	51694.406393	32.939597
771.014122	51745.938363	32.944615
772.032198	51811.987283	32.949632
773.018200	51893.825073	32.954650
773.747439	51935.565011	32.959668
774.355844	52015.487752	32.964685
774.989468	52075.163555	32.969703
775.998754	52139.715926	32.974720
776.374442	52211.224495	32.979738
777.034514	52274.191747	32.984756
777.698232	52356.411175	32.989773
778.497484	52429.592228	32.994791
778.899590	52492.048971	32.999808
779.511698	52571.354969	33.004826
780.392969	52646.616401	33.009844
781.162534	52727.027940	33.014861
781.558270	52817.110075	33.019879
782.714583	52899.881654	33.024896
782.995618	52990.977128	33.029914
784.070115	53068.917635	33.034932
784.923979	53154.168853	33.039949
785.319201	53237.618628	33.044967
786.128903	53324.768306	33.049984
786.802635	53412.946917	33.055002
787.575317	53487.458978	33.060020
788.433819	53570.675567	33.065037
789.165419	53656.661943	33.070055
790.410365	53728.495808	33.075072
790.996203	53815.487776	33.080090
791.929713	53890.998569	33.085108
793.101063	53952.990691	33.090125
793.645784	54020.546569	33.095143
794.657694	54088.164063	33.100160
795.072822	54161.321706	33.105178
796.351031	54236.728565	33.110196
797.201192	54312.235435	33.115213
797.565183	54386.705753	33.120231
798.590469	54463.214395	33.125248
799.092793	54541.160750	33.130266
800.428521	54604.423107	33.135284
801.456186	54671.787738	33.140301
802.576809	54738.301330	33.145319
804.117313	54799.811446	33.150336
804.491479	54863.852757	33.155354
805.308307	54924.291599	33.160372
805.799991	54985.571546	33.165389
806.414289	55057.428963	33.170407
807.258000	55129.183858	33.175424
807.836248	55181.343791	33.180442
808.691794	55263.056544	33.185460
809.739884	55327.449927	33.190477
810.169177	55399.666427	33.195495
810.810962	55473.888615	33.200512
811.493227	55565.450775	33.205530
812.284016	55635.678760	33.210548
813.006807	55724.078540	33.215565
813.495046	55818.501281	33.220583
814.590221	55903.291305	33.225600
814.993069	55984.012334	33.230618
815.869646	56079.154329	33.235636
816.461631	56168.170541	33.240653
816.969663	56266.077551	33.245671
818.416400	56356.559144	33.250688
819.433631	56448.009249	33.255706
820.082207	56529.981559	33.260724
820.824012	56621.855189	33.265741
821.851255	56711.792858	33.270759
822.787160	56796.413464	33.275776
823.698660	56891.383622	33.280794
824.173841	56983.977075	33.285812
825.162845	57055.697425	33.290829
826.261547	57145.831041	33.295847
827.457640	57231.523488	33.300864
828.012244	57320.889008	33.305882
828.978981	57390.461122	33.310900
829.701518	57470.102265	33.315917
830.322940	57560.465402	33.320935
831.332940	57641.955764	33.325952
832.268278	57725.065321	33.330970
832.594994	57804.758271	33.335988
833.849125	57869.516080	33.341005
834.349017	57942.697370	33.346023
835.308041	58019.692302	33.351040
836.559030	58089.869018	33.356058
837.160888	58162.223561	33.361076
838.063697	58228.392958	33.366093
838.739929	58314.460458	33.371111
839.627212	58384.964536	33.376128
840.457413	58458.325764	33.381146
840.942202	58550.713976	33.386164
842.110852	58630.491162	33.391181
842.565971	58703.407894	33.396199
843.373438	58780.884746	33.401216
843.825752	58877.886189	33.406234
845.002701	58963.097152	33.411252
845.918665	59047.216568	33.416269
846.417588	59148.584866	33.421287
847.690841	59244.677707	33.426304
848.319165	59337.116432	33.431322
849.063849	59420.551228	33.436340
850.142363	59518.046765	33.441357
850.932150	59613.710109	33.446375
851.607322	59695.916339	33.451392
852.079550	59806.167938	33.456410
853.069799	59900.499983	33.461428
854.197123	60002.167579	33.466445
854.848157	60098.048083	33.471463
856.022009	60185.011201	33.476480
856.831607	60297.810618	33.481498
857.429019	60401.219248	33.486516
858.305466	60488.963652	33.491533
859.304659	60603.281929	33.496551
860.229361	60702.206907	33.501568
860.782940	60794.598403	33.506586
861.816984	60906.336376	33.511604
863.218553	60983.617283	33.516621
863.923967	61084.552688	33.521639
865.548807	61156.351835	33.526656
866.372031	61240.546380	33.531674
867.701417	61325.020726	33.536692
868.898244	61404.622112	33.541709
869.877092	61487.924629	33.546727
870.681891	61548.023827	33.551744
871.374029	61634.435609	33.556762
872.087543	61712.634231	33.561780
873.394520	61782.812749	33.566797
873.304909	61871.279413	33.571815
874.453114	61944.685786	33.576832
875.502566	62030.152019	33.581850
875.959083	62118.498192	33.586868
876.783966	62210.199775	33.591885
877.310562	62284.094800	33.596903
878.363641	62370.919869	33.601920
878.862884	62461.477659	33.606938
879.585742	62561.530813	33.611956
880.671827	62628.125520	33.616973
881.215853	62727.696427	33.621991
882.546724	62811.397179	33.627008
883.241414	62895.903760	33.632026
883.877491	62973.778852	33.637044
884.675608	63072.028997	33.642061
885.308244	63172.481839	33.647079
886.203224	63260.956190	33.652096
887.294001	63353.375746	33.657114
887.610809	63453.280303	33.662132
888.680986	63553.378146	33.667149
889.298357	63660.259477	33.672167
890.152333	63761.940276	33.677184
891.065535	63871.823273	33.682202
891.645102	63983.939102	33.687220
892.710973	64093.094816	33.692237
893.459206	64214.950148	33.697255
895.002121	64324.672380	33.702272
895.808007	64434.815712	33.707290
896.648884	64545.876310	33.712308
897.901440	64644.971803	33.717325
898.964164	64746.580404	33.722343
899.833986	64853.488234	33.727360
901.007989	64960.076644	33.732378
901.610915	65061.049461	33.737396
902.780254	65156.134000	33.742413
903.968261	65252.084583	33.747431
904.660387	65351.200263	33.752448
905.348409	65450.342372	33.757466
906.573350	65562.895340	33.762484
907.736709	65650.993771	33.767501
908.289395	65760.572266	33.772519
909.042075	65860.960092	33.777536
910.649038	65965.056344	33.782554
911.462994	66058.790067	33.787572
912.396247	66158.373726	33.792589
912.957735	66260.847071	33.797607
914.123531	66348.442943	33.802624
915.206187	66452.299926	33.807642
915.995440	66545.073428	33.812660
917.230648	66645.950778	33.817677
917.957381	66747.301226	33.822695
918.436533	66833.220796	33.827712
919.254573	66941.304489	33.832730
919.714018	67046.552538	33.837748
920.861477	67156.448604	33.842765
921.634036	67265.274144	33.847783
922.695057	67377.832179	33.852800
923.433147	67494.264278	33.857818
924.120706	67609.770133	33.862836
925.272825	67722.587319	33.867853
926.096842	67848.345099	33.872871
927.266062	67960.699765	33.877888
927.824556	68069.677580	33.882906
928.520200	68178.552052	33.887924
929.469540	68272.559221	33.892941
930.024893	68392.513108	33.897959
931.373337	68508.651985	33.902976
932.572497	68607.959504	33.907994
933.141748	68722.378844	33.913012
934.037751	68828.432589	33.918029
934.878324	68944.699090	33.923047
935.564295	69060.851886	33.928064
936.695507	69182.570137	33.933082
937.354910	69301.792792	33.938100
938.750352	69415.667736	33.943117
939.283274	69536.194498	33.948135
940.639788	69648.320564	33.953152
941.615283	69776.006286	33.958170
942.384801	69897.085202	33.963188
943.862777	70002.566198	33.968205
944.770657	70122.367161	33.973223
945.574047	70244.238922	33.978240
946.788275	70344.487944	33.983258
948.428530	70452.201173	33.988276
949.617085	70554.805779	33.993293
950.628533	70647.348582	33.998311
951.795480	70749.237338	34.003328
953.077064	70836.815977	34.008346
953.246113	70942.611359	34.013364
954.636610	71029.522717	34.018381
955.970251	71129.428167	34.023399
957.327391	71207.392202	34.028416
958.486965	71293.260982	34.033434
959.277245	71387.384184	34.038452
960.422918	71459.613928	34.043469
961.171452	71546.932997	34.048487
961.932298	71641.649729	34.053504
963.193912	71716.231489	34.058522
963.887626	71807.256900	34.063540
964.795368	71889.042162	34.068557
965.805970	71981.812500	34.073575
966.114468	72079.769029	34.078592
967.082975	72172.458489	34.083610
967.748530	72287.578255	34.088628
968.831029	72391.763713	34.093645
969.629041	72492.260445	34.098663
970.471013	72596.858065	34.103680
971.590118	72699.573292	34.108698
972.189763	72819.085728	34.113716
973.257780	72932.249451	34.118733
974.310646	73036.133352	34.123751
975.438774	73138.874682	34.128768
976.649485	73249.230728	34.133786
977.586941	73354.979868	34.138804
978.940652	73454.615763	34.143821
979.699622	73569.709097	34.148839
980.415287	73674.136547	34.153856
981.571521	73774.070864	34.158874
982.102226	73869.106518	34.163892
983.132924	73958.312361	34.168909
983.679917	74063.413256	34.173927
984.219080	74172.939621	34.178944
985.238762	74279.483133	34.183962
985.887986	74395.312767	34.188980
987.113125	74514.975942	34.193997
987.764637	74636.658588	34.199015
988.655949	74760.351408	34.204032
990.349447	74863.890066	34.209050
991.135978	74993.781705	34.214068
992.175668	75112.277168	34.219085
993.608065	75213.268030	34.224103
994.325593	75336.088284	34.229120
995.534322	75442.904906	34.234138
996.745205	75549.576390	34.239156
997.611196	75668.311304	34.244173
999.247144	75771.143295	34.249191
1000.062867	75879.844915	34.254208
1001.186077	75982.949152	34.259226
1002.098478	76099.031085	34.264244
1003.159521	76210.748077	34.269261
1003.934478	76321.082828	34.274279
1005.033821	76428.143252	34.279296
1005.811694	76550.828535	34.284314
1006.223746	76676.922519	34.289332
1007.298423	76787.888394	34.294349
1008.048310	76918.878965	34.299367
1008.871364	77051.925518	34.304384
1010.101875	77173.720887	34.309402
1010.931619	77310.920612	34.314420
1011.860094	77456.113694	34.319437
1013.191358	77585.979486	34.324455
1013.981992	77729.116956	34.329472
1014.902435	77848.671279	34.334490
1015.669772	78001.067827	34.339508
1016.978672	78132.621955	34.344525
1018.154594	78265.904699	34.349543
1019.170245	78396.356780	34.354560
1021.233580	78510.948277	34.359578
1022.197154	78645.891732	34.364596
1023.396729	78765.128868	34.369613
1024.476258	78887.584215	34.374631
1026.076559	78989.736473	34.379648
1027.240213	79100.169754	34.384666
1027.817954	79218.560273	34.389684
1028.779199	79329.191326	34.394701
1029.627078	79452.761471	34.399719
1030.284599	79573.764620	34.404736
1031.775751	79681.323336	34.409754
1032.519910	79811.302895	34.414772
1033.552697	79938.310588	34.419789
1034.552267	80045.544830	34.424807
1035.278408	80167.482413	34.429824
1036.783653	80279.839933	34.434842
1037.688563	80397.129470	34.439860
1038.444315	80509.601133	34.444877
1039.843042	80609.663124	34.449895
1040.865155	80728.737524	34.454912
1041.789142	80832.681682	34.459930
1043.055621	80940.813688	34.464948
1043.563510	81058.429295	34.469965
1044.510415	81176.702726	34.474983
1045.434843	81300.499274	34.480000
1046.203609	81409.458845	34.485018
1047.186126	81537.723369	34.490036
1048.305509	81658.443921	34.495053
1049.009569	81796.591109	34.500071
1049.731016	81927.636925	34.505088
1050.798808	82062.023362	34.510106
1052.173182	82210.984689	34.515124
1052.930332	82354.987612	34.520141
1053.737180	82498.787632	34.525159
1054.983514	82643.833736	34.530176
1056.296061	82787.871404	34.535194
1057.066301	82947.454156	34.540212
1058.077897	83082.684274	34.545229
1058.970802	83230.199419	34.550247
1060.150923	83388.765648	34.555264
1061.196133	83546.336619	34.560282
1062.146959	83694.256750	34.565300
1063.601630	83839.669938	34.570317
1064.934735	83971.320337	34.575335
1065.750823	84131.657124	34.580352
1067.546016	84270.740792	34.585370
1068.944911	84408.282452	34.590388
1070.331228	84539.460043	34.595405
1071.614654	84655.872248	34.600423
1072.963795	84792.526485	34.605440
1074.124441	84916.256133	34.610458
1075.409860	85046.466547	34.615476
1076.603564	85148.074960	34.620493
1077.532845	85274.201923	34.625511
1078.056585	85400.931586	34.630528
1080.036616	85517.813105	34.635546
1080.686098	85642.115141	34.640564
1081.807270	85760.588889	34.645581
1083.333448	85889.874611	34.650599
1084.324010	85990.267374	34.655616
1084.940897	86116.196071	34.660634
1086.055192	86228.388277	34.665652
1087.213119	86338.424232	34.670669
1088.861238	86445.063074	34.675687
1089.980077	86567.183862	34.680704
1091.045655	86681.251562	34.685722
1091.800572	86794.876055	34.690740
1092.824017	86913.833332	34.695757
1093.863124	87022.108492	34.700775
1094.539470	87151.138610	34.705792
1095.482291	87288.619595	34.710810
1096.769947	87408.947731	34.715828
1097.361590	87520.458337	34.720845
1098.180812	87642.866855	34.725863
1099.174769	87763.749571	34.730880
1099.726501	87891.052278	34.735898
1100.589587	88027.728571	34.740916
1101.335888	88166.915864	34.745933
1102.950854	88307.306547	34.750951
1104.075534	88442.502024	34.755968
1105.028174	88581.361942	34.760986
1106.392955	88721.567439	34.766004
1107.393831	88873.663871	34.771021
1108.663548	89002.737136	34.776039
1109.572204	89146.831297	34.781056
1111.121952	89281.894833	34.786074
1112.733325	89402.467147	34.791092
1113.984636	89532.191541	34.796109
1115.594160	89662.447890	34.801127
1116.572132	89787.897846	34.806144
1117.925790	89924.659827	34.811162
1119.355787	90023.388749	34.816180
1120.252580	90157.638203	34.821197
1121.237094	90286.271125	34.826215
1122.282996	90409.449713	34.831232
1123.051654	90536.081966	34.836250
1124.437885	90674.513110	34.841268
1125.032798	90807.979721	34.846285
1126.164352	90944.865612	34.851303
1126.945161	91099.074335	34.856320
1127.975278	91230.722380	34.861338
1128.930107	91377.107075	34.866356
1130.055573	91546.247330	34.871373
1130.882669	91689.352894	34.876391
1131.956468	91841.180039	34.881408
1132.841658	92006.193963	34.886426
1133.925091	92167.667258	34.891444
1135.125772	92333.449364	34.896461
1136.223100	92493.771681	34.901479
1137.329667	92663.087928	34.906496
1138.372121	92828.962149	34.911514
1139.660633	92992.141912	34.916532
1140.456498	93166.527253	34.921549
1142.105179	93327.400425	34.926567
1143.152351	93499.230954	34.931584
1144.288641	93667.702525	34.936602
1145.989714	93828.760744	34.941620
1146.988347	93986.003731	34.946637
1148.896324	94133.583367	34.951655
1149.948633	94276.606509	34.956672
1151.655944	94424.605833	34.961690
1153.101789	94563.254193	34.966708
1154.421165	94712.822603	34.971725
1155.750648	94842.129239	34.976743
1157.040789	94977.034811	34.981760
1158.420713	95108.833620	34.986778
1159.663354	95208.924880	34.991796
1160.656342	95335.763877	34.996813
1162.281680	95430.551165	35.001831
1162.794984	95538.281297	35.006848
1163.992114	95651.495307	35.011866
1165.175476	95776.889510	35.016884
1166.015437	95901.497661	35.021901
1167.137950	96013.529741	35.026919
1168.184435	96137.663532	35.031936
1169.351951	96266.010906	35.036954
1170.408733	96389.480202	35.041972
1171.613959	96520.973429	35.046989
1172.664247	96639.403178	35.052007
1173.384693	96781.191785	35.057024
1174.392861	96915.015047	35.062042
1175.222066	97062.228696	35.067060
1176.501107	97213.015742	35.072077
1177.673530	97353.926276	35.077095
1178.554626	97513.863274	35.082112
1179.774774	97659.519254	35.087130
1180.966699	97814.411026	35.092148
1181.732245	97986.712728	35.097165
1183.392173	98136.344488	35.102183
1184.285888	98297.727425	35.107200
1185.386944	98468.612848	35.112218
1186.589897	98624.273872	35.117236
1187.497638	98795.502474	35.122253
1188.770815	98963.447564	35.127271
1189.949214	99135.243034	35.132288
1191.274912	99301.303156	35.137306
1192.399452	99469.009835	35.142324
1193.186699	99643.958846	35.147341
1194.883979	99814.265945	35.152359
1196.236379	99997.106189	35.157376
1197.657634	100155.786180	35.162394
1198.898558	100320.576366	35.167412
1199.940030	100500.559509	35.172429
1201.475930	100650.860043	35.177447
1202.780545	100823.584418	35.182464
1204.184327	100979.653305	35.187482
1205.561553	101143.674698	35.192500
1206.404942	101303.903389	35.197517
1207.742802	101464.858155	35.202535
1209.125848	101624.471732	35.207552
1210.088883	101784.260749	35.212570
1211.378717	101957.774165	35.217588
1212.473102	102119.885815	35.222605
1213.714189	102286.524897	35.227623
1214.638969	102461.460544	35.232640
1215.867487	102627.294087	35.237658
1217.152286	102791.132903	35.242676
1218.489431	102959.564926	35.247693
1220.031295	103124.168833	35.252711
1221.571543	103293.115154	35.257728
1222.480025	103439.401166	35.262746
1224.058594	103589.479642	35.267764
1224.823113	103727.734685	35.272781
1226.247488	103877.219348	35.277799
1227.087599	104018.406661	35.282816
1228.244353	104178.826597	35.287834
1229.640374	104329.698178	35.292852
1230.454558	104492.807262	35.297869
1231.482496	104656.434048	35.302887
1232.612915	104815.185450	35.307904
1233.861141	104979.399615	35.312922
1235.217618	105151.755128	35.317940
1236.211803	105321.220386	35.322957
1238.103647	105468.583958	35.327975
1239.232965	105639.662763	35.332992
1240.425196	105808.030446	35.338010
1242.166569	105953.534988	35.343028
1243.445028	106122.429112	35.348045
1244.598644	106273.547709	35.353063
1245.763766	106447.025191	35.358080
1246.851288	106606.959802	35.363098
1248.441785	106758.081607	35.368116
1249.464989	106932.224366	35.373133
1250.885079	107092.362486	35.378151
1252.182136	107248.755446	35.383168
1253.285764	107418.559859	35.388186
1254.950547	107586.529413	35.393204
1256.118961	107753.927138	35.398221
1257.900568	107894.740764	35.403239
1259.766727	108036.763312	35.408256
1261.073916	108201.566061	35.413274
1262.563422	108335.669000	35.418292
1263.300567	108486.563831	35.423309
1264.805313	108633.046233	35.428327
1265.895632	108781.544866	35.433344
1267.320685	108927.611305	35.438362
1269.559459	109050.414879	35.443380
1270.750990	109195.431369	35.448397
1271.842025	109332.356493	35.453415
1273.222157	109473.236747	35.458432
1273.895221	109620.623169	35.463450
1275.339533	109756.918508	35.468468
1276.118414	109914.942756	35.473485
1277.142392	110070.245232	35.478503
1278.287947	110214.787665	35.483520
1279.419629	110380.367256	35.488538
1280.645483	110542.527503	35.493556
1281.438934	110712.100284	35.498573
1282.386386	110883.953861	35.503591
1283.432221	111054.710558	35.508608
1284.462261	111236.358670	35.513626
1285.663904	111423.469050	35.518644
1287.269501	111608.415010	35.523661
1288.650631	111789.701185	35.528679
1289.981064	111966.381980	35.533696
1291.121271	112147.189976	35.538714
1292.489000	112312.789267	35.543732
1293.995498	112475.183414	35.548749
1294.883972	112641.430803	35.553767
1296.152673	112793.622184	35.558784
1297.698273	112974.555315	35.563802
1299.237848	113134.182050	35.568820
1300.150706	113315.768983	35.573837
1301.484760	113480.938219	35.578855
1302.818053	113637.334335	35.583872
1303.819243	113826.267169	35.588890
1305.147407	113992.960079	35.593908
1306.632969	114173.632837	35.598925
1308.038891	114346.912441	35.603943
1309.228001	114526.014143	35.608960
1310.548386	114692.769890	35.613978
1311.956721	114877.385143	35.618996
1313.144955	115065.955639	35.624013
1314.456310	115236.508692	35.629031
1315.824816	115423.711001	35.634048
1316.828403	115615.398184	35.639066
1318.420685	115808.702666	35.644084
1319.514558	115994.211734	35.649101
1320.850624	116177.176452	35.654119
1322.059453	116370.121937	35.659136
1323.374045	116571.985687	35.664154
1324.709274	116754.416495	35.669172
1325.940635	116959.924454	35.674189
1327.532147	117145.869285	35.679207
1329.124296	117337.722743	35.684224
1330.557770	117524.999744	35.689242
1332.503196	117701.546828	35.694260
1333.999334	117889.088776	35.699277
1335.388435	118075.275102	35.704295
1336.915456	118250.904687	35.709312
1338.184587	118435.447402	35.714330
1339.475524	118596.920807	35.719348
1340.813603	118779.656749	35.724365
1342.200620	118974.714602	35.729383
1343.952212	119142.956747	35.734400
1344.931467	119330.205012	35.739418
1346.090825	119508.915610	35.744436
1347.450767	119684.758736	35.749453
1348.470037	119881.084927	35.754471
1349.807027	120060.644909	35.759488
1350.974989	120264.954326	35.764506
1352.169144	120440.790883	35.769524
1353.564320	120641.723634	35.774541
1354.884573	120843.619695	35.779559
1356.877170	121025.779699	35.784576
1358.107311	121208.138133	35.789594
1359.958853	121385.143022	35.794612
1361.742706	121549.671922	35.799629
1363.330000	121729.026186	35.804647
1364.879180	121892.758606	35.809664
1366.105786	122063.800628	35.814682
1367.390516	122202.777974	35.819700
1368.493634	122388.027134	35.824717
1369.811539	122532.763802	35.829735
1371.305030	122686.440725	35.834752
1372.184906	122860.380107	35.839770
1373.328561	123020.979456	35.844788
1374.437056	123193.187434	35.849805
1375.479556	123363.380431	35.854823
1376.749230	123546.470583	35.859840
1377.884001	123728.684118	35.864858
1379.347521	123906.147423	35.869876
1380.553445	124108.124419	35.874893
1381.709038	124309.236935	35.879911
1383.019821	124496.709648	35.884928
1384.550340	124697.803476	35.889946
1385.820629	124889.440039	35.894964
1387.579472	125087.447775	35.899981
1388.779139	125279.123651	35.904999
1390.426146	125484.258248	35.910016
1391.753392	125674.928609	35.915034
1393.470822	125869.237144	35.920052
1394.666354	126071.002413	35.925069
1396.195027	126262.670934	35.930087
1397.886922	126464.030872	35.935104
1399.074569	126662.254845	35.940122
1400.714985	126840.874657	35.945140
1402.526265	127048.110413	35.950157
1403.675862	127227.520139	35.955175
1405.233658	127422.523804	35.960192
1406.649225	127632.069080	35.965210
1408.160678	127822.053705	35.970228
1409.179646	128022.125830	35.975245
1410.264761	128228.396387	35.980263
1411.655405	128422.280852	35.985280
1413.143644	128631.353417	35.990298
1414.572074	128835.242917	35.995316
1415.834695	129055.781643	36.000333
1417.196112	129256.086952	36.005351
1418.795537	129457.977501	36.010368
1419.979566	129672.579197	36.015386
1421.329256	129886.991516	36.020404
1422.602352	130115.417130	36.025421
1423.798950	130330.325925	36.030439
1425.517215	130547.079218	36.035456
1426.575554	130781.080900	36.040474
1427.839195	130993.424859	36.045492
1429.441725	131228.167297	36.050509
1430.689045	131455.328224	36.055527
1432.834638	131670.159773	36.060544
1433.928032	131903.430309	36.065562
1435.963699	132114.367652	36.070580
1437.520720	132328.600850	36.075597
1439.394973	132535.233750	36.080615
1441.179857	132745.366707	36.085632
1442.431716	132944.676618	36.090650
1443.912479	133135.779027	36.095668
1445.262767	133315.461847	36.100685
1446.368542	133512.100067	36.105703
1447.981362	133694.898559	36.110720
1449.166356	133886.699172	36.115738
1450.279441	134087.255466	36.120756
1451.754900	134281.559419	36.125773
1452.609435	134495.438912	36.130791
1454.537873	134695.641790	36.135808
1455.555666	134906.824743	36.140826
1456.818095	135134.544602	36.145844
1458.212235	135345.113396	36.150861
1459.515879	135572.057164	36.155879
1461.317291	135784.984706	36.160896
1462.249102	136021.330106	36.165914
1463.707876	136234.290016	36.170932
1465.524296	136470.016947	36.175949
1466.614664	136699.626448	36.180967
1468.249808	136924.335740	36.185984
1469.728059	137163.302683	36.191002
1471.291630	137396.289294	36.196020
1472.499870	137642.247496	36.201037
1473.790612	137869.058968	36.206055
1476.492285	138084.825502	36.211072
1478.140271	138330.123919	36.216090
1479.844890	138541.325223	36.221108
1481.579562	138765.551091	36.226125
1482.791650	138986.541321	36.231143
1484.576224	139216.161379	36.236160
1485.874325	139437.001860	36.241178
1487.338756	139660.504296	36.246196
1488.694738	139884.595928	36.251213
1489.783630	140109.301972	36.256231
1491.757239	140337.835983	36.261248
1493.028971	140570.107930	36.266266
1494.886521	140795.862941	36.271284
1496.422360	141014.079052	36.276301
1498.037570	141243.449947	36.281319
1499.459854	141465.654314	36.286336
1501.236396	141689.134812	36.291354
1503.373634	141893.573520	36.296372
1504.935671	142102.148112	36.301389
1506.475108	142318.218335	36.306407
1508.131376	142521.077289	36.311424
1509.883953	142725.012304	36.316442
1511.546597	142922.638265	36.321460
1512.893985	143130.899050	36.326477
1514.177596	143347.384713	36.331495
1515.831332	143542.405027	36.336512
1517.111181	143759.654669	36.341530
1518.506166	143956.303079	36.346548
1519.748477	144183.765154	36.351565
1521.253117	144381.843813	36.356583
1522.732583	144608.130532	36.361600
1523.894199	144819.664388	36.366618
1525.819581	145012.483251	36.371636
1527.261973	145210.323540	36.376653
1528.373877	145421.260923	36.381671
1530.027009	145616.864715	36.386688
1531.621768	145813.125468	36.391706
1532.708596	146027.239871	36.396724
1534.316098	146236.633567	36.401741
1535.560408	146453.223025	36.406759
1536.778657	146663.847590	36.411776
1538.311102	146883.652011	36.416794
1539.680202	147109.302379	36.421812
1540.876393	147335.349431	36.426829
1542.649099	147564.310857	36.431847
1543.912983	147790.616587	36.436864
1545.411056	148035.230026	36.441882
1546.436837	148274.139693	36.446900
1548.342725	148519.452650	36.451917
1549.244693	148785.907523	36.456935
1551.453045	149020.273950	36.461952
1552.714645	149293.166592	36.466970
1554.152545	149546.269475	36.471988
1555.524952	149801.451164	36.477005
1557.290650	150051.323860	36.482023
1559.034306	150298.501627	36.487040
1561.218616	150568.938376	36.492058
1563.064579	150814.443003	36.497076
1564.360020	151061.799154	36.502093
1565.849432	151320.549292	36.507111
1567.430819	151567.065099	36.512128
1568.811992	151832.251596	36.517146
1570.436096	152098.213045	36.522164
1572.363688	152344.235906	36.527181
1574.050854	152607.554299	36.532199
1576.040319	152851.504480	36.537216
1577.717476	153108.882135	36.542234
1579.314351	153345.252995	36.547252
1581.285790	153591.721854	36.552269
1582.856328	153848.754440	36.557287
1584.789671	154081.374763	36.562304
1586.345872	154324.681774	36.567322
1587.864514	154563.241766	36.572340
1589.779368	154797.201286	36.577357
1591.422267	155033.247012	36.582375
1593.078679	155257.576317	36.587392
1594.752600	155500.898429	36.592410
1596.248380	155724.406785	36.597428
1598.342779	155953.857116	36.602445
1599.667114	156196.035121	36.607463
1601.368108	156420.910219	36.612480
1603.215245	156638.764177	36.617498
1604.589231	156874.345438	36.622516
1605.393300	157096.641172	36.627533
1606.972659	157345.773563	36.632551
1608.983939	157588.638420	36.637568
1610.664025	157807.997206	36.642586
1611.945438	158028.168851	36.647604
1613.605679	158245.872393	36.652621
1614.881938	158472.654282	36.657639
1616.549075	158689.319671	36.662656
1618.257032	158912.104789	36.667674
1619.530522	159137.547243	36.672692
1621.574065	159359.888790	36.677709
1622.854915	159587.945255	36.682727
1624.576326	159804.190412	36.687744
1626.145450	160026.205704	36.692762
1627.669304	160257.005088	36.697780
1630.531812	160466.592875	36.702797
1631.905864	160700.056670	36.707815
1633.668972	160918.762209	36.712832
1635.159712	161143.155697	36.717850
1636.281199	161364.806561	36.722868
1637.584563	161602.624635	36.727885
1638.698990	161851.215889	36.732903
1640.331858	162087.881506	36.737920
1641.727969	162346.691197	36.742938
1642.901337	162598.296570	36.747956
1644.582638	162852.055105	36.752973
1645.949354	163130.545290	36.757991
1647.614992	163400.619689	36.763008
1649.309723	163662.181454	36.768026
1650.660068	163938.131191	36.773044
1653.375121	164198.621592	36.778061
1655.192077	164467.753975	36.783079
1657.612556	164710.259768	36.788096
1659.891104	164955.288248	36.793114
1661.321032	165201.239467	36.798132
1663.101983	165435.950001	36.803149
1664.530125	165697.758766	36.808167
1666.557452	165940.182828	36.813184
1668.238817	166187.483108	36.818202
1669.587843	166442.067402	36.823220
1671.050780	166691.802875	36.828237
1672.591277	166951.243394	36.833255
1674.120236	167202.633327	36.838272
1675.681684	167465.308408	36.843290
1677.375255	167731.097261	36.848308
1679.077058	167994.425960	36.853325
1680.482315	168263.143586	36.858343
1682.153625	168521.610056	36.863360
1684.106027	168786.337730	36.868378
1685.212454	169057.708657	36.873396
1686.936342	169319.546191	36.878413
1688.709084	169604.679294	36.883431
1690.384626	169878.109301	36.888448
1691.923038	170154.810305	36.893466
1693.275446	170448.337542	36.898484
1695.220359	170724.686287	36.903501
1697.278186	170992.139537	36.908519
1699.409793	171246.390385	36.913536
1701.157160	171507.262131	36.918554
1703.083052	171774.576744	36.923572
1705.048448	172010.148136	36.928589
1706.292738	172252.558705	36.933607
1707.614444	172500.552767	36.938624
1709.060871	172746.701845	36.943642
1710.309268	173016.009850	36.948660
1712.335981	173270.493294	36.953677
1713.885182	173540.010770	36.958695
1715.537517	173805.479551	36.963712
1717.481951	174071.867835	36.968730
1719.246469	174342.079580	36.973748
1720.846649	174601.231507	36.978765
1722.235581	174869.869882	36.983783
1723.948433	175144.243561	36.988800
1725.453417	175437.948133	36.993818
1727.339698	175711.600321	36.998836
1729.616966	175970.501177	37.003853
1731.632473	176258.040983	37.008871
1733.617448	176510.800539	37.013888
1736.194416	176763.670633	37.018906
1737.851203	177036.581446	37.023924
1739.738658	177284.413295	37.028941
1741.830005	177541.513861	37.033959
1743.558329	177795.983968	37.038976
1745.378754	178046.317647	37.043994
1746.773807	178296.758411	37.049012
1749.002668	178548.438513	37.054029
1750.991484	178797.671483	37.059047
1752.366106	179057.331073	37.064064
1754.396825	179294.938538	37.069082
1755.450949	179556.123810	37.074100
1757.166110	179809.618450	37.079117
1758.927201	180088.394129	37.084135
1760.525976	180347.353496	37.089152
1762.150382	180621.167973	37.094170
1763.551897	180905.791735	37.099188
1765.650475	181173.139632	37.104205
1767.032310	181450.207946	37.109223
1768.522415	181729.227514	37.114240
1770.479383	182015.965408	37.119258
1771.883059	182303.706584	37.124276
1773.809215	182597.901292	37.129293
1775.355170	182879.165153	37.134311
1777.211460	183180.087107	37.139328
1778.967603	183486.775024	37.144346
1780.326529	183795.050774	37.149364
1782.714074	184076.797645	37.154381
1784.878607	184373.262926	37.159399
1786.560041	184669.134326	37.164416
1788.399477	184964.030883	37.169434
1790.062789	185241.255737	37.174452
1792.327513	185527.776944	37.179469
1794.163329	185817.058203	37.184487
1795.913017	186092.091919	37.189504
1798.258715	186355.941943	37.194522
1799.997399	186622.148604	37.199540
1802.345935	186867.461482	37.204557
1804.323363	187117.783598	37.209575
1805.742464	187361.546195	37.214592
1807.796743	187599.118057	37.219610
1809.336030	187839.970763	37.224628
1811.190462	188087.703461	37.229645
1812.649549	188333.419038	37.234663
1814.159876	188589.533735	37.239680
1816.036991	188845.452000	37.244698
1817.708723	189116.112368	37.249716
1819.630912	189373.104999	37.254733
1821.254344	189643.991767	37.259751
1823.119705	189912.265477	37.264768
1825.207486	190166.926398	37.269786
1826.411309	190448.227172	37.274804
1828.569484	190726.154630	37.279821
1830.044775	190994.458197	37.284839
1831.599973	191274.058167	37.289856
1833.516372	191555.759870	37.294874
1835.184021	191848.581981	37.299892
1837.035615	192141.160886	37.304909
1838.571926	192436.405961	37.309927
1840.296173	192739.098137	37.314944
1841.775062	193050.867360	37.319962
1843.904203	193362.586079	37.324980
1845.694239	193664.981520	37.329997
1847.502909	193966.030509	37.335015
1849.081371	194288.147957	37.340032
1851.211275	194603.275599	37.345050
1853.134346	194922.791326	37.350068
1854.982445	195234.198117	37.355085
1857.057735	195541.699677	37.360103
1859.121215	195848.418038	37.365120
1861.178089	196167.069891	37.370138
1863.253999	196492.523713	37.375156
1865.179361	196793.875384	37.380173
1866.887178	197102.688360	37.385191
1868.694527	197421.209773	37.390208
1870.872181	197726.956417	37.395226
1872.395282	198049.131405	37.400244
1874.357533	198365.374622	37.405261
1876.596535	198675.115173	37.410279
1878.240461	198990.435263	37.415296
1880.094099	199309.024068	37.420314
1881.911107	199625.081967	37.425332
1884.032021	199924.732129	37.430349
1885.908084	200244.452541	37.435367
1887.788873	200555.809253	37.440384
1889.954237	200867.579519	37.445402
1892.086794	201197.889027	37.450420
1893.499417	201504.260742	37.455437
1895.720423	201800.579543	37.460455
1897.454715	202133.026837	37.465472
1899.053182	202435.223359	37.470490
1901.037679	202724.666544	37.475508
1902.974537	203017.634938	37.480525
1904.771593	203315.107945	37.485543
1906.377983	203597.329325	37.490560
1908.709407	203875.984277	37.495578
1910.358163	204179.667250	37.500596
1911.935440	204478.628271	37.505613
1914.462295	204759.287517	37.510631
1916.377314	205064.430767	37.515648
1918.118486	205364.423935	37.520666
1920.301474	205662.177786	37.525684
1922.358030	205932.292128	37.530701
1924.959314	206226.681898	37.535719
1926.802269	206535.690602	37.540736
1928.814196	206812.366387	37.545754
1931.074022	207100.810116	37.550772
1933.274696	207367.112373	37.555789
1936.076162	207645.291608	37.560807
1937.826963	207900.508915	37.565824
1940.093430	208184.132718	37.570842
1941.741974	208460.048516	37.575860
1943.968823	208724.460999	37.580877
1945.636031	208996.542353	37.585895
1947.196927	209276.665060	37.590912
1949.102096	209554.398488	37.595930
1950.590030	209834.547968	37.600948
1952.347137	210128.011388	37.605965
1954.207490	210423.160959	37.610983
1956.020999	210713.723611	37.616000
1957.828670	211019.421466	37.621018
1959.520580	211321.851016	37.626036
1961.114966	211641.487239	37.631053
1963.064243	211947.700242	37.636071
1964.407963	212274.158813	37.641088
1966.643113	212591.603240	37.646106
1968.854228	212923.653186	37.651124
1971.127717	213238.745924	37.656141
1973.245754	213555.718429	37.661159
1975.216888	213884.104048	37.666176
1977.131599	214203.663777	37.671194
1979.180444	214528.764629	37.676212
1980.888493	214857.196726	37.681229
1982.666768	215188.628267	37.686247
1984.714627	215515.993909	37.691264
1986.434799	215852.427507	37.696282
1988.673128	216186.914147	37.701300
1989.959678	216520.448815	37.706317
1992.279284	216860.639191	37.711335
1994.336134	217215.880275	37.716352
1996.364833	217555.701161	37.721370
1998.080887	217904.257823	37.726388
1999.952379	218247.979432	37.731405
2002.270438	218583.302693	37.736423
2004.230374	218941.881554	37.741440
2006.404514	219272.863084	37.746458
2008.287009	219607.612598	37.751476
2010.041843	219927.680670	37.756493
2012.351376	220244.957619	37.761511
2013.816282	220590.583052	37.766528
2015.490803	220961.825236	37.771546
2017.522120	221300.723382	37.776564
2019.601947	221633.063498	37.781581
2021.831625	221964.086139	37.786599
2023.497788	222317.534440	37.791616
2025.258157	222660.189198	37.796634
2027.141505	223018.482054	37.801652
2028.789239	223371.836441	37.806669
2031.458718	223715.075303	37.811687
2033.791943	224072.095248	37.816704
2036.020640	224422.505103	37.821722
2037.900504	224780.082611	37.826740
2040.452898	225132.209165	37.831757
2042.823595	225481.483611	37.836775
2044.478138	225837.984033	37.841792
2046.881674	226176.386679	37.846810
2049.852274	226522.294202	37.851828
2051.651350	226860.668503	37.856845
2053.957418	227202.519215	37.861863
2055.659496	227557.266966	37.866880
2057.572183	227901.849491	37.871898
2059.434952	228260.206334	37.876916
2061.329898	228619.880168	37.881933
2063.263785	228970.000025	37.886951
2064.966900	229333.389730	37.891968
2067.480310	229692.284046	37.896986
2069.558876	230064.734708	37.902004
2071.609840	230425.279900	37.907021
2073.625914	230794.340184	37.912039
2076.052373	231163.920974	37.917056
2077.987283	231530.990633	37.922074
2079.997476	231905.999271	37.927092
2081.725749	232277.295218	37.932109
2083.965062	232646.733672	37.937127
2086.027835	233019.782659	37.942144
2088.232345	233391.413683	37.947162
2090.170781	233772.206279	37.952180
2092.198673	234156.364115	37.957197
2094.480287	234532.685846	37.962215
2096.399763	234915.466842	37.967232
2098.487082	235296.063756	37.972250
2100.677679	235682.868370	37.977268
2102.910795	236070.988404	37.982285
2105.519705	236435.251480	37.987303
2107.593298	236814.992497	37.992320
2109.872487	237184.796598	37.997338
2112.699007	237544.863456	38.002356
2114.631838	237907.232183	38.007373
2116.985076	238276.393226	38.012391
2118.956482	238639.850381	38.017408
2121.082303	238993.987995	38.022426
2122.986326	239339.526032	38.027444
2124.782177	239682.593093	38.032461
2127.485866	239999.050672	38.037479
2130.007157	240339.820218	38.042496
2132.228664	240646.246896	38.047514
2135.007013	240964.320795	38.052532
2137.213902	241276.136174	38.057549
2139.291454	241583.756456	38.062567
2141.294770	241906.299138	38.067584
2143.541917	242222.987344	38.072602
2145.831355	242531.973368	38.077620
2147.889895	242864.238034	38.082637
2150.145113	243168.252568	38.087655
2152.171548	243472.304099	38.092672
2154.803479	243792.618211	38.097690
2156.792578	244112.679444	38.102708
2158.215139	244430.113431	38.107725
2160.354982	244758.407488	38.112743
2161.883161	245098.610675	38.117760
2164.160523	245437.044830	38.122778
2165.781990	245777.412687	38.127796
2167.319539	246145.456258	38.132813
2169.445640	246512.340591	38.137831
2171.280430	246875.690504	38.142848
2173.330342	247257.981819	38.147866
2175.574492	247637.677790	38.152884
2177.668911	248025.247440	38.157901
2179.969896	248402.192969	38.162919
2181.857908	248793.429662	38.167936
2183.870779	249192.064735	38.172954
2186.018061	249589.892035	38.177972
2187.540833	250002.018806	38.182989
2189.924266	250398.921557	38.188007
2191.986780	250820.820570	38.193024
2193.708311	251236.754484	38.198042
2196.327242	251656.357343	38.203060
2198.581086	252080.235795	38.208077
2200.557326	252497.249943	38.213095
2202.964663	252927.812120	38.218112
2205.370596	253358.070680	38.223130
2208.035837	253779.880995	38.228148
2209.875565	254217.420035	38.233165
2212.332140	254625.624297	38.238183
2214.894837	255052.788016	38.243200
2217.321648	255469.305197	38.248218
2219.783281	255879.467086	38.253236
2222.408523	256297.249919	38.258253
2225.455443	256696.041862	38.263271
2227.390785	257109.337761	38.268288
2229.622356	257510.876859	38.273306
2232.026482	257907.740602	38.278324
2233.994949	258313.590382	38.283341
2236.675186	258704.238790	38.288359
2239.246723	259088.732179	38.293376
2241.397419	259476.010951	38.298394
2244.059007	259833.792891	38.303412
2246.165257	260189.605726	38.308429
2248.543119	260550.989962	38.313447
2250.554278	260905.091372	38.318464
2252.696332	261261.306289	38.323482
2255.120424	261611.075372	38.328500
2256.770544	261976.310931	38.333517
2259.093953	262331.583801	38.338535
2261.169711	262685.143511	38.343552
2263.169425	263058.784019	38.348570
2265.733538	263434.697916	38.353588
2267.407124	263814.081197	38.358605
2269.643733	264193.451797	38.363623
2271.765904	264589.073496	38.368640
2274.009861	264969.332777	38.373658
2276.349308	265373.456225	38.378676
2277.813754	265767.430485	38.383693
2279.892729	266175.482633	38.388711
2282.236043	266590.834744	38.393728
2284.144608	267009.787172	38.398746
2286.561043	267435.365865	38.403764
2288.787887	267869.535840	38.408781
2290.919451	268284.643356	38.413799
2293.244591	268729.112079	38.418816
2295.472293	269160.920274	38.423834
2297.670611	269602.234225	38.428852
2299.800274	270044.270592	38.433869
2302.367357	270493.909645	38.438887
2304.725470	270949.526421	38.443904
2306.631772	271398.152870	38.448922
2309.361204	271840.094904	38.453940
2312.084503	272299.566389	38.458957
2314.408709	272752.343957	38.463975
2316.888544	273202.454991	38.468992
2319.310024	273650.212827	38.474010
2321.857830	274093.352665	38.479028
2323.986325	274548.473203	38.484045
2326.104911	275002.375950	38.489063
2328.672892	275464.666771	38.494080
2331.106399	275911.482783	38.499098
2334.333322	276341.127268	38.504116
2337.137149	276775.309746	38.509133
2339.985006	277193.633426	38.514151
2343.261467	277620.627817	38.519168
2345.842585	278033.481007	38.524186
2348.511063	278424.346290	38.529204
2350.782657	278836.333730	38.534221
2353.230405	279230.282096	38.539239
2356.104979	279617.456146	38.544256
2358.221660	280009.932429	38.549274
2360.845435	280396.231331	38.554292
2363.236378	280788.181058	38.559309
2365.575023	281176.709399	38.564327
2367.528475	281567.305413	38.569344
2369.558152	281949.633029	38.574362
2372.079691	282298.782007	38.579380
2374.094897	282677.453339	38.584397
2376.068587	283028.822535	38.589415
2378.090507	283402.437011	38.594432
2380.234509	283774.787081	38.599450
2382.279548	284156.729505	38.604468
2384.058374	284559.087075	38.609485
2385.908294	284947.791526	38.614503
2387.912209	285358.343215	38.619520
2390.079839	285773.517264	38.624538
2392.435099	286204.106122	38.629556
2394.218944	286637.960392	38.634573
2396.517858	287075.060252	38.639591
2399.131085	287518.079389	38.644608
2401.749235	287945.575979	38.649626
2404.602991	288377.911970	38.654644
2407.434680	288812.435468	38.659661
2410.130537	289234.684909	38.664679
2412.968507	289659.883304	38.669696
2415.286649	290085.315837	38.674714
2418.141517	290501.390659	38.679732
2420.519350	290941.241022	38.684749
2423.243531	291364.270044	38.689767
2425.924026	291790.251943	38.694784
2428.430940	292209.071697	38.699802
2430.952222	292634.416834	38.704820
2433.210730	293063.562366	38.709837
2435.364772	293483.629596	38.714855
2438.043253	293911.182766	38.719872
2440.266630	294352.371970	38.724890
2442.885279	294780.440888	38.729908
2444.957058	295224.446471	38.734925
2447.117550	295663.280386	38.739943
2449.381653	296118.277943	38.744960
2451.652101	296568.116814	38.749978
2453.983324	297018.757824	38.754996
2456.414667	297484.597518	38.760013
2458.911515	297952.864180	38.765031
2461.489932	298411.768854	38.770048
2463.073551	298892.192673	38.775066
2465.678885	299365.645601	38.780084
2467.864667	299845.768027	38.785101
2470.142579	300330.624480	38.790119
2473.074952	300818.119075	38.795136
2475.552575	301303.499704	38.800154
2478.328431	301779.941143	38.805172
2480.882194	302259.896205	38.810189
2483.557164	302733.810474	38.815207
2486.553829	303209.069266	38.820224
2488.810280	303695.620112	38.825242
2491.478188	304169.835537	38.830260
2493.939693	304637.554085	38.835277
2496.417792	305124.750586	38.840295
2498.956243	305602.766197	38.845312
2501.362809	306073.028470	38.850330
2503.968574	306521.362470	38.855348
2505.906802	306974.855301	38.860365
2508.426205	307419.923192	38.865383
2511.229776	307854.886076	38.870400
2513.493766	308322.571753	38.875418
2515.781737	308765.283845	38.880436
2518.499350	309223.445424	38.885453
2521.158502	309663.606182	38.890471
2524.076884	310117.058929	38.895488
2526.473105	310569.246455	38.900506
2529.174659	311016.329343	38.905524
2531.740824	311468.460936	38.910541
2533.846308	311937.808047	38.915559
2536.227564	312399.159573	38.920576
2538.674801	312864.156108	38.925594
2541.249287	313329.714625	38.930612
2544.056181	313795.920024	38.935629
2546.437270	314277.912478	38.940647
2548.860854	314745.799832	38.945664
2551.763636	315233.927727	38.950682
2554.259293	315713.279198	38.955700
2556.443107	316207.027642	38.960717
2558.503369	316707.904584	38.965735
2561.344450	317188.819578	38.970752
2563.336326	317694.273823	38.975770
2565.953711	318204.223214	38.980788
2568.393895	318740.458758	38.985805
2570.680833	319230.263985	38.990823
2573.043193	319775.344048	38.995840
2575.552817	320303.889502	39.000858
2577.914640	320839.261571	39.005876
2580.572656	321379.789770	39.010893
2583.057077	321916.634239	39.015911
2585.593428	322469.669964	39.020928
2587.927000	323023.673881	39.025946
2590.430851	323582.167655	39.030964
2593.720533	324136.012746	39.035981
2596.153180	324690.827937	39.040999
2598.795129	325245.022096	39.046016
2601.559606	325806.405281	39.051034
2604.077060	326366.706259	39.056052
2606.647171	326920.138292	39.061069
2610.038452	327480.826171	39.066087
2612.924826	328027.445210	39.071104
2615.915928	328576.862516	39.076122
2618.852930	329116.685406	39.081140
2622.024667	329645.065322	39.086157
2624.799047	330179.700500	39.091175
2627.367732	330710.225208	39.096192
2629.868803	331246.571847	39.101210
2632.897759	331766.274484	39.106228
2635.759527	332299.508920	39.111245
2638.337259	332807.264502	39.116263
2641.461572	333315.945532	39.121280
2644.125312	333827.971423	39.126298
2646.600129	334301.630263	39.131316
2649.410196	334780.539673	39.136333
2652.170965	335240.028659	39.141351
2655.208702	335707.062778	39.146368
2657.642708	336168.780843	39.151386
2660.343196	336636.344293	39.156404
2662.842104	337102.895304	39.161421
2664.929893	337590.049463	39.166439
2667.834632	338037.333844	39.171456
2669.898640	338530.502306	39.176474
2672.575039	339013.616887	39.181492
2675.537472	339491.858320	39.186509
2677.830568	339991.174350	39.191527
2680.595034	340462.990633	39.196544
2683.010142	340977.361012	39.201562
2685.748150	341469.967934	39.206580
2687.759166	341982.337318	39.211597
2690.722664	342492.190327	39.216615
2693.793461	342994.760804	39.221632
2696.151125	343528.718773	39.226650
2698.798201	344039.548036	39.231668
2701.420944	344561.572892	39.236685
2703.655462	345093.225810	39.241703
2706.232630	345622.890108	39.246720
2708.468362	346174.208326	39.251738
2711.169411	346730.601118	39.256756
2713.920649	347283.934049	39.261773
2716.102995	347851.644331	39.266791
2719.461350	348406.494742	39.271808
2722.396035	348963.691431	39.276826
2725.253831	349525.007152	39.281844
2728.210368	350076.959517	39.286861
2731.172546	350638.069480	39.291879
2734.092351	351202.531118	39.296896
2736.522284	351768.993594	39.301914
2739.144307	352338.618034	39.306932
2742.002107	352900.532882	39.311949
2744.360244	353488.666351	39.316967
2747.311507	354053.092311	39.321984
2750.078419	354639.878706	39.327002
2752.356401	355213.942642	39.332020
2755.230891	355804.480624	39.337037
2758.086232	356387.679122	39.342055
2760.863698	356980.858361	39.347072
2762.946646	357574.800395	39.352090
2765.866768	358171.394664	39.357108
2768.733721	358770.705856	39.362125
2771.357708	359389.363065	39.367143
2773.997664	359993.974253	39.372160
2776.542822	360612.805802	39.377178
2778.972449	361226.343131	39.382196
2782.197281	361843.426600	39.387213
2785.363686	362456.120533	39.392231
2788.257110	363069.484068	39.397248
2790.885362	363676.689016	39.402266
2793.680034	364258.176635	39.407284
2796.546103	364840.990544	39.412301
2799.185081	365408.961533	39.417319
2802.001067	365972.913050	39.422336
2804.519870	366570.985908	39.427354
2807.216241	367152.248553	39.432372
2810.214800	367729.116309	39.437389
2812.728418	368332.799605	39.442407
2815.723401	368907.749123	39.447424
2817.971126	369517.675054	39.452442
2820.998165	370127.265929	39.457460
2823.794458	370730.642459	39.462477
2826.270496	371356.491951	39.467495
2829.430079	371967.456313	39.472512
2832.208591	372573.549617	39.477530
2834.689484	373213.072255	39.482548
2837.726222	373830.625682	39.487565
2840.381584	374460.079085	39.492583
2843.605872	375091.817665	39.497600
2846.195184	375724.687153	39.502618
2849.245125	376376.146944	39.507636
2852.363600	377013.834330	39.512653
2855.058866	377662.589211	39.517671
2857.719397	378304.311466	39.522688
2860.954495	378956.866527	39.527706
2863.413747	379606.844370	39.532724
2865.992648	380271.886716	39.537741
2868.984848	380933.605023	39.542759
2872.152465	381595.766107	39.547776
2874.616901	382265.307399	39.552794
2877.301036	382939.266621	39.557812
2880.371653	383615.359448	39.562829
2882.949636	384296.844860	39.567847
2886.251103	384986.421637	39.572864
2889.090000	385673.572968	39.577882
2892.215306	386345.295173	39.582900
2895.402893	387037.920466	39.587917
2898.620200	387720.255554	39.592935
2902.055729	388371.600183	39.597952
2905.383942	389048.515462	39.602970
2908.216349	389721.032592	39.607988
2911.550013	390388.689588	39.613005
2914.163088	391050.158382	39.618023
2917.580565	391713.795147	39.623040
2920.704505	392371.100278	39.628058
2923.396918	393036.652392	39.633076
2926.150350	393692.291847	39.638093
2928.665040	394368.015268	39.643111
2931.696433	395032.561910	39.648128
2934.693907	395705.189959	39.653146
2937.298747	396384.966699	39.658164
2940.400801	397056.714254	39.663181
2943.052419	397730.015526	39.668199
2946.462113	398409.217734	39.673216
2949.375097	399068.175032	39.678234
2951.973009	399699.152006	39.683252
2955.182338	400336.104960	39.688269
2958.108600	400967.715185	39.693287
2961.082970	401590.127542	39.698304
2963.773551	402229.660416	39.703322
2966.554845	402857.123810	39.708340
2969.744070	403499.315589	39.713357
2972.256604	404138.204328	39.718375
2974.823287	404778.237616	39.723392
2978.078715	405433.156038	39.728410
2980.655130	406097.674190	39.733428
2983.916830	406750.256963	39.738445
2987.137072	407421.083339	39.743463
2990.211913	408068.040280	39.748480
2993.359015	408729.673511	39.753498
2996.095203	409406.387972	39.758516
2999.799701	410061.845928	39.763533
3002.712909	410722.458567	39.768551
3006.105348	411369.294372	39.773568
3008.971935	412047.880014	39.778586
3012.257919	412707.654500	39.783604
3015.659038	413370.082365	39.788621
3018.550039	414034.071182	39.793639
3021.924152	414679.113762	39.798656
3025.129576	415351.892501	39.803674
3028.049812	415997.129549	39.808692
3031.022732	416654.608584	39.813709
3033.906668	417320.423419	39.818727
3036.766928	417993.245416	39.823744
3039.647956	418666.200169	39.828762
3042.193147	419354.268179	39.833780
3045.188120	420046.276800	39.838797
3047.588191	420749.687971	39.843815
3050.716108	421462.213878	39.848832
3053.218025	422162.051342	39.853850
3055.984685	422889.849516	39.858868
3059.740680	423593.530948	39.863885
3062.594586	424319.782475	39.868903
3065.477921	425059.512307	39.873920
3068.700058	425786.882133	39.878938
3071.377417	426527.693467	39.883956
3074.713065	427263.516583	39.888973
3077.529833	428008.798878	39.893991
3080.623646	428755.941365	39.899008
3084.034600	429489.588277	39.904026
3086.875642	430240.654433	39.909044
3090.230987	431000.861993	39.914061
3092.943991	431761.528787	39.919079
3096.145543	432510.522021	39.924096
3099.140381	433266.591773	39.929114
3101.823614	434026.689678	39.934132
3104.963138	434799.455686	39.939149
3108.067150	435573.849687	39.944167
3111.351277	436356.547594	39.949184
3114.182020	437117.947110	39.954202
3117.006082	437871.930905	39.959220
3120.001457	438609.736137	39.964237
3122.978968	439341.952025	39.969255
3126.187577	440095.376720	39.974272
3129.157397	440848.309660	39.979290
3132.011562	441601.997130	39.984308
3134.727312	442363.176525	39.989325
3137.355716	443131.990839	39.994343
3140.467047	443901.666104	39.999360
3143.756474	444687.185146	40.004378
3146.454548	445487.554254	40.009396
3150.055812	446273.022152	40.014413
3152.970135	447074.417045	40.019431
3156.154825	447872.907117	40.024448
3159.230079	448684.142921	40.029466
3162.736591	449483.893587	40.034484
3166.126398	450292.290136	40.039501
3169.673425	451104.733068	40.044519
3172.780483	451913.724666	40.049536
3176.259004	452721.819092	40.054554
3179.506978	453542.674246	40.059572
3183.095697	454352.464354	40.064589
3186.721959	455150.934804	40.069607
3190.255888	455962.092435	40.074624
3193.758944	456762.801878	40.079642
3197.221843	457564.601957	40.084660
3200.566622	458351.921118	40.089677
3203.803661	459151.270627	40.094695
3207.044113	459946.846590	40.099712
3210.925330	460745.479411	40.104730
3213.781248	461533.014306	40.109748
3217.209185	462323.718212	40.114765
3220.388939	463117.214523	40.119783
3223.569734	463919.988628	40.124800
3226.965099	464715.060829	40.129818
3230.515981	465505.830024	40.134836
3233.908816	466293.054243	40.139853
3237.061496	467095.459751	40.144871
3240.288493	467890.742512	40.149888
3243.675256	468678.131115	40.154906
3246.486906	469482.875795	40.159924
3249.456808	470283.265937	40.164941
3252.699549	471082.975107	40.169959
3255.612007	471893.677784	40.174976
3258.780473	472704.611242	40.179994
3261.881713	473517.848831	40.185012
3265.389997	474327.753763	40.190029
3268.457881	475165.299389	40.195047
3271.233359	475994.868922	40.200064
3274.935950	476815.562631	40.205082
3278.324194	477641.984405	40.210100
3281.632305	478469.445989	40.215117
3284.601966	479296.825415	40.220135
3287.789337	480129.543816	40.225152
3290.844651	480952.341731	40.230170
3294.229484	481766.966681	40.235188
3297.405417	482565.671469	40.240205
3299.980662	483364.589958	40.245223
3302.633379	484181.907601	40.250240
3305.852540	484992.784651	40.255258
3308.891912	485829.425290	40.260276
3311.553286	486646.889103	40.265293
3315.156293	487488.167762	40.270311
3318.391426	488331.235471	40.275328
3322.089095	489169.847690	40.280346
3325.516884	490026.499756	40.285364
3329.513087	490867.615701	40.290381
3333.146741	491712.842510	40.295399
3336.037225	492561.532513	40.300416
3339.524673	493413.321674	40.305434
3342.854161	494271.965154	40.310452
3345.952929	495137.523839	40.315469
3349.057378	496011.019726	40.320487
3352.459428	496879.780770	40.325504
3355.424212	497765.333915	40.330522
3358.592174	498666.110959	40.335540
3362.072096	499542.961860	40.340557
3365.825646	500446.737793	40.345575
3368.827849	501349.375023	40.350592
3372.536237	502246.453007	40.355610
3375.454016	503160.773856	40.360628
3378.613183	504077.936783	40.365645
3382.119860	505007.363236	40.370663
3385.160294	505946.201814	40.375680
3388.734010	506875.719888	40.380698
3391.925253	507815.897085	40.385716
3395.217157	508749.900923	40.390733
3398.212841	509723.614022	40.395751
3400.974543	510691.657305	40.400768
3404.266248	511663.951424	40.405786
3407.410393	512651.853488	40.410804
3410.914404	513644.786741	40.415821
3413.867140	514648.544107	40.420839
3417.272981	515658.828236	40.425856
3420.898867	516677.288606	40.430874
3424.385820	517694.497921	40.435892
3427.826987	518697.227585	40.440909
3431.667874	519733.470664	40.445927
3435.066974	520726.047205	40.450944
3439.192664	521780.320066	40.455962
3442.272246	522777.208981	40.460980
3445.620324	523817.253256	40.465997
3449.518656	524819.180553	40.471015
3452.805745	525836.971320	40.476032
3456.858224	526879.931975	40.481050
3460.058288	527887.422895	40.486068
3463.835287	528908.064796	40.491085
3467.119873	529906.593159	40.496103
3470.829868	530952.967834	40.501120
3474.257976	531930.628943	40.506125
3477.390119	532921.186676	40.511130
3481.199231	533796.297927	40.516135
3484.257922	534653.243114	40.521140
3487.672139	535427.197284	40.526144
3490.408209	536138.337363	40.531149
3493.601509	536776.492401	40.536154
3495.804898	537373.616632	40.541159
3498.361380	537874.303765	40.546164
3500.430847	538373.485864	40.551168
3502.448698	538764.945207	40.556173
3504.687635	539090.156557	40.561178
3506.052779	539427.618304	40.566183
3507.739462	539676.199148	40.571188
3509.188316	539883.710201	40.576192
3510.494985	540034.181627	40.581197
3511.761470	540197.079542	40.586202
3512.619550	540255.719466	40.591207
3514.110785	540316.076882	40.596212
3514.774455	540335.008348	40.601216
3515.850915	540308.682420	40.606221
3516.547738	540305.593250	40.611226
3517.354553	540214.121766	40.616231
3517.873610	540133.097111	40.621236
3518.330549	540026.733361	40.626240
3518.979724	539871.509374	40.631245
3519.260523	539774.412366	40.636250
3519.424056	539587.550779	40.641255
3520.081684	539390.054898	40.646260
3519.833650	539244.055753	40.651264
3520.690703	539050.816230	40.656269
3520.668396	538823.272918	40.661274
3520.582049	538589.777336	40.666279
3521.084754	538383.657363	40.671284
3520.801163	538145.136067	40.676288
3521.605495	537884.117156	40.681293
3520.925840	537642.367931	40.686298
3520.991950	537387.012496	40.691303
3520.825658	537135.224840	40.696308
3520.734316	536877.613056	40.701312
3520.651575	536632.319112	40.706317
3520.746776	536359.820264	40.711322
3520.707644	536093.449277	40.716327
3520.514319	535834.775389	40.721332
3520.215574	535547.929318	40.726336
3520.486129	535306.649626	40.731341
3520.388958	535030.621833	40.736346
3520.054448	534766.598053	40.741351
3520.173834	534459.359593	40.746356
3519.659058	534233.038146	40.751360
3519.798839	533932.605393	40.756365
3519.312711	533696.471613	40.761370
3519.295323	533405.398906	40.766375
3519.345421	533136.285309	40.771380
3518.537513	532920.650235	40.776384
3519.027413	532649.943143	40.781389
3518.332607	532377.650365	40.786394
3518.657631	532097.562952	40.791399
3518.420870	531876.518407	40.796404
3518.031839	531590.876290	40.801408
3517.937646	531357.878483	40.806413
3517.526130	531095.219042	40.811418
3517.532830	530826.274487	40.816423
3517.295772	530629.767599	40.821428
3516.874419	530358.255312	40.826432
3516.760355	530136.358345	40.831437
3516.881233	529881.678811	40.836442
3516.241422	529679.766620	40.841447
3516.807562	529416.469788	40.846452
3516.132388	529199.701259	40.851456
3516.084118	528974.442491	40.856461
3515.511007	528735.165040	40.861466
3515.513215	528534.501065	40.866471
3515.459409	528290.384737	40.871476
3514.961668	528110.866809	40.876480
3515.112499	527851.045824	40.881485
3514.455323	527703.031617	40.886490
3514.454299	527460.056458	40.891495
3514.031155	527287.289238	40.896500
3513.716722	527064.824869	40.901504
3513.776594	526868.679046	40.906509
3513.376303	526728.145297	40.911514
3513.416384	526506.223547	40.916519
3513.326468	526339.003196	40.921524
3512.730536	526138.454003	40.926528
3512.900574	525980.387129	40.931533
3512.765434	525785.370693	40.936538
3512.350780	525634.923469	40.941543
3512.131788	525468.421987	40.946548
3512.259928	525293.675959	40.951552
3511.912530	525135.429798	40.956557
3512.042400	524959.011915	40.961562
3511.878192	524814.380496	40.966567
3511.442252	524652.150549	40.971572
3511.138760	524492.020937	40.976576
3511.308642	524330.702903	40.981581
3511.124983	524217.761459	40.986586
3510.958688	524058.869506	40.991591
3511.119233	523899.974875	40.996596
3510.797449	523764.710163	41.001600
3510.937711	523610.567369	41.006605
3510.671971	523493.994351	41.011610
3510.384556	523345.628606	41.016615
3510.774040	523192.807258	41.021620
3510.078594	523060.375917	41.026624
3510.213718	522938.731091	41.031629
3510.054373	522809.549286	41.036634
3509.976506	522662.104610	41.041639
3509.557333	522564.151952	41.046644
3509.674682	522415.258733	41.051648
3509.474562	522290.831115	41.056653
3509.216475	522176.926664	41.061658
3509.175142	522069.811815	41.066663
3508.968195	521938.305148	41.071668
3508.679711	521851.449277	41.076672
3509.210612	521713.100528	41.081677
3508.809095	521609.628913	41.086682
3508.321365	521503.086424	41.091687
3508.657079	521418.101220	41.096692
3508.494572	521310.191635	41.101696
3508.164076	521200.184544	41.106701
3507.914083	521121.862607	41.111706
3508.018109	521016.285080	41.116711
3507.999352	520914.568577	41.121716
3507.578511	520805.533676	41.126720
3507.724981	520747.167816	41.131725
3507.788607	520633.100594	41.136730
3507.780486	520575.466358	41.141735
3507.533379	520456.340689	41.146740
3507.726170	520390.837552	41.151744
3507.547397	520280.648605	41.156749
3507.492024	520180.551192	41.161754
3507.395041	520150.787421	41.166759
3507.573583	520043.826739	41.171764
3507.214429	519937.961533	41.176768
3507.436539	519866.687866	41.181773
3507.428150	519812.944093	41.186778
3506.913142	519701.489828	41.191783
3507.384584	519609.496438	41.196788
3506.850459	519549.818177	41.201792
3507.203229	519434.230638	41.206797
3506.594441	519408.793547	41.211802
3506.560713	519308.535702	41.216807
3506.835771	519236.239697	41.221812
3506.213665	519184.411086	41.226816
3506.575349	519081.611825	41.231821
3506.590600	519026.901059	41.236826
3506.157558	518964.878821	41.241831
3506.486792	518870.375637	41.246836
3506.033371	518851.587429	41.251840
3506.155287	518754.385945	41.256845
3506.340609	518723.007503	41.261850
3506.103288	518640.070422	41.266855
3506.200349	518580.845079	41.271860
3505.766406	518518.922429	41.276864
3506.187923	518465.814199	41.281869
3505.973325	518414.980602	41.286874
3506.063392	518350.193460	41.291879
3505.849606	518288.943052	41.296884
3505.676806	518252.715540	41.301888
3505.880533	518171.273900	41.306893
3505.675752	518128.376580	41.311898
3505.241750	518058.311210	41.316903
3505.666758	518012.583518	41.321908
3505.896140	517962.285140	41.326912
3505.575015	517909.697022	41.331917
3505.550466	517863.332048	41.336922
3505.666962	517815.528800	41.341927
3505.609312	517748.032069	41.346932
3505.445257	517712.813317	41.351936
3505.483164	517664.010722	41.356941
3505.381205	517605.672968	41.361946
3505.092683	517543.925940	41.366951
3505.325863	517519.869860	41.371956
3505.070861	517460.241037	41.376960
3504.975635	517431.938518	41.381965
3505.136714	517362.838058	41.386970
3505.096375	517348.635058	41.391975
3505.065512	517270.968060	41.396980
3504.993370	517262.180767	41.401984
3505.223620	517195.040821	41.406989
3505.138587	517148.127154	41.411994
3504.625965	517127.171901	41.416999
3504.932045	517088.337735	41.422004
3504.889693	517044.552268	41.427008
3505.137581	517001.378204	41.432013
3504.738025	516974.488355	41.437018
3504.783734	516929.070466	41.442023
3504.604511	516885.154503	41.447028
3504.423545	516854.336098	41.452032
3504.796708	516815.237846	41.457037
3504.509435	516790.251581	41.462042
3504.633954	516753.417531	41.467047
3504.894468	516712.971469	41.472052
3504.462368	516681.535031	41.477056
3505.132292	516640.771238	41.482061
3504.703626	516618.386118	41.487066
3504.470034	516563.706525	41.492071
3504.709680	516529.533990	41.497076
3504.670441	516496.871999	41.502080
3504.554315	516464.120954	41.507085
3504.581587	516422.244511	41.512090
3504.458098	516387.977368	41.517095
3504.507924	516374.972975	41.522100
3504.807997	516314.190319	41.527104
3504.313829	516302.030409	41.532109
3504.433881	516271.011632	41.537114
3504.681467	516227.026472	41.542119
3504.607644	516201.145877	41.547124
3504.123959	516146.807866	41.552128
3504.488841	516134.512059	41.557133
3504.309854	516101.011666	41.562138
3504.336947	516084.116642	41.567143
3504.197110	516041.355366	41.572148
3503.736366	516021.958232	41.577152
3504.200601	515970.959269	41.582157
3504.222577	515977.024514	41.587162
3504.476528	515921.810609	41.592167
3504.277967	515904.344204	41.597172
3504.101657	515881.361912	41.602176
3504.121446	515841.002351	41.607181
3503.754508	515818.555823	41.612186
3503.787741	515785.071824	41.617191
3503.973275	515766.988273	41.622196
3504.060014	515764.901203	41.627200
3503.809184	515724.938139	41.632205
3503.505830	515705.313470	41.637210
3503.687882	515669.378233	41.642215
3503.887744	515672.987985	41.647220
3503.806466	515644.781360	41.652224
3504.124006	515651.305738	41.657229
3504.172538	515596.224366	41.662234
3503.848647	515591.875821	41.667239
3504.055516	515571.563478	41.672244
3503.691065	515533.944271	41.677248
3503.645672	515523.280625	41.682253
3503.818256	515498.523176	41.687258
3503.613825	515480.450376	41.692263
3504.032010	515472.292665	41.697268
3503.901071	515444.245270	41.702272
3504.121608	515434.905018	41.707277
3504.130931	515409.768654	41.712282
3504.004912	515371.099925	41.717287
3503.922868	515345.320447	41.722292
3503.749658	515347.421451	41.727296
3503.961830	515293.729280	41.732301
3503.720774	515289.013546	41.737306
3503.799855	515262.095850	41.742311
3504.148621	515236.197540	41.747316
3503.909434	515211.858765	41.752320
3503.768884	515194.888188	41.757325
3503.825833	515178.695567	41.762330
3503.864560	515160.331118	41.767335
3503.916676	515134.985279	41.772340
3503.607428	515122.390682	41.777344
3503.920270	515098.015066	41.782349
3503.687800	515062.548636	41.787354
3503.902524	515053.461963	41.792359
3504.174708	515030.812211	41.797364
3503.752124	515020.764180	41.802368
3503.755190	514988.952316	41.807373
3503.627564	514971.726597	41.812378
3503.620573	514944.063370	41.817383
3504.005616	514924.025529	41.822388
3503.656384	514915.938265	41.827392
3504.128665	514881.573863	41.832397
3503.775484	514867.114739	41.837402
3503.905886	514847.976831	41.842407
3503.829763	514820.830079	41.847412
3503.832503	514806.618099	41.852416
3504.218219	514777.324695	41.857421
3503.864718	514761.449419	41.862426
3503.691791	514750.451409	41.867431
3503.946787	514722.796984	41.872436
3503.824903	514702.889576	41.877440
3503.663790	514665.438576	41.882445
3503.342122	514664.376857	41.887450
3503.799355	514647.108941	41.892455
3503.835378	514616.049796	41.897460
3503.589376	514609.008161	41.902464
3503.473905	514586.671957	41.907469
3503.557561	514575.633279	41.912474
3503.536000	514559.907651	41.917479
3503.785856	514529.269733	41.922484
3503.221450	514522.480689	41.927488
3503.761859	514499.888979	41.932493
3503.603829	514488.180374	41.937498
3503.734450	514470.609865	41.942503
3503.734118	514436.976742	41.947508
3503.646662	514444.425403	41.952512
3503.609000	514405.892207	41.957517
3503.484939	514401.006000	41.962522
3503.495553	514371.063101	41.967527
3503.578141	514350.870074	41.972532
3503.218933	514354.416744	41.977536
3503.607295	514345.504552	41.982541
3503.571844	514331.500513	41.987546
3503.627918	514323.601785	41.992551
3503.971827	514288.902422	41.997556
3503.769123	514278.667461	42.002560
3503.586937	514256.037900	42.007565
3503.582625	514246.176178	42.012570
3503.511536	514235.161733	42.017575
3503.510859	514194.447394	42.022580
3503.580136	514188.721333	42.027584
3503.524475	514179.676923	42.032589
3503.561294	514166.419982	42.037594
3503.490097	514149.235074	42.042599
3503.642924	514124.630449	42.047604
3503.670408	514116.331524	42.052608
3503.712833	514081.274763	42.057613
3503.754343	514078.334815	42.062618
3503.644859	514059.284500	42.067623
3503.563167	514044.377133	42.072628
3503.548705	514031.836277	42.077632
3503.244501	514005.584073	42.082637
3503.254062	513999.412186	42.087642
3503.231417	513996.735253	42.092647
3503.329224	513967.738830	42.097652
3503.448917	513947.084252	42.102656
3503.470515	513935.346871	42.107661
3503.251954	513937.101171	42.112666
3503.462604	513917.393162	42.117671
3503.811626	513907.576552	42.122676
3503.147932	513892.508148	42.127680
3503.346455	513874.066455	42.132685
3503.397405	513880.583085	42.137690
3503.461261	513845.370711	42.142695
3503.310712	513829.614207	42.147700
3503.434984	513846.690112	42.152704
3503.630872	513798.660484	42.157709
3503.044150	513802.243228	42.162714
3503.578666	513783.191971	42.167719
3503.542788	513762.865225	42.172724
3503.563963	513753.353235	42.177728
3503.423455	513740.123985	42.182733
3503.456053	513723.124550	42.187738
3503.546931	513702.727120	42.192743
3503.815321	513694.693382	42.197748
3503.388853	513691.169809	42.202752
3503.582719	513680.416596	42.207757
3503.420706	513661.121237	42.212762
3503.002399	513643.333150	42.217767
3503.669719	513630.886553	42.222772
3503.202719	513611.791078	42.227776
3503.155948	513601.632215	42.232781
3503.220605	513600.054156	42.237786
3503.557567	513574.610361	42.242791
3503.353274	513551.578712	42.247796
3503.198402	513559.797106	42.252800
3503.344345	513540.554094	42.257805
3503.228732	513522.869775	42.262810
3503.103342	513517.781204	42.267815
3503.403036	513512.372549	42.272820
3503.259898	513502.178279	42.277824
3503.598060	513473.648808	42.282829
3503.554488	513477.651568	42.287834
3503.488025	513460.262890	42.292839
3503.587210	513440.268464	42.297844
3503.355562	513433.021746	42.302848
3503.622001	513405.767982	42.307853
3503.088683	513418.092621	42.312858
3503.166420	513397.646318	42.317863
3503.247696	513365.819016	42.322868
3503.277404	513363.336026	42.327872
3503.306317	513365.860545	42.332877
3503.261891	513357.218554	42.337882
3503.042651	513316.283733	42.342887
3503.059730	513302.523433	42.347892
3502.936214	513309.169019	42.352896
3503.358587	513308.596571	42.357901
3502.909603	513304.975315	42.362906
3502.610580	513290.202789	42.367911
3503.420810	513251.937575	42.372916
3503.133790	513291.840024	42.377920
3503.507999	513260.016804	42.382925
3502.876374	513254.654105	42.387930
3503.075060	513245.467831	42.392935
3503.459851	513232.458637	42.397940
3503.036043	513234.093709	42.402944
3503.315819	513216.093675	42.407949
3503.452567	513212.683303	42.412954
3503.072611	513206.168048	42.417959
3503.645286	513188.222852	42.422964
3503.319855	513173.859039	42.427968
3503.522942	513164.975508	42.432973
3503.373843	513145.121133	42.437978
3503.330315	513120.546076	42.442983
3503.363380	513131.668636	42.447988
3503.149348	513111.672744	42.452992
3503.466374	513077.784422	42.457997
3503.220998	513080.251175	42.463002
3503.268989	513082.064595	42.468007
3503.588286	513062.793639	42.473012
3503.182219	513058.457418	42.478016
3503.167360	513055.070976	42.483021
3503.193375	513048.997302	42.488026
3502.986775	513031.680911	42.493031
3503.315440	513007.400927	42.498036
3503.138546	513010.969642	42.503040
3503.318576	512986.966025	42.508045
3503.055403	512979.015962	42.513050
3502.770464	512963.178726	42.518055
3503.510617	512955.373560	42.523060
3503.078379	512963.130274	42.528064
3503.186680	512948.647136	42.533069
3502.932083	512941.960223	42.538074
3503.127818	512934.392836	42.543079
3503.417140	512929.491445	42.548084
3503.203635	512915.666112	42.553088
3503.371108	512890.096330	42.558093
3503.317576	512895.567653	42.563098
3503.220283	512896.695920	42.568103
3503.498745	512859.778393	42.573108
3503.408131	512852.053903	42.578112
3503.215635	512841.563546	42.583117
3503.177723	512819.566804	42.588122
3503.225480	512815.715185	42.593127
3503.329528	512798.804688	42.598132
3502.890920	512809.243290	42.603136
3503.207559	512792.096861	42.608141
3503.231560	512775.451899	42.613146
3503.292481	512770.030166	42.618151
3503.711016	512758.482135	42.623156
3503.445544	512733.739267	42.628160
3503.451885	512739.100014	42.633165
3503.302722	512720.610851	42.638170
3503.506494	512699.283895	42.643175
3503.301699	512692.538430	42.648180
3503.142462	512665.553078	42.653184
3503.167266	512654.977678	42.658189
3503.521266	512641.416497	42.663194
3503.379703	512638.656978	42.668199
3503.484110	512614.867112	42.673204
3503.434973	512610.828434	42.678208
3502.972591	512619.905198	42.683213
3503.471134	512568.232917	42.688218
3503.278710	512585.511901	42.693223
3503.506725	512566.103061	42.698228
3502.922296	512550.059861	42.703232
3503.558113	512519.761945	42.708237
3503.665683	512526.978300	42.713242
3503.030844	512524.903712	42.718247
3503.130122	512499.698194	42.723252
3503.183710	512484.161078	42.728256
3502.899730	512490.630017	42.733261
3503.183190	512493.974334	42.738266
3503.293685	512462.545370	42.743271
3503.669243	512438.813565	42.748276
3503.176424	512448.704549	42.753280
3503.042985	512447.258857	42.758285
3503.148843	512420.635874	42.763290
3503.176753	512405.355657	42.768295
3503.392721	512415.286383	42.773300
3503.094663	512396.516903	42.778304
3503.365227	512382.968702	42.783309
3503.212882	512379.755602	42.788314
3503.420490	512362.120145	42.793319
3503.304819	512331.536005	42.798324
3503.078670	512337.186539	42.803329
3503.291219	512336.141398	42.808333
3503.148309	512326.553372	42.813338
3503.200412	512295.841485	42.818343
3503.354410	512288.786236	42.823348
3503.431604	512292.921937	42.828353
3503.398667	512269.406206	42.833357
3503.250946	512264.573700	42.838362
3503.352652	512253.429482	42.843367
3503.486765	512220.428263	42.848372
3503.087879	512223.273484	42.853377
3503.383511	512210.075264	42.858381
3503.465421	512194.078158	42.863386
3503.404092	512174.613435	42.868391
3503.424329	512176.026674	42.873396
3503.136410	512170.406967	42.878401
3503.278606	512114.388883	42.883405
3502.982739	512131.583513	42.888410
3503.349815	512132.739603	42.893415
3503.306567	512098.552178	42.898420
3503.268467	512097.748972	42.903425
3503.120143	512098.581858	42.908429
3503.012868	512108.816771	42.913434
3503.191217	512097.812087	42.918439
3503.263792	512069.979811	42.923444
3503.034085	512079.121255	42.928449
3503.261147	512054.501879	42.933453
3503.412327	512053.618172	42.938458
3503.143826	512026.497318	42.943463
3503.297331	512032.543200	42.948468
3503.310228	512018.782516	42.953473
3503.360326	512007.899212	42.958477
3503.035661	511994.596530	42.963482
3503.226321	511988.698787	42.968487
3503.423411	511955.636515	42.973492
3503.113336	511969.646770	42.978497
3503.413099	511948.607201	42.983501
3503.577649	511938.869193	42.988506
3503.259445	511916.409738	42.993511
3503.084693	511889.172679	42.998516
3503.029597	511888.776822	43.003521
3503.197795	511879.847548	43.008525
3503.511021	511862.801887	43.013530
3503.114791	511844.199062	43.018535
3503.026490	511863.384524	43.023540
3503.053003	511841.983338	43.028545
3503.278607	511797.079543	43.033549
3503.330064	511807.896561	43.038554
3502.812694	511820.776264	43.043559
3503.163847	511800.436568	43.048564
3503.298093	511803.349348	43.053569
3503.152306	511787.033756	43.058573
3503.149600	511783.291048	43.063578
3503.031329	511771.220178	43.068583
3503.443396	511759.014894	43.073588
3502.984116	511741.534779	43.078593
3502.916266	511717.062694	43.083597
3503.082628	511748.297745	43.088602
3502.848298	511721.676847	43.093607
3503.165177	511697.194511	43.098612
3502.938084	511715.997399	43.103617
3503.366998	511674.146804	43.108621
3503.272067	511713.516767	43.113626
3503.044067	511655.127616	43.118631
3502.891031	511678.623222	43.123636
3502.904809	511641.036687	43.128641
3503.168139	511672.661230	43.133645
3502.956124	511639.157154	43.138650
3502.839143	511665.682167	43.143655
3503.110267	511620.871881	43.148660
3502.883692	511626.219209	43.153665
3503.514689	511589.597289	43.158669
3503.004998	511634.243239	43.163674
3503.225334	511590.351426	43.168679
3503.353602	511595.035660	43.173684
3503.096575	511571.756719	43.178689
3503.301645	511583.308377	43.183693
3503.337792	511541.924214	43.188698
3503.251619	511520.186337	43.193703
3503.186413	511540.177876	43.198708
3503.203562	511515.540311	43.203713
3503.346714	511516.681252	43.208717
3503.180621	511477.908741	43.213722
3503.159907	511492.581849	43.218727
3503.464305	511486.058933	43.223732
3503.276916	511459.278448	43.228737
3503.470070	511448.018077	43.233741
3503.295104	511447.084716	43.238746
3503.000037	511418.398941	43.243751
3503.259468	511417.599263	43.248756
3503.240366	511406.068899	43.253761
3503.175471	511389.790725	43.258765
3503.058515	511384.599005	43.263770
3503.077023	511363.603165	43.268775
3503.158800	511361.111651	43.273780
3503.111359	511373.512733	43.278785
3503.146809	511355.043484	43.283789
3502.956580	511337.318085	43.288794
3503.043788	511331.031780	43.293799
3503.153558	511332.380352	43.298804
3503.064620	511331.939245	43.303809
3503.344912	511306.501001	43.308813
3503.300070	511299.122668	43.313818
3503.127276	511296.165522	43.318823
3503.325016	511274.787144	43.323828
3503.075609	511263.090740	43.328833
3502.939949	511251.072834	43.333837
3503.135051	511245.730578	43.338842
3502.841363	511252.656795	43.343847
3503.179177	511239.855844	43.348852
3502.959242	511225.321940	43.353857
3503.308043	511203.160806	43.358861
3503.153176	511221.194034	43.363866
3503.163204	511213.048200	43.368871
3503.574816	511180.304616	43.373876
3503.113396	511168.287552	43.378881
3503.039858	511162.886557	43.383885
3502.806984	511167.324472	43.388890
3502.953216	511158.094774	43.393895
3503.082083	511154.584063	43.398900
3502.982010	511146.303840	43.403905
3503.200991	511126.641852	43.408909
3503.165881	511135.247183	43.413914
3502.944298	511132.398892	43.418919
3503.310442	511082.058259	43.423924
3502.859903	511106.461647	43.428929
3503.333251	511072.999889	43.433933
3503.278971	511094.811339	43.438938
3503.253379	511057.634428	43.443943
3502.886660	511044.691751	43.448948
3502.980914	511053.074331	43.453953
3503.195399	511050.359451	43.458957
3503.215051	511020.662116	43.463962
3502.803642	511014.606263	43.468967
3502.934856	511015.142085	43.473972
3502.997374	510990.193068	43.478977
3502.607370	511015.699926	43.483981
3502.619360	511005.530216	43.488986
3502.664919	511002.791441	43.493991
3503.117194	511012.028015	43.498996
3502.631160	511000.874697	43.504001
3502.528310	510972.410721	43.509005
3502.754049	510973.235125	43.514010
3502.972583	510982.761593	43.519015
3503.271670	510983.017949	43.524020
3503.033598	510984.876807	43.529025
3502.791969	510978.187065	43.534029
3503.198126	510964.161023	43.539034
3503.030603	510949.416252	43.544039
3503.174132	510945.549073	43.549044
3502.773744	510962.710815	43.554049
3503.077367	510932.968446	43.559053
3503.128807	510931.139294	43.564058
3502.699548	510930.903725	43.569063
3503.353116	510904.748255	43.574068
3503.121063	510909.843737	43.579073
3503.106958	510901.195698	43.584077
3502.953881	510873.751236	43.589082
3502.900395	510875.985628	43.594087
3503.343488	510854.466770	43.599092
3502.912079	510860.656105	43.604097
3502.927709	510870.315880	43.609101
3503.034825	510864.279192	43.614106
3502.871218	510843.918540	43.619111
3503.318372	510838.738668	43.624116
3502.945456	510825.999153	43.629121
3502.814495	510818.583635	43.634125
3502.929773	510817.604365	43.639130
3502.785947	510816.058999	43.644135
3503.040159	510791.484092	43.649140
3502.996054	510790.277074	43.654145
3503.077060	510774.379949	43.659149
3503.156831	510785.699017	43.664154
3503.079899	510781.006660	43.669159
3503.144451	510757.726364	43.674164
3502.979941	510744.751499	43.679169
3503.185232	510753.116676	43.684173
3503.115429	510750.294919	43.689178
3503.306749	510725.021632	43.694183
3502.984029	510706.557702	43.699188
3502.583770	510712.438642	43.704193
3503.014836	510699.319022	43.709197
3503.081263	510702.343886	43.714202
3502.778471	510718.630460	43.719207
3503.312378	510699.221729	43.724212
3503.105108	510671.836094	43.729217
3503.190865	510656.342810	43.734221
3503.099689	510658.026722	43.739226
3502.929786	510658.610148	43.744231
3503.099915	510636.931808	43.749236
3502.921900	510625.729558	43.754241
3502.996599	510615.903820	43.759245
3503.040455	510609.725277	43.764250
3502.756084	510621.860826	43.769255
3503.105906	510620.642122	43.774260
3502.863086	510611.321856	43.779265
3502.843101	510595.744053	43.784269
3503.053229	510586.959239	43.789274
3503.040148	510579.929689	43.794279
3503.208934	510586.580728	43.799284
3503.031369	510587.367719	43.804289
3503.066796	510557.211793	43.809293
3502.858854	510540.348358	43.814298
3503.181077	510553.703371	43.819303
3503.350504	510545.127320	43.824308
3502.913175	510539.378921	43.829313
3503.116673	510519.415151	43.834317
3502.850017	510518.647994	43.839322
3502.762429	510520.280765	43.844327
3503.136550	510506.006471	43.849332
3502.702434	510533.089255	43.854337
3502.970187	510513.975321	43.859341
3502.881925	510511.561147	43.864346
3502.796647	510476.112397	43.869351
3503.109116	510482.386649	43.874356
3503.073723	510492.054702	43.879361
3503.045284	510484.218129	43.884365
3502.974932	510490.148179	43.889370
3503.318759	510451.444498	43.894375
3503.180486	510429.764050	43.899380
3502.749509	510458.111167	43.904385
3502.898462	510412.760540	43.909389
3503.028539	510446.381375	43.914394
3503.068155	510427.303402	43.919399
3503.210138	510392.830328	43.924404
3502.894093	510393.082741	43.929409
3503.271316	510384.878475	43.934413
3503.281196	510404.201830	43.939418
3503.120054	510369.017790	43.944423
3503.590244	510351.743456	43.949428
3503.232467	510357.567214	43.954433
3503.234398	510329.692667	43.959437
3503.465712	510307.498351	43.964442
3503.376855	510336.398662	43.969447
3503.401845	510294.810876	43.974452
3503.364077	510265.627190	43.979457
3503.383862	510286.416190	43.984461
3503.405465	510244.575873	43.989466
3503.073198	510256.415717	43.994471
3503.801440	510233.383930	43.999476
3503.112631	510205.061874	44.004481
3503.239118	510204.839633	44.009485
3503.114814	510182.903718	44.014490
3502.886968	510200.949558	44.019495
3503.309669	510186.566141	44.024500
3502.936043	510167.300246	44.029505
3503.252404	510150.252379	44.034509
3503.107183	510149.870725	44.039514
3502.874581	510150.413488	44.044519
3503.136083	510135.701382	44.049524
3503.052464	510133.539366	44.054529
3503.258588	510114.030012	44.059533
3503.026533	510104.555998	44.064538
3502.801275	510112.028343	44.069543
3503.008994	510083.766744	44.074548
3502.833361	510070.540176	44.079553
3502.983399	510061.562231	44.084557
3503.098425	510073.635043	44.089562
3502.644015	510059.238380	44.094567
3502.767397	510071.006336	44.099572
3502.969726	510060.097726	44.104577
3502.736942	510061.551132	44.109581
3503.155350	510007.101318	44.114586
3502.754986	510047.990505	44.119591
3502.740196	510013.136727	44.124596
3502.607314	510052.668296	44.129601
3502.748718	510016.221562	44.134605
3502.531861	510051.516877	44.139610
3502.842785	510022.429432	44.144615
3503.208505	510051.612504	44.149620
3502.683106	510016.788848	44.154625
3502.599756	510022.771703	44.159629
3502.829417	510003.713809	44.164634
3502.945272	509976.832473	44.169639
3503.097492	509992.744283	44.174644
3502.833922	509984.135208	44.179649
3502.828087	509979.431393	44.184653
3502.854781	510000.523188	44.189658
3503.003226	509995.542044	44.194663
3503.127570	509968.153456	44.199668
3503.449102	509958.794225	44.204673
3502.968608	509960.792688	44.209677
3503.028152	509958.405664	44.214682
3502.927518	509942.738832	44.219687
3503.335509	509924.664462	44.224692
3503.001230	509905.341461	44.229697
3503.218170	509918.865383	44.234701
3503.206231	509922.459261	44.239706
3503.124335	509907.548284	44.244711
3503.070162	509882.312551	44.249716
3503.157777	509913.108106	44.254721
3502.807532	509868.239653	44.259725
3503.104855	509904.111675	44.264730
3502.869557	509855.835495	44.269735
3502.736205	509848.875243	44.274740
3502.830952	509851.440471	44.279745
3503.028666	509821.864678	44.284749
3503.167353	509851.944008	44.289754
3503.125804	509822.153081	44.294759
3503.206047	509830.538476	44.299764
3502.879635	509808.482253	44.304769
3503.067455	509793.579138	44.309773
3502.865494	509795.533596	44.314778
3502.751024	509797.980129	44.319783
3502.850640	509794.119631	44.324788
3502.618684	509775.943888	44.329793
3502.851808	509750.055468	44.334797
3502.967654	509755.501029	44.339802
3503.076808	509760.947646	44.344807
3503.057873	509761.203698	44.349812
3502.602482	509763.501758	44.354817
3502.792623	509751.734842	44.359821
3502.909600	509758.950888	44.364826
3502.776226	509747.589234	44.369831
3502.960579	509735.722042	44.374836
3502.853414	509734.069602	44.379841
3502.713866	509721.292374	44.384845
3502.859205	509721.016557	44.389850
3503.278280	509723.530544	44.394855
3503.135784	509728.207498	44.399860
3503.046282	509704.545391	44.404865
3502.994999	509682.850245	44.409869
3502.831855	509696.636779	44.414874
3502.934276	509688.526205	44.419879
3503.201291	509681.300244	44.424884
3503.006691	509690.791551	44.429889
3502.915361	509649.625305	44.434893
3503.039875	509651.123453	44.439898
3503.059548	509649.906274	44.444903
3503.515924	509643.105684	44.449908
3502.968864	509616.075604	44.454913
3503.117063	509621.920821	44.459917
3502.824287	509587.868975	44.464922
3502.764009	509622.887471	44.469927
3503.256050	509595.946080	44.474932
3503.162646	509595.303268	44.479937
3502.741830	509575.942982	44.484941
3502.848853	509569.096397	44.489946
3502.666111	509569.175978	44.494951
3503.050064	509552.673335	44.499956
3502.615295	509571.561999	44.504961
3503.178593	509565.908071	44.509965
3503.148285	509568.189561	44.514970
3502.711485	509528.696537	44.519975
3502.693474	509531.987910	44.524980
3503.051359	509525.202841	44.529985
3503.257897	509515.203859	44.534989
3503.187771	509521.741301	44.539994
3502.800300	509519.020140	44.544999
3503.085464	509490.947686	44.550004
3502.802569	509472.020803	44.555009
3502.819997	509488.460299	44.560013
3503.117173	509480.521210	44.565018
3502.844711	509470.496727	44.570023
3503.048836	509497.733228	44.575028
3502.488152	509457.450161	44.580033
3502.607460	509429.454412	44.585037
3502.779550	509457.707867	44.590042
3503.007747	509418.058891	44.595047
3503.040166	509462.473061	44.600052
3502.752271	509438.133665	44.605057
3503.050903	509457.766591	44.610061
3502.494252	509444.953898	44.615066
3503.185780	509417.980698	44.620071
3503.118192	509400.082125	44.625076
3502.762384	509427.002506	44.630081
3502.803786	509404.584079	44.635085
3503.038992	509391.696782	44.640090
3503.043698	509421.393314	44.645095
3503.247832	509388.426135	44.650100
3502.939202	509405.321977	44.655105
3502.741049	509355.571362	44.660109
3502.722640	509341.408731	44.665114
3502.611274	509391.107339	44.670119
3502.776951	509353.997670	44.675124
3502.952204	509375.876220	44.680129
3502.706242	509380.822579	44.685133
3502.978707	509351.082384	44.690138
3502.761094	509371.049961	44.695143
3502.678283	509366.712284	44.700148
3502.504163	509338.206256	44.705153
3502.918053	509330.198059	44.710157
3502.526987	509334.509674	44.715162
3502.292404	509327.919352	44.720167
3502.938403	509333.180072	44.725172
3502.398571	509345.255717	44.730177
3502.610202	509335.458192	44.735181
3502.770923	509341.655667	44.740186
3502.301204	509323.213472	44.745191
3502.884788	509334.656240	44.750196
3502.782313	509343.323712	44.755201
3502.878279	509337.389432	44.760205
3503.098526	509335.128697	44.765210
3502.770318	509340.189250	44.770215
3503.163959	509332.133662	44.775220
3502.925174	509310.366497	44.780225
3503.188563	509299.447753	44.785229
3502.978949	509288.603762	44.790234
3502.903321	509289.222924	44.795239
3503.116734	509292.882500	44.800244
3502.860642	509283.715380	44.805249
3502.640773	509278.589875	44.810253
3503.085535	509269.109608	44.815258
3502.702946	509264.060408	44.820263
3502.801024	509261.262462	44.825268
3502.775204	509274.167569	44.830273
3503.111918	509259.544008	44.835277
3502.947430	509255.725131	44.840282
3502.712875	509245.289789	44.845287
3502.918541	509228.056135	44.850292
3502.772402	509228.433483	44.855297
3503.296242	509214.134451	44.860301
3503.213819	509218.397313	44.865306
3503.024882	509221.209841	44.870311
3503.192936	509204.892763	44.875316
3502.997511	509196.626664	44.880321
3503.099327	509192.917460	44.885325
3502.945055	509191.677148	44.890330
3503.240781	509174.530390	44.895335
3503.456282	509135.742835	44.900340
3503.015756	509145.931011	44.905345
3503.103576	509140.301503	44.910349
3503.253910	509134.358560	44.915354
3503.072026	509118.248485	44.920359
3503.086170	509096.896402	44.925364
3502.853627	509097.034448	44.930369
3503.000965	509116.539901	44.935373
3503.006756	509084.716517	44.940378
3502.494215	509088.389692	44.945383
3502.659937	509067.367761	44.950388
3502.881160	509062.678399	44.955393
3503.258313	509053.309885	44.960397
3503.260452	509056.800534	44.965402
3502.931259	509056.700894	44.970407
3503.253630	509043.850152	44.975412
3503.063952	509042.716611	44.980417
3503.275286	509002.006898	44.985421
3502.895241	509038.088980	44.990426
3503.124723	509001.879131	44.995431
3503.093010	509005.020993	45.000436
3503.060986	508971.887969	45.005441
3502.985551	508986.470693	45.010445
3503.151719	508980.929936	45.015450
3503.009113	508970.884635	45.020455
3502.888564	508947.378168	45.025460
3502.842219	508954.316810	45.030465
3502.699046	508945.131661	45.035469
3502.737308	508933.489376	45.040474
3502.437248	508939.304490	45.045479
3502.899027	508941.103545	45.050484
3503.125832	508939.044093	45.055489
3502.965040	508960.672729	45.060493
3503.033013	508923.021051	45.065498
3502.818829	508915.617859	45.070503
3503.029402	508895.701673	45.075508
3502.768460	508906.873465	45.080513
3503.176581	508900.636733	45.085517
3502.913995	508901.943165	45.090522
3502.881646	508910.802144	45.095527
3503.300009	508880.177995	45.100532
3502.849863	508868.511674	45.105537
3502.891831	508864.558892	45.110541
3503.127648	508858.349378	45.115546
3502.856501	508862.490377	45.120551
3502.893118	508839.717817	45.125556
3502.748892	508831.494043	45.130561
3502.869020	508830.766859	45.135565
3502.962635	508816.990835	45.140570
3503.031445	508820.521588	45.145575
3503.037773	508809.744349	45.150580
3503.210436	508814.321146	45.155585
3503.257691	508783.350735	45.160589
3502.993172	508790.121553	45.165594
3503.025382	508788.598772	45.170599
3503.172718	508772.942271	45.175604
3503.052722	508756.518515	45.180609
3503.251183	508735.946345	45.185613
3503.033766	508745.795933	45.190618
3503.071048	508732.787646	45.195623
3502.985947	508736.039182	45.200628
3503.158845	508707.629039	45.205633
3502.574186	508703.674074	45.210637
3503.094196	508677.435133	45.215642
3502.977208	508719.496941	45.220647
3503.129862	508675.507154	45.225652
3502.895372	508690.317643	45.230657
3502.989215	508651.801192	45.235661
3503.195545	508663.658192	45.240666
3502.839088	508631.688849	45.245671
3502.988564	508649.221340	45.250676
3502.708352	508661.711772	45.255681
3503.044236	508646.126542	45.260685
3502.996166	508624.631924	45.265690
3502.811006	508622.991704	45.270695
3503.132134	508620.259587	45.275700
3502.792362	508627.953050	45.280705
3502.717637	508621.185408	45.285709
3502.912575	508627.175359	45.290714
3502.719851	508630.342738	45.295719
3502.866951	508606.489939	45.300724
3502.987953	508588.914869	45.305729
3503.079500	508580.805491	45.310733
3502.766183	508572.810693	45.315738
3502.775876	508584.496452	45.320743
3503.283677	508580.874730	45.325748
3502.844918	508571.280754	45.330753
3503.283730	508574.297733	45.335757
3503.249203	508546.223671	45.340762
3502.587854	508550.122853	45.345767
3502.949899	508526.893693	45.350772
3502.788348	508536.683977	45.355777
3502.814789	508536.932875	45.360781
3502.647076	508527.549005	45.365786
3502.640629	508507.616077	45.370791
3503.209684	508485.315429	45.375796
3502.976614	508485.301780	45.380801
3502.948904	508484.597949	45.385805
3502.874547	508491.844769	45.390810
3502.680472	508491.673174	45.395815
3503.237391	508483.641980	45.400820
3503.121434	508473.136829	45.405825
3503.050402	508469.960729	45.410829
3503.034603	508462.930740	45.415834
3503.076265	508461.659407	45.420839
3503.435690	508441.769764	45.425844
3503.221803	508424.095674	45.430849
3502.949504	508416.043725	45.435853
3503.198366	508415.093801	45.440858
3503.202209	508402.697681	45.445863
3502.950433	508378.755827	45.450868
3502.816606	508372.199806	45.455873
3502.966624	508374.655331	45.460877
3503.036464	508386.129340	45.465882
3502.816086	508381.458996	45.470887
3502.934055	508358.976509	45.475892
3502.901735	508350.684222	45.480897
3502.937113	508325.988586	45.485901
3503.325991	508323.245715	45.490906
3502.854766	508337.183221	45.495911
3502.921282	508338.488274	45.500916
3502.955683	508316.221317	45.505921
3502.978334	508300.988852	45.510925
3503.124125	508294.641580	45.515930
3503.092110	508289.688466	45.520935
3503.150858	508286.289441	45.525940
3502.480724	508273.089047	45.530945
3502.819442	508263.979153	45.535949
3502.930100	508255.107680	45.540954
3502.727630	508250.232090	45.545959
3502.800382	508249.057018	45.550964
3502.764479	508244.610453	45.555969
3502.462321	508251.387431	45.560973
3502.676958	508251.606589	45.565978
3502.672514	508255.250226	45.570983
3502.896488	508250.509614	45.575988
3502.828154	508251.481824	45.580993
3502.845789	508246.065496	45.585997
3502.751151	508247.294838	45.591002
3502.220803	508214.593280	45.596007
3502.883727	508226.833770	45.601012
3502.565527	508219.902072	45.606017
3502.649213	508198.993237	45.611021
3502.808702	508197.551477	45.616026
3502.660254	508203.646445	45.621031
3502.987653	508199.648397	45.626036
3503.046776	508209.302799	45.631041
3502.912494	508220.859775	45.636045
3503.080082	508206.515027	45.641050
3502.875093	508194.050573	45.646055
3502.748764	508175.502273	45.651060
3502.982150	508173.289905	45.656065
3502.860853	508166.124684	45.661069
3503.199906	508163.794424	45.666074
3502.777613	508171.703513	45.671079
3503.009274	508160.384303	45.676084
3502.569114	508152.915308	45.681089
3502.589394	508135.254504	45.686093
3502.759062	508139.933145	45.691098
3502.591637	508140.566856	45.696103
3502.783752	508136.893748	45.701108
3502.440154	508132.647572	45.706113
3502.752765	508129.511964	45.711117
3502.865760	508137.690631	45.716122
3502.428264	508133.155725	45.721127
3502.880237	508140.623076	45.726132
3502.727111	508137.965842	45.731137
3502.663997	508132.612837	45.736141
3502.796527	508136.538421	45.741146
3502.517870	508141.287921	45.746151
3502.879772	508131.263580	45.751156
3502.408109	508140.799532	45.756161
3502.607515	508142.235382	45.761165
3502.742421	508140.342146	45.766170
3502.451456	508126.676949	45.771175
3502.798224	508113.922849	45.776180
3502.534646	508109.765211	45.781185
3502.643801	508103.170683	45.786189
3502.574533	508112.845431	45.791194
3502.587717	508106.569644	45.796199
3502.538291	508089.982312	45.801204
3502.390157	508099.720128	45.806209
3502.834528	508102.230360	45.811213
3502.467131	508102.996869	45.816218
3502.381109	508098.456998	45.821223
3502.716189	508097.392239	45.826228
3502.657922	508101.803345	45.831233
3502.615290	508100.899475	45.836237
3502.578073	508110.164397	45.841242
3502.706789	508107.513207	45.846247
3502.810240	508094.038622	45.851252
3502.638860	508117.137254	45.856257
3502.712162	508099.923391	45.861261
3502.787378	508116.557447	45.866266
3502.874967	508121.097280	45.871271
3502.571176	508105.005522	45.876276
3502.548616	508116.140149	45.881281
3502.490402	508116.351838	45.886285
3502.715658	508113.786581	45.891290
3502.601774	508108.694569	45.896295
3502.472691	508130.116855	45.901300
3502.621130	508121.340532	45.906305
3502.842658	508106.683604	45.911309
3502.880935	508107.689566	45.916314
3502.751300	508080.844063	45.921319
3502.950465	508069.023976	45.926324
3502.407016	508082.467148	45.931329
3502.656008	508078.785038	45.936333
3502.597804	508086.586025	45.941338
3502.556423	508083.152191	45.946343
3502.943831	508069.329133	45.951348
3502.540301	508098.232353	45.956353
3503.099812	508062.828487	45.961357
3502.863692	508092.464187	45.966362
3502.240392	508072.931823	45.971367
3502.826440	508092.672671	45.976372
3502.800205	508080.230477	45.981377
3502.782341	508059.539905	45.986381
3502.936002	508052.988919	45.991386
3502.725024	508039.462796	45.996391
3502.957338	508049.646464	46.001396
3502.561713	508044.396581	46.006401
3503.033671	508034.253598	46.011405
3503.027909	508047.814196	46.016410
3503.058963	508030.303369	46.021415
3503.036332	508045.030331	46.026420
3503.048136	508004.096817	46.031425
3503.141774	508016.579222	46.036429
3502.905821	508018.083892	46.041434
3502.764982	508008.847278	46.046439
3502.880271	508017.986954	46.051444
3502.876283	507976.904085	46.056449
3502.997062	508002.435880	46.061453
3502.823581	507988.802600	46.066458
3502.896399	507965.668993	46.071463
3503.232092	507966.526765	46.076468
3502.966690	507989.842810	46.081473
3503.220390	507942.597063	46.086477
3503.120670	507947.723099	46.091482
3502.655105	507916.022649	46.096487
3503.099174	507945.601691	46.101492
3502.975679	507926.243143	46.106497
3502.557647	507928.333153	46.111501
3503.135581	507904.613671	46.116506
3502.682891	507889.202992	46.121511
3502.856662	507905.720483	46.126516
3503.023186	507890.768490	46.131521
3502.736917	507901.034209	46.136525
3503.020980	507883.179668	46.141530
3502.539718	507903.140022	46.146535
3503.413332	507860.046120	46.151540
3502.852201	507896.159214	46.156545
3502.847021	507871.772913	46.161549
3503.153323	507838.280657	46.166554
3502.797940	507870.263007	46.171559
3503.127650	507839.954599	46.176564
3502.914163	507848.286196	46.181569
3502.932481	507812.056626	46.186573
3502.984902	507805.572143	46.191578
3502.882157	507806.094451	46.196583
3502.810014	507817.591280	46.201588
3503.076586	507784.105198	46.206593
3502.861381	507802.961096	46.211597
3502.976869	507782.653884	46.216602
3502.986068	507773.545218	46.221607
3503.037249	507772.424119	46.226612
3502.841265	507777.363036	46.231617
3502.970846	507756.294622	46.236621
3502.848736	507762.082005	46.241626
3502.595248	507759.744152	46.246631
3503.022874	507733.771361	46.251636
3502.761483	507732.952644	46.256641
3502.638078	507732.466292	46.261645
3502.947435	507728.875759	46.266650
3502.823280	507724.139431	46.271655
3503.085919	507730.827344	46.276660
3502.919909	507733.434104	46.281665
3502.874293	507719.628612	46.286669
3502.836752	507703.089626	46.291674
3502.824198	507694.945689	46.296679
3503.293836	507681.665887	46.301684
3503.011260	507689.502515	46.306689
3502.925432	507685.620259	46.311693
3503.059612	507692.429683	46.316698
3502.991540	507660.058779	46.321703
3503.058871	507650.940860	46.326708
3502.912196	507656.883950	46.331713
3502.959103	507648.932980	46.336717
3503.180516	507643.636045	46.341722
3502.833677	507635.747302	46.346727
3503.092746	507609.193805	46.351732
3502.999291	507606.729444	46.356737
3502.877968	507605.939179	46.361741
3503.132710	507598.613094	46.366746
3503.175420	507598.606451	46.371751
3503.297876	507564.889740	46.376756
3502.788018	507564.818641	46.381761
3502.830189	507563.091790	46.386765
3503.091080	507556.270684	46.391770
3502.734684	507572.366321	46.396775
3502.832294	507556.969560	46.401780
3502.947381	507537.269285	46.406785
3502.644085	507528.665253	46.411789
3502.928025	507519.867208	46.416794
3502.789045	507518.270179	46.421799
3503.018902	507524.254996	46.426804
3502.829899	507533.190039	46.431809
3503.020399	507529.112281	46.436813
3502.664804	507507.563682	46.441818
3502.540038	507494.883654	46.446823
3502.818278	507483.000072	46.451828
3502.613140	507484.702305	46.456833
3502.609929	507476.657983	46.461837
3502.472315	507485.028360	46.466842
3502.461581	507474.758954	46.471847
3503.000360	507478.367494	46.476852
3502.676575	507486.868490	46.481857
3502.927083	507485.007509	46.486861
3503.044542	507476.286352	46.491866
3502.829506	507482.847471	46.496871
3502.751198	507479.925324	46.501876
3502.572501	507475.146951	46.506881
3502.695876	507455.242885	46.511885
3502.960368	507445.182947	46.516890
3503.061489	507441.574670	46.521895
3503.050376	507436.314424	46.526900
3502.780064	507430.639768	46.531905
3502.902289	507442.257918	46.536909
3503.215638	507440.538792	46.541914
3502.925027	507422.218035	46.546919
3503.001528	507408.392994	46.551924
3502.950686	507403.139017	46.556929
3502.811378	507401.086652	46.561933
3503.057767	507402.616334	46.566938
3503.094695	507401.548061	46.571943
3502.954760	507377.637736	46.576948
3503.077660	507387.282517	46.581953
3503.031682	507371.807092	46.586957
3503.063228	507367.805017	46.591962
3502.864069	507375.021434	46.596967
3503.293618	507362.607880	46.601972
3502.761090	507344.932447	46.606977
3503.208930	507303.219990	46.611981
3502.973689	507340.395882	46.616986
3502.902027	507334.689798	46.621991
3503.091494	507318.873527	46.626996
3502.882360	507294.316255	46.632001
3502.885000	507289.762158	46.637005
3503.193241	507291.029085	46.642010
3503.042834	507288.371290	46.647015
3503.021827	507283.213756	46.652020
3502.691735	507269.908246	46.657025
3503.071134	507259.981832	46.662029
3503.158640	507243.422642	46.667034
3502.785211	507242.874598	46.672039
3503.036648	507241.823009	46.677044
3503.006416	507237.021104	46.682049
3502.881081	507231.222272	46.687053
3502.830196	507218.429169	46.692058
3502.663463	507209.145621	46.697063
3502.848063	507194.999736	46.702068
3502.419819	507204.326947	46.707073
3502.571167	507200.963672	46.712077
3502.928364	507203.133630	46.717082
3502.643366	507212.741783	46.722087
3503.219055	507200.659201	46.727092
3502.959857	507200.953265	46.732097
3502.945729	507191.392598	46.737101
3503.027901	507169.926180	46.742106
3502.588290	507158.459421	46.747111
3502.965278	507160.423866	46.752116
3502.894185	507162.408532	46.757121
3502.819053	507149.922799	46.762125
3502.779016	507158.075520	46.767130
3502.693102	507159.708343	46.772135
3503.209710	507150.974533	46.777140
3502.799939	507136.112974	46.782145
3502.733313	507109.154805	46.787149
3502.712402	507136.481211	46.792154
3502.976057	507111.848954	46.797159
3502.907621	507110.443130	46.802164
3502.530910	507127.857942	46.807169
3502.964191	507118.024127	46.812173
3502.941993	507117.521761	46.817178
3502.664942	507091.962974	46.822183
3502.904207	507074.823056	46.827188
3502.724013	507091.953852	46.832193
3502.835937	507064.056624	46.837197
3502.916915	507081.146152	46.842202
3502.814792	507089.915897	46.847207
3502.897744	507071.383930	46.852212
3502.797129	507090.222493	46.857217
3502.947599	507064.747889	46.862221
3503.194260	507049.074127	46.867226
3502.472031	507051.768901	46.872231
3502.999376	507041.970774	46.877236
3502.911211	507042.895587	46.882241
3502.630266	507041.928131	46.887245
3503.006141	507043.993962	46.892250
3502.679947	507037.771427	46.897255
3502.978363	507034.283678	46.902260
3502.503204	507021.557487	46.907265
3502.653232	507004.988187	46.912269
3502.959939	507011.112831	46.917274
3502.449381	507003.553265	46.922279
3502.983842	506992.792615	46.927284
3502.731302	506999.157450	46.932289
3502.829733	506998.990205	46.937293
3502.784371	506995.253192	46.942298
3502.825518	506989.377368	46.947303
3502.834453	506990.489231	46.952308
3502.538677	506994.887559	46.957313
3502.850013	506982.593615	46.962317
3503.082846	506966.011189	46.967322
3502.728395	506963.638586	46.972327
3502.776015	506957.458137	46.977332
3502.694534	506952.057069	46.982337
3502.723862	506960.603708	46.987341
3502.683526	506948.618316	46.992346
3503.087776	506940.003357	46.997351
3503.130853	506954.012482	47.002356
3503.042736	506952.963945	47.007361
3502.618294	506922.317740	47.012365
3502.584810	506919.590808	47.017370
3502.402212	506925.792820	47.022375
3502.941773	506920.293585	47.027380
3502.582618	506922.829795	47.032385
3502.766058	506925.330845	47.037389
3502.749786	506928.521243	47.042394
3503.176617	506924.658985	47.047399
3502.944167	506923.076673	47.052404
3502.608917	506918.221691	47.057409
3502.363764	506896.604274	47.062413
3502.627755	506903.140499	47.067418
3502.463726	506910.351556	47.072423
3502.884813	506901.885714	47.077428
3502.966143	506889.931650	47.082433
3502.753453	506884.703096	47.087437
3503.043092	506886.276587	47.092442
3502.563286	506875.524377	47.097447
3502.785786	506877.766266	47.102452
3502.706207	506890.074468	47.107457
3502.667042	506892.155317	47.112461
3502.820363	506881.050048	47.117466
3502.570814	506884.783313	47.122471
3502.985187	506885.223915	47.127476
3502.861739	506868.647110	47.132481
3503.006083	506848.334241	47.137485
3502.896032	506851.691271	47.142490
3502.764141	506846.955925	47.147495
3502.738237	506838.763096	47.152500
3502.712648	506848.785840	47.157505
3502.728980	506845.342638	47.162509
3502.833168	506846.591251	47.167514
3502.511733	506854.383799	47.172519
3502.485445	506838.854186	47.177524
3502.988202	506846.668267	47.182529
3502.528779	506828.474760	47.187533
3502.871073	506810.458114	47.192538
3502.567891	506811.821715	47.197543
3503.230712	506796.334945	47.202548
3502.616808	506805.337519	47.207553
3502.891339	506805.091840	47.212557
3502.936564	506804.123417	47.217562
3502.646262	506804.978993	47.222567
3503.059855	506803.749951	47.227572
3502.961099	506780.490081	47.232577
3503.084138	506765.847585	47.237581
3502.811886	506760.577808	47.242586
3502.708042	506764.035073	47.247591
3503.080036	506759.624855	47.252596
3502.813846	506766.396726	47.257601
3503.016552	506757.762933	47.262605
3502.992993	506736.515086	47.267610
3502.844465	506731.326944	47.272615
3502.739161	506731.293095	47.277620
3502.673498	506734.238339	47.282625
3502.684939	506731.554876	47.287629
3502.656546	506726.499542	47.292634
3502.595947	506746.799532	47.297639
3503.012102	506725.532773	47.302644
3502.672618	506733.429426	47.307649
3502.887694	506739.315654	47.312653
3502.943613	506727.213696	47.317658
3502.728691	506700.025333	47.322663
3503.001322	506691.886448	47.327668
3502.799390	506702.038348	47.332673
3502.623863	506689.922346	47.337677
3502.932949	506684.206467	47.342682
3502.618501	506693.768962	47.347687
3502.990945	506688.043071	47.352692
3502.774333	506690.657984	47.357697
3502.435497	506701.691711	47.362701
3502.786988	506688.429825	47.367706
3502.610453	506671.507025	47.372711
3502.825875	506665.148151	47.377716
3502.487668	506662.874138	47.382721
3503.020308	506646.952415	47.387725
3502.660651	506648.982749	47.392730
3502.420759	506656.458899	47.397735
3502.748754	506649.019638	47.402740
3502.693362	506651.609075	47.407745
3502.770846	506648.965761	47.412749
3502.731541	506646.189107	47.417754
3502.585167	506658.963425	47.422759
3502.869164	506642.473804	47.427764
3502.745194	506674.522983	47.432769
3502.841562	506654.672865	47.437773
3503.129965	506628.973422	47.442778
3502.470140	506628.673021	47.447783
3502.954094	506613.973353	47.452788
3502.732320	506615.222903	47.457793
3502.658389	506614.222703	47.462797
3502.840841	506609.032811	47.467802
3502.368809	506608.044933	47.472807
3502.515419	506616.927402	47.477812
3502.624684	506619.035423	47.482817
3502.756801	506600.140985	47.487821
3502.950173	506620.856378	47.492826
3502.531829	506612.017074	47.497831
3503.033006	506606.068411	47.502836
3502.745350	506616.537507	47.507841
3502.636004	506584.930109	47.512845
3502.755698	506571.552971	47.517850
3502.441798	506591.690778	47.522855
3502.993935	506569.036143	47.527860
3502.453241	506575.143079	47.532865
3502.491595	506577.616511	47.537869
3502.837772	506577.157106	47.542874
3502.700208	506577.533154	47.547879
3502.840393	506577.460504	47.552884
3502.619106	506572.587413	47.557889
3502.590641	506584.432355	47.562893
3502.998495	506582.394610	47.567898
3502.993356	506593.426264	47.572903
3503.005909	506576.068688	47.577908
3502.843259	506566.935949	47.582913
3503.037900	506542.010193	47.587917
3503.110547	506537.191833	47.592922
3502.795083	506557.481727	47.597927
3502.936842	506522.393742	47.602932
3502.877556	506527.716207	47.607937
3502.670935	506511.708804	47.612941
3502.670541	506502.246786	47.617946
3502.854338	506495.336249	47.622951
3502.779800	506482.900541	47.627956
3502.660555	506498.605490	47.632961
3502.870557	506492.854609	47.637965
3503.029536	506491.868190	47.642970
3502.896902	506495.228859	47.647975
3502.779749	506490.339285	47.652980
3502.743060	506493.735389	47.657985
3502.542246	506463.862627	47.662989
3502.656695	506449.879023	47.667994
3502.556854	506443.468696	47.672999
3502.863260	506450.048989	47.678004
3502.336711	506464.502742	47.683009
3502.576248	506452.017371	47.688013
3503.033385	506451.338025	47.693018
3502.977964	506465.059512	47.698023
3502.642712	506443.101569	47.703028
3502.371956	506471.682915	47.708033
3502.841042	506453.848259	47.713037
3502.750192	506454.722927	47.718042
3502.458657	506451.429507	47.723047
3502.824345	506448.335810	47.728052
3502.584883	506465.931992	47.733057
3502.540288	506445.193114	47.738061
3502.608533	506467.952471	47.743066
3502.645242	506458.029164	47.748071
3502.465849	506458.108225	47.753076
3502.761972	506469.497143	47.758081
3502.867062	506448.785210	47.763085
3502.619773	506437.692376	47.768090
3502.562383	506441.091763	47.773095
3502.881591	506415.285935	47.778100
3502.748980	506417.027409	47.783105
3502.590854	506436.837174	47.788109
3502.974607	506402.570900	47.793114
3502.461398	506438.628854	47.798119
3502.672978	506414.965242	47.803124
3502.584810	506442.505773	47.808129
3502.787137	506402.449159	47.813133
3502.408416	506438.435257	47.818138
3502.461340	506403.310471	47.823143
3502.974725	506439.054366	47.828148
3502.668735	506412.993148	47.833153
3502.469303	506437.414060	47.838157
3502.980364	506422.507545	47.843162
3502.847340	506420.757671	47.848167
3503.219017	506395.601324	47.853172
3502.778944	506401.945417	47.858177
3503.023708	506380.907726	47.863181
3503.441821	506382.966962	47.868186
3502.818637	506380.687352	47.873191
3503.287152	506359.917873	47.878196
3502.898841	506333.768346	47.883201
3502.567099	506360.031894	47.888205
3503.016307	506345.388092	47.893210
3502.723997	506338.198541	47.898215
3503.084443	506351.601386	47.903220
3502.944269	506336.291725	47.908225
3502.917068	506297.434957	47.913229
3502.914139	506317.473331	47.918234
3502.504874	506303.116980	47.923239
3502.806242	506285.966468	47.928244
3503.157616	506279.535365	47.933249
3502.985735	506303.395503	47.938253
3502.920700	506299.054244	47.943258
3502.952123	506296.822961	47.948263
3503.107616	506253.281968	47.953268
3502.942153	506257.912888	47.958273
3502.917526	506268.694824	47.963277
3503.170542	506259.546826	47.968282
3502.648233	506266.308771	47.973287
3502.911330	506229.531195	47.978292
3502.529212	506234.550570	47.983297
3502.556895	506216.127627	47.988301
3503.046458	506222.071849	47.993306
3503.018209	506218.382565	47.998311
3503.174070	506197.409305	48.003316
3502.779287	506216.548314	48.008321
3502.788298	506217.862617	48.013325
3503.160440	506204.040489	48.018330
3502.712734	506190.904540	48.023335
3502.708298	506187.565692	48.028340
3502.809145	506186.588443	48.033345
3502.824468	506177.073163	48.038349
3502.653219	506175.582310	48.043354
3502.941784	506182.266727	48.048359
3502.838062	506175.401507	48.053364
3502.870158	506184.504701	48.058369
3502.740598	506154.063533	48.063373
3502.649977	506149.523877	48.068378
3502.619146	506155.449170	48.073383
3503.160350	506139.222025	48.078388
3502.883193	506136.634685	48.083393
3502.817091	506142.464356	48.088397
3502.832249	506135.732134	48.093402
3503.008102	506131.352759	48.098407
3503.260703	506132.021356	48.103412
3502.429671	506129.774563	48.108417
3502.510469	506121.159722	48.113421
3502.869321	506109.414263	48.118426
3502.618718	506111.579225	48.123431
3503.058326	506098.808973	48.128436
3502.908153	506095.796748	48.133441
3502.956204	506101.001177	48.138445
3502.813179	506116.305420	48.143450
3502.786622	506114.488086	48.148455
3503.016329	506077.614264	48.153460
3503.098309	506071.326866	48.158465
3503.191294	506055.018682	48.163469
3503.258281	506059.410510	48.168474
3502.953966	506050.451693	48.173479
3503.008902	506041.739698	48.178484
3502.875543	506017.371045	48.183489
3503.143643	506018.948022	48.188493
3503.062447	506028.322210	48.193498
3502.784202	506016.930392	48.198503
3503.168318	506000.171331	48.203508
3502.561611	505996.371022	48.208513
3502.733813	505980.100848	48.213517
3503.092941	505982.827274	48.218522
3503.222668	505980.226203	48.223527
3503.263262	505966.000876	48.228532
3502.844547	505961.209418	48.233537
3502.837870	505942.892819	48.238541
3502.830086	505944.311001	48.243546
3502.659466	505935.533400	48.248551
3502.866365	505929.732223	48.253556
3502.494008	505934.851343	48.258561
3502.758619	505936.327676	48.263565
3502.869233	505940.510232	48.268570
3502.284114	505942.019664	48.273575
3502.797554	505932.374919	48.278580
3502.399759	505926.618714	48.283585
3502.628378	505934.476538	48.288589
3502.462145	505937.741421	48.293594
3502.283913	505943.032264	48.298599
3502.971549	505928.907045	48.303604
3502.837788	505934.292065	48.308609
3502.480597	505940.825631	48.313613
3502.376698	505939.931331	48.318618
3502.773671	505940.121704	48.323623
3502.569252	505940.103518	48.328628
3502.677317	505946.563547	48.333633
3502.779129	505918.463671	48.338637
3502.922750	505909.383382	48.343642
3502.362072	505905.221565	48.348647
3502.664491	505893.130669	48.353652
3502.590148	505889.904016	48.358657
3502.137299	505897.869566	48.363661
3502.485714	505895.284519	48.368666
3502.613255	505897.895757	48.373671
3502.673454	505891.662338	48.378676
3502.952496	505894.401437	48.383681
3502.700731	505897.376236	48.388685
3502.624577	505905.130439	48.393690
3502.581977	505910.197447	48.398695
3502.691411	505891.457630	48.403700
3502.680186	505905.374980	48.408705
3502.503591	505902.164491	48.413709
3503.185375	505896.591856	48.418714
3502.987048	505907.300267	48.423719
3502.912811	505885.856983	48.428724
3502.544732	505879.741853	48.433729
3502.440851	505872.168113	48.438733
3502.739911	505863.265639	48.443738
3502.539213	505861.728811	48.448743
3502.740998	505852.588697	48.453748
3502.433482	505866.856519	48.458753
3502.404329	505862.003461	48.463757
3503.052207	505860.281910	48.468762
3502.478361	505868.469005	48.473767
3502.400423	505858.968291	48.478772
3502.290937	505864.956717	48.483777
3502.643644	505856.501176	48.488781
3502.570820	505857.626034	48.493786
3502.544816	505864.157885	48.498791
3502.841412	505858.038897	48.503796
3502.489979	505867.253477	48.508801
3502.803846	505860.625741	48.513805
3502.917755	505864.251175	48.518810
3502.858817	505867.144901	48.523815
3502.706653	505855.429437	48.528820
3502.559932	505864.611663	48.533825
3502.396697	505863.018313	48.538829
3502.665693	505874.007095	48.543834
3502.813075	505862.396097	48.548839
3502.824365	505859.307710	48.553844
3502.575061	505833.843885	48.558849
3502.574423	505830.453766	48.563853
3502.547257	505821.957045	48.568858
3502.657957	505829.175730	48.573863
3502.540094	505816.493383	48.578868
3502.248182	505819.474540	48.583873
3502.623864	505817.391192	48.588877
3502.564219	505830.860838	48.593882
3502.858524	505817.759133	48.598887
3503.135575	505813.060073	48.603892
3502.936140	505827.665058	48.608897
3502.994054	505826.795779	48.613901
3502.787255	505830.067094	48.618906
3502.682097	505825.377844	48.623911
3503.031081	505821.932464	48.628916
3502.909165	505797.966511	48.633921
3503.208203	505783.396575	48.638925
3503.172557	505784.262550	48.643930
3502.633188	505792.798445	48.648935
3502.934009	505788.196825	48.653940
3502.994067	505789.148878	48.658945
3503.068842	505764.949383	48.663949
3503.087118	505749.057538	48.668954
3502.839941	505747.932863	48.673959
3502.828324	505739.636053	48.678964
3502.921438	505742.455164	48.683969
3502.994915	505739.862948	48.688973
3503.138219	505716.057371	48.693978
3502.584321	505708.908903	48.698983
3503.046957	505698.310617	48.703988
3502.860777	505709.624457	48.708993
3502.631108	505702.880161	48.713997
3503.047666	505692.086744	48.719002
3502.789153	505696.732520	48.724007
3503.006065	505683.997163	48.729012
3502.878455	505669.292156	48.734017
3502.898414	505654.968632	48.739021
3502.998326	505655.408369	48.744026
3502.974834	505649.896526	48.749031
3503.145379	505656.093775	48.754036
3502.809528	505649.619253	48.759041
3502.683361	505631.776635	48.764045
3502.852239	505619.909067	48.769050
3502.721631	505617.349088	48.774055
3502.679017	505617.052316	48.779060
3502.788656	505617.642325	48.784065
3502.898490	505612.868435	48.789069
3502.893533	505614.438004	48.794074
3502.550604	505621.222448	48.799079
3502.765751	505616.229503	48.804084
3502.838316	505613.435002	48.809089
3502.680653	505605.616635	48.814093
3503.077268	505584.806995	48.819098
3502.913634	505570.512419	48.824103
3502.912930	505567.223464	48.829108
3502.765345	505574.230065	48.834113
3502.867220	505572.645388	48.839117
3502.907162	505574.612686	48.844122
3502.560627	505580.841086	48.849127
3502.845239	505568.803382	48.854132
3502.888676	505554.071243	48.859137
3502.909471	505539.747492	48.864141
3502.923665	505538.277876	48.869146
3502.701729	505535.023882	48.874151
3502.945825	505530.835982	48.879156
3502.641127	505536.399950	48.884161
3502.775122	505529.547505	48.889165
3502.637248	505528.810362	48.894170
3502.377695	505529.964754	48.899175
3502.781044	505533.797524	48.904180
3502.567201	505534.438663	48.909185
3502.473645	505530.860761	48.914189
3502.821065	505536.119247	48.919194
3502.385638	505528.142335	48.924199
3502.663758	505523.088808	48.929204
3502.693901	505535.785449	48.934209
3502.555128	505515.819388	48.939213
3502.909702	505500.734411	48.944218
3502.918507	505497.292131	48.949223
3502.993900	505494.648973	48.954228
3502.623372	505489.394341	48.959233
3502.616021	505496.176397	48.964237
3502.581608	505499.926555	48.969242
3502.552370	505501.854192	48.974247
3502.696778	505493.482002	48.979252
3502.909368	505491.728010	48.984257
3502.614757	505496.581956	48.989261
3502.787332	505493.366806	48.994266
3502.668193	505492.120671	48.999271
3502.609880	505492.484215	49.004276
3502.584881	505476.902578	49.009281
3502.761153	505473.788046	49.014285
3502.453239	505475.354909	49.019290
3502.368199	505472.180472	49.024295
3502.579169	505464.961615	49.029300
3502.671464	505468.388136	49.034305
3502.246666	505473.768694	49.039309
3502.893299	505474.881068	49.044314
3502.508587	505478.129966	49.049319
3502.837909	505469.627332	49.054324
3502.615375	505478.366317	49.059329
3503.138729	505470.490853	49.064333
3503.151610	505462.139436	49.069338
3502.698833	505475.064257	49.074343
3503.213182	505470.378202	49.079348
3502.662756	505455.436224	49.084353
3502.504747	505444.025025	49.089357
3502.802723	505422.825959	49.094362
3502.344408	505427.351576	49.099367
3502.632926	505431.253121	49.104372
3502.659923	505427.807953	49.109377
3502.877108	505435.566604	49.114381
3502.769223	505430.574061	49.119386
3502.562098	505426.103232	49.124391
3503.238281	505424.579579	49.129396
3503.020322	505433.672085	49.134401
3502.817918	505432.186092	49.139405
3502.843231	505411.333725	49.144410
3502.900147	505399.939131	49.149415
3502.818468	505380.267510	49.154420
3502.881159	505396.551935	49.159425
3502.621882	505390.318229	49.164429
3502.944631	505398.110816	49.169434
3502.786546	505379.210317	49.174439
3503.058004	505384.885682	49.179444
3502.991843	505391.120438	49.184449
3503.020907	505357.616616	49.189453
3503.192687	505346.102625	49.194458
3502.969995	505348.111459	49.199463
3503.104509	505341.107048	49.204468
3502.823612	505335.635789	49.209473
3502.784115	505317.627341	49.214477
3503.057547	505300.986311	49.219482
3502.714443	505308.985385	49.224487
3502.716836	505307.973046	49.229492
3503.017436	505300.537542	49.234497
3502.834767	505294.494107	49.239501
3502.969215	505311.981752	49.244506
3502.641418	505281.266769	49.249511
3503.031739	505264.607230	49.254516
3502.659487	505257.531072	49.259521
3503.017942	505257.474524	49.264525
3503.089198	505250.328265	49.269530
3502.795583	505248.603653	49.274535
3503.009089	505250.847177	49.279540
3503.236786	505256.934328	49.284545
3502.893814	505224.501123	49.289549
3502.989958	505213.859262	49.294554
3502.752506	505210.354641	49.299559
3502.861590	505215.903914	49.304564
3502.936537	505218.371756	49.309569
3502.603406	505220.448663	49.314573
3502.983002	505217.504364	49.319578
3502.869886	505194.143433	49.324583
3503.024152	505190.475687	49.329588
3502.883748	505178.049457	49.334593
3502.803418	505160.452130	49.339597
3502.683451	505174.083629	49.344602
3502.305023	505178.900305	49.349607
3502.692223	505170.135359	49.354612
3502.650729	505168.775722	49.359617
3502.372195	505175.246537	49.364621
3502.717109	505168.461822	49.369626
3502.655841	505166.649875	49.374631
3502.801924	505176.646449	49.379636
3502.722715	505175.090357	49.384641
3502.733339	505166.992175	49.389645
3502.899274	505141.208688	49.394650
3502.378310	505143.720123	49.399655
3502.879259	505131.141886	49.404660
3502.503405	505141.878825	49.409665
3502.544601	505135.293913	49.414669
3502.591297	505133.363691	49.419674
3502.381787	505150.248011	49.424679
3502.385556	505130.360188	49.429684
3502.513999	505132.870191	49.434689
3502.495884	505125.231966	49.439693
3502.628111	505138.165781	49.444698
3502.345147	505146.914482	49.449703
3502.821297	505136.111305	49.454708
3502.607027	505143.735865	49.459713
3502.568769	505142.223902	49.464717
3502.704570	505133.903504	49.469722
3502.462523	505142.746948	49.474727
3502.550283	505144.807944	49.479732
3502.409624	505144.172433	49.484737
3502.785265	505143.101090	49.489741
3502.830216	505143.498924	49.494746
3502.390928	505145.491411	49.499751
3502.709873	505140.987964	49.504756
3502.689678	505143.470855	49.509761
3502.238961	505141.872271	49.514765
3502.583746	505133.063407	49.519770
3502.811806	505143.350666	49.524775
3502.835504	505143.954275	49.529780
3502.507482	505144.309850	49.534785
3503.276638	505149.856025	49.539789
3502.794651	505138.293416	49.544794
3502.623709	505124.303253	49.549799
3502.627552	505096.065724	49.554804
3502.928438	505105.936663	49.559809
3502.276340	505106.292857	49.564813
3502.604045	505096.120366	49.569818
3502.426685	505095.338841	49.574823
3502.670996	505097.476307	49.579828
3503.002039	505104.103822	49.584833
3503.092209	505106.316254	49.589837
3502.953864	505103.757423	49.594842
3502.737335	505103.083298	49.599847
3502.870079	505091.474101	49.604852
3502.859613	505088.085391	49.609857
3502.508600	505082.726343	49.614861
3502.922874	505072.540155	49.619866
3502.662588	505068.786093	49.624871
3502.754194	505061.535332	49.629876
3502.569028	505059.591144	49.634881
3502.488573	505065.625860	49.639885
3502.645556	505069.244651	49.644890
3502.388301	505067.868504	49.649895
3502.627051	505063.225901	49.654900
3502.662898	505068.230150	49.659905
3502.745032	505073.429499	49.664909
3502.712941	505058.455858	49.669914
3502.740385	505065.738623	49.674919
3502.648909	505059.326464	49.679924
3502.630643	505067.122494	49.684929
3502.742503	505063.714445	49.689933
3502.953738	505062.112438	49.694938
3502.592933	505050.682430	49.699943
3502.648555	505026.990981	49.704948
3502.473698	505028.435643	49.709953
3502.300829	505027.501593	49.714957
3502.910642	505028.012568	49.719962
3502.607305	505031.198081	49.724967
3502.770902	505024.796198	49.729972
3502.797213	505021.755892	49.734977
3502.749217	505025.811924	49.739981
3502.915392	505029.125646	49.744986
3502.600284	505021.635526	49.749991
3502.812708	505020.134536	49.754996
3502.787393	505030.057075	49.760001
3503.099203	505008.804716	49.765005
3502.808122	505006.725450	49.770010
3502.668212	504994.501428	49.775015
3502.804986	504981.221578	49.780020
3502.577089	504987.633855	49.785025
3502.427425	504988.922726	49.790029
3502.681848	504983.973998	49.795034
3502.530697	504986.882444	49.800039
3502.426331	504986.696629	49.805044
3502.409701	504992.012821	49.810049
3502.706007	504981.895830	49.815053
3502.478717	504985.170541	49.820058
3502.461650	504987.349333	49.825063
3502.541532	504990.575492	49.830068
3502.539312	504985.464912	49.835073
3502.413795	504995.150286	49.840077
3502.769363	504979.508055	49.845082
3502.410307	504999.958463	49.850087
3502.593420	504981.408440	49.855092
3502.568222	504983.234287	49.860097
3502.537366	504988.249102	49.865101
3502.671743	504986.203797	49.870106
3502.446169	504998.283388	49.875111
3502.752541	504984.318880	49.880116
3502.736694	504986.548083	49.885121
3502.568551	504993.659374	49.890125
3502.980631	504996.934236	49.895130
3502.646028	504991.420752	49.900135
3502.784392	504986.186743	49.905140
3502.725929	504987.410595	49.910145
3502.464549	504984.365149	49.915149
3503.002252	504982.306700	49.920154
3502.764003	504983.811990	49.925159
3503.020899	504943.439773	49.930164
3502.784121	504943.983349	49.935169
3502.977462	504946.685539	49.940173
3502.885500	504939.109510	49.945178
3502.435426	504952.692147	49.950183
3502.558428	504935.568501	49.955188
3502.560222	504945.284386	49.960193
3502.640932	504940.919751	49.965197
3502.793494	504948.385207	49.970202
3502.755366	504958.714648	49.975207
3503.087607	504942.620631	49.980212
3502.987076	504923.002079	49.985217
3502.462287	504914.836590	49.990221
3502.882687	504900.752783	49.995226
3502.903882	504907.682369	50.000231
3502.703901	504903.159672	50.005236
3502.752886	504898.395204	50.010241
3502.663236	504909.491887	50.015245
3502.671861	504909.490631	50.020250
3502.884007	504906.825769	50.025255
3503.109834	504893.886011	50.030260
3502.702432	504882.412653	50.035265
3502.806490	504873.085055	50.040269
3503.231695	504862.492180	50.045274
3502.386698	504865.257287	50.050279
3502.542745	504861.741006	50.055284
3502.523968	504868.727530	50.060289
3502.300281	504870.028109	50.065293
3502.831428	504861.746305	50.070298
3502.874126	504883.297258	50.075303
3502.617370	504871.344640	50.080308
3502.682774	504875.281575	50.085313
3502.434582	504870.311047	50.090317
3502.618164	504859.604546	50.095322
3502.356664	504869.412692	50.100327
3502.399993	504863.080364	50.105332
3502.589445	504866.289229	50.110337
3502.522677	504875.661756	50.115341
3502.796527	504874.859510	50.120346
3502.439949	504873.499045	50.125351
3502.910249	504867.757094	50.130356
3502.860135	504869.637496	50.135361
3502.642419	504870.127456	50.140365
3502.772259	504833.772838	50.145370
3502.569095	504839.776421	50.150375
3502.587441	504826.312753	50.155380
3502.507213	504825.667678	50.160385
3502.572010	504816.902908	50.165389
3502.475075	504819.397974	50.170394
3502.226065	504832.139247	50.175399
3502.457441	504823.145733	50.180404
3502.741629	504830.438621	50.185409
3502.536409	504830.369955	50.190413
3502.861069	504828.294556	50.195418
3502.599766	504826.716609	50.200423
3502.644295	504816.032059	50.205428
3502.685880	504829.132244	50.210433
3502.730507	504824.317840	50.215437
3502.866793	504824.448222	50.220442
3502.671020	504836.675029	50.225447
3502.824017	504827.643301	50.230452
3502.745801	504831.552340	50.235457
3502.508904	504821.823161	50.240461
3502.794493	504825.725306	50.245466
3502.449412	504820.567658	50.250471
3502.732439	504829.935528	50.255476
3502.688871	504829.183449	50.260481
3502.507478	504834.829359	50.265485
3502.541056	504822.679005	50.270490
3502.588889	504811.740906	50.275495
3502.747749	504818.851189	50.280500
3502.481031	504798.550296	50.285505
3502.363408	504790.573419	50.290509
3502.408811	504799.472813	50.295514
3502.260023	504830.162975	50.300519
3502.478796	504831.393624	50.305524
3502.545068	504832.749587	50.310529
3502.622083	504838.101629	50.315533
3502.410822	504843.701652	50.320538
3502.358290	504845.126996	50.325543
3502.554276	504834.317309	50.330548
3502.759021	504833.677798	50.335553
3502.501788	504836.704245	50.340557
3502.773322	504829.273135	50.345562
3502.759242	504840.863964	50.350567
3502.790334	504818.542438	50.355572
3502.651978	504811.884574	50.360577
3502.755327	504797.294141	50.365581
3503.148171	504794.550098	50.370586
3502.759624	504800.127551	50.375591
3502.951221	504791.848776	50.380596
3502.696407	504796.595414	50.385601
3502.780221	504800.833086	50.390605
3502.481592	504794.352361	50.395610
3502.588916	504796.865750	50.400615
3502.720843	504795.681093	50.405620
3502.612434	504800.353986	50.410625
3502.521635	504800.520259	50.415629
3502.638763	504788.812120	50.420634
3502.282015	504801.013790	50.425639
3502.641320	504791.747016	50.430644
3502.699897	504793.357222	50.435649
3502.420828	504783.533477	50.440653
3502.399649	504789.407104	50.445658
3502.709192	504792.495791	50.450663
3502.957333	504785.979249	50.455668
3502.798893	504777.755792	50.460673
3502.830218	504762.367035	50.465677
3503.180117	504755.631978	50.470682
3502.804248	504759.739895	50.475687
3502.799030	504759.487802	50.480692
3502.741237	504760.964588	50.485697
3502.734676	504764.963527	50.490701
3502.851546	504761.250998	50.495706
3502.722324	504740.118625	50.500711
3502.531584	504717.477797	50.505716
3502.751147	504713.394790	50.510721
3502.579243	504715.749904	50.515725
3502.952595	504710.225646	50.520730
3502.377139	504710.721548	50.525735
3502.386267	504688.099696	50.530740
3502.655681	504661.388253	50.535745
3502.488556	504610.252750	50.540749
3502.793116	504559.751024	50.545754
3502.502681	504502.207785	50.550759
3502.444774	504410.721606	50.555764
3501.971033	504329.017077	50.560769
3501.886932	504237.938985	50.565773
3501.990489	504141.618261	50.570778
3502.019874	504027.798677	50.575783
3501.836772	503907.736614	50.580788
3501.460766	503772.673693	50.585793
3501.761349	503628.089657	50.590797
3501.595982	503474.822775	50.595802
3501.199643	503319.566696	50.600807
3501.287835	503143.887591	50.605812
3500.743226	502964.612210	50.610817
3500.633625	502791.795028	50.615821
3500.371048	502582.762696	50.620826
3500.138121	502396.599756	50.625831
3499.876473	502182.045849	50.630836
3499.999050	501954.269216	50.635841
3499.635922	501733.500503	50.640845
3499.138123	501502.323769	50.645850
3498.527404	501265.796679	50.650855
3498.544541	501021.018069	50.655860
3498.226264	500770.316367	50.660865
3497.899700	500507.464322	50.665869
3498.063305	500237.798740	50.670874
3497.126790	499978.578565	50.675879
3496.793671	499702.858554	50.680884
3496.566911	499409.805349	50.685889
3496.427226	499124.832966	50.690893
3496.019037	498812.714511	50.695898
3495.564220	498523.732638	50.700903
3495.219269	498209.568804	50.705908
3494.575862	497890.839829	50.710913
3493.903661	497585.019264	50.715917
3493.756127	497244.482175	50.720922
3493.364181	496929.949118	50.725927
3492.986283	496604.270186	50.730932
3492.434709	496274.714421	50.735937
3491.958774	495924.635558	50.740941
3491.583979	495580.964119	50.745946
3491.082822	495235.534056	50.750951
3491.176975	494873.446386	50.755956
3490.605920	494509.127533	50.760961
3489.756791	494153.098893	50.765965
3489.594723	493786.776918	50.770970
3489.013134	493411.196748	50.775975
3488.324627	493022.459922	50.780980
3487.656407	492657.157612	50.785985
3487.168971	492264.372560	50.790989
3486.824086	491884.925927	50.795994
3486.271512	491508.492254	50.800999
3485.927358	491102.290403	50.806004
3485.357384	490712.321598	50.811009
3484.595755	490317.867490	50.816013
3484.300281	489910.771031	50.821018
3483.632639	489506.003696	50.826023
3482.967489	489092.718244	50.831028
3482.698255	488677.233831	50.836033
3482.320388	488249.297277	50.841037
3481.920926	487836.347477	50.846042
3480.574790	487432.503921	50.851047
3480.579174	486991.713880	50.856052
3480.231474	486559.580711	50.861057
3479.266768	486131.790422	50.866061
3478.965990	485693.500733	50.871066
3478.702987	485267.657136	50.876071
3477.739636	484818.205833	50.881076
3477.159219	484386.516259	50.886081
3476.322291	483946.650226	50.891085
3476.094234	483485.297853	50.896090
3475.127029	483056.932779	50.901095
3474.461250	482607.028221	50.906100
3474.203990	482151.931273	50.911105
3473.451012	481703.995600	50.916109
3472.843951	481255.722550	50.921114
3472.039826	480805.494206	50.926119
3471.478578	480344.829389	50.931124
3470.833877	479898.507411	50.936129
3470.182039	479441.788229	50.941133
3469.624424	478978.810502	50.946138
3468.850242	478521.582606	50.951143
3468.277734	478057.116038	50.956148
3467.872472	477604.318986	50.961153
3467.169893	477149.784824	50.966157
3466.485632	476681.756206	50.971162
3465.622847	476222.969042	50.976167
3465.282298	475746.248203	50.981172
3464.473847	475280.842030	50.986177
3463.732951	474818.861058	50.991181
3463.280565	474346.939919	50.996186
3462.539854	473883.112780	51.001191
3461.666521	473416.305317	51.006196
3460.891107	472953.780349	51.011201
3460.569415	472483.366627	51.016205
3460.104078	472012.102997	51.021210
3459.131333	471547.448262	51.026215
3458.530076	471079.479785	51.031220
3457.992080	470609.716287	51.036225
3457.095122	470135.081169	51.041229
3456.489554	469654.355941	51.046234
3455.618885	469201.343590	51.051239
3454.918934	468729.382915	51.056244
3454.381083	468261.340682	51.061249
3453.362293	467800.056809	51.066253
3452.838574	467325.501368	51.071258
3451.836225	466868.149316	51.076263
3451.739451	466401.212732	51.081268
3450.768318	465932.679964	51.086273
3449.986934	465473.031568	51.091277
3449.531971	464995.978792	51.096282
3448.602730	464533.037250	51.101287
3448.033307	464062.878340	51.106292
3447.357816	463596.072921	51.111297
3446.604463	463136.116071	51.116301
3445.928428	462660.973202	51.121306
3444.988388	462204.322417	51.126311
3444.272819	461745.090590	51.131316
3443.840564	461277.384905	51.136321
3442.810334	460822.545057	51.141325
3442.120823	460358.055571	51.146330
3441.536934	459905.459146	51.151335
3440.384148	459446.704341	51.156340
3440.078661	458997.189927	51.161345
3439.012287	458541.141602	51.166349
3438.623640	458088.781143	51.171354
3437.931284	457646.706311	51.176359
3437.305272	457173.769389	51.181364
3436.833507	456731.489222	51.186369
3436.045783	456265.508419	51.191373
3435.550624	455808.349609	51.196378
3434.738834	455361.124317	51.201383
3433.796076	454897.067301	51.206388
3432.877512	454445.122405	51.211393
3432.287144	453981.244444	51.216397
3431.694588	453533.034880	51.221402
3430.756744	453085.327662	51.226407
3429.893137	452631.206816	51.231412
3429.281866	452193.019956	51.236417
3428.599539	451751.385556	51.241421
3428.043084	451308.352702	51.246426
3427.095227	450862.582327	51.251431
3426.582935	450412.167531	51.256436
3425.888085	449969.282964	51.261441
3425.037327	449526.160824	51.266445
3424.575889	449085.455224	51.271450
3423.762821	448652.358197	51.276455
3423.215630	448201.043195	51.281460
3422.361111	447751.950270	51.286465
3421.388414	447317.635718	51.291469
3420.789454	446874.829345	51.296474
3420.234249	446442.970168	51.301479
3419.360755	446016.025691	51.306484
3418.493073	445577.754453	51.311489
3418.171133	445135.937495	51.316493
3417.681010	444702.361354	51.321498
3416.431708	444277.627504	51.326503
3415.363112	443836.462811	51.331508
3414.870760	443406.924113	51.336513
3414.245973	442992.880302	51.341517
3413.862759	442558.791604	51.346522
3413.271766	442131.225387	51.351527
3412.207364	441700.223871	51.356532
3411.531279	441276.260128	51.361537
3410.715915	440849.366704	51.366541
3410.418821	440421.876217	51.371546
3409.363183	440005.818932	51.376551
3408.565352	439568.848763	51.381556
3407.949274	439149.915305	51.386561
3407.028857	438733.485104	51.391565
3406.695291	438319.188939	51.396570
3406.022537	437893.414677	51.401575
3405.403046	437460.059827	51.406580
3404.427725	437056.912120	51.411585
3403.770054	436630.783858	51.416589
3403.313650	436205.454280	51.421594
3402.260069	435790.519095	51.426599
3401.772193	435372.060300	51.431604
3400.877517	434952.491033	51.436609
3400.272430	434542.948217	51.441613
3399.626449	434119.416010	51.446618
3398.818283	433706.794376	51.451623
3398.140548	433294.678623	51.456628
3397.232367	432881.704006	51.461633
3396.636963	432468.292423	51.466637
3395.971980	432050.492567	51.471642
3394.973386	431656.809614	51.476647
3394.520834	431245.666427	51.481652
3394.063506	430836.701187	51.486657
3392.980592	430427.447529	51.491661
3392.226338	430018.364007	51.496666
3391.428381	429624.872445	51.501671
3390.789374	429215.250265	51.506676
3390.115349	428830.843501	51.511681
3389.588171	428434.396351	51.516685
3389.340235	428015.500883	51.521690
3388.216585	427625.332229	51.526695
3387.531249	427208.727933	51.531700
3387.013423	426815.861246	51.536705
3385.994108	426418.598307	51.541709
3385.516786	426002.983527	51.546714
3384.678951	425606.086180	51.551719
3383.982938	425200.957161	51.556724
3383.309893	424808.822123	51.561729
3382.597876	424410.871362	51.566733
3382.132818	424004.240183	51.571738
3381.019457	423615.383112	51.576743
3380.453292	423222.725664	51.581748
3380.095683	422820.707905	51.586753
3378.990919	422417.913379	51.591757
3378.472569	422029.092068	51.596762
3377.444339	421635.672141	51.601767
3376.896916	421246.615785	51.606772
3376.409630	420853.149990	51.611777
3375.330761	420468.459599	51.616781
3374.895614	420075.431784	51.621786
3373.920422	419690.307821	51.626791
3373.309977	419296.788721	51.631796
3372.770717	418918.189978	51.636801
3371.873408	418534.384206	51.641805
3371.478933	418145.260483	51.646810
3370.475255	417768.548831	51.651815
3369.831358	417376.710324	51.656820
3369.345091	416992.844071	51.661825
3368.732741	416607.010970	51.666829
3368.044435	416222.048468	51.671834
3367.098537	415844.540088	51.676839
3366.223796	415465.541930	51.681844
3365.712081	415088.310668	51.686849
3365.150229	414710.167759	51.691853
3364.952208	414323.069812	51.696858
3363.413910	413947.485065	51.701863
3362.978960	413574.515891	51.706868
3362.421826	413196.530427	51.711873
3361.311284	412815.146608	51.716877
3360.986254	412428.780509	51.721882
3360.062990	412054.420918	51.726887
3359.428933	411675.005153	51.731892
3358.420081	411312.973393	51.736897
3357.892207	410941.637237	51.741901
3357.161226	410563.569350	51.746906
3356.257170	410204.455178	51.751911
3355.950732	409830.452873	51.756916
3355.389841	409472.470002	51.761921
3354.366237	409095.522582	51.766925
3354.051403	408722.549737	51.771930
3353.089103	408362.203028	51.776935
3352.404995	407986.255441	51.781940
3352.032529	407628.805480	51.786945
3351.118588	407261.652813	51.791949
3350.630443	406888.405370	51.796954
3349.751203	406529.752037	51.801959
3348.865622	406148.451401	51.806964
3348.534803	405787.085037	51.811969
3347.414997	405426.627084	51.816973
3347.023503	405058.501467	51.821978
3346.386555	404693.739743	51.826983
3345.718547	404325.115474	51.831988
3345.066084	403967.743731	51.836993
3344.442584	403596.231842	51.841997
3343.811215	403236.332234	51.847002
3343.002342	402875.236583	51.852007
3342.638653	402505.195798	51.857012
3341.482509	402142.011668	51.862017
3340.900039	401776.699254	51.867021
3340.365058	401408.401235	51.872026
3339.210232	401054.965099	51.877031
3338.670330	400684.016033	51.882036
3337.846691	400336.188000	51.887041
3337.569711	399975.255123	51.892045
3336.983539	399608.952763	51.897050
3335.954187	399253.672302	51.902055
3335.345064	398884.518404	51.907060
3334.990444	398529.580928	51.912065
3333.886751	398174.681808	51.917069
3333.462164	397806.833895	51.922074
3332.951204	397447.130330	51.927079
3332.005178	397088.076352	51.932084
3331.353230	396738.937313	51.937089
3330.678808	396373.883977	51.942093
3330.087513	396011.304891	51.947098
3329.211430	395655.758126	51.952103
3328.599989	395299.047140	51.957108
3327.972549	394944.445027	51.962113
3327.341643	394589.407543	51.967117
3326.643294	394231.554980	51.972122
3326.233761	393878.915727	51.977127
3325.432710	393516.012525	51.982132
3324.606919	393168.465750	51.987137
3324.028214	392806.485996	51.992141
3323.368162	392445.049222	51.997146
3322.215304	392086.407098	52.002151
3321.713816	391734.599408	52.007156
3321.333763	391374.022489	52.012161
3320.449872	391031.065469	52.017165
3319.800333	390679.041697	52.022170
3319.017167	390330.874925	52.027175
3318.445794	389966.067524	52.032180
3317.875805	389619.411035	52.037185
3317.045639	389279.861078	52.042189
3316.440257	388913.471706	52.047194
3315.389550	388572.856484	52.052199
3314.672329	388220.971511	52.057204
3314.200366	387876.367636	52.062209
3313.323720	387530.756457	52.067213
3312.959841	387179.263110	52.072218
3312.289901	386839.893527	52.077223
3311.350035	386490.162893	52.082228
3310.795959	386149.827652	52.087233
3310.136821	385808.030928	52.092237
3309.750937	385453.218511	52.097242
3308.583766	385121.565995	52.102247
3307.894046	384768.575135	52.107252
3307.753738	384429.404595	52.112257
3306.504674	384072.604659	52.117261
3305.923927	383732.251287	52.122266
3305.111295	383390.329304	52.127271
3304.477051	383042.501277	52.132276
3303.562748	382707.913451	52.137281
3303.056422	382376.894914	52.142285
3302.598081	382039.584108	52.147290
3301.530417	381703.383966	52.152295
3301.443620	381362.854749	52.157300
3300.545082	381020.238201	52.162305
3299.978206	380683.593799	52.167309
3299.628166	380335.899474	52.172314
3298.894904	379995.231440	52.177319
3298.131043	379654.768710	52.182324
3297.308462	379314.744654	52.187329
3296.550895	378974.249523	52.192333
3296.062934	378619.897815	52.197338
3295.089133	378288.943431	52.202343
3294.548266	377945.200289	52.207348
3293.841425	377608.831173	52.212353
3293.155426	377268.716890	52.217357
3292.754121	376927.918770	52.222362
3291.960044	376590.944359	52.227367
3291.432027	376243.572536	52.232372
3290.404971	375908.638671	52.237377
3289.542967	375575.329282	52.242381
3289.256178	375234.956499	52.247386
3288.784526	374899.595729	52.252391
3287.609812	374555.084263	52.257396
3287.178139	374221.136053	52.262401
3286.479040	373880.079454	52.267405
3285.997689	373541.732860	52.272410
3285.053553	373215.310778	52.277415
3284.501489	372868.397239	52.282420
3283.810186	372530.736957	52.287425
3282.959248	372197.194796	52.292429
3282.511306	371853.156317	52.297434
3281.569335	371528.246971	52.302439
3280.751431	371202.857582	52.307444
3280.412163	370871.233641	52.312449
3279.560684	370527.807815	52.317453
3279.117561	370188.512193	52.322458
3278.164614	369856.570348	52.327463
3277.666719	369519.338708	52.332468
3276.728508	369189.119292	52.337473
3276.006721	368871.812378	52.342477
3275.539834	368533.143433	52.347482
3274.785645	368197.290351	52.352487
3273.965047	367867.220330	52.357492
3273.496856	367541.925936	52.362497
3272.254883	367210.442004	52.367501
3271.858932	366891.415428	52.372506
3271.245660	366577.305770	52.377511
3270.705702	366231.786708	52.382516
3270.107453	365908.205462	52.387521
3269.084897	365586.393627	52.392525
3268.760349	365259.736735	52.397530
3268.147649	364943.529176	52.402535
3267.219315	364618.718688	52.407540
3266.909439	364295.767174	52.412545
3265.987765	363962.147568	52.417549
3265.358222	363631.023673	52.422554
3264.419918	363311.243255	52.427559
3263.754648	362980.527409	52.432564
3263.359599	362656.407370	52.437569
3262.319442	362336.712629	52.442573
3262.033062	362011.069672	52.447578
3261.336759	361682.512250	52.452583
3260.648752	361364.154592	52.457588
3259.707224	361037.946918	52.462593
3259.030651	360714.926616	52.467597
3258.555034	360397.851983	52.472602
3257.531573	360075.696443	52.477607
3257.120425	359764.637982	52.482612
3256.562026	359432.658835	52.487617
3255.781997	359112.799323	52.492621
3255.170740	358790.748065	52.497626
3254.309184	358475.579330	52.502631
3253.547750	358149.068997	52.507636
3252.780192	357828.053938	52.512641
3252.277851	357514.857909	52.517645
3251.910928	357190.568997	52.522650
3250.896361	356880.961650	52.527655
3250.687861	356565.092047	52.532660
3250.282882	356243.474924	52.537665
3248.993957	355917.185933	52.542669
3248.576573	355595.413917	52.547674
3248.029336	355278.215579	52.552679
3247.246868	354944.460235	52.557684
3246.663848	354629.655621	52.562689
3246.076862	354302.532606	52.567693
3245.538083	353983.288961	52.572698
3244.558813	353653.806229	52.577703
3243.942436	353326.987030	52.582708
3243.393585	353005.957492	52.587713
3242.226853	352689.986324	52.592717
3241.710944	352365.206575	52.597722
3241.144164	352049.238429	52.602727
3240.344217	351729.411452	52.607732
3239.397841	351410.216498	52.612737
3238.837828	351092.867263	52.617741
3238.444858	350777.169429	52.622746
3237.506558	350463.464772	52.627751
3236.828124	350144.779772	52.632756
3236.359354	349823.845513	52.637761
3235.804523	349510.685469	52.642765
3235.300637	349192.399917	52.647770
3234.620994	348880.630349	52.652775
3233.786866	348553.892646	52.657780
3233.086636	348247.416606	52.662785
3231.797884	347934.465461	52.667789
3231.540132	347612.415915	52.672794
3231.004190	347297.229612	52.677799
3230.673004	346989.110252	52.682804
3229.915147	346666.956217	52.687809
3229.139929	346351.522494	52.692813
3228.303986	346029.504447	52.697818
3227.631920	345716.443413	52.702823
3226.934869	345398.268628	52.707828
3226.079695	345090.247326	52.712833
3225.588044	344776.898111	52.717837
3225.128602	344452.673629	52.722842
3224.394704	344143.584541	52.727847
3223.489698	343823.881374	52.732852
3223.110579	343516.387332	52.737857
3222.298184	343200.484162	52.742861
3221.667939	342884.168691	52.747866
3220.402916	342566.450176	52.752871
3220.276529	342246.411713	52.757876
3219.781726	341938.520573	52.762881
3218.737813	341639.114657	52.767885
3218.072225	341325.825652	52.772890
3217.228896	341009.457698	52.777895
3216.650824	340707.046240	52.782900
3215.996345	340391.485236	52.787905
3215.388863	340078.664325	52.792909
3214.681631	339767.206741	52.797914
3213.971140	339461.959194	52.802919
3213.516206	339148.065829	52.807924
3212.738452	338834.781992	52.812929
3211.874584	338533.805282	52.817933
3211.667731	338216.278821	52.822938
3210.706314	337919.031180	52.827943
3209.713687	337614.735803	52.832948
3209.500271	337297.053108	52.837953
3208.579270	336992.947129	52.842957
3208.264190	336687.751082	52.847962
3207.000332	336385.580286	52.852967
3206.598191	336074.540185	52.857972
3205.957294	335773.897261	52.862977
3205.059080	335468.176872	52.867981
3204.697857	335158.347945	52.872986
3203.996995	334861.376202	52.877991
3203.441478	334546.407425	52.882996
3203.135320	334234.045295	52.888001
3202.366499	333923.155084	52.893005
3201.799166	333615.362861	52.898010
3200.556442	333308.465297	52.903015
3200.197008	332989.639719	52.908020
3199.616431	332691.824915	52.913025
3198.599377	332383.003699	52.918029
3198.075483	332068.196844	52.923034
3197.504095	331764.063072	52.928039
3196.586788	331457.691483	52.933044
3196.097691	331157.793641	52.938049
3195.685883	330845.687713	52.943053
3194.899523	330526.078493	52.948058
3194.071665	330230.176484	52.953063
3193.379242	329914.852247	52.958068
3192.723147	329605.783804	52.963073
3192.071583	329306.285944	52.968077
3191.560178	328999.788907	52.973082
3190.537793	328694.746253	52.978087
3189.462883	328386.528257	52.983092
3189.062218	328086.654866	52.988097
3188.396999	327788.298801	52.993101
3187.836320	327478.773719	52.998106
3187.106893	327185.466475	53.003111
3186.763380	326885.579353	53.008116
3185.974865	326573.769855	53.013121
3184.923582	326279.109823	53.018125
3184.689674	325977.445143	53.023130
3183.683484	325675.137689	53.028135
3182.961098	325371.842158	53.033140
3182.184685	325079.018253	53.038145
3181.856282	324775.225313	53.043149
3181.317585	324473.526816	53.048154
3180.512131	324173.549812	53.053159
3179.896914	323881.027083	53.058164
3179.096024	323571.626678	53.063169
3178.514624	323277.161442	53.068173
3178.004159	322971.888461	53.073178
3177.128052	322676.652990	53.078183
3176.464061	322375.934227	53.083188
3175.681684	322070.115407	53.088193
3175.193302	321772.473019	53.093197
3174.705971	321475.771515	53.098202
3174.003728	321183.125928	53.103207
3173.337369	320874.025445	53.108212
3172.732586	320567.664005	53.113217
3171.768765	320268.309394	53.118221
3171.311375	319959.121732	53.123226
3170.428714	319663.800705	53.128231
3170.006745	319367.922044	53.133236
3169.013327	319069.230144	53.138241
3168.339826	318785.534852	53.143245
3167.962490	318475.743849	53.148250
3167.155000	318177.758050	53.153255
3166.299601	317882.248744	53.158260
3165.937261	317584.496179	53.163265
3164.595335	317287.050441	53.168269
3164.497070	316989.075991	53.173274
3164.119056	316699.292983	53.178279
3163.210540	316392.074562	53.183284
3162.315899	316093.535855	53.188289
3161.839350	315802.085210	53.193293
3161.378169	315496.830254	53.198298
3160.493575	315200.782647	53.203303
3160.105168	314902.771376	53.208308
3159.228818	314608.146666	53.213313
3158.471388	314304.539155	53.218317
3157.928975	314008.688562	53.223322
3157.401227	313722.205399	53.228327
3156.449390	313413.762484	53.233332
3155.762258	313118.008646	53.238337
3154.872117	312824.756089	53.243341
3154.434251	312518.342734	53.248346
3153.374610	312228.629374	53.253351
3153.036593	311943.384583	53.258356
3152.309691	311642.234599	53.263361
3151.778464	311352.231590	53.268365
3151.022815	311055.489849	53.273370
3150.148873	310763.655177	53.278375
3149.887573	310468.310592	53.283380
3149.035921	310176.827378	53.288385
3148.235053	309882.941725	53.293389
3147.870152	309577.196260	53.298394
3146.986898	309298.880995	53.303399
3146.307724	309001.281491	53.308404
3145.921622	308698.618314	53.313409
3144.892451	308414.034265	53.318413
3144.128603	308114.637945	53.323418
3143.587412	307830.331819	53.328423
3142.971203	307528.949901	53.333428
3142.379020	307242.333170	53.338433
3141.251359	306952.286322	53.343437
3141.099044	306653.553652	53.348442
3140.317519	306367.092210	53.353447
3139.568956	306083.120508	53.358452
3139.082225	305782.656150	53.363457
3138.056489	305496.129556	53.368461
3137.609177	305201.005357	53.373466
3136.551483	304915.552111	53.378471
3136.327175	304621.078913	53.383476
3135.538117	304338.510476	53.388481
3134.607156	304053.697465	53.393485
3134.054399	303764.265660	53.398490
3133.540051	303464.640870	53.403495
3133.023936	303187.909493	53.408500
3132.243163	302901.669755	53.413505
3131.406504	302606.015899	53.418509
3130.268658	302313.897937	53.423514
3129.644058	302041.154218	53.428519
3129.513109	301758.094527	53.433524
3128.751932	301476.942118	53.438529
3127.630431	301192.943059	53.443533
3127.460543	300912.052569	53.448538
3126.696142	300635.177443	53.453543
3125.793054	300351.829865	53.458548
3125.186617	300056.032727	53.463553
3124.715847	299787.080616	53.468557
3124.173755	299495.474217	53.473562
3123.306395	299223.706219	53.478567
3122.742176	298934.063242	53.483572
3122.141263	298650.766742	53.488577
3121.444200	298376.754827	53.493581
3120.841124	298087.906010	53.498586
3119.900125	297802.089786	53.503591
3119.075366	297518.241106	53.508596
3118.831229	297240.641321	53.513601
3117.899237	296960.781538	53.518605
3117.365849	296668.048422	53.523610
3116.796995	296398.113320	53.528615
3116.386992	296102.201891	53.533620
3115.423373	295820.409900	53.538625
3114.588982	295549.318654	53.543629
3114.322966	295260.692167	53.548634
3113.584633	294977.309811	53.553639
3112.664753	294689.906509	53.558644
3111.915610	294407.136269	53.563649
3111.357868	294129.887196	53.568653
3110.871895	293835.461491	53.573658
3110.135841	293561.295948	53.578663
3109.321558	293280.011591	53.583668
3108.742401	292992.297367	53.588673
3107.922609	292717.481857	53.593677
3107.441050	292424.607048	53.598682
3106.438051	292150.201849	53.603687
3105.923297	291868.486308	53.608692
3105.449581	291594.684319	53.613697
3104.483283	291310.161742	53.618701
3104.293707	291028.266412	53.623706
3103.620562	290758.620777	53.628711
3103.044751	290466.522503	53.633716
3102.355808	290185.469275	53.638721
3101.376929	289896.693992	53.643725
3100.951432	289604.800170	53.648730
3100.247153	289329.325880	53.653735
3099.675407	289041.835042	53.658740
3098.808751	288757.956062	53.663745
3098.112216	288477.717239	53.668749
3097.923637	288191.183619	53.673754
3096.816139	287915.517095	53.678759
3095.745563	287630.013888	53.683764
3095.342561	287345.117876	53.688769
3094.801669	287072.799100	53.693773
3094.175830	286794.712321	53.698778
3093.029871	286518.031950	53.703783
3092.672381	286234.910524	53.708788
3092.205523	285955.244351	53.713793
3091.389319	285675.200286	53.718797
3091.113916	285388.932631	53.723802
3090.054904	285118.196926	53.728807
3089.093288	284831.222465	53.733812
3089.054489	284557.065007	53.738817
3088.258888	284278.672084	53.743821
3087.343904	283996.197503	53.748826
3086.582490	283717.162096	53.753831
3086.136232	283441.056412	53.758836
3085.396666	283161.762520	53.763841
3084.541177	282882.614148	53.768845
3084.191755	282609.421488	53.773850
3083.036423	282323.749459	53.778855
3082.607285	282056.452270	53.783860
3081.856244	281774.383386	53.788865
3080.962645	281505.045568	53.793869
3080.520411	281229.829434	53.798874
3080.077097	280957.516727	53.803879
3079.525132	280681.910221	53.808884
3078.907175	280402.137244	53.813889
3077.958092	280116.533380	53.818893
3077.747330	279832.773619	53.823898
3076.452945	279557.156822	53.828903
3075.800984	279287.270508	53.833908
3075.489593	279012.694974	53.838913
3074.416106	278736.355306	53.843917
3073.652838	278449.549912	53.848922
3073.251852	278175.650492	53.853927
3072.297592	277895.446007	53.858932
3071.802202	277620.670002	53.863937
3070.807312	277354.071928	53.868941
3070.268246	277085.517005	53.873946
3069.797737	276815.983388	53.878951
3069.198244	276550.621487	53.883956
3068.309889	276272.876696	53.888961
3067.755442	275994.824341	53.893965
3067.431032	275732.449545	53.898970
3066.364741	275456.693892	53.903975
3065.732052	275186.116087	53.908980
3065.115712	274913.498210	53.913985
3064.557256	274652.281002	53.918989
3063.889762	274370.706334	53.923994
3063.197689	274109.968701	53.928999
3062.596087	273839.029399	53.934004
3061.944658	273562.800569	53.939009
3060.870742	273295.527087	53.944013
3060.358030	273024.370017	53.949018
3059.985885	272756.730831	53.954023
3059.353165	272478.690878	53.959028
3058.623347	272208.918084	53.964033
3057.664809	271942.976315	53.969037
3057.302713	271671.489962	53.974042
3056.545435	271401.059469	53.979047
3055.679273	271131.512187	53.984052
3055.140294	270860.436018	53.989057
3054.396591	270590.920415	53.994061
3053.847125	270316.178597	53.999066
3052.884464	270059.075400	54.004071
3052.467824	269788.846074	54.009076
3052.062011	269519.888533	54.014081
3051.175881	269257.934478	54.019085
3050.994205	268970.629933	54.024090
3049.846991	268710.449230	54.029095
3049.167698	268443.751090	54.034100
3048.667168	268169.384281	54.039105
3047.912299	267888.461562	54.044109
3047.392675	267623.470329	54.049114
3046.600331	267361.476692	54.054119
3045.914703	267079.168108	54.059124
3045.333339	266811.181769	54.064129
3044.371062	266552.984703	54.069133
3043.971600	266270.045486	54.074138
3042.944907	266005.339038	54.079143
3042.316476	265742.428877	54.084148
3041.726369	265474.470105	54.089153
3041.409716	265211.230750	54.094157
3040.505005	264936.547569	54.099162
3039.938734	264680.453645	54.104167
3039.119259	264414.849422	54.109172
3038.418283	264147.673066	54.114177
3037.391538	263883.757424	54.119181
3036.899471	263617.490681	54.124186
3036.487635	263362.188140	54.129191
3035.833508	263098.519686	54.134196
3035.136821	262836.870132	54.139201
3034.491624	262569.151249	54.144205
3033.849325	262293.893606	54.149210
3033.159461	262035.809091	54.154215
3032.533618	261768.444332	54.159220
3031.822133	261502.748761	54.164225
3030.746315	261245.133452	54.169229
3030.028623	260968.666417	54.174234
3029.490337	260715.066794	54.179239
3028.786844	260442.341763	54.184244
3028.238322	260191.010844	54.189249
3027.469793	259932.915082	54.194253
3027.239908	259670.175579	54.199258
3026.523447	259420.909345	54.204263
3025.625021	259158.989242	54.209268
3025.210394	258894.114978	54.214273
3024.010555	258631.428140	54.219277
3023.330337	258361.986815	54.224282
3023.073566	258106.562314	54.229287
3022.205265	257843.212593	54.234292
3021.546658	257580.797729	54.239297
3020.811329	257334.312468	54.244301
3020.515161	257062.876247	54.249306
3019.738358	256816.143415	54.254311
3019.175430	256555.802869	54.259316
3018.359070	256292.675857	54.264321
3018.042790	256034.690801	54.269325
3017.271840	255762.083375	54.274330
3016.167147	255509.953870	54.279335
3015.956092	255240.823895	54.284340
3015.119521	254976.810309	54.289345
3014.578397	254721.332731	54.294349
3014.115886	254446.437056	54.299354
3013.269698	254197.018663	54.304359
3012.527137	253924.358195	54.309364
3011.842342	253658.819729	54.314369
3010.804457	253411.546428	54.319373
3010.365526	253143.855982	54.324378
3009.779638	252884.949801	54.329383
3008.933011	252619.845852	54.334388
3008.313083	252360.792977	54.339393
3007.583351	252104.711999	54.344397
3007.057387	251844.626304	54.349402
3006.291370	251588.016993	54.354407
3005.621772	251328.540516	54.359412
3005.203765	251072.717265	54.364417
3004.383674	250813.520035	54.369421
3003.374207	250561.152757	54.374426
3003.072899	250298.869124	54.379431
3002.570680	250035.649970	54.384436
3001.712254	249778.421308	54.389441
3000.550047	249537.972597	54.394445
3000.472380	249273.108531	54.399450
2999.618428	249014.174109	54.404455
2998.720291	248761.002492	54.409460
2998.390318	248501.171037	54.414465
2997.551991	248250.129939	54.419469
2997.033549	247988.826656	54.424474
2996.272564	247732.910104	54.429479
2995.943225	247485.380409	54.434484
2995.114945	247226.088366	54.439489
2994.350808	246973.076730	54.444493
2993.707240	246710.242029	54.449498
2992.740111	246457.594464	54.454503
2992.166596	246196.506745	54.459508
2991.854121	245949.944651	54.464513
2990.944427	245687.892434	54.469517
2990.066114	245437.600921	54.474522
2989.502713	245186.445100	54.479527
2989.075963	244925.693002	54.484532
2988.414079	244673.000291	54.489537
2987.302613	244431.584071	54.494541
2987.101858	244163.387160	54.499546
2986.601956	243913.191306	54.504551
2985.225780	243658.448990	54.509556
2984.921535	243412.705022	54.514561
2984.378419	243163.663364	54.519565
2983.440662	242900.704202	54.524570
2982.987514	242655.392674	54.529575
2981.957582	242399.019160	54.534580
2981.483410	242142.048883	54.539585
2981.085902	241903.911163	54.544589
2980.596144	241652.903183	54.549594
2979.600550	241394.998373	54.554599
2978.902562	241135.289910	54.559604
2978.435863	240881.529631	54.564609
2977.675003	240629.420732	54.569613
2977.065880	240377.008226	54.574618
2976.098569	240126.129907	54.579623
2975.372891	239874.984683	54.584628
2974.991069	239621.952108	54.589633
2973.904902	239385.303435	54.594637
2973.451418	239131.111895	54.599642
2972.752356	238887.603933	54.604647
2971.799569	238636.853832	54.609652
2971.619001	238387.968256	54.614657
2970.807342	238142.264310	54.619661
2970.252575	237885.137720	54.624666
2969.783240	237638.591295	54.629671
2968.874240	237382.718758	54.634676
2968.265595	237136.602930	54.639681
2967.778802	236898.234887	54.644685
2966.953750	236638.811301	54.649690
2965.914510	236389.836975	54.654695
2965.475524	236145.275300	54.659700
2965.386230	235892.459493	54.664705
2964.006908	235640.994375	54.669709
2963.897971	235395.872905	54.674714
2962.895675	235147.099359	54.679719
2962.134634	234898.593779	54.684724
2961.649960	234645.079669	54.689729
2960.612083	234399.165466	54.694733
2960.241717	234152.840623	54.699738
2959.417435	233901.801140	54.704743
2958.757453	233656.618275	54.709748
2958.189248	233409.868229	54.714753
2957.537492	233168.632049	54.719757
2957.333230	232914.084839	54.724762
2956.702777	232675.265479	54.729767
2955.788644	232421.035632	54.734772
2954.929355	232171.381077	54.739777
2954.323492	231924.335175	54.744781
2953.725275	231663.818929	54.749786
2953.184233	231423.257045	54.754791
2952.165436	231173.783118	54.759796
2951.765400	230929.584480	54.764801
2951.173518	230680.935461	54.769805
2950.833682	230433.189309	54.774810
2949.803079	230184.611070	54.779815
2949.421539	229928.801322	54.784820
2948.701767	229674.675411	54.789825
2947.704788	229419.957543	54.794829
2947.011111	229166.669168	54.799834
2946.369725	228923.074227	54.804839
2945.826191	228668.694083	54.809844
2945.271299	228423.329939	54.814849
2944.175234	228163.666272	54.819853
2943.732668	227915.230347	54.824858
2942.959149	227675.759073	54.829863
2942.534903	227421.643713	54.834868
2941.934379	227176.086586	54.839873
2941.193125	226930.628820	54.844877
2940.505117	226674.495043	54.849882
2939.888427	226430.750356	54.854887
2938.915689	226174.739542	54.859892
2938.221461	225930.575727	54.864897
2937.414438	225686.443208	54.869901
2937.002777	225433.477522	54.874906
2936.109192	225197.558551	54.879911
2935.588427	224951.015008	54.884916
2935.147399	224705.987218	54.889921
2934.349563	224464.364720	54.894925
2933.674955	224211.329835	54.899930
2932.877753	223972.547545	54.904935
2932.576519	223721.912008	54.909940
2932.102153	223475.085517	54.914945
2931.073663	223232.408422	54.919949
2930.502263	222980.659535	54.924954
2929.301675	222740.251682	54.929959
2928.779714	222501.251989	54.934964
2928.310038	222240.412868	54.939969
2927.620457	222005.081991	54.944973
2927.164831	221755.750110	54.949978
2926.386626	221519.785511	54.954983
2925.577480	221263.878941	54.959988
2925.088958	221029.728530	54.964993
2924.143210	220785.989372	54.969997
2923.818262	220539.810446	54.975002
2922.884870	220294.390592	54.980007
2922.211060	220055.397072	54.985012
2921.651623	219803.885785	54.990017
2920.943020	219567.814395	54.995021
2920.269903	219319.594224	55.000026
2919.439286	219084.943929	55.005031
2919.171596	218840.301792	55.010036
2918.603425	218593.225822	55.015041
2917.654672	218364.846639	55.020045
2917.247090	218113.406176	55.025050
2916.242778	217870.245949	55.030055
2915.652969	217620.045328	55.035060
2915.055877	217375.842149	55.040065
2914.152286	217140.866002	55.045069
2913.536042	216892.912427	55.050074
2912.667226	216656.328515	55.055079
2911.929226	216418.871844	55.060084
2911.527438	216181.388200	55.065089
2910.721280	215951.390315	55.070093
2909.952466	215715.251980	55.075098
2909.297908	215480.000101	55.080103
2908.410425	215243.385739	55.085108
2907.973471	214998.058070	55.090113
2907.321125	214770.190905	55.095117
2907.016397	214543.275020	55.100122
2906.200851	214310.534713	55.105127
2905.597717	214075.572266	55.110132
2904.952797	213830.803595	55.115137
2904.134343	213593.038470	55.120141
2903.480868	213354.942585	55.125146
2902.946629	213114.588480	55.130151
2902.005705	212882.751224	55.135156
2901.745212	212634.858544	55.140161
2900.808871	212403.658653	55.145165
2900.321682	212161.378600	55.150170
2899.303796	211928.309527	55.155175
2899.061350	211696.582233	55.160180
2898.510571	211452.329300	55.165185
2897.620608	211220.871693	55.170189
2897.154078	210969.377755	55.175194
2896.366048	210736.034745	55.180199
2895.285651	210500.664241	55.185204
2894.734049	210265.885450	55.190209
2894.005264	210037.983102	55.195213
2893.521252	209792.834979	55.200218
2892.913817	209568.287947	55.205223
2892.319936	209331.406528	55.210228
2891.669614	209086.758409	55.215233
2890.520099	208853.441399	55.220237
2889.879145	208616.048318	55.225242
2889.626952	208390.940171	55.230247
2888.840322	208157.453773	55.235252
2888.337864	207919.494162	55.240257
2887.465235	207686.481354	55.245261
2887.085582	207450.922297	55.250266
2886.056328	207216.357910	55.255271
2885.644114	206989.803896	55.260276
2884.897242	206752.218449	55.265281
2884.154152	206514.582430	55.270285
2883.779362	206284.283399	55.275290
2883.011792	206045.304057	55.280295
2882.282789	205810.926690	55.285300
2881.772077	205573.550334	55.290305
2880.987083	205339.565498	55.295309
2880.404496	205094.502754	55.300314
2879.469048	204868.535985	55.305319
2878.803302	204628.477203	55.310324
2878.744598	204395.131993	55.315329
2877.326221	204166.660915	55.320333
2877.072477	203924.427195	55.325338
2876.274400	203690.781917	55.330343
2875.977522	203454.665668	55.335348
2874.936846	203220.551659	55.340353
2874.111267	202996.458282	55.345357
2873.952558	202753.310881	55.350362
2872.915308	202524.747803	55.355367
2872.234285	202289.626205	55.360372
2871.618566	202050.728338	55.365377
2870.483948	201827.299364	55.370381
2870.140063	201588.704015	55.375386
2869.549826	201363.523589	55.380391
2868.764005	201129.670576	55.385396
2868.575636	200906.273606	55.390401
2867.692401	200660.590295	55.395405
2867.030527	200429.278475	55.400410
2866.310437	200209.926197	55.405415
2865.592402	199975.494677	55.410420
2865.034274	199728.173351	55.415425
2864.108223	199507.074930	55.420429
2863.347916	199273.696602	55.425434
2862.859958	199046.740625	55.430439
2862.092312	198815.045180	55.435444
2861.332600	198589.610290	55.440449
2860.382717	198352.995572	55.445453
2860.205704	198134.481895	55.450458
2859.284252	197907.739344	55.455463
2858.640576	197680.444771	55.460468
2858.537819	197450.253294	55.465473
2857.649892	197229.450888	55.470477
2856.964268	196995.154469	55.475482
2856.249259	196763.166934	55.480487
2855.323344	196530.004972	55.485492
2855.064877	196296.929224	55.490497
2854.163889	196081.465356	55.495501
2853.632517	195847.264167	55.500506
2852.686320	195624.072813	55.505511
2851.959029	195398.137445	55.510516
2851.489428	195172.442196	55.515521
2850.787960	194943.310905	55.520525
2850.388411	194713.560233	55.525530
2849.518934	194486.328063	55.530535
2848.942541	194258.630595	55.535540
2848.578830	194028.152054	55.540545
2847.431938	193810.446309	55.545549
2846.693221	193578.565930	55.550554
2846.070721	193345.141339	55.555559
2845.339956	193127.690743	55.560564
2844.875643	192897.182403	55.565569
2844.174323	192686.167325	55.570573
2843.764671	192445.307975	55.575578
2843.084112	192226.161097	55.580583
2841.999188	191992.777883	55.585588
2841.674035	191767.558484	55.590593
2840.516087	191545.920062	55.595597
2840.421618	191306.377756	55.600602
2839.533426	191095.653523	55.605607
2838.832469	190870.281450	55.610612
2838.427682	190642.878688	55.615617
2837.503058	190412.403957	55.620621
2837.129309	190179.565640	55.625626
2835.995218	189962.803594	55.630631
2835.364694	189740.377369	55.635636
2835.064505	189508.243129	55.640641
2834.174175	189294.524447	55.645645
2833.758216	189063.288573	55.650650
2832.948530	188833.871915	55.655655
2832.223306	188620.766241	55.660660
2831.805105	188382.231183	55.665665
2831.048280	188157.796701	55.670669
2830.573807	187927.669763	55.675674
2829.772730	187709.185849	55.680679
2829.215188	187470.741075	55.685684
2828.720001	187239.882882	55.690689
2827.578922	187018.720725	55.695693
2826.999428	186790.244452	55.700698
2826.376875	186562.755728	55.705703
2825.717278	186350.451460	55.710708
2824.911632	186107.447551	55.715713
2824.109197	185884.786857	55.720717
2823.859437	185661.352729	55.725722
2822.910430	185442.813845	55.730727
2822.390348	185207.517079	55.735732
2821.951597	184974.358616	55.740737
2821.009381	184763.823873	55.745741
2820.385399	184541.077848	55.750746
2819.823667	184311.580639	55.755751
2819.283541	184086.520969	55.760756
2818.564857	183856.720169	55.765761
2817.821800	183641.808384	55.770765
2817.044949	183408.813304	55.775770
2816.522622	183186.414069	55.780775
2815.651895	182960.865386	55.785780
2815.222243	182724.676759	55.790785
2814.336555	182513.622040	55.795789
2814.080694	182279.952461	55.800794
2813.402518	182046.783510	55.805799
2812.626124	181815.666679	55.810804
2811.902752	181591.780781	55.815809
2810.908684	181374.273807	55.820813
2810.366166	181137.793529	55.825818
2809.501982	180923.193974	55.830823
2808.889765	180696.585571	55.835828
2808.571374	180469.499319	55.840833
2807.604930	180254.906537	55.845837
2807.086400	180022.422723	55.850842
2806.400954	179802.228910	55.855847
2805.817144	179581.740283	55.860852
2804.981344	179355.683125	55.865857
2804.358359	179139.133491	55.870861
2804.021129	178901.564446	55.875866
2803.099755	178677.953940	55.880871
2802.049932	178458.753300	55.885876
2801.645852	178237.454513	55.890881
2800.963057	178018.337937	55.895885
2800.375405	177796.790695	55.900890
2799.714095	177570.957065	55.905895
2799.195310	177345.852524	55.910900
2798.483026	177124.201367	55.915905
2797.714204	176909.492398	55.920909
2797.276903	176684.391225	55.925914
2796.498620	176458.836503	55.930919
2795.692558	176243.259236	55.935924
2795.342727	176016.646960	55.940929
2794.538941	175789.446431	55.945933
2794.153002	175557.716616	55.950938
2793.342232	175331.664421	55.955943
2792.467630	175116.053017	55.960948
2792.030562	174895.044287	55.965953
2791.095649	174666.280888	55.970957
2790.875203	174444.566191	55.975962
2789.643763	174224.869735	55.980967
2789.183042	174000.041315	55.985972
2788.697094	173768.095827	55.990977
2787.784780	173545.439991	55.995981
2787.198766	173313.970817	56.000986
2786.688168	173098.604979	56.005991
2786.004677	172877.544520	56.010996
2785.524126	172656.338674	56.016001
2784.504464	172433.260868	56.021005
2784.069991	172199.561191	56.026010
2783.389580	171978.899468	56.031015
2782.280028	171752.240564	56.036020
2782.316222	171535.321286	56.041025
2781.342952	171306.862866	56.046029
2780.558286	171083.602810	56.051034
2779.958703	170863.939184	56.056039
2779.462749	170639.669387	56.061044
2778.692536	170409.645205	56.066049
2777.846688	170182.762800	56.071053
2777.195797	169958.368836	56.076058
2776.357601	169749.507998	56.081063
2775.669153	169531.023189	56.086068
2775.105154	169300.311601	56.091073
2774.476422	169083.930869	56.096077
2773.785044	168861.088405	56.101082
2773.111411	168644.742678	56.106087
2772.561323	168426.979764	56.111092
2771.864942	168199.144265	56.116097
2770.517612	167983.443069	56.121101
2770.531435	167762.021263	56.126106
2770.036922	167549.493717	56.131111
2769.156755	167335.044695	56.136116
2768.703150	167112.810554	56.141121
2767.678915	166881.156401	56.146125
2767.025635	166668.035841	56.151130
2766.695286	166454.267679	56.156135
2766.060642	166234.330825	56.161140
2765.250928	166017.080605	56.166145
2764.204395	165806.036319	56.171149
2763.992281	165576.855575	56.176154
2763.356405	165364.477157	56.181159
2762.595243	165142.328794	56.186164
2762.010670	164925.901192	56.191169
2761.379097	164707.651272	56.196173
2760.610057	164485.495364	56.201178
2759.583939	164266.255163	56.206183
2759.249886	164053.734708	56.211188
2758.528862	163823.704459	56.216193
2757.818655	163618.849741	56.221197
2757.205914	163399.180484	56.226202
2756.628666	163183.664695	56.231207
2755.924732	162958.621403	56.236212
2755.464720	162734.227457	56.241217
2754.507908	162524.014161	56.246221
2754.106837	162304.139953	56.251226
2753.315597	162083.591437	56.256231
2752.742812	161865.755981	56.261236
2752.248150	161642.887284	56.266241
2751.381489	161432.119325	56.271245
2750.844247	161215.223021	56.276250
2750.440935	160923.217164	56.281255
2749.689125	160697.114816	56.286260
2749.134751	160468.414401	56.291265
2748.160406	160255.890456	56.296269
2747.510308	160019.249196	56.301274
2746.891667	159800.429152	56.306279
2746.240850	159580.000921	56.311284
2745.430640	159349.250474	56.316289
2744.576381	159148.105483	56.321293
2744.014745	158926.675544	56.326298
2743.434624	158705.555044	56.331303
2742.751259	158481.591808	56.336308
2742.254462	158265.813150	56.341313
2741.568727	158042.933709	56.346317
2740.917260	157820.393511	56.351322
2739.821234	157607.256438	56.356327
2739.346848	157385.873264	56.361332
2738.625896	157162.242259	56.366337
2737.816589	156959.170388	56.371341
2737.461050	156732.115411	56.376346
2736.831789	156519.406871	56.381351
2736.374744	156295.065899	56.386356
2735.870932	156076.746743	56.391361
2734.871749	155859.854945	56.396365
2734.287181	155632.335002	56.401370
2733.463143	155410.714789	56.406375
2732.598590	155187.538850	56.411380
2732.274848	154971.511800	56.416385
2731.266541	154756.535241	56.421389
2730.814881	154539.183739	56.426394
2730.198774	154318.567347	56.431399
2729.330673	154102.695611	56.436404
2728.997744	153888.647208	56.441409
2727.934209	153664.228941	56.446413
2727.549571	153449.848303	56.451418
2726.781023	153226.695496	56.456423
2726.099108	153017.067891	56.461428
2725.596307	152792.261551	56.466433
2724.855881	152585.061035	56.471437
2723.999842	152361.050794	56.476442
2723.218095	152140.309697	56.481447
2722.494100	151929.640582	56.486452
2722.115732	151718.384200	56.491457
2721.496896	151511.425322	56.496461
2721.077317	151283.934040	56.501466
2719.923452	151073.122390	56.506471
2719.244555	150854.585191	56.511476
2718.772550	150631.008807	56.516481
2717.845103	150424.626760	56.521485
2717.683677	150203.825752	56.526490
2717.074319	149992.617023	56.531495
2716.072106	149777.430121	56.536500
2715.519598	149562.554695	56.541505
2714.635478	149351.622419	56.546509
2714.413901	149132.592137	56.551514
2713.407362	148920.220437	56.556519
2712.363412	148702.861202	56.561524
2712.123450	148482.745201	56.566529
2711.353576	148270.581754	56.571533
2711.006766	148057.526578	56.576538
2710.560808	147833.571304	56.581543
2709.492145	147620.341067	56.586548
2709.153306	147400.883581	56.591553
2708.240904	147191.342484	56.596557
2707.759493	146972.660350	56.601562
2707.301625	146753.556593	56.606567
2706.167097	146538.208936	56.611572
2705.801180	146308.189619	56.616577
2704.755852	146101.841191	56.621581
2704.120690	145871.943942	56.626586
2703.468697	145656.856246	56.631591
2702.838125	145443.304320	56.636596
2702.213240	145236.246814	56.641601
2701.560375	145023.756042	56.646605
2701.109769	144798.729993	56.651610
2700.273323	144592.523556	56.656615
2699.487978	144370.578094	56.661620
2698.997356	144148.295238	56.666625
2698.480588	143942.347431	56.671629
2697.379997	143721.028375	56.676634
2696.913111	143506.853756	56.681639
2696.288747	143297.801224	56.686644
2695.874873	143075.056409	56.691649
2694.991068	142870.813095	56.696653
2694.072573	142641.734206	56.701658
2693.828092	142437.989703	56.706663
2692.944155	142222.644757	56.711668
2692.570318	142009.113827	56.716673
2691.571236	141787.004718	56.721677
2691.058587	141567.323368	56.726682
2690.137304	141350.071758	56.731687
2689.702222	141140.622690	56.736692
2689.063829	140924.574527	56.741697
2688.008741	140728.847784	56.746701
2687.641621	140500.764886	56.751706
2686.986799	140292.639797	56.756711
2685.886816	140081.270384	56.761716
2685.735674	139858.850409	56.766721
2684.965009	139655.728789	56.771725
2684.440308	139434.222417	56.776730
2683.755821	139221.992731	56.781735
2683.055601	139015.357500	56.786740
2682.530992	138794.986622	56.791745
2681.438648	138580.920259	56.796749
2680.845707	138367.818145	56.801754
2680.199510	138158.016645	56.806759
2679.283757	137953.290566	56.811764
2678.609124	137736.877152	56.816769
2678.092717	137538.722698	56.821773
2677.417492	137318.183311	56.826778
2676.666861	137111.226226	56.831783
2676.264702	136910.504206	56.836788
2675.852010	136695.543343	56.841793
2675.084680	136496.914728	56.846797
2674.767954	136270.583912	56.851802
2674.114294	136056.415450	56.856807
2673.202914	135841.997184	56.861812
2672.529968	135614.279579	56.866817
2671.737970	135409.017963	56.871821
2671.236662	135187.412546	56.876826
2670.671176	134973.072887	56.881831
2669.875837	134765.974262	56.886836
2669.555727	134539.136518	56.891841
2668.608849	134335.774441	56.896845
2668.186221	134115.155603	56.901850
2667.177986	133893.411703	56.906855
2666.291082	133681.635073	56.911860
2665.680393	133462.842174	56.916865
2665.295225	133260.986562	56.921869
2664.794103	133041.036225	56.926874
2664.003657	132824.702934	56.931879
2663.163383	132612.151909	56.936884
2662.830280	132389.309106	56.941889
2661.524737	132182.729056	56.946893
2660.902711	131968.573107	56.951898
2660.544183	131752.179493	56.956903
2659.501638	131549.182563	56.961908
2659.084091	131337.285387	56.966913
2658.289818	131128.701237	56.971917
2657.604954	130912.899210	56.976922
2657.027369	130703.166079	56.981927
2656.207256	130501.043254	56.986932
2655.927780	130287.582427	56.991937
2654.930050	130079.660643	56.996941
2654.582766	129875.206488	57.001946
2653.641060	129656.025340	57.006951
2653.012124	129461.221166	57.011956
2652.389428	129247.530485	57.016961
2651.700724	129038.233819	57.021965
2651.357843	128822.723878	57.026970
2650.357132	128605.541688	57.031975
2649.739896	128399.959888	57.036980
2649.138182	128194.770874	57.041985
2648.178273	127984.369321	57.046989
2647.470132	127783.175547	57.051994
2646.985177	127567.177123	57.056999
2646.206626	127363.216138	57.062004
2645.898732	127162.039667	57.067009
2645.120415	126950.817083	57.072013
2644.676219	126733.472496	57.077018
2643.660896	126529.085295	57.082023
2642.873080	126317.183281	57.087028
2642.252342	126120.750288	57.092033
2641.808915	125917.356522	57.097037
2641.232730	125708.156144	57.102042
2640.235353	125497.385858	57.107047
2639.715877	125284.052377	57.112052
2639.210451	125076.483868	57.117057
2638.466266	124883.444685	57.122061
2637.962883	124665.871934	57.127066
2637.243248	124455.776871	57.132071
2636.305971	124255.902536	57.137076
2635.736714	124032.478367	57.142081
2634.737917	123845.950674	57.147085
2634.521008	123637.814126	57.152090
2633.685568	123434.640770	57.157095
2633.581479	123224.775224	57.162100
2632.808175	122999.804639	57.167105
2631.508178	122812.392163	57.172109
2631.296508	122588.783646	57.177114
2630.512595	122373.623041	57.182119
2629.658097	122186.791966	57.187124
2629.242040	121966.547931	57.192129
2628.886364	121769.926820	57.197133
2628.180010	121554.900212	57.202138
2627.201902	121350.965352	57.207143
2626.520319	121133.017781	57.212148
2625.801539	120934.327211	57.217153
2625.259343	120729.743981	57.222157
2625.032494	120511.551713	57.227162
2623.962868	120300.402035	57.232167
2622.961861	120098.512013	57.237172
2622.763366	119878.250881	57.242177
2622.185058	119686.898982	57.247181
2621.167298	119475.823894	57.252186
2620.782495	119266.148413	57.257191
2620.094534	119055.411703	57.262196
2619.499139	118835.882445	57.267201
2618.675213	118646.887826	57.272205
2617.943808	118429.668882	57.277210
2617.600854	118220.128485	57.282215
2616.408526	118013.238184	57.287220
2616.099456	117802.051656	57.292225
2615.433660	117593.627586	57.297229
2614.740856	117385.882348	57.302234
2614.022578	117173.972307	57.307239
2613.467828	116970.899562	57.312244
2612.792642	116759.747827	57.317249
2611.618272	116555.284836	57.322253
2611.110913	116352.120596	57.327258
2610.755969	116143.176580	57.332263
2609.652691	115942.344356	57.337268
2609.291067	115726.549495	57.342273
2608.703519	115521.639957	57.347277
2608.041245	115333.107372	57.352282
2607.167086	115122.248213	57.357287
2606.437764	114923.376842	57.362292
2606.264509	114708.963482	57.367297
2604.945610	114510.398228	57.372301
2604.620308	114295.568153	57.377306
2604.008140	114102.847674	57.382311
2602.911485	113888.936663	57.387316
2602.699550	113697.298310	57.392321
2602.152928	113488.920570	57.397325
2601.679431	113273.513364	57.402330
2600.767034	113081.051364	57.407335
2600.121962	112874.077915	57.412340
2599.439045	112654.018966	57.417345
2598.452310	112469.830465	57.422349
2598.286972	112254.141997	57.427354
2597.572784	112052.555492	57.432359
2596.705241	111850.036599	57.437364
2595.683916	111628.371181	57.442369
2595.449772	111430.794376	57.447373
2594.761238	111223.067230	57.452378
2593.707663	111027.654305	57.457383
2593.287794	110825.377431	57.462388
2592.681622	110613.612489	57.467393
2591.991956	110426.491838	57.472397
2591.222745	110209.615841	57.477402
2590.412892	110007.166307	57.482407
2589.763937	109820.005725	57.487412
2589.576734	109605.409850	57.492417
2588.286183	109416.374092	57.497421
2588.103946	109195.517651	57.502426
2587.595601	109002.204628	57.507431
2586.632409	108804.510534	57.512436
2586.308214	108586.848573	57.517441
2585.202164	108398.127754	57.522445
2584.690155	108181.463698	57.527450
2584.114846	107978.974703	57.532455
2583.131957	107786.647559	57.537460
2582.698264	107581.493385	57.542465
2581.806686	107395.449480	57.547469
2581.196727	107178.207074	57.552474
2580.516280	106994.835869	57.557479
2580.005252	106784.269182	57.562484
2579.295881	106581.229340	57.567489
2578.525207	106395.630809	57.572493
2578.029775	106190.999459	57.577498
2576.882350	105988.383006	57.582503
2576.488145	105792.602907	57.587508
2576.203978	105588.539620	57.592513
2575.238573	105403.150916	57.597517
2574.820634	105189.899565	57.602522
2574.464605	104981.557437	57.607527
2573.170464	104796.333390	57.612532
2572.756393	104604.899532	57.617537
2572.012228	104407.498554	57.622541
2571.361430	104201.297302	57.627546
2570.848848	103997.556603	57.632551
2569.987744	103789.374721	57.637556
2569.529487	103590.095345	57.642561
2568.782077	103397.645493	57.647565
2568.258453	103190.538319	57.652570
2567.557772	102988.282578	57.657575
2566.553970	102791.399314	57.662580
2566.136899	102588.207533	57.667585
2565.449872	102397.976670	57.672589
2565.017699	102196.928583	57.677594
2564.093659	101991.132466	57.682599
2563.517447	101789.558772	57.687604
2563.085025	101592.043073	57.692609
2562.197423	101387.642106	57.697613
2561.774966	101185.725706	57.702618
2561.138567	100975.407943	57.707623
2559.900887	100789.730615	57.712628
2559.446383	100572.263832	57.717633
2558.552479	100386.256122	57.722637
2557.816365	100181.835363	57.727642
2557.163730	99996.782100	57.732647
2556.511498	99796.036929	57.737652
2556.265030	99603.475401	57.742657
2555.356367	99414.096870	57.747661
2554.799872	99202.209371	57.752666
2554.316341	99021.215734	57.757671
2553.729171	98816.212541	57.762676
2553.334259	98613.476853	57.767681
2552.160367	98412.369681	57.772685
2551.505407	98203.862362	57.777690
2550.770438	98013.497349	57.782695
2550.259092	97816.216586	57.787700
2549.700403	97610.211130	57.792705
2548.746369	97410.454258	57.797709
2548.420402	97215.806851	57.802714
2547.451032	97009.129814	57.807719
2546.737957	96819.576762	57.812724
2546.408855	96613.347288	57.817729
2545.518218	96418.777147	57.822733
2544.950508	96225.222999	57.827738
2544.275335	96029.182340	57.832743
2543.524436	95834.113049	57.837748
2543.074445	95638.211318	57.842753
2542.137409	95433.528575	57.847757
2541.470008	95233.910286	57.852762
2540.723153	95035.257650	57.857767
2539.815124	94847.622860	57.862772
2539.613470	94644.435223	57.867777
2538.901966	94440.638970	57.872781
2538.208168	94255.277239	57.877786
2537.555078	94054.753915	57.882791
2536.833334	93857.065295	57.887796
2536.421716	93662.779090	57.892801
2535.390764	93470.374704	57.897805
2534.815945	93261.906468	57.902810
2534.491029	93070.141916	57.907815
2533.345918	92870.347671	57.912820
2532.918083	92674.886789	57.917825
2531.981610	92487.079699	57.922829
2531.840896	92288.380708	57.927834
2531.044224	92094.289674	57.932839
2530.675078	91893.512478	57.937844
2529.947555	91688.310795	57.942849
2528.829876	91501.073417	57.947853
2528.264372	91292.374871	57.952858
2527.647342	91096.387199	57.957863
2526.849684	90906.979946	57.962868
2526.637967	90709.663305	57.967873
2525.944790	90503.370237	57.972877
2524.872925	90312.768782	57.977882
2524.469669	90104.005046	57.982887
2523.671366	89925.036594	57.987892
2523.152966	89721.056483	57.992897
2522.659847	89523.395646	57.997901
2521.781743	89327.097387	58.002906
2521.317360	89127.387642	58.007911
2520.240852	88934.459352	58.012916
2519.547122	88726.553665	58.017921
2518.644868	88534.203616	58.022925
2518.398212	88348.383059	58.027930
2517.592677	88153.415281	58.032935
2516.981891	87954.348138	58.037940
2516.480421	87762.473950	58.042945
2515.688188	87567.483971	58.047949
2514.856420	87362.650001	58.052954
2514.292970	87179.235389	58.057959
2513.287779	86986.439911	58.062964
2512.751637	86803.138280	58.067969
2512.293981	86603.983218	58.072973
2511.631798	86413.712352	58.077978
2511.263438	86220.657957	58.082983
2510.171737	86031.415812	58.087988
2509.897980	85826.996124	58.092993
2509.058171	85631.898078	58.097997
2508.357876	85440.963573	58.103002
2507.530079	85240.250653	58.108007
2506.955292	85048.310852	58.113012
2506.404204	84866.967890	58.118017
2505.508926	84668.610146	58.123021
2504.847729	84482.565367	58.128026
2504.432814	84280.914917	58.133031
2503.524483	84099.216754	58.138036
2502.944578	83896.841781	58.143041
2501.991393	83712.745310	58.148045
2501.617997	83517.326467	58.153050
2501.023635	83321.792326	58.158055
2500.344057	83149.187262	58.163060
2499.509087	82946.868135	58.168065
2499.043513	82757.917139	58.173069
2498.575749	82567.263166	58.178074
2497.873686	82380.996128	58.183079
2497.092401	82185.331011	58.188084
2496.654282	81985.588575	58.193089
2495.782711	81793.528825	58.198093
2494.892552	81604.509712	58.203098
2494.278600	81414.212610	58.208103
2493.729305	81222.715454	58.213108
2492.901668	81035.751398	58.218113
2492.434447	80837.406177	58.223117
2491.781075	80655.963497	58.228122
2491.182048	80451.875458	58.233127
2489.964734	80278.580693	58.238132
2489.992295	80078.890385	58.243137
2489.340694	79888.505422	58.248141
2488.441010	79697.033456	58.253146
2487.750050	79510.378302	58.258151
2487.328833	79314.619633	58.263156
2486.697483	79122.476701	58.268161
2485.750150	78931.608732	58.273165
2485.313380	78726.130419	58.278170
2484.677849	78537.827582	58.283175
2483.980200	78355.062237	58.288180
2483.627998	78143.346980	58.293185
2482.800079	77950.644100	58.298189
2481.817890	77761.750605	58.303194
2481.324373	77566.888130	58.308199
2480.187054	77369.924365	58.313204
2479.667776	77182.065423	58.318209
2478.918022	76998.509306	58.323213
2478.651124	76798.929083	58.328218
2477.822452	76611.194129	58.333223
2477.000429	76420.931593	58.338228
2476.672565	76227.037767	58.343233
2475.796852	76047.147270	58.348237
2474.963908	75852.095152	58.353242
2474.339279	75659.932887	58.358247
2473.601998	75473.239412	58.363252
2473.051798	75282.025686	58.368257
2472.296183	75101.136091	58.373261
2471.648338	74907.109160	58.378266
2471.231495	74721.791071	58.383271
2470.366392	74550.389659	58.388276
2470.060494	74346.493267	58.393281
2469.194819	74161.523907	58.398285
2468.567276	73976.341094	58.403290
2467.830865	73783.992611	58.408295
2466.925287	73601.087475	58.413300
2466.320075	73396.538555	58.418305
2465.725847	73220.581949	58.423309
2465.291990	73035.953619	58.428314
2465.019407	72846.309160	58.433319
2463.908587	72669.748727	58.438324
2463.295712	72463.645718	58.443329
2462.803935	72275.707579	58.448333
2462.046856	72088.978927	58.453338
2461.459248	71891.721635	58.458343
2460.756034	71700.027739	58.463348
2460.342068	71511.679022	58.468353
2459.300420	71317.065048	58.473357
2458.569690	71126.882400	58.478362
2458.201716	70928.535588	58.483367
2457.574344	70746.961786	58.488372
2456.599581	70557.830495	58.493377
2456.075788	70363.175456	58.498381
2455.393182	70173.602444	58.503386
2454.643535	69984.485288	58.508391
2453.891615	69804.472817	58.513396
2453.721606	69597.024456	58.518401
2452.541144	69434.445681	58.523405
2452.045324	69226.330767	58.528410
2451.413969	69042.682981	58.533415
2450.425581	68856.059486	58.538420
2449.887094	68658.592274	58.543425
2449.090471	68487.320888	58.548429
2448.344608	68293.791948	58.553434
2448.085324	68101.663564	58.558439
2447.208905	67921.928767	58.563444
2446.775929	67728.552161	58.568449
2445.782902	67546.508498	58.573453
2445.119242	67360.360815	58.578458
2444.783863	67185.563235	58.583463
2443.864493	66988.667292	58.588468
2443.477160	66808.434546	58.593473
2442.603219	66621.858590	58.598477
2442.185577	66427.890796	58.603482
2441.384082	66243.358981	58.608487
2440.625920	66060.380014	58.613492
2440.273286	65870.929373	58.618497
2439.105244	65687.854249	58.623501
2438.386099	65500.422257	58.628506
2438.028345	65304.923635	58.633511
2437.337306	65127.674156	58.638516
2436.946281	64944.283413	58.643521
2436.084965	64760.009564	58.648525
2435.482780	64564.965662	58.653530
2434.607119	64377.952530	58.658535
2434.031828	64197.438302	58.663540
2433.565994	64006.833408	58.668545
2432.392508	63825.201682	58.673549
2431.427742	63634.442127	58.678554
2431.147902	63455.325497	58.683559
2430.132590	63282.133830	58.688564
2429.907500	63091.034466	58.693569
2429.096989	62927.834247	58.698573
2428.706130	62739.845268	58.703578
2428.115074	62546.843265	58.708583
2427.300185	62377.107486	58.713588
2427.016739	62186.520334	58.718593
2426.004841	62001.932858	58.723597
2425.429220	61818.221442	58.728602
2424.711854	61633.885277	58.733607
2424.237540	61455.568596	58.738612
2423.593638	61265.434073	58.743617
2422.812771	61074.971777	58.748621
2422.291183	60892.938624	58.753626
2421.572213	60706.667989	58.758631
2420.634154	60515.774063	58.763636
2420.302529	60347.980559	58.768641
2419.716567	60153.612421	58.773645
2418.927395	59963.216485	58.778650
2418.339051	59778.121413	58.783655
2417.467072	59607.083705	58.788660
2417.182071	59403.201222	58.793665
2416.013347	59224.028121	58.798669
2415.601975	59020.733284	58.803674
2415.011937	58845.767525	58.808679
2414.308345	58663.272030	58.813684
2413.524417	58475.036493	58.818689
2412.793936	58299.389085	58.823693
2412.276377	58105.677065	58.828698
2411.920823	57917.673603	58.833703
2411.025537	57733.049420	58.838708
2410.652062	57532.018410	58.843713
2409.377467	57360.777083	58.848717
2408.844134	57157.085110	58.853722
2408.126972	56979.514177	58.858727
2407.464632	56802.395185	58.863732
2406.991786	56613.812664	58.868737
2406.179155	56440.892440	58.873741
2405.461125	56255.871899	58.878746
2404.907815	56069.295276	58.883751
2404.163832	55887.820913	58.888756
2403.594826	55693.015557	58.893761
2402.760709	55518.781309	58.898765
2402.225154	55329.810421	58.903770
2402.046619	55147.402371	58.908775
2400.725989	54957.524912	58.913780
2400.485195	54762.718509	58.918785
2399.674860	54587.017745	58.923789
2399.079717	54401.714708	58.928794
2398.082164	54230.303476	58.933799
2397.438973	54046.239521	58.938804
2396.837864	53856.810025	58.943809
2396.174479	53680.123159	58.948813
2395.710959	53501.349407	58.953818
2394.620158	53308.661562	58.958823
2394.132770	53131.531236	58.963828
2393.577583	52952.283757	58.968833
2392.986746	52766.158082	58.973837
2392.183431	52583.672155	58.978842
2391.755561	52395.486619	58.983847
2391.052293	52220.263164	58.988852
2390.444141	52039.049112	58.993857
2389.642137	51858.370716	58.998861
2389.064570	51675.402495	59.003866
2388.502194	51483.232451	59.008871
2387.694233	51305.952458	59.013876
2387.295938	51118.813326	59.018881
2386.687635	50935.977703	59.023885
2385.835718	50749.983767	59.028890
2384.985831	50569.085406	59.033895
2384.390807	50388.749599	59.038900
2383.802258	50201.748246	59.043905
2383.160595	50012.988661	59.048909
2382.287695	49831.206006	59.053914
2382.056578	49648.184464	59.058919
2380.686591	49459.362695	59.063924
2380.557220	49280.381561	59.068929
2379.744824	49100.491808	59.073933
2379.110269	48921.088181	59.078938
2378.555916	48734.422584	59.083943
2377.552269	48559.962605	59.088948
2377.046869	48366.934246	59.093953
2376.428584	48198.683736	59.098957
2375.723876	48010.727200	59.103962
2375.265587	47824.169795	59.108967
2374.191301	47648.815709	59.113972
2373.930695	47469.705899	59.118977
2373.051953	47283.075333	59.123981
2372.408770	47099.227921	59.128986
2371.759368	46926.065915	59.133991
2371.033500	46746.363406	59.138996
2370.559702	46560.739108	59.144001
2369.647302	46381.835391	59.149005
2369.009587	46201.033141	59.154010
2368.447138	46015.415982	59.159015
2367.539464	45835.653517	59.164020
2367.380419	45647.063038	59.169025
2366.415668	45474.079160	59.174029
2365.774020	45296.127249	59.179034
2365.495290	45111.249578	59.184039
2364.476216	44930.210888	59.189044
2364.065753	44742.195038	59.194049
2363.011270	44575.911176	59.199053
2362.279205	44373.676151	59.204058
2361.920190	44206.893320	59.209063
2361.047151	44021.808267	59.214068
2360.676996	43837.391843	59.219073
2359.898570	43658.978546	59.224077
2359.427345	43467.026312	59.229082
2358.719869	43288.453747	59.234087
2358.049842	43115.911371	59.239092
2357.447765	42925.152870	59.244097
2356.945477	42735.721563	59.249101
2356.185394	42555.289474	59.254106
2355.410932	42373.428933	59.259111
2354.272186	42194.347783	59.264116
2353.792142	42013.914872	59.269121
2352.831655	41822.719343	59.274125
2352.424685	41652.708184	59.279130
2351.908949	41476.157273	59.284135
2351.168722	41291.424959	59.289140
2350.719887	41110.171173	59.294145
2350.007316	40929.362719	59.299149
2349.096408	40756.610107	59.304154
2348.537009	40569.045668	59.309159
2347.903695	40388.043765	59.314164
2347.240060	40214.077917	59.319169
2346.334299	40041.091362	59.324173
2346.092042	39859.410090	59.329178
2345.442857	39679.256115	59.334183
2344.401080	39505.904443	59.339188
2344.150638	39315.923745	59.344193
2343.328249	39138.402038	59.349197
2342.407032	38957.503584	59.354202
2342.342203	38785.650043	59.359207
2341.365158	38606.512657	59.364212
2340.855891	38416.480246	59.369217
2339.807022	38242.013784	59.374221
2339.499171	38056.199660	59.379226
2338.633596	37873.879542	59.384231
2337.772460	37701.786975	59.389236
2337.271647	37512.776622	59.394241
2336.712681	37340.342609	59.399245
2335.878963	37158.734893	59.404250
2335.277803	36975.565240	59.409255
2334.637299	36800.557224	59.414260
2333.910748	36624.774306	59.419265
2332.973860	36456.441637	59.424269
2332.547341	36271.620630	59.429274
2332.012247	36101.960069	59.434279
2331.189457	35932.086030	59.439284
2330.490335	35743.017838	59.444289
2329.650080	35572.012145	59.449293
2328.958238	35395.145915	59.454298
2328.410013	35227.838693	59.459303
2327.699322	35061.346025	59.464308
2327.233108	34880.855212	59.469313
2326.746403	34708.197983	59.474317
2326.072624	34529.719536	59.479322
2325.314519	34350.379185	59.484327
2324.576643	34184.319953	59.489332
2324.094764	33999.978404	59.494337
2323.714338	33828.203200	59.499341
2322.824768	33646.032214	59.504346
2321.860893	33467.276063	59.509351
2321.222984	33294.730107	59.514356
2320.677551	33115.724879	59.519361
2320.004044	32941.282285	59.524365
2319.312949	32759.614199	59.529370
2318.725000	32584.806197	59.534375
2318.138451	32413.528663	59.539380
2317.506040	32236.452559	59.544385
2316.869903	32054.987325	59.549389
2315.817097	31883.054382	59.554394
2315.711188	31705.108740	59.559399
2314.748997	31524.519598	59.564404
2314.429274	31341.765194	59.569409
2313.509458	31177.926585	59.574413
2312.964037	30996.453833	59.579418
2312.445647	30807.283381	59.584423
2311.455631	30638.153492	59.589428
2310.833305	30455.267278	59.594433
2310.088439	30281.752068	59.599437
2309.514120	30103.937475	59.604442
2308.881815	29933.051598	59.609447
2308.133485	29749.118766	59.614452
2307.594724	29571.402262	59.619457
2306.795154	29401.752440	59.624461
2306.069312	29217.648198	59.629466
2305.727582	29045.069635	59.634471
2304.870937	28870.948757	59.639476
2304.338049	28693.768557	59.644481
2303.534181	28508.082595	59.649485
2303.025984	28328.007990	59.654490
2302.187781	28151.070113	59.659495
2301.499920	27975.339470	59.664500
2301.104804	27798.979739	59.669505
2300.126251	27630.823867	59.674509
2299.678546	27452.596197	59.679514
2299.144348	27264.268585	59.684519
2298.193160	27096.080730	59.689524
2297.790449	26918.701718	59.694529
2297.055103	26737.797637	59.699533
2296.413487	26562.937490	59.704538
2295.779418	26387.940597	59.709543
2295.190111	26204.097590	59.714548
2294.691574	26013.212601	59.719553
2293.863832	25846.242421	59.724557
2293.101837	25666.860773	59.729562
2292.677830	25489.787512	59.734567
2291.642330	25310.164925	59.739572
2291.049783	25122.482816	59.744577
2290.447029	24957.800291	59.749581
2289.778772	24775.688892	59.754586
2288.892718	24600.519161	59.759591
2287.640774	24417.053576	59.764596
2287.492093	24242.514765	59.769601
2286.843437	24072.134659	59.774605
2286.298196	23904.401411	59.779610
2285.503502	23731.988424	59.784615
2284.654785	23556.753890	59.789620
2284.155511	23392.784147	59.794625
2283.219441	23217.562448	59.799629
2282.666675	23044.950291	59.804634
2282.057202	22886.128414	59.809639
2281.334510	22713.182748	59.814644
2280.994447	22538.841342	59.819649
2280.117318	22368.442992	59.824653
2279.307871	22204.022959	59.829658
2278.784720	22032.988498	59.834663
2278.272801	21857.483908	59.839668
2277.317547	21681.296681	59.844673
2276.845002	21520.159401	59.849677
2276.163348	21338.403604	59.854682
2275.603046	21176.640194	59.859687
2274.748592	21017.110717	59.864692
2274.346975	20839.475075	59.869697
2273.516896	20671.254145	59.874701
2272.737306	20493.028567	59.879706
2272.259142	20316.603994	59.884711
2271.290198	20146.807853	59.889716
2270.705238	19992.964765	59.894721
2270.108319	19822.748333	59.899725
2269.574567	19650.283018	59.904730
2268.698444	19474.105879	59.909735
2268.071780	19306.325573	59.914740
2267.527854	19134.238998	59.919745
2266.809904	18969.934423	59.924750
2265.902034	18814.922060	59.929754
2265.575852	18643.464372	59.934759
2265.086302	18476.815542	59.939764
2264.540705	18303.522157	59.944769
2263.264316	18140.558662	59.949774
2263.001955	17967.746692	59.954778
2262.500829	17794.822929	59.959783
2261.223174	17635.066889	59.964788
2261.021495	17462.514551	59.969793
2260.076628	17296.521675	59.974798
2259.099690	17126.451647	59.979802
2258.719994	16951.446564	59.984807
2258.214229	16791.853420	59.989812
2257.755429	16631.973837	59.994817
2256.658194	16479.892001	59.999822
2256.083727	16308.387645	60.004826
2255.473775	16139.226721	60.009831
2254.761241	15980.004665	60.014836
2254.059809	15800.205127	60.019841
2253.496579	15636.781773	60.024846
2252.775025	15482.464469	60.029850
2252.278387	15319.120928	60.034855
2251.555109	15142.971438	60.039860
2250.956195	14971.550285	60.044865
2250.055556	14822.704273	60.049870
2249.507579	14651.252846	60.054874
2249.056986	14481.504844	60.059879
2248.056585	14325.179779	60.064884
2247.521686	14169.672351	60.069889
2246.758649	14006.151937	60.074894
2246.044786	13834.604897	60.079898
2245.410970	13668.452920	60.084903
2244.651627	13515.033208	60.089908
2244.416854	13344.401214	60.094913
2243.433572	13194.806193	60.099918
2242.819483	13029.515871	60.104922
2242.350556	12871.286413	60.109927
2241.514275	12712.820719	60.114932
2240.969234	12538.240971	60.119937
2240.208287	12374.757744	60.124942
2239.402322	12218.037411	60.129946
2238.465833	12062.822698	60.134951
2237.599786	11897.453089	60.139956
2237.319550	11743.688679	60.144961
2236.358772	11593.947439	60.149966
2235.524366	11433.960861	60.154970
2235.149793	11276.411993	60.159975
2234.381319	11135.677495	60.164980
2233.875016	10973.940825	60.169985
2233.009671	10829.507109	60.174990
2232.642211	10674.364144	60.179994
2231.831869	10519.340757	60.184999
2230.767325	10360.103475	60.190004
2230.406121	10211.795548	60.195009
2229.620072	10064.506083	60.200014
2228.837526	9918.814510	60.205018
2228.237228	9768.490645	60.210023
2227.443348	9630.581715	60.215028
2227.162051	9476.587347	60.220033
2226.354970	9334.239284	60.225038
2225.485800	9183.772553	60.230042
2225.238962	9030.870421	60.235047
2224.245077	8893.823855	60.240052
2223.943969	8737.258217	60.245057
2222.784781	8597.386842	60.250062
2221.843998	8445.743946	60.255066
2221.456823	8304.858931	60.260071
2220.364457	8170.988811	60.265076
2219.884258	8024.974084	60.270081
2219.295100	7892.953995	60.275086
2218.564147	7761.986320	60.280090
2217.715598	7619.235434	60.285095
2216.847240	7492.086217	60.290100
2216.446310	7357.649395	60.295105
2215.435409	7231.446048	60.300110
2214.377491	7105.022448	60.305114
2213.701071	6972.976973	60.310119
2212.590799	6861.326137	60.315124
2211.983365	6746.395123	60.320129
2211.044439	6635.323860	60.325134
2210.328553	6521.100465	60.330138
2209.467543	6420.512654	60.335143
2208.457773	6319.637920	60.340148
2207.597904	6217.339496	60.345153
2206.607067	6134.819035	60.350158
2205.728829	6052.849131	60.355162
2204.925531	5958.270950	60.360167
2203.990411	5875.991568	60.365172
2203.394397	5800.243144	60.370177
2202.428528	5742.628772	60.375182
2201.636046	5654.889079	60.380186
2201.558053	5587.905326	60.385191
2200.435265	5516.063709	60.390196
2199.538984	5449.581923	60.395201
2199.036439	5380.813555	60.400206
2198.309335	5313.152316	60.405210
2198.017683	5248.317174	60.410215
2197.313664	5185.180529	60.415220
2196.718443	5115.799426	60.420225
2196.031485	5043.121106	60.425230
2195.368854	4983.111010	60.430234
2194.639619	4919.963720	60.435239
2193.856775	4861.572824	60.440244
2193.653302	4787.265175	60.445249
2192.742869	4722.238655	60.450254
2191.660267	4661.706493	60.455258
2191.095564	4595.018188	60.460263
2190.639953	4539.808192	60.465268
2189.822479	4472.494831	60.470273
2189.215957	4419.662072	60.475278
2188.396150	4348.373565	60.480282
2188.238895	4291.807844	60.485287
2187.158283	4240.853214	60.490292
2186.986462	4177.526014	60.495297
2186.211169	4112.777304	60.500302
2185.461163	4056.106186	60.505306
2184.892986	3989.708261	60.510311
2184.100634	3936.409028	60.515316
2183.764305	3868.488911	60.520321
2182.891422	3804.336747	60.525326
2182.736213	3753.457829	60.530330
2182.142701	3677.827918	60.535335
2181.376573	3625.561224	60.540340
2180.581502	3553.849885	60.545345
2179.919828	3489.374553	60.550350
2179.224854	3426.469558	60.555354
2178.233169	3361.853122	60.560359
2177.669012	3305.081272	60.565364
2177.180223	3245.058549	60.570369
2176.465824	3189.669887	60.575374
2175.595065	3129.891997	60.580378
2175.032333	3064.084158	60.585383
2174.151559	3010.721074	60.590388
2174.096933	2946.601354	60.595393
2173.314239	2891.301942	60.600398
2172.584625	2836.434391	60.605402
2171.884894	2763.873429	60.610407
2171.430574	2703.050115	60.615412
2170.597720	2641.044978	60.620417
2169.806594	2594.791518	60.625422
2169.318608	2523.568037	60.630426
2168.872462	2465.417137	60.635431
2168.040716	2413.663590	60.640436
2167.029453	2350.006607	60.645441
2166.397596	2298.742255	60.650446
2165.852938	2238.827144	60.655450
2165.000259	2193.123355	60.660455
2164.286764	2140.225063	60.665460
2164.024246	2080.254796	60.670465
2163.110862	2026.273516	60.675470
2162.485372	1972.910774	60.680474
2161.822380	1919.342829	60.685479
2161.067796	1882.977425	60.690484
2160.707904	1825.160794	60.695489
2159.844272	1772.287653	60.700494
2159.002501	1708.860501	60.705498
2158.653975	1646.990925	60.710503
2158.019125	1607.215441	60.715508
2157.376504	1559.791129	60.720513
2156.657047	1500.320789	60.725518
2156.050803	1443.537590	60.730522
2155.711435	1383.471968	60.735527
2154.645207	1338.063395	60.740532
2154.005323	1280.876102	60.745537
2153.012742	1224.166883	60.750542
2152.237531	1165.862018	60.755546
2151.863822	1132.151543	60.760551
2150.778417	1080.750510	60.765556
2150.369762	1027.303199	60.770561
2149.791357	987.287824	60.775566
2149.038135	943.318843	60.780570
2148.471340	886.974725	60.785575
2147.651046	856.286534	60.790580
2146.883069	798.346307	60.795585
2146.284851	751.402542	60.800590
2145.402066	714.528914	60.805594
2145.153944	673.539394	60.810599
2143.991837	636.921613	60.815604
2143.679739	593.235393	60.820609
2143.132187	557.899465	60.825614
2142.125179	506.876777	60.830618
2141.641666	460.994471	60.835623
2140.683463	430.032575	60.840628
2140.054280	392.450063	60.845633
2139.449640	350.268197	60.850638
2138.862462	311.084822	60.855642
2138.190514	259.986183	60.860647
2137.264798	243.749197	60.865652
2136.610897	201.034653	60.870657
2135.945728	167.877313	60.875662
2134.836040	141.554495	60.880666
2134.697927	109.357661	60.885671
2133.558348	76.332577	60.890676
2132.982620	58.685599	60.895681
2132.322103	41.690793	60.900686
2131.209905	15.453764	60.905690
2130.188802	-5.309634	60.910695
2128.457926	-3.263890	60.915700
2127.527820	-0.222365	60.920705
2127.012050	12.873179	60.925710
2126.034102	21.375651	60.930714
2125.863792	10.409344	60.935719
2125.463077	18.979504	60.940724
2124.766116	10.263595	60.945729
2124.340506	13.953659	60.950734
2123.750702	20.196172	60.955738
2123.127384	23.964921	60.960743
2121.575834	25.715701	60.965748
2121.136671	34.918050	60.970753
2120.492105	43.957445	60.975758
2120.187929	43.486976	60.980762
2119.825932	37.900343	60.985767
2118.870363	43.265727	60.990772
2118.714994	45.386357	60.995777
2118.293203	39.556888	61.000782
2116.947863	49.716780	61.005786
2116.281310	44.482837	61.010791
2115.426599	55.572604	61.015796
2115.726260	49.890440	61.020801
2114.762500	61.442237	61.025806
2113.880231	57.289667	61.030810
2113.185422	49.781400	61.035815
2112.177601	54.819174	61.040820
2112.050663	48.955532	61.045825
2111.068411	53.478292	61.050830
2110.225670	59.007139	61.055834
2110.020215	56.213812	61.060839
2109.548515	60.261304	61.065844
2108.936132	51.312748	61.070849
2108.138116	55.500331	61.075854
2107.191198	59.776202	61.080858
2106.879339	60.964410	61.085863
2106.235240	64.378485	61.090868
2106.188291	60.112293	61.095873
2105.243938	63.652863	61.100878
2104.244253	60.203358	61.105882
2103.487624	63.740950	61.110887
2102.731646	66.923608	61.115892
2101.622258	62.456980	61.120897
2100.837969	69.083633	61.125902
2100.669608	69.618260	61.130906
2100.602771	66.047539	61.135911
2099.745837	71.871973	61.140916
2098.933100	66.490905	61.145921
2098.335202	66.357219	61.150926
2097.168264	65.823374	61.155930
2097.328540	63.929269	61.160935
2096.515024	69.145965	61.165940
2096.206090	63.431053	61.170945
2095.396568	65.735919	61.175950
2094.811971	66.142621	61.180954
2094.016297	56.874629	61.185959
2092.714380	69.853689	61.190964
2092.163218	67.850116	61.195969
2091.586818	65.877358	61.200974
2090.558393	69.156872	61.205978
2090.121602	68.013556	61.210983
2089.769537	70.040819	61.215988
2089.737144	70.664262	61.220993
2089.401184	67.084206	61.225998
2087.927138	73.459178	61.231002
2086.739547	70.518913	61.236007
2085.881771	73.356591	61.241012
2086.004058	64.485426	61.246017
2085.650295	68.474783	61.251022
2084.995660	70.453861	61.256026
2084.247264	69.181790	61.261031
2083.285333	75.767249	61.266036
2082.976231	70.348845	61.271041
2082.275143	67.566358	61.276046
2081.277464	68.204203	61.281050
2080.572939	65.004350	61.286055
2079.882363	69.485570	61.291060
2079.517313	68.050160	61.296065
2078.766767	71.331316	61.301070
2077.648809	73.860184	61.306074
2077.265729	69.059100	61.311079
2076.218058	81.608304	61.316084
2075.862845	69.039078	61.321089
2075.525855	72.704060	61.326094
2075.023888	72.045776	61.331098
2074.226209	64.099655	61.336103
2073.001416	72.598764	61.341108
2072.919905	68.732314	61.346113
2072.808972	68.109752	61.351118
2071.342164	78.173835	61.356122
2070.737475	72.215684	61.361127
2069.775006	67.222682	61.366132
2070.217962	71.011486	61.371137
2068.406238	65.722727	61.376142
2068.340644	70.312937	61.381146
2068.254753	70.582154	61.386151
2066.223076	75.426021	61.391156
2066.026892	61.809651	61.396161
2065.873247	73.928378	61.401166
2065.165837	80.847210	61.406170
2064.020000	75.044327	61.411175
2063.433060	80.442709	61.416180
2063.360858	78.763698	61.421185
2062.213140	69.568925	61.426190
2061.352471	67.612900	61.431194
2061.510120	69.013624	61.436199
2060.168045	74.382023	61.441204
2059.494953	71.931007	61.446209
2058.793727	78.295320	61.451214
2058.479845	77.693927	61.456218
2057.936500	72.181806	61.461223
2056.455925	80.158518	61.466228
2056.728488	71.517404	61.471233
2056.060383	65.293344	61.476238
2054.825468	78.709668	61.481242
2054.420208	63.770234	61.486247
2053.509996	76.201425	61.491252
2052.977025	72.534362	61.496257
2052.583431	68.733211	61.501262
2051.725514	75.217013	61.506266
2051.304017	69.862186	61.511271
2050.530877	85.676438	61.516276
2050.036917	78.651993	61.521281
2049.358253	77.200123	61.526286
2048.712324	76.250861	61.531290
2048.527831	70.634483	61.536295
2047.221787	77.946379	61.541300
2046.964563	72.317888	61.546305
2045.473530	75.016368	61.551310
2044.891493	81.863266	61.556314
2044.910402	71.775268	61.561319
2043.710309	71.396526	61.566324
2042.874855	65.213223	61.571329
2042.645070	68.742916	61.576334
2041.837142	79.724361	61.581338
2041.158114	65.105935	61.586343
2040.441096	72.360623	61.591348
2040.395665	77.726686	61.596353
2039.322802	74.989020	61.601358
2038.761208	76.571702	61.606362
2038.332850	67.267509	61.611367
2037.204687	75.703986	61.616372
2036.896738	73.070440	61.621377
2036.494053	67.455575	61.626382
2035.393999	67.136658	61.631386
2034.730002	77.377712	61.636391
2033.378439	78.079624	61.641396
2033.486014	66.391067	61.646401
2032.903608	74.494913	61.651406
2031.540970	80.732380	61.656410
2031.628911	73.118826	61.661415
2030.717314	81.601366	61.666420
2030.108016	68.479515	61.671425
2029.510680	69.795045	61.676430
2028.550317	86.440146	61.681434
2028.177244	73.561511	61.686439
2027.474647	75.340047	61.691444
2027.082763	72.183634	61.696449
2026.550359	67.802094	61.701454
2025.905889	65.422243	61.706458
2024.798733	65.341012	61.711463
2023.365290	76.915344	61.716468
2023.491555	72.588545	61.721473
2023.127541	69.795158	61.726478
2021.970459	69.005881	61.731482
2021.548837	59.588659	61.736487
2020.327738	66.907580	61.741492
2020.114228	68.371940	61.746497
2019.288436	70.919118	61.751502
2018.686295	70.191584	61.756506
2018.276836	70.532658	61.761511
2017.599484	69.820215	61.766516
2017.335604	66.217692	61.771521
2016.589140	71.305489	61.776526
2016.364702	85.578640	61.781530
2015.490229	67.379843	61.786535
2013.690276	79.714129	61.791540
2013.299054	76.861979	61.796545
2012.398395	75.202490	61.801550
2012.313012	77.881328	61.806554
2011.876054	70.456747	61.811559
2011.081944	78.912758	61.816564
2010.524753	78.996570	61.821569
2009.944454	70.896115	61.826574
2009.264550	74.735384	61.831578
2008.949805	72.471946	61.836583
2007.181426	75.275970	61.841588
2006.610978	77.938752	61.846593
2005.979779	76.868886	61.851598
2005.908242	75.478369	61.856602
2005.262977	65.049497	61.861607
2004.517573	85.527356	61.866612
2003.743863	73.149154	61.871617
2003.104243	77.970828	61.876622
2002.679407	78.514628	61.881626
2002.304947	64.082856	61.886631
2000.867883	68.329320	61.891636
2000.220979	69.807272	61.896641
1999.457710	78.580105	61.901646
1998.877189	76.518131	61.906650
1998.216533	75.683189	61.911655
1998.025174	70.552055	61.916660
1997.331968	73.344714	61.921665
1997.103088	83.122458	61.926670
1996.339411	76.260692	61.931674
1995.890675	81.121461	61.936679
1994.375014	79.977504	61.941684
1993.710578	74.885185	61.946689
1992.804763	84.976966	61.951694
1992.589970	78.428645	61.956698
1991.932236	76.341080	61.961703
1991.616630	82.324065	61.966708
1990.727022	75.389245	61.971713
1989.626326	80.318800	61.976718
1988.622343	91.460699	61.981722
1988.978973	67.933278	61.986727
1987.766465	75.164116	61.991732
1987.270465	75.935267	61.996737
1986.713685	76.783877	62.001742
1986.180979	74.335830	62.006746
1985.835793	88.226004	62.011751
1984.501176	78.329191	62.016756
1983.542699	78.161297	62.021761
1983.265685	77.025756	62.026766
1982.439134	82.914792	62.031770
1982.003230	74.029719	62.036775
1980.750548	72.113866	62.041780
1980.468040	74.928077	62.046785
1980.278302	71.132431	62.051790
1979.185375	75.049881	62.056794
1979.245675	70.465459	62.061799
1979.111276	78.589671	62.066804
1977.959207	70.105296	62.071809
1976.852147	75.433276	62.076814
1975.973457	81.511947	62.081818
1975.294143	71.548977	62.086823
1974.667163	77.434721	62.091828
1974.113453	77.461215	62.096833
1972.926026	70.034334	62.101838
1972.701401	65.285395	62.106842
1971.711879	69.085503	62.111847
1971.278076	76.468724	62.116852
1970.661685	65.710412	62.121857
1970.007126	72.105182	62.126862
1969.653710	67.225291	62.131866
1969.398368	66.466377	62.136871
1968.805878	65.820905	62.141876
1967.704973	64.431350	62.146881
1966.818808	76.284705	62.151886
1966.142003	73.225571	62.156890
1965.731042	76.692561	62.161895
1965.015718	76.301565	62.166900
1964.268089	74.168350	62.171905
1963.221502	76.272753	62.176910
1962.137261	72.227993	62.181914
1962.460846	62.377090	62.186919
1961.461486	69.922625	62.191924
1960.928641	78.464914	62.196929
1960.406761	72.898948	62.201934
1959.738960	77.521667	62.206938
1959.458485	73.562222	62.211943
1958.149021	80.994553	62.216948
1957.340580	77.180418	62.221953
1956.676637	72.223658	62.226958
1955.765263	82.945562	62.231962
1955.790480	75.805613	62.236967
1955.143718	74.241467	62.241972
1954.764493	76.605810	62.246977
1954.414732	73.128895	62.251982
1952.922622	73.873658	62.256986
1952.020864	78.197610	62.261991
1951.410393	84.251059	62.266996
1950.894254	73.793818	62.272001
1950.424415	70.786995	62.277006
1950.005692	75.441144	62.282010
1949.850796	73.985010	62.287015
1948.235181	73.566611	62.292020
1947.471602	73.203781	62.297025
1947.016395	67.442724	62.302030
1946.129667	72.827206	62.307034
1945.984881	74.204964	62.312039
1944.994218	73.750443	62.317044
1944.613472	68.445944	62.322049
1943.495545	69.968716	62.327054
1942.695032	71.788048	62.332058
1942.131619	65.422821	62.337063
1941.432497	71.946100	62.342068
1941.140886	73.023875	62.347073
1940.727374	73.578503	62.352078
1940.056742	80.122496	62.357082
1939.882025	72.419748	62.362087
1938.416640	77.325208	62.367092
1937.443711	71.353009	62.372097
1937.025309	68.068353	62.377102
1936.158333	71.774899	62.382106
1936.213799	67.607582	62.387111
1935.419705	74.776751	62.392116
1934.732746	63.547085	62.397121
1933.677354	64.919579	62.402126
1932.879702	72.494607	62.407130
1932.480300	69.851940	62.412135
1931.899134	79.807035	62.417140
1931.258077	74.138563	62.422145
1931.152063	74.360513	62.427150
1930.006236	62.624925	62.432154
1929.137435	62.901730	62.437159
1928.166579	78.911387	62.442164
1927.644741	75.337208	62.447169
1927.194188	71.377957	62.452174
1926.613946	72.457396	62.457178
1926.579058	65.655018	62.462183
1925.822598	84.082922	62.467188
1924.668074	78.079627	62.472193
1923.952739	71.752713	62.477198
1922.990690	74.469791	62.482202
1922.832193	74.132343	62.487207
1922.280617	81.859135	62.492212
1921.269752	74.714925	62.497217
1920.571193	73.654197	62.502222
1920.022801	75.942892	62.507226
1919.611909	73.242123	62.512231
1919.359670	80.426208	62.517236
1917.983410	73.234345	62.522241
1917.296323	68.579330	62.527246
1916.450530	84.788349	62.532250
1916.178663	72.920326	62.537255
1915.293475	81.884428	62.542260
1915.202117	71.178406	62.547265
1914.181529	72.584808	62.552270
1913.171370	69.461911	62.557274
1912.829339	66.311800	62.562279
1911.677825	68.417109	62.567284
1911.359865	70.092031	62.572289
1910.858069	73.781614	62.577294
1910.361307	77.978203	62.582298
1909.736007	68.599647	62.587303
1908.680132	71.602873	62.592308
1907.843954	78.949050	62.597313
1907.363320	74.991424	62.602318
1907.134725	70.780889	62.607322
1906.674250	68.188925	62.612327
1905.210834	64.983440	62.617332
1904.475363	69.292044	62.622337
1904.014539	69.117717	62.627342
1903.580865	79.735406	62.632346
1903.252348	74.285420	62.637351
1902.467515	78.329037	62.642356
1901.830883	71.783046	62.647361
1900.899978	76.327692	62.652366
1899.978145	72.764980	62.657370
1899.628789	72.003651	62.662375
1899.063572	74.255595	62.667380
1898.459749	66.816531	62.672385
1897.696615	69.300178	62.677390
1896.666277	74.403108	62.682394
1896.090877	67.703889	62.687399
1895.168084	77.528711	62.692404
1894.994584	73.695802	62.697409
1894.896455	70.142677	62.702414
1893.756247	74.097628	62.707418
1892.783645	68.081242	62.712423
1892.071371	74.245481	62.717428
1891.495144	65.698121	62.722433
1891.241808	70.863783	62.727438
1890.621709	72.496785	62.732442
1890.226186	68.530384	62.737447
1888.755243	64.468202	62.742452
1888.289907	70.580620	62.747457
1887.629204	66.821908	62.752462
1886.835582	67.419544	62.757466
1886.781506	64.059710	62.762471
1885.211854	61.987638	62.767476
1884.622393	71.657031	62.772481
1884.391798	66.779736	62.777486
1883.439501	78.257237	62.782490
1883.159980	73.077033	62.787495
1882.714806	74.313241	62.792500
1882.101900	65.727550	62.797505
1880.985602	66.758057	62.802510
1879.891051	72.380566	62.807514
1879.332493	66.535004	62.812519
1878.850578	75.294729	62.817524
1878.630363	60.332284	62.822529
1878.240288	63.797543	62.827534
1877.658382	68.318325	62.832538
1876.891730	65.038507	62.837543
1875.719250	66.812830	62.842548
1875.244968	69.654341	62.847553
1874.717568	70.417880	62.852558
1873.731472	71.279478	62.857562
1873.153783	68.187289	62.862567
1872.384147	72.591215	62.867572
1871.962078	72.644141	62.872577
1871.635494	66.252372	62.877582
1870.202001	73.281786	62.882586
1869.632288	67.505810	62.887591
1868.716809	74.631184	62.892596
1868.088976	65.611032	62.897601
1867.678252	78.514919	62.902606
1867.335403	78.643581	62.907610
1867.354018	68.979871	62.912615
1866.427105	70.934416	62.917620
1865.137597	71.904117	62.922625
1864.828789	69.873157	62.927630
1863.990970	82.586226	62.932634
1863.494530	67.147215	62.937639
1862.098044	71.387307	62.942644
1861.552658	68.203255	62.947649
1861.313548	60.021872	62.952654
1860.615325	65.765971	62.957658
1860.123228	67.530050	62.962663
1859.818335	78.346501	62.967668
1858.889333	70.405541	62.972673
1857.993177	72.744731	62.977678
1857.385584	73.779639	62.982682
1857.226497	66.940213	62.987687
1855.987320	71.823990	62.992692
1854.934230	73.071564	62.997697
1854.416395	68.834417	63.002702
1853.644684	74.028768	63.007706
1853.333051	63.808765	63.012711
1852.936035	66.636434	63.017716
1852.466659	71.536765	63.022721
1851.338353	64.838613	63.027726
1850.566706	71.837070	63.032730
1850.276567	64.706203	63.037735
1849.658987	73.416503	63.042740
1848.656691	67.187222	63.047745
1847.955630	63.565824	63.052750
1847.204884	74.569762	63.057754
1846.895185	63.314925	63.062759
1846.106889	71.186544	63.067764
1846.041878	74.414107	63.072769
1844.349450	77.054782	63.077774
1843.624904	75.279078	63.082778
1843.146715	70.439523	63.087783
1842.649953	74.984643	63.092788
1842.168722	61.628059	63.097793
1841.898263	66.600890	63.102798
1841.357183	71.389599	63.107802
1840.742363	72.849878	63.112807
1839.538548	76.892225	63.117812
1838.742634	65.725629	63.122817
1838.445827	69.359019	63.127822
1836.826933	67.021970	63.132826
1836.685578	67.118642	63.137831
1835.802347	68.214668	63.142836
1835.453382	58.965740	63.147841
1835.057951	68.219534	63.152846
1834.522492	67.030427	63.157850
1834.067456	65.300247	63.162855
1832.821541	75.688922	63.167860
1831.895502	70.398485	63.172865
1831.475719	70.291774	63.177870
1830.953658	68.207944	63.182874
1830.847222	68.554551	63.187879
1829.603384	76.462237	63.192884
1828.665117	75.974208	63.197889
1828.005491	67.867483	63.202894
1827.406652	73.335603	63.207898
1827.265936	64.974589	63.212903
1826.718657	66.731665	63.217908
1825.478203	60.811461	63.222913
1824.906234	63.099184	63.227918
1824.183325	58.989232	63.232922
1824.085972	58.711472	63.237927
1823.139695	75.415864	63.242932
1822.011805	67.807716	63.247937
1821.608039	74.738304	63.252942
1820.727049	70.077836	63.257946
1820.445574	61.789641	63.262951
1820.152069	64.853201	63.267956
1819.049736	66.075490	63.272961
1818.382344	61.674437	63.277966
1817.555370	75.237379	63.282970
1817.447090	69.014391	63.287975
1816.632135	64.373405	63.292980
1816.062234	69.207697	63.297985
1814.784738	73.282254	63.302990
1814.267282	74.315475	63.307994
1813.868536	76.173555	63.312999
1813.346503	74.143342	63.318004
1812.683195	63.594397	63.323009
1811.766867	62.541471	63.328014
1811.118715	64.051205	63.333018
1810.653465	59.777335	63.338023
1809.861384	58.674717	63.343028
1809.136157	54.440555	63.348033
1808.472612	64.910228	63.353038
1807.551061	65.559741	63.358042
1807.050250	62.043759	63.363047
1806.584401	65.573100	63.368052
1806.021125	57.927350	63.373057
1805.045277	55.220119	63.378062
1803.826672	60.237848	63.383066
1803.849174	58.430267	63.388071
1803.293885	63.080881	63.393076
1802.932255	60.011176	63.398081
1802.316402	62.655971	63.403086
1801.081426	62.505241	63.408090
1800.900562	57.500210	63.413095
1800.283312	66.024372	63.418100
1799.373286	64.293906	63.423105
1798.209713	69.771277	63.428110
1797.471460	66.606829	63.433114
1796.895221	58.026388	63.438119
1796.844678	69.994671	63.443124
1796.375056	59.911742	63.448129
1795.486417	68.322876	63.453134
1794.550848	69.081858	63.458138
1794.082007	63.453897	63.463143
1793.853004	65.761285	63.468148
1792.591401	72.932180	63.473153
1791.631617	66.024362	63.478158
1790.824615	63.307669	63.483162
1790.759060	56.142731	63.488167
1790.126624	62.737451	63.493172
1789.656029	65.412801	63.498177
1788.874063	63.535841	63.503182
1787.861190	64.592542	63.508186
1787.723797	70.635546	63.513191
1787.103418	61.481771	63.518196
1785.869736	60.815156	63.523201
1785.093043	72.857751	63.528206
1784.249924	68.661238	63.533210
1784.287913	57.761233	63.538215
1783.476699	69.613757	63.543220
1782.936776	75.477824	63.548225
1781.498850	69.913866	63.553230
1780.722353	70.442579	63.558234
1780.681687	68.704955	63.563239
1779.937896	68.439962	63.568244
1779.586833	60.076091	63.573249
1779.444005	65.613731	63.578254
1778.555803	66.016674	63.583258
1777.705657	58.772896	63.588263
1777.035551	61.899418	63.593268
1776.190293	72.263911	63.598273
1775.217871	56.544124	63.603278
1774.243427	65.773170	63.608282
1774.227426	56.668510	63.613287
1773.483825	56.166935	63.618292
1773.001386	59.369316	63.623297
1772.762811	53.728452	63.628302
1771.390950	66.975785	63.633306
1770.579717	54.589466	63.638311
1770.175893	64.946933	63.643316
1769.612361	57.905234	63.648321
1769.040902	59.126819	63.653326
1767.652906	63.747246	63.658330
1767.332065	59.013617	63.663335
1766.249118	64.593318	63.668340
1766.029214	58.805979	63.673345
1765.980631	50.318382	63.678350
1765.509079	55.189101	63.683354
1764.831318	50.622549	63.688359
1763.676349	60.356524	63.693364
1763.040875	55.480468	63.698369
1762.131837	62.606419	63.703374
1761.117105	63.012115	63.708378
1760.690411	61.187559	63.713383
1759.938639	58.798012	63.718388
1759.525359	56.028267	63.723393
1759.603090	51.154071	63.728398
1758.431659	64.642400	63.733402
1757.698040	54.763844	63.738407
1756.422481	63.554992	63.743412
1756.295488	62.009284	63.748417
1755.666916	59.224841	63.753422
1755.560483	57.775221	63.758426
1754.682380	50.598977	63.763431
1753.173481	59.876631	63.768436
1753.021415	54.452277	63.773441
1752.499005	52.699697	63.778446
1751.988539	56.600421	63.783450
1751.171758	52.161612	63.788455
1750.316313	61.939491	63.793460
1749.705890	59.193171	63.798465
1749.326733	62.260877	63.803470
1748.104623	62.671126	63.808474
1747.587372	55.628393	63.813479
1746.858420	64.384777	63.818484
1746.401312	61.836468	63.823489
1746.222670	57.944469	63.828494
1745.267283	60.464995	63.833498
1744.132536	55.415913	63.838503
1743.626435	59.621889	63.843508
1743.015928	65.170723	63.848513
1742.560403	66.490601	63.853518
1741.924721	65.196001	63.858522
1741.385910	58.358552	63.863527
1740.364812	66.129963	63.868532
1739.841316	69.217441	63.873537
1739.149031	66.842107	63.878542
1738.698903	60.629268	63.883546
1737.795350	58.424690	63.888551
1737.079109	66.742223	63.893556
1736.498773	66.610562	63.898561
1735.936671	61.975182	63.903566
1735.309468	64.123455	63.908570
1734.328785	58.840164	63.913575
1733.589209	63.797614	63.918580
1733.069611	64.138876	63.923585
1732.740967	61.346230	63.928590
1732.096146	70.839922	63.933594
1731.736387	60.832606	63.938599
1730.385837	69.867500	63.943604
1729.687684	65.204840	63.948609
1729.442366	64.892234	63.953614
1728.664805	59.332247	63.958618
1728.065182	59.730376	63.963623
1727.133100	60.238081	63.968628
1726.725269	68.724263	63.973633
1726.205421	61.984734	63.978638
1725.311362	62.383895	63.983642
1724.651332	56.855708	63.988647
1723.827927	63.936529	63.993652
1723.155933	65.924754	63.998657
1722.841678	62.609407	64.003662
1722.056353	60.119541	64.008666
1721.507978	47.891783	64.013671
1720.669729	61.245198	64.018676
1720.135449	60.784514	64.023681
1719.754085	61.064398	64.028686
1718.178224	61.133436	64.033690
1717.595945	57.811773	64.038695
1716.961154	64.080436	64.043700
1716.184361	56.834495	64.048705
1716.287276	60.628342	64.053710
1715.884255	73.743902	64.058714
1715.304727	63.143839	64.063719
1714.183901	71.722766	64.068724
1713.534483	71.436495	64.073729
1712.950438	60.821381	64.078734
1711.707909	65.768830	64.083738
1711.316363	56.518811	64.088743
1710.767258	60.455643	64.093748
1710.412733	54.468913	64.098753
1710.074048	53.224925	64.103758
1708.795212	66.362884	64.108762
1708.375652	57.087352	64.113767
1707.566900	63.971876	64.118772
1706.410728	59.345702	64.123777
1705.442384	56.905412	64.128782
1704.745044	63.064159	64.133786
1704.518370	65.803286	64.138791
1704.030664	68.587028	64.143796
1703.636775	62.918798	64.148801
1703.110558	66.579173	64.153806
1702.697257	68.461656	64.158810
1701.999010	59.772884	64.163815
1701.127852	68.181265	64.168820
1700.432102	66.339527	64.173825
1699.373774	64.109082	64.178830
1698.310159	68.028287	64.183834
1698.113915	57.162343	64.188839
1697.297305	59.796466	64.193844
1696.749683	62.189161	64.198849
1696.970055	59.791888	64.203854
1695.891449	67.709649	64.208858
1695.287349	62.603112	64.213863
1694.396521	54.648286	64.218868
1693.663060	60.642453	64.223873
1692.673762	63.218848	64.228878
1692.049440	67.531925	64.233882
1691.797824	64.364335	64.238887
1690.984321	69.841340	64.243892
1690.681362	62.010765	64.248897
1689.628675	67.584111	64.253902
1688.611450	70.037206	64.258906
1688.668149	56.995798	64.263911
1687.967890	66.449411	64.268916
1686.675245	66.448250	64.273921
1685.828399	61.895961	64.278926
1685.230027	71.286082	64.283930
1685.065657	62.752222	64.288935
1684.581720	63.671327	64.293940
1684.028349	62.354206	64.298945
1683.400939	65.781488	64.303950
1682.223946	69.884295	64.308954
1682.075879	62.888596	64.313959
1681.168605	58.112509	64.318964
1680.033131	64.298275	64.323969
1679.497451	54.317343	64.328974
1678.867298	61.305974	64.333978
1678.383149	65.076370	64.338983
1677.986376	66.383772	64.343988
1677.095434	63.134802	64.348993
1676.225073	63.691071	64.353998
1675.718107	65.192603	64.359002
1675.467071	56.817599	64.364007
1674.916625	62.366366	64.369012
1673.754374	64.848811	64.374017
1673.324941	65.066948	64.379022
1672.611070	69.648154	64.384026
1671.597583	64.119352	64.389031
1670.809358	64.571109	64.394036
1670.097570	66.639788	64.399041
1669.872244	61.171881	64.404046
1669.211570	68.248947	64.409050
1669.035382	60.160111	64.414055
1667.877450	62.416357	64.419060
1667.084525	54.404989	64.424065
1666.397833	58.450419	64.429070
1665.740416	69.983632	64.434074
1665.474834	54.320370	64.439079
1664.355485	62.490625	64.444084
1663.352444	64.331168	64.449089
1663.230523	64.593504	64.454094
1662.748730	63.623001	64.459098
1662.568628	58.979004	64.464103
1660.960959	65.091544	64.469108
1660.329854	62.402151	64.474113
1659.845629	67.629730	64.479118
1659.287781	74.490185	64.484122
1659.349593	61.805949	64.489127
1658.029829	70.804442	64.494132
1657.310437	67.626003	64.499137
1656.619859	63.889453	64.504142
1655.788868	70.555165	64.509146
1655.385514	55.697570	64.514151
1654.313364	53.051431	64.519156
1653.586124	58.670864	64.524161
1653.401003	59.774329	64.529166
1652.675823	61.029819	64.534170
1652.743419	58.314599	64.539175
1651.363829	60.000486	64.544180
1650.718051	57.124185	64.549185
1650.153688	55.173279	64.554190
1649.031819	63.594686	64.559194
1648.114308	59.031559	64.564199
1647.687581	64.007143	64.569204
1647.124299	66.056968	64.574209
1647.056914	56.151472	64.579214
1646.585448	65.844725	64.584218
1645.846058	58.706414	64.589223
1644.899043	71.400587	64.594228
1644.339593	63.289054	64.599233
1643.662773	58.783892	64.604238
1642.229667	58.007094	64.609242
1641.790620	57.946054	64.614247
1641.266642	62.301548	64.619252
1641.044888	61.482137	64.624257
1640.586879	62.056495	64.629262
1639.490828	66.441365	64.634266
1639.052741	59.942773	64.639271
1638.089395	65.599718	64.644276
1637.841314	63.464523	64.649281
1636.587711	49.946852	64.654286
1635.512712	58.073798	64.659290
1635.250842	56.230967	64.664295
1634.874665	58.358307	64.669300
1634.382811	71.527403	64.674305
1633.831836	68.120358	64.679310
1632.608603	67.961534	64.684314
1632.152447	69.514930	64.689319
1631.988571	62.200037	64.694324
1631.149033	58.302649	64.699329
1630.226106	54.000599	64.704334
1629.154938	63.888473	64.709338
1628.890266	57.565772	64.714343
1628.612804	68.751610	64.719348
1627.624070	61.779077	64.724353
1626.665284	60.016995	64.729358
1626.202661	65.778910	64.734362
1625.899502	52.215915	64.739367
1624.990244	61.597077	64.744372
1623.681048	64.423021	64.749377
1623.412830	58.495139	64.754382
1622.695516	69.913287	64.759386
1622.727186	57.298505	64.764391
1622.016562	55.463885	64.769396
1620.868218	63.742846	64.774401
1620.115946	63.212730	64.779406
1619.407786	64.531760	64.784410
1619.323934	54.622577	64.789415
1618.373697	57.473502	64.794420
1617.310412	63.665169	64.799425
1616.547158	57.325479	64.804430
1616.164260	61.592329	64.809434
1615.820572	63.268214	64.814439
1615.442039	69.040428	64.819444
1614.721095	64.166952	64.824449
1614.117789	61.495233	64.829454
1612.934064	74.778979	64.834458
1612.477540	64.496892	64.839463
1611.219759	67.010309	64.844468
1610.305813	73.020556	64.849473
1610.428374	62.539235	64.854478
1609.792335	62.042698	64.859482
1609.292248	57.220875	64.864487
1608.868893	59.757854	64.869492
1607.862836	69.249024	64.874497
1607.304220	65.087807	64.879502
1606.319718	73.151506	64.884506
1605.880411	58.042581	64.889511
1604.630244	62.841471	64.894516
1604.244750	66.096289	64.899521
1603.968185	67.875058	64.904526
1603.362699	66.078934	64.909530
1602.944755	57.946512	64.914535
1601.522916	61.936856	64.919540
1600.861312	60.278965	64.924545
1600.732522	53.548312	64.929550
1599.834450	62.451444	64.934554
1599.403484	56.584116	64.939559
1598.449142	58.363327	64.944564
1597.978355	61.647466	64.949569
1597.845033	54.296187	64.954574
1596.396783	62.794698	64.959578
1595.640132	62.850359	64.964583
1595.080493	67.802911	64.969588
1594.745345	59.111687	64.974593
1594.198005	61.665212	64.979598
1592.863519	61.405806	64.984602
1592.601869	50.608628	64.989607
1591.909686	55.392992	64.994612
1591.436709	64.523492	64.999617
1590.562430	52.445329	65.004622
1589.589555	61.169527	65.009626
1589.240432	54.945410	65.014631
1588.655746	54.188397	65.019636
1588.296258	59.927620	65.024641
1587.515415	45.513247	65.029646
1586.604790	62.946893	65.034650
1585.880768	62.956371	65.039655
1585.556687	67.493014	65.044660
1584.532945	65.323358	65.049665
1583.703685	55.635115	65.054670
1582.943901	67.403805	65.059674
1582.853102	53.073767	65.064679
1582.171308	61.538823	65.069684
1581.449821	69.600165	65.074689
1580.412899	64.347953	65.079694
1579.609151	62.856160	65.084698
1579.286943	70.819372	65.089703
1579.212418	66.790993	65.094708
1578.330941	70.100961	65.099713
1577.354423	61.372863	65.104718
1576.630411	67.679384	65.109722
1576.390230	63.723059	65.114727
1575.501339	60.191516	65.119732
1574.280210	60.090736	65.124737
1573.940539	58.952584	65.129742
1573.297548	65.487516	65.134746
1573.112551	63.440081	65.139751
1572.119080	62.975111	65.144756
1571.328094	60.943529	65.149761
1571.132657	59.112229	65.154766
1570.320529	72.269133	65.159770
1569.520275	55.583779	65.164775
1568.331667	66.829222	65.169780
1567.686598	61.569953	65.174785
1567.489227	54.563183	65.179790
1566.741297	49.124711	65.184794
1566.456113	52.213776	65.189799
1565.445799	59.862094	65.194804
1564.740063	57.916323	65.199809
1564.547915	47.994395	65.204814
1563.605345	61.621467	65.209818
1563.235412	54.569572	65.214823
1562.206401	56.877921	65.219828
1561.541616	60.314319	65.224833
1560.965786	48.805368	65.229838
1559.730174	71.460132	65.234842
1559.135583	50.941491	65.239847
1558.714384	66.662015	65.244852
1558.242923	59.304538	65.249857
1558.170959	53.910060	65.254862
1557.195711	58.444504	65.259866
1556.254009	53.976726	65.264871
1555.542512	65.819752	65.269876
1555.001474	57.801522	65.274881
1554.257180	56.312907	65.279886
1553.137823	73.910630	65.284890
1552.630017	58.617056	65.289895
1552.166363	54.439191	65.294900
1552.124529	55.196607	65.299905
1551.609335	53.597472	65.304910
1550.111511	57.405941	65.309914
1549.563995	52.992233	65.314919
1549.554191	60.763870	65.319924
1548.477937	57.416656	65.324929
1547.763488	54.444058	65.329934
1546.790814	58.304710	65.334938
1546.523766	55.193212	65.339943
1545.285377	57.902282	65.344948
1544.313759	65.181746	65.349953
1543.993442	50.427697	65.354958
1543.593740	61.099919	65.359962
1543.087737	57.479164	65.364967
1542.612614	58.870000	65.369972
1541.898017	56.790019	65.374977
1541.311143	50.903325	65.379982
1540.304814	64.012233	65.384986
1539.837429	48.699636	65.389991
1539.448627	54.730536	65.394996
1538.216531	51.742418	65.400001
1537.814847	52.336230	65.405006
1537.106918	55.790526	65.410010
1536.768830	51.763032	65.415015
1535.534916	53.435293	65.420020
1534.761808	49.581006	65.425025
1534.529286	50.975873	65.430030
1533.666871	65.754058	65.435034
1533.542737	55.807130	65.440039
1532.106777	53.524795	65.445044
1531.308645	46.430561	65.450049
1531.191005	58.470970	65.455054
1530.485195	52.524325	65.460058
1530.174312	61.588070	65.465063
1529.175735	61.820970	65.470068
1528.105315	57.977654	65.475073
1527.665589	48.864658	65.480078
1526.754695	59.160772	65.485082
1527.168874	52.876884	65.490087
1526.007301	61.749360	65.495092
1525.508329	58.176379	65.500097
1524.829811	43.367293	65.505102
1524.024592	47.694948	65.510106
1523.278892	49.204478	65.515111
1522.292939	50.974544	65.520116
1521.890655	53.169126	65.525121
1521.548018	49.225940	65.530126
1520.399591	55.718184	65.535130
1519.724249	45.491408	65.540135
1519.269847	46.177182	65.545140
1518.555250	56.751200	65.550145
1518.334121	60.265348	65.555150
1516.805861	67.037161	65.560154
1516.193926	54.354348	65.565159
1515.798407	51.941387	65.570164
1515.397989	52.583889	65.575169
1515.318248	53.391485	65.580174
1514.203314	60.373594	65.585178
1513.434113	58.261297	65.590183
1512.798499	64.008134	65.595188
1512.096950	51.743282	65.600193
1511.302034	51.798741	65.605198
1510.175442	64.013674	65.610202
1509.903063	57.228575	65.615207
1509.413827	58.331487	65.620212
1509.282751	54.569158	65.625217
1508.020762	49.225010	65.630222
1507.102098	54.012263	65.635226
1506.835843	48.563506	65.640231
1506.268949	52.550508	65.645236
1505.141800	53.814717	65.650241
1504.533207	52.366058	65.655246
1503.688246	65.301094	65.660250
1503.507549	59.370363	65.665255
1503.056420	55.796094	65.670260
1501.917299	59.017709	65.675265
1501.491235	44.925483	65.680270
1500.557016	54.629195	65.685274
1500.484285	48.569343	65.690279
1499.665532	54.271162	65.695284
1498.674623	60.050805	65.700289
1498.377512	55.212525	65.705294
1497.444571	57.395240	65.710298
1497.499387	57.093312	65.715303
1496.127481	58.120442	65.720308
1495.158799	58.957333	65.725313
1494.690575	60.739759	65.730318
1494.242988	56.832177	65.735322
1493.698335	54.020278	65.740327
1492.630313	66.284261	65.745332
1491.669937	53.324080	65.750337
1491.537799	52.443132	65.755342
1491.450944	65.920045	65.760346
1490.467118	57.311429	65.765351
1489.193848	51.221578	65.770356
1488.756690	57.115082	65.775361
1488.485668	56.445447	65.780366
1487.419093	59.713890	65.785370
1486.760778	56.363368	65.790375
1486.177851	59.187506	65.795380
1485.477316	62.427744	65.800385
1485.308298	57.550186	65.805390
1483.928722	52.909163	65.810394
1483.483828	59.319582	65.815399
1483.334592	61.901329	65.820404
1482.586073	55.524653	65.825409
1481.800866	54.217612	65.830414
1480.673277	66.420098	65.835418
1480.381542	56.611782	65.840423
1479.824705	52.380931	65.845428
1478.870545	63.193312	65.850433
1478.038925	54.268766	65.855438
1476.841709	51.002313	65.860442
1476.884375	60.987623	65.865447
1476.468923	63.990162	65.870452
1476.262005	58.544592	65.875457
1475.209561	61.746136	65.880462
1474.417356	61.123058	65.885466
1474.176073	52.861667	65.890471
1472.993448	49.990306	65.895476
1471.785129	57.996561	65.900481
1471.748410	52.910315	65.905486
1470.814200	66.010936	65.910490
1470.520170	55.968011	65.915495
1470.148521	51.884358	65.920500
1469.420351	62.186143	65.925505
1468.845761	51.236867	65.930510
1467.325229	57.696801	65.935514
1466.505575	53.198625	65.940519
1466.079401	55.027990	65.945524
1465.477067	57.445192	65.950529
1465.049323	56.045075	65.955534
1464.313503	53.027013	65.960538
1464.345605	50.323743	65.965543
1463.660010	57.283370	65.970548
1462.731414	58.213255	65.975553
1462.306548	54.959687	65.980558
1460.784499	63.200319	65.985562
1459.895725	50.599376	65.990567
1459.529200	49.396121	65.995572
1458.709859	53.845892	66.000577
1458.521753	55.487607	66.005582
1458.129228	55.639987	66.010586
1457.805424	51.458843	66.015591
1456.469674	51.914097	66.020596
1455.710476	59.437380	66.025601
1455.663988	49.826650	66.030606
1454.406128	62.018305	66.035610
1453.613816	52.999210	66.040615
1453.417870	54.057097	66.045620
1452.534841	48.411470	66.050625
1452.290020	56.792905	66.055630
1451.105341	48.577371	66.060634
1450.826229	48.424711	66.065639
1450.211977	40.309343	66.070644
1449.183838	55.616938	66.075649
1448.506274	51.766420	66.080654
1447.840695	62.812076	66.085658
1447.433045	52.873952	66.090663
1446.888860	55.859104	66.095668
1445.784609	51.822500	66.100673
1445.200183	46.567830	66.105678
1444.182535	58.506833	66.110682
1444.179222	51.459780	66.115687
1443.669707	58.683175	66.120692
1442.535612	51.885228	66.125697
1441.863568	50.941852	66.130702
1441.083397	62.297469	66.135706
1440.915133	54.488122	66.140711
1440.023207	59.946111	66.145716
1439.040104	62.004349	66.150721
1438.831039	56.778333	66.155726
1438.032615	58.398772	66.160730
1437.683905	55.855378	66.165735
1436.776677	54.597708	66.170740
1435.603086	61.579707	66.175745
1435.460040	54.233149	66.180750
1434.825550	63.786740	66.185754
1434.313917	63.044962	66.190759
1433.191641	64.641178	66.195764
1432.472664	64.413345	66.200769
1432.337376	50.929382	66.205774
1431.770385	58.001058	66.210778
1430.509925	56.988773	66.215783
1429.751677	60.162500	66.220788
1429.322829	61.221134	66.225793
1429.388424	55.771685	66.230798
1428.291717	61.087176	66.235802
1427.200932	58.065615	66.240807
1427.154096	55.855882	66.245812
1426.189481	59.966039	66.250817
1425.313755	55.358513	66.255822
1424.119108	60.714805	66.260826
1423.899463	57.833918	66.265831
1423.477045	64.764344	66.270836
1422.947845	63.265237	66.275841
1422.754219	55.882564	66.280846
1421.475652	65.588992	66.285850
1420.796559	54.900777	66.290855
1420.430902	58.770652	66.295860
1419.972332	64.375821	66.300865
1419.081988	52.670892	66.305870
1417.767826	57.749701	66.310874
1417.612822	50.468130	66.315879
1417.340941	52.552110	66.320884
1415.820889	67.840136	66.325889
1415.120738	57.924853	66.330894
1414.562838	65.042400	66.335898
1414.410262	54.087568	66.340903
1414.101461	58.500362	66.345908
1413.022867	67.099485	66.350913
1412.254881	55.241062	66.355918
1411.446722	55.002178	66.360922
1411.464675	53.767782	66.365927
1410.259555	56.463740	66.370932
1408.953878	60.654922	66.375937
1408.876318	48.272011	66.380942
1408.297812	57.345176	66.385946
1407.983308	55.455543	66.390951
1407.283466	50.118298	66.395956
1406.103347	55.511711	66.400961
1405.648020	48.167486	66.405966
1405.308574	62.879913	66.410970
1404.584423	58.235686	66.415975
1403.744990	58.689354	66.420980
1402.909705	51.619996	66.425985
1402.794155	52.538946	66.430990
1401.498108	57.204859	66.435994
1400.859732	53.546830	66.440999
1400.563088	54.545029	66.446004
1400.056506	56.311488	66.451009
1399.097729	51.851221	66.456014
1398.160680	61.859777	66.461018
1397.521963	53.753040	66.466023
1397.121538	59.271694	66.471028
1396.725913	60.635725	66.476033
1396.104910	50.635331	66.481038
1394.924040	56.681752	66.486042
1394.257557	60.120034	66.491047
1394.175259	63.656278	66.496052
1393.038899	55.275390	66.501057
1392.224314	60.574436	66.506062
1391.493560	68.528473	66.511066
1391.805227	52.406089	66.516071
1390.601419	55.857237	66.521076
1389.417477	56.652687	66.526081
1389.008941	48.313817	66.531086
1388.513631	64.853548	66.536090
1388.182114	60.132723	66.541095
1386.920822	60.339626	66.546100
1385.977564	54.317228	66.551105
1385.740895	56.125944	66.556110
1384.765178	65.011509	66.561114
1384.910606	53.895768	66.566119
1384.390843	55.769985	66.571124
1383.534777	62.904967	66.576129
1383.008128	46.545246	66.581134
1381.708900	59.420039	66.586138
1381.002531	52.323889	66.591143
1380.607514	52.210162	66.596148
1379.914764	61.265221	66.601153
1379.537465	56.129035	66.606158
1377.750366	65.242929	66.611162
1377.266998	60.631402	66.616167
1377.157863	58.095668	66.621172
1376.573553	56.207925	66.626177
1376.259653	49.147168	66.631182
1375.572374	61.162992	66.636186
1375.371067	52.428469	66.641191
1373.801835	56.264153	66.646196
1373.279779	59.179567	66.651201
1372.928562	50.079352	66.656206
1371.587793	59.962847	66.661210
1370.788729	53.772449	66.666215
1370.435096	52.081438	66.671220
1370.280353	60.691417	66.676225
1369.718638	52.036264	66.681230
1368.503007	58.725336	66.686234
1367.832812	55.507630	66.691239
1367.616234	58.085892	66.696244
1367.016791	61.111383	66.701249
1366.172319	53.330689	66.706254
1365.166636	56.088006	66.711258
1364.642282	46.952237	66.716263
1364.066149	51.451685	66.721268
1363.379436	57.712891	66.726273
1362.668918	51.432725	66.731278
1361.764505	57.849969	66.736282
1361.340077	54.388185	66.741287
1361.059579	64.081064	66.746292
1360.156001	54.914107	66.751297
1359.323309	48.043061	66.756302
1358.654705	54.946387	66.761306
1358.190997	48.690070	66.766311
1357.814062	56.800759	66.771316
1356.732616	63.504779	66.776321
1356.318183	58.011787	66.781326
1355.467873	62.911230	66.786330
1355.055905	56.804387	66.791335
1354.022722	57.722550	66.796340
1353.028935	56.297314	66.801345
1353.164807	49.018400	66.806350
1352.287974	58.610523	66.811354
1351.560024	47.665169	66.816359
1350.675322	56.107322	66.821364
1349.694782	62.066722	66.826369
1349.524823	55.125016	66.831374
1349.208086	60.554675	66.836378
1348.473577	47.107641	66.841383
1347.582093	54.013283	66.846388
1346.876403	48.016219	66.851393
1346.528497	50.202180	66.856398
1345.211932	60.554943	66.861402
1344.583865	58.484921	66.866407
1343.986608	53.360055	66.871412
1343.494605	56.396857	66.876417
1343.296550	54.646423	66.881422
1342.373528	57.038934	66.886426
1341.614685	59.328073	66.891431
1341.263152	56.435046	66.896436
1340.627765	61.120546	66.901441
1339.675942	52.962674	66.906446
1338.484072	66.410225	66.911450
1338.202028	54.830989	66.916455
1337.882349	57.901901	66.921460
1337.089731	59.680726	66.926465
1336.322313	55.686823	66.931470
1335.347502	63.085132	66.936474
1334.742791	61.213258	66.941479
1334.469395	57.729045	66.946484
1333.966896	58.648010	66.951489
1333.117576	61.626497	66.956494
1332.249312	64.027654	66.961498
1331.895453	55.970273	66.966503
1330.636139	61.411003	66.971508
1329.676928	55.201923	66.976513
1329.356822	55.833262	66.981518
1328.490382	56.128814	66.986522
1328.585529	56.310923	66.991527
1328.316051	56.256097	66.996532
1327.475562	55.874139	67.001537
1326.841819	45.074675	67.006542
1326.110714	56.556554	67.011546
1324.995417	55.095451	67.016551
1323.996947	55.465614	67.021556
1323.511629	55.954478	67.026561
1323.279312	58.180416	67.031566
1322.449672	57.605916	67.036570
1322.194658	48.738011	67.041575
1320.789294	50.041797	67.046580
1319.985818	65.922444	67.051585
1320.231973	57.241374	67.056590
1319.631306	57.439482	67.061594
1318.604813	57.331535	67.066599
1317.862111	49.687654	67.071604
1316.766466	64.031426	67.076609
1316.742325	46.185144	67.081614
1315.780531	63.346260	67.086618
1314.904105	49.614283	67.091623
1314.367027	56.301158	67.096628
1313.698782	51.763198	67.101633
1313.820314	45.598362	67.106638
1312.505678	58.466166	67.111642
1311.641160	50.398512	67.116647
1311.031019	52.544164	67.121652
1310.831806	51.369527	67.126657
1310.599919	42.382830	67.131662
1309.071386	59.771246	67.136666
1308.788262	55.526886	67.141671
1308.073503	59.826026	67.146676
1306.701502	62.499674	67.151681
1306.396187	54.505547	67.156686
1305.722475	60.176473	67.161690
1305.404002	53.430281	67.166695
1305.158009	52.124305	67.171700
1303.875711	48.513484	67.176705
1303.519209	52.668930	67.181710
1302.732028	63.942105	67.186714
1302.294393	51.479256	67.191719
1300.987653	48.807492	67.196724
1299.939418	63.156346	67.201729
1299.927827	48.728616	67.206734
1299.386320	56.605266	67.211738
1299.005865	51.592607	67.216743
1298.316599	57.209233	67.221748
1297.109089	56.248524	67.226753
1296.986793	56.928845	67.231758
1296.161685	66.539572	67.236762
1295.158886	56.953162	67.241767
1294.562536	57.623694	67.246772
1293.993078	60.534042	67.251777
1293.557773	61.402906	67.256782
1292.784692	60.740573	67.261786
1292.085511	55.261328	67.266791
1291.436406	54.897841	67.271796
1290.339704	66.166613	67.276801
1290.542227	56.863252	67.281806
1289.544032	57.181343	67.286810
1288.696894	54.138455	67.291815
1288.040901	58.007194	67.296820
1287.672481	55.984219	67.301825
1286.989835	51.032225	67.306830
1285.828744	63.356794	67.311834
1285.294689	54.416559	67.316839
1284.786426	58.725453	67.321844
1284.387116	63.652562	67.326849
1283.605466	51.755368	67.331854
1282.368846	56.470236	67.336858
1282.141803	56.411821	67.341863
1281.390593	55.719205	67.346868
1281.057838	56.992829	67.351873
1280.152762	50.245289	67.356878
1279.117708	51.083351	67.361882
1279.129051	51.121081	67.366887
1278.597897	50.904430	67.371892
1277.174810	56.666122	67.376897
1276.611425	47.366268	67.381902
1276.177037	58.138633	67.386906
1275.756501	47.300556	67.391911
1275.348503	47.988455	67.396916
1274.399220	54.087991	67.401921
1273.856886	42.184298	67.406926
1272.895820	60.545410	67.411930
1272.055769	45.669070	67.416935
1271.502651	50.743638	67.421940
1270.529931	51.281621	67.426945
1270.428722	51.189008	67.431950
1269.860364	58.186804	67.436954
1268.977342	57.371641	67.441959
1268.046843	53.758521	67.446964
1267.469142	58.109998	67.451969
1267.399482	52.571670	67.456974
1266.331552	65.368731	67.461978
1265.632575	54.174363	67.466983
1264.830082	58.443306	67.471988
1264.390636	62.607216	67.476993
1264.148494	54.951573	67.481998
1262.741574	51.384244	67.487002
1262.143016	48.752868	67.492007
1261.613595	55.971563	67.497012
1261.201298	64.480561	67.502017
1260.722381	45.009736	67.507022
1259.519433	58.173627	67.512026
1259.067497	53.881997	67.517031
1258.620526	57.640233	67.522036
1257.642426	51.517772	67.527041
1256.931438	51.113670	67.532046
1256.012677	59.107084	67.537050
1256.057884	48.936153	67.542055
1255.611748	54.558285	67.547060
1254.194949	51.140770	67.552065
1253.513986	42.014170	67.557070
1252.791832	56.066743	67.562074
1252.960717	50.944668	67.567079
1251.884544	53.352099	67.572084
1250.742596	53.918575	67.577089
1250.595772	45.113911	67.582094
1249.985821	54.218903	67.587098
1249.265471	48.750926	67.592103
1248.058974	57.474517	67.597108
1247.445853	53.960755	67.602113
1247.397238	43.331643	67.607118
1246.799193	59.327866	67.612122
1245.970898	43.691128	67.617127
1245.021738	42.426004	67.622132
1244.529469	58.214588	67.627137
1244.077113	45.292039	67.632142
1242.893732	53.307029	67.637146
1242.064730	53.099899	67.642151
1241.663245	54.029628	67.647156
1241.186378	55.218934	67.652161
1241.164737	44.199164	67.657166
1240.008066	48.522853	67.662170
1239.144795	47.955306	67.667175
1238.500357	50.227856	67.672180
1238.143478	55.201838	67.677185
1237.507968	52.049622	67.682190
1236.453612	60.808954	67.687194
1235.699012	57.522703	67.692199
1235.456173	52.245315	67.697204
1234.811400	53.805109	67.702209
1233.852554	51.762485	67.707214
1233.124801	58.258910	67.712218
1232.866461	52.810515	67.717223
1232.145679	53.734245	67.722228
1230.935217	56.853770	67.727233
1230.569382	45.535482	67.732238
1229.737682	55.129918	67.737242
1229.491396	52.598658	67.742247
1228.872761	56.316383	67.747252
1227.893256	56.369741	67.752257
1227.557822	50.684439	67.757262
1226.971896	50.932266	67.762266
1226.237381	57.142751	67.767271
1224.950269	54.433211	67.772276
1224.209909	66.402305	67.777281
1223.797093	54.689344	67.782286
1223.336826	58.836068	67.787290
1223.063541	48.040824	67.792295
1222.149779	62.488167	67.797300
1221.192938	61.896079	67.802305
1220.809915	51.130900	67.807310
1220.469118	54.842294	67.812314
1219.023888	51.449823	67.817319
1218.541837	54.380979	67.822324
1217.834199	57.914156	67.827329
1217.764291	54.036467	67.832334
1217.056910	57.807732	67.837338
1216.486665	57.400184	67.842343
1215.850660	61.372998	67.847348
1214.956345	63.235842	67.852353
1214.164369	48.266724	67.857358
1213.439409	67.493937	67.862362
1212.908471	59.851108	67.867367
1212.519745	60.875010	67.872372
1211.476188	54.797672	67.877377
1210.553432	53.099414	67.882382
1209.818112	52.563572	67.887386
1209.752763	49.877380	67.892391
1208.762170	58.214980	67.897396
1207.103692	53.120135	67.902401
1207.397591	49.011123	67.907406
1206.890106	55.051463	67.912410
1206.298714	48.146836	67.917415
1206.334784	59.894682	67.922420
1204.926704	59.576216	67.927425
1204.554035	55.604743	67.932430
1203.666827	61.748050	67.937434
1202.938819	65.129925	67.942439
1201.863821	53.255760	67.947444
1201.274068	51.370504	67.952449
1201.051549	50.880853	67.957454
1200.431596	46.199627	67.962458
1199.527255	42.856777	67.967463
1198.702340	43.065343	67.972468
1198.352297	49.038064	67.977473
1197.936107	35.706071	67.982478
1197.047259	51.866811	67.987482
1196.169792	43.323434	67.992487
1195.648061	40.504812	67.997492
1195.047878	44.501891	68.002497
1194.625814	46.310140	68.007502
1193.548592	54.711983	68.012506
1192.949567	46.384533	68.017511
1192.563854	39.191730	68.022516
1191.521288	44.908715	68.027521
1190.818153	41.822464	68.032526
1189.943418	41.647856	68.037530
1189.712382	44.751993	68.042535
1189.278934	43.912674	68.047540
1188.783476	47.390034	68.052545
1187.856915	39.854296	68.057550
1186.673350	39.519061	68.062554
1186.264391	43.296490	68.067559
1186.034182	42.666133	68.072564
1185.299496	40.740850	68.077569
1184.491821	37.985053	68.082574
1183.149024	54.862988	68.087578
1183.162384	42.495624	68.092583
1182.598377	54.630641	68.097588
1181.227732	52.727647	68.102593
1180.877477	50.370629	68.107598
1180.259164	55.165411	68.112602
1180.040104	55.709732	68.117607
1179.716280	44.432088	68.122612
1178.764807	52.325062	68.127617
1178.279435	43.066455	68.132622
1176.976080	55.669152	68.137626
1175.936665	54.293823	68.142631
1175.477637	48.705462	68.147636
1174.854162	61.980661	68.152641
1174.862597	52.096291	68.157646
1174.277419	50.297050	68.162650
1173.463409	41.052862	68.167655
1172.759364	59.399923	68.172660
1172.026243	58.318095	68.177665
1171.108656	45.444326	68.182670
1170.230454	57.553619	68.187674
1169.562454	49.319150	68.192679
1169.370164	51.652276	68.197684
1168.906902	59.357221	68.202689
1168.248953	50.219102	68.207694
1166.749738	53.496545	68.212698
1166.309723	48.400344	68.217703
1166.230451	55.016006	68.222708
1165.338659	48.550267	68.227713
1164.422963	46.570196	68.232718
1163.450271	53.780551	68.237722
1163.098736	46.583892	68.242727
1162.582865	48.765046	68.247732
1162.253463	59.071273	68.252737
1161.350621	43.247730	68.257742
1160.575284	55.184539	68.262746
1160.073122	47.188637	68.267751
1159.643962	49.948958	68.272756
1158.318649	51.891405	68.277761
1158.029332	51.267297	68.282766
1156.996968	55.602791	68.287770
1156.929706	55.231960	68.292775
1156.097417	48.941271	68.297780
1155.072931	49.451260	68.302785
1154.730009	40.438096	68.307790
1153.845162	44.720163	68.312794
1153.646403	42.572454	68.317799
1153.017682	44.024055	68.322804
1151.468369	47.527101	68.327809
1151.375714	40.827035	68.332814
1150.767134	51.606605	68.337818
1150.448589	52.349684	68.342823
1149.273053	47.168611	68.347828
1148.494257	43.909896	68.352833
1148.048335	44.737892	68.357838
1147.728646	54.069555	68.362842
1146.997209	49.390305	68.367847
1146.112896	46.712942	68.372852
1145.619618	45.870531	68.377857
1145.197954	40.451285	68.382862
1143.830468	51.734772	68.387866
1143.646560	45.776220	68.392871
1142.663787	49.807353	68.397876
1142.249294	54.071389	68.402881
1141.473509	39.464029	68.407886
1140.371019	45.688899	68.412890
1140.265590	42.796191	68.417895
1140.137356	50.189219	68.422900
1138.597728	56.032595	68.427905
1137.908643	48.236746	68.432910
1136.998965	51.720071	68.437914
1136.725523	46.400257	68.442919
1136.711197	44.866635	68.447924
1135.496531	44.388131	68.452929
1134.813287	39.589256	68.457934
1134.258786	44.452744	68.462938
1133.746563	49.976586	68.467943
1133.293011	46.879041	68.472948
1131.865382	46.790816	68.477953
1131.473406	49.966288	68.482958
1131.057941	50.773672	68.487962
1130.513715	46.936738	68.492967
1129.263108	51.215487	68.497972
1128.535969	41.413432	68.502977
1128.150780	56.095270	68.507982
1127.679547	43.726139	68.512986
1127.420617	49.424167	68.517991
1126.386575	42.949532	68.522996
1125.083143	52.655292	68.528001
1124.881622	42.932067	68.533006
1124.408839	52.215537	68.538010
1124.016580	55.849966	68.543015
1123.494824	41.651656	68.548020
1122.457994	51.267701	68.553025
1121.771888	49.035078	68.558030
1120.744858	56.265128	68.563034
1120.035257	41.111066	68.568039
1119.820107	48.316060	68.573044
1119.213265	57.909450	68.578049
1118.462003	46.160470	68.583054
1117.617567	59.863494	68.588058
1117.321338	48.062637	68.593063
1116.736934	52.296929	68.598068
1115.380827	49.864938	68.603073
1114.766585	50.167758	68.608078
1114.041917	44.202181	68.613082
1114.019467	45.648824	68.618087
1113.385820	57.941589	68.623092
1112.042493	54.238072	68.628097
1111.457766	46.550218	68.633102
1111.041978	59.757692	68.638106
1110.839369	41.760067	68.643111
1109.949787	51.142952	68.648116
1108.816172	55.748467	68.653121
1108.506486	48.811678	68.658126
1107.732071	55.432249	68.663130
1107.233925	53.459903	68.668135
1106.399880	40.320561	68.673140
1105.437186	46.671446	68.678145
1105.275499	47.559897	68.683150
1104.298394	49.628340	68.688154
1104.022066	42.556934	68.693159
1103.296240	39.673023	68.698164
1102.099989	52.788585	68.703169
1102.336714	48.505726	68.708174
1101.298025	49.973664	68.713178
1100.498540	46.735603	68.718183
1099.881545	50.063570	68.723188
1099.217255	49.158480	68.728193
1098.902049	46.262872	68.733198
1097.624887	53.252008	68.738202
1097.005357	50.486812	68.743207
1096.355421	54.603795	68.748212
1095.563924	46.147715	68.753217
1095.734898	43.182658	68.758222
1094.674357	46.106499	68.763226
1093.980700	42.455778	68.768231
1093.378059	49.583633	68.773236
1092.672902	40.348974	68.778241
1091.817366	38.753615	68.783246
1091.094952	35.151628	68.788250
1090.716138	47.168876	68.793255
1090.163454	39.587903	68.798260
1089.327936	44.387287	68.803265
1088.669607	41.368060	68.808270
1087.786312	46.411596	68.813274
1087.580252	46.136965	68.818279
1086.599178	44.451186	68.823284
1085.165969	54.153952	68.828289
1084.779622	35.931670	68.833294
1084.216971	57.173709	68.838298
1084.171274	34.756011	68.843303
1084.014054	43.842621	68.848308
1083.390648	43.930856	68.853313
1082.323516	38.320978	68.858318
1081.360141	48.439453	68.863322
1080.718021	48.907571	68.868327
1079.766453	46.751884	68.873332
1079.011011	37.924214	68.878337
1079.011237	46.697187	68.883342
1078.513828	51.848083	68.888346
1077.739018	41.899084	68.893351
1076.918237	45.007150	68.898356
1076.282910	44.543754	68.903361
1075.823419	38.286842	68.908366
1074.329106	47.437913	68.913370
1073.853920	43.821833	68.918375
1073.560213	45.759497	68.923380
1072.812460	36.530047	68.928385
1072.061898	51.465551	68.933390
1071.220951	41.016125	68.938394
1070.638568	38.744941	68.943399
1069.926694	35.507150	68.948404
1069.671354	47.742885	68.953409
1068.755620	38.052862	68.958414
1067.542690	38.939804	68.963418
1067.660030	40.684342	68.968423
1067.131631	40.604498	68.973428
1066.537665	41.602719	68.978433
1065.739474	42.302256	68.983438
1064.685146	41.129629	68.988442
1064.418726	37.202789	68.993447
1063.617534	36.869864	68.998452
1062.298159	45.483737	69.003457
1062.143160	33.204683	69.008462
1061.522253	39.603713	69.013466
1060.964287	33.980659	69.018471
1060.690831	46.323358	69.023476
1059.197375	42.601177	69.028481
1059.055501	38.427435	69.033486
1058.246620	36.108705	69.038490
1057.928326	38.654275	69.043495
1056.860187	32.997261	69.048500
1055.822071	44.676252	69.053505
1055.941543	36.956822	69.058510
1055.142720	44.923318	69.063514
1054.406245	46.740603	69.068519
1053.712428	38.658526	69.073524
1052.867267	42.847575	69.078529
1052.677822	49.192164	69.083534
1051.371685	39.147925	69.088538
1050.504007	47.000793	69.093543
1049.927873	42.232215	69.098548
1049.475772	33.614931	69.103553
1049.339909	36.517846	69.108558
1048.807623	43.054174	69.113562
1047.807955	32.016559	69.118567
1047.191583	34.126985	69.123572
1046.388995	43.519696	69.128577
1045.564398	29.675543	69.133582
1044.669957	42.687906	69.138586
1044.078802	39.569693	69.143591
1043.903173	39.302841	69.148596
1043.428937	47.463717	69.153601
1042.342340	33.872562	69.158606
1041.557852	41.377870	69.163610
1041.354978	39.489457	69.168615
1040.803072	37.243395	69.173620
1039.367153	40.562878	69.178625
1038.831416	38.703765	69.183630
1038.166985	49.642049	69.188634
1037.952028	46.167509	69.193639
1037.909642	39.285989	69.198644
1036.459284	54.577268	69.203649
1036.155314	45.442811	69.208654
1035.157748	39.440252	69.213658
1034.139566	47.272912	69.218663
1033.574707	42.933068	69.223668
1033.030459	56.490572	69.228673
1032.810421	42.073976	69.233678
1032.258670	47.728703	69.238682
1031.389204	47.275759	69.243687
1030.732081	49.058347	69.248692
1030.206140	46.708804	69.253697
1029.226517	44.674299	69.258702
1028.412890	51.048805	69.263706
1027.746872	51.407193	69.268711
1027.503885	40.063112	69.273716
1025.921198	41.499350	69.278721
1025.498645	38.595601	69.283726
1025.054534	42.243019	69.288730
1024.582488	44.071860	69.293735
1024.342802	36.439536	69.298740
1023.767810	43.159286	69.303745
1022.319721	33.470401	69.308750
1021.398713	48.407795	69.313754
1021.181644	50.661289	69.318759
1020.946926	36.753257	69.323764
1019.662155	42.037310	69.328769
1019.330964	40.006882	69.333774
1018.666864	43.120001	69.338778
1018.227054	43.391939	69.343783
1017.310690	40.140963	69.348788
1016.389191	44.679647	69.353793
1015.971278	49.089326	69.358798
1015.510626	50.487410	69.363802
1015.029970	46.757092	69.368807
1014.071730	36.110306	69.373812
1013.209086	50.360304	69.378817
1012.977054	40.487409	69.383822
1011.434419	48.010843	69.388826
1010.354995	41.336896	69.393831
1010.809415	33.384400	69.398836
1010.479503	45.611495	69.403841
1010.045551	36.425188	69.408846
1008.900005	34.210503	69.413850
1008.040625	41.076430	69.418855
1007.532834	37.467131	69.423860
1006.745298	38.693289	69.428865
1006.196670	36.038269	69.433870
1005.156634	40.621047	69.438874
1004.564393	38.157477	69.443879
1004.286626	39.163753	69.448884
1003.440607	36.396772	69.453889
1002.446146	30.393738	69.458894
1001.704607	37.193605	69.463898
1001.175509	42.278585	69.468903
1001.061075	25.839258	69.473908
1000.468320	35.993400	69.478913
1000.262467	38.707172	69.483918
999.081625	44.089821	69.488922
998.175967	47.809101	69.493927
997.016840	36.478324	69.498932
996.300409	52.523353	69.503937
995.971796	41.076203	69.508942
995.239464	48.896513	69.513946
994.876285	41.958799	69.518951
994.808156	34.316531	69.523956
993.585445	39.177545	69.528961
992.814452	39.700884	69.533966
992.402365	29.793568	69.538970
991.700637	40.379805	69.543975
990.711528	41.313176	69.548980
989.933876	51.949350	69.553985
989.512160	41.726581	69.558990
989.196028	39.365744	69.563994
988.529979	44.403129	69.568999
987.817285	38.689591	69.574004
986.978259	42.882413	69.579009
986.477026	40.021154	69.584014
985.205234	48.493445	69.589018
984.470230	45.527450	69.594023
984.538197	39.301758	69.599028
984.127605	52.030567	69.604033
983.101214	41.779426	69.609038
982.349200	42.227206	69.614042
981.685395	50.751001	69.619047
981.293013	42.117921	69.624052
980.149915	44.007809	69.629057
979.719559	34.488191	69.634062
978.846117	48.012911	69.639066
978.505869	37.474399	69.644071
977.701739	38.605432	69.649076
976.556205	48.581026	69.654081
976.236124	31.737588	69.659086
975.727947	36.346139	69.664090
975.050879	36.422439	69.669095
974.276603	37.100852	69.674100
973.165373	46.731931	69.679105
973.098574	37.714302	69.684110
972.461982	47.337671	69.689114
972.232329	43.909635	69.694119
970.991437	40.565231	69.699124
970.102951	42.778899	69.704129
969.873495	39.059087	69.709134
969.177371	46.917796	69.714138
968.514366	37.542434	69.719143
968.022750	32.640581	69.724148
967.003047	50.347144	69.729153
967.043861	39.259128	69.734158
965.715693	45.780176	69.739162
964.824896	47.817590	69.744167
964.749603	36.139326	69.749172
964.158063	55.868878	69.754177
963.079199	38.955355	69.759182
962.071684	33.900619	69.764186
962.021920	45.692039	69.769191
961.572125	45.202304	69.774196
960.211726	39.732192	69.779201
959.646986	35.663596	69.784206
958.576677	46.860444	69.789210
958.352547	39.449589	69.794215
958.343493	39.280821	69.799220
957.307816	39.657047	69.804225
956.437530	32.449942	69.809230
956.066095	40.040935	69.814234
955.254669	46.205364	69.819239
954.837350	44.395239	69.824244
953.746665	47.366510	69.829249
953.253701	45.828628	69.834254
952.473415	43.987947	69.839258
951.990484	52.112370	69.844263
951.118267	38.559693	69.849268
950.183669	49.307582	69.854273
949.949609	40.184101	69.859278
949.340267	48.448489	69.864282
948.649665	47.473509	69.869287
948.032062	45.892380	69.874292
947.128601	42.429638	69.879297
946.864483	42.813984	69.884302
946.361156	40.856692	69.889306
944.996823	39.706637	69.894311
944.602385	43.044953	69.899316
943.804025	45.048740	69.904321
944.011376	35.782480	69.909326
942.540471	43.893796	69.914330
941.749104	45.883855	69.919335
941.431349	48.631209	69.924340
941.099031	41.754830	69.929345
940.468322	46.411274	69.934350
939.469900	45.844836	69.939354
939.131676	49.787665	69.944359
937.874051	42.413534	69.949364
936.510888	51.422376	69.954369
936.461244	53.102011	69.959374
935.664599	38.285173	69.964378
935.420563	34.993478	69.969383
935.539137	46.507365	69.974388
933.879235	52.172864	69.979393
933.905056	37.690364	69.984398
932.987985	43.182458	69.989402
931.990090	48.111808	69.994407
931.177804	43.363495	69.999412
930.487199	33.828532	70.004417
930.632311	39.301413	70.009422
929.838338	42.233362	70.014426
928.594252	49.889110	70.019431
927.776148	40.316084	70.024436
927.406838	41.071998	70.029441
927.157667	39.990506	70.034446
926.165121	42.471492	70.039450
925.177908	45.580856	70.044455
924.831279	38.079111	70.049460
924.088514	44.868155	70.054465
924.044738	43.255643	70.059470
922.797161	43.230350	70.064474
921.907872	45.259652	70.069479
921.823879	39.966501	70.074484
920.844879	49.939268	70.079489
920.122713	42.946730	70.084494
919.220508	46.553518	70.089498
918.934014	44.262094	70.094503
918.782387	43.903120	70.099508
917.476220	29.585290	70.104513
916.705471	41.554517	70.109518
915.989488	42.622654	70.114522
915.659425	44.846825	70.119527
915.311629	42.877405	70.124532
914.235370	38.746715	70.129537
913.394693	41.135726	70.134542
912.712524	44.425215	70.139546
912.357546	37.194470	70.144551
911.812878	48.982642	70.149556
910.397958	49.816645	70.154561
909.794144	43.130140	70.159566
908.815765	44.213227	70.164570
908.913350	40.897132	70.169575
908.809616	46.267684	70.174580
908.210285	47.709934	70.179585
907.425701	52.140130	70.184590
906.660540	37.710971	70.189594
906.131715	42.300742	70.194599
905.255379	39.775173	70.199604
903.906540	46.195457	70.204609
903.953920	42.530948	70.209614
903.101254	42.677791	70.214618
901.983926	41.898472	70.219623
901.487241	42.546923	70.224628
900.905969	47.115080	70.229633
900.748465	43.886890	70.234638
899.786814	47.052121	70.239642
898.798632	41.972257	70.244647
898.317819	38.469081	70.249652
897.726931	44.581080	70.254657
897.588914	39.785400	70.259662
896.400183	37.926159	70.264666
895.868754	43.415240	70.269671
895.478359	36.488190	70.274676
894.441207	45.394699	70.279681
893.752478	38.885723	70.284686
893.048383	51.937220	70.289690
892.520566	47.623058	70.294695
892.449543	38.237092	70.299700
891.114237	44.218397	70.304705
890.428069	42.550422	70.309710
890.053705	42.416138	70.314714
888.814637	52.319915	70.319719
887.731369	41.724626	70.324724
887.421891	40.813591	70.329729
887.329957	34.540811	70.334734
886.454784	45.339182	70.339738
886.351437	35.860588	70.344743
885.475000	27.463856	70.349748
884.605358	39.838347	70.354753
884.297378	36.667225	70.359758
883.256455	29.671820	70.364762
882.282737	40.744500	70.369767
881.606046	32.858467	70.374772
881.295398	35.603116	70.379777
881.000537	31.201422	70.384782
879.815529	49.380602	70.389786
878.884749	48.849157	70.394791
878.730987	33.777065	70.399796
878.034332	41.257391	70.404801
877.576508	36.572539	70.409806
876.356336	43.478576	70.414810
875.677252	51.061771	70.419815
875.565047	43.216785	70.424820
874.925942	39.921740	70.429825
874.060787	41.248604	70.434830
873.325925	37.711748	70.439834
872.897979	39.330162	70.444839
871.919639	32.048824	70.449844
870.911887	46.982705	70.454849
870.440559	36.085025	70.459854
869.781110	48.744628	70.464858
869.587362	39.617901	70.469863
869.330335	41.901418	70.474868
867.949853	39.650072	70.479873
867.676124	33.705860	70.484878
866.596458	46.473344	70.489882
866.237598	37.229390	70.494887
865.241993	40.031017	70.499892
864.330776	36.088557	70.504897
864.315802	40.552394	70.509902
863.702095	41.085433	70.514906
862.470832	33.926358	70.519911
862.247555	42.851578	70.524916
861.220784	41.990053	70.529921
861.263480	32.980246	70.534926
859.950463	43.525023	70.539930
859.403885	38.638251	70.544935
858.991519	36.589228	70.549940
858.223417	50.620774	70.554945
857.226082	45.572346	70.559950
856.690117	41.390384	70.564954
855.805767	45.265594	70.569959
855.750448	36.957383	70.574964
854.969604	47.964684	70.579969
854.103296	42.531116	70.584974
853.257381	47.193444	70.589978
852.736321	53.363728	70.594983
852.570735	43.833537	70.599988
851.017548	39.580084	70.604993
850.831895	43.069690	70.609998
849.803946	34.184559	70.615002
849.471123	43.931487	70.620007
849.665743	41.951441	70.625012
848.454420	51.343021	70.630017
848.022610	34.093190	70.635022
847.192073	48.423264	70.640026
846.124120	38.092078	70.645031
845.407857	38.889033	70.650036
844.804571	49.841267	70.655041
844.621779	40.935158	70.660046
843.417339	41.204246	70.665050
842.389419	41.052564	70.670055
842.121057	36.367527	70.675060
841.455963	51.570165	70.680065
841.230388	36.703481	70.685070
840.480500	50.607547	70.690074
839.195948	41.291735	70.695079
838.740461	35.743899	70.700084
838.338592	41.478879	70.705089
838.231100	46.411621	70.710094
837.304330	45.190402	70.715098
836.290848	48.688768	70.720103
835.723210	41.701629	70.725108
835.117087	45.217160	70.730113
834.218979	34.130372	70.735118
833.289624	39.350051	70.740122
832.712105	36.176108	70.745127
832.550118	34.891509	70.750132
832.007875	42.227415	70.755137
830.995577	31.571982	70.760142
830.173710	39.127442	70.765146
829.414477	43.063172	70.770151
829.475998	49.602790	70.775156
828.584454	40.424709	70.780161
827.910107	33.730536	70.785166
827.329854	45.287826	70.790170
826.622106	37.055081	70.795175
825.705413	36.204436	70.800180
824.552173	47.933360	70.805185
824.461533	42.250177	70.810190
823.846363	37.814318	70.815194
823.317009	38.091080	70.820199
822.388257	39.402851	70.825204
821.461309	33.644627	70.830209
821.166612	37.258826	70.835214
820.743845	39.966133	70.840218
819.775226	36.516968	70.845223
819.051190	39.983459	70.850228
818.314846	44.719822	70.855233
818.266325	33.586120	70.860238
817.046478	45.748283	70.865242
816.030762	49.750078	70.870247
815.650198	40.687791	70.875252
815.079547	40.876508	70.880257
814.600356	45.909418	70.885262
814.164728	45.781743	70.890266
813.195313	46.092285	70.895271
812.778324	33.250991	70.900276
812.092295	48.098981	70.905281
811.493442	40.752530	70.910286
810.156255	48.891516	70.915290
809.600021	39.686878	70.920295
809.261327	39.848136	70.925300
808.692502	51.589700	70.930305
808.200730	49.021874	70.935310
807.362851	43.790387	70.940314
806.929394	44.133892	70.945319
806.164843	40.177569	70.950324
804.709708	45.206555	70.955329
804.531165	34.290678	70.960334
803.922812	46.976847	70.965338
803.665134	38.013280	70.970343
802.701089	30.917363	70.975348
801.564479	49.396376	70.980353
801.466933	37.437819	70.985358
800.953022	42.380059	70.990362
800.132327	40.976383	70.995367
799.155900	39.643232	71.000372
798.579815	40.099332	71.005377
798.345381	36.902323	71.010382
797.370968	41.848481	71.015386
796.498884	43.226937	71.020391
795.977316	48.624576	71.025396
795.194090	43.879573	71.030401
794.916289	31.288951	71.035406
794.009971	37.383365	71.040410
792.977636	45.092194	71.045415
792.722826	46.091683	71.050420
791.994303	46.015368	71.055425
791.801007	32.028261	71.060430
790.756520	48.863568	71.065434
790.026621	47.784498	71.070439
789.617473	45.517348	71.075444
789.179142	44.637876	71.080449
788.447338	39.630794	71.085454
787.321948	43.145414	71.090458
786.968356	44.857665	71.095463
786.176923	43.933476	71.100468
784.904606	44.774811	71.105473
784.572120	40.585707	71.110478
783.866119	39.348288	71.115482
783.497247	41.258520	71.120487
783.493242	39.045152	71.125492
782.444223	36.771054	71.130497
781.745666	31.719258	71.135502
780.925488	40.256935	71.140506
780.079661	34.903721	71.145511
779.642916	32.287719	71.150516
778.640766	44.077761	71.155521
778.464166	37.719118	71.160526
777.285524	42.593712	71.165530
776.349294	42.045826	71.170535
776.120151	40.201047	71.175540
775.256188	49.337076	71.180545
775.178465	36.545865	71.185550
774.780562	43.996000	71.190554
773.761736	43.866554	71.195559
772.874998	47.190220	71.200564
772.212366	41.154963	71.205569
771.422494	39.235442	71.210574
770.361089	44.074028	71.215578
769.638409	42.150118	71.220583
769.512059	40.356787	71.225588
768.798856	43.320080	71.230593
769.077647	42.731739	71.235598
767.882633	42.122548	71.240602
767.279301	40.611739	71.245607
766.832262	41.862613	71.250612
765.741726	42.482623	71.255617
764.882895	42.078543	71.260622
764.319253	47.479731	71.265626
763.567408	47.590069	71.270631
763.195606	36.643461	71.275636
761.914593	41.668403	71.280641
761.528139	34.931575	71.285646
761.069151	40.661463	71.290650
760.532011	40.064241	71.295655
760.105228	36.721236	71.300660
759.073922	50.077162	71.305665
758.500041	35.652316	71.310670
757.918052	44.688261	71.315674
756.784093	44.802663	71.320679
756.585142	37.600731	71.325684
755.634339	49.414148	71.330689
755.490349	34.029858	71.335694
754.303014	44.302349	71.340698
753.357231	41.707465	71.345703
753.101818	48.694936	71.350708
752.375928	44.943795	71.355713
752.173384	40.092170	71.360718
750.964265	41.834968	71.365722
750.199130	48.539301	71.370727
750.029699	35.098776	71.375732
749.532969	40.358420	71.380737
748.535944	44.708933	71.385742
747.382730	40.606343	71.390746
746.912294	45.134804	71.395751
746.904070	35.043403	71.400756
745.536271	43.958443	71.405761
744.854805	38.115435	71.410766
744.548397	37.377401	71.415770
743.895852	47.293511	71.420775
743.848335	43.991054	71.425780
742.584250	46.597343	71.430785
742.029196	39.742275	71.435790
741.269830	44.605328	71.440794
740.741831	45.165752	71.445799
739.655207	38.928342	71.450804
738.814289	52.580404	71.455809
738.461525	37.090577	71.460814
737.914050	39.874523	71.465818
737.320845	48.038599	71.470823
736.578802	40.344374	71.475828
735.863132	44.199074	71.480833
735.535934	40.244111	71.485838
734.987116	39.495785	71.490842
733.809127	39.595129	71.495847
733.300030	39.480742	71.500852
732.568148	44.345729	71.505857
732.138576	36.052962	71.510862
731.154216	41.257776	71.515866
730.110880	34.694926	71.520871
729.720122	43.301447	71.525876
728.845997	39.107123	71.530881
729.030058	41.703636	71.535886
728.797207	41.873285	71.540890
727.446362	46.466225	71.545895
727.180290	37.410966	71.550900
726.051527	32.514419	71.555905
725.047120	40.239321	71.560910
724.530922	36.662970	71.565914
724.021113	29.614622	71.570919
723.859428	37.370936	71.575924
722.523189	44.101544	71.580929
722.038070	40.603825	71.585934
721.452917	39.150059	71.590938
720.915360	45.001276	71.595943
720.352590	37.560799	71.600948
719.077870	39.232052	71.605953
718.608721	36.991817	71.610958
718.013187	50.048129	71.615962
717.581908	42.548867	71.620967
716.800555	43.083400	71.625972
715.831573	45.625369	71.630977
715.569111	32.376291	71.635982
714.838210	35.895942	71.640986
714.108266	37.970906	71.645991
713.433541	36.417860	71.650996
712.621248	39.818003	71.656001
712.365344	36.495110	71.661006
711.818482	32.922068	71.666010
711.000412	38.264419	71.671015
710.517058	29.051371	71.676020
709.817812	44.825596	71.681025
708.661152	31.542270	71.686030
707.959417	33.731020	71.691034
707.058934	43.626684	71.696039
707.020885	30.343456	71.701044
706.524642	36.957671	71.706049
705.510959	34.135492	71.711054
704.426293	32.173042	71.716058
703.868040	35.360844	71.721063
704.200368	32.245502	71.726068
702.970201	34.874793	71.731073
702.118270	37.631525	71.736078
701.610637	42.919721	71.741082
701.228684	38.304834	71.746087
700.663529	36.461523	71.751092
699.336182	43.704829	71.756097
699.035737	40.288101	71.761102
698.754369	43.327737	71.766106
697.436798	38.887056	71.771111
696.488372	38.402645	71.776116
695.841288	37.901794	71.781121
695.741093	32.560782	71.786126
695.401734	36.631547	71.791130
694.533438	30.137043	71.796135
693.944134	32.047689	71.801140
692.997768	35.921783	71.806145
692.575239	36.995296	71.811150
691.199302	34.237112	71.816154
690.618105	28.848108	71.821159
690.223360	26.293249	71.826164
689.412127	36.357634	71.831169
689.203870	32.859997	71.836174
688.779022	34.982585	71.841178
687.569484	35.716198	71.846183
687.120155	37.722833	71.851188
686.825259	32.141579	71.856193
685.605877	27.347796	71.861198
684.400019	37.432439	71.866202
683.752649	43.652818	71.871207
683.853361	38.469055	71.876212
683.298154	39.647277	71.881217
682.935213	29.874151	71.886222
681.734020	34.787067	71.891226
681.046903	37.982777	71.896231
680.548139	38.633179	71.901236
680.169523	42.696005	71.906241
679.124773	32.036356	71.911246
678.392353	40.008132	71.916250
677.574971	39.644793	71.921255
677.453063	35.590918	71.926260
676.080917	40.960004	71.931265
675.776159	46.636960	71.936270
675.297666	41.411379	71.941274
674.635728	40.617999	71.946279
673.711451	38.513326	71.951284
672.894499	31.957036	71.956289
672.623777	34.450912	71.961294
671.696239	42.269251	71.966298
671.376982	43.260089	71.971303
670.798286	33.589131	71.976308
669.904398	34.474346	71.981313
669.332909	39.321691	71.986318
669.100086	40.841254	71.991322
667.747455	44.056208	71.996327
667.221245	34.887841	72.001332
666.510703	35.232912	72.006337
666.278376	27.946425	72.011342
665.437148	38.394073	72.016346
664.805820	27.883075	72.021351
664.345903	32.400406	72.026356
663.008066	39.317380	72.031361
662.387370	34.420388	72.036366
662.049198	36.814615	72.041370
661.534118	34.383005	72.046375
660.658667	29.748939	72.051380
659.385979	39.095160	72.056385
659.177477	31.076304	72.061390
658.657288	34.540336	72.066394
658.234253	32.817913	72.071399
657.581887	27.567200	72.076404
656.659370	37.232197	72.081409
656.201931	29.973672	72.086414
655.530608	38.575985	72.091418
654.120691	35.769615	72.096423
653.562897	33.606591	72.101428
652.937621	36.953314	72.106433
653.219390	29.022762	72.111438
652.519660	35.419432	72.116442
651.579353	36.742566	72.121447
651.086290	29.536237	72.126452
650.152423	39.720301	72.131457
649.246631	39.000454	72.136462
648.304282	31.669335	72.141466
647.608103	45.124888	72.146471
647.208616	32.578912	72.151476
646.535011	44.084851	72.156481
646.454107	25.693458	72.161486
645.737421	44.811341	72.166490
644.860606	39.917290	72.171495
644.233424	30.089267	72.176500
643.465154	34.989242	72.181505
642.954452	29.129329	72.186510
642.077930	36.839410	72.191514
641.469806	30.398906	72.196519
641.212015	33.235299	72.201524
639.803670	36.328246	72.206529
639.161233	30.427810	72.211534
638.408167	30.316024	72.216538
637.881739	30.948760	72.221543
638.114248	34.363107	72.226548
637.368287	37.136100	72.231553
636.381643	26.975807	72.236558
635.861121	39.754448	72.241562
634.860771	30.536229	72.246567
634.095372	24.345498	72.251572
632.909217	33.155170	72.256577
633.030934	26.473859	72.261582
632.618670	27.151497	72.266586
631.224164	35.450286	72.271591
630.756972	22.017005	72.276596
630.258776	36.960462	72.281601
629.834362	22.578899	72.286606
629.342189	32.122537	72.291610
628.138193	29.584598	72.296615
627.928384	29.819975	72.301620
627.100395	34.819353	72.306625
626.552699	36.122550	72.311630
625.436042	30.870090	72.316634
624.772628	32.674278	72.321639
624.589254	27.583072	72.326644
623.396795	34.287670	72.331649
622.651500	28.732425	72.336654
622.164622	34.630776	72.341658
621.645826	26.274980	72.346663
621.582417	24.179893	72.351668
620.320229	37.377854	72.356673
619.671554	32.386769	72.361678
618.974197	37.303843	72.366682
618.365922	34.966723	72.371687
618.075379	31.075333	72.376692
616.670577	35.356786	72.381697
616.025414	31.269553	72.386702
615.474109	37.488047	72.391706
615.225832	35.901808	72.396711
614.948190	37.270813	72.401716
613.802832	37.210471	72.406721
613.139002	32.289612	72.411726
612.740453	43.274708	72.416730
611.581392	36.725615	72.421735
610.809819	28.926545	72.426740
610.151862	32.488222	72.431745
609.938363	27.196805	72.436750
609.474708	29.592098	72.441754
608.220674	39.279943	72.446759
607.651481	34.832884	72.451764
607.210019	47.009143	72.456769
606.667677	30.400712	72.461774
605.534875	33.117047	72.466778
604.709624	42.848575	72.471783
604.317199	39.011259	72.476788
603.622536	31.904861	72.481793
603.734914	36.236437	72.486798
602.912063	36.148391	72.491802
601.690950	33.859203	72.496807
601.459093	36.567675	72.501812
600.484843	45.212727	72.506817
599.583491	32.059911	72.511822
599.055272	39.971584	72.516826
598.348303	38.532519	72.521831
598.219609	34.332284	72.526836
597.661881	37.370207	72.531841
596.675310	28.771941	72.536846
595.791950	40.466625	72.541850
595.175243	38.662303	72.546855
594.435953	36.017251	72.551860
593.399983	45.274549	72.556865
592.862895	30.086165	72.561870
592.456613	41.717484	72.566874
592.011995	43.871623	72.571879
591.893619	38.302484	72.576884
590.989063	39.388127	72.581889
589.959026	32.257087	72.586894
589.606849	43.742592	72.591898
588.576383	35.417041	72.596903
587.882402	33.595854	72.601908
587.005145	40.465528	72.606913
586.346804	31.143975	72.611918
586.395568	37.005908	72.616922
585.603188	36.152901	72.621927
584.441455	32.759826	72.626932
583.829538	46.089212	72.631937
583.658496	28.596885	72.636942
582.557569	36.605293	72.641946
581.534543	36.301547	72.646951
581.208207	36.557064	72.651956
580.667771	44.489612	72.656961
580.383509	44.837779	72.661966
579.460010	42.510661	72.666970
578.647828	47.549329	72.671975
578.162712	35.517708	72.676980
577.799193	41.300224	72.681985
576.946457	30.327766	72.686990
575.683566	46.443311	72.691994
575.201116	39.063416	72.696999
575.000824	34.917954	72.702004
574.200152	42.390464	72.707009
573.729138	29.467175	72.712014
572.921894	26.456053	72.717018
572.440149	32.279474	72.722023
571.577905	32.664505	72.727028
570.505914	43.457235	72.732033
570.278863	37.722476	72.737038
569.571091	38.964447	72.742042
568.820341	38.396559	72.747047
568.105173	34.123365	72.752052
567.435520	38.980055	72.757057
566.901828	37.395126	72.762062
566.426820	35.520144	72.767066
565.093150	34.455306	72.772071
564.718761	28.872545	72.777076
563.835466	30.240247	72.782081
563.821338	23.546671	72.787086
563.394055	32.420795	72.792090
562.260345	28.993306	72.797095
561.883526	37.638616	72.802100
561.025328	29.513520	72.807105
560.051373	33.805226	72.812110
559.187085	40.501738	72.817114
558.618259	38.905060	72.822119
557.771778	42.804294	72.827124
557.385605	42.711366	72.832129
557.384969	37.887534	72.837134
556.778465	38.236566	72.842138
555.841083	42.311134	72.847143
555.452142	41.463264	72.852148
554.114236	38.921458	72.857153
553.333733	34.608211	72.862158
552.734952	40.633212	72.867162
552.289631	38.469644	72.872167
552.158822	36.919896	72.877172
551.260880	45.110460	72.882177
550.624329	34.016842	72.887182
549.721785	38.040128	72.892186
548.364908	40.161381	72.897191
548.246646	37.576700	72.902196
547.381944	42.533852	72.907201
547.062334	31.482796	72.912206
546.360522	30.689496	72.917210
545.560821	34.463005	72.922215
545.063990	34.163772	72.927220
544.064488	37.056025	72.932225
543.843561	30.165146	72.937230
543.557363	38.518471	72.942234
542.632545	27.410852	72.947239
541.691619	23.367600	72.952244
541.420763	35.127948	72.957249
540.752522	31.843952	72.962254
539.461821	38.546888	72.967258
538.871892	39.306458	72.972263
538.505790	33.047425	72.977268
537.732119	39.584424	72.982273
537.214714	33.324260	72.987278
536.263778	35.830301	72.992282
535.652126	38.544080	72.997287
535.353585	32.167050	73.002292
534.593724	42.589153	73.007297
533.723871	24.500872	73.012302
533.076004	39.352267	73.017306
532.580545	35.184439	73.022311
532.262988	33.465739	73.027316
530.897971	39.505561	73.032321
530.118718	30.399626	73.037326
529.873737	34.586263	73.042330
529.490116	40.658998	73.047335
529.008879	31.070339	73.052340
527.820676	33.811302	73.057345
527.508431	33.974693	73.062350
526.734810	35.570950	73.067354
525.574958	38.755266	73.072359
525.171340	33.014737	73.077364
524.248590	43.123734	73.082369
524.171880	35.230567	73.087374
523.105421	41.295377	73.092378
522.346572	29.221437	73.097383
522.013140	29.908613	73.102388
521.386022	31.369567	73.107393
521.170983	31.722483	73.112398
519.920580	35.260280	73.117402
518.915049	36.410921	73.122407
518.854427	33.265112	73.127412
518.246916	40.354406	73.132417
517.121025	36.175041	73.137422
516.568030	22.005604	73.142426
515.875211	39.418896	73.147431
515.564181	37.162978	73.152436
514.341889	35.974768	73.157441
513.633842	32.492111	73.162446
513.020267	34.554900	73.167450
512.604090	39.226140	73.172455
512.492220	36.916419	73.177460
511.881852	39.084357	73.182465
511.087701	40.325911	73.187470
510.288156	43.552189	73.192474
509.086311	34.994563	73.197479
508.413350	34.146214	73.202484
507.649538	39.006877	73.207489
507.081419	33.565378	73.212494
506.853198	40.914383	73.217498
506.556052	39.954124	73.222503
505.767030	31.613022	73.227508
504.938415	36.189110	73.232513
504.176296	27.364317	73.237518
503.122756	48.157818	73.242522
502.436593	36.384548	73.247527
501.820873	40.532474	73.252532
501.270262	34.616664	73.257537
501.194583	25.182613	73.262542
500.772384	40.892220	73.267546
499.447595	36.006514	73.272551
499.162757	27.570905	73.277556
497.874863	31.847987	73.282561
496.828475	35.682887	73.287566
496.362887	29.813462	73.292570
495.517703	31.706565	73.297575
495.561909	33.891657	73.302580
494.730268	31.996232	73.307585
494.876077	32.613373	73.312590
494.056059	26.740486	73.317594
493.024723	40.023936	73.322599
492.959198	22.025173	73.327604
491.250241	38.152660	73.332609
490.308009	37.243131	73.337614
489.918448	37.615968	73.342618
489.385831	42.909751	73.347623
489.242366	27.801421	73.352628
487.981531	40.150003	73.357633
487.481017	30.261645	73.362638
486.718305	38.588379	73.367642
486.359905	27.685451	73.372647
486.287063	33.787527	73.377652
485.051818	30.322634	73.382657
484.382256	37.508552	73.387662
483.810581	28.309642	73.392666
482.761151	38.774729	73.397671
482.349888	23.751646	73.402676
481.308038	40.709600	73.407681
481.313699	33.159718	73.412686
480.645980	33.245701	73.417690
479.477221	31.312522	73.422695
479.012450	27.392140	73.427700
478.335424	26.732110	73.432705
477.815298	32.987447	73.437710
477.066875	30.891107	73.442714
476.185417	35.901411	73.447719
476.026956	29.908943	73.452724
474.737287	33.487710	73.457729
473.947083	28.453774	73.462734
473.674600	18.721493	73.467738
472.954659	36.676862	73.472743
472.799127	31.827250	73.477748
471.794497	33.373591	73.482753
470.928056	37.976217	73.487758
470.411704	24.930088	73.492762
469.874525	38.489640	73.497767
469.615230	21.792813	73.502772
468.046433	35.314860	73.507777
467.667399	27.884619	73.512782
467.337209	30.671845	73.517786
466.655986	38.316954	73.522791
465.933158	18.588872	73.527796
465.037262	29.478941	73.532801
464.729515	29.236335	73.537806
463.561429	35.159655	73.542810
462.509285	28.293983	73.547815
462.075281	30.481143	73.552820
461.856443	39.206948	73.557825
461.414375	28.845650	73.562830
460.854380	38.013749	73.567834
459.763267	32.633509	73.572839
459.318093	31.324670	73.577844
458.784245	36.184978	73.582849
457.884568	39.252177	73.587854
457.005060	35.919860	73.592858
456.139213	41.001804	73.597863
456.191318	28.103236	73.602868
455.423729	37.886321	73.607873
454.681171	31.423926	73.612878
453.781840	22.242539	73.617882
453.212551	34.392639	73.622887
452.972634	35.446558	73.627892
451.740932	32.022119	73.632897
451.206131	21.033767	73.637902
450.639827	31.773556	73.642906
450.178315	33.591352	73.647911
449.226111	29.021641	73.652916
448.154371	38.391127	73.657921
447.926948	27.959364	73.662926
447.541912	37.757196	73.667930
446.699244	33.196843	73.672935
445.657723	24.673642	73.677940
444.719989	39.093398	73.682945
444.645528	33.439219	73.687950
444.565774	29.612048	73.692954
443.417451	29.998547	73.697959
442.714834	21.320425	73.702964
441.624676	33.288579	73.707969
441.489264	27.109512	73.712974
441.132800	23.982460	73.717978
439.945984	31.963599	73.722983
439.491604	21.170600	73.727988
438.607678	28.426948	73.732993
438.141414	26.359785	73.737998
437.381358	29.835263	73.743002
436.246173	36.409383	73.748007
436.561345	24.886627	73.753012
435.760707	32.900858	73.758017
434.983302	34.202847	73.763022
434.167095	33.006747	73.768026
433.642292	37.931853	73.773031
432.567611	34.605412	73.778036
431.528469	28.213937	73.783041
431.145859	27.595321	73.788046
430.533304	28.051007	73.793050
430.169845	33.089180	73.798055
430.196539	34.534295	73.803060
428.813128	41.494910	73.808065
428.136995	27.476013	73.813070
427.567555	28.251268	73.818074
426.765428	29.934100	73.823079
426.036237	27.599741	73.828084
425.130499	31.506876	73.833089
424.810166	33.135021	73.838094
424.363379	28.869578	73.843098
423.344640	35.614389	73.848103
422.831420	28.623442	73.853108
421.927951	29.745243	73.858113
421.533813	22.487737	73.863118
421.222697	29.354769	73.868122
419.955290	21.030006	73.873127
419.408168	27.043639	73.878132
418.533545	37.731635	73.883137
418.255863	24.904545	73.888142
418.073745	25.146566	73.893146
416.909748	31.045598	73.898151
416.219575	29.720610	73.903156
415.845646	31.489763	73.908161
415.133471	33.177190	73.913166
414.189299	31.664010	73.918170
413.444449	37.682345	73.923175
412.902548	27.775374	73.928180
412.503836	39.251734	73.933185
411.349214	27.922170	73.938190
410.688975	30.807724	73.943194
410.220767	20.688738	73.948199
409.898752	24.917616	73.953204
409.374692	36.286211	73.958209
408.187733	23.851598	73.963214
407.988223	31.894634	73.968218
407.284617	30.563904	73.973223
406.286843	23.068264	73.978228
405.036809	27.627946	73.983233
404.915111	28.582604	73.988238
404.373167	25.603388	73.993242
403.871633	23.298995	73.998247
403.197254	25.380959	74.003252
402.187751	34.462989	74.008257
401.613469	27.264154	74.013262
401.346010	34.283509	74.018266
400.245900	31.494161	74.023271
399.619179	18.339489	74.028276
398.927758	30.799220	74.033281
398.649299	32.829137	74.038286
398.262305	25.993132	74.043290
396.867961	33.912737	74.048295
396.668931	23.302995	74.053300
395.986164	26.387689	74.058305
395.031759	31.294519	74.063310
394.003908	29.274272	74.068314
393.310730	35.153487	74.073319
393.142461	28.698956	74.078324
392.890674	36.755055	74.083329
392.421770	33.973942	74.088334
391.438999	32.381764	74.093338
390.753254	28.876670	74.098343
389.970056	29.438407	74.103348
389.013467	42.050792	74.108353
388.468337	38.423939	74.113358
388.103097	37.045604	74.118362
386.815752	32.781644	74.123367
386.134838	21.991642	74.128372
385.312073	29.315531	74.133377
385.108896	30.585957	74.138382
384.722747	28.717356	74.143386
384.251428	23.448133	74.148391
383.612264	29.878574	74.153396
382.590491	33.632321	74.158401
382.282906	29.710569	74.163406
381.141153	27.121837	74.168410
380.073404	34.341262	74.173415
379.789147	29.742415	74.178420
379.331077	43.413955	74.183425
379.021286	32.944864	74.188430
378.093370	28.221500	74.193434
377.236402	41.026176	74.198439
376.720375	37.315839	74.203444
375.838501	40.834403	74.208449
375.259442	30.520191	74.213454
374.500245	30.127180	74.218458
373.871580	26.906317	74.223463
373.854755	31.148069	74.228468
372.312916	33.324120	74.233473
371.509966	28.697542	74.238478
371.168211	33.267048	74.243482
370.576739	36.840263	74.248487
370.684790	35.056917	74.253492
369.222843	35.056601	74.258497
368.864673	31.089293	74.263502
368.342772	33.850308	74.268506
367.269319	44.294031	74.273511
366.411292	31.575202	74.278516
365.436980	34.778906	74.283521
365.272429	38.832884	74.288526
364.976348	36.724422	74.293530
364.299409	34.930550	74.298535
363.772137	31.004384	74.303540
362.709817	34.534359	74.308545
362.189409	36.927698	74.313550
361.404899	32.917943	74.318554
360.359595	31.114964	74.323559
359.738678	27.392963	74.328564
359.026772	34.063666	74.333569
358.989658	33.777945	74.338574
358.595694	24.680073	74.343578
357.414368	33.464637	74.348583
357.044989	36.007378	74.353588
356.418970	41.894824	74.358593
355.928104	31.120274	74.363598
354.648946	25.431003	74.368602
354.078235	31.689687	74.373607
353.659977	19.201998	74.378612
352.865916	30.974753	74.383617
351.748703	26.846132	74.388622
351.332460	34.829088	74.393626
350.588090	36.304038	74.398631
350.547444	26.522216	74.403636
349.987707	35.978876	74.408641
348.801644	31.015958	74.413646
348.142044	29.060051	74.418650
347.599571	30.936500	74.423655
347.046785	27.403923	74.428660
346.252303	34.303837	74.433665
345.701412	34.715023	74.438670
345.416063	30.643072	74.443674
344.310438	33.178564	74.448679
343.569598	34.932082	74.453684
342.892405	39.870449	74.458689
342.411922	23.956403	74.463694
341.297135	29.893355	74.468698
340.422382	42.148926	74.473703
340.290993	34.362268	74.478708
339.564819	32.487938	74.483713
339.328353	29.234544	74.488718
338.088424	33.019921	74.493722
337.480607	29.401497	74.498727
337.343096	27.184189	74.503732
336.566880	29.384904	74.508737
335.655701	31.913065	74.513742
335.032224	29.147138	74.518746
334.134370	33.155552	74.523751
333.982675	25.212860	74.528756
332.701941	42.639441	74.533761
331.932312	35.519066	74.538766
331.425840	29.965290	74.543770
330.807326	30.226402	74.548775
330.709433	24.910295	74.553780
329.741835	26.985390	74.558785
328.895997	23.381249	74.563790
328.385898	32.620259	74.568794
327.940569	27.862583	74.573799
327.737535	28.426497	74.578804
326.438776	32.421534	74.583809
325.619781	25.294841	74.588814
325.292324	26.933593	74.593818
324.280797	32.524504	74.598823
323.584651	30.443539	74.603828
322.841402	32.922863	74.608833
322.373006	24.169609	74.613838
322.368118	25.179772	74.618842
321.365446	29.141814	74.623847
320.495896	18.858157	74.628852
319.463784	28.473682	74.633857
319.387493	19.514433	74.638862
318.285136	16.181423	74.643866
317.399150	24.024771	74.648871
316.710600	22.860408	74.653876
316.052760	36.412391	74.658881
315.974886	27.999029	74.663886
315.912126	23.904225	74.668890
314.501654	28.453249	74.673895
314.022007	18.233613	74.678900
313.377782	26.640844	74.683905
312.510990	21.534021	74.688910
311.746867	22.329291	74.693914
311.093578	25.309956	74.698919
311.065832	13.323032	74.703924
309.968644	30.715622	74.708929
309.272825	23.919398	74.713934
308.498914	20.395268	74.718938
307.909656	22.880014	74.723943
307.656010	21.614798	74.728948
306.349601	28.829707	74.733953
305.829418	16.359857	74.738958
305.447369	18.516680	74.743962
304.610897	31.259747	74.748967
303.880416	25.065152	74.753972
302.771476	25.710374	74.758977
302.432347	27.179097	74.763982
301.997030	26.556287	74.768986
301.782193	36.402694	74.773991
300.924349	26.509847	74.778996
299.961359	33.676333	74.784001
299.692326	26.676466	74.789006
298.743796	29.265788	74.794010
297.766906	36.484955	74.799015
297.473226	25.395140	74.804020
296.768231	28.270507	74.809025
296.305028	29.722736	74.814030
295.291154	24.968953	74.819034
294.568773	33.792358	74.824039
294.517923	20.946497	74.829044
293.386695	26.406681	74.834049
292.140331	21.399790	74.839054
291.668659	28.286111	74.844058
291.067344	25.645978	74.849063
291.033052	11.217340	74.854068
290.414282	23.275983	74.859073
289.769693	24.362875	74.864078
288.903042	30.403804	74.869082
288.121035	35.611207	74.874087
287.752346	25.022219	74.879092
286.414364	28.411653	74.884097
286.237573	24.558959	74.889102
285.595599	26.042838	74.894106
284.592796	28.137754	74.899111
283.876015	21.758054	74.904116
283.207540	28.776671	74.909121
282.793406	32.641767	74.914126
282.139815	27.630285	74.919130
281.739027	37.254012	74.924135
280.815273	12.387097	74.929140
280.063616	31.049293	74.934145
279.658473	23.161201	74.939150
279.468867	25.752568	74.944154
278.141523	19.948018	74.949159
277.468713	19.355184	74.954164
276.676033	26.608070	74.959169
276.291339	21.765049	74.964174
275.488853	23.479523	74.969178
274.609683	37.494155	74.974183
273.859905	26.152185	74.979188
273.446059	24.674382	74.984193
273.346907	24.422206	74.989198
272.475152	21.658025	74.994202
271.546483	29.071365	74.999207
271.281664	26.286136	75.004212
270.372956	26.349085	75.009217
269.264315	27.573031	75.014222
268.436679	24.167867	75.019226
268.171390	33.853575	75.024231
267.877714	20.384087	75.029236
267.292571	23.082657	75.034241
266.649993	28.089639	75.039246
265.928612	23.259285	75.044250
265.290938	30.739787	75.049255
264.155153	23.064359	75.054260
263.215637	32.775534	75.059265
262.869470	22.178234	75.064270
262.534121	23.633743	75.069274
261.685843	26.214983	75.074279
260.823530	16.059516	75.079284
260.159447	26.488470	75.084289
259.704580	19.209146	75.089294
259.138796	16.744714	75.094298
258.641068	21.233430	75.099303
257.768897	21.716348	75.104308
257.048403	18.085949	75.109313
256.621436	22.963942	75.114318
255.865901	22.349606	75.119322
254.624227	28.690027	75.124327
254.317365	24.733488	75.129332
253.937695	33.396613	75.134337
253.305248	21.293189	75.139342
252.599735	23.443232	75.144346
251.524252	24.113107	75.149351
251.502546	21.549332	75.154356
250.599013	22.627046	75.159361
249.306551	26.230021	75.164366
248.837607	24.877703	75.169370
248.218345	28.076893	75.174375
248.310737	14.631032	75.179380
247.574505	30.595694	75.184385
246.475811	25.685139	75.189390
245.956065	25.889527	75.194394
245.297148	26.127138	75.199399
244.427667	26.371506	75.204404
243.365112	32.899428	75.209409
242.971645	30.363374	75.214414
242.679571	31.244270	75.219418
242.255605	30.406768	75.224423
241.270655	21.390520	75.229428
240.227106	38.728854	75.234433
239.853296	35.481596	75.239438
239.689662	24.151864	75.244442
238.355115	39.125365	75.249447
237.826780	30.752280	75.254452
237.201307	40.345595	75.259457
236.748223	28.628328	75.264462
236.291958	27.296069	75.269466
235.137626	35.109682	75.274471
234.618082	27.654585	75.279476
234.102645	28.817100	75.284481
233.373324	22.677542	75.289486
232.593972	29.289634	75.294490
231.588183	30.317423	75.299495
231.562396	25.287883	75.304500
230.932137	30.430107	75.309505
230.005035	34.041083	75.314510
228.944983	22.109915	75.319514
228.187885	30.897864	75.324519
228.129461	19.680679	75.329524
227.651817	27.911556	75.334529
226.465928	19.356292	75.339534
226.045017	23.858000	75.344538
225.449074	35.154488	75.349543
224.770682	25.485388	75.354548
223.674739	27.197774	75.359553
222.996855	21.717088	75.364558
222.665705	26.851055	75.369562
222.228539	28.799052	75.374567
222.185267	22.446050	75.379572
220.829033	27.265603	75.384577
219.972354	29.986971	75.389582
219.540402	24.665781	75.394586
218.602686	28.404611	75.399591
217.875494	22.875016	75.404596
217.276790	29.136607	75.409601
216.876113	27.131576	75.414606
216.385943	14.838329	75.419610
215.286180	21.821631	75.424615
214.765714	22.062410	75.429620
214.106878	31.058631	75.434625
213.857800	24.375729	75.439630
212.982063	23.895690	75.444634
211.903228	38.773241	75.449639
211.623476	27.266476	75.454644
211.155514	26.478573	75.459649
210.450079	25.750605	75.464654
209.740763	29.672229	75.469658
208.820828	30.060275	75.474663
208.278463	28.284420	75.479668
207.019423	36.868539	75.484673
206.570519	33.806728	75.489678
206.156558	27.870798	75.494682
205.357301	24.700836	75.499687
205.450607	20.339881	75.504692
204.223547	28.102017	75.509697
203.668920	27.625983	75.514702
203.451606	24.765379	75.519706
202.244181	26.292115	75.524711
201.308133	17.176628	75.529716
200.808734	26.371363	75.534721
200.587515	29.434563	75.539726
199.648889	29.186910	75.544730
198.413956	34.122760	75.549735
198.245895	30.199296	75.554740
197.463985	31.719699	75.559745
197.054342	29.172039	75.564750
196.724741	22.166080	75.569754
195.492844	38.611912	75.574759
194.889661	19.052557	75.579764
194.146735	22.722492	75.584769
193.691971	25.513835	75.589774
192.825498	26.028985	75.594778
191.988548	30.644337	75.599783
191.593464	20.896969	75.604788
191.126708	31.365443	75.609793
190.769642	22.731677	75.614798
189.606796	18.687687	75.619802
188.787144	29.262885	75.624807
188.556826	26.981535	75.629812
187.913788	23.359309	75.634817
187.122962	18.084305	75.639822
186.421209	21.854913	75.644826
185.556018	25.440262	75.649831
185.432455	14.686069	75.654836
184.149169	18.919984	75.659841
183.414539	16.906701	75.664846
182.916087	18.585347	75.669850
182.408685	18.376185	75.674855
182.247437	14.049509	75.679860
181.052782	23.705181	75.684865
180.315201	27.424732	75.689870
180.021928	15.494353	75.694874
179.325257	23.362751	75.699879
178.549037	18.899148	75.704884
177.671867	17.846903	75.709889
177.195538	18.172119	75.714894
176.681230	16.100057	75.719898
175.696124	20.404710	75.724903
175.000184	11.749287	75.729908
174.289475	31.657096	75.734913
174.383525	26.136932	75.739918
173.536677	24.292934	75.744922
172.418857	23.316906	75.749927
171.847441	21.905246	75.754932
171.125555	27.256060	75.759937
170.141866	26.386384	75.764942
169.717541	27.671582	75.769946
168.891099	32.029794	75.774951
168.486745	22.835856	75.779956
168.044773	23.060976	75.784961
167.736495	17.841511	75.789966
166.888702	22.434942	75.794970
165.818629	22.731820	75.799975
165.573065	22.602343	75.804980
164.530489	20.799018	75.809985
163.804190	22.390990	75.814990
163.544001	19.709121	75.819994
162.667595	26.295701	75.824999
161.816057	11.896460	75.830004
160.540148	23.828076	75.835009
160.358561	26.877074	75.840014
160.118795	17.977028	75.845018
159.716221	27.135828	75.850023
159.127643	16.588249	75.855028
158.027588	27.184505	75.860033
157.461648	24.365300	75.865038
156.719901	17.907624	75.870042
155.599607	25.834110	75.875047
155.131814	20.758353	75.880052
154.417178	27.615618	75.885057
154.042894	21.121430	75.890062
154.024010	18.632905	75.895066
152.671346	33.282885	75.900071
151.886480	27.940707	75.905076
151.028083	32.069047	75.910081
151.005371	31.675375	75.915086
150.373185	24.236688	75.920090
149.044249	26.468814	75.925095
148.635579	21.434096	75.930100
148.094707	28.883414	75.935105
147.628958	21.367728	75.940110
146.595410	28.337347	75.945114
145.824551	23.450267	75.950119
145.772014	27.469039	75.955124
145.107519	33.187611	75.960129
143.895572	20.727187	75.965134
143.367546	21.716681	75.970138
142.725319	36.959882	75.975143
142.510964	16.173160	75.980148
141.057135	29.205510	75.985153
140.297181	10.932781	75.990158
140.043504	23.165045	75.995162
139.410755	25.308248	76.000167
139.297296	27.731358	76.005172
138.415759	26.266651	76.010177
137.438332	26.769548	76.015182
137.108710	13.222254	76.020186
136.282882	27.452331	76.025191
135.694695	16.469448	76.030196
134.597897	26.123730	76.035201
134.261829	24.824367	76.040206
134.002492	13.525694	76.045210
132.940012	20.626086	76.050215
132.067338	10.738846	76.055220
131.711740	19.270396	76.060225
130.736462	16.592165	76.065230
129.779614	9.473349	76.070234
128.834761	20.021208	76.075239
128.581044	15.050100	76.080244
128.162625	31.058720	76.085249
128.197311	19.068171	76.090254
127.692598	26.216827	76.095258
126.528521	19.299790	76.100263
126.118096	17.028244	76.105268
124.790480	19.473066	76.110273
123.976405	13.539459	76.115278
123.445333	11.228804	76.120282
122.741918	25.429901	76.125287
122.861309	14.819909	76.130292
121.978711	21.301828	76.135297
121.138734	18.810188	76.140302
120.660895	17.400968	76.145306
119.655777	26.698429	76.150311
118.812843	23.767281	76.155316
118.459871	19.725077	76.160321
118.082896	19.931957	76.165326
117.442377	19.177897	76.170330
116.100082	29.167807	76.175335
115.794985	26.721767	76.180340
114.911707	24.421542	76.185345
114.563128	35.975073	76.190350
113.564655	25.388784	76.195354
112.526056	29.903847	76.200359
112.774455	31.356179	76.205364
111.850963	36.895280	76.210369
110.962569	34.972771	76.215374
110.309415	28.705990	76.220378
109.324742	28.142432	76.225383
109.072982	27.673318	76.230388
108.810822	34.314937	76.235393
107.759361	31.196265	76.240398
107.001724	37.494262	76.245402
106.337440	37.002619	76.250407
106.041208	33.512775	76.255412
105.412580	39.533151	76.260417
104.288091	34.691435	76.265422
103.785543	38.692082	76.270426
103.399960	42.122131	76.275431
103.101564	27.095366	76.280436
101.335177	31.352744	76.285441
100.775625	42.682874	76.290446
100.704573	35.252491	76.295450
100.082040	35.782391	76.300455
99.571848	35.330834	76.305460
98.365692	36.953615	76.310465
97.883046	30.596567	76.315470
97.477055	29.150661	76.320474
96.370206	33.503146	76.325479
95.748885	23.580562	76.330484
95.169458	37.884907	76.335489
94.654875	37.938689	76.340494
94.121860	38.749213	76.345498
92.569208	35.546464	76.350503
92.290307	30.546256	76.355508
91.606463	37.568943	76.360513
91.391010	36.485323	76.365518
91.182120	31.636380	76.370522
90.014833	30.061137	76.375527
89.000003	27.244146	76.380532
88.464339	40.746713	76.385537
88.328528	37.576649	76.390542
87.456195	28.845298	76.395546
86.158423	40.991759	76.400551
85.967970	29.216888	76.405556
85.335271	29.194888	76.410561
84.950134	35.733115	76.415566
84.092610	33.004582	76.420570
83.276817	32.516607	76.425575
82.910069	27.257591	76.430580
82.349200	29.581738	76.435585
81.429008	27.965517	76.440590
80.667713	28.913375	76.445594
79.773389	32.580677	76.450599
79.534123	30.556239	76.455604
78.445481	27.304736	76.460609
77.869923	24.742558	76.465614
77.592370	22.686380	76.470618
76.803998	21.467042	76.475623
76.534059	21.462889	76.480628
75.473659	23.623843	76.485633
74.860825	21.983842	76.490638
74.607607	20.116176	76.495642
73.133874	31.060645	76.500647
72.584158	23.958925	76.505652
72.008191	26.995126	76.510657
71.437363	23.482848	76.515662
71.302592	24.937932	76.520666
69.858007	27.585945	76.525671
69.387063	17.240415	76.530676
68.699129	26.928865	76.535681
68.274587	24.085557	76.540686
67.368336	20.014902	76.545690
66.534749	23.175769	76.550695
66.432307	18.877573	76.555700
65.943396	23.423262	76.560705
64.959555	19.618877	76.565710
64.250404	19.501841	76.570714
63.237785	23.506564	76.575719
63.174556	11.665689	76.580724
62.246903	24.021207	76.585729
61.243653	24.966656	76.590734
60.757386	26.769541	76.595738
59.995935	31.834950	76.600743
59.924281	16.707391	76.605748
59.146208	30.910946	76.610753
57.912326	21.991263	76.615758
57.583890	23.000983	76.620762
56.931172	25.111119	76.625767
56.654850	20.020621	76.630772
55.468416	29.388022	76.635777
55.015372	22.868569	76.640782
54.549576	23.324596	76.645786
53.474430	25.861657	76.650791
52.676705	19.269442	76.655796
52.221343	27.389547	76.660801
51.778939	23.287500	76.665806
51.202562	13.496547	76.670810
49.998300	19.077286	76.675815
49.371245	23.107257	76.680820
48.884814	23.989208	76.685825
48.690567	26.688562	76.690830
48.203748	25.692382	76.695834
47.189315	25.218753	76.700839
46.651242	26.567845	76.705844
45.747743	25.956673	76.710849
44.881268	21.117998	76.715854
44.191486	16.508193	76.720858
43.409633	25.462556	76.725863
43.196307	22.508294	76.730868
42.618573	27.176966	76.735873
41.680917	26.501855	76.740878
40.953914	19.046792	76.745882
40.515619	26.061861	76.750887
40.045796	22.817340	76.755892
38.762135	25.381356	76.760897
38.323076	29.859174	76.765902
38.029012	31.954692	76.770906
37.391308	21.337716	76.775911
36.401405	20.861756	76.780916
35.683045	21.343875	76.785921
34.869416	21.722915	76.790926
34.693381	15.380069	76.795930
33.544916	19.362313	76.800935
32.722063	15.218447	76.805940
32.282796	15.104108	76.810945
31.678608	17.947693	76.815950
31.817364	12.451946	76.820954
30.561181	25.355046	76.825959
29.879477	16.025609	76.830964
29.019708	24.637580	76.835969
28.961083	19.427207	76.840974
28.181415	12.858934	76.845978
27.099892	15.499525	76.850983
26.879380	21.005375	76.855988
26.309356	20.270058	76.860993
24.786473	23.763233	76.865998
24.242685	21.560287	76.871002
23.920706	24.022965	76.876007
23.567116	17.591741	76.881012
22.731571	20.426497	76.886017
21.624419	18.756541	76.891022
21.458321	10.962861	76.896026
20.599417	25.753333	76.901031
20.218284	19.094685	76.906036
19.210723	25.812615	76.911041
18.539305	23.205817	76.916046
18.090400	20.481525	76.921050
17.344670	23.076448	76.926055
16.394506	15.694837	76.931060
15.626819	23.180348	76.936065
15.235228	23.747551	76.941070
14.775719	19.823287	76.946074
14.123795	23.513448	76.951079
13.421097	17.727704	76.956084
12.777982	16.721767	76.961089
12.192171	23.948029	76.966094
11.872721	11.512504	76.971098
10.746648	27.536218	76.976103
10.002297	15.759833	76.981108
9.715820	18.797180	76.986113
8.424985	22.792682	76.991118
7.540778	18.027816	76.996122
6.849801	20.457887	77.001127
6.834814	17.036746	77.006132
6.196625	16.022141	77.011137
5.335516	23.188233	77.016142
4.572700	12.278988	77.021147
3.955981	23.187714	77.026151
3.620444	26.515170	77.031156
3.265511	24.670044	77.036161